Fri Mar 12 13:07:23 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.888087	0.020567	0.000000	0.000027	0.720219

0.852058	0.030303	0.005005	0.000034	0.720225
0.982586	-0.095964	0.010010	0.000009	0.720022
0.919930	-0.146172	0.015014	0.000021	0.719901
0.810746	-0.130023	0.020019	0.000042	0.719894
0.961628	-0.155714	0.025024	0.000014	0.719896
1.087127	-0.175656	0.030029	-0.000010	0.719901
0.848808	-0.138807	0.035034	0.000035	0.719890
0.984787	-0.156932	0.040038	0.000010	0.719902
1.004151	-0.164152	0.045043	0.000006	0.719894
1.041290	-0.169309	0.050048	-0.000001	0.719897
0.901205	-0.143657	0.055053	0.000025	0.719898
1.050359	-0.171614	0.060058	-0.000002	0.719895
1.020834	-0.163750	0.065062	0.000003	0.719900
0.899736	-0.145718	0.070067	0.000026	0.719893
1.099474	-0.178445	0.075072	-0.000011	0.719899
1.159210	-0.283942	0.080077	-0.000022	0.719711
0.957296	-0.306116	0.085082	0.000015	0.719597
1.049966	-0.319619	0.090086	-0.000002	0.719602
1.042277	-0.322059	0.095091	-0.000000	0.719595
0.969326	-0.306185	0.100096	0.000013	0.719600
0.991040	-0.309031	0.105101	0.000009	0.719602
1.167379	-0.395988	0.110106	-0.000023	0.719493
1.148089	-0.503662	0.115110	-0.000020	0.719273
0.940472	-0.470928	0.120115	0.000019	0.719265
0.966438	-0.473583	0.125120	0.000014	0.719269
1.137391	-0.501702	0.130125	-0.000017	0.719273
1.009424	-0.556199	0.135130	0.000007	0.719120
1.047829	-0.643238	0.140134	-0.000000	0.718962
0.922659	-0.624711	0.145139	0.000023	0.718955
0.837512	-0.606667	0.150144	0.000039	0.718960
0.808442	-0.628791	0.155149	0.000044	0.718906
0.847516	-0.771520	0.160154	0.000037	0.718638
0.849809	-0.766599	0.165158	0.000037	0.718648
0.810264	-0.763755	0.170163	0.000044	0.718640
0.977947	-0.849413	0.175168	0.000013	0.718530
0.866446	-0.917986	0.180173	0.000034	0.718355
0.777301	-0.905753	0.185178	0.000051	0.718348
0.677019	-0.882565	0.190182	0.000070	0.718358
0.816269	-1.067211	0.195187	0.000044	0.718042
1.059138	-1.122961	0.200192	-0.000001	0.718017
1.097773	-1.127164	0.205197	-0.000008	0.718022
0.872596	-1.229808	0.210202	0.000034	0.717740
0.855497	-1.242171	0.215206	0.000037	0.717710
0.788890	-1.235922	0.220211	0.000049	0.717698
0.463497	-1.331701	0.225216	0.000110	0.717394
0.614552	-1.364614	0.230221	0.000082	0.717382
0.587931	-1.375471	0.235226	0.000087	0.717351
0.619586	-1.513546	0.240230	0.000081	0.717089
0.586272	-1.511447	0.245235	0.000088	0.717081
0.525380	-1.565148	0.250240	0.000099	0.716954
0.212222	-1.609867	0.255245	0.000158	0.716755
0.313916	-1.630671	0.260250	0.000139	0.716749
0.263339	-1.730768	0.265254	0.000148	0.716533
0.112249	-1.748840	0.270259	0.000176	0.716444
0.243119	-1.798727	0.275264	0.000152	0.716391
0.286507	-1.936902	0.280269	0.000144	0.716132
0.184883	-1.921447	0.285274	0.000163	0.716127
0.245450	-2.021907	0.290278	0.000152	0.715949
0.191940	-2.050510	0.295283	0.000162	0.715874
-0.522588	-1.986047	0.300288	0.000295	0.715749
-1.030283	-1.999399	0.305293	0.000390	0.715543
-0.927963	-2.020391	0.310298	0.000371	0.715537
-0.543740	-2.201062	0.315302	0.000300	0.715315
-0.885756	-2.184491	0.320307	0.000363	0.715227
-0.900207	-2.229258	0.325312	0.000366	0.715133
-1.001413	-2.323664	0.330317	0.000385	0.714909
-1.215062	-2.289976	0.335322	0.000425	0.714901
-1.355420	-2.388732	0.340326	0.000451	0.714655
-2.221774	-2.261641	0.345331	0.000612	0.714600
-2.200202	-2.291477	0.350336	0.000609	0.714549
-2.660965	-2.346368	0.355341	0.000694	0.714277
-2.890992	-2.308538	0.360346	0.000737	0.714270
-3.187179	-2.286190	0.365350	0.000793	0.714210
-3.833489	-2.293225	0.370355	0.000913	0.713967
-3.764942	-2.303678	0.375360	0.000900	0.713970
-4.117445	-2.237505	0.380365	0.000966	0.713977
-4.456856	-2.318765	0.385370	0.001029	0.713695
-4.875571	-2.264116	0.390374	0.001107	0.713655
-5.315186	-2.187802	0.395379	0.001189	0.713651
-5.125323	-2.221165	0.400384	0.001154	0.713652
-5.126479	-2.354461	0.405389	0.001154	0.713386
-5.861486	-2.239131	0.410394	0.001291	0.713355
-6.062299	-2.199396	0.415398	0.001329	0.713363
-5.815747	-2.245687	0.420403	0.001283	0.713358
-6.150488	-2.307564	0.425408	0.001345	0.713116
-6.822860	-2.230724	0.430413	0.001470	0.713030
-6.889661	-2.225184	0.435418	0.001483	0.713017
-6.586853	-2.273731	0.440422	0.001427	0.713028
-6.668997	-2.267889	0.445427	0.001442	0.713010
-7.800242	-2.216757	0.450432	0.001653	0.712711
-7.685523	-2.235793	0.455437	0.001631	0.712713
-7.921761	-2.196845	0.460442	0.001675	0.712707
-7.635617	-2.243760	0.465446	0.001622	0.712715
-7.789497	-2.221642	0.470451	0.001651	0.712704
-7.938378	-2.295274	0.475456	0.001679	0.712505
-8.659442	-2.224488	0.480461	0.001813	0.712390
-8.899539	-2.186926	0.485466	0.001858	0.712379
-8.302013	-2.289836	0.490470	0.001747	0.712386
-8.690521	-2.221128	0.495475	0.001819	0.712385
-8.854789	-2.193276	0.500480	0.001850	0.712382
-8.690947	-2.343618	0.505485	0.001819	0.712141
-9.238062	-2.273518	0.510490	0.001921	0.712086
-9.605544	-2.203306	0.515494	0.001990	0.712095
-9.729763	-2.185135	0.520499	0.002013	0.712087
-9.650234	-2.199079	0.525504	0.001998	0.712087
-9.329391	-2.253397	0.530509	0.001939	0.712093
-10.426946	-2.224456	0.535514	0.002143	0.711761
-10.571770	-2.196895	0.540518	0.002170	0.711764
-10.306047	-2.246953	0.545523	0.002121	0.711758
-10.552185	-2.204158	0.550528	0.002167	0.711756
-10.413790	-2.226634	0.555533	0.002141	0.711760
-10.500266	-2.215578	0.560538	0.002157	0.711752
-10.452251	-2.282429	0.565542	0.002148	0.711635
-11.491375	-2.190458	0.570547	0.002342	0.711449
-11.212485	-2.240005	0.575552	0.002290	0.711449
-11.100148	-2.257017	0.580557	0.002269	0.711455
-11.863050	-2.126519	0.585562	0.002411	0.711444
-11.044799	-2.265094	0.590566	0.002259	0.711459
-10.929439	-2.288867	0.595571	0.002238	0.711452
-12.019803	-2.240664	0.600576	0.002441	0.711160
-12.091553	-2.238603	0.605581	0.002454	0.711139
-12.216023	-2.220146	0.610586	0.002477	0.711131
-12.221024	-2.213903	0.615590	0.002478	0.711142
-12.533245	-2.161285	0.620595	0.002536	0.711136
-12.543476	-2.160565	0.625600	0.002538	0.711133
-11.876540	-2.275977	0.630605	0.002414	0.711140
-12.930414	-2.224782	0.635610	0.002611	0.710867
-13.028823	-2.206353	0.640614	0.002629	0.710869
-12.822950	-2.245198	0.645619	0.002591	0.710864
-13.102731	-2.194370	0.650624	0.002643	0.710866
-12.969007	-2.214845	0.655629	0.002618	0.710873
-13.248720	-2.168526	0.660634	0.002670	0.710866
-13.050418	-2.252388	0.665638	0.002634	0.710769
-14.393207	-2.133136	0.670643	0.002884	0.710529
-13.983182	-2.206173	0.675648	0.002807	0.710529
-13.778713	-2.240507	0.680653	0.002769	0.710533
-14.332815	-2.145366	0.685658	0.002873	0.710525
-13.997502	-2.200243	0.690662	0.002810	0.710535
-13.735596	-2.251652	0.695667	0.002762	0.710525
-14.031031	-2.229921	0.700672	0.002817	0.710463
-14.651056	-2.242889	0.705677	0.002932	0.710217
-14.722838	-2.232682	0.710682	0.002946	0.710211
-14.935316	-2.190136	0.715686	0.002985	0.710221
-15.116023	-2.160557	0.720691	0.003019	0.710215
-15.078046	-2.168308	0.725696	0.003012	0.710213
-14.424008	-2.281942	0.730701	0.002890	0.710219
-14.827306	-2.267297	0.735706	0.002965	0.710104
-15.899019	-2.182288	0.740710	0.003165	0.709892
-15.296706	-2.291393	0.745715	0.003053	0.709889
-15.988531	-2.168615	0.750720	0.003182	0.709887
-15.765020	-2.203613	0.755725	0.003140	0.709897
-15.862410	-2.190949	0.760730	0.003158	0.709887
-15.684032	-2.219545	0.765734	0.003125	0.709894
-15.761057	-2.257825	0.770739	0.003140	0.709790
-16.651632	-2.197942	0.775744	0.003306	0.709592
-16.187083	-2.277891	0.780749	0.003219	0.709597
-16.984830	-2.137716	0.785754	0.003368	0.709593
-16.716015	-2.182275	0.790758	0.003318	0.709600
-16.361664	-2.249063	0.795763	0.003252	0.709592
-16.670634	-2.194201	0.800768	0.003310	0.709592
-16.858058	-2.229248	0.805773	0.003345	0.709455
-17.805453	-2.159147	0.810778	0.003521	0.709257
-17.067103	-2.285751	0.815782	0.003384	0.709267
-17.474917	-2.216665	0.820787	0.003460	0.709260
-17.747617	-2.167096	0.825792	0.003510	0.709261
-17.222228	-2.258672	0.830797	0.003413	0.709265
-17.650179	-2.186934	0.835802	0.003492	0.709256
-17.774014	-2.218693	0.840806	0.003516	0.709148
-18.478133	-2.190147	0.845811	0.003647	0.708954
-18.196198	-2.241767	0.850816	0.003594	0.708951
-18.482347	-2.186876	0.855821	0.003648	0.708959
-18.738735	-2.145906	0.860826	0.003695	0.708949
-18.278517	-2.224348	0.865830	0.003610	0.708956
-18.447122	-2.195398	0.870835	0.003641	0.708954
-18.523708	-2.200040	0.875840	0.003656	0.708917
-18.777553	-2.292319	0.880845	0.003703	0.708642
-19.072900	-2.243116	0.885850	0.003758	0.708635
-19.551407	-2.155501	0.890854	0.003847	0.708639
-19.132784	-2.231599	0.895859	0.003769	0.708636
-19.218392	-2.217596	0.900864	0.003785	0.708633
-19.280300	-2.203802	0.905869	0.003797	0.708639
-19.515743	-2.200112	0.910874	0.003841	0.708562
-19.768815	-2.262346	0.915878	0.003888	0.708347
-20.022513	-2.218071	0.920883	0.003935	0.708345
-20.591611	-2.116256	0.925888	0.004041	0.708345
-19.652275	-2.279944	0.930893	0.003867	0.708353
-20.001919	-2.222191	0.935898	0.003932	0.708343
-20.561462	-2.119898	0.940902	0.004036	0.708348
-20.147113	-2.242833	0.945907	0.003959	0.708250
-21.174056	-2.179505	0.950912	0.004150	0.708010
-20.838582	-2.236541	0.955917	0.004088	0.708015
-21.135794	-2.186883	0.960922	0.004143	0.708008
-20.946616	-2.217260	0.965926	0.004108	0.708015
-20.965800	-2.214744	0.970931	0.004112	0.708013
-21.191659	-2.177881	0.975936	0.004154	0.708006
-21.182153	-2.212090	0.980941	0.004152	0.707941
-21.923029	-2.204828	0.985946	0.004290	0.707690
-21.928669	-2.199666	0.990950	0.004291	0.707699
-21.977424	-2.192578	0.995955	0.004301	0.707695
-21.997088	-2.189781	1.000960	0.004304	0.707694
-21.995299	-2.187577	1.005965	0.004304	0.707699
-22.136710	-2.164130	1.010970	0.004330	0.707695
-21.514646	-2.292215	1.015974	0.004215	0.707660
-22.452379	-2.267432	1.020979	0.004389	0.707374
-23.025455	-2.166730	1.025984	0.004496	0.707371
-22.682989	-2.225757	1.030989	0.004432	0.707375
-22.675276	-2.231262	1.035994	0.004431	0.707367
-22.737730	-2.214613	1.040998	0.004443	0.707378
-22.663884	-2.229183	1.046003	0.004429	0.707375
-22.675112	-2.268262	1.051008	0.004431	0.707292
-23.605606	-2.205731	1.056013	0.004605	0.707085
-23.760038	-2.182954	1.061018	0.004633	0.707075
-23.744847	-2.182558	1.066022	0.004631	0.707081
-23.579959	-2.212617	1.071027	0.004600	0.707080
-23.775443	-2.179723	1.076032	0.004637	0.707076
-23.631663	-2.201821	1.081037	0.004610	0.707083
-23.534511	-2.260122	1.086042	0.004592	0.707000
-24.845039	-2.149427	1.091046	0.004836	0.706753
-24.626075	-2.188931	1.096051	0.004795	0.706752
-24.717750	-2.174306	1.101056	0.004812	0.706748
-24.548992	-2.200470	1.106061	0.004781	0.706756
-24.800993	-2.159909	1.111066	0.004828	0.706747
-24.659882	-2.180328	1.116070	0.004802	0.706757
-24.504845	-2.209292	1.121075	0.004773	0.706754
-25.246598	-2.212831	1.126080	0.004911	0.706481
-25.604234	-2.164741	1.131085	0.004978	0.706449
-25.686184	-2.155617	1.136090	0.004993	0.706438
-25.372416	-2.207593	1.141094	0.004935	0.706446
-25.564464	-2.173987	1.146099	0.004971	0.706445
-25.506102	-2.184475	1.151104	0.004960	0.706444
-25.242270	-2.227666	1.156109	0.004911	0.706452
-26.011709	-2.205550	1.161114	0.005054	0.706221
-26.477485	-2.166946	1.166118	0.005141	0.706131
-25.988378	-2.254568	1.171123	0.005050	0.706130
-26.517886	-2.162515	1.176128	0.005149	0.706125
-26.377401	-2.182556	1.181133	0.005123	0.706135
-26.289576	-2.202256	1.186138	0.005106	0.706127
-26.297653	-2.198493	1.191142	0.005108	0.706131
-26.597415	-2.237145	1.196147	0.005164	0.705946
-27.312780	-2.152554	1.201152	0.005297	0.705860
-26.792772	-2.240486	1.206157	0.005200	0.705869
-27.472655	-2.123796	1.211162	0.005327	0.705860
-27.139396	-2.179641	1.216166	0.005265	0.705867
-26.739401	-2.251689	1.221171	0.005191	0.705865
-27.413112	-2.132102	1.226176	0.005316	0.705864
-27.820590	-2.220956	1.231181	0.005392	0.705539
-27.897112	-2.214925	1.236186	0.005406	0.705524
-27.793876	-2.230658	1.241190	0.005387	0.705529
-28.077252	-2.179295	1.246195	0.005440	0.705530
-28.245988	-2.152829	1.251200	0.005472	0.705523
-27.798282	-2.229156	1.256205	0.005388	0.705530
-28.161462	-2.192425	1.261210	0.005456	0.705473
-29.008437	-2.169802	1.266214	0.005614	0.705215
-28.702089	-2.225740	1.271219	0.005557	0.705212
-28.935053	-2.186503	1.276224	0.005600	0.705207
-28.820919	-2.202204	1.281229	0.005579	0.705217
-28.551796	-2.256314	1.286234	0.005529	0.705204
-28.645153	-2.236460	1.291238	0.005546	0.705210
-29.079423	-2.227668	1.296243	0.005627	0.705072
-29.975420	-2.163171	1.301248	0.005794	0.704880
-29.332377	-2.274483	1.306253	0.005675	0.704887
-30.070632	-2.145435	1.311258	0.005812	0.704881
-29.866146	-2.179959	1.316262	0.005774	0.704885
-29.293796	-2.279986	1.321267	0.005668	0.704889
-29.794706	-2.195072	1.326272	0.005761	0.704880
-30.136077	-2.207804	1.331277	0.005825	0.704732
-30.864988	-2.151777	1.336282	0.005960	0.704583
-30.390952	-2.231918	1.341286	0.005872	0.704591
-30.545383	-2.206484	1.346291	0.005901	0.704587
-30.801851	-2.162278	1.351296	0.005949	0.704584
-30.120103	-2.281192	1.356301	0.005822	0.704589
-30.471205	-2.221510	1.361306	0.005888	0.704583
-31.052123	-2.235067	1.366310	0.005996	0.704347
-31.344614	-2.227417	1.371315	0.006050	0.704257
-31.601420	-2.182878	1.376320	0.006098	0.704254
-31.527355	-2.192411	1.381325	0.006084	0.704261
-31.703233	-2.163346	1.386330	0.006117	0.704257
-31.377481	-2.218680	1.391334	0.006057	0.704262
-31.605547	-2.178142	1.396339	0.006099	0.704262
-31.957862	-2.201239	1.401344	0.006165	0.704088
-32.412489	-2.184556	1.406349	0.006250	0.703958
-32.316415	-2.206064	1.411354	0.006232	0.703949
-32.493468	-2.170712	1.416358	0.006265	0.703957
-32.495719	-2.170936	1.421363	0.006265	0.703955
-32.299442	-2.208529	1.426368	0.006229	0.703950
-32.511568	-2.166537	1.431373	0.006268	0.703958
-32.801332	-2.172346	1.436378	0.006322	0.703842
-33.155324	-2.210407	1.441382	0.006388	0.703638
-33.177665	-2.205270	1.446387	0.006393	0.703640
-33.737918	-2.107903	1.451392	0.006497	0.703635
-33.067810	-2.223593	1.456397	0.006372	0.703642
-33.187349	-2.205729	1.461402	0.006395	0.703635
-33.578513	-2.134138	1.466406	0.006468	0.703639
-33.119526	-2.258602	1.471411	0.006382	0.703553
-34.242773	-2.161978	1.476416	0.006591	0.703343
-34.020718	-2.198367	1.481421	0.006550	0.703350
-34.119915	-2.183664	1.486426	0.006569	0.703344
-33.831210	-2.233715	1.491430	0.006515	0.703346
-33.810782	-2.237750	1.496435	0.006511	0.703345
-34.208416	-2.170340	1.501440	0.006585	0.703338
-34.054406	-2.309295	1.506445	0.006557	0.703113
-35.402529	-2.122926	1.511450	0.006808	0.703004
-35.387579	-2.123511	1.516454	0.006805	0.703008
-34.939161	-2.202078	1.521459	0.006722	0.703011
-35.172215	-2.163237	1.526464	0.006765	0.703005
-35.228308	-2.147909	1.531469	0.006776	0.703016
-35.241025	-2.150169	1.536474	0.006778	0.703006
-35.054026	-2.232477	1.541478	0.006744	0.702907
-36.086410	-2.154649	1.546483	0.006936	0.702692
-36.019431	-2.168182	1.551488	0.006923	0.702689
-35.854117	-2.194535	1.556493	0.006893	0.702695
-35.959395	-2.180058	1.561498	0.006912	0.702686
-36.039482	-2.160531	1.566502	0.006927	0.702697
-36.014540	-2.164946	1.571507	0.006923	0.702697
-35.832775	-2.226563	1.576512	0.006889	0.702638
-36.500486	-2.236415	1.581517	0.007013	0.702377
-37.028324	-2.146011	1.586522	0.007112	0.702369
-36.960136	-2.154855	1.591526	0.007099	0.702376
-36.382258	-2.258905	1.596531	0.006992	0.702374
-36.831295	-2.182397	1.601536	0.007075	0.702366
-36.733124	-2.195893	1.606541	0.007057	0.702374
-36.774176	-2.239462	1.611546	0.007065	0.702271
-37.935976	-2.128994	1.616550	0.007281	0.702076
-37.391870	-2.224824	1.621555	0.007180	0.702078
-37.641533	-2.182513	1.626560	0.007227	0.702073
-37.599909	-2.186969	1.631565	0.007219	0.702079
-37.667857	-2.178564	1.636570	0.007232	0.702071
-37.557651	-2.194787	1.641574	0.007211	0.702078
-37.442765	-2.301791	1.646579	0.007190	0.701903
-39.090884	-2.088425	1.651584	0.007497	0.701740
-38.300877	-2.224480	1.656589	0.007350	0.701750
-38.136551	-2.257066	1.661594	0.007319	0.701743
-38.827254	-2.131866	1.666598	0.007448	0.701747
-38.557142	-2.181464	1.671603	0.007398	0.701744
-38.384501	-2.214723	1.676608	0.007366	0.701739
-38.509479	-2.282961	1.681613	0.007389	0.701555
-39.706984	-2.128387	1.686618	0.007612	0.701436
-39.443587	-2.174475	1.691622	0.007563	0.701437
-38.967395	-2.258701	1.696627	0.007475	0.701439
-39.661147	-2.137273	1.701632	0.007604	0.701434
-38.890531	-2.272150	1.706637	0.007460	0.701439
-38.959835	-2.262535	1.711642	0.007473	0.701433
-39.950544	-2.239060	1.716646	0.007658	0.701123
-40.235426	-2.188651	1.721651	0.007711	0.701122
-40.244485	-2.188775	1.726656	0.007713	0.701118
-39.990339	-2.229323	1.731661	0.007665	0.701128
-40.360427	-2.168883	1.736666	0.007734	0.701116
-40.027708	-2.225677	1.741670	0.007673	0.701121
-39.529523	-2.351630	1.746675	0.007580	0.701046
-40.907257	-2.193219	1.751680	0.007836	0.700869
-40.658224	-2.232356	1.756685	0.007790	0.700880
-40.735305	-2.221968	1.761690	0.007805	0.700873
-40.723918	-2.221886	1.766694	0.007803	0.700877
-40.766116	-2.215138	1.771699	0.007811	0.700875
-40.942320	-2.189154	1.776704	0.007843	0.700864
-41.036431	-2.331898	1.781709	0.007861	0.700541
-41.963504	-2.171855	1.786714	0.008034	0.700530
-42.105917	-2.142768	1.791718	0.008060	0.700537
-41.613282	-2.229740	1.796723	0.007969	0.700539
-41.907802	-2.180112	1.801728	0.008024	0.700533
-41.706053	-2.211283	1.806733	0.007986	0.700542
-41.609005	-2.280033	1.811738	0.007968	0.700438
-42.902698	-2.157108	1.816742	0.008209	0.700219
-42.716121	-2.188962	1.821747	0.008174	0.700222
-42.703248	-2.194189	1.826752	0.008172	0.700216
-42.275223	-2.264715	1.831757	0.008092	0.700227
-42.851968	-2.165640	1.836762	0.008200	0.700220
-42.766904	-2.180700	1.841766	0.008184	0.700220
-42.340914	-2.321015	1.846771	0.008105	0.700089
-43.845717	-2.148302	1.851776	0.008385	0.699895
-43.513346	-2.204928	1.856781	0.008323	0.699900
-43.467183	-2.217013	1.861786	0.008315	0.699892
-43.375245	-2.231030	1.866790	0.008298	0.699897
-43.419992	-2.222056	1.871795	0.008306	0.699899
-43.941255	-2.132448	1.876800	0.008403	0.699892
-43.556156	-2.266671	1.881805	0.008332	0.699759
-44.590440	-2.162323	1.886810	0.008524	0.699596
-44.268547	-2.217351	1.891814	0.008464	0.699601
-43.808669	-2.298104	1.896819	0.008379	0.699603
-44.568579	-2.165393	1.901824	0.008520	0.699597
-44.564958	-2.161931	1.906829	0.008520	0.699605
-44.224792	-2.226101	1.911834	0.008457	0.699598
-44.466013	-2.305219	1.916838	0.008502	0.699350
-45.341717	-2.188249	1.921843	0.008665	0.699270
-45.350663	-2.189081	1.926848	0.008666	0.699265
-44.690731	-2.302516	1.931853	0.008544	0.699274
-45.307949	-2.196710	1.936858	0.008659	0.699265
-45.570206	-2.147254	1.941862	0.008708	0.699270
-45.043196	-2.240519	1.946867	0.008610	0.699271
-45.746611	-2.266417	1.951872	0.008741	0.698964
-46.152600	-2.194092	1.956877	0.008816	0.698963
-46.309408	-2.170856	1.961882	0.008845	0.698954
-46.010575	-2.222392	1.966886	0.008790	0.698957
-45.983626	-2.225782	1.971891	0.008785	0.698960
-46.363012	-2.160507	1.976896	0.008856	0.698955
-45.815713	-2.262848	1.981901	0.008754	0.698945
-46.661993	-2.262881	1.986906	0.008912	0.698638
-47.467125	-2.118023	1.991910	0.009061	0.698641
-46.927609	-2.214099	1.996915	0.008961	0.698641
-46.828427	-2.231747	2.001920	0.008943	0.698641

-46.974504	-2.205629	2.011917	0.008970	0.698641
-47.137302	-2.182141	2.021914	0.009001	0.698629
-47.603312	-2.233944	2.031910	0.009087	0.698354
-47.950269	-2.171536	2.041907	0.009152	0.698355
-47.887992	-2.183386	2.051904	0.009141	0.698353
-47.409415	-2.187434	2.061901	0.009052	0.698518
-47.389347	-2.159237	2.071898	0.009048	0.698583
-46.920162	-2.213791	2.081894	0.008961	0.698642
-46.964342	-2.206385	2.091891	0.008969	0.698640
-47.030534	-2.194091	2.101888	0.008982	0.698641
-47.143297	-2.175645	2.111885	0.009003	0.698637
-47.102056	-2.182090	2.121882	0.008995	0.698639
-46.876803	-2.221277	2.131878	0.008954	0.698641
-47.003352	-2.198603	2.141875	0.008977	0.698641
-46.747446	-2.192854	2.151872	0.008930	0.698745
-46.102438	-2.201651	2.161869	0.008810	0.698960
-46.132880	-2.197657	2.171866	0.008816	0.698957
-46.160569	-2.191539	2.181862	0.008821	0.698959
-46.273814	-2.171931	2.191859	0.008842	0.698958
-45.303325	-2.205805	2.201856	0.008662	0.699240
-45.185464	-2.215024	2.211853	0.008640	0.699264
-45.211878	-2.209710	2.221850	0.008645	0.699265
-45.306460	-2.191584	2.231846	0.008663	0.699267
-44.861654	-2.153427	2.241843	0.008580	0.699505
-44.461055	-2.181113	2.251840	0.008506	0.699594
-44.513196	-2.171904	2.261837	0.008515	0.699594
-44.349578	-2.196938	2.271834	0.008485	0.699602
-43.675425	-2.172238	2.281830	0.008360	0.699896
-43.495900	-2.204112	2.291827	0.008326	0.699896
-43.454784	-2.212574	2.301824	0.008319	0.699893
-43.714344	-2.108520	2.311821	0.008367	0.700010
-42.816823	-2.167418	2.321818	0.008200	0.700215
-42.414287	-2.238792	2.331814	0.008126	0.700215
-42.663275	-2.193091	2.341811	0.008172	0.700218
-42.034223	-2.179254	2.351808	0.008055	0.700473
-42.175066	-2.125237	2.361805	0.008082	0.700531
-41.616947	-2.225241	2.371802	0.007978	0.700530
-41.772003	-2.144551	2.381798	0.008007	0.700637
-40.690074	-2.219723	2.391795	0.007806	0.700876
-40.869098	-2.188235	2.401792	0.007839	0.700874
-40.881692	-2.187159	2.411789	0.007841	0.700872
-40.550043	-2.179191	2.421786	0.007780	0.701007
-40.068617	-2.207797	2.431782	0.007690	0.701123
-40.222905	-2.180489	2.441779	0.007719	0.701122
-40.081089	-2.172798	2.451776	0.007693	0.701189
-39.314677	-2.188012	2.461773	0.007550	0.701434
-39.145201	-2.219250	2.471770	0.007519	0.701432
-39.243712	-2.198994	2.481766	0.007538	0.701437
-38.718676	-2.181508	2.491763	0.007440	0.701662
-38.342157	-2.209306	2.501760	0.007370	0.701741
-38.471701	-2.187108	2.511757	0.007394	0.701739
-38.163415	-2.200687	2.521754	0.007337	0.701823
-37.673002	-2.166065	2.531750	0.007246	0.702069
-37.488765	-2.198736	2.541747	0.007212	0.702069
-37.495180	-2.197257	2.551744	0.007213	0.702070
-37.174737	-2.123159	2.561741	0.007153	0.702335
-36.567663	-2.216418	2.571738	0.007041	0.702365
-36.734961	-2.185171	2.581734	0.007072	0.702367
-36.184841	-2.189824	2.591731	0.006970	0.702556
-35.902794	-2.175119	2.601728	0.006917	0.702687
-36.011724	-2.154627	2.611725	0.006938	0.702689
-35.808216	-2.165050	2.621722	0.006900	0.702741
-35.097091	-2.161599	2.631718	0.006768	0.703004
-34.894771	-2.196912	2.641715	0.006730	0.703005
-35.291275	-2.127351	2.651712	0.006804	0.703002
-34.514089	-2.121690	2.661709	0.006660	0.703293
-34.166663	-2.162085	2.671706	0.006595	0.703336
-33.943126	-2.199863	2.681702	0.006554	0.703340
-33.876253	-2.157015	2.691699	0.006541	0.703451
-33.364193	-2.159721	2.701696	0.006446	0.703629
-33.472630	-2.139549	2.711693	0.006466	0.703631
-33.392613	-2.141899	2.721690	0.006452	0.703654
-32.582888	-2.139607	2.731686	0.006301	0.703950
-32.053896	-2.233158	2.741683	0.006203	0.703951
-32.474902	-2.159545	2.751680	0.006281	0.703948
-32.016358	-2.173454	2.761677	0.006196	0.704084
-31.380613	-2.201109	2.771674	0.006078	0.704257
-31.427880	-2.192386	2.781670	0.006087	0.704257
-31.349754	-2.204467	2.791667	0.006072	0.704261
-30.928526	-2.138553	2.801664	0.005994	0.704545
-30.676072	-2.163173	2.811661	0.005947	0.704585
-30.533707	-2.189421	2.821658	0.005921	0.704583
-30.539084	-2.132116	2.831654	0.005922	0.704697
-29.473581	-2.228504	2.841651	0.005724	0.704885
-29.763242	-2.176141	2.851648	0.005778	0.704886
-29.547455	-2.216215	2.861645	0.005738	0.704882
-29.159577	-2.154199	2.871642	0.005666	0.705146
-28.786916	-2.189009	2.881638	0.005596	0.705210
-28.812634	-2.183817	2.891635	0.005601	0.705211
-28.885445	-2.121349	2.901632	0.005615	0.705310
-27.962688	-2.181323	2.911629	0.005443	0.705520
-27.973174	-2.179429	2.921626	0.005445	0.705520
-27.918329	-2.188715	2.931622	0.005435	0.705520
-27.051826	-2.194602	2.941619	0.005274	0.705819
-27.209072	-2.146650	2.951616	0.005304	0.705859
-26.816108	-2.215822	2.961613	0.005231	0.705860
-27.117249	-2.136194	2.971610	0.005287	0.705912
-26.143344	-2.203591	2.981606	0.005106	0.706125
-26.256285	-2.181917	2.991603	0.005127	0.706128
-26.259191	-2.182502	3.001600	0.005128	0.706126
-25.613417	-2.167337	3.011597	0.005007	0.706387
-25.544145	-2.153098	3.021594	0.004995	0.706441
-25.186246	-2.215898	3.031590	0.004928	0.706442
-25.168315	-2.156058	3.041587	0.004925	0.706569
-24.349619	-2.211864	3.051584	0.004773	0.706749
-24.581382	-2.171072	3.061581	0.004816	0.706748
-24.631947	-2.161294	3.071578	0.004826	0.706749
-23.656556	-2.183115	3.081574	0.004644	0.707054
-23.775280	-2.148575	3.091571	0.004666	0.707081
-23.479837	-2.202575	3.101568	0.004611	0.707078
-23.495674	-2.129375	3.111565	0.004615	0.707219
-22.796405	-2.177705	3.121562	0.004485	0.707372
-22.794735	-2.176576	3.131558	0.004484	0.707374
-22.902731	-2.138218	3.141555	0.004505	0.707412
-21.858322	-2.181068	3.151552	0.004310	0.707700
-21.772730	-2.197819	3.161549	0.004295	0.707696
-22.011007	-2.154583	3.171546	0.004339	0.707698
-21.380377	-2.177291	3.181542	0.004222	0.707877
-21.057199	-2.166188	3.191539	0.004162	0.708015
-20.887657	-2.196421	3.201536	0.004130	0.708014
-21.307876	-2.102356	3.211533	0.004209	0.708052
-20.277204	-2.139066	3.221530	0.004017	0.708347
-19.933227	-2.199296	3.231526	0.003953	0.708349
-20.172012	-2.155152	3.241523	0.003998	0.708352
-19.527340	-2.182417	3.251520	0.003878	0.708527
-19.219803	-2.182348	3.261517	0.003821	0.708636
-19.354174	-2.158063	3.271514	0.003846	0.708637
-19.267853	-2.156410	3.281510	0.003830	0.708671
-18.598464	-2.131983	3.291507	0.003705	0.708958
-18.359367	-2.174962	3.301504	0.003661	0.708957
-18.435707	-2.162035	3.311501	0.003675	0.708956
-17.828909	-2.173407	3.321498	0.003563	0.709149
-17.397389	-2.193703	3.331494	0.003482	0.709262
-17.708464	-2.135856	3.341491	0.003540	0.709266
-17.497918	-2.147656	3.351488	0.003501	0.709318
-16.928079	-2.109134	3.361485	0.003395	0.709598
-16.681509	-2.152975	3.371482	0.003350	0.709598
-16.568510	-2.173714	3.381478	0.003329	0.709596
-16.115977	-2.144560	3.391475	0.003245	0.709815
-15.729375	-2.173367	3.401472	0.003173	0.709895
-15.915628	-2.140307	3.411469	0.003208	0.709895
-15.705215	-2.137240	3.421466	0.003169	0.709975
-14.733632	-2.189377	3.431462	0.002988	0.710217
-14.694159	-2.195018	3.441459	0.002981	0.710220
-14.782739	-2.177566	3.451456	0.002997	0.710223
-14.523437	-2.128347	3.461453	0.002949	0.710413
-13.916349	-2.175122	3.471450	0.002836	0.710535
-14.145151	-2.132329	3.481446	0.002879	0.710539
-13.895039	-2.155863	3.491443	0.002833	0.710581
-13.279171	-2.117758	3.501440	0.002718	0.710876
-12.920446	-2.182364	3.511437	0.002651	0.710874
-12.812507	-2.201379	3.521434	0.002631	0.710874
-12.839781	-2.132833	3.531430	0.002637	0.711001
-12.011952	-2.207921	3.541427	0.002483	0.711145
-12.078061	-2.197565	3.551424	0.002495	0.711142
-12.601057	-2.102229	3.561421	0.002593	0.711146
-11.526335	-2.139024	3.571418	0.002393	0.711455
-11.571220	-2.130649	3.581414	0.002401	0.711455
-11.135462	-2.205884	3.591411	0.002320	0.711460
-11.091330	-2.117793	3.601408	0.002312	0.711651
-10.620947	-2.143969	3.611405	0.002225	0.711765
-10.459472	-2.174992	3.621402	0.002195	0.711761
-10.446925	-2.140942	3.631398	0.002193	0.711833
-9.398038	-2.198891	3.641395	0.001997	0.712089
-9.484074	-2.182595	3.651392	0.002014	0.712091
-9.571058	-2.167582	3.661389	0.002030	0.712090
-9.358890	-2.128918	3.671386	0.001991	0.712242
-8.733452	-2.166503	3.681382	0.001874	0.712389
-8.687246	-2.174046	3.691379	0.001866	0.712390
-8.733338	-2.152900	3.701376	0.001875	0.712415
-7.767458	-2.177727	3.711373	0.001695	0.712708
-7.731628	-2.184205	3.721370	0.001688	0.712708
-7.798222	-2.171649	3.731366	0.001701	0.712709
-7.483114	-2.155495	3.741363	0.001642	0.712852
-6.728238	-2.201581	3.751360	0.001502	0.713028
-6.360255	-2.268104	3.761357	0.001434	0.713026
-6.415401	-2.257901	3.771354	0.001444	0.713026
-6.349593	-2.217876	3.781350	0.001432	0.713129
-4.947211	-2.351038	3.791347	0.001171	0.713361
-5.469736	-2.258702	3.801344	0.001268	0.713359
-5.324962	-2.285298	3.811341	0.001242	0.713357
-5.563664	-2.241920	3.821338	0.001286	0.713359
-4.647786	-2.264617	3.831334	0.001116	0.713638
-4.427171	-2.296706	3.841331	0.001075	0.713652
-4.695391	-2.248305	3.851328	0.001125	0.713653
-4.514674	-2.275801	3.861325	0.001091	0.713662
-3.809030	-2.246976	3.871322	0.000960	0.713969
-3.908663	-2.228101	3.881318	0.000979	0.713971
-3.510237	-2.298669	3.891315	0.000905	0.713971
-3.445438	-2.245922	3.901312	0.000893	0.714099
-2.511304	-2.323848	3.911309	0.000719	0.714274
-3.218285	-2.197437	3.921306	0.000851	0.714275
-3.138804	-2.210315	3.931302	0.000836	0.714277
-2.390478	-2.190721	3.941299	0.000697	0.714581
-2.302617	-2.192731	3.951296	0.000681	0.714607
-2.031172	-2.241893	3.961293	0.000630	0.714605
-2.148086	-2.130256	3.971290	0.000652	0.714785
-1.533103	-2.178128	3.981286	0.000538	0.714908
-1.877480	-2.115887	3.991283	0.000602	0.714909
-1.679846	-2.033697	4.001280	0.000566	0.715142
-1.629545	-1.997802	4.011277	0.000556	0.715230
-1.280428	-2.024196	4.021274	0.000491	0.715301
-0.945857	-1.960066	4.031270	0.000429	0.715546
-1.260090	-1.903749	4.041267	0.000488	0.715547
-0.897755	-1.819956	4.051264	0.000421	0.715840
-1.095215	-1.764410	4.061261	0.000457	0.715880
-0.846853	-1.706990	4.071258	0.000411	0.716082
-0.815160	-1.686498	4.081254	0.000405	0.716133
-0.903736	-1.530505	4.091251	0.000422	0.716411
-0.369557	-1.590314	4.101248	0.000323	0.716480
-0.450701	-1.437590	4.111245	0.000338	0.716754
-0.540570	-1.356009	4.121242	0.000355	0.716883
-0.959102	-1.180364	4.131238	0.000433	0.717083
-0.368886	-1.138258	4.141235	0.000323	0.717374
-0.129407	-1.094375	4.151232	0.000278	0.717545
-0.007693	-1.030641	4.161229	0.000256	0.717713
0.012370	-0.880201	4.171226	0.000252	0.718017
-0.009363	-0.765342	4.181222	0.000256	0.718236
-0.080057	-0.641015	4.191219	0.000270	0.718457
-0.295615	-0.478819	4.201216	0.000310	0.718701
-0.120948	-0.373368	4.211213	0.000277	0.718970
0.152767	-0.270132	4.221210	0.000226	0.719270
0.194390	-0.128786	4.231206	0.000219	0.719563
0.117684	0.021758	4.241203	0.000233	0.719832
0.000000	0.192096	4.251200	0.000255	0.720126

0.260757	0.765708	4.256205	0.000206	0.721347
0.491577	1.976989	4.261210	0.000162	0.723805
0.782478	3.782703	4.266214	0.000107	0.727437
0.986972	6.150467	4.271219	0.000068	0.732110
1.171592	9.030638	4.276224	0.000031	0.737733
1.771486	12.317711	4.281229	-0.000082	0.744230
2.350303	16.063234	4.286234	-0.000192	0.751529
2.709060	20.263915	4.291238	-0.000262	0.759536
3.031291	24.858900	4.296243	-0.000325	0.768175
3.641487	29.778842	4.301248	-0.000442	0.777405
4.310792	35.033020	4.306253	-0.000570	0.787147
4.539737	40.686361	4.311258	-0.000616	0.797342
4.860573	46.625936	4.316262	-0.000679	0.807939
5.413515	52.799796	4.321267	-0.000786	0.818876
5.940661	59.255487	4.326272	-0.000889	0.830142
6.748628	65.893993	4.331277	-0.001043	0.841648
6.955053	72.852471	4.336282	-0.001086	0.853355
7.492793	79.965073	4.341286	-0.001191	0.865252
7.956569	87.271039	4.346291	-0.001282	0.877278
8.380043	94.751574	4.351296	-0.001366	0.889409
8.865663	102.389511	4.356301	-0.001461	0.901641
12.612660	109.613998	4.361306	-0.002163	0.913955
14.781734	117.303050	4.366310	-0.002572	0.926391
15.209307	125.410826	4.371315	-0.002657	0.938833
15.750246	133.600330	4.376320	-0.002763	0.951263
16.374312	141.854598	4.381325	-0.002884	0.963650
16.939574	150.193575	4.386330	-0.002995	0.975987
17.782337	158.572099	4.391334	-0.003157	0.988296
18.564677	167.008753	4.396339	-0.003308	1.000520
19.282316	175.487679	4.401344	-0.003447	1.012640
19.985692	184.025098	4.406349	-0.003584	1.024694
20.440544	192.631736	4.411354	-0.003674	1.036643
21.161034	201.213161	4.416358	-0.003814	1.048483
21.604143	209.872879	4.421363	-0.003902	1.060231
22.316679	218.508546	4.426368	-0.004040	1.071880
22.844730	227.159756	4.431373	-0.004144	1.083383
23.333948	235.831828	4.436378	-0.004241	1.094782
23.940994	244.476360	4.441382	-0.004359	1.106054
24.775007	253.093715	4.446387	-0.004520	1.117227
25.343974	261.739084	4.451392	-0.004632	1.128267
25.871155	270.408849	4.456397	-0.004735	1.139222
26.535355	279.055621	4.461402	-0.004865	1.150072
27.332179	287.679447	4.466406	-0.005018	1.160820
27.656450	296.339875	4.471411	-0.005084	1.171416
28.551117	304.896812	4.476416	-0.005256	1.181909
29.418570	313.476114	4.481421	-0.005424	1.192330
29.674938	322.114312	4.486426	-0.005477	1.202608
30.104887	330.730587	4.491430	-0.005562	1.212807
30.694607	339.285236	4.496435	-0.005678	1.222881
31.004349	347.907824	4.501440	-0.005741	1.232895
31.258879	356.490150	4.506445	-0.005794	1.242773
31.835686	365.000827	4.511450	-0.005907	1.252553
32.239336	373.533839	4.516454	-0.005987	1.262249
32.779826	382.041630	4.521459	-0.006093	1.271868
33.368377	390.507984	4.526464	-0.006208	1.281378
33.911421	398.992468	4.531469	-0.006315	1.290830
34.229621	407.484508	4.536474	-0.006380	1.300179
34.822676	415.976992	4.541478	-0.006496	1.309512
35.677190	424.448776	4.546483	-0.006660	1.318804
36.303511	432.830653	4.551488	-0.006782	1.327893
36.703885	441.280474	4.556493	-0.006862	1.336953
37.178089	449.657741	4.561498	-0.006956	1.345887
37.783100	458.055533	4.566502	-0.007074	1.354807
38.098149	466.451267	4.571507	-0.007138	1.363616
38.458628	474.845656	4.576512	-0.007211	1.372375
39.005373	483.211181	4.581517	-0.007318	1.381080
39.250964	491.609553	4.586522	-0.007369	1.389713
39.802745	499.963934	4.591526	-0.007477	1.398299
40.239645	508.296474	4.596531	-0.007564	1.406791
40.623486	516.646785	4.601536	-0.007640	1.415242
41.009477	524.982687	4.606541	-0.007718	1.423628
41.452626	533.312098	4.611546	-0.007806	1.431967
41.774580	541.642858	4.616550	-0.007871	1.440240
41.965323	549.979200	4.621555	-0.007912	1.448450
42.401860	558.287949	4.626560	-0.007998	1.456626
43.023334	566.547201	4.631565	-0.008119	1.464737
43.127603	574.930214	4.636570	-0.008144	1.472841
43.580329	583.194698	4.641574	-0.008234	1.480842
43.976890	591.456012	4.646579	-0.008313	1.488788
44.760400	599.667806	4.651584	-0.008464	1.496705
45.416020	607.905586	4.656589	-0.008592	1.504584
45.548872	616.229544	4.661594	-0.008622	1.512423
46.004099	624.480123	4.666598	-0.008712	1.520203
46.206674	632.763189	4.671603	-0.008755	1.527934
46.523744	641.032375	4.676608	-0.008819	1.535631
47.213958	649.243518	4.681613	-0.008953	1.543291
47.469130	657.520561	4.686618	-0.009006	1.550909
47.685784	665.802331	4.691622	-0.009051	1.558489
47.914872	674.035604	4.696627	-0.009099	1.565989
48.428885	682.250723	4.701632	-0.009200	1.573479
48.665664	690.488001	4.706637	-0.009250	1.580913
49.094053	698.687681	4.711642	-0.009335	1.588306
49.744325	706.885156	4.716646	-0.009461	1.595694
50.024996	715.102037	4.721651	-0.009519	1.603013
50.430655	723.308050	4.726656	-0.009599	1.610307
50.687988	731.559157	4.731661	-0.009653	1.617586
51.020224	739.758269	4.736666	-0.009720	1.624797
51.361494	748.011670	4.741670	-0.009789	1.632025
51.775021	756.202056	4.746675	-0.009871	1.639177
52.270292	764.352738	4.751680	-0.009968	1.646274
52.617744	772.577664	4.756685	-0.010038	1.653384
52.879330	780.756027	4.761690	-0.010092	1.660412
53.603394	788.902882	4.766694	-0.010232	1.667446
53.787912	797.142524	4.771699	-0.010272	1.674456
54.116409	805.301116	4.776704	-0.010338	1.681388
54.513931	813.483404	4.781709	-0.010418	1.688321
54.845090	821.673849	4.786714	-0.010485	1.695223
55.176262	829.858861	4.791718	-0.010552	1.702092
55.407341	838.056576	4.796723	-0.010600	1.708931
55.775038	846.235648	4.801728	-0.010674	1.715745
56.225306	854.376963	4.806733	-0.010763	1.722512
56.352579	862.563794	4.811738	-0.010792	1.729248
56.880390	870.717585	4.816742	-0.010895	1.735981
57.382524	878.845984	4.821747	-0.010994	1.742665
57.367134	887.062053	4.826752	-0.010996	1.749329
57.970067	895.206066	4.831757	-0.011114	1.755987
58.184060	903.357446	4.836762	-0.011159	1.762576
58.522188	911.526273	4.841766	-0.011227	1.769171
59.069599	919.665967	4.846771	-0.011334	1.775744
59.454012	927.806146	4.851776	-0.011411	1.782272
59.785088	935.992355	4.856781	-0.011478	1.788807
59.947014	944.213125	4.861786	-0.011513	1.795324
60.410568	952.324501	4.866790	-0.011605	1.801768
60.687403	960.461195	4.871795	-0.011662	1.808187
60.769669	968.644957	4.876800	-0.011682	1.814595
61.067701	976.779111	4.881805	-0.011743	1.820969
61.396614	984.888980	4.886810	-0.011809	1.827305
62.234400	992.980138	4.891814	-0.011971	1.833665
62.282335	1001.157728	4.896819	-0.011985	1.839976
62.501116	1009.287590	4.901824	-0.012031	1.846249
62.945867	1017.436211	4.906829	-0.012119	1.852541
63.081485	1025.589217	4.911834	-0.012149	1.858780
63.496465	1033.692716	4.916838	-0.012232	1.864992
63.693692	1041.876695	4.921843	-0.012274	1.871219
64.086231	1049.993997	4.926848	-0.012352	1.877398
64.369330	1058.112323	4.931853	-0.012410	1.883544
64.737033	1066.218332	4.936858	-0.012484	1.889671
65.172530	1074.351778	4.941862	-0.012570	1.895806
65.496823	1082.467224	4.946867	-0.012636	1.901895
65.770612	1090.593720	4.951872	-0.012692	1.907967
65.950110	1098.778364	4.956877	-0.012730	1.914052
66.138013	1106.880873	4.961882	-0.012771	1.920059
66.749995	1114.952569	4.966886	-0.012890	1.926071
67.290928	1123.063307	4.971891	-0.012996	1.932084
67.451586	1131.209632	4.976896	-0.013031	1.938063
67.857109	1139.317887	4.981901	-0.013112	1.944023
68.219285	1147.430175	4.986906	-0.013184	1.949963
68.612719	1155.579230	4.991910	-0.013263	1.955914
68.693629	1163.699273	4.996915	-0.013283	1.961793
69.060723	1171.779918	5.001920	-0.013357	1.967656
69.559730	1179.900757	5.006925	-0.013455	1.973545
69.683565	1188.009958	5.011930	-0.013483	1.979368
70.204972	1196.089404	5.016934	-0.013585	1.985195
70.504227	1204.222145	5.021939	-0.013646	1.991019
70.614431	1212.359730	5.026944	-0.013672	1.996809
70.882657	1220.461835	5.031949	-0.013727	2.002574
71.379345	1228.518911	5.036954	-0.013825	2.008315
71.835152	1236.637492	5.041958	-0.013915	2.014078
72.039648	1244.775891	5.046963	-0.013958	2.019812
72.076728	1252.888624	5.051968	-0.013970	2.025495
72.510859	1261.015602	5.056973	-0.014056	2.031213
72.768129	1269.122719	5.061978	-0.014109	2.036882
73.188992	1277.189642	5.066982	-0.014193	2.042525
73.520646	1285.279680	5.071987	-0.014260	2.048159
73.856195	1293.383782	5.076992	-0.014328	2.053787
74.224914	1301.471938	5.081997	-0.014401	2.059392
74.618907	1309.522738	5.087002	-0.014480	2.064959
75.058117	1317.626429	5.092006	-0.014567	2.070551
75.407156	1325.730979	5.097011	-0.014637	2.076120
75.644997	1333.829709	5.102016	-0.014687	2.081659
76.074453	1341.924415	5.107021	-0.014772	2.087200
76.210097	1350.033586	5.112026	-0.014802	2.092706
76.452493	1358.148291	5.117030	-0.014853	2.098212
77.071035	1366.188974	5.122035	-0.014973	2.103691
77.207333	1374.315058	5.127040	-0.015004	2.109165
77.597900	1382.493499	5.132045	-0.015082	2.114685
77.706664	1390.563389	5.137050	-0.015107	2.120091
78.119829	1398.614106	5.142054	-0.015189	2.125500
78.370600	1406.706673	5.147059	-0.015241	2.130907
78.724254	1414.791558	5.152064	-0.015312	2.136305
79.226258	1422.847550	5.157069	-0.015411	2.141684
79.436200	1430.941652	5.162074	-0.015455	2.147047
79.530530	1439.075081	5.167078	-0.015478	2.152412
79.895613	1447.146421	5.172083	-0.015551	2.157748
80.316166	1455.183838	5.177088	-0.015634	2.163053
80.556792	1463.287760	5.182093	-0.015684	2.168373
80.739600	1471.396991	5.187098	-0.015724	2.173677
81.152498	1479.463929	5.192102	-0.015806	2.178962
81.710461	1487.499355	5.197107	-0.015915	2.184227
81.938900	1495.614089	5.202112	-0.015963	2.189500
82.317096	1503.747224	5.207117	-0.016038	2.194787
82.570998	1511.807918	5.212122	-0.016091	2.200002
82.604702	1519.904665	5.217126	-0.016102	2.205208
82.848539	1527.985610	5.222131	-0.016153	2.210411
83.123868	1536.069868	5.227136	-0.016209	2.215607
83.409196	1544.147174	5.232141	-0.016267	2.220786
83.610235	1552.208499	5.237146	-0.016310	2.225936
84.023959	1560.292062	5.242150	-0.016392	2.231107
84.202376	1568.396051	5.247155	-0.016431	2.236258
84.318932	1576.464971	5.252160	-0.016458	2.241370
84.874534	1584.503276	5.257165	-0.016566	2.246489
85.177667	1592.590791	5.262170	-0.016628	2.251605
85.553773	1600.668107	5.267174	-0.016703	2.256709
85.887911	1608.740886	5.272179	-0.016771	2.261796
86.221519	1616.798907	5.277184	-0.016838	2.266861
86.576301	1624.944684	5.282189	-0.016909	2.271972
86.708256	1633.043210	5.287194	-0.016939	2.277023
87.025782	1641.079309	5.292198	-0.017003	2.282039
87.190483	1649.148106	5.297203	-0.017039	2.287052
87.337150	1657.214211	5.302208	-0.017072	2.292051
87.826138	1665.268926	5.307213	-0.017168	2.297060
88.233139	1673.299264	5.312218	-0.017249	2.302037
88.555632	1681.383296	5.317222	-0.017314	2.307028
88.886795	1689.469602	5.322227	-0.017381	2.312011
89.002780	1697.544507	5.327232	-0.017408	2.316958
89.357805	1705.604106	5.332237	-0.017479	2.321905
89.650934	1713.653146	5.337242	-0.017539	2.326830
90.142990	1721.720131	5.342246	-0.017635	2.331772
90.328597	1729.815590	5.347251	-0.017675	2.336695
90.499982	1737.887315	5.352256	-0.017712	2.341593
90.918926	1745.946370	5.357261	-0.017795	2.346492
91.285546	1754.031727	5.362266	-0.017869	2.351393
91.699002	1762.102146	5.367270	-0.017951	2.356279
92.036400	1770.147523	5.372275	-0.018019	2.361133
92.330618	1778.184719	5.377280	-0.018079	2.365969
92.655183	1786.285216	5.382285	-0.018145	2.370835
92.750734	1794.372577	5.387290	-0.018168	2.375664
93.319900	1802.394236	5.392294	-0.018279	2.380483
93.501443	1810.475560	5.397299	-0.018318	2.385296
93.496066	1818.577532	5.402304	-0.018322	2.390097
94.059136	1826.628796	5.407309	-0.018432	2.394904
94.368350	1834.665115	5.412314	-0.018495	2.399671
94.664186	1842.715434	5.417318	-0.018555	2.404437
94.941115	1850.802784	5.422323	-0.018612	2.409213
95.518148	1858.839330	5.427328	-0.018724	2.413973
95.721441	1866.943324	5.432333	-0.018767	2.418735
95.874973	1874.990347	5.437338	-0.018801	2.423449
96.318406	1883.053372	5.442342	-0.018889	2.428186
96.883070	1891.176551	5.447347	-0.018999	2.432959
96.780718	1899.260701	5.452352	-0.018985	2.437647
97.190283	1907.297512	5.457357	-0.019067	2.442339
97.199386	1915.360605	5.462362	-0.019074	2.447006
97.569444	1923.408475	5.467366	-0.019148	2.451683
97.711175	1931.486996	5.472371	-0.019179	2.456352
98.240393	1939.483005	5.477376	-0.019283	2.460993
98.655921	1947.530267	5.482381	-0.019366	2.465646
98.624536	1955.634178	5.487386	-0.019365	2.470289
99.066641	1963.687512	5.492390	-0.019452	2.474930
99.376580	1971.720654	5.497395	-0.019515	2.479541
99.679910	1979.748161	5.502400	-0.019577	2.484140
100.230490	1987.804793	5.507405	-0.019685	2.488764
100.669219	1995.853297	5.512410	-0.019772	2.493368
101.035973	2003.922691	5.517414	-0.019845	2.497969
101.109908	2012.009131	5.522419	-0.019864	2.502550
101.548050	2020.036081	5.527424	-0.019951	2.507115
101.674271	2028.174655	5.532429	-0.019979	2.511713
101.893166	2036.231629	5.537434	-0.020025	2.516262
102.367119	2044.244437	5.542438	-0.020119	2.520797
102.558681	2052.298149	5.547443	-0.020160	2.525327
102.779200	2060.354926	5.552448	-0.020206	2.529852
103.114677	2068.442064	5.557453	-0.020274	2.534394
103.346371	2076.468922	5.562458	-0.020322	2.538887
103.922262	2084.477800	5.567462	-0.020434	2.543386
104.248381	2092.553245	5.572467	-0.020500	2.547896
104.384202	2100.636118	5.577472	-0.020531	2.552390
104.828187	2108.698476	5.582477	-0.020618	2.556885
105.178194	2116.721065	5.587482	-0.020689	2.561344
105.401940	2124.769291	5.592486	-0.020736	2.565801
105.707439	2132.828426	5.597491	-0.020798	2.570261
105.932154	2140.904836	5.602496	-0.020845	2.574718
106.258936	2148.955500	5.607501	-0.020911	2.579159
106.530105	2156.995019	5.612506	-0.020966	2.583583
106.857794	2165.046827	5.617510	-0.021033	2.588010
106.867995	2173.282862	5.622515	-0.021040	2.592508
107.096094	2181.356075	5.627520	-0.021087	2.596925
107.612101	2189.305600	5.632525	-0.021189	2.601286
107.982429	2197.304488	5.637530	-0.021263	2.605657
107.924786	2205.369158	5.642534	-0.021257	2.610027
108.396231	2213.417340	5.647539	-0.021350	2.614417
108.628893	2221.435269	5.652544	-0.021399	2.618767
108.978161	2229.477996	5.657549	-0.021469	2.623130
109.356654	2237.505778	5.662554	-0.021544	2.627480
109.694827	2245.570959	5.667558	-0.021613	2.631841
110.008145	2253.630388	5.672563	-0.021676	2.636189
110.140469	2261.664400	5.677568	-0.021706	2.640505
110.633030	2269.688380	5.682573	-0.021803	2.644831
110.678110	2277.753231	5.687578	-0.021816	2.649143
110.727674	2285.854724	5.692582	-0.021831	2.653468
111.205647	2293.875410	5.697587	-0.021925	2.657771
111.706933	2301.859524	5.702592	-0.022023	2.662049
112.043947	2309.949212	5.707597	-0.022091	2.666365
112.351836	2317.991500	5.712602	-0.022154	2.670647
112.661038	2326.078022	5.717606	-0.022217	2.674946
112.766171	2334.126209	5.722611	-0.022241	2.679204
113.277335	2342.110234	5.727616	-0.022342	2.683448
113.526514	2350.191701	5.732621	-0.022393	2.687720
113.687595	2358.256406	5.737626	-0.022428	2.691970
113.901740	2366.313871	5.742630	-0.022473	2.696213
114.254085	2374.349641	5.747635	-0.022544	2.700447
114.380297	2382.371075	5.752640	-0.022573	2.704652
114.438026	2390.478476	5.757645	-0.022589	2.708891
114.637638	2398.509747	5.762650	-0.022631	2.713093
114.924995	2406.544298	5.767654	-0.022690	2.717296
115.297278	2414.570505	5.772659	-0.022764	2.721493
115.246004	2422.636346	5.777664	-0.022760	2.725678
115.676979	2430.673441	5.782669	-0.022845	2.729871
115.971220	2438.730340	5.787674	-0.022905	2.734059
116.150902	2446.781925	5.792678	-0.022944	2.738231
116.527493	2454.793519	5.797683	-0.023019	2.742389
116.669173	2462.845266	5.802688	-0.023051	2.746546
117.097925	2470.911248	5.807693	-0.023136	2.750722
117.348270	2479.028402	5.812698	-0.023188	2.754906
117.763184	2487.009547	5.817702	-0.023270	2.759025
117.908621	2495.050981	5.822707	-0.023302	2.763152
118.037649	2503.072237	5.827712	-0.023331	2.767261
118.515712	2511.121545	5.832717	-0.023426	2.771400
118.519419	2519.199378	5.837722	-0.023431	2.775518
118.684851	2527.224323	5.842726	-0.023467	2.779614
119.193901	2535.237775	5.847731	-0.023567	2.783717
119.098387	2543.299173	5.852736	-0.023555	2.787803
119.289024	2551.371806	5.857741	-0.023595	2.791906
119.418093	2559.430227	5.862746	-0.023625	2.795992
119.922187	2567.426214	5.867750	-0.023724	2.800062
120.099420	2575.470019	5.872755	-0.023762	2.804131
120.161258	2583.507918	5.877760	-0.023779	2.808185
120.767016	2591.551991	5.882765	-0.023896	2.812267
120.990235	2599.619720	5.887770	-0.023943	2.816333
121.100379	2607.654918	5.892774	-0.023969	2.820370
121.347814	2615.701566	5.897779	-0.024020	2.824416
121.662938	2623.739041	5.902784	-0.024084	2.828454
121.834403	2631.836481	5.907789	-0.024121	2.832509
122.209469	2639.844134	5.912794	-0.024196	2.836524
122.540454	2647.855817	5.917798	-0.024263	2.840533
122.565330	2655.907486	5.922803	-0.024273	2.844540
122.640563	2663.957900	5.927808	-0.024292	2.848542
123.261598	2671.974932	5.932813	-0.024413	2.852554
123.441956	2680.009221	5.937818	-0.024451	2.856543
123.641999	2688.048207	5.942822	-0.024494	2.860530
123.772681	2696.079766	5.947827	-0.024523	2.864504
123.982340	2704.133318	5.952832	-0.024567	2.868488
124.146980	2712.189918	5.957837	-0.024603	2.872465
124.112927	2720.247637	5.962842	-0.024602	2.876426
124.603804	2728.262221	5.967846	-0.024699	2.880389
124.683868	2736.283645	5.972851	-0.024719	2.884328
124.708882	2744.329233	5.977856	-0.024729	2.888270
125.151836	2752.375761	5.982861	-0.024816	2.892230
125.502892	2760.427778	5.987866	-0.024887	2.896182
125.835900	2768.453283	5.992870	-0.024954	2.900115
125.941036	2776.481728	5.997875	-0.024979	2.904032
126.378756	2784.496550	6.002880	-0.025065	2.907954
126.812870	2792.613510	6.007885	-0.025151	2.911921
127.069876	2800.702668	6.012890	-0.025204	2.915859
127.195845	2808.673505	6.017894	-0.025233	2.919727
127.618141	2816.690293	6.022899	-0.025317	2.923628
127.767424	2824.699413	6.027904	-0.025350	2.927506
128.181493	2832.753756	6.032909	-0.025432	2.931415
128.370500	2840.794355	6.037914	-0.025472	2.935299
128.373961	2848.852930	6.042918	-0.025478	2.939178
128.782204	2856.861270	6.047923	-0.025559	2.943048
128.845878	2864.902135	6.052928	-0.025576	2.946911
129.216218	2872.957532	6.057933	-0.025651	2.950792
129.321345	2881.018470	6.062938	-0.025675	2.954656
129.428277	2889.061733	6.067942	-0.025700	2.958507
129.739369	2897.068690	6.072947	-0.025763	2.962346
129.813419	2905.093999	6.077952	-0.025782	2.966177
130.058177	2913.138306	6.082957	-0.025833	2.970020
130.393618	2921.168350	6.087962	-0.025901	2.973857
130.586379	2929.203156	6.092966	-0.025942	2.977683
130.926641	2937.236616	6.097971	-0.026010	2.981511
131.258692	2945.247174	6.102976	-0.026077	2.985323
131.281590	2953.339979	6.107981	-0.026087	2.989154
131.424708	2961.415219	6.112986	-0.026119	2.992977
131.722178	2969.432885	6.117990	-0.026179	2.996776
132.201404	2977.441667	6.122995	-0.026273	3.000575
132.291997	2985.437508	6.128000	-0.026295	3.004343
132.473589	2993.489668	6.133005	-0.026334	3.008138
132.824194	3001.525011	6.138010	-0.026405	3.011928
132.989470	3009.605441	6.143014	-0.026441	3.015726
133.225791	3017.620008	6.148019	-0.026490	3.019491
133.629549	3025.611172	6.153024	-0.026570	3.023249
133.992556	3033.662218	6.158029	-0.026643	3.027029
134.140567	3041.720480	6.163034	-0.026676	3.030796
134.422186	3049.760882	6.168038	-0.026733	3.034557
134.530939	3057.822643	6.173043	-0.026759	3.038314
134.677806	3065.811205	6.178048	-0.026791	3.042035
134.895812	3073.874937	6.183053	-0.026837	3.045790
135.042298	3081.904924	6.188058	-0.026870	3.049520
135.281185	3089.931262	6.193062	-0.026919	3.053249
135.517744	3097.982637	6.198067	-0.026968	3.056985
135.568653	3106.010306	6.203072	-0.026983	3.060697
135.967411	3114.018890	6.208077	-0.027062	3.064411
136.034739	3122.093655	6.213082	-0.027080	3.068136
136.437567	3130.144718	6.218086	-0.027160	3.071861
136.868520	3138.225326	6.223091	-0.027246	3.075597
136.770416	3146.199701	6.228096	-0.027233	3.079254
137.232196	3154.211843	6.233101	-0.027324	3.082950
137.455769	3162.230690	6.238106	-0.027371	3.086634
137.692642	3170.259941	6.243110	-0.027420	3.090319
137.896431	3178.336418	6.248115	-0.027463	3.094020
138.055799	3186.334761	6.253120	-0.027498	3.097678
138.624333	3194.344013	6.258125	-0.027609	3.101356
138.688309	3202.388287	6.263130	-0.027626	3.105022
138.673594	3210.452732	6.268134	-0.027628	3.108690
139.003849	3218.493614	6.273139	-0.027695	3.112358
139.019614	3226.550728	6.278144	-0.027703	3.116014
139.365379	3234.546578	6.283149	-0.027773	3.119654
139.476454	3242.566284	6.288154	-0.027798	3.123290
139.766788	3250.601809	6.293158	-0.027858	3.126936
139.917634	3258.650983	6.298163	-0.027891	3.130578
139.893154	3266.683299	6.303168	-0.027892	3.134201
140.421636	3274.728651	6.308173	-0.027995	3.137849
140.614988	3282.744413	6.313178	-0.028036	3.141466
141.196802	3290.702207	6.318182	-0.028150	3.145069
141.789100	3298.748401	6.323187	-0.028265	3.148708
142.158898	3306.793921	6.328192	-0.028339	3.152332
142.292923	3314.910945	6.333197	-0.028369	3.155974
142.409624	3322.895296	6.338202	-0.028396	3.159552
142.764578	3330.870504	6.343206	-0.028467	3.163132
142.898654	3338.942821	6.348211	-0.028498	3.166742
143.050081	3346.975811	6.353216	-0.028531	3.170331
143.649448	3354.997164	6.358221	-0.028648	3.173929
143.740616	3363.064273	6.363226	-0.028670	3.177522
143.872179	3371.121216	6.368230	-0.028700	3.181109
144.079764	3379.112472	6.373235	-0.028743	3.184665
144.302068	3387.142357	6.378240	-0.028790	3.188235
144.473431	3395.216557	6.383245	-0.028827	3.191818
144.466038	3403.280969	6.388250	-0.028831	3.195386
144.695761	3411.253359	6.393254	-0.028879	3.198919
144.900299	3419.302885	6.398259	-0.028922	3.202481
144.915663	3427.347541	6.403264	-0.028930	3.206029
145.210469	3435.359076	6.408269	-0.028990	3.209570
145.334254	3443.411381	6.413274	-0.029018	3.213117
145.614062	3451.441602	6.418278	-0.029075	3.216658
145.781469	3459.452251	6.423283	-0.029112	3.220182
145.999683	3467.445623	6.428288	-0.029158	3.223696
146.131920	3475.512222	6.433293	-0.029187	3.227234
146.189838	3483.573275	6.438298	-0.029203	3.230764
146.582414	3491.652704	6.443302	-0.029282	3.234311
146.740473	3499.662146	6.448307	-0.029316	3.237814
146.834333	3507.652645	6.453312	-0.029339	3.241303
146.993311	3515.631429	6.458317	-0.029374	3.244785
147.222047	3523.661228	6.463322	-0.029421	3.248289
147.271087	3531.706339	6.468326	-0.029436	3.251788
147.461434	3539.757203	6.473331	-0.029476	3.255291
147.537189	3547.782004	6.478336	-0.029495	3.258775
147.805478	3555.794894	6.483341	-0.029551	3.262258
147.898372	3563.833258	6.488346	-0.029573	3.265741
148.101564	3571.836949	6.493350	-0.029616	3.269209
148.668042	3579.898588	6.498355	-0.029727	3.272713
148.678801	3587.937871	6.503360	-0.029734	3.276182
148.865355	3595.942194	6.508365	-0.029774	3.279639
149.049769	3603.951625	6.513370	-0.029813	3.283095
149.301828	3611.983089	6.518374	-0.029865	3.286558
149.486367	3620.020518	6.523379	-0.029905	3.290019
149.530083	3628.101009	6.528384	-0.029918	3.293488
149.899309	3636.122940	6.533389	-0.029992	3.296941
150.026940	3644.116756	6.538394	-0.030021	3.300370
150.169850	3652.124157	6.543398	-0.030053	3.303801
150.488552	3660.176176	6.548403	-0.030117	3.307254
150.666987	3668.206084	6.553408	-0.030156	3.310689
150.980593	3676.299075	6.558413	-0.030219	3.314152
151.055638	3684.294979	6.563418	-0.030238	3.317561
151.314877	3692.299749	6.568422	-0.030292	3.320978
151.579932	3700.285930	6.573427	-0.030346	3.324383
151.531979	3708.321956	6.578432	-0.030342	3.327794
152.031842	3716.377738	6.583437	-0.030441	3.331230
151.939267	3724.445354	6.588442	-0.030429	3.334646
152.423250	3732.423581	6.593446	-0.030524	3.338042
152.936843	3740.448945	6.598451	-0.030625	3.341455
153.048535	3748.457127	6.603456	-0.030651	3.344843
153.295355	3756.484693	6.608461	-0.030702	3.348240
153.469884	3764.560138	6.613466	-0.030739	3.351652
153.848078	3772.561037	6.618470	-0.030815	3.355036
153.932042	3780.620818	6.623475	-0.030836	3.358430
154.057371	3788.651061	6.628480	-0.030864	3.361810
154.405750	3796.656166	6.633485	-0.030934	3.365185
154.432858	3804.687324	6.638490	-0.030944	3.368555
154.630455	3812.729113	6.643494	-0.030986	3.371932
154.937339	3820.792874	6.648499	-0.031049	3.375319
155.087513	3828.775908	6.653504	-0.031082	3.378663
155.204023	3836.799690	6.658509	-0.031109	3.382020
155.463857	3844.817869	6.663514	-0.031162	3.385376
155.700469	3852.854336	6.668518	-0.031211	3.388736
155.954208	3860.944691	6.673523	-0.031264	3.392115
156.204537	3869.021762	6.678528	-0.031316	3.395485
156.439405	3876.979810	6.683533	-0.031365	3.398802
156.427068	3884.978479	6.688538	-0.031367	3.402124
156.623015	3892.982623	6.693542	-0.031409	3.405452
157.051752	3901.018999	6.698547	-0.031494	3.408798
157.085703	3909.052557	6.703552	-0.031505	3.412126
157.283253	3917.100042	6.708557	-0.031547	3.415463
157.568622	3925.090791	6.713562	-0.031606	3.418775
157.800650	3933.104426	6.718566	-0.031654	3.422092
157.948123	3941.144273	6.723571	-0.031687	3.425413
158.274854	3949.159080	6.728576	-0.031753	3.428727
158.611556	3957.206779	6.733581	-0.031821	3.432052
158.935629	3965.239937	6.738586	-0.031886	3.435367
159.075268	3973.264894	6.743590	-0.031917	3.438669
159.500722	3981.273614	6.748595	-0.032002	3.441971
159.605862	3989.267492	6.753600	-0.032026	3.445253
159.990597	3997.311965	6.758605	-0.032103	3.448561
160.279549	4005.364460	6.763610	-0.032162	3.451867
160.446019	4013.399551	6.768614	-0.032198	3.455158
160.683885	4021.444293	6.773619	-0.032248	3.458452
160.775614	4029.433547	6.778624	-0.032270	3.461716
161.024188	4037.502868	6.783629	-0.032321	3.465015
161.167754	4045.532409	6.788634	-0.032353	3.468290
161.097069	4053.592049	6.793638	-0.032345	3.471568
161.728147	4061.602765	6.798643	-0.032468	3.474845
161.860800	4069.587792	6.803648	-0.032498	3.478093
161.964982	4077.627242	6.808653	-0.032522	3.481359
162.247719	4085.613992	6.813658	-0.032580	3.484606
162.517508	4093.624771	6.818662	-0.032635	3.487860
162.551795	4101.701003	6.823667	-0.032647	3.491129
162.591764	4109.717944	6.828672	-0.032660	3.494372
162.836004	4117.745740	6.833677	-0.032710	3.497622
163.009348	4125.770391	6.838682	-0.032748	3.500866
163.029562	4133.776505	6.843686	-0.032757	3.504094
163.480138	4141.808625	6.848691	-0.032846	3.507344
163.417685	4149.851583	6.853696	-0.032839	3.510578
163.541085	4157.905477	6.858701	-0.032867	3.513820
163.852096	4165.898011	6.863706	-0.032930	3.517040
164.045131	4173.907070	6.868710	-0.032971	3.520260
164.067839	4181.949055	6.873715	-0.032981	3.523485
164.201172	4189.930722	6.878720	-0.033011	3.526687
164.651336	4197.945537	6.883725	-0.033100	3.529908
164.655567	4206.042371	6.888730	-0.033106	3.533145
164.680295	4214.076281	6.893734	-0.033116	3.536356
164.966309	4222.077422	6.898739	-0.033174	3.539557
165.145042	4230.093247	6.903744	-0.033212	3.542759
165.337833	4238.142011	6.908749	-0.033253	3.545971
165.448771	4246.178408	6.913754	-0.033279	3.549173
165.944558	4254.227121	6.918758	-0.033377	3.552389
166.182278	4262.302605	6.923763	-0.033426	3.555604
165.981592	4270.270187	6.928768	-0.033394	3.558761
166.442801	4278.276778	6.933773	-0.033485	3.561949
166.843018	4286.265319	6.938778	-0.033565	3.565126
166.767675	4294.289955	6.943782	-0.033556	3.568301
167.126423	4302.345041	6.948787	-0.033628	3.571497
167.199464	4310.351815	6.953792	-0.033646	3.574663
167.398339	4318.380248	6.958797	-0.033689	3.577838
167.677133	4326.415618	6.963802	-0.033746	3.581016
167.758372	4334.378333	6.968806	-0.033766	3.584156
168.249679	4342.442039	6.973811	-0.033863	3.587346
168.205028	4350.459078	6.978816	-0.033859	3.590498
168.404548	4358.516370	6.983821	-0.033902	3.593671
168.521607	4366.562959	6.988826	-0.033929	3.596834
168.709898	4374.524008	6.993830	-0.033969	3.599963
169.038361	4382.564096	6.998835	-0.034035	3.603124
169.121049	4390.557988	7.003840	-0.034056	3.606257
169.379325	4398.587070	7.008845	-0.034109	3.609406
169.552142	4406.654125	7.013850	-0.034146	3.612565
169.573905	4414.685462	7.018854	-0.034156	3.615703
170.067676	4422.692833	7.023859	-0.034253	3.618842
170.245178	4430.693633	7.028864	-0.034291	3.621967
170.400981	4438.703756	7.033869	-0.034325	3.625092
170.479463	4446.761592	7.038874	-0.034345	3.628231
170.790034	4454.778906	7.043878	-0.034408	3.631357
171.006768	4462.839556	7.048883	-0.034453	3.634496
170.981130	4470.839658	7.053888	-0.034454	3.637601
171.322102	4478.846139	7.058893	-0.034522	3.640716
171.349845	4486.857113	7.063898	-0.034533	3.643822
171.491537	4494.883217	7.068902	-0.034564	3.646934
171.832242	4502.921135	7.073907	-0.034633	3.650053
171.994994	4510.955663	7.078912	-0.034668	3.653164
172.225628	4518.993288	7.083917	-0.034716	3.656274
172.331004	4527.013223	7.088922	-0.034741	3.659372
172.343441	4535.014735	7.093926	-0.034749	3.662458
172.710997	4543.064609	7.098931	-0.034822	3.665569
172.759157	4551.087901	7.103936	-0.034836	3.668659
173.027977	4559.113676	7.108941	-0.034892	3.671753
173.309129	4567.145519	7.113946	-0.034949	3.674847
173.892477	4575.110338	7.118950	-0.035063	3.677920
174.407863	4583.106163	7.123955	-0.035164	3.681001
174.405167	4591.138530	7.128960	-0.035169	3.684080
174.539161	4599.204430	7.133965	-0.035199	3.687173
174.817963	4607.248810	7.138970	-0.035256	3.690258
175.112019	4615.242684	7.143974	-0.035316	3.693322
175.335117	4623.315042	7.148979	-0.035362	3.696412
175.527804	4631.284976	7.153984	-0.035403	3.699459
175.738474	4639.307893	7.158989	-0.035448	3.702524
175.563236	4647.336502	7.163994	-0.035420	3.705579
175.757287	4655.350932	7.168998	-0.035462	3.708635
176.173979	4663.433981	7.174003	-0.035544	3.711721
176.136287	4671.502377	7.179008	-0.035543	3.714787
176.432066	4679.479464	7.184013	-0.035603	3.717824
176.803228	4687.509394	7.189018	-0.035677	3.720881
176.879356	4695.453800	7.194022	-0.035696	3.723895
177.127117	4703.500887	7.199027	-0.035748	3.726950
177.299683	4711.486052	7.204032	-0.035785	3.729977
177.348431	4719.550876	7.209037	-0.035799	3.733029
177.482670	4727.595433	7.214042	-0.035829	3.736072
177.560461	4735.547623	7.219046	-0.035849	3.739077
177.986973	4743.628344	7.224051	-0.035933	3.742136
178.258758	4751.600484	7.229056	-0.035989	3.745149
178.128903	4759.645723	7.234061	-0.035970	3.748176
178.423283	4767.726580	7.239066	-0.036030	3.751225
178.558185	4775.720249	7.244070	-0.036060	3.754234
178.762694	4783.751826	7.249075	-0.036104	3.757258
179.040092	4791.752199	7.254080	-0.036160	3.760268
179.280113	4799.761411	7.259085	-0.036210	3.763279
179.461569	4807.784906	7.264090	-0.036249	3.766291
179.773352	4815.785265	7.269094	-0.036312	3.769295
179.963136	4823.877189	7.274099	-0.036353	3.772328
180.055956	4831.895587	7.279104	-0.036375	3.775329
180.447834	4839.916514	7.284109	-0.036454	3.778335
180.495962	4847.941333	7.289114	-0.036468	3.781332
180.586280	4855.914758	7.294118	-0.036490	3.784309
180.907562	4864.000463	7.299123	-0.036555	3.787331
181.171607	4871.994739	7.304128	-0.036609	3.790314
181.424471	4880.080855	7.309133	-0.036661	3.793329
181.636626	4888.098678	7.314138	-0.036706	3.796316
181.459028	4896.026636	7.319142	-0.036678	3.799258
181.683410	4904.069010	7.324147	-0.036725	3.802249
181.903186	4912.054117	7.329152	-0.036771	3.805217
181.928097	4920.140382	7.334157	-0.036781	3.808215
182.261944	4928.188014	7.339162	-0.036848	3.811204
182.379364	4936.131522	7.344166	-0.036875	3.814146
182.587283	4944.206859	7.349171	-0.036919	3.817138
182.865154	4952.139225	7.354176	-0.036976	3.820075
183.203071	4960.169088	7.359181	-0.037044	3.823047
183.057899	4968.222944	7.364186	-0.037022	3.826016
183.321943	4976.235856	7.369190	-0.037076	3.828976
183.685954	4984.280755	7.374195	-0.037149	3.831948
183.604312	4992.304798	7.379200	-0.037139	3.834900
183.790977	5000.303662	7.384205	-0.037179	3.837846
183.861645	5008.303414	7.389210	-0.037197	3.840788
184.072099	5016.294668	7.394214	-0.037242	3.843727
184.146647	5024.368691	7.399219	-0.037261	3.846692
184.325238	5032.380144	7.404224	-0.037299	3.849634
184.646567	5040.400088	7.409229	-0.037364	3.852579
184.851508	5048.454098	7.414234	-0.037408	3.855532
184.912851	5056.457442	7.419238	-0.037424	3.858461
185.060728	5064.531332	7.424243	-0.037457	3.861416
185.295587	5072.522060	7.429248	-0.037506	3.864340
185.647961	5080.538187	7.434253	-0.037576	3.867273
185.666569	5088.591598	7.439258	-0.037585	3.870211
185.879217	5096.779426	7.444262	-0.037630	3.873199
186.172428	5104.831245	7.449267	-0.037690	3.876137
186.349981	5112.693858	7.454272	-0.037728	3.879002
186.432466	5120.708328	7.459277	-0.037748	3.881918
186.586268	5128.672618	7.464282	-0.037782	3.884815
186.714734	5136.689865	7.469286	-0.037811	3.887728
187.232473	5144.743288	7.474291	-0.037913	3.890660
187.411734	5152.739098	7.479296	-0.037951	3.893562
187.244986	5160.819563	7.484301	-0.037925	3.896486
187.452026	5168.768185	7.489306	-0.037969	3.899368
187.755778	5176.802330	7.494310	-0.038031	3.902280
187.964982	5184.813849	7.499315	-0.038075	3.905179
187.956811	5192.812454	7.504320	-0.038078	3.908068
188.265594	5200.857679	7.509325	-0.038141	3.910977
188.452422	5208.888480	7.514330	-0.038181	3.913877
188.550182	5216.909969	7.519334	-0.038204	3.916770
188.809531	5224.913551	7.524339	-0.038258	3.919657
189.120701	5232.909224	7.529344	-0.038321	3.922539
189.222249	5240.918966	7.534349	-0.038345	3.925421
189.472406	5248.966237	7.539354	-0.038397	3.928317
189.597580	5256.962362	7.544358	-0.038425	3.931191
189.866180	5265.039891	7.549363	-0.038480	3.934093
190.012307	5273.048618	7.554368	-0.038513	3.936967
190.276386	5281.029491	7.559373	-0.038567	3.939831
190.482399	5289.076752	7.564378	-0.038611	3.942715
190.593858	5297.020305	7.569382	-0.038636	3.945559
190.971708	5305.048259	7.574387	-0.038712	3.948435
191.120080	5313.123222	7.579392	-0.038745	3.951322
191.349078	5321.205471	7.584397	-0.038793	3.954211
191.605897	5329.205693	7.589402	-0.038846	3.957069
191.722691	5337.166902	7.594406	-0.038872	3.959908
192.080414	5345.208186	7.599411	-0.038944	3.962778
192.056198	5353.191335	7.604416	-0.038945	3.965619
192.667689	5361.195425	7.609421	-0.039064	3.968476
192.539531	5369.275981	7.614426	-0.039045	3.971345
192.753053	5377.292457	7.619430	-0.039090	3.974196
192.895903	5385.350692	7.624435	-0.039122	3.977058
193.062970	5393.278907	7.629440	-0.039158	3.979872
193.282438	5401.329335	7.634445	-0.039204	3.982728
193.411706	5409.375745	7.639450	-0.039233	3.985580
193.468419	5417.406641	7.644454	-0.039249	3.988422
193.629888	5425.426077	7.649459	-0.039284	3.991260
193.827368	5433.463779	7.654464	-0.039326	3.994104
193.967589	5441.498430	7.659469	-0.039357	3.996943
194.218810	5449.455002	7.664474	-0.039409	3.999754
194.376174	5457.487108	7.669478	-0.039444	4.002589
195.006990	5465.490210	7.674483	-0.039566	4.005418
195.058143	5473.534296	7.679488	-0.039581	4.008251
195.102970	5481.581722	7.684493	-0.039595	4.011083
195.303703	5489.618110	7.689498	-0.039637	4.013912
195.527831	5497.624546	7.694502	-0.039684	4.016728
195.664620	5505.621898	7.699507	-0.039715	4.019538
195.690786	5513.671639	7.704512	-0.039725	4.022362
196.218733	5521.626586	7.709517	-0.039828	4.025159
196.605012	5529.682646	7.714522	-0.039905	4.027988
196.430184	5537.713695	7.719526	-0.039878	4.030796
196.679348	5545.839002	7.724531	-0.039929	4.033643
197.064490	5553.857081	7.729536	-0.040006	4.036452
197.159500	5561.758403	7.734541	-0.040029	4.039213
197.484690	5569.764463	7.739546	-0.040095	4.042013
197.381257	5577.760471	7.744550	-0.040081	4.044801
197.694871	5585.817721	7.749555	-0.040144	4.047615
197.728272	5593.810077	7.754560	-0.040156	4.050400
197.880258	5601.840645	7.759565	-0.040189	4.053197
198.250871	5609.896411	7.764570	-0.040263	4.056005
198.405602	5617.857316	7.769574	-0.040297	4.058775
198.565655	5625.910710	7.774579	-0.040332	4.061575
198.648621	5633.903649	7.779584	-0.040353	4.064351
198.841109	5641.964211	7.784589	-0.040394	4.067151
198.809080	5649.963922	7.789594	-0.040393	4.069924
199.137607	5657.989569	7.794598	-0.040459	4.072709
199.444331	5666.001892	7.799603	-0.040521	4.075487
199.484162	5674.009810	7.804608	-0.040534	4.078258
199.629700	5682.003604	7.809613	-0.040566	4.081024
199.833809	5689.999646	7.814618	-0.040609	4.083789
199.898213	5698.082730	7.819622	-0.040627	4.086581
199.958704	5706.123556	7.824627	-0.040643	4.089356
200.065874	5714.139962	7.829632	-0.040668	4.092122
200.169403	5722.141139	7.834637	-0.040693	4.094880
200.547387	5730.153400	7.839642	-0.040768	4.097644
200.916823	5738.118924	7.844646	-0.040842	4.100390
201.037972	5746.168544	7.849651	-0.040870	4.103159
201.116267	5754.186223	7.854656	-0.040889	4.105915
201.326133	5762.221589	7.859661	-0.040934	4.108677
201.572199	5770.240149	7.864666	-0.040985	4.111432
201.521802	5778.308179	7.869670	-0.040980	4.114198
201.612044	5786.340800	7.874675	-0.041002	4.116952
201.612474	5794.291920	7.879680	-0.041008	4.119675
202.004553	5802.304009	7.884685	-0.041086	4.122422
202.016036	5810.331125	7.889690	-0.041093	4.125168
202.059930	5818.349615	7.894694	-0.041106	4.127909
202.487563	5826.386846	7.899699	-0.041191	4.130659
202.543212	5834.444991	7.904704	-0.041207	4.133410
202.719003	5842.459320	7.909709	-0.041245	4.136146
203.170135	5850.437051	7.914714	-0.041334	4.138871
203.165998	5858.469547	7.919718	-0.041338	4.141607
203.447392	5866.473334	7.924723	-0.041396	4.144335
203.449443	5874.519039	7.929728	-0.041401	4.147072
203.892985	5882.502148	7.934733	-0.041489	4.149792
203.987714	5890.615056	7.939738	-0.041512	4.152549
203.887675	5898.592090	7.944742	-0.041498	4.155256
204.107691	5906.598180	7.949747	-0.041544	4.157975
204.359791	5914.584554	7.954752	-0.041596	4.160686
204.644268	5922.601867	7.959757	-0.041655	4.163406
204.894751	5930.657063	7.964762	-0.041706	4.166136
204.870757	5938.621741	7.969766	-0.041707	4.168831
205.064727	5946.722755	7.974771	-0.041748	4.171573
205.134276	5954.728002	7.979776	-0.041766	4.174279
205.181877	5962.754007	7.984781	-0.041780	4.176990
205.553070	5970.704219	7.989786	-0.041855	4.179678
205.567158	5978.735344	7.994790	-0.041862	4.182387
205.776939	5986.757877	7.999795	-0.041907	4.185093
206.034233	5994.794350	8.004800	-0.041960	4.187803
206.294757	6002.780373	8.009805	-0.042013	4.190494
206.658155	6010.910376	8.014810	-0.042086	4.193233
206.780830	6018.942991	8.019814	-0.042114	4.195935
206.993594	6026.880380	8.024819	-0.042159	4.198604
207.130954	6034.882960	8.029824	-0.042190	4.201292
207.492164	6042.840899	8.034829	-0.042262	4.203966
207.798423	6050.892387	8.039834	-0.042324	4.206669
207.862613	6058.879326	8.044838	-0.042341	4.209346
207.993910	6066.933665	8.049843	-0.042371	4.212045
208.208990	6074.943079	8.054848	-0.042416	4.214728
208.339723	6082.990133	8.059853	-0.042446	4.217420
208.571727	6090.969259	8.064858	-0.042494	4.220090
208.594976	6099.002804	8.069862	-0.042503	4.222773
208.789268	6106.982120	8.074867	-0.042545	4.225439
208.780349	6115.033423	8.079872	-0.042548	4.228125
209.062695	6123.053186	8.084877	-0.042606	4.230801
209.229225	6131.123712	8.089882	-0.042642	4.233492
209.429009	6139.101875	8.094886	-0.042685	4.236150
209.774036	6147.091278	8.099891	-0.042754	4.238812
209.857176	6155.143118	8.104896	-0.042775	4.241490
209.916435	6163.049473	8.109901	-0.042791	4.244119
210.008119	6171.178935	8.114906	-0.042813	4.246819
210.141648	6179.123322	8.119910	-0.042843	4.249457
210.400228	6187.245286	8.124915	-0.042896	4.252154
210.498107	6195.255430	8.129920	-0.042920	4.254810
210.679948	6203.247583	8.134925	-0.042959	4.257459
210.847266	6211.261226	8.139930	-0.042995	4.260114
210.836948	6219.281918	8.144934	-0.042998	4.262768
211.277504	6227.324778	8.149939	-0.043085	4.265431
211.299529	6235.337704	8.154944	-0.043095	4.268079
211.423896	6243.351023	8.159949	-0.043123	4.270727
211.675533	6251.401984	8.164954	-0.043175	4.273386
211.859191	6259.384096	8.169958	-0.043214	4.276020
212.108532	6267.398882	8.174963	-0.043266	4.278664
212.213467	6275.421496	8.179968	-0.043291	4.281308
212.471188	6283.403484	8.184973	-0.043344	4.283938
212.653388	6291.473082	8.189978	-0.043383	4.286595
212.505710	6299.423080	8.194982	-0.043360	4.289207
212.612705	6307.500777	8.199987	-0.043386	4.291863
212.880508	6315.525347	8.204992	-0.043441	4.294500
213.225414	6323.556882	8.209997	-0.043510	4.297139
213.266931	6331.509477	8.215002	-0.043523	4.299748
213.340127	6339.535709	8.220006	-0.043542	4.302379
213.594093	6347.561610	8.225011	-0.043594	4.305010
213.767041	6355.598272	8.230016	-0.043631	4.307643
213.762723	6363.645056	8.235021	-0.043636	4.310276
214.026048	6371.683829	8.240026	-0.043690	4.312906
214.031779	6379.643760	8.245030	-0.043696	4.315508
214.261914	6387.689408	8.250035	-0.043744	4.318137
214.616298	6395.670254	8.255040	-0.043815	4.320744
214.831694	6403.705164	8.260045	-0.043861	4.323367
215.079588	6411.736656	8.265050	-0.043912	4.325987
214.998769	6419.723862	8.270054	-0.043902	4.328588
215.088295	6427.784998	8.275059	-0.043924	4.331214
214.991594	6435.788905	8.280064	-0.043911	4.333817
215.258207	6443.779181	8.285069	-0.043966	4.336418
215.643992	6451.800642	8.290074	-0.044043	4.339027
215.710249	6459.810800	8.295078	-0.044060	4.341630
215.897285	6467.789585	8.300083	-0.044100	4.344221
216.245372	6475.855537	8.305088	-0.044170	4.346840
216.253717	6483.854527	8.310093	-0.044177	4.349433
216.382319	6491.971501	8.315098	-0.044206	4.352064
216.377837	6500.027669	8.320102	-0.044210	4.354673
216.611037	6508.035659	8.325107	-0.044259	4.357266
216.740275	6515.933753	8.330112	-0.044288	4.359822
216.854475	6523.936344	8.335117	-0.044314	4.362409
217.235178	6531.920185	8.340122	-0.044390	4.364991
217.137936	6539.936502	8.345126	-0.044377	4.367578
217.350418	6547.972924	8.350131	-0.044422	4.370173
217.485544	6556.022455	8.355136	-0.044453	4.372769
217.758406	6564.016116	8.360141	-0.044508	4.375347
218.036474	6572.049418	8.365146	-0.044565	4.377936
218.091895	6580.004353	8.370150	-0.044581	4.380497
218.540363	6588.051018	8.375155	-0.044670	4.383088
218.600013	6596.055202	8.380160	-0.044686	4.385662
218.798505	6604.091788	8.385165	-0.044728	4.388246
218.905659	6612.124100	8.390170	-0.044753	4.390826
219.056821	6620.187669	8.395174	-0.044786	4.393414
219.181890	6628.213670	8.400179	-0.044815	4.395989
219.351082	6636.200822	8.405184	-0.044851	4.398551
219.489757	6644.157149	8.410189	-0.044882	4.401100
219.617976	6652.196352	8.415194	-0.044911	4.403675
219.861936	6660.191582	8.420198	-0.044962	4.406235
219.959739	6668.223222	8.425203	-0.044985	4.408804
220.012845	6676.285711	8.430208	-0.045000	4.411381
220.313504	6684.316778	8.435213	-0.045062	4.413948
220.676017	6692.370271	8.440218	-0.045134	4.416521
220.727962	6700.322783	8.445222	-0.045149	4.419058
220.849710	6708.384606	8.450227	-0.045177	4.421630
220.729937	6716.341125	8.455232	-0.045160	4.424165
221.109628	6724.382043	8.460237	-0.045235	4.426728
221.468717	6732.418269	8.465242	-0.045308	4.429287
221.601613	6740.431140	8.470246	-0.045337	4.431837
221.711269	6748.534469	8.475251	-0.045363	4.434414
221.835546	6756.532286	8.480256	-0.045391	4.436956
221.910370	6764.444960	8.485261	-0.045410	4.439469
222.110971	6772.522787	8.490266	-0.045453	4.442034
222.114705	6780.439667	8.495270	-0.045459	4.444545
222.386366	6788.507214	8.500275	-0.045514	4.447104
222.687888	6796.538723	8.505280	-0.045576	4.449650
222.774549	6804.550105	8.510285	-0.045597	4.452187
222.890168	6812.619019	8.515290	-0.045624	4.454741
222.880075	6820.586564	8.520294	-0.045627	4.457261
223.137642	6828.593867	8.525299	-0.045680	4.459794
223.206952	6836.629848	8.530304	-0.045698	4.462333
223.223933	6844.601831	8.535309	-0.045706	4.464850
223.343301	6852.662235	8.540314	-0.045734	4.467394
223.454049	6860.648176	8.545318	-0.045760	4.469913
223.975832	6868.721216	8.550323	-0.045862	4.472460
223.860909	6876.721876	8.555328	-0.045846	4.474980
224.174280	6884.736226	8.560333	-0.045909	4.477505
224.175634	6892.726813	8.565338	-0.045915	4.480019
224.397385	6900.742418	8.570343	-0.045961	4.482541
224.670394	6908.754156	8.575347	-0.046017	4.485060
224.588755	6916.781061	8.580352	-0.046007	4.487581
224.686928	6924.751987	8.585357	-0.046030	4.490084
224.940973	6932.867210	8.590362	-0.046083	4.492631
225.067968	6940.822062	8.595367	-0.046112	4.495126
225.116235	6948.889732	8.600371	-0.046126	4.497655
225.239435	6956.858602	8.605376	-0.046154	4.500152
225.473359	6964.846921	8.610381	-0.046203	4.502653
225.923447	6972.864836	8.615386	-0.046291	4.505164
225.667323	6980.870488	8.620391	-0.046249	4.507666
225.879891	6988.912543	8.625395	-0.046294	4.510181
226.083220	6997.064221	8.630400	-0.046337	4.512728
226.216783	7005.051103	8.635405	-0.046367	4.515221
226.331218	7013.001576	8.640410	-0.046393	4.517702
226.508979	7020.950983	8.645415	-0.046431	4.520182
226.581839	7028.990773	8.650419	-0.046450	4.522688
226.783763	7036.959943	8.655424	-0.046493	4.525171
226.832761	7045.020912	8.660429	-0.046507	4.527681
227.126831	7053.070660	8.665434	-0.046567	4.530186
226.888087	7061.073285	8.670439	-0.046528	4.532674
227.163349	7069.100027	8.675443	-0.046584	4.535170
227.303573	7077.130136	8.680448	-0.046615	4.537665
227.386267	7085.047392	8.685453	-0.046636	4.540123
227.627227	7093.098884	8.690458	-0.046686	4.542622
227.677819	7101.093556	8.695463	-0.046701	4.545101
227.791781	7109.141642	8.700467	-0.046727	4.547596
227.966818	7117.165654	8.705472	-0.046765	4.550082
228.216947	7125.194759	8.710477	-0.046816	4.552568
228.042903	7133.252626	8.715482	-0.046789	4.555062
228.437029	7141.211219	8.720487	-0.046868	4.557524
228.684689	7149.227467	8.725491	-0.046919	4.560002
228.891611	7157.205901	8.730496	-0.046963	4.562467
228.992273	7165.221537	8.735501	-0.046986	4.564942
229.055181	7173.290290	8.740506	-0.047003	4.567432
229.035189	7181.286836	8.745511	-0.047005	4.569899
229.185445	7189.362070	8.750515	-0.047038	4.572388
229.302183	7197.388162	8.755520	-0.047065	4.574861
229.436149	7205.342536	8.760525	-0.047095	4.577311
229.886035	7213.380467	8.765530	-0.047184	4.579785
230.124137	7221.387973	8.770535	-0.047233	4.582248
230.227898	7229.378896	8.775539	-0.047258	4.584705
230.512803	7237.427597	8.780544	-0.047316	4.587178
230.579924	7245.408010	8.785549	-0.047334	4.589629
230.808124	7253.497206	8.790554	-0.047381	4.592112
231.005670	7261.542067	8.795559	-0.047423	4.594580
231.159147	7269.528256	8.800563	-0.047457	4.597028
231.297354	7277.475988	8.805568	-0.047488	4.599464
231.487258	7285.541115	8.810573	-0.047528	4.601934
231.616891	7293.483190	8.815578	-0.047558	4.604365
231.637002	7301.556178	8.820583	-0.047567	4.606835
231.868919	7309.556793	8.825587	-0.047615	4.609281
232.106876	7317.635328	8.830592	-0.047664	4.611750
232.126846	7325.614049	8.835597	-0.047673	4.614187
232.344376	7333.682931	8.840602	-0.047719	4.616650
232.482082	7341.579136	8.845607	-0.047750	4.619060
232.619846	7349.660777	8.850611	-0.047780	4.621524
232.752231	7357.647405	8.855616	-0.047810	4.623958
232.772258	7365.677169	8.860621	-0.047819	4.626404
233.068662	7373.741211	8.865626	-0.047879	4.628860
233.091150	7381.644116	8.870631	-0.047889	4.631264
233.126703	7389.744193	8.875635	-0.047901	4.633728
233.310258	7397.789250	8.880640	-0.047940	4.636173
233.455544	7405.742975	8.885645	-0.047972	4.638590
233.537384	7413.799514	8.890650	-0.047992	4.641036
233.766474	7421.769083	8.895655	-0.048040	4.643455
233.992570	7429.786134	8.900659	-0.048087	4.645887
234.034224	7437.819375	8.905664	-0.048100	4.648322
234.176018	7445.849911	8.910669	-0.048132	4.650755
234.334786	7453.896108	8.915674	-0.048167	4.653192
234.330105	7461.859424	8.920679	-0.048171	4.655603
234.404445	7469.888033	8.925683	-0.048190	4.658032
234.533799	7477.902473	8.930688	-0.048219	4.660455
234.886731	7485.894070	8.935693	-0.048290	4.662870
235.045836	7493.896436	8.940698	-0.048325	4.665287
235.204193	7501.910259	8.945703	-0.048359	4.667706
235.137463	7509.966671	8.950707	-0.048352	4.670137
235.192465	7518.078545	8.955712	-0.048368	4.672583
235.242154	7526.069320	8.960717	-0.048382	4.674992
235.651479	7534.116782	8.965722	-0.048463	4.677416
235.818103	7541.999352	8.970727	-0.048499	4.679789
235.837885	7549.994171	8.975731	-0.048508	4.682195
236.164795	7558.017629	8.980736	-0.048574	4.684608
236.246296	7566.088637	8.985741	-0.048595	4.687035
236.475183	7574.056648	8.990746	-0.048642	4.689429
236.362349	7582.058998	8.995751	-0.048627	4.691832
236.902461	7590.097569	9.000755	-0.048732	4.694245
236.794745	7598.112391	9.005760	-0.048717	4.696649
236.777656	7606.102729	9.010765	-0.048719	4.699046
237.271361	7614.203774	9.015770	-0.048816	4.701473
237.288358	7622.141157	9.020775	-0.048825	4.703850
237.216349	7630.148679	9.025779	-0.048816	4.706248
237.499517	7638.192110	9.030784	-0.048874	4.708654
237.733209	7646.209120	9.035789	-0.048923	4.711052
237.779815	7654.287352	9.040794	-0.048937	4.713467
237.854060	7662.283227	9.045799	-0.048956	4.715856
238.208151	7670.272933	9.050803	-0.049027	4.718241
238.168827	7678.268764	9.055808	-0.049025	4.720628
238.256664	7686.288564	9.060813	-0.049046	4.723020
238.333443	7694.323895	9.065818	-0.049066	4.725416
238.365127	7702.324169	9.070823	-0.049077	4.727800
238.671284	7710.363511	9.075827	-0.049139	4.730194
238.671116	7718.407335	9.080832	-0.049144	4.732589
238.795313	7726.375624	9.085837	-0.049172	4.734960
239.125463	7734.461260	9.090842	-0.049239	4.737364
238.981676	7742.422477	9.095847	-0.049217	4.739731
239.362257	7750.448636	9.100851	-0.049293	4.742115
239.393945	7758.470130	9.105856	-0.049304	4.744497
239.306501	7766.449186	9.110861	-0.049293	4.746865
239.770019	7774.469675	9.115866	-0.049385	4.749243
239.959996	7782.484018	9.120871	-0.049425	4.751619
240.060771	7790.549931	9.125875	-0.049449	4.754009
240.288881	7798.575003	9.130880	-0.049497	4.756386
240.336911	7806.500862	9.135885	-0.049511	4.758732
240.485679	7814.529973	9.140890	-0.049544	4.761108
240.451058	7822.536699	9.145895	-0.049542	4.763476
240.702901	7830.532903	9.150899	-0.049594	4.765839
240.917932	7838.597196	9.155904	-0.049640	4.768221
240.938353	7846.589172	9.160909	-0.049649	4.770582
241.249193	7854.675543	9.165914	-0.049712	4.772967
241.447145	7862.634450	9.170919	-0.049754	4.775315
241.363783	7870.622280	9.175923	-0.049743	4.777671
241.371081	7878.666083	9.180928	-0.049750	4.780042
241.631946	7886.636735	9.185933	-0.049803	4.782389
241.877729	7894.694986	9.190938	-0.049854	4.784760
241.991257	7902.680175	9.195943	-0.049881	4.787110
242.345545	7910.703497	9.200947	-0.049952	4.789469
242.521215	7918.748561	9.205952	-0.049990	4.791833
242.485263	7926.806315	9.210957	-0.049988	4.794201
242.609153	7934.817221	9.215962	-0.050016	4.796554
242.740798	7942.753515	9.220967	-0.050046	4.798883
243.005212	7950.795750	9.225971	-0.050100	4.801242
243.102545	7958.789469	9.230976	-0.050124	4.803586
243.129376	7966.783921	9.235981	-0.050134	4.805929
243.320089	7974.834939	9.240986	-0.050174	4.808287
243.331456	7982.869034	9.245991	-0.050182	4.810640
243.572643	7990.279172	9.250995	-0.050231	4.812808
243.745425	7994.793085	9.256000	-0.050266	4.814128

243.767617	7997.316302	9.261005	-0.050272	4.814866
243.999720	7998.616847	9.266010	-0.050316	4.815245
243.961581	7999.043179	9.271015	-0.050309	4.815370
244.016295	8000.096551	9.276019	-0.050320	4.815678
244.101597	8000.112870	9.281024	-0.050336	4.815682
244.400496	8000.135849	9.286029	-0.050391	4.815688
244.606633	8000.127438	9.291034	-0.050430	4.815684
244.578319	8000.112029	9.296039	-0.050424	4.815680
244.521918	8000.104704	9.301043	-0.050414	4.815678
244.638334	8000.108718	9.306048	-0.050435	4.815679
244.491764	8000.084988	9.311053	-0.050408	4.815672
244.692833	8000.124532	9.316058	-0.050445	4.815683
244.840393	8000.100228	9.321063	-0.050473	4.815675
244.885738	8000.103091	9.326067	-0.050481	4.815676
244.834988	8000.105465	9.331072	-0.050472	4.815677
244.904205	8000.128997	9.336077	-0.050484	4.815683
245.065174	8000.150812	9.341082	-0.050514	4.815689
244.790498	8000.111130	9.346087	-0.050463	4.815679
244.734520	8000.147579	9.351091	-0.050453	4.815690
245.072591	8000.116753	9.356096	-0.050516	4.815679
245.018559	8000.113736	9.361101	-0.050505	4.815678
245.100205	8000.119322	9.366106	-0.050521	4.815680
245.032910	8000.088336	9.371111	-0.050508	4.815671
245.158592	8000.146942	9.376115	-0.050531	4.815687
245.127857	8000.142168	9.381120	-0.050525	4.815686
245.142015	8000.125311	9.386125	-0.050528	4.815681
245.556061	8000.154429	9.391130	-0.050605	4.815688
245.268009	8000.126271	9.396135	-0.050551	4.815681
245.251267	8000.150546	9.401139	-0.050548	4.815688
245.472122	8000.128497	9.406144	-0.050589	4.815680
245.360847	8000.140566	9.411149	-0.050568	4.815685
245.503927	8000.161025	9.416154	-0.050595	4.815690
245.417220	8000.114778	9.421159	-0.050579	4.815677
245.448122	8000.119542	9.426163	-0.050584	4.815678
245.305508	8000.110821	9.431168	-0.050558	4.815676
245.304109	8000.130007	9.436173	-0.050557	4.815682
245.647009	8000.216686	9.441178	-0.050621	4.815705
245.484496	8000.182021	9.446183	-0.050591	4.815696
245.482293	8000.184114	9.451187	-0.050590	4.815697
245.497794	8000.157671	9.456192	-0.050593	4.815689
245.385445	8000.147305	9.461197	-0.050572	4.815686
245.465822	8000.178491	9.466202	-0.050587	4.815695
245.583802	8000.132357	9.471207	-0.050609	4.815681
245.417977	8000.168095	9.476211	-0.050578	4.815692
245.495285	8000.133045	9.481216	-0.050592	4.815682
245.562829	8000.133066	9.486221	-0.050605	4.815681
245.637345	8000.162022	9.491226	-0.050619	4.815690
245.452123	8000.110977	9.496231	-0.050584	4.815675
245.587520	8000.140919	9.501235	-0.050609	4.815684
245.766075	8000.123522	9.506240	-0.050642	4.815678
245.578870	8000.130091	9.511245	-0.050608	4.815680
245.636268	8000.139554	9.516250	-0.050618	4.815683
245.547118	8000.087931	9.521255	-0.050601	4.815668
245.645537	8000.099126	9.526259	-0.050620	4.815671
245.613514	8000.125289	9.531264	-0.050614	4.815679
245.568838	8000.136301	9.536269	-0.050605	4.815682
245.862532	8000.134647	9.541274	-0.050660	4.815680
245.591399	8000.130249	9.546279	-0.050609	4.815680
245.730577	8000.143172	9.551283	-0.050635	4.815684
245.848153	8000.145070	9.556288	-0.050657	4.815684
245.880586	8000.131711	9.561293	-0.050663	4.815680
245.900908	8000.135237	9.566298	-0.050667	4.815680
246.011613	8000.139159	9.571303	-0.050687	4.815681
245.937193	8000.130474	9.576307	-0.050673	4.815679
245.812130	8000.174345	9.581312	-0.050650	4.815692
245.979076	8000.157828	9.586317	-0.050681	4.815687
246.022931	8000.167072	9.591322	-0.050689	4.815689
245.999115	8000.131452	9.596327	-0.050685	4.815679
245.864341	8000.180503	9.601331	-0.050659	4.815694
245.954123	8000.159533	9.606336	-0.050676	4.815687
245.896588	8000.146852	9.611341	-0.050665	4.815684
246.039657	8000.163041	9.616346	-0.050692	4.815688
246.134285	8000.134677	9.621351	-0.050709	4.815679
246.068401	8000.149616	9.626355	-0.050697	4.815684
245.961066	8000.143600	9.631360	-0.050677	4.815683
245.850625	8000.156750	9.636365	-0.050656	4.815687
246.149521	8000.180802	9.641370	-0.050712	4.815693
246.082671	8000.119931	9.646375	-0.050699	4.815675
246.198560	8000.169841	9.651379	-0.050721	4.815689
246.172248	8000.151260	9.656384	-0.050716	4.815684
246.195991	8000.143098	9.661389	-0.050720	4.815681
246.092941	8000.170245	9.666394	-0.050701	4.815690
246.089398	8000.150966	9.671399	-0.050700	4.815684
246.204373	8000.147485	9.676403	-0.050722	4.815683
246.299660	8000.155427	9.681408	-0.050739	4.815685
246.268617	8000.141040	9.686413	-0.050733	4.815680
246.373616	8000.181166	9.691418	-0.050753	4.815692
246.318382	8000.154644	9.696423	-0.050742	4.815684
246.334169	8000.181581	9.701427	-0.050745	4.815692
246.198219	8000.154819	9.706432	-0.050720	4.815685
246.155576	8000.131703	9.711437	-0.050712	4.815678
246.201178	8000.143111	9.716442	-0.050720	4.815681
245.978637	8000.118148	9.721447	-0.050679	4.815675
246.010228	8000.158152	9.726451	-0.050685	4.815687
246.125367	8000.130121	9.731456	-0.050706	4.815678
246.062327	8000.103472	9.736461	-0.050694	4.815670
246.292820	8000.157374	9.741466	-0.050737	4.815685
246.359461	8000.070910	9.746471	-0.050749	4.815660
246.229227	8000.073064	9.751475	-0.050725	4.815661
246.082372	8000.100569	9.756480	-0.050698	4.815670
246.165174	8000.105106	9.761485	-0.050713	4.815670
246.327098	8000.138682	9.766490	-0.050743	4.815680
246.218827	8000.130516	9.771495	-0.050723	4.815678
246.127420	8000.154649	9.776499	-0.050706	4.815685
246.228635	8000.145607	9.781504	-0.050725	4.815682
246.138264	8000.135596	9.786509	-0.050708	4.815680
246.291199	8000.162621	9.791514	-0.050736	4.815687
246.246508	8000.133067	9.796519	-0.050728	4.815678
246.248339	8000.172589	9.801523	-0.050728	4.815690
246.344265	8000.169867	9.806528	-0.050746	4.815689
246.361919	8000.097554	9.811533	-0.050749	4.815667
246.281818	8000.147491	9.816538	-0.050734	4.815682
246.169734	8000.121116	9.821543	-0.050713	4.815675
246.367562	8000.128585	9.826547	-0.050750	4.815676
246.501556	8000.155303	9.831552	-0.050775	4.815684
246.396500	8000.126906	9.836557	-0.050755	4.815676
246.367857	8000.108287	9.841562	-0.050750	4.815670
246.350041	8000.140018	9.846567	-0.050746	4.815680
246.402611	8000.129121	9.851571	-0.050756	4.815676
246.398634	8000.129050	9.856576	-0.050755	4.815676
246.435434	8000.117897	9.861581	-0.050762	4.815673
246.465962	8000.139736	9.866586	-0.050767	4.815679
246.455092	8000.148093	9.871591	-0.050765	4.815682
246.608243	8000.135623	9.876595	-0.050794	4.815677
246.570442	8000.158490	9.881600	-0.050787	4.815684
246.495097	8000.144452	9.886605	-0.050773	4.815680
246.501079	8000.143475	9.891610	-0.050774	4.815680
246.450789	8000.126641	9.896615	-0.050764	4.815675
246.508708	8000.152126	9.901619	-0.050775	4.815683
246.518514	8000.128793	9.906624	-0.050777	4.815676
246.322323	8000.150160	9.911629	-0.050740	4.815683
246.389092	8000.169384	9.916634	-0.050752	4.815688
246.168434	8000.138046	9.921639	-0.050711	4.815680
246.321177	8000.159730	9.926643	-0.050740	4.815686
246.601488	8000.141848	9.931648	-0.050792	4.815679
246.405986	8000.138673	9.936653	-0.050755	4.815679
246.511957	8000.132911	9.941658	-0.050775	4.815677
246.725024	8000.112872	9.946663	-0.050814	4.815670
246.544065	8000.146229	9.951667	-0.050781	4.815681
246.587306	8000.136248	9.956672	-0.050789	4.815678
246.481491	8000.145202	9.961677	-0.050769	4.815681
246.597196	8000.150274	9.966682	-0.050790	4.815682
246.461815	8000.155546	9.971687	-0.050765	4.815684
246.675878	8000.172887	9.976691	-0.050805	4.815688
246.674592	8000.160049	9.981696	-0.050805	4.815684
246.705595	8000.150937	9.986701	-0.050810	4.815681
246.701794	8000.175422	9.991706	-0.050810	4.815689
246.593946	8000.121359	9.996711	-0.050789	4.815673
246.555149	8000.129264	10.001715	-0.050782	4.815676
246.578099	8000.145642	10.006720	-0.050786	4.815680
246.430282	8000.148578	10.011725	-0.050759	4.815682
246.700875	8000.160430	10.016730	-0.050809	4.815684
246.614044	8000.134463	10.021735	-0.050793	4.815677
246.605120	8000.163135	10.026739	-0.050791	4.815685
246.680620	8000.157947	10.031744	-0.050805	4.815684
246.596159	8000.151234	10.036749	-0.050789	4.815682
246.707178	8000.185053	10.041754	-0.050810	4.815691
246.689481	8000.145261	10.046759	-0.050806	4.815680
246.678222	8000.160017	10.051763	-0.050804	4.815684
246.820928	8000.152716	10.056768	-0.050831	4.815681
246.644157	8000.157317	10.061773	-0.050798	4.815684
246.907743	8000.179731	10.066778	-0.050847	4.815689
246.756513	8000.110019	10.071783	-0.050818	4.815669
246.598978	8000.150161	10.076787	-0.050789	4.815682
246.660395	8000.156487	10.081792	-0.050800	4.815683
246.727116	8000.122333	10.086797	-0.050813	4.815673
246.743221	8000.163154	10.091802	-0.050816	4.815685
246.711482	8000.130607	10.096807	-0.050810	4.815675
246.719930	8000.158494	10.101811	-0.050811	4.815684
246.803911	8000.170524	10.106816	-0.050827	4.815687
246.728573	8000.161824	10.111821	-0.050813	4.815685
247.039740	8000.160455	10.116826	-0.050871	4.815683
246.729676	8000.149018	10.121831	-0.050813	4.815681
246.796138	8000.173575	10.126835	-0.050825	4.815688
246.919231	8000.148875	10.131840	-0.050848	4.815680
246.817562	8000.133343	10.136845	-0.050829	4.815676
246.757718	8000.159055	10.141850	-0.050818	4.815684
246.664234	8000.140453	10.146855	-0.050800	4.815679
246.736751	8000.171513	10.151859	-0.050814	4.815687
246.946638	8000.162097	10.156864	-0.050853	4.815684
246.716121	8000.155152	10.161869	-0.050810	4.815683
246.884928	8000.161084	10.166874	-0.050841	4.815684
246.760299	8000.140910	10.171879	-0.050818	4.815678
246.612322	8000.159856	10.176883	-0.050790	4.815685
246.701212	8000.146344	10.181888	-0.050807	4.815680
246.755486	8000.150420	10.186893	-0.050817	4.815681
246.619926	8000.177040	10.191898	-0.050791	4.815690
246.749586	8000.154582	10.196903	-0.050815	4.815682
246.615759	8000.157744	10.201907	-0.050790	4.815684
246.717010	8000.152974	10.206912	-0.050809	4.815682
246.749525	8000.108657	10.211917	-0.050815	4.815669
247.067549	8000.169318	10.216922	-0.050874	4.815685
246.953414	8000.182407	10.221927	-0.050853	4.815690
246.934467	8000.185296	10.226931	-0.050849	4.815690
246.827342	8000.186756	10.231936	-0.050829	4.815691
247.004123	8000.159723	10.236941	-0.050862	4.815683
246.848683	8000.170008	10.241946	-0.050833	4.815686
246.791623	8000.126375	10.246951	-0.050822	4.815674
246.986735	8000.169030	10.251955	-0.050859	4.815685
246.898052	8000.178262	10.256960	-0.050842	4.815689
246.606063	8000.182063	10.261965	-0.050788	4.815691
247.161105	8000.197458	10.266970	-0.050891	4.815693
246.989355	8000.137020	10.271975	-0.050859	4.815676
246.923299	8000.178645	10.276979	-0.050847	4.815689
246.935231	8000.169224	10.281984	-0.050849	4.815686
246.913956	8000.148590	10.286989	-0.050845	4.815680
246.866930	8000.179847	10.291994	-0.050836	4.815689
246.833972	8000.159023	10.296999	-0.050830	4.815683
246.886221	8000.172674	10.302003	-0.050839	4.815687
246.900087	8000.179298	10.307008	-0.050842	4.815689
246.740943	8000.147888	10.312013	-0.050812	4.815680
246.883702	8000.170479	10.317018	-0.050839	4.815686
246.963244	8000.140803	10.322023	-0.050853	4.815677
246.752644	8000.132045	10.327027	-0.050814	4.815676
246.818299	8000.162994	10.332032	-0.050826	4.815685
247.069153	8000.140365	10.337037	-0.050873	4.815677
247.152868	8000.145986	10.342042	-0.050888	4.815678
246.765668	8000.143974	10.347047	-0.050816	4.815679
246.856299	8000.157179	10.352051	-0.050833	4.815683
247.258935	8000.167969	10.357056	-0.050908	4.815684
246.896442	8000.120453	10.362061	-0.050840	4.815672
247.079260	8000.165044	10.367066	-0.050874	4.815684
247.093980	8000.107628	10.372071	-0.050877	4.815667
247.037317	8000.152608	10.377075	-0.050866	4.815680
247.060776	8000.173265	10.382080	-0.050871	4.815686
246.883200	8000.160773	10.387085	-0.050837	4.815684
247.054341	8000.173148	10.392090	-0.050869	4.815686
247.004261	8000.163789	10.397095	-0.050860	4.815684
246.858402	8000.146473	10.402099	-0.050833	4.815680
247.077940	8000.163903	10.407104	-0.050873	4.815684
246.906258	8000.151506	10.412109	-0.050841	4.815681
247.138172	8000.165934	10.417114	-0.050884	4.815684
247.017690	8000.151164	10.422119	-0.050862	4.815680
247.141775	8000.149967	10.427123	-0.050885	4.815679
247.070363	8000.164816	10.432128	-0.050872	4.815684
246.813758	8000.133962	10.437133	-0.050824	4.815676
247.151586	8000.127688	10.442138	-0.050887	4.815673
246.836484	8000.140722	10.447143	-0.050828	4.815678
246.976755	8000.148327	10.452147	-0.050854	4.815680
247.278513	8000.162820	10.457152	-0.050910	4.815682
247.000240	8000.125209	10.462157	-0.050858	4.815673
247.175966	8000.167550	10.467162	-0.050891	4.815684
247.226284	8000.134198	10.472167	-0.050900	4.815674
247.019633	8000.157530	10.477171	-0.050862	4.815682
247.119522	8000.145265	10.482176	-0.050880	4.815678
247.012319	8000.139250	10.487181	-0.050860	4.815677
247.154206	8000.178908	10.492186	-0.050886	4.815688
247.039105	8000.123659	10.497191	-0.050865	4.815672
247.138313	8000.118855	10.502195	-0.050883	4.815670
247.444215	8000.162239	10.507200	-0.050940	4.815681
247.138529	8000.142331	10.512205	-0.050883	4.815677
247.054813	8000.177265	10.517210	-0.050867	4.815688
247.170641	8000.139636	10.522215	-0.050889	4.815676
247.303460	8000.187688	10.527219	-0.050914	4.815690
247.167780	8000.188685	10.532224	-0.050888	4.815690
247.121525	8000.134551	10.537229	-0.050880	4.815675
247.176307	8000.165324	10.542234	-0.050890	4.815684
247.019670	8000.143562	10.547239	-0.050860	4.815678
247.073416	8000.186062	10.552243	-0.050870	4.815690
247.167056	8000.177965	10.557248	-0.050888	4.815687
247.070162	8000.137956	10.562253	-0.050870	4.815676
246.879323	8000.157275	10.567258	-0.050834	4.815683
247.297785	8000.144836	10.572263	-0.050912	4.815677
247.454140	8000.175120	10.577267	-0.050941	4.815685
247.295160	8000.193888	10.582272	-0.050911	4.815691
247.050759	8000.164298	10.587277	-0.050866	4.815684
247.200718	8000.173128	10.592282	-0.050894	4.815686
247.229495	8000.149034	10.597287	-0.050899	4.815679
247.162398	8000.173561	10.602291	-0.050886	4.815686
247.167197	8000.188578	10.607296	-0.050887	4.815690
247.139152	8000.141145	10.612301	-0.050882	4.815677
247.259083	8000.181515	10.617306	-0.050904	4.815688
247.238931	8000.147020	10.622311	-0.050900	4.815678
247.145626	8000.159379	10.627315	-0.050883	4.815682
247.189256	8000.172890	10.632320	-0.050891	4.815686
247.197285	8000.111096	10.637325	-0.050892	4.815668
247.334224	8000.179498	10.642330	-0.050918	4.815687
247.324368	8000.160116	10.647335	-0.050916	4.815681
247.096898	8000.173503	10.652339	-0.050873	4.815686
247.199205	8000.174087	10.657344	-0.050892	4.815686
247.085366	8000.147682	10.662349	-0.050871	4.815679
247.187546	8000.154669	10.667354	-0.050890	4.815680
247.235876	8000.150108	10.672359	-0.050899	4.815679
247.462824	8000.153781	10.677363	-0.050941	4.815679
247.366170	8000.179964	10.682368	-0.050923	4.815687
247.316745	8000.140724	10.687373	-0.050914	4.815676
247.476184	8000.173194	10.692378	-0.050943	4.815685
247.311931	8000.149174	10.697383	-0.050913	4.815678
247.199428	8000.175100	10.702387	-0.050892	4.815686
247.270460	8000.181583	10.707392	-0.050905	4.815688
247.215900	8000.149733	10.712397	-0.050895	4.815679
247.112648	8000.189687	10.717402	-0.050875	4.815691
247.146926	8000.173156	10.722407	-0.050882	4.815686
247.088224	8000.194616	10.727411	-0.050871	4.815693
247.264601	8000.200672	10.732416	-0.050903	4.815694
247.149912	8000.147564	10.737421	-0.050882	4.815679
247.214578	8000.161416	10.742426	-0.050894	4.815682
247.327517	8000.140822	10.747431	-0.050915	4.815676
247.238172	8000.167123	10.752435	-0.050898	4.815684
247.471812	8000.175175	10.757440	-0.050942	4.815685
247.389723	8000.134338	10.762445	-0.050926	4.815674
247.272055	8000.138829	10.767450	-0.050904	4.815675
247.407580	8000.147425	10.772455	-0.050929	4.815677
247.548052	8000.134750	10.777459	-0.050955	4.815673
247.392549	8000.163182	10.782464	-0.050926	4.815682
247.284712	8000.135806	10.787469	-0.050906	4.815675
247.314024	8000.145883	10.792474	-0.050912	4.815677
247.411878	8000.146395	10.797479	-0.050930	4.815677
247.356847	8000.151902	10.802483	-0.050919	4.815679
247.396012	8000.168544	10.807488	-0.050927	4.815684
247.466958	8000.154741	10.812493	-0.050940	4.815679
247.360982	8000.194652	10.817498	-0.050920	4.815691
247.399694	8000.161111	10.822503	-0.050927	4.815681
247.419201	8000.150745	10.827507	-0.050931	4.815678
247.563228	8000.147736	10.832512	-0.050957	4.815677
247.502748	8000.138208	10.837517	-0.050946	4.815674
247.671895	8000.181512	10.842522	-0.050978	4.815686
247.677233	8000.169848	10.847527	-0.050978	4.815683
247.376445	8000.179911	10.852531	-0.050922	4.815687
247.507120	8000.174551	10.857536	-0.050947	4.815685
247.593522	8000.153526	10.862541	-0.050963	4.815678
247.546290	8000.168767	10.867546	-0.050954	4.815683
247.361566	8000.155091	10.872551	-0.050919	4.815680
247.477723	8000.113197	10.877555	-0.050941	4.815667
247.630849	8000.160511	10.882560	-0.050969	4.815680
247.579010	8000.084935	10.887565	-0.050960	4.815658
247.638800	8000.174505	10.892570	-0.050971	4.815684
247.809672	8000.151648	10.897575	-0.051002	4.815677
247.763570	8000.158367	10.902579	-0.050994	4.815679
247.811556	8000.169814	10.907584	-0.051003	4.815682
247.736084	8000.162178	10.912589	-0.050988	4.815680
247.806241	8000.194269	10.917594	-0.051001	4.815689
247.557828	8000.173154	10.922599	-0.050955	4.815684
247.707596	8000.176643	10.927603	-0.050983	4.815685
247.555334	8000.184844	10.932608	-0.050955	4.815688
247.419433	8000.114310	10.937613	-0.050929	4.815668
247.672470	8000.171784	10.942618	-0.050976	4.815683
247.814424	8000.124971	10.947623	-0.051003	4.815669
247.559544	8000.125103	10.952627	-0.050955	4.815670
247.694471	8000.147567	10.957632	-0.050980	4.815676
247.832259	8000.123106	10.962637	-0.051006	4.815668
247.793545	8000.152363	10.967642	-0.050998	4.815677
247.749835	8000.156986	10.972647	-0.050990	4.815679
247.839216	8000.160564	10.977651	-0.051007	4.815679
247.743221	8000.155798	10.982656	-0.050989	4.815678
247.578020	8000.110411	10.987661	-0.050958	4.815666
247.573972	8000.160514	10.992666	-0.050957	4.815680
247.766700	8000.158295	10.997671	-0.050993	4.815679
247.760069	8000.167789	11.002675	-0.050992	4.815682
247.664725	8000.134210	11.007680	-0.050974	4.815672
247.774483	8000.086875	11.012685	-0.050994	4.815658
247.907295	8000.129589	11.017690	-0.051019	4.815670
247.735999	8000.126805	11.022695	-0.050987	4.815670
247.686798	8000.158028	11.027699	-0.050978	4.815679
247.716540	8000.172382	11.032704	-0.050983	4.815683
247.629257	8000.133596	11.037709	-0.050967	4.815672
247.705577	8000.148705	11.042714	-0.050981	4.815676
247.639798	8000.118808	11.047719	-0.050969	4.815668
247.716028	8000.122173	11.052723	-0.050983	4.815669
247.864576	8000.159804	11.057728	-0.051010	4.815679
247.780021	8000.157359	11.062733	-0.050994	4.815679
247.823311	8000.148447	11.067738	-0.051002	4.815676
247.513104	8000.162627	11.072743	-0.050945	4.815681
247.591452	8000.129729	11.077747	-0.050959	4.815671
247.713145	8000.153047	11.082752	-0.050982	4.815678
247.640315	8000.139049	11.087757	-0.050968	4.815674
247.447784	8000.147664	11.092762	-0.050932	4.815677
247.612822	8000.137523	11.097767	-0.050963	4.815674
247.702749	8000.134704	11.102771	-0.050979	4.815672
247.949232	8000.140829	11.107776	-0.051025	4.815673
247.931898	8000.102109	11.112781	-0.051022	4.815662
247.984769	8000.147797	11.117786	-0.051032	4.815675
247.679936	8000.101214	11.122791	-0.050975	4.815663
247.770207	8000.112279	11.127795	-0.050992	4.815665
247.959993	8000.156985	11.132800	-0.051027	4.815678
247.745820	8000.114006	11.137805	-0.050987	4.815666
247.781767	8000.137001	11.142810	-0.050994	4.815673
247.783505	8000.128482	11.147815	-0.050994	4.815670
247.962494	8000.121769	11.152819	-0.051027	4.815667
247.972730	8000.162497	11.157824	-0.051029	4.815679
247.790064	8000.107218	11.162829	-0.050995	4.815664
247.711920	8000.144377	11.167834	-0.050980	4.815675
247.833340	8000.118582	11.172839	-0.051003	4.815667
247.658133	8000.132816	11.177843	-0.050970	4.815672
247.798164	8000.171377	11.182848	-0.050996	4.815683
247.650489	8000.141220	11.187853	-0.050968	4.815675
247.594994	8000.167003	11.192858	-0.050958	4.815682
247.688293	8000.166374	11.197863	-0.050975	4.815682
247.965416	8000.161252	11.202867	-0.051027	4.815679
248.000345	8000.190637	11.207872	-0.051033	4.815687
247.612954	8000.145917	11.212877	-0.050961	4.815676
247.904223	8000.170917	11.217882	-0.051015	4.815682
247.956925	8000.152548	11.222887	-0.051025	4.815676
247.856850	8000.145581	11.227891	-0.051006	4.815675
247.948701	8000.191902	11.232896	-0.051023	4.815688
247.797176	8000.161682	11.237901	-0.050995	4.815680
247.941495	8000.180029	11.242906	-0.051022	4.815685
247.871083	8000.141516	11.247911	-0.051009	4.815674
247.812156	8000.182189	11.252915	-0.050998	4.815686
247.786230	8000.173222	11.257920	-0.050993	4.815683
247.759525	8000.132215	11.262925	-0.050988	4.815671
248.181950	8000.170018	11.267930	-0.051066	4.815680
247.913089	8000.160314	11.272935	-0.051016	4.815679
247.711932	8000.155978	11.277939	-0.050979	4.815679
247.906404	8000.156990	11.282944	-0.051015	4.815678
247.788852	8000.143334	11.287949	-0.050993	4.815675
247.797266	8000.135991	11.292954	-0.050994	4.815672
247.575750	8000.109975	11.297959	-0.050953	4.815666
247.833142	8000.083182	11.302963	-0.051001	4.815657
248.016196	8000.165143	11.307968	-0.051035	4.815680
247.583983	8000.104751	11.312973	-0.050954	4.815664
247.697532	8000.134342	11.317978	-0.050975	4.815672
247.786722	8000.125106	11.322983	-0.050992	4.815669
247.601276	8000.123160	11.327987	-0.050957	4.815670
247.934774	8000.163791	11.332992	-0.051019	4.815680
247.909881	8000.136691	11.337997	-0.051015	4.815672
247.789908	8000.163564	11.343002	-0.050992	4.815680
247.766537	8000.142895	11.348007	-0.050988	4.815675
247.797069	8000.118829	11.353011	-0.050993	4.815667
247.913324	8000.153802	11.358016	-0.051015	4.815677
247.784867	8000.134632	11.363021	-0.050991	4.815672
247.726109	8000.179578	11.368026	-0.050980	4.815685
247.570197	8000.167436	11.373031	-0.050951	4.815683
247.642733	8000.118430	11.378035	-0.050964	4.815668
247.869925	8000.149864	11.383040	-0.051006	4.815676
247.898548	8000.117227	11.388045	-0.051012	4.815666
247.875230	8000.156342	11.393050	-0.051007	4.815678
247.685644	8000.154330	11.398055	-0.050972	4.815678
247.820522	8000.123415	11.403059	-0.050997	4.815669
247.734347	8000.179660	11.408064	-0.050981	4.815685
247.853363	8000.121800	11.413069	-0.051003	4.815668
247.796633	8000.141157	11.418074	-0.050992	4.815674
248.064426	8000.151898	11.423079	-0.051042	4.815676
248.054876	8000.142129	11.428083	-0.051040	4.815673
248.007185	8000.176579	11.433088	-0.051031	4.815683
248.005116	8000.170134	11.438093	-0.051031	4.815681
248.025098	8000.151235	11.443098	-0.051034	4.815676
247.929716	8000.128331	11.448103	-0.051017	4.815670
247.903853	8000.146053	11.453107	-0.051012	4.815675
247.998380	8000.161458	11.458112	-0.051029	4.815679
247.992685	8000.143211	11.463117	-0.051028	4.815674
247.915499	8000.146223	11.468122	-0.051014	4.815675
247.943534	8000.131725	11.473127	-0.051019	4.815670
248.037653	8000.166339	11.478131	-0.051036	4.815680
247.756315	8000.173514	11.483136	-0.050984	4.815684
247.759194	8000.160744	11.488141	-0.050984	4.815680
247.805908	8000.183914	11.493146	-0.050993	4.815686
247.794360	8000.153828	11.498151	-0.050991	4.815678
247.967395	8000.164100	11.503155	-0.051023	4.815680
247.881889	8000.171248	11.508160	-0.051007	4.815682
247.658918	8000.112113	11.513165	-0.050965	4.815666
247.848966	8000.171769	11.518170	-0.051001	4.815683
248.036233	8000.142772	11.523175	-0.051035	4.815673
247.844851	8000.137527	11.528179	-0.051000	4.815673
247.875869	8000.176456	11.533184	-0.051005	4.815684
247.921168	8000.132346	11.538189	-0.051014	4.815671
247.942849	8000.144434	11.543194	-0.051018	4.815674
247.832027	8000.176793	11.548199	-0.050997	4.815684
247.867244	8000.153871	11.553203	-0.051003	4.815677
248.022079	8000.139294	11.558208	-0.051032	4.815672
247.872601	8000.137932	11.563213	-0.051004	4.815673
247.825676	8000.155313	11.568218	-0.050995	4.815678
248.010309	8000.152963	11.573223	-0.051030	4.815676
248.035144	8000.139480	11.578227	-0.051034	4.815672
247.909075	8000.156646	11.583232	-0.051011	4.815678
247.966859	8000.115941	11.588237	-0.051021	4.815666
248.077998	8000.160440	11.593242	-0.051042	4.815678
248.219372	8000.166996	11.598247	-0.051068	4.815680
248.079699	8000.141238	11.603251	-0.051042	4.815673
248.122401	8000.157938	11.608256	-0.051050	4.815677
247.963484	8000.106246	11.613261	-0.051020	4.815663
247.869735	8000.141017	11.618266	-0.051003	4.815674
248.002183	8000.130347	11.623271	-0.051027	4.815670
247.993505	8000.140876	11.628275	-0.051026	4.815673
248.020714	8000.175473	11.633280	-0.051031	4.815683
248.188708	8000.173920	11.638285	-0.051062	4.815682
248.106836	8000.160843	11.643290	-0.051047	4.815678
247.947123	8000.157179	11.648295	-0.051017	4.815678
247.849918	8000.153461	11.653299	-0.050999	4.815677
248.026752	8000.163795	11.658304	-0.051032	4.815680
248.063256	8000.154773	11.663309	-0.051038	4.815677
248.178804	8000.167316	11.668314	-0.051060	4.815680
248.178547	8000.174778	11.673319	-0.051060	4.815682
247.899133	8000.163835	11.678323	-0.051008	4.815680
248.075884	8000.160289	11.683328	-0.051040	4.815678
247.967474	8000.116890	11.688333	-0.051020	4.815666
248.262329	8000.165435	11.693338	-0.051075	4.815679
248.025211	8000.121016	11.698343	-0.051031	4.815667
248.146159	8000.147525	11.703347	-0.051053	4.815674
248.000319	8000.192127	11.708352	-0.051026	4.815688
247.892235	8000.130584	11.713357	-0.051006	4.815670
247.917987	8000.117116	11.718362	-0.051010	4.815666
247.930702	8000.146140	11.723367	-0.051013	4.815675
248.111772	8000.151205	11.728371	-0.051046	4.815675
247.972918	8000.153217	11.733376	-0.051020	4.815677
247.813324	8000.100448	11.738381	-0.050991	4.815662
248.171900	8000.124404	11.743386	-0.051057	4.815667
248.010757	8000.147406	11.748391	-0.051027	4.815675
248.023871	8000.129464	11.753395	-0.051030	4.815670
248.157431	8000.160447	11.758400	-0.051054	4.815678
247.893245	8000.102779	11.763405	-0.051005	4.815662
247.754646	8000.121877	11.768410	-0.050979	4.815669
247.954907	8000.145401	11.773415	-0.051016	4.815675
248.159134	8000.098530	11.778419	-0.051054	4.815660
248.013912	8000.153818	11.783424	-0.051027	4.815677
247.944457	8000.118523	11.788429	-0.051014	4.815667
248.040867	8000.157445	11.793434	-0.051032	4.815678
247.968826	8000.134919	11.798439	-0.051019	4.815671
248.056422	8000.154481	11.803443	-0.051035	4.815677
248.221194	8000.160349	11.808448	-0.051066	4.815678
248.040818	8000.146742	11.813453	-0.051032	4.815675
248.051077	8000.143699	11.818458	-0.051034	4.815674
248.064326	8000.147111	11.823463	-0.051036	4.815675
248.025489	8000.121920	11.828467	-0.051029	4.815667
248.236711	8000.142420	11.833472	-0.051068	4.815672
248.077068	8000.088582	11.838477	-0.051038	4.815657
248.201654	8000.131163	11.843482	-0.051061	4.815669
248.253065	8000.129855	11.848487	-0.051071	4.815669
248.061125	8000.134209	11.853491	-0.051035	4.815671
248.203334	8000.171739	11.858496	-0.051061	4.815681
248.046225	8000.127549	11.863501	-0.051032	4.815669
248.127250	8000.175830	11.868506	-0.051047	4.815683
248.145016	8000.153692	11.873511	-0.051050	4.815676
248.096979	8000.107001	11.878515	-0.051041	4.815663
248.097392	8000.169988	11.883520	-0.051041	4.815681
248.121992	8000.134083	11.888525	-0.051046	4.815670
248.222390	8000.155989	11.893530	-0.051065	4.815676
248.080412	8000.152612	11.898535	-0.051038	4.815676
248.102093	8000.127336	11.903539	-0.051042	4.815669
248.057099	8000.139411	11.908544	-0.051033	4.815672
248.083663	8000.103538	11.913549	-0.051038	4.815662
248.195937	8000.145919	11.918554	-0.051059	4.815674
248.296137	8000.164619	11.923559	-0.051078	4.815679
248.047047	8000.157371	11.928563	-0.051031	4.815678
248.191969	8000.130890	11.933568	-0.051058	4.815669
248.087325	8000.104632	11.938573	-0.051039	4.815662
248.342113	8000.170677	11.943578	-0.051086	4.815680
248.278864	8000.173915	11.948583	-0.051074	4.815681
248.082366	8000.140830	11.953587	-0.051038	4.815673
248.157900	8000.170873	11.958592	-0.051052	4.815681
248.221215	8000.136663	11.963597	-0.051063	4.815671
248.237683	8000.178559	11.968602	-0.051066	4.815683
248.198946	8000.169384	11.973607	-0.051059	4.815680
248.259803	8000.186378	11.978611	-0.051070	4.815685
248.237001	8000.160380	11.983616	-0.051066	4.815678
248.026993	8000.109995	11.988621	-0.051027	4.815664
248.307031	8000.184989	11.993626	-0.051079	4.815685
248.179551	8000.141280	11.998631	-0.051055	4.815672
248.211748	8000.142863	12.003635	-0.051061	4.815673
248.267866	8000.158713	12.008640	-0.051071	4.815677
248.302454	8000.135781	12.013645	-0.051078	4.815670
248.334401	8000.149103	12.018650	-0.051084	4.815674
248.075581	8000.152373	12.023655	-0.051035	4.815676
247.993443	8000.162778	12.028659	-0.051020	4.815680
248.122569	8000.173406	12.033664	-0.051044	4.815682
248.010582	8000.149164	12.038669	-0.051023	4.815675
248.089892	8000.178201	12.043674	-0.051038	4.815684
248.156212	8000.183540	12.048679	-0.051050	4.815685
248.071687	8000.120244	12.053683	-0.051034	4.815667
248.197134	8000.163907	12.058688	-0.051057	4.815679
248.016182	8000.127872	12.063693	-0.051024	4.815669
248.084920	8000.138588	12.068698	-0.051036	4.815672
248.257910	8000.161670	12.073703	-0.051068	4.815678
248.117032	8000.120947	12.078707	-0.051042	4.815667
248.436750	8000.153882	12.083712	-0.051102	4.815675
248.240776	8000.143224	12.088717	-0.051065	4.815673
248.142057	8000.160834	12.093722	-0.051047	4.815678
248.250225	8000.171122	12.098727	-0.051067	4.815681
248.215062	8000.113964	12.103731	-0.051060	4.815664
248.212301	8000.155548	12.108736	-0.051059	4.815676
248.183706	8000.152943	12.113741	-0.051054	4.815676
248.069268	8000.177770	12.118746	-0.051033	4.815684
247.972970	8000.147377	12.123751	-0.051015	4.815675
247.880193	8000.158678	12.128755	-0.050997	4.815679
248.069047	8000.177747	12.133760	-0.051032	4.815684
248.047986	8000.148574	12.138765	-0.051028	4.815675
248.114639	8000.171000	12.143770	-0.051041	4.815681
247.961490	8000.148227	12.148775	-0.051012	4.815675
247.928153	8000.160490	12.153779	-0.051006	4.815679
247.967315	8000.185673	12.158784	-0.051013	4.815686
247.893568	8000.164187	12.163789	-0.050999	4.815680
247.975184	8000.163369	12.168794	-0.051014	4.815680
247.936413	8000.156328	12.173799	-0.051007	4.815678
247.842102	8000.149455	12.178803	-0.050989	4.815676
248.071456	8000.184127	12.183808	-0.051032	4.815685
247.906136	8000.135534	12.188813	-0.051001	4.815672
247.925078	8000.166794	12.193818	-0.051005	4.815681
247.956321	8000.164092	12.198823	-0.051010	4.815680
248.032947	8000.143976	12.203827	-0.051025	4.815674
247.913764	8000.154848	12.208832	-0.051002	4.815678
248.005008	8000.105078	12.213837	-0.051019	4.815663
248.263505	8000.166912	12.218842	-0.051067	4.815680
248.159584	8000.181234	12.223847	-0.051048	4.815684
247.925815	8000.137937	12.228851	-0.051004	4.815673
248.081137	8000.178881	12.233856	-0.051033	4.815684
247.930648	8000.129462	12.238861	-0.051005	4.815670
247.972699	8000.182448	12.243866	-0.051013	4.815685
248.033032	8000.169541	12.248871	-0.051024	4.815681
247.958248	8000.144836	12.253875	-0.051010	4.815675
248.014049	8000.169221	12.258880	-0.051020	4.815681
247.859293	8000.126138	12.263885	-0.050991	4.815670
248.041815	8000.142969	12.268890	-0.051025	4.815674
247.877124	8000.139225	12.273895	-0.050995	4.815673
247.934987	8000.158305	12.278899	-0.051005	4.815679
248.048873	8000.159077	12.283904	-0.051026	4.815678
248.076231	8000.106136	12.288909	-0.051031	4.815663
247.911738	8000.128017	12.293914	-0.051001	4.815670
247.973280	8000.143954	12.298919	-0.051012	4.815674
248.053686	8000.129238	12.303923	-0.051027	4.815670
247.990336	8000.168772	12.308928	-0.051015	4.815681
248.121332	8000.138862	12.313933	-0.051039	4.815672
248.155064	8000.166092	12.318938	-0.051046	4.815680
248.085377	8000.167091	12.323943	-0.051033	4.815680
248.073706	8000.104976	12.328947	-0.051030	4.815662
248.232336	8000.158785	12.333952	-0.051060	4.815677
248.263324	8000.131524	12.338957	-0.051066	4.815669
248.235691	8000.101178	12.343962	-0.051060	4.815660
248.160852	8000.167215	12.348967	-0.051046	4.815680
248.191877	8000.136752	12.353971	-0.051052	4.815671
248.289264	8000.173555	12.358976	-0.051070	4.815681
248.121762	8000.119589	12.363981	-0.051039	4.815666
248.343886	8000.116778	12.368986	-0.051080	4.815665
248.288601	8000.150038	12.373991	-0.051070	4.815675
248.285592	8000.120091	12.378995	-0.051069	4.815666
248.337651	8000.158293	12.384000	-0.051079	4.815677
248.209429	8000.154072	12.389005	-0.051055	4.815676
248.091256	8000.138271	12.394010	-0.051033	4.815672
248.101534	8000.144837	12.399015	-0.051035	4.815674
248.258612	8000.170864	12.404019	-0.051064	4.815681
248.202566	8000.166746	12.409024	-0.051053	4.815680
248.078188	8000.157250	12.414029	-0.051030	4.815678
248.289811	8000.175621	12.419034	-0.051069	4.815682
248.132122	8000.154909	12.424039	-0.051040	4.815677
248.023339	8000.136057	12.429043	-0.051020	4.815672
248.133760	8000.168801	12.434048	-0.051040	4.815681
248.205364	8000.146469	12.439053	-0.051053	4.815674
248.287111	8000.138180	12.444058	-0.051068	4.815671
248.358423	8000.161749	12.449063	-0.051082	4.815678
248.329046	8000.120698	12.454067	-0.051076	4.815666
248.298869	8000.173581	12.459072	-0.051070	4.815681
248.148039	8000.131629	12.464077	-0.051042	4.815670
248.226298	8000.154243	12.469082	-0.051057	4.815676
248.252672	8000.157867	12.474087	-0.051062	4.815677
248.245547	8000.151339	12.479091	-0.051060	4.815675
248.440558	8000.148090	12.484096	-0.051096	4.815673
248.549403	8000.129565	12.489101	-0.051117	4.815667
248.326577	8000.148364	12.494106	-0.051075	4.815674
248.357188	8000.154192	12.499111	-0.051081	4.815675
248.536491	8000.169904	12.504115	-0.051114	4.815679
248.539520	8000.204109	12.509120	-0.051114	4.815689
248.513114	8000.167377	12.514125	-0.051109	4.815679
248.552126	8000.175476	12.519130	-0.051117	4.815681
248.469106	8000.176258	12.524135	-0.051101	4.815681
248.407885	8000.176327	12.529139	-0.051090	4.815682
248.351353	8000.183944	12.534144	-0.051079	4.815684
248.515283	8000.175920	12.539149	-0.051110	4.815681
248.349420	8000.192440	12.544154	-0.051079	4.815687
248.212966	8000.167802	12.549159	-0.051053	4.815680
248.250024	8000.120356	12.554163	-0.051060	4.815666
248.418359	8000.193539	12.559168	-0.051091	4.815687
248.086670	8000.117694	12.564173	-0.051029	4.815666
248.190605	8000.169549	12.569178	-0.051049	4.815681
248.240740	8000.188504	12.574183	-0.051058	4.815686
248.378892	8000.150170	12.579187	-0.051083	4.815674
248.421066	8000.175402	12.584192	-0.051091	4.815681
248.465141	8000.151556	12.589197	-0.051099	4.815674
248.291132	8000.167944	12.594202	-0.051067	4.815680
248.434792	8000.164929	12.599207	-0.051094	4.815678
248.303469	8000.156388	12.604211	-0.051069	4.815676
248.598005	8000.191050	12.609216	-0.051124	4.815685
248.263981	8000.138653	12.614221	-0.051062	4.815671
248.287555	8000.156110	12.619226	-0.051066	4.815676
248.379350	8000.173606	12.624231	-0.051083	4.815681
248.208907	8000.136673	12.629235	-0.051051	4.815671
248.253256	8000.169413	12.634240	-0.051059	4.815680
248.251340	8000.134146	12.639245	-0.051059	4.815670
248.393265	8000.155657	12.644250	-0.051085	4.815676
248.459226	8000.173802	12.649255	-0.051097	4.815681
248.352501	8000.128294	12.654259	-0.051077	4.815668
248.494956	8000.125260	12.659264	-0.051104	4.815666
248.512259	8000.123399	12.664269	-0.051107	4.815666
248.247237	8000.124432	12.669274	-0.051058	4.815667
248.588198	8000.173726	12.674279	-0.051121	4.815680
248.452088	8000.185391	12.679283	-0.051096	4.815684
248.537704	8000.201719	12.684288	-0.051112	4.815689
248.346678	8000.169790	12.689293	-0.051076	4.815680
248.407399	8000.172903	12.694298	-0.051087	4.815681
248.360946	8000.167873	12.699303	-0.051078	4.815680
248.510044	8000.115838	12.704307	-0.051106	4.815664
248.575826	8000.185223	12.709312	-0.051118	4.815684
248.402235	8000.111942	12.714317	-0.051086	4.815663
248.392191	8000.130989	12.719322	-0.051084	4.815669
248.487220	8000.160280	12.724327	-0.051102	4.815677
248.475219	8000.132322	12.729331	-0.051099	4.815669
248.510140	8000.156369	12.734336	-0.051106	4.815675
248.524126	8000.113886	12.739341	-0.051108	4.815663
248.691649	8000.149691	12.744346	-0.051139	4.815673
248.656281	8000.196085	12.749351	-0.051133	4.815686
248.429874	8000.160379	12.754355	-0.051090	4.815677
248.293273	8000.177374	12.759360	-0.051065	4.815683
248.272852	8000.159955	12.764365	-0.051061	4.815678
248.296542	8000.174211	12.769370	-0.051065	4.815682
248.360374	8000.149618	12.774375	-0.051077	4.815674
248.204713	8000.118263	12.779379	-0.051048	4.815666
248.279866	8000.167516	12.784384	-0.051062	4.815680
248.365934	8000.136878	12.789389	-0.051078	4.815670
248.521934	8000.171429	12.794394	-0.051107	4.815680
248.319228	8000.153189	12.799399	-0.051069	4.815675
248.361095	8000.146388	12.804403	-0.051077	4.815673
248.551285	8000.195372	12.809408	-0.051112	4.815687
248.381598	8000.166992	12.814413	-0.051081	4.815679
248.222210	8000.145184	12.819418	-0.051051	4.815674
248.492738	8000.152768	12.824423	-0.051101	4.815675
248.623080	8000.145267	12.829427	-0.051125	4.815672
248.439497	8000.194595	12.834432	-0.051091	4.815687
248.382479	8000.124271	12.839437	-0.051080	4.815667
248.157662	8000.135565	12.844442	-0.051038	4.815671
248.415613	8000.173904	12.849447	-0.051086	4.815681
248.310298	8000.122014	12.854451	-0.051067	4.815666
248.408646	8000.146021	12.859456	-0.051085	4.815673
248.397027	8000.113799	12.864461	-0.051083	4.815664
248.556106	8000.084345	12.869466	-0.051112	4.815654
248.487352	8000.125926	12.874471	-0.051099	4.815667
248.519946	8000.126449	12.879475	-0.051105	4.815667
248.540133	8000.168405	12.884480	-0.051109	4.815679
248.535845	8000.122423	12.889485	-0.051108	4.815665
248.491802	8000.117432	12.894490	-0.051100	4.815664
248.465794	8000.184261	12.899495	-0.051095	4.815684
248.504559	8000.165667	12.904499	-0.051102	4.815678
248.499339	8000.183725	12.909504	-0.051101	4.815684
248.395593	8000.147874	12.914509	-0.051082	4.815674
248.446120	8000.136943	12.919514	-0.051091	4.815670
248.519536	8000.158411	12.924519	-0.051105	4.815676
248.468827	8000.119150	12.929523	-0.051095	4.815665
248.575311	8000.176384	12.934528	-0.051115	4.815681
248.401346	8000.150070	12.939533	-0.051082	4.815674
248.430666	8000.158012	12.944538	-0.051088	4.815676
248.692399	8000.170791	12.949543	-0.051136	4.815679
248.529965	8000.143596	12.954547	-0.051106	4.815672
248.575803	8000.162481	12.959552	-0.051115	4.815677
248.582731	8000.152979	12.964557	-0.051116	4.815674
248.561311	8000.166504	12.969562	-0.051112	4.815678
248.723669	8000.158455	12.974567	-0.051142	4.815675
248.507841	8000.131461	12.979571	-0.051102	4.815668
248.639534	8000.164550	12.984576	-0.051126	4.815677
248.393060	8000.165884	12.989581	-0.051080	4.815679
248.767987	8000.159148	12.994586	-0.051150	4.815675
248.637153	8000.160222	12.999591	-0.051125	4.815676
248.519744	8000.143365	13.004595	-0.051103	4.815672
248.490753	8000.194132	13.009600	-0.051098	4.815687
248.433180	8000.117394	13.014605	-0.051087	4.815665
248.424270	8000.104433	13.019610	-0.051085	4.815661
248.528936	8000.172313	13.024615	-0.051105	4.815680
248.597950	8000.163818	13.029619	-0.051118	4.815677
248.684289	8000.198307	13.034624	-0.051134	4.815687
248.519373	8000.139044	13.039629	-0.051103	4.815670
248.541507	8000.141531	13.044634	-0.051107	4.815671
248.618785	8000.144913	13.049639	-0.051121	4.815672
248.480511	8000.138394	13.054643	-0.051095	4.815670
248.342728	8000.178856	13.059648	-0.051070	4.815683
248.431858	8000.164282	13.064653	-0.051086	4.815678
248.358497	8000.137464	13.069658	-0.051072	4.815671
248.344674	8000.173531	13.074663	-0.051070	4.815681
248.483794	8000.060482	13.079667	-0.051096	4.815648
248.537679	8000.145688	13.084672	-0.051106	4.815672
248.484942	8000.117069	13.089677	-0.051096	4.815664
248.396065	8000.114554	13.094682	-0.051079	4.815664
248.593002	8000.166850	13.099687	-0.051116	4.815678
248.434269	8000.100215	13.104691	-0.051086	4.815660
248.491997	8000.150253	13.109696	-0.051097	4.815674
248.688560	8000.159840	13.114701	-0.051133	4.815676
248.612759	8000.186361	13.119706	-0.051119	4.815684
248.580276	8000.157003	13.124711	-0.051113	4.815675
248.655226	8000.144334	13.129715	-0.051127	4.815671
248.553146	8000.141604	13.134720	-0.051108	4.815671
248.452846	8000.131430	13.139725	-0.051089	4.815669
248.509623	8000.138750	13.144730	-0.051099	4.815670
248.599611	8000.163690	13.149735	-0.051116	4.815677
248.451154	8000.102559	13.154739	-0.051088	4.815660
248.583883	8000.131395	13.159744	-0.051113	4.815668
248.396371	8000.098455	13.164749	-0.051078	4.815659
248.556378	8000.065813	13.169754	-0.051108	4.815649
248.558846	8000.133104	13.174759	-0.051108	4.815669
248.525734	8000.126155	13.179763	-0.051102	4.815667
248.660260	8000.143277	13.184768	-0.051127	4.815671
248.661792	8000.133687	13.189773	-0.051127	4.815668
248.467187	8000.105970	13.194778	-0.051091	4.815661
248.426954	8000.142677	13.199783	-0.051083	4.815672
248.542457	8000.108246	13.204787	-0.051105	4.815661
248.508185	8000.155724	13.209792	-0.051098	4.815675
248.536947	8000.150846	13.214797	-0.051104	4.815674
248.489127	8000.131916	13.219802	-0.051095	4.815669
248.554740	8000.144717	13.224807	-0.051107	4.815672
248.635300	8000.146017	13.229811	-0.051122	4.815672
248.707477	8000.154654	13.234816	-0.051135	4.815674
248.638180	8000.141780	13.239821	-0.051122	4.815671
248.715166	8000.153698	13.244826	-0.051136	4.815674
248.793881	8000.158171	13.249831	-0.051151	4.815675
248.458514	8000.092941	13.254835	-0.051088	4.815657
248.590944	8000.147394	13.259840	-0.051113	4.815673
248.544393	8000.110335	13.264845	-0.051104	4.815662
248.588094	8000.088618	13.269850	-0.051112	4.815656
248.484659	8000.076258	13.274855	-0.051093	4.815652
248.504389	8000.031734	13.279859	-0.051096	4.815639
248.583700	8000.075716	13.284864	-0.051111	4.815652
248.522554	8000.121692	13.289869	-0.051100	4.815665
248.356366	8000.111517	13.294874	-0.051069	4.815663
248.399180	8000.141030	13.299879	-0.051077	4.815672
248.393814	8000.111044	13.304883	-0.051076	4.815663
248.371474	8000.185406	13.309888	-0.051071	4.815685
248.620154	8000.140323	13.314893	-0.051118	4.815670
248.573214	8000.139556	13.319898	-0.051109	4.815670
248.691246	8000.123315	13.324903	-0.051131	4.815665
248.546701	8000.112423	13.329907	-0.051104	4.815663
248.852026	8000.133382	13.334912	-0.051160	4.815667
248.567604	8000.086060	13.339917	-0.051107	4.815655
248.611107	8000.113449	13.344922	-0.051115	4.815663
248.664767	8000.120718	13.349927	-0.051125	4.815665
248.535456	8000.113276	13.354931	-0.051101	4.815663
248.578589	8000.134253	13.359936	-0.051109	4.815669
248.659778	8000.157983	13.364941	-0.051124	4.815675
248.529501	8000.089674	13.369946	-0.051100	4.815656
248.659865	8000.120606	13.374951	-0.051124	4.815665
248.516427	8000.092652	13.379955	-0.051097	4.815657
248.567790	8000.142587	13.384960	-0.051107	4.815671
248.554621	8000.111407	13.389965	-0.051104	4.815662
248.414188	8000.085637	13.394970	-0.051078	4.815656
248.377196	8000.124530	13.399975	-0.051071	4.815667
248.360056	8000.105030	13.404979	-0.051068	4.815661
248.424805	8000.147709	13.409984	-0.051080	4.815674
248.456953	8000.118331	13.414989	-0.051086	4.815665
248.564762	8000.119006	13.419994	-0.051106	4.815665
248.658671	8000.116252	13.424999	-0.051123	4.815663
248.479968	8000.073847	13.430003	-0.051090	4.815652
248.595336	8000.092793	13.435008	-0.051111	4.815657
248.555754	8000.115631	13.440013	-0.051104	4.815664
248.415044	8000.086654	13.445018	-0.051077	4.815656
248.698114	8000.141414	13.450023	-0.051130	4.815670
248.621433	8000.097460	13.455027	-0.051116	4.815658
248.642137	8000.163980	13.460032	-0.051119	4.815677
248.582633	8000.092548	13.465037	-0.051108	4.815657
248.589666	8000.075574	13.470042	-0.051110	4.815652
248.557835	8000.122025	13.475047	-0.051104	4.815665
248.433105	8000.070888	13.480051	-0.051080	4.815651
248.789230	8000.128968	13.485056	-0.051146	4.815666
248.693122	8000.126335	13.490061	-0.051129	4.815666
248.485330	8000.116553	13.495066	-0.051090	4.815664
248.740705	8000.156986	13.500071	-0.051137	4.815675
248.772251	8000.135072	13.505075	-0.051143	4.815668
248.415784	8000.132487	13.510080	-0.051077	4.815669
248.509431	8000.137202	13.515085	-0.051094	4.815670
248.640858	8000.133989	13.520090	-0.051118	4.815669
248.591254	8000.153462	13.525095	-0.051109	4.815675
248.484016	8000.119690	13.530099	-0.051089	4.815665
248.697297	8000.135953	13.535104	-0.051129	4.815669
248.592267	8000.152392	13.540109	-0.051109	4.815674
248.406533	8000.172860	13.545114	-0.051074	4.815681
248.745574	8000.171947	13.550119	-0.051137	4.815679
248.714292	8000.143676	13.555123	-0.051132	4.815671
248.448511	8000.159643	13.560128	-0.051082	4.815677
248.477751	8000.160111	13.565133	-0.051087	4.815677
248.740540	8000.155825	13.570138	-0.051136	4.815675
248.688982	8000.142172	13.575143	-0.051126	4.815671
248.537771	8000.149321	13.580147	-0.051098	4.815674
248.570724	8000.151984	13.585152	-0.051104	4.815674
248.615406	8000.149500	13.590157	-0.051113	4.815673
248.538066	8000.099131	13.595162	-0.051098	4.815659
248.454163	8000.112710	13.600167	-0.051082	4.815663
248.535456	8000.121495	13.605171	-0.051097	4.815665
248.477678	8000.118416	13.610176	-0.051087	4.815665
248.460891	8000.110664	13.615181	-0.051083	4.815663
248.679085	8000.107791	13.620186	-0.051124	4.815661
248.565882	8000.139043	13.625191	-0.051103	4.815670
248.552542	8000.134550	13.630195	-0.051100	4.815669
248.656514	8000.123419	13.635200	-0.051120	4.815665
248.731929	8000.135311	13.640205	-0.051134	4.815669
248.768111	8000.098526	13.645210	-0.051140	4.815658
248.790657	8000.140521	13.650215	-0.051144	4.815670
248.785253	8000.106265	13.655219	-0.051143	4.815660
248.831290	8000.150776	13.660224	-0.051152	4.815673
248.650540	8000.146770	13.665229	-0.051118	4.815672
248.544362	8000.169596	13.670234	-0.051098	4.815680
248.759862	8000.188031	13.675239	-0.051138	4.815684
248.715040	8000.143527	13.680243	-0.051130	4.815671
248.629292	8000.182698	13.685248	-0.051114	4.815683
248.587273	8000.145712	13.690253	-0.051106	4.815672
248.521542	8000.131829	13.695258	-0.051094	4.815669
248.630908	8000.174164	13.700263	-0.051114	4.815680
248.541832	8000.116131	13.705267	-0.051097	4.815664
248.575193	8000.151896	13.710272	-0.051103	4.815674
248.734160	8000.124575	13.715277	-0.051133	4.815665
248.884950	8000.150501	13.720282	-0.051161	4.815672
248.699504	8000.170974	13.725287	-0.051126	4.815679
248.578019	8000.158321	13.730291	-0.051104	4.815676
248.605194	8000.180107	13.735296	-0.051109	4.815682
248.682052	8000.190955	13.740301	-0.051123	4.815685
248.672170	8000.149153	13.745306	-0.051121	4.815673
248.722671	8000.183061	13.750311	-0.051130	4.815683
248.851160	8000.143502	13.755315	-0.051154	4.815670
248.664497	8000.159685	13.760320	-0.051119	4.815676
248.572439	8000.167794	13.765325	-0.051102	4.815679
248.744867	8000.164178	13.770330	-0.051134	4.815677
248.777487	8000.194593	13.775335	-0.051140	4.815686
248.614623	8000.170594	13.780339	-0.051110	4.815680
248.519144	8000.190390	13.785344	-0.051092	4.815686
248.731582	8000.200235	13.790349	-0.051131	4.815688
248.851153	8000.171208	13.795354	-0.051153	4.815679
248.810856	8000.196170	13.800359	-0.051146	4.815686
248.455807	8000.155175	13.805363	-0.051080	4.815676
248.541150	8000.137336	13.810368	-0.051095	4.815670
248.576813	8000.159260	13.815373	-0.051102	4.815676
248.634439	8000.170863	13.820378	-0.051113	4.815680
248.810775	8000.196136	13.825383	-0.051146	4.815686
248.660810	8000.161670	13.830387	-0.051117	4.815677
248.630158	8000.185721	13.835392	-0.051112	4.815684
248.612861	8000.151271	13.840397	-0.051108	4.815674
248.580894	8000.116584	13.845402	-0.051102	4.815664
248.581547	8000.156088	13.850407	-0.051102	4.815675
248.342913	8000.140469	13.855411	-0.051058	4.815672
248.705407	8000.152746	13.860416	-0.051125	4.815674
248.718252	8000.129461	13.865421	-0.051128	4.815667
248.720791	8000.146577	13.870426	-0.051128	4.815672
248.990088	8000.198980	13.875431	-0.051178	4.815686
248.674495	8000.105246	13.880435	-0.051119	4.815660
248.655044	8000.155100	13.885440	-0.051116	4.815675
248.573052	8000.131345	13.890445	-0.051100	4.815668
248.687574	8000.100101	13.895450	-0.051121	4.815659
248.599244	8000.173392	13.900455	-0.051105	4.815680
248.649722	8000.153920	13.905459	-0.051114	4.815675
248.702888	8000.152641	13.910464	-0.051124	4.815674
248.693207	8000.142869	13.915469	-0.051122	4.815671
248.763708	8000.106641	13.920474	-0.051135	4.815660
248.954392	8000.179120	13.925479	-0.051171	4.815680
248.748250	8000.146945	13.930483	-0.051132	4.815672
248.518939	8000.177383	13.935488	-0.051090	4.815682
248.558726	8000.181224	13.940493	-0.051097	4.815683
248.716952	8000.178446	13.945498	-0.051126	4.815681
248.572773	8000.152614	13.950503	-0.051099	4.815675
248.365733	8000.122561	13.955507	-0.051061	4.815667
248.472071	8000.161644	13.960512	-0.051080	4.815678
248.676804	8000.142539	13.965517	-0.051118	4.815671
248.585621	8000.102621	13.970522	-0.051101	4.815660
248.925698	8000.157238	13.975527	-0.051165	4.815674
248.901202	8000.144024	13.980531	-0.051160	4.815670
248.774997	8000.147308	13.985536	-0.051136	4.815672
248.796031	8000.164724	13.990541	-0.051140	4.815677
248.873608	8000.142489	13.995546	-0.051155	4.815670
248.941130	8000.141443	14.000551	-0.051167	4.815670
248.896514	8000.112955	14.005555	-0.051159	4.815661
248.885535	8000.174691	14.010560	-0.051157	4.815680
248.656781	8000.150690	14.015565	-0.051114	4.815674
248.519451	8000.136713	14.020570	-0.051088	4.815670
248.619086	8000.159674	14.025575	-0.051107	4.815676
248.705357	8000.131175	14.030579	-0.051123	4.815668
248.514069	8000.159026	14.035584	-0.051087	4.815677
248.609984	8000.159507	14.040589	-0.051105	4.815676
248.760329	8000.140587	14.045594	-0.051133	4.815670
248.767388	8000.175926	14.050599	-0.051134	4.815680
248.508089	8000.129011	14.055603	-0.051086	4.815668
248.591811	8000.177336	14.060608	-0.051101	4.815682
248.750782	8000.171367	14.065613	-0.051131	4.815679
248.669839	8000.162574	14.070618	-0.051116	4.815677
248.603614	8000.184981	14.075623	-0.051103	4.815684
248.550297	8000.149947	14.080627	-0.051093	4.815674
248.887628	8000.173560	14.085632	-0.051156	4.815679
248.793702	8000.146409	14.090637	-0.051138	4.815672
248.869168	8000.128410	14.095642	-0.051152	4.815666
248.782884	8000.163302	14.100647	-0.051136	4.815677
248.514360	8000.117305	14.105651	-0.051086	4.815665
248.693248	8000.116996	14.110656	-0.051119	4.815664
248.915058	8000.151547	14.115661	-0.051161	4.815673
248.783854	8000.116318	14.120666	-0.051136	4.815663
248.665569	8000.147488	14.125671	-0.051114	4.815673
248.806468	8000.140158	14.130675	-0.051140	4.815670
248.767282	8000.169409	14.135680	-0.051133	4.815679
248.598033	8000.150644	14.140685	-0.051101	4.815674
248.816725	8000.155252	14.145690	-0.051142	4.815674
248.964884	8000.169392	14.150695	-0.051169	4.815678
248.665732	8000.138911	14.155699	-0.051114	4.815670
248.785715	8000.194230	14.160704	-0.051136	4.815686
248.901746	8000.151267	14.165709	-0.051157	4.815673
248.799534	8000.148535	14.170714	-0.051138	4.815672
248.891014	8000.158553	14.175719	-0.051155	4.815675
248.835471	8000.123483	14.180723	-0.051145	4.815665
249.127069	8000.189059	14.185728	-0.051199	4.815683
248.884981	8000.157368	14.190733	-0.051154	4.815675
248.868845	8000.165641	14.195738	-0.051151	4.815677
248.984456	8000.182456	14.200743	-0.051172	4.815681
248.866134	8000.142097	14.205747	-0.051150	4.815670
248.733291	8000.170896	14.210752	-0.051125	4.815679
248.844108	8000.180160	14.215757	-0.051146	4.815681
248.665851	8000.122816	14.220762	-0.051113	4.815665
248.776997	8000.135288	14.225767	-0.051133	4.815669
248.818520	8000.122076	14.230771	-0.051141	4.815665
248.999512	8000.171979	14.235776	-0.051175	4.815678
248.722878	8000.160013	14.240781	-0.051123	4.815676
248.793315	8000.141932	14.245786	-0.051136	4.815670
248.879099	8000.162533	14.250791	-0.051152	4.815676
248.767737	8000.116950	14.255795	-0.051131	4.815663
248.845830	7999.176629	14.260800	-0.051145	4.815388

248.802212	7996.003552	14.265805	-0.051135	4.814460
248.883309	7990.566710	14.270810	-0.051146	4.812869
249.003943	7983.908918	14.275815	-0.051164	4.810920
248.864617	7976.620735	14.280819	-0.051133	4.808787
248.745652	7969.023946	14.285824	-0.051106	4.806562
248.633858	7961.212499	14.290829	-0.051080	4.804273
248.553086	7953.385067	14.295834	-0.051060	4.801979
248.823894	7945.400664	14.300839	-0.051105	4.799635
248.576544	7937.470942	14.305843	-0.051054	4.797309
248.503385	7929.437146	14.310848	-0.051035	4.794950
248.536044	7921.432228	14.315853	-0.051036	4.792599
248.382052	7913.334091	14.320858	-0.051002	4.790219
248.391161	7905.433366	14.325863	-0.050998	4.787896
248.196708	7897.368190	14.330867	-0.050957	4.785523
248.388557	7889.427904	14.335872	-0.050987	4.783185
248.401222	7881.424394	14.340877	-0.050984	4.780828
248.365429	7873.380768	14.345882	-0.050972	4.778458
248.348916	7865.465281	14.350887	-0.050964	4.776125
248.189877	7857.379362	14.355891	-0.050929	4.773741
248.209179	7849.418260	14.360896	-0.050927	4.771391
248.347314	7841.405462	14.365901	-0.050948	4.769025
248.289352	7833.385754	14.370906	-0.050932	4.766657
248.301053	7825.365618	14.375911	-0.050929	4.764286
248.278839	7817.462029	14.380915	-0.050919	4.761950
248.286892	7809.421305	14.385920	-0.050915	4.759571
248.184206	7801.447671	14.390925	-0.050891	4.757211
248.214448	7793.377290	14.395930	-0.050891	4.754821
248.234942	7785.315070	14.400935	-0.050890	4.752433
248.130512	7777.300830	14.405939	-0.050865	4.750058
247.910451	7769.351513	14.410944	-0.050819	4.747701
247.964241	7761.319681	14.415949	-0.050823	4.745317
248.127381	7753.370797	14.420954	-0.050849	4.742957
247.913531	7745.361075	14.425959	-0.050803	4.740579
247.759220	7737.346597	14.430963	-0.050769	4.738198
247.932291	7729.329932	14.435968	-0.050796	4.735814
247.771512	7721.344513	14.440973	-0.050761	4.733439
247.733221	7713.296140	14.445978	-0.050749	4.731044
247.777961	7705.297693	14.450983	-0.050752	4.728662
247.672818	7697.299841	14.455987	-0.050727	4.726279
247.675188	7689.370881	14.460992	-0.050722	4.723916
247.660168	7681.350506	14.465997	-0.050714	4.721524
247.407386	7673.280976	14.471002	-0.050662	4.719117
247.433525	7665.424953	14.476007	-0.050661	4.716772
247.245222	7657.294203	14.481011	-0.050621	4.714344
247.449711	7649.290874	14.486016	-0.050654	4.711952
247.493080	7641.287194	14.491021	-0.050656	4.709559
247.382362	7633.303138	14.496026	-0.050631	4.707171
247.348539	7625.295576	14.501031	-0.050619	4.704774
247.294503	7617.374322	14.506035	-0.050604	4.702403
247.296794	7609.310576	14.511040	-0.050599	4.699987
247.270930	7601.357011	14.516045	-0.050589	4.697603
247.119228	7593.300542	14.521050	-0.050555	4.695187
247.280084	7585.278304	14.526055	-0.050580	4.692780
247.170001	7577.269945	14.531059	-0.050554	4.690376
247.256740	7569.292861	14.536064	-0.050565	4.687980
246.911445	7561.277945	14.541069	-0.050495	4.685572
246.938220	7553.277606	14.546074	-0.050495	4.683166
247.040727	7545.331573	14.551079	-0.050509	4.680776
246.811939	7537.300797	14.556083	-0.050461	4.678359
246.670783	7529.315112	14.561088	-0.050429	4.675954
246.825583	7521.248986	14.566093	-0.050453	4.673524
246.791008	7513.194448	14.571098	-0.050441	4.671096
246.853280	7505.186960	14.576103	-0.050447	4.668681
246.741654	7497.207720	14.581107	-0.050421	4.666273
246.850909	7489.227299	14.586112	-0.050436	4.663863
246.838725	7481.264990	14.591117	-0.050429	4.661458
246.445075	7473.210471	14.596122	-0.050350	4.659024
246.553381	7465.299243	14.601127	-0.050365	4.656632
246.387727	7457.262249	14.606131	-0.050329	4.654201
246.395804	7449.214563	14.611136	-0.050325	4.651764
246.235257	7441.177858	14.616141	-0.050290	4.649330
246.176778	7433.231178	14.621146	-0.050274	4.646922
246.349395	7425.254179	14.626151	-0.050301	4.644504
246.033699	7417.248349	14.631155	-0.050237	4.642076
246.186313	7409.200431	14.636160	-0.050260	4.639633
246.233288	7401.281916	14.641165	-0.050263	4.637228
246.052972	7393.204836	14.646170	-0.050224	4.634774
246.137111	7385.184830	14.651175	-0.050235	4.632336
246.287509	7377.163966	14.656179	-0.050257	4.629897
246.083344	7369.201306	14.661184	-0.050214	4.627474
246.043395	7361.222525	14.666189	-0.050201	4.625045
245.951950	7353.240759	14.671194	-0.050179	4.622613
245.921354	7345.246873	14.676199	-0.050168	4.620177
245.797362	7337.170210	14.681203	-0.050140	4.617714
245.922200	7329.176676	14.686208	-0.050158	4.615275
245.864551	7321.187367	14.691213	-0.050142	4.612836
245.692452	7313.127763	14.696218	-0.050104	4.610374
245.938605	7305.204040	14.701223	-0.050145	4.607953
245.706578	7297.147989	14.706227	-0.050096	4.605490
245.704037	7289.184880	14.711232	-0.050091	4.603054
245.595410	7281.172078	14.716237	-0.050065	4.600601
245.703298	7273.163302	14.721242	-0.050080	4.598148
245.804800	7265.190353	14.726247	-0.050093	4.595705
245.696507	7257.156826	14.731251	-0.050068	4.593242
245.599451	7249.094058	14.736256	-0.050045	4.590769
245.742232	7241.123643	14.741261	-0.050066	4.588323
245.487028	7233.080099	14.746266	-0.050013	4.585853
245.417064	7225.151257	14.751271	-0.049995	4.583417
245.290569	7217.138486	14.756275	-0.049966	4.580954
245.491663	7209.154494	14.761280	-0.049998	4.578498
245.519153	7201.174243	14.766285	-0.049998	4.576042
245.359353	7193.103607	14.771290	-0.049963	4.573557
245.400502	7185.120815	14.776295	-0.049965	4.571098
245.097962	7177.090927	14.781299	-0.049904	4.568623
245.190627	7169.127738	14.786304	-0.049916	4.566167
245.105126	7161.176614	14.791309	-0.049894	4.563713
245.114498	7153.148526	14.796314	-0.049891	4.561235
245.108087	7145.168324	14.801319	-0.049884	4.558770
245.084888	7137.164252	14.806323	-0.049875	4.556296
245.086490	7129.117997	14.811328	-0.049870	4.553808
245.103450	7121.107341	14.816333	-0.049868	4.551329
245.053025	7113.075191	14.821338	-0.049853	4.548842
245.159198	7105.137297	14.826343	-0.049867	4.546384
245.007470	7097.088295	14.831347	-0.049834	4.543889
244.860166	7089.167559	14.836352	-0.049801	4.541433
244.808549	7081.154023	14.841357	-0.049786	4.538946
244.698808	7073.145268	14.846362	-0.049761	4.536460
244.848583	7065.115174	14.851367	-0.049783	4.533966
244.856290	7057.083357	14.856371	-0.049779	4.531470
244.759893	7049.101848	14.861376	-0.049756	4.528988
244.641167	7041.160029	14.866381	-0.049729	4.526517
244.650464	7033.093340	14.871386	-0.049725	4.524006
244.784903	7025.163493	14.876391	-0.049745	4.521536
244.745803	7017.099029	14.881395	-0.049732	4.519023
244.638725	7009.152716	14.886400	-0.049707	4.516545
244.636418	7001.107934	14.891405	-0.049701	4.514035
244.344101	6992.994010	14.896410	-0.049642	4.511502
244.474649	6985.038131	14.901415	-0.049661	4.509017
244.303986	6977.047217	14.906419	-0.049624	4.506520
244.537138	6969.073254	14.911424	-0.049662	4.504027
244.534915	6961.101733	14.916429	-0.049656	4.501533
244.177342	6953.069079	14.921434	-0.049584	4.499018
244.353890	6945.091898	14.926439	-0.049612	4.496520
244.131069	6937.055158	14.931443	-0.049565	4.494001
244.138337	6929.021785	14.936448	-0.049561	4.491482
244.227817	6921.047822	14.941453	-0.049572	4.488981
244.238494	6913.028362	14.946458	-0.049569	4.486463
244.129209	6905.046441	14.951463	-0.049543	4.483956
244.125220	6897.077865	14.956467	-0.049537	4.481452
244.085332	6889.066489	14.961472	-0.049525	4.478933
244.039748	6881.103358	14.966477	-0.049511	4.476427
243.933153	6873.041276	14.971482	-0.049486	4.473889
244.214040	6864.999280	14.976487	-0.049533	4.471357
244.119718	6856.993762	14.981491	-0.049510	4.468834
244.099090	6849.003831	14.986496	-0.049501	4.466315
244.045695	6841.041565	14.991501	-0.049486	4.463802
244.036546	6833.027912	14.996506	-0.049479	4.461273
243.930857	6825.051617	15.001511	-0.049454	4.458753
243.829582	6817.064024	15.006515	-0.049429	4.456228
244.030550	6809.025871	15.011520	-0.049462	4.453687
243.903113	6801.028005	15.016525	-0.049433	4.451156
243.598925	6792.974932	15.021530	-0.049371	4.448605
243.492425	6785.005780	15.026535	-0.049346	4.446081
243.549572	6776.987809	15.031539	-0.049351	4.443540
243.357378	6769.040783	15.036544	-0.049310	4.441019
243.578730	6761.062168	15.041549	-0.049346	4.438488
243.462567	6753.054396	15.046554	-0.049319	4.435945
243.420879	6745.010916	15.051559	-0.049306	4.433390
243.324280	6736.952265	15.056563	-0.049282	4.430828
243.447556	6728.948119	15.061568	-0.049300	4.428283
243.314246	6720.936621	15.066573	-0.049270	4.425733
243.267188	6712.930475	15.071578	-0.049256	4.423183
243.300185	6704.978704	15.076583	-0.049257	4.420650
243.232512	6697.016383	15.081587	-0.049239	4.418112
243.217474	6689.001102	15.086592	-0.049231	4.415555
243.299735	6680.993839	15.091597	-0.049241	4.413000
242.961631	6672.907952	15.096602	-0.049173	4.410416
242.993067	6664.975337	15.101607	-0.049173	4.407882
242.947508	6656.945050	15.106611	-0.049159	4.405314
243.003540	6649.006585	15.111616	-0.049165	4.402775
243.021885	6641.034309	15.116621	-0.049163	4.400223
242.805667	6632.997523	15.121626	-0.049117	4.397648
243.014270	6625.023548	15.126631	-0.049151	4.395094
242.930113	6616.965736	15.131635	-0.049130	4.392510
242.909208	6608.957328	15.136640	-0.049121	4.389941
242.974428	6600.990997	15.141645	-0.049127	4.387384
242.717772	6592.928146	15.146650	-0.049074	4.384793
242.763202	6585.009422	15.151655	-0.049078	4.382248
242.644090	6576.998319	15.156659	-0.049050	4.379671
242.691181	6569.009296	15.161664	-0.049054	4.377101
242.708552	6560.993517	15.166669	-0.049051	4.374520
242.520609	6552.932076	15.171674	-0.049011	4.371922
242.659185	6544.950641	15.176679	-0.049032	4.369350
242.591148	6537.017498	15.181683	-0.049014	4.366791
242.361992	6528.964504	15.186688	-0.048966	4.364190
242.515474	6521.035536	15.191693	-0.048989	4.361631
242.666043	6512.980821	15.196698	-0.049012	4.359029
242.475265	6505.040972	15.201703	-0.048971	4.356461
242.334924	6496.957257	15.206707	-0.048940	4.353845
242.398391	6488.862747	15.211712	-0.048946	4.351226
242.405724	6480.900486	15.216717	-0.048942	4.348647
242.442726	6472.874922	15.221722	-0.048944	4.346046
242.290205	6464.955335	15.226727	-0.048910	4.343477
242.280406	6456.970152	15.231731	-0.048903	4.340886
241.977808	6448.971956	15.236736	-0.048841	4.338288
241.930827	6440.951087	15.241741	-0.048827	4.335682
241.934706	6432.950285	15.246746	-0.048823	4.333081
241.952195	6424.923289	15.251751	-0.048821	4.330470
241.973277	6416.925030	15.256755	-0.048819	4.327868
242.160164	6408.935555	15.261760	-0.048849	4.325267
242.013861	6400.998538	15.266765	-0.048816	4.322680
241.716310	6392.928090	15.271770	-0.048756	4.320047
241.934401	6384.982925	15.276775	-0.048791	4.317456
241.787813	6376.895008	15.281779	-0.048758	4.314815
241.635962	6368.896322	15.286784	-0.048725	4.312201
241.425295	6360.920167	15.291789	-0.048680	4.309593
241.588505	6352.899057	15.296794	-0.048705	4.306971
241.685676	6344.928222	15.301799	-0.048718	4.304364
241.295485	6336.948160	15.306803	-0.048640	4.301748
241.312451	6328.906097	15.311808	-0.048638	4.299113
241.305834	6320.992354	15.316813	-0.048632	4.296519
241.266874	6312.872973	15.321818	-0.048619	4.293855
241.346119	6304.904058	15.326823	-0.048629	4.291240
241.317408	6296.865702	15.331827	-0.048618	4.288600
241.256020	6288.881574	15.336832	-0.048601	4.285975
241.269288	6280.967861	15.341837	-0.048598	4.283373
241.149531	6272.931463	15.346842	-0.048571	4.280728
241.248420	6264.963656	15.351847	-0.048584	4.278105
241.205699	6256.893536	15.356851	-0.048571	4.275446
241.071394	6248.866836	15.361856	-0.048540	4.272799
241.286481	6240.829341	15.366861	-0.048575	4.270150
241.030490	6232.846140	15.371866	-0.048522	4.267513
241.045045	6224.893825	15.376871	-0.048520	4.264886
241.025376	6216.899167	15.381875	-0.048511	4.262244
241.054270	6208.899670	15.386880	-0.048511	4.259599
241.070425	6200.931898	15.391885	-0.048508	4.256963
240.853865	6192.925503	15.396890	-0.048463	4.254310
241.152606	6184.887311	15.401895	-0.048513	4.251650
240.902253	6176.894777	15.406899	-0.048461	4.248998
240.860832	6168.909940	15.411904	-0.048448	4.246349
240.865535	6160.965478	15.416909	-0.048444	4.243712
240.753750	6152.904294	15.421914	-0.048418	4.241034
240.737831	6144.961019	15.426919	-0.048410	4.238394
240.512547	6136.924574	15.431923	-0.048362	4.235719
240.502862	6128.921743	15.436928	-0.048355	4.233056
240.673220	6120.894321	15.441933	-0.048382	4.230385
240.515428	6112.893750	15.446938	-0.048347	4.227718
240.548896	6104.912290	15.451943	-0.048348	4.225057
240.280870	6096.946717	15.456947	-0.048293	4.222398
240.330616	6088.902875	15.461952	-0.048297	4.219713
240.498599	6080.962415	15.466957	-0.048323	4.217062
240.274023	6072.903426	15.471962	-0.048276	4.214366
240.490656	6064.910844	15.476967	-0.048311	4.211696
240.426909	6056.919764	15.481971	-0.048293	4.209021
240.368466	6048.895421	15.486976	-0.048277	4.206333
240.317417	6040.921647	15.491981	-0.048263	4.203661
240.217606	6032.942402	15.496986	-0.048239	4.200984
240.319061	6024.930308	15.501991	-0.048252	4.198297
240.184559	6016.944751	15.506995	-0.048222	4.195614
240.063425	6008.822726	15.512000	-0.048194	4.192885
240.156762	6000.809631	15.517005	-0.048206	4.190192
240.139059	5992.807106	15.522010	-0.048198	4.187500
240.141538	5984.854518	15.527015	-0.048193	4.184823
240.108165	5976.905419	15.532019	-0.048181	4.182145
240.054397	5968.870428	15.537024	-0.048166	4.179437
240.135933	5960.927810	15.542029	-0.048176	4.176759
239.943250	5952.888417	15.547034	-0.048135	4.174044
240.049913	5944.855402	15.552039	-0.048149	4.171332
240.058656	5936.887215	15.557043	-0.048146	4.168640
239.899760	5928.872635	15.562048	-0.048111	4.165928
239.888672	5920.866610	15.567053	-0.048103	4.163219
239.780732	5912.882033	15.572058	-0.048078	4.160514
239.797351	5904.946310	15.577063	-0.048076	4.157826
239.742867	5896.891140	15.582067	-0.048060	4.155095
239.773331	5888.862255	15.587072	-0.048061	4.152371
239.674037	5880.862489	15.592077	-0.048037	4.149655
239.795514	5872.833583	15.597082	-0.048054	4.146929
239.739557	5864.847422	15.602087	-0.048039	4.144214
239.482499	5856.937006	15.607091	-0.047985	4.141520
239.463468	5848.857346	15.612096	-0.047977	4.138770
239.418768	5840.881132	15.617101	-0.047963	4.136053
239.355900	5832.855897	15.622106	-0.047946	4.133317
239.430842	5824.836482	15.627111	-0.047955	4.130583
239.277694	5816.856310	15.632115	-0.047921	4.127858
239.316341	5808.839691	15.637120	-0.047923	4.125121
239.254545	5800.905168	15.642125	-0.047906	4.122409
239.145771	5792.844387	15.647130	-0.047880	4.119651
239.310321	5784.919305	15.652135	-0.047906	4.116941
239.215232	5776.886081	15.657139	-0.047883	4.114190
239.131465	5768.858762	15.662144	-0.047862	4.111438
239.282070	5760.846167	15.667149	-0.047885	4.108693
239.169585	5752.835266	15.672154	-0.047858	4.105943
239.025788	5744.878258	15.677159	-0.047826	4.103209
238.981758	5736.890069	15.682163	-0.047813	4.100465
238.994545	5728.874188	15.687168	-0.047810	4.097709
238.860438	5720.925668	15.692173	-0.047780	4.094973
238.682581	5712.871812	15.697178	-0.047741	4.092198
238.811905	5704.854006	15.702183	-0.047760	4.089438
238.658580	5696.887140	15.707187	-0.047726	4.086690
238.603026	5688.905536	15.712192	-0.047711	4.083936
238.672563	5680.940631	15.717197	-0.047718	4.081187
238.725790	5672.950099	15.722202	-0.047723	4.078428
238.787306	5664.956500	15.727207	-0.047729	4.075666
238.647560	5656.912381	15.732211	-0.047698	4.072882
238.519728	5648.885067	15.737216	-0.047669	4.070102
238.699523	5640.885870	15.742221	-0.047697	4.067334
238.462854	5632.868628	15.747226	-0.047647	4.064552
238.486208	5624.939842	15.752231	-0.047647	4.061802
238.548650	5616.943760	15.757235	-0.047653	4.059028
238.436356	5608.908282	15.762240	-0.047627	4.056236
238.561801	5600.890896	15.767245	-0.047645	4.053451
238.526925	5592.862380	15.772250	-0.047633	4.050659
238.437454	5584.915264	15.777255	-0.047611	4.047892
238.178440	5576.897473	15.782259	-0.047558	4.045096
238.114214	5568.945998	15.787264	-0.047540	4.042324
238.255248	5560.913370	15.792269	-0.047561	4.039524
237.906011	5552.946684	15.797274	-0.047491	4.036739
238.182712	5544.888019	15.802279	-0.047537	4.033929
238.203046	5536.796865	15.807283	-0.047536	4.031101
237.991102	5528.856263	15.812288	-0.047491	4.028321
237.895981	5520.861725	15.817293	-0.047468	4.025522
238.034871	5512.880332	15.822298	-0.047488	4.022729
238.138281	5504.878390	15.827303	-0.047502	4.019927
237.842009	5496.944214	15.832307	-0.047442	4.017140
237.993005	5488.872140	15.837312	-0.047465	4.014309
238.013640	5480.896848	15.842317	-0.047463	4.011509
237.842860	5472.834483	15.847322	-0.047426	4.008673
237.977296	5464.845777	15.852327	-0.047446	4.005865
237.857570	5456.890101	15.857331	-0.047418	4.003064
237.842440	5448.893641	15.862336	-0.047410	4.000247
237.478138	5440.964832	15.867341	-0.047337	3.997447
237.502145	5432.886753	15.872346	-0.047336	3.994599
237.438359	5424.891877	15.877351	-0.047319	3.991776
237.308457	5416.872170	15.882355	-0.047290	3.988942
237.421396	5408.842524	15.887360	-0.047306	3.986106
237.454874	5400.910502	15.892365	-0.047306	3.983301
237.184234	5392.905723	15.897370	-0.047251	3.980463
237.241938	5384.960936	15.902375	-0.047256	3.977650
237.399751	5376.932490	15.907379	-0.047280	3.974807
237.340816	5368.913852	15.912384	-0.047264	3.971962
237.312953	5360.910062	15.917389	-0.047254	3.969121
237.319070	5352.920942	15.922394	-0.047249	3.966283
237.343827	5344.905918	15.927399	-0.047249	3.963435
237.252084	5336.941751	15.932403	-0.047226	3.960600
237.053145	5328.968356	15.937408	-0.047184	3.957759
237.164368	5320.979571	15.942413	-0.047200	3.954915
236.920936	5312.888604	15.947418	-0.047149	3.952026
236.875713	5304.912056	15.952423	-0.047135	3.949180
236.921693	5296.941171	15.957427	-0.047138	3.946335
237.093414	5288.906042	15.962432	-0.047165	3.943468
236.954873	5280.974126	15.967437	-0.047134	3.940630
236.681092	5272.938704	15.972442	-0.047078	3.937750
236.718309	5264.971326	15.977447	-0.047079	3.934898
236.808978	5256.949547	15.982451	-0.047091	3.932025
236.595968	5248.939312	15.987456	-0.047046	3.929149
236.588909	5240.987254	15.992461	-0.047040	3.926296
236.725699	5232.932003	15.997466	-0.047060	3.923406
236.701388	5224.961186	16.002471	-0.047050	3.920541
236.527269	5216.984777	16.007475	-0.047012	3.917669
236.559561	5208.972489	16.012480	-0.047013	3.914787
236.570723	5200.956785	16.017485	-0.047010	3.911900
236.430457	5192.934046	16.022490	-0.046978	3.909006
236.428432	5184.950810	16.027495	-0.046973	3.906126
236.682155	5176.960149	16.032499	-0.047015	3.903247
236.269010	5168.973856	16.037504	-0.046932	3.900355
236.310201	5161.016453	16.042509	-0.046935	3.897479
236.236757	5152.966561	16.047514	-0.046916	3.894565
236.191106	5144.985055	16.052519	-0.046902	3.891675
236.374224	5136.942239	16.057523	-0.046931	3.888765
236.330388	5128.951026	16.062528	-0.046917	3.885867
236.271793	5121.000134	16.067533	-0.046901	3.882981
236.226183	5112.969399	16.072538	-0.046887	3.880064
236.161609	5105.005011	16.077543	-0.046870	3.877168
236.035970	5096.964943	16.082547	-0.046841	3.874242
235.839955	5088.702437	16.087552	-0.046799	3.871231
236.053973	5080.813159	16.092557	-0.046834	3.868362
236.250465	5072.833851	16.097562	-0.046865	3.865458
236.017483	5064.931053	16.102567	-0.046817	3.862570
235.912283	5056.957138	16.107571	-0.046792	3.859658
235.999241	5048.962459	16.112576	-0.046803	3.856739
236.008580	5040.966149	16.117581	-0.046799	3.853816
235.716011	5032.954299	16.122586	-0.046740	3.850879
235.656832	5024.960399	16.127591	-0.046723	3.847950
235.693563	5016.974915	16.132595	-0.046725	3.845025
235.784100	5008.990777	16.137600	-0.046736	3.842099
235.660826	5001.008576	16.142605	-0.046708	3.839167
235.787684	4992.998849	16.147610	-0.046726	3.836228
235.805674	4984.986104	16.152615	-0.046725	3.833284
235.664404	4977.010638	16.157619	-0.046693	3.830347
235.669669	4968.980426	16.162624	-0.046689	3.827391
235.806117	4961.000579	16.167629	-0.046709	3.824454
235.455511	4953.065818	16.172634	-0.046638	3.821521
235.440087	4945.048611	16.177639	-0.046630	3.818563
235.404724	4937.069212	16.182643	-0.046618	3.815616
235.473773	4929.034198	16.187648	-0.046626	3.812648
235.635900	4921.045561	16.192653	-0.046651	3.809697
235.600271	4913.045101	16.197658	-0.046639	3.806735
235.341987	4905.065633	16.202663	-0.046585	3.803774
235.469198	4897.090018	16.207667	-0.046604	3.800820
235.558018	4889.079918	16.212672	-0.046615	3.797851
235.535358	4881.064163	16.217677	-0.046605	3.794874
235.062389	4873.014282	16.222682	-0.046512	3.791873
235.031646	4865.025188	16.227687	-0.046501	3.788901
235.088593	4857.027072	16.232691	-0.046506	3.785926
234.908845	4849.056971	16.237696	-0.046468	3.782953
235.078920	4841.065461	16.242701	-0.046494	3.779979
234.916170	4833.081871	16.247706	-0.046458	3.776997
235.001958	4825.077065	16.252711	-0.046469	3.774010
235.001037	4817.047919	16.257715	-0.046464	3.771010
234.767968	4809.057687	16.262720	-0.046415	3.768017
234.939168	4801.051683	16.267725	-0.046442	3.765025
234.647857	4793.054527	16.272730	-0.046382	3.762023
234.679514	4785.073979	16.277735	-0.046383	3.759033
234.569836	4777.106838	16.282739	-0.046357	3.756041
234.671620	4769.060680	16.287744	-0.046371	3.753023
234.580173	4761.057050	16.292749	-0.046348	3.750014
234.488039	4753.047486	16.297754	-0.046326	3.747000
234.396140	4745.075910	16.302759	-0.046303	3.743998
234.299282	4737.106114	16.307763	-0.046280	3.740994
234.366326	4729.090233	16.312768	-0.046287	3.737974
234.496700	4721.101629	16.317773	-0.046306	3.734963
234.310967	4713.082389	16.322778	-0.046266	3.731931
234.377579	4705.092551	16.327783	-0.046274	3.728914
234.401753	4697.124239	16.332787	-0.046273	3.725901
234.233895	4689.117738	16.337792	-0.046236	3.722867
234.340287	4681.139821	16.342797	-0.046251	3.719847
234.290856	4673.152834	16.347802	-0.046236	3.716819
234.046127	4665.147960	16.352807	-0.046185	3.713775
234.026402	4657.057137	16.357811	-0.046176	3.710703
234.164612	4649.067902	16.362816	-0.046197	3.707670
234.211305	4641.095203	16.367821	-0.046200	3.704639
233.956105	4633.147889	16.372826	-0.046148	3.701607
234.129830	4625.139002	16.377831	-0.046175	3.698561
234.048423	4617.193491	16.382835	-0.046154	3.695529
233.906079	4609.143240	16.387840	-0.046122	3.692454
233.890425	4601.154323	16.392845	-0.046114	3.689402
233.721680	4593.206656	16.397850	-0.046078	3.686360
233.690450	4585.199396	16.402855	-0.046066	3.683296
233.883836	4577.201796	16.407859	-0.046097	3.680239
233.726664	4569.211366	16.412864	-0.046063	3.677173
233.806205	4561.210197	16.417869	-0.046072	3.674107
233.545770	4553.179159	16.422874	-0.046018	3.671018
233.519718	4545.196894	16.427879	-0.046008	3.667951
233.465768	4537.176130	16.432883	-0.045993	3.664866
233.563794	4529.200514	16.437888	-0.046006	3.661799
233.537505	4521.196231	16.442893	-0.045996	3.658716
233.525026	4513.205868	16.447898	-0.045988	3.655636
233.405869	4505.214979	16.452903	-0.045961	3.652550
233.427220	4497.184903	16.457907	-0.045959	3.649450
233.178077	4489.213342	16.462912	-0.045908	3.646363
233.381614	4481.242472	16.467917	-0.045940	3.643286
233.351714	4473.251652	16.472922	-0.045929	3.640192
233.265901	4465.262659	16.477927	-0.045908	3.637094
233.306959	4457.245946	16.482931	-0.045910	3.633987
233.342144	4449.193064	16.487936	-0.045912	3.630863
233.353190	4441.240382	16.492941	-0.045908	3.627774
233.250761	4433.215726	16.497946	-0.045884	3.624652
233.333941	4425.267610	16.502951	-0.045894	3.621562
233.247602	4417.294112	16.507955	-0.045873	3.618455
233.039851	4409.285641	16.512960	-0.045829	3.615328
233.079694	4401.286660	16.517965	-0.045831	3.612208
233.140046	4393.251556	16.522970	-0.045837	3.609073
233.027030	4385.287670	16.527975	-0.045811	3.605958
232.899836	4377.317372	16.532979	-0.045782	3.602837
232.731061	4369.303608	16.537984	-0.045745	3.599695
232.790776	4361.352998	16.542989	-0.045751	3.596582
232.480007	4353.331672	16.547994	-0.045688	3.593428
232.726761	4345.303526	16.552999	-0.045728	3.590284
232.671435	4337.339128	16.558003	-0.045713	3.587154
232.516876	4329.335733	16.563008	-0.045679	3.584003
232.739671	4321.356403	16.568013	-0.045715	3.580869
232.720942	4313.362761	16.573018	-0.045706	3.577720
232.625508	4305.353282	16.578023	-0.045683	3.574560
232.712690	4297.362060	16.583027	-0.045694	3.571410
232.556069	4289.341259	16.588032	-0.045660	3.568238
232.433640	4281.364622	16.593037	-0.045632	3.565082
232.363734	4273.396749	16.598042	-0.045613	3.561928
232.407646	4265.395221	16.603047	-0.045616	3.558761
232.355667	4257.395330	16.608051	-0.045601	3.555589
232.048861	4249.319321	16.613056	-0.045539	3.552376
232.165125	4241.312692	16.618061	-0.045555	3.549201
232.200481	4233.323167	16.623066	-0.045556	3.546027
232.275336	4225.380973	16.628071	-0.045565	3.542870
232.126806	4217.391310	16.633075	-0.045532	3.539685
232.203466	4209.382518	16.638080	-0.045541	3.536496
232.039348	4201.378012	16.643085	-0.045505	3.533299
231.882737	4193.369319	16.648090	-0.045471	3.530097
231.981957	4185.419586	16.653095	-0.045484	3.526924
231.829818	4177.428243	16.658099	-0.045450	3.523724
231.826142	4169.437564	16.663104	-0.045444	3.520525
231.870884	4161.476149	16.668109	-0.045448	3.517337
231.968282	4153.410498	16.673114	-0.045460	3.514106
231.607606	4145.441155	16.678119	-0.045388	3.510896
231.486882	4137.463850	16.683123	-0.045360	3.507688
231.598149	4129.417742	16.688128	-0.045376	3.504456
231.710866	4121.481244	16.693133	-0.045391	3.501265
231.560632	4113.499574	16.698138	-0.045358	3.498045
231.713303	4105.473071	16.703143	-0.045381	3.494814
231.528744	4097.515085	16.708147	-0.045342	3.491596
231.452531	4089.500414	16.713152	-0.045322	3.488356
231.715280	4081.505960	16.718157	-0.045366	3.485132
231.554848	4073.555972	16.723162	-0.045331	3.481909
231.436883	4065.553835	16.728167	-0.045303	3.478664
231.426410	4057.589199	16.733171	-0.045296	3.475434
231.344491	4049.543070	16.738176	-0.045276	3.472166
231.342447	4041.520484	16.743181	-0.045270	3.468907
231.198759	4033.532086	16.748186	-0.045238	3.465654
231.281651	4025.561520	16.753191	-0.045248	3.462413
231.320573	4017.571267	16.758195	-0.045250	3.459159
230.993212	4009.611811	16.763200	-0.045184	3.455903
231.214726	4001.572250	16.768205	-0.045220	3.452629
230.970171	3993.562548	16.773210	-0.045169	3.449349
231.060141	3985.590759	16.778215	-0.045180	3.446092
230.956813	3977.613172	16.783219	-0.045156	3.442823
230.883879	3969.597329	16.788224	-0.045137	3.439537
231.048853	3961.655791	16.793229	-0.045162	3.436285
230.668478	3953.611148	16.798234	-0.045086	3.432970
230.729053	3945.594565	16.803239	-0.045092	3.429679
230.667386	3937.623000	16.808243	-0.045075	3.426398
230.500251	3929.649584	16.813248	-0.045039	3.423110
230.701999	3921.665621	16.818253	-0.045071	3.419827
230.862411	3913.665416	16.823258	-0.045096	3.416532
230.562638	3905.661085	16.828263	-0.045035	3.413217
230.546412	3897.685687	16.833267	-0.045027	3.409921
230.486114	3889.674911	16.838272	-0.045010	3.406605
230.648546	3881.688814	16.843277	-0.045035	3.403304
230.299450	3873.741858	16.848282	-0.044965	3.399998
230.305656	3865.742195	16.853287	-0.044961	3.396679
230.490996	3857.708258	16.858291	-0.044990	3.393349
230.314684	3849.662270	16.863296	-0.044952	3.389999
230.397825	3841.695428	16.868301	-0.044962	3.386686
230.137683	3833.722668	16.873306	-0.044908	3.383356
230.076193	3825.745540	16.878311	-0.044891	3.380028
230.183364	3817.769452	16.883315	-0.044906	3.376703
230.075109	3809.770215	16.888320	-0.044881	3.373358
230.018934	3801.779003	16.893325	-0.044865	3.370014
230.001843	3793.781229	16.898330	-0.044856	3.366666
229.917139	3785.789772	16.903335	-0.044835	3.363314
230.030789	3777.811605	16.908339	-0.044851	3.359972
229.818129	3769.843408	16.913344	-0.044806	3.356619
229.859766	3761.818269	16.918349	-0.044809	3.353248
229.868250	3753.789218	16.923354	-0.044805	3.349871
229.899869	3745.827022	16.928359	-0.044806	3.346519
229.643364	3737.848224	16.933363	-0.044753	3.343146
229.621995	3729.837905	16.938368	-0.044743	3.339765
229.688976	3721.892275	16.943373	-0.044751	3.336412
229.559887	3713.872121	16.948378	-0.044721	3.333016
229.487149	3705.867801	16.953383	-0.044703	3.329626
229.445300	3697.922725	16.958387	-0.044689	3.326258
229.252398	3689.908519	16.963392	-0.044648	3.322852
229.414274	3681.894111	16.968397	-0.044673	3.319455
229.594022	3673.945728	16.973402	-0.044701	3.316084
229.490183	3665.912381	16.978407	-0.044677	3.312663
229.288452	3657.912933	16.983411	-0.044634	3.309249
229.274524	3649.924892	16.988416	-0.044626	3.305843
229.510048	3641.961600	16.993421	-0.044665	3.302453
229.172634	3633.977964	16.998426	-0.044596	3.299030
228.984747	3626.005440	17.003431	-0.044556	3.295614
229.251380	3617.993915	17.008435	-0.044601	3.292195
229.046270	3609.994434	17.013440	-0.044557	3.288759
229.104980	3602.016730	17.018445	-0.044563	3.285339
228.864871	3594.046693	17.023450	-0.044513	3.281907
228.924433	3586.049993	17.028455	-0.044519	3.278472
228.857823	3578.076000	17.033459	-0.044501	3.275038
228.744742	3570.040744	17.038464	-0.044475	3.271573
228.962787	3562.071446	17.043469	-0.044510	3.268145
228.728743	3554.052660	17.048474	-0.044461	3.264674
228.612358	3546.108293	17.053479	-0.044434	3.261236
228.823743	3538.088207	17.058483	-0.044468	3.257775
228.600464	3530.099915	17.063488	-0.044421	3.254307
228.518396	3522.118765	17.068493	-0.044401	3.250844
228.561783	3514.102950	17.073498	-0.044403	3.247367
228.505019	3506.145185	17.078503	-0.044388	3.243907
228.558163	3498.170689	17.083507	-0.044392	3.240441
228.434585	3490.193163	17.088512	-0.044364	3.236963
228.728466	3482.151065	17.093517	-0.044413	3.233470
228.669400	3474.080345	17.098522	-0.044397	3.229946
228.427260	3466.129153	17.103527	-0.044347	3.226463
228.510554	3458.163333	17.108531	-0.044357	3.222983
228.287637	3450.184200	17.113536	-0.044310	3.219481
228.383449	3442.242282	17.118541	-0.044323	3.216005
228.304849	3434.213670	17.123546	-0.044303	3.212480
228.368703	3426.218121	17.128551	-0.044309	3.208971
228.124246	3418.255487	17.133555	-0.044259	3.205460
227.920024	3410.286544	17.138560	-0.044215	3.201944
228.022439	3402.322117	17.143565	-0.044229	3.198439
227.863073	3394.329748	17.148570	-0.044194	3.194906
227.951140	3386.280308	17.153575	-0.044205	3.191355
227.877102	3378.310330	17.158579	-0.044186	3.187829
227.767250	3370.295535	17.163584	-0.044160	3.184277
227.774929	3362.346773	17.168589	-0.044157	3.180755
227.828471	3354.341205	17.173594	-0.044161	3.177207
227.755457	3346.340589	17.178599	-0.044142	3.173651
227.830917	3338.345176	17.183603	-0.044151	3.170099
227.814458	3330.354258	17.188608	-0.044143	3.166542
227.764488	3322.379080	17.193613	-0.044128	3.162986
227.487309	3314.401386	17.198618	-0.044071	3.159416
227.642287	3306.434121	17.203623	-0.044095	3.155865
227.596684	3298.416443	17.208627	-0.044081	3.152278
227.460264	3290.395176	17.213632	-0.044051	3.148682
227.499971	3282.412558	17.218637	-0.044053	3.145106
227.389580	3274.462068	17.223642	-0.044027	3.141535
227.371155	3266.471346	17.228647	-0.044018	3.137945
227.323902	3258.505802	17.233651	-0.044004	3.134361
227.141519	3250.487868	17.238656	-0.043965	3.130744
227.108909	3242.530262	17.243661	-0.043953	3.127156
227.021681	3234.533969	17.248666	-0.043932	3.123544
226.902038	3226.569529	17.253671	-0.043904	3.119941
227.103036	3218.612830	17.258675	-0.043937	3.116352
227.103189	3210.583905	17.263680	-0.043931	3.112717
226.857422	3202.598544	17.268685	-0.043880	3.109086
226.753002	3194.603690	17.273690	-0.043856	3.105453
226.832721	3186.626579	17.278695	-0.043865	3.101832
226.851947	3178.649728	17.283699	-0.043863	3.098204
226.594671	3170.651790	17.288704	-0.043810	3.094550
226.743156	3162.668390	17.293709	-0.043833	3.090916
226.653764	3154.676630	17.298714	-0.043811	3.087264
226.487430	3146.706254	17.303719	-0.043774	3.083613
226.502885	3138.721524	17.308723	-0.043772	3.079960
226.688132	3130.729021	17.313728	-0.043801	3.076307
226.767727	3122.690005	17.318733	-0.043811	3.072624
226.417634	3114.668381	17.323738	-0.043740	3.068923
226.426215	3106.701415	17.328743	-0.043737	3.065261
226.426086	3098.745539	17.333747	-0.043731	3.061598
226.212050	3090.773725	17.338752	-0.043686	3.057914
226.251148	3082.793069	17.343757	-0.043688	3.054233
226.259945	3074.771783	17.348762	-0.043685	3.050528
226.398281	3066.798824	17.353767	-0.043705	3.046846
226.260315	3058.852518	17.358771	-0.043674	3.043159
226.303810	3050.858110	17.363776	-0.043677	3.039454
226.236953	3042.917129	17.368781	-0.043659	3.035765
225.908363	3034.904954	17.373786	-0.043593	3.032024
225.930252	3026.885808	17.378791	-0.043591	3.028293
225.887568	3018.924782	17.383795	-0.043578	3.024581
225.633251	3010.972250	17.388800	-0.043526	3.020859
225.762701	3002.985490	17.393805	-0.043544	3.017134
225.746686	2994.972410	17.398810	-0.043536	3.013386
225.833735	2986.944496	17.403815	-0.043547	3.009631
225.647570	2979.003881	17.408819	-0.043507	3.005898
225.606786	2971.024007	17.413824	-0.043494	3.002150
225.716787	2963.062760	17.418829	-0.043510	2.998413
225.380183	2955.087030	17.423834	-0.043442	2.994643
225.531408	2947.054592	17.428839	-0.043464	2.990865
225.683825	2939.070451	17.433843	-0.043488	2.987106
225.648703	2931.067362	17.438848	-0.043476	2.983323
225.494196	2923.116187	17.443853	-0.043442	2.979554
225.437986	2915.146215	17.448858	-0.043426	2.975776
225.356643	2907.145002	17.453863	-0.043406	2.971978
225.229116	2899.172810	17.458867	-0.043376	2.968186
225.524029	2891.139281	17.463872	-0.043426	2.964381
225.395946	2883.247253	17.468877	-0.043397	2.960618
225.137605	2875.261540	17.473882	-0.043344	2.956798
225.175641	2867.243841	17.478887	-0.043345	2.952973
225.218985	2859.258787	17.483891	-0.043348	2.949160
225.135855	2851.270354	17.488896	-0.043327	2.945333
225.002944	2843.324447	17.493901	-0.043297	2.941518
225.058419	2835.320319	17.498906	-0.043303	2.937681
225.036285	2827.337669	17.503911	-0.043293	2.933845
225.085789	2819.329120	17.508915	-0.043297	2.929995
224.825254	2811.371425	17.513920	-0.043243	2.926149
224.951988	2803.397469	17.518925	-0.043262	2.922310
224.871227	2795.432128	17.523930	-0.043241	2.918459
224.761480	2787.458591	17.528935	-0.043216	2.914597
224.703383	2779.391416	17.533939	-0.043199	2.910688
224.565613	2771.411456	17.538944	-0.043169	2.906811
224.510243	2763.452395	17.543949	-0.043153	2.902944
224.720006	2755.450257	17.548954	-0.043187	2.899065
224.531601	2747.506042	17.553959	-0.043146	2.895187
224.346251	2739.534470	17.558963	-0.043107	2.891291
224.257995	2731.539937	17.563968	-0.043085	2.887384
224.473576	2723.552430	17.568973	-0.043120	2.883492
224.176232	2715.602228	17.573978	-0.043059	2.879584
224.202501	2707.645268	17.578983	-0.043059	2.875686
224.337359	2699.622085	17.583987	-0.043079	2.871755
224.329198	2691.632837	17.588992	-0.043072	2.867829
224.167946	2683.670469	17.593997	-0.043036	2.863901
223.965881	2675.699014	17.599002	-0.042994	2.859961
224.039972	2667.717002	17.604007	-0.043002	2.856026
223.966574	2659.743667	17.609011	-0.042983	2.852082
223.924635	2651.741908	17.614016	-0.042970	2.848120
224.056315	2643.773185	17.619021	-0.042989	2.844178
223.978065	2635.812860	17.624026	-0.042969	2.840224
223.866713	2627.859894	17.629031	-0.042943	2.836265
223.945451	2619.837510	17.634035	-0.042953	2.832278
223.791699	2611.831619	17.639040	-0.042919	2.828279
223.731184	2603.871490	17.644045	-0.042902	2.824303
223.487913	2595.936655	17.649050	-0.042852	2.820324
223.606542	2587.942980	17.654055	-0.042869	2.816330
223.485200	2579.951411	17.659059	-0.042841	2.812318
223.350898	2571.949805	17.664064	-0.042810	2.808295
223.493236	2563.978758	17.669069	-0.042832	2.804297
223.265232	2556.038197	17.674074	-0.042784	2.800287
223.478890	2548.046306	17.679079	-0.042819	2.796271
223.414267	2540.069577	17.684083	-0.042801	2.792241
223.441948	2532.046171	17.689088	-0.042801	2.788187
223.367600	2524.104819	17.694093	-0.042782	2.784162
223.402298	2516.112453	17.699098	-0.042783	2.780112
223.286728	2508.163365	17.704103	-0.042756	2.776069
223.243558	2500.191695	17.709107	-0.042743	2.772014
222.968061	2492.219680	17.714112	-0.042686	2.767938
223.155944	2484.234020	17.719117	-0.042716	2.763877
223.004111	2476.271149	17.724122	-0.042683	2.759801
222.867177	2468.333014	17.729127	-0.042652	2.755733
222.720090	2460.275707	17.734131	-0.042619	2.751597
222.820239	2452.239750	17.739136	-0.042633	2.747480
222.621075	2444.308216	17.744141	-0.042590	2.743393
222.760619	2436.323068	17.749146	-0.042611	2.739293
222.953731	2428.347685	17.754151	-0.042642	2.735195
222.909669	2420.365149	17.759155	-0.042628	2.731073
222.498862	2412.421999	17.764160	-0.042546	2.726942
222.558214	2404.444161	17.769165	-0.042552	2.722816
222.478802	2396.467855	17.774170	-0.042532	2.718676
222.584863	2388.505614	17.779175	-0.042547	2.714549
222.438902	2380.538190	17.784179	-0.042514	2.710396
222.378845	2372.548200	17.789184	-0.042498	2.706231
222.262104	2364.604262	17.794189	-0.042471	2.702080
222.261366	2356.638940	17.799194	-0.042465	2.697919
222.237604	2348.649925	17.804199	-0.042456	2.693737
222.179428	2340.657833	17.809203	-0.042439	2.689545
221.942944	2332.711071	17.814208	-0.042390	2.685359
222.013836	2324.740820	17.819213	-0.042398	2.681174
222.095120	2316.776971	17.824218	-0.042408	2.676986
222.016805	2308.786347	17.829223	-0.042388	2.672767
222.092551	2300.776654	17.834227	-0.042397	2.668542
221.923761	2292.793462	17.839232	-0.042360	2.664308
222.089676	2284.845224	17.844237	-0.042386	2.660107
221.840998	2276.894259	17.849242	-0.042334	2.655871
221.852406	2268.901992	17.854247	-0.042331	2.651624
221.774488	2260.936398	17.859251	-0.042311	2.647378
221.742953	2252.952485	17.864256	-0.042300	2.643118
221.814461	2245.000912	17.869261	-0.042308	2.638876
221.727110	2237.028287	17.874266	-0.042287	2.634605
221.546396	2229.061233	17.879271	-0.042248	2.630324
221.525978	2221.108375	17.884275	-0.042239	2.626054
221.472719	2213.118559	17.889280	-0.042224	2.621756
221.710258	2205.152476	17.894285	-0.042263	2.617482
221.340972	2197.202854	17.899290	-0.042189	2.613169
221.455094	2189.186850	17.904295	-0.042204	2.608846
221.649679	2181.206038	17.909299	-0.042235	2.604541
221.457403	2173.271289	17.914304	-0.042194	2.600227
221.266655	2165.356234	17.919309	-0.042154	2.595916
221.249801	2157.208709	17.924314	-0.042145	2.591484
221.173266	2149.214870	17.929319	-0.042126	2.587124
220.989385	2141.299175	17.934323	-0.042086	2.582792
221.122577	2133.325071	17.939328	-0.042106	2.578442
221.035095	2125.404927	17.944333	-0.042084	2.574099
220.713417	2117.442402	17.949338	-0.042019	2.569710
220.967558	2109.455907	17.954343	-0.042061	2.565339
220.941396	2101.519999	17.959347	-0.042051	2.560970
220.810082	2093.559470	17.964352	-0.042021	2.556572
220.717316	2085.599635	17.969357	-0.041999	2.552170
220.705113	2077.616289	17.974362	-0.041991	2.547752
220.703903	2069.651021	17.979367	-0.041986	2.543338
220.413513	2061.731637	17.984371	-0.041926	2.538921
220.659536	2053.717668	17.989376	-0.041967	2.534482
220.738853	2045.743084	17.994381	-0.041976	2.530045
220.321141	2037.808023	17.999386	-0.041893	2.525587
220.453386	2029.835160	18.004391	-0.041913	2.521139
220.687571	2021.876565	18.009395	-0.041951	2.516699
220.406981	2013.896564	18.014400	-0.041893	2.512202
220.355690	2005.913435	18.019405	-0.041879	2.507711
220.254640	1997.958802	18.024410	-0.041855	2.503225
220.344209	1989.978113	18.029415	-0.041866	2.498730
220.209577	1982.055895	18.034419	-0.041836	2.494244
220.201830	1974.049477	18.039424	-0.041829	2.489711
220.096413	1966.100280	18.044429	-0.041804	2.485195
219.873029	1958.186951	18.049434	-0.041757	2.480682
219.865260	1950.213255	18.054439	-0.041750	2.476143
219.877505	1942.251025	18.059443	-0.041748	2.471603
219.560224	1934.274876	18.064448	-0.041683	2.467023
219.562459	1926.324575	18.069453	-0.041678	2.462473
219.835022	1918.321770	18.074458	-0.041724	2.457904
219.790701	1910.360802	18.079463	-0.041710	2.453327
219.854721	1902.396428	18.084467	-0.041717	2.448748
219.837010	1894.422758	18.089472	-0.041708	2.444149
219.821037	1886.479797	18.094477	-0.041700	2.439559
219.439955	1878.577010	18.099482	-0.041624	2.434955
219.521185	1870.508710	18.104487	-0.041634	2.430282
219.534172	1862.548092	18.109491	-0.041631	2.425658
219.348957	1854.605572	18.114496	-0.041591	2.421020
219.359773	1846.662286	18.119501	-0.041588	2.416388
219.175164	1838.711327	18.124506	-0.041548	2.411727
219.074002	1830.747708	18.129511	-0.041524	2.407056
218.949266	1822.816299	18.134515	-0.041496	2.402393
218.893926	1814.859801	18.139520	-0.041480	2.397712
219.127677	1806.867820	18.144525	-0.041518	2.393023
218.941011	1798.916909	18.149530	-0.041478	2.388316
218.798915	1790.967902	18.154535	-0.041447	2.383605
219.057736	1782.991456	18.159539	-0.041490	2.378900
219.132613	1775.024320	18.164544	-0.041498	2.374176
218.842478	1767.095595	18.169549	-0.041439	2.369437
218.608666	1759.160151	18.174554	-0.041390	2.364688
218.701366	1751.198056	18.179559	-0.041402	2.359941
218.742636	1743.255472	18.184563	-0.041405	2.355191
218.466749	1735.278931	18.189568	-0.041348	2.350386
218.486898	1727.300315	18.194573	-0.041346	2.345593
218.548069	1719.334489	18.199578	-0.041353	2.340802
218.501287	1711.387697	18.204583	-0.041339	2.336004
218.482611	1703.431247	18.209587	-0.041330	2.331192
218.391179	1695.475913	18.214592	-0.041308	2.326365
218.318431	1687.541526	18.219597	-0.041289	2.321542
218.290911	1679.608003	18.224602	-0.041278	2.316713
218.404367	1671.617768	18.229607	-0.041294	2.311852
218.249200	1663.686924	18.234611	-0.041260	2.306994
218.000706	1655.751041	18.239616	-0.041209	2.302115
217.938120	1647.810156	18.244621	-0.041192	2.297238
218.075942	1639.815478	18.249626	-0.041212	2.292334
217.972743	1631.857337	18.254631	-0.041188	2.287422
217.889840	1623.942591	18.259635	-0.041167	2.282528
217.803797	1616.004474	18.264640	-0.041146	2.277609
217.787430	1608.020858	18.269645	-0.041137	2.272656
217.694084	1600.020898	18.274650	-0.041115	2.267676
217.756044	1592.061328	18.279655	-0.041121	2.262724
217.599611	1584.151465	18.284659	-0.041087	2.257773
217.536267	1576.183785	18.289664	-0.041070	2.252783
217.701934	1568.216810	18.294669	-0.041095	2.247802
217.508308	1560.300857	18.299674	-0.041054	2.242811
217.204113	1552.395808	18.304679	-0.040992	2.237806
217.225449	1544.440875	18.309683	-0.040991	2.232787
217.303193	1536.444140	18.314688	-0.041000	2.227735
217.196856	1528.522034	18.319693	-0.040975	2.222702
217.120597	1520.595059	18.324698	-0.040955	2.217658
217.001244	1512.637875	18.329703	-0.040928	2.212579
217.039257	1504.686393	18.334707	-0.040930	2.207506
216.779164	1496.770821	18.339712	-0.040876	2.202417
217.042705	1488.812163	18.344717	-0.040920	2.197337
216.961435	1480.849890	18.349722	-0.040900	2.192211
216.798344	1472.896333	18.354727	-0.040864	2.187071
216.772850	1464.971756	18.359731	-0.040854	2.181950
216.645951	1457.033219	18.364736	-0.040825	2.176799
216.500166	1449.101578	18.369741	-0.040793	2.171638
216.517423	1441.144574	18.374746	-0.040791	2.166464
216.480999	1433.206312	18.379751	-0.040779	2.161284
216.405858	1425.308360	18.384755	-0.040759	2.156115
216.177698	1417.359881	18.389760	-0.040712	2.150886
216.287743	1409.386031	18.394765	-0.040727	2.145659
216.457489	1401.424849	18.399770	-0.040753	2.140433
216.257779	1393.514496	18.404775	-0.040711	2.135194
216.163441	1385.580975	18.409779	-0.040688	2.129936
216.111159	1377.626254	18.414784	-0.040673	2.124654
216.214843	1369.703325	18.419789	-0.040687	2.119396
216.122431	1361.777035	18.424794	-0.040665	2.114104
216.163926	1353.751444	18.429799	-0.040667	2.108744
216.178363	1345.825514	18.434803	-0.040664	2.103436
215.860105	1337.933869	18.439808	-0.040600	2.098104
216.028172	1329.988253	18.444813	-0.040626	2.092770
215.783551	1322.068650	18.449818	-0.040575	2.087400
215.625131	1314.153831	18.454823	-0.040541	2.082027
215.853126	1306.212456	18.459827	-0.040578	2.076661
215.603471	1298.286136	18.464832	-0.040526	2.071243
215.583389	1290.342403	18.469837	-0.040517	2.065823
215.480197	1282.423458	18.474842	-0.040493	2.060396
215.407296	1274.510312	18.479847	-0.040474	2.054963
215.485733	1266.547650	18.484851	-0.040483	2.049496
215.326946	1258.632830	18.489856	-0.040448	2.044023
215.158612	1250.743866	18.494861	-0.040412	2.038553
215.401302	1242.769365	18.499866	-0.040452	2.033050
215.139909	1234.839827	18.504871	-0.040398	2.027512
215.121284	1226.913762	18.509875	-0.040389	2.021987
215.149191	1218.982848	18.514880	-0.040389	2.016447
215.121399	1211.052333	18.519885	-0.040379	2.010887
215.035261	1203.133755	18.524890	-0.040357	2.005314
215.044596	1195.213340	18.529895	-0.040354	1.999734
214.788214	1187.345414	18.534899	-0.040301	1.994147
214.631428	1179.398013	18.539904	-0.040266	1.988499
214.711007	1171.464640	18.544909	-0.040276	1.982870
214.737492	1163.535810	18.549914	-0.040276	1.977222
214.718069	1155.605467	18.554919	-0.040267	1.971552
214.530138	1147.705494	18.559923	-0.040227	1.965870
214.463831	1139.794674	18.564928	-0.040209	1.960176
214.542248	1131.875232	18.569933	-0.040218	1.954475
214.292184	1123.931293	18.574938	-0.040167	1.948704
214.253198	1115.998912	18.579943	-0.040154	1.942947
214.287928	1108.087313	18.584947	-0.040155	1.937197
213.887082	1100.206205	18.589952	-0.040075	1.931403
214.033750	1092.248164	18.594957	-0.040098	1.925596
214.059627	1084.339432	18.599962	-0.040097	1.919795
214.045130	1076.427840	18.604967	-0.040089	1.913969
213.762406	1068.548623	18.609971	-0.040031	1.908119
213.849338	1060.602607	18.614976	-0.040042	1.902243
213.864725	1052.708463	18.619981	-0.040040	1.896380
213.799763	1044.783975	18.624986	-0.040023	1.890466
213.680835	1036.884801	18.629991	-0.039995	1.884547
213.777008	1028.989382	18.634995	-0.040008	1.878637
213.482835	1021.102822	18.640000	-0.039948	1.872670
213.579460	1013.156955	18.645005	-0.039961	1.866684
213.449751	1005.261799	18.650010	-0.039931	1.860690
213.354713	997.374744	18.655015	-0.039908	1.854688
213.380860	989.452565	18.660019	-0.039908	1.848654
213.464828	981.526323	18.665024	-0.039918	1.842603
213.283580	973.670618	18.670029	-0.039879	1.836555
213.088178	965.786797	18.675034	-0.039838	1.830464
213.027975	957.868567	18.680039	-0.039821	1.824342
213.216021	949.959558	18.685043	-0.039851	1.818237
213.032929	942.065464	18.690048	-0.039812	1.812077
213.210452	934.138980	18.695053	-0.039840	1.805915
213.180988	926.259644	18.700058	-0.039829	1.799744
213.022931	918.387173	18.705063	-0.039794	1.793541
212.849460	910.465150	18.710067	-0.039757	1.787276
212.606711	902.594394	18.715072	-0.039706	1.781020
212.694281	894.705774	18.720077	-0.039718	1.774770
212.544310	886.813547	18.725082	-0.039684	1.768464
212.360098	878.947494	18.730087	-0.039645	1.762153
212.414810	871.063894	18.735091	-0.039650	1.755835
212.429272	863.145779	18.740096	-0.039647	1.749461
212.421990	855.264873	18.745101	-0.039641	1.743091
212.410110	847.384061	18.750106	-0.039633	1.736697
212.327551	839.505617	18.755111	-0.039613	1.730273
212.091426	831.669908	18.760115	-0.039564	1.723840
212.061574	823.785210	18.765120	-0.039553	1.717369
212.073018	815.890964	18.770125	-0.039550	1.710871
211.904191	808.023206	18.775130	-0.039513	1.704346
211.750664	800.158856	18.780135	-0.039479	1.697802
211.714347	792.283579	18.785139	-0.039467	1.691238
211.722032	784.381953	18.790144	-0.039464	1.684633
211.758979	776.532972	18.795149	-0.039465	1.678049
211.423361	768.698363	18.800154	-0.039398	1.671402
211.659472	760.773286	18.805159	-0.039436	1.664729
211.739508	752.915139	18.810163	-0.039446	1.658064
211.456696	745.072228	18.815168	-0.039388	1.651337
211.396224	737.208425	18.820173	-0.039372	1.644594
211.376663	729.370161	18.825178	-0.039363	1.637851
211.241744	721.473774	18.830183	-0.039333	1.631014
211.163365	713.610151	18.835187	-0.039313	1.624184
211.089824	705.752546	18.840192	-0.039294	1.617332
211.118954	697.887744	18.845197	-0.039294	1.610458
211.084078	690.038845	18.850202	-0.039282	1.603560
210.974125	682.206611	18.855207	-0.039257	1.596637
210.875416	674.372653	18.860211	-0.039233	1.589683
210.536545	666.565654	18.865216	-0.039165	1.582688
210.813186	658.677641	18.870221	-0.039211	1.575678
210.768873	650.830542	18.875226	-0.039198	1.568627
210.486153	643.024936	18.880231	-0.039140	1.561547
210.393776	635.204561	18.885235	-0.039118	1.554449
210.419983	627.325412	18.890240	-0.039117	1.547282
210.332624	619.501077	18.895245	-0.039096	1.540116
210.366429	611.662809	18.900250	-0.039097	1.532921
210.319401	603.820193	18.905255	-0.039083	1.525676
210.042671	596.058401	18.910259	-0.039026	1.518437
209.807194	588.239552	18.915264	-0.038977	1.511116
209.923116	580.390464	18.920269	-0.038994	1.503785
209.992641	572.556384	18.925274	-0.039002	1.496425
209.770101	564.761334	18.930279	-0.038955	1.489020
209.873330	556.934846	18.935283	-0.038969	1.481599
209.936117	549.105881	18.940288	-0.038975	1.474132
209.851730	541.255725	18.945293	-0.038955	1.466583
209.458955	533.520051	18.950298	-0.038876	1.459057
209.439988	525.699127	18.955303	-0.038868	1.451469
209.488048	517.897602	18.960307	-0.038871	1.443870
209.202425	510.139091	18.965312	-0.038813	1.436220
209.214548	502.331630	18.970317	-0.038810	1.428528
209.239597	494.528595	18.975322	-0.038810	1.420802
208.970973	486.778776	18.980327	-0.038755	1.413038
208.936853	478.987248	18.985331	-0.038743	1.405228
208.781912	471.227463	18.990336	-0.038709	1.397386
208.603346	463.454997	18.995341	-0.038671	1.389483
208.622037	455.653436	19.000346	-0.038669	1.381538
208.721729	447.860484	19.005351	-0.038682	1.373571
208.649693	440.100612	19.010355	-0.038664	1.365561
208.323274	432.388710	19.015360	-0.038598	1.357510
208.424630	424.599671	19.020365	-0.038612	1.349404
208.528605	416.821852	19.025370	-0.038626	1.341262
208.340893	409.098565	19.030375	-0.038586	1.333077
208.346976	401.343996	19.035379	-0.038582	1.324842
208.176137	393.627834	19.040384	-0.038545	1.316564
208.187022	385.766151	19.045389	-0.038542	1.308111
207.785881	378.081555	19.050394	-0.038462	1.299719
207.739428	370.351706	19.055399	-0.038448	1.291288
208.049207	362.584290	19.060403	-0.038501	1.282827
207.865110	354.902496	19.065408	-0.038461	1.274312
207.701434	347.205706	19.070413	-0.038426	1.265727
207.727035	339.503360	19.075418	-0.038426	1.257113
207.485811	331.825684	19.080423	-0.038376	1.248417
207.349686	324.157979	19.085427	-0.038345	1.239690
207.118822	316.480777	19.090432	-0.038297	1.230873
207.264054	308.749305	19.095437	-0.038319	1.222003
207.069918	301.102550	19.100442	-0.038278	1.213100
206.782139	293.455189	19.105447	-0.038219	1.204111
206.963336	285.758827	19.110451	-0.038248	1.195091
206.639494	278.130199	19.115456	-0.038182	1.185980
206.612878	270.477632	19.120461	-0.038172	1.176831
206.864216	262.775434	19.125466	-0.038214	1.167608
206.663544	255.169795	19.130471	-0.038172	1.158335
206.509389	247.529902	19.135475	-0.038138	1.148955
206.301672	239.912318	19.140480	-0.038094	1.139513
206.356752	232.279202	19.145485	-0.038099	1.130030
206.099232	224.702888	19.150490	-0.038047	1.120470
206.006454	217.105664	19.155495	-0.038024	1.110837
206.062376	209.497905	19.160499	-0.038030	1.101139
205.991475	201.911388	19.165504	-0.038011	1.091355
205.761124	194.379512	19.170509	-0.037964	1.081517
205.735815	186.810139	19.175514	-0.037954	1.071586
205.422597	179.278539	19.180519	-0.037890	1.061546
205.336779	171.743831	19.185523	-0.037870	1.051458
205.065520	164.230462	19.190528	-0.037814	1.041259
205.326430	156.660139	19.195533	-0.037858	1.031006
205.097531	149.173876	19.200538	-0.037810	1.020650
204.971739	141.686339	19.205543	-0.037782	1.010210
204.872064	134.214696	19.210547	-0.037758	0.999690
204.631514	126.741246	19.215552	-0.037708	0.989021
204.478879	119.284418	19.220557	-0.037675	0.978281
204.380758	111.832879	19.225562	-0.037652	0.967443
204.201740	104.421598	19.230567	-0.037614	0.956521
204.119821	97.007807	19.235571	-0.037593	0.945495
204.030195	89.603159	19.240576	-0.037572	0.934350
204.006116	82.213654	19.245581	-0.037563	0.923111
203.640468	74.897323	19.250586	-0.037490	0.911754
203.326365	67.573847	19.255591	-0.037426	0.900257
203.435116	60.433858	19.260595	-0.037442	0.889020