Fri Mar 12 13:10:18 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.912845	-0.035655	0.000000	-0.000012	0.720728

0.816325	-0.113810	0.005005	0.000006	0.720540
0.847521	-0.124544	0.010010	0.000001	0.720530
0.700108	-0.095304	0.015014	0.000028	0.720536
0.727786	-0.098156	0.020019	0.000023	0.720540
0.582038	-0.075953	0.025024	0.000050	0.720532
0.574722	-0.069878	0.030029	0.000051	0.720542
0.616709	-0.083286	0.035034	0.000044	0.720530
0.541706	-0.066783	0.040038	0.000058	0.720536
0.596051	-0.075494	0.045043	0.000048	0.720538
0.635726	-0.087976	0.050048	0.000040	0.720527
0.510421	-0.058907	0.055053	0.000063	0.720540
0.739427	-0.103955	0.060058	0.000021	0.720532
0.902090	-0.130846	0.065062	-0.000009	0.720536
0.836119	-0.117735	0.070067	0.000003	0.720539
0.718697	-0.102875	0.075072	0.000025	0.720527
0.677442	-0.089447	0.080077	0.000032	0.720539
0.664678	-0.245308	0.085082	0.000035	0.720227
0.774296	-0.268103	0.090086	0.000015	0.720221
0.763624	-0.265910	0.095091	0.000017	0.720221
0.605288	-0.239996	0.100096	0.000046	0.720217
0.717591	-0.256296	0.105101	0.000025	0.720224
0.671308	-0.251842	0.110106	0.000034	0.720217
0.549376	-0.311418	0.115110	0.000057	0.720056
0.587339	-0.399333	0.120115	0.000050	0.719897
0.396930	-0.368775	0.125120	0.000085	0.719890
0.474554	-0.376048	0.130125	0.000071	0.719903
0.391887	-0.365629	0.135130	0.000086	0.719894
0.318925	-0.370760	0.140134	0.000100	0.719859
0.564087	-0.546393	0.145139	0.000054	0.719598
0.643323	-0.564053	0.150144	0.000039	0.719591
0.652105	-0.558436	0.155149	0.000038	0.719606
0.706215	-0.572175	0.160154	0.000028	0.719597
0.683474	-0.719918	0.165158	0.000032	0.719298
0.774983	-0.748825	0.170163	0.000015	0.719273
0.628464	-0.726079	0.175168	0.000042	0.719267
0.714958	-0.779814	0.180173	0.000026	0.719191
0.477528	-0.856482	0.185178	0.000071	0.718956
0.466882	-0.853028	0.190182	0.000073	0.718959
0.546078	-0.867830	0.195187	0.000058	0.718958
0.341254	-0.967665	0.200192	0.000096	0.718689
0.257531	-0.974763	0.205197	0.000112	0.718645
0.225449	-0.974412	0.210202	0.000118	0.718635
0.213855	-1.048161	0.215206	0.000120	0.718485
0.405052	-1.149160	0.220211	0.000084	0.718353
0.370004	-1.146183	0.225216	0.000091	0.718346
0.479500	-1.254114	0.230221	0.000071	0.718172
0.369771	-1.316775	0.235226	0.000091	0.718009
0.400667	-1.321275	0.240230	0.000085	0.718011
0.222524	-1.409370	0.245235	0.000119	0.717774
0.483469	-1.495639	0.250240	0.000070	0.717696
0.481044	-1.515173	0.255245	0.000071	0.717656
0.292628	-1.625456	0.260250	0.000106	0.717372
0.272257	-1.620509	0.265254	0.000109	0.717374
-0.015940	-1.658589	0.270259	0.000163	0.717198
-0.438300	-1.645644	0.275264	0.000242	0.717074
-0.227063	-1.678639	0.280269	0.000203	0.717083
-0.247458	-1.844682	0.285274	0.000206	0.716748
-0.299206	-1.835804	0.290278	0.000216	0.716747
-0.080556	-1.949814	0.295283	0.000175	0.716598
0.060984	-2.055789	0.300288	0.000149	0.716438
0.057614	-2.089703	0.305293	0.000150	0.716370
-0.329684	-2.145856	0.310298	0.000222	0.716122
-0.306692	-2.147770	0.315302	0.000218	0.716126
-0.179944	-2.291353	0.320307	0.000194	0.715887
-1.036223	-2.145734	0.325312	0.000354	0.715873
-1.109341	-2.242014	0.330317	0.000367	0.715656
-2.344686	-2.081657	0.335322	0.000597	0.715538
-2.311801	-2.086595	0.340326	0.000591	0.715540
-2.510721	-2.199329	0.345331	0.000628	0.715246
-3.343351	-2.064323	0.350336	0.000783	0.715219
-3.431800	-2.043121	0.355341	0.000800	0.715230
-3.200394	-2.217187	0.360346	0.000757	0.714967
-4.207509	-2.070125	0.365350	0.000944	0.714902
-3.967152	-2.111750	0.370355	0.000900	0.714905
-3.859369	-2.201763	0.375360	0.000880	0.714764
-4.845087	-2.106780	0.380365	0.001063	0.714604
-4.741465	-2.128882	0.385370	0.001044	0.714597
-4.795788	-2.118678	0.390374	0.001054	0.714598
-4.844699	-2.235256	0.395379	0.001063	0.714349
-5.908693	-2.087454	0.400384	0.001261	0.714266
-5.930887	-2.079987	0.405389	0.001265	0.714273
-5.674089	-2.127727	0.410394	0.001217	0.714269
-6.197237	-2.127897	0.415398	0.001315	0.714083
-7.075026	-2.029627	0.420403	0.001478	0.713968
-6.961860	-2.054958	0.425408	0.001457	0.713958
-6.503698	-2.130954	0.430413	0.001372	0.713969
-6.852890	-2.071986	0.435418	0.001437	0.713962
-7.159002	-2.126171	0.440422	0.001494	0.713746
-7.736554	-2.070251	0.445427	0.001602	0.713653
-7.942164	-2.038039	0.450432	0.001640	0.713644
-7.599124	-2.096080	0.455437	0.001576	0.713650
-7.556698	-2.107000	0.460442	0.001568	0.713643
-7.718212	-2.143567	0.465446	0.001598	0.713513
-8.656251	-2.056286	0.470451	0.001773	0.713354
-8.598855	-2.069519	0.475456	0.001762	0.713348
-8.405428	-2.098159	0.480461	0.001726	0.713360
-8.775079	-2.036169	0.485466	0.001795	0.713352
-8.660420	-2.057406	0.490470	0.001774	0.713351
-8.348021	-2.218790	0.495475	0.001716	0.713140
-9.858648	-2.013675	0.500480	0.001997	0.713013
-9.486259	-2.074519	0.505485	0.001928	0.713024
-9.279956	-2.115302	0.510490	0.001889	0.713016
-9.562546	-2.064662	0.515494	0.001942	0.713016
-9.629362	-2.047996	0.520499	0.001954	0.713026
-9.786474	-2.115519	0.525504	0.001984	0.712836
-10.495357	-2.053457	0.530509	0.002116	0.712708
-10.003407	-2.142901	0.535514	0.002024	0.712704
-10.535256	-2.049494	0.540518	0.002123	0.712701
-10.249801	-2.097949	0.545523	0.002070	0.712706
-10.393251	-2.075432	0.550528	0.002097	0.712700
-10.383489	-2.130782	0.555533	0.002095	0.712593
-11.431028	-2.052047	0.560538	0.002290	0.712378
-11.119708	-2.105270	0.565542	0.002232	0.712383
-11.389584	-2.055797	0.570547	0.002282	0.712386
-11.433315	-2.052457	0.575552	0.002290	0.712377
-10.963900	-2.133301	0.580557	0.002203	0.712382
-11.450383	-2.048484	0.585562	0.002294	0.712378
-11.813711	-2.085438	0.590566	0.002361	0.712176
-12.015851	-2.092021	0.595571	0.002399	0.712091
-11.954803	-2.108916	0.600576	0.002388	0.712079
-12.256730	-2.050049	0.605581	0.002444	0.712089
-12.291712	-2.046308	0.610586	0.002450	0.712084
-12.176205	-2.067736	0.615590	0.002429	0.712082
-12.024612	-2.091286	0.620595	0.002401	0.712089
-12.958461	-2.090784	0.625600	0.002574	0.711758
-12.848184	-2.111320	0.630605	0.002554	0.711757
-13.028511	-2.080504	0.635610	0.002588	0.711754
-13.051676	-2.078279	0.640614	0.002592	0.711750
-12.740140	-2.130292	0.645619	0.002534	0.711757
-12.994435	-2.088214	0.650624	0.002581	0.711751
-13.169745	-2.090313	0.655629	0.002614	0.711684
-13.935639	-2.072174	0.660634	0.002757	0.711448
-13.782273	-2.100818	0.665638	0.002728	0.711445
-14.088115	-2.042234	0.670643	0.002785	0.711454
-14.370297	-1.996788	0.675648	0.002837	0.711444
-13.668965	-2.115877	0.680653	0.002707	0.711456
-13.668490	-2.119859	0.685658	0.002707	0.711448
-14.322176	-2.022496	0.690662	0.002829	0.711410
-14.480293	-2.131071	0.695667	0.002858	0.711137
-14.578152	-2.119563	0.700672	0.002876	0.711125
-15.038134	-2.032534	0.705677	0.002962	0.711135
-14.971583	-2.046060	0.710682	0.002950	0.711132
-14.818312	-2.072850	0.715686	0.002921	0.711133
-14.666723	-2.097031	0.720691	0.002893	0.711138
-15.157654	-2.025178	0.725696	0.002984	0.711107
-15.514761	-2.081381	0.730701	0.003051	0.710868
-15.359015	-2.110684	0.735706	0.003022	0.710865
-15.736065	-2.043713	0.740710	0.003092	0.710864
-15.295759	-2.118056	0.745715	0.003010	0.710872
-15.427510	-2.099606	0.750720	0.003035	0.710862
-15.427864	-2.094992	0.755725	0.003035	0.710871
-15.696133	-2.145527	0.760730	0.003085	0.710675
-16.683617	-2.044771	0.765734	0.003269	0.710525
-16.137100	-2.137771	0.770739	0.003167	0.710533
-16.882930	-2.009066	0.775744	0.003306	0.710525
-16.414218	-2.088045	0.780749	0.003218	0.710534
-16.027249	-2.161249	0.785754	0.003146	0.710526
-16.642739	-2.051512	0.790758	0.003261	0.710526
-16.955331	-2.119058	0.795763	0.003319	0.710279
-17.402908	-2.075842	0.800768	0.003403	0.710206
-17.208519	-2.104337	0.805773	0.003366	0.710219
-17.418348	-2.071108	0.810778	0.003405	0.710210
-17.658216	-2.027604	0.815782	0.003450	0.710212
-17.075979	-2.128498	0.820787	0.003342	0.710217
-17.594494	-2.041351	0.825792	0.003438	0.710207
-17.636649	-2.152544	0.830797	0.003446	0.709970
-18.177437	-2.099023	0.835802	0.003547	0.709884
-18.406351	-2.057314	0.840806	0.003590	0.709886
-18.198209	-2.091192	0.845811	0.003551	0.709892
-18.262886	-2.084960	0.850816	0.003563	0.709881
-18.117666	-2.106570	0.855821	0.003536	0.709890
-18.390146	-2.059791	0.860826	0.003587	0.709886
-18.823254	-2.103868	0.865830	0.003667	0.709644
-19.150857	-2.069742	0.870835	0.003728	0.709595
-19.573128	-1.999934	0.875840	0.003807	0.709584
-19.271161	-2.048311	0.880845	0.003751	0.709595
-18.924953	-2.111518	0.885850	0.003686	0.709592
-19.082590	-2.084970	0.890854	0.003716	0.709589
-19.195526	-2.062291	0.895859	0.003737	0.709594
-19.203766	-2.158042	0.900864	0.003738	0.709400
-20.259654	-2.040218	0.905869	0.003935	0.709259
-20.017918	-2.085743	0.910874	0.003890	0.709254
-20.271294	-2.038660	0.915878	0.003937	0.709258
-19.950707	-2.091685	0.920883	0.003877	0.709266
-19.901893	-2.106727	0.925888	0.003868	0.709253
-20.242188	-2.041969	0.930893	0.003932	0.709261
-20.012798	-2.167817	0.935898	0.003889	0.709091
-21.101519	-2.042819	0.940902	0.004092	0.708953
-20.890978	-2.079080	0.945907	0.004053	0.708956
-20.950903	-2.072751	0.950912	0.004064	0.708947
-20.700685	-2.112848	0.955917	0.004017	0.708956
-20.865289	-2.084939	0.960922	0.004048	0.708953
-21.062610	-2.053031	0.965926	0.004085	0.708946
-20.849970	-2.188290	0.970931	0.004045	0.708751
-21.977001	-2.047851	0.975936	0.004255	0.708630
-21.892920	-2.059432	0.980941	0.004239	0.708637
-21.556098	-2.120500	0.985946	0.004177	0.708635
-21.582258	-2.116875	0.990950	0.004181	0.708633
-21.725125	-2.087851	0.995955	0.004208	0.708640
-21.965138	-2.049774	1.000960	0.004253	0.708631
-21.965199	-2.154207	1.005965	0.004253	0.708421
-22.570467	-2.082814	1.010970	0.004365	0.708348
-22.808196	-2.041479	1.015974	0.004410	0.708346
-22.404573	-2.109625	1.020979	0.004335	0.708354
-22.816130	-2.040347	1.025984	0.004411	0.708346
-22.814881	-2.038295	1.030989	0.004411	0.708350
-22.450574	-2.103874	1.035994	0.004343	0.708349
-22.835408	-2.178038	1.040998	0.004415	0.708063
-23.722400	-2.043951	1.046003	0.004580	0.708014
-23.688117	-2.055419	1.051008	0.004574	0.708004
-23.069002	-2.162133	1.056013	0.004458	0.708011
-23.609533	-2.066787	1.061018	0.004559	0.708009
-23.934907	-2.010764	1.066022	0.004620	0.708005
-23.220111	-2.133831	1.071027	0.004487	0.708014
-23.755465	-2.180744	1.076032	0.004586	0.707728
-24.568932	-2.049396	1.081037	0.004738	0.707701
-24.441211	-2.073118	1.086042	0.004714	0.707699
-24.289794	-2.103439	1.091046	0.004686	0.707692
-24.486005	-2.064015	1.096051	0.004722	0.707701
-24.547625	-2.057297	1.101056	0.004734	0.707692
-24.153158	-2.123662	1.106061	0.004660	0.707700
-24.772444	-2.162198	1.111066	0.004776	0.707402
-25.484522	-2.050973	1.116070	0.004908	0.707370
-25.129424	-2.109002	1.121075	0.004842	0.707381
-25.337351	-2.077409	1.126080	0.004881	0.707370
-25.820011	-1.988406	1.131085	0.004971	0.707375
-25.491232	-2.049250	1.136090	0.004910	0.707371
-25.090350	-2.121157	1.141094	0.004835	0.707370
-25.248650	-2.190736	1.146099	0.004865	0.707174
-26.415090	-2.031369	1.151104	0.005082	0.707076
-26.115129	-2.082372	1.156109	0.005026	0.707081
-25.781546	-2.143217	1.161114	0.004964	0.707078
-26.361261	-2.041113	1.166118	0.005072	0.707076
-26.001014	-2.101346	1.171123	0.005005	0.707084
-26.029950	-2.099828	1.176128	0.005010	0.707076
-26.862341	-2.098719	1.181133	0.005165	0.706781
-26.903640	-2.107392	1.186138	0.005173	0.706748
-26.994982	-2.093038	1.191142	0.005190	0.706745
-26.697418	-2.140275	1.196147	0.005134	0.706756
-27.180454	-2.059714	1.201152	0.005224	0.706745
-27.016541	-2.084332	1.206157	0.005194	0.706754
-26.628370	-2.167732	1.211162	0.005122	0.706726
-28.012712	-2.062717	1.216166	0.005379	0.706441
-27.640397	-2.124875	1.221171	0.005310	0.706449
-27.790464	-2.103625	1.226176	0.005338	0.706438
-27.677035	-2.120761	1.231181	0.005317	0.706444
-27.895129	-2.084705	1.236186	0.005358	0.706439
-27.921043	-2.082129	1.241190	0.005362	0.706435
-27.753109	-2.137413	1.246195	0.005331	0.706384
-28.900495	-2.061865	1.251200	0.005545	0.706124
-28.684703	-2.099230	1.256205	0.005505	0.706127
-28.686393	-2.100622	1.261210	0.005505	0.706123
-28.839811	-2.074501	1.266214	0.005534	0.706121
-28.447175	-2.140750	1.271219	0.005461	0.706128
-28.740933	-2.091514	1.276224	0.005515	0.706122
-28.814574	-2.104810	1.281229	0.005529	0.706069
-29.358789	-2.111341	1.286234	0.005630	0.705860
-29.361405	-2.110937	1.291238	0.005631	0.705860
-29.472187	-2.088030	1.296243	0.005651	0.705867
-29.566426	-2.075291	1.301248	0.005669	0.705858
-29.287949	-2.121774	1.306253	0.005617	0.705865
-29.225571	-2.135208	1.311258	0.005606	0.705860
-29.840387	-2.142931	1.316262	0.005720	0.705624
-30.565054	-2.061408	1.321267	0.005855	0.705528
-30.233306	-2.126778	1.326272	0.005793	0.705515
-30.311888	-2.108332	1.331277	0.005808	0.705524
-30.696401	-2.041051	1.336282	0.005879	0.705522
-30.418759	-2.091655	1.341286	0.005828	0.705520
-29.924833	-2.176705	1.346291	0.005736	0.705526
-31.024958	-2.113012	1.351296	0.005941	0.705259
-31.509185	-2.051449	1.356301	0.006031	0.705209
-31.159209	-2.114213	1.361306	0.005966	0.705208
-31.541044	-2.048725	1.366310	0.006037	0.705203
-31.504831	-2.050087	1.371315	0.006030	0.705213
-31.226599	-2.104209	1.376320	0.005978	0.705204
-31.083053	-2.126721	1.381325	0.005952	0.705210
-31.581338	-2.130992	1.386330	0.006044	0.705023
-32.586979	-2.024210	1.391334	0.006232	0.704877
-31.862521	-2.148582	1.396339	0.006097	0.704886
-32.327626	-2.068362	1.401344	0.006183	0.704881
-32.279989	-2.074825	1.406349	0.006175	0.704885
-31.738012	-2.171315	1.411354	0.006074	0.704885
-32.042811	-2.120604	1.416358	0.006130	0.704878
-32.682689	-2.112679	1.421363	0.006250	0.704664
-33.102750	-2.079109	1.426368	0.006328	0.704581
-33.028380	-2.089525	1.431373	0.006314	0.704587
-32.980766	-2.097844	1.436378	0.006305	0.704587
-33.302579	-2.041231	1.441382	0.006365	0.704585
-32.704717	-2.145400	1.446387	0.006254	0.704590
-33.240869	-2.054875	1.451392	0.006354	0.704580
-33.585834	-2.095759	1.456397	0.006418	0.704374
-34.044530	-2.072085	1.461402	0.006503	0.704256
-33.995213	-2.084850	1.466406	0.006494	0.704248
-33.775672	-2.118672	1.471411	0.006453	0.704259
-33.950485	-2.091517	1.476416	0.006486	0.704251
-33.666562	-2.139991	1.481421	0.006433	0.704255
-34.058781	-2.069934	1.486426	0.006506	0.704255
-34.345720	-2.119139	1.491430	0.006560	0.704053
-34.786645	-2.089471	1.496435	0.006642	0.703954
-35.071783	-2.043225	1.501440	0.006695	0.703945
-35.186498	-2.019468	1.506445	0.006716	0.703952
-34.866625	-2.075283	1.511450	0.006657	0.703954
-34.936313	-2.067952	1.516454	0.006670	0.703944
-35.148738	-2.023717	1.521459	0.006709	0.703957
-34.973718	-2.077777	1.526464	0.006677	0.703910
-35.462651	-2.127587	1.531469	0.006768	0.703634
-35.626641	-2.096748	1.536474	0.006798	0.703637
-36.200431	-1.998415	1.541478	0.006905	0.703629
-35.349638	-2.146415	1.546483	0.006747	0.703637
-35.696820	-2.089142	1.551488	0.006811	0.703627
-36.166393	-2.001035	1.556493	0.006899	0.703636
-35.577965	-2.133355	1.561498	0.006789	0.703581
-36.196029	-2.144261	1.566502	0.006904	0.703336
-36.512407	-2.084629	1.571507	0.006963	0.703343
-36.795233	-2.037551	1.576512	0.007016	0.703336
-36.537651	-2.081683	1.581517	0.006968	0.703340
-36.481642	-2.091383	1.586522	0.006958	0.703340
-36.719561	-2.051694	1.591526	0.007002	0.703335
-36.373784	-2.179631	1.596531	0.006938	0.703201
-37.602605	-2.060701	1.601536	0.007166	0.702998
-37.675441	-2.045767	1.606541	0.007180	0.703002
-37.272821	-2.117268	1.611546	0.007105	0.703003
-37.444773	-2.088063	1.616550	0.007137	0.703000
-37.512125	-2.072368	1.621555	0.007149	0.703007
-37.780782	-2.030867	1.626560	0.007199	0.702994
-37.541674	-2.120704	1.631565	0.007155	0.702899
-38.270686	-2.094356	1.636570	0.007291	0.702690
-38.551726	-2.046780	1.641574	0.007343	0.702684
-38.519160	-2.048323	1.646579	0.007337	0.702693
-38.514814	-2.053563	1.651584	0.007336	0.702684
-38.613451	-2.033064	1.656589	0.007355	0.702690
-38.517569	-2.050184	1.661594	0.007337	0.702690
-38.553862	-2.047097	1.666598	0.007344	0.702683
-38.842553	-2.135596	1.671603	0.007397	0.702400
-39.441165	-2.049037	1.676608	0.007509	0.702359
-39.237541	-2.081237	1.681613	0.007471	0.702367
-39.196692	-2.089008	1.686618	0.007463	0.702366
-39.577331	-2.022744	1.691622	0.007534	0.702363
-39.051156	-2.114040	1.696627	0.007436	0.702368
-39.108046	-2.108591	1.701632	0.007447	0.702359
-40.203022	-2.056535	1.706637	0.007651	0.702069
-40.013038	-2.088737	1.711642	0.007615	0.702072
-40.102473	-2.077405	1.716646	0.007632	0.702063
-39.919665	-2.106629	1.721651	0.007598	0.702070
-40.191937	-2.060419	1.726656	0.007649	0.702065
-39.929146	-2.104369	1.731661	0.007600	0.702071
-39.868533	-2.157802	1.736666	0.007589	0.701985
-41.295681	-2.025062	1.741670	0.007854	0.701738
-40.735073	-2.120653	1.746675	0.007750	0.701747
-40.746686	-2.122695	1.751680	0.007752	0.701739
-40.905454	-2.092170	1.756685	0.007782	0.701743
-41.015412	-2.071931	1.761690	0.007802	0.701745
-41.218925	-2.040063	1.766694	0.007840	0.701736
-40.715447	-2.183860	1.771699	0.007746	0.701626
-41.877747	-2.072485	1.776704	0.007963	0.701432
-41.845145	-2.075161	1.781709	0.007957	0.701438
-41.518084	-2.133736	1.786714	0.007896	0.701438
-42.164392	-2.022213	1.791718	0.008016	0.701430
-41.519763	-2.132675	1.796723	0.007896	0.701439
-41.701326	-2.103484	1.801728	0.007930	0.701433
-42.075078	-2.138203	1.806733	0.008000	0.701228
-42.792475	-2.062443	1.811738	0.008133	0.701122
-42.637966	-2.092023	1.816742	0.008105	0.701118
-42.401258	-2.128669	1.821747	0.008061	0.701129
-42.986629	-2.029973	1.826752	0.008169	0.701117
-42.389059	-2.133820	1.831757	0.008058	0.701123
-42.071696	-2.193982	1.836762	0.007999	0.701116
-43.301242	-2.097078	1.841766	0.008228	0.700868
-43.329876	-2.086371	1.846771	0.008233	0.700879
-43.372125	-2.083483	1.851776	0.008241	0.700870
-43.150126	-2.119743	1.856781	0.008200	0.700876
-43.099455	-2.130421	1.861786	0.008191	0.700873
-43.318538	-2.093379	1.866790	0.008231	0.700869
-43.303197	-2.206370	1.871795	0.008229	0.700645
-44.300950	-2.086340	1.876800	0.008414	0.700528
-44.260045	-2.091039	1.881805	0.008407	0.700533
-43.686274	-2.190765	1.886810	0.008300	0.700539
-44.374865	-2.071111	1.891814	0.008428	0.700532
-43.971223	-2.140228	1.896819	0.008353	0.700538
-43.876881	-2.210206	1.901824	0.008336	0.700430
-45.244579	-2.071635	1.906829	0.008590	0.700216
-44.758715	-2.156957	1.911834	0.008500	0.700219
-45.053557	-2.106825	1.916838	0.008555	0.700214
-45.140521	-2.086837	1.921843	0.008571	0.700223
-45.310695	-2.060207	1.926848	0.008603	0.700216
-45.138011	-2.089949	1.931853	0.008570	0.700218
-44.675290	-2.256569	1.936858	0.008484	0.700047
-46.112928	-2.077804	1.941862	0.008752	0.699890
-45.895042	-2.112031	1.946867	0.008711	0.699899
-45.708750	-2.150470	1.951872	0.008677	0.699888
-46.025434	-2.092940	1.956877	0.008736	0.699890
-45.985456	-2.098785	1.961882	0.008728	0.699893
-46.047574	-2.091000	1.966886	0.008740	0.699886
-46.103662	-2.191167	1.971891	0.008750	0.699663
-46.993976	-2.067286	1.976896	0.008916	0.699592
-46.897619	-2.082302	1.981901	0.008898	0.699596
-46.675976	-2.119662	1.986906	0.008857	0.699601
-47.193153	-2.031143	1.991910	0.008953	0.699593
-46.749954	-2.106977	1.996915	0.008871	0.699599
-46.969120	-2.112879	2.001920	0.008912	0.699508

-47.821559	-2.083206	2.011917	0.009070	0.699260
-47.764679	-2.090473	2.021914	0.009060	0.699265
-47.751197	-2.092501	2.031910	0.009057	0.699266
-48.010893	-2.046232	2.041907	0.009106	0.699266
-47.778012	-2.088505	2.051904	0.009062	0.699264
-47.932573	-2.060333	2.061901	0.009091	0.699266
-47.743494	-2.094447	2.071898	0.009056	0.699265
-47.674013	-2.106270	2.081894	0.009043	0.699266
-47.842958	-2.077418	2.091891	0.009075	0.699263
-47.118467	-2.061039	2.101888	0.008940	0.699559
-47.037066	-2.057240	2.111885	0.008925	0.699596
-46.721120	-2.112940	2.121882	0.008866	0.699597
-47.010482	-2.061574	2.131878	0.008920	0.699597
-47.061567	-2.051587	2.141875	0.008929	0.699598
-46.945768	-2.074211	2.151872	0.008908	0.699594
-46.954827	-2.023554	2.161869	0.008909	0.699694
-45.985870	-2.098591	2.171866	0.008729	0.699892
-46.068848	-2.082415	2.181862	0.008745	0.699895
-46.092946	-2.078049	2.191859	0.008749	0.699895
-46.143340	-2.070688	2.201856	0.008758	0.699891
-45.575706	-2.030663	2.211853	0.008653	0.700178
-45.217137	-2.074195	2.221850	0.008586	0.700219
-45.389255	-2.043856	2.231846	0.008618	0.700219
-45.210718	-2.076975	2.241843	0.008585	0.700216
-44.568429	-2.040786	2.251840	0.008465	0.700521
-44.292987	-2.084632	2.261837	0.008414	0.700532
-44.115262	-2.116643	2.271834	0.008381	0.700531
-44.457840	-2.039522	2.281830	0.008445	0.700564
-43.444094	-2.069069	2.291827	0.008256	0.700870
-43.375921	-2.081659	2.301824	0.008243	0.700869
-43.401846	-2.076273	2.311821	0.008248	0.700871
-43.170060	-2.092388	2.321818	0.008205	0.700922
-42.719846	-2.075267	2.331814	0.008121	0.701119
-42.411596	-2.129819	2.341811	0.008064	0.701120
-42.741309	-2.073154	2.351808	0.008125	0.701115
-42.195303	-2.080303	2.361805	0.008024	0.701298
-41.837656	-2.076615	2.371802	0.007957	0.701435
-41.792968	-2.082701	2.381798	0.007949	0.701438
-41.788054	-2.050964	2.391795	0.007948	0.701504
-41.159134	-2.047200	2.401792	0.007831	0.701739
-41.204298	-2.038730	2.411789	0.007839	0.701740
-40.810490	-2.108342	2.421786	0.007766	0.701741
-40.551888	-2.000098	2.431782	0.007718	0.702053
-39.843032	-2.117345	2.441779	0.007586	0.702071
-40.384325	-2.021067	2.451776	0.007687	0.702071
-39.668608	-2.063986	2.461773	0.007554	0.702242
-39.366253	-2.055172	2.471770	0.007497	0.702369
-39.220834	-2.080066	2.481766	0.007470	0.702371
-39.259895	-2.051306	2.491763	0.007478	0.702415
-38.625796	-2.027339	2.501760	0.007360	0.702692
-38.362331	-2.074557	2.511757	0.007311	0.702691
-38.604060	-2.030343	2.521754	0.007356	0.702693
-37.868112	-2.033840	2.531750	0.007219	0.702951
-37.589474	-2.055942	2.541747	0.007167	0.703007
-37.836399	-2.014091	2.551744	0.007213	0.703003
-37.260000	-2.041835	2.561741	0.007105	0.703154
-36.631731	-2.062008	2.571738	0.006989	0.703339
-36.565790	-2.072342	2.581734	0.006976	0.703342
-36.620557	-2.063941	2.591731	0.006987	0.703339
-36.140013	-2.022314	2.601728	0.006897	0.703596
-35.954665	-2.037941	2.611725	0.006863	0.703631
-35.739516	-2.074682	2.621722	0.006823	0.703635
-35.553152	-2.035911	2.631718	0.006788	0.703780
-35.044482	-2.042537	2.641715	0.006693	0.703949
-35.025810	-2.046650	2.651712	0.006690	0.703948
-35.045020	-2.030834	2.661709	0.006693	0.703973
-34.295037	-2.024212	2.671706	0.006554	0.704256
-33.954202	-2.084056	2.681702	0.006490	0.704257
-34.119458	-2.054408	2.691699	0.006521	0.704258
-33.753194	-2.020654	2.701696	0.006453	0.704457
-33.181878	-2.059381	2.711693	0.006347	0.704584
-33.273439	-2.041864	2.721690	0.006364	0.704587
-33.097379	-2.057902	2.731686	0.006331	0.704618
-32.550746	-2.021988	2.741683	0.006229	0.704886
-32.425732	-2.044982	2.751680	0.006206	0.704885
-32.404164	-2.049263	2.761677	0.006202	0.704884
-31.859549	-2.031838	2.771674	0.006101	0.705114
-31.182867	-2.104811	2.781670	0.005975	0.705210
-31.518979	-2.046493	2.791667	0.006037	0.705207
-31.285542	-2.084662	2.801664	0.005994	0.705214
-30.675066	-2.041558	2.811661	0.005880	0.705520
-30.636589	-2.047455	2.821658	0.005873	0.705521
-30.580166	-2.057756	2.831654	0.005863	0.705521
-30.236754	-2.015734	2.841651	0.005799	0.705728
-29.601525	-2.064367	2.851648	0.005680	0.705858
-29.658955	-2.053283	2.861645	0.005691	0.705860
-29.651667	-2.052920	2.871642	0.005690	0.705863
-28.752985	-2.081801	2.881638	0.005522	0.706127
-29.023256	-2.033631	2.891635	0.005573	0.706127
-28.862983	-2.063143	2.901632	0.005543	0.706125
-28.540525	-2.036500	2.911629	0.005483	0.706294
-28.100358	-2.041630	2.921626	0.005401	0.706442
-28.018416	-2.056518	2.931622	0.005386	0.706441
-28.155867	-1.986325	2.941619	0.005411	0.706533
-26.797207	-2.121575	2.951616	0.005159	0.706747
-27.368712	-2.019828	2.961613	0.005265	0.706747
-26.947771	-2.093314	2.971610	0.005187	0.706750
-26.419375	-2.075198	2.981606	0.005088	0.706976
-26.418494	-2.023320	2.991603	0.005088	0.707080
-26.190266	-2.066385	3.001600	0.005046	0.707075
-26.288135	-2.017922	3.011597	0.005064	0.707137
-25.283691	-2.080153	3.021594	0.004877	0.707372
-25.250613	-2.084500	3.031590	0.004871	0.707375
-25.656600	-2.013234	3.041587	0.004946	0.707373
-24.760203	-2.046228	3.051584	0.004780	0.707627
-24.759337	-2.013235	3.061581	0.004779	0.707693
-24.204169	-2.110366	3.071578	0.004676	0.707697
-24.390131	-2.030352	3.081574	0.004711	0.707791
-23.516225	-2.077888	3.091571	0.004548	0.708008
-23.686091	-2.047231	3.101568	0.004580	0.708009
-23.722724	-2.039463	3.111565	0.004587	0.708011
-23.025807	-2.035918	3.121562	0.004457	0.708267
-22.878204	-2.022416	3.131558	0.004429	0.708347
-22.882524	-2.020837	3.141555	0.004430	0.708348
-22.431568	-2.052582	3.151552	0.004346	0.708446
-21.996212	-2.035227	3.161549	0.004265	0.708636
-21.786167	-2.072321	3.171546	0.004226	0.708636
-21.979968	-2.037282	3.181542	0.004262	0.708637
-21.194042	-2.037805	3.191539	0.004116	0.708917
-21.243009	-2.010897	3.201536	0.004125	0.708953
-21.076219	-2.039812	3.211533	0.004094	0.708955
-20.771425	-2.017857	3.221530	0.004037	0.709107
-20.144885	-2.051898	3.231526	0.003921	0.709263
-20.274174	-2.027654	3.241523	0.003945	0.709265
-20.267740	-2.015375	3.251520	0.003944	0.709292
-19.488586	-2.002594	3.261517	0.003799	0.709595
-19.052811	-2.081321	3.271514	0.003718	0.709593
-19.440684	-2.012126	3.281510	0.003790	0.709593
-18.901795	-2.015752	3.291507	0.003689	0.709778
-18.241789	-2.078935	3.301504	0.003567	0.709886
-18.302521	-2.067730	3.311501	0.003578	0.709887
-18.242762	-2.077803	3.321498	0.003567	0.709888
-17.703767	-2.028340	3.331494	0.003466	0.710179
-17.586850	-2.031430	3.341491	0.003445	0.710214
-17.459728	-2.054367	3.351488	0.003421	0.710214
-17.419087	-2.002011	3.361485	0.003414	0.710333
-16.315569	-2.099852	3.371482	0.003208	0.710530
-16.657706	-2.039282	3.381478	0.003272	0.710529
-16.624065	-2.044973	3.391475	0.003266	0.710530
-16.095050	-1.995313	3.401472	0.003167	0.710817
-15.881008	-2.009038	3.411469	0.003127	0.710866
-15.639332	-2.051175	3.421466	0.003082	0.710868
-15.388702	-2.045695	3.431462	0.003036	0.710968
-14.683370	-2.085990	3.441459	0.002904	0.711138
-14.914700	-2.046030	3.451456	0.002948	0.711135
-15.055634	-2.021081	3.461453	0.002974	0.711135
-14.075754	-2.057390	3.471450	0.002791	0.711411
-14.163327	-2.020167	3.481446	0.002808	0.711454
-13.847953	-2.076609	3.491443	0.002749	0.711453
-14.146662	-1.957364	3.501440	0.002805	0.711585
-13.054119	-2.065163	3.511437	0.002601	0.711758
-13.084621	-2.057150	3.521434	0.002607	0.711763
-13.265634	-2.026081	3.531430	0.002641	0.711761
-12.367319	-2.022269	3.541427	0.002473	0.712087
-12.227006	-2.048888	3.551424	0.002447	0.712084
-12.072896	-2.076985	3.561421	0.002419	0.712083
-12.030115	-2.020060	3.571418	0.002411	0.712211
-11.382015	-2.049558	3.581414	0.002290	0.712383
-11.459638	-2.036246	3.591411	0.002305	0.712382
-11.482904	-2.034072	3.601408	0.002309	0.712378
-10.519967	-2.044366	3.611405	0.002130	0.712699
-10.447085	-2.055477	3.621402	0.002116	0.712702
-10.498841	-2.045676	3.631398	0.002126	0.712703
-10.269626	-2.013822	3.641395	0.002083	0.712848
-9.758716	-2.020048	3.651392	0.001988	0.713017
-9.505546	-2.065637	3.661389	0.001941	0.713016
-9.616919	-2.044271	3.671386	0.001962	0.713019
-8.683375	-2.051172	3.681382	0.001788	0.713336
-8.700225	-2.038317	3.691379	0.001791	0.713355
-8.681113	-2.041653	3.701376	0.001788	0.713356
-8.734537	-1.986289	3.711373	0.001798	0.713447
-7.774866	-2.056904	3.721370	0.001619	0.713646
-7.497806	-2.105450	3.731366	0.001567	0.713648
-7.570433	-2.092481	3.741363	0.001581	0.713648
-7.341470	-2.037831	3.751360	0.001538	0.713837
-6.611364	-2.104295	3.761357	0.001402	0.713964
-7.152902	-2.006209	3.771354	0.001503	0.713967
-6.778871	-2.067588	3.781350	0.001434	0.713977
-6.135805	-2.032141	3.791347	0.001314	0.714275
-5.829577	-2.087691	3.801344	0.001257	0.714273
-5.756051	-2.099934	3.811341	0.001243	0.714275
-5.848804	-2.023650	3.821338	0.001261	0.714394
-4.755728	-2.110677	3.831334	0.001057	0.714607
-4.920423	-2.082368	3.841331	0.001088	0.714605
-4.973153	-2.075424	3.851328	0.001098	0.714600
-4.464022	-2.062951	3.861325	0.001003	0.714805
-3.971289	-2.102150	3.871322	0.000911	0.714901
-3.900976	-2.113032	3.881318	0.000898	0.714905
-4.033572	-2.089655	3.891315	0.000923	0.714904
-3.388042	-2.061133	3.901312	0.000803	0.715189
-3.233734	-2.068578	3.911309	0.000774	0.715228
-3.024450	-2.105635	3.921306	0.000735	0.715229
-3.046119	-2.054935	3.931302	0.000739	0.715322
-2.401765	-2.057214	3.941299	0.000619	0.715545
-1.998376	-2.131134	3.951296	0.000544	0.715541
-2.226789	-2.089783	3.961293	0.000587	0.715542
-2.078559	-2.003408	3.971290	0.000559	0.715765
-1.580050	-2.033190	3.981286	0.000466	0.715882
-1.681588	-2.013415	3.991283	0.000485	0.715886
-1.201098	-2.046169	4.001280	0.000396	0.715990
-1.249068	-1.968562	4.011277	0.000405	0.716127
-1.337503	-1.952147	4.021274	0.000421	0.716128
-1.062416	-1.905557	4.031270	0.000370	0.716317
-1.059544	-1.840488	4.041267	0.000369	0.716447
-1.092023	-1.803096	4.051264	0.000375	0.716510
-0.829315	-1.726215	4.061261	0.000327	0.716755
-0.861605	-1.714787	4.071258	0.000333	0.716766
-0.914271	-1.544197	4.081254	0.000342	0.717085
-0.479454	-1.610597	4.091251	0.000261	0.717106
-0.748252	-1.426923	4.101248	0.000311	0.717375
-0.285339	-1.466189	4.111245	0.000225	0.717460
-0.484629	-1.307995	4.121242	0.000262	0.717703
-0.597769	-1.193068	4.131238	0.000283	0.717890
-0.153465	-1.205252	4.141235	0.000201	0.718022
-0.242157	-1.023845	4.151232	0.000217	0.718349
-0.297424	-0.935963	4.161229	0.000227	0.718503
-0.163288	-0.868139	4.171226	0.000202	0.718684
-0.350215	-0.694752	4.181222	0.000237	0.718961
-0.040258	-0.621256	4.191219	0.000179	0.719215
-0.251329	-0.461620	4.201216	0.000219	0.719455
0.176046	-0.414139	4.211213	0.000139	0.719699
0.163314	-0.288394	4.221210	0.000141	0.719942
0.249766	-0.160354	4.231206	0.000125	0.720225
-0.018702	0.042817	4.241203	0.000175	0.720531
0.000000	0.197020	4.251200	0.000171	0.720841

0.087893	0.789648	4.256205	0.000155	0.722037
0.372333	2.011078	4.261210	0.000101	0.724531
0.616721	3.820069	4.266214	0.000054	0.728149
1.093193	6.160027	4.271219	-0.000036	0.732858
1.201945	9.055694	4.276224	-0.000058	0.738479
1.610000	12.384709	4.281229	-0.000136	0.744984
2.039925	16.168141	4.286234	-0.000219	0.752298
2.406673	20.360315	4.291238	-0.000290	0.760283
2.860204	24.945147	4.296243	-0.000377	0.768938
3.268780	29.899214	4.301248	-0.000456	0.778155
4.588209	35.046180	4.306253	-0.000705	0.787902
6.165011	40.487605	4.311258	-0.001003	0.798134
7.088328	46.351272	4.316262	-0.001178	0.808774
7.838022	52.542445	4.321267	-0.001322	0.819788
8.672624	58.984617	4.326272	-0.001481	0.831111
9.884770	65.598931	4.331277	-0.001711	0.842682
10.618892	72.517319	4.336282	-0.001853	0.854461
11.722580	79.582713	4.341286	-0.002063	0.866427
12.443565	86.914170	4.346291	-0.002202	0.878550
13.083390	94.416983	4.351296	-0.002326	0.890757
14.060137	102.027009	4.356301	-0.002513	0.903061
15.077910	109.785082	4.361306	-0.002707	0.915438
15.857277	117.692192	4.366310	-0.002857	0.927814
16.894945	125.694158	4.371315	-0.003056	0.940238
17.972238	133.787046	4.376320	-0.003262	0.952645
18.984488	141.991688	4.381325	-0.003455	0.965040
19.923119	150.286943	4.386330	-0.003636	0.977389
20.925062	158.657661	4.391334	-0.003828	0.989707
21.766307	167.099694	4.396339	-0.003990	1.001935
22.445069	175.588971	4.401344	-0.004122	1.014042
23.297169	184.101451	4.406349	-0.004286	1.026079
23.731804	192.720052	4.411354	-0.004372	1.038022
24.424887	201.308066	4.416358	-0.004507	1.049848
24.903483	209.964089	4.421363	-0.004602	1.061583
25.498299	218.617860	4.426368	-0.004718	1.073213
26.596149	227.185690	4.431373	-0.004928	1.084719
27.298364	235.845298	4.436378	-0.005064	1.096134
27.880442	244.507322	4.441382	-0.005178	1.107408
28.551211	253.173129	4.446387	-0.005309	1.118592
29.234447	261.814736	4.451392	-0.005442	1.129637
29.613630	270.519217	4.456397	-0.005518	1.140588
30.099401	279.214650	4.461402	-0.005614	1.151446
30.354566	287.907356	4.466406	-0.005667	1.162151
30.857385	296.543797	4.471411	-0.005767	1.172742
31.114550	305.195162	4.476416	-0.005820	1.183204
32.057822	313.740787	4.481421	-0.006001	1.193589
32.966524	322.267949	4.486426	-0.006176	1.203854
33.201559	330.914161	4.491430	-0.006225	1.214038
33.849949	339.469307	4.496435	-0.006352	1.224113
34.248875	348.068440	4.501440	-0.006432	1.234107
35.043880	356.556330	4.506445	-0.006585	1.243970
35.375187	365.124795	4.511450	-0.006652	1.253758
36.257854	373.575596	4.516454	-0.006822	1.263442
36.660097	382.128925	4.521459	-0.006903	1.273076
37.355437	390.572088	4.526464	-0.007038	1.282570
37.989842	399.053620	4.531469	-0.007161	1.292025
38.761626	407.495423	4.536474	-0.007310	1.301393
39.138764	416.055491	4.541478	-0.007386	1.310750
39.907443	424.529332	4.546483	-0.007535	1.320018
40.592653	432.907377	4.551488	-0.007668	1.329104
40.870821	441.379118	4.556493	-0.007725	1.338155
41.295391	449.780980	4.561498	-0.007810	1.347098
41.555592	458.220807	4.566502	-0.007864	1.355992
41.985982	466.606425	4.571507	-0.007949	1.364802
42.241299	475.024997	4.576512	-0.008002	1.373559
42.685250	483.392127	4.581517	-0.008090	1.382239
43.463267	491.710115	4.586522	-0.008241	1.390872
44.163521	500.031789	4.591526	-0.008376	1.399441
44.590326	508.386670	4.596531	-0.008461	1.407947
45.071627	516.736490	4.601536	-0.008556	1.416404
45.532356	525.065999	4.606541	-0.008648	1.424788
45.784352	533.435711	4.611546	-0.008700	1.433129
46.138411	541.756817	4.616550	-0.008771	1.441389
46.380638	550.106000	4.621555	-0.008822	1.449612
46.848410	558.394457	4.626560	-0.008914	1.457765
47.355785	566.675240	4.631565	-0.009014	1.465872
47.806805	575.014629	4.636570	-0.009104	1.473982
48.464448	583.242680	4.641574	-0.009231	1.481972
48.960353	591.517423	4.646579	-0.009329	1.489939
49.175974	599.825880	4.651584	-0.009375	1.497852
49.502526	608.099969	4.656589	-0.009441	1.505708
49.797554	616.393551	4.661594	-0.009501	1.513536
50.047611	624.654029	4.666598	-0.009553	1.521287
50.665546	632.879672	4.671603	-0.009673	1.529021
51.110077	641.119237	4.676608	-0.009762	1.536703
51.688808	649.348076	4.681613	-0.009875	1.544356
52.050372	657.625305	4.686618	-0.009947	1.551984
52.145574	665.902658	4.691622	-0.009970	1.559535
52.495118	674.127055	4.696627	-0.010041	1.567039
52.951424	682.348441	4.701632	-0.010131	1.574520
53.601681	690.528053	4.706637	-0.010258	1.581956
53.903023	698.771452	4.711642	-0.010319	1.589364
54.420200	706.977132	4.716646	-0.010421	1.596735
55.002661	715.169178	4.721651	-0.010534	1.604068
55.345437	723.394382	4.726656	-0.010604	1.611364
55.712895	731.627846	4.731661	-0.010677	1.618637
56.014490	739.836967	4.736666	-0.010739	1.625847
56.435701	748.103756	4.741670	-0.010823	1.633092
56.827588	756.301108	4.746675	-0.010901	1.640240
57.288166	764.456401	4.751680	-0.010992	1.647331
57.790979	772.657615	4.756685	-0.011091	1.654436
58.129816	780.843121	4.761690	-0.011159	1.661475
58.724480	789.004366	4.766694	-0.011275	1.668498
59.061723	797.226191	4.771699	-0.011344	1.675509
59.481001	805.381967	4.776704	-0.011427	1.682445
60.045593	813.547592	4.781709	-0.011537	1.689380
60.405949	821.741547	4.786714	-0.011610	1.696283
60.539745	829.948560	4.791718	-0.011640	1.703139
61.016340	838.127253	4.796723	-0.011734	1.709989
61.505561	846.298876	4.801728	-0.011831	1.716808
61.887390	854.463804	4.806733	-0.011907	1.723579
62.275851	862.622661	4.811738	-0.011985	1.730320
62.575980	870.803499	4.816742	-0.012046	1.737042
63.118769	878.949526	4.821747	-0.012152	1.743740
63.251270	887.147461	4.826752	-0.012182	1.750402
63.716051	895.305130	4.831757	-0.012274	1.757048
63.889048	903.478092	4.836762	-0.012311	1.763645
64.267236	911.625688	4.841766	-0.012387	1.770222
64.716935	919.794235	4.846771	-0.012476	1.776801
64.942368	927.946422	4.851776	-0.012524	1.783314
65.481053	936.100947	4.856781	-0.012629	1.789844
65.639416	944.330720	4.861786	-0.012664	1.796363
66.015258	952.427326	4.866790	-0.012739	1.802780
66.393488	960.565764	4.871795	-0.012815	1.809208
66.669805	968.712451	4.876800	-0.012872	1.815606
67.092652	976.828007	4.881805	-0.012956	1.821976
67.581711	984.948686	4.886810	-0.013052	1.828334
68.071274	993.091980	4.891814	-0.013148	1.834689
68.529153	1001.219544	4.896819	-0.013239	1.841005
68.866212	1009.349012	4.901824	-0.013307	1.847287
69.084777	1017.537732	4.906829	-0.013353	1.853578
69.392044	1025.672038	4.911834	-0.013416	1.859818
69.693897	1033.800236	4.916838	-0.013477	1.866031
70.180413	1041.960657	4.921843	-0.013573	1.872269
70.311155	1050.104439	4.926848	-0.013603	1.878433
70.747939	1058.201707	4.931853	-0.013689	1.884576
70.920608	1066.355979	4.936858	-0.013727	1.890713
71.250777	1074.479540	4.941862	-0.013793	1.896824
71.770986	1082.574147	4.946867	-0.013895	1.902915
72.025983	1090.706100	4.951872	-0.013948	1.908985
72.649469	1098.805265	4.956877	-0.014070	1.915052
73.018551	1106.905799	4.961882	-0.014144	1.921073
73.056191	1115.064687	4.966886	-0.014156	1.927080
73.600298	1123.178305	4.971891	-0.014262	1.933092
73.911964	1131.296435	4.976896	-0.014326	1.939063
74.106685	1139.426362	4.981901	-0.014367	1.945011
74.652819	1147.546684	4.986906	-0.014474	1.950973
75.155894	1155.658009	4.991910	-0.014573	1.956904
75.435334	1163.770962	4.996915	-0.014631	1.962795
75.522837	1171.886453	5.001920	-0.014652	1.968649
76.221122	1179.973743	5.006925	-0.014787	1.974531
76.362410	1188.096545	5.011930	-0.014819	1.980362
76.712666	1196.194345	5.016934	-0.014889	1.986179
77.409079	1204.284921	5.021939	-0.015024	1.992011
77.616691	1212.403243	5.026944	-0.015068	1.997794
77.941678	1220.506659	5.031949	-0.015134	2.003562
78.196137	1228.622007	5.036954	-0.015187	2.009314
78.513398	1236.737773	5.041958	-0.015251	2.015057
79.067863	1244.814959	5.046963	-0.015360	2.020781
79.196814	1252.940987	5.051968	-0.015389	2.026478
79.420760	1261.093266	5.056973	-0.015436	2.032188
79.928912	1269.168646	5.061978	-0.015536	2.037857
80.040085	1277.265568	5.066982	-0.015562	2.043485
80.504128	1285.357307	5.071987	-0.015653	2.049130
80.762668	1293.457231	5.076992	-0.015707	2.054743
81.032754	1301.557619	5.081997	-0.015762	2.060343
81.562477	1309.621136	5.087002	-0.015866	2.065929
81.930710	1317.739855	5.092006	-0.015940	2.071521
82.408271	1325.842891	5.097011	-0.016034	2.077097
82.408159	1333.954959	5.102016	-0.016039	2.082618
82.863429	1342.041703	5.107021	-0.016129	2.088152
83.431964	1350.131518	5.112026	-0.016241	2.093684
83.193971	1358.275405	5.117030	-0.016202	2.099159
83.744064	1366.336946	5.122035	-0.016309	2.104641
84.026816	1374.448602	5.127040	-0.016367	2.110117
84.324108	1382.597896	5.132045	-0.016428	2.115605
84.321261	1390.699828	5.137050	-0.016433	2.121018
84.694639	1398.731469	5.142054	-0.016507	2.126406
85.013406	1406.825023	5.147059	-0.016572	2.131817
85.237875	1414.900613	5.152064	-0.016619	2.137193
85.419930	1422.995009	5.157069	-0.016658	2.142564
85.600138	1431.089049	5.162074	-0.016697	2.147921
85.778809	1439.186567	5.167078	-0.016735	2.153267
86.019379	1447.280518	5.172083	-0.016786	2.158603
86.282645	1455.323194	5.177088	-0.016840	2.163894
86.458629	1463.421169	5.182093	-0.016878	2.169201
86.855988	1471.517221	5.187098	-0.016957	2.174513
87.228080	1479.557149	5.192102	-0.017032	2.179774
87.552306	1487.644065	5.197107	-0.017097	2.185048
87.582333	1495.766119	5.202112	-0.017108	2.190305
87.855777	1503.882004	5.207117	-0.017164	2.195568
88.012244	1511.951325	5.212122	-0.017199	2.200777
88.125210	1520.007587	5.217126	-0.017225	2.205962
88.443455	1528.093000	5.222131	-0.017289	2.211171
88.751358	1536.161533	5.227136	-0.017352	2.216357
88.947321	1544.245568	5.232141	-0.017394	2.221530
89.179538	1552.323130	5.237146	-0.017442	2.226691
89.389463	1560.413379	5.242150	-0.017487	2.231845
89.632045	1568.497446	5.247155	-0.017537	2.236986
89.854371	1576.551191	5.252160	-0.017584	2.242095
90.023820	1584.633581	5.257165	-0.017620	2.247206
90.678731	1592.672831	5.262170	-0.017748	2.252320
91.285548	1600.706645	5.267174	-0.017866	2.257415
91.554288	1608.796785	5.272179	-0.017921	2.262504
91.832022	1616.890337	5.277184	-0.017978	2.267584
92.173035	1625.029334	5.282189	-0.018047	2.272687
92.315374	1633.114105	5.287194	-0.018079	2.277727
92.579371	1641.159547	5.292198	-0.018133	2.282743
92.930610	1649.219678	5.297203	-0.018204	2.287763
92.903526	1657.318776	5.302208	-0.018204	2.292765
93.299163	1665.373604	5.307213	-0.018283	2.297764
93.635092	1673.421691	5.312218	-0.018350	2.302743
93.735698	1681.496551	5.317222	-0.018374	2.307708
94.187787	1689.575695	5.322227	-0.018464	2.312695
94.697325	1697.612581	5.327232	-0.018564	2.317649
94.801859	1705.701072	5.332237	-0.018589	2.322591
95.344960	1713.739101	5.337242	-0.018695	2.327527
95.502047	1721.839169	5.342246	-0.018730	2.332459
95.850463	1729.923777	5.347251	-0.018800	2.337387
96.029250	1737.976631	5.352256	-0.018838	2.342271
96.279369	1746.042451	5.357261	-0.018890	2.347159
96.577062	1754.161640	5.362266	-0.018951	2.352072
96.773167	1762.217880	5.367270	-0.018992	2.356929
97.127401	1770.254940	5.372275	-0.019064	2.361777
97.476253	1778.289645	5.377280	-0.019134	2.366614
97.891751	1786.343832	5.382285	-0.019216	2.371457
98.559291	1794.388236	5.387290	-0.019346	2.376305
98.530402	1802.477322	5.392294	-0.019346	2.381114
99.062879	1810.532522	5.397299	-0.019450	2.385938
99.399025	1818.613781	5.402304	-0.019518	2.390751
99.600146	1826.700531	5.407309	-0.019561	2.395548
100.043013	1834.747537	5.412314	-0.019648	2.400330
100.088404	1842.821396	5.417318	-0.019662	2.405088
100.310893	1850.914575	5.422323	-0.019709	2.409861
100.723752	1858.966694	5.427328	-0.019791	2.414616
100.706725	1867.057288	5.432333	-0.019793	2.419350
101.093340	1875.092608	5.437338	-0.019870	2.424074
101.331528	1883.159743	5.442342	-0.019920	2.428795
101.724544	1891.306613	5.447347	-0.019998	2.433566
101.757824	1899.371350	5.452352	-0.020010	2.438252
101.756698	1907.421120	5.457357	-0.020015	2.442918
102.025595	1915.455107	5.462362	-0.020070	2.447586
102.216170	1923.501098	5.467366	-0.020111	2.452247
102.546698	1931.553940	5.472371	-0.020178	2.456913
102.673892	1939.590529	5.477376	-0.020206	2.461545
102.951023	1947.637446	5.482381	-0.020263	2.466186
103.231510	1955.709630	5.487386	-0.020321	2.470833
103.321892	1963.796022	5.492390	-0.020343	2.475465
103.564416	1971.849915	5.497395	-0.020393	2.480081
103.829575	1979.847762	5.502400	-0.020448	2.484658
103.951027	1987.930821	5.507405	-0.020476	2.489264
104.328790	1996.015552	5.512410	-0.020551	2.493882
104.652009	2004.027174	5.517414	-0.020617	2.498446
104.934902	2012.087592	5.522419	-0.020675	2.503026
105.277768	2020.155781	5.527424	-0.020744	2.507606
105.652301	2028.233483	5.532429	-0.020819	2.512186
105.869697	2036.318596	5.537434	-0.020864	2.516750
105.888748	2044.342987	5.542438	-0.020873	2.521257
106.183871	2052.402681	5.547443	-0.020933	2.525796
106.469211	2060.454582	5.552448	-0.020992	2.530321
106.504146	2068.544128	5.557453	-0.021003	2.534842
106.762803	2076.577006	5.562458	-0.021057	2.539338
107.097999	2084.609769	5.567462	-0.021124	2.543833
107.265420	2092.689824	5.572467	-0.021161	2.548333
107.259878	2100.766233	5.577472	-0.021165	2.552811
107.471232	2108.816628	5.582477	-0.021210	2.557283
107.747869	2116.843583	5.587482	-0.021266	2.561738
107.887535	2124.892941	5.592486	-0.021298	2.566188
108.260435	2132.939411	5.597491	-0.021372	2.570645
108.586839	2140.991732	5.602496	-0.021438	2.575094
108.866326	2149.039037	5.607501	-0.021496	2.579530
109.213112	2157.082221	5.612506	-0.021565	2.583960
109.371232	2165.143380	5.617510	-0.021600	2.588379
109.788461	2173.339362	5.622515	-0.021683	2.592882
109.846119	2181.416793	5.627520	-0.021699	2.597288
110.215387	2189.383797	5.632525	-0.021773	2.601648
110.500709	2197.403334	5.637530	-0.021831	2.606023
110.496866	2205.456669	5.642534	-0.021836	2.610390
110.783999	2213.508695	5.647539	-0.021895	2.614768
111.254162	2221.504280	5.652544	-0.021987	2.619120
111.434674	2229.537750	5.657549	-0.022026	2.623467
111.590068	2237.610969	5.662554	-0.022060	2.627825
111.715589	2245.678140	5.667558	-0.022089	2.632172
112.023956	2253.726583	5.672563	-0.022152	2.636513
112.771551	2261.685156	5.677568	-0.022296	2.640828
113.171511	2269.739919	5.682573	-0.022376	2.645164
113.447320	2277.782726	5.687578	-0.022432	2.649478
113.756120	2285.862602	5.692582	-0.022495	2.653807
113.991548	2293.932563	5.697587	-0.022544	2.658120
114.153384	2301.980089	5.702592	-0.022579	2.662408
114.312664	2310.046893	5.707597	-0.022614	2.666699
114.365228	2318.133297	5.712602	-0.022629	2.670988
114.982938	2326.149881	5.717606	-0.022750	2.675268
115.043039	2334.197637	5.722611	-0.022766	2.679522
115.091490	2342.235344	5.727616	-0.022780	2.683764
115.460278	2350.258930	5.732621	-0.022854	2.688012
115.876003	2358.308191	5.737626	-0.022937	2.692269
116.031976	2366.363654	5.742630	-0.022971	2.696507
116.158321	2374.429491	5.747635	-0.023000	2.700741
116.455101	2382.449964	5.752640	-0.023060	2.704956
116.670237	2390.514453	5.757645	-0.023106	2.709182
116.839403	2398.595376	5.762650	-0.023142	2.713407
117.004665	2406.635464	5.767654	-0.023178	2.717604
117.340208	2414.670161	5.772659	-0.023246	2.721802
117.443279	2422.709058	5.777664	-0.023270	2.725981
117.617980	2430.739177	5.782669	-0.023308	2.730154
118.100116	2438.800108	5.787674	-0.023403	2.734355
118.208390	2446.845501	5.792678	-0.023429	2.738519
118.257145	2454.912678	5.797683	-0.023443	2.742684
118.620775	2462.939165	5.802688	-0.023516	2.746841
118.979436	2471.019310	5.807693	-0.023588	2.751019
119.321681	2479.133962	5.812698	-0.023657	2.755207
119.451339	2487.118007	5.817702	-0.023686	2.759309
119.928696	2495.140916	5.822707	-0.023780	2.763446
120.099257	2503.167479	5.827712	-0.023817	2.767560
119.940902	2511.237853	5.832717	-0.023793	2.771670
120.475479	2519.260001	5.837722	-0.023898	2.775791
120.590514	2527.282549	5.842726	-0.023924	2.779881
120.823848	2535.319807	5.847731	-0.023973	2.783980
121.253906	2543.330786	5.852736	-0.024058	2.788071
121.404682	2551.411472	5.857741	-0.024092	2.792174
121.597530	2559.470243	5.862746	-0.024133	2.796263
121.794326	2567.494091	5.867750	-0.024175	2.800329
122.207236	2575.490517	5.872755	-0.024257	2.804387
122.372232	2583.542848	5.877760	-0.024293	2.808453
122.543005	2591.621190	5.882765	-0.024330	2.812527
122.751580	2599.681503	5.887770	-0.024374	2.816587
122.875155	2607.711623	5.892774	-0.024402	2.820622
123.113225	2615.754553	5.897779	-0.024452	2.824664
123.250636	2623.806283	5.902784	-0.024482	2.828699
123.582565	2631.859282	5.907789	-0.024549	2.832740
123.991466	2639.904553	5.912794	-0.024631	2.836776
124.009784	2647.936295	5.917798	-0.024639	2.840776
124.413809	2655.945014	5.922803	-0.024720	2.844782
124.569847	2664.004050	5.927808	-0.024754	2.848793
124.542676	2672.071953	5.932813	-0.024754	2.852792
125.087561	2680.072052	5.937818	-0.024861	2.856784
125.283220	2688.105963	5.942822	-0.024903	2.860768
125.510261	2696.148920	5.947827	-0.024950	2.864752
125.740800	2704.183807	5.952832	-0.024998	2.868727
126.120226	2712.225961	5.957837	-0.025074	2.872708
126.522002	2720.282066	5.962842	-0.025154	2.876692
126.515166	2728.329707	5.967846	-0.025158	2.880643
126.743030	2736.350748	5.972851	-0.025206	2.884589
126.928162	2744.390852	5.977856	-0.025246	2.888537
127.227614	2752.441490	5.982861	-0.025307	2.892490
127.438098	2760.495275	5.987866	-0.025351	2.896435
127.654062	2768.536493	5.992870	-0.025396	2.900368
127.895330	2776.533996	5.997875	-0.025446	2.904276
128.348842	2784.576783	6.002880	-0.025536	2.908213
128.557758	2792.693053	6.007885	-0.025580	2.912166
128.699305	2800.798257	6.012890	-0.025612	2.916105
128.755919	2808.756792	6.017894	-0.025628	2.919963
129.221261	2816.746955	6.022899	-0.025720	2.923853
129.327952	2824.773035	6.027904	-0.025745	2.927736
129.549377	2832.829679	6.032909	-0.025791	2.931635
129.805828	2840.882980	6.037914	-0.025844	2.935529
130.089425	2848.886381	6.042918	-0.025902	2.939395
130.267490	2856.935997	6.047923	-0.025940	2.943272
130.477834	2864.951168	6.052928	-0.025985	2.947130
130.465398	2873.038232	6.057933	-0.025988	2.951005
130.556023	2881.099988	6.062938	-0.026010	2.954869
130.696326	2889.107521	6.067942	-0.026041	2.958704
131.316024	2897.113823	6.072947	-0.026162	2.962558
131.383384	2905.168630	6.077952	-0.026180	2.966402
131.692744	2913.176472	6.082957	-0.026242	2.970231
132.091810	2921.235795	6.087962	-0.026322	2.974083
132.303581	2929.258714	6.092966	-0.026367	2.977904
132.460526	2937.320959	6.097971	-0.026401	2.981736
132.630194	2945.340870	6.102976	-0.026438	2.985544
132.937121	2953.366428	6.107981	-0.026500	2.989356
133.332431	2961.447239	6.112986	-0.026579	2.993194
133.654328	2969.462334	6.117990	-0.026644	2.996992
134.088629	2977.473901	6.122995	-0.026730	3.000790
134.105997	2985.488743	6.128000	-0.026739	3.004563
134.317951	2993.541691	6.133005	-0.026783	3.008359
134.623831	3001.597051	6.138010	-0.026846	3.012156
134.737904	3009.643563	6.143014	-0.026872	3.015934
135.028734	3017.653700	6.148019	-0.026931	3.019700
135.009782	3025.705047	6.153024	-0.026933	3.023465
135.269329	3033.742044	6.158029	-0.026987	3.027232
135.730028	3041.782303	6.163034	-0.027078	3.031005
135.791175	3049.819395	6.168038	-0.027094	3.034753
136.284538	3057.835033	6.173043	-0.027191	3.038508
136.534296	3065.861886	6.178048	-0.027243	3.042250
136.713093	3073.900712	6.183053	-0.027282	3.045991
136.994968	3081.946969	6.188058	-0.027339	3.049735
137.052905	3090.014188	6.193062	-0.027355	3.053474
137.210436	3098.054753	6.198067	-0.027390	3.057200
137.415074	3106.076038	6.203072	-0.027433	3.060915
137.725133	3114.063886	6.208077	-0.027496	3.064616
138.063072	3122.117680	6.213082	-0.027564	3.068343
138.023057	3130.224758	6.218086	-0.027562	3.072072
138.298234	3138.309581	6.223091	-0.027619	3.075802
138.448335	3146.276243	6.228096	-0.027652	3.079467
138.621288	3154.293073	6.233101	-0.027689	3.083152
138.823990	3162.324761	6.238106	-0.027732	3.086840
139.097729	3170.330310	6.243110	-0.027788	3.090515
139.405546	3178.374913	6.248115	-0.027851	3.094205
139.593514	3186.390698	6.253120	-0.027891	3.097872
139.805967	3194.432125	6.258125	-0.027936	3.101548
140.052577	3202.448909	6.263130	-0.027987	3.105209
140.082550	3210.474299	6.268134	-0.027998	3.108861
140.497318	3218.542235	6.273139	-0.028080	3.112544
140.970738	3226.567282	6.278144	-0.028174	3.116207
141.068625	3234.578715	6.283149	-0.028197	3.119842
141.378711	3242.615056	6.288154	-0.028260	3.123493
141.644606	3250.638398	6.293158	-0.028315	3.127132
141.888125	3258.692810	6.298163	-0.028365	3.130780
141.986794	3266.768967	6.303168	-0.028389	3.134428
142.350215	3274.761942	6.308173	-0.028462	3.138045
142.743098	3282.798918	6.313178	-0.028540	3.141679
142.726152	3290.819594	6.318182	-0.028542	3.145283
142.980784	3298.868796	6.323187	-0.028595	3.148908
143.223401	3306.933459	6.328192	-0.028645	3.152535
143.393237	3314.972794	6.333197	-0.028682	3.156144
143.505265	3322.982364	6.338202	-0.028708	3.159732
143.682527	3330.969601	6.343206	-0.028746	3.163309
143.848610	3339.037037	6.348211	-0.028782	3.166918
144.128895	3347.028453	6.353216	-0.028840	3.170493
144.349995	3355.088055	6.358221	-0.028886	3.174092
144.698562	3363.117957	6.363226	-0.028956	3.177679
144.706581	3371.158230	6.368230	-0.028963	3.181252
144.833999	3379.175685	6.373235	-0.028992	3.184816
145.289890	3387.186230	6.378240	-0.029082	3.188387
145.460837	3395.260029	6.383245	-0.029119	3.191970
145.617641	3403.317508	6.388250	-0.029154	3.195541
145.778144	3411.291123	6.393254	-0.029189	3.199071
146.054162	3419.322813	6.398259	-0.029245	3.202628
146.090873	3427.372802	6.403264	-0.029257	3.206178
146.220345	3435.391044	6.408269	-0.029287	3.209715
146.587127	3443.452602	6.413274	-0.029360	3.213277
146.846599	3451.462315	6.418278	-0.029414	3.216807
147.070399	3459.502820	6.423283	-0.029461	3.220345
147.339552	3467.493885	6.428288	-0.029516	3.223860
147.373104	3475.559377	6.433293	-0.029527	3.227394
147.545573	3483.635747	6.438298	-0.029565	3.230934
147.722763	3491.684887	6.443302	-0.029603	3.234459
148.145794	3499.674943	6.448307	-0.029687	3.237964
148.306140	3507.686086	6.453312	-0.029722	3.241464
148.598229	3515.665796	6.458317	-0.029782	3.244952
148.960207	3523.700185	6.463322	-0.029854	3.248462
149.133949	3531.731352	6.468326	-0.029892	3.251959
149.014817	3539.830602	6.473331	-0.029875	3.255471
149.303844	3547.809570	6.478336	-0.029934	3.258943
149.614533	3555.826933	6.483341	-0.029997	3.262429
149.780828	3563.878512	6.488346	-0.030033	3.265920
149.784601	3571.911723	6.493350	-0.030039	3.269393
150.231470	3579.958685	6.498355	-0.030128	3.272885
150.339958	3588.014095	6.503360	-0.030153	3.276364
150.607366	3595.979622	6.508365	-0.030208	3.279807
150.876220	3604.003595	6.513370	-0.030263	3.283272
151.072382	3612.039841	6.518374	-0.030305	3.286735
151.435793	3620.057955	6.523379	-0.030378	3.290193
151.579462	3628.121923	6.528384	-0.030410	3.293659
151.725398	3636.155635	6.533389	-0.030442	3.297108
151.978668	3644.189684	6.538394	-0.030495	3.300558
151.923933	3652.191145	6.543398	-0.030490	3.303979
152.324157	3660.211486	6.548403	-0.030569	3.307421
152.332616	3668.286944	6.553408	-0.030576	3.310868
152.531315	3676.328303	6.558413	-0.030618	3.314305
152.741602	3684.348485	6.563418	-0.030663	3.317729
152.911136	3692.350566	6.568422	-0.030699	3.321140
153.074211	3700.338017	6.573427	-0.030735	3.324542
153.189677	3708.401918	6.578432	-0.030762	3.327970
153.351357	3716.439951	6.583437	-0.030797	3.331386
153.766585	3724.466317	6.588442	-0.030880	3.334803
153.763433	3732.475710	6.593446	-0.030884	3.338193
154.112871	3740.500171	6.598451	-0.030955	3.341600
154.400985	3748.530197	6.603456	-0.031013	3.345003
154.313033	3756.579732	6.608461	-0.031002	3.348397
154.381334	3764.657203	6.613466	-0.031020	3.351805
154.702592	3772.660257	6.618470	-0.031085	3.355187
155.005538	3780.682034	6.623475	-0.031147	3.358573
155.278822	3788.678939	6.628480	-0.031203	3.361944
155.507479	3796.675193	6.633485	-0.031251	3.365310
155.697649	3804.750627	6.638490	-0.031291	3.368704
155.889158	3812.795428	6.643494	-0.031332	3.372082
156.319830	3820.829494	6.648499	-0.031418	3.375461
156.556754	3828.840502	6.653504	-0.031467	3.378820
156.412125	3836.866564	6.658509	-0.031445	3.382168
156.655706	3844.880367	6.663514	-0.031496	3.385521
156.790329	3852.905449	6.668518	-0.031526	3.388872
157.110472	3860.987397	6.673523	-0.031591	3.392249
157.259179	3869.064203	6.678528	-0.031624	3.395616
157.577218	3876.998895	6.683533	-0.031688	3.398925
157.778842	3885.012894	6.688538	-0.031731	3.402260
157.880376	3893.030419	6.693542	-0.031755	3.405590
158.128998	3901.048866	6.698547	-0.031807	3.408923
158.485400	3909.074621	6.703552	-0.031878	3.412258
158.645520	3917.142804	6.708557	-0.031913	3.415601
158.945436	3925.135605	6.713562	-0.031974	3.418914
159.067053	3933.156319	6.718566	-0.032002	3.422230
159.113282	3941.196384	6.723571	-0.032016	3.425548
159.280897	3949.203980	6.728576	-0.032052	3.428853
159.399070	3957.258343	6.733581	-0.032080	3.432173
159.716945	3965.292087	6.738586	-0.032144	3.435487
159.525988	3973.302265	6.743590	-0.032114	3.438772
159.908695	3981.342588	6.748595	-0.032190	3.442085
160.267776	3989.340205	6.753600	-0.032262	3.445377
160.378295	3997.358148	6.758605	-0.032288	3.448665
160.701584	4005.413167	6.763610	-0.032353	3.451972
160.874277	4013.478276	6.768614	-0.032391	3.455276
161.267628	4021.475338	6.773619	-0.032469	3.458556
161.491929	4029.537365	6.778624	-0.032516	3.461853
161.607139	4037.498705	6.783629	-0.032543	3.465103
161.934432	4045.592515	6.788634	-0.032609	3.468410
161.976989	4053.604049	6.793638	-0.032622	3.471672
162.460999	4061.649545	6.798643	-0.032718	3.474958
162.657256	4069.614181	6.803648	-0.032759	3.478199
162.841623	4077.629617	6.808653	-0.032799	3.481458
162.882021	4085.647826	6.813658	-0.032812	3.484710
163.087883	4093.671335	6.818662	-0.032855	3.487966
163.299228	4101.752188	6.823667	-0.032900	3.491243
163.359596	4109.772197	6.828672	-0.032916	3.494487
163.688172	4117.780304	6.833677	-0.032983	3.497731
164.040560	4125.822794	6.838682	-0.033053	3.500988
164.025093	4133.787615	6.843686	-0.033056	3.504198
163.967616	4141.880097	6.848691	-0.033050	3.507455
164.517896	4149.884213	6.853696	-0.033158	3.510693
164.584527	4157.907621	6.858701	-0.033176	3.513921
164.812090	4165.969620	6.863706	-0.033223	3.517166
164.856136	4173.941161	6.868710	-0.033237	3.520366
165.069289	4181.977165	6.873715	-0.033281	3.523594
165.248739	4190.023995	6.878720	-0.033320	3.526822
165.164535	4198.024203	6.883725	-0.033310	3.530021
165.598871	4206.093053	6.888730	-0.033396	3.533260
165.598184	4214.124256	6.893734	-0.033401	3.536468
165.714654	4222.133560	6.898739	-0.033428	3.539668
166.080660	4230.154874	6.903744	-0.033501	3.542877
166.190266	4238.171537	6.908749	-0.033527	3.546074
166.406857	4246.228284	6.913754	-0.033572	3.549287
166.490527	4254.308657	6.918758	-0.033593	3.552502
166.772010	4262.361993	6.923763	-0.033651	3.555709
167.037063	4270.319292	6.928768	-0.033705	3.558875
167.207971	4278.321505	6.933773	-0.033742	3.562054
167.448094	4286.354211	6.938778	-0.033792	3.565243
167.347095	4294.362578	6.943782	-0.033779	3.568410
167.575670	4302.416164	6.948787	-0.033826	3.571602
167.840987	4310.417453	6.953792	-0.033881	3.574771
168.000468	4318.409980	6.958797	-0.033916	3.577931
168.217565	4326.441873	6.963802	-0.033962	3.581105
168.396891	4334.408449	6.968806	-0.034000	3.584249
168.721611	4342.473890	6.973811	-0.034066	3.587434
168.932612	4350.496130	6.978816	-0.034110	3.590596
168.944165	4358.536768	6.983821	-0.034118	3.593756
169.268827	4366.566717	6.988826	-0.034183	3.596918
169.320553	4374.555821	6.993830	-0.034198	3.600054
169.313705	4382.591974	6.998835	-0.034202	3.603204
169.594453	4390.619401	7.003840	-0.034260	3.606355
169.873703	4398.588637	7.008845	-0.034317	3.609482
170.140998	4406.687200	7.013850	-0.034372	3.612655
170.183396	4414.710593	7.018854	-0.034385	3.615790
170.357079	4422.702087	7.023859	-0.034422	3.618914
170.435615	4430.767352	7.028864	-0.034442	3.622061
170.531726	4438.743835	7.033869	-0.034465	3.625171
171.216990	4446.786234	7.038874	-0.034598	3.628320
171.367494	4454.828332	7.043878	-0.034631	3.631452
171.365169	4462.889704	7.048883	-0.034636	3.634584
171.616467	4470.899382	7.053888	-0.034688	3.637700
171.755488	4478.891621	7.058893	-0.034719	3.640804
172.108932	4486.901720	7.063898	-0.034790	3.643918
172.139781	4494.920094	7.068902	-0.034801	3.647024
172.285150	4502.958445	7.073907	-0.034834	3.650138
172.446661	4511.014745	7.078912	-0.034869	3.653256
172.366501	4519.057323	7.083917	-0.034859	3.656361
172.622847	4527.073258	7.088922	-0.034912	3.659461
172.863151	4535.050221	7.093926	-0.034962	3.662543
173.174447	4543.085147	7.098931	-0.035025	3.665646
173.407777	4551.138787	7.103936	-0.035074	3.668752
173.631446	4559.115555	7.108941	-0.035121	3.671826
173.879201	4567.179588	7.113946	-0.035172	3.674931
173.954732	4575.193758	7.118950	-0.035191	3.678010
174.094089	4583.221007	7.123955	-0.035223	3.681093
174.456274	4591.177477	7.128960	-0.035295	3.684152
174.679545	4599.211929	7.133965	-0.035342	3.687235
174.830693	4607.261249	7.138970	-0.035375	3.690319
175.049557	4615.271245	7.143974	-0.035421	3.693387
174.933999	4623.374599	7.148979	-0.035405	3.696479
175.371553	4631.324852	7.153984	-0.035492	3.699525
175.424764	4639.353674	7.158989	-0.035507	3.702588
175.793379	4647.359592	7.163994	-0.035581	3.705648
175.851710	4655.377706	7.168998	-0.035597	3.708702
176.150349	4663.458312	7.174003	-0.035658	3.711784
176.270290	4671.576221	7.179008	-0.035685	3.714872
176.104885	4679.520317	7.184013	-0.035660	3.717885
176.359223	4687.555761	7.189018	-0.035712	3.720941
176.541050	4695.447715	7.194022	-0.035751	3.723938
176.845336	4703.527902	7.199027	-0.035813	3.727006
176.842428	4711.538736	7.204032	-0.035818	3.730039
176.965074	4719.576202	7.209037	-0.035846	3.733082
177.171520	4727.649696	7.214042	-0.035889	3.736138
177.245458	4735.610056	7.219046	-0.035908	3.739146
177.456782	4743.655969	7.224051	-0.035953	3.742186
177.808451	4751.656651	7.229056	-0.036024	3.745211
177.738107	4759.690332	7.234061	-0.036016	3.748236
178.045362	4767.738489	7.239066	-0.036078	3.751272
177.942464	4775.768951	7.244070	-0.036064	3.754290
178.051453	4783.808511	7.249075	-0.036090	3.757313
178.380944	4791.776114	7.254080	-0.036156	3.760313
178.482418	4799.780906	7.259085	-0.036180	3.763318
178.689081	4807.859848	7.264090	-0.036224	3.766352
178.732546	4815.858653	7.269094	-0.036237	3.769349
179.024101	4823.916329	7.274099	-0.036297	3.772371
179.221659	4831.916991	7.279104	-0.036339	3.775368
179.243355	4839.933915	7.284109	-0.036348	3.778364
179.430830	4847.997404	7.289114	-0.036388	3.781379
179.842592	4855.932538	7.294118	-0.036470	3.784348
179.811134	4864.008744	7.299123	-0.036470	3.787358
179.798109	4872.035765	7.304128	-0.036472	3.790348
179.891818	4880.099690	7.309133	-0.036495	3.793351
180.196483	4888.105460	7.314138	-0.036557	3.796335
180.318907	4896.067938	7.319142	-0.036585	3.799297
180.472208	4904.089542	7.324147	-0.036619	3.802279
180.630709	4912.077646	7.329152	-0.036653	3.805246
180.530457	4920.108284	7.334157	-0.036640	3.808221
180.690884	4928.182215	7.339162	-0.036675	3.811215
180.987980	4936.176145	7.344166	-0.036736	3.814180
181.061536	4944.215578	7.349171	-0.036754	3.817155
181.130225	4952.223573	7.354176	-0.036772	3.820116
181.376824	4960.209805	7.359181	-0.036824	3.823071
181.563515	4968.238779	7.364186	-0.036864	3.826037
181.661636	4976.288460	7.369190	-0.036887	3.829007
181.791010	4984.293489	7.374195	-0.036916	3.831959
182.045544	4992.344301	7.379200	-0.036969	3.834928
182.158998	5000.343234	7.384205	-0.036995	3.837873
182.242253	5008.373864	7.389210	-0.037016	3.840826
182.511349	5016.332231	7.394214	-0.037071	3.843754
182.558822	5024.387512	7.399219	-0.037085	3.846712
182.830335	5032.426282	7.404224	-0.037141	3.849665
183.002137	5040.442806	7.409229	-0.037178	3.852606
183.273367	5048.502672	7.414234	-0.037234	3.855563
183.183404	5056.512842	7.419238	-0.037223	3.858491
183.355326	5064.554791	7.424243	-0.037260	3.861435
183.653772	5072.514789	7.429248	-0.037321	3.864348
183.605791	5080.570042	7.434253	-0.037317	3.867288
183.962567	5088.623904	7.439258	-0.037388	3.870232
184.026079	5096.812248	7.444262	-0.037406	3.873218
184.229774	5104.818406	7.449267	-0.037449	3.876138
184.279111	5112.748903	7.454272	-0.037463	3.879025
184.494151	5120.721094	7.459277	-0.037508	3.881928
184.697555	5128.687082	7.464282	-0.037551	3.884826
184.648192	5136.740551	7.469286	-0.037547	3.887749
184.825378	5144.749289	7.474291	-0.037586	3.890659
185.084617	5152.788188	7.479296	-0.037639	3.893578
185.023134	5160.805330	7.484301	-0.037633	3.896481
185.005429	5168.818365	7.489306	-0.037635	3.899381
185.171761	5176.851903	7.494310	-0.037671	3.902290
185.259589	5184.822166	7.499315	-0.037693	3.905173
185.582435	5192.857914	7.504320	-0.037758	3.908081
185.664602	5200.881106	7.509325	-0.037778	3.910979
185.900040	5208.938754	7.514330	-0.037827	3.913889
186.287495	5216.932295	7.519334	-0.037905	3.916777
186.307616	5224.942912	7.524339	-0.037914	3.919662
186.423068	5232.973679	7.529344	-0.037940	3.922554
186.379711	5240.931641	7.534349	-0.037938	3.925415
186.714744	5248.973593	7.539354	-0.038005	3.928310
186.804908	5256.991354	7.544358	-0.038027	3.931191
187.031678	5265.066503	7.549363	-0.038075	3.934092
187.138360	5273.057900	7.554368	-0.038100	3.936959
187.000402	5281.022908	7.559373	-0.038079	3.939810
187.391634	5289.079028	7.564378	-0.038157	3.942701
187.383976	5297.103340	7.569382	-0.038161	3.945571
187.494371	5305.126811	7.574387	-0.038187	3.948441
187.791612	5313.195094	7.579392	-0.038247	3.951328
187.782999	5321.226611	7.584397	-0.038251	3.954195
187.928071	5329.230211	7.589402	-0.038283	3.957052
187.931211	5337.186085	7.594406	-0.038289	3.959888
188.288745	5345.198953	7.599411	-0.038361	3.962748
188.409087	5353.251114	7.604416	-0.038388	3.965616
188.320718	5361.228710	7.609421	-0.038377	3.968452
188.674592	5369.295458	7.614426	-0.038448	3.971324
188.592756	5377.308001	7.619430	-0.038438	3.974169
188.887406	5385.341883	7.624435	-0.038498	3.977025
188.948214	5393.348657	7.629440	-0.038515	3.979865
189.063592	5401.351572	7.634445	-0.038541	3.982703
189.144276	5409.379512	7.639450	-0.038562	3.985547
189.335551	5417.431027	7.644454	-0.038603	3.988399
189.445301	5425.451545	7.649459	-0.038628	3.991237
189.771306	5433.494360	7.654464	-0.038694	3.994085
189.672712	5441.504197	7.659469	-0.038681	3.996911
189.874352	5449.517436	7.664474	-0.038724	3.999742
190.139070	5457.514083	7.669478	-0.038778	4.002566
190.418987	5465.524670	7.674483	-0.038836	4.005393
190.447511	5473.571026	7.679488	-0.038846	4.008226
190.510077	5481.587834	7.684493	-0.038863	4.011048
190.713340	5489.650209	7.689498	-0.038906	4.013886
190.755532	5497.687342	7.694502	-0.038919	4.016710
190.985900	5505.651531	7.699507	-0.038967	4.019510
191.174072	5513.680211	7.704512	-0.039007	4.022330
191.232448	5521.685583	7.709517	-0.039024	4.025138
191.385552	5529.729865	7.714522	-0.039057	4.027958
191.508447	5537.707136	7.719526	-0.039085	4.030753
191.409203	5545.850508	7.724531	-0.039072	4.033601
191.607689	5553.896507	7.729536	-0.039114	4.036417
191.902422	5561.779594	7.734541	-0.039174	4.039175
192.420822	5569.808897	7.739546	-0.039276	4.041986
192.552046	5577.768326	7.744550	-0.039306	4.044765
192.554763	5585.811304	7.749555	-0.039311	4.047569
192.661228	5593.838452	7.754560	-0.039336	4.050368
192.726784	5601.869335	7.759565	-0.039354	4.053165
192.853159	5609.919412	7.764570	-0.039383	4.055967
193.150649	5617.897921	7.769574	-0.039443	4.058746
192.976841	5625.922253	7.774579	-0.039416	4.061531
193.150740	5633.919681	7.779584	-0.039454	4.064310
193.328324	5641.949516	7.784589	-0.039492	4.067099
193.546695	5649.980572	7.789594	-0.039538	4.069886
193.617324	5658.014234	7.794598	-0.039556	4.072671
193.837399	5666.033846	7.799603	-0.039602	4.075451
194.072207	5674.046705	7.804608	-0.039651	4.078227
193.920074	5682.027363	7.809613	-0.039628	4.080984
194.055306	5690.031715	7.814618	-0.039659	4.083752
194.349235	5698.092235	7.819622	-0.039718	4.086539
194.401767	5706.082856	7.824627	-0.039733	4.089297
194.487588	5714.140084	7.829632	-0.039755	4.092076
194.759623	5722.142070	7.834637	-0.039811	4.094837
195.148953	5730.191261	7.839642	-0.039888	4.097615
195.289784	5738.164053	7.844646	-0.039920	4.100360
195.203375	5746.131946	7.849651	-0.039909	4.103099
195.308030	5754.249566	7.854656	-0.039934	4.105890
195.350138	5762.239651	7.859661	-0.039947	4.108635
195.726463	5770.280647	7.864666	-0.040022	4.111399
195.831793	5778.343835	7.869670	-0.040047	4.114166
195.830403	5786.332680	7.874675	-0.040052	4.116904
195.905830	5794.313035	7.879680	-0.040071	4.119638
196.123472	5802.312600	7.884685	-0.040117	4.122379
196.084284	5810.378224	7.889690	-0.040115	4.125137
196.112026	5818.370938	7.894694	-0.040125	4.127870
196.229851	5826.371153	7.899699	-0.040152	4.130604
196.463843	5834.471301	7.904704	-0.040201	4.133372
196.646079	5842.470830	7.909709	-0.040240	4.136103
196.762742	5850.469846	7.914714	-0.040267	4.138831
196.998087	5858.520362	7.919718	-0.040316	4.141577
196.994934	5866.477499	7.924723	-0.040321	4.144286
197.129409	5874.567150	7.929728	-0.040351	4.147040
197.181839	5882.527354	7.934733	-0.040366	4.149747
197.404155	5890.602639	7.939738	-0.040412	4.152493
197.624348	5898.603425	7.944742	-0.040459	4.155212
197.527797	5906.602126	7.949747	-0.040446	4.157925
197.770908	5914.611805	7.954752	-0.040496	4.160644
197.941720	5922.615485	7.959757	-0.040533	4.163359
197.922797	5930.665979	7.964762	-0.040535	4.166085
198.277799	5938.650010	7.969766	-0.040606	4.168791
198.368934	5946.708297	7.974771	-0.040628	4.171517
198.183484	5954.758069	7.979776	-0.040599	4.174236
198.515428	5962.746779	7.984781	-0.040666	4.176938
198.634520	5970.740454	7.989786	-0.040694	4.179638
198.716769	5978.773895	7.994790	-0.040714	4.182348
198.749097	5986.751228	7.999795	-0.040725	4.185038
199.029966	5994.834085	8.004800	-0.040783	4.187764
199.157754	6002.772373	8.009805	-0.040812	4.190438
199.180786	6010.920580	8.014810	-0.040821	4.193180
199.298541	6019.004235	8.019814	-0.040849	4.195899
199.451763	6026.883873	8.024819	-0.040882	4.198549
199.615742	6034.923529	8.029824	-0.040918	4.201250
199.949622	6042.849569	8.034829	-0.040985	4.203913
200.205111	6050.859582	8.039834	-0.041038	4.206602
200.398157	6058.884222	8.044838	-0.041079	4.209294
200.338639	6066.957292	8.049843	-0.041073	4.211997
200.453422	6074.988213	8.054848	-0.041100	4.214686
200.615071	6082.993952	8.059853	-0.041135	4.217366
200.846225	6090.969124	8.064858	-0.041184	4.220034
200.976897	6099.022572	8.069862	-0.041213	4.222726
200.987802	6107.005280	8.074867	-0.041220	4.225392
201.073992	6115.084411	8.079872	-0.041242	4.228088
201.221116	6123.059239	8.084877	-0.041274	4.230749
201.569453	6131.113872	8.089882	-0.041344	4.233436
201.629338	6139.122129	8.094886	-0.041361	4.236103
201.506530	6147.081618	8.099891	-0.041343	4.238751
201.815043	6155.114434	8.104896	-0.041406	4.241426
201.845006	6163.082397	8.109901	-0.041416	4.244075
201.958852	6171.194010	8.114906	-0.041443	4.246770
201.972162	6179.178183	8.119910	-0.041450	4.249421
202.334440	6187.213166	8.124915	-0.041523	4.252090
202.372316	6195.263273	8.129920	-0.041535	4.254759
202.274053	6203.242085	8.134925	-0.041522	4.257402
202.576835	6211.265806	8.139930	-0.041584	4.260061
202.706230	6219.309751	8.144934	-0.041613	4.262724
202.722767	6227.277778	8.149939	-0.041621	4.265360
202.982115	6235.352926	8.154944	-0.041675	4.268031
203.133825	6243.327367	8.159949	-0.041708	4.270666
203.507086	6251.454239	8.164954	-0.041783	4.273352
203.615654	6259.464547	8.169958	-0.041809	4.275995
203.586928	6267.403852	8.174963	-0.041808	4.278613
203.618106	6275.455476	8.179968	-0.041819	4.281266
203.666694	6283.405444	8.184973	-0.041834	4.283884
203.913636	6291.499527	8.189978	-0.041885	4.286549
204.011689	6299.456259	8.194982	-0.041908	4.289167
204.242674	6307.528605	8.199987	-0.041957	4.291822
204.672003	6315.538387	8.204992	-0.042042	4.294456
204.765213	6323.546304	8.209997	-0.042064	4.297086
204.737622	6331.502139	8.215002	-0.042064	4.299695
204.764503	6339.594846	8.220006	-0.042075	4.302349
205.252910	6347.555682	8.225011	-0.042171	4.304961
205.544014	6355.614949	8.230016	-0.042230	4.307602
205.542220	6363.648025	8.235021	-0.042235	4.310231
205.720629	6371.677976	8.240026	-0.042274	4.312858
205.772858	6379.676655	8.245030	-0.042288	4.315473
205.786344	6387.670588	8.250035	-0.042296	4.318084
205.986524	6395.692856	8.255040	-0.042339	4.320704
205.843093	6403.713497	8.260045	-0.042317	4.323320
206.017407	6411.730861	8.265050	-0.042355	4.325935
206.011676	6419.736072	8.270054	-0.042359	4.328544
206.118904	6427.751299	8.275059	-0.042384	4.331155
206.496611	6435.790454	8.280064	-0.042460	4.333774
206.595064	6443.801311	8.285069	-0.042483	4.336380
207.041488	6451.784590	8.290074	-0.042571	4.338978
207.056311	6459.841618	8.295078	-0.042579	4.341596
207.327438	6467.800009	8.300083	-0.042635	4.344181
207.470004	6475.883363	8.305088	-0.042667	4.346805
207.782155	6483.857407	8.310093	-0.042730	4.349393
208.050716	6491.920100	8.315098	-0.042785	4.352007
207.932973	6500.034162	8.320102	-0.042769	4.354635
208.235324	6508.004747	8.325107	-0.042830	4.357217
208.601616	6515.925819	8.330112	-0.042904	4.359781
208.516645	6523.928216	8.335117	-0.042893	4.362368
208.788970	6531.940932	8.340122	-0.042949	4.364958
209.119364	6539.949666	8.345126	-0.043016	4.367547
209.235216	6547.937393	8.350131	-0.043042	4.370125
209.497322	6556.062685	8.355136	-0.043097	4.372747
209.679515	6564.025879	8.360141	-0.043136	4.375315
209.826880	6572.081728	8.365146	-0.043168	4.377911
210.133539	6580.075481	8.370150	-0.043231	4.380486
210.051704	6588.076264	8.375155	-0.043221	4.383060
210.184440	6596.105066	8.380160	-0.043250	4.385643
210.092903	6604.078508	8.385165	-0.043239	4.388205
210.467897	6612.159233	8.390170	-0.043314	4.390802
210.527075	6620.208549	8.395174	-0.043330	4.393386
210.566725	6628.208457	8.400179	-0.043343	4.395953
210.631770	6636.205814	8.405184	-0.043360	4.398517
210.910827	6644.196483	8.410189	-0.043417	4.401079
210.978603	6652.199332	8.415194	-0.043435	4.403642
211.134983	6660.239577	8.420198	-0.043469	4.406216
211.142157	6668.221596	8.425203	-0.043476	4.408770
211.421098	6676.320156	8.430208	-0.043533	4.411360
211.382704	6684.289808	8.435213	-0.043531	4.413906
211.449211	6692.370980	8.440218	-0.043549	4.416487
211.718681	6700.346134	8.445222	-0.043604	4.419033
211.681818	6708.364939	8.450227	-0.043602	4.421590
212.008610	6716.384872	8.455232	-0.043668	4.424148
212.048442	6724.385411	8.460237	-0.043681	4.426697
212.251119	6732.416647	8.465242	-0.043724	4.429255
212.209550	6740.477735	8.470246	-0.043721	4.431819
212.450094	6748.483486	8.475251	-0.043771	4.434366
212.665108	6756.545398	8.480256	-0.043817	4.436929
212.737249	6764.461652	8.485261	-0.043835	4.439444
212.794554	6772.499699	8.490266	-0.043851	4.441996
213.026568	6780.465236	8.495270	-0.043899	4.444524
212.992811	6788.524622	8.500275	-0.043898	4.447080
213.180801	6796.553217	8.505280	-0.043939	4.449625
213.295061	6804.553916	8.510285	-0.043965	4.452159
213.569032	6812.582851	8.515290	-0.044021	4.454702
213.703121	6820.599481	8.520294	-0.044052	4.457238
213.759610	6828.586137	8.525299	-0.044067	4.459764
214.080428	6836.636409	8.530304	-0.044132	4.462309
214.111136	6844.571263	8.535309	-0.044143	4.464815
214.370360	6852.644454	8.540314	-0.044197	4.467364
214.520576	6860.664225	8.545318	-0.044230	4.469894
214.538005	6868.717848	8.550323	-0.044238	4.472433
214.852542	6876.736081	8.555328	-0.044302	4.474961
215.002533	6884.752847	8.560333	-0.044335	4.477486
215.386099	6892.697277	8.565338	-0.044412	4.479988
215.264080	6900.756879	8.570343	-0.044394	4.482522
215.356239	6908.747261	8.575347	-0.044417	4.485035
215.658390	6916.793705	8.580352	-0.044478	4.487564
215.595677	6924.772872	8.585357	-0.044472	4.490069
215.814031	6932.816418	8.590362	-0.044517	4.492594
215.893793	6940.852969	8.595367	-0.044538	4.495115
216.042920	6948.839625	8.600371	-0.044571	4.497620
216.293280	6956.862761	8.605376	-0.044622	4.500134
216.226229	6964.861433	8.610381	-0.044615	4.502638
216.678399	6972.860966	8.615386	-0.044704	4.505143
216.690460	6980.913855	8.620391	-0.044712	4.507662
216.648121	6988.932759	8.625395	-0.044709	4.510169
217.020025	6997.020678	8.630400	-0.044784	4.512697
217.122930	7005.024436	8.635405	-0.044808	4.515196
217.188761	7013.006950	8.640410	-0.044826	4.517687
217.293919	7020.958561	8.645415	-0.044850	4.520168
217.616424	7028.998121	8.650419	-0.044916	4.522675
217.741250	7036.996599	8.655424	-0.044944	4.525167
217.671763	7045.024984	8.660429	-0.044936	4.527667
217.830181	7053.029130	8.665434	-0.044971	4.530158
217.846611	7061.098938	8.670439	-0.044979	4.532668
217.797669	7069.088270	8.675443	-0.044975	4.535152
218.112725	7077.137981	8.680448	-0.045039	4.537654
218.196926	7085.073995	8.685453	-0.045060	4.540118
218.352039	7093.131672	8.690458	-0.045094	4.542619
218.298918	7101.117522	8.695463	-0.045090	4.545096
218.646673	7109.128679	8.700467	-0.045159	4.547580
219.007601	7117.208796	8.705472	-0.045232	4.550085
219.002373	7125.208657	8.710477	-0.045236	4.552562
219.241527	7133.244978	8.715482	-0.045286	4.555049
219.272396	7141.216108	8.720487	-0.045297	4.557515
219.397053	7149.188119	8.725491	-0.045325	4.559980
219.764032	7157.238239	8.730496	-0.045399	4.562468
219.929737	7165.196660	8.735501	-0.045435	4.564926
219.849119	7173.283849	8.740506	-0.045425	4.567422
220.015328	7181.270245	8.745511	-0.045461	4.569886
220.259256	7189.312403	8.750515	-0.045512	4.572366
220.317268	7197.350534	8.755520	-0.045528	4.574843
220.286227	7205.375082	8.760525	-0.045527	4.577314
220.485034	7213.344438	8.765530	-0.045570	4.579767
220.816803	7221.402035	8.770535	-0.045637	4.582246
220.741968	7229.334165	8.775539	-0.045628	4.584685
221.065702	7237.471766	8.780544	-0.045693	4.587186
221.217926	7245.411988	8.785549	-0.045727	4.589625
221.505168	7253.518996	8.790554	-0.045786	4.592114
221.560777	7261.562744	8.795559	-0.045801	4.594582
221.549140	7269.537630	8.800563	-0.045804	4.597028
221.987478	7277.506961	8.805568	-0.045891	4.599470
221.983522	7285.562803	8.810573	-0.045895	4.601938
222.250469	7293.495195	8.815578	-0.045950	4.604366
222.382702	7301.533033	8.820583	-0.045980	4.606826
222.136326	7309.500925	8.825587	-0.045939	4.609263
222.405469	7317.621881	8.830592	-0.045995	4.611745
222.658076	7325.631820	8.835597	-0.046047	4.614192
222.813343	7333.682940	8.840602	-0.046081	4.616650
222.873181	7341.618679	8.845607	-0.046098	4.619072
223.016084	7349.639525	8.850611	-0.046129	4.621518
223.276343	7357.656553	8.855616	-0.046183	4.623962
223.378275	7365.683965	8.860621	-0.046207	4.626408
223.453140	7373.719749	8.865626	-0.046226	4.628855
223.557310	7381.751647	8.870631	-0.046251	4.631300
223.825914	7389.734670	8.875635	-0.046306	4.633728
223.820818	7397.779099	8.880640	-0.046310	4.636174
223.873573	7405.725113	8.885645	-0.046325	4.638588
224.130484	7413.770278	8.890650	-0.046379	4.641032
224.328009	7421.799091	8.895655	-0.046421	4.643469
224.416044	7429.777402	8.900659	-0.046442	4.645889
224.507572	7437.843342	8.905664	-0.046464	4.648335
224.449346	7445.850320	8.910669	-0.046459	4.650762
224.647903	7453.861170	8.915674	-0.046501	4.653188
224.774367	7461.908041	8.920679	-0.046530	4.655624
224.758309	7469.828686	8.925683	-0.046532	4.658021
224.942719	7477.914149	8.930688	-0.046571	4.660466
225.149311	7485.874881	8.935693	-0.046615	4.662872
225.327989	7493.914127	8.940698	-0.046654	4.665301
225.382655	7501.942660	8.945703	-0.046669	4.667725
225.572083	7509.934577	8.950707	-0.046709	4.670137
225.854558	7518.056385	8.955712	-0.046767	4.672586
225.914998	7526.089360	8.960717	-0.046784	4.675008
225.956234	7534.077730	8.965722	-0.046797	4.677415
226.191220	7542.010033	8.970727	-0.046846	4.679804
226.414757	7549.972362	8.975731	-0.046892	4.682200
226.607683	7557.975028	8.980736	-0.046933	4.684608
226.600781	7566.019199	8.985741	-0.046937	4.687026
226.913128	7574.056911	8.990746	-0.047001	4.689442
226.811001	7582.106810	8.995751	-0.046987	4.691860
226.861642	7590.087927	9.000755	-0.047002	4.694256
227.035437	7598.174877	9.005760	-0.047039	4.696683
227.063535	7606.099578	9.010765	-0.047050	4.699059
227.292857	7614.138009	9.015770	-0.047098	4.701469
227.516699	7622.125381	9.020775	-0.047144	4.703861
227.414190	7630.119795	9.025779	-0.047131	4.706256
227.711713	7638.171266	9.030784	-0.047191	4.708665
227.769303	7646.180288	9.035789	-0.047207	4.711061
228.038897	7654.254588	9.040794	-0.047263	4.713474
228.024310	7662.264008	9.045799	-0.047265	4.715868
228.040088	7670.265201	9.050803	-0.047273	4.718258
228.639095	7678.251258	9.055808	-0.047390	4.720640
228.532749	7686.249188	9.060813	-0.047375	4.723027
228.782408	7694.292973	9.065818	-0.047427	4.725426
228.785225	7702.352370	9.070823	-0.047433	4.727828
228.855639	7710.320060	9.075827	-0.047451	4.730202
229.050459	7718.395714	9.080832	-0.047493	4.732606
229.070325	7726.366877	9.085837	-0.047501	4.734978
229.244738	7734.397087	9.090842	-0.047539	4.737367
229.470995	7742.405678	9.095847	-0.047586	4.739747
229.499005	7750.422700	9.100851	-0.047597	4.742130
229.823536	7758.429993	9.105856	-0.047663	4.744507
229.687190	7766.473431	9.110861	-0.047642	4.746895
229.662349	7774.455761	9.115866	-0.047643	4.749264
230.088412	7782.541731	9.120871	-0.047727	4.751661
230.281399	7790.541943	9.125875	-0.047769	4.754032
230.325482	7798.615175	9.130880	-0.047782	4.756423
230.458545	7806.513187	9.135885	-0.047812	4.758762
230.851023	7814.516278	9.140890	-0.047890	4.761129
230.928369	7822.547231	9.145895	-0.047910	4.763505
231.031142	7830.521281	9.150899	-0.047934	4.765862
231.315996	7838.599818	9.155904	-0.047992	4.768249
231.261222	7846.601132	9.160909	-0.047987	4.770612
231.269623	7854.644216	9.165914	-0.047994	4.772987
231.541174	7862.646005	9.170919	-0.048050	4.775347
231.508992	7870.637332	9.175923	-0.048049	4.777704
231.651173	7878.677271	9.180928	-0.048081	4.780074
231.655279	7886.645227	9.185933	-0.048087	4.782421
231.893750	7894.652098	9.190938	-0.048136	4.784779
232.112612	7902.677600	9.195943	-0.048182	4.787140
232.243913	7910.697442	9.200947	-0.048212	4.789499
232.597262	7918.779661	9.205952	-0.048283	4.791874
232.554783	7926.748792	9.210957	-0.048280	4.794217
232.362591	7934.782351	9.215962	-0.048250	4.796578
232.509923	7942.772696	9.220967	-0.048282	4.798923
232.822807	7950.799279	9.225971	-0.048346	4.801277
233.097413	7958.796349	9.230976	-0.048402	4.803622
233.007379	7966.819543	9.235981	-0.048391	4.805975
232.998522	7974.808474	9.240986	-0.048394	4.808316
233.420482	7982.853916	9.245991	-0.048478	4.810671
233.264182	7990.221219	9.250995	-0.048454	4.812828
233.330121	7994.721897	9.256000	-0.048469	4.814145

233.566415	7997.212859	9.261005	-0.048515	4.814873
233.530121	7998.504562	9.266010	-0.048509	4.815251
233.550339	7998.972312	9.271015	-0.048513	4.815388
233.897662	7999.906400	9.276019	-0.048578	4.815659
233.917633	7999.972891	9.281024	-0.048582	4.815679
233.896277	7999.968276	9.286029	-0.048578	4.815677
233.851988	7999.973964	9.291034	-0.048569	4.815679
233.909847	7999.979165	9.296039	-0.048580	4.815680
233.831202	7999.927734	9.301043	-0.048566	4.815666
233.863785	7999.961343	9.306048	-0.048572	4.815675
233.935739	7999.944359	9.311053	-0.048585	4.815670
233.983430	7999.965405	9.316058	-0.048594	4.815676
234.008476	7999.959404	9.321063	-0.048598	4.815674
234.050224	7999.949404	9.326067	-0.048606	4.815671
234.218953	7999.992681	9.331072	-0.048638	4.815683
234.176224	7999.971712	9.336077	-0.048630	4.815677
234.241344	7999.983434	9.341082	-0.048642	4.815680
234.360803	7999.971485	9.346087	-0.048664	4.815676
234.119947	7999.954791	9.351091	-0.048619	4.815672
234.186605	8000.006027	9.356096	-0.048632	4.815687
234.248214	7999.972866	9.361101	-0.048643	4.815677
234.395323	7999.965633	9.366106	-0.048670	4.815674
234.424740	7999.968241	9.371111	-0.048676	4.815675
234.308319	7999.901257	9.376115	-0.048654	4.815656
234.420642	7999.944692	9.381120	-0.048675	4.815668
234.349702	7999.922200	9.386125	-0.048662	4.815662
234.279235	7999.937071	9.391130	-0.048649	4.815666
234.377838	7999.955737	9.396135	-0.048667	4.815671
234.374842	7999.900189	9.401139	-0.048666	4.815655
234.535232	7999.975351	9.406144	-0.048696	4.815676
234.511365	7999.947215	9.411149	-0.048692	4.815668
234.513578	7999.930172	9.416154	-0.048692	4.815663
234.649710	7999.915291	9.421159	-0.048718	4.815658
234.826825	7999.905340	9.426163	-0.048750	4.815655
234.653696	7999.947371	9.431168	-0.048718	4.815668
234.574426	7999.924745	9.436173	-0.048703	4.815661
234.721119	7999.968735	9.441178	-0.048731	4.815674
234.897662	7999.995063	9.446183	-0.048764	4.815680
234.826962	7999.956565	9.451187	-0.048750	4.815670
234.939592	7999.972256	9.456192	-0.048771	4.815674
234.991074	7999.950673	9.461197	-0.048781	4.815667
234.899364	7999.964134	9.466202	-0.048764	4.815671
234.962800	7999.970492	9.471207	-0.048776	4.815673
234.947248	7999.954231	9.476211	-0.048773	4.815668
234.975487	7999.956820	9.481216	-0.048778	4.815669
234.852243	7999.952695	9.486221	-0.048755	4.815668
234.814529	7999.951017	9.491226	-0.048748	4.815668
234.994822	7999.976339	9.496231	-0.048782	4.815675
234.714405	7999.952601	9.501235	-0.048729	4.815669
234.876621	7999.977630	9.506240	-0.048760	4.815675
234.951423	7999.955356	9.511245	-0.048773	4.815669
234.960575	7999.991790	9.516250	-0.048775	4.815679
234.728278	7999.977367	9.521255	-0.048732	4.815676
234.796219	7999.983799	9.526259	-0.048745	4.815678
234.898980	7999.959840	9.531264	-0.048764	4.815670
234.891958	7999.969331	9.536269	-0.048762	4.815673
234.901974	7999.998309	9.541274	-0.048764	4.815681
235.034873	7999.994048	9.546279	-0.048789	4.815680
235.067647	7999.980701	9.551283	-0.048795	4.815675
234.902724	7999.998317	9.556288	-0.048764	4.815681
234.994415	7999.970978	9.561293	-0.048781	4.815673
235.075706	7999.980827	9.566298	-0.048796	4.815675
234.966643	7999.982267	9.571303	-0.048776	4.815676
234.963089	7999.973670	9.576307	-0.048775	4.815674
235.048979	7999.994267	9.581312	-0.048791	4.815680
235.007931	7999.972257	9.586317	-0.048784	4.815673
235.128423	7999.964594	9.591322	-0.048806	4.815670
235.009076	8000.000022	9.596327	-0.048784	4.815681
234.730351	7999.972042	9.601331	-0.048732	4.815675
235.140932	8000.010686	9.606336	-0.048808	4.815684
235.195389	7999.977410	9.611341	-0.048819	4.815674
235.091786	7999.960794	9.616346	-0.048799	4.815670
235.255519	7999.986916	9.621351	-0.048830	4.815676
235.165965	7999.968393	9.626355	-0.048813	4.815671
235.423096	8000.038715	9.631360	-0.048861	4.815691
235.226146	8000.000313	9.636365	-0.048824	4.815680
235.245231	8000.005956	9.641370	-0.048828	4.815682
235.229185	8000.011033	9.646375	-0.048825	4.815684
235.227271	7999.960837	9.651379	-0.048824	4.815669
235.230764	8000.012123	9.656384	-0.048825	4.815684
235.109658	7999.988820	9.661389	-0.048802	4.815678
235.121348	8000.018892	9.666394	-0.048805	4.815686
235.272625	8000.003188	9.671399	-0.048833	4.815681
235.311948	7999.982476	9.676403	-0.048840	4.815675
235.342548	7999.998978	9.681408	-0.048846	4.815680
235.241071	7999.988800	9.686413	-0.048827	4.815677
235.070078	8000.011654	9.691418	-0.048795	4.815685
235.231239	8000.008917	9.696423	-0.048825	4.815683
235.098636	7999.969420	9.701427	-0.048800	4.815672
235.192393	7999.980538	9.706432	-0.048818	4.815675
235.101738	7999.932112	9.711437	-0.048801	4.815661
235.180847	7999.951532	9.716442	-0.048816	4.815666
235.272920	7999.994641	9.721447	-0.048833	4.815679
235.057677	7999.980493	9.726451	-0.048793	4.815675
235.521180	7999.996511	9.731456	-0.048879	4.815678
235.478900	7999.996895	9.736461	-0.048871	4.815678
235.358135	8000.010954	9.741466	-0.048848	4.815683
235.507294	8000.031504	9.746471	-0.048876	4.815688
235.296912	7999.975809	9.751475	-0.048837	4.815673
235.316887	7999.973995	9.756480	-0.048841	4.815672
235.177675	7999.936526	9.761485	-0.048815	4.815662
235.360531	7999.970428	9.766490	-0.048849	4.815671
235.498067	7999.988656	9.771495	-0.048874	4.815676
235.383438	7999.948381	9.776499	-0.048853	4.815665
235.353026	8000.016197	9.781504	-0.048847	4.815685
235.358136	7999.994932	9.786509	-0.048848	4.815678
235.222446	7999.976731	9.791514	-0.048823	4.815674
235.252289	7999.992153	9.796519	-0.048829	4.815678
235.289659	7999.998092	9.801523	-0.048836	4.815680
235.361025	8000.014184	9.806528	-0.048849	4.815684
235.298607	7999.952339	9.811533	-0.048837	4.815666
235.377364	7999.989897	9.816538	-0.048852	4.815677
235.440800	7999.966372	9.821543	-0.048864	4.815670
235.220097	7999.947866	9.826547	-0.048822	4.815665
235.457850	8000.000798	9.831552	-0.048867	4.815680
235.491246	7999.989596	9.836557	-0.048873	4.815676
235.386744	7999.982571	9.841562	-0.048853	4.815675
235.307385	7999.985558	9.846567	-0.048839	4.815676
235.485218	7999.979888	9.851571	-0.048872	4.815673
235.484086	7999.975600	9.856576	-0.048872	4.815672
235.477483	7999.970155	9.861581	-0.048870	4.815670
235.521196	7999.982600	9.866586	-0.048878	4.815674
235.608546	8000.012826	9.871591	-0.048895	4.815682
235.319850	7999.951597	9.876595	-0.048841	4.815666
235.405213	8000.010608	9.881600	-0.048857	4.815683
235.585906	7999.996447	9.886605	-0.048890	4.815678
235.585264	7999.986829	9.891610	-0.048890	4.815675
235.532872	8000.009463	9.896615	-0.048881	4.815682
235.566462	7999.987590	9.901619	-0.048887	4.815675
235.611133	8000.018195	9.906624	-0.048895	4.815684
235.542364	7999.989333	9.911629	-0.048882	4.815676
235.490216	7999.979951	9.916634	-0.048873	4.815673
235.467509	7999.987055	9.921639	-0.048868	4.815675
235.374242	7999.966336	9.926643	-0.048851	4.815670
235.642927	7999.999490	9.931648	-0.048901	4.815678
235.740467	7999.985053	9.936653	-0.048919	4.815674
235.622160	8000.000219	9.941658	-0.048897	4.815679
235.655559	7999.987949	9.946663	-0.048903	4.815675
235.395602	7999.942126	9.951667	-0.048855	4.815663
235.580179	8000.008076	9.956672	-0.048889	4.815681
235.574575	7999.971695	9.961677	-0.048888	4.815670
235.655226	7999.992207	9.966682	-0.048903	4.815676
235.819448	8000.005531	9.971687	-0.048934	4.815679
235.566658	7999.970496	9.976691	-0.048887	4.815670
235.626441	7999.994941	9.981696	-0.048898	4.815677
235.552549	7999.970266	9.986701	-0.048884	4.815670
235.452235	7999.956905	9.991706	-0.048865	4.815667
235.427354	7999.978915	9.996711	-0.048861	4.815673
235.453523	7999.974000	10.001715	-0.048865	4.815672
235.753059	8000.017257	10.006720	-0.048921	4.815683
235.679725	8000.005399	10.011725	-0.048908	4.815680
235.550591	8000.000111	10.016730	-0.048883	4.815679
235.755849	8000.025837	10.021735	-0.048922	4.815685
235.502228	7999.996125	10.026739	-0.048874	4.815678
235.498476	7999.991794	10.031744	-0.048874	4.815677
235.815482	7999.984102	10.036749	-0.048933	4.815673
235.839787	7999.972753	10.041754	-0.048937	4.815670
235.782048	7999.973954	10.046759	-0.048926	4.815670
235.700364	7999.997182	10.051763	-0.048911	4.815677
235.959588	8000.053665	10.056768	-0.048960	4.815693
235.668172	7999.991323	10.061773	-0.048905	4.815676
235.556934	8000.022613	10.066778	-0.048884	4.815685
235.779172	8000.025132	10.071783	-0.048926	4.815685
235.778784	7999.972826	10.076787	-0.048926	4.815670
235.499965	8000.016353	10.081792	-0.048874	4.815684
235.616008	7999.985138	10.086797	-0.048895	4.815674
235.572055	8000.014312	10.091802	-0.048887	4.815683
235.628927	8000.039777	10.096807	-0.048898	4.815690
235.709054	8000.022925	10.101811	-0.048913	4.815685
235.901303	8000.052710	10.106816	-0.048949	4.815693
235.625411	8000.031177	10.111821	-0.048897	4.815688
235.599279	8000.013677	10.116826	-0.048892	4.815683
235.818930	8000.006549	10.121831	-0.048933	4.815680
235.825856	8000.020534	10.126835	-0.048934	4.815684
235.686434	8000.027888	10.131840	-0.048908	4.815686
235.861749	7999.993361	10.136845	-0.048941	4.815675
235.813388	7999.987242	10.141850	-0.048932	4.815674
235.831364	8000.009945	10.146855	-0.048935	4.815680
235.926360	7999.981592	10.151859	-0.048953	4.815672
236.019877	7999.986303	10.156864	-0.048970	4.815673
236.017880	7999.989471	10.161869	-0.048970	4.815674
235.881636	7999.994741	10.166874	-0.048945	4.815676
235.959263	8000.018407	10.171879	-0.048959	4.815682
235.813726	7999.991507	10.176883	-0.048932	4.815675
235.813294	8000.004307	10.181888	-0.048932	4.815679
235.886931	7999.992686	10.186893	-0.048946	4.815675
235.873247	8000.026618	10.191898	-0.048943	4.815685
235.953370	8000.040719	10.196903	-0.048958	4.815689
235.749089	7999.986188	10.201907	-0.048920	4.815674
236.106760	8000.036789	10.206912	-0.048986	4.815687
236.026487	8000.001337	10.211917	-0.048971	4.815677
235.920571	7999.994289	10.216922	-0.048952	4.815675
235.999635	8000.011574	10.221927	-0.048966	4.815680
235.927412	7999.929290	10.226931	-0.048953	4.815656
235.914162	7999.996316	10.231936	-0.048950	4.815676
235.710023	7999.990884	10.236941	-0.048912	4.815675
235.827185	7999.961822	10.241946	-0.048934	4.815666
235.879446	7999.979741	10.246951	-0.048944	4.815671
235.954782	7999.961745	10.251955	-0.048958	4.815666
236.035736	7999.985464	10.256960	-0.048973	4.815672
235.855608	7999.968679	10.261965	-0.048939	4.815668
235.978294	8000.000544	10.266970	-0.048962	4.815677
235.893437	8000.009846	10.271975	-0.048947	4.815680
235.952284	7999.987313	10.276979	-0.048957	4.815673
236.015035	7999.994729	10.281984	-0.048969	4.815675
235.960940	7999.994922	10.286989	-0.048959	4.815675
235.967746	8000.013175	10.291994	-0.048960	4.815681
235.953100	8000.015071	10.296999	-0.048958	4.815681
235.922934	7999.975092	10.302003	-0.048952	4.815670
236.104596	7999.983360	10.307008	-0.048986	4.815671
236.079314	7999.985085	10.312013	-0.048981	4.815672
235.827594	7999.966078	10.317018	-0.048934	4.815668
235.975672	8000.011160	10.322023	-0.048962	4.815680
235.943406	7999.934858	10.327027	-0.048956	4.815658
236.048435	7999.981379	10.332032	-0.048975	4.815671
236.011358	7999.992520	10.337037	-0.048968	4.815675
235.997224	8000.005098	10.342042	-0.048966	4.815678
235.875063	8000.006327	10.347047	-0.048943	4.815679
235.698228	7999.984259	10.352051	-0.048910	4.815674
235.914485	7999.996287	10.357056	-0.048950	4.815676
235.978681	7999.995188	10.362061	-0.048962	4.815675
236.026959	8000.005572	10.367066	-0.048971	4.815678
236.008058	8000.003130	10.372071	-0.048968	4.815678
236.027629	7999.952214	10.377075	-0.048971	4.815663
236.074434	8000.017007	10.382080	-0.048980	4.815681
235.878532	7999.993564	10.387085	-0.048943	4.815675
235.834845	7999.991790	10.392090	-0.048935	4.815675
236.033999	7999.980061	10.397095	-0.048972	4.815671
236.005737	7999.934776	10.402099	-0.048967	4.815658
235.994890	7999.996504	10.407104	-0.048965	4.815676
236.065092	7999.993367	10.412109	-0.048978	4.815675
235.915316	8000.010159	10.417114	-0.048950	4.815680
235.968018	8000.021682	10.422119	-0.048960	4.815683
236.018044	7999.952045	10.427123	-0.048969	4.815663
236.076188	8000.003147	10.432128	-0.048980	4.815677
235.951179	7999.994723	10.437133	-0.048957	4.815675
235.944156	7999.989272	10.442138	-0.048955	4.815674
236.041565	8000.012190	10.447143	-0.048974	4.815680
235.906421	7999.942765	10.452147	-0.048948	4.815660
235.915128	7999.994136	10.457152	-0.048950	4.815675
236.176009	7999.996212	10.462157	-0.048999	4.815675
236.142737	7999.952980	10.467162	-0.048992	4.815662
235.871052	7999.987016	10.472167	-0.048942	4.815674
236.041677	7999.989770	10.477171	-0.048973	4.815674
236.213186	8000.009615	10.482176	-0.049005	4.815679
236.053690	8000.003836	10.487181	-0.048976	4.815678
235.918479	7999.998450	10.492186	-0.048950	4.815677
236.228251	7999.991709	10.497191	-0.049008	4.815673
235.985438	7999.972845	10.502195	-0.048963	4.815669
236.010997	7999.992468	10.507200	-0.048968	4.815675
236.304954	7999.998281	10.512205	-0.049022	4.815675
236.104430	8000.007849	10.517210	-0.048985	4.815679
236.138671	8000.009468	10.522215	-0.048991	4.815679
236.007067	7999.968918	10.527219	-0.048967	4.815668
236.184134	8000.002728	10.532224	-0.049000	4.815677
236.088622	7999.994781	10.537229	-0.048982	4.815675
236.022469	8000.004384	10.542234	-0.048970	4.815678
236.092615	8000.032199	10.547239	-0.048983	4.815686
235.983956	7999.985615	10.552243	-0.048962	4.815673
236.296535	8000.000267	10.557248	-0.049021	4.815675
236.298591	7999.990693	10.562253	-0.049021	4.815673
236.310097	7999.968463	10.567258	-0.049023	4.815666
236.300485	8000.006731	10.572263	-0.049021	4.815677
236.213026	7999.973297	10.577267	-0.049005	4.815668
236.084862	8000.042737	10.582272	-0.048981	4.815689
236.036310	8000.031279	10.587277	-0.048972	4.815686
236.088563	7999.991563	10.592282	-0.048982	4.815674
236.106480	8000.031342	10.597287	-0.048985	4.815685
236.036169	8000.001387	10.602291	-0.048972	4.815677
236.167788	8000.018454	10.607296	-0.048997	4.815681
236.254513	7999.995304	10.612301	-0.049013	4.815674
236.331698	8000.010424	10.617306	-0.049027	4.815678
236.347830	8000.028828	10.622311	-0.049030	4.815684
236.313974	7999.980250	10.627315	-0.049024	4.815670
236.304578	7999.993972	10.632320	-0.049022	4.815674
236.289457	8000.019343	10.637325	-0.049019	4.815681
236.447553	8000.031501	10.642330	-0.049049	4.815684
236.446683	8000.034687	10.647335	-0.049048	4.815685
236.122495	7999.979286	10.652339	-0.048988	4.815670
236.059711	8000.022032	10.657344	-0.048976	4.815683
236.203522	7999.991265	10.662349	-0.049003	4.815673
236.266995	7999.972010	10.667354	-0.049015	4.815667
236.310641	8000.018608	10.672359	-0.049023	4.815681
236.358276	7999.973481	10.677363	-0.049032	4.815667
236.478327	8000.039458	10.682368	-0.049054	4.815686
236.219466	8000.017132	10.687373	-0.049006	4.815681
236.291075	8000.001209	10.692378	-0.049019	4.815676
236.454325	8000.045471	10.697383	-0.049050	4.815688
236.335909	7999.972045	10.702387	-0.049028	4.815667
236.175265	8000.017480	10.707392	-0.048998	4.815681
236.217454	8000.001083	10.712397	-0.049005	4.815676
236.127246	7999.990019	10.717402	-0.048989	4.815673
236.244557	8000.022864	10.722407	-0.049010	4.815682
236.230727	7999.993821	10.727411	-0.049008	4.815674
236.386121	8000.014474	10.732416	-0.049037	4.815679
236.132533	7999.997570	10.737421	-0.048990	4.815675
236.196014	7999.961237	10.742426	-0.049001	4.815665
236.316877	7999.989871	10.747431	-0.049024	4.815672
236.417156	7999.993623	10.752435	-0.049043	4.815673
236.274172	8000.000919	10.757440	-0.049016	4.815676
236.313293	7999.985539	10.762445	-0.049023	4.815671
236.509869	8000.006857	10.767450	-0.049060	4.815676
236.414335	8000.020256	10.772455	-0.049042	4.815681
236.409291	7999.965739	10.777459	-0.049041	4.815665
236.479318	7999.990350	10.782464	-0.049054	4.815672
236.397982	7999.996506	10.787469	-0.049039	4.815674
236.287938	7999.971246	10.792474	-0.049018	4.815667
236.488971	7999.984097	10.797479	-0.049056	4.815670
236.226203	7999.970247	10.802483	-0.049007	4.815667
236.322954	8000.009164	10.807488	-0.049025	4.815678
236.309045	7999.995063	10.812493	-0.049022	4.815674
236.371466	7999.946972	10.817498	-0.049034	4.815660
236.584647	8000.014454	10.822503	-0.049073	4.815678
236.401167	8000.027499	10.827507	-0.049039	4.815683
236.518470	8000.017652	10.832512	-0.049061	4.815680
236.411507	8000.003115	10.837517	-0.049041	4.815676
236.130910	8000.000717	10.842522	-0.048989	4.815676
236.285642	8000.023494	10.847527	-0.049018	4.815682
236.370447	7999.987505	10.852531	-0.049033	4.815671
236.500553	8000.024827	10.857536	-0.049058	4.815682
236.224448	8000.019299	10.862541	-0.049006	4.815681
236.253607	8000.020836	10.867546	-0.049012	4.815682
236.397590	8000.038103	10.872551	-0.049039	4.815686
236.097518	7999.986293	10.877555	-0.048983	4.815672
236.344856	7999.980680	10.882560	-0.049029	4.815670
236.420480	7999.992573	10.887565	-0.049043	4.815673
236.302720	8000.016286	10.892570	-0.049021	4.815680
236.547517	8000.025574	10.897575	-0.049066	4.815682
236.576975	7999.994029	10.902579	-0.049072	4.815672
236.418665	8000.030962	10.907584	-0.049042	4.815684
236.263679	8000.016717	10.912589	-0.049013	4.815680
236.349180	7999.998885	10.917594	-0.049029	4.815675
236.403997	8000.034991	10.922599	-0.049040	4.815685
236.286476	7999.960513	10.927603	-0.049018	4.815664
236.296017	8000.012965	10.932608	-0.049019	4.815679
236.490119	8000.015031	10.937613	-0.049056	4.815679
236.343658	7999.990250	10.942618	-0.049028	4.815672
236.410824	7999.978525	10.947623	-0.049041	4.815669
236.562514	7999.979906	10.952627	-0.049069	4.815668
236.512883	7999.962026	10.957632	-0.049060	4.815663
236.334249	7999.997564	10.962637	-0.049026	4.815675
236.467874	7999.987980	10.967642	-0.049051	4.815671
236.354084	8000.014959	10.972647	-0.049030	4.815680
236.148931	7999.977490	10.977651	-0.048992	4.815670
236.293472	8000.029987	10.982656	-0.049019	4.815684
236.314850	8000.016456	10.987661	-0.049023	4.815680
236.245352	8000.008928	10.992666	-0.049010	4.815678
236.134672	8000.038092	10.997671	-0.048989	4.815687
236.247189	7999.988676	11.002675	-0.049010	4.815672
236.395368	8000.012414	11.007680	-0.049038	4.815679
236.364555	8000.015117	11.012685	-0.049032	4.815680
236.434019	7999.998093	11.017690	-0.049045	4.815674
236.503788	8000.036575	11.022695	-0.049058	4.815685
236.456500	7999.978174	11.027699	-0.049049	4.815668
236.484772	8000.008514	11.032704	-0.049054	4.815677
236.462188	7999.995340	11.037709	-0.049050	4.815673
236.445578	8000.004677	11.042714	-0.049047	4.815676
236.425767	8000.037443	11.047719	-0.049043	4.815686
236.363716	8000.012958	11.052723	-0.049032	4.815679
236.565688	8000.019420	11.057728	-0.049069	4.815680
236.295017	8000.018250	11.062733	-0.049019	4.815681
236.274435	8000.009377	11.067738	-0.049015	4.815678
236.605045	8000.014715	11.072743	-0.049077	4.815678
236.337629	7999.989049	11.077747	-0.049027	4.815672
236.331176	8000.015626	11.082752	-0.049025	4.815680
236.567780	8000.000234	11.087757	-0.049070	4.815674
236.588634	7999.979223	11.092762	-0.049073	4.815668
236.442304	7999.991801	11.097767	-0.049046	4.815672
236.355737	7999.973324	11.102771	-0.049030	4.815667
236.369155	8000.010896	11.107776	-0.049032	4.815678
236.441917	7999.987521	11.112781	-0.049046	4.815671
236.583165	7999.993003	11.117786	-0.049072	4.815672
236.609165	8000.028644	11.122791	-0.049077	4.815682
236.369612	8000.014100	11.127795	-0.049032	4.815679
236.344839	8000.005160	11.132800	-0.049028	4.815677
236.367056	7999.991642	11.137805	-0.049032	4.815673
236.251847	8000.004723	11.142810	-0.049011	4.815677
236.656673	8000.033674	11.147815	-0.049086	4.815684
236.468237	8000.010349	11.152819	-0.049051	4.815678
236.482932	8000.005249	11.157824	-0.049053	4.815676
236.475438	8000.022204	11.162829	-0.049052	4.815681
236.548775	8000.006309	11.167834	-0.049066	4.815676
236.638846	8000.030177	11.172839	-0.049082	4.815683
236.364922	8000.015078	11.177843	-0.049031	4.815680
236.347522	8000.017998	11.182848	-0.049028	4.815680
236.410419	8000.006204	11.187853	-0.049040	4.815677
236.427437	7999.980862	11.192858	-0.049043	4.815669
236.423378	8000.019219	11.197863	-0.049042	4.815680
236.403680	7999.997553	11.202867	-0.049039	4.815674
236.481262	8000.048969	11.207872	-0.049053	4.815689
236.359482	8000.030991	11.212877	-0.049030	4.815684
236.459605	8000.027270	11.217882	-0.049049	4.815683
236.630609	8000.034299	11.222887	-0.049081	4.815684
236.580739	8000.024954	11.227891	-0.049071	4.815681
236.588334	8000.012267	11.232896	-0.049073	4.815678
236.784206	8000.039978	11.237901	-0.049109	4.815685
236.649440	8000.027127	11.242906	-0.049084	4.815682
236.498911	8000.049243	11.247911	-0.049056	4.815689
236.532404	8000.010291	11.252915	-0.049062	4.815677
236.617650	8000.012734	11.257920	-0.049078	4.815678
236.221106	7999.971107	11.262925	-0.049004	4.815667
236.388528	7999.975944	11.267930	-0.049036	4.815668
236.434573	8000.018312	11.272935	-0.049044	4.815680
236.638716	7999.981048	11.277939	-0.049082	4.815668
236.403275	8000.018871	11.282944	-0.049038	4.815680
236.684467	8000.026613	11.287949	-0.049091	4.815681
236.444094	8000.014191	11.292954	-0.049046	4.815679
236.500943	8000.001232	11.297959	-0.049056	4.815675
236.434318	7999.988414	11.302963	-0.049044	4.815671
236.545605	8000.036106	11.307968	-0.049065	4.815685
236.569008	8000.020472	11.312973	-0.049069	4.815680
236.299006	7999.985158	11.317978	-0.049019	4.815671
236.703629	8000.019442	11.322983	-0.049094	4.815679
236.414426	8000.006231	11.327987	-0.049040	4.815677
236.394016	8000.022977	11.332992	-0.049036	4.815682
236.575873	8000.028047	11.337997	-0.049070	4.815682
236.476690	8000.013636	11.343002	-0.049052	4.815679
236.658172	8000.043249	11.348007	-0.049086	4.815686
236.365724	8000.013976	11.353011	-0.049031	4.815679
236.633416	8000.046049	11.358016	-0.049081	4.815687
236.565029	8000.027866	11.363021	-0.049068	4.815682
236.446973	7999.993938	11.368026	-0.049046	4.815673
236.779619	8000.031329	11.373031	-0.049108	4.815682
236.741104	8000.011493	11.378035	-0.049101	4.815677
236.647680	8000.005713	11.383040	-0.049083	4.815675
236.629513	8000.033170	11.388045	-0.049080	4.815684
236.612378	8000.005141	11.393050	-0.049077	4.815675
236.563646	8000.029968	11.398055	-0.049068	4.815683
236.433640	7999.996915	11.403059	-0.049044	4.815674
236.628412	8000.017136	11.408064	-0.049080	4.815679
236.659229	8000.024037	11.413069	-0.049086	4.815681
236.576261	7999.987473	11.418074	-0.049070	4.815670
236.712723	8000.013157	11.423079	-0.049095	4.815677
236.734853	7999.986830	11.428083	-0.049100	4.815670
236.573688	8000.001303	11.433088	-0.049070	4.815675
236.507861	8000.015181	11.438093	-0.049057	4.815679
236.491617	8000.017052	11.443098	-0.049054	4.815680
236.660806	8000.033659	11.448103	-0.049086	4.815684
236.551440	8000.002005	11.453107	-0.049065	4.815675
236.734812	8000.030582	11.458112	-0.049099	4.815682
236.777065	8000.003512	11.463117	-0.049107	4.815674
236.288140	7999.978537	11.468122	-0.049016	4.815669
236.730862	8000.026245	11.473127	-0.049099	4.815681
236.677205	7999.998693	11.478131	-0.049089	4.815673
236.542432	8000.025333	11.483136	-0.049064	4.815682
236.522995	8000.018614	11.488141	-0.049060	4.815680
236.505318	8000.025799	11.493146	-0.049057	4.815682
236.497798	8000.027810	11.498151	-0.049055	4.815683
236.334952	7999.998496	11.503155	-0.049025	4.815675
236.678241	8000.033924	11.508160	-0.049089	4.815684
236.782907	8000.019603	11.513165	-0.049108	4.815679
236.612850	8000.037134	11.518170	-0.049077	4.815685
236.547094	8000.053149	11.523175	-0.049064	4.815690
236.566377	7999.994755	11.528179	-0.049068	4.815673
236.852471	8000.001509	11.533184	-0.049121	4.815673
236.500376	8000.015033	11.538189	-0.049056	4.815679
236.700739	8000.017200	11.543194	-0.049093	4.815679
236.724426	8000.062410	11.548199	-0.049097	4.815692
236.549691	8000.039307	11.553203	-0.049065	4.815686
236.885002	8000.048991	11.558208	-0.049127	4.815687
236.829646	8000.050230	11.563213	-0.049117	4.815688
236.549251	8000.005141	11.568218	-0.049065	4.815676
236.498080	8000.060882	11.573223	-0.049055	4.815692
236.736911	8000.030583	11.578227	-0.049099	4.815682
236.404703	8000.073247	11.583232	-0.049038	4.815696
236.497138	8000.042718	11.588237	-0.049055	4.815687
236.434705	8000.015025	11.593242	-0.049043	4.815679
236.654922	8000.026051	11.598247	-0.049084	4.815681
236.414055	7999.997611	11.603251	-0.049039	4.815674
236.588808	8000.003634	11.608256	-0.049072	4.815675
236.778943	7999.993896	11.613261	-0.049107	4.815671
236.680302	7999.951742	11.618266	-0.049089	4.815660
236.639317	8000.008715	11.623271	-0.049081	4.815676
236.916220	7999.984368	11.628275	-0.049133	4.815668
236.854682	8000.015393	11.633280	-0.049121	4.815677
236.815815	8000.021168	11.638285	-0.049114	4.815679
236.732454	7999.969655	11.643290	-0.049098	4.815665
236.874365	8000.017841	11.648295	-0.049125	4.815678
236.611144	7999.998646	11.653299	-0.049076	4.815674
236.536639	8000.007047	11.658304	-0.049062	4.815676
236.569791	8000.012918	11.663309	-0.049068	4.815678
236.493230	7999.987132	11.668314	-0.049054	4.815671
236.629527	8000.022419	11.673319	-0.049079	4.815680
236.669853	7999.999587	11.678323	-0.049087	4.815674
236.632656	8000.022467	11.683328	-0.049080	4.815680
236.586648	8000.047338	11.688333	-0.049071	4.815688
236.546689	8000.013604	11.693338	-0.049064	4.815678
236.754289	8000.036168	11.698343	-0.049102	4.815684
236.626978	7999.996753	11.703347	-0.049079	4.815673
236.773798	7999.989517	11.708352	-0.049106	4.815670
236.652194	8000.025976	11.713357	-0.049083	4.815681
236.546436	8000.003987	11.718362	-0.049064	4.815675
236.486305	8000.014756	11.723367	-0.049052	4.815679
236.458766	7999.995097	11.728371	-0.049047	4.815673
236.604074	8000.000645	11.733376	-0.049074	4.815674
236.559777	8000.000995	11.738381	-0.049066	4.815675
236.586227	8000.005690	11.743386	-0.049071	4.815676
236.589814	8000.007882	11.748391	-0.049072	4.815676
236.746809	7999.982665	11.753395	-0.049101	4.815668
236.701842	7999.987274	11.758400	-0.049092	4.815670
236.697473	8000.017088	11.763405	-0.049092	4.815679
236.553018	7999.965656	11.768410	-0.049065	4.815664
236.702836	8000.037451	11.773415	-0.049093	4.815685
236.639060	8000.026814	11.778419	-0.049081	4.815682
236.697469	8000.009611	11.783424	-0.049091	4.815676
236.631418	7999.975455	11.788429	-0.049079	4.815667
236.761824	7999.972223	11.793434	-0.049103	4.815665
236.852744	8000.015317	11.798439	-0.049120	4.815677
236.725021	7999.973761	11.803443	-0.049097	4.815666
236.605419	7999.999579	11.808448	-0.049074	4.815674
236.759369	7999.998862	11.813453	-0.049103	4.815673
236.863226	8000.013346	11.818458	-0.049122	4.815677
236.851525	7999.997145	11.823463	-0.049120	4.815672
236.680746	7999.981578	11.828467	-0.049088	4.815668
236.627759	8000.009539	11.833472	-0.049078	4.815677
236.828653	8000.017052	11.838477	-0.049116	4.815678
236.636015	8000.011804	11.843482	-0.049080	4.815677
236.583874	8000.045115	11.848487	-0.049070	4.815687
236.576413	8000.015108	11.853491	-0.049069	4.815679
236.552804	8000.017927	11.858496	-0.049064	4.815680
236.846911	8000.010936	11.863501	-0.049119	4.815676
236.760444	8000.015942	11.868506	-0.049103	4.815678
236.563378	8000.040508	11.873511	-0.049066	4.815686
236.695203	7999.998875	11.878515	-0.049091	4.815673
236.835859	8000.016088	11.883520	-0.049117	4.815678
237.006421	8000.036987	11.888525	-0.049149	4.815683
236.747340	8000.010386	11.893530	-0.049100	4.815676
236.996949	8000.044303	11.898535	-0.049147	4.815685
237.029876	8000.002139	11.903539	-0.049153	4.815673
236.771738	7999.997968	11.908544	-0.049105	4.815673
236.974743	8000.023660	11.913549	-0.049143	4.815679
236.967567	8000.002196	11.918554	-0.049141	4.815673
236.797428	8000.028265	11.923559	-0.049110	4.815681
236.760582	7999.995648	11.928563	-0.049103	4.815672
236.783790	7999.990685	11.933568	-0.049107	4.815670
236.727907	8000.022868	11.938573	-0.049097	4.815680
236.569160	7999.990418	11.943578	-0.049067	4.815671
236.820940	8000.032907	11.948583	-0.049114	4.815683
236.690182	8000.005178	11.953587	-0.049090	4.815675
236.679420	7999.975117	11.958592	-0.049088	4.815666
236.676716	7999.993217	11.963597	-0.049087	4.815672
236.632707	7999.986101	11.968602	-0.049079	4.815670
236.692404	7999.990265	11.973607	-0.049090	4.815671
236.687825	7999.945362	11.978611	-0.049089	4.815658
236.914699	7999.977843	11.983616	-0.049131	4.815666
237.020428	7999.996627	11.988621	-0.049151	4.815671
236.785328	7999.952269	11.993626	-0.049107	4.815659
236.729052	8000.014332	11.998631	-0.049097	4.815678
236.870868	7999.984601	12.003635	-0.049123	4.815668
236.676456	7999.984662	12.008640	-0.049087	4.815669
236.596396	7999.992973	12.013645	-0.049072	4.815672
236.845541	7999.979918	12.018650	-0.049118	4.815667
237.024288	8000.020161	12.023655	-0.049152	4.815678
236.928948	7999.993004	12.028659	-0.049134	4.815670
236.818111	7999.939980	12.033664	-0.049113	4.815656
236.992693	7999.987626	12.038669	-0.049146	4.815669
236.671828	7999.993116	12.043674	-0.049086	4.815672
236.884631	8000.033909	12.048679	-0.049126	4.815683
236.966273	8000.018149	12.053683	-0.049141	4.815678
236.862988	8000.000469	12.058688	-0.049121	4.815673
236.712403	8000.001237	12.063693	-0.049093	4.815674
236.846544	7999.993796	12.068698	-0.049118	4.815671
236.992825	7999.990821	12.073703	-0.049146	4.815670
236.783469	7999.971428	12.078707	-0.049107	4.815665
236.793190	7999.980122	12.083712	-0.049108	4.815667
236.746101	8000.007111	12.088717	-0.049100	4.815675
236.577897	7999.974508	12.093722	-0.049068	4.815667
236.618702	8000.016792	12.098727	-0.049076	4.815679
236.712159	7999.978808	12.103731	-0.049093	4.815667
236.593388	7999.969417	12.108736	-0.049071	4.815665
236.605665	7999.988826	12.113741	-0.049073	4.815671
236.586659	7999.978912	12.118746	-0.049070	4.815668
236.883565	8000.010390	12.123751	-0.049125	4.815676
236.735270	8000.000522	12.128755	-0.049097	4.815674
236.734299	8000.002639	12.133760	-0.049097	4.815674
237.033522	8000.030953	12.138765	-0.049153	4.815681
236.598218	7999.985496	12.143770	-0.049072	4.815670
236.871715	8000.005922	12.148775	-0.049123	4.815675
236.807710	7999.985675	12.153779	-0.049111	4.815669
236.749723	7999.967659	12.158784	-0.049100	4.815664
236.745990	8000.010291	12.163789	-0.049099	4.815676
236.623627	7999.986967	12.168794	-0.049077	4.815670
236.880912	8000.013535	12.173799	-0.049124	4.815677
236.840342	8000.011811	12.178803	-0.049117	4.815676
236.605605	7999.983470	12.183808	-0.049073	4.815669
236.842729	8000.006510	12.188813	-0.049117	4.815675
236.764223	7999.982827	12.193818	-0.049103	4.815668
236.727111	8000.003573	12.198823	-0.049096	4.815675
236.714396	7999.985221	12.203827	-0.049093	4.815669
236.780033	7999.991617	12.208832	-0.049106	4.815671
236.749100	8000.035944	12.213837	-0.049100	4.815684
236.576648	8000.019282	12.218842	-0.049068	4.815680
236.646992	8000.020417	12.223847	-0.049081	4.815680
236.709238	8000.007545	12.228851	-0.049092	4.815676
236.659547	7999.969385	12.233856	-0.049083	4.815665
236.954376	8000.002963	12.238861	-0.049138	4.815673
236.647561	7999.999074	12.243866	-0.049081	4.815674
236.677277	7999.998485	12.248871	-0.049086	4.815673
236.748864	7999.974024	12.253875	-0.049100	4.815666
236.561049	7999.937902	12.258880	-0.049065	4.815656
236.702821	7999.980749	12.263885	-0.049091	4.815668
236.651742	7999.972451	12.268890	-0.049081	4.815666
236.723340	8000.019502	12.273895	-0.049095	4.815679
236.655623	8000.019474	12.278899	-0.049082	4.815680
236.837783	8000.035223	12.283904	-0.049116	4.815683
236.974772	8000.037434	12.288909	-0.049142	4.815683
237.003695	8000.009082	12.293914	-0.049147	4.815675
236.744019	8000.017694	12.298919	-0.049099	4.815679
236.982240	7999.996992	12.303923	-0.049143	4.815671
237.034486	7999.996767	12.308928	-0.049153	4.815671
237.095189	8000.005217	12.313933	-0.049164	4.815673
236.976033	7999.993685	12.318938	-0.049142	4.815670
237.065684	7999.987661	12.323943	-0.049158	4.815668
236.967762	7999.987145	12.328947	-0.049140	4.815669
236.887538	7999.945289	12.333952	-0.049125	4.815657
236.982028	7999.956419	12.338957	-0.049143	4.815660
236.896471	7999.971046	12.343962	-0.049127	4.815664
236.779242	8000.015047	12.348967	-0.049105	4.815678
236.893791	7999.983809	12.353971	-0.049126	4.815668
236.806666	7999.982400	12.358976	-0.049110	4.815668
236.928798	8000.022796	12.363981	-0.049133	4.815679
236.832792	7999.998829	12.368986	-0.049115	4.815673
236.849915	7999.995903	12.373991	-0.049118	4.815672
236.753382	7999.972995	12.378995	-0.049100	4.815665
236.668315	7999.997236	12.384000	-0.049084	4.815673
237.062939	8000.014282	12.389005	-0.049158	4.815676
236.980866	7999.984137	12.394010	-0.049142	4.815668
236.939095	8000.011212	12.399015	-0.049135	4.815676
236.819403	7999.995402	12.404019	-0.049112	4.815672
236.789585	7999.998121	12.409024	-0.049107	4.815673
236.817427	7999.986828	12.414029	-0.049112	4.815669
236.679353	7999.983530	12.419034	-0.049086	4.815669
236.909180	7999.995779	12.424039	-0.049129	4.815671
236.871585	7999.974891	12.429043	-0.049122	4.815665
236.897619	7999.956098	12.434048	-0.049127	4.815660
237.050453	7999.989518	12.439053	-0.049155	4.815669
236.905343	7999.975432	12.444058	-0.049128	4.815665
236.905360	8000.009586	12.449063	-0.049128	4.815675
237.030115	7999.996657	12.454067	-0.049151	4.815671
237.020993	8000.014653	12.459072	-0.049150	4.815676
237.124592	8000.013123	12.464077	-0.049169	4.815675
236.777538	7999.986169	12.469082	-0.049104	4.815669
236.899404	8000.005213	12.474087	-0.049127	4.815674
236.911337	7999.995799	12.479091	-0.049129	4.815671
236.772806	8000.025580	12.484096	-0.049103	4.815681
236.843131	8000.024580	12.489101	-0.049116	4.815680
236.847276	7999.979817	12.494106	-0.049117	4.815667
236.966934	8000.008432	12.499111	-0.049139	4.815675
236.918632	7999.985236	12.504115	-0.049130	4.815668
236.949658	7999.969726	12.509120	-0.049136	4.815664
237.095554	7999.994495	12.514125	-0.049163	4.815670
236.972933	7999.992513	12.519130	-0.049140	4.815670
237.014299	8000.039076	12.524135	-0.049148	4.815684
236.820392	8000.007124	12.529139	-0.049112	4.815675
236.894471	8000.004050	12.534144	-0.049126	4.815674
237.165846	8000.009500	12.539149	-0.049176	4.815674
236.776042	7999.995731	12.544154	-0.049104	4.815672
236.868669	8000.000427	12.549159	-0.049121	4.815673
236.860606	8000.000296	12.554163	-0.049119	4.815673
236.796175	7999.997119	12.559168	-0.049107	4.815672
236.959525	8000.027507	12.564173	-0.049138	4.815680
236.826967	7999.982671	12.569178	-0.049113	4.815668
236.940798	8000.021865	12.574183	-0.049134	4.815679
237.159285	8000.002979	12.579187	-0.049175	4.815672
236.889351	8000.015695	12.584192	-0.049125	4.815677
237.005588	8000.033581	12.589197	-0.049146	4.815682
236.981923	8000.015053	12.594202	-0.049142	4.815677
236.949063	8000.056147	12.599207	-0.049136	4.815689
236.960007	7999.999753	12.604211	-0.049138	4.815672
237.161144	7999.915478	12.609216	-0.049175	4.815647
237.191194	7999.969329	12.614221	-0.049181	4.815662
236.745625	7999.989882	12.619226	-0.049098	4.815670
236.900515	8000.042548	12.624231	-0.049127	4.815685
237.063191	8000.025962	12.629235	-0.049157	4.815680
236.982073	8000.007573	12.634240	-0.049142	4.815675
236.917282	8000.024670	12.639245	-0.049130	4.815680
236.926180	7999.999196	12.644250	-0.049131	4.815672
237.088756	8000.056255	12.649255	-0.049162	4.815688
237.092907	7999.994415	12.654259	-0.049162	4.815670
236.994338	8000.014168	12.659264	-0.049144	4.815676
237.057433	8000.050408	12.664269	-0.049156	4.815687
236.810541	7999.984513	12.669274	-0.049110	4.815669
236.709505	7999.990351	12.674279	-0.049091	4.815671
236.884566	7999.998514	12.679283	-0.049124	4.815672
236.871188	7999.959872	12.684288	-0.049121	4.815661
236.770647	8000.004143	12.689293	-0.049102	4.815675
236.935341	8000.002532	12.694298	-0.049133	4.815673
237.016407	8000.024120	12.699303	-0.049148	4.815679
236.975130	7999.999970	12.704307	-0.049140	4.815672
237.075855	7999.973845	12.709312	-0.049159	4.815664
237.174072	7999.997844	12.714317	-0.049177	4.815671
236.964271	7999.956029	12.719322	-0.049138	4.815660
236.968214	7999.998786	12.724327	-0.049139	4.815672
236.832535	8000.014738	12.729331	-0.049114	4.815677
236.963502	8000.008313	12.734336	-0.049138	4.815675
236.824238	8000.015668	12.739341	-0.049112	4.815678
236.951582	7999.973962	12.744346	-0.049136	4.815665
236.892690	7999.982616	12.749351	-0.049125	4.815668
236.896954	8000.015771	12.754355	-0.049126	4.815677
237.000168	7999.974743	12.759360	-0.049145	4.815665
237.204236	8000.018597	12.764365	-0.049183	4.815677
237.096493	7999.979498	12.769370	-0.049163	4.815666
236.990795	8000.015147	12.774375	-0.049143	4.815677
236.908071	8000.013809	12.779379	-0.049128	4.815677
236.830754	7999.979471	12.784384	-0.049113	4.815667
236.867631	8000.073992	12.789389	-0.049120	4.815695
236.823502	8000.063672	12.794394	-0.049112	4.815692
236.962946	8000.060586	12.799399	-0.049138	4.815690
236.840739	8000.007378	12.804403	-0.049115	4.815675
236.857058	7999.979890	12.809408	-0.049118	4.815667
236.898050	7999.998695	12.814413	-0.049126	4.815672
236.732233	7999.987477	12.819418	-0.049095	4.815670
236.566387	8000.014683	12.824423	-0.049064	4.815679
236.601533	7999.982161	12.829427	-0.049070	4.815669
236.829586	7999.977304	12.834432	-0.049113	4.815666
236.761406	8000.042377	12.839437	-0.049100	4.815686
236.729017	8000.001294	12.844442	-0.049094	4.815674
236.644036	8000.038344	12.849447	-0.049078	4.815685
236.692394	8000.018844	12.854451	-0.049087	4.815679
236.610916	8000.028200	12.859456	-0.049072	4.815682
236.805403	8000.032407	12.864461	-0.049108	4.815683
236.700977	8000.011507	12.869466	-0.049089	4.815677
236.700447	7999.999757	12.874471	-0.049089	4.815674
236.585587	7999.973351	12.879475	-0.049067	4.815666
236.802820	8000.005677	12.884480	-0.049108	4.815675
236.839131	8000.037215	12.889485	-0.049114	4.815684
236.830716	7999.973037	12.894490	-0.049113	4.815665
236.868415	8000.027012	12.899495	-0.049120	4.815681
236.904607	8000.047874	12.904499	-0.049127	4.815687
236.817197	8000.015508	12.909504	-0.049110	4.815678
236.942176	8000.043142	12.914509	-0.049134	4.815685
236.783672	7999.993617	12.919514	-0.049104	4.815671
236.795796	8000.004485	12.924519	-0.049106	4.815675
236.689116	8000.005963	12.929523	-0.049086	4.815675
236.822958	8000.001719	12.934528	-0.049111	4.815674
237.009107	8000.015398	12.939533	-0.049146	4.815677
236.857796	7999.991606	12.944538	-0.049118	4.815670
236.844520	7999.983918	12.949543	-0.049115	4.815668
236.952202	8000.013407	12.954547	-0.049135	4.815676
236.866443	8000.018425	12.959552	-0.049119	4.815678
236.921903	8000.050272	12.964557	-0.049130	4.815687
236.735881	8000.018448	12.969562	-0.049095	4.815679
236.674066	8000.046266	12.974567	-0.049083	4.815687
236.903257	8000.023283	12.979571	-0.049126	4.815680
236.692920	7999.999605	12.984576	-0.049087	4.815674
236.802709	8000.048340	12.989581	-0.049107	4.815687
236.625912	8000.023069	12.994586	-0.049074	4.815681
236.976720	8000.051148	12.999591	-0.049140	4.815687
236.788958	8000.029969	13.004595	-0.049105	4.815682
236.778986	8000.013796	13.009600	-0.049103	4.815677
236.890048	8000.035869	13.014605	-0.049124	4.815683
236.899020	8000.003992	13.019610	-0.049125	4.815674
236.948597	8000.025071	13.024615	-0.049134	4.815680
236.892568	8000.001750	13.029619	-0.049124	4.815673
236.946636	8000.012228	13.034624	-0.049134	4.815676
237.119170	8000.016081	13.039629	-0.049166	4.815676
236.710367	7999.981726	13.044634	-0.049090	4.815668
236.889641	8000.005967	13.049639	-0.049123	4.815675
236.833484	8000.003991	13.054643	-0.049113	4.815674
236.676178	8000.031335	13.059648	-0.049084	4.815683
236.904856	8000.027555	13.064653	-0.049126	4.815681
236.790089	7999.981939	13.069658	-0.049105	4.815668
236.797553	8000.021550	13.074663	-0.049106	4.815680
236.968557	8000.028580	13.079667	-0.049138	4.815681
237.106309	7999.999851	13.084672	-0.049164	4.815672
236.954373	8000.004867	13.089677	-0.049135	4.815674
236.728936	7999.924376	13.094682	-0.049093	4.815651
237.044632	7999.924136	13.099687	-0.049152	4.815650
237.232544	7999.980538	13.104691	-0.049187	4.815665
237.058879	7999.928633	13.109696	-0.049155	4.815651
237.036921	8000.013665	13.114701	-0.049151	4.815676
236.965260	8000.010371	13.119706	-0.049137	4.815675
237.045970	7999.998865	13.124711	-0.049152	4.815672
237.022006	8000.020891	13.129715	-0.049148	4.815678
237.238289	8000.010508	13.134720	-0.049188	4.815674
237.207958	8000.032431	13.139725	-0.049182	4.815681
236.891330	8000.017709	13.144730	-0.049123	4.815678
237.085361	8000.032583	13.149735	-0.049159	4.815681
237.179608	8000.015959	13.154739	-0.049177	4.815676
236.984787	8000.005339	13.159744	-0.049141	4.815674
236.994587	8000.043921	13.164749	-0.049143	4.815685
236.993645	7999.992671	13.169754	-0.049142	4.815670
237.208869	8000.022830	13.174759	-0.049182	4.815678
237.119266	7999.988294	13.179763	-0.049166	4.815668
236.991136	8000.003300	13.184768	-0.049142	4.815673
237.288622	8000.033721	13.189773	-0.049197	4.815681
237.258781	7999.990543	13.194778	-0.049192	4.815668
237.374236	7999.962521	13.199783	-0.049213	4.815660
237.200665	7999.981063	13.204787	-0.049181	4.815666
237.090562	8000.002765	13.209792	-0.049160	4.815673
237.115691	8000.018112	13.214797	-0.049165	4.815677
237.197924	8000.013035	13.219802	-0.049180	4.815675
237.219875	8000.000580	13.224807	-0.049184	4.815671
237.219039	8000.009104	13.229811	-0.049184	4.815674
237.130125	8000.009801	13.234816	-0.049167	4.815675
237.241325	7999.999855	13.239821	-0.049188	4.815671
237.252587	7999.972285	13.244826	-0.049190	4.815663
237.091916	7999.987833	13.249831	-0.049160	4.815668
237.336324	7999.981106	13.254835	-0.049206	4.815665
237.047565	8000.005259	13.259840	-0.049152	4.815674
237.252498	8000.034184	13.264845	-0.049190	4.815681
237.089952	8000.016614	13.269850	-0.049160	4.815677
237.216926	8000.013327	13.274855	-0.049184	4.815675
237.216980	7999.999451	13.279859	-0.049184	4.815671
237.034701	8000.065883	13.284864	-0.049150	4.815691
237.062408	8000.078070	13.289869	-0.049155	4.815695
236.986423	8000.014935	13.294874	-0.049141	4.815677
236.963600	8000.040181	13.299879	-0.049136	4.815684
237.064419	7999.994845	13.304883	-0.049155	4.815670
236.924271	8000.007523	13.309888	-0.049129	4.815675
237.069003	8000.028004	13.314893	-0.049156	4.815680
236.942560	7999.980065	13.319898	-0.049132	4.815667
237.105361	8000.017915	13.324903	-0.049163	4.815677
237.021226	8000.008016	13.329907	-0.049147	4.815675
236.834739	7999.974050	13.334912	-0.049112	4.815665
237.027745	8000.012388	13.339917	-0.049148	4.815676
236.944773	7999.976891	13.344922	-0.049133	4.815666
236.979228	8000.014804	13.349927	-0.049139	4.815677
236.889330	8000.012283	13.354931	-0.049122	4.815676
236.942444	7999.996062	13.359936	-0.049132	4.815671
237.045527	8000.029746	13.364941	-0.049151	4.815681
237.142348	7999.973672	13.369946	-0.049169	4.815664
237.098571	7999.982569	13.374951	-0.049161	4.815667
237.154279	7999.996276	13.379955	-0.049172	4.815670
236.976554	7999.974192	13.384960	-0.049138	4.815665
237.147917	8000.020720	13.389965	-0.049170	4.815678
237.181989	7999.995652	13.394970	-0.049177	4.815670
236.949790	7999.998304	13.399975	-0.049133	4.815672
236.980880	8000.009479	13.404979	-0.049139	4.815675
237.030184	7999.973984	13.409984	-0.049148	4.815665
237.067584	8000.023685	13.414989	-0.049155	4.815679
236.900622	8000.002842	13.419994	-0.049124	4.815674
237.118630	7999.986082	13.424999	-0.049165	4.815668
237.060797	8000.013965	13.430003	-0.049154	4.815676
237.004157	8000.000240	13.435008	-0.049143	4.815672
237.277943	8000.028143	13.440013	-0.049194	4.815679
237.102837	7999.998630	13.445018	-0.049162	4.815671
237.207132	8000.007784	13.450023	-0.049181	4.815674
237.249034	7999.983911	13.455027	-0.049189	4.815666
237.183009	8000.024470	13.460032	-0.049177	4.815679
237.080125	8000.042019	13.465037	-0.049157	4.815684
236.833779	8000.014556	13.470042	-0.049112	4.815677
237.140220	8000.031246	13.475047	-0.049169	4.815681
236.980821	8000.027602	13.480051	-0.049139	4.815680
237.003495	8000.003418	13.485056	-0.049143	4.815673
236.960395	8000.035808	13.490061	-0.049135	4.815683
236.993499	8000.003254	13.495066	-0.049141	4.815673
236.974429	8000.018955	13.500071	-0.049138	4.815678
237.137102	8000.010908	13.505075	-0.049168	4.815675
237.098505	7999.999609	13.510080	-0.049161	4.815672
237.120879	7999.993565	13.515085	-0.049165	4.815670
237.014121	7999.972627	13.520090	-0.049145	4.815664
237.018759	7999.981240	13.525095	-0.049146	4.815667
237.049396	7999.964655	13.530099	-0.049152	4.815662
236.967148	7999.977201	13.535104	-0.049136	4.815666
237.313992	8000.014823	13.540109	-0.049201	4.815675
237.271035	7999.999185	13.545114	-0.049193	4.815671
237.171235	8000.026390	13.550119	-0.049174	4.815679
237.240927	8000.018975	13.555123	-0.049187	4.815677
237.167477	8000.017787	13.560128	-0.049173	4.815677
237.080292	7999.981155	13.565133	-0.049157	4.815666
236.887671	7999.836087	13.570138	-0.049121	4.815625
237.286202	7999.941785	13.575143	-0.049195	4.815654
237.219256	7999.960981	13.580147	-0.049183	4.815660
237.228566	7999.952592	13.585152	-0.049185	4.815657
237.411399	7999.977958	13.590157	-0.049219	4.815664
237.297579	7999.976118	13.595162	-0.049198	4.815664
237.284460	7999.983376	13.600167	-0.049195	4.815666
237.297014	8000.005992	13.605171	-0.049197	4.815673
237.226408	7999.970695	13.610176	-0.049184	4.815663
237.129388	8000.019292	13.615181	-0.049166	4.815677
237.041099	7999.991181	13.620186	-0.049150	4.815670
237.342791	8000.009928	13.625191	-0.049206	4.815674
237.372182	8000.020008	13.630195	-0.049211	4.815676
237.289859	8000.016542	13.635200	-0.049196	4.815676
237.421672	8000.045354	13.640205	-0.049221	4.815684
237.567426	8000.028495	13.645210	-0.049248	4.815678
237.381033	8000.050032	13.650215	-0.049213	4.815685
237.414166	8000.008939	13.655219	-0.049219	4.815673
237.361011	7999.957913	13.660224	-0.049209	4.815658
237.348895	8000.037767	13.665229	-0.049207	4.815682
237.375539	7999.994435	13.670234	-0.049212	4.815669
237.372075	8000.005051	13.675239	-0.049211	4.815672
237.399782	8000.017238	13.680243	-0.049216	4.815675
237.237566	8000.002875	13.685248	-0.049186	4.815672
237.446394	8000.026528	13.690253	-0.049225	4.815678
237.240384	8000.024265	13.695258	-0.049187	4.815678
237.287922	8000.044244	13.700263	-0.049195	4.815684
237.247917	8000.030788	13.705267	-0.049188	4.815680
237.315780	8000.037220	13.710272	-0.049201	4.815682
237.318087	8000.023380	13.715277	-0.049201	4.815678
237.378907	7999.991274	13.720282	-0.049212	4.815668
237.301628	7999.983620	13.725287	-0.049198	4.815666
237.403135	8000.018346	13.730291	-0.049217	4.815676
237.241742	8000.008266	13.735296	-0.049187	4.815674
237.371336	8000.027436	13.740301	-0.049211	4.815679
237.233444	7999.971839	13.745306	-0.049185	4.815663
237.295649	8000.000594	13.750311	-0.049197	4.815671
237.238680	8000.028491	13.755315	-0.049186	4.815680
237.275964	7999.976791	13.760320	-0.049193	4.815664
237.379279	8000.019019	13.765325	-0.049212	4.815676
237.047849	7999.981643	13.770330	-0.049150	4.815667
237.001164	7999.990493	13.775335	-0.049142	4.815670
237.147019	7999.982175	13.780339	-0.049169	4.815666
237.063696	7999.957346	13.785344	-0.049153	4.815660
237.267775	8000.020413	13.790349	-0.049191	4.815677
237.007470	8000.014072	13.795354	-0.049143	4.815676
237.371747	8000.033830	13.800359	-0.049211	4.815680
237.192776	8000.023466	13.805363	-0.049177	4.815678
237.183990	7999.997707	13.810368	-0.049176	4.815671
237.239256	8000.047696	13.815373	-0.049186	4.815685
237.235171	7999.988924	13.820378	-0.049185	4.815668
237.202898	7999.989469	13.825383	-0.049179	4.815668
237.329424	8000.024600	13.830387	-0.049203	4.815678
237.371947	7999.987928	13.835392	-0.049211	4.815667
237.361111	8000.031513	13.840397	-0.049209	4.815680
237.156298	8000.023934	13.845402	-0.049170	4.815679
237.261858	8000.016031	13.850407	-0.049190	4.815676
237.369653	8000.050859	13.855411	-0.049210	4.815685
237.360092	7999.999470	13.860416	-0.049208	4.815670
237.381250	8000.026495	13.865421	-0.049212	4.815678
237.457874	7999.985037	13.870426	-0.049227	4.815666
237.358814	8000.002648	13.875431	-0.049208	4.815671
237.342219	8000.030130	13.880435	-0.049205	4.815680
237.491116	7999.998378	13.885440	-0.049233	4.815670
237.404436	8000.034334	13.890445	-0.049217	4.815680
237.260142	8000.011722	13.895450	-0.049190	4.815675
237.348468	8000.024888	13.900455	-0.049206	4.815678
237.426338	8000.024010	13.905459	-0.049221	4.815677
237.354449	8000.026050	13.910464	-0.049207	4.815678
237.499854	8000.018791	13.915469	-0.049234	4.815675
237.389885	8000.002070	13.920474	-0.049214	4.815671
237.067041	8000.011796	13.925479	-0.049154	4.815675
237.166291	8000.025139	13.930483	-0.049172	4.815679
237.243185	7999.989023	13.935488	-0.049186	4.815668
237.115825	8000.015782	13.940493	-0.049163	4.815676
237.175103	7999.997526	13.945498	-0.049174	4.815671
237.315924	8000.027551	13.950503	-0.049200	4.815679
237.264116	8000.010702	13.955507	-0.049190	4.815674
237.137519	8000.013993	13.960512	-0.049167	4.815676
237.348459	8000.040881	13.965517	-0.049206	4.815683
237.377894	8000.000795	13.970522	-0.049211	4.815671
237.386373	8000.035087	13.975527	-0.049213	4.815681
237.534390	8000.022534	13.980531	-0.049240	4.815676
237.401320	7999.996900	13.985536	-0.049216	4.815670
237.514642	8000.039290	13.990541	-0.049237	4.815681
237.372435	7999.981488	13.995546	-0.049210	4.815665
237.286927	7999.997183	14.000551	-0.049194	4.815670
237.181202	8000.025360	14.005555	-0.049175	4.815679
237.119103	7999.999806	14.010560	-0.049163	4.815672
237.346059	8000.023751	14.015565	-0.049205	4.815678
237.307424	8000.000711	14.020570	-0.049198	4.815671
237.406615	8000.001245	14.025575	-0.049216	4.815671
237.144446	8000.025826	14.030579	-0.049168	4.815679
237.361039	7999.941801	14.035584	-0.049208	4.815654
237.233459	8000.009117	14.040589	-0.049184	4.815674
237.213143	7999.999181	14.045594	-0.049180	4.815671
237.392538	8000.026627	14.050599	-0.049214	4.815678
237.268471	8000.033160	14.055603	-0.049191	4.815681
237.347902	7999.990680	14.060608	-0.049205	4.815668
237.370137	8000.016655	14.065613	-0.049210	4.815675
237.454632	8000.031894	14.070618	-0.049225	4.815680
237.379097	8000.027470	14.075623	-0.049211	4.815679
237.295950	8000.027193	14.080627	-0.049196	4.815679
237.541652	8000.017286	14.085632	-0.049241	4.815675
237.341442	8000.049272	14.090637	-0.049204	4.815685
237.261776	8000.035176	14.095642	-0.049189	4.815681
237.358541	8000.017525	14.100647	-0.049207	4.815676
237.453959	8000.010527	14.105651	-0.049225	4.815673
237.298404	7999.986665	14.110656	-0.049196	4.815667
237.476766	8000.009825	14.115661	-0.049229	4.815673
237.447202	8000.007211	14.120666	-0.049224	4.815672
237.313993	8000.013597	14.125671	-0.049199	4.815675
237.499476	8000.022996	14.130675	-0.049233	4.815677
237.274743	7999.988411	14.135680	-0.049192	4.815668
237.245183	8000.007144	14.140685	-0.049186	4.815673
237.162691	7999.984463	14.145690	-0.049171	4.815667
237.332310	8000.020290	14.150695	-0.049202	4.815677
237.332031	8000.019217	14.155699	-0.049202	4.815676
237.172023	8000.017698	14.160704	-0.049172	4.815677
237.215605	8000.022670	14.165709	-0.049181	4.815678
237.231104	7999.989831	14.170714	-0.049183	4.815668
237.140038	7999.999032	14.175719	-0.049166	4.815671
237.156222	8000.009966	14.180723	-0.049169	4.815675
237.205661	8000.018234	14.185728	-0.049179	4.815677
237.243229	8000.027379	14.190733	-0.049186	4.815679
237.155064	8000.001404	14.195738	-0.049169	4.815672
237.174504	8000.002784	14.200743	-0.049173	4.815672
237.348150	8000.018396	14.205747	-0.049205	4.815676
237.266705	7999.973318	14.210752	-0.049190	4.815663
237.361618	8000.028217	14.215757	-0.049208	4.815679
237.474158	8000.009754	14.220762	-0.049228	4.815673
237.369582	8000.046488	14.225767	-0.049209	4.815684
237.349637	8000.050434	14.230771	-0.049205	4.815685
237.404544	8000.038511	14.235776	-0.049215	4.815682
237.440241	8000.043356	14.240781	-0.049222	4.815683
237.323951	8000.013725	14.245786	-0.049200	4.815675
237.230355	8000.042097	14.250791	-0.049183	4.815684
237.357850	8000.032415	14.255795	-0.049207	4.815680
237.342625	7999.144150	14.260800	-0.049203	4.815420

237.457246	7995.971079	14.265805	-0.049223	4.814492
237.439099	7990.528432	14.270810	-0.049216	4.812899
237.224364	7983.886986	14.275815	-0.049171	4.810956
237.219274	7976.637637	14.280819	-0.049166	4.808833
237.229287	7968.995423	14.285824	-0.049162	4.806594
237.363985	7961.186168	14.290829	-0.049182	4.804304
237.092109	7953.370227	14.295834	-0.049127	4.802013
237.131724	7945.339350	14.300839	-0.049129	4.799657
237.067655	7937.470383	14.305843	-0.049112	4.797347
237.169500	7929.377018	14.310848	-0.049125	4.794970
237.153156	7921.420855	14.315853	-0.049117	4.792632
237.061209	7913.365602	14.320858	-0.049095	4.790264
237.133226	7905.411094	14.325863	-0.049103	4.787924
236.963815	7897.422153	14.330867	-0.049066	4.785574
237.130542	7889.414177	14.335872	-0.049092	4.783216
237.032426	7881.422472	14.340877	-0.049069	4.780862
236.850139	7873.414582	14.345882	-0.049029	4.778503
236.896813	7865.432733	14.350887	-0.049033	4.776149
236.956865	7857.393613	14.355891	-0.049039	4.773777
236.783308	7849.384105	14.360896	-0.049001	4.771414
236.842509	7841.363538	14.365901	-0.049007	4.769045
236.849731	7833.418151	14.370906	-0.049003	4.766698
236.888509	7825.334509	14.375911	-0.049005	4.764308
236.712365	7817.412815	14.380915	-0.048967	4.761966
236.746422	7809.353003	14.385920	-0.048968	4.759581
236.605193	7801.433356	14.390925	-0.048937	4.757237
236.731756	7793.396311	14.395930	-0.048955	4.754856
236.492391	7785.288670	14.400935	-0.048905	4.752455
236.606381	7777.340629	14.405939	-0.048921	4.750098
236.526695	7769.322899	14.410944	-0.048901	4.747720
236.533091	7761.321687	14.415949	-0.048897	4.745345
236.355777	7753.375174	14.420954	-0.048859	4.742986
236.382183	7745.338067	14.425959	-0.048859	4.740598
236.284929	7737.392005	14.430963	-0.048835	4.738237
236.327266	7729.316944	14.435968	-0.048838	4.735836
236.328262	7721.338948	14.440973	-0.048833	4.733462
236.046488	7713.312027	14.445978	-0.048775	4.731073
236.189280	7705.256427	14.450983	-0.048796	4.728674
236.351698	7697.304553	14.455987	-0.048821	4.726304
236.180696	7689.290917	14.460992	-0.048784	4.723915
236.050765	7681.376979	14.465997	-0.048755	4.721555
236.291632	7673.324738	14.471002	-0.048795	4.719151
236.416060	7665.388476	14.476007	-0.048813	4.716781
236.308227	7657.343585	14.481011	-0.048787	4.714378
236.185692	7649.277671	14.486016	-0.048759	4.711968
236.146423	7641.291712	14.491021	-0.048747	4.709580
235.922136	7633.307437	14.496026	-0.048700	4.707192
235.877506	7625.288960	14.501031	-0.048686	4.704791
235.990777	7617.351767	14.506035	-0.048702	4.702414
235.879430	7609.262888	14.511040	-0.048676	4.699990
235.847887	7601.345324	14.516045	-0.048665	4.697617
235.769897	7593.292056	14.521050	-0.048645	4.695201
235.787224	7585.259155	14.526055	-0.048643	4.692790
235.814009	7577.308400	14.531059	-0.048643	4.690403
235.729888	7569.277940	14.536064	-0.048622	4.687991
235.746132	7561.225212	14.541069	-0.048620	4.685570
235.893066	7553.288399	14.546074	-0.048642	4.683183
235.723350	7545.304159	14.551079	-0.048605	4.680781
235.974100	7537.332399	14.556083	-0.048647	4.678381
235.583525	7529.282829	14.561088	-0.048569	4.675957
235.400084	7521.230253	14.566093	-0.048529	4.673530
235.655119	7513.156943	14.571098	-0.048571	4.671096
235.517813	7505.171986	14.576103	-0.048541	4.668687
235.584061	7497.218911	14.581107	-0.048548	4.666287
235.473280	7489.215493	14.586112	-0.048522	4.663870
235.386211	7481.241153	14.591117	-0.048500	4.661461
235.419513	7473.224926	14.596122	-0.048501	4.659037
235.320761	7465.287774	14.601127	-0.048478	4.656637
235.388050	7457.254183	14.606131	-0.048485	4.654206
235.159065	7449.212594	14.611136	-0.048437	4.651771
235.300535	7441.175258	14.616141	-0.048458	4.649336
235.195116	7433.234166	14.621146	-0.048433	4.646930
235.152876	7425.191365	14.626151	-0.048420	4.644491
235.379154	7417.272697	14.631155	-0.048457	4.642088
235.109313	7409.234772	14.636160	-0.048402	4.639648
235.056172	7401.282733	14.641165	-0.048387	4.637233
234.767155	7393.214347	14.646170	-0.048328	4.634781
234.845587	7385.185724	14.651175	-0.048337	4.632340
235.116600	7377.210769	14.656179	-0.048382	4.629914
235.071750	7369.180138	14.661184	-0.048369	4.627470
235.092665	7361.177396	14.666189	-0.048367	4.625033
234.915934	7353.228967	14.671194	-0.048329	4.622611
234.911271	7345.176306	14.676199	-0.048323	4.620156
234.809111	7337.232301	14.681203	-0.048299	4.617733
234.749036	7329.195347	14.686208	-0.048282	4.615281
234.718531	7321.183134	14.691213	-0.048272	4.612834
234.767513	7313.133266	14.696218	-0.048275	4.610375
234.634798	7305.183788	14.701223	-0.048245	4.607945
234.676718	7297.167994	14.706227	-0.048248	4.605494
234.648879	7289.179994	14.711232	-0.048238	4.603050
234.685362	7281.182923	14.716237	-0.048239	4.600601
234.620265	7273.218779	14.721242	-0.048222	4.598162
234.676381	7265.158895	14.726247	-0.048227	4.595692
234.744396	7257.150131	14.731251	-0.048234	4.593236
234.561157	7249.092219	14.736256	-0.048195	4.590764
234.663112	7241.139776	14.741261	-0.048209	4.588322
234.457634	7233.110973	14.746266	-0.048165	4.585856
234.336252	7225.142221	14.751271	-0.048138	4.583408
234.445296	7217.110144	14.756275	-0.048153	4.580938
234.510592	7209.099742	14.761280	-0.048160	4.578474
234.542352	7201.179935	14.766285	-0.048160	4.576036
234.307720	7193.171999	14.771290	-0.048111	4.573570
234.282613	7185.122155	14.776295	-0.048101	4.571089
234.395021	7177.124776	14.781299	-0.048117	4.568624
234.203291	7169.097466	14.786304	-0.048076	4.566148
234.326169	7161.117787	14.791309	-0.048094	4.563685
234.430333	7153.162673	14.796314	-0.048108	4.561229
234.049716	7145.142282	14.801319	-0.048032	4.558750
234.145708	7137.208969	14.806323	-0.048045	4.556298
234.157103	7129.126933	14.811328	-0.048041	4.553798
234.071899	7121.106310	14.816333	-0.048020	4.551316
234.048015	7113.088771	14.821338	-0.048011	4.548833
234.068890	7105.097544	14.826343	-0.048009	4.546357
234.118473	7097.115542	14.831347	-0.048013	4.543883
233.850057	7089.126664	14.836352	-0.047958	4.541405
233.890217	7081.127310	14.841357	-0.047960	4.538922
234.007385	7073.177078	14.846362	-0.047977	4.536454
233.845245	7065.116398	14.851367	-0.047942	4.533950
233.685078	7057.158633	14.856371	-0.047906	4.531476
233.825525	7049.061724	14.861376	-0.047927	4.528958
233.746655	7041.095188	14.866381	-0.047907	4.526479
233.535429	7033.106948	14.871386	-0.047863	4.523991
233.522151	7025.157789	14.876391	-0.047855	4.521515
233.533858	7017.158736	14.881395	-0.047852	4.519022
233.613910	7009.161565	14.886400	-0.047862	4.516528
233.687579	7001.101823	14.891405	-0.047870	4.514013
233.561237	6993.023201	14.896410	-0.047842	4.511490
233.490690	6985.006637	14.901415	-0.047823	4.508986
233.564121	6977.097175	14.906419	-0.047832	4.506514
233.561488	6969.055973	14.911424	-0.047826	4.503999
233.570035	6961.128892	14.916429	-0.047822	4.501519
233.440971	6953.101775	14.921434	-0.047793	4.499005
233.377062	6945.082578	14.926439	-0.047776	4.496493
233.408166	6937.058025	14.931443	-0.047776	4.493978
233.073844	6929.059440	14.936448	-0.047709	4.491468
233.187828	6921.053048	14.941453	-0.047725	4.488956
233.048351	6913.044724	14.946458	-0.047694	4.486442
233.078550	6905.039200	14.951463	-0.047694	4.483927
232.996718	6897.110838	14.956467	-0.047674	4.481434
233.104466	6889.059847	14.961472	-0.047689	4.478903
233.118656	6881.069941	14.966477	-0.047686	4.476389
232.839652	6873.060027	14.971482	-0.047629	4.473866
232.798862	6864.984686	14.976487	-0.047616	4.471322
232.878829	6857.034369	14.981491	-0.047626	4.468816
232.820466	6849.039634	14.986496	-0.047609	4.466294
232.716845	6841.048995	14.991501	-0.047585	4.463772
232.881994	6833.095260	14.996506	-0.047611	4.461262
232.704237	6825.050372	15.001511	-0.047572	4.458719
232.772901	6817.095942	15.006515	-0.047580	4.456205
232.666157	6808.994261	15.011520	-0.047555	4.453642
232.646771	6800.979015	15.016525	-0.047546	4.451106
232.820703	6792.993431	15.021530	-0.047573	4.448578
232.608507	6785.020393	15.026535	-0.047528	4.446051
232.565313	6777.018204	15.031539	-0.047515	4.443514
232.402380	6769.027161	15.036544	-0.047479	4.440979
232.613707	6761.023782	15.041549	-0.047513	4.438440
232.608279	6753.047601	15.046554	-0.047507	4.435907
232.612016	6744.967804	15.051559	-0.047503	4.433339
232.563691	6736.949402	15.056563	-0.047488	4.430790
232.515700	6728.940543	15.061568	-0.047474	4.428242
232.697217	6720.966267	15.066573	-0.047503	4.425705
232.516234	6712.982331	15.071578	-0.047464	4.423161
232.422433	6704.970400	15.076583	-0.047441	4.420608
232.504118	6697.045612	15.081587	-0.047451	4.418082
232.466000	6688.985338	15.086592	-0.047439	4.415510
232.192267	6680.981405	15.091597	-0.047383	4.412954
232.188257	6672.981834	15.096602	-0.047377	4.410399
232.225161	6664.984294	15.101607	-0.047378	4.407843
232.173174	6656.986982	15.106611	-0.047363	4.405285
232.055541	6648.987625	15.111616	-0.047336	4.402725
232.233714	6640.965605	15.116621	-0.047364	4.400158
232.160547	6633.008968	15.121626	-0.047345	4.397609
232.026482	6624.958698	15.126631	-0.047315	4.395028
232.023696	6616.998535	15.131635	-0.047309	4.392475
232.019037	6608.967177	15.136640	-0.047303	4.389898
231.946921	6600.979648	15.141645	-0.047285	4.387333
231.987645	6592.976351	15.146650	-0.047287	4.384762
232.006243	6584.999501	15.151655	-0.047285	4.382198
232.194145	6576.997056	15.156659	-0.047315	4.379625
231.795136	6569.021722	15.161664	-0.047236	4.377056
231.814586	6561.003692	15.166669	-0.047234	4.374474
231.869038	6552.992642	15.171674	-0.047239	4.371893
231.666950	6544.975706	15.176679	-0.047196	4.369307
231.770878	6536.998352	15.181683	-0.047210	4.366734
231.692084	6528.965400	15.186688	-0.047190	4.364141
231.571271	6521.051149	15.191693	-0.047162	4.361584
231.535330	6513.020158	15.196698	-0.047151	4.358988
231.706037	6504.983082	15.201703	-0.047177	4.356390
231.771363	6497.008816	15.206707	-0.047184	4.353811
231.571165	6488.871149	15.211712	-0.047141	4.351175
231.611209	6480.927207	15.216717	-0.047144	4.348602
231.634784	6472.943046	15.221722	-0.047143	4.346014
231.525636	6464.959687	15.226727	-0.047117	4.343424
231.524580	6456.976930	15.231731	-0.047112	4.340833
231.452688	6448.955286	15.236736	-0.047093	4.338228
231.490156	6440.968799	15.241741	-0.047095	4.335633
231.531470	6432.976443	15.246746	-0.047097	4.333035
231.320156	6424.923420	15.251751	-0.047053	4.330414
231.374748	6416.954814	15.256755	-0.047058	4.327820
231.074517	6408.969189	15.261760	-0.046997	4.325217
231.183839	6400.977359	15.266765	-0.047012	4.322614
231.222929	6392.946920	15.271770	-0.047014	4.319995
230.950689	6384.987781	15.276775	-0.046958	4.317396
231.190392	6376.946202	15.281779	-0.046997	4.314772
231.249922	6368.928910	15.286784	-0.047003	4.312154
231.074200	6360.931548	15.291789	-0.046965	4.309538
230.968940	6352.945084	15.296794	-0.046940	4.306925
231.269093	6344.900433	15.301799	-0.046991	4.304294
231.227774	6336.968876	15.306803	-0.046978	4.301696
230.894259	6328.949220	15.311808	-0.046911	4.299066
231.084735	6320.967484	15.316813	-0.046941	4.296450
231.031540	6312.918545	15.321818	-0.046926	4.293809
231.004367	6304.874891	15.326823	-0.046916	4.291168
230.889552	6296.908710	15.331827	-0.046889	4.288550
230.875876	6288.901218	15.336832	-0.046881	4.285918
230.937034	6280.920478	15.341837	-0.046887	4.283294
230.795375	6272.951706	15.346842	-0.046856	4.280670
230.850470	6264.951528	15.351847	-0.046861	4.278036
230.770667	6256.952195	15.356851	-0.046841	4.275399
230.619595	6248.918054	15.361856	-0.046807	4.272749
230.602449	6240.861781	15.366861	-0.046799	4.270091
230.726923	6232.889970	15.371866	-0.046817	4.267461
230.651375	6224.842410	15.376871	-0.046798	4.264802
230.388777	6216.965475	15.381875	-0.046744	4.262196
230.365905	6208.898225	15.386880	-0.046734	4.259527
230.456482	6200.940452	15.391885	-0.046746	4.256894
230.363372	6192.918180	15.396890	-0.046723	4.254237
230.424748	6184.890085	15.401895	-0.046729	4.251577
230.330829	6176.911813	15.406899	-0.046707	4.248931
230.077405	6168.921409	15.411904	-0.046654	4.246278
230.152523	6160.889196	15.416909	-0.046663	4.243612
230.316306	6152.936520	15.421914	-0.046688	4.240972
229.892342	6144.942709	15.426919	-0.046604	4.238310
229.971825	6137.003349	15.431923	-0.046614	4.235670
229.856814	6128.943290	15.436928	-0.046587	4.232987
229.994770	6120.884734	15.441933	-0.046607	4.230304
230.033173	6112.915658	15.446938	-0.046609	4.227649
230.023725	6104.920242	15.451943	-0.046602	4.224983
230.119309	6096.953873	15.456947	-0.046615	4.222326
229.750334	6088.960654	15.461952	-0.046541	4.219653
229.869559	6080.946669	15.466957	-0.046558	4.216977
230.066671	6072.947495	15.471962	-0.046589	4.214305
229.924599	6064.917070	15.476967	-0.046558	4.211617
229.828751	6056.958476	15.481971	-0.046535	4.208952
229.754632	6048.937204	15.486976	-0.046516	4.206265
229.819304	6040.917693	15.491981	-0.046522	4.203578
229.769936	6032.965504	15.496986	-0.046508	4.200910
229.585180	6024.937113	15.501991	-0.046468	4.198214
229.744488	6016.990381	15.506995	-0.046493	4.195547
229.532021	6008.855275	15.512000	-0.046448	4.192812
229.414369	6000.816270	15.517005	-0.046421	4.190107
229.444284	5992.884405	15.522010	-0.046421	4.187439
229.527718	5984.849239	15.527015	-0.046431	4.184735
229.344820	5976.948408	15.532019	-0.046392	4.182071
229.241821	5968.922293	15.537024	-0.046368	4.179364
229.473212	5960.905139	15.542029	-0.046406	4.176662
229.335988	5952.934048	15.547034	-0.046375	4.173970
229.177400	5944.869085	15.552039	-0.046340	4.171244
229.331297	5936.904190	15.557043	-0.046364	4.168554
229.245738	5928.895294	15.562048	-0.046342	4.165845
229.307896	5920.928109	15.567053	-0.046349	4.163149
229.182561	5912.906147	15.572058	-0.046320	4.160431
229.002953	5904.933726	15.577063	-0.046282	4.157727
228.985678	5896.913995	15.582067	-0.046273	4.155008
229.080431	5888.863424	15.587072	-0.046285	4.152277
229.183966	5880.878478	15.592077	-0.046300	4.149567
229.066524	5872.884466	15.597082	-0.046272	4.146850
228.975497	5864.843405	15.602087	-0.046250	4.144115
229.093132	5856.916759	15.607091	-0.046267	4.141420
228.869184	5848.895640	15.612096	-0.046220	4.138687
228.780499	5840.881453	15.617101	-0.046198	4.135956
228.776787	5832.901567	15.622106	-0.046192	4.133235
229.061592	5824.840482	15.627111	-0.046240	4.130489
228.916429	5816.907388	15.632115	-0.046208	4.127780
228.821553	5808.858016	15.637120	-0.046185	4.125029
228.861951	5800.910407	15.642125	-0.046187	4.122313
228.731936	5792.930569	15.647130	-0.046158	4.119582
228.622261	5784.948027	15.652135	-0.046132	4.116849
228.633530	5776.931659	15.657139	-0.046129	4.114104
228.460501	5768.861131	15.662144	-0.046092	4.111336
228.472735	5760.853693	15.667149	-0.046089	4.108590
228.659281	5752.879512	15.672154	-0.046118	4.105856
228.635789	5744.862286	15.677159	-0.046109	4.103103
228.619682	5736.905578	15.682163	-0.046100	4.100369
228.422877	5728.921263	15.687168	-0.046058	4.097621
228.306078	5720.885758	15.692173	-0.046031	4.094854
228.374144	5712.914667	15.697178	-0.046039	4.092111
228.319402	5704.888517	15.702183	-0.046023	4.089345
228.258287	5696.954074	15.707187	-0.046007	4.086608
228.297021	5688.927836	15.712192	-0.046009	4.083840
228.242960	5680.954129	15.717197	-0.045994	4.081086
228.089535	5672.986209	15.722202	-0.045960	4.078331
228.073847	5664.939648	15.727207	-0.045952	4.075549
228.040566	5656.949828	15.732211	-0.045940	4.072785
228.066667	5648.880097	15.737216	-0.045940	4.069991
228.243158	5640.897137	15.742221	-0.045967	4.067228
228.122120	5632.904757	15.747226	-0.045940	4.064456
227.817217	5624.951571	15.752231	-0.045878	4.061693
227.887859	5616.963176	15.757235	-0.045886	4.058921
227.827636	5608.946140	15.762240	-0.045869	4.056135
227.858117	5600.942517	15.767245	-0.045870	4.053353
227.894775	5592.918104	15.772250	-0.045871	4.050562
227.905330	5584.948733	15.777255	-0.045868	4.047789
227.666787	5576.950604	15.782259	-0.045818	4.044999
227.502472	5568.980004	15.787264	-0.045783	4.042218
227.569694	5560.920940	15.792269	-0.045790	4.039408
227.425544	5552.952558	15.797274	-0.045758	4.036625
227.508605	5544.881635	15.802279	-0.045768	4.033807
227.505455	5536.845962	15.807283	-0.045762	4.030998
227.469155	5528.857494	15.812288	-0.045750	4.028203
227.541691	5520.889440	15.817293	-0.045758	4.025415
227.419494	5512.951490	15.822298	-0.045730	4.022633
227.568560	5504.892243	15.827303	-0.045753	4.019810
227.614035	5496.916159	15.832307	-0.045756	4.017013
227.358406	5488.896804	15.837312	-0.045703	4.014194
227.539833	5480.895612	15.842317	-0.045732	4.011387
227.514988	5472.905679	15.847322	-0.045722	4.008578
227.510609	5464.899144	15.852327	-0.045716	4.005761
227.466799	5456.938163	15.857331	-0.045703	4.002959
227.325414	5448.913690	15.862336	-0.045671	4.000130
227.330884	5440.959957	15.867341	-0.045667	3.997326
227.380057	5432.930174	15.872346	-0.045671	3.994494
227.239642	5424.882989	15.877351	-0.045639	3.991652
227.207850	5416.909018	15.882355	-0.045628	3.988834
227.097146	5408.913471	15.887360	-0.045602	3.986006
227.190551	5400.903531	15.892365	-0.045615	3.983174
227.295634	5392.918104	15.897370	-0.045629	3.980349
227.064649	5384.946208	15.902375	-0.045581	3.977521
226.912835	5376.989547	15.907379	-0.045547	3.974698
226.989008	5368.932774	15.912384	-0.045556	3.971841
226.821954	5360.921501	15.917389	-0.045520	3.968994
226.746709	5352.974907	15.922394	-0.045501	3.966169
226.699629	5344.952777	15.927399	-0.045487	3.963317
226.685182	5337.000664	15.932403	-0.045479	3.960487
226.762897	5328.990176	15.937408	-0.045488	3.957636
226.717530	5320.994925	15.942413	-0.045474	3.954787
226.750670	5312.957864	15.947418	-0.045475	3.951922
226.474121	5304.919942	15.952423	-0.045418	3.949049
226.543267	5296.954882	15.957427	-0.045426	3.946206
226.369586	5288.950770	15.962432	-0.045389	3.943343
226.632022	5280.933533	15.967437	-0.045432	3.940481
226.624487	5272.990407	15.972442	-0.045426	3.937638
226.332134	5264.999292	15.977447	-0.045366	3.934771
226.402811	5257.038582	15.982451	-0.045374	3.931920
226.065908	5248.998865	15.987456	-0.045306	3.929030
226.126370	5240.977287	15.992461	-0.045312	3.926152
226.260675	5232.996056	15.997466	-0.045332	3.923288
226.123253	5224.991906	16.002471	-0.045301	3.920409
226.275321	5217.040495	16.007475	-0.045324	3.917551
226.054129	5208.995214	16.012480	-0.045278	3.914651
226.063015	5200.956266	16.017485	-0.045274	3.911756
226.044344	5193.006077	16.022490	-0.045265	3.908889
226.100668	5184.984307	16.027495	-0.045271	3.905997
226.307641	5177.027173	16.032499	-0.045304	3.903128
226.026900	5168.982119	16.037504	-0.045246	3.900216
225.927821	5161.048461	16.042509	-0.045223	3.897346
225.851644	5153.001324	16.047514	-0.045203	3.894432
225.794056	5144.949783	16.052519	-0.045187	3.891516
225.802745	5136.974857	16.057523	-0.045184	3.888626
225.832219	5129.011639	16.062528	-0.045184	3.885739
225.953597	5121.026201	16.067533	-0.045201	3.882843
225.809477	5112.989602	16.072538	-0.045169	3.879922
225.683234	5105.017410	16.077543	-0.045141	3.877022
225.887066	5096.969907	16.082547	-0.045173	3.874098
225.606104	5088.733505	16.087552	-0.045116	3.871095
225.826552	5080.841269	16.092557	-0.045151	3.868224
225.841305	5072.892423	16.097562	-0.045149	3.865327
225.641617	5064.953598	16.102567	-0.045107	3.862426
225.392906	5056.963693	16.107571	-0.045055	3.859504
225.340057	5049.025507	16.112576	-0.045040	3.856602
225.554005	5040.976978	16.117581	-0.045075	3.853664
225.479718	5032.965883	16.122586	-0.045056	3.850731
225.427131	5024.952901	16.127591	-0.045040	3.847795
225.648440	5016.979264	16.132595	-0.045076	3.844877
225.359093	5009.042836	16.137600	-0.045017	3.841960
225.097437	5001.046389	16.142605	-0.044963	3.839020
225.142755	4993.062609	16.147610	-0.044967	3.836088
225.316675	4985.020743	16.152615	-0.044994	3.833135
225.132488	4977.039333	16.157619	-0.044954	3.830195
225.242605	4969.015109	16.162624	-0.044970	3.827243
225.310623	4961.013000	16.167629	-0.044977	3.824295
225.363437	4953.095772	16.172634	-0.044982	3.821377
225.229491	4945.086269	16.177639	-0.044951	3.818418
225.164444	4937.100173	16.182643	-0.044934	3.815467
225.121272	4929.069203	16.187648	-0.044921	3.812498
224.839119	4921.053389	16.192653	-0.044863	3.809527
224.827839	4913.094707	16.197658	-0.044856	3.806580
224.943903	4905.063123	16.202663	-0.044872	3.803607
224.933553	4897.115923	16.207667	-0.044865	3.800660
224.810356	4889.126898	16.212672	-0.044837	3.797693
224.867466	4881.120042	16.217677	-0.044842	3.794721
224.721878	4873.053402	16.222682	-0.044810	3.791720
224.506445	4865.061994	16.227687	-0.044765	3.788743
224.657523	4857.064249	16.232691	-0.044787	3.785769
224.630688	4849.111058	16.237696	-0.044777	3.782805
224.478550	4841.097168	16.242701	-0.044744	3.779814
224.506319	4833.142387	16.247706	-0.044744	3.776847
224.617076	4825.085189	16.252711	-0.044759	3.773841
224.744603	4817.086794	16.257715	-0.044778	3.770854
224.538306	4809.090024	16.262720	-0.044734	3.767859
224.522724	4801.080531	16.267725	-0.044726	3.764861
224.417616	4793.147910	16.272730	-0.044701	3.761886
224.259016	4785.116695	16.277735	-0.044666	3.758872
224.443775	4777.136489	16.282739	-0.044695	3.755882
224.509136	4769.077714	16.287744	-0.044702	3.752857
224.131506	4761.087007	16.292749	-0.044627	3.749846
224.175649	4753.109773	16.297754	-0.044630	3.746846
224.180215	4745.077551	16.302759	-0.044625	3.743823
224.226229	4737.127090	16.307763	-0.044629	3.740829
224.091900	4729.152119	16.312768	-0.044599	3.737819
223.999862	4721.137959	16.317773	-0.044576	3.734793
224.272660	4713.132024	16.322778	-0.044622	3.731776
223.897416	4705.110867	16.327783	-0.044547	3.728736
223.993867	4697.136493	16.332787	-0.044559	3.725722
224.079176	4689.171722	16.337792	-0.044570	3.722708
223.940758	4681.182407	16.342797	-0.044539	3.719678
223.908587	4673.249627	16.347802	-0.044528	3.716670
224.004153	4665.161269	16.352807	-0.044540	3.713603
224.013897	4657.094149	16.357811	-0.044537	3.710539
223.616302	4649.134014	16.362816	-0.044458	3.707503
223.756413	4641.125897	16.367821	-0.044479	3.704460
223.656556	4633.204722	16.372826	-0.044455	3.701442
223.563884	4625.192128	16.377831	-0.044432	3.698387
223.663900	4617.209557	16.382835	-0.044446	3.695345
223.805707	4609.188252	16.387840	-0.044467	3.692287
223.470178	4601.197709	16.392845	-0.044399	3.689226
223.629787	4593.239925	16.397850	-0.044424	3.686188
223.530788	4585.208763	16.402855	-0.044400	3.683112
223.535227	4577.242660	16.407859	-0.044396	3.680062
223.479223	4569.262778	16.412864	-0.044380	3.677002
223.510871	4561.232442	16.417869	-0.044381	3.673922
223.583215	4553.206909	16.422874	-0.044389	3.670843
223.270974	4545.224563	16.427879	-0.044325	3.667768
223.267765	4537.205446	16.432883	-0.044320	3.664684
223.444664	4529.248176	16.437888	-0.044347	3.661626
223.263563	4521.245664	16.442893	-0.044308	3.658539
223.455855	4513.239109	16.447898	-0.044339	3.655457
223.323062	4505.237188	16.452903	-0.044309	3.652366
223.274541	4497.252491	16.457907	-0.044295	3.649281
223.071307	4489.278750	16.462912	-0.044252	3.646193
223.233328	4481.245534	16.467917	-0.044277	3.643090
223.172955	4473.278804	16.472922	-0.044260	3.640004
223.068573	4465.303392	16.477927	-0.044236	3.636911
223.216816	4457.299552	16.482931	-0.044258	3.633811
223.110915	4449.234177	16.487936	-0.044233	3.630677
222.882518	4441.263905	16.492941	-0.044185	3.627574
222.856570	4433.267105	16.497946	-0.044175	3.624464
222.950069	4425.290441	16.502951	-0.044187	3.621363
222.811720	4417.326503	16.507955	-0.044156	3.618257
222.599231	4409.332284	16.512960	-0.044112	3.615135
222.671691	4401.303281	16.517965	-0.044120	3.612004
222.807076	4393.305509	16.522970	-0.044140	3.608884
222.658581	4385.321255	16.527975	-0.044107	3.605760
222.701304	4377.330330	16.532979	-0.044110	3.602635
222.643495	4369.349543	16.537984	-0.044094	3.599508
222.641926	4361.386015	16.542989	-0.044088	3.596388
222.638324	4353.374653	16.547994	-0.044082	3.593245
222.562967	4345.332563	16.552999	-0.044063	3.590086
222.538131	4337.377327	16.558003	-0.044053	3.586960
222.463097	4329.393012	16.563008	-0.044034	3.583818
222.503562	4321.403365	16.568013	-0.044036	3.580674
222.444822	4313.434300	16.573018	-0.044020	3.577533
222.365293	4305.386729	16.578023	-0.044000	3.574358
222.391289	4297.399494	16.583027	-0.044000	3.571206
222.423308	4289.405429	16.588032	-0.044000	3.568050
222.309755	4281.407856	16.593037	-0.043974	3.564885
222.217223	4273.475037	16.598042	-0.043952	3.561743
222.261867	4265.429567	16.603047	-0.043955	3.558558
222.260243	4257.459279	16.608051	-0.043949	3.555398
222.190702	4249.357210	16.613056	-0.043931	3.552182
222.032397	4241.368950	16.618061	-0.043896	3.549005
222.194159	4233.349803	16.623066	-0.043921	3.545822
222.040746	4225.385785	16.628071	-0.043887	3.542649
221.979334	4217.416560	16.633075	-0.043871	3.539474
221.991051	4209.467006	16.638080	-0.043868	3.536306
221.882424	4201.431989	16.643085	-0.043842	3.533098
221.858865	4193.433821	16.648090	-0.043833	3.529904
221.740586	4185.439184	16.653095	-0.043805	3.526705
221.807848	4177.473593	16.658099	-0.043813	3.523521
221.568902	4169.493387	16.663104	-0.043763	3.520319
221.527375	4161.493739	16.668109	-0.043750	3.517112
221.624780	4153.471281	16.673114	-0.043763	3.513897
221.565461	4145.472867	16.678119	-0.043747	3.510685
221.485321	4137.495065	16.683123	-0.043726	3.507476
221.464656	4129.463359	16.688128	-0.043717	3.504245
221.524127	4121.508044	16.693133	-0.043723	3.501045
221.602061	4113.546928	16.698138	-0.043733	3.497839
221.305138	4105.529479	16.703143	-0.043672	3.494597
221.684127	4097.535543	16.708147	-0.043737	3.491381
221.290224	4089.546076	16.713152	-0.043659	3.488141
221.358338	4081.546421	16.718157	-0.043666	3.484908
221.308156	4073.609739	16.723162	-0.043652	3.481693
221.225462	4065.590563	16.728167	-0.043631	3.478441
221.160469	4057.619077	16.733171	-0.043614	3.475206
221.184739	4049.571092	16.738176	-0.043613	3.471940
221.171848	4041.571262	16.743181	-0.043605	3.468689
221.216086	4033.566714	16.748186	-0.043608	3.465435
220.941222	4025.608982	16.753191	-0.043552	3.462187
221.209670	4017.610708	16.758195	-0.043597	3.458936
221.032490	4009.625798	16.763200	-0.043559	3.455674
220.948351	4001.622677	16.768205	-0.043538	3.452404
220.941265	3993.588889	16.773210	-0.043531	3.449121
220.998053	3985.614046	16.778215	-0.043536	3.445861
220.857835	3977.645179	16.783219	-0.043505	3.442594
220.759089	3969.646308	16.788224	-0.043481	3.439312
220.813774	3961.695868	16.793229	-0.043486	3.436053
220.907601	3953.692752	16.798234	-0.043499	3.432770
220.673374	3945.629206	16.803239	-0.043450	3.429448
220.829410	3937.681885	16.808243	-0.043474	3.426184
220.856091	3929.670868	16.813248	-0.043473	3.422887
220.671857	3921.672843	16.818253	-0.043434	3.419584
220.936697	3913.709807	16.823258	-0.043478	3.416308
220.778776	3905.694107	16.828263	-0.043443	3.412992
220.656438	3897.691625	16.833267	-0.043415	3.409680
220.466558	3889.727490	16.838272	-0.043375	3.406378
220.655046	3881.729806	16.843277	-0.043405	3.403072
220.633647	3873.773170	16.848282	-0.043395	3.399773
220.479050	3865.803102	16.853287	-0.043361	3.396460
220.611718	3857.773182	16.858291	-0.043381	3.393129
220.323170	3849.713012	16.863296	-0.043322	3.389768
220.359897	3841.751232	16.868301	-0.043324	3.386455
220.290525	3833.773250	16.873306	-0.043305	3.383129
220.374169	3825.775211	16.878311	-0.043316	3.379797
220.285894	3817.845982	16.883315	-0.043294	3.376484
220.232184	3809.809619	16.888320	-0.043279	3.373124
220.413063	3801.770219	16.893325	-0.043307	3.369768
220.407381	3793.851601	16.898330	-0.043301	3.366452
220.119596	3785.835426	16.903335	-0.043242	3.363082
220.222970	3777.859264	16.908339	-0.043256	3.359740
220.169793	3769.894820	16.913344	-0.043241	3.356393
220.023866	3761.858019	16.918349	-0.043209	3.353010
219.998722	3753.870863	16.923354	-0.043199	3.349648
220.160634	3745.861446	16.928359	-0.043224	3.346280
219.984816	3737.884191	16.933363	-0.043186	3.342910
219.953470	3729.887697	16.938368	-0.043175	3.339534
219.902322	3721.927627	16.943373	-0.043160	3.336169
220.079388	3713.922447	16.948378	-0.043188	3.332790
219.697620	3705.893964	16.953383	-0.043111	3.329377
219.781075	3697.957456	16.958387	-0.043122	3.326017
220.081986	3689.928133	16.963392	-0.043173	3.322622
219.775142	3681.953170	16.968397	-0.043110	3.319224
219.645447	3674.046465	16.973402	-0.043081	3.315858
219.848846	3665.943060	16.978407	-0.043113	3.312418
219.899061	3657.952428	16.983411	-0.043118	3.309016
219.830324	3649.965216	16.988416	-0.043100	3.305608
219.629938	3641.997294	16.993421	-0.043057	3.302199
219.789857	3634.029581	16.998426	-0.043082	3.298801
219.477796	3626.051749	17.003431	-0.043018	3.295377
219.472627	3618.057717	17.008435	-0.043012	3.291954
219.555008	3610.031366	17.013440	-0.043022	3.288517
219.443165	3602.054160	17.018445	-0.042996	3.285090
219.510611	3594.084388	17.023450	-0.043004	3.281669
219.359886	3586.086050	17.028455	-0.042970	3.278225
219.380385	3578.112553	17.033459	-0.042969	3.274793
219.234175	3570.122740	17.038464	-0.042936	3.271345
219.130296	3562.115863	17.043469	-0.042912	3.267888
219.272283	3554.080601	17.048474	-0.042933	3.264424
219.128058	3546.141366	17.053479	-0.042901	3.260986
219.006483	3538.175325	17.058483	-0.042873	3.257535
219.099195	3530.161351	17.063488	-0.042885	3.254067
219.135824	3522.130102	17.068493	-0.042887	3.250586
219.069730	3514.188808	17.073498	-0.042869	3.247136
219.040629	3506.175734	17.078503	-0.042859	3.243653
219.045890	3498.218311	17.083507	-0.042854	3.240192
219.045577	3490.247697	17.088512	-0.042849	3.236721
219.060740	3482.211906	17.093517	-0.042847	3.233218
219.074404	3474.184958	17.098522	-0.042844	3.229716
218.909714	3466.201955	17.103527	-0.042808	3.226221
218.826825	3458.238573	17.108531	-0.042787	3.222735
218.717691	3450.243556	17.113536	-0.042762	3.219230
218.772823	3442.270328	17.118541	-0.042767	3.215737
218.725253	3434.298352	17.123546	-0.042753	3.212237
218.741413	3426.269407	17.128551	-0.042751	3.208711
218.733620	3418.284188	17.133555	-0.042744	3.205199
218.665874	3410.331842	17.138560	-0.042726	3.201695
218.532139	3402.340701	17.143565	-0.042696	3.198167
218.610196	3394.359497	17.148570	-0.042705	3.194649
218.548281	3386.346716	17.153575	-0.042689	3.191107
218.410100	3378.379793	17.158579	-0.042658	3.187578
218.267844	3370.412990	17.163584	-0.042626	3.184046
218.389277	3362.381918	17.168589	-0.042643	3.180492
218.573320	3354.404379	17.173594	-0.042672	3.176960
218.118759	3346.421298	17.178599	-0.042582	3.173395
218.212849	3338.383911	17.183603	-0.042595	3.169825
218.247947	3330.438343	17.188608	-0.042596	3.166289
218.323267	3322.434725	17.193613	-0.042605	3.162725
218.180285	3314.484378	17.198618	-0.042573	3.159172
218.207109	3306.474133	17.203623	-0.042573	3.155595
218.012548	3298.473618	17.208627	-0.042531	3.152009
218.025046	3290.473226	17.213632	-0.042528	3.148427
218.012579	3282.468366	17.218637	-0.042521	3.144839
217.879535	3274.549149	17.223642	-0.042491	3.141279
217.848003	3266.531066	17.228647	-0.042480	3.137676
218.105920	3258.532554	17.233651	-0.042523	3.134090
217.731186	3250.560461	17.238656	-0.042448	3.130484
217.815890	3242.562699	17.243661	-0.042458	3.126882
217.954151	3234.588855	17.248666	-0.042479	3.123290
217.805050	3226.624331	17.253671	-0.042446	3.119685
217.851967	3218.655113	17.258675	-0.042449	3.116082
217.694588	3210.667911	17.263680	-0.042415	3.112457
217.650937	3202.635385	17.268685	-0.042401	3.108813
217.700066	3194.648386	17.273690	-0.042405	3.105190
217.579474	3186.682206	17.278695	-0.042378	3.101564
217.643139	3178.684957	17.283699	-0.042384	3.097928
217.430904	3170.722773	17.288704	-0.042340	3.094291
217.419263	3162.710158	17.293709	-0.042332	3.090637
217.611400	3154.714464	17.298714	-0.042363	3.086994
217.306373	3146.762724	17.303719	-0.042301	3.083345
217.282286	3138.784572	17.308723	-0.042291	3.079692
217.211819	3130.819931	17.313728	-0.042273	3.076039
217.318058	3122.735953	17.318733	-0.042287	3.072335
217.394666	3114.727185	17.323738	-0.042296	3.068660
217.123341	3106.746558	17.328743	-0.042240	3.064977
217.222435	3098.780442	17.333747	-0.042254	3.061314
217.188024	3090.813814	17.338752	-0.042242	3.057639
217.092022	3082.846887	17.343757	-0.042219	3.053958
217.221814	3074.856249	17.348762	-0.042238	3.050271
216.889723	3066.901258	17.353767	-0.042171	3.046575
216.927500	3058.909125	17.358771	-0.042173	3.042874
217.016858	3050.921358	17.363776	-0.042184	3.039174
216.836700	3042.975256	17.368781	-0.042145	3.035475
216.746081	3034.986012	17.373786	-0.042123	3.031756
216.594936	3026.965332	17.378791	-0.042090	3.028015
216.625058	3018.974567	17.383795	-0.042090	3.024292
216.662468	3011.019610	17.388800	-0.042092	3.020582
216.472079	3003.043497	17.393805	-0.042051	3.016845
216.629018	2995.028938	17.398810	-0.042075	3.013104
216.645572	2987.011028	17.403815	-0.042073	3.009349
216.522819	2979.082311	17.408819	-0.042045	3.005624
216.291986	2971.115747	17.413824	-0.041997	3.001872
216.442884	2963.116952	17.418829	-0.042020	2.998119
216.383791	2955.143691	17.423834	-0.042004	2.994362
216.298802	2947.110400	17.428839	-0.041983	2.990572
216.318974	2939.129058	17.433843	-0.041981	2.986806
216.365601	2931.134491	17.438848	-0.041985	2.983030
216.265299	2923.149858	17.443853	-0.041961	2.979248
216.096210	2915.244672	17.448858	-0.041924	2.975494
216.306378	2907.194529	17.453863	-0.041958	2.971686
216.219987	2899.221196	17.458867	-0.041937	2.967895
216.071426	2891.255587	17.463872	-0.041904	2.964099
216.083276	2883.271868	17.468877	-0.041901	2.960298
216.310632	2875.303316	17.473882	-0.041938	2.956510
216.180685	2867.300427	17.478887	-0.041908	2.952683
215.967627	2859.337857	17.483891	-0.041864	2.948866
215.962582	2851.345576	17.488896	-0.041857	2.945040
215.878347	2843.362514	17.493901	-0.041836	2.941210
215.813361	2835.404058	17.498906	-0.041819	2.937387
215.990592	2827.381569	17.503911	-0.041847	2.933541
215.959808	2819.381827	17.508915	-0.041836	2.929691
215.869977	2811.421739	17.513920	-0.041814	2.925851
215.712669	2803.470483	17.518925	-0.041780	2.922007
215.828601	2795.495283	17.523930	-0.041796	2.918161
215.793758	2787.480022	17.528935	-0.041784	2.914282
215.672496	2779.428277	17.533939	-0.041756	2.910376
215.696259	2771.465337	17.538944	-0.041756	2.906515
215.542468	2763.489534	17.543949	-0.041722	2.902633
215.579636	2755.547622	17.548954	-0.041723	2.898773
215.738645	2747.532926	17.553959	-0.041748	2.894879
215.622764	2739.583126	17.558963	-0.041721	2.890997
215.371807	2731.621390	17.563968	-0.041669	2.887096
215.226691	2723.644719	17.568973	-0.041637	2.883188
215.306370	2715.671695	17.573978	-0.041647	2.879289
215.300769	2707.699870	17.578983	-0.041640	2.875380
215.335860	2699.689209	17.583987	-0.041642	2.871450
215.275149	2691.714207	17.588992	-0.041625	2.867526
215.182954	2683.707426	17.593997	-0.041603	2.863579
215.195964	2675.766345	17.599002	-0.041600	2.859666
215.236311	2667.791963	17.604007	-0.041602	2.855732
215.192110	2659.793285	17.609011	-0.041589	2.851776
215.032910	2651.835761	17.614016	-0.041554	2.847828
215.022409	2643.819633	17.619021	-0.041547	2.843854
215.071669	2635.877068	17.624026	-0.041551	2.839914
214.868476	2627.929018	17.629031	-0.041508	2.835952
214.815493	2619.928065	17.634035	-0.041493	2.831966
214.847512	2611.908050	17.639040	-0.041493	2.827971
214.693054	2603.935669	17.644045	-0.041459	2.823982
214.656024	2595.994891	17.649050	-0.041447	2.820011
214.556642	2588.005784	17.654055	-0.041423	2.816006
214.719255	2579.986795	17.659059	-0.041449	2.811995
214.690212	2572.013641	17.664064	-0.041438	2.807991
214.482095	2564.039007	17.669069	-0.041394	2.803970
214.679897	2556.074913	17.674074	-0.041426	2.799972
214.455542	2548.128832	17.679079	-0.041379	2.795953
214.537984	2540.122303	17.684083	-0.041389	2.791915
214.546054	2532.151981	17.689088	-0.041385	2.787885
214.509851	2524.150884	17.694093	-0.041373	2.783832
214.448477	2516.196996	17.699098	-0.041356	2.779795
214.272333	2508.241665	17.704103	-0.041318	2.775744
214.346773	2500.219699	17.709107	-0.041327	2.771669
214.386093	2492.242998	17.714112	-0.041329	2.767608
214.084646	2484.290396	17.719117	-0.041268	2.763534
214.324645	2476.325214	17.724122	-0.041307	2.759479
214.300642	2468.375204	17.729127	-0.041298	2.755411
213.952861	2460.333210	17.734131	-0.041228	2.751269
214.003037	2452.331352	17.739136	-0.041232	2.747166
214.068594	2444.351136	17.744141	-0.041239	2.743069
214.002579	2436.402013	17.749146	-0.041221	2.738974
213.763304	2428.448434	17.754151	-0.041171	2.734860
213.988256	2420.440955	17.759155	-0.041208	2.730740
213.855900	2412.497583	17.764160	-0.041178	2.726625
213.756645	2404.509310	17.769165	-0.041155	2.722483
213.861287	2396.560056	17.774170	-0.041169	2.718367
213.880270	2388.577755	17.779175	-0.041167	2.714223
213.759890	2380.599725	17.784179	-0.041140	2.710066
213.550924	2372.632049	17.789184	-0.041095	2.705902
213.664309	2364.639837	17.794189	-0.041111	2.701739
213.732372	2356.692193	17.799194	-0.041119	2.697590
213.581610	2348.719317	17.804199	-0.041086	2.693408
213.681810	2340.706607	17.809203	-0.041099	2.689214
213.622301	2332.766044	17.814208	-0.041083	2.685042
213.304980	2324.809143	17.819213	-0.041018	2.680837
213.474927	2316.865652	17.824218	-0.041045	2.676665
213.493732	2308.822099	17.829223	-0.041043	2.672423
213.445913	2300.838967	17.834227	-0.041029	2.668203
213.329178	2292.878655	17.839232	-0.041002	2.663983
213.368823	2284.917826	17.844237	-0.041004	2.659766
213.434055	2276.951777	17.849242	-0.041011	2.655542
213.139728	2268.989566	17.854247	-0.040951	2.651290
213.278058	2260.977300	17.859251	-0.040972	2.647032
213.000312	2253.060803	17.864256	-0.040915	2.642791
213.074382	2245.085003	17.869261	-0.040923	2.638535
213.280840	2237.099016	17.874266	-0.040957	2.634275
213.105775	2229.119925	17.879271	-0.040919	2.629987
212.996373	2221.160360	17.884275	-0.040893	2.625706
212.894376	2213.195806	17.889280	-0.040869	2.621417
212.760493	2205.228316	17.894285	-0.040839	2.617116
212.940387	2197.246032	17.899290	-0.040867	2.612822
213.020430	2189.243863	17.904295	-0.040877	2.608503
213.050970	2181.279501	17.909299	-0.040877	2.604194
212.798568	2173.360132	17.914304	-0.040825	2.599883
212.825596	2165.396167	17.919309	-0.040825	2.595560
212.930423	2157.255381	17.924314	-0.040839	2.591138
212.792180	2149.261056	17.929319	-0.040808	2.586772
212.733239	2141.345502	17.934323	-0.040792	2.582448
212.682440	2133.424244	17.939328	-0.040777	2.578113
212.455155	2125.473049	17.944333	-0.040730	2.573742
212.381564	2117.506735	17.949338	-0.040711	2.569367
212.307691	2109.542148	17.954343	-0.040692	2.564985
212.664506	2101.566219	17.959347	-0.040753	2.560619
212.514799	2093.640100	17.964352	-0.040720	2.556237
212.325291	2085.659293	17.969357	-0.040680	2.551816
212.433473	2077.686466	17.974362	-0.040695	2.547411
212.526771	2069.699706	17.979367	-0.040707	2.542991
212.405369	2061.770417	17.984371	-0.040679	2.538579
212.253605	2053.814273	17.989376	-0.040645	2.534143
212.181918	2045.816572	17.994381	-0.040627	2.529681
212.131051	2037.880926	17.999386	-0.040612	2.525248
212.112979	2029.913201	18.004391	-0.040604	2.520791
212.049549	2021.970129	18.009395	-0.040587	2.516337
212.048291	2013.962570	18.014400	-0.040581	2.511843
211.849529	2005.983668	18.019405	-0.040539	2.507343
212.009854	1998.027181	18.024410	-0.040564	2.502873
211.810969	1990.072034	18.029415	-0.040521	2.498371
211.781216	1982.110851	18.034419	-0.040511	2.493868
211.874905	1974.116945	18.039424	-0.040523	2.489349
211.967407	1966.121976	18.044429	-0.040535	2.484820
212.040690	1958.213444	18.049434	-0.040543	2.480331
211.720295	1950.273973	18.054439	-0.040478	2.475787
211.696600	1942.299677	18.059443	-0.040469	2.471237
211.793494	1934.318338	18.064448	-0.040482	2.466683
211.662602	1926.364547	18.069453	-0.040452	2.462119
211.513253	1918.448384	18.074458	-0.040419	2.457568
211.770941	1910.417909	18.079463	-0.040462	2.452972
211.547873	1902.482207	18.084467	-0.040415	2.448387
211.364855	1894.559756	18.089472	-0.040376	2.443803
211.277149	1886.587645	18.094477	-0.040354	2.439190
211.234605	1878.658112	18.099482	-0.040341	2.434595
210.963042	1870.617874	18.104487	-0.040285	2.429910
211.363655	1862.613911	18.109491	-0.040355	2.425289
211.328972	1854.661419	18.114496	-0.040343	2.420656
211.122989	1846.735655	18.119501	-0.040300	2.416016
211.210051	1838.763917	18.124506	-0.040311	2.411362
211.124146	1830.790298	18.129511	-0.040289	2.406686
210.978557	1822.866482	18.134515	-0.040257	2.402024
210.947024	1814.934698	18.139520	-0.040246	2.397358
210.990469	1806.947206	18.144525	-0.040249	2.392656
211.020178	1798.976952	18.149530	-0.040249	2.387954
210.843518	1791.045528	18.154535	-0.040211	2.383249
210.777212	1783.108491	18.159539	-0.040194	2.378540
210.781383	1775.144123	18.164544	-0.040189	2.373811
210.537946	1767.174405	18.169549	-0.040139	2.369049
210.804704	1759.198689	18.174554	-0.040183	2.364316
210.641809	1751.271662	18.179559	-0.040148	2.359567
210.704928	1743.329375	18.184563	-0.040154	2.354818
210.490123	1735.353042	18.189568	-0.040109	2.350017
210.477198	1727.366829	18.194573	-0.040101	2.345216
210.464805	1719.430556	18.199578	-0.040094	2.340435
210.408175	1711.479814	18.204583	-0.040078	2.335632
210.307350	1703.524907	18.209587	-0.040054	2.330813
210.452551	1695.548097	18.214592	-0.040076	2.325991
210.268995	1687.610750	18.219597	-0.040037	2.321156
210.146803	1679.704987	18.224602	-0.040009	2.316335
210.030930	1671.734338	18.229607	-0.039982	2.311465
210.071091	1663.753305	18.234611	-0.039984	2.306591
209.946621	1655.832062	18.239616	-0.039956	2.301730
209.887146	1647.867113	18.244621	-0.039939	2.296837
210.197762	1639.890556	18.249626	-0.039992	2.291957
209.766057	1631.971560	18.254631	-0.039907	2.287040
209.721215	1624.017508	18.259635	-0.039893	2.282124
209.908081	1616.067998	18.264640	-0.039923	2.277219
209.750605	1608.078293	18.269645	-0.039888	2.272250
209.680300	1600.097596	18.274650	-0.039870	2.267282
209.726680	1592.132249	18.279655	-0.039873	2.262324
209.927266	1584.177380	18.284659	-0.039905	2.257374
209.686532	1576.266573	18.289664	-0.039855	2.252403
209.392211	1568.336096	18.294669	-0.039795	2.247403
209.484282	1560.385674	18.299674	-0.039807	2.242414
209.427668	1552.452601	18.304679	-0.039792	2.237411
209.411263	1544.506234	18.309683	-0.039783	2.232393
209.306135	1536.564290	18.314688	-0.039759	2.227358
209.323699	1528.598567	18.319693	-0.039757	2.222307
209.272510	1520.676282	18.324698	-0.039742	2.217267
209.250811	1512.704256	18.329703	-0.039733	2.212185
209.093795	1504.766678	18.334707	-0.039698	2.207102
209.162749	1496.826570	18.339712	-0.039706	2.202026
209.074493	1488.899447	18.344717	-0.039684	2.196932
209.129314	1480.932696	18.349722	-0.039689	2.191814
209.090475	1472.962444	18.354727	-0.039677	2.186674
208.989918	1465.032008	18.359731	-0.039653	2.181541
208.879061	1457.125125	18.364736	-0.039627	2.176410
208.770669	1449.161181	18.369741	-0.039602	2.171230
208.885961	1441.207932	18.374746	-0.039618	2.166066
208.784413	1433.276263	18.379751	-0.039594	2.160883
208.738179	1425.360550	18.384755	-0.039580	2.155703
208.617307	1417.425544	18.389760	-0.039552	2.150491
208.392317	1409.481322	18.394765	-0.039505	2.145251
208.652685	1401.515962	18.399770	-0.039549	2.140030
208.708979	1393.585194	18.404775	-0.039554	2.134799
208.436382	1385.664539	18.409779	-0.039498	2.129531
208.542178	1377.718369	18.414784	-0.039512	2.124269
208.336635	1369.805485	18.419789	-0.039469	2.118986
208.271728	1361.872998	18.424794	-0.039452	2.113691
208.103401	1353.873678	18.429799	-0.039415	2.108327
208.130733	1345.935135	18.434803	-0.039415	2.103009
208.208175	1337.998696	18.439808	-0.039424	2.097685
208.077366	1330.062316	18.444813	-0.039395	2.092326
208.000275	1322.148931	18.449818	-0.039375	2.086975
207.857675	1314.232022	18.454823	-0.039344	2.081600
207.890988	1306.306118	18.459827	-0.039345	2.076223
207.791157	1298.366515	18.464832	-0.039321	2.070810
207.706016	1290.421365	18.469837	-0.039300	2.065380
207.905383	1282.485627	18.474842	-0.039332	2.059971
207.778697	1274.572845	18.479847	-0.039303	2.054530
207.680729	1266.639714	18.484851	-0.039279	2.049064
207.657431	1258.720460	18.489856	-0.039270	2.043600
207.458309	1250.821846	18.494861	-0.039228	2.038119
207.397386	1242.892571	18.499866	-0.039211	2.032615
207.436945	1234.914828	18.504871	-0.039213	2.027072
207.456289	1226.990676	18.509875	-0.039212	2.021550
207.211733	1219.108621	18.514880	-0.039161	2.016015
207.244491	1211.128183	18.519885	-0.039162	2.010424
207.344429	1203.205401	18.524890	-0.039175	2.004865
207.243841	1195.294867	18.529895	-0.039151	1.999279
207.298163	1187.373345	18.534899	-0.039156	1.993685
207.255029	1179.447795	18.539904	-0.039143	1.988063
207.028737	1171.546071	18.544909	-0.039096	1.982422
207.132723	1163.626714	18.549914	-0.039110	1.976787
207.001091	1155.708748	18.554919	-0.039080	1.971112
207.082760	1147.769604	18.559923	-0.039090	1.965429
206.984431	1139.880053	18.564928	-0.039067	1.959745
207.024529	1131.942984	18.569933	-0.039069	1.954025
206.833347	1124.010137	18.574938	-0.039028	1.948267
206.726938	1116.093505	18.579943	-0.039003	1.942512
206.722660	1108.170673	18.584947	-0.038997	1.936747
206.854547	1100.229108	18.589952	-0.039017	1.930966
206.453060	1092.359047	18.594957	-0.038937	1.925161
206.700991	1084.429182	18.599962	-0.038978	1.919367
206.769037	1076.501542	18.604967	-0.038985	1.913536
206.676088	1068.590484	18.609971	-0.038963	1.907682
206.591612	1060.698472	18.614976	-0.038942	1.901825
206.536339	1052.786742	18.619981	-0.038927	1.895939
206.488755	1044.878777	18.624986	-0.038913	1.890038
206.283149	1036.991215	18.629991	-0.038869	1.884116
206.297972	1029.086288	18.634995	-0.038867	1.878187
206.379459	1021.154274	18.640000	-0.038877	1.872227
206.077775	1013.258043	18.645005	-0.038815	1.866230
206.155163	1005.344675	18.650010	-0.038825	1.860245
206.099488	997.450176	18.655015	-0.038809	1.854239
206.165982	989.516744	18.660019	-0.038816	1.848199
206.073455	981.649655	18.665024	-0.038794	1.842171
205.881100	973.771508	18.670029	-0.038753	1.836103
205.909916	965.854334	18.675034	-0.038753	1.830010
205.846560	957.946389	18.680039	-0.038736	1.823894
205.710286	950.074425	18.685043	-0.038706	1.817776
205.854440	942.142252	18.690048	-0.038727	1.811624
205.620556	934.265153	18.695053	-0.038679	1.805449
205.502521	926.414352	18.700058	-0.038651	1.799287
205.588510	918.475983	18.705063	-0.038662	1.793060
205.522405	910.530374	18.710067	-0.038645	1.786787
205.421085	902.660496	18.715072	-0.038621	1.780547
205.389013	894.774314	18.720077	-0.038610	1.774281
205.619965	886.845082	18.725082	-0.038647	1.767991
205.268211	879.017542	18.730087	-0.038577	1.761687
205.101058	871.158021	18.735091	-0.038541	1.755359
205.153017	863.253041	18.740096	-0.038545	1.748998
205.200244	855.337756	18.745101	-0.038549	1.742605
205.165610	847.483648	18.750106	-0.038537	1.736227
205.077849	839.590953	18.755111	-0.038516	1.729788
205.237242	831.691326	18.760115	-0.038540	1.723351
205.001636	823.868331	18.765120	-0.038491	1.716902
205.042902	815.945794	18.770125	-0.038494	1.710382
204.925990	808.099606	18.775130	-0.038467	1.703880
204.918117	800.215716	18.780135	-0.038460	1.697335
204.775405	792.345347	18.785139	-0.038428	1.690759
204.700327	784.482127	18.790144	-0.038409	1.684173
204.583953	776.635633	18.795149	-0.038383	1.677569
204.541616	768.770466	18.800154	-0.038369	1.670932
204.380408	760.904052	18.805159	-0.038334	1.664253
204.527301	753.023813	18.810163	-0.038357	1.657576
204.505500	745.152307	18.815168	-0.038347	1.650857
204.491645	737.278082	18.820173	-0.038340	1.644109
204.433334	729.455904	18.825178	-0.038324	1.637372
204.271385	721.557862	18.830183	-0.038288	1.630527
204.188729	713.692613	18.835187	-0.038268	1.623693
204.087235	705.857612	18.840192	-0.038244	1.616854
204.024157	697.990172	18.845197	-0.038227	1.609962
203.888652	690.167863	18.850202	-0.038197	1.603070
203.935190	682.303581	18.855207	-0.038200	1.596138
203.730794	674.485600	18.860211	-0.038157	1.589180
203.669832	666.631127	18.865216	-0.038140	1.582180
203.687426	658.783929	18.870221	-0.038139	1.575166
203.755431	650.920261	18.875226	-0.038146	1.568114
203.662760	643.098111	18.880231	-0.038124	1.561043
203.335879	635.312724	18.885235	-0.038058	1.553940
203.426545	627.430383	18.890240	-0.038069	1.546777
203.419284	619.581016	18.895245	-0.038063	1.539596
203.444464	611.755804	18.900250	-0.038063	1.532409
203.349717	603.920739	18.905255	-0.038040	1.525161
203.417423	596.101193	18.910259	-0.038047	1.517917
203.280133	588.298592	18.915264	-0.038017	1.510623
203.151823	580.471931	18.920269	-0.037988	1.503273
203.158845	572.666129	18.925274	-0.037984	1.495926
203.139670	564.841122	18.930279	-0.037975	1.488522
202.978086	557.048485	18.935283	-0.037940	1.481088
202.984952	549.238603	18.940288	-0.037936	1.473628
202.900068	541.381238	18.945293	-0.037915	1.466069
202.606356	533.632419	18.950298	-0.037855	1.458542
202.614247	525.806683	18.955303	-0.037852	1.450950
202.709422	517.983631	18.960307	-0.037864	1.443335
202.512563	510.235658	18.965312	-0.037823	1.435706
202.386426	502.435369	18.970317	-0.037794	1.427995
202.573810	494.614762	18.975322	-0.037824	1.420274
202.297764	486.874881	18.980327	-0.037767	1.412515
202.173959	479.089323	18.985331	-0.037739	1.404693
202.101228	471.337467	18.990336	-0.037721	1.396869
201.922205	463.546201	18.995341	-0.037682	1.388943
201.900652	455.764333	19.000346	-0.037673	1.381008
201.744942	448.011451	19.005351	-0.037639	1.373034
201.803838	440.212689	19.010355	-0.037645	1.365003
201.914268	432.447112	19.015360	-0.037660	1.356968
201.757253	424.696563	19.020365	-0.037626	1.348854
201.554222	416.971577	19.025370	-0.037583	1.340709
201.441097	409.233608	19.030375	-0.037557	1.332517
201.288557	401.491917	19.035379	-0.037524	1.324263
201.451041	393.738160	19.040384	-0.037549	1.316001
201.457314	385.847021	19.045389	-0.037545	1.307511
201.262443	378.159787	19.050394	-0.037504	1.299149
201.172276	370.437959	19.055399	-0.037482	1.290715
201.139635	362.718170	19.060403	-0.037471	1.282238
201.314878	354.990517	19.065408	-0.037498	1.273735
201.080375	347.301495	19.070413	-0.037449	1.265141
201.072089	339.610267	19.075418	-0.037443	1.256528
200.856427	331.927618	19.080423	-0.037398	1.247826
200.765060	324.245726	19.085427	-0.037376	1.239087
200.785118	316.540375	19.090432	-0.037374	1.230281
200.575652	308.864897	19.095437	-0.037330	1.221401
200.754474	301.158870	19.100442	-0.037359	1.212497
200.398615	293.535221	19.105447	-0.037287	1.203518
200.494662	285.855683	19.110451	-0.037300	1.194495
200.518657	278.185835	19.115456	-0.037300	1.185401
200.067122	270.599282	19.120461	-0.037211	1.176239
200.091095	262.935569	19.125466	-0.037210	1.167010
199.952605	255.318758	19.130471	-0.037179	1.157731
199.652309	247.680994	19.135475	-0.037118	1.148317
199.937480	239.998223	19.140480	-0.037167	1.138893
199.740536	232.398233	19.145485	-0.037125	1.129391
199.641184	224.808184	19.150490	-0.037101	1.119842
199.568761	217.207921	19.155495	-0.037083	1.110203
199.389917	209.638396	19.160499	-0.037045	1.100496
199.403528	202.045961	19.165504	-0.037042	1.090716
199.244606	194.488362	19.170509	-0.037008	1.080854
198.873496	186.981597	19.175514	-0.036934	1.070920
198.879444	179.400398	19.180519	-0.036930	1.060880
198.565938	171.887794	19.185523	-0.036867	1.050763
198.285851	164.392962	19.190528	-0.036810	1.040578
198.176072	156.870517	19.195533	-0.036784	1.030296
197.867275	149.401004	19.200538	-0.036722	1.019935
197.322333	141.970942	19.205543	-0.036616	1.009465
197.178769	134.486386	19.210547	-0.036584	0.998907
196.755369	127.035059	19.215552	-0.036500	0.988214
196.137403	119.629955	19.220557	-0.036380	0.977422
195.858249	112.190588	19.225562	-0.036323	0.966545
195.504059	104.789911	19.230567	-0.036253	0.955582
194.718723	97.456425	19.235571	-0.036102	0.944479
194.448352	90.060082	19.240576	-0.036046	0.933285
193.959521	82.709884	19.245581	-0.035951	0.921967
193.446950	75.391235	19.250586	-0.035850	0.910551
192.763152	68.097148	19.255591	-0.035718	0.898980
192.216771	61.025665	19.260595	-0.035612	0.887651