Fri Mar 12 13:13:14 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.064919	-0.060880	0.000000	0.000002	0.720550

-0.148538	-0.031206	0.005005	0.000042	0.720534
0.101219	-0.072011	0.010010	-0.000004	0.720541
0.229834	-0.097664	0.015014	-0.000028	0.720535
0.118111	-0.076078	0.020019	-0.000008	0.720539
0.152286	-0.082653	0.025024	-0.000014	0.720538
0.046668	-0.063304	0.030029	0.000006	0.720539
-0.046800	-0.043184	0.035034	0.000023	0.720545
0.051995	-0.065073	0.040038	0.000005	0.720537
0.320487	-0.111474	0.045043	-0.000045	0.720540
0.500030	-0.142153	0.050048	-0.000078	0.720542
0.343775	-0.116720	0.055053	-0.000049	0.720537
0.176721	-0.082068	0.060058	-0.000018	0.720547
0.116949	-0.076473	0.065062	-0.000007	0.720537
0.166380	-0.082515	0.070067	-0.000016	0.720542
-0.060621	-0.170055	0.075072	0.000026	0.720290
-0.073821	-0.202948	0.080077	0.000029	0.720221
0.117848	-0.234441	0.085082	-0.000007	0.720226
0.195471	-0.250854	0.090086	-0.000021	0.720221
-0.014744	-0.212520	0.095091	0.000018	0.720223
0.065013	-0.223766	0.100096	0.000003	0.720228
0.137042	-0.254955	0.105101	-0.000010	0.720192
0.183556	-0.409877	0.110106	-0.000019	0.719903
0.185517	-0.415390	0.115110	-0.000019	0.719893
0.229581	-0.420875	0.120115	-0.000028	0.719898
0.124241	-0.400346	0.125120	-0.000008	0.719901
0.060775	-0.416268	0.130125	0.000004	0.719847
0.079930	-0.541899	0.135130	0.000001	0.719606
-0.191514	-0.498005	0.140134	0.000051	0.719598
-0.038273	-0.523529	0.145139	0.000023	0.719601
-0.227918	-0.489650	0.150144	0.000058	0.719601
-0.207732	-0.617836	0.155149	0.000054	0.719355
0.035067	-0.701223	0.160154	0.000009	0.719276
0.011350	-0.701999	0.165158	0.000014	0.719266
0.143866	-0.722883	0.170163	-0.000011	0.719272
-0.011720	-0.844632	0.175168	0.000018	0.718977
0.008899	-0.858919	0.180173	0.000014	0.718956
0.172338	-0.883493	0.185178	-0.000016	0.718965
0.037797	-0.957754	0.190182	0.000009	0.718771
0.255123	-1.060140	0.195187	-0.000031	0.718645
0.052583	-1.023607	0.200192	0.000006	0.718646
-0.319573	-1.038070	0.205197	0.000076	0.718486
-0.391184	-1.090194	0.210202	0.000089	0.718358
-0.345065	-1.102731	0.215206	0.000080	0.718350
-0.184270	-1.201848	0.220211	0.000051	0.718210
-0.035972	-1.324011	0.225216	0.000023	0.718021
-0.038744	-1.328548	0.230221	0.000024	0.718011
0.064873	-1.452008	0.235226	0.000004	0.717804
-0.141700	-1.467317	0.240230	0.000043	0.717701
-0.118827	-1.486687	0.245235	0.000039	0.717670
0.079747	-1.667510	0.250240	0.000002	0.717383
-0.220983	-1.617274	0.255245	0.000058	0.717376
-0.368765	-1.680906	0.260250	0.000085	0.717198
-0.452652	-1.723940	0.265254	0.000101	0.717083
-0.703386	-1.697125	0.270259	0.000148	0.717048
-1.056517	-1.778483	0.275264	0.000214	0.716763
-0.892210	-1.814311	0.280269	0.000183	0.716750
-0.580708	-1.955890	0.285274	0.000125	0.716579
-0.669910	-2.008451	0.290278	0.000142	0.716444
-0.691523	-2.043361	0.295283	0.000146	0.716367
-0.571179	-2.180633	0.300288	0.000124	0.716137
-0.665796	-2.170057	0.305293	0.000141	0.716125
-0.575913	-2.303951	0.310298	0.000125	0.715891
-0.720645	-2.283461	0.315302	0.000152	0.715881
-1.090820	-2.365401	0.320307	0.000221	0.715588
-3.436897	-1.965077	0.325312	0.000657	0.715553
-2.940463	-2.090215	0.330317	0.000565	0.715480
-3.517880	-2.108111	0.335322	0.000673	0.715240
-3.953725	-2.035557	0.340326	0.000754	0.715230
-3.725159	-2.075305	0.345331	0.000711	0.715232
-4.038794	-2.178025	0.350336	0.000770	0.714917
-5.036938	-2.006630	0.355341	0.000955	0.714904
-4.769438	-2.049540	0.360346	0.000906	0.714914
-4.322542	-2.203536	0.365350	0.000823	0.714766
-5.657799	-2.044540	0.370355	0.001071	0.714609
-5.493020	-2.073045	0.375360	0.001040	0.714611
-5.530272	-2.069056	0.380365	0.001047	0.714606
-5.634487	-2.151209	0.385370	0.001067	0.714406
-7.018535	-1.969760	0.390374	0.001325	0.714276
-6.485564	-2.064098	0.395379	0.001225	0.714278
-6.363275	-2.083384	0.400384	0.001203	0.714282
-6.880310	-1.998867	0.405389	0.001299	0.714267
-6.866092	-2.147436	0.410394	0.001296	0.713977
-7.261048	-2.081365	0.415398	0.001370	0.713969
-7.878576	-1.969865	0.420403	0.001485	0.713971
-7.367828	-2.060129	0.425408	0.001390	0.713973
-7.444825	-2.067005	0.430413	0.001404	0.713932
-8.042009	-2.098132	0.435418	0.001515	0.713658
-8.356289	-2.046155	0.440422	0.001574	0.713650
-8.572373	-2.005236	0.445427	0.001614	0.713655
-8.058871	-2.096503	0.450432	0.001519	0.713656
-8.616276	-2.000464	0.455437	0.001622	0.713649
-8.771785	-2.076434	0.460442	0.001651	0.713443
-9.251098	-2.034060	0.465446	0.001741	0.713357
-9.218585	-2.038375	0.470451	0.001735	0.713360
-9.298880	-2.020433	0.475456	0.001750	0.713367
-9.297381	-2.026090	0.480461	0.001749	0.713356
-8.880042	-2.102580	0.485466	0.001672	0.713352
-10.077107	-2.054865	0.490470	0.001895	0.713023
-10.455691	-1.985110	0.495475	0.001965	0.713027
-9.857379	-2.092356	0.500480	0.001854	0.713026
-9.995853	-2.072050	0.505485	0.001880	0.713017
-9.968214	-2.072792	0.510490	0.001874	0.713025
-10.173650	-2.038790	0.515494	0.001913	0.713020
-10.644261	-2.092161	0.520499	0.002000	0.712747
-11.329112	-1.987438	0.525504	0.002128	0.712713
-11.363759	-1.984689	0.530509	0.002134	0.712706
-10.904849	-2.063569	0.535514	0.002049	0.712711
-11.515597	-1.958171	0.540518	0.002163	0.712704
-11.532968	-1.954149	0.545523	0.002166	0.712706
-10.947936	-2.056247	0.550528	0.002057	0.712711
-12.129875	-1.999069	0.555533	0.002277	0.712405
-12.322711	-1.972873	0.560538	0.002313	0.712389
-12.017199	-2.030263	0.565542	0.002256	0.712383
-11.855226	-2.057883	0.570547	0.002226	0.712385
-12.351569	-1.966518	0.575552	0.002319	0.712391
-12.382755	-1.963796	0.580557	0.002324	0.712385
-11.721766	-2.077746	0.585562	0.002201	0.712393
-12.402455	-2.077455	0.590566	0.002328	0.712152
-13.232600	-1.959278	0.595571	0.002483	0.712092
-12.571684	-2.073807	0.600576	0.002360	0.712099
-12.918163	-2.016939	0.605581	0.002424	0.712089
-13.003749	-1.997668	0.610586	0.002440	0.712097
-12.931193	-2.013587	0.615590	0.002427	0.712091
-12.959391	-2.021580	0.620595	0.002432	0.712065
-13.623898	-2.052650	0.625600	0.002556	0.711767
-13.953264	-1.999337	0.630605	0.002617	0.711756
-13.647205	-2.048172	0.635610	0.002560	0.711768
-13.841377	-2.018323	0.640614	0.002596	0.711758
-13.940490	-1.998405	0.645619	0.002615	0.711762
-13.643570	-2.049291	0.650624	0.002560	0.711766
-14.066394	-1.996275	0.655629	0.002638	0.711722
-14.697868	-2.014567	0.660634	0.002756	0.711461
-14.743048	-2.010677	0.665638	0.002764	0.711453
-14.798502	-1.999048	0.670643	0.002775	0.711456
-14.803472	-1.996493	0.675648	0.002776	0.711459
-15.048699	-1.956253	0.680653	0.002821	0.711452
-14.512037	-2.048648	0.685658	0.002721	0.711459
-14.918260	-1.979210	0.690662	0.002797	0.711453
-15.531383	-2.005411	0.695667	0.002911	0.711183
-15.562992	-2.018293	0.700672	0.002917	0.711146
-15.726750	-1.995422	0.705677	0.002948	0.711133
-15.647359	-2.005046	0.710682	0.002933	0.711142
-15.895211	-1.964256	0.715686	0.002979	0.711135
-15.648803	-2.006263	0.720691	0.002933	0.711139
-15.587717	-2.015245	0.725696	0.002922	0.711143
-16.135716	-2.000789	0.730701	0.003024	0.710976
-16.531692	-1.980795	0.735706	0.003098	0.710875
-16.446174	-1.998824	0.740710	0.003082	0.710870
-16.850134	-1.927242	0.745715	0.003157	0.710869
-16.399408	-2.004174	0.750720	0.003073	0.710876
-16.457102	-2.000084	0.755725	0.003084	0.710863
-16.726098	-1.945516	0.760730	0.003134	0.710876
-16.460501	-2.077104	0.765734	0.003085	0.710708
-17.362783	-2.004654	0.770739	0.003253	0.710532
-17.233867	-2.025453	0.775744	0.003229	0.710536
-17.973203	-1.898519	0.780749	0.003366	0.710526
-17.313015	-2.010867	0.785754	0.003244	0.710537
-17.259709	-2.023701	0.790758	0.003234	0.710530
-17.902243	-1.908625	0.795763	0.003353	0.710531
-17.570561	-2.041087	0.800768	0.003292	0.710385
-18.684384	-1.929604	0.805773	0.003499	0.710211
-18.465159	-1.963725	0.810778	0.003458	0.710221
-18.654362	-1.932442	0.815782	0.003493	0.710216
-18.721917	-1.921510	0.820787	0.003506	0.710213
-18.288825	-1.995580	0.825792	0.003425	0.710220
-18.727861	-1.919618	0.830797	0.003507	0.710215
-18.422573	-1.970873	0.835802	0.003450	0.710221
-18.521661	-2.089129	0.840806	0.003469	0.709950
-19.707192	-1.906444	0.845811	0.003690	0.709892
-19.250201	-1.987197	0.850816	0.003605	0.709894
-19.009479	-2.035537	0.855821	0.003560	0.709883
-19.295203	-1.978033	0.860826	0.003613	0.709896
-19.495992	-1.946987	0.865830	0.003650	0.709886
-19.220640	-1.995096	0.870835	0.003599	0.709888
-19.654568	-2.037727	0.875840	0.003680	0.709648
-20.763239	-1.870166	0.880845	0.003886	0.709588
-20.248525	-1.956135	0.885850	0.003791	0.709600
-19.905805	-2.019764	0.890854	0.003727	0.709595
-20.671731	-1.884681	0.895859	0.003869	0.709592
-20.287193	-1.951899	0.900864	0.003798	0.709594
-20.155336	-1.980250	0.905869	0.003773	0.709584
-20.139143	-2.053111	0.910874	0.003770	0.709444
-21.482524	-1.902921	0.915878	0.004021	0.709266
-20.998050	-1.990292	0.920883	0.003930	0.709264
-21.148632	-1.960505	0.925888	0.003958	0.709270
-21.750723	-1.858322	0.930893	0.004071	0.709259
-21.090100	-1.973381	0.935898	0.003948	0.709265
-21.229379	-1.949430	0.940902	0.003974	0.709263
-21.831864	-1.844057	0.945907	0.004086	0.709259
-21.363299	-2.031665	0.950912	0.003999	0.709050
-22.285807	-1.918028	0.955917	0.004170	0.708949
-22.144563	-1.938420	0.960922	0.004144	0.708958
-22.116556	-1.948181	0.965926	0.004139	0.708949
-22.402326	-1.896249	0.970931	0.004192	0.708951
-21.951002	-1.974673	0.975936	0.004108	0.708954
-22.357726	-1.905043	0.980941	0.004184	0.708949
-22.280773	-1.973036	0.985946	0.004170	0.708840
-23.031353	-1.941075	0.990950	0.004309	0.708636
-23.044015	-1.938754	0.995955	0.004312	0.708636
-23.180314	-1.910227	1.000960	0.004337	0.708645
-23.063581	-1.934631	1.005965	0.004315	0.708637
-22.686809	-1.999575	1.010970	0.004245	0.708642
-23.186509	-1.912709	1.015974	0.004338	0.708637
-23.086778	-1.958904	1.020979	0.004320	0.708580
-23.386304	-2.018863	1.025984	0.004376	0.708353
-23.790439	-1.950702	1.030989	0.004451	0.708345
-23.809768	-1.943843	1.035994	0.004455	0.708352
-23.448241	-2.009500	1.040998	0.004387	0.708350
-23.803628	-1.947768	1.046003	0.004453	0.708346
-23.890537	-1.929565	1.051008	0.004470	0.708352
-23.870887	-2.024410	1.056013	0.004466	0.708169
-24.806014	-1.932821	1.061018	0.004640	0.708018
-24.690322	-1.957075	1.066022	0.004619	0.708011
-24.625961	-1.967081	1.071027	0.004607	0.708014
-24.490830	-1.990635	1.076032	0.004582	0.708015
-24.711032	-1.955526	1.081037	0.004623	0.708006
-24.782338	-1.937691	1.086042	0.004636	0.708016
-24.705479	-2.053625	1.091046	0.004622	0.707811
-25.682168	-1.937307	1.096051	0.004803	0.707696
-25.646102	-1.941297	1.101056	0.004797	0.707700
-25.587170	-1.954072	1.106061	0.004786	0.707696
-25.402915	-1.984008	1.111066	0.004752	0.707702
-25.447599	-1.977613	1.116070	0.004760	0.707698
-25.780621	-1.920175	1.121075	0.004822	0.707694
-25.569703	-2.072327	1.126080	0.004783	0.707465
-26.653990	-1.924505	1.131085	0.004985	0.707373
-26.354686	-1.975495	1.136090	0.004929	0.707378
-26.105411	-2.022741	1.141094	0.004883	0.707372
-26.782353	-1.903026	1.146099	0.005009	0.707370
-26.569573	-1.937038	1.151104	0.004969	0.707378
-26.527922	-1.950932	1.156109	0.004961	0.707365
-26.535313	-2.050196	1.161114	0.004963	0.707163
-27.401563	-1.939270	1.166118	0.005124	0.707076
-27.358852	-1.947208	1.171123	0.005116	0.707075
-26.788130	-2.045958	1.176128	0.005010	0.707081
-27.188294	-1.981174	1.181133	0.005084	0.707068
-27.259656	-1.962285	1.186138	0.005098	0.707080
-27.029758	-2.019956	1.191142	0.005055	0.707047
-27.972132	-2.000351	1.196147	0.005230	0.706749
-28.080872	-1.978649	1.201152	0.005251	0.706753
-28.342535	-1.936606	1.206157	0.005299	0.706744
-27.960575	-2.000546	1.211162	0.005228	0.706752
-28.105045	-1.977683	1.216166	0.005255	0.706746
-28.516219	-1.905453	1.221171	0.005332	0.706744
-28.193636	-1.957877	1.226176	0.005272	0.706754
-28.717295	-2.016841	1.231181	0.005369	0.706448
-29.190147	-1.934236	1.236186	0.005457	0.706445
-29.248928	-1.926335	1.241190	0.005468	0.706440
-29.093020	-1.955810	1.246195	0.005439	0.706436
-29.229379	-1.927787	1.251200	0.005465	0.706444
-29.119365	-1.951451	1.256205	0.005444	0.706436
-28.751474	-2.014712	1.261210	0.005376	0.706440
-29.219258	-2.056077	1.266214	0.005463	0.706189
-30.225180	-1.909892	1.271219	0.005650	0.706123
-29.564921	-2.023721	1.276224	0.005527	0.706130
-29.669018	-2.008633	1.281229	0.005547	0.706123
-30.107283	-1.929357	1.286234	0.005628	0.706126
-30.055182	-1.938385	1.291238	0.005619	0.706126
-29.963347	-1.956283	1.296243	0.005602	0.706123
-30.276678	-2.017552	1.301248	0.005660	0.705887
-30.915410	-1.918450	1.306253	0.005779	0.705858
-30.641041	-1.965394	1.311258	0.005728	0.705862
-30.608926	-1.971947	1.316262	0.005722	0.705860
-30.965289	-1.909326	1.321267	0.005788	0.705858
-30.810065	-1.934488	1.326272	0.005760	0.705863
-30.689151	-1.963002	1.331277	0.005737	0.705849
-31.411580	-1.995864	1.336282	0.005872	0.705524
-31.426528	-1.993756	1.341286	0.005874	0.705523
-31.875620	-1.915999	1.346291	0.005958	0.705518
-31.574014	-1.965202	1.351296	0.005902	0.705527
-31.633159	-1.958123	1.356301	0.005913	0.705520
-31.522386	-1.974121	1.361306	0.005892	0.705527
-31.565813	-1.992846	1.366310	0.005900	0.705474
-32.739211	-1.916105	1.371315	0.006119	0.705208
-32.383910	-1.976745	1.376320	0.006053	0.705213
-32.508339	-1.958220	1.381325	0.006076	0.705206
-32.679973	-1.925852	1.386330	0.006108	0.705209
-32.558130	-1.949564	1.391334	0.006085	0.705205
-32.691079	-1.926690	1.396339	0.006110	0.705203
-32.434824	-1.968626	1.401344	0.006062	0.705211
-33.227789	-1.988290	1.406349	0.006210	0.704886
-33.411786	-1.955888	1.411354	0.006244	0.704886
-33.213278	-1.991407	1.416358	0.006208	0.704885
-33.313326	-1.974746	1.421363	0.006226	0.704883
-33.165041	-1.998986	1.426368	0.006199	0.704887
-33.385077	-1.963570	1.431373	0.006240	0.704880
-33.276362	-2.018420	1.436378	0.006219	0.704808
-34.018294	-1.995569	1.441382	0.006358	0.704588
-34.138883	-1.975866	1.446387	0.006380	0.704584
-34.339703	-1.935545	1.451392	0.006417	0.704593
-34.347152	-1.939924	1.456397	0.006419	0.704581
-33.793963	-2.035770	1.461402	0.006316	0.704587
-34.040901	-1.992263	1.466406	0.006362	0.704586
-34.646652	-1.970883	1.471411	0.006475	0.704411
-35.010026	-1.979411	1.476416	0.006542	0.704263
-34.710290	-2.037005	1.481421	0.006487	0.704255
-35.151542	-1.955717	1.486426	0.006569	0.704260
-35.312899	-1.927350	1.491430	0.006599	0.704259
-35.040320	-1.978476	1.496435	0.006548	0.704254
-34.758072	-2.026176	1.501440	0.006496	0.704259
-35.654427	-1.973455	1.506445	0.006663	0.704043
-36.311168	-1.902163	1.511450	0.006785	0.703951
-35.683145	-2.016196	1.516454	0.006668	0.703947
-35.977640	-1.965136	1.521459	0.006723	0.703944
-35.947324	-1.965562	1.526464	0.006717	0.703954
-35.935537	-1.972591	1.531469	0.006715	0.703944
-35.927188	-1.969410	1.536474	0.006713	0.703953
-36.206831	-2.009954	1.541478	0.006766	0.703771
-37.163849	-1.909280	1.546483	0.006944	0.703630
-36.636637	-2.000157	1.551488	0.006846	0.703636
-37.294559	-1.887085	1.556493	0.006968	0.703627
-37.076819	-1.923482	1.561498	0.006928	0.703632
-36.704487	-1.993128	1.566502	0.006858	0.703625
-37.229700	-1.899152	1.571507	0.006956	0.703626
-36.974825	-1.966886	1.576512	0.006909	0.703581
-37.436629	-2.008267	1.581517	0.006995	0.703331
-37.421277	-2.007538	1.586522	0.006992	0.703338
-38.067939	-1.892757	1.591526	0.007112	0.703337
-37.957929	-1.914472	1.596531	0.007092	0.703333
-37.406367	-2.006833	1.601536	0.006989	0.703345
-38.231826	-1.864311	1.606541	0.007143	0.703335
-37.925319	-1.942904	1.611546	0.007086	0.703287
-38.159460	-2.042250	1.616550	0.007130	0.703002
-38.511625	-1.981211	1.621555	0.007195	0.702998
-38.878225	-1.913039	1.626560	0.007263	0.703004
-38.666525	-1.953812	1.631565	0.007224	0.702998
-38.490488	-1.981232	1.636570	0.007191	0.703006
-38.643832	-1.954484	1.641574	0.007220	0.703005
-38.698870	-1.998124	1.646579	0.007230	0.702897
-39.238411	-2.001143	1.651584	0.007331	0.702696
-39.535647	-1.954570	1.656589	0.007386	0.702683
-39.632890	-1.932879	1.661594	0.007404	0.702692
-39.334421	-1.985685	1.666598	0.007349	0.702693
-39.641778	-1.933059	1.671603	0.007406	0.702688
-39.579780	-1.940495	1.676608	0.007394	0.702695
-39.370094	-2.039074	1.681613	0.007355	0.702572
-40.419604	-1.950843	1.686618	0.007551	0.702372
-40.477279	-1.941884	1.691622	0.007562	0.702369
-40.681757	-1.907213	1.696627	0.007600	0.702365
-40.182566	-1.992027	1.701632	0.007507	0.702374
-40.387013	-1.960875	1.706637	0.007545	0.702363
-40.872972	-1.871150	1.711642	0.007635	0.702369
-40.186536	-2.022861	1.716646	0.007508	0.702310
-41.114567	-1.977010	1.721651	0.007680	0.702068
-41.334851	-1.933383	1.726656	0.007721	0.702077
-41.594549	-1.892453	1.731661	0.007770	0.702066
-41.247313	-1.952414	1.736666	0.007705	0.702070
-41.228655	-1.954751	1.741670	0.007702	0.702072
-41.585531	-1.892402	1.746675	0.007768	0.702069
-41.109611	-1.996610	1.751680	0.007680	0.702030
-41.991680	-1.984359	1.756685	0.007844	0.701736
-42.190840	-1.947239	1.761690	0.007881	0.701739
-42.212011	-1.942667	1.766694	0.007885	0.701741
-42.179926	-1.950831	1.771699	0.007879	0.701736
-42.172370	-1.948411	1.776704	0.007878	0.701744
-42.439610	-1.905323	1.781709	0.007927	0.701734
-41.899192	-2.015508	1.786714	0.007827	0.701706
-42.772172	-1.993509	1.791718	0.007989	0.701436
-43.222651	-1.916239	1.796723	0.008073	0.701429
-43.044873	-1.943288	1.801728	0.008040	0.701439
-43.131537	-1.932358	1.806733	0.008056	0.701430
-42.981466	-1.955044	1.811738	0.008028	0.701438
-42.835250	-1.982171	1.816742	0.008001	0.701436
-42.841513	-2.023050	1.821747	0.008002	0.701351
-43.775062	-1.967671	1.826752	0.008176	0.701126
-44.004895	-1.931709	1.831757	0.008219	0.701115
-43.975339	-1.933062	1.836762	0.008214	0.701123
-43.636235	-1.994623	1.841766	0.008151	0.701121
-43.866447	-1.955357	1.846771	0.008193	0.701117
-43.709490	-1.980661	1.851776	0.008164	0.701123
-43.790503	-2.029035	1.856781	0.008179	0.700995
-44.833922	-1.902386	1.861786	0.008374	0.700875
-44.381146	-1.983718	1.866790	0.008289	0.700874
-44.445023	-1.974921	1.871795	0.008301	0.700868
-44.612511	-1.940868	1.876800	0.008332	0.700877
-44.737211	-1.923304	1.881805	0.008356	0.700867
-44.550562	-1.952981	1.886810	0.008321	0.700875
-45.007874	-2.022181	1.891814	0.008406	0.700569
-45.623849	-1.932638	1.896819	0.008521	0.700528
-45.271990	-1.989507	1.901824	0.008455	0.700540
-45.301956	-1.991030	1.906829	0.008461	0.700526
-45.680474	-1.920615	1.911834	0.008532	0.700531
-45.610534	-1.931291	1.916838	0.008519	0.700535
-45.500820	-1.984249	1.921843	0.008498	0.700467
-46.194676	-1.980771	1.926848	0.008627	0.700223
-46.752701	-1.885194	1.931853	0.008731	0.700215
-46.584577	-1.914035	1.936858	0.008700	0.700218
-46.245755	-1.973932	1.941862	0.008637	0.700219
-46.627834	-1.907886	1.946867	0.008708	0.700214
-46.529031	-1.921786	1.951872	0.008690	0.700222
-46.398090	-1.948652	1.956877	0.008665	0.700215
-47.148861	-1.971365	1.961882	0.008805	0.699897
-47.227748	-1.957271	1.966886	0.008820	0.699897
-47.372030	-1.936438	1.971891	0.008847	0.699887
-46.896176	-2.015390	1.976896	0.008758	0.699899
-47.258746	-1.956051	1.981901	0.008826	0.699888
-47.443154	-1.919408	1.986906	0.008860	0.699896
-46.944278	-2.045275	1.991910	0.008767	0.699821
-48.354834	-1.903363	1.996915	0.009030	0.699598
-47.758269	-2.008616	2.001920	0.008919	0.699600

-47.985596	-1.969178	2.011917	0.008961	0.699598
-47.863895	-1.991717	2.021914	0.008939	0.699596
-48.017692	-1.964083	2.031910	0.008967	0.699597
-48.414168	-1.986743	2.041907	0.009041	0.699407
-48.584475	-1.954548	2.051904	0.009073	0.699410
-48.545780	-1.940923	2.061901	0.009066	0.699452
-47.763414	-2.008726	2.071898	0.008920	0.699598
-48.036231	-1.960752	2.081894	0.008971	0.699596
-48.022961	-1.963991	2.091891	0.008969	0.699594
-47.686864	-2.022994	2.101888	0.008906	0.699596
-47.991704	-1.967307	2.111885	0.008963	0.699599
-47.843451	-1.995043	2.121882	0.008935	0.699596
-47.949048	-1.976622	2.131878	0.008955	0.699595
-47.839705	-1.996379	2.141875	0.008935	0.699594
-47.882777	-1.965008	2.151872	0.008943	0.699642
-47.241405	-1.955038	2.161869	0.008824	0.699895
-47.123709	-1.976169	2.171866	0.008802	0.699894
-47.466783	-1.914627	2.181862	0.008866	0.699895
-46.942240	-2.009777	2.191859	0.008768	0.699891
-46.491504	-1.948539	2.201856	0.008684	0.700179
-46.277068	-1.966808	2.211853	0.008644	0.700219
-46.076612	-2.002351	2.221850	0.008607	0.700219
-46.401886	-1.947028	2.231846	0.008668	0.700214
-45.529229	-1.964624	2.241843	0.008505	0.700494
-45.477172	-1.955699	2.251840	0.008495	0.700530
-45.065170	-2.026576	2.261837	0.008419	0.700535
-45.134990	-2.012763	2.271834	0.008432	0.700538
-44.629353	-1.962177	2.281830	0.008338	0.700823
-44.172964	-2.018904	2.291827	0.008253	0.700873
-44.392061	-1.979358	2.301824	0.008294	0.700874
-44.330845	-1.990416	2.311821	0.008282	0.700874
-44.136614	-1.909192	2.321818	0.008246	0.701108
-43.868906	-1.950629	2.331814	0.008196	0.701121
-43.840670	-1.954146	2.341811	0.008191	0.701124
-43.329047	-1.923609	2.351808	0.008096	0.701370
-42.820998	-1.980994	2.361805	0.008002	0.701438
-43.065921	-1.937616	2.371802	0.008047	0.701437
-42.737946	-1.918680	2.381798	0.007986	0.701593
-41.875012	-2.000870	2.391795	0.007826	0.701738
-42.048180	-1.967971	2.401792	0.007858	0.701742
-41.972579	-1.975066	2.411789	0.007844	0.701755
-41.551041	-1.892607	2.421786	0.007765	0.702074
-41.297711	-1.939621	2.431782	0.007718	0.702070
-41.375282	-1.925893	2.441779	0.007733	0.702070
-40.586408	-1.942333	2.451776	0.007586	0.702321
-40.416950	-1.950116	2.461773	0.007554	0.702366
-40.289299	-1.972092	2.471770	0.007531	0.702368
-40.324708	-1.904489	2.481766	0.007537	0.702491
-39.432199	-1.966439	2.491763	0.007371	0.702688
-39.483428	-1.956093	2.501760	0.007381	0.702690
-39.408841	-1.968916	2.511757	0.007367	0.702691
-38.976329	-1.898210	2.521754	0.007286	0.702989
-38.717651	-1.937781	2.531750	0.007238	0.703003
-38.772910	-1.928303	2.541747	0.007249	0.703002
-38.277629	-1.911104	2.551744	0.007157	0.703215
-37.731532	-1.945866	2.561741	0.007055	0.703341
-37.801086	-1.932910	2.571738	0.007068	0.703342
-37.655971	-1.937362	2.581734	0.007041	0.703385
-37.052459	-1.920498	2.591731	0.006929	0.703636
-36.893576	-1.947845	2.601728	0.006899	0.703638
-36.881201	-1.949342	2.611725	0.006897	0.703639
-36.567295	-1.890559	2.621722	0.006838	0.703871
-36.066066	-1.939653	2.631718	0.006745	0.703952
-36.170974	-1.922254	2.641715	0.006765	0.703949
-35.828895	-1.932699	2.651712	0.006701	0.704051
-34.901563	-1.992899	2.661709	0.006529	0.704263
-35.223726	-1.937311	2.671706	0.006589	0.704259
-35.049194	-1.970005	2.681702	0.006556	0.704256
-34.438686	-1.965853	2.691699	0.006442	0.704483
-34.370383	-1.925546	2.701696	0.006430	0.704589
-34.186714	-1.957813	2.711693	0.006396	0.704590
-34.242630	-1.932201	2.721690	0.006406	0.704621
-33.263392	-1.975447	2.731686	0.006224	0.704886
-33.620537	-1.912501	2.741683	0.006290	0.704884
-33.379701	-1.952631	2.751680	0.006246	0.704890
-32.878126	-1.934887	2.761677	0.006152	0.705106
-32.489449	-1.952072	2.771674	0.006080	0.705210
-32.542202	-1.943044	2.781670	0.006090	0.705209
-32.580390	-1.907379	2.791667	0.006097	0.705267
-31.488908	-1.975394	2.801664	0.005894	0.705522
-31.422237	-1.985830	2.811661	0.005881	0.705525
-31.448691	-1.981957	2.821658	0.005886	0.705523
-31.227794	-1.946395	2.831654	0.005845	0.705674
-30.644017	-1.958952	2.841651	0.005737	0.705858
-30.557227	-1.973984	2.851648	0.005721	0.705859
-30.691498	-1.948054	2.861645	0.005746	0.705862
-29.989138	-1.959178	2.871642	0.005615	0.706092
-29.991341	-1.942136	2.881638	0.005615	0.706125
-30.086277	-1.926756	2.891635	0.005633	0.706122
-29.596350	-1.926291	2.901632	0.005542	0.706298
-29.183597	-1.927991	2.911629	0.005465	0.706443
-29.119733	-1.938508	2.921626	0.005453	0.706444
-28.894385	-1.942805	2.931622	0.005411	0.706516
-28.216145	-1.946362	2.941619	0.005285	0.706752
-27.953050	-1.992547	2.951616	0.005236	0.706753
-28.290606	-1.930964	2.961613	0.005299	0.706756
-27.688122	-1.909686	2.971610	0.005187	0.707014
-27.516633	-1.906765	2.981606	0.005155	0.707081
-27.405884	-1.927506	2.991603	0.005135	0.707079
-27.093185	-1.915178	3.001600	0.005076	0.707216
-26.663378	-1.910314	3.011597	0.004996	0.707379
-26.499863	-1.941239	3.021594	0.004966	0.707375
-26.640391	-1.888254	3.031590	0.004992	0.707431
-25.733193	-1.917064	3.041587	0.004823	0.707698
-25.493297	-1.960240	3.051584	0.004779	0.707697
-25.693546	-1.924613	3.061581	0.004816	0.707697
-25.035826	-1.925779	3.071578	0.004694	0.707929
-24.780521	-1.930655	3.081574	0.004646	0.708011
-25.012948	-1.890034	3.091571	0.004689	0.708009
-24.531855	-1.931796	3.101568	0.004600	0.708097
-23.825776	-1.931096	3.111565	0.004469	0.708351
-23.621079	-1.968075	3.121562	0.004431	0.708350
-24.011567	-1.899167	3.131558	0.004503	0.708348
-23.354145	-1.923414	3.141555	0.004381	0.708534
-23.115562	-1.914854	3.151552	0.004337	0.708636
-23.078401	-1.920061	3.161549	0.004330	0.708639
-22.954442	-1.898790	3.171546	0.004307	0.708726
-22.253970	-1.910357	3.181542	0.004176	0.708953
-22.211380	-1.917936	3.191539	0.004168	0.708952
-22.173265	-1.924092	3.201536	0.004161	0.708954
-21.634545	-1.886719	3.211533	0.004061	0.709221
-21.216040	-1.940205	3.221530	0.003983	0.709263
-21.314860	-1.923441	3.231526	0.004002	0.709261
-21.043661	-1.916535	3.241523	0.003951	0.709371
-20.309313	-1.937582	3.251520	0.003815	0.709591
-20.386961	-1.922442	3.261517	0.003829	0.709593
-20.340756	-1.929766	3.271514	0.003821	0.709595
-19.814573	-1.896907	3.281510	0.003723	0.709848
-19.405318	-1.950051	3.291507	0.003646	0.709888
-19.496250	-1.932075	3.301504	0.003663	0.709891
-19.335263	-1.916148	3.311501	0.003634	0.709980
-18.543922	-1.940168	3.321498	0.003486	0.710214
-18.770321	-1.900005	3.331494	0.003528	0.710214
-18.379649	-1.969849	3.341491	0.003456	0.710213
-18.130857	-1.903556	3.351488	0.003409	0.710434
-17.573695	-1.953811	3.361485	0.003306	0.710532
-17.790499	-1.915515	3.371482	0.003346	0.710531
-17.531768	-1.942946	3.381478	0.003298	0.710568
-16.692064	-1.942947	3.391475	0.003142	0.710867
-16.787023	-1.924957	3.401472	0.003160	0.710869
-16.593792	-1.957225	3.411469	0.003124	0.710873
-16.535012	-1.905635	3.421466	0.003113	0.710997
-15.920277	-1.947307	3.431462	0.002998	0.711132
-15.998379	-1.932829	3.441459	0.003013	0.711133
-16.099832	-1.902950	3.451456	0.003032	0.711157
-14.957527	-1.957875	3.461453	0.002819	0.711453
-15.163822	-1.921846	3.471450	0.002858	0.711452
-15.192928	-1.915864	3.481446	0.002863	0.711453
-14.686037	-1.914091	3.491443	0.002769	0.711637
-14.152086	-1.948198	3.501440	0.002669	0.711758
-14.080506	-1.959765	3.511437	0.002656	0.711760
-14.296808	-1.907334	3.521434	0.002696	0.711788
-13.484688	-1.902649	3.531430	0.002545	0.712086
-13.183986	-1.956924	3.541427	0.002489	0.712084
-13.451490	-1.906775	3.551424	0.002539	0.712089
-12.787745	-1.931056	3.561421	0.002416	0.712276
-12.558553	-1.914840	3.571418	0.002373	0.712390
-12.610190	-1.907000	3.581414	0.002383	0.712387
-12.458646	-1.899738	3.591411	0.002355	0.712455
-11.569759	-1.930285	3.601408	0.002189	0.712710
-11.252650	-1.984656	3.611405	0.002130	0.712714
-11.418525	-1.957012	3.621402	0.002161	0.712710
-11.079293	-1.947644	3.631398	0.002098	0.712849
-10.399512	-1.982564	3.641395	0.001971	0.713020
-10.605861	-1.943979	3.651392	0.002010	0.713024
-10.249382	-2.006972	3.661389	0.001944	0.713025
-9.977114	-1.942429	3.671386	0.001893	0.713249
-9.373431	-1.993402	3.681382	0.001781	0.713362
-9.591427	-1.956004	3.691379	0.001821	0.713359
-9.164330	-2.029848	3.701376	0.001742	0.713363
-8.714516	-2.003916	3.711373	0.001658	0.713574
-8.801377	-1.947472	3.721370	0.001674	0.713656
-8.543201	-1.992790	3.731366	0.001626	0.713657
-8.621793	-1.971976	3.741363	0.001641	0.713670
-7.767042	-1.972721	3.751360	0.001482	0.713971
-7.500303	-2.020193	3.761357	0.001432	0.713971
-7.866718	-1.955175	3.771354	0.001501	0.713971
-7.573570	-1.933450	3.781350	0.001446	0.714118
-6.853724	-1.982025	3.791347	0.001312	0.714276
-6.772973	-1.994471	3.801344	0.001297	0.714280
-6.574200	-2.028810	3.811341	0.001260	0.714282
-6.157944	-1.980733	3.821338	0.001183	0.714524
-5.498358	-2.055563	3.831334	0.001060	0.714609
-6.001001	-1.968247	3.841331	0.001154	0.714604
-5.462674	-2.061227	3.851328	0.001053	0.714610
-5.262968	-1.964981	3.861325	0.001016	0.714872
-4.993362	-1.992640	3.871322	0.000966	0.714912
-4.957131	-1.999674	3.881318	0.000959	0.714911
-5.030520	-1.925425	3.891315	0.000973	0.715032
-3.791259	-2.044472	3.901312	0.000742	0.715234
-3.708639	-2.059060	3.911309	0.000727	0.715234
-4.049940	-1.998286	3.921306	0.000791	0.715234
-3.245575	-2.034662	3.931302	0.000641	0.715446
-2.889369	-2.046749	3.941299	0.000575	0.715547
-2.694769	-2.081404	3.951296	0.000539	0.715547
-3.062332	-2.015204	3.961293	0.000607	0.715549
-2.844353	-1.934371	3.971290	0.000566	0.715786
-2.070100	-2.022204	3.981286	0.000422	0.715885
-2.497971	-1.945419	3.991283	0.000502	0.715886
-2.388367	-1.912478	4.001280	0.000482	0.715990
-1.690441	-1.964053	4.011277	0.000352	0.716134
-1.625826	-1.974131	4.021274	0.000340	0.716137
-2.035872	-1.834437	4.031270	0.000416	0.716268
-1.984049	-1.752418	4.041267	0.000407	0.716449
-1.987761	-1.726959	4.051264	0.000407	0.716498
-1.338385	-1.711197	4.061261	0.000286	0.716758
-1.205901	-1.733837	4.071258	0.000262	0.716760
-0.974502	-1.643492	4.081254	0.000219	0.717020
-1.032351	-1.598769	4.091251	0.000229	0.717088
-1.447669	-1.429603	4.101248	0.000307	0.717276
-1.220912	-1.417581	4.111245	0.000265	0.717380
-1.059683	-1.304501	4.121242	0.000235	0.717660
-0.998716	-1.265966	4.131238	0.000223	0.717758
-0.608589	-1.205841	4.141235	0.000151	0.718014
-0.693628	-1.108399	4.151232	0.000166	0.718176
-0.452740	-1.060282	4.161229	0.000122	0.718356
-0.778981	-0.872258	4.171226	0.000182	0.718612
-0.726233	-0.789111	4.181222	0.000172	0.718795
-0.784699	-0.673498	4.191219	0.000183	0.719002
-0.743360	-0.545359	4.201216	0.000176	0.719269
-0.377644	-0.462213	4.211213	0.000107	0.719562
-0.233212	-0.375762	4.221210	0.000081	0.719783
-0.516709	-0.203903	4.231206	0.000133	0.720022
-0.613482	-0.041372	4.241203	0.000151	0.720308
-0.389385	0.064672	4.251200	0.000110	0.720595
0.000000	0.179870	4.261197	0.000037	0.720958

-0.172300	0.798285	4.266202	0.000069	0.722114
-0.060213	2.049873	4.271206	0.000047	0.724607
0.393956	3.820689	4.276211	-0.000039	0.728223
0.711357	6.178853	4.281216	-0.000099	0.732912
0.843718	9.076360	4.286221	-0.000126	0.738544
0.992397	12.438887	4.291226	-0.000156	0.745024
1.454516	16.212246	4.296230	-0.000244	0.752329
1.873070	20.394474	4.301235	-0.000325	0.760313
2.172703	24.992414	4.306240	-0.000383	0.768941
2.776977	29.918713	4.311245	-0.000499	0.778171
3.126489	35.224587	4.316250	-0.000568	0.787895
3.330277	40.881208	4.321254	-0.000609	0.798077
3.723356	46.797346	4.326259	-0.000686	0.808646
4.239333	52.970541	4.331264	-0.000786	0.819560
4.933571	59.403323	4.336269	-0.000920	0.830828
5.466353	66.077524	4.341274	-0.001023	0.842303
5.975517	72.985509	4.346278	-0.001123	0.854006
7.173760	79.977445	4.351283	-0.001350	0.865886
8.588700	87.136799	4.356288	-0.001618	0.877936
9.156159	94.627667	4.361293	-0.001729	0.890114
9.733890	102.273060	4.366298	-0.001841	0.902373
10.378060	110.060709	4.371302	-0.001966	0.914705
11.071341	117.946033	4.376307	-0.002101	0.927036
11.726451	125.962179	4.381312	-0.002228	0.939392
12.508319	134.066239	4.386317	-0.002379	0.951751
12.971828	142.298421	4.391322	-0.002470	0.964058
13.614993	150.595206	4.396326	-0.002595	0.976349
14.017646	159.009018	4.401331	-0.002676	0.988594
14.492742	167.449825	4.406336	-0.002770	1.000745
15.181869	175.897676	4.411341	-0.002904	1.012813
15.727838	184.409454	4.416346	-0.003011	1.024791
16.201785	192.973521	4.421350	-0.003105	1.036686
16.827213	201.538105	4.426355	-0.003227	1.048481
17.461252	210.127115	4.431360	-0.003350	1.060180
18.113566	218.751532	4.436365	-0.003477	1.071801
18.525896	227.394579	4.441370	-0.003560	1.083268
19.252795	236.016622	4.446374	-0.003701	1.094657
20.113340	244.616329	4.451379	-0.003866	1.105930
20.770845	253.249980	4.456384	-0.003994	1.117087
21.318317	261.898318	4.461389	-0.004102	1.128128
21.732914	270.564801	4.466394	-0.004185	1.139056
22.280724	279.223189	4.471398	-0.004292	1.149898
22.604526	287.908672	4.476403	-0.004358	1.160625
23.131018	296.507229	4.481408	-0.004462	1.171190
23.818651	305.089205	4.486413	-0.004596	1.181673
24.357400	313.688794	4.491418	-0.004701	1.192055
24.913163	322.263313	4.496422	-0.004810	1.202320
25.356867	330.866108	4.501427	-0.004899	1.212509
25.892758	339.423016	4.506432	-0.005004	1.222578
26.384270	348.011698	4.511437	-0.005101	1.232592
26.915821	356.532661	4.516442	-0.005206	1.242456
27.689679	365.023238	4.521446	-0.005355	1.252254
28.036070	373.565571	4.526451	-0.005425	1.261953
28.427691	382.083254	4.531456	-0.005504	1.271558
29.390777	390.504132	4.536461	-0.005688	1.281090
29.638963	399.030856	4.541466	-0.005740	1.290536
29.908362	407.547426	4.546470	-0.005796	1.299906
30.490211	416.033648	4.551475	-0.005910	1.309233
30.815552	424.585454	4.556480	-0.005976	1.318517
31.226923	432.999062	4.561485	-0.006058	1.327605
31.761735	441.393120	4.566490	-0.006163	1.336631
32.180285	449.789706	4.571494	-0.006246	1.345579
32.580358	458.213826	4.576499	-0.006326	1.354493
32.947819	466.591512	4.581504	-0.006400	1.363295
33.331771	474.980776	4.586509	-0.006477	1.372055
33.737742	483.331117	4.591514	-0.006558	1.380723
33.899905	491.739030	4.596518	-0.006594	1.389355
34.284269	500.109911	4.601523	-0.006671	1.397932
34.755910	508.408273	4.606528	-0.006764	1.406399
35.345886	516.731134	4.611533	-0.006879	1.414859
35.766737	525.044912	4.616538	-0.006963	1.423232
36.297885	533.354332	4.621542	-0.007067	1.431569
36.945034	541.645686	4.626547	-0.007193	1.439858
37.198605	549.972776	4.631552	-0.007246	1.448072
37.514941	558.321060	4.636557	-0.007310	1.456270
37.914145	566.599572	4.641562	-0.007390	1.464367
38.312066	574.947117	4.646566	-0.007469	1.472486
38.763549	583.231132	4.651571	-0.007559	1.480508
39.329591	591.465591	4.656576	-0.007669	1.488457
39.496585	599.788354	4.661581	-0.007706	1.496385
39.879409	608.044092	4.666586	-0.007783	1.504242
40.250685	616.318954	4.671590	-0.007857	1.512074
40.604952	624.578754	4.676595	-0.007928	1.519849
41.002590	632.813560	4.681600	-0.008008	1.527567
41.487137	641.069017	4.686605	-0.008103	1.535279
41.755845	649.332150	4.691610	-0.008159	1.542926
42.071797	657.590929	4.696614	-0.008223	1.550539
42.426116	665.851923	4.701619	-0.008294	1.558122
42.785623	674.050878	4.706624	-0.008366	1.565613
43.366305	682.277100	4.711629	-0.008480	1.573125
43.590154	690.515263	4.716634	-0.008527	1.580560
44.184532	698.710643	4.721638	-0.008643	1.587975
44.639367	706.950829	4.726643	-0.008733	1.595376
44.853476	715.175306	4.731648	-0.008778	1.602694
45.419738	723.375668	4.736653	-0.008889	1.610007
45.723561	731.604401	4.741658	-0.008951	1.617275
46.029920	739.815017	4.746662	-0.009013	1.624494
46.289439	748.082809	4.751667	-0.009067	1.631725
46.667066	756.278656	4.756672	-0.009143	1.638878
47.171953	764.427554	4.761677	-0.009242	1.645977
47.342043	772.662824	4.766682	-0.009279	1.653074
47.754210	780.821130	4.771686	-0.009361	1.660107
48.207006	788.994663	4.776691	-0.009450	1.667129
48.107600	797.252812	4.781696	-0.009437	1.674118
48.647434	805.392619	4.786701	-0.009543	1.681065
48.797691	813.594335	4.791706	-0.009576	1.687982
49.292046	821.759072	4.796710	-0.009674	1.694886
49.708674	829.925493	4.801715	-0.009757	1.701753
49.976737	838.101737	4.806720	-0.009812	1.708581
50.403571	846.301314	4.811725	-0.009897	1.715422
50.693324	854.443510	4.816730	-0.009956	1.722170
51.009904	862.618336	4.821734	-0.010020	1.728923
51.542818	870.771269	4.826739	-0.010125	1.735658
51.649423	878.954322	4.831744	-0.010150	1.742338
52.237500	887.086831	4.836749	-0.010265	1.749012
52.635446	895.249597	4.841754	-0.010344	1.755661
52.815542	903.419875	4.846758	-0.010383	1.762263
53.179472	911.577925	4.851763	-0.010456	1.768854
53.425874	919.744204	4.856768	-0.010507	1.775412
53.867380	927.886462	4.861773	-0.010594	1.781951
54.066396	936.072511	4.866778	-0.010637	1.788471
54.425810	944.274463	4.871782	-0.010709	1.794999
54.937117	952.375126	4.876787	-0.010810	1.801443
55.284800	960.496956	4.881792	-0.010880	1.807860
55.916565	968.622305	4.886797	-0.011002	1.814291
56.318707	976.744530	4.891802	-0.011083	1.820669
56.503236	984.908646	4.896806	-0.011122	1.827031
57.026530	993.053728	4.901811	-0.011225	1.833397
57.176956	1001.205475	4.906816	-0.011258	1.839702
57.571369	1009.332232	4.911821	-0.011337	1.845994
58.018900	1017.468353	4.916826	-0.011426	1.852279
58.121483	1025.644811	4.921830	-0.011450	1.858532
58.662818	1033.735588	4.926835	-0.011556	1.864751
58.883299	1041.895682	4.931840	-0.011602	1.870964
59.264665	1050.035621	4.936845	-0.011679	1.877159
59.631567	1058.134453	4.941850	-0.011752	1.883302
59.674324	1066.295654	4.946854	-0.011765	1.889434
59.997233	1074.437940	4.951859	-0.011831	1.895564
60.305714	1082.543902	4.956864	-0.011894	1.901645
60.470317	1090.690766	4.961869	-0.011930	1.907722
60.953239	1098.809690	4.966874	-0.012025	1.913793
61.547886	1106.861779	4.971878	-0.012141	1.919809
62.140833	1114.962637	4.976883	-0.012256	1.925841
62.222483	1123.131811	4.981888	-0.012277	1.931848
62.967153	1131.210445	4.986893	-0.012421	1.937843
63.396500	1139.318896	4.991898	-0.012506	1.943807
63.632483	1147.469858	4.996902	-0.012555	1.949762
63.917981	1155.654492	5.001907	-0.012614	1.955728
64.114348	1163.746483	5.006912	-0.012655	1.961600
64.728753	1171.807535	5.011917	-0.012775	1.967477
65.052543	1179.938819	5.016922	-0.012841	1.973355
65.292385	1188.046295	5.021926	-0.012891	1.979190
65.776686	1196.137997	5.026931	-0.012986	1.985022
66.083671	1204.246508	5.031936	-0.013048	1.990831
66.530241	1212.358675	5.036941	-0.013137	1.996639
66.903765	1220.445874	5.041946	-0.013212	2.002406
67.224656	1228.563185	5.046950	-0.013277	2.008171
67.443168	1236.716820	5.051955	-0.013323	2.013935
67.898083	1244.780250	5.056960	-0.013412	2.019643
68.447820	1252.868518	5.061965	-0.013520	2.025363
68.683931	1261.018287	5.066970	-0.013569	2.031076
68.913436	1269.152444	5.071974	-0.013617	2.036762
69.508386	1277.210551	5.076979	-0.013733	2.042417
69.748627	1285.304954	5.081984	-0.013783	2.048045
70.008028	1293.441893	5.086989	-0.013837	2.053689
70.293454	1301.534741	5.091994	-0.013895	2.059290
70.730739	1309.597608	5.096998	-0.013982	2.064870
71.020835	1317.721949	5.102003	-0.014041	2.070462
71.277724	1325.829856	5.107008	-0.014094	2.076024
71.566663	1333.916505	5.112013	-0.014153	2.081560
71.805052	1342.014330	5.117018	-0.014203	2.087084
72.133534	1350.101808	5.122022	-0.014269	2.092596
72.677945	1358.184880	5.127027	-0.014376	2.098111
73.067162	1366.251371	5.132032	-0.014454	2.103585
73.476954	1374.358539	5.137037	-0.014535	2.109074
73.827021	1382.519572	5.142042	-0.014606	2.114578
74.308526	1390.553225	5.147046	-0.014701	2.119996
74.699988	1398.637192	5.152051	-0.014779	2.125425
74.551800	1406.778432	5.157056	-0.014756	2.130827
74.963163	1414.859368	5.162061	-0.014838	2.136228
75.120158	1422.954130	5.167066	-0.014873	2.141601
75.464678	1431.015969	5.172070	-0.014942	2.146956
75.914813	1439.108730	5.177075	-0.015031	2.152328
76.270143	1447.181126	5.182080	-0.015103	2.157664
76.596814	1455.259987	5.187085	-0.015169	2.162988
76.561839	1463.385204	5.192090	-0.015167	2.168296
76.818558	1471.476347	5.197094	-0.015220	2.173596
77.294642	1479.537289	5.202099	-0.015314	2.178883
77.290967	1487.627011	5.207104	-0.015319	2.184132
77.826807	1495.688961	5.212109	-0.015424	2.189400
78.177489	1503.812673	5.217114	-0.015494	2.194678
78.311616	1511.886138	5.222118	-0.015525	2.199891
78.724082	1519.926941	5.227123	-0.015607	2.205097
79.029788	1528.004296	5.232128	-0.015669	2.210303
79.459883	1536.092712	5.237133	-0.015754	2.215516
79.603603	1544.181484	5.242138	-0.015786	2.220690
80.247291	1552.203363	5.247142	-0.015911	2.225855
80.555641	1560.316690	5.252147	-0.015974	2.231036
80.871047	1568.406693	5.257152	-0.016038	2.236191
81.425378	1576.438212	5.262157	-0.016146	2.241317
81.694291	1584.527619	5.267162	-0.016202	2.246444
81.593856	1592.665082	5.272166	-0.016188	2.251556
82.042897	1600.744763	5.277171	-0.016277	2.256669
82.280926	1608.801580	5.282176	-0.016327	2.261737
82.550160	1616.892821	5.287181	-0.016382	2.266818
82.652228	1625.042372	5.292186	-0.016406	2.271910
83.125804	1633.099614	5.297190	-0.016500	2.276964
83.315198	1641.155732	5.302195	-0.016540	2.281983
83.392959	1649.215872	5.307200	-0.016560	2.286983
83.764490	1657.281298	5.312205	-0.016634	2.292000
84.316329	1665.309711	5.317210	-0.016742	2.296999
84.505975	1673.387493	5.322214	-0.016783	2.301987
84.838534	1681.453405	5.327219	-0.016850	2.306969
85.203628	1689.509076	5.332224	-0.016923	2.311936
85.453615	1697.599616	5.337229	-0.016975	2.316904
85.749346	1705.646908	5.342234	-0.017035	2.321839
86.109737	1713.708359	5.347238	-0.017108	2.326777
86.706243	1721.759659	5.352243	-0.017224	2.331719
87.042482	1729.837057	5.357248	-0.017292	2.336643
87.219313	1737.915938	5.362253	-0.017330	2.341546
87.733077	1745.965663	5.367258	-0.017431	2.346448
87.794704	1754.097710	5.372262	-0.017447	2.351352
88.318516	1762.156469	5.377267	-0.017550	2.356240
88.667029	1770.196618	5.382272	-0.017620	2.361092
88.965007	1778.258538	5.387277	-0.017681	2.365943
88.940231	1786.377801	5.392282	-0.017682	2.370792
89.138417	1794.440462	5.397286	-0.017724	2.375616
89.544262	1802.500173	5.402291	-0.017805	2.380444
89.747676	1810.543679	5.407296	-0.017848	2.385237
90.218548	1818.598813	5.412301	-0.017941	2.390048
90.590592	1826.682392	5.417306	-0.018015	2.394859
90.711562	1834.732875	5.422310	-0.018043	2.399620
90.941646	1842.789404	5.427315	-0.018091	2.404385
91.209504	1850.866082	5.432320	-0.018146	2.409154
91.529466	1858.956822	5.437325	-0.018211	2.413926
91.702193	1867.021695	5.442330	-0.018248	2.418663
92.017570	1875.045366	5.447334	-0.018312	2.423376
92.589957	1883.101498	5.452339	-0.018424	2.428120
92.660065	1891.250594	5.457344	-0.018442	2.432869
93.239693	1899.286872	5.462349	-0.018555	2.437583
93.281375	1907.348250	5.467354	-0.018568	2.442261
93.439862	1915.398419	5.472358	-0.018603	2.446933
93.748711	1923.479499	5.477363	-0.018666	2.451624
94.045704	1931.516036	5.482368	-0.018726	2.456281
94.598321	1939.531836	5.487373	-0.018835	2.460935
94.921667	1947.580367	5.492378	-0.018900	2.465582
95.127656	1955.640542	5.497382	-0.018944	2.470219
95.660029	1963.729160	5.502387	-0.019048	2.474887
95.863004	1971.759733	5.507392	-0.019091	2.479489
96.031705	1979.825987	5.512397	-0.019128	2.484099
96.376513	1987.880374	5.517402	-0.019197	2.488708
96.597535	1995.949451	5.522406	-0.019243	2.493307
96.933962	2004.029395	5.527411	-0.019311	2.497912
97.190042	2012.048428	5.532416	-0.019364	2.502469
97.340887	2020.141185	5.537421	-0.019397	2.507051
97.493949	2028.238589	5.542426	-0.019431	2.511627
97.965504	2036.276319	5.547430	-0.019524	2.516185
98.279569	2044.330512	5.552435	-0.019588	2.520732
98.308242	2052.366104	5.557440	-0.019598	2.525240
98.656501	2060.418995	5.562445	-0.019669	2.529772
99.117806	2068.454768	5.567450	-0.019760	2.534295
99.455320	2076.499139	5.572454	-0.019828	2.538805
99.699645	2084.564575	5.577459	-0.019878	2.543313
99.826430	2092.633851	5.582464	-0.019907	2.547806
100.028413	2100.727058	5.587469	-0.019950	2.552310
100.357969	2108.766038	5.592474	-0.020017	2.556785
100.504976	2116.802580	5.597478	-0.020049	2.561238
101.113974	2124.836693	5.602483	-0.020168	2.565714
101.280072	2132.888664	5.607488	-0.020204	2.570161
101.674922	2140.953416	5.612493	-0.020283	2.574623
101.862266	2149.014981	5.617498	-0.020323	2.579062
102.668430	2156.985995	5.622502	-0.020478	2.583485
102.978150	2165.087718	5.627507	-0.020541	2.587939
103.119013	2173.274240	5.632512	-0.020573	2.592419
103.343831	2181.373961	5.637517	-0.020620	2.596850
103.537235	2189.377045	5.642522	-0.020661	2.601219
103.671096	2197.393369	5.647526	-0.020691	2.605584
104.034604	2205.421421	5.652531	-0.020764	2.609963
104.191137	2213.472174	5.657536	-0.020798	2.614333
104.605309	2221.482564	5.662541	-0.020881	2.618691
104.937662	2229.513798	5.667546	-0.020948	2.623047
105.178132	2237.556039	5.672550	-0.020998	2.627397
105.485667	2245.636294	5.677555	-0.021060	2.631763
105.658431	2253.703724	5.682560	-0.021098	2.636107
105.876773	2261.739328	5.687565	-0.021143	2.640429
106.132684	2269.765523	5.692570	-0.021196	2.644742
106.398190	2277.804970	5.697574	-0.021251	2.649055
106.922286	2285.866998	5.702579	-0.021354	2.653391
107.248412	2293.895764	5.707584	-0.021420	2.657688
107.505821	2301.954347	5.712589	-0.021473	2.661990
107.513777	2310.033002	5.717594	-0.021480	2.666279
107.663498	2318.080304	5.722598	-0.021513	2.670554
107.935247	2326.175360	5.727603	-0.021569	2.674855
108.399038	2334.140844	5.732608	-0.021660	2.679093
108.804780	2342.171864	5.737613	-0.021741	2.683356
109.007396	2350.245217	5.742618	-0.021784	2.687620
108.813396	2358.339013	5.747622	-0.021753	2.691864
109.492110	2366.361075	5.752627	-0.021885	2.696118
109.771600	2374.373931	5.757632	-0.021942	2.700336
109.760002	2382.436858	5.762637	-0.021945	2.704554
110.212647	2390.480588	5.767642	-0.022034	2.708786
110.321343	2398.561002	5.772646	-0.022060	2.713008
110.417086	2406.633429	5.777651	-0.022083	2.717218
110.549708	2414.652159	5.782656	-0.022113	2.721397
110.938874	2422.667754	5.787661	-0.022190	2.725583
111.189150	2430.735938	5.792666	-0.022242	2.729782
111.407961	2438.770338	5.797670	-0.022288	2.733954
111.869541	2446.811921	5.802675	-0.022379	2.738139
112.276231	2454.813249	5.807680	-0.022460	2.742293
112.742797	2462.856250	5.812685	-0.022552	2.746466
112.846097	2470.962534	5.817690	-0.022577	2.750643
112.957959	2479.079589	5.822694	-0.022603	2.754820
113.321788	2487.083151	5.827699	-0.022676	2.758947
113.624549	2495.081073	5.832704	-0.022737	2.763061
113.814707	2503.109798	5.837709	-0.022778	2.767179
114.119617	2511.167143	5.842714	-0.022840	2.771311
114.066365	2519.252205	5.847718	-0.022835	2.775430
114.351958	2527.267378	5.852723	-0.022894	2.779528
114.525491	2535.296538	5.857728	-0.022931	2.783620
114.818619	2543.344636	5.862733	-0.022991	2.787723
115.077024	2551.418041	5.867738	-0.023044	2.791830
115.342998	2559.443348	5.872742	-0.023099	2.795907
115.739346	2567.469152	5.877747	-0.023178	2.799986
115.932585	2575.489489	5.882752	-0.023219	2.804045
116.052807	2583.544241	5.887757	-0.023247	2.808111
116.382088	2591.599714	5.892762	-0.023313	2.812183
116.480478	2599.660634	5.897766	-0.023337	2.816239
116.813401	2607.693875	5.902771	-0.023404	2.820289
117.119551	2615.700139	5.907776	-0.023466	2.824317
117.423831	2623.776929	5.912781	-0.023528	2.828375
117.721204	2631.846896	5.917786	-0.023589	2.832423
118.010594	2639.885024	5.922790	-0.023648	2.836450
118.554088	2647.910226	5.927795	-0.023754	2.840478
118.451920	2655.951355	5.932800	-0.023741	2.844472
118.630134	2664.005290	5.937805	-0.023779	2.848482
118.954947	2672.050312	5.942810	-0.023845	2.852491
119.467120	2680.060441	5.947814	-0.023945	2.856487
119.975989	2688.079291	5.952819	-0.024045	2.860482
120.335450	2696.075221	5.957824	-0.024117	2.864451
120.499939	2704.173400	5.962829	-0.024153	2.868455
120.876582	2712.207810	5.967834	-0.024229	2.872433
121.003072	2720.253004	5.972838	-0.024257	2.876397
121.473445	2728.282376	5.977843	-0.024350	2.880366
121.473736	2736.305487	5.982848	-0.024355	2.884301
121.841009	2744.356081	5.987853	-0.024429	2.888265
121.958996	2752.443110	5.992858	-0.024456	2.892227
122.280722	2760.460481	5.997862	-0.024521	2.896161
122.508952	2768.517228	6.002867	-0.024569	2.900103
122.699432	2776.536015	6.007872	-0.024610	2.904020
122.920534	2784.582264	6.012877	-0.024656	2.907946
123.180984	2792.681478	6.017882	-0.024710	2.911895
123.330949	2800.771151	6.022886	-0.024743	2.915827
123.751146	2808.727376	6.027891	-0.024826	2.919705
123.920039	2816.749728	6.032896	-0.024863	2.923595
123.894718	2824.800242	6.037901	-0.024864	2.927484
124.226500	2832.826322	6.042906	-0.024930	2.931375
124.283288	2840.867960	6.047910	-0.024946	2.935253
124.501698	2848.912413	6.052915	-0.024992	2.939136
124.860809	2856.903591	6.057920	-0.025064	2.942996
124.965124	2864.966941	6.062925	-0.025089	2.946872
125.317072	2873.017413	6.067930	-0.025160	2.950750
125.543033	2881.052483	6.072934	-0.025207	2.954608
125.821063	2889.080150	6.077939	-0.025264	2.958461
125.904881	2897.105333	6.082944	-0.025285	2.962297
126.131946	2905.132121	6.087949	-0.025332	2.966136
126.384499	2913.174573	6.092954	-0.025384	2.969980
126.443110	2921.245731	6.097958	-0.025401	2.973821
126.739144	2929.271727	6.102963	-0.025461	2.977649
126.980587	2937.269920	6.107968	-0.025511	2.981456
127.313011	2945.295809	6.112973	-0.025578	2.985275
127.464198	2953.384442	6.117978	-0.025612	2.989110
127.555341	2961.435057	6.122982	-0.025634	2.992919
128.038830	2969.466991	6.127987	-0.025729	2.996734
128.183320	2977.485625	6.132992	-0.025761	3.000521
128.262002	2985.492221	6.137997	-0.025781	3.004295
128.535170	2993.554216	6.143002	-0.025837	3.008099
128.549709	3001.601212	6.148006	-0.025845	3.011878
128.859991	3009.661921	6.153011	-0.025908	3.015674
129.026377	3017.663333	6.158016	-0.025944	3.019430
129.354483	3025.680592	6.163021	-0.026010	3.023197
129.637260	3033.729475	6.168026	-0.026068	3.026971
129.856784	3041.750966	6.173030	-0.026114	3.030725
130.447349	3049.796889	6.178035	-0.026229	3.034504
130.570588	3057.846632	6.183040	-0.026258	3.038257
130.812294	3065.863216	6.188045	-0.026308	3.041995
131.122714	3073.892107	6.193050	-0.026371	3.045738
131.142759	3081.934069	6.198054	-0.026380	3.049469
131.421997	3090.005730	6.203059	-0.026437	3.053221
131.497846	3098.024652	6.208064	-0.026456	3.056934
132.010592	3106.024757	6.213069	-0.026557	3.060655
132.147008	3114.074772	6.218074	-0.026588	3.064376
132.221735	3122.111137	6.223078	-0.026607	3.068084
132.348440	3130.225929	6.228083	-0.026636	3.071826
132.408393	3138.314004	6.233088	-0.026652	3.075548
132.640183	3146.255682	6.238093	-0.026700	3.079206
132.960257	3154.258583	6.243098	-0.026765	3.082891
133.256403	3162.267517	6.248102	-0.026825	3.086574
133.683707	3170.300226	6.253107	-0.026910	3.090270
133.547389	3178.379129	6.258112	-0.026890	3.093956
133.735242	3186.385011	6.263117	-0.026930	3.097620
134.032758	3194.436726	6.268122	-0.026991	3.101304
134.007970	3202.450934	6.273126	-0.026991	3.104953
134.559595	3210.473176	6.278131	-0.027099	3.108627
134.604566	3218.537938	6.283136	-0.027113	3.112294
134.517633	3226.616443	6.288141	-0.027102	3.115956
134.725638	3234.609592	6.293146	-0.027146	3.119588
135.041783	3242.582109	6.298150	-0.027210	3.123212
135.263939	3250.652809	6.303155	-0.027257	3.126871
135.348968	3258.683715	6.308160	-0.027278	3.130503
135.539510	3266.733656	6.313165	-0.027318	3.134143
135.940339	3274.759166	6.318170	-0.027398	3.137777
135.874302	3282.788055	6.323174	-0.027391	3.141388
136.119844	3290.824060	6.328179	-0.027442	3.145012
136.414876	3298.844442	6.333184	-0.027502	3.148626
136.455776	3306.912274	6.338189	-0.027515	3.152247
136.733285	3314.969112	6.343194	-0.027572	3.155869
137.021034	3322.929650	6.348198	-0.027631	3.159444
137.345797	3330.947471	6.353203	-0.027696	3.163042
137.478571	3338.975020	6.358208	-0.027726	3.166632
137.691327	3347.018020	6.363213	-0.027771	3.170228
137.762337	3355.094476	6.368218	-0.027789	3.173829
137.924925	3363.114456	6.373222	-0.027825	3.177405
138.323863	3371.145417	6.378227	-0.027904	3.180991
138.230118	3379.152741	6.383232	-0.027892	3.184542
138.427236	3387.198852	6.388237	-0.027934	3.188119
138.717976	3395.247972	6.393242	-0.027993	3.191697
139.133626	3403.256939	6.398246	-0.028076	3.195258
139.294045	3411.312790	6.403251	-0.028111	3.198825
139.378978	3419.311306	6.408256	-0.028132	3.202360
139.505442	3427.360104	6.413261	-0.028161	3.205915
139.963001	3435.386568	6.418266	-0.028251	3.209469
139.863033	3443.442877	6.423270	-0.028238	3.213010
140.120838	3451.504157	6.428275	-0.028291	3.216564
140.474119	3459.469453	6.433280	-0.028362	3.220075
140.518890	3467.490391	6.438285	-0.028376	3.223595
140.654025	3475.554443	6.443290	-0.028406	3.227133
140.934740	3483.589538	6.448294	-0.028464	3.230661
141.215830	3491.686410	6.453299	-0.028521	3.234211
141.309317	3499.681013	6.458304	-0.028544	3.237706
141.531451	3507.683098	6.463309	-0.028590	3.241205
141.710477	3515.710847	6.468314	-0.028629	3.244710
141.822132	3523.705513	6.473318	-0.028655	3.248193
142.056317	3531.775114	6.478323	-0.028704	3.251711
142.352327	3539.811914	6.483328	-0.028764	3.255213
142.368401	3547.805484	6.488333	-0.028772	3.258681
142.561824	3555.851868	6.493338	-0.028813	3.262176
142.955764	3563.851102	6.498342	-0.028892	3.265654
143.257814	3571.894909	6.503347	-0.028953	3.269144
143.488610	3579.948174	6.508352	-0.029002	3.272631
143.799973	3587.962281	6.513357	-0.029065	3.276102
144.023708	3595.978501	6.518362	-0.029112	3.279565
144.073564	3603.998744	6.523366	-0.029126	3.283021
144.360568	3612.037266	6.528371	-0.029185	3.286489
144.475382	3620.061421	6.533376	-0.029211	3.289941
144.619832	3628.117599	6.538381	-0.029243	3.293404
144.656869	3636.143893	6.543386	-0.029255	3.296847
144.742066	3644.164077	6.548390	-0.029277	3.300285
145.071875	3652.200009	6.553395	-0.029343	3.303736
145.413909	3660.193722	6.558400	-0.029412	3.307166
145.705019	3668.223116	6.563405	-0.029471	3.310605
146.062640	3676.318086	6.568410	-0.029543	3.314071
146.247065	3684.308022	6.573414	-0.029583	3.317482
146.406016	3692.345224	6.578419	-0.029618	3.320909
146.803586	3700.306579	6.583424	-0.029697	3.324308
146.940472	3708.345560	6.588429	-0.029727	3.327728
146.990093	3716.436620	6.593434	-0.029742	3.331163
147.268185	3724.443082	6.598438	-0.029799	3.334567
147.615375	3732.475430	6.603443	-0.029869	3.337981
147.602955	3740.511364	6.608448	-0.029872	3.341379
147.516689	3748.515338	6.613453	-0.029861	3.344758
147.837116	3756.555684	6.618458	-0.029926	3.348164
148.048386	3764.615319	6.623462	-0.029970	3.351570
148.081814	3772.673429	6.628467	-0.029982	3.354966
148.365457	3780.650596	6.633472	-0.030040	3.358334
148.481898	3788.685223	6.638477	-0.030067	3.361716
148.357933	3796.737495	6.643482	-0.030049	3.365093
148.759487	3804.713316	6.648486	-0.030129	3.368454
148.917838	3812.787398	6.653491	-0.030163	3.371844
149.247789	3820.805070	6.658496	-0.030230	3.375213
149.445959	3828.801062	6.663501	-0.030272	3.378564
149.783684	3836.843326	6.668506	-0.030340	3.381937
149.869859	3844.850000	6.673510	-0.030361	3.385283
149.902794	3852.947783	6.678515	-0.030373	3.388661
149.980741	3860.999643	6.683520	-0.030393	3.392018
150.337226	3869.030088	6.688525	-0.030464	3.395373
150.683250	3877.013939	6.693530	-0.030534	3.398705
150.952332	3884.989679	6.698534	-0.030589	3.402028
151.302158	3892.998969	6.703539	-0.030659	3.405363
151.165793	3901.057563	6.708544	-0.030639	3.408700
151.175674	3909.095242	6.713549	-0.030646	3.412029
151.512366	3917.121973	6.718554	-0.030714	3.415362
151.778227	3925.123278	6.723558	-0.030769	3.418678
151.901414	3933.157881	6.728563	-0.030797	3.422000
152.048606	3941.156738	6.733568	-0.030830	3.425305
152.234352	3949.195846	6.738573	-0.030869	3.428625
152.509285	3957.251457	6.743578	-0.030926	3.431951
152.458319	3965.304470	6.748582	-0.030922	3.435262
152.694579	3973.301513	6.753587	-0.030971	3.438556
153.011862	3981.311919	6.758592	-0.031035	3.441856
153.041024	3989.327674	6.763597	-0.031046	3.445144
153.309847	3997.365993	6.768602	-0.031101	3.448447
153.344067	4005.411275	6.773606	-0.031112	3.451742
153.690927	4013.448224	6.778611	-0.031182	3.455040
153.837969	4021.482337	6.783616	-0.031215	3.458328
153.918974	4029.510340	6.788621	-0.031235	3.461607
154.278662	4037.527523	6.793626	-0.031307	3.464888
154.284999	4045.548496	6.798630	-0.031314	3.468157
154.629028	4053.612303	6.803635	-0.031383	3.471450
154.726369	4061.665900	6.808640	-0.031406	3.474728
154.583882	4069.684657	6.813645	-0.031385	3.477981
154.905581	4077.683394	6.818650	-0.031450	3.481238
155.109441	4085.622045	6.823654	-0.031493	3.484464
155.298381	4093.688059	6.828659	-0.031534	3.487737
155.363804	4101.706617	6.833664	-0.031551	3.490985
155.510479	4109.740993	6.838669	-0.031583	3.494238
155.821127	4117.760847	6.843674	-0.031647	3.497488
155.916945	4125.763258	6.848678	-0.031670	3.500721
156.175204	4133.784505	6.853683	-0.031723	3.503963
156.372821	4141.826539	6.858688	-0.031765	3.507209
156.536056	4149.856274	6.863693	-0.031800	3.510446
156.606951	4157.984515	6.868698	-0.031819	3.513717
156.696476	4165.947111	6.873702	-0.031841	3.516919
156.873584	4173.924297	6.878707	-0.031879	3.520126
157.030548	4181.968027	6.883712	-0.031913	3.523356
157.263206	4189.972119	6.888717	-0.031962	3.526570
157.391750	4198.036815	6.893722	-0.031991	3.529802
157.332597	4206.067770	6.898726	-0.031985	3.533012
157.904610	4214.114476	6.903731	-0.032097	3.536244
158.295452	4222.074520	6.908736	-0.032175	3.539433
158.321816	4230.110912	6.913741	-0.032185	3.542639
158.326175	4238.188396	6.918746	-0.032191	3.545857
158.654708	4246.184580	6.923750	-0.032257	3.549050
158.874552	4254.279498	6.928755	-0.032304	3.552276
159.100132	4262.352370	6.933760	-0.032351	3.555490
159.489933	4270.265445	6.938765	-0.032429	3.558643
159.567321	4278.334901	6.943770	-0.032448	3.561846
159.548230	4286.300574	6.948774	-0.032450	3.565002
159.873996	4294.331469	6.953779	-0.032516	3.568191
159.977482	4302.388439	6.958784	-0.032540	3.571381
160.113439	4310.382315	6.963789	-0.032571	3.574544
160.350332	4318.426574	6.968794	-0.032620	3.577728
160.670563	4326.418188	6.973798	-0.032685	3.580890
160.809501	4334.439733	6.978803	-0.032716	3.584055
160.901159	4342.459184	6.983808	-0.032738	3.587216
161.203472	4350.457793	6.988813	-0.032800	3.590372
161.506688	4358.542971	6.993818	-0.032861	3.593559
161.295487	4366.586657	6.998822	-0.032827	3.596712
161.664085	4374.527987	7.003827	-0.032901	3.599839
161.831499	4382.546578	7.008832	-0.032937	3.602987
161.919677	4390.594675	7.013837	-0.032959	3.606142
162.193508	4398.631844	7.018842	-0.033015	3.609295
162.235910	4406.655883	7.023846	-0.033028	3.612434
162.450181	4414.711516	7.028851	-0.033073	3.615588
162.497618	4422.734072	7.033856	-0.033087	3.618720
162.785048	4430.714653	7.038861	-0.033146	3.621841
162.940648	4438.758813	7.043866	-0.033180	3.624980
162.968287	4446.771663	7.048870	-0.033191	3.628100
162.982891	4454.841321	7.053875	-0.033199	3.631240
163.415913	4462.883174	7.058880	-0.033284	3.634377
163.574965	4470.880449	7.063885	-0.033319	3.637487
163.775936	4478.892204	7.068890	-0.033362	3.640601
163.745605	4486.888236	7.073894	-0.033361	3.643700
164.025863	4494.956743	7.078899	-0.033419	3.646832
164.027513	4502.947362	7.083904	-0.033424	3.649925
164.232117	4510.991433	7.088909	-0.033468	3.653040
164.369862	4519.058361	7.093914	-0.033498	3.656160
164.453280	4527.021861	7.098918	-0.033519	3.659237
164.767349	4535.082515	7.103923	-0.033583	3.662354
165.004357	4543.063817	7.108928	-0.033632	3.665435
165.352763	4551.085791	7.113933	-0.033702	3.668533
165.411390	4559.186201	7.118938	-0.033718	3.671651
165.580107	4567.169115	7.123942	-0.033755	3.674723
166.005100	4575.166020	7.128947	-0.033839	3.677805
166.096680	4583.200245	7.133952	-0.033862	3.680891
166.278736	4591.178204	7.138957	-0.033901	3.683954
166.607487	4599.246912	7.143962	-0.033967	3.687053
166.350652	4607.270765	7.148966	-0.033925	3.690118
166.466491	4615.316591	7.153971	-0.033951	3.693197
166.772244	4623.323993	7.158976	-0.034013	3.696265
166.974340	4631.295090	7.163981	-0.034056	3.699313
167.079963	4639.374148	7.168986	-0.034081	3.702398
167.252518	4647.326978	7.173990	-0.034118	3.705433
167.478125	4655.369893	7.178995	-0.034166	3.708502
167.645850	4663.445493	7.184000	-0.034202	3.711579
167.796163	4671.533110	7.189005	-0.034235	3.714657
167.909806	4679.536147	7.194010	-0.034262	3.717700
168.064292	4687.483105	7.199014	-0.034296	3.720721
168.158121	4695.458600	7.204019	-0.034318	3.723748
168.524596	4703.501510	7.209024	-0.034392	3.726805
168.535429	4711.507032	7.214029	-0.034399	3.729836
168.475730	4719.588776	7.219034	-0.034393	3.732892
168.534297	4727.631630	7.224038	-0.034409	3.735934
168.900424	4735.612873	7.229043	-0.034482	3.738957
168.898742	4743.649542	7.234048	-0.034487	3.741990
169.205683	4751.609604	7.239053	-0.034550	3.744999
169.682795	4759.663380	7.244058	-0.034644	3.748045
169.552310	4767.703729	7.249062	-0.034625	3.751069
169.512484	4775.758997	7.254067	-0.034622	3.754098
169.834748	4783.790851	7.259072	-0.034688	3.757125
170.157539	4791.736158	7.264077	-0.034753	3.760116
170.550211	4799.801822	7.269082	-0.034831	3.763152
170.507026	4807.825126	7.274086	-0.034828	3.766160
170.851498	4815.829450	7.279091	-0.034898	3.769166
170.955606	4823.910879	7.284096	-0.034922	3.772194
170.819174	4831.924967	7.289101	-0.034902	3.775189
171.262950	4839.936953	7.294106	-0.034990	3.778193
171.372029	4847.979076	7.299110	-0.035016	3.781199
171.225999	4855.966010	7.304115	-0.034994	3.784176
171.532682	4864.010748	7.309120	-0.035056	3.787183
171.915365	4872.003825	7.314125	-0.035132	3.790169
171.949302	4880.107227	7.319130	-0.035144	3.793187
171.854472	4888.103009	7.324134	-0.035131	3.796159
172.253728	4896.035426	7.329139	-0.035211	3.799116
172.575507	4904.097351	7.334144	-0.035276	3.802117
172.479361	4912.083497	7.339149	-0.035263	3.805079
172.966930	4920.124986	7.344154	-0.035359	3.808071
173.068891	4928.119691	7.349158	-0.035383	3.811036
173.090372	4936.192850	7.354163	-0.035393	3.814025
173.223974	4944.189865	7.359168	-0.035423	3.816986
173.490139	4952.198158	7.364173	-0.035478	3.819952
173.730881	4960.209190	7.369178	-0.035528	3.822916
173.736256	4968.235847	7.374182	-0.035534	3.825879
173.807038	4976.280233	7.379187	-0.035552	3.828847
174.141280	4984.337049	7.384192	-0.035620	3.831822
174.172214	4992.295390	7.389197	-0.035631	3.834753
174.438299	5000.360258	7.394202	-0.035685	3.837726
174.604175	5008.335218	7.399206	-0.035721	3.840661
174.672105	5016.341427	7.404211	-0.035739	3.843604
174.841153	5024.383019	7.409216	-0.035776	3.846559
175.309219	5032.341776	7.414221	-0.035868	3.849488
175.483924	5040.455237	7.419226	-0.035906	3.852465
175.321019	5048.461615	7.424230	-0.035881	3.855394
175.702218	5056.515603	7.429235	-0.035957	3.858349
175.857453	5064.540565	7.434240	-0.035991	3.861286
175.922462	5072.490335	7.439245	-0.036008	3.864192
176.363166	5080.571836	7.444250	-0.036096	3.867152
176.611797	5088.582024	7.449254	-0.036147	3.870079
176.762326	5096.799067	7.454259	-0.036181	3.873077
176.697802	5104.863568	7.459264	-0.036174	3.876013
176.960862	5112.748305	7.464269	-0.036228	3.878889
177.104251	5120.740761	7.469274	-0.036260	3.881798
177.440790	5128.687685	7.474278	-0.036328	3.884693
177.382284	5136.746917	7.479283	-0.036322	3.887619
177.651078	5144.722498	7.484288	-0.036377	3.890518
177.670974	5152.773326	7.489293	-0.036386	3.893438
178.039743	5160.830755	7.494298	-0.036460	3.896364
177.863103	5168.745404	7.499302	-0.036432	3.899227
177.904321	5176.823575	7.504307	-0.036445	3.902150
178.118001	5184.841807	7.509312	-0.036490	3.905053
178.303867	5192.824324	7.514317	-0.036530	3.907940
178.633182	5200.859036	7.519322	-0.036596	3.910847
178.518184	5208.928012	7.524326	-0.036580	3.913755
178.634783	5216.984969	7.529331	-0.036607	3.916661
179.047169	5224.912280	7.534336	-0.036689	3.919524
179.062794	5232.914419	7.539341	-0.036697	3.922405
179.310770	5240.947110	7.544346	-0.036749	3.925298
179.576920	5248.971015	7.549350	-0.036803	3.928187
179.741495	5256.980852	7.554355	-0.036839	3.931066
179.768404	5265.048818	7.559360	-0.036849	3.933962
179.822743	5273.056921	7.564365	-0.036865	3.936834
180.289238	5281.067775	7.569370	-0.036957	3.939713
180.356827	5289.077476	7.574374	-0.036975	3.942582
180.343124	5297.079614	7.579379	-0.036977	3.945445
180.630932	5305.109388	7.584384	-0.037036	3.948321
180.736355	5313.133122	7.589389	-0.037061	3.951189
180.846579	5321.244737	7.594394	-0.037087	3.954087
180.978307	5329.219486	7.599398	-0.037116	3.956935
181.057700	5337.191192	7.604403	-0.037136	3.959778
181.161587	5345.197293	7.609408	-0.037161	3.962632
181.353817	5353.168992	7.614413	-0.037202	3.965473
181.766494	5361.222848	7.619418	-0.037284	3.968345
181.856814	5369.269118	7.624422	-0.037306	3.971206
181.988128	5377.324564	7.629427	-0.037335	3.974070
182.049449	5385.354881	7.634432	-0.037352	3.976921
181.882269	5393.310197	7.639437	-0.037326	3.979740
182.204905	5401.367039	7.644442	-0.037391	3.982601
182.334478	5409.358605	7.649446	-0.037421	3.985433
182.771272	5417.385729	7.654451	-0.037507	3.988282
182.682475	5425.435216	7.659456	-0.037496	3.991127
183.059554	5433.423829	7.664461	-0.037571	3.993957
183.362856	5441.518059	7.669466	-0.037633	3.996820
183.279810	5449.473976	7.674470	-0.037623	3.999626
183.440161	5457.515567	7.679475	-0.037658	4.002465
183.653975	5465.533042	7.684480	-0.037703	4.005294
183.775701	5473.543595	7.689485	-0.037731	4.008117
183.833887	5481.593776	7.694490	-0.037747	4.010951
184.090351	5489.623033	7.699494	-0.037800	4.013778
184.066573	5497.674129	7.704499	-0.037801	4.016607
184.229553	5505.653229	7.709504	-0.037836	4.019411
184.421567	5513.645592	7.714509	-0.037877	4.022219
184.776316	5521.632896	7.719514	-0.037948	4.025025
184.867199	5529.701672	7.724518	-0.037970	4.027854
185.067388	5537.719665	7.729523	-0.038013	4.030665
185.274946	5545.851912	7.734528	-0.038057	4.033514
185.149322	5553.854373	7.739533	-0.038039	4.036310
185.235541	5561.814781	7.744538	-0.038060	4.039093
185.454894	5569.821520	7.749542	-0.038106	4.041892
185.587396	5577.766017	7.754547	-0.038136	4.044667
185.864161	5585.814687	7.759552	-0.038192	4.047477
185.957153	5593.819489	7.764557	-0.038215	4.050268
186.335806	5601.901239	7.769562	-0.038291	4.053088
186.326400	5609.895552	7.774566	-0.038294	4.055870
186.410955	5617.889641	7.779571	-0.038315	4.058651
186.560775	5625.945861	7.784576	-0.038348	4.061452
186.588241	5633.892258	7.789581	-0.038358	4.064212
186.713899	5641.976831	7.794586	-0.038387	4.067020
186.878175	5649.937584	7.799590	-0.038423	4.069782
187.204073	5658.008988	7.804595	-0.038489	4.072584
187.356417	5666.025493	7.809600	-0.038522	4.075362
187.521605	5674.032581	7.814605	-0.038558	4.078136
187.520062	5682.051892	7.819610	-0.038563	4.080909
187.599282	5689.998431	7.824614	-0.038583	4.083656
187.716884	5698.068202	7.829619	-0.038610	4.086445
187.949564	5706.081072	7.834624	-0.038659	4.089214
188.049854	5714.089296	7.839629	-0.038683	4.091977
188.065633	5722.178787	7.844634	-0.038691	4.094765
188.206714	5730.141972	7.849638	-0.038722	4.097510
188.406366	5738.182693	7.854643	-0.038765	4.100280
188.477091	5746.202141	7.859648	-0.038783	4.103039
188.536921	5754.198365	7.864653	-0.038799	4.105788
188.914607	5762.234205	7.869658	-0.038875	4.108553
189.251505	5770.258066	7.874662	-0.038943	4.111312
189.143022	5778.340729	7.879667	-0.038928	4.114083
189.337433	5786.385519	7.884672	-0.038969	4.116843
189.457356	5794.289979	7.889677	-0.038997	4.119553
189.684482	5802.328900	7.894682	-0.039044	4.122307
189.574577	5810.312755	7.899686	-0.039029	4.125037
190.046892	5818.367186	7.904691	-0.039122	4.127797
190.219267	5826.397984	7.909696	-0.039159	4.130543
190.259279	5834.416163	7.914701	-0.039172	4.133281
190.391878	5842.508637	7.919706	-0.039202	4.136043
190.580704	5850.442429	7.924710	-0.039242	4.138751
190.619721	5858.483117	7.929715	-0.039255	4.141491
190.831878	5866.472529	7.934720	-0.039299	4.144214
190.928930	5874.526443	7.939725	-0.039323	4.146956
191.254203	5882.544617	7.944730	-0.039388	4.149686
191.360152	5890.597969	7.949734	-0.039413	4.152424
191.573918	5898.614299	7.954739	-0.039458	4.155149
191.715256	5906.620097	7.959744	-0.039490	4.157868
191.584132	5914.618505	7.964749	-0.039471	4.160579
191.860565	5922.642187	7.969754	-0.039527	4.163301
191.984159	5930.616527	7.974758	-0.039555	4.166004
191.998619	5938.659778	7.979763	-0.039563	4.168727
192.149126	5946.733254	7.984768	-0.039597	4.171459
192.554693	5954.700065	7.989773	-0.039677	4.174157
192.723882	5962.772533	7.994778	-0.039714	4.176886
192.813245	5970.710545	7.999782	-0.039736	4.179567
192.959778	5978.759188	8.004787	-0.039768	4.182284
193.114547	5986.763772	8.009792	-0.039802	4.184984
193.212752	5994.772658	8.014797	-0.039826	4.187684
193.457904	6002.826521	8.019802	-0.039877	4.190399
193.443952	6010.925608	8.024806	-0.039879	4.193124
193.509970	6018.957756	8.029811	-0.039897	4.195826
193.753991	6026.870508	8.034816	-0.039947	4.198487
193.963095	6034.852723	8.039821	-0.039992	4.201170
194.149636	6042.866895	8.044826	-0.040031	4.203862
194.112758	6050.933297	8.049830	-0.040030	4.206567
194.143786	6058.902157	8.054835	-0.040041	4.209239
194.444169	6066.976873	8.059840	-0.040102	4.211947
194.392494	6074.922170	8.064845	-0.040097	4.214606
194.501457	6083.001068	8.069850	-0.040123	4.217310
194.791075	6090.974190	8.074854	-0.040182	4.219979
195.105516	6098.988191	8.079859	-0.040246	4.222660
195.188980	6106.975969	8.084864	-0.040267	4.225328
195.327949	6115.011177	8.089869	-0.040298	4.228011
195.596448	6123.044926	8.094874	-0.040353	4.230692
195.430356	6131.127533	8.099878	-0.040327	4.233384
195.589387	6139.093254	8.104883	-0.040362	4.236039
195.879873	6147.139997	8.109888	-0.040421	4.238720
195.925593	6155.099465	8.114893	-0.040435	4.241368
196.279912	6163.093658	8.119898	-0.040506	4.244029
196.272234	6171.137103	8.124902	-0.040510	4.246701
196.209470	6179.147661	8.129907	-0.040503	4.249360
196.397585	6187.217395	8.134912	-0.040544	4.252040
196.434370	6195.210792	8.139917	-0.040556	4.254691
196.605428	6203.277125	8.144922	-0.040593	4.257365
196.638527	6211.245818	8.149926	-0.040604	4.260005
196.879726	6219.294976	8.154931	-0.040654	4.262671
197.214323	6227.313717	8.159936	-0.040722	4.265326
197.175425	6235.309794	8.164941	-0.040720	4.267969
197.368945	6243.347191	8.169946	-0.040761	4.270626
197.581929	6251.426058	8.174950	-0.040806	4.273295
197.763564	6259.449365	8.179955	-0.040845	4.275943
197.957535	6267.429103	8.184960	-0.040886	4.278576
197.789269	6275.440235	8.189965	-0.040860	4.281215
198.162405	6283.402572	8.194970	-0.040935	4.283840
198.276518	6291.484702	8.199974	-0.040961	4.286501
198.325017	6299.447277	8.204979	-0.040975	4.289120
198.573614	6307.553208	8.209984	-0.041027	4.291787
198.638611	6315.529091	8.214989	-0.041044	4.294407
198.733753	6323.578580	8.219994	-0.041067	4.297051
198.687485	6331.531821	8.224998	-0.041064	4.299660
198.862439	6339.589290	8.230003	-0.041101	4.302303
198.920449	6347.585033	8.235008	-0.041117	4.304924
199.179935	6355.578017	8.240013	-0.041171	4.307543
199.250023	6363.618622	8.245018	-0.041189	4.310175
199.497320	6371.658116	8.250022	-0.041240	4.312807
199.650531	6379.662778	8.255027	-0.041274	4.315425
199.852395	6387.711398	8.260032	-0.041317	4.318056
199.792765	6395.668643	8.265037	-0.041311	4.320653
199.999618	6403.695447	8.270042	-0.041355	4.323274
200.223435	6411.706720	8.275046	-0.041402	4.325888
200.439816	6419.713519	8.280051	-0.041447	4.328499
200.356356	6427.753919	8.285056	-0.041437	4.331117
200.361181	6435.761728	8.290061	-0.041443	4.333723
200.682445	6443.813586	8.295066	-0.041508	4.336345
200.822999	6451.800370	8.300070	-0.041539	4.338943
200.886053	6459.810956	8.305075	-0.041556	4.341546
200.931394	6467.837336	8.310080	-0.041570	4.344152
201.005076	6475.846797	8.315085	-0.041589	4.346752
201.235392	6483.891549	8.320090	-0.041637	4.349363
201.392681	6491.902266	8.325094	-0.041671	4.351960
201.651507	6499.990010	8.330099	-0.041725	4.354582
201.880708	6508.035103	8.335104	-0.041773	4.357188
201.892125	6515.910882	8.340109	-0.041780	4.359736
202.193379	6523.939123	8.345114	-0.041841	4.362334
202.095424	6531.940458	8.350118	-0.041828	4.364919
202.038288	6539.956352	8.355123	-0.041823	4.367507
202.729333	6547.947171	8.360128	-0.041956	4.370090
202.612881	6556.012531	8.365133	-0.041940	4.372691
202.808329	6564.056457	8.370138	-0.041982	4.375286
202.735097	6572.019121	8.375142	-0.041973	4.377851
202.927016	6580.034902	8.380147	-0.042014	4.380433
203.107177	6588.079001	8.385152	-0.042053	4.383023
203.042221	6596.079913	8.390157	-0.042046	4.385596
203.298564	6604.083672	8.395162	-0.042099	4.388170
203.456189	6612.118283	8.400166	-0.042133	4.390752
203.521851	6620.162213	8.405171	-0.042151	4.393334
203.852650	6628.199533	8.410176	-0.042218	4.395915
203.955818	6636.167679	8.415181	-0.042242	4.398471
203.876826	6644.207886	8.420186	-0.042233	4.401047
204.062157	6652.182083	8.425190	-0.042272	4.403602
204.117928	6660.204097	8.430195	-0.042288	4.406170
204.442173	6668.235246	8.435200	-0.042353	4.408741
204.232590	6676.231926	8.440205	-0.042320	4.411297
204.693257	6684.313432	8.445210	-0.042411	4.413882
204.691410	6692.374839	8.450214	-0.042415	4.416456
204.735097	6700.346319	8.455219	-0.042429	4.419000
204.978939	6708.384957	8.460224	-0.042479	4.421566
205.095011	6716.311763	8.465229	-0.042506	4.424093
205.326129	6724.422775	8.470234	-0.042554	4.426679
205.266875	6732.388915	8.475238	-0.042549	4.429215
205.802025	6740.455012	8.480243	-0.042653	4.431784
206.059456	6748.503469	8.485248	-0.042707	4.434345
205.965803	6756.495814	8.490253	-0.042694	4.436885
206.196451	6764.460675	8.495258	-0.042742	4.439417
206.266641	6772.502216	8.500262	-0.042761	4.441970
206.279253	6780.422241	8.505267	-0.042768	4.444483
206.242654	6788.543376	8.510272	-0.042767	4.447059
206.634129	6796.487225	8.515277	-0.042845	4.449578
206.755127	6804.596975	8.520282	-0.042872	4.452148
206.852839	6812.589444	8.525286	-0.042896	4.454678
206.941193	6820.621167	8.530291	-0.042918	4.457220
207.161854	6828.598604	8.535296	-0.042964	4.459743
207.079916	6836.649548	8.540301	-0.042954	4.462288
207.296116	6844.595707	8.545306	-0.042999	4.464798
207.274258	6852.666953	8.550310	-0.043000	4.467346
207.491010	6860.664818	8.555315	-0.043046	4.469870
207.637272	6868.742379	8.560320	-0.043078	4.472418
207.874810	6876.714585	8.565325	-0.043128	4.474931
208.125908	6884.719980	8.570330	-0.043180	4.477453
208.012215	6892.723019	8.575335	-0.043164	4.479972
208.196419	6900.727368	8.580339	-0.043203	4.482491
208.631329	6908.757527	8.585344	-0.043289	4.485017
208.579585	6916.763575	8.590349	-0.043285	4.487533
208.771870	6924.794527	8.595354	-0.043326	4.490056
208.957447	6932.833131	8.600359	-0.043366	4.492580
209.079127	6940.819214	8.605363	-0.043394	4.495085
209.116910	6948.898250	8.610368	-0.043406	4.497619
209.338906	6956.868545	8.615373	-0.043452	4.500117
209.645105	6964.913400	8.620378	-0.043515	4.502637
209.572248	6972.858492	8.625383	-0.043506	4.505124
209.538875	6980.870501	8.630387	-0.043505	4.507630
209.750557	6988.965794	8.635392	-0.043550	4.510162
209.655645	6997.007299	8.640397	-0.043537	4.512674
209.904533	7005.041483	8.645402	-0.043589	4.515184
210.248393	7013.007459	8.650407	-0.043658	4.517672
210.318766	7020.959046	8.655411	-0.043676	4.520152
210.484781	7029.010474	8.660416	-0.043712	4.522663
210.484241	7036.960432	8.665421	-0.043717	4.525140
210.585661	7045.031348	8.670426	-0.043742	4.527654
210.512255	7053.028746	8.675431	-0.043733	4.530143
210.791011	7061.062288	8.680435	-0.043790	4.532643
210.979682	7069.108000	8.685440	-0.043831	4.535145
211.102512	7077.072227	8.690445	-0.043859	4.537620
211.132898	7085.108793	8.695450	-0.043869	4.540116
211.173020	7093.110508	8.700455	-0.043882	4.542600
211.578703	7101.048092	8.705459	-0.043963	4.545063
211.709753	7109.163895	8.710464	-0.043993	4.547580
211.719621	7117.194206	8.715469	-0.044000	4.550069
211.964301	7125.225699	8.720474	-0.044050	4.552557
211.869138	7133.234117	8.725479	-0.044038	4.555035
211.866556	7141.206053	8.730483	-0.044042	4.557502
212.192945	7149.253524	8.735488	-0.044108	4.559991
212.249524	7157.201618	8.740493	-0.044124	4.562447
212.297691	7165.217755	8.745498	-0.044138	4.564923
212.594118	7173.262570	8.750503	-0.044199	4.567407
212.598216	7181.257330	8.755507	-0.044205	4.569874
212.749162	7189.339943	8.760512	-0.044238	4.572366
213.001123	7197.312193	8.765517	-0.044290	4.574824
213.204684	7205.377192	8.770522	-0.044333	4.577308
213.079644	7213.328970	8.775527	-0.044315	4.579756
213.076932	7221.383062	8.780531	-0.044320	4.582234
213.698808	7229.416526	8.785536	-0.044441	4.584705
213.700375	7237.445922	8.790541	-0.044446	4.587173
213.611008	7245.430043	8.795546	-0.044435	4.589626
213.809333	7253.494102	8.800551	-0.044477	4.592102
213.842557	7261.550693	8.805555	-0.044488	4.594574
214.128671	7269.570498	8.810560	-0.044547	4.597034
214.265688	7277.463515	8.815565	-0.044578	4.599454
214.318021	7285.554522	8.820570	-0.044593	4.601933
214.391159	7293.502020	8.825575	-0.044611	4.604366
214.585290	7301.544467	8.830579	-0.044653	4.606828
215.033143	7309.537017	8.835584	-0.044741	4.609272
214.978050	7317.556708	8.840589	-0.044736	4.611724
215.164972	7325.637818	8.845594	-0.044776	4.614193
215.300675	7333.674258	8.850599	-0.044807	4.616647
215.432838	7341.599420	8.855603	-0.044836	4.619066
215.328629	7349.669993	8.860608	-0.044822	4.621528
215.476158	7357.591326	8.865613	-0.044855	4.623944
215.747258	7365.678862	8.870618	-0.044911	4.626408
215.912791	7373.695883	8.875623	-0.044947	4.628850
215.910495	7381.721133	8.880627	-0.044951	4.631293
216.152748	7389.779677	8.885632	-0.045002	4.633745
216.232177	7397.726306	8.890637	-0.045022	4.636161
216.126084	7405.766205	8.895642	-0.045007	4.638605
216.204902	7413.760278	8.900647	-0.045027	4.641033
216.344173	7421.750471	8.905651	-0.045058	4.643459
216.717550	7429.801000	8.910656	-0.045133	4.645901
216.554547	7437.797983	8.915661	-0.045108	4.648327
216.825579	7445.822891	8.920666	-0.045163	4.650759
217.202876	7453.868906	8.925671	-0.045239	4.653196
217.218663	7461.862512	8.930675	-0.045247	4.655617
217.341517	7469.864764	8.935680	-0.045275	4.658039
217.477849	7477.871281	8.940685	-0.045306	4.660460
217.551668	7485.901424	8.945690	-0.045325	4.662888
217.775347	7493.907420	8.950695	-0.045371	4.665307
217.910155	7501.915242	8.955699	-0.045402	4.667725
217.905046	7509.973246	8.960704	-0.045406	4.670158
217.996259	7518.041054	8.965709	-0.045428	4.672592
218.351652	7526.080146	8.970714	-0.045500	4.675015
218.474486	7534.050949	8.975719	-0.045528	4.677417
218.698878	7542.018115	8.980723	-0.045575	4.679817
218.807036	7550.050062	8.985728	-0.045600	4.682235
218.757960	7557.989893	8.990733	-0.045596	4.684624
218.952549	7566.058677	8.995738	-0.045637	4.687051
218.917003	7574.040024	9.000743	-0.045636	4.689450
219.148492	7582.060297	9.005747	-0.045684	4.691859
219.220767	7590.097333	9.010752	-0.045703	4.694272
219.308841	7598.111588	9.015757	-0.045724	4.696678
219.693545	7606.062179	9.020762	-0.045801	4.699062
219.700370	7614.123790	9.025767	-0.045808	4.701479
219.701318	7622.105110	9.030771	-0.045813	4.703871
219.918597	7630.180659	9.035776	-0.045859	4.706289
220.150793	7638.163549	9.040781	-0.045907	4.708678
220.398354	7646.210196	9.045786	-0.045959	4.711085
220.359507	7654.258861	9.050791	-0.045957	4.713492
220.405996	7662.245440	9.055795	-0.045970	4.715879
220.581816	7670.287310	9.060800	-0.046008	4.718281
220.608656	7678.244272	9.065805	-0.046018	4.720657
220.785853	7686.274546	9.070810	-0.046057	4.723053
221.074555	7694.325644	9.075815	-0.046116	4.725454
220.842538	7702.332352	9.080819	-0.046078	4.727842
221.076097	7710.359815	9.085824	-0.046126	4.730233
221.180577	7718.372420	9.090829	-0.046151	4.732620
221.464498	7726.382418	9.095834	-0.046209	4.735003
221.238494	7734.445186	9.100839	-0.046172	4.737403
221.418151	7742.416190	9.105843	-0.046211	4.739773
221.610240	7750.473333	9.110848	-0.046252	4.742167
221.757497	7758.412237	9.115853	-0.046284	4.744525
222.037030	7766.478527	9.120858	-0.046342	4.746919
222.300271	7774.468864	9.125863	-0.046396	4.749290
222.513270	7782.472233	9.130867	-0.046441	4.751663
222.696981	7790.542569	9.135872	-0.046480	4.754055
222.863662	7798.568382	9.140877	-0.046516	4.756433
222.738078	7806.510606	9.145882	-0.046498	4.758786
222.778328	7814.513495	9.150887	-0.046511	4.761155
223.114772	7822.532322	9.155891	-0.046579	4.763526
223.154825	7830.546456	9.160896	-0.046591	4.765896
223.253473	7838.555806	9.165901	-0.046615	4.768263
223.336549	7846.605984	9.170906	-0.046636	4.770641
223.564149	7854.629249	9.175911	-0.046683	4.773010
223.580107	7862.641201	9.180915	-0.046691	4.775374
223.675773	7870.657110	9.185920	-0.046714	4.777738
223.768837	7878.630399	9.190925	-0.046737	4.780089
224.084396	7886.665722	9.195930	-0.046801	4.782456
223.889724	7894.653728	9.200935	-0.046770	4.784809
224.008210	7902.654139	9.205939	-0.046797	4.787164
224.308162	7910.695025	9.210944	-0.046858	4.789529
224.466197	7918.743315	9.215949	-0.046893	4.791896
224.560296	7926.757559	9.220954	-0.046915	4.794251
224.720379	7934.774618	9.225959	-0.046950	4.796606
224.685388	7942.709881	9.230963	-0.046949	4.798937
224.613359	7950.822916	9.235968	-0.046941	4.801319
224.928259	7958.716953	9.240973	-0.047005	4.803633
225.084560	7966.796729	9.245978	-0.047039	4.806002
225.133229	7974.856521	9.250983	-0.047053	4.808364
225.166690	7982.875294	9.255987	-0.047065	4.810713
225.597422	7990.332681	9.260992	-0.047150	4.812895
225.379791	7994.857969	9.265997	-0.047112	4.814220

225.528086	7997.215864	9.271002	-0.047141	4.814910
225.794307	7998.606086	9.276007	-0.047192	4.815315
225.731469	7999.062821	9.281011	-0.047180	4.815449
225.754503	7999.716217	9.286016	-0.047185	4.815640
226.002263	7999.711660	9.291021	-0.047231	4.815638
225.953751	7999.720482	9.296026	-0.047222	4.815641
226.071935	7999.760794	9.301031	-0.047244	4.815652
226.229394	7999.762256	9.306035	-0.047273	4.815651
226.481911	7999.805795	9.311040	-0.047320	4.815663
226.223237	7999.732274	9.316045	-0.047272	4.815643
226.196579	7999.979406	9.321050	-0.047267	4.815715
226.339544	7999.885665	9.326055	-0.047294	4.815687
226.490967	7999.942519	9.331059	-0.047322	4.815703
226.630403	7999.891405	9.336064	-0.047348	4.815687
226.420441	7999.987265	9.341069	-0.047309	4.815716
226.444846	7999.874544	9.346074	-0.047313	4.815683
226.574148	7999.881956	9.351079	-0.047337	4.815685
226.411489	7999.831319	9.356083	-0.047307	4.815671
226.922491	7999.931305	9.361088	-0.047402	4.815698
226.691263	7999.882766	9.366093	-0.047359	4.815685
226.659469	7999.853441	9.371098	-0.047353	4.815676
226.665332	7999.970913	9.376103	-0.047354	4.815710
226.470035	7999.881335	9.381107	-0.047318	4.815685
226.729128	7999.902573	9.386112	-0.047366	4.815690
226.813240	7999.991426	9.391117	-0.047382	4.815716
226.747775	7999.881527	9.396122	-0.047369	4.815684
226.924833	7999.792602	9.401127	-0.047402	4.815657
226.818181	7999.953083	9.406131	-0.047383	4.815705
226.943194	7999.950823	9.411136	-0.047406	4.815703
226.660901	7999.911066	9.416141	-0.047353	4.815693
226.756480	7999.957419	9.421146	-0.047371	4.815706
226.867710	7999.896247	9.426151	-0.047392	4.815688
226.925988	7999.873706	9.431155	-0.047402	4.815681
226.885212	7999.887987	9.436160	-0.047395	4.815685
226.854627	7999.887493	9.441165	-0.047389	4.815685
226.837585	7999.790111	9.446170	-0.047386	4.815657
226.913071	7999.933246	9.451175	-0.047400	4.815698
226.945546	7999.977518	9.456179	-0.047406	4.815711
226.929944	7999.797991	9.461184	-0.047403	4.815659
226.904241	8000.012063	9.466189	-0.047398	4.815721
227.019560	7999.875192	9.471194	-0.047420	4.815681
227.125558	7999.908908	9.476199	-0.047439	4.815690
226.994792	7999.863051	9.481203	-0.047415	4.815677
226.937519	7999.874933	9.486208	-0.047404	4.815681
227.027530	7999.925465	9.491213	-0.047421	4.815695
227.100059	7999.865804	9.496218	-0.047434	4.815678
227.097265	7999.926582	9.501223	-0.047434	4.815695
227.166437	7999.935163	9.506227	-0.047447	4.815698
227.247484	7999.904451	9.511232	-0.047462	4.815688
227.308705	7999.961990	9.516237	-0.047473	4.815705
227.238730	7999.935251	9.521242	-0.047460	4.815697
227.231041	7999.897777	9.526247	-0.047459	4.815686
227.347199	7999.858026	9.531251	-0.047480	4.815674
227.253539	7999.869322	9.536256	-0.047463	4.815678
227.242442	8000.004664	9.541261	-0.047461	4.815718
227.214936	7999.880434	9.546266	-0.047456	4.815681
227.275183	7999.991314	9.551271	-0.047467	4.815714
227.347641	7999.929518	9.556275	-0.047480	4.815695
227.435667	7999.843428	9.561280	-0.047497	4.815670
227.447880	7999.890575	9.566285	-0.047499	4.815683
227.497064	7999.868955	9.571290	-0.047508	4.815677
227.403618	7999.916536	9.576295	-0.047491	4.815691
227.451309	7999.894892	9.581299	-0.047499	4.815685
227.675042	7999.831261	9.586304	-0.047541	4.815665
227.635382	7999.833822	9.591309	-0.047534	4.815666
227.635455	7999.846626	9.596314	-0.047534	4.815670
227.593399	7999.897169	9.601319	-0.047526	4.815685
227.502543	7999.983208	9.606323	-0.047509	4.815710
227.628206	7999.810221	9.611328	-0.047532	4.815659
227.745028	7999.947622	9.616333	-0.047554	4.815699
227.484921	7999.946636	9.621338	-0.047505	4.815700
227.150662	7999.986075	9.626343	-0.047443	4.815713
227.252070	7999.841510	9.631347	-0.047462	4.815670
227.419994	7999.892229	9.636352	-0.047493	4.815684
227.310568	7999.924613	9.641357	-0.047473	4.815694
227.691740	7999.819763	9.646362	-0.047544	4.815661
227.645467	7999.937467	9.651367	-0.047535	4.815696
227.500918	7999.922333	9.656371	-0.047508	4.815692
227.695625	7999.835826	9.661376	-0.047544	4.815666
227.584321	7999.910865	9.666381	-0.047524	4.815689
227.503684	7999.831666	9.671386	-0.047509	4.815666
227.450844	7999.954599	9.676391	-0.047499	4.815702
227.711784	7999.904372	9.681395	-0.047547	4.815686
227.641705	7999.817873	9.686400	-0.047534	4.815661
227.617924	7999.901790	9.691405	-0.047530	4.815686
227.704843	7999.914925	9.696410	-0.047546	4.815689
227.809979	7999.857922	9.701415	-0.047566	4.815672
227.539419	7999.819419	9.706419	-0.047515	4.815662
227.558298	7999.945641	9.711424	-0.047519	4.815699
227.737583	7999.916509	9.716429	-0.047552	4.815690
227.868868	7999.821511	9.721434	-0.047576	4.815661
227.792446	7999.833085	9.726439	-0.047562	4.815665
227.602101	7999.885510	9.731443	-0.047527	4.815681
227.714296	7999.862769	9.736448	-0.047548	4.815674
227.731318	7999.898256	9.741453	-0.047551	4.815684
227.797339	7999.841691	9.746458	-0.047563	4.815667
227.791687	7999.985660	9.751463	-0.047562	4.815710
227.794794	7999.954761	9.756467	-0.047562	4.815700
227.701302	7999.865750	9.761472	-0.047545	4.815675
227.757755	7999.968033	9.766477	-0.047556	4.815705
227.726129	7999.875749	9.771482	-0.047550	4.815678
227.558089	7999.917862	9.776487	-0.047518	4.815691
227.710488	7999.860553	9.781491	-0.047547	4.815673
227.782262	7999.881981	9.786496	-0.047560	4.815679
227.621696	7999.944489	9.791501	-0.047530	4.815698
227.567720	7999.852914	9.796506	-0.047520	4.815672
227.869734	7999.908992	9.801511	-0.047576	4.815687
227.760648	7999.874154	9.806515	-0.047556	4.815677
227.822365	7999.804715	9.811520	-0.047567	4.815656
227.747333	8000.003057	9.816525	-0.047553	4.815715
227.698955	7999.876356	9.821530	-0.047544	4.815678
227.787984	7999.795618	9.826535	-0.047561	4.815654
227.662728	7999.956870	9.831539	-0.047537	4.815702
227.819004	7999.787575	9.836544	-0.047566	4.815651
227.694811	7999.974455	9.841549	-0.047543	4.815707
227.719130	7999.878803	9.846554	-0.047548	4.815679
227.775316	7999.825282	9.851559	-0.047558	4.815663
227.644345	7999.897871	9.856563	-0.047534	4.815685
227.821928	7999.883652	9.861568	-0.047567	4.815680
227.707261	7999.826314	9.866573	-0.047546	4.815663
227.848060	7999.872329	9.871578	-0.047572	4.815676
227.773044	7999.811361	9.876583	-0.047558	4.815659
227.645865	7999.960844	9.881587	-0.047534	4.815703
227.865515	7999.806441	9.886592	-0.047575	4.815657
227.713912	7999.920316	9.891597	-0.047547	4.815691
227.853221	7999.883072	9.896602	-0.047573	4.815679
227.703328	7999.897732	9.901607	-0.047545	4.815684
227.827618	7999.892259	9.906611	-0.047568	4.815682
227.703226	7999.866779	9.911616	-0.047545	4.815675
227.732530	7999.888590	9.916621	-0.047550	4.815681
227.799569	7999.833109	9.921626	-0.047562	4.815665
227.783771	7999.896880	9.926631	-0.047559	4.815684
227.971057	7999.924435	9.931635	-0.047594	4.815691
228.144646	7999.823715	9.936640	-0.047627	4.815660
227.847602	7999.911773	9.941645	-0.047571	4.815688
227.733781	7999.844845	9.946650	-0.047550	4.815669
227.891888	7999.855923	9.951655	-0.047579	4.815671
227.722209	7999.842520	9.956659	-0.047548	4.815668
227.892502	7999.890076	9.961664	-0.047580	4.815681
227.880067	7999.898411	9.966669	-0.047577	4.815684
227.997673	7999.856549	9.971674	-0.047599	4.815671
227.642756	7999.817756	9.976679	-0.047533	4.815661
227.665265	7999.880008	9.981683	-0.047537	4.815679
227.874429	7999.899378	9.986688	-0.047576	4.815684
227.944698	7999.841815	9.991693	-0.047589	4.815667
227.950968	7999.872860	9.996698	-0.047590	4.815676
228.050555	7999.829641	10.001703	-0.047609	4.815663
228.000719	7999.894998	10.006707	-0.047599	4.815682
228.205426	7999.885485	10.011712	-0.047638	4.815678
227.875707	7999.878042	10.016717	-0.047576	4.815678
228.093804	7999.800448	10.021722	-0.047617	4.815654
228.211382	7999.923990	10.026727	-0.047639	4.815690
227.925971	7999.824421	10.031731	-0.047585	4.815662
228.009721	7999.852444	10.036736	-0.047601	4.815670
228.005801	7999.913205	10.041741	-0.047600	4.815687
227.921601	7999.841418	10.046746	-0.047584	4.815667
227.916962	7999.853079	10.051751	-0.047584	4.815670
227.834739	7999.890170	10.056755	-0.047568	4.815681
227.773279	7999.848628	10.061760	-0.047557	4.815670
228.064369	7999.912002	10.066765	-0.047611	4.815687
227.963082	7999.797254	10.071770	-0.047592	4.815654
227.952470	7999.913398	10.076775	-0.047590	4.815688
227.825264	7999.898543	10.081779	-0.047566	4.815684
228.181141	7999.767675	10.086784	-0.047633	4.815644
228.075425	7999.975129	10.091789	-0.047613	4.815705
228.052241	7999.843497	10.096794	-0.047609	4.815667
228.010691	7999.944203	10.101799	-0.047601	4.815696
228.043438	7999.880700	10.106803	-0.047607	4.815678
228.083322	7999.836520	10.111808	-0.047614	4.815665
228.021099	7999.870732	10.116813	-0.047603	4.815675
228.183906	7999.803986	10.121818	-0.047633	4.815655
228.139658	7999.867299	10.126823	-0.047625	4.815673
227.880741	7999.907950	10.131827	-0.047576	4.815686
228.095541	7999.851645	10.136832	-0.047616	4.815669
228.093395	7999.907099	10.141837	-0.047616	4.815685
228.029651	7999.829237	10.146842	-0.047604	4.815663
228.112959	7999.848717	10.151847	-0.047620	4.815668
228.345095	7999.899404	10.156851	-0.047663	4.815682
228.094613	7999.820672	10.161856	-0.047616	4.815660
228.261133	7999.890578	10.166861	-0.047647	4.815680
228.233332	7999.813295	10.171866	-0.047642	4.815657
228.332111	7999.888514	10.176871	-0.047660	4.815679
228.206468	7999.875819	10.181875	-0.047637	4.815675
228.284394	7999.831184	10.186880	-0.047651	4.815662
228.299010	7999.902915	10.191885	-0.047654	4.815683
228.238650	7999.876330	10.196890	-0.047643	4.815675
228.241024	7999.815539	10.201895	-0.047643	4.815658
228.120685	7999.859487	10.206899	-0.047621	4.815671
228.259406	7999.862784	10.211904	-0.047646	4.815671
228.147641	7999.889796	10.216909	-0.047626	4.815680
228.042177	7999.860351	10.221914	-0.047606	4.815672
228.207956	7999.812861	10.226919	-0.047637	4.815657
228.115217	7999.860454	10.231923	-0.047620	4.815671
228.203090	7999.877873	10.236928	-0.047636	4.815676
228.313295	7999.997030	10.241933	-0.047656	4.815710
228.200428	7999.814865	10.246938	-0.047635	4.815658
228.227757	7999.809967	10.251943	-0.047640	4.815656
228.105712	7999.967003	10.256947	-0.047618	4.815703
228.183704	7999.843401	10.261952	-0.047632	4.815666
228.120475	7999.918148	10.266957	-0.047620	4.815688
228.255834	7999.781597	10.271962	-0.047645	4.815648
228.312392	7999.876412	10.276967	-0.047656	4.815675
228.341629	7999.865142	10.281971	-0.047661	4.815672
228.299531	7999.770555	10.286976	-0.047654	4.815644
228.171637	7999.922161	10.291981	-0.047630	4.815689
228.258809	7999.773096	10.296986	-0.047646	4.815645
228.405687	7999.938729	10.301991	-0.047673	4.815693
228.251081	7999.862606	10.306995	-0.047644	4.815671
228.461421	7999.808364	10.312000	-0.047684	4.815655
228.157225	7999.873897	10.317005	-0.047627	4.815675
228.131336	7999.863874	10.322010	-0.047622	4.815672
228.255877	7999.839197	10.327015	-0.047645	4.815665
228.230382	7999.881470	10.332019	-0.047640	4.815677
228.206421	7999.882149	10.337024	-0.047636	4.815677
228.438829	7999.847470	10.342029	-0.047679	4.815666
228.254700	7999.830632	10.347034	-0.047645	4.815662
228.444573	7999.875303	10.352039	-0.047680	4.815674
228.401114	7999.877803	10.357043	-0.047672	4.815675
228.469175	7999.867158	10.362048	-0.047685	4.815672
228.292531	7999.845104	10.367053	-0.047652	4.815666
228.148967	7999.892947	10.372058	-0.047625	4.815681
228.427227	7999.834462	10.377063	-0.047677	4.815662
228.412993	7999.907863	10.382067	-0.047674	4.815684
228.263967	7999.816890	10.387072	-0.047646	4.815658
228.265422	7999.936430	10.392077	-0.047647	4.815693
228.274086	7999.844793	10.397082	-0.047648	4.815666
228.202855	7999.930083	10.402087	-0.047635	4.815691
228.185892	7999.877518	10.407091	-0.047632	4.815676
228.398959	7999.792372	10.412096	-0.047671	4.815650
228.283842	7999.946319	10.417101	-0.047650	4.815696
228.321450	7999.863685	10.422106	-0.047657	4.815671
228.420206	7999.878078	10.427111	-0.047675	4.815675
228.353005	7999.792691	10.432115	-0.047663	4.815651
228.163585	7999.925166	10.437120	-0.047627	4.815690
228.215411	7999.829956	10.442125	-0.047637	4.815662
228.224420	7999.752198	10.447130	-0.047639	4.815639
228.305880	7999.932785	10.452135	-0.047654	4.815692
228.176352	7999.854931	10.457139	-0.047630	4.815670
228.175272	7999.897597	10.462144	-0.047630	4.815682
228.241727	7999.844240	10.467149	-0.047642	4.815666
228.146458	7999.821362	10.472154	-0.047624	4.815660
228.389088	7999.867950	10.477159	-0.047669	4.815672
228.243712	7999.879481	10.482163	-0.047642	4.815676
228.425549	7999.892009	10.487168	-0.047676	4.815679
228.446564	7999.872069	10.492173	-0.047680	4.815673
228.388435	7999.814573	10.497178	-0.047669	4.815657
228.338902	7999.860728	10.502183	-0.047660	4.815670
228.149328	7999.880085	10.507187	-0.047624	4.815677
228.195507	7999.908571	10.512192	-0.047633	4.815685
228.278343	7999.830934	10.517197	-0.047648	4.815662
228.254887	7999.889246	10.522202	-0.047644	4.815679
228.649919	7999.896669	10.527207	-0.047718	4.815680
228.501627	7999.813177	10.532211	-0.047690	4.815656
228.302398	7999.866527	10.537216	-0.047653	4.815672
228.319779	7999.934034	10.542221	-0.047656	4.815692
228.561147	7999.817330	10.547226	-0.047701	4.815657
228.533822	7999.910796	10.552231	-0.047696	4.815684
228.171326	7999.888952	10.557235	-0.047628	4.815680
228.398918	7999.815779	10.562240	-0.047671	4.815657
228.283572	7999.930238	10.567245	-0.047649	4.815691
228.193945	7999.792201	10.572250	-0.047632	4.815651
228.308719	7999.855939	10.577255	-0.047654	4.815669
228.356149	7999.908989	10.582259	-0.047663	4.815685
228.448826	7999.773885	10.587264	-0.047680	4.815645
228.268736	7999.912914	10.592269	-0.047646	4.815686
228.327134	7999.856226	10.597274	-0.047657	4.815669
228.462629	7999.845599	10.602279	-0.047682	4.815665
228.343824	7999.810603	10.607283	-0.047660	4.815656
228.567715	7999.859024	10.612288	-0.047702	4.815669
228.575367	7999.937046	10.617293	-0.047703	4.815692
228.281682	7999.821335	10.622298	-0.047648	4.815659
228.477288	7999.859696	10.627303	-0.047685	4.815670
228.543598	7999.892775	10.632307	-0.047697	4.815679
228.458482	7999.843381	10.637312	-0.047681	4.815665
228.304696	7999.824897	10.642317	-0.047653	4.815660
228.402603	7999.894767	10.647322	-0.047671	4.815680
228.537402	7999.843577	10.652327	-0.047696	4.815665
228.521038	7999.814499	10.657331	-0.047693	4.815656
228.476307	7999.858597	10.662336	-0.047684	4.815669
228.548942	7999.970746	10.667341	-0.047698	4.815702
228.699492	7999.798156	10.672346	-0.047726	4.815651
228.586993	7999.847565	10.677351	-0.047705	4.815665
228.392569	7999.920201	10.682355	-0.047669	4.815688
228.392510	7999.835894	10.687360	-0.047669	4.815663
228.268810	7999.822162	10.692365	-0.047646	4.815660
228.341987	7999.876694	10.697370	-0.047659	4.815675
228.510277	7999.815372	10.702375	-0.047691	4.815656
228.322504	7999.919062	10.707379	-0.047656	4.815688
228.303628	7999.836586	10.712384	-0.047652	4.815664
228.478906	7999.897030	10.717389	-0.047685	4.815680
228.226485	7999.855616	10.722394	-0.047638	4.815670
228.220536	7999.807497	10.727399	-0.047636	4.815656
228.505710	7999.907059	10.732403	-0.047690	4.815683
228.375089	7999.782234	10.737408	-0.047665	4.815647
228.273549	7999.934265	10.742413	-0.047646	4.815692
228.472762	7999.870239	10.747418	-0.047683	4.815673
228.649372	7999.924302	10.752423	-0.047716	4.815688
228.467125	7999.841331	10.757427	-0.047682	4.815664
228.340692	7999.799810	10.762432	-0.047659	4.815653
228.412527	7999.908744	10.767437	-0.047672	4.815684
228.564780	7999.788471	10.772442	-0.047700	4.815648
228.596607	7999.882890	10.777447	-0.047706	4.815676
228.435284	7999.862149	10.782451	-0.047676	4.815670
228.404036	7999.796549	10.787456	-0.047670	4.815651
228.426527	7999.946308	10.792461	-0.047675	4.815695
228.409317	7999.867060	10.797466	-0.047671	4.815672
228.590806	7999.829428	10.802471	-0.047705	4.815660
228.300670	7999.889851	10.807475	-0.047651	4.815679
228.515642	7999.814341	10.812480	-0.047691	4.815656
228.350414	8000.003764	10.817485	-0.047660	4.815712
228.345385	7999.857483	10.822490	-0.047659	4.815670
228.474271	7999.811534	10.827495	-0.047683	4.815656
228.665768	7999.863702	10.832499	-0.047719	4.815670
228.680069	7999.778558	10.837504	-0.047721	4.815645
228.592091	7999.910532	10.842509	-0.047705	4.815684
228.573331	7999.847267	10.847514	-0.047702	4.815665
228.664886	7999.793247	10.852519	-0.047719	4.815649
228.385652	7999.875189	10.857523	-0.047667	4.815675
228.511013	7999.870801	10.862528	-0.047690	4.815673
228.598366	7999.864735	10.867533	-0.047706	4.815670
228.561153	7999.849194	10.872538	-0.047699	4.815666
228.417271	7999.875688	10.877543	-0.047672	4.815675
228.294843	7999.880119	10.882547	-0.047650	4.815676
228.436139	7999.814094	10.887552	-0.047676	4.815656
228.353909	7999.913079	10.892557	-0.047660	4.815686
228.369916	7999.841836	10.897562	-0.047663	4.815665
228.488975	7999.864025	10.902567	-0.047686	4.815671
228.378703	7999.868651	10.907571	-0.047665	4.815673
228.426034	7999.837396	10.912576	-0.047674	4.815663
228.422065	7999.852270	10.917581	-0.047673	4.815668
228.464610	7999.886034	10.922586	-0.047681	4.815677
228.437397	7999.827968	10.927591	-0.047676	4.815660
228.309116	7999.910205	10.932595	-0.047652	4.815685
228.485897	7999.818073	10.937600	-0.047685	4.815657
228.481064	7999.825462	10.942605	-0.047684	4.815660
228.247723	7999.879330	10.947610	-0.047640	4.815676
228.529089	7999.809157	10.952615	-0.047693	4.815655
228.655877	7999.943520	10.957619	-0.047716	4.815693
228.835764	7999.824759	10.962624	-0.047750	4.815658
228.728478	7999.874253	10.967629	-0.047730	4.815673
228.662781	7999.800627	10.972634	-0.047717	4.815651
228.429355	7999.908918	10.977639	-0.047674	4.815684
228.363868	7999.924936	10.982643	-0.047662	4.815689
228.502405	7999.771361	10.987648	-0.047688	4.815644
228.385996	7999.890072	10.992653	-0.047666	4.815679
228.352989	7999.862860	10.997658	-0.047660	4.815671
228.638457	7999.803424	11.002663	-0.047713	4.815652
228.803125	7999.938398	11.007667	-0.047744	4.815691
228.848009	7999.843074	11.012672	-0.047752	4.815663
228.707274	7999.876023	11.017677	-0.047726	4.815673
228.727391	7999.888083	11.022682	-0.047729	4.815677
228.671106	7999.834884	11.027687	-0.047719	4.815661
228.721001	7999.842088	11.032691	-0.047728	4.815663
228.682389	7999.859606	11.037696	-0.047721	4.815669
228.712243	7999.844077	11.042701	-0.047726	4.815664
228.687234	7999.852209	11.047706	-0.047722	4.815666
228.842400	7999.940076	11.052711	-0.047751	4.815691
228.821646	7999.870375	11.057715	-0.047747	4.815671
228.794878	7999.887016	11.062720	-0.047742	4.815676
228.706009	7999.877046	11.067725	-0.047725	4.815674
228.699513	7999.805441	11.072730	-0.047724	4.815653
228.802509	7999.850849	11.077735	-0.047743	4.815665
228.624002	7999.882122	11.082739	-0.047710	4.815675
228.699843	7999.864132	11.087744	-0.047724	4.815670
228.628081	7999.914198	11.092749	-0.047710	4.815685
228.570512	7999.786279	11.097754	-0.047700	4.815648
228.791013	7999.890137	11.102759	-0.047741	4.815677
228.809794	7999.864825	11.107763	-0.047744	4.815670
228.775514	7999.782101	11.112768	-0.047738	4.815646
228.797031	7999.910503	11.117773	-0.047742	4.815683
228.787587	7999.872998	11.122778	-0.047740	4.815672
228.716580	7999.856913	11.127783	-0.047727	4.815668
228.586334	7999.849479	11.132787	-0.047702	4.815666
228.668444	7999.821985	11.137792	-0.047718	4.815658
228.506987	7999.929300	11.142797	-0.047688	4.815690
228.549064	7999.790179	11.147802	-0.047695	4.815649
228.748188	7999.848873	11.152807	-0.047732	4.815665
228.677346	7999.890416	11.157811	-0.047719	4.815678
228.546149	7999.825341	11.162816	-0.047695	4.815659
228.579683	7999.844020	11.167821	-0.047701	4.815665
228.539970	7999.824170	11.172826	-0.047694	4.815659
228.859746	7999.895477	11.177831	-0.047753	4.815678
228.749545	7999.902238	11.182835	-0.047733	4.815681
228.847892	7999.823783	11.187840	-0.047751	4.815657
228.736329	7999.867872	11.192845	-0.047730	4.815671
228.648070	7999.870718	11.197850	-0.047714	4.815672
228.840547	7999.882351	11.202855	-0.047749	4.815675
228.643982	7999.848237	11.207859	-0.047713	4.815665
228.600395	7999.789908	11.212864	-0.047705	4.815649
228.549403	7999.908605	11.217869	-0.047695	4.815684
228.836967	7999.834262	11.222874	-0.047749	4.815660
228.787595	7999.834533	11.227879	-0.047739	4.815661
228.602213	7999.898776	11.232883	-0.047705	4.815680
228.759275	7999.789252	11.237888	-0.047734	4.815648
228.730300	7999.920042	11.242893	-0.047729	4.815686
228.667851	7999.771769	11.247898	-0.047717	4.815643
228.728603	7999.805826	11.252903	-0.047728	4.815653
228.901464	7999.950536	11.257907	-0.047761	4.815694
228.637778	7999.752070	11.262912	-0.047711	4.815637
228.734349	7999.881678	11.267917	-0.047729	4.815675
228.748868	7999.936334	11.272922	-0.047732	4.815691
228.811014	7999.766589	11.277927	-0.047743	4.815641
228.779135	7999.903735	11.282931	-0.047738	4.815681
228.809937	7999.946915	11.287936	-0.047743	4.815694
228.849769	7999.887793	11.292941	-0.047751	4.815676
228.735458	7999.871011	11.297946	-0.047729	4.815672
228.859715	7999.912493	11.302951	-0.047752	4.815683
228.949148	7999.783739	11.307955	-0.047769	4.815645
228.723150	7999.858000	11.312960	-0.047727	4.815668
228.911874	7999.879177	11.317965	-0.047762	4.815673
228.861678	7999.807935	11.322970	-0.047753	4.815653
228.943114	7999.830587	11.327975	-0.047768	4.815659
228.573258	7999.905734	11.332979	-0.047699	4.815683
228.827481	7999.851131	11.337984	-0.047746	4.815665
229.055335	7999.890012	11.342989	-0.047789	4.815676
228.786942	7999.868615	11.347994	-0.047739	4.815671
228.741155	7999.862540	11.352999	-0.047730	4.815669
228.967344	7999.853373	11.358003	-0.047772	4.815665
228.977802	7999.840733	11.363008	-0.047774	4.815662
228.769834	7999.845920	11.368013	-0.047735	4.815664
228.793316	7999.899653	11.373018	-0.047740	4.815680
229.044140	7999.835391	11.378023	-0.047786	4.815660
228.784460	7999.847216	11.383027	-0.047738	4.815665
228.733815	7999.836794	11.388032	-0.047729	4.815662
228.774659	7999.952701	11.393037	-0.047736	4.815695
228.746647	7999.830593	11.398042	-0.047731	4.815660
229.004576	7999.847548	11.403047	-0.047779	4.815664
228.870809	7999.858199	11.408051	-0.047754	4.815667
228.645479	7999.801213	11.413056	-0.047712	4.815652
228.475486	7999.862503	11.418061	-0.047680	4.815670
228.788708	7999.860072	11.423066	-0.047739	4.815668
228.998790	7999.834638	11.428071	-0.047778	4.815660
228.753470	7999.927797	11.433075	-0.047732	4.815688
228.809723	7999.855067	11.438080	-0.047742	4.815667
228.736167	7999.863485	11.443085	-0.047729	4.815670
228.737411	7999.833623	11.448090	-0.047729	4.815661
228.973997	7999.877980	11.453095	-0.047773	4.815673
228.774494	7999.859827	11.458099	-0.047736	4.815668
228.755686	7999.817903	11.463104	-0.047732	4.815656
228.837164	7999.933397	11.468109	-0.047747	4.815690
228.750696	7999.791140	11.473114	-0.047731	4.815648
228.871585	7999.836836	11.478119	-0.047754	4.815661
228.797263	7999.884726	11.483123	-0.047740	4.815675
228.912560	7999.851364	11.488128	-0.047761	4.815665
228.919227	7999.851469	11.493133	-0.047762	4.815665
228.844110	7999.796900	11.498138	-0.047748	4.815650
228.679577	7999.847607	11.503143	-0.047718	4.815665
228.686630	7999.902142	11.508147	-0.047719	4.815681
228.859365	7999.775796	11.513152	-0.047751	4.815643
228.845490	7999.903628	11.518157	-0.047749	4.815681
228.677570	7999.844364	11.523162	-0.047717	4.815664
228.935487	7999.871990	11.528167	-0.047765	4.815671
228.878281	7999.797434	11.533171	-0.047755	4.815650
228.785022	7999.821542	11.538176	-0.047737	4.815657
229.025474	7999.861693	11.543181	-0.047782	4.815668
228.799224	7999.902869	11.548186	-0.047740	4.815681
228.710395	7999.798991	11.553191	-0.047723	4.815651
228.672360	7999.928568	11.558195	-0.047716	4.815689
228.862861	7999.853730	11.563200	-0.047752	4.815666
228.907973	7999.887536	11.568205	-0.047760	4.815676
228.833471	7999.829776	11.573210	-0.047746	4.815659
228.850949	7999.869539	11.578215	-0.047749	4.815671
228.759782	7999.887278	11.583219	-0.047732	4.815676
228.789243	7999.789573	11.588224	-0.047738	4.815648
228.716856	7999.958081	11.593229	-0.047724	4.815697
228.693328	7999.767749	11.598234	-0.047720	4.815642
229.017651	7999.894621	11.603239	-0.047780	4.815677
228.999344	7999.799348	11.608243	-0.047777	4.815650
228.856966	7999.889895	11.613248	-0.047750	4.815677
228.612697	7999.832604	11.618253	-0.047705	4.815661
228.752967	7999.812450	11.623258	-0.047731	4.815655
228.809236	7999.817622	11.628263	-0.047741	4.815656
228.702434	7999.916212	11.633267	-0.047721	4.815685
228.618312	7999.814544	11.638272	-0.047706	4.815656
228.789878	7999.902675	11.643277	-0.047738	4.815681
228.742452	7999.878432	11.648282	-0.047729	4.815674
228.808832	7999.801596	11.653287	-0.047741	4.815651
228.747204	7999.912652	11.658291	-0.047730	4.815684
228.821237	7999.864753	11.663296	-0.047743	4.815670
228.765062	7999.870249	11.668301	-0.047733	4.815671
228.877634	7999.836843	11.673306	-0.047754	4.815661
228.840972	7999.881071	11.678311	-0.047747	4.815674
228.760234	7999.838150	11.683315	-0.047732	4.815662
228.862992	7999.899562	11.688320	-0.047751	4.815680
228.761368	7999.858440	11.693325	-0.047732	4.815668
228.812520	7999.880604	11.698330	-0.047742	4.815674
228.879312	7999.850729	11.703335	-0.047754	4.815665
228.842766	7999.869347	11.708339	-0.047747	4.815671
228.790845	7999.901591	11.713344	-0.047737	4.815680
228.804570	7999.883668	11.718349	-0.047740	4.815675
228.587680	7999.833220	11.723354	-0.047700	4.815661
228.794974	7999.863233	11.728359	-0.047738	4.815669
228.763561	7999.881934	11.733363	-0.047732	4.815675
228.898959	7999.839291	11.738368	-0.047757	4.815662
229.080269	7999.845408	11.743373	-0.047791	4.815663
229.062894	7999.805642	11.748378	-0.047788	4.815651
228.990211	7999.879170	11.753383	-0.047774	4.815673
228.758692	7999.876508	11.758387	-0.047731	4.815673
228.997501	7999.877148	11.763392	-0.047776	4.815672
229.227480	7999.832826	11.768397	-0.047818	4.815658
228.986055	7999.816132	11.773402	-0.047773	4.815655
228.941545	7999.857032	11.778407	-0.047765	4.815667
229.030028	7999.820037	11.783411	-0.047782	4.815656
228.881097	7999.919016	11.788416	-0.047754	4.815685
228.852595	7999.779826	11.793421	-0.047748	4.815645
229.011081	7999.914701	11.798426	-0.047778	4.815683
229.161718	7999.852027	11.803431	-0.047806	4.815664
228.738599	7999.837744	11.808435	-0.047727	4.815662
228.728574	7999.808768	11.813440	-0.047725	4.815654
228.839913	7999.873519	11.818445	-0.047746	4.815672
228.745610	7999.933893	11.823450	-0.047728	4.815690
228.986532	7999.847061	11.828455	-0.047773	4.815664
228.868999	7999.815287	11.833459	-0.047751	4.815655
228.892181	7999.819927	11.838464	-0.047756	4.815656
228.907438	7999.963168	11.843469	-0.047758	4.815698
229.026102	7999.813540	11.848474	-0.047780	4.815654
229.062948	7999.896302	11.853479	-0.047787	4.815678
228.826658	7999.864750	11.858483	-0.047743	4.815670
228.977347	7999.824487	11.863488	-0.047771	4.815657
229.188282	7999.869499	11.868493	-0.047811	4.815669
228.945457	7999.833574	11.873498	-0.047765	4.815660
228.729590	7999.932543	11.878503	-0.047725	4.815690
228.875994	7999.821780	11.883507	-0.047752	4.815657
229.097980	7999.800806	11.888512	-0.047794	4.815650
229.011020	7999.933865	11.893517	-0.047777	4.815689
228.957350	7999.769725	11.898522	-0.047767	4.815641
229.039071	7999.853208	11.903527	-0.047783	4.815665
228.796883	7999.897329	11.908531	-0.047738	4.815679
228.990513	7999.864161	11.913536	-0.047774	4.815669
228.928761	7999.868500	11.918541	-0.047762	4.815670
228.983769	7999.882189	11.923546	-0.047772	4.815674
229.099238	7999.792270	11.928551	-0.047794	4.815647
229.118412	7999.916366	11.933555	-0.047797	4.815683
229.010097	7999.826047	11.938560	-0.047777	4.815657
228.876682	7999.870852	11.943565	-0.047752	4.815671
228.973806	7999.864943	11.948570	-0.047770	4.815669
229.109582	7999.819104	11.953575	-0.047795	4.815655
228.990145	7999.912156	11.958579	-0.047773	4.815683
228.766185	7999.815707	11.963584	-0.047731	4.815656
229.105485	7999.877725	11.968589	-0.047795	4.815672
228.928152	7999.812973	11.973594	-0.047762	4.815654
228.914879	7999.866114	11.978599	-0.047759	4.815670
228.940756	7999.864394	11.983603	-0.047764	4.815669
228.877885	7999.859111	11.988608	-0.047752	4.815668
228.902780	7999.793347	11.993613	-0.047757	4.815648
228.708664	7999.935352	11.998618	-0.047721	4.815691
228.819751	7999.869907	12.003623	-0.047741	4.815671
229.074618	7999.863336	12.008627	-0.047789	4.815668
229.006077	7999.861163	12.013632	-0.047776	4.815668
229.136262	7999.848317	12.018637	-0.047800	4.815663
229.088420	7999.815530	12.023642	-0.047791	4.815654
229.043988	7999.841491	12.028647	-0.047783	4.815662
228.987641	7999.940894	12.033651	-0.047772	4.815691
229.031656	7999.801803	12.038656	-0.047780	4.815650
229.054659	7999.835253	12.043661	-0.047785	4.815660
228.978645	7999.902324	12.048666	-0.047771	4.815680
229.043042	7999.875613	12.053671	-0.047783	4.815672
229.033346	7999.812493	12.058675	-0.047781	4.815653
229.077534	7999.826007	12.063680	-0.047789	4.815657
229.283282	7999.863466	12.068685	-0.047827	4.815667
229.111403	7999.917256	12.073690	-0.047795	4.815684
229.133027	7999.820491	12.078695	-0.047799	4.815655
228.814531	7999.817496	12.083699	-0.047740	4.815656
229.008390	7999.876106	12.088704	-0.047776	4.815672
229.008724	7999.814214	12.093709	-0.047776	4.815654
229.070783	7999.924061	12.098714	-0.047788	4.815686
229.096348	7999.839098	12.103719	-0.047792	4.815661
229.135836	7999.840798	12.108723	-0.047800	4.815661
228.908928	7999.883031	12.113728	-0.047757	4.815675
229.215612	7999.869824	12.118733	-0.047814	4.815669
229.156150	7999.826178	12.123738	-0.047803	4.815657
228.998522	7999.880197	12.128743	-0.047774	4.815673
229.111521	7999.859604	12.133747	-0.047795	4.815667
228.919654	7999.935482	12.138752	-0.047759	4.815690
228.928502	7999.881197	12.143757	-0.047761	4.815674
228.979314	7999.791306	12.148762	-0.047770	4.815647
229.043030	7999.846753	12.153767	-0.047782	4.815663
229.123984	7999.932359	12.158771	-0.047797	4.815688
228.811516	7999.764054	12.163776	-0.047739	4.815640
228.972150	7999.869083	12.168781	-0.047769	4.815670
229.047699	7999.867095	12.173786	-0.047783	4.815669
229.285994	7999.797295	12.178791	-0.047827	4.815648
229.093378	7999.922251	12.183795	-0.047791	4.815685
229.272439	7999.874975	12.188800	-0.047825	4.815670
229.357557	7999.811246	12.193805	-0.047840	4.815651
229.121552	7999.892817	12.198810	-0.047796	4.815676
229.280033	7999.827068	12.203815	-0.047826	4.815656
229.320965	7999.909896	12.208819	-0.047834	4.815680
229.280642	7999.809999	12.213824	-0.047826	4.815651
229.247643	7999.862823	12.218829	-0.047820	4.815667
229.363408	7999.830535	12.223834	-0.047841	4.815657
229.411245	7999.886796	12.228839	-0.047850	4.815673
229.346099	7999.835588	12.233843	-0.047838	4.815659
229.346265	7999.859066	12.238848	-0.047838	4.815665
229.281066	7999.875088	12.243853	-0.047826	4.815670
229.001117	7999.899392	12.248858	-0.047774	4.815679
229.089424	7999.875200	12.253863	-0.047790	4.815671
229.134282	7999.824696	12.258867	-0.047798	4.815656
229.068025	7999.881254	12.263872	-0.047786	4.815673
229.235031	7999.849791	12.268877	-0.047817	4.815663
229.047470	7999.832896	12.273882	-0.047782	4.815659
229.051035	7999.858563	12.278887	-0.047783	4.815667
228.864141	7999.935588	12.283891	-0.047748	4.815690
229.072268	7999.809811	12.288896	-0.047787	4.815652
229.168693	7999.861517	12.293901	-0.047805	4.815667
228.916280	7999.832907	12.298906	-0.047758	4.815660
229.291840	7999.879503	12.303911	-0.047828	4.815672
229.290778	7999.834663	12.308915	-0.047827	4.815659
229.057706	7999.863990	12.313920	-0.047784	4.815668
229.095057	7999.847515	12.318925	-0.047791	4.815663
229.170570	7999.908488	12.323930	-0.047805	4.815681
229.298505	7999.849718	12.328935	-0.047829	4.815663
229.084096	7999.801444	12.333939	-0.047789	4.815650
228.970812	7999.910601	12.338944	-0.047768	4.815682
229.025879	7999.892277	12.343949	-0.047778	4.815677
228.859186	7999.841570	12.348954	-0.047747	4.815663
229.217436	7999.818521	12.353959	-0.047813	4.815654
229.105514	7999.882880	12.358963	-0.047793	4.815674
229.181988	7999.856363	12.363968	-0.047807	4.815665
229.134790	7999.811848	12.368973	-0.047798	4.815653
229.104987	7999.864723	12.373978	-0.047792	4.815668
229.241272	7999.800752	12.378983	-0.047818	4.815649
229.221237	7999.847381	12.383987	-0.047814	4.815663
229.124523	7999.788196	12.388992	-0.047796	4.815646
229.142893	7999.932555	12.393997	-0.047799	4.815688
228.928944	7999.850139	12.399002	-0.047759	4.815665
229.011630	7999.807715	12.404007	-0.047775	4.815652
229.062297	7999.878960	12.409011	-0.047784	4.815673
229.251095	7999.848915	12.414016	-0.047819	4.815663
229.209451	7999.901600	12.419021	-0.047812	4.815679
229.080702	7999.833362	12.424026	-0.047788	4.815659
229.252102	7999.848925	12.429031	-0.047819	4.815663
229.276665	7999.840781	12.434035	-0.047824	4.815660
229.124736	7999.800982	12.439040	-0.047796	4.815650
229.334298	7999.871584	12.444045	-0.047835	4.815669
229.128639	7999.898151	12.449050	-0.047796	4.815678
229.101489	7999.851824	12.454055	-0.047791	4.815665
229.309407	7999.845565	12.459059	-0.047830	4.815662
229.195707	7999.781837	12.464064	-0.047809	4.815644
229.024497	7999.846309	12.469069	-0.047777	4.815663
229.015143	7999.865365	12.474074	-0.047775	4.815669
229.197758	7999.812811	12.479079	-0.047809	4.815653
229.096547	7999.930700	12.484083	-0.047790	4.815688
229.072581	7999.768105	12.489088	-0.047786	4.815640
229.329074	7999.933372	12.494093	-0.047834	4.815687
229.271935	7999.854547	12.499098	-0.047823	4.815665
229.275260	7999.873807	12.504103	-0.047823	4.815670
229.316353	7999.843519	12.509107	-0.047831	4.815661
229.194861	7999.805278	12.514112	-0.047808	4.815651
229.206764	7999.940996	12.519117	-0.047811	4.815690
229.068131	7999.814972	12.524122	-0.047785	4.815654
229.026012	7999.801486	12.529127	-0.047777	4.815650
229.215391	7999.889904	12.534131	-0.047812	4.815675
228.999780	7999.773313	12.539136	-0.047772	4.815642
229.325900	7999.903417	12.544141	-0.047833	4.815679
229.272983	7999.898294	12.549146	-0.047823	4.815677
229.101690	7999.769611	12.554151	-0.047791	4.815641
229.190777	7999.934317	12.559155	-0.047807	4.815688
229.228524	7999.819669	12.564160	-0.047814	4.815655
229.248607	7999.856274	12.569165	-0.047818	4.815665
229.302140	7999.842193	12.574170	-0.047828	4.815661
229.211134	7999.866337	12.579175	-0.047811	4.815668
229.156493	7999.912410	12.584179	-0.047801	4.815682
229.162182	7999.839933	12.589184	-0.047802	4.815661
229.331831	7999.914161	12.594189	-0.047833	4.815682
229.262845	7999.867161	12.599194	-0.047821	4.815668
229.346339	7999.795936	12.604199	-0.047836	4.815647
229.210750	7999.878056	12.609203	-0.047811	4.815672
229.402303	7999.876869	12.614208	-0.047846	4.815670
229.321588	7999.827545	12.619213	-0.047831	4.815656
229.198985	7999.979240	12.624218	-0.047809	4.815701
229.279701	7999.780979	12.629223	-0.047823	4.815643
229.148293	7999.888778	12.634227	-0.047799	4.815675
229.145289	7999.844974	12.639232	-0.047798	4.815662
229.372252	7999.816610	12.644237	-0.047841	4.815653
229.050320	7999.792217	12.649242	-0.047781	4.815647
228.933039	7999.860759	12.654247	-0.047759	4.815668
229.111745	7999.937267	12.659251	-0.047792	4.815690
229.125124	7999.823294	12.664256	-0.047795	4.815656
228.995511	7999.844683	12.669261	-0.047770	4.815663
228.998133	7999.900215	12.674266	-0.047771	4.815679
229.391214	7999.798758	12.679271	-0.047844	4.815648
229.219780	7999.874965	12.684275	-0.047812	4.815671
229.178962	7999.751583	12.689280	-0.047804	4.815635
229.411888	7999.920740	12.694285	-0.047848	4.815683
229.290175	7999.878226	12.699290	-0.047825	4.815671
229.181594	7999.841259	12.704295	-0.047805	4.815661
229.154280	7999.856825	12.709299	-0.047800	4.815666
229.304214	7999.852833	12.714304	-0.047828	4.815664
229.171210	7999.854958	12.719309	-0.047803	4.815665
229.120177	7999.910694	12.724314	-0.047793	4.815682
229.301467	7999.787686	12.729319	-0.047827	4.815645
229.114611	7999.921271	12.734323	-0.047792	4.815685
229.217075	7999.849284	12.739328	-0.047811	4.815663
229.403396	7999.868289	12.744333	-0.047846	4.815668
229.392414	7999.851035	12.749338	-0.047844	4.815663
229.474741	7999.836351	12.754343	-0.047859	4.815658
229.385890	7999.918157	12.759347	-0.047843	4.815683
229.488239	7999.849370	12.764352	-0.047862	4.815662
229.300199	7999.819661	12.769357	-0.047827	4.815654
229.017447	7999.903681	12.774362	-0.047774	4.815680
229.275330	7999.881151	12.779367	-0.047822	4.815672
229.297292	7999.815339	12.784371	-0.047826	4.815653
229.087685	7999.779948	12.789376	-0.047787	4.815644
229.159508	7999.921966	12.794381	-0.047800	4.815685
229.263667	7999.784910	12.799386	-0.047820	4.815644
229.073382	7999.857613	12.804391	-0.047784	4.815666
229.417117	7999.872749	12.809395	-0.047848	4.815669
229.399263	7999.850049	12.814400	-0.047845	4.815663
229.516877	7999.798582	12.819405	-0.047867	4.815647
229.240846	7999.870971	12.824410	-0.047815	4.815670
229.351686	7999.816194	12.829415	-0.047836	4.815653
229.462419	7999.896944	12.834419	-0.047856	4.815676
229.263768	7999.747543	12.839424	-0.047819	4.815633
229.292730	7999.919819	12.844429	-0.047825	4.815684
229.258405	7999.827489	12.849434	-0.047818	4.815657
229.343984	7999.826730	12.854439	-0.047834	4.815656
229.265466	7999.823329	12.859443	-0.047820	4.815656
229.457030	7999.841351	12.864448	-0.047855	4.815660
229.476927	7999.968661	12.869453	-0.047859	4.815697
229.385340	7999.836991	12.874458	-0.047842	4.815659
229.426598	7999.856861	12.879463	-0.047850	4.815665
229.518341	7999.816717	12.884467	-0.047867	4.815652
229.186319	7999.808168	12.889472	-0.047805	4.815651
229.209662	7999.849093	12.894477	-0.047809	4.815663
229.343605	7999.900337	12.899482	-0.047834	4.815678
229.447013	7999.828365	12.904487	-0.047853	4.815656
229.377222	7999.876329	12.909491	-0.047840	4.815670
229.239286	7999.880509	12.914496	-0.047815	4.815672
229.385503	7999.860450	12.919501	-0.047842	4.815666
229.151877	7999.846015	12.924506	-0.047798	4.815663
229.265491	7999.881991	12.929511	-0.047819	4.815673
229.329712	7999.830732	12.934515	-0.047831	4.815657
229.508777	7999.879500	12.939520	-0.047865	4.815671
229.569465	7999.834587	12.944525	-0.047876	4.815657
229.428100	7999.807764	12.949530	-0.047849	4.815650
229.585597	7999.798559	12.954535	-0.047879	4.815647
229.371523	7999.931706	12.959539	-0.047839	4.815687
229.356864	7999.819416	12.964544	-0.047836	4.815654
229.471440	7999.835131	12.969549	-0.047857	4.815658
229.257324	7999.897846	12.974554	-0.047818	4.815677
229.267500	7999.838247	12.979559	-0.047819	4.815660
229.573945	7999.900805	12.984563	-0.047876	4.815677
229.286507	7999.767049	12.989568	-0.047823	4.815639
229.094489	7999.825850	12.994573	-0.047787	4.815657
229.304717	7999.900732	12.999578	-0.047826	4.815678
229.503260	7999.758792	13.004583	-0.047863	4.815636
229.538052	7999.949305	13.009587	-0.047870	4.815691
229.551948	7999.762773	13.014592	-0.047872	4.815636
229.558417	7999.834374	13.019597	-0.047873	4.815657
229.328351	7999.962996	13.024602	-0.047831	4.815696
229.404255	7999.799873	13.029607	-0.047845	4.815648
229.414391	7999.826713	13.034611	-0.047846	4.815656
229.258562	7999.808195	13.039616	-0.047817	4.815651
229.411415	7999.898160	13.044621	-0.047846	4.815677
229.192609	7999.796457	13.049626	-0.047805	4.815648
229.430983	7999.771479	13.054631	-0.047849	4.815640
229.270930	7999.934309	13.059635	-0.047820	4.815688
229.197557	7999.800798	13.064640	-0.047806	4.815649
229.274592	7999.823379	13.069645	-0.047820	4.815656
229.187396	7999.874263	13.074650	-0.047804	4.815671
229.256868	7999.857238	13.079655	-0.047817	4.815665
229.334573	7999.815800	13.084659	-0.047831	4.815653
229.337414	7999.778493	13.089664	-0.047832	4.815642
229.367509	7999.844072	13.094669	-0.047837	4.815661
229.355434	7999.899367	13.099674	-0.047835	4.815677
229.654663	7999.823079	13.104679	-0.047891	4.815654
229.352818	7999.935604	13.109683	-0.047835	4.815688
229.173276	7999.820660	13.114688	-0.047801	4.815655
229.294835	7999.847159	13.119693	-0.047824	4.815662
229.334222	7999.870201	13.124698	-0.047831	4.815669
229.332670	7999.793339	13.129703	-0.047831	4.815646
229.296134	7999.838636	13.134707	-0.047824	4.815660
229.394816	7999.829551	13.139712	-0.047842	4.815657
229.495286	7999.870651	13.144717	-0.047861	4.815668
229.372855	7999.898558	13.149722	-0.047838	4.815677
229.481827	7999.786124	13.154727	-0.047858	4.815644
229.255302	7999.943615	13.159731	-0.047816	4.815691
229.329806	7999.761262	13.164736	-0.047830	4.815637
229.405049	7999.891597	13.169741	-0.047844	4.815675
229.472227	7999.878803	13.174746	-0.047856	4.815671
229.423311	7999.801178	13.179751	-0.047847	4.815648
229.688844	7999.816122	13.184755	-0.047897	4.815651
229.381096	7999.833575	13.189760	-0.047839	4.815658
229.536778	7999.878766	13.194765	-0.047868	4.815670
229.632113	7999.777851	13.199770	-0.047886	4.815641
229.760633	7999.888769	13.204775	-0.047910	4.815672
229.568926	7999.814180	13.209779	-0.047874	4.815651
229.300226	7999.865344	13.214784	-0.047824	4.815668
229.475511	7999.819074	13.219789	-0.047857	4.815653
229.573987	7999.920970	13.224794	-0.047875	4.815683
229.439863	7999.808891	13.229799	-0.047850	4.815651
229.266741	7999.835982	13.234803	-0.047818	4.815659
229.317654	7999.836799	13.239808	-0.047827	4.815659
229.435740	7999.852571	13.244813	-0.047849	4.815663
229.323006	7999.894507	13.249818	-0.047828	4.815676
229.359674	7999.795850	13.254823	-0.047835	4.815647
229.513194	7999.830334	13.259827	-0.047864	4.815656
229.368716	7999.929385	13.264832	-0.047837	4.815686
229.563869	7999.902645	13.269837	-0.047873	4.815677
229.379818	7999.818575	13.274842	-0.047839	4.815654
229.394595	7999.844422	13.279847	-0.047841	4.815661
229.590957	7999.809164	13.284851	-0.047878	4.815650
229.513131	7999.854863	13.289856	-0.047863	4.815664
229.388271	7999.783486	13.294861	-0.047840	4.815643
229.202384	7999.879736	13.299866	-0.047806	4.815672
229.380325	7999.875129	13.304871	-0.047839	4.815670
229.490915	7999.802206	13.309875	-0.047859	4.815648
229.480501	7999.846856	13.314880	-0.047857	4.815661
229.267156	7999.876501	13.319885	-0.047818	4.815671
229.381858	7999.885816	13.324890	-0.047839	4.815673
229.420986	7999.780795	13.329895	-0.047846	4.815642
229.395607	7999.827339	13.334899	-0.047841	4.815656
229.330958	7999.873251	13.339904	-0.047829	4.815670
229.428150	7999.818254	13.344909	-0.047847	4.815653
229.438750	7999.899526	13.349914	-0.047849	4.815677
229.558519	7999.801139	13.354919	-0.047872	4.815648
229.545150	7999.882026	13.359923	-0.047869	4.815671
229.496500	7999.803337	13.364928	-0.047860	4.815649
229.562375	7999.818269	13.369933	-0.047872	4.815653
229.437953	7999.905905	13.374938	-0.047849	4.815679
229.154953	7999.769019	13.379943	-0.047796	4.815640
229.285584	7999.845820	13.384947	-0.047821	4.815662
229.254233	8000.049141	13.389952	-0.047815	4.815722
229.395482	7999.786757	13.394957	-0.047841	4.815644
229.192290	7999.879528	13.399962	-0.047803	4.815672
229.291989	7999.796825	13.404967	-0.047822	4.815648
229.455909	7999.921118	13.409971	-0.047852	4.815683
229.236649	7999.821541	13.414976	-0.047811	4.815655
229.269041	7999.799650	13.419981	-0.047817	4.815649
229.342638	7999.884071	13.424986	-0.047831	4.815673
229.168949	7999.788430	13.429991	-0.047799	4.815646
229.378849	7999.919866	13.434995	-0.047838	4.815683
229.352854	7999.797789	13.440000	-0.047833	4.815648
229.354436	7999.888520	13.445005	-0.047833	4.815674
229.228565	7999.806455	13.450010	-0.047810	4.815651
229.252555	7999.819645	13.455015	-0.047814	4.815655
229.273317	7999.946968	13.460019	-0.047818	4.815692
229.231065	7999.761668	13.465024	-0.047810	4.815638
229.273709	7999.924559	13.470029	-0.047818	4.815685
229.285307	7999.810558	13.475034	-0.047820	4.815652
229.165840	7999.867326	13.480039	-0.047798	4.815669
229.151534	7999.826542	13.485043	-0.047795	4.815657
229.185977	7999.892190	13.490048	-0.047802	4.815676
229.431896	7999.837453	13.495053	-0.047847	4.815659
229.251707	7999.810006	13.500058	-0.047814	4.815652
229.391447	7999.814387	13.505063	-0.047840	4.815652
229.442533	7999.952871	13.510067	-0.047849	4.815693
229.200014	7999.784622	13.515072	-0.047804	4.815645
229.228170	7999.887520	13.520077	-0.047809	4.815675
229.119410	7999.849483	13.525082	-0.047789	4.815664
229.296435	7999.882211	13.530087	-0.047822	4.815673
229.284105	7999.823317	13.535091	-0.047819	4.815656
229.260391	7999.880559	13.540096	-0.047815	4.815672
229.496942	7999.822470	13.545101	-0.047859	4.815654
229.083124	7999.875567	13.550106	-0.047782	4.815672
229.100826	7999.784074	13.555111	-0.047785	4.815645
229.124708	7999.835680	13.560115	-0.047790	4.815660
229.037441	7999.891899	13.565120	-0.047773	4.815677
229.200914	7999.784611	13.570125	-0.047804	4.815645
229.293118	7999.897077	13.575130	-0.047821	4.815677
229.314072	7999.782160	13.580135	-0.047825	4.815643
229.352804	7999.902302	13.585139	-0.047832	4.815678
229.367106	7999.899329	13.590144	-0.047835	4.815677
229.664648	7999.938267	13.595149	-0.047890	4.815687
229.611929	7999.786945	13.600154	-0.047880	4.815643
229.403445	7999.872161	13.605159	-0.047841	4.815669
229.441551	7999.826884	13.610163	-0.047848	4.815656
229.382430	7999.790714	13.615168	-0.047837	4.815646
229.363967	7999.859779	13.620173	-0.047834	4.815666
229.392333	7999.925331	13.625178	-0.047839	4.815685
229.481328	7999.786963	13.630183	-0.047856	4.815644
229.343998	7999.819966	13.635187	-0.047830	4.815654
229.433454	7999.864090	13.640192	-0.047847	4.815667
229.519808	7999.844135	13.645197	-0.047863	4.815660
229.453015	7999.814244	13.650202	-0.047850	4.815652
229.374561	7999.867404	13.655207	-0.047836	4.815668
229.605282	7999.843370	13.660211	-0.047879	4.815660
229.360088	7999.885308	13.665216	-0.047833	4.815673
229.373386	7999.794811	13.670221	-0.047835	4.815647
229.470657	7999.896688	13.675226	-0.047854	4.815676
229.576717	7999.770334	13.680231	-0.047873	4.815639
229.526160	7999.869831	13.685235	-0.047864	4.815668
229.517513	7999.933719	13.690240	-0.047862	4.815687
229.798752	7999.802715	13.695245	-0.047914	4.815647
229.746139	7999.823209	13.700250	-0.047905	4.815653
229.391028	7999.907131	13.705255	-0.047839	4.815680
229.569582	7999.824630	13.710259	-0.047872	4.815655
229.483430	7999.779488	13.715264	-0.047856	4.815642
229.592033	7999.869808	13.720269	-0.047876	4.815668
229.468026	7999.891287	13.725274	-0.047853	4.815675
229.640473	7999.757464	13.730279	-0.047885	4.815635
229.643701	7999.909051	13.735283	-0.047885	4.815679
229.546280	7999.872264	13.740288	-0.047867	4.815669
229.693904	7999.809541	13.745293	-0.047895	4.815650
229.723183	7999.876175	13.750298	-0.047900	4.815669
229.636207	7999.856630	13.755303	-0.047884	4.815664
229.554201	7999.824360	13.760307	-0.047869	4.815655
229.509698	7999.855656	13.765312	-0.047860	4.815664
229.776297	7999.842871	13.770317	-0.047910	4.815659
229.789191	7999.822800	13.775322	-0.047912	4.815653
229.718761	7999.896366	13.780327	-0.047899	4.815675
229.583942	7999.810954	13.785331	-0.047874	4.815651
229.559322	7999.857510	13.790336	-0.047869	4.815664
229.607406	7999.776111	13.795341	-0.047878	4.815640
229.700260	7999.792544	13.800346	-0.047896	4.815645
229.497229	7999.906660	13.805351	-0.047858	4.815679
229.682311	7999.853078	13.810355	-0.047892	4.815662
229.715088	7999.810917	13.815360	-0.047898	4.815650
229.914470	7999.803453	13.820365	-0.047935	4.815647
229.680808	7999.941622	13.825370	-0.047892	4.815688
229.630327	7999.749785	13.830375	-0.047882	4.815632
229.556237	7999.925738	13.835379	-0.047869	4.815684
229.394641	7999.811082	13.840384	-0.047838	4.815651
229.431310	7999.802066	13.845389	-0.047845	4.815649
229.650063	7999.784242	13.850394	-0.047886	4.815642
229.742270	7999.873232	13.855399	-0.047903	4.815668
229.815537	7999.805043	13.860403	-0.047917	4.815648
229.809375	7999.870039	13.865408	-0.047916	4.815667
229.851549	7999.785342	13.870413	-0.047923	4.815642
229.711364	7999.915412	13.875418	-0.047897	4.815680
229.814154	7999.772997	13.880423	-0.047916	4.815638
229.719121	7999.817353	13.885427	-0.047899	4.815652
229.581376	7999.856752	13.890432	-0.047873	4.815664
229.638393	7999.842727	13.895437	-0.047884	4.815660
229.583804	7999.851450	13.900442	-0.047873	4.815662
229.431863	7999.792443	13.905447	-0.047845	4.815646
229.594439	7999.888968	13.910451	-0.047875	4.815673
229.531575	7999.851670	13.915456	-0.047864	4.815663
229.560113	7999.830784	13.920461	-0.047869	4.815656
229.595936	7999.831358	13.925466	-0.047875	4.815656
229.667067	7999.894397	13.930471	-0.047889	4.815675
229.833320	7999.845847	13.935475	-0.047920	4.815660
229.679696	7999.886058	13.940480	-0.047891	4.815672
229.614168	7999.831642	13.945485	-0.047879	4.815656
229.779505	7999.842840	13.950490	-0.047910	4.815659
229.519200	7999.853586	13.955495	-0.047861	4.815663
229.681835	7999.850867	13.960499	-0.047891	4.815662
229.641209	7999.822464	13.965504	-0.047884	4.815654
229.517688	7999.787391	13.970509	-0.047861	4.815644
229.561193	7999.943895	13.975514	-0.047869	4.815690
229.558869	7999.795520	13.980519	-0.047868	4.815646
229.780242	7999.882320	13.985523	-0.047910	4.815670
229.660740	7999.814230	13.990528	-0.047887	4.815651
229.734075	7999.846356	13.995533	-0.047901	4.815660
229.628353	7999.838248	14.000538	-0.047881	4.815658
229.579984	7999.896161	14.005543	-0.047872	4.815675
229.663808	7999.880434	14.010547	-0.047888	4.815670
229.563277	7999.878813	14.015552	-0.047869	4.815670
229.528429	7999.846235	14.020557	-0.047862	4.815661
229.389104	7999.805572	14.025562	-0.047836	4.815650
229.429697	7999.888394	14.030567	-0.047844	4.815674
229.476272	7999.833649	14.035571	-0.047853	4.815658
229.405759	7999.870929	14.040576	-0.047839	4.815669
229.546882	7999.779289	14.045581	-0.047866	4.815641
229.658199	7999.917676	14.050586	-0.047886	4.815681
229.626988	7999.766701	14.055591	-0.047881	4.815637
229.635661	7999.867152	14.060595	-0.047882	4.815667
229.615600	7999.951132	14.065600	-0.047878	4.815691
229.900132	7999.807375	14.070605	-0.047931	4.815648
229.785901	7999.887706	14.075610	-0.047910	4.815672
229.814783	7999.895639	14.080615	-0.047915	4.815674
229.889534	7999.799728	14.085619	-0.047929	4.815646
229.645512	7999.806468	14.090624	-0.047884	4.815649
229.590822	7999.829063	14.095629	-0.047874	4.815656
229.788835	7999.853592	14.100634	-0.047910	4.815662
229.644881	7999.825660	14.105639	-0.047884	4.815655
229.769759	7999.921579	14.110643	-0.047907	4.815682
229.741209	7999.841079	14.115648	-0.047902	4.815659
229.654646	7999.883437	14.120653	-0.047885	4.815671
229.623428	7999.846649	14.125658	-0.047880	4.815661
229.677634	7999.789892	14.130663	-0.047890	4.815644
229.818144	7999.865787	14.135667	-0.047916	4.815665
229.445451	7999.905671	14.140672	-0.047846	4.815679
229.464924	7999.809938	14.145677	-0.047850	4.815651
229.564799	7999.804074	14.150682	-0.047868	4.815649
229.664106	7999.893178	14.155687	-0.047887	4.815674
229.587245	7999.820438	14.160691	-0.047873	4.815653
229.597665	7999.781118	14.165696	-0.047874	4.815642
229.737600	7999.901824	14.170701	-0.047901	4.815676
229.590300	7999.879174	14.175706	-0.047873	4.815670
229.550190	7999.845444	14.180711	-0.047866	4.815661
229.699555	7999.891600	14.185715	-0.047893	4.815674
229.562673	7999.781611	14.190720	-0.047868	4.815642
229.677354	7999.916850	14.195725	-0.047889	4.815681
229.853473	7999.782019	14.200730	-0.047922	4.815641
229.650700	7999.882267	14.205735	-0.047884	4.815671
229.670974	7999.804688	14.210739	-0.047888	4.815648
229.557259	7999.902101	14.215744	-0.047867	4.815677
229.743018	7999.797306	14.220749	-0.047901	4.815646
229.636421	7999.919379	14.225754	-0.047881	4.815682
229.394213	7999.767142	14.230759	-0.047836	4.815639
229.565401	7999.858469	14.235763	-0.047868	4.815665
229.703254	7999.892702	14.240768	-0.047894	4.815674
229.660176	7999.793827	14.245773	-0.047886	4.815645
229.538082	7999.972209	14.250778	-0.047863	4.815698
229.696757	7999.828560	14.255783	-0.047892	4.815655
229.893123	7999.881877	14.260787	-0.047929	4.815670
229.839518	7999.871406	14.265792	-0.047919	4.815667
229.791192	7999.550479	14.270797	-0.047910	4.815573

229.874434	7996.332542	14.275802	-0.047923	4.814631
229.656307	7990.759526	14.280807	-0.047879	4.813001
229.754369	7984.011053	14.285811	-0.047893	4.811025
229.681809	7976.646713	14.290816	-0.047874	4.808869
229.481714	7969.057936	14.295821	-0.047832	4.806646
229.511155	7961.218586	14.300826	-0.047833	4.804347
229.621802	7953.367176	14.305831	-0.047848	4.802044
229.660848	7945.411015	14.310835	-0.047850	4.799709
229.448557	7937.459304	14.315840	-0.047805	4.797375
229.639382	7929.439788	14.320845	-0.047836	4.795019
229.602804	7921.443224	14.325850	-0.047824	4.792669
229.410345	7913.371990	14.330855	-0.047782	4.790296
229.403369	7905.435781	14.335859	-0.047776	4.787962
229.395624	7897.375125	14.340864	-0.047769	4.785589
229.239840	7889.424605	14.345869	-0.047735	4.783249
229.315075	7881.413299	14.350874	-0.047744	4.780888
229.239173	7873.409253	14.355879	-0.047724	4.778529
229.400175	7865.459868	14.360883	-0.047749	4.776184
229.078431	7857.402439	14.365888	-0.047684	4.773808
229.336196	7849.366949	14.370893	-0.047727	4.771435
229.070783	7841.345857	14.375898	-0.047672	4.769067
229.129380	7833.380303	14.380903	-0.047678	4.766713
229.261615	7825.356201	14.385907	-0.047697	4.764340
229.043412	7817.439591	14.390912	-0.047651	4.762000
229.090059	7809.407664	14.395917	-0.047655	4.759622
229.063522	7801.439002	14.400922	-0.047645	4.757263
229.014547	7793.353947	14.405927	-0.047630	4.754868
228.827139	7785.351519	14.410931	-0.047590	4.752497
228.613929	7777.303417	14.415936	-0.047545	4.750111
228.757738	7769.348422	14.420941	-0.047567	4.747751
228.736109	7761.354619	14.425946	-0.047557	4.745378
228.610561	7753.320687	14.430951	-0.047529	4.742992
228.572264	7745.373656	14.435955	-0.047516	4.740631
228.643207	7737.368678	14.440960	-0.047524	4.738251
228.681185	7729.328559	14.445965	-0.047526	4.735860
228.702696	7721.344786	14.450970	-0.047525	4.733484
228.640342	7713.317077	14.455975	-0.047508	4.731094
228.651205	7705.299352	14.460979	-0.047505	4.728706
228.569447	7697.306863	14.465984	-0.047484	4.726324
228.619200	7689.315385	14.470989	-0.047488	4.723941
228.452907	7681.365872	14.475994	-0.047452	4.721570
228.458483	7673.308900	14.480999	-0.047448	4.719165
228.346792	7665.335579	14.486003	-0.047422	4.716784
228.101872	7657.335000	14.491008	-0.047371	4.714394
228.160769	7649.321057	14.496013	-0.047377	4.711998
228.224403	7641.293471	14.501018	-0.047383	4.709597
228.375089	7633.267464	14.506023	-0.047406	4.707195
228.338900	7625.331760	14.511027	-0.047394	4.704819
228.112074	7617.303962	14.516032	-0.047347	4.702415
228.102408	7609.350544	14.521037	-0.047340	4.700032
228.345989	7601.370541	14.526042	-0.047380	4.697638
228.046143	7593.269392	14.531047	-0.047319	4.695208
228.165240	7585.353955	14.536051	-0.047336	4.692832
228.139822	7577.245213	14.541056	-0.047326	4.690397
228.222300	7569.305438	14.546061	-0.047336	4.688011
227.838300	7561.265374	14.551066	-0.047259	4.685595
227.858816	7553.318921	14.556071	-0.047258	4.683205
227.955883	7545.342691	14.561075	-0.047271	4.680804
227.897910	7537.283724	14.566080	-0.047254	4.678378
228.030835	7529.309647	14.571085	-0.047274	4.675975
228.052259	7521.245921	14.576090	-0.047273	4.673545
227.688760	7513.149536	14.581095	-0.047200	4.671104
227.687217	7505.225575	14.586099	-0.047194	4.668713
227.659879	7497.223901	14.591104	-0.047184	4.666297
227.613079	7489.258351	14.596109	-0.047170	4.663892
227.539696	7481.260694	14.601114	-0.047151	4.661475
227.609142	7473.211956	14.606119	-0.047159	4.659041
227.768899	7465.303886	14.611123	-0.047183	4.656649
227.493930	7457.198472	14.616128	-0.047127	4.654196
227.591351	7449.240718	14.621133	-0.047140	4.651786
227.640066	7441.194218	14.626138	-0.047143	4.649348
227.595960	7433.282468	14.631143	-0.047130	4.646950
227.364125	7425.248867	14.636147	-0.047082	4.644513
227.198244	7417.241311	14.641152	-0.047046	4.642083
227.308944	7409.209737	14.646157	-0.047061	4.639645
227.067981	7401.246513	14.651162	-0.047011	4.637226
226.975207	7393.167607	14.656167	-0.046988	4.634770
227.321440	7385.193125	14.661171	-0.047047	4.632345
227.170961	7377.156526	14.666176	-0.047014	4.629900
227.130857	7369.239164	14.671181	-0.047002	4.627490
227.084171	7361.211175	14.676186	-0.046988	4.625045
226.906517	7353.214027	14.681191	-0.046949	4.622608
227.061561	7345.185433	14.686195	-0.046973	4.620160
227.084768	7337.166149	14.691200	-0.046972	4.617713
227.064154	7329.181797	14.696205	-0.046963	4.615276
226.904316	7321.184349	14.701210	-0.046928	4.612834
226.880965	7313.151299	14.706215	-0.046918	4.610379
226.997636	7305.232707	14.711219	-0.046935	4.607959
226.735814	7297.158377	14.716224	-0.046881	4.605489
226.809685	7289.200305	14.721229	-0.046889	4.603053
226.792469	7281.195576	14.726234	-0.046881	4.600602
226.658320	7273.201415	14.731239	-0.046851	4.598153
226.656849	7265.219496	14.736243	-0.046845	4.595706
226.561355	7257.139228	14.741248	-0.046822	4.593228
226.686531	7249.103597	14.746253	-0.046840	4.590762
226.513405	7241.145092	14.751258	-0.046803	4.588319
226.378986	7233.093270	14.756263	-0.046772	4.585845
226.674375	7225.176729	14.761267	-0.046822	4.583412
226.524150	7217.127516	14.766272	-0.046789	4.580937
226.369775	7209.155770	14.771277	-0.046755	4.578484
226.444339	7201.186613	14.776282	-0.046764	4.576031
226.266255	7193.125296	14.781287	-0.046725	4.573547
226.277823	7185.130540	14.786291	-0.046722	4.571083
226.202125	7177.113102	14.791296	-0.046703	4.568611
226.543268	7169.088258	14.796301	-0.046761	4.566136
226.115912	7161.137596	14.801306	-0.046676	4.563681
226.204078	7153.144661	14.806311	-0.046687	4.561212
226.209477	7145.153376	14.811315	-0.046683	4.558743
226.048233	7137.130883	14.816320	-0.046648	4.556262
225.988232	7129.149656	14.821325	-0.046632	4.553793
226.171198	7121.115070	14.826330	-0.046660	4.551306
226.080773	7113.091314	14.831335	-0.046638	4.548821
225.966643	7105.118451	14.836339	-0.046612	4.546350
225.753644	7097.107256	14.841344	-0.046567	4.543866
225.946686	7089.150442	14.846349	-0.046598	4.541398
225.964376	7081.135609	14.851354	-0.046596	4.538911
225.735985	7073.165923	14.856359	-0.046548	4.536435
225.895630	7065.139898	14.861363	-0.046572	4.533942
225.941385	7057.100927	14.866368	-0.046576	4.531442
225.844835	7049.060340	14.871373	-0.046552	4.528941
225.708963	7041.146864	14.876378	-0.046522	4.526478
225.517917	7033.120893	14.881383	-0.046481	4.523978
225.754626	7025.173373	14.886387	-0.046520	4.521502
225.576267	7017.108163	14.891392	-0.046481	4.518987
225.822678	7009.180260	14.896397	-0.046522	4.516515
225.701563	7001.107564	14.901402	-0.046494	4.513995
225.475285	6992.975334	14.906407	-0.046447	4.511455
225.486455	6985.034572	14.911411	-0.046444	4.508974
225.594486	6977.069392	14.916416	-0.046459	4.506484
225.619862	6969.059419	14.921421	-0.046458	4.503979
225.437503	6961.096666	14.926426	-0.046419	4.501486
225.517942	6953.058236	14.931431	-0.046429	4.498970
225.527558	6945.134524	14.936435	-0.046425	4.496487
225.320704	6937.081872	14.941440	-0.046381	4.493962
225.431939	6929.039672	14.946445	-0.046397	4.491440
225.364030	6921.057447	14.951450	-0.046379	4.488934
225.003352	6913.045923	14.956455	-0.046307	4.486417
225.112946	6905.075881	14.961459	-0.046322	4.483913
225.150181	6897.083224	14.966464	-0.046323	4.481401
225.286440	6889.047340	14.971469	-0.046344	4.478874
225.055777	6881.075505	14.976474	-0.046295	4.476364
225.077285	6873.040012	14.981479	-0.046294	4.473833
225.063107	6865.028290	14.986483	-0.046286	4.471309
224.898671	6857.034722	14.991488	-0.046250	4.468788
224.952514	6848.997661	14.996493	-0.046255	4.466253
225.010593	6841.060031	15.001498	-0.046261	4.463748
224.874181	6833.046182	15.006503	-0.046230	4.461217
225.033456	6825.073799	15.011507	-0.046255	4.458698
225.069174	6817.035347	15.016512	-0.046256	4.456157
224.971020	6809.026855	15.021517	-0.046232	4.453623
224.785937	6801.011270	15.026522	-0.046193	4.451085
224.969642	6792.997480	15.031527	-0.046222	4.448548
225.008752	6785.030502	15.036531	-0.046224	4.446023
224.537586	6777.006999	15.041536	-0.046131	4.443477
224.692420	6769.030885	15.046541	-0.046154	4.440948
224.907729	6761.022046	15.051546	-0.046189	4.438406
224.693635	6753.016875	15.056551	-0.046144	4.435863
224.517105	6745.012908	15.061555	-0.046106	4.433318
224.494358	6736.926979	15.066560	-0.046096	4.430747
224.342106	6728.962432	15.071565	-0.046063	4.428212
224.456933	6720.994628	15.076570	-0.046079	4.425676
224.453869	6712.981194	15.081575	-0.046073	4.423124
224.392295	6704.992872	15.086579	-0.046057	4.420578
224.227228	6696.992186	15.091584	-0.046021	4.418025
224.267039	6688.982238	15.096589	-0.046023	4.415470
224.296609	6680.993701	15.101594	-0.046023	4.412919
224.271856	6672.934441	15.106599	-0.046013	4.410345
224.236883	6665.010913	15.111603	-0.046001	4.407812
224.165921	6656.950075	15.116608	-0.045983	4.405233
224.321188	6649.015079	15.121613	-0.046007	4.402695
224.014249	6641.001708	15.126618	-0.045944	4.400127
224.055456	6632.996980	15.131623	-0.045947	4.397563
224.257842	6624.990253	15.136627	-0.045979	4.394997
224.014096	6616.976410	15.141632	-0.045928	4.392425
223.902241	6608.974777	15.146637	-0.045902	4.389856
224.021352	6601.002938	15.151642	-0.045919	4.387297
223.817527	6592.945345	15.156647	-0.045876	4.384707
223.868610	6585.060771	15.161651	-0.045880	4.382172
223.820794	6577.026362	15.166656	-0.045866	4.379587
223.752669	6569.023278	15.171661	-0.045848	4.377010
223.683712	6561.003640	15.176666	-0.045830	4.374427
223.758373	6552.991871	15.181671	-0.045839	4.371845
223.827022	6544.998478	15.186675	-0.045846	4.369268
223.669479	6536.966747	15.191680	-0.045812	4.366676
223.519243	6528.920381	15.196685	-0.045779	4.364077
223.649179	6521.006690	15.201690	-0.045798	4.361521
223.491819	6512.974881	15.206695	-0.045763	4.358924
223.589824	6505.045096	15.211699	-0.045776	4.356360
223.528532	6496.931255	15.216704	-0.045759	4.353734
223.522551	6488.882898	15.221709	-0.045753	4.351127
223.457392	6480.953296	15.226714	-0.045736	4.348558
223.340221	6472.936118	15.231719	-0.045709	4.345958
223.398910	6465.019192	15.236723	-0.045714	4.343390
223.259316	6456.986140	15.241728	-0.045683	4.340781
223.333414	6448.970702	15.246733	-0.045692	4.338179
223.426115	6440.969254	15.251738	-0.045704	4.335579
223.209022	6432.960135	15.256743	-0.045658	4.332973
223.156321	6424.929292	15.261747	-0.045643	4.330360
223.112085	6416.942443	15.266752	-0.045629	4.327759
223.287366	6408.947841	15.271757	-0.045657	4.325156
223.186332	6401.020721	15.276762	-0.045633	4.322571
223.038619	6392.972185	15.281767	-0.045600	4.319945
223.080021	6385.001729	15.286771	-0.045603	4.317344
222.932727	6376.930528	15.291776	-0.045570	4.314707
222.694216	6368.910396	15.296781	-0.045520	4.312085
222.776758	6360.900096	15.301786	-0.045530	4.309466
222.866176	6352.901153	15.306791	-0.045542	4.306850
222.762318	6344.957433	15.311795	-0.045517	4.304249
222.622911	6336.946054	15.316800	-0.045486	4.301623
222.819341	6328.949555	15.321805	-0.045517	4.299004
222.721211	6320.948901	15.326810	-0.045494	4.296379
222.595622	6312.896798	15.331815	-0.045465	4.293736
222.833247	6304.904350	15.336819	-0.045504	4.291113
222.561857	6296.914276	15.341824	-0.045448	4.288486
222.453793	6288.937426	15.346829	-0.045423	4.285863
222.533547	6280.967367	15.351834	-0.045433	4.283241
222.583203	6272.928979	15.356839	-0.045437	4.280596
222.564163	6264.966499	15.361843	-0.045428	4.277973
222.439851	6256.938743	15.366848	-0.045399	4.275326
222.345382	6248.887787	15.371853	-0.045377	4.272670
222.272004	6240.873483	15.376858	-0.045358	4.270025
222.269908	6232.883079	15.381863	-0.045352	4.267387
222.386789	6224.867037	15.386867	-0.045369	4.264739
222.174470	6216.930915	15.391872	-0.045324	4.262113
222.012159	6208.869163	15.396877	-0.045288	4.259445
222.152714	6200.945661	15.401882	-0.045309	4.256824
222.076302	6192.907658	15.406887	-0.045290	4.254160
222.119739	6184.954264	15.411891	-0.045293	4.251525
221.805920	6176.893452	15.416896	-0.045229	4.248849
222.142413	6168.902284	15.421901	-0.045286	4.246200
221.983852	6160.929085	15.426906	-0.045252	4.243551
221.787698	6152.955437	15.431911	-0.045210	4.240900
221.970386	6144.977840	15.436915	-0.045239	4.238249
221.810807	6136.973802	15.441920	-0.045204	4.235585
221.726459	6128.920176	15.446925	-0.045183	4.232903
221.698337	6120.910336	15.451930	-0.045172	4.230235
221.785678	6112.898412	15.456935	-0.045183	4.227565
221.715779	6104.930820	15.461939	-0.045165	4.224907
221.482630	6096.935758	15.466944	-0.045116	4.222236
221.589922	6088.904760	15.471949	-0.045131	4.219556
221.651293	6080.992301	15.476954	-0.045137	4.216912
221.428026	6072.898391	15.481959	-0.045091	4.214204
221.515074	6064.925249	15.486963	-0.045101	4.211537
221.482293	6056.929137	15.491968	-0.045090	4.208859
221.425857	6048.924896	15.496973	-0.045074	4.206177
221.629913	6040.942779	15.501978	-0.045107	4.203503
221.477633	6032.941527	15.506983	-0.045074	4.200818
221.530373	6024.972440	15.511987	-0.045078	4.198144
221.368585	6016.955784	15.516992	-0.045043	4.195449
221.572235	6008.849987	15.521997	-0.045075	4.192727
221.624366	6000.830364	15.527002	-0.045080	4.190031
221.226411	5992.870374	15.532007	-0.045001	4.187348
220.936258	5984.881551	15.537011	-0.044941	4.184654
221.169074	5976.923433	15.542016	-0.044979	4.181975
221.054246	5968.903129	15.547021	-0.044953	4.179270
221.022679	5960.941735	15.552026	-0.044942	4.176583
221.122882	5952.915446	15.557031	-0.044955	4.173875
221.071711	5944.896650	15.562035	-0.044940	4.171165
220.974091	5936.877278	15.567040	-0.044917	4.168453
220.855958	5928.873096	15.572045	-0.044890	4.165744
221.162288	5920.951867	15.577050	-0.044942	4.163066
220.849491	5912.905789	15.582055	-0.044878	4.160337
220.955560	5904.939964	15.587059	-0.044893	4.157639
220.940700	5896.913542	15.592064	-0.044884	4.154916
220.664982	5888.857374	15.597069	-0.044828	4.152179
220.746970	5880.855637	15.602074	-0.044838	4.149463
220.668940	5872.890486	15.607079	-0.044818	4.146755
220.696271	5864.905722	15.612083	-0.044818	4.144040
220.604863	5856.915756	15.617088	-0.044796	4.141320
220.633823	5848.891928	15.622093	-0.044796	4.138588
220.840977	5840.922833	15.627098	-0.044829	4.135876
220.619840	5832.849035	15.632103	-0.044783	4.133120
220.628244	5824.860157	15.637107	-0.044779	4.130395
220.517239	5816.900137	15.642112	-0.044753	4.127676
220.278093	5808.874317	15.647117	-0.044703	4.124931
220.530703	5800.934305	15.652122	-0.044745	4.122220
220.439769	5792.868990	15.657127	-0.044723	4.119459
220.509779	5784.950794	15.662131	-0.044731	4.116750
220.198997	5776.912732	15.667136	-0.044668	4.113993
220.241191	5768.880488	15.672141	-0.044670	4.111240
220.348631	5760.837481	15.677146	-0.044685	4.108483
220.169725	5752.853527	15.682151	-0.044647	4.105740
220.181008	5744.917655	15.687155	-0.044643	4.103014
220.052356	5736.909831	15.692160	-0.044614	4.100260
220.117118	5728.911734	15.697165	-0.044621	4.097511
220.068344	5720.911628	15.702170	-0.044607	4.094757
220.025808	5712.865938	15.707175	-0.044594	4.091985
219.969682	5704.877880	15.712179	-0.044578	4.089232
219.928749	5696.935357	15.717184	-0.044565	4.086492
219.977232	5688.917752	15.722189	-0.044569	4.083726
219.788551	5680.964759	15.727194	-0.044529	4.080977
219.777892	5672.973026	15.732199	-0.044521	4.078215
219.749240	5664.942318	15.737203	-0.044511	4.075438
219.705510	5656.915910	15.742208	-0.044497	4.072660
219.627951	5648.883766	15.747213	-0.044478	4.069878
219.511860	5640.962313	15.752218	-0.044451	4.067131
219.692728	5632.898132	15.757223	-0.044479	4.064338
219.818451	5624.953242	15.762227	-0.044497	4.061583
219.555075	5616.948962	15.767232	-0.044443	4.058800
219.337314	5608.928625	15.772237	-0.044397	4.056010
219.654535	5600.934559	15.777242	-0.044451	4.053235
219.424351	5592.900728	15.782247	-0.044403	4.050437
219.343774	5584.967513	15.787251	-0.044383	4.047673
219.424037	5576.934385	15.792256	-0.044392	4.044876
219.659448	5568.945817	15.797261	-0.044431	4.042094
219.544451	5560.943695	15.802266	-0.044404	4.039300
219.355841	5552.978047	15.807271	-0.044364	4.036517
219.228974	5544.901860	15.812275	-0.044335	4.033693
219.177141	5536.817415	15.817280	-0.044320	4.030866
218.983645	5528.892935	15.822285	-0.044279	4.028090
219.208747	5520.878090	15.827290	-0.044316	4.025288
219.277749	5512.896107	15.832295	-0.044323	4.022492
219.040017	5504.930552	15.837299	-0.044274	4.019696
218.919758	5496.957420	15.842304	-0.044246	4.016897
219.089391	5488.899627	15.847309	-0.044273	4.014070
218.878105	5480.908049	15.852314	-0.044228	4.011259
218.707176	5472.913250	15.857319	-0.044191	4.008446
218.812551	5464.876168	15.862323	-0.044205	4.005620
218.863148	5456.942942	15.867328	-0.044209	4.002827
218.687632	5448.911281	15.872333	-0.044172	3.999995
218.843358	5441.017159	15.877338	-0.044195	3.997214
218.583226	5432.946803	15.882343	-0.044142	3.994362
218.544274	5424.917192	15.887347	-0.044129	3.991527
218.494014	5416.885003	15.892352	-0.044114	3.988688
218.512474	5408.889784	15.897357	-0.044113	3.985861
218.275312	5400.963347	15.902362	-0.044063	3.983053
218.226134	5392.928894	15.907367	-0.044049	3.980207
218.323749	5384.983131	15.912371	-0.044062	3.977393
218.256073	5376.956608	15.917376	-0.044044	3.974546
218.268225	5368.937355	15.922381	-0.044041	3.971700
218.587005	5360.887243	15.927386	-0.044095	3.968847
218.399398	5352.896921	15.932391	-0.044055	3.966005
218.370430	5344.971480	15.937395	-0.044044	3.963186
218.398399	5336.969140	15.942400	-0.044044	3.960338
218.251303	5328.983669	15.947405	-0.044012	3.957492
218.365473	5321.008806	15.952410	-0.044028	3.954652
217.993397	5312.930388	15.957415	-0.043953	3.951765
218.218305	5304.933672	15.962419	-0.043990	3.948914
218.228257	5296.951486	15.967424	-0.043986	3.946064
217.843907	5288.966634	15.972429	-0.043910	3.943203
217.929132	5281.005436	15.977434	-0.043920	3.940357
217.976615	5272.989065	15.982439	-0.043924	3.937489
218.072684	5264.998744	15.987443	-0.043937	3.934628
217.930094	5256.960892	15.992448	-0.043905	3.931744
217.888010	5248.980486	15.997453	-0.043892	3.928881
218.030032	5240.989647	16.002458	-0.043913	3.926015
217.707939	5233.002116	16.007463	-0.043848	3.923140
217.725008	5225.007621	16.012467	-0.043846	3.920266
217.806204	5217.014838	16.017472	-0.043855	3.917392
217.822896	5209.000870	16.022477	-0.043853	3.914507
217.889082	5201.007580	16.027482	-0.043860	3.911628
217.684446	5192.942433	16.032487	-0.043817	3.908716
217.532861	5184.967121	16.037491	-0.043784	3.905835
217.408768	5177.004107	16.042496	-0.043755	3.902957
217.579870	5168.983205	16.047501	-0.043782	3.900062
217.578243	5161.030777	16.052506	-0.043776	3.897186
217.280541	5152.983433	16.057511	-0.043716	3.894268
217.438008	5144.981056	16.062515	-0.043740	3.891373
217.512769	5136.985526	16.067520	-0.043748	3.888476
217.409276	5128.945209	16.072525	-0.043724	3.885557
217.332397	5121.025624	16.077530	-0.043704	3.882681
217.229965	5112.974146	16.082535	-0.043680	3.879754
217.228976	5105.034064	16.087539	-0.043675	3.876868
217.141991	5096.940718	16.092544	-0.043653	3.873921
217.387242	5088.745531	16.097549	-0.043693	3.870942
217.342059	5080.872152	16.102554	-0.043680	3.868073
217.067354	5072.870844	16.107559	-0.043623	3.865150
217.217453	5064.960154	16.112563	-0.043646	3.862266
216.904522	5056.974851	16.117568	-0.043583	3.859343
216.981185	5048.967373	16.122573	-0.043592	3.856418
217.085914	5040.987426	16.127578	-0.043606	3.853502
217.112710	5032.930854	16.132583	-0.043606	3.850553
216.937722	5024.980321	16.137587	-0.043568	3.847637
216.888791	5016.972646	16.142592	-0.043554	3.844701
216.787607	5009.036153	16.147597	-0.043530	3.841787
216.724953	5001.034706	16.152602	-0.043513	3.838848
216.553794	4993.082936	16.157607	-0.043476	3.835923
216.891748	4985.041339	16.162611	-0.043533	3.832973
216.771244	4977.018362	16.167616	-0.043506	3.830018
216.679748	4969.053361	16.172621	-0.043483	3.827082
216.582139	4961.016122	16.177626	-0.043460	3.824118
216.543001	4953.077403	16.182631	-0.043447	3.821189
216.544847	4945.090855	16.187635	-0.043443	3.818241
216.469045	4937.103156	16.192640	-0.043423	3.815288
216.584665	4929.058210	16.197645	-0.043439	3.812317
216.588657	4921.064807	16.202650	-0.043435	3.809359
216.559153	4913.082950	16.207655	-0.043424	3.806403
216.527694	4905.113323	16.212659	-0.043413	3.803449
216.518487	4897.125875	16.217664	-0.043406	3.800486
216.301109	4889.115776	16.222669	-0.043360	3.797509
216.228863	4881.100089	16.227674	-0.043342	3.794530
216.124401	4873.052357	16.232679	-0.043317	3.791536
216.160804	4865.057985	16.237683	-0.043319	3.788562
216.033211	4857.039472	16.242688	-0.043290	3.785574
216.028644	4849.066022	16.247693	-0.043283	3.782603
216.085839	4841.089263	16.252698	-0.043289	3.779629
215.873844	4833.090728	16.257703	-0.043244	3.776639
216.010358	4825.116747	16.262707	-0.043264	3.773664
216.022482	4817.045537	16.267712	-0.043261	3.770647
215.886116	4809.078281	16.272717	-0.043231	3.767663
215.901176	4801.073951	16.277722	-0.043228	3.764667
215.815619	4793.103831	16.282727	-0.043207	3.761679
216.000147	4785.146740	16.287731	-0.043236	3.758699
215.710242	4777.124608	16.292736	-0.043177	3.755682
215.598848	4769.126231	16.297741	-0.043151	3.752675
215.831117	4761.099651	16.302746	-0.043189	3.749663
215.561861	4753.102437	16.307751	-0.043134	3.746648
215.545348	4745.129112	16.312755	-0.043125	3.743646
215.593505	4737.103474	16.317760	-0.043129	3.740623
215.447186	4729.147042	16.322765	-0.043097	3.737619
215.259395	4721.156700	16.327770	-0.043056	3.734598
215.167562	4713.119736	16.332775	-0.043034	3.731560
215.412703	4705.135629	16.337779	-0.043075	3.728548
215.305821	4697.158054	16.342784	-0.043049	3.725527
215.504003	4689.151005	16.347789	-0.043081	3.722500
215.569650	4681.177009	16.352794	-0.043088	3.719480
215.047196	4673.233326	16.357799	-0.042986	3.716454
215.049446	4665.168753	16.362803	-0.042981	3.713393
215.111716	4657.078199	16.367808	-0.042987	3.710321
215.275990	4649.091941	16.372813	-0.043012	3.707289
215.047695	4641.150841	16.377818	-0.042965	3.704261
214.842766	4633.173021	16.382823	-0.042921	3.701218
215.118271	4625.177752	16.387827	-0.042967	3.698177
214.942378	4617.201424	16.392832	-0.042929	3.695130
214.746608	4609.200373	16.397837	-0.042888	3.692071
214.849588	4601.200185	16.402842	-0.042902	3.689016
214.937699	4593.185536	16.407847	-0.042913	3.685954
214.928158	4585.241084	16.412851	-0.042906	3.682913
214.688030	4577.233848	16.417856	-0.042856	3.679840
214.496960	4569.263509	16.422861	-0.042815	3.676779
214.601011	4561.249199	16.427866	-0.042829	3.673707
214.560114	4553.206605	16.432871	-0.042816	3.670617
214.610148	4545.206085	16.437875	-0.042820	3.667544
214.568875	4537.199772	16.442880	-0.042807	3.664463
214.391136	4529.234602	16.447885	-0.042769	3.661392
214.494387	4521.246556	16.452890	-0.042783	3.658317
214.480659	4513.226231	16.457895	-0.042775	3.655223
214.151565	4505.273903	16.462899	-0.042709	3.652145
214.295455	4497.243469	16.467904	-0.042730	3.649047
214.253022	4489.220510	16.472909	-0.042717	3.645944
214.211690	4481.283365	16.477914	-0.042704	3.642872
214.082681	4473.261504	16.482919	-0.042675	3.639762
214.237977	4465.321841	16.487923	-0.042699	3.636688
214.264060	4457.270717	16.492928	-0.042698	3.633566
214.071891	4449.228876	16.497933	-0.042657	3.630438
214.344674	4441.262711	16.502938	-0.042703	3.627350
214.265164	4433.245286	16.507943	-0.042683	3.624229
214.210049	4425.309250	16.512947	-0.042667	3.621138
214.143276	4417.290332	16.517952	-0.042650	3.618012
213.985761	4409.288000	16.522957	-0.042615	3.614888
214.200759	4401.311819	16.527962	-0.042650	3.611781
213.860437	4393.300418	16.532967	-0.042581	3.608642
213.893756	4385.330164	16.537971	-0.042582	3.605527
213.928918	4377.345921	16.542976	-0.042584	3.602403
213.700966	4369.351602	16.547981	-0.042536	3.599266
213.543532	4361.411834	16.552986	-0.042501	3.596149
213.617981	4353.359702	16.557991	-0.042510	3.592992
213.515678	4345.368720	16.562995	-0.042486	3.589852
213.545166	4337.377613	16.568000	-0.042486	3.586712
213.641937	4329.373534	16.573005	-0.042499	3.583566
213.649905	4321.393220	16.578010	-0.042495	3.580424
213.329071	4313.420174	16.583015	-0.042430	3.577273
213.417443	4305.409298	16.588019	-0.042441	3.574116
213.680603	4297.374447	16.593024	-0.042485	3.570952
213.332167	4289.405854	16.598029	-0.042415	3.567794
213.363434	4281.396721	16.603034	-0.042415	3.564627
213.356811	4273.419577	16.608039	-0.042409	3.561470
213.307332	4265.448757	16.613043	-0.042394	3.558311
213.246577	4257.443384	16.618048	-0.042378	3.555135
213.320362	4249.318788	16.623053	-0.042386	3.551912
213.234570	4241.359593	16.628058	-0.042365	3.548748
213.157134	4233.359820	16.633063	-0.042345	3.545565
213.105914	4225.414704	16.638067	-0.042331	3.542402
213.268822	4217.403380	16.643072	-0.042356	3.539216
213.102816	4209.427970	16.648077	-0.042320	3.536032
213.033560	4201.433726	16.653082	-0.042302	3.532840
213.022892	4193.425885	16.658087	-0.042294	3.529641
212.971269	4185.465123	16.663091	-0.042280	3.526458
213.022078	4177.426545	16.668096	-0.042284	3.523243
212.806480	4169.465544	16.673101	-0.042238	3.520048
212.857021	4161.514812	16.678106	-0.042243	3.516863
212.761834	4153.496915	16.683111	-0.042220	3.513643
212.838201	4145.484067	16.688115	-0.042229	3.510428
212.826418	4137.517953	16.693120	-0.042221	3.507225
212.609763	4129.514499	16.698125	-0.042176	3.503999
212.762959	4121.534737	16.703130	-0.042199	3.500790
212.745545	4113.530606	16.708135	-0.042190	3.497564
212.725565	4105.544904	16.713139	-0.042181	3.494341
212.551197	4097.540799	16.718144	-0.042144	3.491104
212.528906	4089.523007	16.723149	-0.042134	3.487863
212.521567	4081.567046	16.728154	-0.042128	3.484644
212.296021	4073.622549	16.733159	-0.042081	3.481420
212.447966	4065.611026	16.738163	-0.042104	3.478178
212.510664	4057.596288	16.743168	-0.042110	3.474928
212.395938	4049.547015	16.748173	-0.042083	3.471656
212.365744	4041.567758	16.753178	-0.042073	3.468412
212.434804	4033.558149	16.758183	-0.042080	3.465156
212.401543	4025.597946	16.763187	-0.042069	3.461913
212.335043	4017.624920	16.768192	-0.042051	3.458661
212.206445	4009.627705	16.773197	-0.042022	3.455394
212.396243	4001.628507	16.778202	-0.042052	3.452134
212.077712	3993.607610	16.783207	-0.041987	3.448845
211.745868	3985.651272	16.788211	-0.041920	3.445579
211.945014	3977.653443	16.793216	-0.041952	3.442310
211.942711	3969.628510	16.798221	-0.041947	3.439021
211.957837	3961.687413	16.803226	-0.041944	3.435763
211.534981	3953.678719	16.808231	-0.041860	3.432459
211.644832	3945.657817	16.813235	-0.041875	3.429166
211.725650	3937.683361	16.818240	-0.041885	3.425887
211.568617	3929.673963	16.823245	-0.041851	3.422583
211.882004	3921.675188	16.828250	-0.041904	3.419295
211.690715	3913.718901	16.833255	-0.041863	3.416005
211.513517	3905.722369	16.838259	-0.041825	3.412696
211.632183	3897.701549	16.843264	-0.041842	3.409384
211.521163	3889.738516	16.848269	-0.041816	3.406084
211.446796	3881.774923	16.853274	-0.041797	3.402782
211.468915	3873.748571	16.858279	-0.041796	3.399454
211.532911	3865.804741	16.863283	-0.041802	3.396159
211.500123	3857.739297	16.868288	-0.041791	3.392807
211.460903	3849.674135	16.873293	-0.041778	3.389451
211.376588	3841.764699	16.878298	-0.041757	3.386155
211.179955	3833.766936	16.883303	-0.041716	3.382815
211.114952	3825.785451	16.888307	-0.041698	3.379483
211.374759	3817.836565	16.893312	-0.041741	3.376173
211.264753	3809.785772	16.898317	-0.041716	3.372804
211.088148	3801.788297	16.903322	-0.041678	3.369452
210.944551	3793.847452	16.908327	-0.041646	3.366121
211.129089	3785.820140	16.913331	-0.041675	3.362762
211.192311	3777.850608	16.918336	-0.041681	3.359420
210.970962	3769.912022	16.923341	-0.041635	3.356078
210.951521	3761.884608	16.928346	-0.041626	3.352702
210.842448	3753.844141	16.933351	-0.041600	3.349313
210.742530	3745.882911	16.938355	-0.041577	3.345955
210.880648	3737.888309	16.943360	-0.041597	3.342588
210.685919	3729.878233	16.948365	-0.041556	3.339199
210.606784	3721.951937	16.953370	-0.041536	3.335847
210.651672	3713.909942	16.958375	-0.041539	3.332446
210.887004	3705.865324	16.963379	-0.041577	3.329048
210.784164	3697.945407	16.968384	-0.041553	3.325687
210.526467	3689.953805	16.973389	-0.041500	3.322286
210.866755	3681.960311	16.978394	-0.041558	3.318904
210.690955	3673.998468	16.983399	-0.041520	3.315512
210.483266	3665.997107	16.988403	-0.041476	3.312098
210.624677	3657.956223	16.993408	-0.041497	3.308677
210.446336	3649.971828	16.998413	-0.041459	3.305265
210.248413	3642.047212	17.003418	-0.041417	3.301874
210.125373	3634.052590	17.008423	-0.041388	3.298452
210.171947	3626.048931	17.013427	-0.041392	3.295029
210.082548	3618.061416	17.018432	-0.041370	3.291605
210.033645	3610.030581	17.023437	-0.041356	3.288160
210.018384	3602.066223	17.028442	-0.041348	3.284741
210.108557	3594.094824	17.033447	-0.041359	3.281319
210.115061	3586.098655	17.038451	-0.041355	3.277881
210.004137	3578.093277	17.043456	-0.041329	3.274429
209.709759	3570.113818	17.048461	-0.041269	3.270979
209.827256	3562.150198	17.053466	-0.041286	3.267547
209.750637	3554.092708	17.058471	-0.041266	3.264064
210.002131	3546.119892	17.063475	-0.041308	3.260627
209.929198	3538.162074	17.068480	-0.041289	3.257179
209.592910	3530.158449	17.073485	-0.041221	3.253698
209.780679	3522.147624	17.078490	-0.041251	3.250231
209.766175	3514.168973	17.083495	-0.041243	3.246766
209.638527	3506.184918	17.088499	-0.041214	3.243290
209.797072	3498.200151	17.093504	-0.041238	3.239822
209.759346	3490.217033	17.098509	-0.041226	3.236343
209.670800	3482.217920	17.103514	-0.041204	3.232851
209.589994	3474.185318	17.108519	-0.041184	3.229341
209.421638	3466.192528	17.113523	-0.041147	3.225840
209.395082	3458.221597	17.118528	-0.041137	3.222352
209.323161	3450.232941	17.123533	-0.041119	3.218850
209.378914	3442.275161	17.128538	-0.041124	3.215363
209.350017	3434.273550	17.133543	-0.041113	3.211850
209.289411	3426.289388	17.138547	-0.041097	3.208339
209.147426	3418.303263	17.143552	-0.041065	3.204819
209.095175	3410.330931	17.148557	-0.041050	3.201306
209.301456	3402.349172	17.153562	-0.041083	3.197796
209.087976	3394.348198	17.158567	-0.041038	3.194255
209.156755	3386.332791	17.163571	-0.041046	3.190717
209.030619	3378.384391	17.168576	-0.041017	3.187195
209.048109	3370.378229	17.173581	-0.041015	3.183651
209.089289	3362.388558	17.178586	-0.041018	3.180110
209.171821	3354.396054	17.183591	-0.041028	3.176567
209.002503	3346.397390	17.188595	-0.040991	3.173005
208.842432	3338.402690	17.193600	-0.040956	3.169442
208.762099	3330.429663	17.198605	-0.040936	3.165888
208.723868	3322.463649	17.203610	-0.040923	3.162335
208.812823	3314.469780	17.208615	-0.040935	3.158771
208.827473	3306.473973	17.213619	-0.040932	3.155199
208.774846	3298.474251	17.218624	-0.040917	3.151618
208.561065	3290.469449	17.223629	-0.040872	3.148023
208.526990	3282.498744	17.228634	-0.040860	3.144448
208.446896	3274.528435	17.233639	-0.040840	3.140867
208.411492	3266.540645	17.238643	-0.040829	3.137275
208.406258	3258.559743	17.243648	-0.040822	3.133685
208.476147	3250.518925	17.248653	-0.040830	3.130066
208.389698	3242.583103	17.253658	-0.040809	3.126483
208.269328	3234.619008	17.258663	-0.040781	3.122882
208.094570	3226.617790	17.263667	-0.040743	3.119258
208.136331	3218.683021	17.268672	-0.040746	3.115669
207.989422	3210.648085	17.273677	-0.040713	3.112023
208.038968	3202.655988	17.278682	-0.040717	3.108400
208.025461	3194.628652	17.283687	-0.040710	3.104754
207.982516	3186.680963	17.288691	-0.040696	3.101139
207.879070	3178.709572	17.293696	-0.040672	3.097506
207.936167	3170.689661	17.298701	-0.040677	3.093853
208.178521	3162.674870	17.303706	-0.040717	3.090208
207.942678	3154.730718	17.308711	-0.040668	3.086568
207.840856	3146.736777	17.313715	-0.040644	3.082908
207.917360	3138.771095	17.318720	-0.040653	3.079264
207.721434	3130.822072	17.323725	-0.040611	3.075611
207.764687	3122.734513	17.328730	-0.040614	3.071901
207.706191	3114.742454	17.333735	-0.040598	3.068226
207.481670	3106.785788	17.338739	-0.040551	3.064555
207.665767	3098.824702	17.343744	-0.040580	3.060896
207.560264	3090.823596	17.348749	-0.040555	3.057201
207.494257	3082.859244	17.353754	-0.040537	3.053521
207.322368	3074.858065	17.358759	-0.040500	3.049814
207.372058	3066.888334	17.363763	-0.040504	3.046127
207.639612	3058.896956	17.368768	-0.040549	3.042437
207.587966	3050.905157	17.373773	-0.040534	3.038726
207.432058	3042.974936	17.378778	-0.040500	3.035035
207.303744	3034.967723	17.383783	-0.040471	3.031304
207.198109	3026.966734	17.388787	-0.040446	3.027573
207.093840	3018.994927	17.393792	-0.040421	3.023851
207.248144	3010.979231	17.398797	-0.040445	3.020117
207.155775	3003.057943	17.403802	-0.040422	3.016410
206.952569	2995.052068	17.408807	-0.040379	3.012653
206.858893	2987.028793	17.413811	-0.040356	3.008889
207.062358	2979.058137	17.418816	-0.040389	3.005159
206.928991	2971.094946	17.423821	-0.040359	3.001412
206.939282	2963.120619	17.428826	-0.040356	2.997662
206.850084	2955.135661	17.433831	-0.040334	2.993897
206.850057	2947.096418	17.438835	-0.040329	2.990106
207.001772	2939.124600	17.443840	-0.040352	2.986350
206.929492	2931.141039	17.448845	-0.040333	2.982572
206.836457	2923.192916	17.453850	-0.040310	2.978806
206.812485	2915.198800	17.458855	-0.040301	2.975016
206.555665	2907.229944	17.463859	-0.040248	2.971221
206.650244	2899.231099	17.468864	-0.040260	2.967426
206.582997	2891.257855	17.473869	-0.040242	2.963629
206.526322	2883.295692	17.478874	-0.040226	2.959833
206.599841	2875.310769	17.483879	-0.040235	2.956029
206.466891	2867.314617	17.488883	-0.040205	2.952203
206.345994	2859.332817	17.493888	-0.040177	2.948380
206.139471	2851.342696	17.498893	-0.040134	2.944543
206.292736	2843.380650	17.503898	-0.040157	2.940734
206.227287	2835.406487	17.508903	-0.040139	2.936902
206.093388	2827.400899	17.513907	-0.040109	2.933047
206.246158	2819.400544	17.518912	-0.040132	2.929204
205.984050	2811.441733	17.523917	-0.040078	2.925354
205.999190	2803.463168	17.528922	-0.040076	2.921504
205.977288	2795.491430	17.533927	-0.040067	2.917651
206.038861	2787.487533	17.538931	-0.040073	2.913781
206.008821	2779.419329	17.543936	-0.040062	2.909870
205.855285	2771.455349	17.548941	-0.040028	2.905998
205.839542	2763.516380	17.553946	-0.040020	2.902140
205.826441	2755.533812	17.558951	-0.040012	2.898256
205.791248	2747.564402	17.563955	-0.040001	2.894372
205.899996	2739.566695	17.568960	-0.040016	2.890476
205.761942	2731.606535	17.573965	-0.039985	2.886581
205.492560	2723.648871	17.578970	-0.039929	2.882674
205.548934	2715.670861	17.583975	-0.039935	2.878770
205.685983	2707.674902	17.588979	-0.039955	2.874856
205.390307	2699.718550	17.593984	-0.039895	2.870932
205.324691	2691.706178	17.598989	-0.039877	2.866988
205.529954	2683.730795	17.603994	-0.039910	2.863072
205.465260	2675.761821	17.608999	-0.039893	2.859138
205.314857	2667.781929	17.614003	-0.039860	2.855189
205.425690	2659.779851	17.619008	-0.039875	2.851238
205.531479	2651.778036	17.624013	-0.039890	2.847282
205.378423	2643.848723	17.629018	-0.039856	2.843341
205.138776	2635.895085	17.634023	-0.039806	2.839378
205.045681	2627.945418	17.639027	-0.039784	2.835420
205.066700	2619.911198	17.644032	-0.039782	2.831420
204.921088	2611.902337	17.649037	-0.039750	2.827418
204.945540	2603.939174	17.654042	-0.039749	2.823443
204.877219	2595.954793	17.659047	-0.039731	2.819446
204.768062	2588.005768	17.664051	-0.039706	2.815459
204.702984	2580.015719	17.669056	-0.039688	2.811448
204.667627	2572.014428	17.674061	-0.039676	2.807427
204.605195	2564.061856	17.679066	-0.039660	2.803424
204.667323	2556.079036	17.684071	-0.039666	2.799407
204.589215	2548.121391	17.689075	-0.039646	2.795389
204.737393	2540.119358	17.694080	-0.039669	2.791355
204.513879	2532.155924	17.699085	-0.039622	2.787314
204.678186	2524.156601	17.704090	-0.039647	2.783271
204.612414	2516.199912	17.709095	-0.039630	2.779231
204.523889	2508.235993	17.714099	-0.039608	2.775179
204.471164	2500.260560	17.719104	-0.039593	2.771118
204.503111	2492.240405	17.724109	-0.039594	2.767033
204.298853	2484.310510	17.729114	-0.039550	2.762975
204.132198	2476.351948	17.734119	-0.039514	2.758897
204.265012	2468.360873	17.739123	-0.039534	2.754815
204.216018	2460.296480	17.744128	-0.039519	2.750679
203.995002	2452.326533	17.749133	-0.039473	2.746574
204.060430	2444.359032	17.754138	-0.039480	2.742481
204.023835	2436.400925	17.759143	-0.039468	2.738382
204.068664	2428.420294	17.764147	-0.039471	2.734269
203.894112	2420.461394	17.769152	-0.039433	2.730148
203.868716	2412.484797	17.774157	-0.039423	2.726021
203.853881	2404.533489	17.779162	-0.039415	2.721901
203.708031	2396.581602	17.784167	-0.039383	2.717766
203.603362	2388.600349	17.789171	-0.039358	2.713613
203.669126	2380.596575	17.794176	-0.039365	2.709452
203.554069	2372.608191	17.799181	-0.039339	2.705281
203.630117	2364.652857	17.804186	-0.039347	2.701133
203.538898	2356.702377	17.809191	-0.039325	2.696971
203.510538	2348.715534	17.814195	-0.039315	2.692787
203.288461	2340.768073	17.819200	-0.039268	2.688605
203.068175	2332.795467	17.824205	-0.039222	2.684404
203.237301	2324.807878	17.829210	-0.039248	2.680212
203.258900	2316.847618	17.834215	-0.039247	2.676020
203.080783	2308.844278	17.839219	-0.039209	2.671785
203.278639	2300.851654	17.844224	-0.039240	2.667573
203.330835	2292.850987	17.849229	-0.039245	2.663340
203.069152	2284.931910	17.854234	-0.039191	2.659125
202.972038	2276.966654	17.859239	-0.039167	2.654888
202.855866	2268.967238	17.864243	-0.039141	2.650625
203.002534	2261.007361	17.869248	-0.039163	2.646394
202.898568	2253.027489	17.874253	-0.039138	2.642128
203.075895	2245.054551	17.879258	-0.039166	2.637879
202.863601	2237.115270	17.884263	-0.039121	2.633614
202.769956	2229.120518	17.889267	-0.039099	2.629321
202.746807	2221.164426	17.894272	-0.039089	2.625046
202.587671	2213.205960	17.899277	-0.039054	2.620753
202.798945	2205.223378	17.904282	-0.039088	2.616466
202.766111	2197.246213	17.909287	-0.039077	2.612158
202.823086	2189.249994	17.914291	-0.039082	2.607838
202.582129	2181.333475	17.919296	-0.039032	2.603535
202.448680	2173.363866	17.924301	-0.039002	2.599203
202.589231	2165.400365	17.929306	-0.039023	2.594885
202.444108	2157.218136	17.934311	-0.038991	2.590422
202.176294	2149.299184	17.939315	-0.038936	2.586086
202.404092	2141.352300	17.944320	-0.038973	2.581761
202.256615	2133.416163	17.949325	-0.038940	2.577410
202.164599	2125.472583	17.954330	-0.038918	2.573050
202.203354	2117.483402	17.959335	-0.038920	2.568668
202.072337	2109.533809	17.964339	-0.038890	2.564288
202.062045	2101.609503	17.969344	-0.038883	2.559922
202.162631	2093.630676	17.974349	-0.038897	2.555527
202.143535	2085.654451	17.979354	-0.038888	2.551117
201.970041	2077.688824	17.984359	-0.038850	2.546695
202.002398	2069.723591	17.989363	-0.038851	2.542280
201.914367	2061.797901	17.994368	-0.038830	2.537870
201.947297	2053.792688	17.999373	-0.038830	2.533417
201.799905	2045.832129	18.004378	-0.038798	2.528969
201.681441	2037.870230	18.009383	-0.038771	2.524513
201.618060	2029.926540	18.014387	-0.038754	2.520064
201.629500	2021.979512	18.019392	-0.038750	2.515611
201.425596	2013.982020	18.024397	-0.038707	2.511106
201.650227	2005.982344	18.029402	-0.038744	2.506622
201.671367	1998.018380	18.034407	-0.038743	2.502136
201.379542	1990.084523	18.039411	-0.038683	2.497636
201.457197	1982.104099	18.044416	-0.038692	2.493129
201.485858	1974.109716	18.049421	-0.038692	2.488601
201.306594	1966.187063	18.054426	-0.038654	2.484091
201.125105	1958.252587	18.059431	-0.038615	2.479566
201.157987	1950.279890	18.064435	-0.038616	2.475027
201.130529	1942.315993	18.069440	-0.038605	2.470480
200.929487	1934.339240	18.074445	-0.038563	2.465904
200.905194	1926.388066	18.079450	-0.038553	2.461347
200.884225	1918.430536	18.084455	-0.038544	2.456779
200.822318	1910.462531	18.089459	-0.038527	2.452193
201.048907	1902.471853	18.094464	-0.038564	2.447607
200.920591	1894.502677	18.099469	-0.038535	2.442998
200.855565	1886.583702	18.104474	-0.038518	2.438414
200.845467	1878.600262	18.109479	-0.038511	2.433788
200.741827	1870.564553	18.114483	-0.038486	2.429116
200.832328	1862.607983	18.119488	-0.038498	2.424496
200.695804	1854.670890	18.124493	-0.038467	2.419861
200.674606	1846.741266	18.129498	-0.038458	2.415230
200.580935	1838.776490	18.134503	-0.038435	2.410564
200.149221	1830.858587	18.139507	-0.038350	2.405890
200.162764	1822.902064	18.144512	-0.038347	2.401220
200.411602	1814.913443	18.149517	-0.038388	2.396539
200.170459	1806.971598	18.154522	-0.038338	2.391839
200.322262	1798.978149	18.159527	-0.038361	2.387130
200.334702	1791.026154	18.164531	-0.038358	2.382425
200.246113	1783.098937	18.169536	-0.038336	2.377717
200.168534	1775.128771	18.174541	-0.038317	2.372975
200.109307	1767.173416	18.179546	-0.038301	2.368234
199.824922	1759.246848	18.184551	-0.038242	2.363483
199.905801	1751.281363	18.189555	-0.038252	2.358728
200.048265	1743.310015	18.194560	-0.038274	2.353965
200.004124	1735.314734	18.199565	-0.038260	2.349163
199.836447	1727.382382	18.204570	-0.038224	2.344379
199.626347	1719.463801	18.209575	-0.038179	2.339590
199.579548	1711.501922	18.214579	-0.038165	2.334778
199.650321	1703.519085	18.219584	-0.038173	2.329953
199.430645	1695.581770	18.224589	-0.038127	2.325122
199.522666	1687.625215	18.229594	-0.038139	2.320295
199.499882	1679.706984	18.234599	-0.038130	2.315472
199.330326	1671.735133	18.239603	-0.038093	2.310593
199.008963	1663.819644	18.244608	-0.038028	2.305726
199.247228	1655.805578	18.249613	-0.038067	2.300835
199.065651	1647.892497	18.254618	-0.038028	2.295961
198.972805	1639.927611	18.259623	-0.038006	2.291051
198.953256	1631.957356	18.264627	-0.037997	2.286134
199.005597	1624.027378	18.269632	-0.038001	2.281238
198.786274	1616.097799	18.274637	-0.037955	2.276308
198.839603	1608.080221	18.279642	-0.037960	2.271336
198.875684	1600.095575	18.284647	-0.037961	2.266372
198.743920	1592.164687	18.289651	-0.037932	2.261416
198.703882	1584.228530	18.294656	-0.037919	2.256454
198.670941	1576.259304	18.299661	-0.037908	2.251461
198.556406	1568.323610	18.304666	-0.037881	2.246470
198.515127	1560.390184	18.309671	-0.037868	2.241477
198.568700	1552.452787	18.314675	-0.037873	2.236478
198.587663	1544.493506	18.319680	-0.037871	2.231451
198.199346	1536.575476	18.324685	-0.037794	2.226402
198.292668	1528.613723	18.329690	-0.037806	2.221357
198.495234	1520.656586	18.334695	-0.037838	2.216314
198.359201	1512.702934	18.339699	-0.037808	2.211230
198.239485	1504.788044	18.344704	-0.037780	2.206162
198.235294	1496.834703	18.349709	-0.037774	2.201067
198.141910	1488.922566	18.354714	-0.037752	2.195979
198.076410	1480.955575	18.359719	-0.037734	2.190846
197.870631	1473.000086	18.364723	-0.037691	2.185696
198.001632	1465.055250	18.369728	-0.037710	2.180571
197.886305	1457.117781	18.374733	-0.037683	2.175417
197.849818	1449.162293	18.379738	-0.037671	2.170246
197.813925	1441.220904	18.384743	-0.037660	2.165071
197.568859	1433.321894	18.389747	-0.037609	2.159893
197.483910	1425.406489	18.394752	-0.037588	2.154706
197.468871	1417.423645	18.399757	-0.037580	2.149468
197.523454	1409.478498	18.404762	-0.037585	2.144250
197.339973	1401.559097	18.409767	-0.037545	2.139013
197.333784	1393.607790	18.414771	-0.037539	2.133759
197.668916	1385.623916	18.419776	-0.037596	2.128503
197.356001	1377.731198	18.424781	-0.037533	2.123233
197.332828	1369.811833	18.429786	-0.037523	2.117959
197.243435	1361.859835	18.434791	-0.037501	2.112644
197.236145	1353.856133	18.439795	-0.037495	2.107289
197.171394	1345.944771	18.444800	-0.037478	2.101977
197.111115	1338.012906	18.449805	-0.037461	2.096638
197.136676	1330.077250	18.454810	-0.037461	2.091291
196.888098	1322.178848	18.459815	-0.037409	2.085929
196.916748	1314.236195	18.464819	-0.037409	2.080550
196.940096	1306.315270	18.469824	-0.037409	2.075171
196.980874	1298.347064	18.474829	-0.037411	2.069748
196.851985	1290.436803	18.479834	-0.037382	2.064333
196.754347	1282.520259	18.484839	-0.037358	2.058903
196.656262	1274.588837	18.489843	-0.037335	2.053448
196.635143	1266.659102	18.494848	-0.037326	2.047988
196.704470	1258.707862	18.499853	-0.037333	2.042507
196.419710	1250.836260	18.504858	-0.037275	2.037031
196.475430	1242.880402	18.509863	-0.037280	2.031516
196.172680	1234.954119	18.514867	-0.037219	2.025970
196.394739	1227.000433	18.519872	-0.037255	2.020444
196.232709	1219.090098	18.524877	-0.037220	2.014893
195.973606	1211.189812	18.529882	-0.037166	2.009323
195.989478	1203.252690	18.534887	-0.037164	2.003741
195.942835	1195.332340	18.539891	-0.037150	1.998149
196.064776	1187.397669	18.544896	-0.037168	1.992548
195.841667	1179.486858	18.549901	-0.037121	1.986913
195.918002	1171.557982	18.554906	-0.037130	1.981279
195.805880	1163.647996	18.559911	-0.037104	1.975624
195.665147	1155.712061	18.564915	-0.037072	1.969930
195.797474	1147.800462	18.569920	-0.037092	1.964267
195.553054	1139.915322	18.574925	-0.037041	1.958566
195.512685	1131.979964	18.579930	-0.037029	1.952833
195.367388	1124.034568	18.584935	-0.036996	1.947066
195.391551	1116.101718	18.589939	-0.036996	1.941308
195.246385	1108.208629	18.594944	-0.036963	1.935544
194.987435	1100.301871	18.599949	-0.036910	1.929741
195.115922	1092.364673	18.604954	-0.036929	1.923940
195.165524	1084.457464	18.609959	-0.036933	1.918135
194.994311	1076.555074	18.614963	-0.036896	1.912291
195.206850	1068.604078	18.619968	-0.036930	1.906436
194.974164	1060.720005	18.624973	-0.036882	1.900563
194.799375	1052.843505	18.629978	-0.036844	1.894684
194.702044	1044.925281	18.634983	-0.036821	1.888764
194.628876	1037.015968	18.639987	-0.036802	1.882835
194.712810	1029.116579	18.644992	-0.036812	1.876912
194.717598	1021.172786	18.649997	-0.036808	1.870929
194.699913	1013.249756	18.655002	-0.036799	1.864939
194.605938	1005.375752	18.660007	-0.036777	1.858958
194.459625	997.473476	18.665011	-0.036744	1.852930
194.416336	989.571607	18.670016	-0.036731	1.846895
194.531467	981.651496	18.675021	-0.036747	1.840845
194.283667	973.803948	18.680026	-0.036696	1.834787
194.317829	965.881061	18.685031	-0.036697	1.828685
194.144427	957.982477	18.690035	-0.036660	1.822557
194.088833	950.108264	18.695040	-0.036644	1.816441
193.993857	942.190799	18.700045	-0.036621	1.810265
194.080634	934.283849	18.705050	-0.036632	1.804099
193.942988	926.424454	18.710055	-0.036602	1.797922
194.054222	918.468566	18.715059	-0.036617	1.791677
194.098327	910.537857	18.720064	-0.036620	1.785423
193.842781	902.687727	18.725069	-0.036567	1.779173
193.806497	894.801839	18.730074	-0.036555	1.772901
193.740846	886.915411	18.735079	-0.036538	1.766601
193.768085	879.024143	18.740083	-0.036538	1.760287
193.678173	871.175536	18.745088	-0.036516	1.753970
193.430643	863.292165	18.750093	-0.036465	1.747582
193.413604	855.405561	18.755098	-0.036456	1.741197
193.654177	847.491541	18.760103	-0.036496	1.734799
193.329006	839.642496	18.765107	-0.036430	1.728358
193.310182	831.782821	18.770112	-0.036422	1.721924
193.049199	823.929328	18.775117	-0.036368	1.715439
192.983250	816.023233	18.780122	-0.036351	1.708911
193.209052	808.111875	18.785127	-0.036387	1.702392
193.065998	800.247731	18.790131	-0.036356	1.695839
193.152455	792.353685	18.795136	-0.036367	1.689266
192.860510	784.521473	18.800141	-0.036307	1.682669
192.869215	776.659772	18.805146	-0.036304	1.676061
192.914989	768.772363	18.810151	-0.036307	1.669410
192.590557	760.940351	18.815155	-0.036241	1.662729
192.567568	753.091950	18.820160	-0.036232	1.656049
192.533013	745.198608	18.825165	-0.036220	1.649301
192.533575	737.339205	18.830170	-0.036215	1.642559
192.352213	729.514457	18.835175	-0.036176	1.635795
192.373047	721.578215	18.840179	-0.036175	1.628934
192.133329	713.753420	18.845184	-0.036125	1.622104
192.129410	705.883089	18.850189	-0.036119	1.615239
192.178310	698.015809	18.855194	-0.036123	1.608354
192.280510	690.156179	18.860199	-0.036137	1.601455
191.923325	682.363021	18.865203	-0.036066	1.594518
191.999552	674.491141	18.870208	-0.036075	1.587544
191.854328	666.652162	18.875213	-0.036042	1.580536
191.723338	658.840864	18.880218	-0.036013	1.573524
191.647672	650.994032	18.885223	-0.035994	1.566456
191.612305	643.152826	18.890227	-0.035982	1.559368
191.600855	635.316073	18.895232	-0.035975	1.552254
191.291977	627.490103	18.900237	-0.035912	1.545074
191.480441	619.632476	18.905242	-0.035942	1.537905
191.471751	611.792960	18.910247	-0.035935	1.530689
191.249218	603.990588	18.915251	-0.035889	1.523442
191.219607	596.185545	18.920256	-0.035878	1.516186
191.124125	588.352642	18.925261	-0.035855	1.508860
191.176127	580.516131	18.930266	-0.035860	1.501517
191.065759	572.722198	18.935271	-0.035834	1.494153
190.803682	564.919220	18.940275	-0.035780	1.486721
191.071847	557.082525	18.945280	-0.035825	1.479301
190.567613	549.310991	18.950285	-0.035726	1.471786
190.718316	541.437493	18.955290	-0.035749	1.464237
190.726662	533.637210	18.960295	-0.035745	1.456697
190.635115	525.828909	18.965299	-0.035723	1.449094
190.581692	518.049256	18.970304	-0.035708	1.441485
190.619873	510.246702	18.975309	-0.035710	1.433828
190.383577	502.477066	18.980314	-0.035661	1.426118
190.066520	494.745890	18.985319	-0.035597	1.418391
190.109634	486.926255	18.990323	-0.035600	1.410592
190.280900	479.120546	18.995328	-0.035627	1.402786
190.045379	471.380078	19.000333	-0.035578	1.394933
190.028624	463.573293	19.005338	-0.035570	1.387006
189.929657	455.811741	19.010343	-0.035546	1.379065
189.703103	448.057924	19.015347	-0.035499	1.371064
189.740982	440.289201	19.020352	-0.035501	1.363047
189.589524	432.547251	19.025357	-0.035467	1.354977
189.562638	424.779466	19.030362	-0.035457	1.346853
189.392163	417.051366	19.035367	-0.035421	1.338696
189.330189	409.289784	19.040371	-0.035404	1.330473
189.198694	401.566283	19.045376	-0.035374	1.322227
188.985583	393.822978	19.050381	-0.035330	1.313894
188.840844	385.987577	19.055386	-0.035298	1.305420
188.962958	378.243042	19.060391	-0.035315	1.297038
188.845010	370.518970	19.065395	-0.035288	1.288580
188.729392	362.829232	19.070400	-0.035262	1.280104
188.639704	355.118574	19.075405	-0.035240	1.271553
188.698814	347.388118	19.080410	-0.035246	1.262951
188.591273	339.707450	19.085415	-0.035221	1.254313
188.446899	332.014706	19.090419	-0.035189	1.245595
188.484770	324.326857	19.095424	-0.035191	1.236857
188.233971	316.643824	19.100429	-0.035139	1.228005
187.984252	308.988975	19.105434	-0.035088	1.219122
187.967188	301.304208	19.110439	-0.035079	1.210184
187.946459	293.618551	19.115443	-0.035070	1.201179
187.997355	285.955673	19.120448	-0.035075	1.192147
187.759595	278.316019	19.125453	-0.035026	1.183014
187.795526	270.654669	19.130458	-0.035027	1.173841
187.641095	263.028471	19.135463	-0.034994	1.164599
187.357702	255.432532	19.140467	-0.034936	1.155293
187.416919	247.742389	19.145472	-0.034942	1.145867
187.260813	240.134609	19.150477	-0.034908	1.136419
187.021137	232.540976	19.155482	-0.034858	1.126892
186.954106	224.947713	19.160487	-0.034841	1.117322
186.973342	217.321978	19.165491	-0.034839	1.107646
186.623757	209.790124	19.170496	-0.034769	1.097924
186.708642	202.173282	19.175501	-0.034780	1.088102
186.629769	194.613778	19.180506	-0.034760	1.078229
186.463328	187.062006	19.185511	-0.034724	1.068255
185.978330	179.573319	19.190515	-0.034629	1.058197
186.097110	171.999045	19.195520	-0.034646	1.048068
186.011081	164.470642	19.200525	-0.034625	1.037854
185.740041	156.983047	19.205530	-0.034570	1.027551
185.687327	149.476039	19.210535	-0.034555	1.017168
185.586110	141.975533	19.215539	-0.034532	1.006676
185.375208	134.533076	19.220544	-0.034487	0.996129
185.092017	127.051354	19.225549	-0.034430	0.985394
184.878511	119.615489	19.230554	-0.034385	0.974625
184.445754	112.227340	19.235559	-0.034300	0.963750
183.724735	104.899598	19.240563	-0.034161	0.952764
183.503355	97.494242	19.245568	-0.034115	0.941665
182.668123	90.208038	19.250573	-0.033954	0.930452
181.979975	82.901282	19.255578	-0.033821	0.919108
181.147900	75.614975	19.260583	-0.033662	0.907616
180.328527	68.345094	19.265587	-0.033504	0.896005
179.667150	61.293881	19.270592	-0.033377	0.884634