Fri Mar 12 13:16:12 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.224062	0.143192	0.000000	0.000022	0.720794

0.354198	0.114151	0.005005	-0.000002	0.720782
0.455392	-0.020798	0.010010	-0.000021	0.720552
0.392658	-0.010178	0.015014	-0.000009	0.720551
0.306958	0.002311	0.020019	0.000007	0.720545
0.429632	-0.015884	0.025024	-0.000016	0.720553
0.177754	0.023543	0.030029	0.000031	0.720542
0.369716	-0.005881	0.035034	-0.000005	0.720551
0.561883	-0.039663	0.040038	-0.000040	0.720552
0.407755	-0.015582	0.045043	-0.000012	0.720545
0.255153	0.016869	0.050048	0.000017	0.720555
0.282772	0.006563	0.055053	0.000012	0.720545
0.195586	0.025422	0.060058	0.000028	0.720551
0.157333	0.032634	0.065062	0.000035	0.720552
0.219728	0.019148	0.070067	0.000024	0.720547
0.298817	0.004987	0.075072	0.000009	0.720547
0.196525	-0.138151	0.080077	0.000028	0.720229
0.153941	-0.127592	0.085082	0.000036	0.720235
0.169107	-0.130963	0.090086	0.000033	0.720234
0.290096	-0.155042	0.095091	0.000011	0.720228
0.282954	-0.148853	0.100096	0.000012	0.720238
0.287314	-0.155015	0.105101	0.000012	0.720227
0.399237	-0.233191	0.110106	-0.000009	0.720113
0.153210	-0.292017	0.115110	0.000037	0.719910
0.136441	-0.292552	0.120115	0.000040	0.719903
0.007494	-0.263960	0.125120	0.000064	0.719914
0.001255	-0.267955	0.130125	0.000065	0.719904
-0.009247	-0.275786	0.135130	0.000067	0.719885
0.146315	-0.441653	0.140134	0.000038	0.719612
0.109862	-0.439473	0.145139	0.000045	0.719604
0.226375	-0.453647	0.150144	0.000023	0.719617
0.047755	-0.427653	0.155149	0.000057	0.719605
0.297639	-0.592891	0.160154	0.000010	0.719367
0.280013	-0.634194	0.165158	0.000014	0.719279
0.188342	-0.619407	0.170163	0.000031	0.719276
0.316428	-0.649458	0.175168	0.000007	0.719262
0.062312	-0.753083	0.180173	0.000054	0.718968
-0.176194	-0.709533	0.185178	0.000099	0.718970
-0.155566	-0.714509	0.190182	0.000095	0.718967
-0.204612	-0.787764	0.195187	0.000104	0.718806
-0.367412	-0.834729	0.200192	0.000135	0.718656
-0.203705	-0.869814	0.205197	0.000104	0.718644
-0.119477	-0.900944	0.210202	0.000089	0.718612
-0.000771	-1.048424	0.215206	0.000067	0.718362
0.012895	-1.055400	0.220211	0.000064	0.718353
0.174590	-1.112533	0.225216	0.000034	0.718297
-0.095515	-1.206194	0.230221	0.000085	0.718017
-0.114409	-1.199506	0.235226	0.000088	0.718024
0.019610	-1.289065	0.240230	0.000063	0.717894
0.104365	-1.400600	0.245235	0.000048	0.717703
-0.136587	-1.351361	0.250240	0.000093	0.717715
-0.085341	-1.495432	0.255245	0.000083	0.717449
-0.232684	-1.499538	0.260250	0.000111	0.717389
-0.711066	-1.446255	0.265254	0.000200	0.717325
-0.673322	-1.572499	0.270259	0.000193	0.717089
-0.363556	-1.622464	0.275264	0.000135	0.717099
-0.271114	-1.752104	0.280269	0.000118	0.716875
-0.489123	-1.768403	0.285274	0.000159	0.716766
-0.554774	-1.795350	0.290278	0.000171	0.716689
-0.489321	-1.927647	0.295283	0.000159	0.716450
-0.234957	-1.967395	0.300288	0.000112	0.716461
-0.356519	-2.107597	0.305293	0.000134	0.716141
-0.396339	-2.099948	0.310298	0.000142	0.716142
-1.248934	-2.049628	0.315302	0.000301	0.715940
-2.158351	-1.914800	0.320307	0.000470	0.715886
-1.915821	-1.995494	0.325312	0.000425	0.715812
-3.245491	-1.890801	0.330317	0.000672	0.715550
-2.804176	-1.967171	0.335322	0.000590	0.715554
-3.059446	-1.956176	0.340326	0.000638	0.715486
-4.259111	-1.868435	0.345331	0.000861	0.715236
-3.609630	-1.981223	0.350336	0.000741	0.715242
-4.063779	-1.903580	0.355341	0.000825	0.715235
-4.640940	-1.944426	0.360346	0.000933	0.714950
-4.819359	-1.929353	0.365350	0.000966	0.714917
-5.056578	-1.890392	0.370355	0.001010	0.714910
-4.421086	-2.037188	0.375360	0.000892	0.714843
-6.242662	-1.828971	0.380365	0.001231	0.714612
-6.007316	-1.869637	0.385370	0.001187	0.714615
-5.921070	-1.885156	0.390374	0.001171	0.714614
-6.166183	-1.843646	0.395379	0.001217	0.714610
-5.883732	-2.014474	0.400384	0.001164	0.714371
-6.943050	-1.871092	0.405389	0.001362	0.714281
-6.953350	-1.867249	0.410394	0.001364	0.714284
-6.458745	-1.954774	0.415398	0.001272	0.714286
-6.934256	-1.890054	0.420403	0.001360	0.714246
-7.313006	-1.956568	0.425408	0.001431	0.713979
-7.679584	-1.894789	0.430413	0.001499	0.713972
-8.035563	-1.829674	0.435418	0.001565	0.713976
-7.406117	-1.938829	0.440422	0.001448	0.713981
-7.919860	-1.852048	0.445427	0.001544	0.713972
-8.311136	-1.930761	0.450432	0.001617	0.713677
-8.607261	-1.889265	0.455437	0.001672	0.713654
-8.834672	-1.846546	0.460442	0.001714	0.713659
-8.815061	-1.848309	0.465446	0.001711	0.713662
-8.919236	-1.832571	0.470451	0.001730	0.713656
-8.554163	-1.912842	0.475456	0.001662	0.713626
-9.391993	-1.897045	0.480461	0.001818	0.713360
-9.542881	-1.867725	0.485466	0.001846	0.713365
-9.112432	-1.942256	0.490470	0.001766	0.713369
-9.273823	-1.918128	0.495475	0.001796	0.713360
-9.277023	-1.913630	0.500480	0.001797	0.713368
-9.562475	-1.936884	0.505485	0.001850	0.713220
-10.633382	-1.842257	0.510490	0.002050	0.713029
-10.248730	-1.911494	0.515494	0.001978	0.713027
-10.521951	-1.866182	0.520499	0.002029	0.713021
-10.181267	-1.919977	0.525504	0.001966	0.713034
-10.530611	-1.861690	0.530509	0.002031	0.713026
-10.378248	-1.895540	0.535514	0.002002	0.713013
-10.678152	-1.989930	0.540518	0.002058	0.712719
-11.573070	-1.834038	0.545523	0.002225	0.712711
-11.671058	-1.812106	0.550528	0.002243	0.712720
-11.078508	-1.920661	0.555533	0.002133	0.712714
-11.158453	-1.904688	0.560538	0.002148	0.712718
-11.520229	-1.839557	0.565542	0.002215	0.712719
-11.388912	-1.935547	0.570547	0.002191	0.712574
-11.995490	-1.918461	0.575552	0.002304	0.712393
-12.395934	-1.849809	0.580557	0.002379	0.712387
-12.465606	-1.835941	0.585562	0.002392	0.712390
-12.066780	-1.905904	0.590566	0.002317	0.712392
-12.166732	-1.891539	0.595571	0.002336	0.712385
-12.124780	-1.894229	0.600576	0.002328	0.712395
-12.360856	-1.959275	0.605581	0.002372	0.712181
-13.141969	-1.865054	0.610586	0.002518	0.712092
-12.956568	-1.894914	0.615590	0.002483	0.712098
-13.050236	-1.882293	0.620595	0.002501	0.712090
-12.942175	-1.898254	0.625600	0.002481	0.712096
-13.182886	-1.858218	0.630605	0.002526	0.712090
-13.388671	-1.820959	0.635610	0.002564	0.712091
-13.304465	-1.976814	0.640614	0.002548	0.711811
-14.274638	-1.829264	0.645619	0.002729	0.711760
-14.423202	-1.797033	0.650624	0.002757	0.711771
-13.944645	-1.887549	0.655629	0.002668	0.711761
-13.948194	-1.885191	0.660634	0.002668	0.711764
-14.217225	-1.835760	0.665638	0.002718	0.711767
-14.271055	-1.830706	0.670643	0.002728	0.711758
-13.784169	-2.004084	0.675648	0.002638	0.711585
-14.980899	-1.855754	0.680653	0.002861	0.711456
-14.981620	-1.854761	0.685658	0.002861	0.711457
-14.599215	-1.919965	0.690662	0.002790	0.711463
-14.862689	-1.877863	0.695667	0.002839	0.711453
-14.868574	-1.872389	0.700672	0.002840	0.711462
-14.994073	-1.852370	0.705677	0.002863	0.711457
-15.333774	-1.915423	0.710682	0.002927	0.711211
-15.887696	-1.848981	0.715686	0.003030	0.711146
-16.243564	-1.789395	0.720691	0.003096	0.711138
-15.489682	-1.920329	0.725696	0.002956	0.711145
-15.919938	-1.845414	0.730701	0.003036	0.711142
-16.268298	-1.783646	0.735706	0.003101	0.711141
-15.333715	-1.947680	0.740710	0.002927	0.711146
-15.796151	-1.942704	0.745715	0.003013	0.710991
-16.864176	-1.808877	0.750720	0.003212	0.710878
-16.508781	-1.876858	0.755725	0.003146	0.710869
-16.246136	-1.920374	0.760730	0.003097	0.710875
-16.443291	-1.883360	0.765734	0.003134	0.710879
-16.933685	-1.801167	0.770739	0.003225	0.710869
-16.463405	-1.880119	0.775744	0.003138	0.710878
-16.842076	-1.954059	0.780749	0.003208	0.710596
-17.912634	-1.795477	0.785754	0.003408	0.710531
-17.240754	-1.912158	0.790758	0.003283	0.710537
-17.328215	-1.899968	0.795763	0.003299	0.710531
-17.471919	-1.870408	0.800768	0.003326	0.710538
-17.487456	-1.870175	0.805773	0.003329	0.710533
-17.335182	-1.897386	0.810778	0.003300	0.710533
-17.834612	-1.962856	0.815782	0.003393	0.710224
-18.401564	-1.867596	0.820787	0.003499	0.710213
-18.116718	-1.912222	0.825792	0.003446	0.710225
-18.088512	-1.919823	0.830797	0.003441	0.710220
-18.595787	-1.829379	0.835802	0.003535	0.710220
-18.256353	-1.888303	0.840806	0.003472	0.710223
-18.192066	-1.949201	0.845811	0.003460	0.710124
-19.305698	-1.864478	0.850816	0.003668	0.709896
-19.225365	-1.880391	0.855821	0.003653	0.709893
-19.260807	-1.874305	0.860826	0.003659	0.709893
-19.139026	-1.892725	0.865830	0.003637	0.709899
-19.666329	-1.803472	0.870835	0.003735	0.709889
-19.399315	-1.844963	0.875840	0.003685	0.709902
-19.140837	-1.898090	0.880845	0.003637	0.709887
-19.998332	-1.889957	0.885850	0.003797	0.709598
-20.205705	-1.851669	0.890854	0.003836	0.709601
-20.298970	-1.839219	0.895859	0.003853	0.709592
-19.786456	-1.926339	0.900864	0.003758	0.709600
-20.346429	-1.829153	0.905869	0.003862	0.709595
-20.353123	-1.827487	0.910874	0.003863	0.709596
-20.005976	-1.886776	0.915878	0.003799	0.709601
-20.743312	-1.899798	0.920883	0.003936	0.709312
-21.089180	-1.859801	0.925888	0.004000	0.709269
-20.894843	-1.897669	0.930893	0.003964	0.709262
-20.883603	-1.898147	0.935898	0.003962	0.709265
-20.989729	-1.877084	0.940902	0.003982	0.709269
-21.000184	-1.879468	0.945907	0.003984	0.709261
-20.690238	-1.930491	0.950912	0.003926	0.709269
-21.590945	-1.926292	0.955917	0.004094	0.708956
-21.746533	-1.897038	0.960922	0.004123	0.708959
-21.610033	-1.918633	0.965926	0.004098	0.708964
-22.143269	-1.826711	0.970931	0.004197	0.708958
-22.056006	-1.839063	0.975936	0.004181	0.708964
-21.661424	-1.911255	0.980941	0.004107	0.708961
-21.986046	-1.858502	0.985946	0.004168	0.708950
-22.623291	-1.895258	0.990950	0.004287	0.708649
-22.710894	-1.884512	0.995955	0.004303	0.708639
-22.771338	-1.869682	1.000960	0.004314	0.708647
-22.647882	-1.893981	1.005965	0.004291	0.708643
-22.738468	-1.877910	1.010970	0.004308	0.708642
-22.582235	-1.902283	1.015974	0.004279	0.708649
-22.877403	-1.860037	1.020979	0.004334	0.708628
-23.311244	-1.918366	1.025984	0.004415	0.708357
-23.583153	-1.871924	1.030989	0.004466	0.708352
-23.749761	-1.841446	1.035994	0.004497	0.708354
-23.367518	-1.906103	1.040998	0.004426	0.708361
-23.716407	-1.847655	1.046003	0.004491	0.708353
-23.738328	-1.839537	1.051008	0.004495	0.708362
-23.732700	-1.844042	1.056013	0.004494	0.708355
-24.321563	-1.904390	1.061018	0.004603	0.708023
-24.259521	-1.916145	1.066022	0.004592	0.708022
-25.003962	-1.787581	1.071027	0.004731	0.708013
-24.681412	-1.840940	1.076032	0.004671	0.708021
-24.444483	-1.885618	1.081037	0.004626	0.708016
-24.639046	-1.850002	1.086042	0.004663	0.708018
-24.575434	-1.859506	1.091046	0.004651	0.708022
-24.864187	-1.921893	1.096051	0.004705	0.707794
-25.515715	-1.848607	1.101056	0.004826	0.707707
-25.513448	-1.850292	1.106061	0.004826	0.707705
-25.539099	-1.845949	1.111066	0.004831	0.707704
-25.266794	-1.890122	1.116070	0.004780	0.707713
-25.424633	-1.868600	1.121075	0.004809	0.707700
-25.418499	-1.865175	1.126080	0.004808	0.707709
-25.406948	-1.975162	1.131085	0.004806	0.707492
-26.465466	-1.841563	1.136090	0.005003	0.707381
-26.274361	-1.871033	1.141094	0.004968	0.707391
-26.361940	-1.860591	1.146099	0.004984	0.707380
-26.330178	-1.861970	1.151104	0.004978	0.707389
-26.533686	-1.827714	1.156109	0.005016	0.707384
-26.482675	-1.838008	1.161114	0.005007	0.707382
-26.245849	-1.957961	1.166118	0.004963	0.707226
-27.497053	-1.806359	1.171123	0.005196	0.707082
-27.311305	-1.834332	1.176128	0.005161	0.707093
-27.097924	-1.873646	1.181133	0.005121	0.707090
-27.301658	-1.839387	1.186138	0.005159	0.707086
-27.158682	-1.863663	1.191142	0.005133	0.707088
-27.445329	-1.816608	1.196147	0.005186	0.707080
-27.231607	-1.918803	1.201152	0.005147	0.706951
-28.321757	-1.823351	1.206157	0.005350	0.706752
-28.391454	-1.810612	1.211162	0.005363	0.706753
-28.009893	-1.874930	1.216166	0.005292	0.706760
-28.401308	-1.810129	1.221171	0.005364	0.706750
-28.305674	-1.822470	1.226176	0.005347	0.706760
-28.282760	-1.830281	1.231181	0.005342	0.706752
-28.166354	-1.851376	1.236186	0.005321	0.706751
-28.467592	-1.932955	1.241190	0.005377	0.706479
-29.324510	-1.797679	1.246195	0.005537	0.706444
-29.163651	-1.821688	1.251200	0.005507	0.706454
-29.008903	-1.851133	1.256205	0.005478	0.706450
-29.615596	-1.744303	1.261210	0.005591	0.706447
-28.902056	-1.866015	1.266214	0.005458	0.706458
-28.933925	-1.865613	1.271219	0.005464	0.706447
-29.504282	-1.864173	1.276224	0.005570	0.706246
-30.181964	-1.798072	1.281229	0.005697	0.706136
-29.572825	-1.909099	1.286234	0.005583	0.706131
-29.897368	-1.846427	1.291238	0.005644	0.706140
-30.381673	-1.763546	1.296243	0.005734	0.706133
-29.753164	-1.874610	1.301248	0.005617	0.706135
-29.737377	-1.878235	1.306253	0.005614	0.706133
-30.467048	-1.829367	1.311258	0.005750	0.705970
-30.503266	-1.870373	1.316262	0.005757	0.705874
-30.527853	-1.871613	1.321267	0.005761	0.705863
-30.834971	-1.812514	1.326272	0.005819	0.705872
-30.705198	-1.837856	1.331277	0.005794	0.705867
-30.487242	-1.878025	1.336282	0.005754	0.705864
-30.871783	-1.806715	1.341286	0.005826	0.705870
-31.583377	-1.839244	1.346291	0.005958	0.705549
-31.498702	-1.862519	1.351296	0.005942	0.705533
-31.603933	-1.844570	1.356301	0.005962	0.705531
-31.941285	-1.785901	1.361306	0.006025	0.705528
-31.521725	-1.857355	1.366310	0.005947	0.705535
-31.598402	-1.848879	1.371315	0.005961	0.705524
-31.547695	-1.853841	1.376320	0.005952	0.705532
-32.266566	-1.866846	1.381325	0.006086	0.705248
-32.586142	-1.826271	1.386330	0.006145	0.705215
-32.263837	-1.878917	1.391334	0.006085	0.705224
-32.699787	-1.806235	1.396339	0.006166	0.705214
-32.359641	-1.861674	1.401344	0.006103	0.705225
-32.280720	-1.878337	1.406349	0.006089	0.705219
-32.897488	-1.768070	1.411354	0.006203	0.705220
-33.073032	-1.882788	1.416358	0.006236	0.704926
-33.454731	-1.831865	1.421363	0.006307	0.704891
-33.367812	-1.843365	1.426368	0.006291	0.704899
-33.220639	-1.870024	1.431373	0.006264	0.704898
-33.441961	-1.833121	1.436378	0.006305	0.704893
-33.182243	-1.875814	1.441382	0.006257	0.704900
-33.561171	-1.812907	1.446387	0.006327	0.704891
-33.802898	-1.913624	1.451392	0.006372	0.704601
-33.955797	-1.888104	1.456397	0.006401	0.704597
-34.548522	-1.781422	1.461402	0.006511	0.704599
-34.002981	-1.877011	1.466406	0.006410	0.704603
-34.007157	-1.880910	1.471411	0.006411	0.704593
-34.249692	-1.835188	1.476416	0.006456	0.704598
-34.386838	-1.857599	1.481421	0.006481	0.704504
-35.107599	-1.847858	1.486426	0.006616	0.704264
-34.556039	-1.941774	1.491430	0.006513	0.704273
-35.574554	-1.766419	1.496435	0.006703	0.704260
-35.180592	-1.832548	1.501440	0.006629	0.704268
-34.529542	-1.950163	1.506445	0.006508	0.704265
-35.175671	-1.836320	1.511450	0.006628	0.704262
-35.263331	-1.892846	1.516454	0.006645	0.704117
-35.971623	-1.847993	1.521459	0.006777	0.703953
-35.536821	-1.921522	1.526464	0.006696	0.703961
-35.876671	-1.862436	1.531469	0.006759	0.703957
-35.955727	-1.848763	1.536474	0.006774	0.703956
-35.378751	-1.949265	1.541478	0.006667	0.703961
-36.051802	-1.834644	1.546483	0.006792	0.703950
-36.302490	-1.929537	1.551488	0.006839	0.703669
-36.462411	-1.916725	1.556493	0.006869	0.703637
-37.181212	-1.789531	1.561498	0.007002	0.703635
-36.880191	-1.838207	1.566502	0.006946	0.703645
-36.827719	-1.852625	1.571507	0.006937	0.703634
-36.907109	-1.834211	1.576512	0.006951	0.703643
-37.191219	-1.786260	1.581517	0.007004	0.703637
-37.298232	-1.866220	1.586522	0.007024	0.703437
-37.329124	-1.902853	1.591526	0.007030	0.703352
-37.568727	-1.864846	1.596531	0.007075	0.703343
-37.610588	-1.854942	1.601536	0.007083	0.703348
-37.598285	-1.857750	1.606541	0.007080	0.703346
-37.500245	-1.875689	1.611546	0.007062	0.703345
-37.538371	-1.875769	1.616550	0.007069	0.703331
-38.416552	-1.880641	1.621555	0.007233	0.703005
-38.315384	-1.893187	1.626560	0.007214	0.703016
-38.807224	-1.807575	1.631565	0.007306	0.703012
-38.711360	-1.826904	1.636570	0.007288	0.703007
-38.132438	-1.923822	1.641574	0.007180	0.703020
-38.817555	-1.807729	1.646579	0.007308	0.703008
-38.682117	-1.827468	1.651584	0.007283	0.703016
-38.850915	-1.938542	1.656589	0.007314	0.702731
-39.464172	-1.846111	1.661594	0.007428	0.702697
-39.550056	-1.827935	1.666598	0.007444	0.702703
-39.391722	-1.859291	1.671603	0.007415	0.702696
-39.144031	-1.900283	1.676608	0.007369	0.702702
-39.365975	-1.862830	1.681613	0.007410	0.702698
-39.520787	-1.843526	1.686618	0.007439	0.702681
-39.573734	-1.983217	1.691622	0.007449	0.702380
-40.043673	-1.903087	1.696627	0.007537	0.702372
-40.485583	-1.821121	1.701632	0.007619	0.702379
-40.053891	-1.900446	1.706637	0.007539	0.702374
-40.261988	-1.865112	1.711642	0.007577	0.702370
-40.411334	-1.833845	1.716646	0.007605	0.702379
-40.446763	-1.866322	1.721651	0.007612	0.702301
-40.999944	-1.875056	1.726656	0.007715	0.702084
-40.923557	-1.889945	1.731661	0.007701	0.702081
-41.313671	-1.821653	1.736666	0.007773	0.702078
-40.854286	-1.899703	1.741670	0.007688	0.702086
-41.072614	-1.866132	1.746675	0.007729	0.702075
-41.119991	-1.853937	1.751680	0.007737	0.702083
-40.988464	-1.946416	1.756685	0.007713	0.701943
-42.226792	-1.822699	1.761690	0.007944	0.701746
-41.907048	-1.875312	1.766694	0.007884	0.701755
-41.955512	-1.869944	1.771699	0.007893	0.701748
-41.967718	-1.865295	1.776704	0.007896	0.701753
-41.967406	-1.866619	1.781709	0.007896	0.701751
-42.428481	-1.786327	1.786714	0.007981	0.701747
-41.734646	-1.958254	1.791718	0.007852	0.701649
-42.719562	-1.884689	1.796723	0.008036	0.701442
-42.988419	-1.835471	1.801728	0.008086	0.701445
-43.175654	-1.801423	1.806733	0.008121	0.701446
-43.181938	-1.804500	1.811738	0.008122	0.701438
-42.690222	-1.888824	1.816742	0.008030	0.701444
-43.272171	-1.788478	1.821747	0.008139	0.701437
-42.887702	-1.879083	1.826752	0.008067	0.701393
-43.573471	-1.888301	1.831757	0.008195	0.701126
-44.095002	-1.796645	1.836762	0.008292	0.701123
-43.921634	-1.825205	1.841766	0.008260	0.701128
-43.721381	-1.862721	1.846771	0.008223	0.701124
-44.007580	-1.810024	1.851776	0.008276	0.701128
-43.907583	-1.826425	1.856781	0.008257	0.701130
-43.802273	-1.849169	1.861786	0.008238	0.701122
-43.875483	-1.937634	1.866790	0.008252	0.700917
-44.650702	-1.820845	1.871795	0.008396	0.700873
-44.435970	-1.855782	1.876800	0.008356	0.700880
-44.039782	-1.926312	1.881805	0.008282	0.700880
-44.843132	-1.784976	1.886810	0.008432	0.700876
-44.495749	-1.845262	1.891814	0.008367	0.700879
-44.089419	-2.006574	1.896819	0.008292	0.700699
-45.877213	-1.767116	1.901824	0.008625	0.700538
-45.437719	-1.845216	1.906829	0.008543	0.700539
-45.189141	-1.890811	1.911834	0.008497	0.700536
-45.057132	-1.910536	1.916838	0.008472	0.700544
-45.450167	-1.843021	1.921843	0.008545	0.700538
-45.200520	-1.887267	1.926848	0.008499	0.700539
-45.613118	-1.968039	1.931853	0.008576	0.700226
-46.553189	-1.802621	1.936858	0.008751	0.700221
-46.343387	-1.836413	1.941862	0.008712	0.700228
-46.228039	-1.861905	1.946867	0.008690	0.700218
-46.408932	-1.824869	1.951872	0.008724	0.700228
-46.281476	-1.847979	1.956877	0.008700	0.700227
-46.183801	-1.882056	1.961882	0.008682	0.700193
-46.463776	-1.974167	1.966886	0.008734	0.699905
-47.302312	-1.830313	1.971891	0.008891	0.699893
-47.428047	-1.803616	1.976896	0.008914	0.699902
-46.815429	-1.913248	1.981901	0.008800	0.699901
-47.308713	-1.826965	1.986906	0.008892	0.699897
-47.084641	-1.862036	1.991910	0.008850	0.699907
-46.886490	-1.950332	1.996915	0.008813	0.699800
-48.026884	-1.841504	2.001920	0.009026	0.699608

-47.972332	-1.850877	2.011917	0.009016	0.699608
-48.166582	-1.817034	2.021914	0.009052	0.699606
-47.829343	-1.878631	2.031910	0.008989	0.699603
-48.050333	-1.838441	2.041907	0.009030	0.699605
-47.931405	-1.859565	2.051904	0.009008	0.699605
-47.980523	-1.851604	2.061901	0.009018	0.699603
-48.166483	-1.819932	2.071898	0.009052	0.699600
-48.222741	-1.808620	2.081894	0.009063	0.699602
-47.997586	-1.848650	2.091891	0.009021	0.699602
-47.950336	-1.855258	2.101888	0.009012	0.699606
-47.654415	-1.910218	2.111885	0.008957	0.699601
-48.086403	-1.831975	2.121882	0.009038	0.699603
-47.789785	-1.821955	2.131878	0.008983	0.699731
-47.005477	-1.877406	2.141875	0.008837	0.699902
-47.112821	-1.858755	2.151872	0.008857	0.699901
-46.924050	-1.891448	2.161869	0.008822	0.699903
-47.281183	-1.828865	2.171866	0.008888	0.699900
-47.001234	-1.830482	2.181862	0.008836	0.699998
-46.110780	-1.878163	2.191859	0.008671	0.700223
-46.253023	-1.852710	2.201856	0.008697	0.700223
-46.283796	-1.847098	2.211853	0.008703	0.700223
-46.412679	-1.797477	2.221850	0.008727	0.700277
-45.330522	-1.862373	2.231846	0.008526	0.700537
-45.268892	-1.872005	2.241843	0.008514	0.700539
-45.410584	-1.846458	2.251840	0.008541	0.700540
-45.159006	-1.847671	2.261837	0.008494	0.700628
-44.643321	-1.818497	2.271834	0.008398	0.700873
-44.292430	-1.879440	2.281830	0.008333	0.700877
-44.573934	-1.828654	2.291827	0.008385	0.700878
-44.058874	-1.873704	2.301824	0.008290	0.700972
-43.773338	-1.850964	2.311821	0.008237	0.701121
-43.651747	-1.872135	2.321818	0.008214	0.701122
-43.838831	-1.838187	2.331814	0.008249	0.701123
-42.983063	-1.840459	2.341811	0.008090	0.701427
-42.742733	-1.876936	2.351808	0.008045	0.701440
-42.975458	-1.834270	2.361805	0.008088	0.701442
-42.762444	-1.798970	2.371802	0.008049	0.701590
-41.738750	-1.903266	2.381798	0.007858	0.701749
-42.167463	-1.827661	2.391795	0.007938	0.701747
-41.736980	-1.903100	2.401792	0.007858	0.701749
-41.490900	-1.792955	2.411789	0.007812	0.702061
-41.025382	-1.868844	2.421786	0.007726	0.702075
-41.042046	-1.865980	2.431782	0.007729	0.702075
-40.758599	-1.847728	2.441779	0.007676	0.702213
-40.209250	-1.865934	2.451776	0.007574	0.702375
-40.389716	-1.833708	2.461773	0.007608	0.702374
-40.274627	-1.843048	2.471770	0.007587	0.702397
-39.705430	-1.796477	2.481766	0.007481	0.702696
-39.641398	-1.808659	2.491763	0.007469	0.702694
-39.410779	-1.848456	2.501760	0.007426	0.702697
-38.971256	-1.796300	2.511757	0.007344	0.702960
-38.385823	-1.876685	2.521754	0.007235	0.703009
-38.612143	-1.836982	2.531750	0.007278	0.703007
-38.488507	-1.798226	2.541747	0.007255	0.703130
-37.598530	-1.850068	2.551744	0.007089	0.703345
-37.780598	-1.816630	2.561741	0.007123	0.703347
-37.533008	-1.861656	2.571738	0.007077	0.703345
-36.766695	-1.873095	2.581734	0.006934	0.703598
-36.850556	-1.838112	2.591731	0.006950	0.703638
-36.566742	-1.887350	2.601728	0.006897	0.703640
-36.965914	-1.777208	2.611725	0.006972	0.703719
-35.956617	-1.841467	2.621722	0.006784	0.703952
-36.122066	-1.812078	2.631718	0.006815	0.703952
-35.883693	-1.852592	2.641715	0.006770	0.703955
-35.231707	-1.829807	2.651712	0.006649	0.704236
-35.047026	-1.848149	2.661709	0.006615	0.704265
-34.920650	-1.871679	2.671706	0.006591	0.704263
-35.035304	-1.791759	2.681702	0.006613	0.704382
-34.027639	-1.865844	2.691699	0.006425	0.704595
-33.896317	-1.888627	2.701696	0.006401	0.704596
-34.200876	-1.834322	2.711693	0.006458	0.704596
-33.602809	-1.824717	2.721690	0.006346	0.704830
-33.662933	-1.782563	2.731686	0.006358	0.704893
-33.236041	-1.858698	2.741683	0.006278	0.704893
-33.198816	-1.787908	2.751680	0.006271	0.705049
-32.447501	-1.838774	2.761677	0.006132	0.705216
-32.491569	-1.832695	2.771674	0.006140	0.705212
-32.593475	-1.804776	2.781670	0.006159	0.705231
-31.709967	-1.813942	2.791667	0.005995	0.705530
-31.491666	-1.852850	2.801664	0.005954	0.705530
-31.656418	-1.824054	2.811661	0.005985	0.705528
-31.056781	-1.826606	2.821658	0.005873	0.705738
-30.901947	-1.791955	2.831654	0.005845	0.705863
-30.536110	-1.855958	2.841651	0.005777	0.705865
-30.498518	-1.861991	2.851648	0.005770	0.705866
-29.930968	-1.838554	2.861645	0.005664	0.706117
-29.881090	-1.840907	2.871642	0.005655	0.706130
-29.915621	-1.834082	2.881638	0.005661	0.706131
-29.489596	-1.838833	2.891635	0.005582	0.706274
-28.970665	-1.844768	2.901632	0.005486	0.706448
-29.053905	-1.829066	2.911629	0.005501	0.706449
-29.107842	-1.800697	2.921626	0.005511	0.706487
-28.245562	-1.821625	2.931622	0.005351	0.706753
-28.013082	-1.862979	2.941619	0.005308	0.706753
-28.299408	-1.810765	2.951616	0.005361	0.706756
-27.528571	-1.825731	2.961613	0.005218	0.707001
-27.313509	-1.823030	2.971610	0.005178	0.707084
-27.308730	-1.823367	2.981606	0.005177	0.707084
-27.076102	-1.829983	2.991603	0.005134	0.707154
-26.548514	-1.810159	3.001600	0.005035	0.707383
-26.243255	-1.864017	3.011597	0.004979	0.707383
-26.547598	-1.811319	3.021594	0.005035	0.707380
-25.718368	-1.831041	3.031590	0.004881	0.707637
-25.626608	-1.813531	3.041587	0.004864	0.707705
-25.475593	-1.840050	3.051584	0.004836	0.707705
-25.387429	-1.807087	3.061581	0.004820	0.707803
-24.801600	-1.805796	3.071578	0.004711	0.708015
-24.663936	-1.828765	3.081574	0.004685	0.708018
-24.577457	-1.844483	3.091571	0.004669	0.708017
-24.075947	-1.786011	3.101568	0.004576	0.708313
-23.499957	-1.868423	3.111565	0.004469	0.708353
-23.899286	-1.797944	3.121562	0.004543	0.708352
-23.612280	-1.803338	3.131558	0.004490	0.708443
-22.893797	-1.832062	3.141555	0.004356	0.708642
-23.046543	-1.802489	3.151552	0.004385	0.708647
-22.911109	-1.828297	3.161549	0.004360	0.708643
-22.349866	-1.778340	3.171546	0.004255	0.708943
-22.188896	-1.799253	3.181542	0.004225	0.708959
-22.114350	-1.811907	3.191539	0.004212	0.708960
-21.732628	-1.785256	3.201536	0.004141	0.709149
-21.015648	-1.852853	3.211533	0.004007	0.709269
-21.503106	-1.766400	3.221530	0.004098	0.709268
-21.105662	-1.815510	3.231526	0.004024	0.709312
-20.702865	-1.742360	3.241523	0.003949	0.709602
-19.892521	-1.886339	3.251520	0.003798	0.709602
-20.179921	-1.836597	3.261517	0.003852	0.709599
-19.937390	-1.793528	3.271514	0.003807	0.709771
-19.255581	-1.852647	3.281510	0.003680	0.709896
-19.333886	-1.838606	3.291507	0.003695	0.709896
-19.342884	-1.835470	3.301504	0.003696	0.709899
-18.872888	-1.768847	3.311501	0.003609	0.710199
-18.746080	-1.781974	3.321498	0.003586	0.710218
-18.215475	-1.876369	3.331494	0.003487	0.710218
-18.435209	-1.760385	3.341491	0.003528	0.710372
-17.384937	-1.864369	3.351488	0.003332	0.710538
-17.509203	-1.842999	3.361485	0.003356	0.710536
-17.653365	-1.818279	3.371482	0.003383	0.710534
-16.937297	-1.795715	3.381478	0.003249	0.710833
-16.872710	-1.786470	3.391475	0.003237	0.710875
-16.531496	-1.846249	3.401472	0.003174	0.710877
-16.609001	-1.778795	3.411469	0.003188	0.710984
-15.809884	-1.840486	3.421466	0.003040	0.711144
-15.752746	-1.852932	3.431462	0.003029	0.711140
-15.961372	-1.815160	3.441459	0.003068	0.711141
-15.210341	-1.824387	3.451456	0.002928	0.711389
-15.240578	-1.784593	3.461453	0.002934	0.711458
-15.000997	-1.828257	3.471450	0.002890	0.711456
-14.834423	-1.794729	3.481446	0.002859	0.711581
-14.212103	-1.813981	3.491443	0.002743	0.711764
-14.084455	-1.835583	3.501440	0.002719	0.711766
-14.480807	-1.754601	3.511437	0.002793	0.711787
-13.462095	-1.782814	3.521434	0.002603	0.712092
-13.235326	-1.823645	3.531430	0.002561	0.712091
-13.521120	-1.771301	3.541427	0.002615	0.712094
-12.750131	-1.806459	3.551424	0.002471	0.712297
-12.735201	-1.761563	3.561421	0.002468	0.712392
-12.573491	-1.790683	3.571418	0.002438	0.712391
-12.479333	-1.749539	3.581414	0.002421	0.712506
-11.731102	-1.778849	3.591411	0.002282	0.712713
-11.450616	-1.828072	3.601408	0.002230	0.712714
-11.634631	-1.797358	3.611405	0.002264	0.712710
-10.829322	-1.802563	3.621402	0.002114	0.712985
-10.845390	-1.778919	3.631398	0.002117	0.713026
-10.478780	-1.843840	3.641395	0.002049	0.713027
-10.473584	-1.803247	3.651392	0.002048	0.713109
-9.881777	-1.780071	3.661389	0.001938	0.713365
-9.702665	-1.811976	3.671386	0.001905	0.713365
-9.861234	-1.785720	3.681382	0.001934	0.713361
-9.225776	-1.801637	3.691379	0.001816	0.713554
-8.910513	-1.804974	3.701376	0.001758	0.713659
-9.047964	-1.781618	3.711373	0.001783	0.713657
-8.715785	-1.823183	3.721370	0.001721	0.713692
-8.111850	-1.789470	3.731366	0.001609	0.713972
-7.328603	-1.928340	3.741363	0.001463	0.713973
-7.457673	-1.904157	3.751360	0.001488	0.713976
-7.594114	-1.880982	3.761357	0.001513	0.713973
-6.733981	-1.882779	3.771354	0.001353	0.714274
-6.904579	-1.848248	3.781350	0.001385	0.714282
-6.569660	-1.908775	3.791347	0.001323	0.714280
-6.890670	-1.830252	3.801344	0.001382	0.714322
-5.832010	-1.871156	3.811341	0.001185	0.714615
-5.750129	-1.887783	3.821338	0.001170	0.714611
-6.015062	-1.840695	3.831334	0.001220	0.714611
-5.608404	-1.875936	3.841331	0.001144	0.714684
-4.897569	-1.888029	3.851328	0.001012	0.714912
-4.770654	-1.910986	3.861325	0.000988	0.714911
-4.980096	-1.873430	3.871322	0.001027	0.714911
-4.577797	-1.873847	3.881318	0.000952	0.715052
-3.586180	-1.958078	3.891315	0.000768	0.715236
-4.116632	-1.862627	3.901312	0.000867	0.715237
-3.818396	-1.916774	3.911309	0.000811	0.715235
-3.389703	-1.891512	3.921306	0.000732	0.715436
-3.041081	-1.895948	3.931302	0.000667	0.715551
-2.859330	-1.928713	3.941299	0.000633	0.715550
-2.843387	-1.931112	3.951296	0.000630	0.715550
-2.372727	-1.885795	3.961293	0.000543	0.715806
-2.245657	-1.869345	3.971290	0.000519	0.715884
-2.193670	-1.877692	3.981286	0.000509	0.715885
-2.056501	-1.869110	3.991283	0.000484	0.715950
-1.726211	-1.832917	4.001280	0.000423	0.716139
-1.539029	-1.867398	4.011277	0.000388	0.716136
-1.713154	-1.813964	4.021274	0.000420	0.716180
-1.418087	-1.728091	4.031270	0.000365	0.716454
-1.315733	-1.747737	4.041267	0.000346	0.716451
-1.262659	-1.676582	4.051264	0.000337	0.716611
-0.789196	-1.684753	4.061261	0.000249	0.716761
-0.980783	-1.646670	4.071258	0.000284	0.716769
-1.024386	-1.478192	4.081254	0.000292	0.717087
-0.833542	-1.511389	4.091251	0.000257	0.717088
-1.047129	-1.335563	4.101248	0.000297	0.717361
-0.523207	-1.414611	4.111245	0.000199	0.717389
-0.522202	-1.255282	4.121242	0.000199	0.717704
-0.653909	-1.196705	4.131238	0.000224	0.717773
-0.558133	-1.089971	4.141235	0.000206	0.718018
-0.338006	-1.030032	4.151232	0.000165	0.718213
-0.296481	-0.964810	4.161229	0.000157	0.718357
-0.347749	-0.813257	4.171226	0.000167	0.718638
-0.363896	-0.721446	4.181222	0.000170	0.718813
-0.100596	-0.672926	4.191219	0.000121	0.719001
-0.126058	-0.529685	4.201216	0.000126	0.719274
-0.253437	-0.376445	4.211213	0.000149	0.719532
-0.314754	-0.245631	4.221210	0.000161	0.719768
-0.080134	-0.158754	4.231206	0.000117	0.720021
-0.086645	-0.020675	4.241203	0.000118	0.720291
0.036059	0.099724	4.251200	0.000095	0.720571
0.000000	0.304412	4.261197	0.000102	0.720961

0.083754	0.890473	4.266202	0.000086	0.722142
0.271001	2.121119	4.271206	0.000051	0.724621
0.491731	3.933600	4.276211	0.000008	0.728237
0.622768	6.317573	4.281216	-0.000018	0.732911
1.096405	9.146336	4.286221	-0.000108	0.738528
1.585753	12.457760	4.291226	-0.000201	0.745027
1.708571	16.286171	4.296230	-0.000226	0.752322
2.197341	20.454939	4.301235	-0.000320	0.760303
2.708398	25.018788	4.306240	-0.000418	0.768938
3.085609	29.979085	4.311245	-0.000491	0.778157
3.580420	35.265235	4.316250	-0.000587	0.787891
4.050147	40.869411	4.321254	-0.000678	0.798065
4.421613	46.801314	4.326259	-0.000751	0.808654
4.730800	53.020080	4.331264	-0.000813	0.819584
5.226409	59.479801	4.336269	-0.000909	0.830838
9.631601	65.495436	4.341274	-0.001733	0.842355
10.625229	72.387197	4.346278	-0.001923	0.854170
11.127614	79.573891	4.351283	-0.002021	0.866165
11.629302	86.932526	4.356288	-0.002119	0.878273
12.390450	94.420825	4.361293	-0.002265	0.890496
13.252056	102.055102	4.366298	-0.002431	0.902809
13.734926	109.895141	4.371302	-0.002526	0.915172
14.825911	117.745460	4.376307	-0.002734	0.927549
15.594096	125.775833	4.381312	-0.002882	0.939949
16.072070	133.957231	4.386317	-0.002977	0.952336
17.181946	142.118767	4.391322	-0.003188	0.964696
18.077952	150.409082	4.396326	-0.003361	0.977032
19.140012	158.756125	4.401331	-0.003564	0.989337
19.988102	167.199050	4.406336	-0.003727	1.001573
20.630224	175.697058	4.411341	-0.003852	1.013688
21.874325	184.137916	4.416346	-0.004089	1.025724
22.448305	192.721050	4.421350	-0.004202	1.037656
23.069166	201.327175	4.426355	-0.004323	1.049494
23.598357	209.969981	4.431360	-0.004427	1.061228
24.067620	218.648360	4.436365	-0.004520	1.072866
24.918096	227.251533	4.441370	-0.004684	1.084366
25.294261	235.949432	4.446374	-0.004760	1.095763
26.212325	244.551632	4.451379	-0.004936	1.107038
26.828666	253.219676	4.456384	-0.005057	1.118217
27.449020	261.873178	4.461389	-0.005178	1.129268
27.967884	270.553153	4.466394	-0.005280	1.140223
28.306490	279.262051	4.471398	-0.005349	1.151070
29.219378	287.849192	4.476403	-0.005524	1.161788
29.650847	296.496642	4.481408	-0.005610	1.172380
30.474934	305.064422	4.486413	-0.005769	1.182862
31.190701	313.668676	4.491418	-0.005908	1.193274
31.813132	322.246233	4.496422	-0.006029	1.203544
32.540204	330.826827	4.501427	-0.006170	1.213752
32.948837	339.431454	4.506432	-0.006252	1.223839
33.506248	348.021677	4.511437	-0.006361	1.233856
34.405908	356.507241	4.516442	-0.006534	1.243739
35.180668	365.008261	4.521446	-0.006684	1.253537
35.979483	373.499407	4.526451	-0.006838	1.263253
36.695028	382.004317	4.531456	-0.006977	1.272893
37.536724	390.461684	4.536461	-0.007139	1.282432
38.176838	398.964605	4.541466	-0.007264	1.291912
38.510799	407.484145	4.546470	-0.007331	1.301285
39.087673	416.024684	4.551475	-0.007444	1.310658
39.884543	424.498101	4.556480	-0.007598	1.319932
40.285528	432.936338	4.561485	-0.007678	1.329032
41.174523	441.310212	4.566490	-0.007849	1.338088
41.398709	449.753918	4.571494	-0.007896	1.347040
41.998989	458.161272	4.576499	-0.008014	1.355960
42.566492	466.530966	4.581504	-0.008125	1.364777
42.806170	474.963125	4.586509	-0.008175	1.373545
43.555391	483.304023	4.591514	-0.008320	1.382251
44.225287	491.659645	4.596518	-0.008450	1.390903
44.668627	500.039511	4.601523	-0.008538	1.399489
44.899637	508.421754	4.606528	-0.008586	1.407988
45.381634	516.771274	4.611533	-0.008681	1.416446
46.152290	525.068686	4.616538	-0.008830	1.424848
46.728699	533.391940	4.621542	-0.008943	1.433195
47.127728	541.721112	4.626547	-0.009023	1.441470
47.756194	550.003198	4.631552	-0.009145	1.449689
48.324411	558.311009	4.636557	-0.009256	1.457877
48.940676	566.598237	4.641562	-0.009376	1.466006
49.338508	574.957969	4.646566	-0.009456	1.474126
49.688055	583.259960	4.651571	-0.009526	1.482138
50.356923	591.496882	4.656576	-0.009656	1.490095
50.949475	599.762688	4.661581	-0.009772	1.498024
51.347191	608.047850	4.666586	-0.009851	1.505900
51.611754	616.358479	4.671590	-0.009906	1.513739
52.009314	624.623544	4.676595	-0.009985	1.521514
52.743407	632.829213	4.681600	-0.010127	1.529246
53.265559	641.085389	4.686605	-0.010230	1.536953
53.612957	649.356578	4.691610	-0.010300	1.544610
54.264678	657.583220	4.696614	-0.010426	1.552233
55.072843	665.779603	4.701619	-0.010582	1.559813
55.196822	674.064076	4.706624	-0.010611	1.567337
55.629479	682.305598	4.711629	-0.010697	1.574831
56.135385	690.530501	4.716634	-0.010796	1.582285
56.555682	698.756594	4.721638	-0.010880	1.589692
57.071367	706.991832	4.726643	-0.010981	1.597087
57.547187	715.197323	4.731648	-0.011075	1.604415
57.843222	723.434425	4.736653	-0.011135	1.611712
58.564771	731.623773	4.741658	-0.011275	1.618995
59.303984	739.779391	4.746662	-0.011418	1.626217
59.844029	748.052401	4.751667	-0.011524	1.633481
60.122278	756.269970	4.756672	-0.011581	1.640630
60.383226	764.481093	4.761677	-0.011635	1.647739
60.833869	772.679575	4.766682	-0.011724	1.654832
61.152136	780.866320	4.771686	-0.011789	1.661867
61.872767	789.012658	4.776691	-0.011928	1.668893
62.302277	797.218523	4.781696	-0.012013	1.675900
62.409423	805.441302	4.786701	-0.012039	1.682848
62.778588	813.631444	4.791706	-0.012113	1.689776
63.526705	821.764706	4.796710	-0.012257	1.696678
64.294479	829.888061	4.801715	-0.012405	1.703545
64.682703	838.101847	4.806720	-0.012483	1.710411
65.000439	846.304525	4.811725	-0.012547	1.717230
65.813161	854.415228	4.816730	-0.012704	1.724011
66.138503	862.598823	4.821734	-0.012770	1.730762
66.488313	870.797688	4.826739	-0.012840	1.737502
66.824781	878.972423	4.831744	-0.012908	1.744194
67.424935	887.106034	4.836749	-0.013025	1.750861
67.554967	895.325549	4.841754	-0.013055	1.757513
67.837010	903.478948	4.846758	-0.013113	1.764105
68.262187	911.643980	4.851763	-0.013197	1.770700
68.503121	919.839584	4.856768	-0.013247	1.777272
69.034218	927.961503	4.861773	-0.013351	1.783797
69.651257	936.117342	4.866778	-0.013471	1.790335
69.692800	944.345508	4.871782	-0.013484	1.796836
70.218836	952.444437	4.876787	-0.013588	1.803271
70.529175	960.599402	4.881792	-0.013651	1.809701
70.927315	968.747511	4.886797	-0.013730	1.816113
71.368100	976.878666	4.891802	-0.013817	1.822494
71.727975	985.014332	4.896806	-0.013890	1.828846
72.153611	993.160241	4.901811	-0.013974	1.835193
72.425458	1001.294654	4.906816	-0.014030	1.841490
72.622581	1009.434435	4.911821	-0.014072	1.847761
73.217543	1017.565842	4.916826	-0.014188	1.854051
73.361031	1025.711269	4.921830	-0.014220	1.860277
73.806866	1033.834842	4.926835	-0.014308	1.866502
74.552702	1041.934798	4.931840	-0.014452	1.872722
74.725026	1050.101559	4.936845	-0.014490	1.878905
75.036100	1058.216917	4.941850	-0.014553	1.885046
75.292033	1066.358254	4.946854	-0.014606	1.891180
75.865273	1074.462396	4.951859	-0.014718	1.897302
75.979775	1082.622325	4.956864	-0.014744	1.903394
76.453806	1090.726903	4.961869	-0.014838	1.909466
77.043461	1098.840018	4.966874	-0.014953	1.915537
77.200028	1106.965183	4.971878	-0.014987	1.921550
77.571240	1115.088036	4.976883	-0.015062	1.927567
77.949684	1123.217828	4.981888	-0.015137	1.933570
78.268175	1131.333927	4.986893	-0.015202	1.939538
78.768879	1139.434206	4.991898	-0.015301	1.945496
78.963862	1147.609102	4.996902	-0.015342	1.951457
79.460449	1155.721667	5.001907	-0.015440	1.957386
79.592210	1163.834441	5.006912	-0.015470	1.963259
79.809708	1171.946663	5.011917	-0.015515	1.969123
80.545252	1180.002438	5.016922	-0.015657	1.974984
80.785948	1188.105240	5.021926	-0.015708	1.980809
80.948692	1196.252706	5.026931	-0.015743	1.986640
81.419426	1204.360007	5.031936	-0.015836	1.992458
81.811343	1212.456186	5.036941	-0.015914	1.998243
82.444644	1220.516942	5.041946	-0.016037	2.004011
82.544202	1228.655482	5.046950	-0.016061	2.009762
82.944274	1236.777424	5.051955	-0.016141	2.015516
83.095533	1244.899719	5.056960	-0.016174	2.021227
83.259195	1253.018714	5.061965	-0.016210	2.026922
83.897818	1261.119631	5.066970	-0.016334	2.032636
84.195849	1269.215095	5.071974	-0.016395	2.038296
84.234333	1277.336520	5.076979	-0.016407	2.043932
84.570266	1285.428396	5.081984	-0.016475	2.049562
85.131337	1293.489414	5.086989	-0.016585	2.055178
85.508551	1301.581445	5.091994	-0.016660	2.060781
85.600986	1309.696875	5.096998	-0.016683	2.066356
86.019636	1317.810465	5.102003	-0.016766	2.071948
86.388220	1325.890609	5.107008	-0.016840	2.077497
86.418662	1333.995018	5.112013	-0.016851	2.083014
86.950283	1342.064451	5.117018	-0.016955	2.088542
87.445639	1350.145023	5.122022	-0.017052	2.094059
87.499926	1358.283931	5.127027	-0.017068	2.099558
87.976933	1366.357956	5.132032	-0.017162	2.105040
88.402370	1374.454120	5.137037	-0.017246	2.110517
88.710232	1382.620614	5.142042	-0.017309	2.116016
88.999096	1390.661117	5.147046	-0.017368	2.121414
89.328357	1398.735523	5.152051	-0.017434	2.126826
89.612478	1406.839837	5.157056	-0.017492	2.132238
89.559223	1414.959196	5.162061	-0.017488	2.137615
90.185804	1422.988243	5.167066	-0.017610	2.142984
90.605803	1431.058727	5.172070	-0.017693	2.148346
90.732168	1439.199542	5.177075	-0.017722	2.153714
90.941299	1447.282273	5.182080	-0.017766	2.159038
91.479623	1455.300452	5.187085	-0.017871	2.164337
91.814297	1463.407673	5.192090	-0.017939	2.169663
91.985571	1471.515131	5.197094	-0.017976	2.174960
92.254497	1479.604577	5.202099	-0.018031	2.180241
92.353880	1487.703184	5.207104	-0.018055	2.185501
92.678509	1495.796731	5.212109	-0.018121	2.190764
93.021293	1503.896045	5.217114	-0.018190	2.196021
93.459033	1511.923912	5.222118	-0.018277	2.201228
93.866673	1519.985344	5.227123	-0.018358	2.206441
94.200105	1528.076604	5.232128	-0.018425	2.211653
94.841339	1536.112611	5.237133	-0.018550	2.216846
95.005686	1544.230514	5.242138	-0.018585	2.222037
95.275260	1552.312719	5.247142	-0.018641	2.227201
95.659996	1560.418696	5.252147	-0.018718	2.232379
95.964499	1568.508105	5.257152	-0.018780	2.237528
96.084245	1576.580824	5.262157	-0.018807	2.242637
96.247734	1584.681822	5.267162	-0.018843	2.247757
96.599104	1592.749401	5.272166	-0.018913	2.252860
97.100043	1600.791814	5.277171	-0.019012	2.257949
97.261151	1608.890202	5.282176	-0.019047	2.263032
97.313890	1616.979166	5.287181	-0.019062	2.268089
97.901603	1625.087372	5.292186	-0.019177	2.273192
98.175463	1633.131201	5.297190	-0.019233	2.278216
98.579487	1641.164686	5.302195	-0.019313	2.283234
99.064050	1649.211342	5.307200	-0.019409	2.288256
99.286059	1657.288148	5.312205	-0.019455	2.293264
99.570868	1665.381236	5.317210	-0.019514	2.298275
99.857492	1673.431213	5.322214	-0.019572	2.303249
100.165203	1681.511701	5.327219	-0.019635	2.308233
100.769005	1689.573927	5.332224	-0.019752	2.313220
100.857505	1697.651543	5.337229	-0.019774	2.318162
101.433435	1705.683246	5.342234	-0.019887	2.323107
101.798366	1713.744280	5.347238	-0.019960	2.328041
101.930114	1721.873991	5.352243	-0.019989	2.332987
102.457852	1729.907626	5.357248	-0.020093	2.337896
102.597975	1737.983481	5.362253	-0.020124	2.342790
103.883961	1745.956479	5.367258	-0.020369	2.347704
104.833235	1754.001735	5.372262	-0.020551	2.352624
105.180842	1762.083377	5.377267	-0.020621	2.357507
105.416717	1770.180676	5.382272	-0.020670	2.362379
105.885842	1778.242790	5.387277	-0.020762	2.367240
106.293756	1786.356476	5.392282	-0.020844	2.372116
106.203145	1794.465998	5.397286	-0.020832	2.376939
106.583827	1802.517665	5.402291	-0.020908	2.381756
106.891103	1810.589674	5.407296	-0.020971	2.386570
107.035946	1818.690426	5.412301	-0.021003	2.391378
107.394172	1826.764008	5.417306	-0.021075	2.396177
107.538305	1834.811573	5.422310	-0.021107	2.400934
107.771992	1842.882921	5.427315	-0.021155	2.405703
108.095055	1850.944727	5.432320	-0.021221	2.410463
108.278988	1859.022513	5.437325	-0.021260	2.415213
108.635710	1867.074722	5.442330	-0.021332	2.419952
108.684569	1875.147601	5.447334	-0.021346	2.424669
109.110757	1883.186350	5.452339	-0.021431	2.429387
109.618127	1891.322707	5.457344	-0.021530	2.434158
109.800761	1899.348607	5.462349	-0.021570	2.438831
110.059730	1907.408565	5.467354	-0.021623	2.443521
110.258999	1915.446097	5.472358	-0.021665	2.448184
110.638943	1923.495411	5.477363	-0.021741	2.452858
110.722457	1931.577484	5.482368	-0.021762	2.457521
111.012209	1939.603685	5.487373	-0.021821	2.462157
111.290613	1947.673919	5.492378	-0.021878	2.466809
111.628971	1955.720384	5.497382	-0.021946	2.471444
111.708714	1963.814776	5.502387	-0.021967	2.476077
111.991407	1971.866778	5.507392	-0.022024	2.480693
112.303259	1979.885192	5.512397	-0.022088	2.485284
112.491085	1987.964127	5.517402	-0.022128	2.489891
112.789004	1996.026002	5.522406	-0.022189	2.494487
113.129053	2004.075706	5.527411	-0.022257	2.499072
113.444524	2012.122863	5.532416	-0.022321	2.503645
113.638316	2020.194812	5.537421	-0.022362	2.508214
113.978315	2028.294412	5.542426	-0.022431	2.512802
114.168312	2036.340508	5.547430	-0.022471	2.517340
114.431076	2044.379109	5.552435	-0.022526	2.521870
114.663684	2052.429231	5.557440	-0.022574	2.526397
114.763467	2060.505630	5.562445	-0.022598	2.530921
115.205932	2068.560895	5.567450	-0.022685	2.535450
115.485333	2076.576784	5.572454	-0.022743	2.539936
116.060398	2084.602800	5.577459	-0.022855	2.544442
116.081441	2092.705688	5.582464	-0.022864	2.548943
116.027709	2100.798590	5.587469	-0.022859	2.553425
116.517107	2108.828089	5.592474	-0.022956	2.557902
116.936819	2116.834681	5.597478	-0.023039	2.562354
116.884452	2124.930700	5.602483	-0.023034	2.566814
117.354823	2132.969717	5.607488	-0.023127	2.571272
117.675269	2141.021110	5.612493	-0.023192	2.575718
117.845128	2149.102427	5.617498	-0.023229	2.580163
118.065103	2157.120738	5.622502	-0.023275	2.584568
118.651928	2165.158891	5.627507	-0.023389	2.589002
119.030952	2173.398111	5.632512	-0.023465	2.593524
119.171505	2181.416751	5.637517	-0.023497	2.597902
119.303278	2189.447520	5.642522	-0.023526	2.602278
119.664710	2197.443423	5.647526	-0.023599	2.606644
119.834719	2205.489453	5.652531	-0.023636	2.611016
120.247576	2213.538261	5.657536	-0.023718	2.615399
120.423466	2221.561959	5.662541	-0.023756	2.619745
120.798610	2229.599915	5.667546	-0.023831	2.624105
120.919746	2237.657048	5.672550	-0.023859	2.628451
121.362082	2245.715563	5.677555	-0.023946	2.632811
121.790836	2253.728534	5.682560	-0.024031	2.637139
122.122724	2261.726021	5.687565	-0.024098	2.641445
122.685505	2269.766237	5.692570	-0.024208	2.645782
123.079293	2277.810579	5.697574	-0.024287	2.650103
123.193848	2285.910398	5.702579	-0.024313	2.654429
123.467428	2293.961204	5.707584	-0.024369	2.658731
123.618500	2301.998422	5.712589	-0.024403	2.663011
124.004728	2310.069487	5.717594	-0.024480	2.667318
124.198239	2318.133623	5.722598	-0.024521	2.671601
124.319264	2326.214901	5.727603	-0.024549	2.675882
124.766775	2334.235868	5.732608	-0.024637	2.680145
124.663279	2342.272573	5.737613	-0.024623	2.684375
124.956913	2350.327327	5.742618	-0.024683	2.688632
125.143714	2358.377593	5.747622	-0.024723	2.692874
125.372133	2366.423146	5.752627	-0.024771	2.697109
125.718262	2374.464938	5.757632	-0.024840	2.701342
125.998472	2382.462944	5.762637	-0.024898	2.705542
126.398535	2390.536970	5.767642	-0.024978	2.709783
126.496043	2398.619349	5.772646	-0.025001	2.714002
126.665269	2406.660777	5.777651	-0.025038	2.718198
127.415327	2414.630395	5.782656	-0.025182	2.722387
127.308698	2422.716591	5.787661	-0.025168	2.726576
127.558650	2430.785423	5.792666	-0.025220	2.730771
127.786429	2438.834417	5.797670	-0.025267	2.734949
128.060431	2446.861945	5.802675	-0.025323	2.739112
128.280190	2454.919174	5.807680	-0.025369	2.743280
128.544015	2462.942931	5.812685	-0.025424	2.747428
128.988240	2471.034262	5.817690	-0.025512	2.751615
129.239617	2479.126198	5.822694	-0.025564	2.755784
129.545458	2487.102835	5.827699	-0.025626	2.759891
129.840688	2495.124523	5.832704	-0.025686	2.764014
129.977425	2503.155538	5.837709	-0.025717	2.768126
130.281540	2511.217575	5.842714	-0.025779	2.772258
130.577066	2519.274426	5.847718	-0.025839	2.776381
130.848752	2527.308746	5.852723	-0.025895	2.780485
131.189889	2535.339631	5.857728	-0.025963	2.784584
131.405649	2543.382954	5.862733	-0.026009	2.788677
131.726473	2551.438988	5.867738	-0.026074	2.792776
131.956747	2559.474907	5.872742	-0.026122	2.796854
132.172005	2567.512054	5.877747	-0.026167	2.800925
132.555525	2575.544699	5.882752	-0.026243	2.804998
132.564451	2583.617514	5.887757	-0.026250	2.809064
132.851100	2591.684381	5.892762	-0.026309	2.813136
132.955477	2599.739234	5.897766	-0.026334	2.817187
133.164723	2607.765057	5.902771	-0.026378	2.821222
133.337321	2615.786096	5.907776	-0.026415	2.825248
133.687016	2623.815943	5.912781	-0.026485	2.829282
133.963413	2631.926519	5.917786	-0.026542	2.833347
134.131375	2639.954703	5.922790	-0.026579	2.837358
134.331991	2647.957373	5.927795	-0.026621	2.841353
134.876648	2655.939925	5.932800	-0.026728	2.845352
135.125194	2663.968816	5.937805	-0.026779	2.849351
135.241377	2672.078934	5.942810	-0.026806	2.853377
135.411803	2680.106721	5.947814	-0.026843	2.857360
135.703684	2688.127067	5.952819	-0.026902	2.861341
135.973802	2696.190313	5.957824	-0.026958	2.865336
136.082729	2704.221587	5.962829	-0.026983	2.869301
136.487458	2712.287365	5.967834	-0.027064	2.873293
136.620329	2720.326369	5.972838	-0.027094	2.877252
136.776598	2728.342086	5.977843	-0.027128	2.881195
137.219032	2736.361182	5.982848	-0.027216	2.885150
137.205486	2744.417401	5.987853	-0.027218	2.889093
137.806981	2752.463569	5.992858	-0.027336	2.893058
137.834629	2760.531653	5.997862	-0.027346	2.896998
138.219486	2768.552601	6.002867	-0.027423	2.900929
138.426123	2776.567767	6.007872	-0.027466	2.904842
138.455692	2784.644886	6.012877	-0.027477	2.908771
139.031217	2792.726860	6.017882	-0.027590	2.912725
138.965427	2800.817844	6.022886	-0.027583	2.916645
139.133754	2808.801720	6.027891	-0.027619	2.920520
139.511812	2816.781715	6.032896	-0.027695	2.924398
139.641786	2824.828759	6.037901	-0.027724	2.928291
139.995583	2832.865391	6.042906	-0.027795	2.932186
140.154513	2840.921817	6.047910	-0.027830	2.936074
140.410975	2848.919299	6.052915	-0.027883	2.939934
140.913823	2856.938401	6.057920	-0.027982	2.943812
140.947634	2864.978820	6.062925	-0.027993	2.947671
141.316359	2873.054206	6.067930	-0.028067	2.951559
141.480531	2881.113565	6.072934	-0.028103	2.955423
141.723545	2889.098570	6.077939	-0.028153	2.959251
142.058645	2897.132585	6.082944	-0.028221	2.963102
142.045687	2905.192995	6.087949	-0.028224	2.966943
142.339802	2913.241424	6.092954	-0.028284	2.970788
142.583013	2921.286176	6.097958	-0.028334	2.974625
142.806097	2929.306748	6.102963	-0.028381	2.978444
143.050052	2937.348691	6.107968	-0.028431	2.982269
143.037663	2945.384838	6.112973	-0.028434	2.986073
143.544026	2953.413769	6.117978	-0.028534	2.989895
143.733151	2961.496155	6.122982	-0.028574	2.993722
143.981983	2969.510476	6.127987	-0.028626	2.997515
144.270580	2977.544809	6.132992	-0.028685	3.001314
144.545096	2985.530542	6.137997	-0.028741	3.005085
145.011470	2993.558779	6.143002	-0.028833	3.008880
145.160009	3001.623481	6.148006	-0.028866	3.012672
145.619994	3009.665762	6.153011	-0.028957	3.016464
145.814568	3017.714163	6.158016	-0.028998	3.020241
145.699895	3025.740916	6.163021	-0.028982	3.023988
146.081486	3033.770636	6.168026	-0.029058	3.027756
146.146311	3041.830814	6.173030	-0.029075	3.031518
146.378758	3049.863506	6.178035	-0.029124	3.035271
146.882955	3057.852562	6.183040	-0.029223	3.039011
147.180477	3065.867075	6.188045	-0.029283	3.042749
147.222169	3073.942274	6.193050	-0.029296	3.046499
147.516754	3081.964970	6.198054	-0.029356	3.050231
147.795444	3090.022907	6.203059	-0.029414	3.053974
148.072434	3098.068760	6.208064	-0.029470	3.057707
148.134412	3106.096581	6.213069	-0.029487	3.061417
148.509728	3114.119042	6.218074	-0.029562	3.065135
148.629824	3122.170055	6.223078	-0.029590	3.068849
148.969501	3130.251279	6.228083	-0.029658	3.072583
149.376117	3138.313270	6.233088	-0.029739	3.076307
149.586827	3146.249955	6.238093	-0.029783	3.079959
149.961037	3154.270234	6.243098	-0.029858	3.083653
149.846649	3162.327933	6.248102	-0.029842	3.087337
150.332380	3170.327086	6.253107	-0.029938	3.091017
150.634863	3178.417419	6.258112	-0.029999	3.094727
150.614106	3186.426883	6.263117	-0.030001	3.098380
151.035172	3194.443255	6.268122	-0.030084	3.102052
151.162829	3202.482276	6.273126	-0.030113	3.105716
151.427147	3210.511012	6.278131	-0.030168	3.109378
151.485996	3218.594630	6.283136	-0.030184	3.113051
151.882464	3226.599094	6.288141	-0.030263	3.116699
152.046427	3234.639709	6.293146	-0.030299	3.120349
152.060899	3242.647357	6.298150	-0.030306	3.123973
152.432079	3250.653874	6.303155	-0.030381	3.127608
152.919903	3258.728958	6.308160	-0.030477	3.131274
153.032585	3266.742683	6.313165	-0.030503	3.134892
153.317985	3274.777166	6.318170	-0.030561	3.138523
153.616979	3282.823934	6.323174	-0.030622	3.142156
153.564667	3290.847876	6.328179	-0.030618	3.145759
153.820402	3298.903752	6.333184	-0.030670	3.149385
154.209686	3306.932310	6.338189	-0.030748	3.153001
154.484932	3314.997451	6.343194	-0.030805	3.156624
154.762167	3322.984498	6.348198	-0.030861	3.160208
154.970376	3330.981166	6.353203	-0.030905	3.163790
155.328380	3339.009596	6.358208	-0.030977	3.167388
155.395912	3347.052299	6.363213	-0.030995	3.170975
155.788394	3355.091737	6.368218	-0.031073	3.174571
156.113406	3363.130133	6.373222	-0.031139	3.178159
156.236959	3371.170421	6.378227	-0.031167	3.181736
156.432010	3379.205926	6.383232	-0.031209	3.185309
156.593054	3387.223505	6.388237	-0.031244	3.188869
156.850798	3395.285349	6.393242	-0.031297	3.192449
156.938285	3403.364130	6.398246	-0.031318	3.196025
157.057852	3411.334386	6.403251	-0.031346	3.199550
157.630262	3419.351926	6.408256	-0.031458	3.203112
157.518339	3427.408786	6.413261	-0.031442	3.206658
157.841274	3435.430561	6.418266	-0.031507	3.210202
158.191398	3443.472300	6.423270	-0.031578	3.213753
158.545665	3451.467963	6.428275	-0.031649	3.217280
158.560234	3459.523012	6.433280	-0.031657	3.220814
158.884622	3467.503702	6.438285	-0.031722	3.224325
159.213872	3475.566296	6.443290	-0.031789	3.227869
159.394571	3483.638218	6.448294	-0.031828	3.231406
159.702291	3491.684361	6.453299	-0.031890	3.234933
159.836731	3499.709025	6.458304	-0.031920	3.238440
160.041053	3507.704443	6.463309	-0.031964	3.241933
160.358520	3515.720354	6.468314	-0.032028	3.245436
160.632118	3523.736213	6.473318	-0.032084	3.248933
160.780094	3531.770996	6.478323	-0.032117	3.252430
161.079290	3539.845937	6.483328	-0.032178	3.255946
161.066744	3547.818597	6.488333	-0.032180	3.259402
161.518572	3555.840842	6.493338	-0.032270	3.262894
161.643937	3563.883706	6.498342	-0.032298	3.266378
161.815137	3571.918755	6.503347	-0.032335	3.269857
162.232863	3579.995004	6.508352	-0.032418	3.273360
162.351438	3587.994280	6.513357	-0.032446	3.276813
162.580013	3596.029074	6.518362	-0.032493	3.280283
163.018553	3604.015750	6.523366	-0.032580	3.283737
163.284131	3612.065909	6.528371	-0.032635	3.287207
163.375928	3620.118539	6.533376	-0.032657	3.290668
163.302069	3628.168367	6.538381	-0.032649	3.294118
163.922317	3636.163630	6.543386	-0.032769	3.297568
164.014824	3644.222824	6.548390	-0.032792	3.301020
164.164080	3652.191197	6.553395	-0.032825	3.304433
164.493461	3660.265194	6.558400	-0.032891	3.307894
164.582567	3668.326712	6.563405	-0.032913	3.311337
164.702620	3676.360213	6.568410	-0.032941	3.314766
165.071230	3684.333879	6.573414	-0.033014	3.318175
165.323832	3692.352611	6.578419	-0.033067	3.321595
165.471241	3700.377242	6.583424	-0.033099	3.325010
165.688214	3708.384952	6.588429	-0.033145	3.328417
165.907342	3716.439095	6.593434	-0.033191	3.331840
166.325584	3724.498954	6.598438	-0.033274	3.335270
166.449637	3732.519929	6.603443	-0.033302	3.338668
166.775882	3740.538913	6.608448	-0.033368	3.342070
167.068796	3748.526226	6.613453	-0.033428	3.345454
167.296491	3756.614063	6.618458	-0.033475	3.348874
167.393124	3764.662332	6.623462	-0.033499	3.352269
167.727281	3772.673815	6.628467	-0.033566	3.355654
168.164198	3780.682470	6.633472	-0.033652	3.359038
167.977517	3788.743364	6.638477	-0.033623	3.362418
168.439309	3796.755917	6.643482	-0.033714	3.365797
168.540304	3804.762930	6.648486	-0.033738	3.369158
168.575776	3812.814908	6.653491	-0.033750	3.372532
168.940084	3820.887268	6.658496	-0.033823	3.375923
169.190094	3828.868545	6.663501	-0.033875	3.379268
169.423476	3836.892176	6.668506	-0.033923	3.382627
169.573756	3844.938418	6.673510	-0.033956	3.385989
169.771293	3852.956519	6.678515	-0.033998	3.389338
170.141322	3861.055898	6.683520	-0.034073	3.392723
170.167202	3869.082825	6.688525	-0.034083	3.396063
170.447840	3877.048208	6.693530	-0.034140	3.399382
170.740697	3885.040809	6.698534	-0.034200	3.402710
170.790182	3893.045116	6.703539	-0.034214	3.406032
171.155248	3901.058136	6.708544	-0.034287	3.409364
171.366790	3909.082869	6.713549	-0.034332	3.412693
171.323299	3917.161603	6.718554	-0.034329	3.416032
171.597791	3925.161452	6.723558	-0.034385	3.419346
172.120813	3933.146431	6.728563	-0.034488	3.422659
172.279704	3941.202692	6.733568	-0.034522	3.425986
172.363460	3949.239664	6.738573	-0.034543	3.429299
172.780175	3957.279206	6.743578	-0.034626	3.432621
172.934102	3965.331488	6.748582	-0.034660	3.435936
172.970843	3973.331964	6.753587	-0.034672	3.439223
173.265896	3981.351854	6.758592	-0.034732	3.442523
173.722128	3989.332220	6.763597	-0.034822	3.445809
173.783510	3997.388221	6.768602	-0.034839	3.449110
173.955995	4005.482710	6.773606	-0.034876	3.452427
174.064185	4013.484783	6.778611	-0.034901	3.455701
174.527559	4021.505752	6.783616	-0.034993	3.458992
174.494083	4029.526152	6.788621	-0.034992	3.462262
174.743942	4037.572867	6.793626	-0.035044	3.465550
174.820375	4045.625065	6.798630	-0.035063	3.468831
174.953810	4053.648910	6.803635	-0.035093	3.472099
175.358554	4061.714198	6.808640	-0.035174	3.475389
175.493523	4069.666349	6.813645	-0.035204	3.478622
175.513585	4077.705114	6.818650	-0.035213	3.481883
175.965605	4085.672704	6.823654	-0.035302	3.485127
176.267702	4093.667426	6.828659	-0.035364	3.488373
176.553735	4101.738185	6.833664	-0.035422	3.491646
176.699715	4109.778137	6.838669	-0.035454	3.494900
177.067564	4117.782048	6.843674	-0.035528	3.498143
177.312434	4125.831782	6.848678	-0.035579	3.501397
177.270323	4133.823028	6.853683	-0.035576	3.504616
177.650453	4141.881253	6.858688	-0.035652	3.507872
177.797931	4149.927057	6.863693	-0.035685	3.511112
177.889545	4157.968348	6.868698	-0.035707	3.514346
178.032380	4165.975038	6.873702	-0.035739	3.517565
178.180474	4173.968485	6.878707	-0.035772	3.520776
178.477359	4181.985211	6.883712	-0.035832	3.523997
178.502847	4190.026985	6.888717	-0.035842	3.527218
179.094186	4198.047939	6.893722	-0.035957	3.530444
179.259415	4206.082250	6.898726	-0.035993	3.533660
179.330124	4214.138154	6.903731	-0.036012	3.536878
179.412988	4222.156668	6.908736	-0.036032	3.540079
179.654694	4230.167396	6.913741	-0.036082	3.543279
179.866709	4238.210460	6.918746	-0.036127	3.546488
180.150145	4246.252425	6.923750	-0.036185	3.549695
180.493212	4254.338215	6.928755	-0.036254	3.552919
180.819903	4262.402055	6.933760	-0.036320	3.556131
180.809188	4270.322832	6.938765	-0.036323	3.559273
180.989570	4278.331801	6.943770	-0.036362	3.562452
181.231550	4286.335576	6.948774	-0.036412	3.565629
181.276080	4294.329580	6.953779	-0.036426	3.568793
181.419133	4302.434873	6.958784	-0.036458	3.572001
181.519335	4310.424922	6.963789	-0.036481	3.575160
181.819658	4318.428828	6.968794	-0.036543	3.578327
182.251038	4326.470025	6.973798	-0.036628	3.581509
182.439560	4334.447428	6.978803	-0.036668	3.584657
182.853498	4342.502095	6.983808	-0.036751	3.587839
182.977186	4350.500103	6.988813	-0.036779	3.590987
183.395384	4358.538807	6.993818	-0.036862	3.594157
183.625046	4366.569721	6.998822	-0.036910	3.597315
183.637755	4374.572394	7.003827	-0.036917	3.600454
183.932107	4382.586623	7.008832	-0.036977	3.603602
184.101071	4390.601787	7.013837	-0.037014	3.606744
184.527147	4398.635276	7.018842	-0.037099	3.609898
184.766394	4406.678858	7.023846	-0.037148	3.613048
184.816441	4414.746964	7.028851	-0.037163	3.616199
185.043602	4422.736775	7.033856	-0.037210	3.619322
185.068627	4430.753432	7.038861	-0.037220	3.622447
185.370148	4438.770456	7.043866	-0.037281	3.625577
185.765796	4446.795991	7.048870	-0.037360	3.628711
185.812444	4454.847383	7.053875	-0.037374	3.631842
186.092100	4462.917679	7.058880	-0.037431	3.634984
186.158351	4470.903660	7.063885	-0.037449	3.638084
186.438146	4478.922793	7.068890	-0.037506	3.641201
186.577698	4486.898140	7.073894	-0.037537	3.644294
186.675383	4494.941313	7.078899	-0.037561	3.647410
187.246580	4502.975878	7.083904	-0.037672	3.650532
187.320429	4511.040305	7.088909	-0.037691	3.653650
187.345006	4519.080235	7.093914	-0.037701	3.656755
187.770703	4527.053566	7.098918	-0.037785	3.659842
187.899157	4535.066960	7.103923	-0.037815	3.662933
188.098641	4543.123750	7.108928	-0.037857	3.666041
188.198913	4551.108927	7.113933	-0.037881	3.669116
188.464966	4559.173387	7.118938	-0.037935	3.672223
188.505629	4567.190801	7.123942	-0.037948	3.675303
188.668811	4575.184799	7.128947	-0.037984	3.678375
188.898126	4583.266676	7.133952	-0.038032	3.681480
189.020465	4591.215857	7.138957	-0.038060	3.684529
189.145355	4599.285740	7.143962	-0.038088	3.687621
189.511837	4607.272180	7.148966	-0.038161	3.690685
189.745107	4615.297907	7.153971	-0.038210	3.693758
189.809648	4623.364418	7.158976	-0.038227	3.696840
189.868884	4631.348811	7.163981	-0.038244	3.699888
190.256077	4639.368377	7.168986	-0.038321	3.702954
190.372898	4647.400898	7.173990	-0.038348	3.706017
190.492029	4655.409606	7.178995	-0.038375	3.709068
190.796287	4663.520583	7.184000	-0.038437	3.712159
191.055074	4671.564948	7.189005	-0.038490	3.715222
190.926226	4679.539819	7.194010	-0.038472	3.718246
191.343982	4687.543705	7.199014	-0.038554	3.721292
191.580956	4695.476901	7.204019	-0.038604	3.724305
191.619488	4703.567844	7.209024	-0.038616	3.727370
191.827533	4711.558945	7.214029	-0.038660	3.730398
192.185415	4719.588448	7.219034	-0.038732	3.733443
192.181457	4727.674814	7.224038	-0.038736	3.736497
192.325849	4735.607032	7.229043	-0.038768	3.739495
192.682081	4743.681448	7.234048	-0.038840	3.742548
192.805795	4751.679376	7.239053	-0.038868	3.745565
192.951599	4759.709809	7.244058	-0.038900	3.748592
193.278722	4767.766241	7.249062	-0.038967	3.751631
193.560228	4775.783165	7.254067	-0.039024	3.754651
193.653905	4783.822443	7.259072	-0.039047	3.757673
193.480365	4791.803984	7.264077	-0.039020	3.760664
193.641353	4799.833726	7.269082	-0.039055	3.763679
193.967915	4807.878184	7.274086	-0.039121	3.766701
194.065836	4815.816409	7.279091	-0.039144	3.769675
194.546356	4823.916336	7.284096	-0.039239	3.772716
194.788390	4831.923012	7.289101	-0.039289	3.775715
194.947657	4839.924443	7.294106	-0.039324	3.778707
195.246013	4847.969941	7.299110	-0.039385	3.781716
195.262974	4855.955130	7.304115	-0.039393	3.784694
195.321421	4864.067357	7.309120	-0.039409	3.787718
195.554092	4872.024705	7.314125	-0.039458	3.790686
196.006613	4880.144910	7.319130	-0.039547	3.793717
196.120195	4888.152429	7.324134	-0.039573	3.796696
196.227635	4896.084250	7.329139	-0.039599	3.799644
196.688838	4904.111693	7.334144	-0.039690	3.802634
196.906242	4912.119545	7.339149	-0.039735	3.805608
196.947411	4920.127216	7.344154	-0.039748	3.808576
197.122512	4928.189023	7.349158	-0.039786	3.811565
197.426525	4936.194032	7.354163	-0.039848	3.814533
197.553724	4944.229173	7.359168	-0.039877	3.817506
197.630855	4952.227872	7.364173	-0.039896	3.820462
197.940906	4960.206715	7.369178	-0.039959	3.823414
198.241341	4968.261010	7.374182	-0.040020	3.826391
198.316577	4976.265934	7.379187	-0.040039	3.829342
198.449603	4984.346726	7.384192	-0.040069	3.832320
198.711091	4992.368009	7.389197	-0.040123	3.835277
199.048471	5000.353085	7.394202	-0.040191	3.838220
199.146024	5008.411516	7.399206	-0.040215	3.841183
199.276480	5016.351005	7.404211	-0.040244	3.844100
199.581762	5024.416222	7.409216	-0.040306	3.847064
199.624049	5032.411293	7.414221	-0.040319	3.849996
199.790989	5040.469511	7.419226	-0.040355	3.852950
200.200161	5048.519725	7.424230	-0.040437	3.855905
200.440617	5056.472015	7.429235	-0.040487	3.858818
200.582731	5064.564898	7.434240	-0.040518	3.861777
200.999489	5072.536096	7.439245	-0.040601	3.864696
201.157372	5080.588421	7.444250	-0.040636	3.867637
201.254373	5088.651120	7.449254	-0.040659	3.870578
201.298937	5096.871169	7.454259	-0.040673	3.873574
201.632536	5104.870061	7.459264	-0.040740	3.876492
201.592413	5112.761292	7.464269	-0.040737	3.879361
201.676077	5120.749678	7.469274	-0.040758	3.882266
202.065155	5128.717450	7.474278	-0.040836	3.885168
202.284046	5136.727091	7.479283	-0.040882	3.888078
202.543421	5144.768248	7.484288	-0.040935	3.890999
202.586326	5152.803736	7.489293	-0.040948	3.893912
202.676130	5160.841934	7.494298	-0.040970	3.896824
202.883444	5168.824780	7.499302	-0.041014	3.899716
203.134722	5176.825171	7.504307	-0.041066	3.902614
203.358280	5184.867646	7.509312	-0.041113	3.905523
203.431534	5192.888548	7.514317	-0.041132	3.908420
203.587632	5200.912023	7.519322	-0.041166	3.911317
203.976219	5208.945146	7.524326	-0.041243	3.914220
204.105238	5216.928354	7.529331	-0.041273	3.917098
204.398947	5224.942920	7.534336	-0.041333	3.919988
204.532961	5232.984689	7.539341	-0.041363	3.922883
204.502063	5240.972172	7.544346	-0.041362	3.925753
204.798305	5249.034194	7.549350	-0.041422	3.928654
204.917984	5257.002406	7.554355	-0.041450	3.931515
205.295600	5265.075032	7.559360	-0.041525	3.934417
205.184112	5273.082332	7.564365	-0.041510	3.937284
205.561580	5281.062388	7.569370	-0.041585	3.940148
205.933407	5289.086230	7.574374	-0.041660	3.943026
205.919373	5297.113303	7.579379	-0.041662	3.945895
206.082414	5305.162867	7.584384	-0.041698	3.948774
206.080217	5313.206351	7.589389	-0.041703	3.951646
206.449815	5321.241940	7.594394	-0.041777	3.954519
206.561620	5329.218087	7.599398	-0.041803	3.957364
206.832966	5337.180915	7.604403	-0.041858	3.960206
207.116455	5345.237609	7.609408	-0.041916	3.963079
207.056993	5353.264932	7.614413	-0.041910	3.965933
207.343151	5361.243723	7.619418	-0.041969	3.968774
207.773293	5369.279537	7.624422	-0.042054	3.971636
207.756738	5377.293236	7.629427	-0.042056	3.974480
207.966168	5385.345153	7.634432	-0.042100	3.977339
208.033529	5393.347076	7.639437	-0.042118	3.980177
208.233758	5401.359107	7.644442	-0.042161	3.983018
208.192662	5409.423497	7.649446	-0.042158	3.985871
208.198174	5417.449989	7.654451	-0.042164	3.988710
208.609296	5425.497036	7.659456	-0.042246	3.991561
208.845397	5433.466105	7.664461	-0.042295	3.994379
208.892781	5441.516816	7.669466	-0.042309	3.997221
209.194011	5449.508561	7.674470	-0.042370	4.000044
209.328976	5457.533140	7.679475	-0.042401	4.002874
209.627164	5465.548094	7.684480	-0.042461	4.005701
209.658723	5473.569321	7.689485	-0.042473	4.008525
210.121364	5481.627504	7.694490	-0.042564	4.011366
210.321062	5489.667799	7.699494	-0.042606	4.014194
210.302911	5497.677298	7.704499	-0.042608	4.017007
210.481815	5505.681903	7.709504	-0.042647	4.019818
210.831194	5513.700710	7.714509	-0.042717	4.022636
210.973509	5521.680014	7.719514	-0.042748	4.025434
211.262091	5529.729897	7.724518	-0.042807	4.028257
211.514544	5537.754104	7.729523	-0.042860	4.031069
211.601900	5545.896569	7.734528	-0.042881	4.033917
211.983378	5553.868592	7.739533	-0.042957	4.036709
212.263897	5561.778185	7.744538	-0.043015	4.039475
212.304982	5569.854812	7.749542	-0.043027	4.042294
212.524456	5577.776358	7.754547	-0.043073	4.045059
212.786659	5585.818129	7.759552	-0.043127	4.047865
213.025712	5593.830697	7.764557	-0.043177	4.050659
212.796442	5601.915219	7.769562	-0.043140	4.053468
213.009745	5609.960738	7.774566	-0.043185	4.056269
213.169363	5617.921572	7.779571	-0.043219	4.059038
213.245893	5625.975893	7.784576	-0.043239	4.061836
213.485956	5633.947175	7.789581	-0.043289	4.064605
213.620852	5641.965235	7.794586	-0.043319	4.067388
214.013071	5649.997282	7.799590	-0.043397	4.070176
214.046470	5658.024318	7.804595	-0.043409	4.072957
214.359170	5666.050995	7.809600	-0.043472	4.075739
214.514981	5674.051669	7.814605	-0.043506	4.078508
214.715567	5682.051542	7.819610	-0.043549	4.081275
214.861531	5690.073579	7.824614	-0.043581	4.084047
215.073409	5698.095810	7.829619	-0.043626	4.086819
215.303453	5706.130110	7.834624	-0.043674	4.089593
215.255169	5714.163666	7.839629	-0.043670	4.092360
215.552014	5722.139305	7.844634	-0.043730	4.095111
215.802135	5730.178511	7.849638	-0.043782	4.097881
215.681353	5738.184024	7.854643	-0.043765	4.100633
216.042504	5746.252673	7.859648	-0.043837	4.103411
216.137372	5754.262571	7.864653	-0.043860	4.106163
216.150879	5762.269157	7.869658	-0.043868	4.108912
216.412715	5770.314508	7.874662	-0.043922	4.111675
216.497393	5778.361126	7.879667	-0.043943	4.114434
216.828341	5786.376610	7.884672	-0.044010	4.117184
216.977941	5794.355088	7.889677	-0.044043	4.119917
217.373192	5802.344432	7.894682	-0.044121	4.122655
217.561635	5810.370639	7.899686	-0.044162	4.125401
217.328147	5818.376621	7.904691	-0.044123	4.128133
217.763243	5826.426538	7.909696	-0.044210	4.130887
217.957259	5834.424856	7.914701	-0.044251	4.133618
218.018555	5842.482808	7.919706	-0.044267	4.136366
218.102472	5850.477508	7.924710	-0.044288	4.139091
218.590751	5858.519945	7.929715	-0.044384	4.141835
218.736405	5866.488310	7.934720	-0.044417	4.144548
218.823793	5874.539335	7.939725	-0.044438	4.147287
219.093859	5882.538758	7.944730	-0.044494	4.150008
219.388790	5890.642009	7.949734	-0.044554	4.152763
219.464147	5898.642441	7.954739	-0.044573	4.155479
219.600872	5906.639578	7.959744	-0.044604	4.158193
219.722981	5914.665543	7.964749	-0.044631	4.160914
219.891328	5922.632537	7.969754	-0.044668	4.163614
220.066459	5930.674675	7.974758	-0.044706	4.166338
219.995979	5938.672279	7.979763	-0.044698	4.169043
220.314477	5946.734062	7.984768	-0.044762	4.171771
220.343739	5954.737878	7.989773	-0.044773	4.174475
220.605953	5962.750273	7.994778	-0.044827	4.177183
220.803155	5970.773830	7.999782	-0.044869	4.179892
220.870277	5978.731912	8.004787	-0.044887	4.182575
221.064145	5986.779995	8.009792	-0.044928	4.185289
221.265966	5994.838696	8.014797	-0.044971	4.188005
221.353365	6002.811731	8.019802	-0.044992	4.190688
221.687164	6010.970570	8.024806	-0.045059	4.193435
221.855671	6018.951500	8.029811	-0.045096	4.196119
221.925201	6026.895178	8.034816	-0.045114	4.198787
221.858445	6034.921742	8.039821	-0.045107	4.201480
222.318487	6042.835484	8.044826	-0.045198	4.204139
222.688647	6050.965004	8.049830	-0.045272	4.206868
222.523832	6058.886168	8.054835	-0.045246	4.209520
222.589363	6066.984334	8.059840	-0.045264	4.212231
222.884793	6075.005131	8.064845	-0.045324	4.214917
223.014190	6082.984819	8.069850	-0.045353	4.217586
223.248123	6091.001064	8.074854	-0.045402	4.220267
223.407783	6098.979830	8.079859	-0.045437	4.222932
223.709834	6107.010025	8.084864	-0.045498	4.225615
223.899720	6115.050634	8.089869	-0.045539	4.228298
223.987338	6123.058195	8.094874	-0.045560	4.230967
224.193865	6131.142417	8.099878	-0.045604	4.233661
224.336306	6139.145527	8.104883	-0.045636	4.236326
224.656035	6147.140203	8.109888	-0.045700	4.238988
224.871848	6155.138307	8.114893	-0.045746	4.241649
225.161787	6163.096182	8.119898	-0.045805	4.244295
225.348268	6171.174005	8.124902	-0.045845	4.246979
225.610309	6179.183369	8.129907	-0.045899	4.249638
225.930605	6187.232985	8.134912	-0.045963	4.252310
225.812022	6195.283862	8.139917	-0.045947	4.254977
225.899706	6203.265262	8.144922	-0.045968	4.257620
226.105095	6211.292825	8.149926	-0.046011	4.260279
226.321246	6219.261934	8.154931	-0.046057	4.262916
226.489168	6227.305397	8.159936	-0.046093	4.265576
226.733481	6235.319780	8.164941	-0.046144	4.268225
226.952937	6243.362610	8.169946	-0.046190	4.270882
227.026757	6251.450330	8.174950	-0.046209	4.273551
227.094863	6259.471299	8.179955	-0.046227	4.276196
227.524048	6267.443412	8.184960	-0.046312	4.278826
227.638524	6275.487467	8.189965	-0.046338	4.281476
227.578906	6283.435636	8.194970	-0.046333	4.284091
227.809408	6291.503834	8.199974	-0.046381	4.286746
227.865867	6299.461762	8.204979	-0.046396	4.289362
228.207404	6307.543009	8.209984	-0.046465	4.292019
228.432041	6315.579962	8.214989	-0.046512	4.294659
228.391060	6323.562758	8.219994	-0.046510	4.297278
228.466986	6331.595209	8.224998	-0.046529	4.299912
228.431540	6339.568579	8.230003	-0.046528	4.302524
228.794211	6347.562096	8.235008	-0.046600	4.305144
229.178370	6355.651744	8.240013	-0.046677	4.307794
229.025125	6363.620673	8.245018	-0.046654	4.310399
229.383794	6371.724835	8.250022	-0.046726	4.313051
229.584873	6379.651334	8.255027	-0.046768	4.315641
229.530391	6387.688975	8.260032	-0.046763	4.318265
229.613002	6395.742740	8.265037	-0.046784	4.320893
229.951642	6403.700872	8.270042	-0.046852	4.323490
230.309517	6411.740176	8.275046	-0.046924	4.326112
230.495296	6419.711590	8.280051	-0.046964	4.328710
230.650382	6427.784504	8.285056	-0.046998	4.331338
230.917249	6435.814838	8.290061	-0.047053	4.333952
230.915631	6443.838614	8.295066	-0.047057	4.336560
231.115511	6451.815828	8.300070	-0.047100	4.339153
231.404051	6459.806611	8.305075	-0.047159	4.341749
231.445340	6467.824796	8.310080	-0.047172	4.344351
231.507736	6475.883009	8.315085	-0.047188	4.346964
231.744896	6483.882770	8.320090	-0.047238	4.349558
232.001744	6491.953541	8.325094	-0.047291	4.352174
231.944458	6499.998940	8.330099	-0.047285	4.354778
232.233892	6508.011333	8.335104	-0.047344	4.357371
232.453048	6515.952732	8.340109	-0.047390	4.359940
232.283037	6523.928749	8.345114	-0.047364	4.362516
232.745940	6531.923280	8.350118	-0.047455	4.365101
232.883017	6539.991887	8.355123	-0.047486	4.367705
232.973288	6548.005258	8.360128	-0.047508	4.370290
233.259397	6556.046870	8.365133	-0.047566	4.372884
233.383194	6564.054707	8.370138	-0.047595	4.375464
233.547133	6572.068530	8.375142	-0.047630	4.378045
233.708930	6580.058077	8.380147	-0.047666	4.380617
234.119635	6588.078018	8.385152	-0.047747	4.383198
234.128185	6596.101270	8.390157	-0.047754	4.385777
234.211075	6604.112388	8.395162	-0.047775	4.388350
234.530486	6612.167913	8.400166	-0.047839	4.390938
234.631921	6620.172695	8.405171	-0.047863	4.393506
234.760639	6628.204148	8.410176	-0.047893	4.396082
235.000601	6636.181969	8.415181	-0.047942	4.398639
235.046090	6644.212630	8.420186	-0.047956	4.401211
235.281923	6652.187315	8.425190	-0.048005	4.403765
235.200863	6660.191403	8.430195	-0.047995	4.406324
235.529865	6668.238479	8.435200	-0.048062	4.408898
235.676856	6676.304035	8.440205	-0.048094	4.411476
235.545098	6684.309294	8.445210	-0.048075	4.414031
235.871306	6692.391338	8.450214	-0.048141	4.416612
236.071822	6700.321531	8.455219	-0.048183	4.419142
236.276021	6708.389551	8.460224	-0.048226	4.421715
236.258452	6716.345074	8.465229	-0.048228	4.424249
236.307399	6724.420911	8.470234	-0.048243	4.426820
236.519261	6732.462796	8.475238	-0.048287	4.429380
236.367482	6740.469446	8.480243	-0.048264	4.431925
236.909362	6748.452197	8.485248	-0.048370	4.434465
237.222745	6756.515681	8.490253	-0.048434	4.437027
237.253726	6764.455020	8.495258	-0.048445	4.439548
237.367887	6772.573963	8.500262	-0.048471	4.442124
237.503521	6780.470856	8.505267	-0.048502	4.444628
237.721364	6788.555469	8.510272	-0.048547	4.447191
237.956935	6796.545020	8.515277	-0.048596	4.449722
238.078699	6804.594934	8.520282	-0.048624	4.452271
238.234465	6812.623423	8.525286	-0.048658	4.454811
238.311090	6820.613092	8.530291	-0.048678	4.457338
238.465607	6828.624175	8.535296	-0.048712	4.459870
238.653038	6836.670141	8.540301	-0.048752	4.462411
238.779029	6844.627501	8.545306	-0.048781	4.464923
239.003669	6852.686269	8.550310	-0.048828	4.467466
239.237438	6860.659479	8.555315	-0.048876	4.469980
239.287878	6868.750335	8.560320	-0.048891	4.472530
239.362537	6876.770200	8.565325	-0.048910	4.475056
239.521327	6884.758003	8.570330	-0.048945	4.477570
239.747704	6892.739722	8.575335	-0.048992	4.480081
239.873811	6900.753880	8.580339	-0.049021	4.482601
239.918148	6908.754554	8.585344	-0.049034	4.485115
240.243362	6916.798701	8.590349	-0.049100	4.487642
240.406615	6924.761539	8.595354	-0.049135	4.490141
240.588732	6932.851170	8.600359	-0.049175	4.492679
240.410332	6940.836279	8.605363	-0.049146	4.495182
240.638337	6948.876847	8.610368	-0.049194	4.497702
240.695460	6956.854750	8.615373	-0.049210	4.500200
240.771624	6964.878859	8.620378	-0.049229	4.502711
241.304233	6972.890558	8.625383	-0.049334	4.505219
241.182936	6980.908469	8.630387	-0.049316	4.507725
241.426523	6988.935785	8.635392	-0.049367	4.510233
241.536415	6997.016758	8.640397	-0.049392	4.512757
241.529747	7005.009157	8.645402	-0.049396	4.515251
241.675235	7013.024838	8.650407	-0.049429	4.517751
241.754610	7020.977396	8.655411	-0.049449	4.520230
242.191587	7028.998911	8.660416	-0.049535	4.522730
242.289354	7036.981314	8.665421	-0.049558	4.525216
242.274229	7044.986994	8.670426	-0.049561	4.527708
242.524674	7053.038479	8.675431	-0.049613	4.530212
242.821427	7061.063082	8.680435	-0.049673	4.532707
242.905274	7069.107647	8.685440	-0.049694	4.535207
243.235867	7077.127022	8.690445	-0.049761	4.537698
243.423629	7085.078328	8.695450	-0.049801	4.540166
243.629911	7093.127570	8.700455	-0.049844	4.542663
243.558910	7101.124434	8.705459	-0.049836	4.545141
243.883651	7109.146715	8.710464	-0.049902	4.547627
243.984660	7117.190807	8.715469	-0.049926	4.550119
244.026072	7125.196260	8.720474	-0.049939	4.552596
244.255699	7133.237510	8.725479	-0.049987	4.555084
244.422707	7141.235052	8.730483	-0.050023	4.557556
244.377703	7149.214689	8.735488	-0.050020	4.560022
244.728230	7157.264739	8.740493	-0.050090	4.562508
244.838395	7165.207969	8.745498	-0.050116	4.564960
245.030835	7173.312127	8.750503	-0.050157	4.567460
245.231542	7181.262761	8.755507	-0.050200	4.569911
245.342511	7189.357914	8.760512	-0.050225	4.572406
245.590692	7197.374965	8.765517	-0.050277	4.574875
245.746563	7205.410932	8.770522	-0.050311	4.577349
245.900342	7213.400563	8.775527	-0.050345	4.579807
245.816551	7221.406347	8.780531	-0.050334	4.582268
246.047216	7229.405488	8.785536	-0.050383	4.584726
246.144095	7237.506930	8.790541	-0.050406	4.587214
246.489271	7245.424104	8.795546	-0.050475	4.589645
246.746288	7253.551392	8.800551	-0.050528	4.592139
246.612783	7261.516819	8.805555	-0.050509	4.594581
246.736648	7269.572683	8.810560	-0.050537	4.597050
247.224076	7277.476490	8.815565	-0.050633	4.599471
247.259840	7285.546308	8.820570	-0.050645	4.601941
247.605217	7293.511010	8.825575	-0.050714	4.604378
247.470290	7301.568214	8.830579	-0.050694	4.606842
247.542070	7309.520264	8.835584	-0.050713	4.609273
247.700881	7317.599196	8.840589	-0.050747	4.611741
248.014304	7325.636487	8.845594	-0.050811	4.614195
248.156028	7333.687376	8.850599	-0.050843	4.616651
248.273953	7341.606426	8.855603	-0.050870	4.619066
248.378118	7349.654653	8.860608	-0.050894	4.621520
248.535958	7357.629340	8.865613	-0.050929	4.623949
248.543576	7365.694303	8.870618	-0.050935	4.626405
248.808074	7373.712537	8.875623	-0.050990	4.628845
248.918350	7381.751341	8.880627	-0.051016	4.631290
249.045963	7389.754408	8.885632	-0.051044	4.633723
249.165465	7397.784335	8.890637	-0.051072	4.636163
249.424793	7405.730375	8.895642	-0.051125	4.638576
249.372220	7413.836400	8.900647	-0.051121	4.641037
249.485791	7421.742242	8.905651	-0.051147	4.643435
249.804096	7429.821631	8.910656	-0.051212	4.645884
249.854357	7437.814025	8.915661	-0.051226	4.648306
249.969275	7445.813891	8.920666	-0.051253	4.650729
250.310744	7453.891910	8.925671	-0.051321	4.653175
250.397569	7461.886799	8.930675	-0.051343	4.655594
250.508557	7469.894231	8.935680	-0.051369	4.658015
250.705227	7477.935119	8.940685	-0.051410	4.660445
251.018303	7485.921811	8.945690	-0.051474	4.662858
251.189217	7493.971151	8.950695	-0.051511	4.665288
251.199233	7501.912325	8.955699	-0.051518	4.667684
251.502397	7509.924108	8.960704	-0.051579	4.670100
251.708473	7518.054704	8.965709	-0.051623	4.672551
251.666489	7526.062021	8.970714	-0.051620	4.674964
251.720190	7534.096757	8.975719	-0.051636	4.677383
251.916361	7542.040970	8.980723	-0.051677	4.679774
252.155289	7550.014470	8.985728	-0.051727	4.682172
252.528473	7557.983559	8.990733	-0.051802	4.684568
252.335586	7566.058567	8.995738	-0.051771	4.686995
252.468576	7574.052304	9.000743	-0.051801	4.689396
252.424638	7582.086556	9.005747	-0.051798	4.691808
252.761109	7590.110695	9.010752	-0.051866	4.694215
252.983958	7598.157091	9.015757	-0.051912	4.696628
252.904106	7606.062949	9.020762	-0.051903	4.698997
252.926621	7614.138175	9.025767	-0.051912	4.701417
253.234733	7622.143482	9.030771	-0.051975	4.703813
253.411000	7630.160380	9.035776	-0.052013	4.706212
253.567935	7638.243937	9.040781	-0.052047	4.708630
253.619432	7646.227498	9.045786	-0.052062	4.711017
253.816413	7654.276898	9.050791	-0.052104	4.713421
253.769714	7662.261602	9.055795	-0.052100	4.715806
253.932712	7670.237431	9.060800	-0.052136	4.718187
254.227812	7678.262439	9.065805	-0.052196	4.720581
254.191315	7686.229073	9.070810	-0.052194	4.722956
254.320157	7694.322713	9.075815	-0.052223	4.725368
254.495938	7702.373802	9.080819	-0.052261	4.727766
254.739859	7710.373052	9.085824	-0.052312	4.730148
254.768290	7718.412169	9.090829	-0.052322	4.732540
254.907392	7726.366156	9.095834	-0.052353	4.734906
255.380999	7734.438817	9.100839	-0.052447	4.737304
255.452499	7742.418187	9.105843	-0.052465	4.739675
255.600213	7750.419192	9.110848	-0.052498	4.742051
255.695354	7758.425829	9.115853	-0.052521	4.744427
255.662859	7766.446745	9.120858	-0.052520	4.746807
255.897367	7774.515641	9.125863	-0.052569	4.749199
256.024035	7782.519033	9.130867	-0.052598	4.751571
256.086918	7790.535251	9.135872	-0.052614	4.753946
256.045636	7798.581741	9.140877	-0.052612	4.756328
256.387326	7806.499531	9.145882	-0.052681	4.758671
256.534835	7814.581645	9.150887	-0.052713	4.761061
256.662248	7822.499704	9.155891	-0.052742	4.763401
256.756440	7830.530154	9.160896	-0.052765	4.765774
256.920713	7838.590892	9.165901	-0.052801	4.768154
256.901974	7846.603710	9.170906	-0.052802	4.770520
256.999171	7854.666437	9.175911	-0.052826	4.772898
257.197718	7862.612775	9.180915	-0.052868	4.775241
257.567396	7870.640569	9.185920	-0.052942	4.777606
257.514776	7878.655189	9.190925	-0.052937	4.779968
257.518889	7886.673470	9.195930	-0.052943	4.782329
257.881037	7894.636984	9.200935	-0.053016	4.784671
258.058533	7902.714494	9.205939	-0.053054	4.787047
257.959013	7910.715708	9.210944	-0.053041	4.789400
258.280474	7918.769363	9.215949	-0.053106	4.791765
258.203497	7926.774565	9.220954	-0.053097	4.794117
258.437988	7934.803151	9.225959	-0.053145	4.796473
258.585704	7942.781281	9.230963	-0.053178	4.798814
258.703927	7950.779960	9.235968	-0.053205	4.801159
258.727820	7958.775833	9.240973	-0.053215	4.803503
258.884334	7966.792604	9.245978	-0.053249	4.805852
259.382678	7974.856046	9.250983	-0.053347	4.808211
259.396140	7982.838069	9.255987	-0.053355	4.810548
259.482435	7990.355553	9.260992	-0.053376	4.812747
259.694704	7994.912582	9.265997	-0.053418	4.814079

259.701703	7997.405657	9.271002	-0.053421	4.814808
259.805171	7998.811465	9.276007	-0.053441	4.815218
259.841158	7999.234912	9.281011	-0.053448	4.815342
259.932621	8000.163324	9.286016	-0.053466	4.815613
259.824292	8000.239511	9.291021	-0.053446	4.815636
259.884404	8000.184956	9.296026	-0.053457	4.815619
260.193978	8000.212428	9.301031	-0.053514	4.815626
260.136515	8000.246728	9.306035	-0.053504	4.815636
260.094625	8000.188373	9.311040	-0.053496	4.815619
260.116003	8000.234638	9.316045	-0.053500	4.815633
260.350845	8000.213903	9.321050	-0.053543	4.815626
260.424875	8000.217243	9.326055	-0.053557	4.815626
260.349445	8000.257658	9.331059	-0.053543	4.815638
260.388319	8000.223046	9.336064	-0.053550	4.815628
260.494213	8000.321952	9.341069	-0.053570	4.815656
260.552031	8000.219302	9.346074	-0.053581	4.815626
260.763149	8000.239830	9.351079	-0.053620	4.815631
260.546923	8000.274743	9.356083	-0.053580	4.815642
260.558964	8000.182025	9.361088	-0.053582	4.815615
260.891366	8000.333754	9.366093	-0.053644	4.815658
260.877959	8000.273726	9.371098	-0.053641	4.815641
260.732479	8000.298046	9.376103	-0.053614	4.815648
260.655110	8000.233771	9.381107	-0.053599	4.815630
260.938685	8000.226647	9.386112	-0.053652	4.815626
260.966104	8000.321070	9.391117	-0.053657	4.815654
260.797215	8000.252097	9.396122	-0.053626	4.815635
261.000991	8000.244739	9.401127	-0.053664	4.815631
261.079646	8000.206505	9.406131	-0.053678	4.815620
261.030234	8000.201423	9.411136	-0.053669	4.815619
260.985825	8000.263703	9.416141	-0.053661	4.815637
261.206082	8000.263022	9.421146	-0.053702	4.815636
261.279686	8000.283443	9.426151	-0.053715	4.815641
261.103462	8000.274155	9.431155	-0.053683	4.815640
261.313697	8000.277582	9.436160	-0.053722	4.815640
261.369708	8000.287036	9.441165	-0.053732	4.815642
261.077061	8000.291867	9.446170	-0.053678	4.815645
261.235685	8000.302996	9.451175	-0.053707	4.815647
261.305576	8000.261415	9.456179	-0.053720	4.815635
261.229124	8000.234532	9.461184	-0.053706	4.815627
261.416722	8000.305939	9.466189	-0.053741	4.815647
261.379793	8000.259410	9.471194	-0.053734	4.815634
261.441377	8000.293518	9.476199	-0.053745	4.815644
261.350232	8000.325134	9.481203	-0.053728	4.815653
261.405274	8000.319620	9.486208	-0.053738	4.815651
261.517956	8000.327864	9.491213	-0.053759	4.815653
261.280371	8000.244952	9.496218	-0.053715	4.815630
261.380688	8000.290372	9.501223	-0.053734	4.815643
261.464920	8000.298151	9.506227	-0.053749	4.815645
261.447662	8000.290390	9.511232	-0.053746	4.815643
261.385083	8000.304316	9.516237	-0.053734	4.815647
261.605019	8000.275863	9.521242	-0.053775	4.815638
261.703510	8000.356497	9.526247	-0.053793	4.815661
261.477482	8000.369890	9.531251	-0.053751	4.815666
261.535165	8000.328109	9.536256	-0.053762	4.815653
261.653030	8000.337505	9.541261	-0.053784	4.815656
261.514896	8000.291460	9.546266	-0.053758	4.815643
261.602373	8000.322787	9.551271	-0.053774	4.815651
261.621892	8000.309218	9.556275	-0.053778	4.815647
261.752664	8000.268630	9.561280	-0.053802	4.815635
261.671568	8000.296137	9.566285	-0.053787	4.815643
261.705877	8000.241159	9.571290	-0.053793	4.815627
261.871035	8000.323949	9.576295	-0.053824	4.815651
261.571495	8000.299832	9.581299	-0.053768	4.815645
261.796815	8000.297098	9.586304	-0.053810	4.815643
261.804377	8000.368772	9.591309	-0.053812	4.815664
261.514227	8000.311701	9.596314	-0.053758	4.815649
261.576300	8000.318050	9.601319	-0.053769	4.815650
261.862147	8000.343004	9.606323	-0.053822	4.815656
261.718676	8000.332114	9.611328	-0.053796	4.815654
261.871207	8000.369844	9.616333	-0.053824	4.815664
261.895890	8000.347815	9.621338	-0.053828	4.815657
261.931284	8000.349457	9.626343	-0.053835	4.815658
261.936697	8000.353814	9.631347	-0.053836	4.815659
261.910005	8000.302111	9.636352	-0.053831	4.815644
261.851438	8000.344938	9.641357	-0.053820	4.815657
261.835194	8000.339329	9.646362	-0.053817	4.815655
261.973755	8000.371491	9.651367	-0.053843	4.815664
261.977289	8000.343777	9.656371	-0.053843	4.815656
261.862010	8000.332279	9.661376	-0.053822	4.815653
261.851474	8000.380162	9.666381	-0.053820	4.815667
261.795148	8000.321568	9.671386	-0.053809	4.815650
261.782969	8000.374763	9.676391	-0.053807	4.815666
261.824392	8000.338057	9.681395	-0.053815	4.815655
261.963147	8000.367018	9.686400	-0.053840	4.815663
262.110944	8000.320300	9.691405	-0.053868	4.815648
262.017801	8000.286736	9.696410	-0.053850	4.815639
261.966031	8000.341422	9.701415	-0.053841	4.815655
262.146701	8000.356116	9.706419	-0.053874	4.815659
262.006621	8000.371980	9.711424	-0.053848	4.815664
261.799005	8000.401693	9.716429	-0.053810	4.815674
261.970574	8000.344684	9.721434	-0.053841	4.815656
262.089663	8000.326333	9.726439	-0.053864	4.815650
262.037660	8000.327616	9.731443	-0.053854	4.815651
261.922815	8000.289426	9.736448	-0.053832	4.815640
261.818456	8000.346456	9.741453	-0.053813	4.815657
261.826579	8000.310274	9.746458	-0.053814	4.815647
261.794441	8000.362076	9.751463	-0.053808	4.815662
261.959053	8000.383984	9.756467	-0.053839	4.815668
262.082023	8000.387056	9.761472	-0.053862	4.815668
262.076883	8000.375220	9.766477	-0.053861	4.815665
261.884285	8000.343236	9.771482	-0.053825	4.815656
261.888486	8000.342232	9.776487	-0.053826	4.815656
262.021815	8000.357221	9.781491	-0.053850	4.815660
262.040106	8000.342564	9.786496	-0.053854	4.815655
262.064438	8000.405969	9.791501	-0.053858	4.815674
261.988914	8000.338516	9.796506	-0.053844	4.815654
261.893548	8000.348703	9.801511	-0.053826	4.815658
261.833668	8000.355197	9.806515	-0.053815	4.815660
261.992509	8000.394098	9.811520	-0.053845	4.815670
261.840112	8000.395878	9.816525	-0.053816	4.815672
261.891752	8000.344386	9.821530	-0.053826	4.815656
262.030743	8000.380827	9.826535	-0.053852	4.815666
261.911687	8000.355383	9.831539	-0.053830	4.815660
261.814851	8000.314283	9.836544	-0.053811	4.815648
262.008825	8000.345214	9.841549	-0.053847	4.815656
261.988360	8000.363032	9.846554	-0.053844	4.815661
262.068985	8000.376092	9.851559	-0.053859	4.815665
262.080457	8000.341032	9.856563	-0.053861	4.815655
262.252471	8000.328885	9.861568	-0.053893	4.815650
262.195888	8000.396308	9.866573	-0.053882	4.815670
262.162425	8000.377602	9.871578	-0.053876	4.815665
262.104438	8000.344612	9.876583	-0.053865	4.815656
262.201129	8000.393178	9.881587	-0.053883	4.815669
262.109322	8000.367111	9.886592	-0.053866	4.815662
262.286059	8000.352906	9.891597	-0.053899	4.815657
262.318829	8000.325669	9.896602	-0.053905	4.815649
262.061586	8000.372728	9.901607	-0.053857	4.815664
262.183538	8000.352288	9.906611	-0.053879	4.815657
262.216525	8000.375250	9.911616	-0.053886	4.815664
262.180278	8000.381062	9.916621	-0.053879	4.815666
262.174068	8000.353189	9.921626	-0.053878	4.815658
262.214484	8000.349573	9.926631	-0.053885	4.815656
262.218763	8000.363523	9.931635	-0.053886	4.815660
262.278041	8000.382643	9.936640	-0.053897	4.815666
262.374223	8000.404502	9.941645	-0.053915	4.815672
262.244000	8000.343632	9.946650	-0.053890	4.815655
262.177769	8000.368178	9.951655	-0.053878	4.815662
262.014740	8000.368715	9.956659	-0.053848	4.815663
262.233183	8000.317811	9.961664	-0.053888	4.815647
262.416521	8000.393425	9.966669	-0.053922	4.815668
262.296527	8000.329518	9.971674	-0.053900	4.815650
262.236373	8000.346687	9.976679	-0.053889	4.815656
262.320875	8000.359811	9.981683	-0.053904	4.815659
262.156514	8000.366735	9.986688	-0.053874	4.815662
262.386296	8000.399319	9.991693	-0.053916	4.815670
262.452546	8000.342726	9.996698	-0.053929	4.815653
262.431485	8000.388302	10.001703	-0.053925	4.815667
262.390684	8000.400447	10.006707	-0.053917	4.815670
262.365252	8000.400028	10.011712	-0.053912	4.815670
262.577370	8000.404557	10.016717	-0.053952	4.815671
262.464074	8000.327943	10.021722	-0.053931	4.815649
262.572284	8000.386310	10.026727	-0.053951	4.815665
262.487827	8000.393470	10.031731	-0.053935	4.815668
262.355150	8000.330424	10.036736	-0.053910	4.815650
262.624496	8000.398899	10.041741	-0.053960	4.815669
262.462280	8000.362069	10.046746	-0.053930	4.815659
262.353344	8000.357082	10.051751	-0.053910	4.815658
262.339510	8000.336561	10.056755	-0.053907	4.815652
262.359934	8000.326210	10.061760	-0.053911	4.815649
262.490547	8000.428731	10.066765	-0.053935	4.815678
262.422504	8000.357128	10.071770	-0.053922	4.815658
262.411608	8000.387918	10.076775	-0.053920	4.815667
262.590396	8000.386562	10.081779	-0.053954	4.815665
262.579170	8000.316955	10.086784	-0.053951	4.815645
262.520907	8000.422799	10.091789	-0.053941	4.815676
262.452164	8000.401380	10.096794	-0.053928	4.815670
262.517527	8000.396036	10.101799	-0.053940	4.815669
262.268105	8000.379143	10.106803	-0.053893	4.815665
262.555109	8000.395574	10.111808	-0.053947	4.815668
262.580155	8000.441903	10.116813	-0.053951	4.815682
262.608502	8000.413526	10.121818	-0.053957	4.815673
262.438273	8000.405402	10.126823	-0.053925	4.815672
262.448525	8000.397021	10.131827	-0.053927	4.815669
262.421132	8000.358122	10.136832	-0.053922	4.815658
262.522643	8000.369388	10.141837	-0.053940	4.815661
262.678554	8000.377271	10.146842	-0.053969	4.815662
262.627678	8000.386048	10.151847	-0.053960	4.815665
262.481205	8000.342000	10.156851	-0.053933	4.815653
262.605283	8000.290623	10.161856	-0.053956	4.815637
262.699421	8000.364780	10.166861	-0.053973	4.815659
262.512501	8000.320071	10.171866	-0.053938	4.815646
262.546117	8000.313140	10.176871	-0.053945	4.815644
262.765121	8000.393609	10.181875	-0.053985	4.815667
262.552857	8000.344214	10.186880	-0.053946	4.815653
262.565741	8000.370053	10.191885	-0.053948	4.815661
262.640770	8000.357390	10.196890	-0.053962	4.815657
262.745331	8000.372978	10.201895	-0.053981	4.815661
262.636332	8000.356242	10.206899	-0.053961	4.815656
262.556834	8000.376299	10.211904	-0.053946	4.815663
262.663902	8000.386588	10.216909	-0.053966	4.815665
262.623636	8000.328255	10.221914	-0.053959	4.815648
262.644112	8000.362761	10.226919	-0.053962	4.815658
262.612491	8000.341949	10.231923	-0.053956	4.815652
262.545975	8000.283187	10.236928	-0.053944	4.815636
262.665615	8000.384461	10.241933	-0.053966	4.815665
262.656257	8000.350128	10.246938	-0.053964	4.815655
262.678249	8000.355823	10.251943	-0.053968	4.815656
262.714911	8000.331854	10.256947	-0.053975	4.815649
262.749901	8000.314266	10.261952	-0.053982	4.815644
262.824609	8000.333638	10.266957	-0.053996	4.815649
262.622753	8000.319657	10.271962	-0.053958	4.815646
262.695559	8000.358222	10.276967	-0.053971	4.815657
262.843214	8000.396942	10.281971	-0.053999	4.815667
262.735105	8000.327888	10.286976	-0.053979	4.815648
262.649990	8000.395914	10.291981	-0.053963	4.815668
262.550889	8000.320600	10.296986	-0.053944	4.815646
262.717604	8000.325455	10.301991	-0.053975	4.815647
262.550972	8000.345157	10.306995	-0.053944	4.815654
262.546337	8000.331193	10.312000	-0.053943	4.815650
262.791088	8000.345867	10.317005	-0.053989	4.815653
262.889878	8000.348545	10.322010	-0.054007	4.815653
262.504259	8000.351854	10.327015	-0.053935	4.815656
262.566040	8000.359267	10.332019	-0.053947	4.815658
262.583437	8000.293332	10.337024	-0.053950	4.815638
262.689181	8000.352727	10.342029	-0.053970	4.815655
262.650542	8000.323256	10.347034	-0.053962	4.815647
262.813634	8000.330188	10.352039	-0.053993	4.815648
262.685833	8000.333436	10.357043	-0.053969	4.815650
262.587177	8000.332889	10.362048	-0.053950	4.815650
262.815657	8000.385745	10.367053	-0.053993	4.815664
262.848637	8000.358512	10.372058	-0.053999	4.815656
262.612729	8000.320479	10.377063	-0.053955	4.815646
262.927527	8000.359792	10.382067	-0.054014	4.815656
262.807038	8000.332188	10.387072	-0.053991	4.815649
262.925689	8000.304218	10.392077	-0.054013	4.815640
262.762788	8000.343206	10.397082	-0.053983	4.815652
262.856904	8000.349011	10.402087	-0.054000	4.815653
262.749742	8000.376093	10.407091	-0.053980	4.815662
262.647217	8000.321014	10.412096	-0.053961	4.815646
262.935657	8000.338538	10.417101	-0.054015	4.815650
262.988562	8000.367166	10.422106	-0.054025	4.815658
262.841723	8000.390395	10.427111	-0.053997	4.815665
262.765788	8000.373131	10.432115	-0.053983	4.815661
262.930283	8000.345910	10.437120	-0.054014	4.815652
262.879602	8000.344010	10.442125	-0.054004	4.815652
262.838841	8000.344408	10.447130	-0.053997	4.815652
262.944162	8000.367485	10.452135	-0.054016	4.815658
263.008245	8000.346100	10.457139	-0.054028	4.815652
262.590037	8000.244214	10.462144	-0.053950	4.815624
262.725491	8000.295549	10.467149	-0.053975	4.815638
262.826576	8000.323896	10.472154	-0.053994	4.815646
262.933277	8000.281847	10.477159	-0.054014	4.815633
262.693264	8000.338799	10.482163	-0.053969	4.815651
262.733204	8000.283912	10.487168	-0.053977	4.815635
262.912026	8000.385085	10.492173	-0.054010	4.815664
262.809164	8000.336408	10.497178	-0.053991	4.815650
262.934091	8000.326697	10.502183	-0.054014	4.815646
262.996722	8000.345872	10.507187	-0.054025	4.815652
262.796157	8000.292396	10.512192	-0.053988	4.815637
262.967475	8000.351794	10.517197	-0.054020	4.815654
262.875047	8000.316105	10.522202	-0.054003	4.815644
262.910392	8000.264346	10.527207	-0.054009	4.815628
262.902895	8000.349660	10.532211	-0.054008	4.815653
262.900711	8000.286608	10.537216	-0.054007	4.815635
262.942497	8000.355639	10.542221	-0.054015	4.815655
262.711641	8000.363612	10.547226	-0.053972	4.815658
262.909201	8000.358291	10.552231	-0.054009	4.815656
262.805134	8000.376879	10.557235	-0.053989	4.815662
262.730314	8000.355361	10.562240	-0.053975	4.815656
262.903140	8000.410512	10.567245	-0.054008	4.815671
262.993645	8000.400239	10.572250	-0.054024	4.815668
262.758331	8000.356875	10.577255	-0.053980	4.815656
262.736650	8000.355449	10.582259	-0.053976	4.815656
262.865136	8000.294532	10.587264	-0.054000	4.815637
262.917022	8000.359455	10.592269	-0.054010	4.815656
262.868336	8000.363996	10.597274	-0.054001	4.815658
262.987286	8000.377683	10.602279	-0.054023	4.815661
263.028631	8000.415735	10.607283	-0.054031	4.815672
262.928433	8000.369238	10.612288	-0.054012	4.815659
263.136591	8000.419627	10.617293	-0.054051	4.815673
263.090105	8000.394299	10.622298	-0.054042	4.815665
262.830953	8000.410354	10.627303	-0.053994	4.815671
262.923082	8000.392631	10.632307	-0.054011	4.815666
262.992662	8000.342499	10.637312	-0.054024	4.815651
263.056064	8000.328579	10.642317	-0.054035	4.815646
263.017643	8000.326879	10.647322	-0.054028	4.815646
263.089413	8000.332320	10.652327	-0.054041	4.815647
263.110915	8000.358299	10.657331	-0.054045	4.815655
263.043901	8000.314480	10.662336	-0.054033	4.815642
263.020913	8000.326917	10.667341	-0.054029	4.815646
263.187849	8000.306144	10.672346	-0.054060	4.815639
263.217592	8000.350414	10.677351	-0.054065	4.815652
263.163082	8000.401852	10.682355	-0.054055	4.815667
262.967053	8000.377286	10.687360	-0.054018	4.815661
263.254015	8000.412942	10.692365	-0.054072	4.815670
263.015625	8000.327875	10.697370	-0.054027	4.815646
262.975801	8000.307996	10.702375	-0.054020	4.815641
263.116914	8000.374378	10.707379	-0.054046	4.815660
263.116257	8000.309215	10.712384	-0.054046	4.815641
263.278907	8000.315072	10.717389	-0.054076	4.815641
263.224978	8000.328071	10.722394	-0.054066	4.815646
263.234695	8000.337838	10.727399	-0.054068	4.815648
263.197875	8000.394905	10.732403	-0.054061	4.815665
263.283765	8000.378148	10.737408	-0.054077	4.815660
263.175103	8000.407341	10.742413	-0.054057	4.815669
262.957296	8000.309795	10.747418	-0.054016	4.815641
262.950798	8000.311821	10.752423	-0.054015	4.815642
263.067742	8000.322271	10.757427	-0.054036	4.815645
263.152813	8000.337541	10.762432	-0.054052	4.815649
263.246188	8000.405279	10.767437	-0.054070	4.815668
263.271889	8000.361906	10.772442	-0.054074	4.815655
263.258833	8000.328581	10.777447	-0.054072	4.815646
263.024478	8000.325817	10.782451	-0.054028	4.815646
263.219721	8000.256378	10.787456	-0.054064	4.815625
263.482170	8000.282021	10.792461	-0.054113	4.815631
263.292287	8000.335520	10.797466	-0.054078	4.815647
263.229199	8000.337689	10.802471	-0.054066	4.815648
263.328648	8000.399119	10.807475	-0.054085	4.815666
263.112781	8000.376364	10.812480	-0.054044	4.815660
263.170113	8000.397589	10.817485	-0.054055	4.815666
263.303089	8000.355969	10.822490	-0.054080	4.815653
263.430064	8000.367651	10.827495	-0.054103	4.815656
263.418554	8000.401636	10.832499	-0.054101	4.815666
263.098049	8000.379307	10.837504	-0.054041	4.815661
263.522391	8000.408665	10.842509	-0.054120	4.815668
263.414821	8000.357774	10.847514	-0.054100	4.815653
263.202905	8000.403437	10.852519	-0.054061	4.815668
263.274223	8000.411006	10.857523	-0.054074	4.815670
263.161032	8000.364296	10.862528	-0.054053	4.815656
263.259331	8000.372306	10.867533	-0.054071	4.815658
263.255666	8000.388263	10.872538	-0.054070	4.815663
263.348906	8000.359878	10.877543	-0.054088	4.815654
263.450825	8000.426688	10.882547	-0.054107	4.815673
263.335853	8000.394901	10.887552	-0.054085	4.815665
263.499959	8000.418939	10.892557	-0.054116	4.815671
263.268425	8000.351071	10.897562	-0.054073	4.815652
263.098399	8000.367514	10.902567	-0.054041	4.815658
263.172396	8000.410371	10.907571	-0.054055	4.815670
263.332310	8000.367055	10.912576	-0.054084	4.815656
263.208551	8000.375709	10.917581	-0.054061	4.815660
263.069436	8000.362753	10.922586	-0.054035	4.815656
263.261102	8000.379764	10.927591	-0.054071	4.815660
263.138581	8000.416207	10.932595	-0.054048	4.815672
263.198559	8000.377666	10.937600	-0.054059	4.815660
263.450664	8000.394598	10.942605	-0.054106	4.815664
263.342637	8000.309524	10.947610	-0.054086	4.815640
263.230737	8000.290604	10.952615	-0.054065	4.815635
263.619654	8000.358898	10.957619	-0.054137	4.815653
263.575843	8000.317594	10.962624	-0.054129	4.815641
263.565352	8000.397520	10.967629	-0.054127	4.815664
263.364532	8000.356854	10.972634	-0.054090	4.815653
263.353655	8000.352400	10.977639	-0.054088	4.815652
263.482254	8000.371586	10.982643	-0.054112	4.815657
263.371544	8000.334529	10.987648	-0.054091	4.815647
263.416204	8000.368363	10.992653	-0.054099	4.815656
263.351529	8000.352350	10.997658	-0.054087	4.815652
263.338912	8000.276311	11.002663	-0.054085	4.815630
263.463199	8000.374459	11.007667	-0.054108	4.815658
263.333148	8000.301841	11.012672	-0.054084	4.815637
263.417534	8000.355549	11.017677	-0.054099	4.815653
263.476026	8000.337276	11.022682	-0.054110	4.815647
263.509141	8000.316453	11.027687	-0.054116	4.815641
263.571297	8000.344165	11.032691	-0.054128	4.815649
263.315524	8000.322894	11.037696	-0.054080	4.815644
263.451671	8000.326182	11.042701	-0.054105	4.815644
263.355994	8000.320343	11.047706	-0.054087	4.815643
263.379573	8000.351697	11.052711	-0.054092	4.815652
263.403553	8000.403349	11.057715	-0.054096	4.815667
263.206929	8000.361684	11.062720	-0.054060	4.815656
263.408485	8000.382062	11.067725	-0.054097	4.815660
263.274532	8000.369189	11.072730	-0.054072	4.815657
263.223506	8000.345923	11.077735	-0.054063	4.815651
263.499884	8000.388883	11.082739	-0.054114	4.815662
263.341279	8000.330751	11.087744	-0.054084	4.815646
263.404431	8000.373432	11.092749	-0.054096	4.815658
263.408953	8000.385250	11.097754	-0.054097	4.815661
263.320159	8000.389135	11.102759	-0.054080	4.815663
263.405944	8000.394805	11.107763	-0.054096	4.815664
263.345593	8000.378863	11.112768	-0.054085	4.815660
263.540903	8000.417294	11.117773	-0.054121	4.815670
263.332412	8000.360483	11.122778	-0.054082	4.815655
263.525039	8000.334790	11.127783	-0.054118	4.815646
263.551440	8000.360850	11.132787	-0.054123	4.815654
263.336725	8000.360542	11.137792	-0.054083	4.815655
263.316675	8000.416815	11.142797	-0.054079	4.815671
263.317635	8000.391194	11.147802	-0.054079	4.815664
263.430032	8000.346034	11.152807	-0.054100	4.815650
263.367690	8000.397344	11.157811	-0.054089	4.815665
263.478137	8000.347880	11.162816	-0.054109	4.815650
263.544960	8000.367124	11.167821	-0.054122	4.815656
263.490749	8000.363031	11.172826	-0.054111	4.815655
263.472518	8000.363797	11.177831	-0.054108	4.815655
263.496917	8000.393028	11.182835	-0.054113	4.815663
263.323233	8000.331446	11.187840	-0.054080	4.815646
263.409472	8000.334987	11.192845	-0.054096	4.815647
263.606152	8000.363828	11.197850	-0.054133	4.815654
263.370913	8000.306580	11.202855	-0.054089	4.815639
263.443140	8000.338729	11.207859	-0.054102	4.815648
263.328935	8000.312295	11.212864	-0.054081	4.815641
263.290981	8000.326623	11.217869	-0.054074	4.815645
263.257684	8000.373067	11.222874	-0.054068	4.815659
263.295383	8000.382224	11.227879	-0.054075	4.815661
263.351992	8000.392757	11.232883	-0.054085	4.815664
263.283572	8000.354254	11.237888	-0.054072	4.815653
263.377399	8000.360055	11.242893	-0.054090	4.815654
263.459394	8000.363527	11.247898	-0.054105	4.815655
263.553072	8000.329809	11.252903	-0.054122	4.815645
263.532614	8000.375396	11.257907	-0.054119	4.815658
263.568176	8000.343932	11.262912	-0.054125	4.815649
263.631413	8000.354574	11.267917	-0.054137	4.815651
263.571581	8000.294851	11.272922	-0.054126	4.815634
263.560139	8000.264756	11.277927	-0.054123	4.815626
263.559220	8000.341634	11.282931	-0.054123	4.815648
263.382970	8000.287486	11.287936	-0.054090	4.815633
263.616371	8000.304112	11.292941	-0.054134	4.815637
263.626739	8000.344862	11.297946	-0.054136	4.815649
263.408259	8000.349832	11.302951	-0.054095	4.815651
263.380785	8000.379284	11.307955	-0.054090	4.815660
263.494986	8000.282888	11.312960	-0.054111	4.815631
263.531697	8000.304844	11.317965	-0.054118	4.815637
263.424898	8000.295620	11.322970	-0.054098	4.815635
263.432231	8000.320300	11.327975	-0.054099	4.815642
263.614159	8000.327540	11.332979	-0.054133	4.815644
263.491174	8000.264650	11.337984	-0.054110	4.815626
263.379218	8000.299130	11.342989	-0.054089	4.815636
263.599027	8000.321941	11.347994	-0.054130	4.815642
263.585788	8000.288612	11.352999	-0.054128	4.815632
263.667273	8000.325184	11.358003	-0.054143	4.815643
263.487632	8000.341470	11.363008	-0.054109	4.815648
263.682351	8000.391640	11.368013	-0.054145	4.815662
263.664652	8000.352898	11.373018	-0.054142	4.815651
263.531428	8000.341105	11.378023	-0.054117	4.815648
263.756464	8000.344778	11.383027	-0.054159	4.815648
263.814799	8000.363884	11.388032	-0.054170	4.815653
263.584961	8000.357988	11.393037	-0.054127	4.815653
263.545417	8000.392583	11.398042	-0.054120	4.815663
263.671527	8000.374347	11.403047	-0.054143	4.815657
263.563392	8000.380052	11.408051	-0.054123	4.815659
263.475492	8000.367932	11.413056	-0.054106	4.815656
263.603230	8000.378559	11.418061	-0.054130	4.815659
263.536171	8000.355031	11.423066	-0.054118	4.815652
263.423789	8000.354259	11.428071	-0.054097	4.815652
263.710171	8000.353595	11.433075	-0.054150	4.815651
263.726770	8000.335705	11.438080	-0.054153	4.815646
263.626255	8000.379984	11.443085	-0.054134	4.815659
263.798752	8000.364642	11.448090	-0.054166	4.815654
263.687888	8000.341466	11.453095	-0.054146	4.815647
263.845801	8000.346179	11.458099	-0.054175	4.815648
263.650558	8000.299196	11.463104	-0.054139	4.815635
263.829286	8000.344833	11.468109	-0.054172	4.815648
263.698412	8000.357643	11.473114	-0.054147	4.815652
263.631163	8000.283915	11.478119	-0.054135	4.815631
263.752288	8000.364924	11.483123	-0.054157	4.815654
263.802344	8000.361465	11.488128	-0.054167	4.815653
263.657354	8000.372977	11.493133	-0.054140	4.815657
263.465281	8000.393331	11.498138	-0.054104	4.815664
263.506367	8000.407882	11.503143	-0.054111	4.815668
263.554583	8000.436435	11.508147	-0.054120	4.815676
263.642650	8000.388741	11.513152	-0.054137	4.815661
263.734850	8000.380631	11.518157	-0.054154	4.815659
263.722963	8000.402862	11.523162	-0.054152	4.815665
263.493315	8000.379881	11.528167	-0.054109	4.815660
263.623082	8000.402290	11.533171	-0.054133	4.815665
263.738892	8000.355049	11.538176	-0.054154	4.815651
263.842409	8000.347124	11.543181	-0.054174	4.815648
263.721355	8000.376115	11.548186	-0.054151	4.815657
263.763321	8000.393885	11.553191	-0.054159	4.815662
263.778842	8000.414427	11.558195	-0.054162	4.815668
263.467738	8000.370891	11.563200	-0.054104	4.815657
263.578582	8000.380174	11.568205	-0.054124	4.815659
263.725253	8000.415676	11.573210	-0.054152	4.815669
263.759037	8000.360687	11.578215	-0.054158	4.815653
263.676909	8000.391381	11.583219	-0.054142	4.815662
263.873050	8000.357202	11.588224	-0.054179	4.815651
263.835418	8000.361923	11.593229	-0.054172	4.815653
263.508210	8000.375797	11.598234	-0.054111	4.815658
263.609706	8000.324050	11.603239	-0.054130	4.815643
263.730749	8000.353793	11.608243	-0.054152	4.815651
263.508403	8000.355496	11.613248	-0.054111	4.815652
263.831532	8000.372520	11.618253	-0.054171	4.815656
263.913646	8000.371722	11.623258	-0.054186	4.815655
263.935387	8000.336828	11.628263	-0.054190	4.815645
263.729055	8000.374038	11.633267	-0.054152	4.815657
263.683991	8000.369025	11.638272	-0.054143	4.815656
263.859538	8000.372958	11.643277	-0.054176	4.815656
263.691558	8000.350985	11.648282	-0.054145	4.815650
263.741555	8000.297329	11.653287	-0.054154	4.815634
263.808003	8000.378512	11.658291	-0.054166	4.815658
263.628066	8000.337119	11.663296	-0.054133	4.815646
263.684118	8000.327351	11.668301	-0.054143	4.815643
263.872498	8000.332561	11.673306	-0.054178	4.815644
263.778786	8000.296849	11.678311	-0.054161	4.815634
263.789304	8000.362167	11.683315	-0.054162	4.815653
263.696547	8000.330742	11.688320	-0.054145	4.815644
263.870174	8000.351732	11.693325	-0.054177	4.815650
263.794482	8000.309906	11.698330	-0.054163	4.815638
263.896733	8000.281668	11.703335	-0.054182	4.815629
263.955484	8000.331754	11.708339	-0.054193	4.815643
263.891704	8000.322163	11.713344	-0.054181	4.815641
263.989061	8000.337635	11.718349	-0.054199	4.815645
263.938604	8000.383799	11.723354	-0.054190	4.815659
263.683767	8000.379631	11.728359	-0.054142	4.815659
263.809675	8000.404113	11.733363	-0.054166	4.815665
263.721037	8000.363144	11.738368	-0.054149	4.815654
263.755009	8000.344470	11.743373	-0.054156	4.815648
263.749772	8000.382830	11.748378	-0.054155	4.815659
263.890656	8000.387264	11.753383	-0.054181	4.815660
263.895501	8000.381999	11.758387	-0.054182	4.815658
263.745077	8000.366721	11.763392	-0.054154	4.815655
263.811005	8000.364590	11.768397	-0.054166	4.815654
263.708214	8000.355430	11.773402	-0.054147	4.815651
263.822543	8000.319914	11.778407	-0.054168	4.815641
263.871316	8000.368768	11.783411	-0.054177	4.815655
263.778992	8000.333079	11.788416	-0.054160	4.815645
263.854187	8000.355664	11.793421	-0.054174	4.815651
263.747885	8000.338971	11.798426	-0.054154	4.815646
263.791857	8000.330073	11.803431	-0.054162	4.815644
264.036900	8000.343685	11.808435	-0.054207	4.815646
263.744070	8000.288700	11.813440	-0.054153	4.815632
264.058677	8000.345101	11.818445	-0.054211	4.815647
263.920053	8000.319336	11.823450	-0.054186	4.815640
263.811821	8000.300475	11.828455	-0.054165	4.815635
263.903856	8000.331879	11.833459	-0.054182	4.815644
263.829900	8000.332803	11.838464	-0.054169	4.815644
263.845179	8000.348001	11.843469	-0.054171	4.815649
263.716217	8000.360842	11.848474	-0.054147	4.815653
263.753041	8000.335807	11.853479	-0.054154	4.815646
263.976479	8000.331978	11.858483	-0.054196	4.815643
263.906640	8000.331901	11.863488	-0.054183	4.815644
263.893633	8000.262263	11.868493	-0.054180	4.815623
263.976691	8000.336242	11.873498	-0.054196	4.815645
263.978967	8000.256174	11.878503	-0.054196	4.815621
263.998206	8000.367559	11.883507	-0.054200	4.815654
263.890905	8000.336964	11.888512	-0.054180	4.815645
263.914118	8000.375789	11.893517	-0.054184	4.815656
263.897294	8000.348809	11.898522	-0.054181	4.815649
263.781146	8000.330887	11.903527	-0.054159	4.815644
263.956105	8000.323062	11.908531	-0.054191	4.815641
263.896723	8000.351992	11.913536	-0.054180	4.815650
263.786066	8000.344840	11.918541	-0.054160	4.815648
264.011222	8000.329291	11.923546	-0.054202	4.815642
263.994147	8000.306579	11.928551	-0.054198	4.815636
263.984823	8000.359824	11.933555	-0.054197	4.815651
264.096566	8000.337082	11.938560	-0.054217	4.815644
263.983782	8000.308534	11.943565	-0.054196	4.815636
263.865277	8000.342906	11.948570	-0.054174	4.815647
263.999220	8000.317323	11.953575	-0.054199	4.815639
264.057061	8000.350305	11.958579	-0.054210	4.815648
263.861380	8000.323607	11.963584	-0.054173	4.815641
263.727546	8000.358796	11.968589	-0.054148	4.815652
264.004220	8000.362246	11.973594	-0.054200	4.815652
264.097351	8000.282594	11.978599	-0.054217	4.815628
263.904960	8000.356344	11.983603	-0.054181	4.815651
263.984776	8000.345896	11.988608	-0.054196	4.815647
264.146517	8000.349603	11.993613	-0.054226	4.815648
264.102831	8000.407627	11.998618	-0.054218	4.815665
264.008696	8000.372975	12.003623	-0.054200	4.815655
264.143312	8000.424301	12.008627	-0.054226	4.815670
263.984584	8000.356553	12.013632	-0.054196	4.815651
263.977213	8000.330796	12.018637	-0.054194	4.815643
263.987282	8000.374746	12.023642	-0.054196	4.815656
263.827936	8000.273880	12.028647	-0.054167	4.815627
263.937961	8000.382476	12.033651	-0.054187	4.815658
263.982250	8000.342611	12.038656	-0.054195	4.815646
264.162019	8000.345545	12.043661	-0.054229	4.815646
264.082102	8000.380548	12.048666	-0.054214	4.815657
264.000253	8000.301240	12.053671	-0.054198	4.815634
263.978066	8000.331846	12.058675	-0.054194	4.815643
263.888542	8000.357080	12.063680	-0.054178	4.815651
263.866258	8000.355644	12.068685	-0.054173	4.815651
263.982192	8000.362875	12.073690	-0.054195	4.815652
264.068004	8000.346117	12.078695	-0.054211	4.815647
263.938938	8000.381385	12.083699	-0.054187	4.815658
263.778188	8000.337101	12.088704	-0.054157	4.815646
263.911648	8000.299761	12.093709	-0.054182	4.815634
263.923723	8000.354423	12.098714	-0.054184	4.815650
263.843690	8000.325343	12.103719	-0.054169	4.815642
264.046721	8000.388466	12.108723	-0.054207	4.815660
264.070532	8000.346130	12.113728	-0.054211	4.815647
263.987018	8000.375735	12.118733	-0.054195	4.815656
263.883808	8000.359092	12.123738	-0.054176	4.815652
263.868900	8000.323599	12.128743	-0.054173	4.815641
264.071662	8000.373902	12.133747	-0.054211	4.815655
263.844081	8000.389403	12.138752	-0.054169	4.815661
264.049058	8000.368184	12.143757	-0.054207	4.815654
264.131281	8000.396225	12.148762	-0.054222	4.815661
263.894384	8000.348561	12.153767	-0.054178	4.815649
264.085129	8000.359150	12.158771	-0.054213	4.815651
264.171977	8000.345613	12.163776	-0.054229	4.815646
264.066709	8000.385542	12.168781	-0.054210	4.815659
263.825446	8000.395479	12.173786	-0.054165	4.815663
264.030531	8000.373194	12.178791	-0.054203	4.815655
264.180353	8000.399136	12.183795	-0.054231	4.815662
264.052421	8000.387428	12.188800	-0.054207	4.815659
264.075989	8000.369653	12.193805	-0.054211	4.815654
264.092682	8000.399827	12.198810	-0.054214	4.815663
263.948309	8000.339790	12.203815	-0.054187	4.815646
263.925617	8000.350096	12.208819	-0.054183	4.815649
264.050376	8000.358538	12.213824	-0.054206	4.815651
264.147863	8000.239441	12.218829	-0.054224	4.815616
264.154119	8000.369838	12.223834	-0.054226	4.815654
264.227408	8000.300542	12.228839	-0.054239	4.815633
264.309358	8000.414021	12.233843	-0.054254	4.815666
263.970309	8000.345462	12.238848	-0.054191	4.815647
264.132937	8000.342776	12.243853	-0.054221	4.815646
264.108613	8000.340238	12.248858	-0.054217	4.815645
264.105187	8000.310273	12.253863	-0.054216	4.815636
264.012123	8000.396327	12.258867	-0.054199	4.815662
264.036386	8000.344386	12.263872	-0.054203	4.815647
264.351585	8000.321764	12.268877	-0.054262	4.815639
264.090854	8000.392262	12.273882	-0.054213	4.815660
264.248905	8000.349983	12.278887	-0.054243	4.815647
264.377226	8000.388390	12.283891	-0.054267	4.815658
264.118197	8000.361724	12.288896	-0.054218	4.815651
264.114472	8000.349911	12.293901	-0.054218	4.815648
264.238666	8000.377569	12.298906	-0.054241	4.815656
264.016500	8000.372866	12.303911	-0.054199	4.815655
264.207817	8000.399486	12.308915	-0.054235	4.815662
264.133637	8000.367297	12.313920	-0.054221	4.815653
264.153088	8000.365474	12.318925	-0.054225	4.815652
264.030885	8000.393378	12.323930	-0.054202	4.815661
264.083640	8000.375012	12.328935	-0.054212	4.815656
264.287004	8000.365515	12.333939	-0.054249	4.815652
264.026524	8000.386887	12.338944	-0.054201	4.815659
264.164265	8000.376318	12.343949	-0.054226	4.815656
264.205796	8000.420782	12.348954	-0.054234	4.815668
263.973660	8000.300569	12.353959	-0.054191	4.815634
264.145588	8000.327939	12.358963	-0.054223	4.815641
264.251223	8000.298689	12.363968	-0.054242	4.815632
264.178256	8000.316717	12.368973	-0.054229	4.815638
264.114869	8000.337038	12.373978	-0.054217	4.815644
264.135566	8000.308535	12.378983	-0.054221	4.815636
264.206984	8000.369508	12.383987	-0.054234	4.815653
264.326833	8000.336218	12.388992	-0.054256	4.815643
264.317340	8000.302950	12.393997	-0.054254	4.815633
264.263747	8000.391785	12.399002	-0.054244	4.815660
264.214989	8000.319426	12.404007	-0.054235	4.815639
264.384421	8000.348892	12.409011	-0.054267	4.815646
264.145725	8000.336442	12.414016	-0.054222	4.815644
264.258493	8000.335077	12.419021	-0.054243	4.815643
264.283539	8000.381408	12.424026	-0.054248	4.815656
264.296867	8000.317540	12.429031	-0.054250	4.815638
264.444406	8000.374417	12.434035	-0.054278	4.815654
264.252079	8000.370202	12.439040	-0.054242	4.815653
264.063343	8000.357501	12.444045	-0.054207	4.815651
264.272134	8000.376930	12.449050	-0.054246	4.815655
264.248581	8000.348772	12.454055	-0.054241	4.815647
264.344000	8000.394117	12.459059	-0.054259	4.815660
264.225101	8000.361197	12.464064	-0.054237	4.815651
264.147942	8000.356728	12.469069	-0.054222	4.815650
264.156002	8000.361128	12.474074	-0.054224	4.815651
264.072372	8000.289267	12.479079	-0.054208	4.815631
264.421346	8000.317395	12.484083	-0.054273	4.815637
264.388459	8000.336078	12.489088	-0.054267	4.815643
264.143573	8000.348092	12.494093	-0.054221	4.815647
264.257251	8000.363831	12.499098	-0.054242	4.815651
264.239240	8000.301587	12.504103	-0.054239	4.815633
264.212802	8000.356688	12.509107	-0.054234	4.815650
264.271156	8000.355502	12.514112	-0.054245	4.815649
264.227068	8000.355845	12.519117	-0.054236	4.815649
264.267136	8000.399218	12.524122	-0.054244	4.815662
264.135563	8000.357546	12.529127	-0.054219	4.815650
264.226950	8000.364376	12.534131	-0.054236	4.815652
264.159256	8000.365402	12.539136	-0.054224	4.815652
263.983395	8000.357184	12.544141	-0.054191	4.815651
264.214153	8000.387652	12.549146	-0.054234	4.815659
264.273176	8000.314918	12.554151	-0.054245	4.815637
264.176134	8000.317600	12.559155	-0.054227	4.815638
264.170653	8000.335663	12.564160	-0.054226	4.815644
264.299229	8000.279019	12.569165	-0.054249	4.815626
264.181776	8000.342245	12.574170	-0.054228	4.815646
264.242431	8000.312260	12.579175	-0.054239	4.815636
264.355094	8000.370703	12.584179	-0.054260	4.815653
264.429843	8000.363376	12.589184	-0.054274	4.815651
264.292791	8000.367541	12.594189	-0.054248	4.815652
264.212522	8000.405742	12.599194	-0.054233	4.815664
264.199957	8000.396988	12.604199	-0.054231	4.815661
264.238251	8000.363433	12.609203	-0.054238	4.815651
264.283259	8000.350281	12.614208	-0.054246	4.815647
264.362625	8000.281084	12.619213	-0.054261	4.815627
264.165886	8000.407096	12.624218	-0.054224	4.815665
263.947103	8000.326619	12.629223	-0.054183	4.815642
264.096543	8000.326921	12.634227	-0.054211	4.815641
264.010604	8000.330853	12.639232	-0.054195	4.815643
264.139389	8000.266736	12.644237	-0.054219	4.815624
264.311669	8000.350717	12.649242	-0.054251	4.815647
264.198568	8000.360613	12.654247	-0.054230	4.815651
264.180210	8000.390214	12.659251	-0.054227	4.815660
264.231179	8000.342982	12.664256	-0.054236	4.815646
264.310932	8000.275927	12.669261	-0.054251	4.815626
264.161960	8000.362135	12.674266	-0.054223	4.815651
263.762277	8000.296859	12.679271	-0.054148	4.815634
263.980745	8000.365574	12.684275	-0.054189	4.815653
264.180947	8000.316508	12.689280	-0.054226	4.815638
264.352897	8000.315042	12.694285	-0.054258	4.815637
264.175914	8000.373024	12.699290	-0.054225	4.815655
264.387369	8000.394633	12.704295	-0.054265	4.815660
264.345516	8000.430258	12.709299	-0.054257	4.815670
264.231674	8000.367515	12.714304	-0.054236	4.815653
264.130986	8000.341301	12.719309	-0.054217	4.815646
264.197378	8000.416076	12.724314	-0.054229	4.815667
264.067380	8000.328505	12.729319	-0.054205	4.815642
264.389963	8000.381835	12.734323	-0.054265	4.815656
264.353109	8000.381229	12.739328	-0.054258	4.815656
264.301260	8000.338724	12.744333	-0.054248	4.815644
264.140406	8000.414057	12.749338	-0.054218	4.815667
264.155785	8000.340611	12.754343	-0.054221	4.815645
264.248992	8000.336790	12.759347	-0.054238	4.815644
264.048737	8000.344193	12.764352	-0.054201	4.815647
264.018355	8000.336217	12.769357	-0.054195	4.815645
264.389536	8000.419178	12.774362	-0.054264	4.815667
264.333409	8000.386215	12.779367	-0.054254	4.815658
264.114959	8000.367688	12.784371	-0.054213	4.815653
264.193425	8000.391396	12.789376	-0.054228	4.815660
264.275340	8000.357485	12.794381	-0.054243	4.815650
264.066269	8000.398922	12.799386	-0.054204	4.815663
264.049097	8000.366596	12.804391	-0.054201	4.815653
264.515470	8000.371011	12.809395	-0.054288	4.815652
264.322910	8000.395628	12.814400	-0.054252	4.815660
264.248958	8000.358102	12.819405	-0.054238	4.815650
264.210080	8000.404457	12.824410	-0.054231	4.815664
264.033950	8000.375941	12.829415	-0.054198	4.815656
264.102329	8000.414436	12.834419	-0.054210	4.815667
264.283564	8000.380013	12.839424	-0.054244	4.815656
264.080825	8000.401260	12.844429	-0.054206	4.815663
264.156199	8000.402488	12.849434	-0.054220	4.815663
264.116614	8000.381545	12.854439	-0.054213	4.815657
264.225149	8000.376906	12.859443	-0.054233	4.815656
264.165011	8000.389804	12.864448	-0.054222	4.815660
264.162015	8000.356642	12.869453	-0.054221	4.815650
264.474807	8000.407676	12.874458	-0.054279	4.815663
264.183133	8000.389020	12.879463	-0.054225	4.815659
264.131501	8000.396717	12.884467	-0.054215	4.815662
264.073634	8000.389359	12.889472	-0.054205	4.815660
264.299086	8000.326822	12.894477	-0.054247	4.815641
264.211310	8000.346744	12.899482	-0.054230	4.815647
264.121546	8000.365565	12.904487	-0.054213	4.815653
264.357986	8000.397195	12.909491	-0.054257	4.815661
264.433308	8000.413374	12.914496	-0.054271	4.815665
264.366698	8000.358880	12.919501	-0.054259	4.815650
264.299640	8000.417590	12.924506	-0.054246	4.815667
264.138617	8000.354076	12.929511	-0.054216	4.815649
264.167601	8000.413288	12.934515	-0.054222	4.815666
264.282917	8000.409828	12.939520	-0.054243	4.815665
264.298136	8000.374828	12.944525	-0.054246	4.815655
264.362372	8000.369466	12.949530	-0.054258	4.815653
264.288473	8000.376798	12.954535	-0.054244	4.815655
264.372450	8000.382439	12.959539	-0.054260	4.815656
264.301983	8000.359923	12.964544	-0.054246	4.815650
264.346313	8000.383072	12.969549	-0.054255	4.815657
264.413914	8000.396989	12.974554	-0.054267	4.815660
264.311797	8000.315214	12.979559	-0.054248	4.815637
264.313416	8000.370774	12.984563	-0.054248	4.815653
264.290469	8000.371463	12.989568	-0.054244	4.815654
264.248986	8000.316312	12.994573	-0.054236	4.815638
264.253558	8000.403961	12.999578	-0.054237	4.815663
264.136464	8000.312329	13.004583	-0.054215	4.815637
264.462249	8000.348622	13.009587	-0.054276	4.815646
264.291912	8000.341562	13.014592	-0.054244	4.815645
264.186629	8000.348382	13.019597	-0.054224	4.815647
264.259162	8000.382672	13.024602	-0.054238	4.815657
264.410424	8000.318922	13.029607	-0.054266	4.815638
264.477382	8000.322149	13.034611	-0.054278	4.815638
264.530137	8000.356116	13.039616	-0.054288	4.815648
264.435609	8000.343887	13.044621	-0.054271	4.815645
264.393303	8000.404070	13.049626	-0.054263	4.815663
264.426350	8000.335183	13.054631	-0.054269	4.815642
264.518752	8000.321737	13.059635	-0.054286	4.815638
264.425842	8000.393909	13.064640	-0.054269	4.815660
264.382858	8000.355821	13.069645	-0.054261	4.815649
264.379309	8000.443339	13.074650	-0.054260	4.815674
264.325158	8000.399728	13.079655	-0.054250	4.815662
264.300860	8000.397191	13.084659	-0.054245	4.815661
264.463818	8000.382762	13.089664	-0.054275	4.815656
264.447349	8000.321611	13.094669	-0.054272	4.815638
264.241856	8000.373786	13.099674	-0.054234	4.815655
264.164382	8000.302026	13.104679	-0.054220	4.815634
264.438605	8000.324660	13.109683	-0.054271	4.815639
264.559165	8000.409934	13.114688	-0.054293	4.815664
264.516720	8000.322725	13.119693	-0.054285	4.815638
264.475324	8000.332725	13.124698	-0.054277	4.815641
264.410705	8000.293215	13.129703	-0.054265	4.815630
264.596271	8000.316537	13.134707	-0.054300	4.815636
264.449709	8000.365403	13.139712	-0.054272	4.815651
264.464676	8000.304766	13.144717	-0.054275	4.815633
264.268315	8000.390199	13.149722	-0.054239	4.815659
264.346087	8000.364766	13.154727	-0.054253	4.815651
264.444544	8000.372779	13.159731	-0.054271	4.815653
264.444898	8000.385598	13.164736	-0.054271	4.815657
264.256107	8000.291725	13.169741	-0.054236	4.815631
264.362610	8000.373564	13.174746	-0.054256	4.815654
264.467096	8000.313322	13.179751	-0.054275	4.815636
264.479654	8000.417123	13.184755	-0.054278	4.815666
264.330847	8000.381578	13.189760	-0.054250	4.815656
264.246539	8000.368447	13.194765	-0.054234	4.815653
264.476688	8000.430947	13.199770	-0.054277	4.815670
264.184547	8000.396263	13.204775	-0.054222	4.815661
264.332149	8000.397604	13.209779	-0.054250	4.815661
264.368138	8000.408868	13.214784	-0.054257	4.815664
264.385706	8000.376042	13.219789	-0.054260	4.815655
264.297193	8000.419449	13.224794	-0.054243	4.815668
264.324870	8000.365428	13.229799	-0.054248	4.815652
264.469864	8000.400903	13.234803	-0.054275	4.815661
264.273603	8000.397691	13.239808	-0.054239	4.815661
264.306747	8000.308514	13.244813	-0.054245	4.815635
264.447793	8000.364217	13.249818	-0.054271	4.815651
264.417362	8000.362648	13.254823	-0.054265	4.815651
264.341920	8000.361411	13.259827	-0.054251	4.815651
264.446036	8000.354564	13.264832	-0.054271	4.815648
264.368701	8000.333004	13.269837	-0.054256	4.815642
264.185295	8000.362043	13.274842	-0.054222	4.815651
264.267925	8000.296104	13.279847	-0.054237	4.815632
264.503807	8000.322383	13.284851	-0.054281	4.815638
264.407892	8000.369941	13.289856	-0.054263	4.815653
264.530727	8000.359129	13.294861	-0.054286	4.815649
264.602766	8000.377391	13.299866	-0.054299	4.815654
264.372483	8000.326630	13.304871	-0.054256	4.815640
264.275407	8000.309019	13.309875	-0.054238	4.815636
264.356252	8000.333833	13.314880	-0.054253	4.815642
264.274901	8000.329295	13.319885	-0.054238	4.815641
264.335811	8000.413593	13.324890	-0.054250	4.815666
264.369128	8000.350052	13.329895	-0.054256	4.815647
264.418510	8000.307065	13.334899	-0.054265	4.815634
264.320473	8000.302255	13.339904	-0.054246	4.815633
264.247584	8000.312808	13.344909	-0.054233	4.815637
264.408322	8000.363493	13.349914	-0.054263	4.815651
264.238894	8000.313727	13.354919	-0.054231	4.815637
264.312045	8000.306374	13.359923	-0.054245	4.815635
264.476335	8000.360321	13.364928	-0.054275	4.815650
264.347530	8000.290925	13.369933	-0.054251	4.815630
264.286112	8000.317687	13.374938	-0.054240	4.815638
264.470285	8000.364482	13.379943	-0.054274	4.815651
264.498482	8000.333966	13.384947	-0.054279	4.815642
264.428381	8000.348837	13.389952	-0.054266	4.815646
264.338214	8000.311046	13.394957	-0.054249	4.815636
264.629790	8000.345713	13.399962	-0.054304	4.815645
264.525390	8000.294873	13.404967	-0.054284	4.815630
264.531047	8000.356907	13.409971	-0.054285	4.815648
264.558488	8000.377645	13.414976	-0.054290	4.815654
264.418187	8000.321946	13.419981	-0.054264	4.815639
264.503531	8000.401303	13.424986	-0.054280	4.815661
264.419796	8000.359345	13.429991	-0.054264	4.815650
264.497150	8000.281571	13.434995	-0.054279	4.815626
264.511444	8000.330930	13.440000	-0.054281	4.815641
264.669649	8000.304675	13.445005	-0.054311	4.815632
264.823194	8000.396897	13.450010	-0.054339	4.815659
264.501095	8000.336089	13.455015	-0.054279	4.815642
264.584350	8000.301133	13.460019	-0.054295	4.815632
264.493748	8000.297512	13.465024	-0.054278	4.815631
264.508989	8000.308438	13.470029	-0.054280	4.815634
264.518313	8000.370532	13.475034	-0.054282	4.815652
264.397050	8000.339709	13.480039	-0.054259	4.815644
264.521674	8000.356695	13.485043	-0.054283	4.815648
264.491505	8000.385035	13.490048	-0.054277	4.815657
264.614168	8000.326158	13.495053	-0.054300	4.815639
264.675272	8000.384827	13.500058	-0.054311	4.815656
264.459569	8000.292650	13.505063	-0.054271	4.815630
264.484510	8000.331503	13.510067	-0.054276	4.815641
264.658047	8000.363172	13.515072	-0.054308	4.815650
264.659411	8000.296972	13.520077	-0.054308	4.815630
264.699992	8000.388415	13.525082	-0.054316	4.815657
264.736535	8000.331334	13.530087	-0.054322	4.815640
264.726092	8000.352520	13.535091	-0.054320	4.815646
264.612680	8000.391248	13.540096	-0.054299	4.815658
264.497079	8000.359450	13.545101	-0.054278	4.815649
264.672690	8000.322799	13.550106	-0.054310	4.815638
264.571564	8000.354251	13.555111	-0.054291	4.815647
264.717078	8000.323516	13.560115	-0.054318	4.815638
264.524560	8000.366291	13.565120	-0.054282	4.815651
264.457756	8000.314998	13.570125	-0.054270	4.815636
264.591654	8000.362040	13.575130	-0.054295	4.815650
264.505221	8000.342466	13.580135	-0.054279	4.815644
264.701119	8000.347801	13.585139	-0.054315	4.815645
264.459103	8000.333161	13.590144	-0.054270	4.815642
264.328607	8000.297915	13.595149	-0.054246	4.815632
264.652507	8000.393988	13.600154	-0.054306	4.815659
264.672149	8000.322746	13.605159	-0.054310	4.815638
264.638346	8000.333938	13.610163	-0.054303	4.815641
264.700431	8000.419325	13.615168	-0.054315	4.815666
264.790688	8000.352441	13.620173	-0.054332	4.815646
264.739366	8000.353734	13.625178	-0.054322	4.815646
264.420156	8000.343173	13.630183	-0.054262	4.815645
264.452200	8000.321264	13.635187	-0.054268	4.815638
264.574328	8000.385202	13.640192	-0.054291	4.815656
264.480130	8000.301420	13.645197	-0.054273	4.815632
264.736936	8000.345131	13.650202	-0.054321	4.815644
264.480542	8000.329187	13.655207	-0.054273	4.815641
264.500030	8000.376496	13.660211	-0.054277	4.815654
264.574656	8000.367031	13.665216	-0.054291	4.815651
264.625120	8000.351831	13.670221	-0.054300	4.815646
264.737189	8000.408130	13.675226	-0.054321	4.815662
264.652657	8000.346933	13.680231	-0.054305	4.815645
264.706628	8000.332859	13.685235	-0.054315	4.815641
264.743021	8000.385784	13.690240	-0.054322	4.815656
264.609228	8000.334463	13.695245	-0.054297	4.815641
264.509611	8000.391573	13.700250	-0.054279	4.815659
264.650559	8000.362900	13.705255	-0.054305	4.815650
264.584657	8000.330846	13.710259	-0.054292	4.815641
264.445079	8000.383030	13.715264	-0.054266	4.815656
264.427637	8000.322931	13.720269	-0.054263	4.815639
264.514152	8000.359587	13.725274	-0.054279	4.815649
264.484522	8000.338806	13.730279	-0.054274	4.815643
264.528108	8000.335242	13.735283	-0.054282	4.815642
264.505521	8000.390407	13.740288	-0.054277	4.815658
264.532427	8000.339577	13.745293	-0.054282	4.815643
264.491629	8000.373083	13.750298	-0.054275	4.815653
264.533482	8000.325702	13.755303	-0.054282	4.815639
264.720421	8000.375747	13.760307	-0.054317	4.815653
264.675330	8000.363258	13.765312	-0.054309	4.815650
264.470806	8000.325734	13.770317	-0.054271	4.815640
264.570154	8000.356190	13.775322	-0.054289	4.815648
264.523222	8000.300949	13.780327	-0.054280	4.815632
264.491803	8000.349562	13.785331	-0.054274	4.815646
264.742291	8000.341904	13.790336	-0.054321	4.815643
264.713102	8000.284816	13.795341	-0.054315	4.815626
264.776868	8000.384115	13.800346	-0.054327	4.815655
264.665020	8000.380146	13.805351	-0.054306	4.815655
264.460571	8000.358644	13.810355	-0.054268	4.815649
264.476029	8000.374913	13.815360	-0.054271	4.815654
264.479436	8000.323699	13.820365	-0.054272	4.815639
264.639239	8000.357280	13.825370	-0.054302	4.815648
264.603560	8000.297951	13.830375	-0.054295	4.815631
264.671172	8000.271283	13.835379	-0.054307	4.815623
264.696825	8000.353937	13.840384	-0.054312	4.815647
264.795593	8000.333119	13.845389	-0.054330	4.815640
264.568038	8000.371049	13.850394	-0.054288	4.815652
264.663213	8000.328811	13.855399	-0.054306	4.815640
264.712973	8000.297579	13.860403	-0.054315	4.815630
264.894340	8000.345398	13.865408	-0.054349	4.815643
264.720372	8000.282740	13.870413	-0.054316	4.815626
264.718073	8000.379890	13.875418	-0.054316	4.815654
264.505629	8000.336896	13.880423	-0.054276	4.815643
264.618599	8000.337671	13.885427	-0.054297	4.815642
264.819303	8000.362308	13.890432	-0.054334	4.815649
264.566202	8000.333602	13.895437	-0.054287	4.815641
264.675007	8000.356738	13.900442	-0.054307	4.815648
264.613191	8000.279893	13.905447	-0.054296	4.815626
264.552061	8000.351516	13.910451	-0.054285	4.815647
264.594947	8000.315900	13.915456	-0.054292	4.815636
264.671283	8000.326756	13.920461	-0.054307	4.815639
264.642222	8000.345502	13.925466	-0.054301	4.815645
264.519244	8000.332807	13.930471	-0.054278	4.815641
264.621657	8000.318457	13.935475	-0.054297	4.815637
264.850006	8000.363839	13.940480	-0.054340	4.815649
264.862335	8000.286069	13.945485	-0.054342	4.815626
264.834692	8000.356104	13.950490	-0.054337	4.815647
264.679156	8000.371715	13.955495	-0.054308	4.815652
264.631217	8000.349566	13.960499	-0.054299	4.815646
264.512645	8000.380733	13.965504	-0.054277	4.815656
264.589107	8000.302944	13.970509	-0.054291	4.815632
264.811049	8000.412305	13.975514	-0.054332	4.815663
264.617247	8000.372819	13.980519	-0.054296	4.815653
264.360430	8000.350461	13.985523	-0.054248	4.815647
264.544214	8000.403659	13.990528	-0.054282	4.815662
264.608274	8000.351300	13.995533	-0.054294	4.815646
264.429202	8000.369730	14.000538	-0.054261	4.815653
264.686629	8000.355777	14.005543	-0.054309	4.815647
264.845915	8000.357308	14.010547	-0.054338	4.815647
264.612140	8000.375912	14.015552	-0.054295	4.815654
264.356207	8000.363181	14.020557	-0.054247	4.815651
264.757387	8000.288563	14.025562	-0.054322	4.815627
264.747860	8000.309764	14.030567	-0.054320	4.815634
264.714255	8000.286782	14.035571	-0.054314	4.815627
264.842371	8000.339070	14.040576	-0.054337	4.815642
264.810712	8000.306507	14.045581	-0.054331	4.815632
264.884698	8000.397429	14.050586	-0.054345	4.815659
264.824746	8000.319545	14.055591	-0.054334	4.815636
264.679442	8000.316098	14.060595	-0.054307	4.815636
264.823538	8000.398553	14.065600	-0.054334	4.815659
264.660198	8000.300823	14.070605	-0.054303	4.815631
264.801959	8000.339450	14.075610	-0.054330	4.815642
264.738860	8000.344823	14.080615	-0.054318	4.815644
264.765455	8000.315348	14.085619	-0.054323	4.815635
264.807350	8000.383316	14.090624	-0.054330	4.815655
264.650144	8000.292095	14.095629	-0.054301	4.815629
264.556519	8000.396297	14.100634	-0.054284	4.815660
264.780253	8000.330527	14.105639	-0.054325	4.815640
264.865806	8000.365031	14.110643	-0.054341	4.815649
264.742676	8000.381171	14.115648	-0.054318	4.815655
264.632262	8000.341981	14.120653	-0.054298	4.815644
264.843758	8000.351842	14.125658	-0.054337	4.815646
264.848356	8000.342301	14.130663	-0.054338	4.815643
264.726961	8000.303999	14.135667	-0.054315	4.815632
264.885005	8000.323667	14.140672	-0.054344	4.815637
264.843470	8000.313372	14.145677	-0.054337	4.815634
264.927410	8000.352122	14.150682	-0.054352	4.815645
264.799186	8000.356430	14.155687	-0.054328	4.815647
264.784076	8000.311321	14.160691	-0.054325	4.815634
264.751482	8000.366323	14.165696	-0.054319	4.815650
264.559221	8000.365312	14.170701	-0.054284	4.815651
264.863904	8000.368153	14.175706	-0.054340	4.815650
264.838244	8000.388022	14.180711	-0.054335	4.815656
264.619461	8000.367353	14.185715	-0.054295	4.815651
264.769477	8000.412523	14.190720	-0.054323	4.815664
264.877200	8000.377967	14.195725	-0.054342	4.815653
264.903541	8000.391210	14.200730	-0.054347	4.815657
264.654075	8000.379652	14.205735	-0.054301	4.815655
264.822608	8000.343953	14.210739	-0.054332	4.815643
264.914883	8000.396724	14.215744	-0.054349	4.815658
264.634840	8000.370781	14.220749	-0.054297	4.815652
264.905923	8000.399774	14.225754	-0.054348	4.815659
264.924779	8000.358424	14.230759	-0.054351	4.815647
264.653614	8000.348647	14.235763	-0.054300	4.815646
264.594336	8000.377579	14.240768	-0.054289	4.815654
264.691963	8000.361015	14.245773	-0.054308	4.815649
264.776734	8000.327151	14.250778	-0.054323	4.815639
264.624888	8000.366319	14.255783	-0.054295	4.815651
264.767512	8000.360102	14.260787	-0.054321	4.815648
264.717486	8000.388117	14.265792	-0.054312	4.815657
264.662316	7999.303183	14.270797	-0.054301	4.815340

264.784987	7996.135736	14.275802	-0.054322	4.814413
264.895250	7990.592450	14.280807	-0.054339	4.812792
264.755246	7983.924513	14.285811	-0.054308	4.810842
264.585416	7976.646679	14.290816	-0.054272	4.808712
264.534601	7968.995558	14.295821	-0.054257	4.806472
264.583818	7961.230235	14.300826	-0.054261	4.804197
264.378653	7953.396553	14.305831	-0.054218	4.801902
264.739826	7945.358055	14.310835	-0.054280	4.799544
264.682620	7937.459747	14.315840	-0.054264	4.797227
264.551951	7929.389809	14.320845	-0.054235	4.794859
264.535265	7921.456298	14.325850	-0.054226	4.792529
264.663496	7913.406550	14.330855	-0.054245	4.790164
264.305029	7905.375138	14.335859	-0.054173	4.787804
264.226610	7897.354894	14.340864	-0.054153	4.785446
264.374329	7889.373555	14.345869	-0.054175	4.783097
264.427646	7881.409663	14.350874	-0.054180	4.780752
264.286536	7873.381380	14.355879	-0.054148	4.778388
264.326862	7865.424119	14.360883	-0.054151	4.776044
264.482102	7857.374839	14.365888	-0.054174	4.773670
264.217078	7849.352750	14.370893	-0.054120	4.771305
264.243529	7841.347909	14.375898	-0.054119	4.768942
264.354754	7833.404105	14.380903	-0.054135	4.766596
264.285143	7825.366893	14.385907	-0.054116	4.764222
264.161502	7817.445023	14.390912	-0.054088	4.761882
263.938560	7809.390829	14.395917	-0.054041	4.759501
264.091414	7801.409448	14.400922	-0.054065	4.757139
263.861381	7793.352772	14.405927	-0.054017	4.754755
263.644072	7785.283513	14.410931	-0.053971	4.752366
264.088075	7777.322557	14.415936	-0.054048	4.750006
263.666637	7769.310816	14.420941	-0.053964	4.747632
263.944027	7761.272746	14.425946	-0.054011	4.745247
263.958606	7753.373687	14.430951	-0.054008	4.742903
263.902062	7745.315909	14.435955	-0.053993	4.740511
263.836592	7737.360913	14.440960	-0.053975	4.738148
263.701037	7729.354619	14.445965	-0.053945	4.735769
263.784343	7721.333514	14.450970	-0.053955	4.733384
263.635120	7713.302702	14.455975	-0.053922	4.730996
263.699225	7705.295803	14.460979	-0.053928	4.728612
263.636662	7697.355720	14.465984	-0.053912	4.726248
263.590006	7689.309784	14.470989	-0.053898	4.723851
263.659959	7681.308753	14.475994	-0.053905	4.721466
263.553761	7673.313402	14.480999	-0.053880	4.719081
263.520432	7665.359352	14.486003	-0.053869	4.716708
263.490130	7657.326757	14.491008	-0.053858	4.714310
263.363572	7649.272437	14.496013	-0.053829	4.711904
263.419559	7641.309325	14.501018	-0.053834	4.709525
263.371979	7633.280557	14.506023	-0.053820	4.707124
263.343985	7625.276921	14.511027	-0.053810	4.704730
263.488063	7617.370364	14.516032	-0.053831	4.702363
263.208817	7609.257413	14.521037	-0.053774	4.699934
263.171045	7601.337900	14.526042	-0.053762	4.697561
263.250307	7593.274279	14.531047	-0.053771	4.695144
263.350307	7585.281522	14.536051	-0.053785	4.692747
263.475193	7577.311695	14.541056	-0.053803	4.690355
263.267844	7569.278433	14.546061	-0.053759	4.687943
263.314075	7561.243571	14.551066	-0.053762	4.685530
263.301964	7553.283137	14.556071	-0.053755	4.683137
263.201539	7545.284793	14.561075	-0.053731	4.680733
263.064397	7537.327767	14.566080	-0.053700	4.678339
262.952497	7529.284787	14.571085	-0.053674	4.675918
262.936323	7521.235078	14.576090	-0.053665	4.673494
262.927763	7513.142983	14.581095	-0.053659	4.671056
262.868837	7505.189495	14.586099	-0.053642	4.668658
262.814982	7497.201859	14.591104	-0.053627	4.666249
262.797853	7489.215420	14.596109	-0.053619	4.663838
263.009004	7481.247427	14.601114	-0.053653	4.661432
262.844132	7473.219103	14.606119	-0.053617	4.659007
262.792401	7465.283188	14.611123	-0.053602	4.656609
262.946351	7457.258129	14.616128	-0.053625	4.654181
262.645412	7449.190449	14.621133	-0.053564	4.651741
262.624079	7441.177404	14.626138	-0.053555	4.649315
262.776046	7433.247326	14.631143	-0.053578	4.646913
262.868100	7425.211981	14.636147	-0.053590	4.644478
262.510541	7417.265259	14.641152	-0.053518	4.642068
262.302199	7409.179074	14.646157	-0.053474	4.639615
262.491615	7401.253262	14.651162	-0.053504	4.637210
262.376893	7393.223081	14.656167	-0.053477	4.634771
262.338957	7385.193183	14.661171	-0.053465	4.632331
262.455242	7377.158492	14.666176	-0.053481	4.629889
262.416226	7369.197618	14.671181	-0.053469	4.627467
262.380902	7361.177349	14.676186	-0.053457	4.625026
262.265125	7353.216635	14.681191	-0.053430	4.622602
262.207248	7345.173094	14.686195	-0.053414	4.620152
262.247393	7337.252661	14.691200	-0.053416	4.617738
262.001625	7329.170538	14.696205	-0.053365	4.615273
262.286492	7321.181779	14.701210	-0.053413	4.612835
262.098750	7313.153315	14.706215	-0.053373	4.610384
262.184643	7305.163811	14.711219	-0.053383	4.607944
262.265451	7297.182604	14.716224	-0.053393	4.605504
261.960903	7289.135508	14.721229	-0.053331	4.603044
262.101723	7281.156639	14.726234	-0.053352	4.600603
262.145434	7273.205532	14.731239	-0.053355	4.598169
261.987031	7265.192679	14.736243	-0.053320	4.595714
262.020644	7257.162472	14.741248	-0.053321	4.593254
261.845372	7249.096229	14.746253	-0.053283	4.590780
261.733783	7241.144162	14.751258	-0.053257	4.588341
261.798122	7233.085145	14.756263	-0.053264	4.585867
261.670940	7225.156947	14.761267	-0.053235	4.583432
261.806772	7217.151071	14.766272	-0.053255	4.580973
261.625839	7209.160490	14.771277	-0.053216	4.578516
261.467628	7201.137681	14.776282	-0.053182	4.576048
261.526455	7193.164213	14.781287	-0.053187	4.573594
261.519845	7185.098940	14.786291	-0.053181	4.571111
261.544367	7177.136216	14.791296	-0.053180	4.568657
261.321353	7169.102764	14.796301	-0.053133	4.566181
261.408320	7161.143372	14.801306	-0.053144	4.563726
261.257410	7153.152817	14.806311	-0.053111	4.561260
261.244227	7145.131682	14.811315	-0.053103	4.558783
261.458750	7137.158337	14.816320	-0.053138	4.556320
261.509467	7129.099128	14.821325	-0.053142	4.553829
261.329030	7121.086835	14.826330	-0.053103	4.551351
261.171045	7113.104085	14.831335	-0.053068	4.548880
261.306488	7105.089906	14.836339	-0.053088	4.546399
261.189986	7097.111672	14.841344	-0.053061	4.543928
260.896231	7089.146902	14.846349	-0.053002	4.541458
261.012153	7081.125794	14.851354	-0.053018	4.538971
260.897933	7073.161750	14.856359	-0.052991	4.536500
260.953098	7065.089441	14.861363	-0.052996	4.533994
260.926010	7057.111541	14.866368	-0.052986	4.531515
260.959839	7049.064309	14.871373	-0.052987	4.529014
261.036593	7041.133633	14.876378	-0.052996	4.526548
260.880879	7033.078494	14.881383	-0.052962	4.524042
260.837512	7025.163422	14.886387	-0.052949	4.521578
260.805443	7017.141382	14.891392	-0.052937	4.519079
260.730812	7009.139148	14.896397	-0.052918	4.516584
260.868103	7001.090666	14.901402	-0.052938	4.514075
260.799576	6993.043266	14.906407	-0.052920	4.511564
260.592331	6985.010522	14.911411	-0.052877	4.509056
260.624331	6977.044272	14.916416	-0.052877	4.506568
260.807243	6969.038175	14.921421	-0.052906	4.504066
260.818086	6961.098863	14.926426	-0.052903	4.501583
260.578255	6953.079403	14.931431	-0.052853	4.499073
260.594155	6945.110026	14.936435	-0.052851	4.496579
260.660170	6937.088802	14.941440	-0.052858	4.494066
260.480845	6929.065434	14.946445	-0.052819	4.491551
260.503296	6921.035708	14.951450	-0.052818	4.489033
260.533340	6913.096956	14.956455	-0.052818	4.486543
260.471927	6905.023355	14.961459	-0.052802	4.484008
260.493172	6897.113473	14.966464	-0.052800	4.481523
260.444391	6889.060744	14.971469	-0.052786	4.478992
260.578889	6881.092014	14.976474	-0.052806	4.476487
260.301861	6873.063755	14.981479	-0.052749	4.473960
260.248750	6865.020803	14.986483	-0.052734	4.471428
260.456301	6856.988402	14.991488	-0.052767	4.468898
260.289371	6849.024206	14.996493	-0.052731	4.466388
260.271225	6841.058860	15.001498	-0.052722	4.463876
260.236865	6833.047759	15.006503	-0.052710	4.461348
260.146637	6825.010262	15.011507	-0.052688	4.458810
260.265748	6817.043974	15.016512	-0.052705	4.456294
260.179818	6808.998796	15.021517	-0.052684	4.453751
260.034334	6800.992565	15.026522	-0.052652	4.451218
259.951603	6793.013821	15.031527	-0.052631	4.448693
259.794477	6784.995275	15.036531	-0.052596	4.446154
259.989435	6777.050602	15.041536	-0.052628	4.443638
259.786737	6769.050723	15.046541	-0.052585	4.441101
259.853974	6761.017375	15.051546	-0.052592	4.438553
260.027748	6753.024521	15.056551	-0.052619	4.436018
259.824376	6744.985441	15.061555	-0.052576	4.433464
259.746452	6736.958139	15.066560	-0.052556	4.430914
259.816947	6728.974593	15.071565	-0.052564	4.428376
259.880761	6720.968226	15.076570	-0.052570	4.425830
259.811074	6712.983138	15.081575	-0.052552	4.423288
259.720291	6704.969667	15.086579	-0.052530	4.420736
259.912855	6697.020233	15.091584	-0.052561	4.418204
259.523020	6688.991247	15.096589	-0.052483	4.415642
259.585290	6680.984498	15.101594	-0.052489	4.413089
259.838212	6672.946112	15.106599	-0.052531	4.410524
259.746162	6664.935410	15.111603	-0.052509	4.407965
259.471385	6656.967520	15.116608	-0.052452	4.405418
259.462372	6648.967795	15.121613	-0.052445	4.402860
259.366868	6640.985869	15.126618	-0.052422	4.400306
259.586820	6633.025767	15.131623	-0.052458	4.397759
259.507510	6625.012902	15.136627	-0.052438	4.395192
259.466336	6617.009947	15.141632	-0.052425	4.392627
259.313246	6608.938687	15.146637	-0.052391	4.390038
259.461016	6600.987604	15.151642	-0.052413	4.387487
259.420194	6592.989021	15.156647	-0.052401	4.384919
259.414526	6584.991605	15.161651	-0.052394	4.382350
259.386405	6576.964338	15.166656	-0.052384	4.379770
259.289179	6568.995489	15.171661	-0.052360	4.377206
259.459819	6560.984700	15.176666	-0.052387	4.374630
259.266122	6553.018332	15.181671	-0.052346	4.372063
259.053944	6544.942767	15.186675	-0.052301	4.369460
259.216412	6537.014057	15.191680	-0.052326	4.366905
259.084731	6528.986261	15.196685	-0.052296	4.364315
259.124616	6521.035379	15.201690	-0.052298	4.361749
259.064446	6513.003190	15.206695	-0.052282	4.359154
259.040552	6505.040772	15.211699	-0.052272	4.356581
259.051370	6497.018672	15.216704	-0.052269	4.353987
258.860866	6488.880985	15.221709	-0.052228	4.351353
258.942477	6480.887367	15.226714	-0.052238	4.348766
258.776172	6472.961406	15.231719	-0.052202	4.346198
258.690831	6464.920075	15.236723	-0.052181	4.343591
258.673129	6456.985168	15.241728	-0.052172	4.341017
258.653441	6448.988658	15.246733	-0.052163	4.338422
258.550102	6440.999700	15.251738	-0.052139	4.335828
258.702089	6432.959147	15.256743	-0.052162	4.333216
258.651315	6424.922044	15.261747	-0.052147	4.330603
258.599579	6416.995386	15.266752	-0.052132	4.328025
258.657549	6408.914745	15.271757	-0.052138	4.325395
258.629764	6400.971254	15.276762	-0.052127	4.322808
258.468594	6392.978081	15.281767	-0.052092	4.320202
258.520228	6384.956247	15.286771	-0.052096	4.317586
258.538622	6376.962982	15.291776	-0.052094	4.314979
258.387725	6368.916325	15.296781	-0.052061	4.312351
258.508698	6360.889319	15.301786	-0.052078	4.309729
258.302183	6352.939789	15.306791	-0.052035	4.307129
258.221060	6344.891025	15.311795	-0.052014	4.304496
258.207358	6336.973406	15.316800	-0.052006	4.301905
258.174068	6328.933329	15.321805	-0.051995	4.299272
258.371250	6320.974515	15.326810	-0.052026	4.296666
258.035608	6312.948785	15.331815	-0.051959	4.294032
258.060333	6304.883076	15.336819	-0.051958	4.291386
258.147255	6296.921574	15.341824	-0.051969	4.288773
257.960828	6288.921389	15.346829	-0.051929	4.286144
258.138270	6280.928399	15.351834	-0.051957	4.283518
258.117477	6272.963325	15.356839	-0.051948	4.280898
257.981833	6264.915038	15.361843	-0.051917	4.278249
257.908458	6256.950758	15.366848	-0.051898	4.275625
257.895288	6248.888479	15.371853	-0.051890	4.272969
257.795130	6240.851496	15.376858	-0.051867	4.270318
257.933217	6232.889887	15.381863	-0.051887	4.267693
257.671113	6224.871925	15.386867	-0.051833	4.265044
257.621078	6216.990382	15.391872	-0.051818	4.262440
257.689452	6208.864019	15.396877	-0.051826	4.259755
257.577492	6200.935465	15.401882	-0.051800	4.257132
257.573980	6192.898533	15.406887	-0.051794	4.254472
257.578381	6184.890925	15.411891	-0.051789	4.251821
257.643011	6176.868747	15.416896	-0.051796	4.249163
257.466364	6168.918566	15.421901	-0.051758	4.246526
257.572524	6160.879827	15.426906	-0.051773	4.243860
257.497924	6152.965933	15.431911	-0.051753	4.241232
257.280955	6144.911651	15.436915	-0.051708	4.238555
257.410036	6136.978432	15.441920	-0.051727	4.235919
257.498621	6128.908640	15.446925	-0.051738	4.233236
257.441673	6120.891315	15.451930	-0.051722	4.230568
257.334015	6112.938675	15.456935	-0.051697	4.227918
257.309299	6104.904325	15.461939	-0.051687	4.225241
257.336119	6096.943758	15.466944	-0.051686	4.222587
257.197412	6088.932339	15.471949	-0.051655	4.219912
257.160259	6080.963204	15.476954	-0.051643	4.217252
257.301168	6072.974108	15.481959	-0.051664	4.214584
257.094854	6064.899771	15.486963	-0.051620	4.211883
257.078244	6056.921923	15.491968	-0.051612	4.209214
256.972638	6048.944438	15.496973	-0.051587	4.206543
257.084320	6040.900088	15.501978	-0.051603	4.203850
257.195991	6032.963297	15.506983	-0.051618	4.201191
257.051674	6024.938099	15.511987	-0.051586	4.198499
257.133341	6016.965840	15.516992	-0.051596	4.195824
256.848082	6008.871828	15.521997	-0.051538	4.193103
256.777271	6000.803261	15.527002	-0.051519	4.190392
256.897422	5992.906459	15.532007	-0.051536	4.187738
256.773940	5984.834201	15.537011	-0.051508	4.185021
256.792478	5976.926704	15.542016	-0.051506	4.182359
256.845031	5968.904534	15.547021	-0.051511	4.179657
256.988508	5960.915091	15.552026	-0.051532	4.176966
256.777764	5952.946208	15.557031	-0.051488	4.174276
256.810527	5944.881955	15.562035	-0.051489	4.171554
256.795156	5936.894806	15.567040	-0.051481	4.168856
256.437656	5928.893923	15.572045	-0.051409	4.166148
256.277229	5920.920310	15.577050	-0.051374	4.163450
256.416407	5912.916802	15.582055	-0.051394	4.160743
256.324360	5904.919946	15.587059	-0.051372	4.158034
256.455581	5896.914184	15.592064	-0.051391	4.155323
256.431895	5888.884927	15.597069	-0.051381	4.152600
256.195827	5880.861015	15.602074	-0.051332	4.149875
256.192432	5872.887620	15.607079	-0.051326	4.147168
256.214274	5864.859755	15.612083	-0.051325	4.144441
256.655677	5856.930600	15.617088	-0.051402	4.141751
256.449651	5848.893761	15.622093	-0.051358	4.139014
256.316170	5840.886314	15.627098	-0.051328	4.136287
256.462088	5832.880538	15.632103	-0.051350	4.133562
256.307538	5824.859763	15.637107	-0.051316	4.130826
256.335448	5816.887127	15.642112	-0.051316	4.128107
256.269858	5808.876533	15.647117	-0.051299	4.125372
256.205230	5800.927907	15.652122	-0.051281	4.122657
256.223306	5792.912996	15.657127	-0.051279	4.119918
256.163498	5784.941909	15.662131	-0.051263	4.117191
256.321857	5776.892267	15.667136	-0.051287	4.114438
255.948679	5768.879815	15.672141	-0.051212	4.111690
255.845740	5760.866298	15.677146	-0.051188	4.108942
255.949503	5752.898568	15.682151	-0.051202	4.106212
255.925741	5744.823646	15.687155	-0.051192	4.103440
255.941315	5736.879935	15.692160	-0.051190	4.100713
255.853570	5728.881917	15.697165	-0.051168	4.097964
255.869130	5720.897101	15.702170	-0.051166	4.095219
255.644690	5712.911580	15.707175	-0.051119	4.092468
255.495763	5704.856050	15.712179	-0.051086	4.089693
255.668053	5696.935625	15.717184	-0.051113	4.086966
255.605488	5688.883971	15.722189	-0.051096	4.084190
255.449062	5680.979971	15.727194	-0.051062	4.081461
255.647343	5672.954146	15.732199	-0.051093	4.078693
255.618790	5664.945516	15.737203	-0.051083	4.075926
255.555323	5656.934724	15.742208	-0.051066	4.073155
255.464037	5648.892652	15.747213	-0.051043	4.070372
255.512620	5640.911734	15.752218	-0.051047	4.067610
255.607875	5632.919898	15.757223	-0.051060	4.064843
255.265782	5624.963165	15.762227	-0.050991	4.062080
255.445678	5616.980527	15.767232	-0.051019	4.059314
255.223670	5608.981287	15.772237	-0.050972	4.056534
254.991586	5600.934142	15.777242	-0.050924	4.053735
255.130226	5592.912139	15.782247	-0.050944	4.050949
255.016116	5584.901760	15.787251	-0.050918	4.048161
255.090921	5576.936486	15.792256	-0.050927	4.045390
254.839271	5568.955571	15.797261	-0.050874	4.042606
254.921765	5560.941829	15.802266	-0.050885	4.039814
254.992736	5553.009255	15.807271	-0.050893	4.037048
254.998594	5544.922163	15.812275	-0.050888	4.034226
255.245838	5536.829399	15.817280	-0.050929	4.031403
255.018479	5528.884267	15.822285	-0.050882	4.028622
254.844631	5520.890633	15.827290	-0.050844	4.025824
254.857214	5512.925673	15.832295	-0.050841	4.023036
254.828023	5504.904810	15.837299	-0.050830	4.020226
254.818865	5496.931429	15.842304	-0.050823	4.017431
254.869302	5488.914691	15.847309	-0.050827	4.014620
254.690992	5480.893309	15.852314	-0.050789	4.011802
254.901063	5472.904669	15.857319	-0.050823	4.009000
254.551986	5464.892535	15.862323	-0.050753	4.006178
254.753923	5456.944702	15.867328	-0.050785	4.003386
254.786831	5448.921341	15.872333	-0.050786	4.000562
254.614575	5440.921850	15.877338	-0.050748	3.997742
254.652262	5432.932641	15.882343	-0.050750	3.994926
254.705121	5424.867841	15.887347	-0.050755	3.992082
254.690572	5416.885271	15.892352	-0.050747	3.989264
254.568016	5408.915128	15.897357	-0.050719	3.986447
254.562002	5400.911703	15.902362	-0.050712	3.983618
254.446488	5392.957911	15.907367	-0.050686	3.980803
254.215801	5384.953492	15.912371	-0.050637	3.977965
254.224365	5376.969162	15.917376	-0.050634	3.975137
254.215178	5368.936775	15.922381	-0.050627	3.972290
254.140668	5360.922059	15.927386	-0.050608	3.969445
254.276770	5352.951430	15.932391	-0.050628	3.966618
254.400523	5344.908840	15.937395	-0.050646	3.963763
254.406618	5336.978613	15.942400	-0.050641	3.960944
254.199977	5328.997639	15.947405	-0.050598	3.958101
254.158296	5320.975048	15.952410	-0.050585	3.955244
254.331702	5312.960073	15.957415	-0.050612	3.952391
254.102324	5304.910980	15.962419	-0.050564	3.949517
254.182452	5296.959376	15.967424	-0.050573	3.946682
254.293966	5288.940242	15.972429	-0.050589	3.943820
254.071501	5280.996681	15.977434	-0.050542	3.940978
253.880819	5273.052137	15.982439	-0.050502	3.938134
253.797182	5264.972902	15.987443	-0.050481	3.935241
254.039638	5256.975714	15.992448	-0.050521	3.932382
253.669160	5248.962780	15.997453	-0.050446	3.929504
253.653578	5240.983240	16.002458	-0.050438	3.926642
253.828045	5233.009478	16.007463	-0.050465	3.923783
253.610122	5225.010995	16.012467	-0.050420	3.920907
253.770401	5217.019165	16.017472	-0.050444	3.918037
253.824369	5209.026424	16.022477	-0.050449	3.915163
253.770357	5200.971385	16.027482	-0.050434	3.912263
253.569215	5192.991452	16.032487	-0.050391	3.909385
253.563422	5184.977074	16.037491	-0.050385	3.906496
253.561943	5177.003014	16.042496	-0.050379	3.903619
253.414981	5168.992288	16.047501	-0.050346	3.900724
253.220894	5161.032374	16.052506	-0.050305	3.897845
253.527784	5153.008946	16.057511	-0.050357	3.894950
253.362070	5144.974021	16.062515	-0.050321	3.892040
253.313864	5136.974301	16.067520	-0.050307	3.889142
253.293546	5129.008371	16.072525	-0.050297	3.886255
253.389849	5120.986218	16.077530	-0.050310	3.883348
253.338792	5113.022643	16.082535	-0.050295	3.880457
253.231284	5105.034548	16.087539	-0.050270	3.877554
253.350669	5096.997326	16.092544	-0.050287	3.874635
253.271579	5088.771784	16.097549	-0.050267	3.871642
253.236126	5080.810914	16.102554	-0.050255	3.868743
253.367732	5072.919752	16.107559	-0.050274	3.865871
253.285350	5064.923683	16.112563	-0.050254	3.862955
253.083589	5056.963343	16.117568	-0.050211	3.860047
253.170043	5049.023142	16.122573	-0.050222	3.857149
253.002634	5041.001261	16.127578	-0.050185	3.854215
253.219167	5032.992445	16.132583	-0.050221	3.851291
252.996965	5024.966277	16.137587	-0.050174	3.848349
252.906779	5016.999483	16.142592	-0.050152	3.845430
252.906573	5009.043109	16.147597	-0.050147	3.842514
252.690611	5001.023227	16.152602	-0.050101	3.839568
252.833821	4993.080312	16.157607	-0.050123	3.836656
252.718001	4985.011908	16.162611	-0.050096	3.833689
252.616420	4977.022004	16.167616	-0.050072	3.830750
252.678305	4969.035752	16.172621	-0.050078	3.827813
252.544035	4961.043942	16.177626	-0.050048	3.824868
252.569814	4953.088976	16.182631	-0.050047	3.821937
252.485431	4945.050816	16.187635	-0.050026	3.818971
252.574881	4937.078245	16.192640	-0.050038	3.816031
252.430366	4929.064508	16.197645	-0.050005	3.813068
252.369196	4921.033647	16.202650	-0.049989	3.810099
252.561067	4913.102306	16.207655	-0.050019	3.807169
252.499394	4905.065383	16.212659	-0.050002	3.804192
252.495212	4897.129964	16.217664	-0.049996	3.801252
252.424950	4889.099372	16.222669	-0.049978	3.798273
252.406052	4881.124225	16.227674	-0.049969	3.795314
252.156434	4873.094205	16.232679	-0.049918	3.792326
252.044291	4865.068325	16.237683	-0.049891	3.789341
252.164138	4857.086157	16.242688	-0.049908	3.786375
252.000709	4849.086923	16.247693	-0.049873	3.783394
252.144143	4841.087360	16.252698	-0.049894	3.780417
252.023990	4833.156808	16.257703	-0.049867	3.777457
252.146879	4825.068950	16.262707	-0.049884	3.774443
252.090055	4817.106221	16.267712	-0.049868	3.771468
251.760049	4809.072068	16.272717	-0.049802	3.768458
252.023626	4801.073326	16.277722	-0.049845	3.765472
252.113823	4793.126457	16.282727	-0.049857	3.762500
251.908137	4785.104877	16.287731	-0.049813	3.759490
251.846342	4777.170018	16.292736	-0.049797	3.756514
251.812095	4769.111685	16.297741	-0.049785	3.753490
251.657599	4761.090598	16.302746	-0.049751	3.750474
251.707989	4753.124739	16.307751	-0.049755	3.747482
251.701700	4745.065046	16.312755	-0.049749	3.744450
251.564492	4737.156883	16.317760	-0.049718	3.741470
251.564203	4729.134652	16.322765	-0.049713	3.738448
251.568631	4721.111996	16.327770	-0.049708	3.735424
251.467746	4713.162872	16.332775	-0.049684	3.732422
251.505631	4705.102314	16.337779	-0.049686	3.729379
251.536274	4697.156956	16.342784	-0.049686	3.726377
251.441009	4689.159191	16.347789	-0.049663	3.723349
251.344750	4681.138365	16.352794	-0.049640	3.720311
251.731371	4673.179655	16.357799	-0.049707	3.717305
251.462913	4665.150849	16.362803	-0.049652	3.714254
251.475126	4657.081869	16.367808	-0.049649	3.711192
251.304860	4649.112707	16.372813	-0.049612	3.708162
251.440308	4641.141787	16.377818	-0.049632	3.705135
251.487735	4633.214233	16.382823	-0.049635	3.702120
251.439670	4625.159193	16.387827	-0.049621	3.699052
251.259394	4617.220259	16.392832	-0.049582	3.696023
251.348423	4609.188397	16.397837	-0.049594	3.692962
251.036131	4601.197780	16.402842	-0.049530	3.689904
251.052845	4593.235487	16.407847	-0.049528	3.686863
251.087829	4585.195291	16.412851	-0.049529	3.683790
251.026499	4577.247310	16.417856	-0.049513	3.680748
250.979872	4569.275617	16.422861	-0.049499	3.677694
251.048415	4561.220635	16.427866	-0.049506	3.674608
251.070833	4553.215351	16.432871	-0.049505	3.671538
250.924548	4545.220787	16.437875	-0.049473	3.668465
250.943293	4537.224301	16.442880	-0.049471	3.665393
250.840879	4529.262998	16.447885	-0.049447	3.662329
250.838939	4521.210784	16.452890	-0.049441	3.659229
250.983379	4513.290734	16.457895	-0.049463	3.656182
250.848425	4505.217397	16.462899	-0.049432	3.653066
250.959745	4497.223941	16.467904	-0.049448	3.649985
250.803537	4489.265240	16.472909	-0.049413	3.646907
251.031892	4481.224710	16.477914	-0.049451	3.643805
250.920472	4473.299073	16.482919	-0.049425	3.640737
250.614897	4465.305748	16.487923	-0.049362	3.637634
250.562101	4457.314737	16.492928	-0.049347	3.634536
250.521045	4449.278254	16.497933	-0.049334	3.631418
250.425999	4441.247641	16.502938	-0.049311	3.628298
250.478794	4433.261034	16.507943	-0.049316	3.625196
250.368668	4425.295080	16.512947	-0.049290	3.622096
250.348253	4417.296814	16.517952	-0.049281	3.618983
250.292429	4409.355214	16.522957	-0.049266	3.615888
250.488155	4401.288182	16.527962	-0.049297	3.612748
250.469417	4393.289678	16.532967	-0.049288	3.609627
250.304084	4385.333304	16.537971	-0.049252	3.606515
250.289601	4377.346772	16.542976	-0.049244	3.603393
250.337718	4369.364294	16.547981	-0.049248	3.600272
250.315450	4361.386596	16.552986	-0.049238	3.597148
250.159363	4353.385647	16.557991	-0.049204	3.594008
250.280139	4345.339985	16.562995	-0.049221	3.590856
250.185198	4337.384499	16.568000	-0.049198	3.587730
250.129336	4329.371213	16.573005	-0.049183	3.584580
249.822478	4321.392760	16.578010	-0.049120	3.581433
249.803011	4313.430653	16.583015	-0.049111	3.578299
249.704586	4305.414766	16.588019	-0.049088	3.575138
249.742790	4297.427669	16.593024	-0.049090	3.571990
249.812828	4289.387541	16.598029	-0.049097	3.568819
249.724700	4281.393829	16.603034	-0.049076	3.565659
249.608754	4273.459029	16.608039	-0.049049	3.562519
249.549682	4265.419822	16.613043	-0.049033	3.559336
249.639127	4257.493431	16.618048	-0.049044	3.556199
249.694612	4249.397037	16.623053	-0.049049	3.552991
249.664720	4241.314305	16.628058	-0.049038	3.549783
249.582077	4233.392930	16.633063	-0.049018	3.546635
249.425552	4225.404876	16.638067	-0.048983	3.543455
249.545052	4217.424499	16.643072	-0.049000	3.540284
249.532681	4209.448623	16.648077	-0.048993	3.537108
249.466868	4201.441679	16.653082	-0.048975	3.533914
249.586507	4193.421703	16.658087	-0.048992	3.530719
249.451590	4185.435303	16.663091	-0.048962	3.527526
249.480324	4177.451551	16.668096	-0.048962	3.524336
249.373666	4169.497835	16.673101	-0.048937	3.521151
249.194736	4161.481295	16.678106	-0.048898	3.517936
249.338830	4153.502678	16.683111	-0.048920	3.514743
249.329925	4145.464439	16.688115	-0.048913	3.511519
249.249616	4137.482627	16.693120	-0.048893	3.508312
249.402745	4129.467591	16.698125	-0.048916	3.505096
249.091651	4121.531507	16.703130	-0.048853	3.501895
248.943976	4113.545175	16.708135	-0.048820	3.498675
249.208703	4105.517115	16.713139	-0.048864	3.495448
249.129747	4097.537883	16.718144	-0.048844	3.492228
249.251385	4089.537987	16.723149	-0.048862	3.489002
249.027899	4081.571742	16.728154	-0.048815	3.485776
249.031535	4073.610548	16.733159	-0.048810	3.482556
248.903172	4065.593126	16.738163	-0.048781	3.479307
248.864768	4057.636988	16.743168	-0.048769	3.476081
248.741034	4049.614230	16.748173	-0.048740	3.472824
248.694502	4041.562952	16.753178	-0.048726	3.469554
248.761067	4033.593994	16.758183	-0.048734	3.466318
248.676135	4025.623061	16.763187	-0.048712	3.463073
248.614711	4017.604871	16.768192	-0.048696	3.459807
248.582034	4009.651714	16.773197	-0.048684	3.456565
248.522527	4001.617151	16.778202	-0.048668	3.453286
248.601471	3993.607377	16.783207	-0.048678	3.450018
248.289630	3985.645124	16.788211	-0.048614	3.446754
248.312030	3977.637562	16.793216	-0.048613	3.443480
248.261185	3969.658038	16.798221	-0.048598	3.440211
248.334470	3961.670698	16.803226	-0.048607	3.436940
248.309617	3953.675354	16.808231	-0.048597	3.433659
248.166002	3945.628976	16.813235	-0.048565	3.430351
248.209817	3937.663150	16.818240	-0.048568	3.427078
248.179015	3929.660983	16.823245	-0.048557	3.423785
248.190128	3921.682028	16.828250	-0.048554	3.420500
248.231884	3913.735465	16.833255	-0.048556	3.417226
248.107941	3905.697513	16.838259	-0.048528	3.413905
247.987504	3897.720801	16.843264	-0.048500	3.410607
247.933037	3889.728269	16.848269	-0.048485	3.407301
247.920539	3881.728717	16.853274	-0.048477	3.403990
247.827227	3873.764045	16.858279	-0.048455	3.400688
247.806280	3865.798092	16.863283	-0.048445	3.397385
247.973481	3857.774496	16.868288	-0.048471	3.394061
248.026809	3849.702906	16.873293	-0.048476	3.390710
247.693939	3841.753611	16.878298	-0.048409	3.387393
247.886800	3833.741629	16.883303	-0.048439	3.384065
247.454152	3825.811355	16.888307	-0.048354	3.380745
247.473235	3817.830555	16.893312	-0.048352	3.377417
247.549672	3809.803405	16.898317	-0.048361	3.374069
247.678186	3801.784982	16.903322	-0.048380	3.370723
247.519396	3793.845256	16.908327	-0.048345	3.367396
247.559189	3785.838327	16.913331	-0.048347	3.364045
247.533130	3777.880748	16.918336	-0.048337	3.360709
247.459565	3769.903190	16.923341	-0.048318	3.357359
247.318392	3761.877789	16.928346	-0.048286	3.353984
247.418902	3753.858962	16.933351	-0.048300	3.350616
247.400827	3745.865835	16.938355	-0.048291	3.347252
247.270312	3737.886808	16.943360	-0.048262	3.343886
247.346031	3729.922369	16.948365	-0.048270	3.340531
247.181420	3721.909221	16.953370	-0.048235	3.337142
247.227264	3713.939825	16.958375	-0.048238	3.333777
247.104513	3705.890666	16.963379	-0.048210	3.330368
247.326981	3697.900598	16.968384	-0.048246	3.326993
247.071197	3689.955431	16.973389	-0.048193	3.323617
247.132838	3681.964015	16.978394	-0.048199	3.320229
247.251511	3674.002881	16.983399	-0.048216	3.316852
247.096535	3665.976394	16.988403	-0.048182	3.313434
247.037696	3657.968073	16.993408	-0.048166	3.310024
247.138062	3649.960478	16.998413	-0.048179	3.306617
246.941360	3641.999265	17.003418	-0.048137	3.303214
247.186995	3634.006864	17.008423	-0.048178	3.299812
246.906864	3626.071821	17.013427	-0.048120	3.296411
247.068832	3618.016472	17.018432	-0.048145	3.292971
246.889491	3610.035111	17.023437	-0.048107	3.289547
246.851157	3602.051638	17.028442	-0.048094	3.286123
246.748552	3594.115032	17.033447	-0.048070	3.282713
246.857641	3586.092757	17.038451	-0.048085	3.279272
246.692270	3578.154526	17.043456	-0.048049	3.275852
246.739412	3570.106055	17.048461	-0.048052	3.272389
246.756182	3562.075366	17.053466	-0.048050	3.268929
246.696280	3554.108634	17.058471	-0.048034	3.265491
246.386165	3546.162356	17.063475	-0.047971	3.262047
246.507552	3538.151897	17.068480	-0.047988	3.258589
246.500123	3530.171082	17.073485	-0.047982	3.255135
246.388316	3522.146400	17.078490	-0.047956	3.251654
246.336480	3514.188160	17.083495	-0.047941	3.248201
246.308250	3506.177293	17.088499	-0.047930	3.244722
246.114387	3498.250676	17.093504	-0.047889	3.241270
246.058270	3490.258146	17.098509	-0.047873	3.237790
246.112297	3482.218865	17.103514	-0.047878	3.234291
246.185021	3474.189383	17.108519	-0.047886	3.230793
245.912574	3466.192201	17.113523	-0.047830	3.227292
245.846731	3458.216648	17.118528	-0.047813	3.223804
245.946509	3450.272048	17.123533	-0.047826	3.220333
245.671520	3442.282803	17.128538	-0.047770	3.216823
245.835468	3434.275347	17.133543	-0.047795	3.213320
245.882728	3426.253421	17.138547	-0.047798	3.209801
245.782003	3418.325989	17.143552	-0.047774	3.206314
245.724487	3410.351351	17.148557	-0.047758	3.202804
245.745326	3402.340493	17.153562	-0.047757	3.199278
245.740504	3394.370631	17.158567	-0.047751	3.195765
245.441253	3386.374654	17.163571	-0.047690	3.192224
245.774054	3378.335843	17.168576	-0.047747	3.188687
245.885494	3370.330493	17.173581	-0.047762	3.185151
245.735846	3362.383669	17.178586	-0.047729	3.181626
245.535087	3354.451340	17.183591	-0.047686	3.178102
245.444031	3346.411176	17.188595	-0.047664	3.174530
245.478980	3338.410805	17.193600	-0.047665	3.170978
245.436029	3330.436734	17.198605	-0.047652	3.167430
245.356010	3322.431760	17.203610	-0.047632	3.163862
245.331605	3314.495566	17.208615	-0.047622	3.160324
245.095784	3306.513306	17.213619	-0.047573	3.156751
245.156505	3298.492465	17.218624	-0.047579	3.153171
245.207271	3290.471911	17.223629	-0.047583	3.149586
245.196096	3282.460949	17.228634	-0.047576	3.145998
245.180662	3274.521500	17.233639	-0.047568	3.142439
245.157587	3266.527148	17.238643	-0.047558	3.138850
245.149069	3258.565522	17.243648	-0.047552	3.135272
245.150021	3250.562807	17.248653	-0.047546	3.131673
244.957875	3242.572426	17.253658	-0.047505	3.128066
245.025790	3234.569784	17.258663	-0.047513	3.124461
245.027779	3226.637492	17.263667	-0.047508	3.120881
244.801126	3218.663132	17.268672	-0.047460	3.117267
244.799162	3210.662672	17.273677	-0.047455	3.113647
244.855010	3202.634758	17.278682	-0.047460	3.110014
244.839105	3194.650202	17.283687	-0.047452	3.106392
244.712218	3186.675080	17.288691	-0.047423	3.102766
244.681225	3178.682571	17.293696	-0.047412	3.099131
244.681227	3170.741594	17.298701	-0.047407	3.095517
244.448993	3162.744927	17.303706	-0.047358	3.091863
244.905487	3154.703417	17.308711	-0.047438	3.088216
244.651498	3146.732043	17.313715	-0.047385	3.084564
244.433178	3138.794608	17.318720	-0.047339	3.080925
244.405995	3130.828873	17.323725	-0.047329	3.077277
244.537459	3122.768655	17.328730	-0.047348	3.073589
244.417052	3114.745733	17.333735	-0.047321	3.069902
244.372915	3106.758690	17.338739	-0.047307	3.066231
244.471854	3098.769328	17.343744	-0.047320	3.062560
244.434054	3090.827888	17.348749	-0.047308	3.058901
244.290894	3082.853998	17.353754	-0.047276	3.055218
244.369791	3074.872382	17.358759	-0.047286	3.051537
244.166338	3066.878805	17.363763	-0.047243	3.047833
244.225972	3058.884090	17.368768	-0.047248	3.044136
244.068355	3050.961247	17.373773	-0.047214	3.040458
244.089264	3042.960307	17.378778	-0.047212	3.036747
244.185434	3034.961329	17.383783	-0.047225	3.033037
244.164156	3026.932637	17.388787	-0.047216	3.029302
244.096175	3018.968982	17.393792	-0.047198	3.025591
244.011911	3011.024196	17.398797	-0.047177	3.021883
243.839523	3003.032237	17.403802	-0.047140	3.018145
243.978787	2995.056360	17.408807	-0.047160	3.014424
243.806178	2987.052963	17.413811	-0.047123	3.010671
243.616350	2979.081426	17.418816	-0.047082	3.006927
243.682061	2971.087023	17.423821	-0.047089	3.003180
243.558503	2963.111237	17.428826	-0.047061	2.999428
243.821007	2955.157113	17.433831	-0.047105	2.995701
243.446632	2947.149640	17.438835	-0.047030	2.991912
243.441103	2939.142503	17.443840	-0.047024	2.988137
243.576298	2931.123926	17.448845	-0.047043	2.984359
243.558821	2923.162055	17.453850	-0.047035	2.980595
243.530359	2915.210104	17.458855	-0.047024	2.976830
243.267614	2907.225437	17.463859	-0.046970	2.973034
243.182018	2899.219652	17.468864	-0.046949	2.969231
243.183054	2891.260198	17.473869	-0.046944	2.965450
243.385376	2883.262381	17.478874	-0.046976	2.961656
243.187671	2875.325616	17.483879	-0.046934	2.957866
243.077578	2867.320333	17.488883	-0.046909	2.954043
243.127910	2859.303573	17.493888	-0.046913	2.950218
243.196541	2851.328486	17.498893	-0.046920	2.946408
242.907172	2843.375760	17.503898	-0.046861	2.942586
243.110026	2835.390490	17.508903	-0.046894	2.938769
242.942964	2827.411525	17.513907	-0.046857	2.934930
242.940758	2819.412790	17.518912	-0.046852	2.931086
242.962932	2811.432263	17.523917	-0.046851	2.927246
242.930116	2803.436483	17.528922	-0.046839	2.923391
242.903598	2795.497780	17.533927	-0.046829	2.919560
242.616708	2787.555467	17.538931	-0.046770	2.915707
242.809530	2779.427261	17.543936	-0.046801	2.911785
242.839719	2771.439872	17.548941	-0.046801	2.907917
242.554323	2763.512059	17.553946	-0.046743	2.904056
242.437920	2755.573054	17.558951	-0.046716	2.900193
242.618317	2747.581685	17.563955	-0.046744	2.896316
242.560609	2739.586969	17.568960	-0.046728	2.892419
242.489261	2731.612250	17.573965	-0.046710	2.888526
242.251087	2723.628554	17.578970	-0.046660	2.884614
242.384904	2715.674320	17.583975	-0.046680	2.880732
242.234466	2707.706413	17.588979	-0.046647	2.876822
242.382832	2699.689911	17.593984	-0.046669	2.872899
242.431027	2691.677711	17.598989	-0.046673	2.868967
242.337084	2683.698767	17.603994	-0.046650	2.865039
242.225522	2675.761313	17.608999	-0.046624	2.861125
242.333328	2667.791092	17.614003	-0.046639	2.857201
242.287131	2659.793528	17.619008	-0.046625	2.853250
242.295941	2651.791386	17.624013	-0.046621	2.849294
242.243387	2643.828724	17.629018	-0.046606	2.845349
242.220124	2635.888287	17.634023	-0.046597	2.841410
241.944638	2627.928451	17.639027	-0.046540	2.837443
241.906188	2619.918415	17.644032	-0.046528	2.833458
242.059102	2611.897229	17.649037	-0.046551	2.829473
241.982941	2603.920297	17.654042	-0.046532	2.825492
241.915092	2595.978693	17.659047	-0.046514	2.821523
241.878579	2588.006648	17.664051	-0.046502	2.817535
241.745871	2580.017694	17.669056	-0.046472	2.813527
241.787185	2572.017704	17.674061	-0.046474	2.809518
241.689686	2564.044471	17.679066	-0.046451	2.805509
241.917212	2556.076225	17.684071	-0.046488	2.801515
241.665879	2548.116917	17.689075	-0.046436	2.797493
241.380268	2540.153365	17.694080	-0.046378	2.793460
241.471151	2532.138065	17.699085	-0.046389	2.789417
241.348938	2524.159691	17.704090	-0.046361	2.785375
241.380780	2516.216319	17.709095	-0.046362	2.781353
241.454227	2508.219911	17.714099	-0.046370	2.777302
241.496456	2500.235702	17.719104	-0.046373	2.773248
241.422378	2492.247298	17.724109	-0.046354	2.769180
241.348645	2484.257774	17.729114	-0.046335	2.765105
241.450837	2476.327309	17.734119	-0.046349	2.761065
241.141135	2468.390220	17.739123	-0.046286	2.756991
241.045046	2460.350900	17.744128	-0.046263	2.752871
241.398768	2452.293187	17.749133	-0.046323	2.748763
241.060279	2444.339960	17.754138	-0.046255	2.744660
240.900715	2436.434102	17.759143	-0.046220	2.740587
240.880962	2428.456266	17.764147	-0.046211	2.736478
240.991722	2420.450738	17.769152	-0.046226	2.732358
240.848182	2412.495287	17.774157	-0.046195	2.728241
240.801440	2404.496367	17.779162	-0.046181	2.724102
240.831718	2396.543217	17.784167	-0.046181	2.719984
240.842029	2388.591243	17.789171	-0.046178	2.715860
240.657477	2380.609184	17.794176	-0.046138	2.711702
240.796953	2372.610259	17.799181	-0.046159	2.707549
240.716429	2364.637344	17.804186	-0.046139	2.703389
240.473590	2356.706408	17.809191	-0.046088	2.699234
240.582186	2348.727622	17.814195	-0.046103	2.695071
240.691231	2340.695502	17.819200	-0.046118	2.690872
240.651941	2332.760394	17.824205	-0.046106	2.686709
240.559803	2324.767367	17.829210	-0.046083	2.682506
240.701759	2316.823214	17.834215	-0.046104	2.678336
240.607263	2308.860221	17.839219	-0.046082	2.674135
240.384207	2300.860968	17.844224	-0.046035	2.669900
240.383018	2292.901252	17.849229	-0.046029	2.665694
240.212016	2284.925288	17.854234	-0.045992	2.661461
240.144970	2276.978840	17.859239	-0.045975	2.657244
240.100685	2268.988800	17.864243	-0.045961	2.652998
240.103708	2260.985837	17.869248	-0.045956	2.648742
239.982536	2253.054592	17.874253	-0.045929	2.644509
239.893890	2245.081838	17.879258	-0.045907	2.640249
239.871403	2237.129036	17.884263	-0.045897	2.635998
239.858728	2229.112398	17.889267	-0.045890	2.631705
239.843888	2221.123364	17.894272	-0.045882	2.627421
239.814875	2213.186294	17.899277	-0.045871	2.623156
239.796359	2205.206913	17.904282	-0.045862	2.618863
239.730977	2197.249041	17.909287	-0.045845	2.614571
239.685477	2189.254696	17.914291	-0.045831	2.610253
239.791620	2181.272915	17.919296	-0.045846	2.605945
239.676864	2173.357422	17.924301	-0.045819	2.601652
239.496298	2165.396554	17.929306	-0.045780	2.597322
239.679435	2157.318641	17.934311	-0.045809	2.592945
239.652479	2149.235550	17.939315	-0.045799	2.588544
239.510702	2141.307928	17.944320	-0.045767	2.584213
239.421340	2133.405092	17.949325	-0.045745	2.579892
239.324237	2125.460629	17.954330	-0.045722	2.575540
239.358257	2117.493780	17.959335	-0.045723	2.571177
239.221779	2109.534364	17.964339	-0.045693	2.566799
239.251182	2101.569071	17.969344	-0.045693	2.562422
239.356219	2093.626772	17.974349	-0.045707	2.558055
239.157697	2085.653871	17.979354	-0.045665	2.553643
239.200980	2077.667851	17.984359	-0.045668	2.549233
239.208667	2069.687183	17.989363	-0.045664	2.544816
238.963233	2061.771703	17.994368	-0.045613	2.540409
239.105449	2053.805528	17.999373	-0.045634	2.535994
239.057079	2045.807675	18.004378	-0.045620	2.531540
238.888693	2037.862768	18.009383	-0.045583	2.527099
238.726770	2029.935005	18.014387	-0.045548	2.522660
238.925355	2021.941884	18.019392	-0.045580	2.518203
238.895584	2013.974302	18.024397	-0.045569	2.513736
238.505541	2005.997230	18.029402	-0.045491	2.509229
238.528640	1998.036965	18.034407	-0.045490	2.504754
238.520892	1990.072465	18.039411	-0.045484	2.500266
238.489080	1982.111834	18.044416	-0.045472	2.495770
238.539488	1974.140856	18.049421	-0.045477	2.491266
238.534828	1966.139909	18.054426	-0.045470	2.486734
238.302505	1958.228433	18.059431	-0.045422	2.482227
238.351701	1950.274577	18.064435	-0.045426	2.477708
238.201922	1942.312630	18.069440	-0.045393	2.473162
238.459588	1934.295900	18.074445	-0.045435	2.468606
238.314986	1926.337040	18.079450	-0.045403	2.464045
238.343295	1918.400073	18.084455	-0.045403	2.459501
238.252385	1910.453135	18.089459	-0.045381	2.454934
238.068868	1902.489774	18.094464	-0.045342	2.450342
238.120558	1894.519227	18.099469	-0.045346	2.445755
238.024331	1886.571695	18.104474	-0.045323	2.441162
238.085393	1878.625743	18.109479	-0.045329	2.436572
237.785100	1870.635221	18.114483	-0.045268	2.431921
237.853835	1862.615459	18.119488	-0.045276	2.427272
238.048864	1854.650358	18.124493	-0.045307	2.422655
237.899761	1846.712432	18.129498	-0.045274	2.418019
237.821487	1838.777749	18.134503	-0.045254	2.413382
237.742418	1830.808334	18.139507	-0.045234	2.408715
237.689096	1822.848053	18.144512	-0.045219	2.404046
237.643908	1814.921567	18.149517	-0.045205	2.399389
237.527319	1806.968324	18.154522	-0.045178	2.394701
237.522414	1798.992248	18.159527	-0.045172	2.389999
237.360199	1791.028091	18.164531	-0.045137	2.385283
237.407545	1783.063821	18.169536	-0.045140	2.380574
237.609925	1775.109194	18.174541	-0.045173	2.375874
237.451906	1767.143791	18.179546	-0.045138	2.371129
237.449373	1759.193934	18.184551	-0.045132	2.366396
237.325818	1751.247263	18.189555	-0.045104	2.361646
237.244922	1743.313241	18.194560	-0.045084	2.356898
237.169078	1735.357855	18.199565	-0.045064	2.352127
237.191075	1727.345640	18.204570	-0.045063	2.347321
237.300754	1719.371637	18.209575	-0.045078	2.342535
237.227740	1711.453656	18.214579	-0.045060	2.337757
237.093626	1703.514749	18.219584	-0.045029	2.332953
237.084311	1695.541267	18.224589	-0.045022	2.328128
236.896753	1687.609637	18.229594	-0.044982	2.323303
236.914434	1679.670429	18.234599	-0.044980	2.318481
236.996987	1671.707090	18.239603	-0.044990	2.313639
236.926821	1663.723753	18.244608	-0.044972	2.308762
236.803555	1655.799539	18.249613	-0.044944	2.303907
236.667005	1647.860330	18.254618	-0.044913	2.299031
236.722202	1639.898480	18.259623	-0.044918	2.294147
236.526697	1631.954596	18.264627	-0.044877	2.289242
236.570752	1623.979914	18.269632	-0.044880	2.284329
236.668230	1616.056356	18.274637	-0.044893	2.279440
236.606061	1608.101285	18.279642	-0.044876	2.274508
236.458812	1600.082823	18.284647	-0.044843	2.269519
236.437645	1592.119753	18.289651	-0.044834	2.264564
236.229920	1584.216519	18.294656	-0.044790	2.259619
236.311170	1576.273574	18.299661	-0.044800	2.254664
236.429784	1568.277078	18.304666	-0.044817	2.249667
236.372085	1560.347177	18.309671	-0.044801	2.244686
236.196575	1552.446390	18.314675	-0.044763	2.239701
236.162908	1544.491774	18.319680	-0.044752	2.234684
236.255608	1536.511428	18.324685	-0.044764	2.229651
236.018057	1528.581767	18.329690	-0.044714	2.224609
235.910995	1520.668383	18.334695	-0.044689	2.219577
235.941439	1512.712740	18.339699	-0.044689	2.214519
235.930584	1504.737514	18.344704	-0.044682	2.209434
235.911301	1496.812575	18.349709	-0.044673	2.204368
235.733890	1488.893596	18.354714	-0.044635	2.199280
235.791801	1480.934783	18.359719	-0.044641	2.194176
235.673700	1472.964333	18.364723	-0.044613	2.189037
235.454989	1465.033693	18.369728	-0.044568	2.183902
235.668233	1457.081300	18.374733	-0.044602	2.178780
235.623338	1449.138638	18.379738	-0.044588	2.173629
235.458496	1441.199000	18.384743	-0.044552	2.168457
235.547007	1433.247584	18.389747	-0.044564	2.163287
235.543639	1425.319120	18.394752	-0.044558	2.158112
235.516016	1417.389054	18.399757	-0.044548	2.152922
235.356688	1409.438472	18.404762	-0.044513	2.147692
235.414785	1401.493761	18.409767	-0.044518	2.142475
235.262235	1393.590272	18.414771	-0.044485	2.137252
235.214192	1385.633607	18.419776	-0.044470	2.131990
235.273508	1377.684928	18.424781	-0.044476	2.126732
235.259772	1369.754623	18.429786	-0.044469	2.121465
235.250756	1361.837934	18.434791	-0.044462	2.116195
235.021765	1353.865232	18.439795	-0.044414	2.110853
235.178910	1345.885474	18.444800	-0.044438	2.105530
235.008421	1337.987366	18.449805	-0.044401	2.100217
234.925900	1330.061123	18.454810	-0.044380	2.094880
234.869170	1322.116454	18.459815	-0.044364	2.089519
234.858856	1314.188910	18.464819	-0.044357	2.084161
234.760617	1306.284641	18.469824	-0.044334	2.078795
234.856046	1298.347595	18.474829	-0.044346	2.073413
234.748100	1290.379936	18.479834	-0.044321	2.067976
234.572355	1282.479040	18.484839	-0.044283	2.062563
234.798459	1274.535428	18.489843	-0.044320	2.057147
234.715015	1266.603380	18.494848	-0.044299	2.051694
234.682705	1258.687681	18.499853	-0.044288	2.046242
234.514171	1250.769941	18.504858	-0.044251	2.040760
234.488660	1242.865390	18.509863	-0.044242	2.035288
234.248525	1234.925404	18.514867	-0.044192	2.029754
234.137220	1226.989137	18.519872	-0.044166	2.024221
234.308661	1219.049201	18.524877	-0.044192	2.018699
234.092984	1211.142376	18.529882	-0.044147	2.013145
234.083764	1203.201848	18.534887	-0.044140	2.007573
234.197535	1195.263787	18.539891	-0.044156	2.002001
234.290944	1187.335264	18.544896	-0.044168	1.996418
234.016485	1179.441395	18.549901	-0.044112	1.990804
233.903539	1171.510138	18.554906	-0.044086	1.985166
233.963030	1163.593755	18.559911	-0.044092	1.979540
233.865531	1155.695473	18.564915	-0.044068	1.973894
233.736686	1147.755463	18.569920	-0.044039	1.968199
233.824248	1139.835689	18.574925	-0.044050	1.962525
233.733339	1131.940535	18.579930	-0.044028	1.956833
233.584757	1123.988721	18.584935	-0.043995	1.951078
233.719033	1116.015848	18.589939	-0.044015	1.945320
233.534979	1108.123516	18.594944	-0.043975	1.939570
233.563697	1100.226969	18.599949	-0.043976	1.933822
233.286334	1092.316958	18.604954	-0.043919	1.928014
233.343479	1084.397317	18.609959	-0.043924	1.922218
233.330586	1076.502943	18.614963	-0.043917	1.916416
233.139299	1068.581414	18.619968	-0.043876	1.910555
233.299429	1060.647113	18.624973	-0.043900	1.904707
233.161084	1052.756636	18.629978	-0.043869	1.898840
233.272117	1044.830138	18.634983	-0.043885	1.892956
233.040529	1036.933255	18.639987	-0.043837	1.887036
233.093891	1029.016688	18.644992	-0.043841	1.881116
232.987159	1021.143758	18.649997	-0.043816	1.875192
232.812173	1013.213293	18.655002	-0.043778	1.869197
232.770145	1005.304565	18.660007	-0.043765	1.863215
232.768234	997.408726	18.665011	-0.043760	1.857228
232.661304	989.495187	18.670016	-0.043735	1.851196
232.637194	981.594589	18.675021	-0.043725	1.845164
232.496371	973.716157	18.680026	-0.043694	1.839115
232.355338	965.837997	18.685031	-0.043662	1.833047
232.382066	957.911052	18.690035	-0.043662	1.826940
232.468631	949.991650	18.695040	-0.043673	1.820826
232.553344	942.099817	18.700045	-0.043683	1.814713
232.439614	934.197867	18.705050	-0.043657	1.808547
232.406754	926.312210	18.710055	-0.043646	1.802383
232.594059	918.405698	18.715059	-0.043675	1.796207
232.286123	910.495594	18.720064	-0.043613	1.789948
232.112353	902.621782	18.725069	-0.043575	1.783711
232.032954	894.738921	18.730074	-0.043555	1.777457
232.075763	886.828349	18.735079	-0.043558	1.771174
232.031880	878.948333	18.740083	-0.043545	1.764882
231.890020	871.081923	18.745088	-0.043513	1.758566
231.901416	863.201492	18.750093	-0.043510	1.752235
231.814148	855.306562	18.755098	-0.043489	1.745858
231.589480	847.453755	18.760103	-0.043442	1.739473
231.922823	839.529595	18.765107	-0.043499	1.733078
231.662571	831.663678	18.770112	-0.043445	1.726631
231.557600	823.811689	18.775117	-0.043420	1.720191
231.476297	815.941428	18.780122	-0.043400	1.713715
231.297814	808.059384	18.785127	-0.043362	1.707192
231.296007	800.171245	18.790131	-0.043356	1.700662
231.268463	792.301103	18.795136	-0.043346	1.694118
231.312095	784.409931	18.800141	-0.043349	1.687541
231.173855	776.549756	18.805146	-0.043318	1.680940
231.088486	768.703447	18.810151	-0.043297	1.674331
231.153181	760.812465	18.815155	-0.043304	1.667679
231.008136	752.957678	18.820160	-0.043271	1.661002
230.963398	745.112193	18.825165	-0.043258	1.654320
230.894359	737.233703	18.830170	-0.043240	1.647579
230.993428	729.357204	18.835175	-0.043253	1.640836
230.800934	721.526014	18.840179	-0.043212	1.634063
230.591968	713.632994	18.845184	-0.043168	1.627206
230.525165	705.789197	18.850189	-0.043150	1.620383
230.359633	697.949262	18.855194	-0.043114	1.613521
230.423259	690.068155	18.860199	-0.043121	1.606625
230.594259	682.205447	18.865203	-0.043148	1.599731
230.568836	674.358078	18.870208	-0.043138	1.592793
230.441225	666.522347	18.875213	-0.043109	1.585820
230.242748	658.708803	18.880218	-0.043067	1.578826
230.350940	650.841923	18.885223	-0.043082	1.571797
230.164935	643.031762	18.890227	-0.043042	1.564745
229.959818	635.225208	18.895232	-0.042999	1.557662
230.086256	627.351036	18.900237	-0.043017	1.550533
229.829809	619.532056	18.905242	-0.042964	1.543365
229.715935	611.708444	18.910247	-0.042938	1.536181
229.746538	603.872112	18.915251	-0.042938	1.528973
229.634234	596.041806	18.920256	-0.042912	1.521714
229.600770	588.238741	18.925261	-0.042901	1.514459
229.415996	580.406465	18.930266	-0.042862	1.507117
229.638155	572.553012	18.935271	-0.042898	1.499783
229.382897	564.779649	18.940275	-0.042845	1.492414
229.249301	556.962203	18.945280	-0.042815	1.484986
229.446546	549.134805	18.950285	-0.042847	1.477562
229.349759	541.287428	18.955290	-0.042823	1.470036
229.038446	533.511271	18.960295	-0.042760	1.462505
229.062120	525.704918	18.965299	-0.042760	1.454960
228.777420	517.922407	18.970304	-0.042702	1.447349
229.001352	510.101416	18.975309	-0.042738	1.439742
228.843004	502.319930	18.980314	-0.042703	1.432072
228.880092	494.509647	18.985319	-0.042705	1.424363
228.921901	486.727532	18.990323	-0.042708	1.416642
228.645757	478.970926	18.995328	-0.042651	1.408851
228.933155	471.142222	19.000333	-0.042700	1.401038
228.698478	463.401829	19.005338	-0.042651	1.393183
228.424609	455.646479	19.010343	-0.042595	1.385261
228.414786	447.870485	19.015347	-0.042588	1.377318
228.302839	440.099106	19.020352	-0.042562	1.369316
228.271542	432.339396	19.025357	-0.042551	1.361293
228.174159	424.590993	19.030362	-0.042528	1.353222
228.134332	416.813406	19.035367	-0.042515	1.345083
228.112451	409.080621	19.040371	-0.042506	1.336944
227.939014	401.336148	19.045376	-0.042469	1.328716
228.001955	393.582958	19.050381	-0.042475	1.320470
228.026077	385.786899	19.055386	-0.042475	1.312119
227.815524	378.003163	19.060391	-0.042430	1.303685
227.850039	370.276386	19.065395	-0.042432	1.295303
227.644905	362.568622	19.070400	-0.042389	1.286843
227.651551	354.862835	19.075405	-0.042385	1.278368
227.438335	347.173674	19.080410	-0.042340	1.269814
227.351570	339.471919	19.085415	-0.042319	1.261212
227.225791	331.790031	19.090419	-0.042290	1.252566
227.019066	324.102703	19.095424	-0.042247	1.243838
227.136941	316.399359	19.100429	-0.042264	1.235092
227.116382	308.677949	19.105434	-0.042255	1.226237
226.935349	301.023029	19.110439	-0.042216	1.217362
226.816795	293.354156	19.115443	-0.042189	1.208419
226.879342	285.664895	19.120448	-0.042195	1.199420
226.947121	277.993068	19.125453	-0.042203	1.190376
226.858026	270.339370	19.130458	-0.042181	1.181252
226.771981	262.705229	19.135463	-0.042160	1.172081
226.705976	255.071285	19.140467	-0.042143	1.162842
226.565665	247.443518	19.145472	-0.042112	1.153521
226.523031	239.793946	19.150477	-0.042099	1.144118
226.495070	232.162812	19.155482	-0.042089	1.134663
226.343203	224.561805	19.160487	-0.042055	1.125140
226.003778	217.021769	19.165491	-0.041987	1.115571
226.056323	209.387191	19.170496	-0.041992	1.105885
226.022987	201.813516	19.175501	-0.041981	1.096173
225.733018	194.256725	19.180506	-0.041922	1.086338
225.636335	186.708866	19.185511	-0.041899	1.076469
225.726285	179.109873	19.190515	-0.041911	1.066484
225.379420	171.603249	19.195520	-0.041841	1.056426
225.440751	164.033536	19.200525	-0.041848	1.046282
225.480718	156.504624	19.205530	-0.041850	1.036089
225.194334	149.023848	19.210535	-0.041792	1.025783
225.102492	141.533727	19.215539	-0.041770	1.015407
225.074817	134.022972	19.220544	-0.041760	1.004910
225.329329	126.499309	19.225549	-0.041802	0.994353
225.050314	119.038986	19.230554	-0.041745	0.983641
224.941695	111.596860	19.235559	-0.041720	0.972880
224.763133	104.178759	19.240563	-0.041682	0.962016
224.489521	96.791439	19.245568	-0.041626	0.951049
224.313603	89.400362	19.250573	-0.041589	0.939974
224.160012	82.015107	19.255578	-0.041555	0.928781
224.142463	74.635065	19.260583	-0.041547	0.917496
223.953818	67.283584	19.265587	-0.041507	0.906069
223.798583	60.180565	19.270592	-0.041473	0.894897