Fri Mar 12 13:19:07 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.414299	0.110342	0.000000	0.000040	0.721429

0.530124	0.094921	0.005005	0.000018	0.721439
0.684374	-0.022324	0.010010	-0.000011	0.721262
0.458349	-0.053262	0.015014	0.000032	0.721122
0.713113	-0.096919	0.020019	-0.000016	0.721126
0.523820	-0.062096	0.025024	0.000019	0.721128
0.317415	-0.026964	0.030029	0.000058	0.721125
0.677457	-0.087067	0.035034	-0.000009	0.721133
0.569976	-0.072368	0.040038	0.000011	0.721124
0.615484	-0.076540	0.045043	0.000002	0.721132
0.648669	-0.084112	0.050048	-0.000004	0.721129
0.751452	-0.103840	0.055053	-0.000023	0.721126
0.767591	-0.105084	0.060058	-0.000026	0.721129
0.648545	-0.087730	0.065062	-0.000004	0.721122
0.688348	-0.090926	0.070067	-0.000012	0.721130
0.578084	-0.071565	0.075072	0.000009	0.721129
0.566544	-0.191260	0.080077	0.000011	0.720890
0.745646	-0.224261	0.085082	-0.000022	0.720888
0.620173	-0.205444	0.090086	0.000001	0.720881
0.505814	-0.183846	0.095091	0.000022	0.720883
0.438348	-0.171947	0.100096	0.000035	0.720883
0.535770	-0.191474	0.105101	0.000017	0.720879
0.451022	-0.237378	0.110106	0.000032	0.720759
0.372337	-0.335142	0.115110	0.000047	0.720539
0.298974	-0.318704	0.120115	0.000061	0.720546
0.533009	-0.360616	0.125120	0.000017	0.720545
0.293316	-0.320742	0.130125	0.000062	0.720540
0.653912	-0.410049	0.135130	-0.000006	0.720491
0.458945	-0.511357	0.140134	0.000031	0.720223
0.595328	-0.531163	0.145139	0.000005	0.720232
0.451750	-0.506541	0.150144	0.000032	0.720230
0.480674	-0.515216	0.155149	0.000027	0.720223
0.379640	-0.645837	0.160154	0.000046	0.719930
0.325139	-0.652764	0.165158	0.000056	0.719898
0.444704	-0.672153	0.170163	0.000033	0.719901
0.453006	-0.689947	0.175168	0.000032	0.719869
0.079688	-0.761510	0.180173	0.000101	0.719597
0.167688	-0.773378	0.185178	0.000085	0.719605
0.432379	-0.822771	0.190182	0.000036	0.719601
0.462791	-0.925375	0.195187	0.000030	0.719409
0.428442	-0.986145	0.200192	0.000036	0.719277
0.522461	-1.007556	0.205197	0.000019	0.719268
0.364460	-1.048863	0.210202	0.000048	0.719131
0.422844	-1.146259	0.215206	0.000037	0.718960
0.268976	-1.115766	0.220211	0.000066	0.718966
0.311556	-1.206767	0.225216	0.000058	0.718801
0.176484	-1.263736	0.230221	0.000083	0.718641
0.237434	-1.269013	0.235226	0.000072	0.718652
0.153900	-1.363410	0.240230	0.000087	0.718437
0.258965	-1.423189	0.245235	0.000068	0.718356
0.366286	-1.456648	0.250240	0.000048	0.718328
0.111938	-1.569287	0.255245	0.000095	0.718016
0.171041	-1.575583	0.260250	0.000084	0.718024
0.183052	-1.667074	0.265254	0.000082	0.717848
0.044734	-1.711628	0.270259	0.000108	0.717711
0.075980	-1.735276	0.275264	0.000102	0.717675
-0.173393	-1.840602	0.280269	0.000148	0.717379
-0.106010	-1.846285	0.285274	0.000136	0.717392
-0.161658	-1.948376	0.290278	0.000146	0.717170
-0.041273	-2.013061	0.295283	0.000124	0.717085
-0.162346	-2.057772	0.300288	0.000146	0.716954
-0.428900	-2.110196	0.305293	0.000196	0.716756
-0.960202	-2.023283	0.310298	0.000295	0.716741
-2.115447	-1.965979	0.315302	0.000510	0.716447
-2.220906	-1.943997	0.320307	0.000529	0.716454
-2.672733	-1.880183	0.325312	0.000613	0.716421
-3.011987	-1.966504	0.330317	0.000677	0.716130
-2.741580	-2.009745	0.335322	0.000626	0.716140
-3.550891	-1.869554	0.340326	0.000777	0.716132
-3.793545	-1.936470	0.345331	0.000822	0.715914
-3.917724	-1.926477	0.350336	0.000845	0.715890
-4.205157	-1.881809	0.355341	0.000899	0.715877
-3.880243	-1.989032	0.360346	0.000838	0.715779
-4.913121	-1.922009	0.365350	0.001030	0.715548
-4.586124	-1.980651	0.370355	0.000969	0.715547
-4.988011	-1.906378	0.375360	0.001044	0.715552
-5.291506	-1.908913	0.380365	0.001101	0.715440
-5.747297	-1.927792	0.385370	0.001185	0.715242
-5.629463	-1.952085	0.390374	0.001164	0.715235
-6.244044	-1.841377	0.395379	0.001278	0.715238
-5.919119	-1.898471	0.400384	0.001217	0.715239
-6.546628	-1.933928	0.405389	0.001334	0.714947
-7.180812	-1.836087	0.410394	0.001452	0.714917
-7.140197	-1.846584	0.415398	0.001445	0.714911
-6.419727	-1.974736	0.420403	0.001310	0.714911
-7.142611	-1.843669	0.425408	0.001445	0.714916
-7.292078	-1.921404	0.430413	0.001473	0.714709
-7.660929	-1.903260	0.435418	0.001541	0.714615
-7.947758	-1.852668	0.440422	0.001595	0.714614
-7.989644	-1.844691	0.445427	0.001602	0.714615
-7.455092	-1.940432	0.450432	0.001503	0.714614
-7.738283	-1.926103	0.455437	0.001556	0.714542
-8.739065	-1.877693	0.460442	0.001742	0.714284
-8.673137	-1.891636	0.465446	0.001730	0.714280
-8.592676	-1.905260	0.470451	0.001715	0.714281
-8.698850	-1.884966	0.475456	0.001734	0.714284
-8.997208	-1.834991	0.480461	0.001790	0.714278
-8.743085	-1.908355	0.485466	0.001743	0.714222
-9.532849	-1.896375	0.490470	0.001890	0.713967
-9.437838	-1.908429	0.495475	0.001872	0.713976
-9.465815	-1.903442	0.500480	0.001877	0.713976
-9.504104	-1.901526	0.505485	0.001884	0.713967
-9.821100	-1.840687	0.510490	0.001943	0.713976
-9.826853	-1.842761	0.515494	0.001944	0.713969
-9.860777	-1.981060	0.520499	0.001950	0.713683
-10.652681	-1.853628	0.525504	0.002098	0.713656
-11.010214	-1.794282	0.530509	0.002164	0.713647
-10.109837	-1.949239	0.535514	0.001997	0.713658
-10.402341	-1.899752	0.540518	0.002051	0.713653
-10.924816	-1.806543	0.545523	0.002148	0.713653
-10.243404	-1.977681	0.550528	0.002021	0.713554
-11.348678	-1.880475	0.555533	0.002227	0.713356
-11.298177	-1.883309	0.560538	0.002218	0.713368
-11.442445	-1.861526	0.565542	0.002245	0.713361
-11.035060	-1.932812	0.570547	0.002169	0.713363
-10.975061	-1.943381	0.575552	0.002157	0.713364
-11.553928	-1.842713	0.580557	0.002265	0.713359
-11.645530	-1.988922	0.585562	0.002282	0.713035
-12.008966	-1.930753	0.590566	0.002350	0.713022
-12.556763	-1.830715	0.595571	0.002452	0.713027
-12.421381	-1.853539	0.600576	0.002427	0.713030
-12.113250	-1.913104	0.605581	0.002369	0.713021
-12.112065	-1.907429	0.610586	0.002369	0.713033
-12.160584	-1.948471	0.615590	0.002378	0.712934
-13.074765	-1.897015	0.620595	0.002548	0.712712
-12.716277	-1.959514	0.625600	0.002481	0.712715
-13.441802	-1.835452	0.630605	0.002616	0.712704
-13.050195	-1.900168	0.635610	0.002543	0.712715
-12.977662	-1.916068	0.640614	0.002530	0.712709
-13.428132	-1.834703	0.645619	0.002614	0.712711
-13.113390	-1.954675	0.650624	0.002555	0.712584
-13.892764	-1.916324	0.655629	0.002700	0.712384
-13.665780	-1.951436	0.660634	0.002658	0.712394
-14.077681	-1.882742	0.665638	0.002734	0.712385
-14.088933	-1.879754	0.670643	0.002737	0.712387
-13.665658	-1.952233	0.675648	0.002658	0.712393
-14.326312	-1.838862	0.680653	0.002781	0.712385
-14.167716	-1.958796	0.685658	0.002751	0.712202
-14.883584	-1.887915	0.690662	0.002884	0.712089
-15.199881	-1.831317	0.695667	0.002943	0.712090
-15.053347	-1.855623	0.700672	0.002916	0.712093
-15.263851	-1.820853	0.705677	0.002955	0.712088
-14.931447	-1.876829	0.710682	0.002893	0.712095
-15.132529	-1.843933	0.715686	0.002930	0.712089
-15.257042	-1.826365	0.720691	0.002954	0.712080
-15.603816	-1.922570	0.725696	0.003018	0.711765
-16.195738	-1.821476	0.730701	0.003128	0.711756
-16.174722	-1.818015	0.735706	0.003124	0.711771
-15.641026	-1.917261	0.740710	0.003025	0.711762
-16.080580	-1.837094	0.745715	0.003107	0.711766
-15.858347	-1.875947	0.750720	0.003065	0.711768
-15.876631	-1.877658	0.755725	0.003069	0.711758
-16.137382	-1.928303	0.760730	0.003117	0.711564
-17.199925	-1.794061	0.765734	0.003315	0.711454
-16.921828	-1.842361	0.770739	0.003263	0.711457
-16.600114	-1.897064	0.775744	0.003203	0.711462
-17.186741	-1.798514	0.780749	0.003312	0.711450
-16.948195	-1.836871	0.785754	0.003268	0.711459
-16.654341	-1.892009	0.790758	0.003213	0.711453
-16.831597	-1.897318	0.795763	0.003246	0.711380
-17.613879	-1.874764	0.800768	0.003392	0.711147
-17.499394	-1.901224	0.805773	0.003371	0.711135
-17.751319	-1.852965	0.810778	0.003417	0.711142
-17.806863	-1.844277	0.815782	0.003428	0.711139
-17.639478	-1.874414	0.820787	0.003396	0.711139
-17.483793	-1.897969	0.825792	0.003367	0.711147
-17.968678	-1.845508	0.830797	0.003458	0.711079
-18.253234	-1.896190	0.835802	0.003511	0.710877
-18.441229	-1.866518	0.840806	0.003546	0.710870
-18.685492	-1.822518	0.845811	0.003591	0.710871
-18.533899	-1.847496	0.850816	0.003563	0.710875
-18.504208	-1.857241	0.855821	0.003557	0.710866
-18.394694	-1.870693	0.860826	0.003537	0.710878
-18.825001	-1.842798	0.865830	0.003617	0.710781
-19.692018	-1.813006	0.870835	0.003778	0.710532
-18.957736	-1.942449	0.875840	0.003642	0.710535
-19.586462	-1.835054	0.880845	0.003759	0.710525
-19.468268	-1.850057	0.885850	0.003736	0.710538
-19.143408	-1.910056	0.890854	0.003676	0.710533
-19.258715	-1.889817	0.895859	0.003697	0.710533
-19.536307	-1.894072	0.900864	0.003749	0.710426
-20.463589	-1.834607	0.905869	0.003922	0.710214
-19.940629	-1.923036	0.910874	0.003824	0.710224
-20.401583	-1.845026	0.915878	0.003910	0.710216
-20.435445	-1.836294	0.920883	0.003916	0.710221
-19.931797	-1.925421	0.925888	0.003823	0.710223
-20.535109	-1.822198	0.930893	0.003935	0.710214
-20.478482	-1.890440	0.935898	0.003924	0.710098
-21.089963	-1.883062	0.940902	0.004038	0.709895
-21.150803	-1.875144	0.945907	0.004049	0.709889
-21.376453	-1.831141	0.950912	0.004091	0.709897
-21.380691	-1.833506	0.955917	0.004092	0.709891
-21.087734	-1.881495	0.960922	0.004037	0.709899
-21.526654	-1.806511	0.965926	0.004119	0.709893
-21.495773	-1.812168	0.970931	0.004113	0.709893
-21.309532	-1.983296	0.975936	0.004079	0.709617
-21.927702	-1.886666	0.980941	0.004194	0.709590
-22.155174	-1.841050	0.985946	0.004236	0.709600
-22.003732	-1.869871	0.990950	0.004208	0.709596
-22.188185	-1.838595	0.995955	0.004242	0.709593
-22.140663	-1.842926	1.000960	0.004233	0.709602
-22.255413	-1.839408	1.005965	0.004255	0.709568
-22.610628	-1.925050	1.010970	0.004321	0.709270
-22.814459	-1.889851	1.015974	0.004359	0.709268
-23.204428	-1.821517	1.020979	0.004431	0.709265
-22.564228	-1.932257	1.025984	0.004312	0.709272
-22.929462	-1.873247	1.030989	0.004380	0.709260
-23.029479	-1.851869	1.035994	0.004398	0.709267
-22.935913	-1.898261	1.040998	0.004381	0.709208
-23.898011	-1.851491	1.046003	0.004560	0.708958
-23.897211	-1.849720	1.051008	0.004560	0.708962
-24.320768	-1.778011	1.056013	0.004639	0.708955
-23.721286	-1.880445	1.061018	0.004527	0.708964
-23.762911	-1.876688	1.066022	0.004535	0.708956
-24.475929	-1.750972	1.071027	0.004667	0.708954
-23.772339	-1.872858	1.076032	0.004536	0.708961
-24.092219	-1.941513	1.081037	0.004596	0.708709
-25.213127	-1.774077	1.086042	0.004805	0.708645
-24.924863	-1.825763	1.091046	0.004751	0.708644
-24.630680	-1.880492	1.096051	0.004696	0.708640
-24.769017	-1.852365	1.101056	0.004722	0.708647
-25.232247	-1.774126	1.106061	0.004808	0.708638
-24.821127	-1.845877	1.111066	0.004732	0.708641
-24.627699	-1.941173	1.116070	0.004696	0.708519
-26.073166	-1.768738	1.121075	0.004965	0.708349
-25.427455	-1.881174	1.126080	0.004844	0.708354
-25.518272	-1.870555	1.131085	0.004861	0.708343
-25.819656	-1.813914	1.136090	0.004917	0.708349
-25.759937	-1.825178	1.141094	0.004906	0.708348
-25.823696	-1.815136	1.146099	0.004918	0.708345
-25.729024	-1.894868	1.151104	0.004900	0.708219
-27.122774	-1.752747	1.156109	0.005160	0.708006
-26.503299	-1.859070	1.161114	0.005044	0.708015
-26.474471	-1.865646	1.166118	0.005039	0.708012
-27.008244	-1.771517	1.171123	0.005138	0.708010
-26.673973	-1.828330	1.176128	0.005076	0.708015
-26.631034	-1.839562	1.181133	0.005068	0.708008
-26.686231	-1.827074	1.186138	0.005078	0.708014
-26.893922	-1.926247	1.191142	0.005117	0.707741
-27.621111	-1.819706	1.196147	0.005252	0.707695
-27.363817	-1.862645	1.201152	0.005204	0.707700
-27.580179	-1.827230	1.206157	0.005245	0.707694
-27.481659	-1.841363	1.211162	0.005226	0.707701
-27.083771	-1.913720	1.216166	0.005152	0.707698
-27.410317	-1.877849	1.221171	0.005213	0.707654
-28.037477	-1.901910	1.226176	0.005330	0.707381
-28.455802	-1.830610	1.231181	0.005407	0.707375
-28.563105	-1.809614	1.236186	0.005427	0.707379
-28.308529	-1.857283	1.241190	0.005380	0.707374
-28.461199	-1.832090	1.246195	0.005408	0.707370
-28.366543	-1.843630	1.251200	0.005391	0.707381
-28.708843	-1.787632	1.256205	0.005454	0.707371
-28.784461	-1.892447	1.261210	0.005468	0.707133
-29.208172	-1.844173	1.266214	0.005547	0.707079
-29.548714	-1.784052	1.271219	0.005611	0.707078
-29.316843	-1.819587	1.276224	0.005567	0.707089
-29.181873	-1.849086	1.281229	0.005542	0.707079
-29.149663	-1.850625	1.286234	0.005536	0.707087
-29.327230	-1.821382	1.291238	0.005569	0.707082
-29.645321	-1.893885	1.296243	0.005628	0.706823
-29.905901	-1.881165	1.301248	0.005677	0.706755
-30.410922	-1.793512	1.306253	0.005771	0.706751
-30.331530	-1.803930	1.311258	0.005756	0.706758
-30.196848	-1.830150	1.316262	0.005731	0.706754
-30.322256	-1.808492	1.321267	0.005754	0.706752
-30.190415	-1.829271	1.326272	0.005730	0.706758
-30.394666	-1.870569	1.331277	0.005768	0.706602
-31.158375	-1.810336	1.336282	0.005910	0.706450
-30.747505	-1.884661	1.341286	0.005833	0.706447
-30.946032	-1.851018	1.346291	0.005870	0.706444
-30.869086	-1.860691	1.351296	0.005856	0.706452
-30.947769	-1.852334	1.356301	0.005870	0.706441
-30.901356	-1.855711	1.361306	0.005862	0.706451
-31.035847	-1.964702	1.366310	0.005887	0.706184
-31.819834	-1.854414	1.371315	0.006033	0.706124
-31.806326	-1.852471	1.376320	0.006030	0.706133
-31.661683	-1.882795	1.381325	0.006003	0.706124
-31.680380	-1.874917	1.386330	0.006007	0.706133
-31.900276	-1.836337	1.391334	0.006048	0.706132
-32.018824	-1.839815	1.396339	0.006070	0.706083
-32.200948	-1.912844	1.401344	0.006103	0.705871
-32.350107	-1.891530	1.406349	0.006131	0.705860
-32.776379	-1.813054	1.411354	0.006210	0.705865
-32.520416	-1.858448	1.416358	0.006163	0.705866
-32.618638	-1.842178	1.421363	0.006181	0.705863
-32.508317	-1.858969	1.426368	0.006160	0.705869
-32.590917	-1.959832	1.431373	0.006176	0.705637
-33.711412	-1.815011	1.436378	0.006384	0.705526
-33.674694	-1.821748	1.441382	0.006378	0.705526
-33.709103	-1.816931	1.446387	0.006384	0.705524
-33.389953	-1.871417	1.451392	0.006324	0.705528
-33.775499	-1.806369	1.456397	0.006396	0.705521
-33.630068	-1.828103	1.461402	0.006369	0.705530
-33.387783	-1.947542	1.466406	0.006324	0.705376
-34.595521	-1.815098	1.471411	0.006549	0.705210
-34.115591	-1.896388	1.476416	0.006459	0.705218
-34.451456	-1.841434	1.481421	0.006522	0.705208
-34.448671	-1.838710	1.486426	0.006521	0.705215
-34.413515	-1.847456	1.491430	0.006515	0.705210
-34.626152	-1.811524	1.496435	0.006554	0.705206
-34.402698	-1.951136	1.501440	0.006513	0.705005
-35.266078	-1.856278	1.506445	0.006673	0.704886
-35.309133	-1.844608	1.511450	0.006681	0.704895
-35.245410	-1.858213	1.516454	0.006669	0.704890
-35.503336	-1.814321	1.521459	0.006717	0.704886
-35.475620	-1.815423	1.526464	0.006712	0.704894
-35.380772	-1.835159	1.531469	0.006695	0.704888
-35.533701	-1.888409	1.536474	0.006723	0.704726
-36.389516	-1.800216	1.541478	0.006882	0.704596
-36.294843	-1.821198	1.546483	0.006865	0.704588
-36.132925	-1.845181	1.551488	0.006834	0.704598
-36.353640	-1.808696	1.556493	0.006875	0.704592
-36.347810	-1.807718	1.561498	0.006874	0.704597
-35.816161	-1.905016	1.566502	0.006775	0.704592
-36.146032	-1.928776	1.571507	0.006837	0.704425
-37.379025	-1.786200	1.576512	0.007066	0.704270
-37.237029	-1.816159	1.581517	0.007040	0.704260
-37.036855	-1.850567	1.586522	0.007002	0.704263
-37.001608	-1.856190	1.591526	0.006996	0.704264
-37.201978	-1.823601	1.596531	0.007033	0.704258
-37.057430	-1.845652	1.601536	0.007006	0.704266
-37.015836	-1.901960	1.606541	0.006998	0.704167
-38.122790	-1.809413	1.611546	0.007204	0.703956
-37.796828	-1.867100	1.616550	0.007144	0.703957
-37.964108	-1.840756	1.621555	0.007175	0.703950
-38.008881	-1.826618	1.626560	0.007183	0.703962
-38.011228	-1.833511	1.631565	0.007184	0.703948
-37.829988	-1.861294	1.636570	0.007150	0.703957
-37.927636	-1.903433	1.641574	0.007168	0.703837
-39.244998	-1.768869	1.646579	0.007413	0.703635
-38.444067	-1.907024	1.651584	0.007264	0.703644
-38.818953	-1.844824	1.656589	0.007334	0.703635
-39.121726	-1.787861	1.661594	0.007390	0.703641
-38.622809	-1.877546	1.666598	0.007297	0.703639
-38.675525	-1.870388	1.671603	0.007307	0.703635
-38.862577	-1.903288	1.676608	0.007342	0.703501
-40.029159	-1.774945	1.681613	0.007559	0.703341
-39.372833	-1.887980	1.686618	0.007437	0.703349
-39.373728	-1.889248	1.691622	0.007437	0.703346
-39.678945	-1.836760	1.696627	0.007494	0.703342
-39.325906	-1.895759	1.701632	0.007428	0.703350
-39.415744	-1.884147	1.706637	0.007445	0.703341
-40.182257	-1.885552	1.711642	0.007587	0.703063
-40.841367	-1.793885	1.716646	0.007710	0.703011
-40.679840	-1.823919	1.721651	0.007680	0.703008
-40.350770	-1.878996	1.726656	0.007618	0.703015
-40.784908	-1.807924	1.731661	0.007699	0.703003
-40.777622	-1.806980	1.736666	0.007698	0.703007
-40.400574	-1.873586	1.741670	0.007628	0.703009
-40.825485	-1.878268	1.746675	0.007707	0.702846
-41.634189	-1.804881	1.751680	0.007857	0.702703
-41.270382	-1.875270	1.756685	0.007790	0.702692
-41.576515	-1.816396	1.761690	0.007846	0.702701
-41.744896	-1.788958	1.766694	0.007878	0.702696
-41.384813	-1.855284	1.771699	0.007811	0.702692
-41.320951	-1.862690	1.776704	0.007799	0.702700
-41.963731	-1.800681	1.781709	0.007918	0.702593
-42.442001	-1.825023	1.786714	0.008007	0.702372
-41.880098	-1.924440	1.791718	0.007903	0.702374
-42.771407	-1.769294	1.796723	0.008069	0.702366
-42.591946	-1.796079	1.801728	0.008035	0.702377
-42.245212	-1.863847	1.806733	0.007971	0.702365
-42.636596	-1.789773	1.811738	0.008043	0.702373
-42.547418	-1.805362	1.816742	0.008027	0.702374
-43.027985	-1.867618	1.821747	0.008116	0.702075
-43.149469	-1.844294	1.826752	0.008139	0.702078
-43.423442	-1.800186	1.831757	0.008190	0.702069
-43.439132	-1.793450	1.836762	0.008193	0.702077
-43.012529	-1.869631	1.841766	0.008113	0.702077
-43.453132	-1.792994	1.846771	0.008195	0.702073
-43.101372	-1.852318	1.851776	0.008130	0.702080
-43.563833	-1.931314	1.856781	0.008216	0.701753
-44.016809	-1.853548	1.861786	0.008300	0.701747
-44.063394	-1.843889	1.866790	0.008309	0.701750
-43.895322	-1.879179	1.871795	0.008277	0.701739
-43.991297	-1.857434	1.876800	0.008295	0.701749
-44.481125	-1.775449	1.881805	0.008386	0.701738
-44.195776	-1.854098	1.886810	0.008333	0.701682
-44.421453	-1.933237	1.891814	0.008375	0.701440
-44.853807	-1.858336	1.896819	0.008456	0.701436
-45.065674	-1.816891	1.901824	0.008495	0.701444
-44.917097	-1.848394	1.906829	0.008467	0.701434
-44.785256	-1.870244	1.911834	0.008443	0.701437
-45.217579	-1.792109	1.916838	0.008523	0.701439
-45.257479	-1.842470	1.921843	0.008531	0.701323
-45.642570	-1.870034	1.926848	0.008602	0.701128
-45.691125	-1.865188	1.931853	0.008611	0.701120
-45.859164	-1.832600	1.936858	0.008643	0.701126
-45.669679	-1.863883	1.941862	0.008607	0.701131
-45.883037	-1.830535	1.946867	0.008647	0.701121
-45.898383	-1.822902	1.951872	0.008650	0.701131
-45.788756	-1.910881	1.956877	0.008629	0.700993
-46.646849	-1.813489	1.961882	0.008789	0.700880
-46.373480	-1.860848	1.966886	0.008738	0.700883
-46.407414	-1.860572	1.971891	0.008744	0.700872
-46.258746	-1.882651	1.976896	0.008717	0.700881
-46.592540	-1.828056	1.981901	0.008779	0.700871
-46.773148	-1.802742	1.986906	0.008812	0.700857
-46.774279	-1.958622	1.991910	0.008813	0.700541
-47.125934	-1.898180	1.996915	0.008878	0.700536
-47.506224	-1.829078	2.001920	0.008949	0.700539

-47.404307	-1.847325	2.011917	0.008930	0.700539
-47.508266	-1.829436	2.021914	0.008949	0.700538
-47.674640	-1.879822	2.031910	0.008980	0.700375
-48.440965	-1.819536	2.041907	0.009122	0.700221
-47.840244	-1.850318	2.051904	0.009011	0.700376
-47.872007	-1.862108	2.061901	0.009016	0.700340
-47.563722	-1.869403	2.071898	0.008959	0.700437
-47.840065	-1.774439	2.081894	0.009010	0.700530
-47.056526	-1.910577	2.091891	0.008864	0.700537
-47.348342	-1.857762	2.101888	0.008919	0.700539
-47.171069	-1.890257	2.111885	0.008886	0.700537
-47.233906	-1.879162	2.121882	0.008897	0.700537
-47.229830	-1.881426	2.131878	0.008896	0.700534
-47.288033	-1.871157	2.141875	0.008907	0.700534
-47.430532	-1.842541	2.151872	0.008934	0.700541
-46.545189	-1.833681	2.161869	0.008769	0.700879
-46.378428	-1.864764	2.171866	0.008737	0.700876
-46.540014	-1.836870	2.181862	0.008767	0.700875
-46.395465	-1.861947	2.191859	0.008741	0.700876
-46.498151	-1.784344	2.201856	0.008759	0.700997
-45.686648	-1.866239	2.211853	0.008608	0.701124
-46.093233	-1.793422	2.221850	0.008684	0.701125
-45.901454	-1.827886	2.231846	0.008648	0.701124
-45.262941	-1.796517	2.241843	0.008529	0.701419
-45.268444	-1.786266	2.251840	0.008530	0.701438
-44.704795	-1.886500	2.261837	0.008425	0.701438
-44.901549	-1.784235	2.271834	0.008462	0.701574
-44.140902	-1.834873	2.281830	0.008320	0.701747
-44.175012	-1.829018	2.291827	0.008326	0.701746
-44.372657	-1.793538	2.301824	0.008363	0.701747
-43.316169	-1.819094	2.311821	0.008166	0.702076
-43.286388	-1.824632	2.321818	0.008161	0.702076
-43.127073	-1.852957	2.331814	0.008131	0.702076
-43.205296	-1.785175	2.341811	0.008145	0.702185
-42.197122	-1.872174	2.351808	0.007958	0.702373
-42.342884	-1.846023	2.361805	0.007985	0.702374
-42.564415	-1.807175	2.371802	0.008026	0.702372
-41.637489	-1.835574	2.381798	0.007853	0.702649
-41.515516	-1.835622	2.391795	0.007830	0.702693
-41.677941	-1.805921	2.401792	0.007860	0.702695
-41.363475	-1.793679	2.411789	0.007802	0.702833
-40.721401	-1.820296	2.421786	0.007682	0.703011
-40.383515	-1.881464	2.431782	0.007619	0.703009
-40.726071	-1.820962	2.441779	0.007683	0.703008
-39.830706	-1.847313	2.451776	0.007516	0.703277
-39.712415	-1.836114	2.461773	0.007494	0.703343
-39.680591	-1.840738	2.471770	0.007488	0.703345
-39.476714	-1.866282	2.481766	0.007450	0.703367
-39.269042	-1.770528	2.491763	0.007411	0.703635
-38.828947	-1.848368	2.501760	0.007329	0.703636
-39.004809	-1.817125	2.511757	0.007362	0.703636
-38.324810	-1.808202	2.521754	0.007235	0.703899
-38.062111	-1.828104	2.531750	0.007186	0.703953
-37.930444	-1.851961	2.541747	0.007162	0.703953
-37.835303	-1.825440	2.551744	0.007144	0.704041
-37.038680	-1.856960	2.561741	0.006995	0.704264
-37.193278	-1.831098	2.571738	0.007024	0.704260
-37.165302	-1.836157	2.581734	0.007019	0.704260
-36.468008	-1.824723	2.591731	0.006889	0.704534
-36.121918	-1.857952	2.601728	0.006824	0.704592
-36.399090	-1.807214	2.611725	0.006876	0.704594
-36.228802	-1.794592	2.621722	0.006844	0.704681
-35.448980	-1.829872	2.631718	0.006699	0.704890
-35.287146	-1.860270	2.641715	0.006669	0.704887
-35.395301	-1.838772	2.651712	0.006689	0.704892
-34.715522	-1.822374	2.661709	0.006562	0.705169
-34.520193	-1.835956	2.671706	0.006526	0.705212
-34.307046	-1.872901	2.681702	0.006486	0.705214
-34.613555	-1.772210	2.691699	0.006543	0.705307
-33.409009	-1.878015	2.701696	0.006319	0.705527
-33.691975	-1.826207	2.711693	0.006371	0.705529
-33.576366	-1.848636	2.721690	0.006350	0.705526
-33.032938	-1.806670	2.731686	0.006248	0.705805
-32.698298	-1.838071	2.741683	0.006186	0.705862
-32.689732	-1.837960	2.751680	0.006184	0.705866
-32.744021	-1.785181	2.761677	0.006194	0.705953
-32.080319	-1.815375	2.771674	0.006071	0.706130
-32.055068	-1.821504	2.781670	0.006066	0.706127
-32.066245	-1.812003	2.791667	0.006068	0.706142
-31.068278	-1.839964	2.801664	0.005882	0.706444
-31.259854	-1.806275	2.811661	0.005918	0.706443
-31.006533	-1.848937	2.821658	0.005870	0.706448
-30.948877	-1.757027	2.831654	0.005859	0.706653
-30.272157	-1.829561	2.841651	0.005733	0.706750
-30.262011	-1.830314	2.851648	0.005731	0.706752
-30.244246	-1.774173	2.861645	0.005728	0.706872
-29.251688	-1.845964	2.871642	0.005543	0.707083
-29.543917	-1.794958	2.881638	0.005597	0.707081
-29.554290	-1.793026	2.891635	0.005599	0.707081
-28.728229	-1.795344	2.901632	0.005445	0.707372
-28.645904	-1.806001	2.911629	0.005430	0.707380
-28.601044	-1.813796	2.921626	0.005422	0.707381
-28.372667	-1.756070	2.931622	0.005379	0.707579
-27.818464	-1.794654	2.941619	0.005276	0.707700
-27.637531	-1.826508	2.951616	0.005242	0.707700
-27.628308	-1.794675	2.961613	0.005240	0.707768
-26.750418	-1.826386	2.971610	0.005077	0.708018
-26.925061	-1.798371	2.981606	0.005109	0.708012
-26.909724	-1.799384	2.991603	0.005106	0.708016
-26.332293	-1.771177	3.001600	0.004999	0.708279
-25.949966	-1.800082	3.011597	0.004927	0.708357
-25.813519	-1.826267	3.021594	0.004902	0.708354
-26.021855	-1.761438	3.031590	0.004941	0.708409
-25.013727	-1.825756	3.041587	0.004753	0.708641
-25.143920	-1.801571	3.051584	0.004777	0.708643
-25.070412	-1.813379	3.061581	0.004763	0.708645
-24.402437	-1.810043	3.071578	0.004639	0.708891
-24.213246	-1.809445	3.081574	0.004603	0.708960
-24.305256	-1.794406	3.091571	0.004620	0.708957
-24.056541	-1.798909	3.101568	0.004574	0.709037
-23.101531	-1.853489	3.111565	0.004396	0.709268
-23.118002	-1.850821	3.121562	0.004399	0.709268
-23.356098	-1.809397	3.131558	0.004443	0.709266
-22.934712	-1.797859	3.141555	0.004365	0.709440
-22.469110	-1.800038	3.151552	0.004278	0.709601
-22.554393	-1.783661	3.161549	0.004294	0.709604
-22.352102	-1.803062	3.171546	0.004256	0.709637
-21.861689	-1.761757	3.181542	0.004165	0.709895
-21.422729	-1.840683	3.191539	0.004083	0.709894
-21.675838	-1.793849	3.201536	0.004130	0.709897
-20.967635	-1.799362	3.211533	0.003998	0.710139
-20.924069	-1.765511	3.221530	0.003990	0.710222
-20.607827	-1.822331	3.231526	0.003931	0.710221
-20.484804	-1.805686	3.241523	0.003908	0.710298
-19.843596	-1.800123	3.251520	0.003789	0.710538
-19.726298	-1.821020	3.261517	0.003767	0.710538
-19.710170	-1.824944	3.271514	0.003764	0.710536
-19.342287	-1.775875	3.281510	0.003695	0.710765
-18.911992	-1.797904	3.291507	0.003615	0.710874
-18.877200	-1.803629	3.301504	0.003608	0.710875
-18.570994	-1.855840	3.311501	0.003551	0.710880
-18.585994	-1.721955	3.321498	0.003554	0.711142
-18.047156	-1.817695	3.331494	0.003453	0.711143
-18.196151	-1.792548	3.341491	0.003481	0.711140
-17.590330	-1.773903	3.351488	0.003368	0.711393
-17.332955	-1.785831	3.361485	0.003320	0.711461
-17.262038	-1.798736	3.371482	0.003307	0.711461
-17.021906	-1.782510	3.381478	0.003262	0.711578
-16.367057	-1.806620	3.391475	0.003140	0.711763
-16.465398	-1.788228	3.401472	0.003158	0.711765
-16.260128	-1.823858	3.411469	0.003120	0.711767
-15.787155	-1.753930	3.421466	0.003032	0.712075
-15.261973	-1.838328	3.431462	0.002934	0.712093
-15.424415	-1.808788	3.441459	0.002964	0.712094
-15.386642	-1.760919	3.451456	0.002957	0.712203
-14.677338	-1.793190	3.461453	0.002825	0.712391
-14.668952	-1.795737	3.471450	0.002823	0.712389
-14.745128	-1.777685	3.481446	0.002837	0.712398
-13.931404	-1.764008	3.491443	0.002686	0.712714
-13.753378	-1.796350	3.501440	0.002653	0.712713
-13.575552	-1.825280	3.511437	0.002619	0.712719
-13.551064	-1.740286	3.521434	0.002615	0.712897
-12.791081	-1.809447	3.531430	0.002473	0.713029
-13.016606	-1.768865	3.541427	0.002515	0.713030
-12.687140	-1.819590	3.551424	0.002454	0.713046
-12.023451	-1.776114	3.561421	0.002330	0.713368
-11.983324	-1.784868	3.571418	0.002323	0.713365
-11.935037	-1.792836	3.581414	0.002313	0.713366
-11.789290	-1.744335	3.591411	0.002286	0.713514
-11.008322	-1.809346	3.601408	0.002141	0.713662
-11.208152	-1.774837	3.611405	0.002178	0.713660
-11.062224	-1.798983	3.621402	0.002151	0.713664
-10.225983	-1.792823	3.631398	0.001995	0.713972
-10.284665	-1.781615	3.641395	0.002006	0.713974
-9.957745	-1.838280	3.651392	0.001945	0.713977
-9.975936	-1.776826	3.661389	0.001948	0.714093
-9.240397	-1.811486	3.671386	0.001811	0.714284
-9.093541	-1.838312	3.681382	0.001784	0.714283
-8.956351	-1.863140	3.691379	0.001758	0.714283
-8.580318	-1.851234	3.701376	0.001688	0.714439
-7.948835	-1.876435	3.711373	0.001570	0.714613
-8.193976	-1.832007	3.721370	0.001616	0.714615
-8.038911	-1.861122	3.731366	0.001587	0.714612
-7.974791	-1.783766	3.741363	0.001575	0.714788
-7.049215	-1.885886	3.751360	0.001402	0.714913
-7.310051	-1.837836	3.761357	0.001451	0.714916
-7.040268	-1.887073	3.771354	0.001401	0.714914
-6.533946	-1.832476	3.781350	0.001306	0.715201
-6.436766	-1.833669	3.791347	0.001288	0.715234
-5.961345	-1.916702	3.801344	0.001200	0.715237
-6.403080	-1.811328	3.811341	0.001282	0.715290
-5.197070	-1.895090	3.821338	0.001057	0.715550
-5.391173	-1.862122	3.831334	0.001093	0.715547
-5.557654	-1.832615	3.841331	0.001124	0.715547
-5.121406	-1.830613	3.851328	0.001043	0.715705
-4.309375	-1.883270	3.861325	0.000891	0.715888
-4.217722	-1.899708	3.871322	0.000874	0.715888
-4.486387	-1.852157	3.881318	0.000924	0.715887
-3.870436	-1.889028	3.891315	0.000810	0.716032
-3.356881	-1.927999	3.901312	0.000714	0.716136
-3.822319	-1.845003	3.911309	0.000800	0.716136
-3.454992	-1.910272	3.921306	0.000732	0.716137
-3.014357	-1.829182	3.931302	0.000650	0.716453
-2.554317	-1.912583	3.941299	0.000564	0.716450
-2.415837	-1.936376	3.951296	0.000538	0.716452
-2.428368	-1.883376	3.961293	0.000540	0.716552
-1.759833	-1.898186	3.971290	0.000416	0.716759
-2.146574	-1.829961	3.981286	0.000488	0.716758
-1.790293	-1.893378	3.991283	0.000421	0.716758
-1.451189	-1.790381	4.001280	0.000358	0.717082
-1.399500	-1.796499	4.011277	0.000348	0.717088
-0.830524	-1.897169	4.021274	0.000243	0.717089
-1.255750	-1.708258	4.031270	0.000322	0.717313
-0.821203	-1.750322	4.041267	0.000241	0.717383
-0.996585	-1.700105	4.051264	0.000273	0.717421
-0.746119	-1.596821	4.061261	0.000226	0.717713
-0.738681	-1.600353	4.071258	0.000225	0.717709
-0.649322	-1.492046	4.081254	0.000208	0.717955
-0.684554	-1.452022	4.091251	0.000215	0.718022
-0.536294	-1.357079	4.101248	0.000187	0.718262
-0.605399	-1.295218	4.111245	0.000200	0.718360
-0.583470	-1.174114	4.121242	0.000195	0.718607
-0.522987	-1.136221	4.131238	0.000184	0.718703
-0.476340	-1.012488	4.141235	0.000175	0.718963
-0.267112	-0.955263	4.151232	0.000136	0.719150
-0.212125	-0.890199	4.161229	0.000126	0.719298
-0.252601	-0.726538	4.171226	0.000133	0.719606
-0.215394	-0.634309	4.181222	0.000126	0.719801
-0.249805	-0.526243	4.191219	0.000132	0.720002
-0.072335	-0.439416	4.201216	0.000099	0.720236
0.028559	-0.300806	4.211213	0.000080	0.720544
-0.187986	-0.130021	4.221210	0.000120	0.720805
-0.042402	-0.039646	4.231206	0.000093	0.721034
-0.043914	0.085424	4.241203	0.000093	0.721279
0.000000	0.241111	4.251200	0.000085	0.721601

0.166195	0.839149	4.256205	0.000053	0.722834
0.187482	2.109639	4.261210	0.000049	0.725330
0.413508	3.927013	4.266214	0.000005	0.728954
0.785268	6.270080	4.271219	-0.000066	0.733627
0.998845	9.158961	4.276224	-0.000107	0.739265
1.263207	12.505730	4.281229	-0.000159	0.745748
1.759387	16.278323	4.286234	-0.000254	0.753056
1.947187	20.506538	4.291238	-0.000291	0.761041
2.052382	25.138279	4.296243	-0.000314	0.769659
2.679730	30.055586	4.301248	-0.000434	0.778872
3.063633	35.353654	4.306253	-0.000509	0.788583
3.601044	40.951359	4.311258	-0.000613	0.798757
4.229664	46.833582	4.316262	-0.000734	0.809330
4.876387	52.997574	4.321267	-0.000858	0.820259
5.291240	59.483706	4.326272	-0.000940	0.831524
5.933867	66.143381	4.331277	-0.001064	0.842998
6.799067	73.002790	4.336282	-0.001229	0.854713
7.443118	80.098515	4.341286	-0.001354	0.866593
9.350911	87.178650	4.346291	-0.001714	0.878646
10.043166	94.657175	4.351296	-0.001848	0.890829
10.423846	102.350839	4.356301	-0.001923	0.903098
10.922406	110.172110	4.361306	-0.002021	0.915433
11.820697	118.021808	4.366310	-0.002194	0.927754
12.734369	125.998786	4.371315	-0.002369	0.940109
13.595859	134.102338	4.376320	-0.002535	0.952478
13.909545	142.371542	4.381325	-0.002599	0.964791
14.714875	150.652278	4.386330	-0.002754	0.977090
15.480325	159.019088	4.391334	-0.002902	0.989348
16.134895	167.452672	4.396339	-0.003030	1.001524
16.912947	175.910931	4.401344	-0.003180	1.013617
17.487261	184.431868	4.406349	-0.003293	1.025605
18.313028	192.961535	4.411354	-0.003452	1.037526
19.103463	201.513157	4.416358	-0.003605	1.049332
19.581525	210.134915	4.421363	-0.003699	1.061028
20.119463	218.787580	4.426368	-0.003805	1.072651
20.521344	227.436340	4.431373	-0.003886	1.084112
21.330760	236.051277	4.436378	-0.004042	1.095501
21.860088	244.702181	4.441382	-0.004146	1.106757
22.329034	253.365908	4.446387	-0.004239	1.117902
22.980126	262.004395	4.451392	-0.004366	1.128944
23.294415	270.691155	4.456397	-0.004430	1.139867
23.714922	279.378335	4.461402	-0.004514	1.150709
24.286241	288.005747	4.466406	-0.004626	1.161409
25.227655	296.552921	4.471411	-0.004807	1.171990
25.735017	305.171824	4.476416	-0.004908	1.182472
26.205414	313.781899	4.481421	-0.005001	1.192845
27.128635	322.305354	4.486426	-0.005178	1.203116
27.703050	330.891112	4.491430	-0.005291	1.213304
28.056508	339.491659	4.496435	-0.005362	1.223380
28.626560	348.071982	4.501440	-0.005474	1.233393
29.351768	356.570007	4.506445	-0.005615	1.243261
29.956330	365.107081	4.511450	-0.005733	1.253072
30.324361	373.653475	4.516454	-0.005807	1.262772
30.899299	382.157932	4.521459	-0.005920	1.272390
31.566158	390.628477	4.526464	-0.006049	1.281915
31.672493	399.176819	4.531469	-0.006075	1.291351
32.099179	407.653890	4.536474	-0.006160	1.300700
32.631818	416.157930	4.541478	-0.006265	1.310031
33.039809	424.682484	4.546483	-0.006346	1.319295
33.758050	433.046293	4.551488	-0.006485	1.328378
34.118747	441.469587	4.556493	-0.006558	1.337398
34.613024	449.858807	4.561498	-0.006656	1.346346
34.855903	458.303845	4.566502	-0.006706	1.355249
35.371630	466.652164	4.571507	-0.006808	1.364040
35.981437	475.025970	4.576512	-0.006927	1.372818
36.319289	483.391118	4.581517	-0.006995	1.381484
36.530734	491.812794	4.586522	-0.007040	1.390132
37.203249	500.133365	4.591526	-0.007171	1.398701
37.407666	508.491361	4.596531	-0.007214	1.407178
37.630174	516.874241	4.601536	-0.007261	1.415632
38.074721	525.170722	4.606541	-0.007350	1.423986
38.622266	533.493331	4.611546	-0.007457	1.432334
39.040283	541.788153	4.616550	-0.007540	1.440584
39.472107	550.090139	4.621555	-0.007626	1.448797
40.294035	558.355695	4.626560	-0.007785	1.456991
40.800196	566.634648	4.631565	-0.007884	1.465101
41.126530	575.008561	4.636570	-0.007950	1.473229
41.454164	583.309415	4.641574	-0.008017	1.481243
41.757615	591.587504	4.646579	-0.008079	1.489188
42.186061	599.879786	4.651584	-0.008164	1.497123
42.645037	608.119025	4.656589	-0.008255	1.504971
43.101531	616.403170	4.661594	-0.008345	1.512820
43.275647	624.685169	4.666598	-0.008383	1.520584
43.790013	632.912184	4.671603	-0.008484	1.528308
44.268128	641.171679	4.676608	-0.008579	1.536018
44.738811	649.392219	4.681613	-0.008672	1.543652
45.201152	657.645875	4.686618	-0.008763	1.551278
45.688394	665.879203	4.691622	-0.008860	1.558851
46.115887	674.087112	4.696627	-0.008945	1.566356
46.557139	682.341579	4.701632	-0.009032	1.573868
47.098506	690.529327	4.706637	-0.009138	1.581300
47.589327	698.757773	4.711642	-0.009235	1.588725
47.828122	707.022443	4.716646	-0.009285	1.596112
48.354911	715.206859	4.721651	-0.009388	1.603435
48.953767	723.410331	4.726656	-0.009505	1.610751
49.452256	731.617108	4.731661	-0.009604	1.618023
49.750458	739.849064	4.736666	-0.009664	1.625256
50.419873	748.070258	4.741670	-0.009794	1.632499
50.774926	756.280839	4.746675	-0.009866	1.639657
50.930225	764.508603	4.751680	-0.009900	1.646772
51.367839	772.697325	4.756685	-0.009987	1.653861
51.831051	780.866936	4.761690	-0.010079	1.660906
52.256548	789.043774	4.766694	-0.010163	1.667923
52.752543	797.234951	4.771699	-0.010261	1.674932
53.526858	805.368540	4.776704	-0.010411	1.681900
53.962008	813.539032	4.781709	-0.010497	1.688825
54.425525	821.739266	4.786714	-0.010589	1.695750
55.110373	829.884951	4.791718	-0.010722	1.702630
55.461622	838.091501	4.796723	-0.010792	1.709489
55.667926	846.326437	4.801728	-0.010836	1.716326
56.016346	854.492545	4.806733	-0.010906	1.723097
56.614847	862.634545	4.811738	-0.011023	1.729854
56.853092	870.837402	4.816742	-0.011073	1.736588
57.433599	878.954974	4.821747	-0.011186	1.743270
58.059147	887.102472	4.826752	-0.011308	1.749956
58.457995	895.277917	4.831757	-0.011388	1.756610
58.812053	903.448062	4.836762	-0.011459	1.763230
59.478069	911.570828	4.841766	-0.011588	1.769825
59.624731	919.772929	4.846771	-0.011621	1.776395
60.111371	927.925403	4.851776	-0.011717	1.782943
60.388634	936.104377	4.856781	-0.011774	1.789462
60.636513	944.328726	4.861786	-0.011826	1.795989
61.050516	952.445490	4.866790	-0.011908	1.802429
61.279800	960.590572	4.871795	-0.011956	1.808845
61.814434	968.723059	4.876800	-0.012061	1.815265
62.162541	976.856627	4.881805	-0.012131	1.821641
62.462678	985.007501	4.886810	-0.012192	1.828003
62.947211	993.147383	4.891814	-0.012288	1.834356
63.388844	1001.242617	4.896819	-0.012375	1.840647
63.960288	1009.362551	4.901824	-0.012487	1.846950
64.502499	1017.499740	4.906829	-0.012593	1.853242
64.986977	1025.629059	4.911834	-0.012689	1.859500
65.143662	1033.799536	4.916838	-0.012724	1.865730
65.619480	1041.940510	4.921843	-0.012818	1.871953
66.053836	1050.086374	4.926848	-0.012904	1.878155
66.116754	1058.237008	4.931853	-0.012921	1.884297
66.394812	1066.367426	4.936858	-0.012978	1.890429
67.023914	1074.477255	4.941862	-0.013100	1.896565
67.420074	1082.585298	4.946867	-0.013179	1.902654
67.653767	1090.748724	4.951872	-0.013228	1.908746
68.103004	1098.864473	4.956877	-0.013317	1.914807
68.396987	1106.980899	4.961882	-0.013377	1.920832
68.918056	1115.080748	4.966886	-0.013480	1.926851
69.103612	1123.236088	4.971891	-0.013520	1.932855
69.921263	1131.306863	4.976896	-0.013677	1.938848
70.331685	1139.398730	4.981901	-0.013759	1.944793
70.500457	1147.585134	4.986906	-0.013796	1.950762
70.628042	1155.768871	4.991910	-0.013825	1.956707
70.936681	1163.829558	4.996915	-0.013888	1.962564
71.345700	1171.929330	5.001920	-0.013969	1.968442
71.622015	1180.048904	5.006925	-0.014026	1.974303
72.163126	1188.116907	5.011930	-0.014132	1.980138
72.617045	1196.210345	5.016934	-0.014222	1.985965
72.905674	1204.336945	5.021939	-0.014281	1.991780
73.447395	1212.440269	5.026944	-0.014387	1.997589
73.852442	1220.516576	5.031949	-0.014468	2.003347
74.235211	1228.627306	5.036954	-0.014544	2.009110
74.759322	1236.733861	5.041958	-0.014647	2.014868
75.154624	1244.821152	5.046963	-0.014726	2.020584
75.281436	1252.986273	5.051968	-0.014755	2.026309
75.516003	1261.132068	5.056973	-0.014804	2.032016
75.984342	1269.209273	5.061978	-0.014897	2.037683
76.529405	1277.261582	5.066982	-0.015003	2.043325
76.637047	1285.383183	5.071987	-0.015029	2.048955
76.861659	1293.519598	5.076992	-0.015076	2.054591
77.410218	1301.562976	5.081997	-0.015183	2.060181
77.824867	1309.654151	5.087002	-0.015266	2.065774
78.191979	1317.767920	5.092006	-0.015340	2.071363
78.338017	1325.900184	5.097011	-0.015372	2.076928
79.130433	1333.931572	5.102016	-0.015525	2.082473
79.694394	1342.000032	5.107021	-0.015635	2.088006
80.113983	1350.122628	5.112026	-0.015719	2.093546
80.478578	1358.234781	5.117030	-0.015792	2.099059
80.844296	1366.307126	5.122035	-0.015865	2.104531
81.186110	1374.453571	5.127040	-0.015934	2.110036
81.385656	1382.608988	5.132045	-0.015977	2.115519
81.573577	1390.689165	5.137050	-0.016017	2.120936
82.061646	1398.743416	5.142054	-0.016113	2.126351
82.522963	1406.802214	5.147059	-0.016204	2.131753
82.981580	1414.891164	5.152064	-0.016295	2.137160
83.338759	1422.950057	5.157069	-0.016367	2.142524
83.751156	1431.037159	5.162074	-0.016449	2.147899
84.146419	1439.154420	5.167078	-0.016528	2.153278
84.323446	1447.238945	5.172083	-0.016566	2.158602
84.492878	1455.348957	5.177088	-0.016603	2.163929
84.710969	1463.426702	5.182093	-0.016649	2.169225
85.108762	1471.532145	5.187098	-0.016728	2.174544
85.166016	1479.645049	5.192102	-0.016744	2.179823
85.340417	1487.714785	5.197107	-0.016782	2.185072
86.145585	1495.753364	5.202112	-0.016937	2.190346
86.657315	1503.838181	5.207117	-0.017038	2.195610
87.256197	1511.867605	5.212122	-0.017155	2.200834
87.788887	1519.933438	5.217126	-0.017259	2.206063
87.901172	1528.049742	5.222131	-0.017285	2.211273
88.283784	1536.151168	5.227136	-0.017362	2.216486
88.695543	1544.197773	5.232141	-0.017444	2.221654
88.722181	1552.326545	5.237146	-0.017454	2.226828
89.071791	1560.423839	5.242150	-0.017525	2.231999
89.316304	1568.497625	5.247155	-0.017575	2.237134
89.793796	1576.545729	5.252160	-0.017670	2.242261
89.786038	1584.670139	5.257165	-0.017674	2.247382
89.978424	1592.752902	5.262170	-0.017715	2.252482
90.618090	1600.788177	5.267174	-0.017839	2.257580
90.731937	1608.875440	5.272179	-0.017866	2.262653
91.344428	1616.940794	5.277184	-0.017985	2.267745
91.432782	1625.101588	5.282189	-0.018007	2.272839
91.693891	1633.179220	5.287194	-0.018061	2.277885
91.743041	1641.246060	5.292198	-0.018075	2.282894
92.016701	1649.278243	5.297203	-0.018131	2.287891
92.533074	1657.349900	5.302208	-0.018233	2.292921
92.837468	1665.403406	5.307213	-0.018295	2.297911
92.976199	1673.473260	5.312218	-0.018326	2.302887
93.404747	1681.530600	5.317222	-0.018411	2.307868
93.494483	1689.635473	5.322227	-0.018433	2.312839
93.918745	1697.693441	5.327232	-0.018517	2.317799
94.263624	1705.735223	5.332237	-0.018587	2.322732
94.346861	1713.821811	5.337242	-0.018608	2.327659
94.737511	1721.909476	5.342246	-0.018686	2.332603
94.897577	1729.954120	5.347251	-0.018721	2.337490
95.616158	1737.974773	5.352256	-0.018860	2.342399
96.038185	1746.042600	5.357261	-0.018944	2.347301
96.402266	1754.133361	5.362266	-0.019017	2.352203
96.778957	1762.216144	5.367270	-0.019092	2.357090
96.933784	1770.273731	5.372275	-0.019126	2.361934
97.213600	1778.347316	5.377280	-0.019184	2.366787
97.492001	1786.409603	5.382285	-0.019241	2.371624
97.829246	1794.478538	5.387290	-0.019309	2.376460
97.990786	1802.568021	5.392294	-0.019344	2.381283
98.287490	1810.617999	5.397299	-0.019405	2.386085
98.730414	1818.684880	5.402304	-0.019493	2.390898
98.913967	1826.764916	5.407309	-0.019532	2.395689
99.160741	1834.823157	5.412314	-0.019583	2.400462
99.733594	1842.851244	5.417318	-0.019695	2.405233
99.952515	1850.923868	5.422323	-0.019741	2.409994
100.471734	1858.985238	5.427328	-0.019843	2.414762
100.774225	1867.041714	5.432333	-0.019905	2.419500
101.238965	1875.082537	5.437338	-0.019997	2.424233
101.457528	1883.182666	5.442342	-0.020043	2.428972
101.514198	1891.338946	5.447347	-0.020059	2.433722
102.095754	1899.357772	5.452352	-0.020172	2.438422
102.340006	1907.384299	5.457357	-0.020223	2.443093
102.496107	1915.450367	5.462362	-0.020257	2.447771
102.953453	1923.500278	5.467366	-0.020348	2.452453
103.214131	1931.555051	5.472371	-0.020402	2.457114
103.324169	1939.630343	5.477376	-0.020427	2.461767
103.614959	1947.680223	5.482381	-0.020487	2.466410
103.924902	1955.750330	5.487386	-0.020550	2.471057
104.222636	1963.831691	5.492390	-0.020611	2.475701
104.245990	1971.869689	5.497395	-0.020620	2.480291
104.825652	1979.888997	5.502400	-0.020733	2.484903
105.019946	1987.957908	5.507405	-0.020775	2.489506
105.144827	1996.049500	5.512410	-0.020803	2.494108
105.543190	2004.100629	5.517414	-0.020883	2.498699
105.649737	2012.151741	5.522419	-0.020908	2.503260
106.063983	2020.202573	5.527424	-0.020990	2.507835
106.389057	2028.305921	5.532429	-0.021056	2.512425
106.538466	2036.373266	5.537434	-0.021089	2.516973
106.833511	2044.399603	5.542438	-0.021150	2.521500
107.055579	2052.432069	5.547443	-0.021196	2.526018
107.594866	2060.461652	5.552448	-0.021302	2.530548
107.915685	2068.534161	5.557453	-0.021367	2.535079
108.143641	2076.561130	5.562458	-0.021415	2.539570
108.402975	2084.631313	5.567462	-0.021468	2.544078
108.498972	2092.700468	5.572467	-0.021491	2.548567
109.107436	2100.745052	5.577472	-0.021610	2.553070
109.517200	2108.796670	5.582477	-0.021692	2.557555
109.937998	2116.815192	5.587482	-0.021775	2.562015
110.117483	2124.901113	5.592486	-0.021814	2.566487
110.226804	2132.973506	5.597491	-0.021840	2.570939
110.674130	2141.036424	5.602496	-0.021928	2.575401
110.925026	2149.082793	5.607501	-0.021980	2.579833
111.039223	2157.135513	5.612506	-0.022007	2.584252
111.166116	2165.211645	5.617510	-0.022036	2.588676
111.732408	2173.366595	5.622515	-0.022146	2.593166
112.090503	2181.427298	5.627520	-0.022218	2.597583
111.987515	2189.463568	5.632525	-0.022204	2.601947
112.268744	2197.453311	5.637530	-0.022262	2.606305
112.423551	2205.499712	5.642534	-0.022296	2.610678
112.689349	2213.551111	5.647539	-0.022351	2.615053
113.306252	2221.540516	5.652544	-0.022471	2.619411
113.748589	2229.557983	5.657549	-0.022559	2.623766
114.032226	2237.595029	5.662554	-0.022617	2.628113
114.219614	2245.691151	5.667558	-0.022657	2.632478
114.639419	2253.712513	5.672563	-0.022740	2.636811
114.889764	2261.766724	5.677568	-0.022792	2.641143
115.018213	2269.830603	5.682573	-0.022822	2.645465
115.194411	2277.882591	5.687578	-0.022860	2.649777
115.435520	2285.970916	5.692582	-0.022910	2.654106
115.562720	2293.998777	5.697587	-0.022939	2.658387
115.833357	2302.056249	5.702592	-0.022994	2.662687
116.084029	2310.114038	5.707597	-0.023046	2.666979
116.477583	2318.165805	5.712602	-0.023125	2.671270
116.504915	2326.272301	5.717606	-0.023135	2.675559
116.736527	2334.262911	5.722611	-0.023184	2.679794
117.322138	2342.266691	5.727616	-0.023298	2.684051
117.439940	2350.315165	5.732621	-0.023325	2.688295
117.709984	2358.384808	5.737626	-0.023381	2.692553
117.943476	2366.452147	5.742630	-0.023430	2.696801
118.140622	2374.473504	5.747635	-0.023472	2.701016
118.478882	2382.495936	5.752640	-0.023540	2.705233
118.814561	2390.555930	5.757645	-0.023608	2.709463
118.856335	2398.645342	5.762650	-0.023621	2.713684
119.003536	2406.699968	5.767654	-0.023653	2.717887
119.413946	2414.677434	5.772659	-0.023735	2.722059
119.423526	2422.747053	5.777664	-0.023742	2.726248
119.488945	2430.817629	5.782669	-0.023760	2.730434
119.888880	2438.846415	5.787674	-0.023839	2.734613
120.251655	2446.881843	5.792678	-0.023912	2.738786
120.606313	2454.882249	5.797683	-0.023983	2.742935
120.713338	2462.955788	5.802688	-0.024009	2.747099
121.049168	2471.035916	5.807693	-0.024077	2.751275
121.414398	2479.133575	5.812698	-0.024150	2.755455
121.616080	2487.153898	5.817702	-0.024193	2.759579
122.025796	2495.131402	5.822707	-0.024274	2.763688
122.326154	2503.181509	5.827712	-0.024335	2.767821
122.479287	2511.240242	5.832717	-0.024369	2.771943
122.777182	2519.275762	5.837722	-0.024430	2.776056
123.048148	2527.321605	5.842726	-0.024486	2.780166
123.340903	2535.324714	5.847731	-0.024545	2.784250
123.525251	2543.405920	5.852736	-0.024585	2.788361
123.707613	2551.478426	5.857741	-0.024624	2.792462
123.767908	2559.530729	5.862746	-0.024641	2.796539
123.887825	2567.584837	5.867750	-0.024668	2.800614
124.080046	2575.568696	5.872755	-0.024710	2.804653
124.448190	2583.619575	5.877760	-0.024783	2.808729
124.600292	2591.696041	5.882765	-0.024817	2.812800
124.735657	2599.737699	5.887770	-0.024847	2.816846
125.272085	2607.747503	5.892774	-0.024953	2.820894
125.378130	2615.760365	5.897779	-0.024978	2.824913
125.580164	2623.837462	5.902784	-0.025021	2.828963
126.057735	2631.900451	5.907789	-0.025115	2.833016
126.310271	2639.923820	5.912794	-0.025167	2.837031
126.622351	2647.959461	5.917798	-0.025230	2.841050
126.846814	2655.964450	5.922803	-0.025277	2.845043
127.116778	2664.019707	5.927808	-0.025333	2.849057
127.336813	2672.077007	5.932813	-0.025379	2.853064
127.498592	2680.113217	5.937818	-0.025415	2.857052
127.753554	2688.169204	5.942822	-0.025467	2.861049
127.890895	2696.177702	5.947827	-0.025498	2.865011
128.227957	2704.228160	5.952832	-0.025566	2.868998
128.487910	2712.295486	5.957837	-0.025620	2.872985
128.773744	2720.322338	5.962842	-0.025678	2.876947
128.960430	2728.382953	5.967846	-0.025719	2.880914
129.277307	2736.361891	5.972851	-0.025783	2.884844
129.676864	2744.431372	5.977856	-0.025862	2.888817
129.831928	2752.499750	5.982861	-0.025897	2.892770
130.219629	2760.516971	5.987866	-0.025974	2.896706
130.537350	2768.569083	5.992870	-0.026039	2.900649
130.811409	2776.562094	5.997875	-0.026095	2.904556
130.995254	2784.644723	6.002880	-0.026134	2.908496
131.197209	2792.751864	6.007885	-0.026177	2.912444
131.515284	2800.803882	6.012890	-0.026242	2.916366
131.796980	2808.778021	6.017894	-0.026299	2.920243
131.977514	2816.784983	6.022899	-0.026338	2.924125
132.267707	2824.820445	6.027904	-0.026398	2.928021
132.462640	2832.875235	6.032909	-0.026439	2.931917
132.593676	2840.922523	6.037914	-0.026469	2.935800
132.904794	2848.933673	6.042918	-0.026532	2.939671
133.116638	2856.943580	6.047923	-0.026577	2.943530
133.393565	2864.996780	6.052928	-0.026634	2.947409
133.810750	2873.052082	6.057933	-0.026717	2.951290
134.261776	2881.068213	6.062938	-0.026806	2.955150
134.549397	2889.104848	6.067942	-0.026865	2.959005
134.425229	2897.161108	6.072947	-0.026847	2.962844
134.778466	2905.193500	6.077952	-0.026918	2.966691
135.063086	2913.237966	6.082957	-0.026976	2.970535
135.144232	2921.291140	6.087962	-0.026997	2.974368
135.308460	2929.361006	6.092966	-0.027032	2.978208
135.503699	2937.362314	6.097971	-0.027074	2.982012
135.795454	2945.385439	6.102976	-0.027134	2.985827
136.183487	2953.408753	6.107981	-0.027211	2.989641
136.420731	2961.478362	6.112986	-0.027261	2.993465
136.892960	2969.507052	6.117990	-0.027354	2.997276
136.950847	2977.517741	6.122995	-0.027370	3.001054
137.201052	2985.529556	6.128000	-0.027422	3.004836
137.347580	2993.593098	6.133005	-0.027454	3.008633
137.460171	3001.629215	6.138010	-0.027481	3.012411
137.857965	3009.689544	6.143014	-0.027560	3.016209
138.293502	3017.673561	6.148019	-0.027646	3.019969
138.315100	3025.730401	6.153024	-0.027656	3.023737
138.490864	3033.779220	6.158029	-0.027694	3.027505
138.641273	3041.826741	6.163034	-0.027727	3.031266
138.897360	3049.890792	6.168038	-0.027780	3.035035
139.051374	3057.892345	6.173043	-0.027814	3.038766
139.383835	3065.913572	6.178048	-0.027881	3.042509
139.612693	3073.942777	6.183053	-0.027929	3.046247
139.680618	3081.970943	6.188058	-0.027947	3.049972
140.002534	3090.067151	6.193062	-0.028012	3.053736
140.125109	3098.083895	6.198067	-0.028040	3.057449
140.278977	3106.116037	6.203072	-0.028074	3.061166
140.253939	3114.166187	6.208077	-0.028075	3.064878
140.542835	3122.179095	6.213082	-0.028134	3.068584
140.819551	3130.288621	6.218086	-0.028191	3.072328
140.949802	3138.339502	6.223091	-0.028220	3.076035
141.289546	3146.323082	6.228096	-0.028289	3.079716
141.470351	3154.327743	6.233101	-0.028327	3.083394
141.682979	3162.330655	6.238106	-0.028372	3.087069
141.918675	3170.370939	6.243110	-0.028421	3.090758
142.029557	3178.423966	6.248115	-0.028447	3.094442
142.311826	3186.436549	6.253120	-0.028505	3.098112
142.654061	3194.460984	6.258125	-0.028574	3.101785
142.818919	3202.482013	6.263130	-0.028610	3.105444
143.067168	3210.532418	6.268134	-0.028662	3.109115
143.262221	3218.579213	6.273139	-0.028703	3.112779
143.619587	3226.644211	6.278144	-0.028775	3.116453
143.963519	3234.629243	6.283149	-0.028844	3.120087
143.986352	3242.643902	6.288154	-0.028854	3.123715
144.258657	3250.699851	6.293158	-0.028910	3.127368
144.464378	3258.733896	6.298163	-0.028954	3.131005
144.795111	3266.762285	6.303168	-0.029020	3.134640
144.931565	3274.810980	6.308173	-0.029051	3.138272
145.138137	3282.830243	6.313178	-0.029095	3.141889
145.453071	3290.862827	6.318182	-0.029159	3.145513
145.464710	3298.890688	6.323187	-0.029166	3.149117
146.098841	3306.942882	6.328192	-0.029289	3.152755
146.180948	3314.998543	6.333197	-0.029310	3.156366
146.328654	3322.987261	6.338202	-0.029343	3.159946
146.764887	3330.982267	6.343206	-0.029429	3.163537
147.056067	3339.034938	6.348211	-0.029489	3.167144
147.126158	3347.069276	6.353216	-0.029507	3.170728
147.172284	3355.157854	6.358221	-0.029521	3.174332
147.540709	3363.136113	6.363226	-0.029595	3.177897
147.904472	3371.177403	6.368230	-0.029668	3.181485
147.941508	3379.202294	6.373235	-0.029680	3.185047
148.178979	3387.259284	6.378240	-0.029730	3.188629
148.363365	3395.329826	6.383245	-0.029769	3.192210
148.704474	3403.323956	6.388250	-0.029838	3.195760
148.980048	3411.333388	6.393254	-0.029894	3.199310
149.088706	3419.344352	6.398259	-0.029920	3.202850
149.223282	3427.379499	6.403264	-0.029950	3.206398
149.419477	3435.444040	6.408269	-0.029992	3.209957
149.571773	3443.491240	6.413274	-0.030026	3.213502
149.955446	3451.517794	6.418278	-0.030102	3.217045
150.043423	3459.535631	6.423283	-0.030124	3.220567
150.285338	3467.535742	6.428288	-0.030174	3.224084
150.524282	3475.579947	6.433293	-0.030224	3.227616
150.684156	3483.629049	6.438298	-0.030259	3.231143
151.087918	3491.694325	6.443302	-0.030340	3.234684
151.212153	3499.697307	6.448307	-0.030368	3.238181
151.559782	3507.692572	6.453312	-0.030438	3.241681
151.711533	3515.704758	6.458317	-0.030472	3.245177
151.594741	3523.741872	6.463322	-0.030455	3.248668
152.020837	3531.803634	6.468326	-0.030540	3.252189
152.322330	3539.844081	6.473331	-0.030601	3.255691
152.457623	3547.850255	6.478336	-0.030632	3.259168
152.812011	3555.871652	6.483341	-0.030703	3.262656
153.121704	3563.882079	6.488346	-0.030766	3.266135
153.095525	3571.970161	6.493350	-0.030766	3.269629
153.329530	3580.007021	6.498355	-0.030815	3.273109
153.862643	3588.021024	6.503360	-0.030920	3.276586
154.094583	3596.030518	6.508365	-0.030968	3.280046
154.344108	3604.015787	6.513370	-0.031020	3.283492
154.491149	3612.104562	6.518374	-0.031052	3.286975
154.470439	3620.116011	6.523379	-0.031054	3.290415
154.724972	3628.163517	6.528384	-0.031107	3.293877
155.037579	3636.194731	6.533389	-0.031170	3.297331
155.216218	3644.204198	6.538394	-0.031209	3.300767
155.898479	3652.188075	6.543398	-0.031341	3.304207
156.303330	3660.211915	6.548403	-0.031421	3.307651
156.757213	3668.283876	6.553408	-0.031511	3.311113
157.064364	3676.332104	6.558413	-0.031574	3.314555
157.092583	3684.349737	6.563418	-0.031584	3.317971
157.344085	3692.376486	6.568422	-0.031636	3.321395
157.349007	3700.384871	6.573427	-0.031643	3.324799
157.668950	3708.374500	6.578432	-0.031707	3.328203
158.202294	3716.427393	6.583437	-0.031812	3.331638
158.169189	3724.499385	6.588442	-0.031811	3.335056
158.504953	3732.516426	6.593446	-0.031879	3.338462
158.666595	3740.546656	6.598451	-0.031914	3.341863
158.945248	3748.548350	6.603456	-0.031971	3.345253
159.321703	3756.586088	6.608461	-0.032047	3.348658
159.330861	3764.638061	6.613466	-0.032054	3.352052
159.595048	3772.696945	6.618470	-0.032108	3.355455
159.710080	3780.679723	6.623475	-0.032135	3.358817
159.855400	3788.721476	6.628480	-0.032167	3.362202
160.111661	3796.765608	6.633485	-0.032220	3.365588
160.344933	3804.761098	6.638490	-0.032269	3.368949
160.702514	3812.821174	6.643494	-0.032341	3.372339
160.919377	3820.849287	6.648499	-0.032386	3.375707
161.108540	3828.853516	6.653504	-0.032427	3.379060
161.438821	3836.898691	6.658509	-0.032494	3.382432
161.346550	3844.921200	6.663514	-0.032482	3.385776
161.729391	3852.930965	6.668518	-0.032558	3.389129
161.985914	3861.027748	6.673523	-0.032611	3.392510
162.000354	3869.097524	6.678528	-0.032619	3.395867
162.109438	3877.072669	6.683533	-0.032645	3.399186
162.487949	3885.039893	6.688538	-0.032721	3.402507
162.985813	3893.068379	6.693542	-0.032819	3.405854
162.975599	3901.078723	6.698547	-0.032822	3.409173
163.219373	3909.120290	6.703552	-0.032873	3.412511
163.542963	3917.172299	6.708557	-0.032938	3.415852
163.672554	3925.168256	6.713562	-0.032968	3.419160
163.900286	3933.189658	6.718566	-0.033015	3.422479
164.042321	3941.222983	6.723571	-0.033047	3.425796
164.332464	3949.242909	6.728576	-0.033106	3.429110
164.654671	3957.293155	6.733581	-0.033171	3.432434
164.920465	3965.334702	6.738586	-0.033226	3.435749
165.380715	3973.350045	6.743590	-0.033317	3.439057
165.614313	3981.361314	6.748595	-0.033366	3.442352
165.788062	3989.386754	6.753600	-0.033404	3.445648
166.121689	3997.419230	6.758605	-0.033471	3.448949
166.177606	4005.461375	6.763610	-0.033487	3.452241
166.428506	4013.525326	6.768614	-0.033539	3.455546
166.744079	4021.498614	6.773619	-0.033603	3.458812
166.970526	4029.535733	6.778624	-0.033650	3.462099
167.041853	4037.579979	6.783629	-0.033669	3.465380
167.273422	4045.575386	6.788634	-0.033717	3.468644
167.529826	4053.646328	6.793638	-0.033770	3.471935
167.736762	4061.677494	6.798643	-0.033814	3.475206
167.947263	4069.670663	6.803648	-0.033858	3.478459
168.041543	4077.695227	6.808653	-0.033881	3.481717
168.078825	4085.687153	6.813658	-0.033893	3.484958
168.453559	4093.711699	6.818662	-0.033968	3.488219
168.574302	4101.765394	6.823667	-0.033996	3.491481
168.891669	4109.772664	6.828672	-0.034060	3.494727
168.844841	4117.836058	6.833677	-0.034057	3.497981
169.000176	4125.845532	6.838682	-0.034091	3.501217
169.417988	4133.822745	6.843686	-0.034174	3.504446
169.521736	4141.893113	6.848691	-0.034199	3.507698
169.596692	4149.929770	6.853696	-0.034218	3.510934
170.115865	4157.925671	6.858701	-0.034320	3.514163
170.179464	4165.936179	6.863706	-0.034337	3.517382
170.492501	4173.979320	6.868710	-0.034401	3.520618
170.607312	4181.935286	6.873715	-0.034427	3.523810
170.750664	4190.007892	6.878720	-0.034459	3.527047
170.968324	4198.077650	6.883725	-0.034505	3.530282
171.327376	4206.080111	6.888730	-0.034577	3.533492
171.498535	4214.153515	6.893734	-0.034614	3.536721
171.626882	4222.138187	6.898739	-0.034644	3.539910
171.656005	4230.193232	6.903744	-0.034654	3.543122
172.221583	4238.216892	6.908749	-0.034765	3.546334
172.274188	4246.194664	6.913754	-0.034780	3.549510
172.462400	4254.350987	6.918758	-0.034820	3.552758
172.784169	4262.395599	6.923763	-0.034885	3.555962
172.999282	4270.320941	6.928768	-0.034931	3.559113
173.007848	4278.343567	6.933773	-0.034938	3.562294
173.131830	4286.325413	6.938778	-0.034966	3.565459
173.539988	4294.355027	6.943782	-0.035047	3.568648
173.665571	4302.414376	6.948787	-0.035076	3.571838
173.735482	4310.432891	6.953792	-0.035094	3.575008
174.309349	4318.442277	6.958797	-0.035206	3.578185
174.463265	4326.453247	6.963802	-0.035240	3.581349
174.905005	4334.435373	6.968806	-0.035328	3.584506
174.957589	4342.505353	6.973811	-0.035343	3.587684
175.083155	4350.551029	6.978816	-0.035371	3.590851
175.169502	4358.600345	6.983821	-0.035393	3.594016
175.181162	4366.581022	6.988826	-0.035400	3.597150
175.632958	4374.579282	6.993830	-0.035490	3.600299
175.728955	4382.599866	6.998835	-0.035513	3.603445
175.945712	4390.613304	7.003840	-0.035558	3.606589
176.422344	4398.652864	7.008845	-0.035652	3.609747
176.388069	4406.700000	7.013850	-0.035651	3.612891
176.674423	4414.735435	7.018854	-0.035710	3.616037
177.011605	4422.743993	7.023859	-0.035778	3.619171
177.232635	4430.745396	7.028864	-0.035824	3.622296
177.407684	4438.773886	7.033869	-0.035862	3.625427
177.447152	4446.814884	7.038874	-0.035875	3.628558
178.052824	4454.873119	7.043878	-0.035993	3.631707
178.188758	4462.931942	7.048883	-0.036023	3.634841
178.491938	4470.894435	7.053888	-0.036085	3.637940
178.753485	4478.944064	7.058893	-0.036139	3.641068
179.035149	4486.875209	7.063898	-0.036197	3.644149
179.126036	4494.952196	7.068902	-0.036219	3.647278
179.326940	4502.989045	7.073907	-0.036262	3.650392
179.580888	4511.001744	7.078912	-0.036314	3.653495
179.713301	4519.059602	7.083917	-0.036344	3.656610
179.716391	4527.056291	7.088922	-0.036350	3.659695
180.035273	4535.090967	7.093926	-0.036415	3.662801
180.228489	4543.120033	7.098931	-0.036456	3.665898
180.372507	4551.140635	7.103936	-0.036488	3.668988
180.703434	4559.184736	7.108941	-0.036555	3.672090
181.015564	4567.180142	7.113946	-0.036618	3.675169
181.195681	4575.197743	7.118950	-0.036657	3.678251
181.449113	4583.234367	7.123955	-0.036709	3.681340
181.894730	4591.168080	7.128960	-0.036798	3.684391
182.093216	4599.266912	7.133965	-0.036840	3.687497
182.034143	4607.291722	7.138970	-0.036834	3.690565
182.256627	4615.349571	7.143974	-0.036881	3.693651
182.329613	4623.379928	7.148979	-0.036900	3.696719
182.462774	4631.359031	7.153984	-0.036930	3.699767
182.766677	4639.384413	7.158989	-0.036992	3.702835
182.900271	4647.374395	7.163994	-0.037022	3.705882
183.311158	4655.425215	7.168998	-0.037104	3.708956
183.465195	4663.483937	7.174003	-0.037138	3.712025
183.623249	4671.559007	7.179008	-0.037172	3.715097
183.560126	4679.562122	7.184013	-0.037166	3.718134
183.629716	4687.552539	7.189018	-0.037184	3.721167
184.032724	4695.500164	7.194022	-0.037264	3.724190
184.223130	4703.542209	7.199027	-0.037305	3.727240
184.097741	4711.584608	7.204032	-0.037287	3.730281
184.449827	4719.638764	7.209037	-0.037358	3.733335
184.542313	4727.655741	7.214042	-0.037380	3.736366
184.966477	4735.614526	7.219046	-0.037464	3.739381
184.848737	4743.671929	7.224051	-0.037448	3.742417
185.025940	4751.687529	7.229056	-0.037486	3.745442
185.474735	4759.693568	7.234061	-0.037575	3.748468
185.552364	4767.760092	7.239066	-0.037595	3.751505
185.863182	4775.767222	7.244070	-0.037658	3.754523
185.951792	4783.821285	7.249075	-0.037680	3.757550
185.890881	4791.828703	7.254080	-0.037673	3.760555
186.170669	4799.816572	7.259085	-0.037731	3.763557
186.229351	4807.846995	7.264090	-0.037747	3.766568
186.533870	4815.894720	7.269094	-0.037809	3.769588
186.681351	4823.962774	7.274099	-0.037842	3.772611
186.756834	4831.949843	7.279104	-0.037861	3.775598
187.014350	4839.972401	7.284109	-0.037914	3.778601
186.973170	4847.990182	7.289114	-0.037912	3.781593
187.149109	4856.011302	7.294118	-0.037950	3.784588
187.317457	4864.034288	7.299123	-0.037986	3.787582
187.537417	4872.057266	7.304128	-0.038033	3.790575
187.858883	4880.113384	7.309133	-0.038098	3.793579
187.896092	4888.137451	7.314138	-0.038110	3.796563
188.231962	4896.109002	7.319142	-0.038178	3.799532
188.327480	4904.120456	7.324147	-0.038201	3.802508
188.388352	4912.116691	7.329152	-0.038217	3.805475
188.585872	4920.158394	7.334157	-0.038259	3.808460
188.928095	4928.186250	7.339162	-0.038328	3.811440
189.180040	4936.224950	7.344166	-0.038381	3.814420
189.304045	4944.248747	7.349171	-0.038409	3.817389
189.192159	4952.257817	7.354176	-0.038393	3.820346
189.518296	4960.244451	7.359181	-0.038459	3.823301
189.494403	4968.255801	7.364186	-0.038460	3.826256
190.126798	4976.279880	7.369190	-0.038583	3.829227
190.142116	4984.342240	7.374195	-0.038591	3.832196
190.439898	4992.338817	7.379200	-0.038652	3.835145
190.918369	5000.346747	7.384205	-0.038746	3.838100
190.728848	5008.362183	7.389210	-0.038716	3.841041
190.994431	5016.374274	7.394214	-0.038771	3.843988
191.100949	5024.409207	7.399219	-0.038796	3.846938
191.241681	5032.451858	7.404224	-0.038828	3.849890
191.423994	5040.485647	7.409229	-0.038867	3.852836
191.596990	5048.524482	7.414234	-0.038904	3.855782
191.906667	5056.524426	7.419238	-0.038967	3.858714
191.922317	5064.555321	7.424243	-0.038976	3.861649
192.015431	5072.565002	7.429248	-0.038998	3.864576
192.350090	5080.620670	7.434253	-0.039066	3.867523
192.420113	5088.625946	7.439258	-0.039084	3.870443
192.759533	5096.866996	7.444262	-0.039153	3.873452
192.932857	5104.875662	7.449267	-0.039190	3.876371
193.092848	5112.726329	7.454272	-0.039225	3.879230
193.387773	5120.775804	7.459277	-0.039285	3.882162
193.387197	5128.715748	7.464282	-0.039290	3.885046
193.783393	5136.772109	7.469286	-0.039369	3.887978
194.048729	5144.765037	7.474291	-0.039424	3.890882
194.078722	5152.777365	7.479296	-0.039435	3.893787
194.458854	5160.846239	7.484301	-0.039511	3.896716
194.536694	5168.788779	7.489306	-0.039531	3.899592
194.655286	5176.873282	7.494310	-0.039558	3.902517
194.604005	5184.861261	7.499315	-0.039554	3.905403
195.040788	5192.848824	7.504320	-0.039640	3.908295
195.056785	5200.930050	7.509325	-0.039649	3.911211
195.254448	5208.938657	7.514330	-0.039691	3.914102
195.508436	5216.965991	7.519334	-0.039743	3.916999
195.546742	5224.934933	7.524339	-0.039756	3.919868
195.441471	5232.977827	7.529344	-0.039741	3.922759
195.844229	5240.989539	7.534349	-0.039822	3.925646
195.942394	5248.978384	7.539354	-0.039845	3.928518
196.107686	5257.043703	7.544358	-0.039881	3.931416
196.453749	5265.063314	7.549363	-0.039951	3.934298
196.525020	5273.082650	7.554368	-0.039969	3.937174
196.633869	5281.087702	7.559373	-0.039995	3.940042
196.665109	5289.080672	7.564378	-0.040006	3.942903
196.864269	5297.140169	7.569382	-0.040048	3.945789
196.972148	5305.156836	7.574387	-0.040074	3.948656
197.107335	5313.204282	7.579392	-0.040104	3.951532
197.420695	5321.263840	7.584397	-0.040168	3.954413
197.612565	5329.220579	7.589402	-0.040209	3.957253
197.839435	5337.219119	7.594406	-0.040256	3.960107
198.039699	5345.217797	7.599411	-0.040299	3.962958
198.204582	5353.250362	7.604416	-0.040335	3.965819
198.322535	5361.248005	7.609421	-0.040362	3.968665
198.274587	5369.312971	7.614426	-0.040358	3.971529
198.692267	5377.331747	7.619430	-0.040441	3.974383
198.766012	5385.370079	7.624435	-0.040460	3.977236
198.883432	5393.332877	7.629440	-0.040487	3.980060
199.267384	5401.362075	7.634445	-0.040564	3.982911
199.490860	5409.375568	7.639450	-0.040611	3.985752
199.597347	5417.411793	7.644454	-0.040636	3.988596
199.955738	5425.487211	7.649459	-0.040708	3.991456
200.043910	5433.494384	7.654464	-0.040730	3.994286
200.247864	5441.539128	7.659469	-0.040773	3.997129
200.071154	5449.521198	7.664474	-0.040746	3.999942
200.257911	5457.557852	7.669478	-0.040786	4.002777
200.535055	5465.574916	7.674483	-0.040842	4.005606
200.680765	5473.569093	7.679488	-0.040875	4.008422
200.885257	5481.624925	7.684493	-0.040918	4.011258
201.055435	5489.667650	7.689498	-0.040955	4.014088
201.126992	5497.706292	7.694502	-0.040974	4.016912
201.267840	5505.678151	7.699507	-0.041005	4.019712
201.681879	5513.681869	7.704512	-0.041088	4.022526
201.820766	5521.708807	7.709517	-0.041119	4.025341
202.027136	5529.725995	7.714522	-0.041162	4.028152
202.003194	5537.766045	7.719526	-0.041163	4.030966
202.196605	5545.904086	7.724531	-0.041205	4.033815
202.500374	5553.859125	7.729536	-0.041266	4.036600
202.719766	5561.804638	7.734541	-0.041312	4.039378
202.645661	5569.835384	7.739546	-0.041304	4.042180
202.819163	5577.793082	7.744550	-0.041341	4.044958
202.905844	5585.859475	7.749555	-0.041363	4.047770
203.011615	5593.864360	7.754560	-0.041388	4.050560
203.326271	5601.935139	7.759565	-0.041452	4.053374
203.257606	5609.919930	7.764570	-0.041444	4.056150
203.710753	5617.902840	7.769574	-0.041534	4.058931
203.883991	5625.965955	7.774579	-0.041571	4.061734
203.892485	5633.934429	7.779584	-0.041578	4.064499
203.966469	5641.990298	7.784589	-0.041597	4.067295
204.290137	5649.964062	7.789594	-0.041663	4.070063
204.600022	5658.016993	7.794598	-0.041726	4.072856
204.707954	5666.033226	7.799603	-0.041751	4.075632
204.702206	5674.009891	7.804608	-0.041755	4.078391
205.090156	5682.071972	7.809613	-0.041833	4.081183
205.070747	5690.044763	7.814618	-0.041834	4.083937
205.131697	5698.112035	7.819622	-0.041851	4.086722
205.349667	5706.097163	7.824627	-0.041897	4.089480
205.432202	5714.150174	7.829632	-0.041917	4.092257
205.769742	5722.202361	7.834637	-0.041986	4.095035
205.959172	5730.167939	7.839642	-0.042026	4.097780
206.073454	5738.226281	7.844646	-0.042053	4.100553
206.137977	5746.208468	7.849651	-0.042070	4.103298
206.185102	5754.217610	7.854656	-0.042084	4.106050
206.528738	5762.264522	7.859661	-0.042153	4.108817
206.792202	5770.298199	7.864666	-0.042208	4.111577
206.927597	5778.338576	7.869670	-0.042238	4.114335
207.133234	5786.381778	7.874675	-0.042282	4.117093
206.799235	5794.332022	7.879680	-0.042225	4.119811
207.216134	5802.371779	7.884685	-0.042308	4.122567
207.341653	5810.344739	7.889690	-0.042336	4.125295
207.647060	5818.396858	7.894694	-0.042398	4.128050
207.618265	5826.450240	7.899699	-0.042398	4.130800
208.026513	5834.446422	7.904704	-0.042479	4.133533
208.303622	5842.522419	7.909709	-0.042536	4.136291
208.200763	5850.463624	7.914714	-0.042522	4.138995
208.263752	5858.528778	7.919718	-0.042539	4.141743
208.463916	5866.492580	7.924723	-0.042582	4.144455
208.761421	5874.538136	7.929728	-0.042643	4.147195
209.039774	5882.587980	7.934733	-0.042700	4.149935
209.145420	5890.636433	7.939738	-0.042725	4.152669
209.553218	5898.615325	7.944742	-0.042806	4.155382
209.396650	5906.620970	7.949747	-0.042782	4.158096
209.463347	5914.640692	7.954752	-0.042800	4.160815
209.723789	5922.658146	7.959757	-0.042853	4.163534
209.899769	5930.645083	7.964762	-0.042891	4.166240
209.904289	5938.712324	7.969766	-0.042898	4.168969
210.183555	5946.725742	7.974771	-0.042955	4.171682
210.133709	5954.726844	7.979776	-0.042951	4.174385
210.509882	5962.800356	7.984781	-0.043026	4.177115
210.571539	5970.748094	7.989786	-0.043043	4.179797
210.745716	5978.771366	7.994790	-0.043081	4.182505
210.963682	5986.805900	7.999795	-0.043126	4.185214
210.745373	5994.786636	8.004800	-0.043091	4.187900
211.296938	6002.839444	8.009805	-0.043199	4.190616
211.132195	6010.965250	8.014810	-0.043174	4.193347
211.331867	6018.979684	8.019814	-0.043216	4.196043
211.669735	6026.934549	8.024819	-0.043284	4.198718
211.575339	6034.924056	8.029824	-0.043272	4.201399
211.736004	6042.885519	8.034829	-0.043307	4.204072
212.045597	6050.939716	8.039834	-0.043370	4.206775
212.348118	6058.903433	8.044838	-0.043431	4.209446
212.447079	6067.031564	8.049843	-0.043455	4.212169
212.668195	6074.959666	8.054848	-0.043502	4.214824
212.764086	6083.021811	8.059853	-0.043525	4.217520
212.937065	6090.998057	8.064858	-0.043562	4.220187
212.941854	6098.980719	8.069862	-0.043568	4.222853
213.262872	6107.048867	8.074867	-0.043633	4.225549
213.381830	6115.055237	8.079872	-0.043661	4.228221
213.394733	6123.122308	8.084877	-0.043669	4.230910
213.428917	6131.142339	8.089882	-0.043680	4.233581
213.674597	6139.163211	8.094886	-0.043731	4.236254
213.643542	6147.139950	8.099891	-0.043731	4.238907
213.730002	6155.171867	8.104896	-0.043752	4.241578
214.227024	6163.134268	8.109901	-0.043850	4.244229
214.398926	6171.163684	8.114906	-0.043887	4.246897
214.370616	6179.179359	8.119910	-0.043887	4.249556
214.517093	6187.249815	8.124915	-0.043920	4.252234
214.819386	6195.271184	8.129920	-0.043981	4.254895
214.832850	6203.267901	8.134925	-0.043989	4.257544
215.076434	6211.296375	8.139930	-0.044040	4.260203
215.100540	6219.299079	8.144934	-0.044049	4.262851
215.223706	6227.345686	8.149939	-0.044077	4.265512
215.233419	6235.351241	8.154944	-0.044085	4.268157
215.675182	6243.405218	8.159949	-0.044172	4.270820
215.845656	6251.438399	8.164954	-0.044209	4.273472
215.690500	6259.489857	8.169958	-0.044186	4.276126
216.104599	6267.453849	8.174963	-0.044268	4.278754
216.318472	6275.392962	8.179968	-0.044313	4.281371
216.477021	6283.427620	8.184973	-0.044348	4.284017
216.614820	6291.484932	8.189978	-0.044379	4.286668
216.815488	6299.491570	8.194982	-0.044421	4.289302
217.005176	6307.536762	8.199987	-0.044462	4.291946
216.923732	6315.553739	8.204992	-0.044452	4.294578
217.206669	6323.588581	8.209997	-0.044510	4.297217
217.515388	6331.555480	8.215002	-0.044573	4.299832
217.643190	6339.602235	8.220006	-0.044602	4.302470
217.699644	6347.599434	8.225011	-0.044617	4.305089
217.770944	6355.636485	8.230016	-0.044636	4.307721
217.932015	6363.639143	8.235021	-0.044671	4.310340
218.067352	6371.696060	8.240026	-0.044702	4.312975
218.425000	6379.703125	8.245030	-0.044774	4.315593
218.643488	6387.701177	8.250035	-0.044820	4.318206
218.464860	6395.692138	8.255040	-0.044792	4.320813
218.608362	6403.721779	8.260045	-0.044823	4.323432
218.828725	6411.715354	8.265050	-0.044870	4.326039
218.906648	6419.739052	8.270054	-0.044890	4.328653
219.169818	6427.777964	8.275059	-0.044944	4.331272
219.330325	6435.769371	8.280064	-0.044979	4.333873
219.542788	6443.872111	8.285069	-0.045024	4.336509
219.423906	6451.784156	8.290074	-0.045007	4.339079
219.639504	6459.829369	8.295078	-0.045052	4.341693
219.878792	6467.820330	8.300083	-0.045102	4.344288
219.919775	6475.858807	8.305088	-0.045115	4.346896
220.149188	6483.856829	8.310093	-0.045163	4.349490
220.177698	6491.970826	8.315098	-0.045174	4.352118
220.314572	6500.022933	8.320102	-0.045204	4.354726
220.514224	6508.020763	8.325107	-0.045247	4.357315
220.772157	6515.909289	8.330112	-0.045300	4.359868
221.003083	6523.983782	8.335117	-0.045348	4.362479
221.002533	6531.927504	8.340122	-0.045353	4.365044
221.205628	6539.974546	8.345126	-0.045397	4.367643
221.579180	6548.018387	8.350131	-0.045471	4.370240
221.623526	6556.039466	8.355136	-0.045485	4.372827
221.734926	6564.064070	8.360141	-0.045511	4.375413
221.918621	6572.047530	8.365146	-0.045550	4.377985
222.108588	6580.057969	8.370150	-0.045591	4.380564
222.375801	6588.079587	8.375155	-0.045646	4.383145
222.491124	6596.061155	8.380160	-0.045673	4.385712
222.693014	6604.108137	8.385165	-0.045716	4.388298
222.588415	6612.131265	8.390170	-0.045701	4.390873
222.709224	6620.177560	8.395174	-0.045729	4.393456
222.829240	6628.225738	8.400179	-0.045757	4.396037
222.945568	6636.182299	8.405184	-0.045784	4.398588
223.072478	6644.259377	8.410189	-0.045813	4.401176
223.137352	6652.186203	8.415194	-0.045830	4.403714
223.157954	6660.216944	8.420198	-0.045839	4.406283
223.470448	6668.242803	8.425203	-0.045902	4.408851
223.909140	6676.298831	8.430208	-0.045989	4.411428
224.260713	6684.379700	8.435213	-0.046060	4.414010
224.148329	6692.396332	8.440218	-0.046045	4.416568
224.416439	6700.341257	8.445222	-0.046100	4.419104
224.678180	6708.369320	8.450227	-0.046154	4.421665
224.467569	6716.328833	8.455232	-0.046120	4.424200
224.672572	6724.444601	8.460237	-0.046163	4.426785
224.895001	6732.454065	8.465242	-0.046210	4.429335
225.052288	6740.475067	8.470246	-0.046244	4.431887
225.164314	6748.523016	8.475251	-0.046271	4.434446
225.210787	6756.490078	8.480256	-0.046284	4.436977
225.658519	6764.485699	8.485261	-0.046373	4.439518
225.692027	6772.496627	8.490266	-0.046385	4.442060
225.907237	6780.450654	8.495270	-0.046430	4.444584
226.092420	6788.555507	8.500275	-0.046470	4.447153
226.230306	6796.498154	8.505280	-0.046501	4.449670
226.181308	6804.608531	8.510285	-0.046497	4.452238
226.261593	6812.570945	8.515290	-0.046517	4.454757
226.537374	6820.652009	8.520294	-0.046574	4.457314
226.716302	6828.582894	8.525299	-0.046612	4.459821
226.546727	6836.614452	8.530304	-0.046586	4.462357
227.075872	6844.643250	8.535309	-0.046690	4.464894
226.910350	6852.729448	8.540314	-0.046664	4.467445
227.090262	6860.708312	8.545318	-0.046703	4.469961
227.249159	6868.778197	8.550323	-0.046738	4.472505
227.297507	6876.711195	8.555328	-0.046752	4.475004
227.407324	6884.769016	8.560333	-0.046778	4.477541
227.598908	6892.691622	8.565338	-0.046818	4.480034
227.773673	6900.681468	8.570343	-0.046856	4.482547
228.006940	6908.760735	8.575347	-0.046905	4.485087
228.013319	6916.753503	8.580352	-0.046911	4.487597
228.243542	6924.804258	8.585357	-0.046960	4.490125
228.208782	6932.851264	8.590362	-0.046958	4.492650
228.234864	6940.843451	8.595367	-0.046969	4.495156
228.468738	6948.928870	8.600371	-0.047017	4.497690
228.453468	6956.841738	8.605376	-0.047020	4.500168
228.751490	6964.855945	8.610381	-0.047080	4.502678
229.013880	6972.863079	8.615386	-0.047135	4.505184
228.920944	6980.929745	8.620391	-0.047123	4.507706
228.909354	6988.966245	8.625395	-0.047126	4.510217
229.088007	6996.990683	8.630400	-0.047164	4.512724
229.420325	7005.041453	8.635405	-0.047231	4.515237
229.540220	7013.004396	8.640410	-0.047259	4.517722
229.544254	7020.985671	8.645415	-0.047265	4.520210
229.685951	7028.992389	8.650419	-0.047297	4.522706
229.772869	7036.960869	8.655424	-0.047318	4.525188
229.838222	7045.035243	8.660429	-0.047335	4.527701
229.935607	7053.044658	8.665434	-0.047359	4.530193
230.072899	7061.082372	8.670439	-0.047390	4.532693
230.267826	7069.105123	8.675443	-0.047431	4.535186
230.167304	7077.085939	8.680448	-0.047418	4.537665
230.624374	7085.085855	8.685453	-0.047508	4.540149
230.645167	7093.144203	8.690458	-0.047517	4.542649
230.845376	7101.095217	8.695463	-0.047560	4.545115
231.092804	7109.163240	8.700467	-0.047611	4.547616
231.168275	7117.123782	8.705472	-0.047630	4.550081
231.276308	7125.219659	8.710477	-0.047656	4.552588
231.405756	7133.260393	8.715482	-0.047685	4.555076
231.574259	7141.257935	8.720487	-0.047722	4.557549
231.734910	7149.245784	8.725491	-0.047757	4.560018
231.854768	7157.249325	8.730496	-0.047785	4.562490
232.118331	7165.175757	8.735501	-0.047839	4.564937
232.161902	7173.283507	8.740506	-0.047852	4.567439
232.193037	7181.276277	8.745511	-0.047863	4.569904
232.508924	7189.358522	8.750515	-0.047927	4.572395
232.626460	7197.351672	8.755520	-0.047955	4.574858
232.730502	7205.435442	8.760525	-0.047979	4.577346
232.680918	7213.346496	8.765530	-0.047975	4.579781
232.919210	7221.389936	8.770535	-0.048025	4.582255
233.294185	7229.386685	8.775539	-0.048100	4.584713
233.357390	7237.438403	8.780544	-0.048117	4.587186
233.542908	7245.447459	8.785549	-0.048157	4.589646
233.846373	7253.530884	8.790554	-0.048219	4.592126
233.972567	7261.520343	8.795559	-0.048247	4.594577
234.279099	7269.588221	8.800563	-0.048310	4.597050
234.469569	7277.499675	8.805568	-0.048350	4.599474
234.649131	7285.556134	8.810573	-0.048389	4.601941
234.622159	7293.526369	8.815578	-0.048389	4.604380
234.742113	7301.554830	8.820583	-0.048417	4.606836
235.043414	7309.552803	8.825587	-0.048478	4.609281
234.950083	7317.567546	8.830592	-0.048466	4.611730
235.319932	7325.659057	8.835597	-0.048540	4.614201
235.358093	7333.702862	8.840602	-0.048553	4.616656
235.245322	7341.605572	8.845607	-0.048537	4.619067
235.321974	7349.663016	8.850611	-0.048556	4.621524
235.488715	7357.632615	8.855616	-0.048593	4.623952
235.666681	7365.718243	8.860621	-0.048631	4.626415
235.673509	7373.679850	8.865626	-0.048638	4.628839
235.894254	7381.699273	8.870631	-0.048684	4.631278
235.909630	7389.770994	8.875635	-0.048692	4.633733
235.795706	7397.763576	8.880640	-0.048676	4.636162
236.118799	7405.740539	8.885645	-0.048742	4.638585
236.274036	7413.800671	8.890650	-0.048776	4.641032
236.416581	7421.751895	8.895655	-0.048808	4.643445
236.487551	7429.830705	8.900659	-0.048826	4.645895
236.606369	7437.764559	8.905664	-0.048853	4.648300
236.803153	7445.870803	8.910669	-0.048895	4.650756
236.822607	7453.877761	8.915674	-0.048904	4.653180
237.099458	7461.870119	8.920679	-0.048961	4.655599
237.273239	7469.901503	8.925683	-0.048999	4.658028
237.386158	7477.866700	8.930688	-0.049025	4.660436
237.540908	7485.931303	8.935693	-0.049059	4.662873
237.809638	7493.908616	8.940698	-0.049114	4.665282
237.645904	7501.925618	8.945703	-0.049089	4.667702
237.867476	7509.985657	8.950707	-0.049136	4.670133
238.034931	7518.058031	8.955712	-0.049172	4.672567
238.399667	7526.135618	8.960717	-0.049245	4.675001
238.215460	7534.073873	8.965722	-0.049216	4.677393
238.311824	7541.970885	8.970727	-0.049239	4.679770
238.546347	7550.028355	8.975731	-0.049288	4.682194
238.608130	7557.962476	8.980736	-0.049305	4.684580
238.769833	7566.084080	8.985741	-0.049341	4.687021
238.883839	7574.045483	8.990746	-0.049367	4.689413
238.977744	7582.046238	8.995751	-0.049390	4.691816
239.129147	7590.138898	9.000755	-0.049423	4.694244
239.550996	7598.186557	9.005760	-0.049507	4.696658
239.729910	7606.091088	9.010765	-0.049546	4.699027
239.837364	7614.135709	9.015770	-0.049571	4.701438
239.960253	7622.111632	9.020775	-0.049599	4.703826
240.003526	7630.162023	9.025779	-0.049612	4.706236
240.265751	7638.163922	9.030784	-0.049666	4.708630
240.381768	7646.254513	9.035789	-0.049693	4.711049
240.575171	7654.241265	9.040794	-0.049735	4.713436
240.636461	7662.196591	9.045799	-0.049751	4.715812
240.661899	7670.305222	9.050803	-0.049761	4.718233
240.909085	7678.232601	9.055808	-0.049812	4.720599
241.213388	7686.285991	9.060813	-0.049874	4.723000
241.337824	7694.306408	9.065818	-0.049903	4.725391
241.395898	7702.319866	9.070823	-0.049919	4.727779
241.696577	7710.353267	9.075827	-0.049980	4.730170
241.546775	7718.371940	9.080832	-0.049958	4.732558
241.693345	7726.393255	9.085837	-0.049990	4.734944
241.918618	7734.436253	9.090842	-0.050037	4.737335
241.986013	7742.398832	9.095847	-0.050055	4.739702
242.035788	7750.417804	9.100851	-0.050070	4.742084
242.025993	7758.390788	9.105856	-0.050073	4.744451
242.166741	7766.458788	9.110861	-0.050105	4.746845
242.262993	7774.492544	9.115866	-0.050128	4.749228
242.245069	7782.497531	9.120871	-0.050130	4.751601
242.473025	7790.552468	9.125875	-0.050177	4.753987
242.589236	7798.564943	9.130880	-0.050204	4.756360
242.751667	7806.486010	9.135885	-0.050240	4.758704
242.954920	7814.555067	9.140890	-0.050283	4.761091
243.052991	7822.510851	9.145895	-0.050306	4.763443
243.304078	7830.573889	9.150899	-0.050358	4.765826
243.255568	7838.582413	9.155904	-0.050355	4.768192
243.467167	7846.609790	9.160909	-0.050399	4.770562
243.493322	7854.663228	9.165914	-0.050409	4.772938
243.618425	7862.605528	9.170919	-0.050438	4.775281
243.888130	7870.693481	9.175923	-0.050494	4.777664
243.950154	7878.611161	9.180928	-0.050510	4.779998
243.969228	7886.659383	9.185933	-0.050519	4.782368
244.191894	7894.683636	9.190938	-0.050566	4.784730
244.212513	7902.649716	9.195943	-0.050575	4.787074
244.400961	7910.742055	9.200947	-0.050615	4.789453
244.756164	7918.773952	9.205952	-0.050687	4.791812
244.853245	7926.810472	9.210957	-0.050710	4.794173
245.119290	7934.821573	9.215962	-0.050765	4.796525
245.108563	7942.776222	9.220967	-0.050768	4.798860
245.242640	7950.796532	9.225971	-0.050798	4.801212
245.282764	7958.766158	9.230976	-0.050811	4.803549
245.301427	7966.789432	9.235981	-0.050820	4.805900
245.470496	7974.849914	9.240986	-0.050857	4.808261
245.710944	7982.831304	9.245991	-0.050907	4.810597
245.897382	7990.278036	9.250995	-0.050946	4.812775
245.739031	7994.736123	9.256000	-0.050920	4.814080

246.215612	7997.303362	9.261005	-0.051010	4.814829
246.481487	7998.640980	9.266010	-0.051060	4.815219
246.249767	7999.090942	9.271015	-0.051018	4.815352
246.383032	8000.097727	9.276019	-0.051043	4.815646
246.590128	8000.047710	9.281024	-0.051082	4.815630
246.583323	7999.995288	9.286029	-0.051080	4.815615
246.559342	8000.104869	9.291034	-0.051076	4.815647
246.674813	8000.020268	9.296039	-0.051098	4.815621
246.730769	8000.030789	9.301043	-0.051108	4.815624
246.474679	8000.062934	9.306048	-0.051060	4.815635
246.774760	8000.041118	9.311053	-0.051116	4.815627
246.784089	8000.094655	9.316058	-0.051118	4.815643
246.796251	8000.020121	9.321063	-0.051120	4.815621
246.905293	8000.043247	9.326067	-0.051141	4.815627
247.147980	8000.079221	9.331072	-0.051186	4.815636
247.164300	8000.089098	9.336077	-0.051189	4.815639
247.138806	8000.099364	9.341082	-0.051184	4.815642
247.232268	8000.007999	9.346087	-0.051202	4.815615
247.220457	8000.083614	9.351091	-0.051200	4.815637
247.098719	8000.098723	9.356096	-0.051177	4.815642
247.331751	8000.131338	9.361101	-0.051220	4.815651
247.391880	8000.102423	9.366106	-0.051232	4.815642
247.239948	8000.106365	9.371111	-0.051203	4.815644
247.434216	8000.136215	9.376115	-0.051240	4.815652
247.434170	8000.054007	9.381120	-0.051240	4.815628
247.423500	8000.020740	9.386125	-0.051238	4.815618
247.327462	8000.051213	9.391130	-0.051220	4.815627
247.371693	8000.020973	9.396135	-0.051228	4.815618
247.479219	8000.095323	9.401139	-0.051248	4.815640
247.336992	8000.088746	9.406144	-0.051222	4.815638
247.659527	8000.058755	9.411149	-0.051282	4.815628
247.683717	8000.110399	9.416154	-0.051286	4.815643
247.786763	8000.020256	9.421159	-0.051306	4.815616
247.608000	8000.085687	9.426163	-0.051272	4.815636
247.731667	8000.084496	9.431168	-0.051295	4.815635
247.699957	8000.074375	9.436173	-0.051290	4.815632
247.599653	8000.133607	9.441178	-0.051271	4.815650
247.660563	8000.053456	9.446183	-0.051282	4.815626
247.698915	8000.116008	9.451187	-0.051290	4.815645
247.467068	8000.070606	9.456192	-0.051246	4.815632
247.628249	8000.122340	9.461197	-0.051276	4.815647
247.728613	8000.162410	9.466202	-0.051295	4.815658
247.603892	8000.086718	9.471207	-0.051272	4.815636
247.642899	8000.149280	9.476211	-0.051279	4.815655
247.761286	8000.122379	9.481216	-0.051301	4.815646
247.812073	8000.105057	9.486221	-0.051311	4.815641
247.767452	8000.093658	9.491226	-0.051303	4.815638
247.760064	8000.065782	9.496231	-0.051301	4.815630
247.945151	8000.113634	9.501235	-0.051336	4.815643
247.722627	8000.061978	9.506240	-0.051294	4.815629
247.753737	8000.015509	9.511245	-0.051300	4.815615
247.859033	8000.090892	9.516250	-0.051320	4.815636
247.820347	8000.008056	9.521255	-0.051313	4.815612
247.862969	8000.122993	9.526259	-0.051321	4.815646
247.852695	8000.036347	9.531264	-0.051319	4.815621
247.823998	8000.071118	9.536269	-0.051313	4.815631
247.688290	8000.050766	9.541274	-0.051288	4.815626
247.769776	8000.057431	9.546279	-0.051303	4.815627
247.978423	8000.096057	9.551283	-0.051342	4.815637
247.853609	8000.069476	9.556288	-0.051319	4.815630
247.786701	8000.085476	9.561293	-0.051307	4.815635
247.973915	8000.117348	9.566298	-0.051342	4.815644
247.829794	8000.053084	9.571303	-0.051315	4.815626
247.959206	8000.094694	9.576307	-0.051339	4.815637
248.083576	8000.064687	9.581312	-0.051362	4.815628
248.058337	8000.032250	9.586317	-0.051357	4.815618
247.985985	8000.106883	9.591322	-0.051344	4.815641
247.924949	8000.047173	9.596327	-0.051333	4.815623
248.090527	8000.070152	9.601331	-0.051364	4.815629
248.103240	8000.070361	9.606336	-0.051366	4.815629
247.975185	7999.996750	9.611341	-0.051342	4.815608
248.138372	8000.104037	9.616346	-0.051373	4.815639
247.940559	8000.058120	9.621351	-0.051336	4.815626
248.084619	8000.128795	9.626355	-0.051363	4.815646
247.938125	8000.076237	9.631360	-0.051335	4.815632
247.893931	8000.047763	9.636365	-0.051327	4.815624
248.135517	8000.046352	9.641370	-0.051372	4.815622
248.148226	8000.010261	9.646375	-0.051375	4.815611
248.224746	8000.080907	9.651379	-0.051389	4.815632
247.975677	8000.068322	9.656384	-0.051343	4.815629
248.025967	8000.028571	9.661389	-0.051352	4.815617
248.127959	8000.112442	9.666394	-0.051371	4.815641
248.037635	8000.059729	9.671399	-0.051354	4.815626
248.054198	8000.104844	9.676403	-0.051357	4.815640
248.136811	8000.066686	9.681408	-0.051373	4.815628
248.363361	8000.057557	9.686413	-0.051415	4.815624
248.417842	8000.100086	9.691418	-0.051425	4.815636
248.190352	8000.082513	9.696423	-0.051383	4.815632
248.228696	8000.147200	9.701427	-0.051390	4.815651
248.292421	8000.123682	9.706432	-0.051402	4.815644
248.169916	8000.066175	9.711437	-0.051379	4.815628
248.329447	8000.132832	9.716442	-0.051409	4.815646
248.422288	8000.016898	9.721447	-0.051426	4.815612
248.365466	8000.070430	9.726451	-0.051416	4.815628
248.343289	8000.136270	9.731456	-0.051412	4.815647
248.392781	8000.047391	9.736461	-0.051421	4.815621
248.326521	8000.140275	9.741466	-0.051409	4.815649
248.168228	8000.068306	9.746471	-0.051379	4.815628
248.316161	8000.140113	9.751475	-0.051407	4.815649
248.298493	8000.107799	9.756480	-0.051403	4.815639
248.437335	8000.067350	9.761485	-0.051429	4.815627
248.292350	8000.085284	9.766490	-0.051402	4.815633
248.262133	8000.067713	9.771495	-0.051397	4.815628
248.293722	8000.108802	9.776499	-0.051403	4.815640
248.158142	8000.096993	9.781504	-0.051377	4.815637
248.537160	7999.999588	9.786509	-0.051448	4.815606
248.692339	8000.044821	9.791514	-0.051477	4.815619
248.385064	8000.015275	9.796519	-0.051420	4.815612
248.586229	8000.072999	9.801523	-0.051457	4.815628
248.623903	8000.052260	9.806528	-0.051464	4.815621
248.726583	8000.021901	9.811533	-0.051484	4.815612
248.553369	8000.133333	9.816538	-0.051451	4.815646
248.552684	8000.091685	9.821543	-0.051451	4.815633
248.413163	8000.142806	9.826547	-0.051425	4.815649
248.382014	8000.077174	9.831552	-0.051420	4.815630
248.370434	8000.056703	9.836557	-0.051417	4.815624
248.445869	8000.055797	9.841562	-0.051431	4.815623
248.338690	8000.058329	9.846567	-0.051412	4.815625
248.552560	8000.011626	9.851571	-0.051451	4.815610
248.519648	8000.045261	9.856576	-0.051445	4.815620
248.458654	8000.056018	9.861581	-0.051434	4.815623
248.764292	8000.115440	9.866586	-0.051491	4.815639
248.616942	8000.090627	9.871591	-0.051464	4.815633
248.729472	8000.060428	9.876595	-0.051485	4.815623
248.737274	8000.116079	9.881600	-0.051486	4.815640
248.665502	8000.107442	9.886605	-0.051473	4.815637
248.612909	8000.120470	9.891610	-0.051463	4.815641
248.694912	8000.032119	9.896615	-0.051478	4.815615
248.554257	8000.077884	9.901619	-0.051452	4.815629
248.514976	8000.082587	9.906624	-0.051445	4.815631
248.612323	8000.086308	9.911629	-0.051463	4.815631
248.621585	8000.144117	9.916634	-0.051465	4.815648
248.485334	8000.114146	9.921639	-0.051439	4.815640
248.651051	8000.127519	9.926643	-0.051470	4.815643
248.652331	8000.168116	9.931648	-0.051471	4.815655
248.779658	8000.131751	9.936653	-0.051494	4.815644
248.892513	8000.128250	9.941658	-0.051515	4.815642
248.849931	8000.050687	9.946663	-0.051508	4.815620
248.932088	8000.135306	9.951667	-0.051523	4.815644
248.928652	8000.153405	9.956672	-0.051522	4.815650
248.924583	8000.067925	9.961677	-0.051522	4.815625
248.875186	8000.110902	9.966682	-0.051512	4.815637
248.674357	8000.095897	9.971687	-0.051475	4.815634
248.866465	8000.084074	9.976691	-0.051511	4.815630
248.639977	8000.041960	9.981696	-0.051469	4.815618
248.780025	8000.016479	9.986701	-0.051495	4.815610
248.944586	8000.090692	9.991706	-0.051526	4.815631
248.606047	8000.041418	9.996711	-0.051462	4.815618
248.785409	8000.108398	10.001715	-0.051496	4.815637
248.830134	8000.094180	10.006720	-0.051504	4.815633
248.856734	8000.093548	10.011725	-0.051509	4.815632
248.922042	8000.089274	10.016730	-0.051522	4.815631
248.937123	8000.056424	10.021735	-0.051524	4.815621
249.003143	8000.080990	10.026739	-0.051537	4.815628
248.844779	8000.111518	10.031744	-0.051507	4.815638
248.933383	8000.068118	10.036749	-0.051524	4.815625
248.876487	8000.098160	10.041754	-0.051513	4.815634
248.826764	8000.092017	10.046759	-0.051504	4.815632
248.858578	8000.076521	10.051763	-0.051510	4.815627
248.782693	8000.105187	10.056768	-0.051496	4.815636
248.638654	8000.009960	10.061773	-0.051469	4.815609
248.557290	8000.047078	10.066778	-0.051454	4.815620
248.709178	8000.066633	10.071783	-0.051482	4.815625
248.777327	8000.126467	10.076787	-0.051495	4.815642
248.724903	8000.046609	10.081792	-0.051485	4.815619
249.052778	8000.070091	10.086797	-0.051546	4.815625
249.214267	8000.153865	10.091802	-0.051577	4.815648
248.872067	8000.057552	10.096807	-0.051513	4.815622
248.945669	8000.093985	10.101811	-0.051527	4.815632
249.096218	8000.107113	10.106816	-0.051555	4.815635
248.756815	8000.102667	10.111821	-0.051491	4.815636
248.869569	8000.172836	10.116826	-0.051513	4.815656
248.978757	8000.072114	10.121831	-0.051533	4.815626
249.085796	8000.113363	10.126835	-0.051553	4.815637
248.852853	8000.051924	10.131840	-0.051509	4.815620
248.854095	8000.065828	10.136845	-0.051510	4.815624
248.920773	8000.126706	10.141850	-0.051522	4.815642
248.771203	8000.054878	10.146855	-0.051494	4.815621
248.697107	8000.066489	10.151859	-0.051481	4.815625
248.698079	8000.060102	10.156864	-0.051481	4.815623
248.718789	8000.013463	10.161869	-0.051485	4.815610
248.960316	8000.021662	10.166874	-0.051530	4.815611
249.084353	8000.026884	10.171879	-0.051553	4.815612
249.093990	8000.090039	10.176883	-0.051555	4.815630
248.842847	8000.056065	10.181888	-0.051508	4.815621
248.795396	8000.022199	10.186893	-0.051499	4.815612
248.986753	8000.097915	10.191898	-0.051535	4.815633
249.035852	8000.046399	10.196903	-0.051544	4.815618
248.891328	8000.045121	10.201907	-0.051517	4.815618
248.878019	8000.114309	10.206912	-0.051515	4.815638
248.934244	8000.070383	10.211917	-0.051525	4.815625
249.022827	8000.108128	10.216922	-0.051542	4.815636
248.980200	8000.043376	10.221927	-0.051534	4.815617
249.022133	8000.078227	10.226931	-0.051542	4.815627
248.853118	8000.082957	10.231936	-0.051510	4.815629
248.811108	8000.006471	10.236941	-0.051502	4.815607
248.983435	8000.085082	10.241946	-0.051535	4.815629
249.023227	8000.057972	10.246951	-0.051542	4.815621
248.837517	8000.064566	10.251955	-0.051508	4.815624
248.903757	8000.145724	10.256960	-0.051520	4.815647
249.017174	8000.056815	10.261965	-0.051541	4.815621
249.059163	8000.075652	10.266970	-0.051549	4.815626
248.788163	8000.063777	10.271975	-0.051498	4.815624
249.139414	8000.085505	10.276979	-0.051564	4.815629
249.032467	8000.119004	10.281984	-0.051544	4.815639
249.034408	8000.015471	10.286989	-0.051544	4.815609
249.120348	8000.082002	10.291994	-0.051560	4.815628
249.136050	8000.028875	10.296999	-0.051563	4.815612
249.095722	8000.063457	10.302003	-0.051556	4.815622
249.021382	8000.092148	10.307008	-0.051542	4.815631
249.218097	8000.036624	10.312013	-0.051579	4.815614
249.163895	8000.105148	10.317018	-0.051569	4.815634
248.921140	8000.085190	10.322023	-0.051524	4.815630
249.159703	8000.116831	10.327027	-0.051568	4.815638
249.031304	8000.111544	10.332032	-0.051544	4.815637
249.000705	8000.053394	10.337037	-0.051539	4.815620
248.972431	8000.109526	10.342042	-0.051533	4.815636
248.938164	8000.036369	10.347047	-0.051527	4.815615
249.131601	8000.056599	10.352051	-0.051563	4.815620
248.979289	8000.072278	10.357056	-0.051535	4.815626
248.928683	8000.049037	10.362061	-0.051525	4.815619
249.177485	8000.111808	10.367066	-0.051572	4.815636
249.011513	8000.063202	10.372071	-0.051541	4.815623
249.033225	8000.044340	10.377075	-0.051545	4.815617
249.064908	8000.111056	10.382080	-0.051551	4.815636
248.936483	8000.045977	10.387085	-0.051527	4.815618
249.073268	8000.106927	10.392090	-0.051553	4.815635
249.103947	8000.071127	10.397095	-0.051558	4.815625
249.348139	8000.118876	10.402099	-0.051604	4.815637
249.214040	8000.147663	10.407104	-0.051579	4.815646
249.316820	8000.043633	10.412109	-0.051598	4.815616
249.468458	8000.037559	10.417114	-0.051626	4.815613
249.264433	8000.089768	10.422119	-0.051588	4.815629
249.306760	8000.132100	10.427123	-0.051596	4.815641
249.461025	8000.138882	10.432128	-0.051625	4.815643
249.182143	8000.088440	10.437133	-0.051573	4.815629
249.173143	8000.184391	10.442138	-0.051572	4.815657
249.207011	8000.150778	10.447143	-0.051578	4.815647
249.230475	8000.088168	10.452147	-0.051582	4.815629
249.023130	8000.168083	10.457152	-0.051544	4.815653
248.912713	8000.085145	10.462157	-0.051523	4.815630
249.116790	8000.052163	10.467162	-0.051561	4.815619
248.943665	8000.078181	10.472167	-0.051529	4.815627
249.043030	8000.111830	10.477171	-0.051548	4.815637
249.006035	8000.099488	10.482176	-0.051541	4.815633
248.789181	8000.067139	10.487181	-0.051500	4.815625
249.013500	8000.103886	10.492186	-0.051542	4.815635
249.194853	8000.096160	10.497191	-0.051576	4.815631
249.244027	8000.068134	10.502195	-0.051585	4.815623
249.123095	8000.092865	10.507200	-0.051563	4.815631
249.204176	8000.005566	10.512205	-0.051578	4.815605
249.284567	8000.048517	10.517210	-0.051593	4.815617
249.180086	8000.058567	10.522215	-0.051573	4.815621
249.121513	8000.103530	10.527219	-0.051563	4.815634
248.963100	8000.095620	10.532224	-0.051533	4.815632
249.143749	8000.086814	10.537229	-0.051567	4.815629
249.130197	8000.173082	10.542234	-0.051564	4.815654
248.933372	8000.114365	10.547239	-0.051528	4.815638
249.040315	8000.138528	10.552243	-0.051548	4.815645
248.986499	8000.186772	10.557248	-0.051538	4.815659
249.021137	8000.097650	10.562253	-0.051544	4.815633
249.150530	8000.114705	10.567258	-0.051568	4.815637
248.886510	8000.099740	10.572263	-0.051519	4.815634
249.060453	8000.023560	10.577267	-0.051551	4.815611
249.356817	8000.112729	10.582272	-0.051607	4.815636
249.130281	8000.002279	10.587277	-0.051565	4.815604
249.037911	8000.174818	10.592282	-0.051547	4.815655
249.252975	8000.093968	10.597287	-0.051588	4.815631
249.149216	8000.114706	10.602291	-0.051568	4.815637
249.145859	8000.140280	10.607296	-0.051568	4.815645
249.246165	8000.039413	10.612301	-0.051586	4.815615
249.415898	8000.147880	10.617306	-0.051618	4.815646
249.317147	8000.115314	10.622311	-0.051600	4.815636
249.162596	8000.104263	10.627315	-0.051571	4.815634
249.212863	8000.138183	10.632320	-0.051580	4.815644
249.115725	8000.101373	10.637325	-0.051562	4.815633
249.109557	8000.143984	10.642330	-0.051561	4.815646
249.156752	8000.127671	10.647335	-0.051570	4.815641
249.227920	8000.148050	10.652339	-0.051583	4.815646
249.165803	8000.172669	10.657344	-0.051572	4.815654
249.390904	8000.053544	10.662349	-0.051614	4.815618
249.459944	8000.090972	10.667354	-0.051627	4.815629
249.298117	8000.032823	10.672359	-0.051596	4.815612
249.386513	8000.094056	10.677363	-0.051613	4.815630
249.302529	8000.086287	10.682368	-0.051597	4.815628
249.300541	8000.042482	10.687373	-0.051597	4.815615
249.303186	8000.089508	10.692378	-0.051598	4.815629
249.287452	8000.065766	10.697383	-0.051595	4.815622
249.272714	8000.071936	10.702387	-0.051592	4.815624
249.144832	8000.098689	10.707392	-0.051568	4.815632
249.054077	8000.011800	10.712397	-0.051551	4.815607
249.329137	8000.147603	10.717402	-0.051603	4.815646
249.295600	8000.075524	10.722407	-0.051596	4.815625
249.212009	8000.105132	10.727411	-0.051581	4.815634
249.200100	8000.118822	10.732416	-0.051579	4.815638
249.309688	8000.075763	10.737421	-0.051599	4.815625
249.464137	8000.127392	10.742426	-0.051628	4.815639
249.346314	8000.131886	10.747431	-0.051606	4.815641
249.559810	8000.102261	10.752435	-0.051646	4.815631
249.484909	8000.096775	10.757440	-0.051632	4.815630
249.316590	8000.059876	10.762445	-0.051601	4.815620
249.522721	8000.076042	10.767450	-0.051639	4.815624
249.243346	8000.121687	10.772455	-0.051587	4.815639
249.368683	8000.077816	10.777459	-0.051610	4.815625
249.283284	8000.099921	10.782464	-0.051595	4.815632
249.318817	8000.032168	10.787469	-0.051601	4.815612
249.352858	8000.046605	10.792474	-0.051608	4.815616
249.265756	8000.098578	10.797479	-0.051591	4.815632
249.602835	8000.157447	10.802483	-0.051654	4.815647
249.608302	8000.139388	10.807488	-0.051655	4.815642
249.310903	8000.117473	10.812493	-0.051600	4.815637
249.203622	8000.081566	10.817498	-0.051580	4.815627
249.128269	8000.093157	10.822503	-0.051566	4.815631
249.244526	8000.135623	10.827507	-0.051588	4.815643
249.403765	8000.136079	10.832512	-0.051617	4.815642
249.199556	8000.076174	10.837517	-0.051579	4.815626
249.276791	8000.069959	10.842522	-0.051594	4.815623
249.213326	8000.037967	10.847527	-0.051582	4.815614
249.151872	8000.157623	10.852531	-0.051571	4.815650
249.184517	8000.174173	10.857536	-0.051577	4.815654
248.974013	8000.101353	10.862541	-0.051538	4.815634
249.131927	8000.106058	10.867546	-0.051567	4.815635
249.233581	8000.076750	10.872551	-0.051586	4.815626
249.235444	8000.040482	10.877555	-0.051586	4.815615
249.254665	8000.127282	10.882560	-0.051590	4.815640
249.344785	8000.077500	10.887565	-0.051607	4.815625
249.258660	8000.104932	10.892570	-0.051591	4.815634
249.240958	8000.082225	10.897575	-0.051588	4.815627
249.325813	8000.062253	10.902579	-0.051603	4.815621
249.496350	8000.098128	10.907584	-0.051635	4.815631
249.332993	8000.073054	10.912589	-0.051605	4.815624
249.549790	8000.073378	10.917594	-0.051645	4.815623
249.410351	8000.063641	10.922599	-0.051619	4.815621
249.363196	8000.087435	10.927603	-0.051611	4.815628
249.452160	8000.046176	10.932608	-0.051627	4.815616
249.474943	7999.983554	10.937613	-0.051631	4.815597
249.539039	8000.138351	10.942618	-0.051643	4.815642
249.227839	8000.107670	10.947623	-0.051585	4.815635
249.490966	8000.052158	10.952627	-0.051634	4.815617
249.446278	8000.052503	10.957632	-0.051626	4.815617
249.088492	8000.068045	10.962637	-0.051560	4.815624
249.282314	8000.082943	10.967642	-0.051596	4.815627
249.350044	8000.068032	10.972647	-0.051608	4.815622
249.322154	8000.036618	10.977651	-0.051603	4.815613
249.294778	8000.068208	10.982656	-0.051598	4.815623
249.231164	8000.004182	10.987661	-0.051586	4.815604
249.245093	8000.098371	10.992666	-0.051589	4.815632
249.138284	8000.062471	10.997671	-0.051569	4.815622
249.452237	8000.044088	11.002675	-0.051628	4.815615
249.402414	8000.059297	11.007680	-0.051618	4.815620
249.119169	8000.028004	11.012685	-0.051566	4.815612
249.411795	8000.070133	11.017690	-0.051620	4.815623
249.468147	8000.034750	11.022695	-0.051631	4.815612
249.509897	8000.009807	11.027699	-0.051639	4.815605
249.262250	8000.054900	11.032704	-0.051592	4.815619
249.388522	8000.005705	11.037709	-0.051616	4.815604
249.620499	8000.092761	11.042714	-0.051659	4.815628
249.247844	8000.112332	11.047719	-0.051590	4.815636
249.346119	8000.135287	11.052723	-0.051608	4.815642
249.307235	8000.153877	11.057728	-0.051601	4.815648
249.256704	8000.064439	11.062733	-0.051592	4.815622
249.259642	8000.117875	11.067738	-0.051592	4.815637
249.283846	8000.030720	11.072743	-0.051597	4.815612
249.325353	8000.052752	11.077747	-0.051605	4.815618
249.336946	8000.065756	11.082752	-0.051607	4.815622
249.434162	8000.032105	11.087757	-0.051625	4.815611
249.498999	8000.050246	11.092762	-0.051637	4.815616
249.289663	8000.062862	11.097767	-0.051598	4.815621
249.395337	8000.067786	11.102771	-0.051618	4.815622
249.375726	8000.066403	11.107776	-0.051614	4.815622
249.291929	8000.042622	11.112781	-0.051599	4.815615
249.293455	8000.065072	11.117786	-0.051599	4.815622
249.484239	8000.042551	11.122791	-0.051634	4.815614
249.352456	7999.993433	11.127795	-0.051610	4.815601
249.637964	8000.085630	11.132800	-0.051663	4.815626
249.646073	8000.053734	11.137805	-0.051665	4.815617
249.787278	8000.079523	11.142810	-0.051691	4.815624
249.306254	8000.050352	11.147815	-0.051602	4.815617
249.718442	8000.072004	11.152819	-0.051678	4.815622
249.503845	8000.128311	11.157824	-0.051638	4.815639
249.382044	8000.079354	11.162829	-0.051616	4.815626
249.399954	8000.106342	11.167834	-0.051619	4.815633
249.436483	8000.038605	11.172839	-0.051626	4.815613
249.359980	8000.004266	11.177843	-0.051612	4.815604
249.344991	8000.014702	11.182848	-0.051609	4.815607
249.493556	8000.010714	11.187853	-0.051637	4.815605
249.577831	8000.036645	11.192858	-0.051652	4.815612
249.328751	8000.042209	11.197863	-0.051606	4.815615
249.362657	8000.042763	11.202867	-0.051612	4.815615
249.666753	8000.071200	11.207872	-0.051669	4.815622
249.480604	7999.978489	11.212877	-0.051634	4.815596
249.228976	8000.090783	11.217882	-0.051588	4.815630
249.338471	8000.051993	11.222887	-0.051608	4.815618
249.547925	8000.039385	11.227891	-0.051647	4.815613
249.442932	8000.091068	11.232896	-0.051628	4.815629
249.537625	8000.052037	11.237901	-0.051645	4.815617
249.556400	8000.086512	11.242906	-0.051649	4.815627
249.324044	8000.021879	11.247911	-0.051606	4.815609
249.288476	8000.013830	11.252915	-0.051599	4.815607
249.534505	8000.075489	11.257920	-0.051645	4.815624
249.345179	8000.014758	11.262925	-0.051610	4.815607
249.405507	8000.086211	11.267930	-0.051621	4.815627
249.333775	8000.050882	11.272935	-0.051608	4.815617
249.385734	8000.028240	11.277939	-0.051617	4.815611
249.450672	8000.047450	11.282944	-0.051629	4.815616
249.386751	7999.996232	11.287949	-0.051618	4.815601
249.535006	8000.050963	11.292954	-0.051645	4.815616
249.385601	8000.111533	11.297959	-0.051617	4.815635
249.247764	8000.093280	11.302963	-0.051592	4.815630
249.553574	8000.111067	11.307968	-0.051649	4.815634
249.670860	8000.046778	11.312973	-0.051671	4.815615
249.494495	8000.115452	11.317978	-0.051638	4.815636
249.430514	8000.088790	11.322983	-0.051626	4.815628
249.633112	8000.058987	11.327987	-0.051664	4.815618
249.507397	8000.110333	11.332992	-0.051640	4.815634
249.412930	8000.051143	11.337997	-0.051623	4.815617
249.577143	8000.105067	11.343002	-0.051653	4.815632
249.550770	8000.089693	11.348007	-0.051649	4.815628
249.526454	8000.070082	11.353011	-0.051644	4.815622
249.704106	8000.131698	11.358016	-0.051677	4.815639
249.787014	8000.009193	11.363021	-0.051693	4.815603
249.624481	8000.040722	11.368026	-0.051662	4.815613
249.304894	8000.033395	11.373031	-0.051603	4.815612
249.601352	8000.036081	11.378035	-0.051658	4.815612
249.723665	8000.137372	11.383040	-0.051681	4.815641
249.559073	8000.053552	11.388045	-0.051650	4.815617
249.916719	8000.089266	11.393050	-0.051717	4.815626
249.638268	8000.117842	11.398055	-0.051665	4.815636
249.441518	8000.060193	11.403059	-0.051629	4.815620
249.557023	8000.085563	11.408064	-0.051650	4.815626
249.769662	8000.001470	11.413069	-0.051690	4.815601
249.711295	8000.032556	11.418074	-0.051679	4.815610
249.528990	8000.024258	11.423079	-0.051645	4.815609
249.532156	8000.020041	11.428083	-0.051646	4.815607
249.692098	8000.036525	11.433088	-0.051676	4.815611
249.553834	7999.990504	11.438093	-0.051650	4.815599
249.703321	8000.082626	11.443098	-0.051678	4.815625
249.505167	7999.999329	11.448103	-0.051641	4.815601
249.568241	8000.004629	11.453107	-0.051653	4.815603
249.696306	8000.086793	11.458112	-0.051677	4.815626
249.679198	7999.998965	11.463117	-0.051673	4.815601
249.658147	8000.087247	11.468122	-0.051670	4.815626
249.498412	8000.007778	11.473127	-0.051640	4.815604
249.859176	7999.991223	11.478131	-0.051707	4.815597
249.888673	8000.068582	11.483136	-0.051713	4.815620
249.514102	8000.021923	11.488141	-0.051643	4.815608
249.846948	8000.092468	11.493146	-0.051705	4.815627
249.895030	8000.069763	11.498151	-0.051714	4.815620
249.810226	8000.056643	11.503155	-0.051698	4.815617
249.649115	8000.056162	11.508160	-0.051668	4.815617
249.680019	8000.031043	11.513165	-0.051674	4.815610
249.711504	8000.102028	11.518170	-0.051680	4.815631
249.770577	8000.082705	11.523175	-0.051691	4.815625
249.913861	8000.053006	11.528179	-0.051718	4.815615
249.953485	8000.021621	11.533184	-0.051725	4.815606
249.593933	8000.047811	11.538189	-0.051658	4.815615
249.621338	8000.034380	11.543194	-0.051663	4.815611
249.709280	8000.008052	11.548199	-0.051680	4.815603
249.783330	7999.991107	11.553203	-0.051693	4.815598
249.600428	8000.093842	11.558208	-0.051659	4.815629
249.696996	8000.013200	11.563213	-0.051677	4.815605
249.767266	8000.035701	11.568218	-0.051691	4.815611
249.488498	8000.065339	11.573223	-0.051639	4.815621
249.572757	8000.035748	11.578227	-0.051654	4.815612
249.845983	8000.134154	11.583232	-0.051705	4.815639
249.762014	8000.084744	11.588237	-0.051690	4.815625
249.899090	8000.077366	11.593242	-0.051715	4.815622
249.994704	8000.126972	11.598247	-0.051733	4.815636
249.658268	8000.053171	11.603251	-0.051671	4.815616
249.841466	8000.161858	11.608256	-0.051705	4.815647
250.142759	8000.115509	11.613261	-0.051761	4.815632
250.020580	8000.129541	11.618266	-0.051738	4.815637
249.703534	8000.137202	11.623271	-0.051679	4.815641
249.823537	8000.090041	11.628275	-0.051702	4.815626
249.842998	8000.160831	11.633280	-0.051705	4.815647
249.582686	8000.096809	11.638285	-0.051657	4.815630
249.659746	8000.125826	11.643290	-0.051671	4.815638
249.798992	8000.074707	11.648295	-0.051697	4.815622
249.884558	8000.053679	11.653299	-0.051713	4.815616
249.990924	8000.145102	11.658304	-0.051733	4.815642
249.882588	8000.081415	11.663309	-0.051713	4.815624
249.988157	8000.116234	11.668314	-0.051732	4.815633
249.824464	8000.142405	11.673319	-0.051702	4.815642
249.632156	8000.065608	11.678323	-0.051666	4.815620
249.748454	8000.103805	11.683328	-0.051688	4.815631
249.601276	8000.052300	11.688333	-0.051661	4.815616
249.716736	8000.097957	11.693338	-0.051682	4.815629
249.751892	8000.130564	11.698343	-0.051689	4.815639
249.724684	8000.069264	11.703347	-0.051684	4.815621
249.787851	8000.130088	11.708352	-0.051696	4.815638
249.967291	8000.032642	11.713357	-0.051729	4.815609
249.928403	8000.044825	11.718362	-0.051722	4.815613
249.668126	8000.143099	11.723367	-0.051673	4.815643
249.626480	8000.097581	11.728371	-0.051666	4.815630
249.824966	8000.149927	11.733376	-0.051703	4.815644
249.685403	8000.108155	11.738381	-0.051677	4.815632
249.835806	8000.073233	11.743386	-0.051705	4.815621
249.810638	8000.102723	11.748391	-0.051700	4.815630
249.865040	8000.040615	11.753395	-0.051710	4.815612
249.741697	8000.057832	11.758400	-0.051687	4.815617
249.657964	7999.993479	11.763405	-0.051672	4.815599
249.823277	8000.062368	11.768410	-0.051703	4.815618
249.801783	8000.052413	11.773415	-0.051699	4.815616
249.885781	8000.045240	11.778419	-0.051714	4.815613
249.838170	8000.124549	11.783424	-0.051705	4.815636
249.782291	8000.088408	11.788429	-0.051695	4.815626
249.941384	8000.093134	11.793434	-0.051725	4.815627
249.666571	8000.122836	11.798439	-0.051674	4.815637
249.878724	8000.102799	11.803443	-0.051713	4.815630
249.711984	8000.131055	11.808448	-0.051682	4.815639
249.718910	8000.070311	11.813453	-0.051683	4.815621
249.815299	8000.100710	11.818458	-0.051701	4.815630
249.775289	8000.096859	11.823463	-0.051694	4.815629
249.621999	8000.047391	11.828467	-0.051665	4.815615
250.019116	8000.085882	11.833472	-0.051739	4.815624
249.971557	7999.993287	11.838477	-0.051731	4.815597
249.766914	8000.057231	11.843482	-0.051693	4.815617
249.890016	8000.090199	11.848487	-0.051716	4.815626
250.057357	8000.028860	11.853491	-0.051747	4.815607
249.877366	8000.115626	11.858496	-0.051713	4.815634
249.938183	8000.024793	11.863501	-0.051725	4.815607
250.202351	8000.068598	11.868506	-0.051774	4.815618
250.087197	8000.081677	11.873511	-0.051752	4.815623
250.068656	8000.051482	11.878515	-0.051749	4.815614
249.961963	8000.064699	11.883520	-0.051729	4.815618
249.875158	8000.062223	11.888525	-0.051713	4.815618
250.069220	8000.053637	11.893530	-0.051749	4.815615
249.983178	8000.132321	11.898535	-0.051733	4.815638
250.023217	8000.094537	11.903539	-0.051741	4.815627
250.016971	8000.174519	11.908544	-0.051740	4.815650
249.997894	8000.087725	11.913549	-0.051736	4.815625
250.132736	8000.074973	11.918554	-0.051761	4.815621
250.009143	8000.059086	11.923559	-0.051738	4.815616
249.872743	8000.064346	11.928563	-0.051713	4.815619
249.994834	8000.094095	11.933568	-0.051736	4.815627
249.848195	8000.045802	11.938573	-0.051708	4.815613
249.837967	8000.088348	11.943578	-0.051707	4.815626
249.824422	8000.105215	11.948583	-0.051704	4.815631
249.856385	8000.024590	11.953587	-0.051710	4.815607
249.841164	8000.041430	11.958592	-0.051707	4.815612
249.755043	8000.060320	11.963597	-0.051691	4.815618
249.969617	8000.044593	11.968602	-0.051731	4.815612
249.972888	8000.092697	11.973607	-0.051732	4.815626
249.930280	8000.052501	11.978611	-0.051724	4.815615
250.002583	8000.100661	11.983616	-0.051738	4.815629
249.979981	8000.055452	11.988621	-0.051733	4.815616
249.973431	8000.057484	11.993626	-0.051732	4.815616
249.966332	8000.081930	11.998631	-0.051731	4.815623
249.886333	8000.050736	12.003635	-0.051716	4.815615
249.867479	8000.125174	12.008640	-0.051713	4.815636
249.913307	8000.080010	12.013645	-0.051721	4.815623
249.813725	8000.067717	12.018650	-0.051703	4.815620
250.067411	8000.134841	12.023655	-0.051750	4.815638
249.972757	8000.054293	12.028659	-0.051732	4.815615
250.072818	8000.113581	12.033664	-0.051751	4.815632
250.115495	8000.115346	12.038669	-0.051759	4.815632
250.092082	8000.114968	12.043674	-0.051755	4.815632
250.119936	8000.055631	12.048679	-0.051760	4.815615
250.258988	8000.037608	12.053683	-0.051786	4.815609
250.235613	8000.048977	12.058688	-0.051781	4.815612
249.889941	8000.061511	12.063693	-0.051717	4.815618
250.000626	8000.109227	12.068698	-0.051738	4.815631
250.025512	8000.096822	12.073703	-0.051742	4.815627
250.047933	8000.115341	12.078707	-0.051747	4.815633
250.166930	8000.190954	12.083712	-0.051769	4.815654
250.212608	8000.113755	12.088717	-0.051777	4.815631
250.198918	8000.104993	12.093722	-0.051775	4.815629
250.125229	8000.097392	12.098727	-0.051761	4.815627
250.292667	8000.038189	12.103731	-0.051792	4.815609
250.275942	8000.043259	12.108736	-0.051789	4.815611
250.110333	8000.062992	12.113741	-0.051759	4.815617
250.101773	8000.047908	12.118746	-0.051757	4.815613
250.175528	8000.040568	12.123751	-0.051771	4.815610
249.997523	8000.008849	12.128755	-0.051738	4.815602
250.185852	8000.058894	12.133760	-0.051773	4.815616
250.222990	7999.981557	12.138765	-0.051780	4.815593
250.088484	8000.007134	12.143770	-0.051755	4.815601
249.915678	8000.106830	12.148775	-0.051723	4.815631
250.038623	8000.050107	12.153779	-0.051746	4.815614
250.136539	8000.063448	12.158784	-0.051764	4.815617
250.045250	8000.054493	12.163789	-0.051747	4.815615
250.141735	8000.012288	12.168794	-0.051765	4.815602
250.055368	8000.034377	12.173799	-0.051749	4.815609
250.118430	8000.057828	12.178803	-0.051761	4.815616
250.039791	8000.080043	12.183808	-0.051746	4.815622
250.113526	8000.018249	12.188813	-0.051760	4.815604
250.003069	8000.044217	12.193818	-0.051739	4.815612
249.878199	8000.093441	12.198823	-0.051716	4.815627
249.910821	8000.011760	12.203827	-0.051722	4.815603
250.107432	8000.053398	12.208832	-0.051759	4.815614
249.927361	8000.042999	12.213837	-0.051725	4.815612
249.944026	8000.074238	12.218842	-0.051728	4.815621
249.897346	8000.059602	12.223847	-0.051720	4.815617
249.782899	8000.035322	12.228851	-0.051698	4.815611
249.816588	8000.090327	12.233856	-0.051705	4.815626
249.970400	8000.046919	12.238861	-0.051733	4.815613
250.124085	8000.039811	12.243866	-0.051762	4.815610
250.058457	8000.049425	12.248871	-0.051750	4.815613
249.992968	8000.034483	12.253875	-0.051738	4.815609
250.064893	8000.138158	12.258880	-0.051751	4.815639
249.757824	8000.019989	12.263885	-0.051694	4.815606
249.771693	7999.996728	12.268890	-0.051697	4.815599
250.063390	8000.042047	12.273895	-0.051751	4.815611
250.076765	8000.017710	12.278899	-0.051754	4.815604
250.061529	8000.031346	12.283904	-0.051751	4.815608
249.909635	7999.979765	12.288909	-0.051722	4.815594
250.096672	7999.987080	12.293914	-0.051757	4.815595
250.141420	8000.033723	12.298919	-0.051766	4.815608
250.010046	7999.995287	12.303923	-0.051741	4.815598
250.227966	8000.049017	12.308928	-0.051782	4.815612
250.269925	7999.986706	12.313933	-0.051790	4.815594
250.254487	7999.998204	12.318938	-0.051787	4.815597
250.296832	8000.035199	12.323943	-0.051795	4.815608
250.370436	8000.018247	12.328947	-0.051809	4.815603
250.207226	8000.011326	12.333952	-0.051778	4.815601
250.172047	8000.019299	12.338957	-0.051772	4.815604
250.198572	8000.040020	12.343962	-0.051777	4.815610
249.941083	8000.060395	12.348967	-0.051729	4.815617
250.018909	7999.997600	12.353971	-0.051743	4.815598
250.306056	8000.055659	12.358976	-0.051797	4.815614
250.251326	8000.043027	12.363981	-0.051787	4.815611
250.188712	8000.045215	12.368986	-0.051775	4.815611
250.250135	8000.072911	12.373991	-0.051787	4.815619
250.181072	8000.001321	12.378995	-0.051774	4.815599
250.234049	8000.039556	12.384000	-0.051784	4.815610
250.134437	8000.028330	12.389005	-0.051765	4.815607
250.362966	8000.014965	12.394010	-0.051808	4.815602
250.172350	8000.023614	12.399015	-0.051772	4.815605
250.149745	8000.009370	12.404019	-0.051768	4.815601
250.310515	8000.058967	12.409024	-0.051798	4.815615
250.122001	7999.998248	12.414029	-0.051763	4.815598
250.071759	7999.983554	12.419034	-0.051754	4.815594
250.188753	8000.039914	12.424039	-0.051775	4.815610
250.127269	8000.041053	12.429043	-0.051764	4.815611
250.129274	8000.113695	12.434048	-0.051765	4.815632
249.958481	8000.035112	12.439053	-0.051733	4.815610
250.172284	8000.059946	12.444058	-0.051773	4.815616
250.157397	8000.108823	12.449063	-0.051770	4.815630
250.014309	8000.033894	12.454067	-0.051743	4.815609
250.275472	8000.060566	12.459072	-0.051792	4.815616
250.182181	8000.077204	12.464077	-0.051775	4.815621
250.076120	8000.037044	12.469082	-0.051755	4.815610
250.142035	8000.084032	12.474087	-0.051767	4.815623
250.056217	8000.031388	12.479091	-0.051751	4.815608
250.215343	8000.048927	12.484096	-0.051781	4.815612
249.933427	8000.042211	12.489101	-0.051728	4.815612
250.021317	8000.068202	12.494106	-0.051745	4.815619
250.072917	8000.103211	12.499111	-0.051755	4.815629
250.069368	8000.048702	12.504115	-0.051754	4.815613
250.143614	8000.133197	12.509120	-0.051768	4.815637
250.302834	8000.138992	12.514125	-0.051797	4.815638
250.124949	8000.050684	12.519130	-0.051764	4.815613
250.180545	8000.096436	12.524135	-0.051775	4.815626
250.114779	8000.048390	12.529139	-0.051763	4.815613
250.089446	8000.065065	12.534144	-0.051758	4.815618
249.891847	8000.025552	12.539149	-0.051721	4.815607
250.052519	8000.035642	12.544154	-0.051751	4.815609
250.019308	8000.042580	12.549159	-0.051745	4.815611
249.924205	8000.037833	12.554163	-0.051727	4.815611
250.224162	8000.058730	12.559168	-0.051783	4.815615
250.315679	8000.074102	12.564173	-0.051800	4.815619
250.166550	8000.048190	12.569178	-0.051772	4.815612
250.129209	8000.127666	12.574183	-0.051766	4.815636
250.245447	8000.108205	12.579187	-0.051787	4.815630
250.281733	8000.079970	12.584192	-0.051794	4.815621
250.166395	8000.048201	12.589197	-0.051773	4.815612
250.213534	8000.107696	12.594202	-0.051781	4.815630
250.278595	8000.151467	12.599207	-0.051794	4.815642
250.055206	8000.054945	12.604211	-0.051752	4.815615
250.212236	8000.035079	12.609216	-0.051781	4.815608
250.271628	8000.044590	12.614221	-0.051792	4.815611
250.187625	8000.027211	12.619226	-0.051777	4.815606
250.149587	8000.073576	12.624231	-0.051770	4.815620
250.215232	8000.047953	12.629235	-0.051782	4.815612
250.296374	8000.085579	12.634240	-0.051797	4.815623
250.270382	8000.065941	12.639245	-0.051792	4.815617
250.254349	8000.030448	12.644250	-0.051789	4.815607
250.231827	8000.067456	12.649255	-0.051785	4.815618
250.287232	8000.018176	12.654259	-0.051796	4.815603
250.217286	8000.056548	12.659264	-0.051783	4.815615
250.109156	8000.023829	12.664269	-0.051762	4.815606
249.958804	8000.018185	12.669274	-0.051735	4.815605
250.107123	8000.017396	12.674279	-0.051762	4.815604
250.164781	7999.998050	12.679283	-0.051773	4.815598
250.490153	8000.018292	12.684288	-0.051834	4.815602
250.260705	7999.946230	12.689293	-0.051791	4.815582
250.322645	8000.005966	12.694298	-0.051802	4.815599
250.306818	8000.061234	12.699303	-0.051800	4.815616
250.130292	8000.056231	12.704307	-0.051767	4.815615
250.165979	8000.094186	12.709312	-0.051773	4.815626
250.042588	8000.065489	12.714317	-0.051750	4.815618
250.178406	8000.043143	12.719322	-0.051776	4.815611
250.057298	8000.050787	12.724327	-0.051753	4.815614
250.138369	7999.981638	12.729331	-0.051768	4.815593
250.342895	8000.044760	12.734336	-0.051807	4.815611
250.190810	8000.055103	12.739341	-0.051778	4.815614
250.303299	8000.051597	12.744346	-0.051799	4.815613
250.165484	8000.116627	12.749351	-0.051774	4.815632
250.063809	8000.006068	12.754355	-0.051755	4.815601
250.297216	8000.088879	12.759360	-0.051798	4.815624
250.295542	8000.037603	12.764365	-0.051798	4.815609
250.146986	8000.012768	12.769370	-0.051770	4.815602
250.140897	8000.077805	12.774375	-0.051769	4.815621
250.070464	8000.045698	12.779379	-0.051756	4.815612
250.312309	8000.052837	12.784384	-0.051801	4.815613
250.224819	8000.081315	12.789389	-0.051785	4.815622
250.148391	8000.062991	12.794394	-0.051771	4.815617
250.095540	8000.112319	12.799399	-0.051761	4.815631
249.958803	8000.034290	12.804403	-0.051736	4.815609
250.041850	8000.081556	12.809408	-0.051751	4.815623
250.253052	8000.078587	12.814413	-0.051790	4.815621
250.254017	8000.089283	12.819418	-0.051791	4.815624
250.105690	8000.089010	12.824423	-0.051763	4.815625
250.093470	7999.996990	12.829427	-0.051761	4.815598
250.165825	8000.089995	12.834432	-0.051774	4.815625
250.023456	8000.071667	12.839437	-0.051748	4.815620
250.254343	8000.028444	12.844442	-0.051791	4.815606
250.276569	8000.050164	12.849447	-0.051795	4.815612
250.047536	7999.971702	12.854451	-0.051752	4.815591
250.157828	8000.071730	12.859456	-0.051773	4.815619
250.259086	8000.073379	12.864461	-0.051792	4.815619
250.307737	8000.030396	12.869466	-0.051801	4.815606
250.295072	8000.013110	12.874471	-0.051799	4.815601
249.855215	7999.988878	12.879475	-0.051717	4.815596
250.071361	8000.025495	12.884480	-0.051757	4.815606
250.087183	8000.042840	12.889485	-0.051760	4.815611
250.039511	8000.027119	12.894490	-0.051751	4.815607
250.088623	8000.062089	12.899495	-0.051760	4.815617
250.166153	7999.964053	12.904499	-0.051775	4.815588
250.277059	8000.016043	12.909504	-0.051796	4.815602
250.212981	8000.024614	12.914509	-0.051784	4.815605
250.212250	8000.040622	12.919514	-0.051784	4.815610
250.153277	8000.005499	12.924519	-0.051773	4.815600
250.204704	7999.999932	12.929523	-0.051782	4.815598
250.354336	8000.050416	12.934528	-0.051810	4.815612
250.195014	8000.047829	12.939533	-0.051781	4.815612
249.996580	8000.007235	12.944538	-0.051744	4.815601
250.312060	8000.068958	12.949543	-0.051802	4.815618
250.376354	7999.950420	12.954547	-0.051814	4.815583
250.099090	7999.999302	12.959552	-0.051763	4.815598
250.028096	7999.977864	12.964557	-0.051750	4.815592
250.269967	8000.007426	12.969562	-0.051795	4.815600
250.282440	8000.046070	12.974567	-0.051797	4.815611
250.204309	8000.027720	12.979571	-0.051783	4.815606
250.445350	8000.099978	12.984576	-0.051828	4.815626
250.169732	8000.060264	12.989581	-0.051776	4.815616
250.175558	8000.029397	12.994586	-0.051777	4.815607
250.339677	8000.065169	12.999591	-0.051808	4.815616
250.308450	8000.036904	13.004595	-0.051802	4.815608
250.059478	8000.101194	13.009600	-0.051756	4.815628
249.956947	8000.025856	13.014605	-0.051737	4.815607
250.142551	8000.023539	13.019610	-0.051771	4.815605
250.101163	8000.046359	13.024615	-0.051764	4.815612
250.034670	7999.973743	13.029619	-0.051751	4.815591
250.338943	8000.004319	13.034624	-0.051808	4.815599
250.168285	8000.021835	13.039629	-0.051776	4.815605
250.069593	7999.987134	13.044634	-0.051758	4.815595
250.193799	8000.019053	13.049639	-0.051781	4.815604
250.200448	7999.970049	13.054643	-0.051782	4.815589
250.196103	8000.045790	13.059648	-0.051782	4.815611
249.906729	8000.074188	13.064653	-0.051728	4.815621
250.112964	8000.023090	13.069658	-0.051766	4.815605
250.288303	8000.056909	13.074663	-0.051799	4.815614
250.056310	8000.008295	13.079667	-0.051756	4.815601
250.206384	8000.052380	13.084672	-0.051784	4.815613
250.283451	8000.034418	13.089677	-0.051798	4.815608
250.193554	7999.987047	13.094682	-0.051781	4.815594
250.405639	8000.046021	13.099687	-0.051821	4.815611
250.248229	7999.976197	13.104691	-0.051792	4.815591
250.282289	8000.074986	13.109696	-0.051798	4.815620
250.220901	8000.048365	13.114701	-0.051787	4.815612
250.260888	7999.988158	13.119706	-0.051794	4.815594
250.302896	8000.061450	13.124711	-0.051802	4.815616
250.247638	7999.990084	13.129715	-0.051792	4.815595
250.367560	8000.041154	13.134720	-0.051814	4.815609
250.352313	8000.050519	13.139725	-0.051811	4.815612
250.128239	7999.999898	13.144730	-0.051770	4.815598
250.287160	8000.068685	13.149735	-0.051799	4.815618
250.468939	8000.058832	13.154739	-0.051833	4.815614
250.429168	8000.053917	13.159744	-0.051826	4.815613
250.351520	8000.024896	13.164749	-0.051811	4.815605
250.514531	7999.988044	13.169754	-0.051842	4.815593
250.524560	8000.013836	13.174759	-0.051844	4.815601
250.175606	8000.020978	13.179763	-0.051779	4.815604
250.163974	8000.015454	13.184768	-0.051777	4.815603
250.344387	8000.044016	13.189773	-0.051810	4.815610
250.405418	8000.049283	13.194778	-0.051822	4.815611
250.192003	8000.119490	13.199783	-0.051782	4.815633
250.129103	7999.993545	13.204787	-0.051770	4.815596
250.275716	8000.076013	13.209792	-0.051798	4.815620
250.258781	8000.081079	13.214797	-0.051795	4.815621
250.276736	8000.020513	13.219802	-0.051798	4.815604
250.367553	8000.101006	13.224807	-0.051815	4.815627
250.356613	8000.047445	13.229811	-0.051813	4.815611
250.422602	8000.043182	13.234816	-0.051825	4.815610
250.369983	8000.056211	13.239821	-0.051815	4.815614
250.261325	8000.017076	13.244826	-0.051795	4.815603
250.171421	8000.121324	13.249831	-0.051779	4.815634
250.227249	8000.033612	13.254835	-0.051789	4.815608
250.333267	8000.044949	13.259840	-0.051809	4.815611
250.091137	8000.048490	13.264845	-0.051764	4.815613
250.247928	8000.082007	13.269850	-0.051793	4.815622
250.484639	8000.118960	13.274855	-0.051837	4.815631
250.220667	8000.052741	13.279859	-0.051788	4.815613
250.190851	8000.077885	13.284864	-0.051782	4.815621
250.358742	8000.083822	13.289869	-0.051814	4.815622
250.340684	8000.013061	13.294874	-0.051810	4.815601
250.385263	8000.085328	13.299879	-0.051819	4.815622
250.437162	8000.012501	13.304883	-0.051828	4.815601
250.441028	8000.077699	13.309888	-0.051829	4.815620
250.264490	8000.098322	13.314893	-0.051796	4.815626
250.268872	8000.061026	13.319898	-0.051797	4.815616
250.428504	8000.068964	13.324903	-0.051827	4.815617
250.142340	8000.025875	13.329907	-0.051774	4.815606
250.353916	8000.050673	13.334912	-0.051813	4.815612
250.432956	8000.112823	13.339917	-0.051828	4.815630
250.331427	8000.035366	13.344922	-0.051809	4.815608
250.284137	8000.067700	13.349927	-0.051800	4.815617
250.369841	8000.014642	13.354931	-0.051816	4.815601
250.481308	7999.996171	13.359936	-0.051837	4.815596
250.348306	7999.996147	13.364941	-0.051812	4.815596
250.184268	8000.008432	13.369946	-0.051782	4.815601
250.406807	8000.127370	13.374951	-0.051823	4.815634
250.290503	8000.064620	13.379955	-0.051802	4.815616
250.333496	8000.118710	13.384960	-0.051810	4.815632
250.292212	8000.036893	13.389965	-0.051802	4.815608
250.435632	8000.043500	13.394970	-0.051829	4.815610
250.176245	8000.059572	13.399975	-0.051781	4.815616
250.192093	8000.047020	13.404979	-0.051784	4.815612
250.320330	8000.042702	13.409984	-0.051807	4.815610
250.389194	8000.063045	13.414989	-0.051820	4.815616
250.208925	8000.004594	13.419994	-0.051787	4.815599
250.272186	8000.076097	13.424999	-0.051799	4.815620
250.449598	8000.034140	13.430003	-0.051832	4.815607
250.418741	8000.087029	13.435008	-0.051826	4.815622
250.471172	8000.056920	13.440013	-0.051836	4.815613
250.370560	8000.001900	13.445018	-0.051817	4.815598
250.325695	8000.044951	13.450023	-0.051809	4.815611
250.324999	8000.013979	13.455027	-0.051809	4.815601
250.536152	8000.062261	13.460032	-0.051848	4.815615
250.325278	8000.087664	13.465037	-0.051809	4.815623
250.100741	8000.057323	13.470042	-0.051767	4.815615
250.354909	8000.046511	13.475047	-0.051814	4.815611
250.357682	8000.057237	13.480051	-0.051815	4.815614
250.356607	8000.074306	13.485056	-0.051815	4.815619
250.334044	8000.085688	13.490061	-0.051811	4.815622
250.519176	8000.008621	13.495066	-0.051845	4.815599
250.409040	8000.047408	13.500071	-0.051825	4.815611
250.218600	8000.020824	13.505075	-0.051789	4.815604
250.498411	8000.056342	13.510080	-0.051841	4.815613
250.488344	8000.045504	13.515085	-0.051840	4.815610
250.511984	8000.014927	13.520090	-0.051844	4.815601
250.526624	8000.093114	13.525095	-0.051847	4.815624
250.416150	8000.003765	13.530099	-0.051826	4.815598
250.359411	8000.048759	13.535104	-0.051816	4.815611
250.344355	8000.085888	13.540109	-0.051813	4.815622
250.434629	7999.999805	13.545114	-0.051830	4.815597
250.354735	8000.035880	13.550119	-0.051815	4.815608
250.260441	8000.002318	13.555123	-0.051797	4.815598
250.365194	8000.045666	13.560128	-0.051817	4.815611
250.323035	8000.019358	13.565133	-0.051809	4.815603
250.503224	7999.992395	13.570138	-0.051843	4.815594
250.601214	8000.014279	13.575143	-0.051861	4.815600
250.715211	7999.999052	13.580147	-0.051882	4.815595
250.590742	8000.031199	13.585152	-0.051859	4.815605
250.468425	8000.047365	13.590157	-0.051836	4.815611
250.276315	7999.996196	13.595162	-0.051801	4.815596
250.397613	8000.005646	13.600167	-0.051823	4.815599
250.209426	7999.994047	13.605171	-0.051788	4.815596
250.387781	8000.011899	13.610176	-0.051821	4.815601
250.438145	8000.010586	13.615181	-0.051831	4.815600
250.248906	7999.962667	13.620186	-0.051796	4.815587
250.550185	8000.070072	13.625191	-0.051852	4.815617
250.448323	8000.020371	13.630195	-0.051833	4.815603
250.329351	8000.016304	13.635200	-0.051811	4.815602
250.287282	8000.031639	13.640205	-0.051803	4.815607
250.337684	8000.034598	13.645210	-0.051812	4.815607
250.318164	8000.119703	13.650215	-0.051809	4.815632
250.190741	8000.037554	13.655219	-0.051785	4.815609
250.270158	8000.059135	13.660224	-0.051800	4.815615
250.439490	8000.087518	13.665229	-0.051832	4.815622
250.311088	8000.008556	13.670234	-0.051808	4.815600
250.235895	8000.071401	13.675239	-0.051794	4.815619
250.404366	8000.016486	13.680243	-0.051825	4.815602
250.346575	8000.025159	13.685248	-0.051814	4.815605
250.390907	8000.003460	13.690253	-0.051823	4.815598
250.523893	8000.019507	13.695258	-0.051847	4.815602
250.570478	8000.050165	13.700263	-0.051856	4.815611
250.349024	8000.029483	13.705267	-0.051815	4.815606
250.291761	8000.022149	13.710272	-0.051804	4.815604
250.505126	8000.022418	13.715277	-0.051844	4.815603
250.244493	8000.020319	13.720282	-0.051796	4.815604
250.316182	8000.064197	13.725287	-0.051809	4.815616
250.186750	8000.047148	13.730291	-0.051785	4.815612
250.260685	8000.063302	13.735296	-0.051799	4.815616
250.130460	8000.108168	13.740301	-0.051775	4.815630
250.415245	8000.047670	13.745306	-0.051828	4.815611
250.524957	8000.103913	13.750311	-0.051848	4.815627
250.470002	8000.035754	13.755315	-0.051838	4.815607
250.588905	8000.078265	13.760320	-0.051860	4.815619
250.575904	8000.074854	13.765325	-0.051858	4.815618
250.474386	8000.009142	13.770330	-0.051839	4.815599
250.290768	8000.054207	13.775335	-0.051805	4.815613
250.427264	8000.025466	13.780339	-0.051830	4.815604
250.437151	8000.032036	13.785344	-0.051832	4.815606
250.238949	8000.022410	13.790349	-0.051795	4.815604
250.268184	7999.972705	13.795354	-0.051801	4.815590
250.307864	8000.014996	13.800359	-0.051808	4.815602
250.226736	7999.999799	13.805363	-0.051793	4.815598
250.175532	8000.110015	13.810368	-0.051784	4.815630
250.302785	8000.139849	13.815373	-0.051807	4.815638
250.423850	8000.080959	13.820378	-0.051830	4.815621
250.301675	8000.086450	13.825383	-0.051807	4.815623
250.148438	8000.066878	13.830387	-0.051779	4.815618
250.405735	8000.075336	13.835392	-0.051827	4.815619
250.330965	8000.107223	13.840397	-0.051813	4.815629
250.141673	8000.021933	13.845402	-0.051777	4.815605
250.276998	8000.065778	13.850407	-0.051803	4.815617
250.116856	8000.027942	13.855411	-0.051773	4.815606
250.073369	8000.006951	13.860416	-0.051765	4.815601
250.206186	8000.056095	13.865421	-0.051790	4.815614
250.216739	8000.044524	13.870426	-0.051792	4.815611
250.227053	8000.108760	13.875431	-0.051794	4.815630
250.143293	8000.036930	13.880435	-0.051778	4.815609
250.318426	8000.024833	13.885440	-0.051811	4.815605
250.270833	8000.068907	13.890445	-0.051802	4.815618
250.132318	7999.997256	13.895450	-0.051776	4.815597
250.341414	8000.042301	13.900455	-0.051815	4.815610
250.066088	8000.023946	13.905459	-0.051764	4.815606
250.099309	8000.033032	13.910464	-0.051770	4.815608
250.157372	8000.085231	13.915469	-0.051781	4.815623
250.262484	7999.988711	13.920474	-0.051800	4.815594
250.312778	8000.037580	13.925479	-0.051810	4.815608
250.306549	7999.977689	13.930483	-0.051809	4.815591
250.219725	8000.017922	13.935488	-0.051793	4.815603
250.115458	8000.116598	13.940493	-0.051773	4.815632
250.157154	7999.994489	13.945498	-0.051781	4.815596
250.302165	8000.107895	13.950503	-0.051808	4.815629
250.146057	8000.032754	13.955507	-0.051779	4.815608
250.220893	8000.015822	13.960512	-0.051793	4.815602
250.347914	8000.119327	13.965517	-0.051817	4.815632
250.156242	8000.077774	13.970522	-0.051781	4.815621
250.072386	8000.115920	13.975527	-0.051766	4.815632
250.181091	8000.070711	13.980531	-0.051786	4.815619
250.385736	8000.017452	13.985536	-0.051824	4.815602
250.380287	8000.101718	13.990541	-0.051823	4.815627
250.226248	8000.078929	13.995546	-0.051794	4.815621
250.180837	8000.098481	14.000551	-0.051786	4.815627
250.260254	8000.037847	14.005555	-0.051801	4.815609
250.129569	8000.079502	14.010560	-0.051776	4.815621
250.375792	8000.033326	14.015565	-0.051822	4.815607
250.212117	7999.986890	14.020570	-0.051792	4.815594
250.360608	8000.064050	14.025575	-0.051820	4.815616
250.184314	8000.030222	14.030579	-0.051787	4.815607
250.304085	8000.071679	14.035584	-0.051809	4.815618
250.378162	8000.099581	14.040589	-0.051823	4.815626
250.278235	8000.006133	14.045594	-0.051804	4.815599
250.301134	8000.052422	14.050599	-0.051809	4.815613
250.305063	8000.039676	14.055603	-0.051809	4.815609
250.255356	8000.036736	14.060608	-0.051800	4.815608
250.424875	8000.041631	14.065613	-0.051832	4.815609
250.259456	7999.999438	14.070618	-0.051801	4.815597
250.232226	8000.049182	14.075623	-0.051796	4.815612
250.372674	8000.043995	14.080627	-0.051822	4.815610
250.476166	8000.088391	14.085632	-0.051842	4.815622
250.152672	8000.126911	14.090637	-0.051781	4.815635
250.323554	8000.094458	14.095642	-0.051813	4.815625
250.351254	8000.093844	14.100647	-0.051818	4.815625
250.272491	8000.024231	14.105651	-0.051804	4.815605
250.204569	8000.015656	14.110656	-0.051791	4.815602
250.456874	8000.020830	14.115661	-0.051838	4.815603
250.558899	8000.027831	14.120666	-0.051857	4.815604
250.457318	8000.047537	14.125671	-0.051838	4.815611
250.296375	8000.058804	14.130675	-0.051808	4.815615
250.469513	8000.055216	14.135680	-0.051841	4.815613
250.443279	8000.052657	14.140685	-0.051836	4.815612
250.247692	8000.006770	14.145690	-0.051799	4.815600
250.443453	8000.066547	14.150695	-0.051836	4.815616
250.385093	8000.035705	14.155699	-0.051825	4.815607
250.542341	8000.028656	14.160704	-0.051854	4.815605
250.407906	8000.093741	14.165709	-0.051829	4.815624
250.302669	7999.998071	14.170714	-0.051810	4.815597
250.371296	7999.995987	14.175719	-0.051823	4.815596
250.205316	8000.009308	14.180723	-0.051792	4.815601
250.487418	8000.026711	14.185728	-0.051844	4.815604
250.479458	8000.057550	14.190733	-0.051843	4.815613
250.244699	8000.005687	14.195738	-0.051799	4.815599
250.207103	8000.045653	14.200743	-0.051792	4.815611
250.219587	8000.021301	14.205747	-0.051795	4.815604
250.181481	8000.027091	14.210752	-0.051788	4.815606
250.168992	8000.109108	14.215757	-0.051785	4.815630
250.312670	8000.034570	14.220762	-0.051812	4.815607
250.337455	8000.058467	14.225767	-0.051817	4.815614
250.359763	8000.071646	14.230771	-0.051821	4.815618
250.364942	8000.053581	14.235776	-0.051822	4.815613
250.303839	8000.117723	14.240781	-0.051811	4.815632
250.097639	8000.042835	14.245786	-0.051772	4.815611
250.220936	8000.072604	14.250791	-0.051795	4.815619
250.064357	8000.049775	14.255795	-0.051766	4.815613
250.043495	7999.140821	14.260800	-0.051762	4.815347

250.111951	7995.976577	14.265805	-0.051772	4.814422
250.233255	7990.557729	14.270810	-0.051792	4.812836
250.201627	7983.914671	14.275815	-0.051781	4.810892
250.150339	7976.645992	14.280819	-0.051767	4.808765
250.337296	7969.003784	14.285824	-0.051797	4.806526
250.315723	7961.179730	14.290829	-0.051788	4.804233
249.977489	7953.325889	14.295834	-0.051720	4.801932
250.242699	7945.384929	14.300839	-0.051764	4.799602
250.171590	7937.484257	14.305843	-0.051746	4.797284
249.981283	7929.380519	14.310848	-0.051705	4.794905
249.972696	7921.394003	14.315853	-0.051698	4.792560
249.970010	7913.330775	14.320858	-0.051693	4.790190
250.004395	7905.439790	14.325863	-0.051694	4.787870
249.865388	7897.364555	14.330867	-0.051663	4.785495
249.969365	7889.426073	14.335872	-0.051677	4.783158
250.184322	7881.396467	14.340877	-0.051712	4.780793
250.015972	7873.396427	14.345882	-0.051675	4.778437
249.889354	7865.449659	14.350887	-0.051647	4.776095
249.800771	7857.399374	14.355891	-0.051625	4.773721
249.719625	7849.357461	14.360896	-0.051605	4.771349
249.668697	7841.349569	14.365901	-0.051590	4.768985
249.665814	7833.365286	14.370906	-0.051584	4.766627
249.861703	7825.356722	14.375911	-0.051615	4.764260
249.408853	7817.420408	14.380915	-0.051526	4.761915
249.524899	7809.341796	14.385920	-0.051542	4.759525
249.621431	7801.442069	14.390925	-0.051555	4.757187
249.437323	7793.385959	14.395930	-0.051516	4.754803
249.553264	7785.329914	14.400935	-0.051532	4.752416
249.545203	7777.290224	14.405939	-0.051525	4.750033
249.471507	7769.305457	14.410944	-0.051507	4.747666
249.443516	7761.331501	14.415949	-0.051496	4.745300
249.339050	7753.335515	14.420954	-0.051472	4.742927
249.382875	7745.374507	14.425959	-0.051475	4.740563
249.318678	7737.415341	14.430963	-0.051457	4.738198
249.127681	7729.321403	14.435968	-0.051417	4.735793
249.207337	7721.332883	14.440973	-0.051426	4.733417
249.025456	7713.321789	14.445978	-0.051387	4.731033
249.033793	7705.282998	14.450983	-0.051384	4.728640
249.038102	7697.332074	14.455987	-0.051379	4.726272
249.079936	7689.311111	14.460992	-0.051382	4.723881
249.016049	7681.345636	14.465997	-0.051365	4.721506
249.073419	7673.309884	14.471002	-0.051370	4.719109
249.204511	7665.356188	14.476007	-0.051390	4.716735
248.891759	7657.332891	14.481011	-0.051326	4.714339
248.935238	7649.298809	14.486016	-0.051329	4.711939
249.079988	7641.297772	14.491021	-0.051351	4.709547
248.939698	7633.260036	14.496026	-0.051320	4.707143
248.767860	7625.328460	14.501031	-0.051282	4.704770
248.791746	7617.323098	14.506035	-0.051282	4.702373
248.869060	7609.262786	14.511040	-0.051291	4.699959
248.791768	7601.377414	14.516045	-0.051271	4.697596
248.568770	7593.317113	14.521050	-0.051225	4.695179
248.740991	7585.296808	14.526055	-0.051251	4.692773
248.740582	7577.256642	14.531059	-0.051246	4.690360
248.700076	7569.287945	14.536064	-0.051234	4.687967
248.890544	7561.248812	14.541069	-0.051264	4.685551
248.593277	7553.277550	14.546074	-0.051203	4.683155
248.716978	7545.332420	14.551079	-0.051221	4.680765
248.675171	7537.271194	14.556083	-0.051208	4.678339
248.653327	7529.314826	14.561088	-0.051199	4.675944
248.487064	7521.249977	14.566093	-0.051163	4.673514
248.327488	7513.108650	14.571098	-0.051128	4.671061
248.534082	7505.222680	14.576103	-0.051161	4.668683
248.371534	7497.181903	14.581107	-0.051126	4.666257
248.189752	7489.262141	14.586112	-0.051087	4.663866
248.343640	7481.240286	14.591117	-0.051110	4.661443
248.098231	7473.205655	14.596122	-0.051059	4.659016
248.132115	7465.315608	14.601127	-0.051060	4.656630
248.176647	7457.227398	14.606131	-0.051064	4.654183
248.099103	7449.189481	14.611136	-0.051044	4.651751
248.201999	7441.207838	14.616141	-0.051058	4.649334
248.081505	7433.232836	14.621146	-0.051030	4.646917
248.326291	7425.236125	14.626151	-0.051071	4.644493
248.134152	7417.229182	14.631155	-0.051030	4.642065
248.003690	7409.197832	14.636160	-0.051000	4.639628
247.774893	7401.289838	14.641165	-0.050953	4.637227
247.795599	7393.190180	14.646170	-0.050951	4.634767
247.767055	7385.224148	14.651175	-0.050941	4.632346
247.808010	7377.140243	14.656179	-0.050943	4.629887
248.082503	7369.189087	14.661184	-0.050989	4.627468
247.876639	7361.181113	14.666189	-0.050946	4.625030
247.865306	7353.208310	14.671194	-0.050938	4.622602
247.839881	7345.189516	14.676199	-0.050928	4.620158
247.648228	7337.193372	14.681203	-0.050887	4.617721
247.538835	7329.167773	14.686208	-0.050862	4.615272
247.604667	7321.229284	14.691213	-0.050869	4.612849
247.575823	7313.139630	14.696218	-0.050858	4.610379
247.740838	7305.209494	14.701223	-0.050884	4.607956
247.553567	7297.166325	14.706227	-0.050844	4.605497
247.479243	7289.181509	14.711232	-0.050825	4.603055
247.627747	7281.200715	14.716237	-0.050847	4.600612
247.488524	7273.172505	14.721242	-0.050816	4.598154
247.673896	7265.189928	14.726247	-0.050846	4.595709
247.471360	7257.136851	14.731251	-0.050803	4.593240
247.417910	7249.101137	14.736256	-0.050788	4.590775
247.514598	7241.141668	14.741261	-0.050800	4.588333
247.314169	7233.085430	14.746266	-0.050758	4.585860
247.444794	7225.145582	14.751271	-0.050777	4.583421
247.476089	7217.149254	14.756275	-0.050778	4.580963
247.375109	7209.190073	14.761280	-0.050754	4.578515
247.250097	7201.151073	14.766285	-0.050725	4.576042
247.185866	7193.119319	14.771290	-0.050708	4.573569
247.073304	7185.086030	14.776295	-0.050682	4.571095
246.947401	7177.099728	14.781299	-0.050653	4.568633
246.907693	7169.134663	14.786304	-0.050641	4.566177
246.947004	7161.168530	14.791309	-0.050643	4.563720
246.789731	7153.132690	14.796314	-0.050609	4.561239
247.069105	7145.179193	14.801319	-0.050655	4.558783
246.896847	7137.158237	14.806323	-0.050618	4.556304
247.031834	7129.169518	14.811328	-0.050638	4.553834
246.915544	7121.108659	14.816333	-0.050611	4.551340
246.890887	7113.095155	14.821338	-0.050601	4.548860
246.903002	7105.122124	14.826343	-0.050599	4.546391
246.967965	7097.087659	14.831347	-0.050605	4.543901
246.698419	7089.160186	14.836352	-0.050550	4.541443
246.729611	7081.155835	14.841357	-0.050551	4.538960
246.509517	7073.134281	14.846362	-0.050505	4.536470
246.631839	7065.103991	14.851367	-0.050522	4.533976
246.509080	7057.094754	14.856371	-0.050494	4.531487
246.581578	7049.055525	14.861376	-0.050502	4.528988
246.714643	7041.144714	14.866381	-0.050522	4.526528
246.519799	7033.056980	14.871386	-0.050481	4.524010
246.484398	7025.149065	14.876391	-0.050469	4.521548
246.556675	7017.135482	14.881395	-0.050477	4.519051
246.591743	7009.161635	14.886400	-0.050479	4.516565
246.426120	7001.108707	14.891405	-0.050442	4.514053
246.287213	6993.035118	14.896410	-0.050411	4.511533
246.239570	6985.024316	14.901415	-0.050397	4.509031
246.079183	6977.054906	14.906419	-0.050362	4.506541
246.269864	6969.015039	14.911424	-0.050393	4.504028
246.411069	6961.113741	14.916429	-0.050414	4.501557
246.169939	6953.061636	14.921434	-0.050364	4.499036
246.391960	6945.109526	14.926439	-0.050400	4.496547
246.277718	6937.077259	14.931443	-0.050373	4.494030
246.165025	6929.036588	14.936448	-0.050347	4.491509
246.246155	6921.061263	14.941453	-0.050357	4.489007
246.143292	6913.071323	14.946458	-0.050333	4.486499
246.181869	6905.037736	14.951463	-0.050335	4.483977
246.057140	6897.127584	14.956467	-0.050307	4.481491
245.912557	6889.051325	14.961472	-0.050274	4.478952
246.075372	6881.121255	14.966477	-0.050300	4.476458
245.838055	6873.050207	14.971482	-0.050250	4.473917
245.896742	6865.027113	14.976487	-0.050256	4.471390
245.797812	6857.021232	14.981491	-0.050232	4.468867
245.891892	6849.028571	14.986496	-0.050245	4.466348
245.871494	6841.025909	14.991501	-0.050236	4.463824
245.752199	6833.029964	14.996506	-0.050208	4.461299
245.792368	6825.035670	15.001511	-0.050211	4.458775
245.715960	6817.047337	15.006515	-0.050191	4.456251
245.732149	6809.040689	15.011520	-0.050189	4.453719
245.735188	6801.025935	15.016525	-0.050184	4.451184
245.589412	6793.013737	15.021530	-0.050152	4.448647
245.404968	6785.008654	15.026535	-0.050113	4.446111
245.536523	6777.027644	15.031539	-0.050132	4.443583
245.568276	6768.982592	15.036544	-0.050133	4.441032
245.470106	6761.044289	15.041549	-0.050109	4.438513
245.279528	6753.025299	15.046554	-0.050068	4.435967
245.608011	6745.000726	15.051559	-0.050124	4.433420
245.340141	6736.968548	15.056563	-0.050069	4.430866
245.376109	6728.976953	15.061568	-0.050071	4.428325
245.483308	6720.971236	15.066573	-0.050086	4.425778
245.503394	6712.981193	15.071578	-0.050084	4.423235
245.377694	6704.989124	15.076583	-0.050056	4.420688
245.291771	6697.084350	15.081587	-0.050035	4.418169
245.289312	6689.031135	15.086592	-0.050029	4.415600
245.184922	6681.013555	15.091597	-0.050004	4.413042
244.823843	6672.912852	15.096602	-0.049932	4.410454
245.103454	6664.959186	15.101607	-0.049979	4.407914
244.851243	6656.989344	15.106611	-0.049927	4.405365
244.835493	6648.983255	15.111616	-0.049918	4.402805
244.911011	6641.032010	15.116621	-0.049927	4.400261
244.974218	6633.034863	15.121626	-0.049934	4.397700
244.831749	6625.050726	15.126631	-0.049902	4.395141
244.670387	6617.000557	15.131635	-0.049867	4.392560
244.686572	6608.919994	15.136640	-0.049865	4.389968
244.828442	6600.985914	15.141645	-0.049886	4.387422
244.610337	6592.919929	15.146650	-0.049840	4.384831
244.804136	6584.992238	15.151655	-0.049871	4.382284
244.597528	6576.987056	15.156659	-0.049828	4.379709
244.394151	6569.054523	15.161664	-0.049785	4.377156
244.538823	6561.031045	15.166669	-0.049806	4.374574
244.576671	6552.981312	15.171674	-0.049808	4.371982
244.371229	6544.965167	15.176679	-0.049765	4.369397
244.372028	6537.021529	15.181683	-0.049760	4.366835
244.514360	6528.962782	15.186688	-0.049781	4.364236
244.286105	6521.057164	15.191693	-0.049733	4.361682
244.129370	6512.972263	15.196698	-0.049699	4.359069
244.222111	6505.055320	15.201703	-0.049711	4.356511
244.151832	6496.977403	15.206707	-0.049693	4.353898
243.969437	6488.866144	15.211712	-0.049654	4.351272
244.108652	6480.934468	15.216717	-0.049674	4.348704
244.054916	6472.950737	15.221722	-0.049659	4.346117
244.201973	6464.949304	15.226727	-0.049681	4.343524
244.197028	6456.962538	15.231731	-0.049675	4.340933
244.118916	6448.944607	15.236736	-0.049656	4.338330
244.301650	6440.997039	15.241741	-0.049685	4.335750
244.039676	6432.927395	15.246746	-0.049631	4.333125
244.124882	6424.947305	15.251751	-0.049641	4.330531
244.198851	6416.952076	15.256755	-0.049650	4.327930
244.147188	6408.922245	15.261760	-0.049635	4.325315
244.122235	6400.993463	15.266765	-0.049625	4.322732
244.001165	6392.943310	15.271770	-0.049597	4.320107
244.015021	6384.974450	15.276775	-0.049595	4.317508
243.981286	6376.927331	15.281779	-0.049583	4.314882
243.827383	6368.908947	15.286784	-0.049550	4.312262
243.948519	6360.940648	15.291789	-0.049567	4.309659
243.586808	6352.960831	15.296794	-0.049494	4.307047
243.927868	6344.920637	15.301799	-0.049553	4.304419
244.013105	6337.006722	15.306803	-0.049564	4.301829
243.775838	6328.921446	15.311808	-0.049514	4.299179
243.710800	6320.985611	15.316813	-0.049497	4.296578
243.781474	6312.973247	15.321818	-0.049505	4.293950
243.907210	6304.888318	15.326823	-0.049523	4.291298
243.823233	6296.914328	15.331827	-0.049502	4.288679
243.909152	6288.895383	15.336832	-0.049513	4.286045
243.969456	6280.949392	15.341837	-0.049519	4.283433
243.729163	6272.927671	15.346842	-0.049469	4.280792
243.717059	6264.943062	15.351847	-0.049462	4.278164
243.710800	6256.965116	15.356851	-0.049455	4.275536
243.553956	6248.866281	15.361856	-0.049421	4.272866
243.681562	6240.868255	15.366861	-0.049440	4.270229
243.642847	6232.844537	15.371866	-0.049427	4.267581
243.671736	6224.876950	15.376871	-0.049427	4.264950
243.439007	6216.969483	15.381875	-0.049379	4.262336
243.377678	6208.916947	15.386880	-0.049362	4.259673
243.554929	6200.994112	15.391885	-0.049390	4.257054
243.439353	6192.908759	15.396890	-0.049363	4.254376
243.506263	6184.901711	15.401895	-0.049371	4.251725
243.627811	6176.875517	15.406899	-0.049388	4.249066
243.319391	6168.894595	15.411904	-0.049326	4.246416
243.441552	6160.917916	15.416909	-0.049343	4.243770
243.156120	6152.955877	15.421914	-0.049285	4.241124
243.375380	6144.939398	15.426919	-0.049321	4.238462
243.291028	6136.990130	15.431923	-0.049300	4.235818
243.173050	6128.924884	15.436928	-0.049272	4.233134
243.052676	6120.900506	15.441933	-0.049245	4.230462
242.980779	6112.910749	15.446938	-0.049226	4.227800
243.025610	6104.879535	15.451943	-0.049229	4.225123
243.105683	6096.959027	15.456947	-0.049239	4.222482
242.767726	6088.936278	15.461952	-0.049171	4.219801
242.772076	6081.033678	15.466957	-0.049167	4.217162
242.930001	6072.906277	15.471962	-0.049191	4.214448
242.780645	6064.928785	15.476967	-0.049158	4.211779
242.889329	6056.917701	15.481971	-0.049173	4.209100
242.762958	6048.922684	15.486976	-0.049144	4.206422
243.005561	6040.973498	15.491981	-0.049184	4.203761
242.782160	6032.960994	15.496986	-0.049138	4.201073
242.764660	6024.983512	15.501991	-0.049129	4.198397
242.621535	6016.962117	15.506995	-0.049097	4.195703
242.681579	6008.873483	15.512000	-0.049103	4.192986
242.436966	6000.858357	15.517005	-0.049053	4.190290
242.456438	5992.849247	15.522010	-0.049051	4.187597
242.516987	5984.878269	15.527015	-0.049057	4.184915
242.539768	5976.926593	15.532019	-0.049056	4.182237
242.419113	5968.907848	15.537024	-0.049029	4.179534
242.394083	5960.963383	15.542029	-0.049019	4.176855
242.374739	5952.891566	15.547034	-0.049010	4.174131
242.220940	5944.910880	15.552039	-0.048976	4.171435
242.290441	5936.912205	15.557043	-0.048984	4.168734
242.199968	5928.892719	15.562048	-0.048962	4.166022
242.300113	5920.933825	15.567053	-0.048975	4.163330
242.185353	5912.907187	15.572058	-0.048949	4.160612
242.070427	5904.928239	15.577063	-0.048922	4.157908
242.110856	5896.934425	15.582067	-0.048925	4.155199
242.059102	5888.863445	15.587072	-0.048910	4.152461
242.073135	5880.866323	15.592077	-0.048907	4.149747
241.954870	5872.913094	15.597082	-0.048880	4.147045
241.998175	5864.898773	15.602087	-0.048883	4.144322
242.116293	5856.901730	15.607091	-0.048900	4.141604
241.975411	5848.876057	15.612096	-0.048868	4.138871
241.934392	5840.963979	15.617101	-0.048856	4.136177
241.701583	5832.914714	15.622106	-0.048807	4.133431
241.850548	5824.869833	15.627111	-0.048830	4.130690
241.818102	5816.903647	15.632115	-0.048818	4.127972
241.597134	5808.892067	15.637120	-0.048772	4.125234
241.675015	5800.924194	15.642125	-0.048781	4.122512
241.638969	5792.893666	15.647130	-0.048769	4.119767
241.688222	5784.998530	15.652135	-0.048773	4.117066
241.685710	5776.945481	15.657139	-0.048768	4.114310
241.515659	5768.877735	15.662144	-0.048731	4.111544
241.589874	5760.871790	15.667149	-0.048740	4.108801
241.458669	5752.880817	15.672154	-0.048710	4.106058
241.661378	5744.892457	15.677159	-0.048743	4.103319
241.579194	5736.907600	15.682163	-0.048722	4.100575
241.476082	5728.898973	15.687168	-0.048698	4.097821
241.335042	5720.940811	15.692173	-0.048666	4.095082
241.247264	5712.899809	15.697178	-0.048645	4.092314
241.219157	5704.899104	15.702183	-0.048634	4.089558
241.216102	5696.956252	15.707187	-0.048629	4.086820
241.344917	5688.904903	15.712192	-0.048647	4.084046
241.286163	5680.984927	15.717197	-0.048631	4.081312
241.230244	5672.943649	15.722202	-0.048616	4.078534
241.103862	5664.973934	15.727207	-0.048587	4.075778
241.282958	5656.943168	15.732211	-0.048615	4.073004
241.001326	5648.905856	15.737216	-0.048558	4.070219
241.036051	5640.954994	15.742221	-0.048559	4.067466
241.003756	5632.893364	15.747226	-0.048548	4.064672
240.958098	5624.959357	15.752231	-0.048534	4.061920
240.993129	5616.950960	15.757235	-0.048535	4.059142
240.742562	5608.968004	15.762240	-0.048484	4.056367
240.987827	5600.939368	15.767245	-0.048524	4.053581
240.889371	5592.918018	15.772250	-0.048500	4.050790
240.917098	5584.945360	15.777255	-0.048500	4.048016
241.011369	5576.943074	15.782259	-0.048513	4.045232
240.743225	5568.974228	15.787264	-0.048458	4.042451
240.800971	5560.943346	15.792269	-0.048463	4.039652
240.727483	5552.988948	15.797274	-0.048444	4.036876
240.846893	5544.929836	15.802279	-0.048462	4.034064
240.777429	5536.836249	15.807283	-0.048443	4.031235
240.572004	5528.867661	15.812288	-0.048400	4.028446
240.435738	5520.892741	15.817293	-0.048369	4.025653
240.287908	5512.928383	15.822298	-0.048337	4.022863
240.476508	5504.928950	15.827303	-0.048367	4.020063
240.751038	5496.952576	15.832307	-0.048413	4.017270
240.243105	5488.915046	15.837312	-0.048313	4.014442
240.392154	5480.913599	15.842317	-0.048335	4.011635
240.204281	5472.915052	15.847322	-0.048295	4.008822
240.459903	5464.891566	15.852327	-0.048338	4.006005
240.428151	5456.929207	15.857331	-0.048327	4.003203
240.302968	5448.901347	15.862336	-0.048298	4.000375
240.312108	5440.962555	15.867341	-0.048295	3.997578
240.064482	5432.955235	15.872346	-0.048243	3.994750
240.109686	5424.914563	15.877351	-0.048247	3.991914
240.189456	5416.916002	15.882355	-0.048256	3.989091
240.052056	5408.890763	15.887360	-0.048226	3.986253
240.114594	5400.935241	15.892365	-0.048232	3.983441
240.106658	5392.949808	15.897370	-0.048225	3.980616
239.893146	5384.963853	15.902375	-0.048180	3.977784
239.997539	5376.951063	15.907379	-0.048195	3.974947
240.008955	5368.900838	15.912384	-0.048192	3.972092
240.166841	5360.926826	15.917389	-0.048216	3.969265
239.834456	5352.959009	15.922394	-0.048149	3.966430
239.817766	5344.952032	15.927399	-0.048141	3.963584
239.916670	5336.988254	15.932403	-0.048154	3.960754
239.761115	5328.985437	15.937408	-0.048120	3.957903
239.692097	5321.026320	15.942413	-0.048102	3.955068
239.591490	5312.983416	15.947418	-0.048078	3.952199
239.553790	5304.938946	15.952423	-0.048065	3.949330
239.541847	5296.983024	15.957427	-0.048058	3.946490
239.453014	5288.929159	15.962432	-0.048036	3.943612
239.504701	5280.982529	15.967437	-0.048041	3.940772
239.334697	5272.998536	15.972442	-0.048004	3.937913
239.464597	5264.974065	15.977447	-0.048023	3.935043
239.520502	5257.012254	15.982451	-0.048028	3.932192
239.214926	5248.944661	15.987456	-0.047966	3.929295
239.475471	5241.018995	15.992461	-0.048010	3.926456
239.364391	5232.989131	15.997466	-0.047984	3.923572
239.412319	5225.016207	16.002471	-0.047987	3.920708
239.285581	5217.051070	16.007475	-0.047959	3.917842
239.312105	5209.018043	16.012480	-0.047958	3.914952
239.465198	5200.991364	16.017485	-0.047982	3.912065
239.270965	5192.991089	16.022490	-0.047940	3.909179
239.099228	5185.023342	16.027495	-0.047903	3.906303
239.122088	5176.996932	16.032499	-0.047902	3.903407
239.041730	5168.961990	16.037504	-0.047882	3.900503
239.108798	5161.036742	16.042509	-0.047890	3.897641
239.014477	5153.009292	16.047514	-0.047867	3.894736
239.147569	5144.970696	16.052519	-0.047886	3.891829
238.984644	5137.000273	16.057523	-0.047851	3.888939
238.894878	5129.003546	16.062528	-0.047829	3.886038
239.066636	5121.033287	16.067533	-0.047856	3.883150
238.930531	5113.034663	16.072538	-0.047825	3.880244
238.917005	5105.037223	16.077543	-0.047818	3.877338
238.894662	5097.043692	16.082547	-0.047808	3.874432
238.740787	5088.763089	16.087552	-0.047774	3.871416
238.697256	5080.857556	16.092557	-0.047761	3.868537
238.582555	5072.889019	16.097562	-0.047734	3.865631
238.615292	5064.967239	16.102567	-0.047735	3.862742
238.745423	5056.996426	16.107571	-0.047755	3.859836
238.680035	5049.010730	16.112576	-0.047737	3.856918
238.995053	5041.000675	16.117581	-0.047791	3.853997
238.756017	5033.001725	16.122586	-0.047741	3.851067
238.480005	5024.990572	16.127591	-0.047684	3.848128
238.734571	5016.991784	16.132595	-0.047727	3.845203
238.588281	5009.029125	16.137600	-0.047694	3.842281
238.507419	5001.070613	16.142605	-0.047674	3.839360
238.464427	4993.116060	16.147610	-0.047661	3.836438
238.551161	4985.043885	16.152615	-0.047672	3.833474
238.605015	4977.054474	16.157619	-0.047677	3.830537
238.409939	4969.048065	16.162624	-0.047635	3.827586
238.377659	4961.041989	16.167629	-0.047624	3.824637
238.352581	4953.073870	16.172634	-0.047614	3.821699
238.314918	4945.071164	16.177639	-0.047602	3.818747
238.478846	4937.084993	16.182643	-0.047627	3.815802
238.431437	4929.067346	16.187648	-0.047613	3.812839
238.491777	4921.096109	16.192653	-0.047619	3.809893
238.334004	4913.090623	16.197658	-0.047585	3.806927
238.012495	4905.091777	16.202663	-0.047520	3.803958
238.008949	4897.139570	16.207667	-0.047514	3.801011
237.998967	4889.132495	16.212672	-0.047507	3.798041
238.154638	4881.110118	16.217677	-0.047531	3.795067
237.990838	4873.075134	16.222682	-0.047495	3.792078
237.824906	4865.043332	16.227687	-0.047459	3.789089
237.838772	4857.116243	16.232691	-0.047456	3.786140
237.860787	4849.069122	16.237696	-0.047455	3.783144
237.790852	4841.132724	16.242701	-0.047437	3.780185
237.594600	4833.110621	16.247706	-0.047395	3.777189
237.639473	4825.089574	16.252711	-0.047399	3.774196
237.655633	4817.135939	16.257715	-0.047396	3.771225
237.459079	4809.103022	16.262720	-0.047355	3.768218
237.596019	4801.095431	16.267725	-0.047375	3.765225
237.509941	4793.130332	16.272730	-0.047354	3.762241
237.384473	4785.131546	16.277735	-0.047325	3.759241
237.516583	4777.156599	16.282739	-0.047345	3.756253
237.483487	4769.099226	16.287744	-0.047333	3.753228
237.445945	4761.129233	16.292749	-0.047321	3.750233
237.273925	4753.137479	16.297754	-0.047284	3.747225
237.405841	4745.113328	16.302759	-0.047303	3.744209
237.253848	4737.192947	16.307763	-0.047270	3.741223
237.094308	4729.153560	16.312768	-0.047235	3.738190
237.229749	4721.177474	16.317773	-0.047255	3.735185
237.136192	4713.156093	16.322778	-0.047232	3.732155
237.051498	4705.132450	16.327783	-0.047211	3.729122
237.325975	4697.163511	16.332787	-0.047257	3.726116
237.142658	4689.165775	16.337792	-0.047218	3.723085
237.029485	4681.180037	16.342797	-0.047192	3.720059
236.947813	4673.228475	16.347802	-0.047172	3.717043
236.973841	4665.187613	16.352807	-0.047171	3.713994
237.091168	4657.087439	16.357811	-0.047188	3.710922
236.876468	4649.126330	16.362816	-0.047143	3.707892
236.960969	4641.145819	16.367821	-0.047153	3.704859
237.114350	4633.178801	16.372826	-0.047177	3.701831
237.013088	4625.180808	16.377831	-0.047153	3.698783
236.885240	4617.248513	16.382835	-0.047124	3.695756
236.702755	4609.222481	16.387840	-0.047084	3.692689
236.773785	4601.213455	16.392845	-0.047093	3.689633
236.723566	4593.242743	16.397850	-0.047078	3.686586
236.780026	4585.242197	16.402855	-0.047083	3.683528
236.679798	4577.285606	16.407859	-0.047060	3.680480
236.607347	4569.267003	16.412864	-0.047041	3.677406
236.509266	4561.243020	16.417869	-0.047017	3.674327
236.488994	4553.234416	16.422874	-0.047008	3.671254
236.342377	4545.237787	16.427879	-0.046976	3.668179
236.450547	4537.246162	16.432883	-0.046991	3.665110
236.685644	4529.248541	16.437888	-0.047030	3.662040
236.701751	4521.265101	16.442893	-0.047027	3.658966
236.314536	4513.296388	16.447898	-0.046950	3.655885
236.318814	4505.286803	16.452903	-0.046946	3.652797
236.560865	4497.241039	16.457907	-0.046986	3.649697
236.289058	4489.278485	16.462912	-0.046930	3.646614
236.246024	4481.268300	16.467917	-0.046917	3.643516
236.284090	4473.253709	16.472922	-0.046919	3.640415
236.259944	4465.296168	16.477927	-0.046909	3.637333
236.108250	4457.313189	16.482931	-0.046876	3.634234
236.077967	4449.282790	16.487936	-0.046865	3.631118
236.101287	4441.282083	16.492941	-0.046864	3.628012
235.996537	4433.247405	16.497946	-0.046839	3.624886
235.986240	4425.285284	16.502951	-0.046832	3.621789
236.185514	4417.290380	16.507955	-0.046864	3.618682
235.880726	4409.334640	16.512960	-0.046802	3.615574
235.826681	4401.341726	16.517965	-0.046787	3.612455
235.912605	4393.291443	16.522970	-0.046798	3.609315
235.860364	4385.337049	16.527975	-0.046783	3.606206
235.847599	4377.369167	16.532979	-0.046775	3.603091
235.834007	4369.360402	16.537984	-0.046768	3.599956
235.728180	4361.409062	16.542989	-0.046743	3.596839
235.733037	4353.413720	16.547994	-0.046738	3.593705
235.633339	4345.365293	16.552999	-0.046715	3.590544
235.806280	4337.394079	16.558003	-0.046742	3.587418
235.590326	4329.372197	16.563008	-0.046696	3.584259
235.600783	4321.423524	16.568013	-0.046693	3.581133
235.400615	4313.442465	16.573018	-0.046651	3.577984
235.627400	4305.401680	16.578023	-0.046688	3.574822
235.385234	4297.436306	16.583027	-0.046637	3.571673
235.266264	4289.437399	16.588032	-0.046610	3.568512
235.429039	4281.428828	16.593037	-0.046635	3.565352
235.364121	4273.466204	16.598042	-0.046618	3.562201
235.095408	4265.457958	16.603047	-0.046563	3.559023
235.142170	4257.473732	16.608051	-0.046566	3.555861
234.997671	4249.380991	16.613056	-0.046534	3.552648
235.046287	4241.368495	16.618061	-0.046538	3.549469
235.207935	4233.360200	16.623066	-0.046563	3.546292
235.325593	4225.389782	16.628071	-0.046580	3.543127
235.082205	4217.473989	16.633075	-0.046529	3.539969
234.976478	4209.464116	16.638080	-0.046504	3.536775
235.012139	4201.470407	16.643085	-0.046506	3.533589
234.864605	4193.443828	16.648090	-0.046473	3.530382
234.799592	4185.455846	16.653095	-0.046456	3.527189
235.043494	4177.464861	16.658099	-0.046496	3.524002
235.011543	4169.491935	16.663104	-0.046485	3.520810
234.863808	4161.530450	16.668109	-0.046452	3.517617
234.765519	4153.521094	16.673114	-0.046429	3.514403
234.773594	4145.504705	16.678119	-0.046425	3.511187
234.675481	4137.512404	16.683123	-0.046402	3.507974
234.542072	4129.492168	16.688128	-0.046372	3.504746
234.750638	4121.552141	16.693133	-0.046405	3.501558
234.580737	4113.561117	16.698138	-0.046369	3.498335
234.502696	4105.560320	16.703143	-0.046349	3.495107
234.703962	4097.565240	16.708147	-0.046381	3.491888
234.357647	4089.580154	16.713152	-0.046312	3.488652
234.355435	4081.568674	16.718157	-0.046306	3.485413
234.321501	4073.615734	16.723162	-0.046295	3.482195
234.193080	4065.615207	16.728167	-0.046265	3.478951
234.060424	4057.671812	16.733171	-0.046236	3.475727
234.182081	4049.599552	16.738176	-0.046253	3.472455
234.306513	4041.557678	16.743181	-0.046271	3.469193
234.259392	4033.577671	16.748186	-0.046257	3.465948
234.086423	4025.639759	16.753191	-0.046220	3.462713
234.073103	4017.628373	16.758195	-0.046212	3.459450
234.095823	4009.649224	16.763200	-0.046211	3.456198
234.061806	4001.637785	16.768205	-0.046200	3.452928
233.951081	3993.618749	16.773210	-0.046174	3.449649
233.920012	3985.648280	16.778215	-0.046163	3.446390
234.086346	3977.670900	16.783219	-0.046189	3.443131
233.794351	3969.690228	16.788224	-0.046129	3.439853
233.859119	3961.726317	16.793229	-0.046136	3.436590
234.071289	3953.662100	16.798234	-0.046170	3.433288
233.918738	3945.646778	16.803239	-0.046137	3.429990
234.083864	3937.677705	16.808243	-0.046162	3.426719
233.970114	3929.684495	16.813248	-0.046136	3.423426
233.949609	3921.742106	16.818253	-0.046127	3.420153
233.823616	3913.781231	16.823258	-0.046098	3.416866
233.934058	3905.724590	16.828263	-0.046114	3.413545
233.849807	3897.761383	16.833267	-0.046093	3.410252
233.585381	3889.748455	16.838272	-0.046039	3.406929
233.686326	3881.770311	16.843277	-0.046052	3.403630
233.656597	3873.798727	16.848282	-0.046041	3.400326
233.527657	3865.819140	16.853287	-0.046012	3.397012
233.610060	3857.786825	16.858291	-0.046022	3.393681
233.549129	3849.710595	16.863296	-0.046006	3.390322
233.467701	3841.764153	16.868301	-0.045986	3.387014
233.377538	3833.791033	16.873306	-0.045964	3.383691
233.426488	3825.795293	16.878311	-0.045968	3.380360
233.322698	3817.860771	16.883315	-0.045943	3.377046
232.940086	3809.871886	16.888320	-0.045867	3.373696
232.975968	3801.830052	16.893325	-0.045868	3.370336
232.982377	3793.855420	16.898330	-0.045864	3.366999
233.129440	3785.822263	16.903335	-0.045886	3.363639
232.997030	3777.883576	16.908339	-0.045857	3.360306
232.845966	3769.915034	16.913344	-0.045823	3.356956
233.119550	3761.894131	16.918349	-0.045869	3.353596
233.043685	3753.877957	16.923354	-0.045850	3.350222
233.084855	3745.859760	16.928359	-0.045852	3.346848
233.102467	3737.902773	16.933363	-0.045850	3.343496
232.875516	3729.924000	16.938368	-0.045803	3.340122
233.015772	3721.942069	16.943373	-0.045824	3.336756
232.817653	3713.959314	16.948378	-0.045782	3.333375
232.724665	3705.932774	16.953383	-0.045759	3.329976
232.732556	3697.983718	16.958387	-0.045756	3.326609
232.693080	3689.952668	16.963392	-0.045743	3.323203
232.692341	3681.984545	16.968397	-0.045738	3.319821
232.573194	3674.051167	16.973402	-0.045711	3.316446
232.677825	3665.993112	16.978407	-0.045725	3.313023
232.713239	3657.987597	16.983411	-0.045726	3.309616
232.580334	3649.980388	16.988416	-0.045696	3.306199
232.495419	3642.005043	16.993421	-0.045675	3.302793
232.587529	3634.036037	16.998426	-0.045687	3.299394
232.228288	3626.091525	17.003431	-0.045615	3.295984
232.328381	3618.057321	17.008435	-0.045629	3.292550
232.219868	3610.057497	17.013440	-0.045603	3.289119
232.380801	3602.073814	17.018445	-0.045628	3.285701
232.357263	3594.122291	17.023450	-0.045619	3.282287
232.297400	3586.107550	17.028455	-0.045602	3.278841
232.395907	3578.152192	17.033459	-0.045615	3.275423
232.036708	3570.135823	17.038464	-0.045543	3.271957
232.207308	3562.114621	17.043469	-0.045570	3.268505
232.079704	3554.112396	17.048474	-0.045541	3.265047
231.972026	3546.150842	17.053479	-0.045516	3.261604
231.972740	3538.179158	17.058483	-0.045511	3.258156
231.924238	3530.189441	17.063488	-0.045497	3.254696
232.029216	3522.181883	17.068493	-0.045511	3.251230
231.920800	3514.191710	17.073498	-0.045486	3.247759
231.887738	3506.184490	17.078503	-0.045474	3.244280
231.877966	3498.251902	17.083507	-0.045467	3.240831
231.992091	3490.220917	17.088512	-0.045483	3.237340
231.719907	3482.268845	17.093517	-0.045428	3.233864
231.743989	3474.199839	17.098522	-0.045427	3.230346
231.848245	3466.211450	17.103527	-0.045441	3.226862
231.600941	3458.261686	17.108531	-0.045390	3.223377
231.561003	3450.250570	17.113536	-0.045377	3.219870
231.509916	3442.310510	17.118541	-0.045363	3.216389
231.348691	3434.326118	17.123546	-0.045327	3.212881
231.309937	3426.305570	17.128551	-0.045315	3.209358
231.378503	3418.341920	17.133555	-0.045323	3.205861
231.202457	3410.332805	17.138560	-0.045285	3.202330
231.079972	3402.387742	17.143565	-0.045257	3.198825
231.112753	3394.393515	17.148570	-0.045258	3.195301
231.107638	3386.343146	17.153575	-0.045252	3.191747
231.132802	3378.369460	17.158579	-0.045251	3.188224
231.192428	3370.362491	17.163584	-0.045257	3.184684
231.132159	3362.433663	17.168589	-0.045241	3.181170
230.960841	3354.451117	17.173594	-0.045204	3.177623
230.911104	3346.439858	17.178599	-0.045189	3.174064
231.238526	3338.404032	17.183603	-0.045245	3.170507
231.029109	3330.438080	17.188608	-0.045201	3.166954
231.009299	3322.484524	17.193613	-0.045192	3.163410
230.944985	3314.506426	17.198618	-0.045175	3.159850
230.936054	3306.520786	17.203623	-0.045168	3.156285
230.880667	3298.522173	17.208627	-0.045152	3.152708
230.902102	3290.490998	17.213632	-0.045151	3.149115
230.951947	3282.509387	17.218637	-0.045155	3.145542
230.839103	3274.541638	17.223642	-0.045129	3.141964
230.617503	3266.561043	17.228647	-0.045083	3.138371
230.676961	3258.594667	17.233651	-0.045089	3.134793
230.515335	3250.589821	17.238656	-0.045053	3.131184
230.549038	3242.586765	17.243661	-0.045054	3.127579
230.618651	3234.615652	17.248666	-0.045062	3.123987
230.513455	3226.641302	17.253671	-0.045038	3.120382
230.405164	3218.690335	17.258675	-0.045012	3.116782
230.431428	3210.671789	17.263680	-0.045012	3.113154
230.662959	3202.637283	17.268685	-0.045050	3.109524
230.472742	3194.694779	17.273690	-0.045009	3.105912
230.190640	3186.702117	17.278695	-0.044952	3.102269
230.221867	3178.732836	17.283699	-0.044952	3.098647
230.294455	3170.735120	17.288704	-0.044961	3.095009
230.222450	3162.723687	17.293709	-0.044942	3.091354
230.200924	3154.744023	17.298714	-0.044933	3.087712
230.187393	3146.747711	17.303719	-0.044925	3.084058
230.179797	3138.829860	17.308723	-0.044919	3.080435
230.184325	3130.831528	17.313728	-0.044914	3.076773
230.199476	3122.806934	17.318733	-0.044912	3.073094
230.182862	3114.748281	17.323738	-0.044904	3.069394
229.845929	3106.792473	17.328743	-0.044836	3.065721
229.890177	3098.852816	17.333747	-0.044839	3.062070
229.959456	3090.865189	17.338752	-0.044847	3.058393
229.901783	3082.883257	17.343757	-0.044831	3.054709
230.042214	3074.881153	17.348762	-0.044852	3.051020
229.809441	3066.904171	17.353767	-0.044803	3.047320
229.672357	3058.945989	17.358771	-0.044772	3.043629
229.596025	3050.950861	17.363776	-0.044753	3.039920
229.799534	3042.988305	17.368781	-0.044786	3.036234
229.692849	3034.997681	17.373786	-0.044761	3.032516
229.528112	3026.983382	17.378791	-0.044725	3.028780
229.502131	3019.004121	17.383795	-0.044715	3.025062
229.513878	3011.031416	17.388800	-0.044712	3.021344
229.419599	3003.058894	17.393805	-0.044689	3.017617
229.429118	2995.056701	17.398810	-0.044686	3.013876
229.370206	2987.039630	17.403815	-0.044670	3.010120
229.451027	2979.092460	17.408819	-0.044680	3.006399
229.204334	2971.117788	17.413824	-0.044628	3.002645
229.351948	2963.129530	17.418829	-0.044651	2.998899
229.377209	2955.165443	17.423834	-0.044650	2.995153
229.266092	2947.123749	17.428839	-0.044624	2.991360
229.303362	2939.149336	17.433843	-0.044626	2.987600
229.157022	2931.148304	17.438848	-0.044594	2.983815
229.125847	2923.193406	17.443853	-0.044583	2.980052
228.964055	2915.265806	17.448858	-0.044548	2.976290
229.124216	2907.210563	17.453863	-0.044572	2.972480
229.081438	2899.239886	17.458867	-0.044559	2.968695
228.908420	2891.271051	17.463872	-0.044522	2.964898
228.882500	2883.318996	17.468877	-0.044512	2.961113
228.812126	2875.358337	17.473882	-0.044493	2.957316
228.742146	2867.337269	17.478887	-0.044475	2.953486
228.713255	2859.320898	17.483891	-0.044465	2.949655
228.801922	2851.332889	17.488896	-0.044476	2.945839
228.804339	2843.368447	17.493901	-0.044471	2.942024
228.710756	2835.429317	17.498906	-0.044449	2.938212
228.586135	2827.435698	17.503911	-0.044420	2.934367
228.717223	2819.438372	17.508915	-0.044440	2.930528
228.445033	2811.480595	17.513920	-0.044384	2.926683
228.523685	2803.494390	17.518925	-0.044393	2.922837
228.534835	2795.520238	17.523930	-0.044390	2.918988
228.602310	2787.523950	17.528935	-0.044398	2.915126
228.603668	2779.457830	17.533939	-0.044393	2.911222
228.339741	2771.489694	17.538944	-0.044338	2.907346
228.196147	2763.527400	17.543949	-0.044306	2.903474
228.161248	2755.573417	17.548954	-0.044295	2.899607
228.093408	2747.599732	17.553959	-0.044277	2.895723
228.288361	2739.596740	17.558963	-0.044308	2.891834
228.137759	2731.615960	17.563968	-0.044275	2.887932
228.119352	2723.658148	17.568973	-0.044266	2.884043
228.117016	2715.689520	17.573978	-0.044261	2.880144
228.032285	2707.728789	17.578983	-0.044240	2.876240
227.950108	2699.727116	17.583987	-0.044219	2.872310
227.978729	2691.716397	17.588992	-0.044219	2.868376
227.934710	2683.733053	17.593997	-0.044206	2.864446
227.867116	2675.801340	17.599002	-0.044188	2.860535
227.821214	2667.817350	17.604007	-0.044175	2.856594
228.083038	2659.795772	17.609011	-0.044218	2.852647
227.995389	2651.822779	17.614016	-0.044197	2.848698
227.765227	2643.870731	17.619021	-0.044149	2.844746
227.779317	2635.917241	17.624026	-0.044146	2.840802
227.744733	2627.933215	17.629031	-0.044135	2.836834
227.788452	2619.935156	17.634035	-0.044138	2.832858
227.660026	2611.935988	17.639040	-0.044109	2.828866
227.704588	2603.936552	17.644045	-0.044112	2.824879
227.592893	2596.007487	17.649050	-0.044086	2.820911
227.438331	2588.027815	17.654055	-0.044052	2.816911
227.539095	2580.026515	17.659059	-0.044065	2.812908
227.391910	2572.042672	17.664064	-0.044033	2.808895
227.318240	2564.087934	17.669069	-0.044014	2.804894
227.628475	2556.112072	17.674074	-0.044067	2.800900
227.488549	2548.142474	17.679079	-0.044035	2.796876
227.435319	2540.163872	17.684083	-0.044020	2.792848
227.527080	2532.144804	17.689088	-0.044032	2.788801
227.558545	2524.144942	17.694093	-0.044033	2.784755
227.428730	2516.235787	17.699098	-0.044004	2.780740
227.172250	2508.272969	17.704103	-0.043951	2.776684
227.213879	2500.273011	17.709107	-0.043953	2.772620
227.175484	2492.284919	17.714112	-0.043941	2.768552
226.973910	2484.331371	17.719117	-0.043898	2.764486
226.839856	2476.405548	17.724122	-0.043868	2.760432
226.932145	2468.385516	17.729127	-0.043880	2.756338
226.998091	2460.346935	17.734131	-0.043887	2.752226
226.979442	2452.323608	17.739136	-0.043879	2.748111
226.860179	2444.370966	17.744141	-0.043851	2.744020
226.577074	2436.470251	17.749146	-0.043793	2.739939
226.749644	2428.462673	17.754151	-0.043820	2.735826
226.890125	2420.476290	17.759155	-0.043841	2.731715
226.640643	2412.512569	17.764160	-0.043790	2.727585
226.582190	2404.536497	17.769165	-0.043774	2.723455
226.574621	2396.580937	17.774170	-0.043767	2.719332
226.536727	2388.621832	17.779175	-0.043755	2.715199
226.618790	2380.626903	17.784179	-0.043765	2.711048
226.449457	2372.638333	17.789184	-0.043728	2.706879
226.413459	2364.683860	17.794189	-0.043716	2.702730
226.394590	2356.738367	17.799194	-0.043708	2.698580
226.439299	2348.741975	17.804199	-0.043711	2.694401
226.588452	2340.732860	17.809203	-0.043734	2.690215
226.311644	2332.799462	17.814208	-0.043677	2.686036
226.178297	2324.829152	17.819213	-0.043647	2.681839
226.216968	2316.888487	17.824218	-0.043649	2.677663
226.005767	2308.893444	17.829223	-0.043604	2.673435
225.837735	2300.900010	17.834227	-0.043568	2.669205
225.866214	2292.914888	17.839232	-0.043568	2.664985
225.927234	2284.951388	17.844237	-0.043574	2.660771
225.820511	2276.993896	17.849242	-0.043549	2.656543
225.893661	2268.985439	17.854247	-0.043558	2.652293
225.854355	2261.010585	17.859251	-0.043545	2.648047
225.850060	2253.040150	17.864256	-0.043539	2.643799
225.703688	2245.093558	17.869261	-0.043507	2.639547
225.719640	2237.146873	17.874266	-0.043505	2.635299
225.800240	2229.128135	17.879271	-0.043515	2.631009
225.769754	2221.163469	17.884275	-0.043504	2.626735
225.779264	2213.185937	17.889280	-0.043500	2.622449
225.875504	2205.227213	17.894285	-0.043513	2.618172
225.729631	2197.280221	17.899290	-0.043481	2.613878
225.508785	2189.286072	17.904295	-0.043435	2.609546
225.630302	2181.328756	17.909299	-0.043452	2.605251
225.477868	2173.384947	17.914304	-0.043418	2.600937
225.173864	2165.437110	17.919309	-0.043357	2.596603
225.219911	2157.335290	17.924314	-0.043360	2.592202
225.148299	2149.286563	17.929319	-0.043342	2.587815
225.288744	2141.340457	17.934323	-0.043363	2.583490
225.278655	2133.408773	17.939328	-0.043356	2.579156
225.167761	2125.467765	17.944333	-0.043330	2.574803
225.152847	2117.522467	17.949338	-0.043322	2.570446
224.955148	2109.569681	17.954343	-0.043280	2.566065
225.081839	2101.623340	17.959347	-0.043298	2.561703
225.010847	2093.659426	17.964352	-0.043280	2.557310
224.855124	2085.697087	17.969357	-0.043246	2.552904
224.869527	2077.714292	17.974362	-0.043243	2.548491
224.799811	2069.737419	17.979367	-0.043225	2.544068
224.824458	2061.784366	17.984371	-0.043225	2.539657
224.667952	2053.843516	17.989376	-0.043190	2.535233
224.613994	2045.848340	17.994381	-0.043175	2.530777
224.876855	2037.852193	17.999386	-0.043219	2.526336
224.916723	2029.891528	18.004391	-0.043221	2.521891
224.633077	2021.980798	18.009395	-0.043163	2.517443
224.710206	2013.995588	18.014400	-0.043172	2.512971
224.667687	2005.995510	18.019405	-0.043159	2.508474
224.885868	1998.010569	18.024410	-0.043195	2.503996
224.760816	1990.065255	18.029415	-0.043166	2.499508
224.709512	1982.149881	18.034419	-0.043152	2.495034
224.415980	1974.166789	18.039424	-0.043092	2.490496
224.571487	1966.191391	18.044429	-0.043116	2.485987
224.601660	1958.246082	18.049434	-0.043116	2.481477
224.481403	1950.293352	18.054439	-0.043089	2.476944
224.448012	1942.327519	18.059443	-0.043077	2.472402
224.311608	1934.362185	18.064448	-0.043047	2.467844
224.111837	1926.409833	18.069453	-0.043004	2.463280
224.206692	1918.442511	18.074458	-0.043017	2.458721
224.226489	1910.475285	18.079463	-0.043015	2.454148
224.117887	1902.500690	18.084467	-0.042990	2.449553
223.913213	1894.564566	18.089472	-0.042947	2.444964
224.019732	1886.603335	18.094477	-0.042961	2.440375
224.085495	1878.647005	18.099482	-0.042969	2.435777
224.022794	1870.604743	18.104487	-0.042952	2.431111
223.984558	1862.638368	18.109491	-0.042939	2.426482
223.734978	1854.710085	18.114496	-0.042888	2.421850
223.726370	1846.759568	18.119501	-0.042881	2.417215
223.746532	1838.807930	18.124506	-0.042880	2.412572
223.513006	1830.843733	18.129511	-0.042831	2.407894
223.682062	1822.867107	18.134515	-0.042857	2.403230
223.537699	1814.944967	18.139520	-0.042825	2.398565
223.464482	1806.995711	18.144525	-0.042807	2.393880
223.580052	1799.015663	18.149530	-0.042823	2.389183
223.459397	1791.056721	18.154535	-0.042795	2.384470
223.357443	1783.113972	18.159539	-0.042771	2.379759
223.736015	1775.119869	18.164544	-0.042837	2.375047
223.616985	1767.160792	18.169549	-0.042809	2.370306
223.435456	1759.236070	18.174554	-0.042770	2.365571
223.420932	1751.269271	18.179559	-0.042762	2.360815
223.354401	1743.355535	18.184563	-0.042745	2.356077
223.056745	1735.390636	18.189568	-0.042684	2.351280
222.929338	1727.414711	18.194573	-0.042655	2.346480
223.252994	1719.440406	18.199578	-0.042711	2.341708
223.162994	1711.484506	18.204583	-0.042689	2.336904
223.051112	1703.545151	18.209587	-0.042663	2.332098
222.868564	1695.604805	18.214592	-0.042624	2.327276
222.817844	1687.638632	18.219597	-0.042609	2.322439
222.898510	1679.705763	18.224602	-0.042619	2.317622
222.942702	1671.714960	18.229607	-0.042622	2.312758
222.778827	1663.791131	18.234611	-0.042586	2.307907
222.679837	1655.832599	18.239616	-0.042563	2.303029
222.491606	1647.898911	18.244621	-0.042522	2.298149
222.652594	1639.944319	18.249626	-0.042547	2.293275
222.548660	1631.968541	18.254631	-0.042523	2.288356
222.693081	1624.005544	18.259635	-0.042545	2.283455
222.435540	1616.102433	18.264640	-0.042491	2.278546
222.414152	1608.131774	18.269645	-0.042482	2.273604
222.255685	1600.133908	18.274650	-0.042448	2.268623
222.363096	1592.157416	18.279655	-0.042462	2.263668
222.475920	1584.217299	18.284659	-0.042478	2.258725
222.198597	1576.307320	18.289664	-0.042422	2.253755
222.085553	1568.344556	18.294669	-0.042395	2.248756
222.130040	1560.396468	18.299674	-0.042399	2.243769
222.083617	1552.456650	18.304679	-0.042385	2.238768
222.087516	1544.525329	18.309683	-0.042380	2.233766
222.167545	1536.553989	18.314688	-0.042390	2.228734
222.122672	1528.593976	18.319693	-0.042377	2.223686
221.998242	1520.695633	18.324698	-0.042348	2.218659
221.825476	1512.752242	18.329703	-0.042311	2.213588
221.869883	1504.785833	18.334707	-0.042314	2.208510
221.704786	1496.863333	18.339712	-0.042278	2.203429
221.776569	1488.916037	18.344717	-0.042286	2.198342
221.921104	1480.961495	18.349722	-0.042308	2.193245
221.418747	1473.034076	18.354727	-0.042210	2.188095
221.452964	1465.082465	18.359731	-0.042211	2.182966
221.547813	1457.117036	18.364736	-0.042223	2.177822
221.562945	1449.157628	18.369741	-0.042221	2.172662
221.482097	1441.225244	18.374746	-0.042201	2.167498
221.434534	1433.281696	18.379751	-0.042187	2.162318
221.336664	1425.384670	18.384755	-0.042163	2.157151
221.209949	1417.450489	18.389760	-0.042135	2.151944
221.264814	1409.471594	18.394765	-0.042140	2.146713
221.287409	1401.543254	18.399770	-0.042139	2.141499
220.979868	1393.636635	18.404775	-0.042077	2.136256
220.928575	1385.684762	18.409779	-0.042062	2.130993
220.908133	1377.743170	18.414784	-0.042053	2.125728
220.868765	1369.812010	18.419789	-0.042040	2.120455
220.845775	1361.902440	18.424794	-0.042031	2.115184
220.772265	1353.875824	18.429799	-0.042012	2.109817
220.882687	1345.925970	18.434803	-0.042028	2.104506
220.707886	1338.028791	18.439808	-0.041990	2.099189
220.602610	1330.095772	18.444813	-0.041965	2.093841
220.569138	1322.164565	18.449818	-0.041954	2.088487
220.656462	1314.208243	18.454823	-0.041965	2.083115
220.673536	1306.300290	18.459827	-0.041963	2.077755
220.664931	1298.363936	18.464832	-0.041956	2.072359
220.651765	1290.413223	18.469837	-0.041949	2.066938
220.531223	1282.519120	18.474842	-0.041921	2.061531
220.329758	1274.601669	18.479847	-0.041878	2.056086
220.488848	1266.646590	18.484851	-0.041903	2.050637
220.436238	1258.715282	18.489856	-0.041888	2.045169
220.284773	1250.816568	18.494861	-0.041855	2.039698
220.250615	1242.909052	18.499866	-0.041843	2.034218
220.290684	1234.920994	18.504871	-0.041845	2.028675
220.245468	1226.995274	18.509875	-0.041832	2.023152
219.967900	1219.114360	18.514880	-0.041775	2.017620
219.986435	1211.163373	18.519885	-0.041773	2.012055
220.118594	1203.219295	18.524890	-0.041793	2.006492
219.854632	1195.328393	18.529895	-0.041739	2.000909
219.978595	1187.401669	18.534899	-0.041757	1.995325
219.972108	1179.462675	18.539904	-0.041750	1.989704
219.841288	1171.548793	18.544909	-0.041721	1.984071
219.847246	1163.642990	18.549914	-0.041717	1.978443
219.569383	1155.741752	18.554919	-0.041660	1.972771
219.527933	1147.814180	18.559923	-0.041647	1.967089
219.490221	1139.896587	18.564928	-0.041635	1.961399
219.344814	1132.003389	18.569933	-0.041603	1.955698
219.462271	1124.015980	18.574938	-0.041619	1.949940
219.322526	1116.099263	18.579943	-0.041588	1.944189
219.417353	1108.170142	18.584947	-0.041601	1.938437
219.463280	1100.252347	18.589952	-0.041604	1.932672
219.258078	1092.354603	18.594957	-0.041561	1.926875
219.046270	1084.473044	18.599962	-0.041516	1.921073
219.152419	1076.535179	18.604967	-0.041531	1.915247
219.011160	1068.631951	18.609971	-0.041500	1.909401
219.005541	1060.714348	18.614976	-0.041494	1.903541
218.886432	1052.822774	18.619981	-0.041466	1.897670
219.080515	1044.877347	18.624986	-0.041497	1.891776
218.950858	1036.964191	18.629991	-0.041468	1.885851
218.929679	1029.072358	18.634995	-0.041459	1.879935
219.014665	1021.166352	18.640000	-0.041470	1.874003
218.849030	1013.247879	18.645005	-0.041434	1.868013
218.719936	1005.368280	18.650010	-0.041405	1.862038
218.505567	997.481098	18.655015	-0.041360	1.856027
218.479643	989.563922	18.660019	-0.041350	1.849997
218.470142	981.655338	18.665024	-0.041343	1.843955
218.325300	973.772691	18.670029	-0.041311	1.837897
218.442638	965.860395	18.675034	-0.041327	1.831827
218.354057	957.948113	18.680039	-0.041306	1.825712
218.440008	950.043519	18.685043	-0.041317	1.819604
218.348243	942.161281	18.690048	-0.041294	1.813472
218.203968	934.270269	18.695053	-0.041262	1.807305
218.205709	926.394243	18.700058	-0.041258	1.801146
218.182401	918.496956	18.705063	-0.041248	1.794947
218.099848	910.542707	18.710067	-0.041228	1.788674
218.015045	902.662298	18.715072	-0.041207	1.782437
218.013275	894.775366	18.720077	-0.041201	1.776183
218.181488	886.856213	18.725082	-0.041228	1.769903
217.718814	879.035414	18.730087	-0.041136	1.763600
217.681384	871.164530	18.735091	-0.041124	1.757287
217.686068	863.263606	18.740096	-0.041120	1.750933
217.670851	855.363732	18.745101	-0.041112	1.744554
217.513215	847.521567	18.750106	-0.041078	1.738180
217.447027	839.622071	18.755111	-0.041060	1.731748
217.380490	831.747599	18.760115	-0.041043	1.725312
217.507998	823.856417	18.765120	-0.041061	1.718863
217.426382	815.978521	18.770125	-0.041041	1.712374
217.432484	808.080638	18.775130	-0.041037	1.705855
217.184352	800.232696	18.780135	-0.040986	1.699320
217.136088	792.365953	18.785139	-0.040972	1.692769
217.195828	784.464993	18.790144	-0.040978	1.686179
217.057497	776.615953	18.795149	-0.040947	1.679580
217.153330	768.751083	18.800154	-0.040960	1.672973
217.006479	760.873613	18.805159	-0.040927	1.666297
216.999652	753.016930	18.810163	-0.040921	1.659630
216.942426	745.169240	18.815168	-0.040905	1.652937
216.913419	737.279806	18.820173	-0.040895	1.646185
216.792724	729.459459	18.825178	-0.040867	1.639452
216.493899	721.615027	18.830183	-0.040806	1.632646
216.585323	713.684853	18.835187	-0.040818	1.625791
216.707152	705.821781	18.840192	-0.040836	1.618970
216.455127	697.985755	18.845197	-0.040784	1.612091
216.496923	690.121840	18.850202	-0.040787	1.605200
216.418298	682.291651	18.855207	-0.040767	1.598291
216.498821	674.425893	18.860211	-0.040777	1.591344
216.490377	666.578149	18.865216	-0.040770	1.584369
216.230862	658.775182	18.870221	-0.040717	1.577368
216.426285	650.892461	18.875226	-0.040748	1.570329
216.200725	643.088778	18.880231	-0.040701	1.563269
216.129404	635.275077	18.885235	-0.040683	1.556190
215.914104	627.440557	18.890240	-0.040638	1.549039
215.877348	619.590394	18.895245	-0.040626	1.541866
215.670354	611.792978	18.900250	-0.040582	1.534683
215.487125	603.964816	18.905255	-0.040543	1.527442
215.478329	596.131554	18.910259	-0.040536	1.520187
215.585232	588.296335	18.915264	-0.040551	1.512913
215.403624	580.472852	18.920269	-0.040512	1.505571
215.417331	572.658572	18.925274	-0.040510	1.498232
215.371311	564.824447	18.930279	-0.040496	1.490829
215.225356	557.038988	18.935283	-0.040464	1.483419
215.241797	549.229642	18.940288	-0.040462	1.475975
215.087602	541.369788	18.945293	-0.040428	1.468418
215.203321	533.545582	18.950298	-0.040445	1.460898
215.121285	525.754217	18.955303	-0.040424	1.453340
214.964528	517.971532	18.960307	-0.040390	1.445739
214.867678	510.198511	18.965312	-0.040367	1.438117
214.760674	502.399861	18.970317	-0.040342	1.430428
214.758039	494.610346	18.975322	-0.040336	1.422723
214.618158	486.837557	18.980327	-0.040305	1.414970
214.575128	479.043447	18.985331	-0.040292	1.407168
214.501969	471.275658	18.990336	-0.040274	1.399345
214.527235	463.478607	18.995341	-0.040273	1.391465
214.363372	455.716270	19.000346	-0.040238	1.383543
214.442950	447.926034	19.005351	-0.040248	1.375589
214.589657	440.129349	19.010355	-0.040270	1.367593
214.397449	432.404041	19.015360	-0.040229	1.359565
214.081683	424.687838	19.020365	-0.040165	1.351478
214.147464	416.909789	19.025370	-0.040172	1.343344
214.103394	409.158361	19.030375	-0.040159	1.335169
213.999638	401.416164	19.035379	-0.040135	1.326943
214.002827	393.687852	19.040384	-0.040131	1.318700
213.903561	385.864286	19.045389	-0.040107	1.310283
213.925405	378.083005	19.050394	-0.040106	1.301880
213.706934	370.391109	19.055399	-0.040060	1.293476
213.651020	362.662851	19.060403	-0.040045	1.285007
213.610486	354.971492	19.065408	-0.040032	1.276526
213.267525	347.293170	19.070413	-0.039964	1.267945
213.368061	339.574063	19.075418	-0.039977	1.259344
213.291630	331.869349	19.080423	-0.039958	1.250666
213.187890	324.189756	19.085427	-0.039934	1.241951
213.083148	316.512229	19.090432	-0.039909	1.233177
213.059629	308.791018	19.095437	-0.039900	1.224305
213.058473	301.117973	19.100442	-0.039895	1.215428
212.728620	293.474520	19.105447	-0.039828	1.206456
212.894408	285.780231	19.110451	-0.039854	1.197455
212.932879	278.106359	19.115456	-0.039857	1.188385
212.639346	270.490412	19.120461	-0.039797	1.179247
212.651345	262.838671	19.125466	-0.039794	1.170057
212.463448	255.213930	19.130471	-0.039754	1.160786
212.406274	247.572337	19.135475	-0.039739	1.151447
212.231434	239.944589	19.140480	-0.039701	1.142023
211.965019	232.350200	19.145485	-0.039647	1.132543
211.932580	224.729988	19.150490	-0.039636	1.123001
211.877306	217.129595	19.155495	-0.039621	1.113397
211.782828	209.535897	19.160499	-0.039598	1.103709
211.829067	201.940579	19.165504	-0.039602	1.093965
211.526812	194.395220	19.170509	-0.039541	1.084120
211.399396	186.852239	19.175514	-0.039512	1.074227
211.371568	179.265625	19.180519	-0.039502	1.064208
211.264379	171.729558	19.185523	-0.039477	1.054142
210.977231	164.231480	19.190528	-0.039419	1.043988
210.991459	156.687659	19.195533	-0.039417	1.033744
210.869508	149.185180	19.200538	-0.039389	1.023421
210.314545	141.766642	19.205543	-0.039281	1.013005
210.189493	134.274079	19.210547	-0.039253	1.002482
209.689662	126.856378	19.215552	-0.039155	0.991861
209.027302	119.444406	19.220557	-0.039027	0.981092
208.661656	112.023443	19.225562	-0.038954	0.970265
208.198265	104.628678	19.230567	-0.038863	0.959329
207.751816	97.243540	19.235571	-0.038775	0.948286
207.226695	89.887898	19.240576	-0.038672	0.937136
206.811685	82.517637	19.245581	-0.038590	0.925859
206.308713	75.196171	19.250586	-0.038492	0.914493
205.714163	67.871524	19.255591	-0.038376	0.902955
205.159463	60.804412	19.260595	-0.038269	0.891685