Fri Mar 12 13:22:04 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.388863	-0.017406	0.000000	-0.000017	0.720877

0.239793	0.010477	0.005005	0.000011	0.720880
0.274258	0.006035	0.010010	0.000005	0.720883
0.171384	0.020734	0.015014	0.000024	0.720876
0.271704	0.008055	0.020019	0.000005	0.720886
0.222048	0.012563	0.025024	0.000014	0.720878
0.139639	0.027862	0.030029	0.000030	0.720879
0.348641	-0.007661	0.035034	-0.000009	0.720882
0.183889	0.018414	0.040038	0.000021	0.720876
0.366829	-0.009375	0.045043	-0.000013	0.720885
0.241420	0.011202	0.050048	0.000011	0.720882
0.303790	-0.000907	0.055053	-0.000001	0.720880
0.396786	-0.016844	0.060058	-0.000018	0.720881
0.401139	-0.019097	0.065062	-0.000019	0.720878
0.462119	-0.027072	0.070067	-0.000030	0.720884
0.460644	-0.070964	0.075072	-0.000030	0.720797
0.381914	-0.186261	0.080077	-0.000015	0.720543
0.350122	-0.180055	0.085082	-0.000010	0.720544
0.142316	-0.145557	0.090086	0.000029	0.720539
0.389668	-0.183472	0.095091	-0.000017	0.720551
0.188271	-0.151859	0.100096	0.000021	0.720542
0.047574	-0.127211	0.105101	0.000047	0.720542
0.154128	-0.249102	0.110106	0.000027	0.720339
0.273715	-0.330212	0.115110	0.000005	0.720221
0.454858	-0.356339	0.120115	-0.000029	0.720233
0.102975	-0.298480	0.125120	0.000036	0.720224
0.242847	-0.321934	0.130125	0.000010	0.720227
0.293829	-0.430160	0.135130	0.000001	0.720032
0.133957	-0.469676	0.140134	0.000031	0.719898
0.052023	-0.450817	0.145139	0.000046	0.719906
0.132128	-0.467985	0.150144	0.000031	0.719900
0.119866	-0.506568	0.155149	0.000033	0.719820
0.104053	-0.612860	0.160154	0.000036	0.719605
0.031458	-0.603228	0.165158	0.000050	0.719598
0.103096	-0.611404	0.170163	0.000037	0.719608
-0.129969	-0.637686	0.175168	0.000080	0.719474
-0.038160	-0.754187	0.180173	0.000063	0.719276
0.065036	-0.772656	0.185178	0.000044	0.719276
0.113806	-0.785626	0.190182	0.000035	0.719268
0.018186	-0.905788	0.195187	0.000053	0.718997
0.136701	-0.944827	0.200192	0.000030	0.718962
-0.043423	-0.912164	0.205197	0.000064	0.718963
0.065908	-1.045082	0.210202	0.000044	0.718739
-0.107956	-1.062726	0.215206	0.000076	0.718643
0.114659	-1.096928	0.220211	0.000035	0.718654
0.101616	-1.211600	0.225216	0.000037	0.718423
-0.091573	-1.211274	0.230221	0.000073	0.718356
0.108670	-1.246160	0.235226	0.000036	0.718357
-0.030174	-1.394637	0.240230	0.000062	0.718015
-0.155650	-1.368112	0.245235	0.000085	0.718024
-0.169542	-1.423481	0.250240	0.000088	0.717909
-0.198964	-1.520779	0.255245	0.000093	0.717707
-0.229163	-1.513041	0.260250	0.000099	0.717711
-0.180339	-1.655631	0.265254	0.000090	0.717447
-0.006386	-1.715797	0.270259	0.000057	0.717389
-0.192217	-1.743331	0.275264	0.000092	0.717269
-0.276543	-1.821288	0.280269	0.000108	0.717085
-0.142885	-1.852879	0.285274	0.000083	0.717070
-0.121634	-2.017296	0.290278	0.000079	0.716752
-0.373685	-1.966967	0.295283	0.000126	0.716763
-0.350893	-2.100880	0.300288	0.000122	0.716506
-0.154962	-2.164136	0.305293	0.000085	0.716450
-0.331878	-2.233218	0.310298	0.000118	0.716251
-0.406114	-2.282344	0.315302	0.000132	0.716127
-0.442570	-2.339528	0.320307	0.000139	0.716001
-2.059012	-2.112054	0.325312	0.000440	0.715881
-1.931495	-2.155300	0.330317	0.000416	0.715840
-3.201677	-2.076621	0.335322	0.000652	0.715548
-3.632477	-2.001817	0.340326	0.000733	0.715544
-3.108375	-2.099917	0.345331	0.000635	0.715535
-3.794696	-2.131159	0.350336	0.000763	0.715230
-4.352280	-2.031759	0.355341	0.000867	0.715231
-4.401318	-2.018784	0.360346	0.000876	0.715239
-4.286369	-2.154902	0.365350	0.000854	0.715010
-5.244368	-2.033333	0.370355	0.001033	0.714912
-5.218295	-2.039994	0.375360	0.001028	0.714908
-4.925937	-2.092010	0.380365	0.000973	0.714908
-5.608904	-2.112302	0.385370	0.001101	0.714627
-6.224236	-2.013893	0.390374	0.001215	0.714604
-5.931166	-2.060691	0.395379	0.001161	0.714615
-5.984999	-2.054885	0.400384	0.001171	0.714608
-6.743369	-2.047727	0.405389	0.001312	0.714354
-7.021976	-2.034765	0.410394	0.001364	0.714281
-6.949043	-2.051974	0.415398	0.001350	0.714272
-6.931458	-2.051188	0.420403	0.001347	0.714280
-7.124576	-2.018915	0.425408	0.001383	0.714276
-7.438296	-2.111453	0.430413	0.001441	0.713981
-7.656844	-2.076769	0.435418	0.001482	0.713973
-8.217761	-1.981440	0.440422	0.001586	0.713964
-7.442228	-2.113573	0.445427	0.001442	0.713976
-7.733167	-2.065481	0.450432	0.001496	0.713968
-8.788366	-2.034364	0.455437	0.001692	0.713656
-8.731747	-2.043403	0.460442	0.001682	0.713658
-9.129945	-1.977296	0.465446	0.001756	0.713649
-8.705181	-2.048197	0.470451	0.001677	0.713658
-8.874489	-2.020162	0.475456	0.001708	0.713654
-9.152987	-1.975697	0.480461	0.001760	0.713644
-9.059265	-2.131545	0.485466	0.001743	0.713367
-9.783382	-2.007013	0.490470	0.001878	0.713358
-9.895560	-1.981975	0.495475	0.001898	0.713368
-9.456750	-2.064014	0.500480	0.001817	0.713361
-9.813577	-2.001076	0.505485	0.001883	0.713359
-9.813611	-2.013206	0.510490	0.001883	0.713335
-10.243334	-2.092868	0.515494	0.001963	0.713025
-10.603397	-2.025862	0.520499	0.002030	0.713030
-11.200537	-1.922066	0.525504	0.002141	0.713025
-10.630672	-2.022945	0.530509	0.002035	0.713026
-10.251910	-2.086873	0.535514	0.001965	0.713034
-11.055839	-1.948821	0.540518	0.002114	0.713023
-10.748019	-2.097757	0.545523	0.002057	0.712836
-11.404201	-2.044915	0.550528	0.002179	0.712708
-11.659136	-1.998012	0.555533	0.002227	0.712711
-11.479665	-2.027061	0.560538	0.002193	0.712717
-11.902473	-1.956637	0.565542	0.002272	0.712708
-11.347513	-2.051648	0.570547	0.002169	0.712715
-11.442444	-2.041370	0.575552	0.002186	0.712702
-12.082493	-2.086346	0.580557	0.002306	0.712385
-12.092007	-2.080782	0.585562	0.002307	0.712393
-12.728832	-1.972102	0.590566	0.002426	0.712384
-12.396218	-2.029420	0.595571	0.002364	0.712388
-12.240473	-2.056594	0.600576	0.002335	0.712389
-12.622773	-1.987623	0.605581	0.002406	0.712390
-12.332976	-2.093107	0.610586	0.002352	0.712283
-13.415169	-1.997280	0.615590	0.002554	0.712090
-12.887876	-2.088270	0.620595	0.002455	0.712096
-13.419140	-1.995810	0.625600	0.002554	0.712091
-13.413946	-1.997843	0.630605	0.002553	0.712089
-12.781027	-2.106950	0.635610	0.002436	0.712097
-13.525675	-1.979249	0.640614	0.002574	0.712087
-13.618472	-2.063839	0.645619	0.002591	0.711885
-14.091918	-2.039155	0.650624	0.002680	0.711766
-14.283092	-2.006510	0.655629	0.002715	0.711763
-14.341816	-1.994569	0.660634	0.002726	0.711766
-14.490429	-1.973305	0.665638	0.002754	0.711756
-13.881679	-2.077287	0.670643	0.002640	0.711765
-14.233553	-2.016594	0.675648	0.002706	0.711761
-14.609748	-2.023670	0.680653	0.002776	0.711613
-15.294593	-1.977922	0.685658	0.002903	0.711461
-15.191156	-2.001412	0.690662	0.002884	0.711451
-15.197929	-1.996029	0.695667	0.002885	0.711459
-15.206552	-1.995286	0.700672	0.002887	0.711458
-15.154338	-2.006988	0.705677	0.002877	0.711453
-15.440988	-1.952828	0.710682	0.002931	0.711459
-15.178844	-2.011251	0.715686	0.002882	0.711436
-15.552736	-2.093375	0.720691	0.002951	0.711139
-16.172674	-1.984048	0.725696	0.003067	0.711137
-16.426881	-1.940246	0.730701	0.003114	0.711134
-15.809155	-2.045954	0.735706	0.002999	0.711143
-16.083243	-2.000174	0.740710	0.003050	0.711137
-15.988283	-2.012999	0.745715	0.003032	0.711145
-15.910002	-2.033882	0.750720	0.003018	0.711131
-16.358343	-2.086056	0.755725	0.003101	0.710867
-16.760410	-2.010273	0.760730	0.003176	0.710876
-16.896230	-1.991750	0.765734	0.003201	0.710864
-16.627719	-2.037107	0.770739	0.003151	0.710869
-16.769214	-2.012803	0.775744	0.003178	0.710868
-17.204912	-1.935680	0.780749	0.003259	0.710867
-16.388823	-2.138470	0.785754	0.003107	0.710752
-17.795506	-2.000444	0.790758	0.003369	0.710527
-17.459862	-2.056361	0.795763	0.003306	0.710535
-17.656988	-2.024721	0.800768	0.003343	0.710528
-17.881988	-1.984323	0.805773	0.003385	0.710529
-17.776479	-2.000322	0.810778	0.003365	0.710534
-17.680323	-2.023447	0.815782	0.003347	0.710522
-17.695409	-2.111144	0.820787	0.003350	0.710342
-18.574455	-2.020713	0.825792	0.003514	0.710209
-18.624332	-2.012186	0.830797	0.003523	0.710209
-18.230361	-2.078188	0.835802	0.003450	0.710217
-18.654015	-2.007191	0.840806	0.003529	0.710208
-18.678143	-1.999192	0.845811	0.003533	0.710216
-18.615719	-2.011889	0.850816	0.003521	0.710213
-18.727534	-2.103821	0.855821	0.003542	0.709989
-19.665071	-1.983369	0.860826	0.003717	0.709896
-19.611858	-1.999851	0.865830	0.003707	0.709882
-19.078667	-2.088013	0.870835	0.003608	0.709896
-19.296736	-2.051542	0.875840	0.003648	0.709891
-19.752288	-1.972827	0.880845	0.003733	0.709886
-19.475859	-2.016479	0.885850	0.003681	0.709897
-19.853936	-2.036513	0.890854	0.003752	0.709722
-20.627150	-1.963197	0.895859	0.003896	0.709593
-20.037253	-2.069899	0.900864	0.003786	0.709590
-20.315498	-2.020087	0.905869	0.003838	0.709591
-20.598714	-1.964551	0.910874	0.003890	0.709601
-20.485828	-1.989441	0.915878	0.003869	0.709591
-20.218967	-2.035255	0.920883	0.003820	0.709595
-20.307032	-2.103189	0.925888	0.003836	0.709428
-21.888955	-1.904514	0.930893	0.004131	0.709261
-21.025767	-2.055126	0.935898	0.003970	0.709268
-21.196919	-2.029041	0.940902	0.004002	0.709259
-21.566855	-1.958480	0.945907	0.004071	0.709268
-21.211385	-2.023637	0.950912	0.004004	0.709264
-21.486244	-1.976691	0.955917	0.004056	0.709260
-21.104729	-2.083113	0.960922	0.003985	0.709183
-22.224904	-2.002060	0.965926	0.004193	0.708946
-22.016224	-2.035520	0.970931	0.004154	0.708954
-22.000127	-2.038205	0.975936	0.004151	0.708954
-22.301751	-1.984264	0.980941	0.004207	0.708954
-22.000613	-2.034709	0.985946	0.004151	0.708961
-22.276845	-1.991219	0.990950	0.004203	0.708949
-22.178036	-2.044316	0.995955	0.004184	0.708878
-22.658099	-2.079825	1.000960	0.004274	0.708636
-22.639235	-2.085263	1.005965	0.004270	0.708632
-22.759664	-2.058159	1.010970	0.004293	0.708643
-23.266635	-1.973152	1.015974	0.004387	0.708632
-22.825001	-2.048134	1.020979	0.004305	0.708640
-22.565391	-2.097181	1.025984	0.004256	0.708634
-23.612383	-2.017499	1.030989	0.004451	0.708420
-24.047909	-1.974476	1.035994	0.004532	0.708351
-23.875869	-2.009006	1.040998	0.004500	0.708343
-23.835857	-2.013343	1.046003	0.004493	0.708349
-24.113947	-1.964802	1.051008	0.004545	0.708347
-23.934996	-1.997915	1.056013	0.004511	0.708344
-23.811273	-2.016394	1.061018	0.004488	0.708352
-24.129961	-2.002448	1.066022	0.004548	0.708266
-24.697050	-2.028055	1.071027	0.004653	0.708012
-24.127348	-2.130114	1.076032	0.004547	0.708011
-24.950408	-1.984748	1.081037	0.004700	0.708008
-24.733958	-2.018355	1.086042	0.004660	0.708018
-24.523744	-2.061362	1.091046	0.004621	0.708007
-24.738155	-2.020587	1.096051	0.004661	0.708012
-24.973856	-2.060920	1.101056	0.004705	0.707847
-25.849282	-1.981914	1.106061	0.004868	0.707693
-25.463256	-2.045944	1.111066	0.004796	0.707702
-25.869894	-1.978028	1.116070	0.004871	0.707693
-25.692725	-2.006077	1.121075	0.004839	0.707700
-25.531313	-2.036803	1.126080	0.004808	0.707696
-26.105474	-1.936615	1.131085	0.004915	0.707692
-25.742927	-2.025334	1.136090	0.004848	0.707644
-26.535036	-2.020124	1.141094	0.004995	0.707371
-26.387723	-2.043009	1.146099	0.004968	0.707378
-26.799455	-1.970680	1.151104	0.005044	0.707376
-26.539128	-2.017949	1.156109	0.004996	0.707374
-26.115862	-2.091071	1.161114	0.004917	0.707379
-26.710268	-1.989877	1.166118	0.005028	0.707369
-26.390840	-2.075956	1.171123	0.004968	0.707311
-26.940847	-2.093420	1.176128	0.005071	0.707079
-27.340205	-2.024462	1.181133	0.005145	0.707074
-27.416706	-2.006404	1.186138	0.005159	0.707083
-27.265725	-2.038498	1.191142	0.005131	0.707073
-26.940522	-2.094104	1.196147	0.005071	0.707078
-27.292844	-2.030847	1.201152	0.005136	0.707079
-27.755297	-2.054432	1.206157	0.005222	0.706866
-28.227593	-2.024353	1.211162	0.005310	0.706757
-28.558496	-1.970081	1.216166	0.005372	0.706748
-28.268246	-2.021325	1.221171	0.005318	0.706749
-27.994193	-2.068282	1.226176	0.005267	0.706752
-28.630423	-1.956165	1.231181	0.005385	0.706750
-28.302939	-2.010510	1.236186	0.005324	0.706758
-28.280453	-2.066286	1.241190	0.005320	0.706654
-29.137612	-2.018433	1.246195	0.005480	0.706443
-29.077732	-2.030128	1.251200	0.005469	0.706441
-29.476373	-1.963079	1.256205	0.005543	0.706433
-28.923592	-2.057781	1.261210	0.005440	0.706441
-28.762681	-2.089117	1.266214	0.005410	0.706436
-29.105443	-2.024260	1.271219	0.005474	0.706443
-28.827709	-2.157280	1.276224	0.005422	0.706275
-30.132030	-2.001120	1.281229	0.005665	0.706122
-30.005118	-2.019484	1.286234	0.005641	0.706130
-29.826120	-2.054780	1.291238	0.005608	0.706124
-29.947415	-2.031616	1.296243	0.005630	0.706127
-29.867051	-2.045215	1.301248	0.005615	0.706128
-29.968886	-2.030139	1.306253	0.005634	0.706122
-29.758320	-2.167138	1.311258	0.005595	0.705922
-30.523193	-2.063789	1.316262	0.005738	0.705856
-31.122369	-1.955398	1.321267	0.005849	0.705859
-30.491585	-2.068242	1.326272	0.005732	0.705858
-30.773648	-2.020300	1.331277	0.005784	0.705854
-30.602363	-2.045101	1.336282	0.005752	0.705865
-30.490498	-2.119770	1.341286	0.005731	0.705755
-31.424259	-2.067771	1.346291	0.005905	0.705525
-31.203258	-2.106830	1.351296	0.005864	0.705526
-31.700116	-2.022263	1.356301	0.005957	0.705517
-31.475852	-2.057016	1.361306	0.005915	0.705528
-31.782281	-2.006822	1.366310	0.005972	0.705519
-32.172478	-1.935334	1.371315	0.006044	0.705523
-31.611391	-2.105337	1.376320	0.005940	0.705382
-32.520332	-2.031953	1.381325	0.006109	0.705204
-32.295511	-2.065878	1.386330	0.006067	0.705216
-32.562167	-2.025408	1.391334	0.006117	0.705202
-32.517663	-2.029281	1.396339	0.006109	0.705210
-32.397971	-2.049854	1.401344	0.006086	0.705212
-32.801327	-1.981758	1.406349	0.006161	0.705204
-32.645752	-2.085873	1.411354	0.006133	0.705050
-33.704340	-1.980143	1.416358	0.006330	0.704883
-33.378342	-2.037109	1.421363	0.006269	0.704886
-33.471017	-2.020288	1.426368	0.006286	0.704886
-33.619205	-1.996322	1.431373	0.006314	0.704881
-33.430547	-2.025664	1.436378	0.006279	0.704890
-33.458531	-2.024135	1.441382	0.006284	0.704883
-33.227045	-2.106877	1.446387	0.006241	0.704800
-33.902434	-2.091510	1.451392	0.006366	0.704588
-34.401353	-2.004626	1.456397	0.006459	0.704584
-34.273461	-2.022325	1.461402	0.006435	0.704594
-34.325795	-2.017150	1.466406	0.006445	0.704586
-34.473215	-1.988012	1.471411	0.006473	0.704591
-34.312005	-2.016028	1.476416	0.006443	0.704593
-34.252678	-2.079253	1.481421	0.006432	0.704487
-35.075879	-2.043250	1.486426	0.006585	0.704264
-35.156871	-2.034087	1.491430	0.006600	0.704253
-35.285646	-2.009242	1.496435	0.006624	0.704257
-34.966791	-2.065093	1.501440	0.006565	0.704259
-35.187251	-2.027890	1.506445	0.006606	0.704255
-35.265726	-2.010115	1.511450	0.006620	0.704262
-35.249812	-2.061394	1.516454	0.006617	0.704165
-36.309477	-1.979075	1.521459	0.006814	0.703950
-35.786994	-2.070186	1.526464	0.006717	0.703954
-36.065659	-2.023843	1.531469	0.006769	0.703947
-36.000372	-2.031972	1.536474	0.006757	0.703954
-36.242007	-1.993546	1.541478	0.006802	0.703945
-36.008741	-2.032127	1.546483	0.006758	0.703951
-35.839188	-2.101141	1.551488	0.006727	0.703873
-37.302671	-1.961473	1.556493	0.006999	0.703628
-36.638169	-2.075510	1.561498	0.006876	0.703637
-36.902266	-2.033270	1.566502	0.006925	0.703627
-37.284425	-1.963211	1.571507	0.006996	0.703631
-37.019128	-2.010367	1.576512	0.006946	0.703632
-36.853950	-2.042767	1.581517	0.006916	0.703626
-36.448822	-2.144211	1.586522	0.006840	0.703567
-37.588119	-2.056640	1.591526	0.007052	0.703334
-37.459914	-2.079393	1.596531	0.007029	0.703334
-37.403857	-2.086189	1.601536	0.007018	0.703340
-37.918458	-1.999282	1.606541	0.007114	0.703331
-37.529425	-2.062778	1.611546	0.007041	0.703342
-37.596722	-2.054502	1.616550	0.007054	0.703335
-38.245960	-2.065857	1.621555	0.007175	0.703078
-38.614732	-2.037101	1.626560	0.007243	0.703004
-38.714908	-2.021492	1.631565	0.007262	0.702999
-38.192314	-2.109811	1.636570	0.007165	0.703009
-38.991622	-1.972484	1.641574	0.007314	0.702998
-38.694474	-2.024240	1.646579	0.007258	0.703001
-38.229472	-2.103720	1.651584	0.007172	0.703008
-39.258691	-2.048419	1.656589	0.007363	0.702749
-39.770753	-1.983549	1.661594	0.007459	0.702696
-39.092340	-2.109351	1.666598	0.007332	0.702686
-39.157701	-2.094154	1.671603	0.007345	0.702693
-39.725355	-1.992912	1.676608	0.007450	0.702693
-39.776886	-1.987057	1.681613	0.007460	0.702686
-39.277357	-2.070302	1.686618	0.007367	0.702698
-39.973802	-2.066550	1.691622	0.007496	0.702455
-40.548615	-2.006462	1.696627	0.007603	0.702369
-40.064105	-2.092478	1.701632	0.007513	0.702370
-40.572734	-2.005310	1.706637	0.007608	0.702363
-40.736157	-1.970699	1.711642	0.007638	0.702374
-40.227856	-2.063969	1.716646	0.007544	0.702368
-40.418879	-2.030305	1.721651	0.007579	0.702368
-40.495913	-2.096797	1.726656	0.007594	0.702206
-41.633989	-1.962460	1.731661	0.007805	0.702067
-41.091782	-2.053363	1.736666	0.007704	0.702079
-41.545494	-1.976177	1.741670	0.007789	0.702071
-41.655904	-1.956076	1.746675	0.007809	0.702072
-40.679469	-2.129424	1.751680	0.007628	0.702073
-41.471584	-1.992746	1.756685	0.007775	0.702064
-41.425839	-2.064079	1.761690	0.007767	0.701936
-42.109116	-2.039621	1.766694	0.007894	0.701739
-42.116774	-2.036878	1.771699	0.007895	0.701742
-42.270030	-2.007362	1.776704	0.007924	0.701747
-42.530383	-1.964729	1.781709	0.007972	0.701739
-41.778734	-2.095683	1.786714	0.007832	0.701745
-42.312891	-2.003841	1.791718	0.007932	0.701738
-42.513854	-2.020354	1.796723	0.007969	0.701633
-42.688356	-2.085917	1.801728	0.008002	0.701437
-42.951479	-2.042131	1.806733	0.008051	0.701431
-43.044873	-2.020977	1.811738	0.008068	0.701440
-43.058409	-2.021042	1.816742	0.008070	0.701435
-42.864149	-2.055692	1.821747	0.008034	0.701435
-42.828297	-2.061595	1.826752	0.008028	0.701436
-43.094443	-2.109747	1.831757	0.008077	0.701242
-43.682048	-2.065251	1.836762	0.008187	0.701120
-43.635611	-2.075046	1.841766	0.008178	0.701117
-43.937489	-2.020840	1.846771	0.008234	0.701118
-43.599885	-2.079165	1.851776	0.008171	0.701122
-43.958646	-2.019362	1.856781	0.008238	0.701113
-43.763799	-2.050419	1.861786	0.008202	0.701121
-44.367710	-2.063834	1.866790	0.008314	0.700875
-44.222573	-2.092038	1.871795	0.008287	0.700871
-44.548998	-2.032337	1.876800	0.008348	0.700874
-44.642654	-2.018535	1.881805	0.008365	0.700868
-44.236856	-2.085902	1.886810	0.008290	0.700878
-44.463520	-2.050000	1.891814	0.008332	0.700869
-44.756248	-2.098952	1.896819	0.008386	0.700664
-45.656284	-2.002111	1.901824	0.008554	0.700535
-45.588669	-2.018645	1.906829	0.008541	0.700526
-45.195664	-2.083812	1.911834	0.008468	0.700536
-45.354596	-2.059908	1.916838	0.008498	0.700527
-45.539612	-2.025424	1.921843	0.008532	0.700530
-45.348237	-2.058523	1.926848	0.008497	0.700532
-46.038779	-2.064615	1.931853	0.008625	0.700270
-46.157992	-2.067612	1.936858	0.008647	0.700221
-46.481398	-2.013412	1.941862	0.008708	0.700214
-46.481198	-2.012997	1.946867	0.008707	0.700215
-46.331563	-2.038461	1.951872	0.008680	0.700217
-46.276861	-2.051883	1.956877	0.008669	0.700210
-46.380170	-2.029237	1.961882	0.008689	0.700218
-46.846280	-2.079521	1.966886	0.008775	0.699948
-47.461248	-1.996941	1.971891	0.008890	0.699893
-47.282073	-2.028636	1.976896	0.008857	0.699893
-47.306008	-2.028186	1.981901	0.008861	0.699886
-47.267611	-2.029698	1.986906	0.008854	0.699897
-47.317321	-2.024652	1.991910	0.008863	0.699889
-47.397232	-2.010104	1.996915	0.008878	0.699889
-47.932107	-2.027141	2.001920	0.008978	0.699661

-48.040724	-2.039861	2.011917	0.008998	0.699596
-47.890973	-2.066551	2.021914	0.008970	0.699596
-48.090715	-2.031720	2.031910	0.009007	0.699595
-48.013118	-2.046581	2.041907	0.008993	0.699593
-47.737334	-2.094400	2.051904	0.008941	0.699596
-48.203557	-2.009697	2.061901	0.009028	0.699599
-47.778139	-2.084317	2.071898	0.008949	0.699601
-48.176379	-2.015318	2.081894	0.009023	0.699597
-48.095676	-2.031003	2.091891	0.009008	0.699595
-48.113867	-2.026433	2.101888	0.009011	0.699597
-48.227605	-2.005477	2.111885	0.009032	0.699599
-47.994129	-2.047175	2.121882	0.008989	0.699599
-47.495194	-2.008032	2.131878	0.008896	0.699859
-47.132948	-2.056326	2.141875	0.008828	0.699892
-47.060439	-2.067622	2.151872	0.008815	0.699895
-47.317416	-2.022470	2.161869	0.008863	0.699894
-47.215397	-2.041032	2.171866	0.008844	0.699893
-46.871747	-1.992747	2.181862	0.008780	0.700116
-46.327539	-2.040654	2.191859	0.008678	0.700215
-46.357755	-2.036482	2.201856	0.008684	0.700213
-46.264828	-2.050532	2.211853	0.008667	0.700218
-46.100146	-2.005737	2.221850	0.008636	0.700368
-45.628045	-2.009849	2.231846	0.008548	0.700531
-45.647192	-2.007535	2.241843	0.008552	0.700529
-45.438595	-2.043869	2.251840	0.008513	0.700530
-44.942472	-2.040830	2.261837	0.008420	0.700716
-44.202575	-2.096047	2.271834	0.008283	0.700872
-44.767800	-1.995390	2.281830	0.008388	0.700871
-44.304869	-2.079623	2.291827	0.008302	0.700868
-44.225157	-2.025967	2.301824	0.008287	0.701005
-43.512063	-2.096049	2.311821	0.008154	0.701121
-43.820497	-2.040375	2.321818	0.008211	0.701123
-43.899613	-2.026057	2.331814	0.008226	0.701123
-43.163335	-2.003689	2.341811	0.008089	0.701434
-42.979046	-2.036341	2.351808	0.008054	0.701435
-42.777978	-2.070017	2.361805	0.008017	0.701439
-42.491317	-2.030810	2.371802	0.007964	0.701622
-42.269218	-2.011080	2.381798	0.007922	0.701742
-42.203907	-2.023906	2.391795	0.007910	0.701740
-42.324098	-1.956263	2.401792	0.007932	0.701833
-40.987647	-2.075755	2.411789	0.007684	0.702074
-41.171193	-2.042971	2.421786	0.007718	0.702074
-41.394784	-2.003471	2.431782	0.007759	0.702073
-40.524747	-2.036233	2.441779	0.007597	0.702321
-40.567099	-2.003731	2.451776	0.007605	0.702371
-40.235096	-2.063221	2.461773	0.007543	0.702371
-40.281735	-1.994926	2.471770	0.007552	0.702492
-39.533101	-2.029205	2.481766	0.007413	0.702692
-39.481642	-2.038904	2.491763	0.007403	0.702691
-39.407551	-2.053219	2.501760	0.007389	0.702689
-38.763171	-2.031659	2.511757	0.007269	0.702965
-38.720294	-2.019399	2.521754	0.007261	0.703005
-38.591102	-2.042377	2.531750	0.007237	0.703005
-38.503874	-1.988954	2.541747	0.007221	0.703145
-37.898842	-2.000817	2.551744	0.007108	0.703339
-37.583832	-2.054410	2.561741	0.007049	0.703344
-37.481024	-2.074271	2.571738	0.007030	0.703341
-37.006671	-2.034264	2.581734	0.006942	0.703592
-37.074928	-2.001745	2.591731	0.006955	0.703633
-37.030268	-2.009109	2.601728	0.006946	0.703635
-36.472064	-2.034825	2.611725	0.006842	0.703784
-35.898409	-2.053165	2.621722	0.006735	0.703953
-36.034053	-2.028887	2.631718	0.006761	0.703953
-36.146088	-2.010329	2.641715	0.006782	0.703950
-35.549452	-1.963671	2.651712	0.006670	0.704259
-34.969495	-2.066392	2.661709	0.006562	0.704260
-35.377999	-1.991684	2.671706	0.006638	0.704264
-34.655325	-2.008725	2.681702	0.006504	0.704490
-34.362384	-2.010400	2.691699	0.006449	0.704591
-34.191728	-2.043328	2.701696	0.006418	0.704586
-34.240200	-2.012523	2.711693	0.006426	0.704631
-33.551075	-2.007687	2.721690	0.006298	0.704888
-33.356038	-2.042867	2.731686	0.006262	0.704888
-33.540642	-2.009745	2.741683	0.006296	0.704888
-33.137407	-1.963131	2.751680	0.006221	0.705127
-32.400860	-2.051370	2.761677	0.006084	0.705214
-32.773978	-1.985729	2.771674	0.006153	0.705212
-32.324572	-2.023433	2.781670	0.006070	0.705297
-31.946253	-1.977118	2.791667	0.005999	0.705526
-31.699189	-2.020600	2.801664	0.005953	0.705527
-31.894301	-1.983859	2.811661	0.005989	0.705531
-30.941537	-1.989085	2.821658	0.005812	0.705863
-30.814174	-2.009635	2.831654	0.005788	0.705867
-30.859286	-2.002819	2.841651	0.005797	0.705865
-30.826362	-1.955741	2.851648	0.005790	0.705971
-30.059938	-2.013482	2.861645	0.005648	0.706130
-30.143751	-1.998797	2.871642	0.005663	0.706129
-29.769898	-2.055470	2.881638	0.005594	0.706149
-29.438332	-1.967578	2.891635	0.005532	0.706445
-29.042519	-2.037495	2.901632	0.005458	0.706446
-29.289351	-1.992389	2.911629	0.005504	0.706448
-28.622559	-2.009007	2.921626	0.005380	0.706654
-28.184907	-2.037707	2.931622	0.005299	0.706753
-28.493917	-1.982686	2.941619	0.005356	0.706753
-28.332669	-1.974017	2.951616	0.005326	0.706828
-27.570552	-1.983003	2.961613	0.005184	0.707083
-27.479301	-1.999601	2.971610	0.005167	0.707082
-27.579389	-1.981354	2.981606	0.005186	0.707083
-26.974578	-1.954617	2.991603	0.005073	0.707353
-26.458027	-2.033703	3.001600	0.004977	0.707379
-26.670955	-1.995772	3.011597	0.005016	0.707379
-26.207400	-2.004570	3.021594	0.004930	0.707527
-25.646397	-2.017784	3.031590	0.004826	0.707702
-25.773007	-1.995394	3.041587	0.004849	0.707701
-25.640873	-2.019591	3.051584	0.004825	0.707700
-25.061409	-1.980607	3.061581	0.004717	0.707985
-24.825825	-2.007181	3.071578	0.004673	0.708016
-24.714105	-2.027895	3.081574	0.004652	0.708015
-24.671471	-1.978089	3.091571	0.004644	0.708130
-23.637036	-2.050253	3.101568	0.004451	0.708355
-23.950526	-1.993036	3.111565	0.004510	0.708357
-23.887808	-2.003299	3.121562	0.004498	0.708359
-23.278486	-2.005233	3.131558	0.004384	0.708573
-23.407322	-1.948309	3.141555	0.004408	0.708641
-22.986571	-2.023437	3.151552	0.004330	0.708641
-22.994767	-1.962568	3.161549	0.004332	0.708760
-21.840709	-2.068079	3.171546	0.004117	0.708961
-22.340433	-1.978686	3.181542	0.004210	0.708961
-22.134503	-2.017947	3.191539	0.004171	0.708956
-21.544836	-1.992419	3.201536	0.004062	0.709218
-21.487692	-1.977474	3.211533	0.004051	0.709268
-21.294126	-2.012228	3.221530	0.004015	0.709268
-21.091583	-1.979252	3.231526	0.003977	0.709406
-20.375327	-2.011910	3.241523	0.003844	0.709596
-20.462311	-1.995999	3.251520	0.003860	0.709597
-20.580155	-1.973222	3.261517	0.003882	0.709600
-19.639568	-2.002911	3.271514	0.003707	0.709876
-19.687918	-1.985404	3.281510	0.003716	0.709894
-19.514992	-2.017572	3.291507	0.003683	0.709891
-19.594662	-1.927317	3.301504	0.003698	0.710043
-18.502958	-2.032381	3.311501	0.003495	0.710222
-18.548499	-2.024991	3.321498	0.003503	0.710221
-18.760254	-1.988683	3.331494	0.003543	0.710218
-17.945850	-1.984289	3.341491	0.003391	0.710517
-17.771386	-2.006363	3.351488	0.003359	0.710535
-17.619399	-2.033039	3.361485	0.003330	0.710536
-17.640059	-1.979683	3.371482	0.003334	0.710635
-16.974450	-1.978000	3.381478	0.003210	0.710875
-16.618990	-2.043635	3.391475	0.003144	0.710871
-17.171468	-1.944421	3.401472	0.003247	0.710872
-16.152593	-2.013244	3.411469	0.003057	0.711097
-16.184659	-1.985621	3.421466	0.003063	0.711141
-16.094188	-2.001098	3.431462	0.003046	0.711142
-16.145779	-1.923541	3.441459	0.003056	0.711279
-15.497921	-1.949844	3.451456	0.002935	0.711457
-15.292013	-1.986753	3.461453	0.002897	0.711456
-15.511854	-1.900463	3.471450	0.002937	0.711550
-14.538209	-1.965574	3.481446	0.002756	0.711767
-14.579058	-1.960355	3.491443	0.002764	0.711762
-14.948957	-1.873061	3.501440	0.002833	0.711805
-13.674740	-1.955765	3.511437	0.002595	0.712093
-13.722838	-1.947452	3.521434	0.002604	0.712092
-13.930813	-1.911317	3.531430	0.002643	0.712091
-13.218991	-1.904064	3.541427	0.002510	0.712358
-12.911232	-1.945544	3.551424	0.002453	0.712384
-12.981857	-1.930981	3.561421	0.002466	0.712388
-12.602325	-1.892521	3.571418	0.002396	0.712600
-12.125038	-1.920830	3.581414	0.002307	0.712713
-11.953909	-1.953541	3.591411	0.002275	0.712708
-12.041979	-1.897477	3.601408	0.002291	0.712789
-10.746972	-2.009227	3.611405	0.002050	0.713026
-11.049277	-1.955307	3.621402	0.002106	0.713026
-10.799527	-1.998846	3.631398	0.002060	0.713028
-10.893244	-1.896507	3.641395	0.002077	0.713198
-9.652918	-2.035490	3.651392	0.001846	0.713361
-9.830104	-2.003471	3.661389	0.001879	0.713362
-9.905040	-1.989158	3.671386	0.001893	0.713364
-9.468268	-1.985578	3.681382	0.001812	0.713526
-9.068545	-1.992909	3.691379	0.001737	0.713653
-9.159546	-1.977385	3.701376	0.001754	0.713652
-8.880083	-2.024761	3.711373	0.001702	0.713657
-8.500110	-1.971822	3.721370	0.001631	0.713897
-8.166417	-1.991578	3.731366	0.001569	0.713976
-8.327861	-1.964999	3.741363	0.001599	0.713971
-7.932207	-2.011640	3.751360	0.001526	0.714019
-6.998909	-2.047144	3.761357	0.001352	0.714279
-7.051762	-2.037198	3.771354	0.001362	0.714280
-7.175292	-2.014857	3.781350	0.001385	0.714280
-7.307569	-1.930875	3.791347	0.001409	0.714400
-6.260595	-2.012771	3.801344	0.001214	0.714608
-6.191953	-2.025100	3.811341	0.001201	0.714608
-6.283759	-2.007152	3.821338	0.001219	0.714611
-5.635240	-2.010585	3.831334	0.001098	0.714834
-5.663683	-1.968760	3.841331	0.001103	0.714907
-5.474893	-2.002808	3.851328	0.001068	0.714906
-5.492405	-1.955444	3.861325	0.001071	0.714994
-4.414070	-2.027423	3.871322	0.000870	0.715232
-4.280636	-2.052515	3.881318	0.000845	0.715230
-4.464074	-2.019936	3.891315	0.000880	0.715229
-4.255164	-1.989874	3.901312	0.000841	0.715363
-3.191370	-2.087495	3.911309	0.000643	0.715545
-3.316444	-2.064881	3.921306	0.000666	0.715546
-3.357266	-2.056330	3.931302	0.000673	0.715549
-3.045980	-2.016164	3.941299	0.000615	0.715738
-2.313598	-2.073898	3.951296	0.000479	0.715882
-2.258343	-2.081436	3.961293	0.000469	0.715887
-2.442047	-2.049600	3.971290	0.000503	0.715885
-2.088272	-2.035731	3.981286	0.000437	0.716038
-1.743626	-2.049730	3.991283	0.000373	0.716132
-1.911515	-2.018542	4.001280	0.000404	0.716134
-2.031793	-1.950306	4.011277	0.000426	0.716227
-1.405576	-1.948422	4.021274	0.000310	0.716452
-1.175997	-1.989615	4.031270	0.000267	0.716451
-1.173834	-1.945656	4.041267	0.000267	0.716539
-1.033036	-1.860923	4.051264	0.000240	0.716756
-1.044616	-1.858724	4.061261	0.000242	0.716757
-0.864560	-1.774077	4.071258	0.000209	0.716988
-0.924740	-1.713804	4.081254	0.000220	0.717086
-0.793790	-1.669078	4.091251	0.000195	0.717220
-0.643590	-1.614291	4.101248	0.000167	0.717382
-0.593483	-1.559998	4.111245	0.000158	0.717507
-0.846054	-1.413391	4.121242	0.000205	0.717708
-0.610705	-1.356866	4.131238	0.000161	0.717902
-0.550870	-1.308294	4.141235	0.000150	0.718019
-0.513924	-1.158575	4.151232	0.000143	0.718328
-0.495253	-1.095353	4.161229	0.000139	0.718459
-0.356102	-1.024914	4.171226	0.000113	0.718647
-0.409960	-0.875837	4.181222	0.000123	0.718923
-0.332310	-0.791808	4.191219	0.000109	0.719116
-0.351334	-0.682608	4.201216	0.000112	0.719325
-0.220840	-0.564567	4.211213	0.000088	0.719603
-0.143429	-0.444036	4.221210	0.000073	0.719868
-0.227389	-0.301898	4.231206	0.000089	0.720119
0.077057	-0.222574	4.241203	0.000032	0.720382
-0.111574	-0.051065	4.251200	0.000067	0.720653
-0.175988	0.109455	4.261197	0.000079	0.720947
0.000000	0.237604	4.271194	0.000046	0.721260

-0.178246	0.898476	4.276198	0.000079	0.722497
0.205957	2.092540	4.281203	0.000006	0.724971
0.488733	3.901405	4.286208	-0.000047	0.728600
0.650361	6.279415	4.291213	-0.000079	0.733271
0.995197	9.138117	4.296218	-0.000145	0.738898
1.349278	12.470364	4.301222	-0.000213	0.745388
1.586539	16.282158	4.306227	-0.000260	0.752686
2.094575	20.452590	4.311232	-0.000357	0.760673
2.414657	25.047029	4.316237	-0.000420	0.769298
2.804829	30.006569	4.321242	-0.000496	0.778515
3.448730	35.263103	4.326246	-0.000619	0.788239
4.093876	40.843467	4.331251	-0.000743	0.798421
4.459507	46.777769	4.336256	-0.000815	0.809008
4.873506	52.978795	4.341261	-0.000896	0.819934
5.513485	59.422546	4.346266	-0.001019	0.831199
6.211458	66.072694	4.351270	-0.001154	0.842678
6.983548	72.946015	4.356275	-0.001302	0.854394
7.465421	80.076095	4.361280	-0.001396	0.866288
8.823426	87.235807	4.366285	-0.001654	0.878317
11.509904	94.376539	4.371290	-0.002159	0.890525
11.800966	102.103154	4.376294	-0.002218	0.902826
12.508265	109.903529	4.381299	-0.002355	0.915188
13.174764	117.823348	4.386304	-0.002484	0.927557
14.121242	125.812267	4.391309	-0.002665	0.939942
15.085994	133.915916	4.396314	-0.002850	0.952340
15.930297	142.116842	4.401318	-0.003013	0.964690
16.664536	150.434828	4.406323	-0.003155	0.977026
17.515840	158.818432	4.411328	-0.003319	0.989330
18.384971	167.230931	4.416333	-0.003486	1.001528
19.426069	175.675117	4.421338	-0.003686	1.013666
20.473238	184.138910	4.426342	-0.003886	1.025687
21.261006	192.693210	4.431347	-0.004039	1.037631
22.013380	201.279142	4.436352	-0.004184	1.049473
22.865705	209.868622	4.441357	-0.004349	1.061210
23.481470	218.537139	4.446362	-0.004469	1.072868
24.195143	227.177391	4.451366	-0.004607	1.084386
24.784381	235.850019	4.456371	-0.004723	1.095797
25.586770	244.484997	4.461376	-0.004878	1.107089
25.868438	253.211655	4.466381	-0.004936	1.118269
26.744011	261.828159	4.471386	-0.005105	1.129327
27.359666	270.485971	4.476390	-0.005225	1.140274
28.009687	279.158754	4.481395	-0.005352	1.151143
28.717511	287.797081	4.486400	-0.005489	1.161879
29.103283	296.461581	4.491405	-0.005567	1.172482
29.948054	305.032932	4.496410	-0.005729	1.182971
30.808115	313.613566	4.501414	-0.005895	1.193382
31.380301	322.213320	4.506419	-0.006007	1.203668
31.949245	330.822607	4.511424	-0.006119	1.213877
33.117608	339.297549	4.516429	-0.006342	1.223962
33.704431	347.904151	4.521434	-0.006457	1.234002
33.907396	356.511985	4.526438	-0.006500	1.243889
34.770960	364.997400	4.531443	-0.006667	1.253685
35.594397	373.490952	4.536448	-0.006826	1.263406
36.234596	382.004003	4.541453	-0.006950	1.273040
36.856637	390.505496	4.546458	-0.007072	1.282586
37.411022	399.007935	4.551462	-0.007180	1.292048
37.906473	407.494399	4.556467	-0.007278	1.301414
38.544020	416.031609	4.561472	-0.007403	1.310793
38.916953	424.559069	4.566477	-0.007478	1.320048
39.699948	432.938545	4.571482	-0.007629	1.329153
40.058026	441.389338	4.576486	-0.007701	1.338196
40.403085	449.802078	4.581491	-0.007771	1.347135
41.114090	458.184835	4.586496	-0.007909	1.356048
41.436268	466.581707	4.591501	-0.007974	1.364850
41.912930	474.981504	4.596506	-0.008068	1.373625
42.470562	483.334519	4.601510	-0.008178	1.382310
43.044543	491.703198	4.606515	-0.008290	1.390960
43.599529	500.063774	4.611520	-0.008399	1.399544
44.141897	508.391657	4.616525	-0.008505	1.408040
44.727571	516.742802	4.621530	-0.008620	1.416516
45.086139	525.084150	4.626534	-0.008692	1.424894
45.771320	533.391607	4.631539	-0.008825	1.433243
46.094916	541.733343	4.636544	-0.008891	1.441518
46.647623	550.018111	4.641549	-0.008999	1.449727
47.023916	558.364585	4.646554	-0.009074	1.457921
47.548032	566.644207	4.651558	-0.009177	1.466028
48.066316	574.983583	4.656563	-0.009279	1.474147
48.942009	583.202716	4.661568	-0.009448	1.482163
49.239134	591.500655	4.666573	-0.009509	1.490119
49.969340	599.754978	4.671578	-0.009650	1.498059
50.203059	608.051678	4.676582	-0.009699	1.505921
50.531995	616.358239	4.681587	-0.009765	1.513765
51.037743	624.602300	4.686592	-0.009865	1.521538
51.442721	632.860782	4.691597	-0.009946	1.529269
51.874518	641.129834	4.696602	-0.010032	1.536974
52.655882	649.316708	4.701606	-0.010182	1.544618
53.227309	657.566334	4.706611	-0.010294	1.552250
53.495871	665.845649	4.711616	-0.010350	1.559826
53.499851	674.132200	4.716621	-0.010356	1.567334
54.151363	682.342584	4.721626	-0.010483	1.574832
54.823456	690.517593	4.726630	-0.010613	1.582265
54.994521	698.788385	4.731635	-0.010650	1.589677
55.633010	706.997701	4.736640	-0.010774	1.597066
55.759283	715.241109	4.741645	-0.010803	1.604379
56.216321	723.460213	4.746650	-0.010894	1.611683
56.814310	731.647852	4.751654	-0.011011	1.618947
57.131731	739.865015	4.756659	-0.011075	1.626164
57.853566	748.099470	4.761664	-0.011215	1.633421
58.097941	756.302961	4.766669	-0.011266	1.640553
58.493760	764.491091	4.771674	-0.011345	1.647661
58.742844	772.719642	4.776678	-0.011396	1.654753
58.928794	780.914368	4.781683	-0.011436	1.661778
59.357935	789.099325	4.786688	-0.011522	1.668797
59.995472	797.237068	4.791693	-0.011646	1.675775
60.634869	805.386161	4.796698	-0.011770	1.682734
60.917712	813.588132	4.801702	-0.011828	1.689660
61.090470	821.811205	4.806707	-0.011866	1.696562
61.642541	829.962312	4.811712	-0.011974	1.703425
61.981686	838.153327	4.816717	-0.012042	1.710266
62.396906	846.349278	4.821722	-0.012125	1.717093
62.743928	854.496886	4.826726	-0.012195	1.723845
63.012712	862.669087	4.831731	-0.012250	1.730580
63.294896	870.875741	4.836736	-0.012308	1.737319
64.206675	878.933500	4.841741	-0.012483	1.743991
64.471593	887.140659	4.846746	-0.012538	1.750676
64.717670	895.335946	4.851750	-0.012589	1.757323
65.252290	903.450442	4.856755	-0.012694	1.763917
65.719633	911.609667	4.861760	-0.012786	1.770514
65.872209	919.804534	4.866765	-0.012820	1.777075
66.233684	927.962011	4.871770	-0.012893	1.783608
66.604249	936.136533	4.876774	-0.012967	1.790132
67.160211	944.296877	4.881779	-0.013076	1.796643
67.349069	952.447834	4.886784	-0.013116	1.803079
67.923133	960.550203	4.891789	-0.013229	1.809500
68.368794	968.698960	4.896794	-0.013317	1.815919
68.722712	976.839527	4.901798	-0.013388	1.822298
69.353985	984.947909	4.906803	-0.013511	1.828663
69.621155	993.134912	4.911808	-0.013566	1.835023
69.946263	1001.261714	4.916813	-0.013632	1.841322
70.171617	1009.426890	4.921818	-0.013679	1.847616
70.722627	1017.553682	4.926822	-0.013787	1.853898
71.106598	1025.672415	4.931827	-0.013864	1.860133
71.550963	1033.800274	4.936832	-0.013952	1.866361
71.540810	1042.007764	4.941837	-0.013955	1.872576
71.868603	1050.140265	4.946842	-0.014022	1.878752
72.223547	1058.227138	4.951846	-0.014093	1.884877
72.764676	1066.321310	4.956851	-0.014199	1.891009
73.090214	1074.478772	4.961856	-0.014265	1.897144
73.416103	1082.580642	4.966861	-0.014331	1.903217
73.687478	1090.728121	4.971866	-0.014387	1.909299
74.383309	1098.812708	4.976870	-0.014522	1.915362
74.552269	1106.954215	4.981875	-0.014558	1.921389
74.947206	1115.066959	4.986880	-0.014637	1.927402
75.454517	1123.178662	4.991885	-0.014737	1.933407
75.604320	1131.333285	4.996890	-0.014770	1.939385
75.915115	1139.447413	5.001894	-0.014833	1.945333
76.382308	1147.578466	5.006899	-0.014926	1.951292
76.661291	1155.734311	5.011904	-0.014983	1.957230
76.737589	1163.845521	5.016909	-0.015003	1.963097
77.187598	1171.927160	5.021914	-0.015092	1.968964
77.617677	1180.029316	5.026918	-0.015177	1.974827
77.728787	1188.144089	5.031923	-0.015203	1.980647
78.156383	1196.244696	5.036928	-0.015288	1.986474
78.405734	1204.361482	5.041933	-0.015340	1.992276
78.880993	1212.444588	5.046938	-0.015433	1.998061
79.095199	1220.557775	5.051942	-0.015479	2.003823
79.592648	1228.633495	5.056947	-0.015576	2.009572
79.998293	1236.763018	5.061952	-0.015657	2.015332
80.230463	1244.867120	5.066957	-0.015706	2.021040
80.632156	1252.961954	5.071962	-0.015786	2.026743
80.976384	1261.101402	5.076966	-0.015855	2.032455
81.071395	1269.223625	5.081971	-0.015878	2.038114
81.221766	1277.339420	5.086976	-0.015912	2.043758
81.611215	1285.410608	5.091981	-0.015989	2.049379
81.985919	1293.512343	5.096986	-0.016064	2.055005
82.543513	1301.574831	5.101990	-0.016174	2.060607
82.779936	1309.670889	5.106995	-0.016223	2.066184
82.899535	1317.817277	5.112000	-0.016250	2.071769
83.238831	1325.902185	5.117005	-0.016319	2.077319
83.578506	1333.983905	5.122010	-0.016387	2.082852
84.081677	1342.052803	5.127014	-0.016486	2.088377
84.381259	1350.150408	5.132019	-0.016547	2.093888
84.932546	1358.231478	5.137024	-0.016655	2.099397
85.227055	1366.309647	5.142029	-0.016715	2.104864
85.515453	1374.454871	5.147034	-0.016775	2.110362
85.765918	1382.605350	5.152038	-0.016826	2.115845
85.840559	1390.684615	5.157043	-0.016846	2.121250
86.488823	1398.717903	5.162048	-0.016972	2.126665
86.550792	1406.826862	5.167053	-0.016988	2.132060
86.739412	1414.937293	5.172058	-0.017029	2.137455
87.278617	1422.980513	5.177062	-0.017135	2.142825
87.528021	1431.059773	5.182067	-0.017186	2.148178
87.774163	1439.191449	5.187072	-0.017237	2.153551
87.985559	1447.261442	5.192077	-0.017282	2.158868
88.257165	1455.344823	5.197082	-0.017338	2.164186
88.403752	1463.446967	5.202086	-0.017370	2.169491
88.659028	1471.534657	5.207091	-0.017423	2.174784
89.157023	1479.594791	5.212096	-0.017521	2.180068
89.491634	1487.646694	5.217101	-0.017589	2.185319
89.685736	1495.779451	5.222106	-0.017630	2.190597
90.258017	1503.848932	5.227110	-0.017742	2.195856
90.678863	1511.886743	5.232115	-0.017826	2.201068
90.713120	1520.016471	5.237120	-0.017837	2.206292
91.068892	1528.068740	5.242125	-0.017909	2.211482
91.586115	1536.129224	5.247130	-0.018010	2.216681
91.941727	1544.210397	5.252134	-0.018082	2.221865
92.081177	1552.308364	5.257139	-0.018113	2.227029
92.451222	1560.399340	5.262144	-0.018187	2.232197
92.825972	1568.456117	5.267149	-0.018262	2.237331
93.031416	1576.535295	5.272154	-0.018306	2.242453
93.260549	1584.629553	5.277158	-0.018354	2.247575
93.781928	1592.689068	5.282163	-0.018456	2.252689
94.073685	1600.795485	5.287168	-0.018516	2.257800
94.117656	1608.891002	5.292173	-0.018529	2.262872
94.636971	1616.936038	5.297178	-0.018631	2.267942
94.711940	1625.118178	5.302182	-0.018651	2.273047
94.882469	1633.179898	5.307187	-0.018688	2.278075
95.602241	1641.172360	5.312192	-0.018827	2.283095
95.658008	1649.245481	5.317197	-0.018843	2.288097
96.008475	1657.322043	5.322202	-0.018913	2.293116
96.298677	1665.393657	5.327206	-0.018972	2.298115
96.590289	1673.427219	5.332211	-0.019032	2.303081
97.141253	1681.471793	5.337216	-0.019140	2.308064
97.473928	1689.554851	5.342221	-0.019207	2.313041
97.708522	1697.636238	5.347226	-0.019256	2.317998
98.238807	1705.675498	5.352230	-0.019360	2.322944
98.804157	1713.707964	5.357235	-0.019470	2.327878
99.068532	1721.832312	5.362240	-0.019525	2.332832
99.310965	1729.889923	5.367245	-0.019575	2.337734
99.460082	1737.995125	5.372250	-0.019608	2.342646
99.568224	1746.089593	5.377254	-0.019634	2.347538
99.925680	1754.165981	5.382259	-0.019706	2.352429
100.309435	1762.237929	5.387264	-0.019782	2.357309
100.588174	1770.268591	5.392269	-0.019840	2.362146
100.978758	1778.328260	5.397274	-0.019918	2.367000
101.213858	1786.413109	5.402278	-0.019967	2.371846
101.275969	1794.507490	5.407283	-0.019983	2.376674
101.496685	1802.573971	5.412288	-0.020030	2.381488
101.554339	1810.637444	5.417293	-0.020046	2.386278
101.892789	1818.689354	5.422298	-0.020114	2.391073
102.492744	1826.718756	5.427302	-0.020231	2.395866
102.646175	1834.779981	5.432307	-0.020265	2.400633
102.770004	1842.875883	5.437312	-0.020293	2.405409
102.984398	1850.935226	5.442317	-0.020338	2.410160
103.284241	1859.017929	5.447322	-0.020400	2.414923
103.607436	1867.064568	5.452326	-0.020465	2.419657
103.691576	1875.128348	5.457331	-0.020486	2.424373
104.086107	1883.199818	5.462336	-0.020565	2.429108
104.378799	1891.327075	5.467341	-0.020624	2.433859
104.603142	1899.365861	5.472346	-0.020671	2.438543
104.687830	1907.422740	5.477350	-0.020692	2.443219
104.925271	1915.433703	5.482355	-0.020742	2.447871
105.290726	1923.519047	5.487360	-0.020815	2.452566
105.363911	1931.578443	5.492365	-0.020834	2.457215
105.787815	1939.595847	5.497370	-0.020918	2.461858
105.861019	1947.691102	5.502374	-0.020937	2.466510
106.135817	1955.738303	5.507379	-0.020994	2.471141
106.550673	1963.795924	5.512384	-0.021076	2.475780
106.900989	1971.835171	5.517389	-0.021147	2.480395
107.132776	1979.872931	5.522394	-0.021195	2.484991
107.639126	1987.916769	5.527398	-0.021295	2.489602
107.821711	1996.012827	5.532403	-0.021334	2.494211
108.220034	2004.058029	5.537408	-0.021413	2.498798
108.359080	2012.110586	5.542413	-0.021444	2.503362
108.566096	2020.189377	5.547418	-0.021488	2.507937
108.893244	2028.277857	5.552422	-0.021554	2.512519
109.065050	2036.328773	5.557427	-0.021592	2.517059
109.474748	2044.368822	5.562432	-0.021673	2.521602
109.664657	2052.397152	5.567437	-0.021714	2.526115
109.942400	2060.448557	5.572442	-0.021771	2.530638
110.287179	2068.531731	5.577446	-0.021840	2.535176
110.255475	2076.595782	5.582451	-0.021840	2.539669
110.703263	2084.638586	5.587456	-0.021928	2.544175
110.755625	2092.709651	5.592461	-0.021943	2.548662
111.415675	2100.727121	5.597466	-0.022071	2.553153
111.556850	2108.814741	5.602470	-0.022103	2.557639
111.909582	2116.822571	5.607475	-0.022174	2.562088
111.953969	2124.915525	5.612480	-0.022187	2.566554
112.265038	2132.960867	5.617485	-0.022251	2.571005
112.478768	2141.037730	5.622490	-0.022296	2.575458
112.727458	2149.081315	5.627494	-0.022347	2.579889
112.834749	2157.125267	5.632499	-0.022373	2.584302
113.210812	2165.183055	5.637504	-0.022448	2.588733
113.210142	2173.418848	5.642509	-0.022453	2.593228
113.471636	2181.434586	5.647514	-0.022507	2.597613
113.743876	2189.437707	5.652518	-0.022563	2.601985
114.063292	2197.439374	5.657523	-0.022628	2.606352
114.144402	2205.491229	5.662528	-0.022648	2.610722
114.386607	2213.520166	5.667533	-0.022698	2.615084
114.897927	2221.517713	5.672538	-0.022799	2.619439
114.835755	2229.615260	5.677542	-0.022792	2.623803
115.205534	2237.617726	5.682547	-0.022867	2.628137
115.537634	2245.689427	5.687552	-0.022934	2.632498
115.814638	2253.723587	5.692557	-0.022990	2.636829
115.898696	2261.779127	5.697562	-0.023011	2.641151
116.173587	2269.818340	5.702566	-0.023068	2.645469
116.237157	2277.866363	5.707571	-0.023085	2.649772
116.646109	2285.945568	5.712576	-0.023166	2.654106
116.733390	2293.974850	5.717581	-0.023188	2.658386
116.908430	2302.024054	5.722586	-0.023226	2.662675
117.243466	2310.083922	5.727590	-0.023293	2.666974
117.471324	2318.128756	5.732595	-0.023341	2.671250
117.743132	2326.217912	5.737600	-0.023397	2.675546
117.962118	2334.226646	5.742605	-0.023443	2.679789
118.120411	2342.273933	5.747610	-0.023478	2.684042
118.533110	2350.322909	5.752614	-0.023560	2.688305
118.493902	2358.382986	5.757619	-0.023558	2.692539
118.827575	2366.428060	5.762624	-0.023625	2.696781
118.931080	2374.488654	5.767629	-0.023650	2.701011
119.530338	2382.466550	5.772634	-0.023766	2.705221
119.611587	2390.549874	5.777638	-0.023787	2.709448
119.763096	2398.611696	5.782643	-0.023820	2.713661
120.093063	2406.645004	5.787648	-0.023887	2.717864
120.276629	2414.657327	5.792653	-0.023926	2.722040
120.553539	2422.681179	5.797658	-0.023983	2.726222
120.756120	2430.766154	5.802662	-0.024026	2.730424
120.903910	2438.820096	5.807667	-0.024059	2.734600
121.156235	2446.873443	5.812672	-0.024111	2.738776
121.438872	2454.899910	5.817677	-0.024169	2.742934
121.642305	2462.951118	5.822682	-0.024212	2.747093
121.873072	2471.036943	5.827686	-0.024260	2.751265
122.163181	2479.133060	5.832691	-0.024320	2.755440
122.225662	2487.152005	5.837696	-0.024337	2.759555
122.622274	2495.126646	5.842701	-0.024416	2.763661
122.881759	2503.166124	5.847706	-0.024469	2.767786
123.136965	2511.215803	5.852710	-0.024522	2.771910
123.348002	2519.268681	5.857715	-0.024567	2.776027
123.574094	2527.312852	5.862720	-0.024614	2.780134
123.425942	2535.353601	5.867725	-0.024592	2.784211
124.016120	2543.362111	5.872730	-0.024707	2.788309
124.036520	2551.461194	5.877734	-0.024716	2.792414
124.215878	2559.504392	5.882739	-0.024754	2.796493
124.759346	2567.501254	5.887744	-0.024861	2.800565
125.045396	2575.506956	5.892749	-0.024919	2.804620
125.116909	2583.587597	5.897754	-0.024938	2.808694
125.276689	2591.655575	5.902758	-0.024973	2.812761
125.595595	2599.686566	5.907763	-0.025038	2.816813
125.824226	2607.750249	5.912768	-0.025085	2.820870
125.870322	2615.776073	5.917773	-0.025099	2.824891
126.164068	2623.813805	5.922778	-0.025159	2.828927
126.318130	2631.902272	5.927782	-0.025193	2.832975
126.561482	2639.940226	5.932787	-0.025244	2.836997
126.644537	2647.982855	5.937792	-0.025264	2.841006
127.086679	2655.943360	5.942797	-0.025352	2.844989
127.304484	2664.004872	5.947802	-0.025398	2.849004
127.481232	2672.049131	5.952806	-0.025436	2.853002
127.508716	2680.103966	5.957811	-0.025446	2.856992
127.641846	2688.166389	5.962816	-0.025476	2.860986
127.865759	2696.181851	5.967821	-0.025523	2.864956
128.002127	2704.220931	5.972826	-0.025554	2.868927
128.439087	2712.292092	5.977830	-0.025641	2.872925
128.403389	2720.325988	5.982835	-0.025639	2.876873
128.933782	2728.338189	5.987840	-0.025743	2.880836
129.011264	2736.359997	5.992845	-0.025763	2.884774
129.048176	2744.431148	5.997850	-0.025775	2.888728
129.251754	2752.496774	6.002854	-0.025818	2.892682
129.580918	2760.527631	6.007859	-0.025885	2.896622
130.027456	2768.545713	6.012864	-0.025973	2.900556
129.962710	2776.589126	6.017869	-0.025966	2.904469
130.282607	2784.629166	6.022874	-0.026031	2.908396
130.514592	2792.737544	6.027878	-0.026080	2.912347
130.562974	2800.817353	6.032883	-0.026094	2.916268
130.854759	2808.790397	6.037888	-0.026153	2.920145
131.074514	2816.777574	6.042893	-0.026200	2.924020
131.099916	2824.817432	6.047898	-0.026210	2.927905
131.292426	2832.875642	6.052902	-0.026251	2.931803
131.710547	2840.898690	6.057907	-0.026334	2.935690
131.710871	2848.940410	6.062912	-0.026339	2.939559
131.741625	2856.970572	6.067917	-0.026350	2.943419
131.987627	2865.007489	6.072922	-0.026401	2.947289
132.336304	2873.051162	6.077926	-0.026471	2.951161
132.331403	2881.122258	6.082931	-0.026476	2.955024
132.700113	2889.127022	6.087936	-0.026550	2.958869
132.929400	2897.126651	6.092941	-0.026597	2.962699
133.033318	2905.181689	6.097946	-0.026622	2.966545
133.005457	2913.259409	6.102950	-0.026622	2.970389
133.170850	2921.273019	6.107955	-0.026658	2.974208
133.601041	2929.298324	6.112960	-0.026744	2.978041
133.781226	2937.341114	6.117965	-0.026782	2.981864
134.080186	2945.333533	6.122970	-0.026843	2.985665
134.687425	2953.370233	6.127974	-0.026962	2.989497
134.643781	2961.447617	6.132979	-0.026959	2.993311
134.716523	2969.517666	6.137984	-0.026977	2.997123
135.128113	2977.509176	6.142989	-0.027059	3.000909
135.227277	2985.522728	6.147994	-0.027083	3.004685
135.293243	2993.601092	6.152998	-0.027101	3.008486
135.628535	3001.614152	6.158003	-0.027168	3.012264
135.878261	3009.679749	6.163008	-0.027220	3.016058
135.999373	3017.687718	6.168013	-0.027248	3.019814
136.232226	3025.720097	6.173018	-0.027296	3.023582
136.527611	3033.764792	6.178022	-0.027357	3.027354
136.490385	3041.827539	6.183027	-0.027355	3.031113
136.793017	3049.875010	6.188032	-0.027417	3.034877
137.199712	3057.858064	6.193037	-0.027498	3.038612
137.412170	3065.860519	6.198042	-0.027542	3.042341
137.390367	3073.940197	6.203046	-0.027544	3.046091
137.481177	3081.971715	6.208051	-0.027566	3.049819
137.594352	3090.053987	6.213056	-0.027592	3.053567
137.917941	3098.064511	6.218061	-0.027658	3.057287
138.069669	3106.093806	6.223066	-0.027691	3.061003
138.439336	3114.090990	6.228070	-0.027765	3.064710
138.238450	3122.186875	6.233075	-0.027733	3.068431
138.293005	3130.273221	6.238080	-0.027748	3.072156
138.737102	3138.303930	6.243085	-0.027836	3.075868
138.700378	3146.309068	6.248090	-0.027835	3.079542
138.916659	3154.315803	6.253094	-0.027880	3.083223
139.054396	3162.315624	6.258099	-0.027911	3.086894
139.283797	3170.349925	6.263104	-0.027959	3.090580
139.297497	3178.436204	6.268109	-0.027967	3.094276
139.573421	3186.434586	6.273114	-0.028023	3.097939
139.903947	3194.476844	6.278118	-0.028090	3.101620
139.970635	3202.494906	6.283123	-0.028108	3.105273
140.116227	3210.537226	6.288128	-0.028140	3.108937
140.465040	3218.564004	6.293133	-0.028210	3.112599
140.516541	3226.636251	6.298138	-0.028225	3.116264
140.838939	3234.627663	6.303142	-0.028291	3.119900
140.814259	3242.631280	6.308147	-0.028291	3.123521
141.226575	3250.688630	6.313152	-0.028373	3.127182
141.309920	3258.749433	6.318157	-0.028394	3.130826
141.444479	3266.770296	6.323162	-0.028424	3.134450
141.641279	3274.815186	6.328166	-0.028466	3.138083
141.781592	3282.804945	6.333171	-0.028498	3.141684
142.003622	3290.857091	6.338176	-0.028544	3.145313
142.308836	3298.866675	6.343181	-0.028606	3.148923
142.376914	3306.944310	6.348186	-0.028624	3.152548
142.448258	3315.028177	6.353190	-0.028643	3.156172
142.505663	3322.992869	6.358195	-0.028659	3.159738
142.903996	3330.995684	6.363200	-0.028738	3.163332
143.030254	3339.026487	6.368205	-0.028767	3.166922
143.219431	3347.052678	6.373210	-0.028807	3.170509
143.391162	3355.130426	6.378214	-0.028845	3.174114
143.772654	3363.117187	6.383219	-0.028921	3.177683
143.857761	3371.187322	6.388224	-0.028942	3.181273
144.116797	3379.171809	6.393229	-0.028995	3.184828
144.250786	3387.216787	6.398234	-0.029026	3.188400
144.391933	3395.297686	6.403238	-0.029057	3.191985
144.683680	3403.292879	6.408243	-0.029117	3.195534
144.952883	3411.314104	6.413248	-0.029172	3.199090
145.115200	3419.338269	6.418253	-0.029207	3.202638
145.193658	3427.384332	6.423258	-0.029227	3.206189
145.348047	3435.424373	6.428262	-0.029261	3.209736
145.479977	3443.462731	6.433267	-0.029291	3.213278
145.487105	3451.528898	6.438272	-0.029298	3.216823
145.773518	3459.532165	6.443277	-0.029356	3.220347
146.093121	3467.514161	6.448282	-0.029421	3.223860
146.214627	3475.577783	6.453286	-0.029449	3.227397
146.315995	3483.601503	6.458291	-0.029473	3.230911
146.719313	3491.692350	6.463296	-0.029553	3.234463
146.694363	3499.716941	6.468301	-0.029554	3.237965
146.676437	3507.733086	6.473306	-0.029556	3.241460
147.097641	3515.725075	6.478310	-0.029640	3.244958
147.187647	3523.746478	6.483315	-0.029662	3.248452
147.309702	3531.787984	6.488320	-0.029690	3.251952
147.429199	3539.815433	6.493325	-0.029717	3.255442
147.600365	3547.807922	6.498330	-0.029754	3.258916
147.866909	3555.870219	6.503334	-0.029809	3.262419
147.758338	3563.908518	6.508339	-0.029794	3.265894
148.168171	3571.923171	6.513344	-0.029876	3.269375
148.434483	3579.973392	6.518349	-0.029930	3.272862
148.810863	3587.972366	6.523354	-0.030006	3.276327
149.118924	3595.984746	6.528358	-0.030068	3.279792
149.365070	3603.991769	6.533363	-0.030119	3.283248
149.661004	3612.074046	6.538368	-0.030180	3.286735
149.791832	3620.090496	6.543373	-0.030209	3.290184
150.014302	3628.125383	6.548378	-0.030256	3.293640
150.348031	3636.187989	6.553382	-0.030323	3.297109
150.195700	3644.206488	6.558387	-0.030300	3.300537
150.479153	3652.183363	6.563392	-0.030358	3.303960
150.690842	3660.237188	6.568397	-0.030403	3.307409
150.753005	3668.301857	6.573402	-0.030420	3.310854
151.106143	3676.376968	6.578406	-0.030491	3.314311
151.221094	3684.333658	6.583411	-0.030517	3.317704
151.320649	3692.388737	6.588416	-0.030541	3.321136
151.401527	3700.368611	6.593421	-0.030562	3.324531
151.401683	3708.398362	6.598426	-0.030567	3.327941
151.685930	3716.477682	6.603430	-0.030625	3.331379
151.684648	3724.484365	6.608435	-0.030630	3.334772
151.955394	3732.502730	6.613440	-0.030686	3.338176
152.107162	3740.535363	6.618445	-0.030719	3.341579
152.223920	3748.526076	6.623450	-0.030746	3.344959
152.665095	3756.609263	6.628454	-0.030834	3.348387
152.783797	3764.617016	6.633459	-0.030861	3.351767
152.869546	3772.672105	6.638464	-0.030882	3.355163
152.879487	3780.701852	6.643469	-0.030889	3.358542
153.129784	3788.709355	6.648474	-0.030941	3.361917
153.673638	3796.711728	6.653478	-0.031048	3.365297
153.583315	3804.768545	6.658483	-0.031036	3.368673
153.872029	3812.825613	6.663488	-0.031095	3.372060
154.033191	3820.865241	6.668493	-0.031130	3.375431
154.133603	3828.840484	6.673498	-0.031154	3.378770
154.316302	3836.886962	6.678502	-0.031193	3.382139
154.613424	3844.880976	6.683507	-0.031254	3.385486
154.844671	3852.934310	6.688512	-0.031302	3.388852
154.815182	3861.043243	6.693517	-0.031302	3.392229
155.039622	3869.095358	6.698522	-0.031349	3.395587
155.436020	3877.037444	6.703526	-0.031428	3.398903
155.534316	3884.999647	6.708531	-0.031452	3.402213
155.772284	3893.049084	6.713536	-0.031501	3.405561
155.928439	3901.063643	6.718541	-0.031536	3.408888
156.140253	3909.104116	6.723546	-0.031580	3.412225
156.278209	3917.164732	6.728550	-0.031611	3.415565
156.240283	3925.146585	6.733555	-0.031609	3.418862
156.483242	3933.181033	6.738560	-0.031660	3.422188
156.678846	3941.200814	6.743565	-0.031701	3.425502
156.603300	3949.242400	6.748570	-0.031693	3.428813
157.068385	3957.286874	6.753574	-0.031785	3.432141
156.968199	3965.332438	6.758579	-0.031771	3.435446
157.247406	3973.317513	6.763584	-0.031828	3.438737
157.579136	3981.352516	6.768589	-0.031895	3.442046
157.732643	3989.333716	6.773594	-0.031929	3.445324
157.917749	3997.407712	6.778598	-0.031969	3.448638
158.116691	4005.420531	6.783603	-0.032011	3.451924
158.387404	4013.493355	6.788608	-0.032067	3.455234
158.638507	4021.491525	6.793613	-0.032119	3.458510
158.661464	4029.548609	6.798618	-0.032128	3.461799
158.961707	4037.552884	6.803622	-0.032189	3.465072
159.042105	4045.568619	6.808627	-0.032210	3.468340
159.169936	4053.636536	6.813632	-0.032239	3.471628
159.324927	4061.691571	6.818637	-0.032273	3.474908
159.712590	4069.640508	6.823642	-0.032350	3.478149
159.858712	4077.692337	6.828646	-0.032383	3.481421
159.897910	4085.663944	6.833651	-0.032395	3.484654
160.134455	4093.708427	6.838656	-0.032444	3.487920
160.222626	4101.767576	6.843661	-0.032466	3.491184
160.434165	4109.770580	6.848666	-0.032511	3.494426
160.837483	4117.816414	6.853670	-0.032591	3.497689
160.776696	4125.821725	6.858675	-0.032585	3.500917
160.977775	4133.815613	6.863680	-0.032628	3.504146
161.256447	4141.882305	6.868685	-0.032685	3.507404
161.278903	4149.887950	6.873690	-0.032694	3.510626
161.464095	4157.937366	6.878694	-0.032734	3.513868
161.372626	4165.988366	6.883699	-0.032722	3.517099
161.656185	4173.965041	6.888704	-0.032780	3.520309
161.642344	4182.000712	6.893709	-0.032783	3.523530
161.703766	4190.026297	6.898714	-0.032800	3.526747
162.094035	4198.042796	6.903718	-0.032878	3.529967
162.227515	4206.076144	6.908723	-0.032908	3.533183
162.475216	4214.125431	6.913728	-0.032959	3.536406
162.614133	4222.128571	6.918733	-0.032990	3.539604
162.966217	4230.145675	6.923738	-0.033061	3.542811
163.236598	4238.174785	6.928742	-0.033116	3.546018
163.182883	4246.206549	6.933747	-0.033112	3.549213
163.562333	4254.308979	6.938752	-0.033188	3.552446
163.713298	4262.380188	6.943757	-0.033221	3.555657
163.688432	4270.309742	6.948762	-0.033222	3.558804
163.944694	4278.356987	6.953766	-0.033275	3.562002
163.906011	4286.353001	6.958771	-0.033273	3.565169
164.291788	4294.350832	6.963776	-0.033350	3.568347
164.630058	4302.399747	6.968781	-0.033418	3.571540
164.838767	4310.414157	6.973786	-0.033462	3.574713
164.944805	4318.447261	6.978790	-0.033487	3.577887
164.751271	4326.467457	6.983795	-0.033456	3.581045
165.350198	4334.442497	6.988800	-0.033573	3.584205
165.247351	4342.525793	6.993805	-0.033559	3.587385
165.335484	4350.528550	6.998810	-0.033581	3.590536
165.665065	4358.586105	7.003814	-0.033647	3.593712
165.727169	4366.577951	7.008819	-0.033664	3.596852
165.961498	4374.566831	7.013824	-0.033713	3.599993
166.043120	4382.580913	7.018829	-0.033733	3.603137
166.378755	4390.607812	7.023834	-0.033801	3.606290
166.537202	4398.644943	7.028838	-0.033836	3.609440
166.532529	4406.658425	7.033843	-0.033840	3.612573
166.820107	4414.740512	7.038848	-0.033899	3.615738
167.095731	4422.742633	7.043853	-0.033956	3.618868
167.080704	4430.709023	7.048858	-0.033958	3.621975
167.507134	4438.745819	7.053862	-0.034043	3.625117
167.729351	4446.767194	7.058867	-0.034089	3.628246
167.941689	4454.841261	7.063872	-0.034134	3.631392
168.267782	4462.900037	7.068877	-0.034200	3.634533
168.381159	4470.917169	7.073882	-0.034226	3.637648
168.640169	4478.935165	7.078886	-0.034280	3.640766
168.534761	4486.930546	7.083891	-0.034265	3.643862
169.028559	4494.934135	7.088896	-0.034363	3.646974
169.209235	4502.963887	7.093901	-0.034402	3.650086
169.342764	4510.998156	7.098906	-0.034432	3.653196
169.573280	4519.047264	7.103910	-0.034480	3.656311
169.960246	4527.023086	7.108915	-0.034557	3.659399
169.962113	4535.080591	7.113920	-0.034563	3.662506
170.069955	4543.118310	7.118925	-0.034588	3.665605
170.299571	4551.102733	7.123930	-0.034636	3.668685
170.523970	4559.185276	7.128934	-0.034683	3.671800
170.463996	4567.205300	7.133939	-0.034677	3.674880
170.476438	4575.197901	7.138944	-0.034685	3.677949
170.830013	4583.237910	7.143949	-0.034756	3.681043
171.078339	4591.183487	7.148954	-0.034807	3.684095
171.298062	4599.251021	7.153958	-0.034853	3.687190
171.343211	4607.274150	7.158963	-0.034867	3.690262
171.589306	4615.314417	7.163968	-0.034918	3.693342
171.994296	4623.335524	7.168973	-0.034999	3.696417
172.038550	4631.311069	7.173978	-0.035012	3.699462
172.121762	4639.372554	7.178982	-0.035033	3.702539
172.277628	4647.345896	7.183987	-0.035067	3.705581
172.537666	4655.410962	7.188992	-0.035121	3.708659
172.599044	4663.486699	7.193997	-0.035138	3.711733
172.659245	4671.561847	7.199002	-0.035154	3.714804
172.858190	4679.525402	7.204006	-0.035196	3.717833
173.304661	4687.483759	7.209011	-0.035285	3.720865
173.354115	4695.470945	7.214016	-0.035299	3.723895
173.359928	4703.557305	7.219021	-0.035305	3.726958
173.345110	4711.565016	7.224026	-0.035308	3.729990
173.867136	4719.598837	7.229030	-0.035410	3.733041
173.959429	4727.610467	7.234035	-0.035433	3.736071
174.112638	4735.598342	7.239040	-0.035466	3.739092
174.337277	4743.661096	7.244045	-0.035514	3.742139
174.278407	4751.661322	7.249050	-0.035508	3.745154
174.564844	4759.717695	7.254054	-0.035566	3.748196
174.691636	4767.749204	7.259059	-0.035595	3.751222
174.968102	4775.776305	7.264064	-0.035652	3.754248
175.049985	4783.794632	7.269069	-0.035672	3.757263
175.114496	4791.802216	7.274074	-0.035690	3.760271
175.284282	4799.795620	7.279078	-0.035727	3.763274
175.356299	4807.810650	7.284083	-0.035745	3.766281
175.580681	4815.872001	7.289088	-0.035792	3.769306
176.054417	4823.911386	7.294093	-0.035886	3.772326
176.043234	4831.913395	7.299098	-0.035889	3.775318
176.238012	4839.971132	7.304102	-0.035930	3.778334
176.416776	4847.974468	7.309107	-0.035969	3.781326
176.757115	4855.971160	7.314112	-0.036037	3.784317
176.592286	4864.042328	7.319117	-0.036012	3.787322
176.828449	4872.016222	7.324122	-0.036061	3.790298
177.196956	4880.116151	7.329126	-0.036135	3.793321
177.264832	4888.128032	7.334131	-0.036153	3.796302
177.411079	4896.102949	7.339136	-0.036185	3.799269
177.507635	4904.090465	7.344141	-0.036209	3.802237
177.652063	4912.105868	7.349146	-0.036241	3.805214
177.887863	4920.134899	7.354150	-0.036290	3.808196
178.134712	4928.146925	7.359155	-0.036341	3.811169
178.365870	4936.177204	7.364160	-0.036389	3.814147
178.570140	4944.239914	7.369165	-0.036433	3.817133
178.666787	4952.223989	7.374170	-0.036456	3.820086
178.911726	4960.235345	7.379174	-0.036507	3.823050
178.757257	4968.231960	7.384179	-0.036483	3.825997
179.081133	4976.303016	7.389184	-0.036549	3.828980
179.115029	4984.341107	7.394189	-0.036560	3.831942
179.284540	4992.360761	7.399194	-0.036597	3.834898
179.309724	5000.369391	7.404198	-0.036607	3.837845
179.524691	5008.362431	7.409203	-0.036652	3.840787
179.866666	5016.340948	7.414208	-0.036721	3.843725
180.075496	5024.384249	7.419213	-0.036765	3.846681
180.222032	5032.407509	7.424218	-0.036798	3.849626
180.319615	5040.479769	7.429222	-0.036821	3.852586
180.414714	5048.524305	7.434227	-0.036844	3.855534
180.529525	5056.502251	7.439232	-0.036871	3.858455
180.806050	5064.561107	7.444237	-0.036928	3.861407
180.891356	5072.503387	7.449242	-0.036949	3.864310
181.078748	5080.594113	7.454246	-0.036989	3.867267
181.156586	5088.622600	7.459251	-0.037009	3.870197
181.367123	5096.803387	7.464256	-0.037053	3.873183
181.486706	5104.851440	7.469261	-0.037081	3.876117
181.590477	5112.742584	7.474266	-0.037105	3.878990
182.141469	5120.778777	7.479270	-0.037213	3.881923
182.131307	5128.680299	7.484275	-0.037216	3.884794
182.124778	5136.733698	7.489280	-0.037220	3.887719
182.669578	5144.769023	7.494285	-0.037327	3.890644
182.691601	5152.812481	7.499290	-0.037336	3.893561
182.615434	5160.885273	7.504294	-0.037327	3.896484
182.854905	5168.786176	7.509299	-0.037377	3.899349
183.183266	5176.825618	7.514304	-0.037444	3.902263
183.495974	5184.846115	7.519309	-0.037507	3.905168
183.446216	5192.855252	7.524314	-0.037503	3.908060
183.694731	5200.907644	7.529318	-0.037555	3.910971
183.701999	5208.941361	7.534323	-0.037561	3.913869
183.832283	5216.926187	7.539328	-0.037591	3.916749
184.011434	5224.942202	7.544333	-0.037629	3.919639
184.477304	5232.923552	7.549338	-0.037721	3.922519
184.599829	5240.957956	7.554342	-0.037749	3.925411
184.664671	5248.964758	7.559347	-0.037767	3.928289
184.978886	5257.018819	7.564352	-0.037830	3.931186
185.141474	5265.077876	7.569357	-0.037866	3.934081
185.086151	5273.056285	7.574362	-0.037861	3.936940
185.338993	5281.096600	7.579366	-0.037913	3.939825
185.366130	5289.086085	7.584371	-0.037923	3.942686
185.577126	5297.101979	7.589376	-0.037968	3.945557
185.672947	5305.131231	7.594381	-0.037991	3.948429
185.816710	5313.171893	7.599386	-0.038023	3.951304
186.141662	5321.249872	7.604390	-0.038089	3.954193
186.049388	5329.231632	7.609395	-0.038077	3.957039
186.341596	5337.199586	7.614400	-0.038136	3.959884
186.541413	5345.220829	7.619405	-0.038179	3.962744
186.726720	5353.222333	7.624410	-0.038219	3.965595
186.911532	5361.230582	7.629414	-0.038258	3.968446
187.208252	5369.286791	7.634419	-0.038319	3.971315
187.343985	5377.342536	7.639424	-0.038349	3.974178
187.501858	5385.356466	7.644429	-0.038384	3.977024
187.527802	5393.316377	7.649434	-0.038394	3.979848
187.719542	5401.407255	7.654438	-0.038435	3.982718
187.726125	5409.382184	7.659443	-0.038441	3.985542
188.181137	5417.393098	7.664448	-0.038531	3.988384
188.420607	5425.458777	7.669453	-0.038581	3.991240
188.451238	5433.505511	7.674458	-0.038592	3.994084
188.726998	5441.554694	7.679462	-0.038649	3.996931
188.984326	5449.491978	7.684467	-0.038702	3.999736
189.084832	5457.544840	7.689472	-0.038726	4.002577
189.301691	5465.551216	7.694477	-0.038771	4.005401
189.565086	5473.551483	7.699482	-0.038826	4.008222
189.818843	5481.599657	7.704486	-0.038878	4.011058
190.125172	5489.620196	7.709491	-0.038940	4.013883
190.019436	5497.709342	7.714496	-0.038926	4.016723
190.377209	5505.646610	7.719501	-0.038998	4.019515
190.387509	5513.667224	7.724506	-0.039005	4.022330
190.571508	5521.683151	7.729510	-0.039044	4.025143
190.750269	5529.743330	7.734515	-0.039083	4.027969
190.961144	5537.726677	7.739520	-0.039128	4.030768
191.272695	5545.853230	7.744525	-0.039191	4.033616
191.637823	5553.852034	7.749530	-0.039264	4.036418
192.024176	5561.801113	7.754534	-0.039341	4.039201
191.943078	5569.838486	7.759539	-0.039331	4.042005
192.177428	5577.765018	7.764544	-0.039380	4.044774
192.479031	5585.844725	7.769549	-0.039442	4.047596
192.701763	5593.816104	7.774554	-0.039488	4.050376
192.920993	5601.856002	7.779558	-0.039534	4.053178
193.088396	5609.912709	7.784563	-0.039571	4.055984
193.256152	5617.898702	7.789568	-0.039607	4.058763
193.384560	5625.966487	7.794573	-0.039636	4.061568
193.641672	5633.916758	7.799578	-0.039689	4.064331
193.899381	5641.962545	7.804582	-0.039743	4.067127
194.098224	5649.977657	7.809587	-0.039785	4.069908
194.205305	5658.034527	7.814592	-0.039810	4.072701
194.559574	5666.044573	7.819597	-0.039881	4.075480
194.437211	5674.018973	7.824602	-0.039864	4.078237
194.528549	5682.067836	7.829606	-0.039886	4.081021
194.679347	5690.052075	7.834611	-0.039919	4.083782
194.912692	5698.060217	7.839616	-0.039968	4.086550
194.716418	5706.133416	7.844621	-0.039937	4.089333
194.888746	5714.134140	7.849626	-0.039974	4.092094
195.259825	5722.180603	7.854630	-0.040048	4.094872
195.509419	5730.145820	7.859635	-0.040100	4.097618
195.607623	5738.137786	7.864640	-0.040124	4.100369
195.555675	5746.170020	7.869645	-0.040119	4.103131
196.004970	5754.201145	7.874650	-0.040208	4.105897
196.176290	5762.269406	7.879654	-0.040245	4.108670
196.152239	5770.295102	7.884659	-0.040246	4.111423
196.249074	5778.338001	7.889664	-0.040269	4.114183
196.503635	5786.324833	7.894669	-0.040322	4.116923
196.735036	5794.300640	7.899674	-0.040370	4.119658
196.944652	5802.366608	7.904678	-0.040414	4.122421
196.843651	5810.356439	7.909683	-0.040401	4.125153
196.890515	5818.383550	7.914688	-0.040415	4.127897
197.309862	5826.427080	7.919693	-0.040498	4.130650
197.684793	5834.424708	7.924698	-0.040573	4.133384
197.927205	5842.510416	7.929702	-0.040624	4.136145
197.829601	5850.461801	7.934707	-0.040611	4.138855
197.870018	5858.534430	7.939712	-0.040623	4.141605
197.978584	5866.488928	7.944717	-0.040649	4.144314
198.098557	5874.552928	7.949722	-0.040676	4.147059
198.434685	5882.551326	7.954726	-0.040744	4.149783
198.644450	5890.597240	7.959731	-0.040789	4.152519
198.696379	5898.629223	7.964736	-0.040804	4.155246
199.161650	5906.635616	7.969741	-0.040895	4.157968
199.207239	5914.589160	7.974746	-0.040909	4.160666
199.322625	5922.634896	7.979750	-0.040936	4.163394
199.602016	5930.675764	7.984755	-0.040993	4.166120
199.829101	5938.679497	7.989760	-0.041041	4.168831
199.715639	5946.723100	7.994765	-0.041025	4.171550
199.938295	5954.734780	7.999770	-0.041071	4.174260
200.100649	5962.797233	8.004774	-0.041107	4.176985
200.375373	5970.749347	8.009779	-0.041163	4.179672
200.396255	5978.748383	8.014784	-0.041172	4.182370
200.734715	5986.754255	8.019789	-0.041241	4.185073
200.853718	5994.795762	8.024794	-0.041268	4.187783
200.947372	6002.834078	8.029798	-0.041291	4.190490
201.152757	6010.903753	8.034803	-0.041334	4.193207
201.377826	6018.948400	8.039808	-0.041381	4.195914
201.672284	6026.894825	8.044813	-0.041441	4.198587
202.128999	6034.890618	8.049818	-0.041532	4.201277
202.455711	6042.862299	8.054822	-0.041598	4.203955
202.598624	6050.906397	8.059827	-0.041630	4.206654
202.514249	6058.895668	8.064832	-0.041619	4.209331
202.895687	6066.983835	8.069837	-0.041695	4.212043
203.190567	6074.967121	8.074842	-0.041756	4.214718
203.091295	6083.020800	8.079846	-0.041742	4.217411
203.152552	6090.966369	8.084851	-0.041759	4.220068
203.349173	6099.021365	8.089856	-0.041801	4.222760
203.544128	6107.009607	8.094861	-0.041842	4.225429
203.678740	6114.996347	8.099866	-0.041873	4.228095
203.833365	6123.051297	8.104870	-0.041907	4.230782
204.089740	6131.103779	8.109875	-0.041960	4.233468
204.163518	6139.132083	8.114880	-0.041979	4.236142
204.260644	6147.102885	8.119885	-0.042002	4.238795
204.477628	6155.118494	8.124890	-0.042048	4.241463
204.631188	6163.088428	8.129894	-0.042081	4.244113
204.526502	6171.180715	8.134899	-0.042067	4.246800
204.949163	6179.130643	8.139904	-0.042151	4.249443
205.007237	6187.233304	8.144909	-0.042167	4.252131
205.122014	6195.228394	8.149914	-0.042194	4.254782
205.224451	6203.302390	8.154918	-0.042218	4.257458
205.605455	6211.293746	8.159923	-0.042294	4.260108
205.574885	6219.337244	8.164928	-0.042294	4.262769
205.895026	6227.314952	8.169933	-0.042359	4.265410
205.970442	6235.361916	8.174938	-0.042378	4.268070
206.437878	6243.356275	8.179942	-0.042470	4.270714
206.222438	6251.459843	8.184947	-0.042435	4.273387
206.451831	6259.455490	8.189952	-0.042483	4.276026
206.585253	6267.445399	8.194957	-0.042513	4.278661
206.617675	6275.422037	8.199962	-0.042525	4.281289
206.921828	6283.435554	8.204966	-0.042586	4.283930
207.072168	6291.468482	8.209971	-0.042620	4.286574
207.078756	6299.456865	8.214976	-0.042626	4.289201
207.206070	6307.556432	8.219981	-0.042655	4.291864
207.432629	6315.512193	8.224986	-0.042702	4.294479
207.702631	6323.593627	8.229990	-0.042758	4.297133
207.554438	6331.507557	8.234995	-0.042736	4.299728
207.722341	6339.590059	8.240000	-0.042772	4.302379
208.067007	6347.570435	8.245005	-0.042842	4.304996
208.067680	6355.609773	8.250010	-0.042847	4.307628
208.153682	6363.626255	8.255014	-0.042868	4.310252
208.484242	6371.677283	8.260019	-0.042935	4.312887
208.838210	6379.668809	8.265024	-0.043006	4.315502
208.946066	6387.661426	8.270029	-0.043031	4.318113
208.921096	6395.646650	8.275034	-0.043032	4.320719
208.907511	6403.717810	8.280038	-0.043035	4.323352
209.180612	6411.707004	8.285043	-0.043091	4.325958
209.370491	6419.730779	8.290048	-0.043131	4.328574
209.459891	6427.794313	8.295053	-0.043153	4.331200
209.347590	6435.760660	8.300058	-0.043138	4.333792
209.555619	6443.890936	8.305062	-0.043182	4.336437
209.721404	6451.822514	8.310067	-0.043218	4.339017
209.824064	6459.810218	8.315072	-0.043242	4.341612
209.946181	6467.822544	8.320077	-0.043270	4.344214
210.029670	6475.838609	8.325082	-0.043291	4.346815
210.200797	6483.890455	8.330086	-0.043328	4.349427
210.371452	6491.957829	8.335091	-0.043365	4.352042
210.449365	6500.039725	8.340096	-0.043385	4.354660
210.669442	6508.013671	8.345101	-0.043431	4.357242
210.771153	6515.928176	8.350106	-0.043455	4.359803
210.928455	6523.985401	8.355110	-0.043490	4.362408
211.032140	6531.919995	8.360115	-0.043514	4.364973
211.105549	6539.948871	8.365120	-0.043533	4.367565
211.150072	6547.989880	8.370125	-0.043546	4.370160
211.445194	6556.034832	8.375130	-0.043607	4.372757
211.739971	6564.088574	8.380134	-0.043667	4.375354
211.624863	6572.085977	8.385139	-0.043651	4.377929
211.640785	6580.079831	8.390144	-0.043659	4.380503
211.815680	6588.118229	8.395149	-0.043697	4.383090
212.023770	6596.058877	8.400154	-0.043741	4.385645
212.182589	6604.116877	8.405158	-0.043775	4.388235
212.215401	6612.090516	8.410163	-0.043787	4.390796
212.487106	6620.171712	8.415168	-0.043843	4.393391
212.621880	6628.235814	8.420173	-0.043873	4.395979
212.588124	6636.179002	8.425178	-0.043872	4.398525
212.852089	6644.203669	8.430182	-0.043926	4.401098
212.885245	6652.191132	8.435187	-0.043938	4.403655
213.149666	6660.212650	8.440192	-0.043992	4.406224
213.435040	6668.221049	8.445197	-0.044050	4.408787
213.515708	6676.257040	8.450202	-0.044071	4.411356
213.565722	6684.360803	8.455206	-0.044085	4.413945
213.875853	6692.339117	8.460211	-0.044148	4.416494
213.740251	6700.308481	8.465216	-0.044128	4.419036
213.875903	6708.376191	8.470221	-0.044159	4.421609
214.049137	6716.335416	8.475226	-0.044196	4.424147
214.263181	6724.408489	8.480230	-0.044241	4.426720
214.272737	6732.432444	8.485235	-0.044248	4.429274
214.499783	6740.451034	8.490240	-0.044296	4.431826
214.712810	6748.507936	8.495245	-0.044341	4.434389
214.841730	6756.493139	8.500250	-0.044370	4.436927
215.069177	6764.442278	8.505254	-0.044418	4.439453
215.060610	6772.501581	8.510259	-0.044421	4.442011
215.319785	6780.457586	8.515264	-0.044475	4.444536
215.587434	6788.559949	8.520269	-0.044530	4.447106
215.724699	6796.511130	8.525274	-0.044561	4.449626
215.893566	6804.617347	8.530278	-0.044597	4.452194
215.831214	6812.601995	8.535283	-0.044591	4.454721
215.745100	6820.624036	8.540288	-0.044580	4.457258
216.101169	6828.598761	8.545293	-0.044652	4.459781
216.136704	6836.640339	8.550298	-0.044664	4.462322
216.128941	6844.619791	8.555302	-0.044667	4.464842
216.245210	6852.686410	8.560307	-0.044694	4.467388
216.388145	6860.679163	8.565312	-0.044726	4.469910
216.534552	6868.727967	8.570317	-0.044759	4.472447
216.586514	6876.731908	8.575322	-0.044773	4.474969
216.867097	6884.776574	8.580327	-0.044831	4.477504
217.180757	6892.727321	8.585331	-0.044895	4.480007
217.198281	6900.727467	8.590336	-0.044903	4.482523
217.325390	6908.735956	8.595341	-0.044932	4.485041
217.519422	6916.748325	8.600346	-0.044973	4.487559
217.749216	6924.782824	8.605351	-0.045021	4.490082
218.038124	6932.814400	8.610355	-0.045080	4.492604
218.044128	6940.812490	8.615360	-0.045087	4.495112
218.250515	6948.887901	8.620365	-0.045130	4.497644
218.306739	6956.841736	8.625370	-0.045146	4.500136
218.551241	6964.888082	8.630375	-0.045197	4.502656
218.714875	6972.902827	8.635379	-0.045233	4.505165
218.536383	6980.903083	8.640384	-0.045205	4.507666
218.829734	6988.952713	8.645389	-0.045264	4.510183
218.858644	6996.978144	8.650394	-0.045275	4.512691
219.057457	7005.061707	8.655399	-0.045317	4.515215
219.355531	7013.012004	8.660403	-0.045378	4.517697
219.394737	7020.947741	8.665408	-0.045391	4.520172
219.459991	7029.008880	8.670413	-0.045408	4.522685
219.552279	7036.936009	8.675418	-0.045430	4.525155
219.782529	7045.057104	8.680423	-0.045478	4.527684
219.857223	7053.063479	8.685427	-0.045498	4.530176
219.901968	7061.048393	8.690432	-0.045511	4.532659
220.325053	7069.105595	8.695437	-0.045595	4.535164
220.508882	7077.076445	8.700442	-0.045635	4.537641
220.762631	7085.115675	8.705447	-0.045687	4.540138
220.755056	7093.108641	8.710451	-0.045691	4.542618
220.795948	7101.101678	8.715456	-0.045704	4.545097
220.870100	7109.165410	8.720461	-0.045723	4.547597
220.691813	7117.137177	8.725466	-0.045695	4.550067
221.096959	7125.222190	8.730471	-0.045776	4.552571
221.067707	7133.233220	8.735475	-0.045775	4.555050
221.044580	7141.238486	8.740480	-0.045776	4.557526
221.269609	7149.204558	8.745485	-0.045823	4.559989
221.394468	7157.242173	8.750490	-0.045852	4.562473
221.591245	7165.241454	8.755495	-0.045894	4.564943
221.658407	7173.296253	8.760499	-0.045912	4.567429
221.764715	7181.252066	8.765504	-0.045937	4.569883
222.014667	7189.365663	8.770509	-0.045988	4.572385
222.268982	7197.347987	8.775514	-0.046041	4.574845
222.469467	7205.418035	8.780519	-0.046084	4.577330
222.582064	7213.388310	8.785523	-0.046110	4.579784
222.437536	7221.393058	8.790528	-0.046088	4.582246
222.541837	7229.398379	8.795533	-0.046113	4.584707
222.713314	7237.440411	8.800538	-0.046150	4.587179
222.791595	7245.432151	8.805543	-0.046170	4.589633
222.824775	7253.495440	8.810547	-0.046181	4.592108
222.976677	7261.516067	8.815552	-0.046215	4.594569
223.232793	7269.582651	8.820557	-0.046268	4.597043
223.063708	7277.462708	8.825562	-0.046241	4.599457
223.228834	7285.552394	8.830567	-0.046277	4.601935
223.606290	7293.524908	8.835571	-0.046353	4.604376
223.502385	7301.539961	8.840576	-0.046339	4.606828
223.659367	7309.576451	8.845581	-0.046373	4.609286
223.635831	7317.578549	8.850586	-0.046374	4.611732
224.152679	7325.613396	8.855591	-0.046475	4.614186
224.193202	7333.667064	8.860595	-0.046488	4.616645
224.286420	7341.605324	8.865600	-0.046511	4.619068
224.547598	7349.655366	8.870605	-0.046565	4.621523
224.517396	7357.601044	8.875610	-0.046564	4.623945
224.686168	7365.659682	8.880615	-0.046601	4.626400
224.949665	7373.690972	8.885619	-0.046655	4.628845
224.822371	7381.689236	8.890624	-0.046637	4.631280
224.741805	7389.772833	8.895629	-0.046627	4.633739
224.952657	7397.762535	8.900634	-0.046672	4.636167
225.039140	7405.738831	8.905639	-0.046693	4.638591
225.079714	7413.777864	8.910643	-0.046706	4.641033
225.252139	7421.736039	8.915648	-0.046743	4.643448
225.676646	7429.806066	8.920653	-0.046827	4.645896
225.709788	7437.782734	8.925658	-0.046839	4.648315
225.960663	7445.849690	8.930663	-0.046891	4.650759
226.188808	7453.891032	8.935667	-0.046938	4.653195
226.245400	7461.867040	8.940672	-0.046954	4.655609
226.087165	7469.880574	8.945677	-0.046930	4.658034
226.267406	7477.873590	8.950682	-0.046969	4.660451
226.402575	7485.922325	8.955687	-0.046999	4.662884
226.512393	7493.900799	8.960691	-0.047025	4.665294
226.592122	7501.920560	8.965696	-0.047045	4.667715
226.947881	7509.946731	8.970701	-0.047116	4.670137
226.971894	7518.068920	8.975706	-0.047126	4.672587
226.971546	7526.115513	8.980711	-0.047131	4.675013
227.220530	7534.063859	8.985715	-0.047183	4.677407
227.256542	7542.021531	8.990720	-0.047195	4.679804
227.458486	7550.033970	8.995725	-0.047238	4.682215
227.621009	7557.976712	9.000730	-0.047273	4.684604
227.757276	7566.070906	9.005735	-0.047304	4.687038
227.941276	7574.067814	9.010739	-0.047343	4.689441
227.919202	7582.079102	9.015744	-0.047344	4.691847
228.387679	7590.108982	9.020749	-0.047437	4.694257
228.331609	7598.139827	9.025754	-0.047432	4.696667
228.582516	7606.040400	9.030759	-0.047483	4.699036
228.854571	7614.163981	9.035763	-0.047539	4.701471
228.877233	7622.148390	9.040768	-0.047549	4.703863
228.913058	7630.181818	9.045773	-0.047561	4.706268
229.072357	7638.177507	9.050778	-0.047596	4.708661
229.280280	7646.225721	9.055783	-0.047640	4.711068
229.222743	7654.241614	9.060787	-0.047634	4.713465
229.316844	7662.234562	9.065792	-0.047657	4.715853
229.453974	7670.284234	9.070797	-0.047688	4.718257
229.536858	7678.218367	9.075802	-0.047708	4.720625
229.556750	7686.253321	9.080807	-0.047717	4.723023
229.691402	7694.299657	9.085811	-0.047748	4.725422
229.857793	7702.320042	9.090816	-0.047784	4.727812
229.950724	7710.348082	9.095821	-0.047806	4.730204
230.105504	7718.392339	9.100826	-0.047840	4.732599
230.387268	7726.398926	9.105831	-0.047898	4.734981
230.453827	7734.446416	9.110835	-0.047916	4.737374
230.434069	7742.417331	9.115840	-0.047917	4.739744
230.683971	7750.418074	9.120845	-0.047969	4.742121
230.854887	7758.417917	9.125850	-0.048006	4.744497
230.844940	7766.452558	9.130855	-0.048009	4.746882
231.038110	7774.449208	9.135859	-0.048051	4.749254
231.105954	7782.481219	9.140864	-0.048069	4.751636
231.177700	7790.528927	9.145869	-0.048087	4.754021
231.032925	7798.566680	9.150874	-0.048065	4.756403
231.445249	7806.494569	9.155879	-0.048147	4.758749
231.831976	7814.520143	9.160883	-0.048225	4.761123
231.555750	7822.479749	9.165888	-0.048178	4.763478
232.003273	7830.575476	9.170893	-0.048267	4.765870
232.195844	7838.623725	9.175898	-0.048308	4.768248
232.337684	7846.629981	9.180903	-0.048340	4.770612
232.466191	7854.643276	9.185907	-0.048369	4.772978
232.627818	7862.617637	9.190912	-0.048404	4.775330
232.620427	7870.640391	9.195917	-0.048408	4.777696
232.947962	7878.631291	9.200922	-0.048474	4.780051
233.216224	7886.708142	9.205927	-0.048530	4.782429
233.216353	7894.685802	9.210931	-0.048535	4.784779
233.113877	7902.689317	9.215936	-0.048521	4.787135
233.384397	7910.727432	9.220941	-0.048577	4.789498
233.383198	7918.762593	9.225946	-0.048582	4.791861
233.462716	7926.775261	9.230951	-0.048602	4.794216
233.577314	7934.825372	9.235955	-0.048628	4.796580
233.866592	7942.773601	9.240960	-0.048687	4.798913
233.913849	7950.796682	9.245965	-0.048701	4.801267
234.097402	7958.756590	9.250970	-0.048741	4.803601
234.276632	7966.814115	9.255975	-0.048779	4.805962
234.437232	7974.834894	9.260979	-0.048814	4.808312
234.400820	7982.833110	9.265984	-0.048813	4.810655
234.505861	7990.223053	9.270989	-0.048837	4.812818
234.570903	7994.699426	9.275994	-0.048852	4.814127

234.874314	7997.209747	9.280999	-0.048910	4.814860
234.723620	7998.510353	9.286003	-0.048883	4.815242
234.644736	7998.949852	9.291008	-0.048869	4.815370
234.774428	7999.932779	9.296013	-0.048894	4.815657
234.808158	7999.904507	9.301018	-0.048900	4.815649
235.043660	7999.893367	9.306023	-0.048944	4.815645
235.086330	7999.900461	9.311027	-0.048952	4.815646
235.072587	7999.842605	9.316032	-0.048949	4.815630
235.185020	7999.895653	9.321037	-0.048970	4.815645
235.309380	7999.886988	9.326042	-0.048993	4.815641
235.346523	7999.871579	9.331047	-0.049000	4.815637
235.198964	7999.947112	9.336051	-0.048973	4.815660
235.185079	7999.847628	9.341056	-0.048970	4.815631
235.319701	7999.930919	9.346061	-0.048995	4.815654
235.178334	7999.853925	9.351066	-0.048969	4.815632
235.228209	7999.868606	9.356071	-0.048978	4.815636
235.502965	7999.884784	9.361075	-0.049029	4.815640
235.400044	7999.848969	9.366080	-0.049010	4.815630
235.470742	7999.909882	9.371085	-0.049023	4.815647
235.390329	7999.895776	9.376090	-0.049008	4.815644
235.626171	7999.847286	9.381095	-0.049052	4.815628
235.380190	7999.928702	9.386099	-0.049007	4.815653
235.472125	7999.842666	9.391104	-0.049024	4.815628
235.668905	7999.936568	9.396109	-0.049060	4.815654
235.628067	7999.902822	9.401114	-0.049053	4.815645
235.649630	7999.892498	9.406119	-0.049057	4.815641
235.701649	7999.900811	9.411123	-0.049067	4.815644
235.688116	7999.813071	9.416128	-0.049064	4.815618
235.838583	7999.875273	9.421133	-0.049092	4.815636
235.740984	7999.853418	9.426138	-0.049074	4.815630
235.738989	7999.844849	9.431143	-0.049074	4.815627
235.589566	7999.891534	9.436147	-0.049046	4.815641
235.828956	7999.839899	9.441152	-0.049090	4.815625
235.945940	7999.880214	9.446157	-0.049112	4.815636
235.715924	7999.898914	9.451162	-0.049069	4.815643
235.719879	7999.866959	9.456167	-0.049070	4.815634
235.931950	7999.873587	9.461171	-0.049110	4.815635
235.839369	7999.810187	9.466176	-0.049092	4.815616
235.679621	7999.872716	9.471181	-0.049063	4.815636
235.793794	7999.862820	9.476186	-0.049084	4.815632
235.863409	7999.843666	9.481191	-0.049097	4.815626
235.736935	7999.883250	9.486195	-0.049073	4.815638
235.787284	7999.852044	9.491200	-0.049083	4.815629
235.998364	7999.902417	9.496205	-0.049122	4.815643
235.921408	7999.933196	9.501210	-0.049108	4.815652
235.817859	7999.919783	9.506215	-0.049088	4.815649
235.926194	7999.908726	9.511219	-0.049109	4.815645
235.855585	7999.892644	9.516224	-0.049095	4.815641
236.041830	7999.950087	9.521229	-0.049130	4.815656
236.068692	7999.885414	9.526234	-0.049135	4.815637
236.150849	7999.838711	9.531239	-0.049150	4.815623
236.050122	7999.917136	9.536243	-0.049132	4.815647
235.953043	7999.844057	9.541248	-0.049114	4.815626
236.293703	7999.818607	9.546253	-0.049177	4.815617
235.974374	7999.808114	9.551258	-0.049118	4.815615
235.916467	7999.830662	9.556263	-0.049107	4.815622
236.058997	7999.855379	9.561267	-0.049133	4.815629
236.063431	7999.828768	9.566272	-0.049134	4.815621
236.224355	7999.905015	9.571277	-0.049164	4.815642
236.171197	7999.843318	9.576282	-0.049154	4.815625
236.307731	7999.851928	9.581287	-0.049180	4.815626
236.169116	7999.916934	9.586291	-0.049154	4.815646
236.185911	7999.831818	9.591296	-0.049157	4.815621
236.513506	7999.871266	9.596301	-0.049218	4.815631
236.397401	7999.867256	9.601306	-0.049196	4.815631
236.435510	7999.867873	9.606311	-0.049204	4.815631
236.404788	7999.907937	9.611315	-0.049198	4.815642
236.404308	7999.848159	9.616320	-0.049198	4.815625
236.356660	7999.881545	9.621325	-0.049189	4.815635
236.369877	7999.852941	9.626330	-0.049191	4.815626
236.547072	7999.846198	9.631335	-0.049224	4.815624
236.518331	7999.926854	9.636339	-0.049219	4.815647
236.418648	7999.924177	9.641344	-0.049201	4.815647
236.547270	7999.955075	9.646349	-0.049225	4.815656
236.544829	7999.871782	9.651354	-0.049224	4.815631
236.350239	7999.859034	9.656359	-0.049188	4.815628
236.422711	7999.944527	9.661363	-0.049201	4.815653
236.375978	7999.880799	9.666368	-0.049193	4.815635
236.408451	7999.919749	9.671373	-0.049199	4.815646
236.541718	7999.918701	9.676378	-0.049224	4.815645
236.671246	7999.900515	9.681383	-0.049248	4.815639
236.686088	7999.901823	9.686387	-0.049250	4.815639
236.629479	7999.830463	9.691392	-0.049240	4.815619
236.615153	7999.871860	9.696397	-0.049237	4.815631
236.730191	7999.884393	9.701402	-0.049259	4.815634
236.657124	7999.889618	9.706407	-0.049245	4.815636
236.384175	7999.884142	9.711411	-0.049194	4.815636
236.433181	7999.825163	9.716416	-0.049203	4.815618
236.677830	7999.895292	9.721421	-0.049249	4.815637
236.499844	7999.853993	9.726426	-0.049216	4.815626
236.669015	7999.894084	9.731431	-0.049247	4.815637
236.606652	7999.940041	9.736435	-0.049236	4.815651
236.491512	7999.847457	9.741440	-0.049214	4.815624
236.826866	7999.945736	9.746445	-0.049277	4.815651
236.868937	7999.929339	9.751450	-0.049285	4.815646
236.835648	7999.872232	9.756455	-0.049278	4.815630
236.876365	7999.943337	9.761459	-0.049286	4.815651
236.865426	7999.878052	9.766464	-0.049284	4.815631
236.818559	7999.919990	9.771469	-0.049275	4.815644
236.500256	7999.900973	9.776474	-0.049216	4.815640
236.633500	7999.898857	9.781479	-0.049241	4.815639
236.671635	7999.884531	9.786483	-0.049248	4.815634
236.508570	7999.869089	9.791488	-0.049218	4.815631
236.680343	7999.936974	9.796493	-0.049250	4.815650
236.698965	7999.936209	9.801498	-0.049253	4.815649
236.713469	7999.831843	9.806503	-0.049256	4.815619
236.578474	7999.940668	9.811507	-0.049231	4.815651
236.645496	7999.906529	9.816512	-0.049243	4.815641
236.634642	7999.913826	9.821517	-0.049241	4.815643
236.425741	7999.902981	9.826522	-0.049202	4.815641
236.741887	7999.845115	9.831527	-0.049261	4.815622
236.770895	7999.960860	9.836531	-0.049267	4.815656
236.671488	7999.864259	9.841536	-0.049248	4.815628
236.780164	7999.905508	9.846541	-0.049268	4.815640
236.772009	7999.927792	9.851546	-0.049267	4.815646
236.703874	7999.901076	9.856551	-0.049254	4.815639
236.739375	7999.935806	9.861555	-0.049261	4.815649
236.770713	7999.887214	9.866560	-0.049267	4.815635
236.747424	7999.937005	9.871565	-0.049262	4.815649
236.718371	7999.882101	9.876570	-0.049257	4.815633
236.879571	7999.894313	9.881575	-0.049287	4.815636
236.992824	7999.967658	9.886579	-0.049308	4.815657
236.899589	7999.971489	9.891584	-0.049291	4.815659
236.905146	7999.998264	9.896589	-0.049292	4.815666
236.659326	7999.981484	9.901594	-0.049246	4.815663
236.740461	7999.979594	9.906599	-0.049261	4.815662
236.838178	7999.955557	9.911603	-0.049279	4.815654
236.894733	7999.955405	9.916608	-0.049290	4.815654
236.929668	7999.934623	9.921613	-0.049296	4.815648
236.651427	7999.944004	9.926618	-0.049245	4.815652
236.859400	7999.931355	9.931623	-0.049283	4.815647
236.828895	7999.909515	9.936627	-0.049278	4.815641
236.762515	7999.897770	9.941632	-0.049265	4.815638
236.752130	7999.928557	9.946637	-0.049263	4.815647
236.979511	7999.947175	9.951642	-0.049306	4.815651
236.752013	7999.845303	9.956647	-0.049263	4.815622
236.889164	7999.894484	9.961651	-0.049289	4.815636
237.141496	7999.872945	9.966656	-0.049336	4.815629
237.231392	7999.905352	9.971661	-0.049353	4.815638
236.897064	7999.928770	9.976666	-0.049290	4.815646
236.883392	7999.865575	9.981671	-0.049288	4.815628
237.144309	7999.965856	9.986675	-0.049336	4.815656
236.999851	7999.858920	9.991680	-0.049310	4.815625
237.032938	7999.939508	9.996685	-0.049316	4.815649
237.074744	7999.886816	10.001690	-0.049324	4.815633
237.168917	7999.894743	10.006695	-0.049341	4.815635
237.147466	7999.943497	10.011699	-0.049337	4.815649
236.973858	7999.908671	10.016704	-0.049305	4.815640
237.152258	7999.872062	10.021709	-0.049338	4.815628
236.998026	7999.848224	10.026714	-0.049309	4.815622
237.091399	7999.852935	10.031719	-0.049327	4.815623
237.101687	7999.927819	10.036723	-0.049329	4.815645
236.999821	7999.882411	10.041728	-0.049310	4.815632
237.045254	7999.931178	10.046733	-0.049318	4.815646
237.146590	7999.906132	10.051738	-0.049337	4.815638
237.096030	7999.850880	10.056743	-0.049328	4.815622
236.893648	7999.871093	10.061747	-0.049290	4.815629
236.706381	7999.809364	10.066752	-0.049255	4.815612
236.892042	7999.906293	10.071757	-0.049290	4.815640
236.979232	7999.895961	10.076762	-0.049306	4.815636
236.717528	7999.836231	10.081767	-0.049257	4.815620
237.125574	7999.847094	10.086771	-0.049333	4.815621
236.922510	7999.829938	10.091776	-0.049295	4.815617
237.113429	7999.884258	10.096781	-0.049331	4.815632
236.964092	7999.861566	10.101786	-0.049303	4.815626
237.098380	7999.830648	10.106791	-0.049328	4.815616
237.018932	7999.907283	10.111795	-0.049313	4.815639
236.936213	7999.825895	10.116800	-0.049298	4.815616
237.076857	7999.880470	10.121805	-0.049324	4.815631
237.106829	7999.900168	10.126810	-0.049330	4.815637
236.928645	7999.907963	10.131815	-0.049297	4.815640
237.256031	7999.939939	10.136819	-0.049358	4.815648
237.242774	7999.832988	10.141824	-0.049355	4.815616
236.972176	7999.911871	10.146829	-0.049305	4.815641
237.064856	7999.874945	10.151834	-0.049322	4.815630
237.178296	7999.865038	10.156839	-0.049343	4.815626
236.991328	7999.822525	10.161843	-0.049308	4.815615
237.067205	7999.840830	10.166848	-0.049322	4.815620
237.206393	7999.877236	10.171853	-0.049348	4.815630
237.217241	7999.874210	10.176858	-0.049350	4.815629
237.149773	7999.904074	10.181863	-0.049338	4.815638
237.072668	7999.925244	10.186867	-0.049324	4.815644
237.131374	7999.864286	10.191872	-0.049334	4.815626
236.963767	7999.896802	10.196877	-0.049303	4.815636
237.123182	7999.902581	10.201882	-0.049333	4.815637
237.318303	7999.908937	10.206887	-0.049369	4.815638
237.330492	7999.912338	10.211891	-0.049372	4.815639
237.168984	7999.871303	10.216896	-0.049342	4.815628
237.396013	7999.915533	10.221901	-0.049384	4.815640
237.308710	7999.916258	10.226906	-0.049368	4.815641
237.295637	7999.943800	10.231911	-0.049365	4.815649
237.280361	8000.002260	10.236915	-0.049362	4.815666
237.312163	7999.873622	10.241920	-0.049368	4.815628
237.370005	7999.947139	10.246925	-0.049379	4.815649
237.174041	7999.922626	10.251930	-0.049343	4.815643
237.338624	7999.859109	10.256935	-0.049373	4.815624
237.251318	7999.928146	10.261939	-0.049357	4.815644
237.142458	7999.897568	10.266944	-0.049337	4.815636
237.421794	7999.899949	10.271949	-0.049389	4.815635
237.081871	7999.845358	10.276954	-0.049325	4.815621
237.291794	7999.874368	10.281959	-0.049365	4.815628
237.433912	7999.949247	10.286963	-0.049391	4.815650
237.209471	7999.901858	10.291968	-0.049349	4.815637
237.353898	7999.945821	10.296973	-0.049376	4.815649
237.227838	7999.919235	10.301978	-0.049353	4.815642
237.325268	7999.872779	10.306983	-0.049371	4.815628
237.299097	7999.929995	10.311987	-0.049366	4.815645
237.148910	7999.888076	10.316992	-0.049338	4.815633
237.212104	7999.899772	10.321997	-0.049350	4.815636
237.233896	7999.921473	10.327002	-0.049354	4.815642
237.252049	7999.874802	10.332007	-0.049357	4.815629
237.274286	7999.889039	10.337011	-0.049361	4.815633
237.249481	7999.877965	10.342016	-0.049357	4.815630
237.152658	7999.919096	10.347021	-0.049339	4.815642
237.131644	7999.925162	10.352026	-0.049335	4.815644
237.283933	7999.871053	10.357031	-0.049363	4.815627
237.411088	7999.924343	10.362035	-0.049387	4.815642
237.339406	7999.855941	10.367040	-0.049374	4.815623
237.457755	7999.842911	10.372045	-0.049396	4.815618
237.469914	7999.854850	10.377050	-0.049398	4.815622
237.498737	7999.851047	10.382055	-0.049403	4.815621
237.430016	7999.909710	10.387059	-0.049391	4.815638
237.283953	7999.887071	10.392064	-0.049363	4.815632
237.369010	7999.932209	10.397069	-0.049379	4.815645
237.311074	7999.940880	10.402074	-0.049368	4.815648
237.441559	7999.896025	10.407079	-0.049393	4.815634
237.559217	7999.960903	10.412083	-0.049415	4.815652
237.395149	7999.940107	10.417088	-0.049384	4.815647
237.460327	7999.961442	10.422093	-0.049396	4.815653
237.377207	7999.889652	10.427098	-0.049381	4.815632
237.413437	7999.858217	10.432103	-0.049388	4.815623
237.519194	7999.939981	10.437107	-0.049407	4.815646
237.556774	7999.866940	10.442112	-0.049414	4.815625
237.562448	7999.942817	10.447117	-0.049415	4.815647
237.427447	7999.940636	10.452122	-0.049390	4.815647
237.476749	7999.879525	10.457127	-0.049399	4.815629
237.637590	7999.949371	10.462131	-0.049429	4.815649
237.224832	7999.940566	10.467136	-0.049353	4.815648
237.409344	7999.909393	10.472141	-0.049387	4.815638
237.245579	7999.914219	10.477146	-0.049356	4.815640
237.510530	7999.895019	10.482151	-0.049406	4.815633
237.405241	7999.944553	10.487155	-0.049386	4.815648
237.334490	7999.916726	10.492160	-0.049373	4.815641
237.348068	7999.950035	10.497165	-0.049376	4.815650
237.210699	7999.943547	10.502170	-0.049350	4.815649
237.365237	7999.890541	10.507175	-0.049379	4.815633
237.428210	7999.950266	10.512179	-0.049391	4.815650
237.621939	7999.897894	10.517184	-0.049427	4.815634
237.500636	7999.956776	10.522189	-0.049404	4.815651
237.557704	7999.944890	10.527194	-0.049415	4.815648
237.595797	7999.890003	10.532199	-0.049422	4.815631
237.539497	7999.970215	10.537203	-0.049411	4.815655
237.415008	7999.876409	10.542208	-0.049388	4.815628
237.625840	7999.929985	10.547213	-0.049427	4.815643
237.445052	7999.933468	10.552218	-0.049394	4.815645
237.575930	7999.836318	10.557223	-0.049418	4.815616
237.535258	7999.949871	10.562227	-0.049411	4.815649
237.421368	7999.844496	10.567232	-0.049389	4.815619
237.507256	7999.891782	10.572237	-0.049405	4.815632
237.463650	7999.938043	10.577242	-0.049397	4.815646
237.446075	7999.874784	10.582247	-0.049394	4.815628
237.435652	7999.961075	10.587251	-0.049392	4.815653
237.371544	7999.861841	10.592256	-0.049380	4.815624
237.721605	7999.882443	10.597261	-0.049445	4.815629
237.648665	7999.963454	10.602266	-0.049432	4.815653
237.384929	7999.878071	10.607271	-0.049383	4.815629
237.456750	7999.902715	10.612275	-0.049396	4.815636
237.342565	7999.874186	10.617280	-0.049375	4.815628
237.448471	7999.935672	10.622285	-0.049395	4.815646
237.408262	7999.939292	10.627290	-0.049387	4.815647
237.514085	7999.852411	10.632295	-0.049407	4.815621
237.626952	7999.871314	10.637299	-0.049428	4.815626
237.640133	7999.875798	10.642304	-0.049430	4.815627
237.509167	7999.903569	10.647309	-0.049406	4.815636
237.360215	7999.920375	10.652314	-0.049378	4.815641
237.529686	7999.882555	10.657319	-0.049410	4.815630
237.495705	7999.955656	10.662323	-0.049403	4.815651
237.397253	7999.908168	10.667328	-0.049385	4.815638
237.293116	7999.897947	10.672333	-0.049366	4.815635
237.461498	7999.931623	10.677338	-0.049397	4.815644
237.449514	7999.880196	10.682343	-0.049395	4.815629
237.635407	7999.970728	10.687347	-0.049430	4.815655
237.448885	7999.935692	10.692352	-0.049395	4.815646
237.531753	7999.947706	10.697357	-0.049410	4.815649
237.479010	7999.894553	10.702362	-0.049400	4.815633
237.419371	7999.880781	10.707367	-0.049389	4.815630
237.507718	7999.914232	10.712371	-0.049406	4.815639
237.436847	7999.868257	10.717376	-0.049393	4.815626
237.337220	7999.879457	10.722381	-0.049374	4.815630
237.393764	7999.919865	10.727386	-0.049385	4.815641
237.609839	7999.852910	10.732391	-0.049425	4.815621
237.801675	7999.937134	10.737395	-0.049461	4.815644
237.771390	7999.852321	10.742400	-0.049455	4.815620
237.897610	7999.918406	10.747405	-0.049478	4.815638
237.823136	7999.936416	10.752410	-0.049465	4.815644
237.749627	7999.918151	10.757415	-0.049451	4.815639
237.675853	7999.960722	10.762419	-0.049437	4.815652
237.520520	7999.914449	10.767424	-0.049408	4.815639
237.430107	7999.920461	10.772429	-0.049391	4.815641
237.525052	7999.977500	10.777434	-0.049409	4.815657
237.510845	7999.872668	10.782439	-0.049406	4.815627
237.574735	7999.954823	10.787443	-0.049418	4.815651
237.462769	7999.891106	10.792448	-0.049398	4.815632
237.624067	7999.920398	10.797453	-0.049428	4.815640
237.777538	7999.895128	10.802458	-0.049456	4.815632
237.505675	7999.871522	10.807463	-0.049406	4.815626
237.532089	7999.942397	10.812467	-0.049411	4.815647
237.865780	7999.939253	10.817472	-0.049473	4.815645
237.881273	7999.919224	10.822477	-0.049476	4.815639
237.609308	7999.924435	10.827482	-0.049425	4.815641
237.692853	7999.930056	10.832487	-0.049441	4.815643
237.804321	7999.959611	10.837491	-0.049461	4.815651
237.626578	7999.886291	10.842496	-0.049428	4.815630
237.495534	7999.891646	10.847501	-0.049404	4.815632
237.452421	7999.916567	10.852506	-0.049396	4.815640
237.523058	7999.852600	10.857511	-0.049409	4.815621
237.683742	7999.959802	10.862515	-0.049439	4.815651
237.855192	7999.902800	10.867520	-0.049471	4.815634
237.755468	7999.926806	10.872525	-0.049452	4.815641
237.424220	7999.908645	10.877530	-0.049391	4.815638
237.837538	7999.872631	10.882535	-0.049468	4.815625
237.864716	7999.927508	10.887539	-0.049473	4.815641
237.601953	7999.878431	10.892544	-0.049424	4.815628
237.867780	7999.960649	10.897549	-0.049473	4.815651
237.798055	7999.976601	10.902554	-0.049460	4.815656
237.791483	7999.973293	10.907559	-0.049459	4.815655
237.740649	7999.981012	10.912563	-0.049450	4.815657
237.554355	7999.910756	10.917568	-0.049415	4.815638
237.688651	7999.907591	10.922573	-0.049440	4.815636
237.609009	7999.935124	10.927578	-0.049425	4.815645
237.657640	7999.811027	10.932583	-0.049434	4.815608
237.667053	7999.881627	10.937587	-0.049436	4.815629
237.651716	7999.912334	10.942592	-0.049433	4.815638
237.587627	7999.942254	10.947597	-0.049421	4.815647
237.692699	7999.950357	10.952602	-0.049441	4.815649
237.712817	7999.896247	10.957607	-0.049444	4.815633
237.480776	7999.917047	10.962611	-0.049401	4.815640
237.490259	7999.877708	10.967616	-0.049403	4.815628
237.574755	7999.970870	10.972621	-0.049419	4.815655
237.461555	7999.975446	10.977626	-0.049398	4.815657
237.678213	7999.936253	10.982631	-0.049438	4.815645
237.810657	7999.960810	10.987635	-0.049463	4.815651
237.647203	7999.914406	10.992640	-0.049432	4.815638
237.509160	7999.928187	10.997645	-0.049407	4.815643
237.563589	7999.929067	11.002650	-0.049417	4.815643
237.651965	7999.849375	11.007655	-0.049433	4.815619
237.638205	7999.953758	11.012659	-0.049431	4.815650
237.386954	7999.894194	11.017664	-0.049384	4.815634
237.504611	7999.906770	11.022669	-0.049406	4.815637
237.345468	7999.893525	11.027674	-0.049376	4.815634
237.460704	7999.871906	11.032679	-0.049398	4.815627
237.561502	7999.933310	11.037683	-0.049417	4.815644
237.611938	7999.937328	11.042688	-0.049426	4.815645
237.617450	7999.939553	11.047693	-0.049427	4.815646
237.734554	7999.945716	11.052698	-0.049449	4.815647
237.546186	7999.839136	11.057703	-0.049414	4.815617
237.591933	7999.902852	11.062707	-0.049422	4.815635
237.709594	7999.884475	11.067712	-0.049444	4.815629
237.833812	7999.916370	11.072717	-0.049467	4.815638
237.414198	7999.890376	11.077722	-0.049389	4.815632
237.594143	7999.816434	11.082727	-0.049423	4.815610
237.987983	7999.956225	11.087731	-0.049496	4.815649
237.624876	7999.931143	11.092736	-0.049428	4.815643
237.528898	7999.925323	11.097741	-0.049411	4.815642
237.584648	7999.945438	11.102746	-0.049421	4.815648
237.557638	7999.883094	11.107751	-0.049416	4.815630
237.607352	7999.921257	11.112755	-0.049425	4.815641
237.609414	7999.973593	11.117760	-0.049426	4.815656
237.572139	7999.962318	11.122765	-0.049419	4.815653
237.566226	7999.972897	11.127770	-0.049418	4.815656
237.429627	7999.895973	11.132775	-0.049392	4.815634
237.604252	7999.920144	11.137779	-0.049425	4.815640
237.624007	7999.857489	11.142784	-0.049428	4.815622
237.789713	7999.892190	11.147789	-0.049459	4.815631
237.810401	7999.929884	11.152794	-0.049463	4.815642
237.848573	7999.860054	11.157799	-0.049470	4.815621
237.583289	7999.932619	11.162803	-0.049421	4.815644
237.387927	7999.900643	11.167808	-0.049384	4.815636
237.688232	7999.877746	11.172813	-0.049440	4.815627
237.624091	7999.945023	11.177818	-0.049428	4.815647
237.644535	7999.880243	11.182823	-0.049432	4.815628
237.748267	7999.941695	11.187827	-0.049452	4.815646
237.796304	7999.912585	11.192832	-0.049461	4.815637
237.816599	7999.897971	11.197837	-0.049464	4.815633
237.685030	7999.918260	11.202842	-0.049440	4.815639
237.732989	7999.896621	11.207847	-0.049449	4.815633
237.608629	7999.953319	11.212851	-0.049426	4.815650
237.584104	7999.862195	11.217856	-0.049421	4.815623
237.857715	7999.906112	11.222861	-0.049472	4.815635
237.880375	7999.904345	11.227866	-0.049476	4.815634
237.537869	7999.861451	11.232871	-0.049413	4.815623
237.745842	7999.841331	11.237875	-0.049451	4.815616
237.797767	7999.838969	11.242880	-0.049461	4.815616
237.598749	7999.848562	11.247885	-0.049424	4.815619
237.790772	7999.894362	11.252890	-0.049460	4.815632
237.821740	7999.846831	11.257895	-0.049465	4.815618
237.818211	7999.924694	11.262899	-0.049465	4.815641
237.547698	7999.889369	11.267904	-0.049414	4.815631
237.829329	7999.909933	11.272909	-0.049467	4.815636
237.792429	7999.971246	11.277914	-0.049460	4.815654
237.763656	7999.903536	11.282919	-0.049455	4.815635
237.928577	7999.953168	11.287923	-0.049485	4.815648
237.764591	7999.901418	11.292928	-0.049455	4.815634
237.770201	7999.913251	11.297933	-0.049456	4.815637
237.780889	7999.971064	11.302938	-0.049458	4.815654
237.832189	7999.900379	11.307943	-0.049468	4.815633
237.607536	7999.928771	11.312947	-0.049426	4.815643
237.469096	7999.898782	11.317952	-0.049400	4.815635
237.668914	7999.940438	11.322957	-0.049437	4.815646
237.747883	7999.928907	11.327962	-0.049452	4.815642
237.715274	7999.886753	11.332967	-0.049446	4.815630
237.784157	7999.890002	11.337971	-0.049459	4.815631
237.732504	7999.907314	11.342976	-0.049449	4.815636
237.673373	7999.920235	11.347981	-0.049438	4.815640
237.954675	7999.952535	11.352986	-0.049490	4.815648
237.930004	7999.903037	11.357991	-0.049486	4.815634
237.853210	7999.955167	11.362995	-0.049472	4.815649
237.649144	7999.917713	11.368000	-0.049434	4.815639
237.839613	7999.890905	11.373005	-0.049469	4.815631
237.644442	7999.916571	11.378010	-0.049433	4.815639
237.552730	7999.874529	11.383015	-0.049416	4.815627
237.872350	7999.857281	11.388019	-0.049475	4.815621
237.795873	7999.833631	11.393024	-0.049461	4.815614
237.814776	7999.909722	11.398029	-0.049464	4.815636
237.618813	7999.930038	11.403034	-0.049428	4.815643
237.923399	7999.851706	11.408039	-0.049485	4.815619
237.765559	7999.915333	11.413043	-0.049455	4.815638
237.731832	7999.878498	11.418048	-0.049449	4.815627
237.802881	7999.906332	11.423053	-0.049462	4.815635
237.764929	7999.886507	11.428058	-0.049455	4.815630
237.697666	7999.865140	11.433063	-0.049443	4.815624
237.593998	7999.893352	11.438067	-0.049423	4.815632
237.675960	7999.887206	11.443072	-0.049439	4.815630
237.830753	7999.881170	11.448077	-0.049468	4.815628
237.687501	7999.908743	11.453082	-0.049441	4.815636
237.873861	7999.850915	11.458087	-0.049476	4.815619
237.899927	7999.923920	11.463091	-0.049480	4.815640
237.887127	7999.866074	11.468096	-0.049478	4.815623
238.083610	7999.887397	11.473101	-0.049515	4.815628
237.936549	7999.933054	11.478106	-0.049487	4.815642
237.922361	7999.897601	11.483111	-0.049485	4.815632
237.913120	7999.893183	11.488115	-0.049483	4.815631
237.857463	7999.864532	11.493120	-0.049473	4.815623
237.810282	7999.928882	11.498125	-0.049464	4.815642
237.685278	7999.885234	11.503130	-0.049441	4.815630
237.828952	7999.889692	11.508135	-0.049467	4.815630
237.823877	7999.960059	11.513139	-0.049466	4.815651
237.483632	7999.885180	11.518144	-0.049403	4.815631
237.701036	7999.917514	11.523149	-0.049444	4.815639
237.970245	7999.938945	11.528154	-0.049494	4.815644
237.769195	7999.893000	11.533159	-0.049456	4.815631
237.737205	7999.943719	11.538163	-0.049450	4.815646
237.858706	7999.943549	11.543168	-0.049473	4.815646
237.879176	7999.886242	11.548173	-0.049477	4.815629
237.874385	7999.905378	11.553178	-0.049476	4.815635
237.748797	7999.871328	11.558183	-0.049453	4.815625
237.654268	7999.938114	11.563187	-0.049435	4.815645
237.677283	7999.917139	11.568192	-0.049439	4.815639
237.791598	7999.933931	11.573197	-0.049461	4.815643
237.935621	7999.996035	11.578202	-0.049487	4.815661
237.843774	7999.895283	11.583207	-0.049470	4.815632
238.035565	7999.947485	11.588211	-0.049506	4.815646
237.957404	7999.918470	11.593216	-0.049491	4.815638
237.836748	7999.904779	11.598221	-0.049469	4.815635
237.870164	7999.921331	11.603226	-0.049475	4.815639
237.811194	7999.873413	11.608231	-0.049464	4.815626
238.242832	7999.932695	11.613235	-0.049545	4.815641
237.982117	7999.890054	11.618240	-0.049496	4.815630
238.073405	7999.899003	11.623245	-0.049513	4.815632
238.039237	7999.943282	11.628250	-0.049507	4.815645
238.100653	7999.938939	11.633255	-0.049518	4.815643
238.116768	7999.988301	11.638259	-0.049521	4.815658
238.002934	7999.926687	11.643264	-0.049500	4.815640
237.942524	7999.878746	11.648269	-0.049489	4.815626
237.883322	7999.934362	11.653274	-0.049478	4.815643
237.785547	7999.843122	11.658279	-0.049460	4.815617
237.822657	7999.912036	11.663283	-0.049467	4.815637
237.801920	7999.921308	11.668288	-0.049463	4.815640
237.865293	7999.859357	11.673293	-0.049474	4.815621
237.850810	7999.885809	11.678298	-0.049472	4.815629
237.896493	7999.848122	11.683303	-0.049480	4.815618
237.942648	7999.929991	11.688307	-0.049489	4.815641
237.835585	7999.932531	11.693312	-0.049469	4.815643
238.006680	7999.909680	11.698317	-0.049501	4.815635
238.102564	7999.952860	11.703322	-0.049519	4.815647
237.987331	7999.901897	11.708327	-0.049497	4.815633
238.184167	7999.987271	11.713331	-0.049534	4.815657
238.117012	7999.882648	11.718336	-0.049521	4.815627
238.183514	7999.907207	11.723341	-0.049534	4.815634
238.117060	7999.961638	11.728346	-0.049522	4.815650
238.100222	7999.867436	11.733351	-0.049518	4.815622
238.073760	7999.992962	11.738355	-0.049514	4.815659
237.841641	7999.991345	11.743360	-0.049470	4.815660
238.122800	7999.959600	11.748365	-0.049523	4.815649
237.933939	7999.949076	11.753370	-0.049487	4.815647
237.781585	7999.927401	11.758375	-0.049459	4.815641
237.983331	7999.994707	11.763379	-0.049497	4.815660
238.042415	7999.938024	11.768384	-0.049508	4.815643
238.052830	7999.939260	11.773389	-0.049510	4.815644
238.116967	7999.913613	11.778394	-0.049522	4.815636
237.923715	7999.869929	11.783399	-0.049486	4.815624
237.942120	7999.878767	11.788403	-0.049489	4.815626
237.924987	7999.868884	11.793408	-0.049486	4.815624
238.075099	7999.883053	11.798413	-0.049514	4.815627
237.840539	7999.942239	11.803418	-0.049470	4.815646
237.780368	7999.908178	11.808423	-0.049459	4.815636
237.771813	7999.940062	11.813427	-0.049457	4.815645
237.809847	7999.924667	11.818432	-0.049465	4.815641
237.910136	7999.959379	11.823437	-0.049483	4.815650
237.981889	7999.995764	11.828442	-0.049497	4.815660
237.902018	7999.968856	11.833447	-0.049482	4.815653
237.902302	8000.012625	11.838451	-0.049482	4.815666
237.769375	7999.964579	11.843456	-0.049457	4.815652
237.889303	7999.904610	11.848461	-0.049479	4.815634
237.998795	7999.959751	11.853466	-0.049500	4.815650
237.749909	7999.942919	11.858471	-0.049453	4.815646
237.928362	7999.913783	11.863475	-0.049487	4.815637
237.890814	7999.883290	11.868480	-0.049480	4.815628
237.934412	7999.909613	11.873485	-0.049488	4.815636
237.859036	7999.945755	11.878490	-0.049474	4.815646
237.781441	7999.919951	11.883495	-0.049459	4.815639
237.787500	8000.005442	11.888499	-0.049461	4.815664
237.803539	7999.956602	11.893504	-0.049464	4.815650
238.000442	7999.910686	11.898509	-0.049500	4.815636
237.902102	7999.876008	11.903514	-0.049482	4.815626
237.785439	7999.836764	11.908519	-0.049460	4.815615
238.002151	7999.947008	11.913523	-0.049501	4.815646
237.937194	7999.925678	11.918528	-0.049488	4.815640
237.966889	7999.904811	11.923533	-0.049494	4.815634
237.988266	7999.947854	11.928538	-0.049498	4.815646
238.142927	7999.911928	11.933543	-0.049527	4.815635
238.011969	7999.959980	11.938547	-0.049502	4.815650
237.820635	7999.960090	11.943552	-0.049467	4.815651
237.973455	7999.948685	11.948557	-0.049495	4.815647
237.975397	7999.975403	11.953562	-0.049496	4.815655
237.947763	7999.882093	11.958567	-0.049490	4.815627
237.832875	7999.994449	11.963571	-0.049469	4.815661
237.967952	7999.925118	11.968576	-0.049494	4.815640
238.020136	7999.901412	11.973581	-0.049504	4.815633
238.157748	7999.953805	11.978586	-0.049530	4.815647
238.054502	7999.928654	11.983591	-0.049510	4.815641
238.140719	7999.904432	11.988595	-0.049526	4.815633
237.772271	7999.840838	11.993600	-0.049458	4.815616
237.916046	7999.846365	11.998605	-0.049485	4.815617
237.966969	7999.928311	12.003610	-0.049494	4.815641
237.736597	7999.861612	12.008615	-0.049451	4.815622
238.055716	7999.964972	12.013619	-0.049511	4.815651
238.151042	7999.928087	12.018624	-0.049528	4.815640
238.148968	7999.912044	12.023629	-0.049528	4.815635
238.003557	7999.957727	12.028634	-0.049501	4.815649
238.049259	7999.922175	12.033639	-0.049510	4.815639
238.177777	7999.990433	12.038643	-0.049534	4.815658
238.119683	7999.924383	12.043648	-0.049523	4.815639
238.035280	7999.904874	12.048653	-0.049507	4.815634
238.134749	7999.919291	12.053658	-0.049526	4.815637
238.196427	7999.832763	12.058663	-0.049537	4.815612
238.136709	7999.946010	12.063667	-0.049526	4.815645
237.933212	7999.955530	12.068672	-0.049488	4.815649
237.859224	7999.924448	12.073677	-0.049474	4.815640
237.970901	7999.961478	12.078682	-0.049495	4.815651
237.804521	7999.935307	12.083687	-0.049464	4.815644
238.164828	7999.969952	12.088691	-0.049531	4.815652
238.044760	7999.953069	12.093696	-0.049509	4.815648
238.107344	7999.981834	12.098701	-0.049521	4.815656
237.990715	7999.977814	12.103706	-0.049499	4.815655
237.800537	7999.984347	12.108711	-0.049463	4.815658
238.113024	7999.991535	12.113715	-0.049522	4.815659
238.111478	7999.959489	12.118720	-0.049521	4.815649
237.991608	7999.983170	12.123725	-0.049499	4.815657
238.062310	8000.005662	12.128730	-0.049512	4.815663
237.976694	7999.958380	12.133735	-0.049496	4.815650
238.010420	7999.961061	12.138739	-0.049503	4.815650
237.868668	7999.881918	12.143744	-0.049476	4.815628
237.788000	7999.917974	12.148749	-0.049461	4.815639
238.166627	7999.905950	12.153754	-0.049532	4.815633
237.791465	7999.874269	12.158759	-0.049462	4.815626
237.835311	7999.957168	12.163763	-0.049470	4.815650
238.005672	7999.926834	12.168768	-0.049502	4.815640
238.117405	7999.955326	12.173773	-0.049523	4.815648
238.102054	7999.982831	12.178778	-0.049520	4.815656
238.169753	7999.949770	12.183783	-0.049532	4.815646
238.061792	7999.999261	12.188787	-0.049512	4.815661
237.895277	7999.966682	12.193792	-0.049481	4.815652
238.125906	7999.933053	12.198797	-0.049524	4.815641
238.207176	7999.982401	12.203802	-0.049539	4.815656
237.746579	7999.899171	12.208807	-0.049454	4.815633
237.974929	7999.977581	12.213811	-0.049496	4.815655
238.144995	7999.971792	12.218816	-0.049528	4.815653
238.191187	8000.005629	12.223821	-0.049536	4.815662
237.899313	8000.017990	12.228826	-0.049482	4.815667
238.075658	7999.962135	12.233831	-0.049515	4.815650
238.316957	7999.978846	12.238835	-0.049560	4.815654
238.186991	8000.005565	12.243840	-0.049536	4.815662
237.975226	8000.004277	12.248845	-0.049496	4.815663
238.078550	8000.017690	12.253850	-0.049516	4.815666
238.216524	7999.929193	12.258855	-0.049541	4.815640
237.892929	7999.954917	12.263859	-0.049481	4.815649
237.907644	7999.880438	12.268864	-0.049484	4.815627
238.175959	7999.947753	12.273869	-0.049534	4.815646
238.028722	7999.991272	12.278874	-0.049506	4.815659
237.902725	7999.946540	12.283879	-0.049483	4.815646
238.085265	7999.969772	12.288883	-0.049517	4.815652
238.028192	7999.911211	12.293888	-0.049506	4.815636
238.013376	7999.950466	12.298893	-0.049503	4.815647
238.040175	7999.986125	12.303898	-0.049509	4.815657
238.099993	7999.914510	12.308903	-0.049520	4.815636
238.226240	7999.995540	12.313907	-0.049543	4.815659
238.087654	7999.932458	12.318912	-0.049517	4.815641
238.256732	7999.939462	12.323917	-0.049549	4.815643
238.143845	7999.929099	12.328922	-0.049528	4.815640
238.096046	7999.870687	12.333927	-0.049519	4.815623
238.153522	7999.906842	12.338931	-0.049530	4.815634
237.899109	7999.942223	12.343936	-0.049482	4.815645
237.822236	7999.882275	12.348941	-0.049468	4.815628
238.106270	7999.994675	12.353946	-0.049521	4.815660
237.958410	7999.923972	12.358951	-0.049493	4.815640
238.225221	7999.949634	12.363955	-0.049543	4.815646
238.179256	7999.883781	12.368960	-0.049534	4.815627
238.121230	7999.903124	12.373965	-0.049524	4.815633
238.050992	7999.893451	12.378970	-0.049511	4.815630
238.152872	7999.945266	12.383975	-0.049530	4.815645
238.211017	7999.992106	12.388979	-0.049541	4.815658
238.033597	7999.991373	12.393984	-0.049507	4.815659
238.033798	7999.916659	12.398989	-0.049507	4.815637
238.200788	7999.899079	12.403994	-0.049539	4.815631
238.042263	7999.874102	12.408999	-0.049509	4.815625
238.127649	7999.944864	12.414003	-0.049525	4.815645
238.077093	7999.918430	12.419008	-0.049516	4.815637
238.298766	7999.913476	12.424013	-0.049557	4.815635
238.023089	7999.946379	12.429018	-0.049506	4.815646
237.976417	7999.887986	12.434023	-0.049497	4.815629
238.225478	7999.954990	12.439027	-0.049543	4.815647
238.042470	7999.903999	12.444032	-0.049509	4.815633
238.111592	7999.928601	12.449037	-0.049522	4.815640
238.159839	7999.959269	12.454042	-0.049531	4.815649
238.167607	7999.938047	12.459047	-0.049533	4.815643
238.317607	7999.976765	12.464051	-0.049561	4.815653
238.223541	7999.978448	12.469056	-0.049543	4.815654
238.179713	7999.915831	12.474061	-0.049535	4.815636
238.251724	7999.953287	12.479066	-0.049548	4.815647
238.050816	7999.911614	12.484071	-0.049511	4.815636
238.254122	7999.959733	12.489075	-0.049549	4.815649
238.276217	7999.954754	12.494080	-0.049553	4.815647
238.080212	8000.001754	12.499085	-0.049516	4.815662
238.035580	7999.959404	12.504090	-0.049508	4.815650
238.185197	7999.957555	12.509095	-0.049536	4.815648
238.189927	7999.996059	12.514099	-0.049537	4.815660
238.116875	7999.944711	12.519104	-0.049523	4.815645
238.226837	7999.925141	12.524109	-0.049544	4.815639
238.242166	7999.981963	12.529114	-0.049547	4.815655
238.106058	7999.922123	12.534119	-0.049521	4.815638
238.205146	7999.978164	12.539123	-0.049540	4.815654
238.246491	7999.944676	12.544128	-0.049547	4.815644
238.174936	7999.922172	12.549133	-0.049534	4.815638
238.215829	7999.973002	12.554138	-0.049542	4.815653
238.299834	7999.877228	12.559143	-0.049557	4.815624
238.271002	7999.923728	12.564147	-0.049552	4.815638
237.937542	7999.908732	12.569152	-0.049490	4.815635
238.058934	7999.932043	12.574157	-0.049513	4.815641
238.163426	7999.963621	12.579162	-0.049532	4.815650
238.031266	7999.883565	12.584167	-0.049507	4.815627
238.090875	7999.961382	12.589171	-0.049519	4.815650
238.282388	7999.898301	12.594176	-0.049554	4.815631
238.175905	7999.899782	12.599181	-0.049534	4.815631
238.305501	7999.952047	12.604186	-0.049559	4.815646
238.255112	7999.922413	12.609191	-0.049549	4.815638
238.284775	7999.985870	12.614195	-0.049555	4.815656
238.228238	7999.939059	12.619200	-0.049544	4.815643
238.314357	7999.942587	12.624205	-0.049560	4.815643
238.243906	7999.971336	12.629210	-0.049547	4.815652
237.977754	7999.955293	12.634215	-0.049498	4.815649
238.171056	7999.979767	12.639219	-0.049534	4.815655
238.265615	7999.959949	12.644224	-0.049551	4.815649
238.232730	7999.892172	12.649229	-0.049545	4.815629
238.295052	7999.950820	12.654234	-0.049557	4.815646
238.264782	7999.839322	12.659239	-0.049551	4.815613
238.433359	7999.951991	12.664243	-0.049583	4.815646
238.296787	7999.927368	12.669248	-0.049557	4.815639
238.310742	7999.912651	12.674253	-0.049560	4.815635
238.358971	7999.963600	12.679258	-0.049569	4.815649
238.404743	7999.937656	12.684263	-0.049577	4.815641
238.190254	7999.913908	12.689267	-0.049537	4.815636
238.268298	7999.949328	12.694272	-0.049552	4.815646
238.166358	7999.917793	12.699277	-0.049533	4.815637
238.042047	7999.960615	12.704282	-0.049510	4.815650
237.981785	7999.847565	12.709287	-0.049498	4.815617
238.183105	7999.969302	12.714291	-0.049536	4.815652
238.117964	7999.947969	12.719296	-0.049524	4.815646
238.215520	7999.895110	12.724301	-0.049542	4.815630
238.315334	7999.915938	12.729306	-0.049561	4.815636
238.192391	7999.889401	12.734311	-0.049538	4.815628
238.059592	7999.954501	12.739315	-0.049513	4.815648
238.075639	7999.948357	12.744320	-0.049516	4.815646
238.088890	7999.850372	12.749325	-0.049518	4.815617
238.091431	7999.908053	12.754330	-0.049519	4.815634
238.107654	7999.859216	12.759335	-0.049522	4.815620
238.419853	7999.888815	12.764339	-0.049580	4.815627
238.243211	7999.935060	12.769344	-0.049547	4.815641
238.072995	7999.904557	12.774349	-0.049516	4.815633
238.298329	7999.961571	12.779354	-0.049558	4.815649
238.232095	7999.870840	12.784359	-0.049545	4.815623
238.302609	7999.901868	12.789363	-0.049558	4.815631
238.322559	7999.933146	12.794368	-0.049562	4.815641
238.306792	7999.899803	12.799373	-0.049559	4.815631
238.227326	7999.929473	12.804378	-0.049544	4.815640
238.154509	7999.915488	12.809383	-0.049531	4.815636
238.286859	7999.959258	12.814387	-0.049556	4.815648
238.216876	7999.929307	12.819392	-0.049543	4.815640
238.191023	7999.888329	12.824397	-0.049538	4.815628
238.486815	7999.949685	12.829402	-0.049593	4.815645
238.416086	7999.870622	12.834407	-0.049580	4.815622
238.253251	7999.939506	12.839411	-0.049549	4.815643
238.201107	7999.939731	12.844416	-0.049540	4.815643
238.327948	7999.910828	12.849421	-0.049563	4.815634
238.257190	7999.967325	12.854426	-0.049550	4.815651
237.985188	7999.945850	12.859431	-0.049499	4.815646
238.235109	7999.946689	12.864435	-0.049546	4.815645
238.221718	7999.915519	12.869440	-0.049544	4.815636
238.263539	7999.895916	12.874445	-0.049551	4.815630
238.320079	7999.922448	12.879450	-0.049562	4.815637
238.253969	7999.878684	12.884455	-0.049550	4.815625
238.364995	7999.929581	12.889459	-0.049570	4.815639
238.089108	7999.969952	12.894464	-0.049519	4.815652
238.162657	7999.875076	12.899469	-0.049533	4.815624
238.225515	7999.967890	12.904474	-0.049544	4.815651
238.007114	7999.886440	12.909479	-0.049504	4.815628
238.217718	7999.960294	12.914483	-0.049543	4.815649
238.290343	7999.949728	12.919488	-0.049556	4.815646
238.117877	7999.873290	12.924493	-0.049524	4.815624
238.125478	7999.982289	12.929498	-0.049526	4.815656
238.202440	7999.885333	12.934503	-0.049540	4.815627
238.256633	7999.871266	12.939507	-0.049550	4.815623
238.318413	7999.882940	12.944512	-0.049562	4.815626
238.390072	7999.856347	12.949517	-0.049575	4.815618
238.259623	7999.886261	12.954522	-0.049551	4.815627
238.149775	7999.861004	12.959527	-0.049530	4.815620
238.240412	7999.891290	12.964531	-0.049547	4.815629
238.246635	7999.840156	12.969536	-0.049548	4.815614
238.106238	7999.867775	12.974541	-0.049522	4.815622
238.145882	7999.976224	12.979546	-0.049530	4.815654
238.259153	7999.902271	12.984551	-0.049551	4.815632
238.106986	7999.954249	12.989555	-0.049522	4.815648
238.148265	7999.939974	12.994560	-0.049530	4.815643
238.065852	7999.905553	12.999565	-0.049515	4.815634
238.166070	7999.975488	13.004570	-0.049534	4.815654
237.985581	7999.938414	13.009575	-0.049500	4.815644
238.212397	7999.908992	13.014579	-0.049542	4.815634
238.093620	7999.957241	13.019584	-0.049520	4.815649
238.034954	7999.942417	13.024589	-0.049509	4.815645
238.196128	7999.984518	13.029594	-0.049539	4.815656
238.170918	7999.931808	13.034599	-0.049534	4.815641
238.110164	7999.967119	13.039603	-0.049523	4.815651
238.227873	7999.882563	13.044608	-0.049545	4.815626
238.214351	7999.888750	13.049613	-0.049543	4.815628
238.302354	7999.900848	13.054618	-0.049559	4.815631
238.116419	7999.862619	13.059623	-0.049524	4.815621
238.218875	7999.936859	13.064627	-0.049543	4.815642
238.338894	7999.955879	13.069632	-0.049566	4.815647
238.345820	7999.920768	13.074637	-0.049567	4.815637
238.301432	7999.980893	13.079642	-0.049559	4.815655
238.264894	7999.901315	13.084647	-0.049552	4.815631
238.302602	7999.948892	13.089651	-0.049559	4.815645
238.168620	7999.962738	13.094656	-0.049534	4.815650
238.054887	7999.924608	13.099661	-0.049513	4.815639
238.255226	7999.967342	13.104666	-0.049550	4.815651
238.064003	7999.913016	13.109671	-0.049515	4.815636
238.456042	7999.901210	13.114675	-0.049588	4.815631
238.337232	7999.974008	13.119680	-0.049566	4.815652
238.236011	7999.954226	13.124685	-0.049547	4.815647
238.216842	7999.979535	13.129690	-0.049543	4.815655
238.365115	7999.927496	13.134695	-0.049571	4.815639
238.225868	7999.933785	13.139699	-0.049545	4.815641
238.176007	7999.947923	13.144704	-0.049536	4.815646
238.375470	7999.963958	13.149709	-0.049573	4.815649
238.416613	7999.950748	13.154714	-0.049580	4.815645
238.038517	7999.919018	13.159719	-0.049510	4.815638
238.038008	7999.972381	13.164723	-0.049510	4.815653
238.218238	7999.944341	13.169728	-0.049544	4.815644
238.111456	7999.956492	13.174733	-0.049524	4.815648
238.356879	7999.955124	13.179738	-0.049569	4.815647
238.241912	7999.925514	13.184743	-0.049548	4.815639
238.321954	7999.973775	13.189747	-0.049563	4.815652
238.299305	7999.945657	13.194752	-0.049559	4.815644
238.147550	7999.954946	13.199757	-0.049530	4.815648
238.305884	8000.022619	13.204762	-0.049560	4.815667
238.203954	7999.875804	13.209767	-0.049541	4.815624
238.182020	7999.920282	13.214771	-0.049537	4.815637
238.199609	7999.960061	13.219776	-0.049540	4.815649
238.251527	7999.922475	13.224781	-0.049550	4.815638
238.193557	7999.970639	13.229786	-0.049539	4.815652
238.115463	7999.944827	13.234791	-0.049525	4.815645
238.132053	7999.963242	13.239795	-0.049528	4.815650
238.234385	7999.953156	13.244800	-0.049547	4.815647
238.242509	7999.920199	13.249805	-0.049548	4.815637
238.357813	7999.969030	13.254810	-0.049570	4.815651
238.226225	7999.875107	13.259815	-0.049545	4.815624
238.256116	7999.895872	13.264819	-0.049551	4.815630
238.309665	7999.901008	13.269824	-0.049561	4.815631
238.240969	7999.892426	13.274829	-0.049548	4.815629
238.267582	7999.973980	13.279834	-0.049553	4.815653
238.268666	7999.901415	13.284839	-0.049553	4.815631
238.400605	8000.002819	13.289843	-0.049578	4.815660
238.325708	7999.969586	13.294848	-0.049564	4.815651
238.193836	7999.941837	13.299853	-0.049539	4.815644
238.371203	7999.998076	13.304858	-0.049572	4.815659
238.188106	7999.950286	13.309863	-0.049538	4.815646
238.186331	7999.983348	13.314867	-0.049538	4.815656
238.203224	7999.982554	13.319872	-0.049541	4.815656
238.099020	7999.916826	13.324877	-0.049522	4.815637
238.070114	7999.992146	13.329882	-0.049516	4.815659
238.009759	7999.928194	13.334887	-0.049505	4.815641
238.212583	7999.994451	13.339891	-0.049543	4.815659
238.113809	7999.993922	13.344896	-0.049525	4.815659
238.168650	7999.982001	13.349901	-0.049535	4.815656
238.305962	8000.007705	13.354906	-0.049560	4.815662
238.167646	7999.942493	13.359911	-0.049535	4.815644
238.246745	7999.990739	13.364915	-0.049549	4.815658
238.103523	7999.964941	13.369920	-0.049523	4.815651
238.203261	7999.924926	13.374925	-0.049541	4.815639
238.146443	7999.913334	13.379930	-0.049531	4.815636
238.248356	7999.910713	13.384935	-0.049550	4.815634
238.312501	7999.950178	13.389939	-0.049562	4.815646
238.192033	7999.950366	13.394944	-0.049539	4.815646
238.156767	7999.956201	13.399949	-0.049533	4.815648
238.213476	7999.987006	13.404954	-0.049543	4.815657
237.937649	7999.943054	13.409959	-0.049492	4.815645
238.027724	7999.946646	13.414963	-0.049509	4.815646
238.104922	7999.961771	13.419968	-0.049523	4.815650
238.234548	7999.930778	13.424973	-0.049547	4.815640
238.077846	8000.006166	13.429978	-0.049518	4.815663
238.236063	7999.935074	13.434983	-0.049547	4.815641
238.116204	7999.940609	13.439987	-0.049525	4.815644
238.214083	7999.945395	13.444992	-0.049543	4.815645
238.225433	7999.956254	13.449997	-0.049546	4.815648
238.391566	7999.951469	13.455002	-0.049577	4.815646
238.266659	7999.909956	13.460007	-0.049553	4.815634
238.114788	7999.900030	13.465011	-0.049525	4.815632
238.182877	7999.942761	13.470016	-0.049538	4.815644
238.431787	7999.873135	13.475021	-0.049584	4.815622
238.434459	7999.953235	13.480026	-0.049585	4.815646
238.128887	7999.904532	13.485031	-0.049528	4.815633
238.272016	7999.997576	13.490035	-0.049554	4.815660
238.373678	8000.021637	13.495040	-0.049573	4.815666
238.396001	7999.936606	13.500045	-0.049577	4.815641
238.316231	7999.985485	13.505050	-0.049563	4.815656
238.200433	7999.953726	13.510055	-0.049541	4.815647
238.275461	8000.005109	13.515059	-0.049555	4.815662
238.139121	7999.959141	13.520064	-0.049530	4.815649
238.264012	7999.940881	13.525069	-0.049553	4.815643
238.354133	7999.976496	13.530074	-0.049570	4.815653
238.130201	7999.918439	13.535079	-0.049528	4.815637
238.223013	7999.956232	13.540083	-0.049545	4.815648
238.354928	7999.959433	13.545088	-0.049570	4.815648
238.354232	7999.916727	13.550093	-0.049570	4.815636
238.251095	7999.957756	13.555098	-0.049551	4.815648
238.355608	7999.953043	13.560103	-0.049570	4.815646
238.454879	7999.911952	13.565107	-0.049589	4.815634
238.230982	7999.933951	13.570112	-0.049547	4.815641
238.409471	7999.901614	13.575117	-0.049580	4.815631
238.400883	7999.987936	13.580122	-0.049579	4.815656
238.245845	7999.902172	13.585127	-0.049550	4.815632
238.371601	7999.966116	13.590131	-0.049573	4.815650
238.257065	7999.970670	13.595136	-0.049552	4.815652
238.514793	7999.956692	13.600141	-0.049600	4.815646
238.387060	8000.011200	13.605146	-0.049576	4.815663
238.463903	7999.970815	13.610151	-0.049590	4.815651
238.574292	7999.964061	13.615155	-0.049611	4.815648
238.520835	7999.965333	13.620160	-0.049601	4.815649
238.292933	7999.874121	13.625165	-0.049558	4.815623
238.392219	7999.948311	13.630170	-0.049577	4.815645
238.322067	7999.951448	13.635175	-0.049564	4.815646
238.399879	8000.008212	13.640179	-0.049579	4.815662
238.328496	7999.981441	13.645184	-0.049565	4.815655
238.319192	7999.972752	13.650189	-0.049563	4.815652
238.348622	7999.945476	13.655194	-0.049569	4.815644
238.415999	7999.877185	13.660199	-0.049581	4.815624
238.375065	7999.893603	13.665203	-0.049574	4.815629
238.272758	7999.966668	13.670208	-0.049555	4.815651
238.353677	7999.981854	13.675213	-0.049570	4.815655
238.373829	8000.030214	13.680218	-0.049574	4.815669
238.264408	7999.980413	13.685223	-0.049553	4.815655
238.415777	7999.979659	13.690227	-0.049582	4.815654
238.543269	7999.981721	13.695232	-0.049605	4.815654
238.455760	7999.936543	13.700237	-0.049589	4.815641
238.420959	7999.951993	13.705242	-0.049583	4.815646
238.326010	7999.914167	13.710247	-0.049565	4.815635
238.356072	7999.960552	13.715251	-0.049570	4.815648
238.197195	7999.886468	13.720256	-0.049541	4.815627
238.288128	7999.877265	13.725261	-0.049558	4.815624
238.608179	7999.968902	13.730266	-0.049617	4.815650
238.267784	7999.929241	13.735271	-0.049554	4.815640
238.334454	7999.973017	13.740275	-0.049567	4.815652
238.297445	7999.915847	13.745280	-0.049560	4.815636
238.241623	7999.911743	13.750285	-0.049549	4.815635
238.163197	7999.936094	13.755290	-0.049535	4.815642
238.258324	7999.903476	13.760295	-0.049552	4.815632
238.485533	7999.926363	13.765299	-0.049595	4.815638
238.379062	7999.954530	13.770304	-0.049575	4.815646
238.180601	7999.969468	13.775309	-0.049538	4.815652
238.581772	7999.968484	13.780314	-0.049613	4.815650
238.347508	7999.920933	13.785319	-0.049569	4.815637
238.416772	7999.934863	13.790323	-0.049582	4.815641
238.395309	7999.941989	13.795328	-0.049578	4.815643
238.310823	7999.863771	13.800333	-0.049562	4.815620
238.470463	7999.940004	13.805338	-0.049592	4.815642
238.361757	7999.910495	13.810343	-0.049572	4.815634
238.546804	7999.935903	13.815347	-0.049606	4.815640
238.586612	7999.915200	13.820352	-0.049614	4.815634
238.395045	7999.861935	13.825357	-0.049578	4.815619
238.394775	7999.899291	13.830362	-0.049578	4.815630
238.237459	7999.888209	13.835367	-0.049549	4.815628
238.441405	7999.925665	13.840371	-0.049587	4.815638
238.334997	7999.965574	13.845376	-0.049567	4.815650
238.278037	7999.897407	13.850381	-0.049556	4.815630
238.404287	7999.977370	13.855386	-0.049580	4.815653
238.381532	7999.867060	13.860391	-0.049575	4.815621
238.584576	7999.937591	13.865395	-0.049613	4.815641
238.384219	7999.985588	13.870400	-0.049576	4.815656
238.440261	7999.914979	13.875405	-0.049586	4.815635
238.509637	7999.964135	13.880410	-0.049599	4.815649
238.185642	7999.962099	13.885415	-0.049539	4.815650
238.313669	7999.938553	13.890419	-0.049563	4.815642
238.326348	7999.884321	13.895424	-0.049565	4.815626
238.441587	7999.861635	13.900429	-0.049587	4.815619
238.449386	7999.958896	13.905434	-0.049588	4.815647
238.388332	7999.892798	13.910439	-0.049577	4.815628
238.315310	7999.997292	13.915443	-0.049563	4.815659
238.298413	7999.964997	13.920448	-0.049560	4.815650
238.303944	7999.924526	13.925453	-0.049561	4.815638
238.519345	7999.997392	13.930458	-0.049601	4.815658
238.579616	7999.961008	13.935463	-0.049613	4.815647
238.544145	7999.935885	13.940467	-0.049606	4.815640
238.525223	7999.950523	13.945472	-0.049602	4.815645
238.593604	7999.887585	13.950477	-0.049615	4.815626
238.545255	7999.903883	13.955482	-0.049606	4.815631
238.351125	7999.916756	13.960487	-0.049570	4.815636
238.494156	7999.918003	13.965491	-0.049597	4.815635
238.582289	7999.900215	13.970496	-0.049613	4.815630
238.505745	7999.888304	13.975501	-0.049599	4.815626
238.484799	7999.957348	13.980506	-0.049595	4.815647
238.468912	7999.935744	13.985511	-0.049592	4.815641
238.321228	7999.889594	13.990515	-0.049565	4.815628
238.229105	7999.905184	13.995520	-0.049547	4.815633
238.293283	7999.837909	14.000525	-0.049559	4.815613
238.438803	7999.891498	14.005530	-0.049586	4.815628
238.209029	7999.840818	14.010535	-0.049544	4.815614
238.671640	7999.935826	14.015539	-0.049630	4.815640
238.547660	7999.861238	14.020544	-0.049607	4.815618
238.417162	7999.860197	14.025549	-0.049582	4.815619
238.495054	7999.999153	14.030554	-0.049597	4.815659
238.415059	7999.902861	14.035559	-0.049582	4.815631
238.531986	7999.921831	14.040563	-0.049604	4.815636
238.521997	7999.936614	14.045568	-0.049602	4.815641
238.526477	7999.912137	14.050573	-0.049603	4.815633
238.592859	7999.940964	14.055578	-0.049615	4.815641
238.364403	7999.873227	14.060583	-0.049573	4.815623
238.500286	7999.858346	14.065587	-0.049598	4.815618
238.478707	7999.913504	14.070592	-0.049594	4.815634
238.373863	7999.865911	14.075597	-0.049575	4.815621
238.683113	7999.929620	14.080602	-0.049632	4.815638
238.787054	7999.931302	14.085607	-0.049652	4.815638
238.641567	7999.863838	14.090611	-0.049624	4.815619
238.424433	7999.899822	14.095616	-0.049584	4.815630
238.542202	7999.857963	14.100621	-0.049606	4.815617
238.451441	7999.918407	14.105626	-0.049589	4.815636
238.540323	7999.888890	14.110631	-0.049606	4.815626
238.548443	7999.909303	14.115635	-0.049607	4.815632
238.752146	7999.941418	14.120640	-0.049645	4.815641
238.703120	7999.941694	14.125645	-0.049636	4.815641
238.717753	7999.957942	14.130650	-0.049639	4.815646
238.670871	7999.959320	14.135655	-0.049630	4.815646
238.565720	7999.946947	14.140659	-0.049610	4.815643
238.655957	7999.994306	14.145664	-0.049627	4.815657
238.518259	7999.962192	14.150669	-0.049602	4.815648
238.573571	8000.010054	14.155674	-0.049612	4.815662
238.479127	7999.917798	14.160679	-0.049594	4.815635
238.619886	7999.924344	14.165683	-0.049621	4.815636
238.331582	7999.912212	14.170688	-0.049567	4.815634
238.440889	7999.877688	14.175693	-0.049587	4.815624
238.375974	7999.971639	14.180698	-0.049575	4.815651
238.455769	7999.925964	14.185703	-0.049590	4.815638
238.567375	7999.968331	14.190707	-0.049611	4.815650
238.489693	7999.982020	14.195712	-0.049596	4.815654
238.473597	7999.952940	14.200717	-0.049593	4.815646
238.620351	7999.983067	14.205722	-0.049621	4.815654
238.527954	7999.934608	14.210727	-0.049604	4.815640
238.588390	7999.925979	14.215731	-0.049615	4.815637
238.508987	7999.982337	14.220736	-0.049600	4.815654
238.442802	7999.915088	14.225741	-0.049588	4.815635
238.468872	7999.979555	14.230746	-0.049593	4.815653
238.542578	7999.989287	14.235751	-0.049606	4.815656
238.491699	7999.927623	14.240755	-0.049597	4.815638
238.399984	7999.968837	14.245760	-0.049580	4.815651
238.259201	7999.904653	14.250765	-0.049554	4.815632
238.395358	7999.946349	14.255770	-0.049579	4.815644
238.348637	7999.916775	14.260775	-0.049570	4.815636
238.385634	7999.972879	14.265779	-0.049577	4.815652
238.565992	7999.998212	14.270784	-0.049611	4.815658
238.552238	7999.965968	14.275789	-0.049608	4.815649
238.509518	7999.332314	14.280794	-0.049600	4.815464

238.531598	7995.993202	14.285799	-0.049602	4.814487
238.619558	7990.567948	14.290803	-0.049615	4.812899
238.401892	7983.921798	14.295808	-0.049570	4.810955
238.416096	7976.620098	14.300813	-0.049568	4.808816
238.463141	7969.089895	14.305818	-0.049572	4.806610
238.241638	7961.204438	14.310823	-0.049525	4.804300
238.322118	7953.395527	14.315827	-0.049535	4.802010
238.235399	7945.339958	14.320832	-0.049514	4.799646
238.200928	7937.439093	14.325837	-0.049502	4.797327
238.168249	7929.452820	14.330842	-0.049491	4.794982
238.014731	7921.425196	14.335847	-0.049457	4.792624
238.086605	7913.358046	14.340851	-0.049465	4.790252
238.157655	7905.413720	14.345856	-0.049473	4.787916
238.062842	7897.335211	14.350861	-0.049450	4.785539
238.152567	7889.407437	14.355866	-0.049462	4.783204
238.060697	7881.423869	14.360871	-0.049440	4.780853
238.117574	7873.419744	14.365875	-0.049445	4.778494
238.067206	7865.449932	14.370880	-0.049431	4.776145
238.180961	7857.385638	14.375885	-0.049446	4.773765
238.026662	7849.386483	14.380890	-0.049413	4.771405
238.063256	7841.316545	14.385895	-0.049414	4.769022
238.249429	7833.415154	14.390899	-0.049444	4.766687
238.001812	7825.356102	14.395904	-0.049392	4.764306
237.858040	7817.433281	14.400909	-0.049360	4.761964
238.051174	7809.376953	14.405914	-0.049391	4.759579
237.846407	7801.432897	14.410919	-0.049348	4.757228
237.975703	7793.359582	14.415923	-0.049367	4.754837
237.744385	7785.329516	14.420928	-0.049318	4.752458
237.663237	7777.291500	14.425933	-0.049298	4.750076
237.729434	7769.319099	14.430938	-0.049305	4.747711
237.540984	7761.294365	14.435943	-0.049265	4.745330
237.794616	7753.363400	14.440947	-0.049307	4.742974
237.629645	7745.366953	14.445952	-0.049271	4.740599
237.490552	7737.342282	14.450957	-0.049240	4.738215
237.695460	7729.350215	14.455962	-0.049273	4.735838
237.386002	7721.324718	14.460967	-0.049210	4.733451
237.635293	7713.316945	14.465971	-0.049251	4.731067
237.516663	7705.306652	14.470976	-0.049224	4.728681
237.348449	7697.308395	14.475981	-0.049187	4.726299
237.211789	7689.299860	14.480986	-0.049157	4.723912
237.138871	7681.298067	14.485991	-0.049138	4.721525
237.307763	7673.319089	14.490995	-0.049164	4.719144
237.281983	7665.367601	14.496000	-0.049154	4.716770
237.072137	7657.288075	14.501005	-0.049110	4.714357
237.180671	7649.345763	14.506010	-0.049125	4.711983
237.214102	7641.251331	14.511015	-0.049126	4.709562
237.307641	7633.319029	14.516019	-0.049138	4.707189
237.133938	7625.332493	14.521024	-0.049101	4.704799
237.188931	7617.327701	14.526029	-0.049106	4.702401
237.284219	7609.307457	14.531034	-0.049118	4.699998
237.123250	7601.342714	14.536039	-0.049083	4.697611
237.210990	7593.285847	14.541043	-0.049094	4.695194
237.171609	7585.320730	14.546048	-0.049082	4.692804
236.959669	7577.263031	14.551053	-0.049037	4.690385
237.130673	7569.316719	14.556058	-0.049064	4.687997
236.871919	7561.273356	14.561063	-0.049010	4.685580
236.835072	7553.302907	14.566067	-0.048998	4.683184
236.762971	7545.307331	14.571072	-0.048979	4.680778
236.815369	7537.265715	14.576077	-0.048984	4.678357
236.915595	7529.346620	14.581082	-0.048998	4.675972
236.754664	7521.251144	14.586087	-0.048962	4.673533
236.572394	7513.129851	14.591091	-0.048923	4.671085
236.651030	7505.181611	14.596096	-0.048933	4.668687
236.517918	7497.199355	14.601101	-0.048903	4.666278
236.656399	7489.286401	14.606106	-0.048923	4.663888
236.600393	7481.250715	14.611111	-0.048908	4.661461
236.580787	7473.212142	14.616115	-0.048899	4.659031
236.526538	7465.288093	14.621120	-0.048883	4.656634
236.469473	7457.195886	14.626125	-0.048868	4.654186
236.465368	7449.219460	14.631130	-0.048862	4.651771
236.404615	7441.177999	14.636135	-0.048845	4.649335
236.267384	7433.242553	14.641139	-0.048814	4.646930
236.460367	7425.214237	14.646144	-0.048845	4.644496
236.369801	7417.217255	14.651149	-0.048823	4.642070
236.321945	7409.241029	14.656154	-0.048809	4.639649
236.289435	7401.258743	14.661159	-0.048798	4.637224
236.359533	7393.227391	14.666163	-0.048805	4.634784
236.347026	7385.211437	14.671168	-0.048798	4.632347
236.205484	7377.138008	14.676173	-0.048766	4.629891
236.364834	7369.235336	14.681178	-0.048791	4.627486
236.152401	7361.131454	14.686183	-0.048746	4.625018
236.356124	7353.208410	14.691187	-0.048779	4.622604
236.308275	7345.200270	14.696192	-0.048765	4.620163
235.871111	7337.223968	14.701197	-0.048678	4.617731
236.109492	7329.219277	14.706202	-0.048717	4.615288
236.155409	7321.195276	14.711207	-0.048721	4.612838
236.097350	7313.132662	14.716211	-0.048705	4.610375
236.022006	7305.232684	14.721216	-0.048685	4.607961
236.110035	7297.175483	14.726221	-0.048697	4.605497
236.144636	7289.196072	14.731226	-0.048698	4.603055
235.827535	7281.138733	14.736231	-0.048634	4.600589
235.862882	7273.200497	14.741235	-0.048635	4.598157
235.964017	7265.194038	14.746240	-0.048649	4.595704
235.868015	7257.110744	14.751245	-0.048625	4.593225
235.697484	7249.123572	14.756250	-0.048588	4.590775
235.617960	7241.145624	14.761255	-0.048568	4.588326
235.688832	7233.102509	14.766259	-0.048576	4.585855
235.720070	7225.148116	14.771264	-0.048577	4.583411
235.596583	7217.133420	14.776269	-0.048549	4.580947
235.599160	7209.149099	14.781274	-0.048544	4.578491
235.545207	7201.140853	14.786279	-0.048529	4.576026
235.713186	7193.160534	14.791283	-0.048555	4.573569
235.687010	7185.120302	14.796288	-0.048545	4.571092
235.508303	7177.096155	14.801293	-0.048506	4.568618
235.330720	7169.140177	14.806298	-0.048468	4.566163
235.384797	7161.112759	14.811303	-0.048473	4.563686
235.385166	7153.160674	14.816307	-0.048468	4.561231
235.135788	7145.155412	14.821312	-0.048416	4.558757
235.115395	7137.154532	14.826317	-0.048407	4.556284
235.221093	7129.139231	14.831322	-0.048422	4.553805
235.278144	7121.062950	14.836327	-0.048427	4.551306
235.139778	7113.099985	14.841331	-0.048396	4.548840
235.143182	7105.111406	14.846336	-0.048392	4.546365
235.055107	7097.106557	14.851341	-0.048370	4.543884
235.261906	7089.172828	14.856346	-0.048403	4.541424
235.127774	7081.085462	14.861351	-0.048373	4.538914
235.152620	7073.183593	14.866355	-0.048373	4.536461
235.188681	7065.131194	14.871360	-0.048374	4.533959
235.164137	7057.088657	14.876365	-0.048364	4.531460
235.194202	7049.110421	14.881370	-0.048365	4.528979
234.995522	7041.119101	14.886375	-0.048322	4.526492
234.809947	7033.081037	14.891379	-0.048283	4.523989
234.806378	7025.131319	14.896384	-0.048277	4.521512
234.619247	7017.126276	14.901389	-0.048237	4.519017
234.644072	7009.185135	14.906394	-0.048236	4.516540
234.716085	7001.070918	14.911399	-0.048244	4.514009
234.676761	6993.007132	14.916403	-0.048232	4.511491
234.744711	6985.042894	14.921408	-0.048239	4.509004
234.635435	6977.054593	14.926413	-0.048214	4.506507
234.739688	6969.047938	14.931418	-0.048228	4.504003
234.621098	6961.123512	14.936423	-0.048201	4.501523
234.646030	6953.069596	14.941427	-0.048200	4.499002
234.789677	6945.117728	14.946432	-0.048222	4.496512
234.551178	6937.058346	14.951437	-0.048172	4.493985
234.466884	6929.080724	14.956442	-0.048151	4.491483
234.524646	6921.048484	14.961447	-0.048157	4.488963
234.424063	6913.083981	14.966451	-0.048133	4.486462
234.368706	6905.049973	14.971456	-0.048117	4.483938
234.311855	6897.076145	14.976461	-0.048102	4.481432
234.724756	6889.082922	14.981466	-0.048173	4.478920
234.442080	6881.092683	14.986471	-0.048115	4.476405
234.034112	6873.031118	14.991475	-0.048034	4.473865
234.276273	6865.024426	14.996480	-0.048074	4.471344
234.228567	6856.974990	15.001485	-0.048060	4.468807
234.205494	6849.043678	15.006490	-0.048050	4.466305
233.963225	6841.028429	15.011495	-0.048000	4.463775
234.238494	6833.046184	15.016499	-0.048046	4.461256
234.200858	6825.084039	15.021504	-0.048034	4.458741
233.928699	6817.015774	15.026509	-0.047978	4.456189
234.131269	6809.047891	15.031514	-0.048011	4.453670
234.008675	6800.994919	15.036519	-0.047983	4.451121
233.969958	6793.027340	15.041523	-0.047970	4.448599
234.058835	6785.012372	15.046528	-0.047982	4.446060
234.045334	6777.003330	15.051533	-0.047974	4.443521
233.994194	6769.044657	15.056538	-0.047959	4.440996
233.823963	6761.039072	15.061543	-0.047922	4.438455
233.907008	6753.028706	15.066547	-0.047932	4.435912
233.789295	6745.003163	15.071552	-0.047905	4.433362
233.644080	6736.923782	15.076557	-0.047873	4.430792
233.737416	6728.982064	15.081562	-0.047885	4.428267
233.545940	6720.968642	15.086567	-0.047844	4.425715
233.672446	6712.973787	15.091571	-0.047863	4.423170
233.519980	6704.974987	15.096576	-0.047829	4.420621
233.485150	6697.004517	15.101581	-0.047817	4.418079
233.603584	6689.040186	15.106586	-0.047834	4.415539
233.417237	6680.983502	15.111591	-0.047794	4.412967
233.426294	6672.966598	15.116595	-0.047791	4.410406
233.345736	6664.999749	15.121600	-0.047771	4.407860
233.183876	6656.990065	15.126605	-0.047735	4.405298
233.228635	6649.049989	15.131610	-0.047739	4.402758
233.284504	6640.967078	15.136615	-0.047744	4.400171
233.229972	6633.019394	15.141619	-0.047728	4.397625
233.357658	6624.971948	15.146624	-0.047747	4.395046
233.492916	6616.991340	15.151629	-0.047767	4.392488
233.270067	6609.004088	15.156634	-0.047720	4.389924
232.956743	6600.975564	15.161639	-0.047657	4.387344
232.956850	6592.956009	15.166643	-0.047651	4.384768
233.120962	6584.987733	15.171648	-0.047677	4.382208
232.869758	6576.957888	15.176653	-0.047625	4.379624
233.111199	6569.059578	15.181658	-0.047665	4.377083
233.162939	6560.951216	15.186663	-0.047669	4.374473
233.187187	6553.003190	15.191667	-0.047668	4.371912
233.218076	6544.976434	15.196672	-0.047669	4.369325
233.159945	6536.993874	15.201677	-0.047653	4.366749
232.987962	6529.017298	15.206682	-0.047616	4.364174
232.781050	6521.050057	15.211687	-0.047572	4.361599
232.985206	6513.010898	15.216691	-0.047605	4.359003
232.810659	6505.033255	15.221696	-0.047567	4.356422
232.722731	6496.956413	15.226701	-0.047545	4.353808
232.829126	6488.898821	15.231706	-0.047560	4.351200
232.672834	6480.922731	15.236711	-0.047526	4.348616
232.466459	6472.929383	15.241715	-0.047482	4.346024
232.440877	6464.981373	15.246720	-0.047472	4.343446
232.524278	6456.974239	15.251725	-0.047482	4.340848
232.531139	6448.986003	15.256730	-0.047479	4.338254
232.363214	6440.972693	15.261735	-0.047442	4.335649
232.546309	6432.977764	15.266739	-0.047471	4.333052
232.489870	6424.961156	15.271744	-0.047455	4.330443
232.429146	6416.948544	15.276749	-0.047439	4.327835
232.499419	6408.986745	15.281754	-0.047447	4.325243
232.429328	6400.978268	15.286759	-0.047428	4.322632
232.492436	6392.938140	15.291763	-0.047435	4.320011
232.182895	6385.026196	15.296768	-0.047372	4.317427
232.469304	6376.907468	15.301773	-0.047420	4.314779
232.576259	6368.921999	15.306778	-0.047435	4.312171
232.305849	6360.945412	15.311783	-0.047379	4.309562
232.269968	6352.931004	15.316787	-0.047367	4.306940
232.271092	6344.897727	15.321792	-0.047362	4.304311
232.149059	6336.931420	15.326797	-0.047335	4.301701
232.162320	6328.956246	15.331802	-0.047332	4.299088
232.203930	6320.957624	15.336807	-0.047334	4.296466
232.269415	6312.919526	15.341811	-0.047341	4.293830
232.165951	6304.932376	15.346816	-0.047317	4.291207
232.029770	6296.913921	15.351821	-0.047286	4.288572
232.109175	6288.940599	15.356826	-0.047296	4.285952
231.886281	6280.936157	15.361831	-0.047249	4.283317
231.874623	6272.924689	15.366835	-0.047242	4.280681
231.975909	6264.972125	15.371840	-0.047256	4.278063
231.721171	6256.934190	15.376845	-0.047203	4.275413
231.695635	6248.965400	15.381850	-0.047193	4.272785
231.682239	6240.851731	15.386855	-0.047185	4.270108
231.726923	6232.873040	15.391859	-0.047188	4.267475
231.780930	6224.850825	15.396864	-0.047193	4.264826
231.831880	6216.915817	15.401869	-0.047197	4.262203
231.643277	6208.942168	15.406874	-0.047157	4.259565
231.272404	6200.933260	15.411879	-0.047083	4.256911
231.374987	6192.894783	15.416883	-0.047097	4.254250
231.371807	6184.938650	15.421888	-0.047091	4.251614
231.219568	6176.874896	15.426893	-0.047057	4.248939
231.089877	6168.940775	15.431898	-0.047028	4.246306
231.331579	6160.908042	15.436903	-0.047068	4.243641
231.441688	6152.927237	15.441907	-0.047083	4.240991
231.225303	6144.956999	15.446912	-0.047038	4.238340
231.117805	6136.947408	15.451917	-0.047012	4.235675
231.358690	6128.945902	15.456922	-0.047052	4.233015
231.216506	6120.898700	15.461927	-0.047020	4.230333
231.265908	6112.926883	15.466931	-0.047024	4.227677
231.218319	6104.911459	15.471936	-0.047010	4.225004
230.992631	6096.927034	15.476941	-0.046963	4.222338
231.015380	6088.965524	15.481946	-0.046962	4.219680
230.927044	6080.989967	15.486951	-0.046941	4.217015
230.896933	6072.966372	15.491955	-0.046930	4.214333
231.022719	6064.915138	15.496960	-0.046948	4.211641
230.962690	6056.943738	15.501965	-0.046932	4.208972
230.984658	6048.943199	15.506970	-0.046930	4.206293
230.933661	6040.950965	15.511975	-0.046916	4.203614
231.118232	6032.968554	15.516979	-0.046945	4.200939
231.042969	6024.955657	15.521984	-0.046926	4.198249
230.903318	6016.948123	15.526989	-0.046895	4.195559
230.855745	6008.868532	15.531994	-0.046880	4.192844
230.882006	6000.854021	15.536999	-0.046880	4.190150
230.919208	5992.849873	15.542003	-0.046882	4.187457
230.790473	5984.867396	15.547008	-0.046853	4.184769
230.654438	5976.942232	15.552013	-0.046822	4.182097
230.680047	5968.934462	15.557018	-0.046822	4.179398
230.583688	5960.960888	15.562023	-0.046799	4.176708
230.412113	5952.927505	15.567027	-0.046761	4.173995
230.406858	5944.860577	15.572032	-0.046755	4.171270
230.294143	5936.889363	15.577037	-0.046729	4.168575
230.529072	5928.897719	15.582042	-0.046768	4.165875
230.321670	5920.905970	15.587047	-0.046724	4.163168
230.348433	5912.942814	15.592051	-0.046724	4.160472
230.403545	5904.948836	15.597056	-0.046729	4.157764
230.329294	5896.878936	15.602061	-0.046710	4.155027
230.519303	5888.862201	15.607066	-0.046740	4.152309
230.485208	5880.898957	15.612071	-0.046728	4.149605
230.303613	5872.861612	15.617075	-0.046689	4.146873
230.373786	5864.913439	15.622080	-0.046697	4.144171
230.107355	5856.922798	15.627085	-0.046642	4.141450
230.133135	5848.926130	15.632090	-0.046642	4.138728
229.993498	5840.892122	15.637095	-0.046611	4.135990
230.138433	5832.909038	15.642099	-0.046632	4.133271
229.960427	5824.909069	15.647104	-0.046594	4.130540
229.962432	5816.878614	15.652109	-0.046589	4.127799
229.961725	5808.874618	15.657114	-0.046584	4.125065
229.922235	5800.925770	15.662119	-0.046571	4.122348
229.997545	5792.902168	15.667123	-0.046580	4.119605
229.992762	5784.969875	15.672128	-0.046574	4.116891
229.788382	5776.915443	15.677133	-0.046531	4.114130
229.820114	5768.894926	15.682138	-0.046532	4.111382
229.893608	5760.836312	15.687143	-0.046540	4.108620
229.859708	5752.847226	15.692147	-0.046528	4.105878
229.864408	5744.877468	15.697152	-0.046524	4.103141
229.706915	5736.900213	15.702157	-0.046490	4.100398
229.709542	5728.946671	15.707162	-0.046485	4.097664
229.639710	5720.924161	15.712167	-0.046467	4.094903
229.296120	5712.942293	15.717171	-0.046398	4.092150
229.623725	5704.902395	15.722176	-0.046453	4.089385
229.572947	5696.922600	15.727181	-0.046439	4.086633
229.569706	5688.946320	15.732186	-0.046433	4.083881
229.298692	5680.962610	15.737191	-0.046377	4.081121
229.385009	5672.952919	15.742195	-0.046388	4.078355
229.541559	5664.974693	15.747200	-0.046412	4.075600
229.439858	5656.925653	15.752205	-0.046388	4.072814
229.513486	5648.911098	15.757210	-0.046396	4.070041
229.471366	5640.920230	15.762215	-0.046383	4.067272
229.436324	5632.912929	15.767219	-0.046372	4.064496
229.191043	5625.009773	15.772224	-0.046321	4.061751
229.292492	5616.935845	15.777229	-0.046334	4.058950
229.123636	5608.986539	15.782234	-0.046298	4.056186
229.047051	5600.947280	15.787239	-0.046278	4.053391
229.017358	5592.916121	15.792243	-0.046268	4.050597
229.061997	5584.920558	15.797248	-0.046271	4.047815
228.826481	5576.914595	15.802253	-0.046222	4.045023
229.015205	5568.995568	15.807258	-0.046252	4.042265
228.997208	5560.938611	15.812263	-0.046243	4.039455
228.964728	5552.985364	15.817267	-0.046232	4.036679
228.797543	5544.903143	15.822272	-0.046195	4.033853
228.736154	5536.780995	15.827277	-0.046179	4.031013
229.083348	5528.877893	15.832282	-0.046238	4.028255
228.841014	5520.873916	15.837287	-0.046188	4.025449
228.683982	5512.914646	15.842291	-0.046153	4.022659
228.750704	5504.927043	15.847296	-0.046161	4.019861
228.438366	5496.938667	15.852301	-0.046097	4.017054
228.498787	5488.947401	15.857306	-0.046103	4.014250
228.498361	5480.885342	15.862311	-0.046098	4.011419
228.355289	5472.882457	15.867315	-0.046066	4.008603
228.299363	5464.921255	15.872320	-0.046051	4.005802
228.304057	5456.915908	15.877325	-0.046046	4.002985
228.329584	5448.939178	15.882330	-0.046046	4.000176
228.562610	5440.937309	15.887335	-0.046084	3.997359
228.367976	5432.927891	15.892339	-0.046043	3.994531
228.352683	5424.907121	15.897344	-0.046035	3.991699
228.308525	5416.899578	15.902349	-0.046021	3.988870
228.177237	5408.935344	15.907354	-0.045992	3.986053
228.272294	5400.936236	15.912359	-0.046004	3.983225
228.033790	5392.938138	15.917363	-0.045954	3.980390
227.941100	5384.971578	15.922368	-0.045932	3.977566
227.988214	5376.927516	15.927373	-0.045936	3.974716
228.087106	5368.955377	15.932378	-0.045949	3.971889
227.929657	5360.928127	15.937383	-0.045914	3.969037
227.865698	5352.941779	15.942387	-0.045897	3.966199
227.947017	5344.945423	15.947392	-0.045907	3.963357
227.845259	5336.957465	15.952397	-0.045883	3.960514
228.001064	5328.989994	15.957402	-0.045907	3.957680
227.888000	5320.968538	15.962407	-0.045880	3.954820
227.874638	5312.920061	15.967411	-0.045873	3.951951
227.935002	5304.952553	15.972416	-0.045879	3.949109
227.959559	5296.961056	15.977421	-0.045878	3.946256
228.040299	5288.965572	15.982426	-0.045888	3.943401
227.648599	5280.994046	15.987431	-0.045810	3.940543
227.533658	5273.022544	15.992435	-0.045783	3.937689
227.523220	5265.014178	15.997440	-0.045776	3.934821
227.483814	5256.973925	16.002445	-0.045764	3.931939
227.484278	5249.001982	16.007450	-0.045758	3.929080
227.549644	5240.997780	16.012455	-0.045765	3.926209
227.580712	5232.987251	16.017459	-0.045766	3.923333
227.437449	5225.046178	16.022464	-0.045734	3.920476
227.213403	5217.026585	16.027469	-0.045687	3.917588
227.516682	5209.020620	16.032474	-0.045739	3.914712
227.468887	5200.974391	16.037479	-0.045724	3.911813
227.155322	5192.969547	16.042483	-0.045661	3.908921
227.434060	5184.984136	16.047488	-0.045708	3.906046
227.282809	5176.997508	16.052493	-0.045674	3.903160
227.470771	5169.018985	16.057498	-0.045704	3.900281
227.252937	5161.020968	16.062503	-0.045658	3.897385
227.309759	5152.987782	16.067507	-0.045664	3.894480
227.122785	5145.005359	16.072512	-0.045624	3.891586
227.018204	5136.978077	16.077517	-0.045599	3.888676
227.373524	5128.983996	16.082522	-0.045660	3.885784
227.426756	5121.025632	16.087527	-0.045665	3.882897
227.192824	5113.016393	16.092531	-0.045616	3.879984
227.020962	5105.064891	16.097536	-0.045579	3.877091
226.948327	5096.975034	16.102541	-0.045560	3.874147
226.936862	5088.788587	16.107546	-0.045552	3.871167
226.999179	5080.846900	16.112551	-0.045559	3.868275
226.929241	5072.899522	16.117555	-0.045541	3.865377
226.811118	5064.991579	16.122560	-0.045513	3.862490
226.621805	5056.966154	16.127565	-0.045473	3.859556
226.943587	5048.995579	16.132570	-0.045528	3.856650
226.752883	5040.955993	16.137575	-0.045487	3.853707
226.640886	5032.959201	16.142579	-0.045461	3.850778
226.823181	5024.998150	16.147584	-0.045490	3.847867
226.669836	5016.988606	16.152589	-0.045456	3.844928
226.798754	5009.068110	16.157594	-0.045475	3.842026
226.684888	5001.043943	16.162599	-0.045448	3.839079
226.491685	4993.112046	16.167603	-0.045407	3.836161
226.361215	4985.056215	16.172608	-0.045378	3.833197
226.505889	4977.013065	16.177613	-0.045399	3.830241
226.473185	4969.041303	16.182618	-0.045388	3.827306
226.399698	4961.007713	16.187623	-0.045369	3.824344
226.284470	4953.118202	16.192627	-0.045343	3.821432
226.459044	4945.080184	16.197632	-0.045370	3.818470
226.185717	4937.091174	16.202637	-0.045314	3.815514
226.383793	4929.067579	16.207642	-0.045346	3.812553
226.099755	4921.062215	16.212647	-0.045287	3.809585
226.192750	4913.075729	16.217651	-0.045300	3.806631
226.276596	4905.113638	16.222656	-0.045310	3.803683
226.067557	4897.125270	16.227661	-0.045266	3.800717
226.125503	4889.137557	16.232666	-0.045271	3.797755
226.189329	4881.101922	16.237671	-0.045278	3.794772
225.964655	4873.067062	16.242675	-0.045231	3.791781
226.019368	4865.082396	16.247680	-0.045236	3.788813
226.099050	4857.074808	16.252685	-0.045246	3.785834
226.016956	4849.097448	16.257690	-0.045225	3.782861
225.942914	4841.102479	16.262695	-0.045206	3.779879
225.794970	4833.106612	16.267699	-0.045173	3.776892
225.728600	4825.120553	16.272704	-0.045156	3.773909
225.556169	4817.099692	16.277709	-0.045119	3.770908
225.781132	4809.111123	16.282714	-0.045155	3.767925
225.772082	4801.103086	16.287719	-0.045148	3.764928
225.685690	4793.118682	16.292723	-0.045127	3.761935
225.864105	4785.143515	16.297728	-0.045155	3.758949
225.819205	4777.101068	16.302733	-0.045142	3.755931
225.515476	4769.130189	16.307738	-0.045080	3.752931
225.327180	4761.128750	16.312743	-0.045040	3.749920
225.523338	4753.084128	16.317747	-0.045071	3.746899
225.596537	4745.117449	16.322752	-0.045079	3.743902
225.266583	4737.139339	16.327757	-0.045013	3.740889
225.375266	4729.154273	16.332762	-0.045028	3.737881
225.383090	4721.145566	16.337767	-0.045024	3.734860
225.044755	4713.166916	16.342771	-0.044956	3.731839
225.308035	4705.136849	16.347776	-0.045000	3.728811
225.271910	4697.147123	16.352781	-0.044988	3.725788
225.309773	4689.223483	16.357786	-0.044990	3.722790
225.155600	4681.173539	16.362791	-0.044956	3.719736
225.083906	4673.226218	16.367795	-0.044937	3.716721
225.134250	4665.202672	16.372800	-0.044941	3.713678
225.084228	4657.059057	16.377805	-0.044927	3.710584
225.028637	4649.129530	16.382810	-0.044911	3.707569
225.076327	4641.115264	16.387815	-0.044915	3.704522
224.977487	4633.176980	16.392819	-0.044891	3.701497
224.839786	4625.203548	16.397824	-0.044860	3.698456
224.684604	4617.217430	16.402829	-0.044826	3.695406
224.676495	4609.232384	16.407834	-0.044820	3.692359
224.696173	4601.197366	16.412839	-0.044818	3.689290
224.751861	4593.218891	16.417843	-0.044823	3.686241
225.129070	4585.220750	16.422848	-0.044888	3.683191
224.702046	4577.251674	16.427853	-0.044804	3.680128
224.661862	4569.283943	16.432858	-0.044791	3.677074
224.777028	4561.257935	16.437863	-0.044807	3.673998
224.735372	4553.201990	16.442867	-0.044794	3.670905
224.641591	4545.262777	16.447872	-0.044772	3.667852
224.580961	4537.193261	16.452877	-0.044755	3.664748
224.788081	4529.280322	16.457882	-0.044788	3.661708
224.468620	4521.275973	16.462887	-0.044724	3.658616
224.538152	4513.271452	16.467891	-0.044731	3.655532
224.599297	4505.253206	16.472896	-0.044738	3.652440
224.432714	4497.200767	16.477901	-0.044701	3.649326
224.462021	4489.274239	16.482906	-0.044702	3.646264
224.332763	4481.253958	16.487911	-0.044672	3.643158
224.267467	4473.282912	16.492915	-0.044655	3.640070
224.430596	4465.333436	16.497920	-0.044680	3.636995
224.295305	4457.270536	16.502925	-0.044650	3.633864
224.363695	4449.270402	16.507930	-0.044657	3.630761
224.189815	4441.281968	16.512935	-0.044620	3.627653
223.975375	4433.257556	16.517939	-0.044575	3.624527
224.134112	4425.320597	16.522944	-0.044599	3.621443
223.898617	4417.301136	16.527949	-0.044550	3.618313
223.947791	4409.327048	16.532954	-0.044554	3.615206
223.899292	4401.309930	16.537959	-0.044540	3.612077
223.934574	4393.277850	16.542963	-0.044541	3.608941
223.833911	4385.343871	16.547968	-0.044517	3.605838
223.908201	4377.350024	16.552973	-0.044526	3.602713
224.079110	4369.341020	16.557978	-0.044552	3.599582
223.824743	4361.414058	16.562983	-0.044500	3.596469
223.634056	4353.384459	16.567987	-0.044459	3.593315
223.861376	4345.373952	16.572992	-0.044496	3.590177
223.784910	4337.360576	16.577997	-0.044477	3.587026
223.705240	4329.394194	16.583002	-0.044457	3.583891
223.701546	4321.412641	16.588007	-0.044451	3.580750
223.881689	4313.415175	16.593011	-0.044479	3.577605
223.692530	4305.450901	16.598016	-0.044439	3.574460
223.597007	4297.403030	16.603021	-0.044416	3.571281
223.826724	4289.411137	16.608026	-0.044453	3.568131
223.548484	4281.403674	16.613031	-0.044396	3.564958
223.629611	4273.447092	16.618035	-0.044406	3.561812
223.664661	4265.459159	16.623040	-0.044408	3.558650
223.421393	4257.467514	16.628045	-0.044357	3.555475
223.311738	4249.363041	16.633050	-0.044332	3.552256
223.330878	4241.354578	16.638055	-0.044330	3.549077
223.139176	4233.398138	16.643059	-0.044289	3.545909
223.148463	4225.435372	16.648064	-0.044286	3.542742
223.128856	4217.412148	16.653069	-0.044277	3.539547
223.259200	4209.458469	16.658074	-0.044296	3.536381
223.194668	4201.448374	16.663079	-0.044279	3.533184
223.093239	4193.441328	16.668083	-0.044254	3.529984
223.162736	4185.491847	16.673088	-0.044262	3.526810
223.216515	4177.452385	16.678093	-0.044267	3.523596
223.090445	4169.501810	16.683098	-0.044238	3.520410
223.104164	4161.537656	16.688103	-0.044236	3.517219
222.908427	4153.543913	16.693107	-0.044194	3.514007
223.002378	4145.494054	16.698112	-0.044206	3.510778
223.032419	4137.477467	16.703117	-0.044207	3.507558
223.001505	4129.488473	16.708122	-0.044196	3.504345
222.880703	4121.567297	16.713127	-0.044168	3.501152
222.748859	4113.559771	16.718131	-0.044138	3.497922
222.906699	4105.557229	16.723136	-0.044163	3.494700
222.631746	4097.568788	16.728141	-0.044106	3.491467
222.621007	4089.564075	16.733146	-0.044099	3.488232
222.689380	4081.561350	16.738151	-0.044106	3.484998
222.586290	4073.639670	16.743155	-0.044082	3.481789
222.568902	4065.618449	16.748160	-0.044074	3.478538
222.486092	4057.613765	16.753165	-0.044053	3.475289
222.663642	4049.593640	16.758170	-0.044081	3.472040
222.608053	4041.581061	16.763175	-0.044065	3.468783
222.518810	4033.587931	16.768179	-0.044044	3.465529
222.280166	4025.644962	16.773184	-0.043994	3.462288
222.255308	4017.617355	16.778189	-0.043984	3.459017
222.304170	4009.635052	16.783194	-0.043988	3.455763
222.147731	4001.648496	16.788199	-0.043954	3.452498
222.194103	3993.592106	16.793203	-0.043957	3.449207
222.180084	3985.641357	16.798208	-0.043949	3.445955
222.131667	3977.652893	16.803213	-0.043935	3.442683
222.165521	3969.662315	16.808218	-0.043936	3.439410
221.938916	3961.730230	16.813223	-0.043889	3.436149
221.837082	3953.681580	16.818227	-0.043865	3.432841
222.071308	3945.673972	16.823232	-0.043903	3.429559
222.235245	3937.666041	16.828237	-0.043928	3.426270
222.014154	3929.692852	16.833242	-0.043882	3.422980
221.809502	3921.723810	16.838247	-0.043839	3.419689
221.767102	3913.752913	16.843251	-0.043826	3.416399
221.864269	3905.764553	16.848256	-0.043839	3.413104
221.725240	3897.699294	16.853261	-0.043807	3.409765
221.780766	3889.751767	16.858266	-0.043813	3.406479
221.807734	3881.760018	16.863271	-0.043812	3.403171
221.715815	3873.775436	16.868275	-0.043790	3.399857
221.587244	3865.843117	16.873280	-0.043761	3.396562
221.721593	3857.718421	16.878285	-0.043781	3.393192
221.587948	3849.701606	16.883290	-0.043751	3.389854
221.569916	3841.751981	16.888295	-0.043742	3.386545
221.679115	3833.746943	16.893299	-0.043757	3.383214
221.500511	3825.820536	16.898304	-0.043719	3.379903
221.225966	3817.850329	16.903309	-0.043663	3.376566
221.545378	3809.823363	16.908314	-0.043717	3.373224
221.307860	3801.842789	16.913319	-0.043667	3.369878
221.068192	3793.848081	16.918323	-0.043618	3.366522
221.171398	3785.863338	16.923328	-0.043632	3.363180
221.313176	3777.861601	16.928333	-0.043653	3.359828
221.185280	3769.923710	16.933338	-0.043624	3.356490
221.303564	3761.882699	16.938343	-0.043641	3.353115
221.166961	3753.835444	16.943347	-0.043610	3.349724
221.359894	3745.881192	16.948352	-0.043641	3.346381
221.097390	3737.891480	16.953357	-0.043587	3.343003
221.043283	3729.904392	16.958362	-0.043571	3.339630
221.061275	3721.932407	16.963367	-0.043569	3.336263
220.862319	3713.915128	16.968371	-0.043527	3.332866
220.904690	3705.901183	16.973376	-0.043530	3.329475
220.935617	3697.931003	16.978381	-0.043530	3.326099
221.073886	3689.958718	16.983386	-0.043551	3.322722
220.837382	3681.980513	16.988391	-0.043502	3.319326
220.801480	3674.024419	16.993395	-0.043490	3.315943
220.877549	3666.015936	16.998400	-0.043499	3.312538
220.743539	3657.953726	17.003405	-0.043469	3.309099
220.553065	3649.983301	17.008410	-0.043428	3.305694
220.668023	3642.009290	17.013415	-0.043444	3.302295
220.499177	3634.034484	17.018419	-0.043408	3.298881
220.509327	3626.072409	17.023424	-0.043404	3.295476
220.493186	3618.046580	17.028429	-0.043396	3.292040
220.546272	3610.062958	17.033434	-0.043401	3.288620
220.447887	3602.069277	17.038439	-0.043377	3.285187
220.260866	3594.115263	17.043443	-0.043337	3.281764
220.389735	3586.133776	17.048448	-0.043356	3.278337
220.444424	3578.118730	17.053453	-0.043361	3.274890
220.402389	3570.125968	17.058458	-0.043348	3.271445
220.415189	3562.125076	17.063463	-0.043345	3.267995
220.141543	3554.107479	17.068467	-0.043289	3.264522
220.101836	3546.190486	17.073472	-0.043277	3.261099
220.169058	3538.157348	17.078477	-0.043284	3.257626
220.262716	3530.146168	17.083482	-0.043296	3.254160
220.079293	3522.174761	17.088487	-0.043257	3.250697
220.090559	3514.163059	17.093491	-0.043254	3.247220
219.983293	3506.206806	17.098496	-0.043228	3.243758
219.883720	3498.238303	17.103501	-0.043205	3.240288
220.021285	3490.264961	17.108506	-0.043225	3.236822
219.910141	3482.226610	17.113511	-0.043199	3.233313
219.816666	3474.177518	17.118515	-0.043177	3.229797
219.785653	3466.224257	17.123520	-0.043166	3.226321
219.695454	3458.227335	17.128525	-0.043144	3.222820
219.817570	3450.244170	17.133530	-0.043161	3.219330
219.798659	3442.276461	17.138535	-0.043153	3.215837
219.584282	3434.278949	17.143539	-0.043107	3.212319
219.734277	3426.272237	17.148544	-0.043130	3.208809
219.510587	3418.308157	17.153549	-0.043083	3.205297
219.302896	3410.361324	17.158554	-0.043039	3.201790
219.550075	3402.358137	17.163559	-0.043080	3.198274
219.451464	3394.361899	17.168563	-0.043057	3.194742
219.209700	3386.404459	17.173568	-0.043007	3.191217
219.180034	3378.365797	17.178573	-0.042996	3.187662
219.567907	3370.344768	17.183578	-0.043063	3.184127
219.396751	3362.416385	17.188583	-0.043026	3.180607
219.198130	3354.419329	17.193587	-0.042984	3.177050
219.254681	3346.429925	17.198592	-0.042989	3.173504
219.125920	3338.406265	17.203597	-0.042960	3.169931
219.089557	3330.450773	17.208602	-0.042948	3.166388
219.093428	3322.478600	17.213607	-0.042943	3.162836
219.036822	3314.486990	17.218611	-0.042928	3.159268
218.992643	3306.552829	17.223616	-0.042914	3.155722
218.681206	3298.531556	17.228621	-0.042851	3.152122
219.157633	3290.476080	17.233626	-0.042934	3.148537
218.941664	3282.502903	17.238631	-0.042889	3.144954
218.976072	3274.526183	17.243635	-0.042890	3.141377
218.852460	3266.576845	17.248640	-0.042862	3.137800
218.709114	3258.562257	17.253645	-0.042830	3.134190
218.722794	3250.583067	17.258650	-0.042828	3.130598
218.766824	3242.578186	17.263655	-0.042831	3.126992
218.801237	3234.600068	17.268659	-0.042832	3.123393
218.953501	3226.611146	17.273664	-0.042855	3.119790
218.597979	3218.670147	17.278669	-0.042784	3.116183
218.838265	3210.656422	17.283674	-0.042823	3.112565
218.783742	3202.631088	17.288679	-0.042808	3.108924
218.557154	3194.660580	17.293683	-0.042760	3.105296
218.722287	3186.692518	17.298688	-0.042786	3.101682
218.530813	3178.726947	17.303693	-0.042745	3.098049
218.620974	3170.741799	17.308698	-0.042757	3.094416
218.342966	3162.742887	17.313703	-0.042700	3.090756
218.541333	3154.725988	17.318707	-0.042731	3.087105
218.529240	3146.767755	17.323712	-0.042724	3.083466
218.290850	3138.781869	17.328717	-0.042674	3.079800
218.230751	3130.845387	17.333722	-0.042658	3.076161
218.396015	3122.776372	17.338727	-0.042684	3.072467
218.124413	3114.747254	17.343731	-0.042628	3.068767
218.220784	3106.788078	17.348736	-0.042641	3.065111
218.181642	3098.818334	17.353741	-0.042628	3.061440
218.237480	3090.856556	17.358746	-0.042633	3.057772
218.039333	3082.877661	17.363751	-0.042591	3.054081
217.932287	3074.858627	17.368755	-0.042566	3.050370
218.077790	3066.900250	17.373760	-0.042588	3.046695
217.805920	3058.929180	17.378765	-0.042532	3.042990
218.059760	3050.927678	17.383770	-0.042574	3.039291
218.114779	3042.967828	17.388775	-0.042579	3.035598
217.903860	3034.962715	17.393779	-0.042535	3.031866
217.739298	3027.002962	17.398784	-0.042499	3.028153
217.853390	3018.965759	17.403789	-0.042515	3.024413
217.703369	3011.028215	17.408794	-0.042482	3.020702
217.654551	3003.045836	17.413799	-0.042468	3.016970
217.689857	2995.055870	17.418803	-0.042469	3.013235
217.604777	2987.067124	17.423808	-0.042448	3.009489
217.433830	2979.082768	17.428813	-0.042411	3.005736
217.491587	2971.118916	17.433818	-0.042417	3.002000
217.619252	2963.122393	17.438823	-0.042435	2.998247
217.481115	2955.142732	17.443827	-0.042404	2.994484
217.451184	2947.138533	17.448832	-0.042393	2.990710
217.340807	2939.143080	17.453837	-0.042368	2.986931
217.459725	2931.160483	17.458842	-0.042385	2.983166
217.392000	2923.183396	17.463847	-0.042367	2.979388
217.353552	2915.221240	17.468851	-0.042355	2.975615
217.389484	2907.224412	17.473856	-0.042356	2.971824
217.197442	2899.233950	17.478861	-0.042315	2.968019
217.132115	2891.256635	17.483866	-0.042298	2.964223
217.108093	2883.315933	17.488871	-0.042288	2.960441
217.197582	2875.316879	17.493875	-0.042300	2.956632
217.092798	2867.347748	17.498880	-0.042275	2.952822
216.947406	2859.330031	17.503885	-0.042243	2.948983
216.970735	2851.356058	17.508890	-0.042242	2.945167
216.885610	2843.398967	17.513895	-0.042221	2.941350
216.801332	2835.413147	17.518899	-0.042200	2.937514
216.881826	2827.435447	17.523904	-0.042210	2.933685
216.478381	2819.443740	17.528909	-0.042129	2.929819
216.564117	2811.457911	17.533914	-0.042140	2.925976
216.596779	2803.463759	17.538919	-0.042141	2.922122
216.424332	2795.496174	17.543923	-0.042104	2.918264
216.512279	2787.540927	17.548928	-0.042115	2.914421
216.548313	2779.440140	17.553933	-0.042116	2.910500
216.629263	2771.470753	17.558938	-0.042126	2.906640
216.507264	2763.509910	17.563943	-0.042098	2.902768
216.211526	2755.553953	17.568947	-0.042038	2.898883
216.527777	2747.576876	17.573952	-0.042092	2.895016
216.461756	2739.573379	17.578957	-0.042074	2.891111
216.324156	2731.612338	17.583962	-0.042043	2.887216
216.201683	2723.644471	17.588967	-0.042015	2.883315
216.482267	2715.644388	17.593971	-0.042062	2.879414
216.412879	2707.715759	17.598976	-0.042044	2.875523
216.305035	2699.715127	17.603981	-0.042019	2.871590
216.119791	2691.732292	17.608986	-0.041979	2.867656
215.947719	2683.769808	17.613991	-0.041942	2.863727
216.013024	2675.768203	17.618995	-0.041949	2.859787
216.292050	2667.797741	17.624000	-0.041996	2.855869
216.085554	2659.805164	17.629005	-0.041952	2.851907
216.018850	2651.824378	17.634010	-0.041935	2.847953
215.961174	2643.858094	17.639015	-0.041919	2.844002
215.849377	2635.905285	17.644019	-0.041893	2.840048
215.767690	2627.957676	17.649024	-0.041872	2.836094
215.667829	2619.925479	17.654029	-0.041849	2.832090
215.929668	2611.914124	17.659034	-0.041892	2.828112
215.804132	2603.938171	17.664039	-0.041864	2.824124
215.793790	2595.962237	17.669043	-0.041856	2.820137
215.707039	2588.039386	17.674048	-0.041835	2.816167
215.430796	2580.052425	17.679053	-0.041779	2.812147
215.539470	2572.036473	17.684058	-0.041794	2.808130
215.528943	2564.068633	17.689063	-0.041786	2.804124
215.498566	2556.098363	17.694067	-0.041776	2.800110
215.364584	2548.155231	17.699072	-0.041745	2.796098
215.386001	2540.132654	17.704077	-0.041744	2.792049
215.346506	2532.162706	17.709082	-0.041732	2.788017
215.326678	2524.176144	17.714087	-0.041723	2.783972
215.381785	2516.187552	17.719091	-0.041728	2.779925
215.391723	2508.248393	17.724096	-0.041725	2.775894
215.127257	2500.261400	17.729101	-0.041670	2.771817
215.254404	2492.270506	17.734106	-0.041689	2.767755
215.235905	2484.297328	17.739111	-0.041680	2.763687
214.956094	2476.353133	17.744115	-0.041623	2.759613
215.092030	2468.396341	17.749120	-0.041643	2.755551
214.816428	2460.349865	17.754125	-0.041586	2.751412
214.960918	2452.332980	17.759130	-0.041608	2.747307
214.890343	2444.372832	17.764135	-0.041590	2.743213
214.834925	2436.412507	17.769139	-0.041574	2.739113
214.895228	2428.466151	17.774144	-0.041580	2.735021
214.825618	2420.455206	17.779149	-0.041562	2.730882
214.656455	2412.511130	17.784154	-0.041525	2.726765
214.658979	2404.549656	17.789159	-0.041521	2.722644
214.597219	2396.578424	17.794163	-0.041504	2.718507
214.502708	2388.634686	17.799168	-0.041481	2.714376
214.457313	2380.613839	17.804173	-0.041468	2.710201
214.538431	2372.641112	17.809178	-0.041477	2.706053
214.647369	2364.673035	17.814183	-0.041493	2.701903
214.524137	2356.701474	17.819187	-0.041464	2.697730
214.640139	2348.724823	17.824192	-0.041481	2.693563
214.364501	2340.737467	17.829197	-0.041424	2.689360
214.609400	2332.756898	17.834202	-0.041465	2.685186
214.661824	2324.804773	17.839207	-0.041469	2.681008
214.210652	2316.875113	17.844211	-0.041380	2.676804
214.236869	2308.891921	17.849216	-0.041380	2.672595
214.147598	2300.869191	17.854221	-0.041358	2.668351
214.194200	2292.900504	17.859226	-0.041362	2.664138
214.195146	2284.921705	17.864231	-0.041357	2.659910
213.994557	2276.981980	17.869235	-0.041314	2.655683
214.067703	2268.992755	17.874240	-0.041322	2.651440
214.153233	2260.987219	17.879245	-0.041333	2.647183
213.915064	2253.065541	17.884250	-0.041284	2.642943
213.919076	2245.094230	17.889255	-0.041279	2.638685
214.107207	2237.105234	17.894259	-0.041309	2.634423
214.021367	2229.138982	17.899264	-0.041288	2.630148
213.794787	2221.169702	17.904269	-0.041241	2.625855
213.852045	2213.199059	17.909274	-0.041246	2.621573
213.676117	2205.256687	17.914279	-0.041208	2.617284
213.553024	2197.282711	17.919283	-0.041180	2.612974
213.688505	2189.283465	17.924288	-0.041200	2.608661
213.602979	2181.317389	17.929293	-0.041179	2.604344
213.725405	2173.354173	17.934298	-0.041197	2.600035
213.715193	2165.412317	17.939303	-0.041189	2.595721
213.468852	2157.276929	17.944307	-0.041138	2.591279
213.580270	2149.281415	17.949312	-0.041154	2.586930
213.504956	2141.339279	17.954317	-0.041135	2.582590
213.614936	2133.402941	17.959322	-0.041150	2.578259
213.605513	2125.471542	17.964327	-0.041143	2.573915
213.313561	2117.496741	17.969331	-0.041084	2.569520
213.499152	2109.548415	17.974336	-0.041113	2.565166
213.290465	2101.609199	17.979341	-0.041069	2.560781
213.368276	2093.657041	17.984346	-0.041078	2.556402
213.252048	2085.693931	17.989351	-0.041051	2.551995
212.963493	2077.725653	17.994355	-0.040992	2.547566
213.183484	2069.739355	17.999360	-0.041028	2.543155
213.083183	2061.780611	18.004365	-0.041004	2.538729
213.013140	2053.818201	18.009370	-0.040986	2.534296
212.984909	2045.852381	18.014375	-0.040976	2.529856
212.790156	2037.888057	18.019379	-0.040934	2.525396
212.853920	2029.937138	18.024384	-0.040941	2.520955
212.877282	2021.965274	18.029389	-0.040940	2.516492
212.762804	2013.999960	18.034394	-0.040914	2.512014
212.851147	2005.995334	18.039399	-0.040925	2.507521
212.751051	1998.026521	18.044403	-0.040901	2.503026
212.770950	1990.089481	18.049408	-0.040900	2.498550
212.410152	1982.147715	18.054413	-0.040827	2.494035
212.470356	1974.154729	18.059418	-0.040833	2.489514
212.489996	1966.194403	18.064423	-0.040832	2.485000
212.355865	1958.249284	18.069427	-0.040802	2.480476
212.324851	1950.311078	18.074432	-0.040791	2.475954
212.253958	1942.314920	18.079437	-0.040772	2.471388
212.355890	1934.349786	18.084442	-0.040786	2.466845
212.262013	1926.397052	18.089447	-0.040763	2.462285
212.102982	1918.443696	18.094451	-0.040729	2.457712
212.283387	1910.465097	18.099456	-0.040757	2.453141
212.151811	1902.482048	18.104461	-0.040727	2.448536
212.151929	1894.526801	18.109466	-0.040722	2.443948
212.171821	1886.587930	18.114471	-0.040721	2.439362
211.934683	1878.663636	18.119475	-0.040671	2.434756
212.020174	1870.594390	18.124480	-0.040682	2.430083
212.158642	1862.606326	18.129485	-0.040703	2.425451
212.121955	1854.683665	18.134490	-0.040691	2.420835
211.983980	1846.766301	18.139495	-0.040660	2.416206
211.805678	1838.798571	18.144499	-0.040621	2.411535
211.866932	1830.835035	18.149504	-0.040628	2.406877
211.573511	1822.909648	18.154509	-0.040568	2.402203
211.533062	1814.957904	18.159514	-0.040555	2.397525
211.678476	1806.983638	18.164519	-0.040577	2.392840
211.599915	1798.992487	18.169523	-0.040557	2.388117
211.293133	1791.085724	18.174528	-0.040495	2.383417
211.396281	1783.110290	18.179533	-0.040509	2.378699
211.311889	1775.160820	18.184538	-0.040488	2.373972
211.264941	1767.190473	18.189543	-0.040474	2.369227
211.109786	1759.233950	18.194547	-0.040440	2.364472
211.300063	1751.282694	18.199552	-0.040470	2.359738
211.229614	1743.335582	18.204557	-0.040452	2.354975
211.073904	1735.372692	18.209562	-0.040418	2.350187
211.204962	1727.376115	18.214567	-0.040437	2.345392
210.995222	1719.449538	18.219571	-0.040393	2.340602
211.168568	1711.492957	18.224576	-0.040420	2.335815
211.065055	1703.519822	18.229581	-0.040396	2.330985
211.243205	1695.541624	18.234586	-0.040424	2.326166
210.873323	1687.657680	18.239591	-0.040350	2.321348
210.859603	1679.696316	18.244595	-0.040342	2.316503
210.909104	1671.741422	18.249600	-0.040346	2.311657
210.562391	1663.790838	18.254605	-0.040276	2.306770
210.639650	1655.835573	18.259610	-0.040285	2.301906
210.595160	1647.904130	18.264615	-0.040272	2.297035
210.442394	1639.931392	18.269619	-0.040238	2.292120
210.366373	1631.989059	18.274624	-0.040219	2.287219
210.376005	1624.032528	18.279629	-0.040216	2.282306
210.295686	1616.102010	18.284634	-0.040196	2.277391
210.307050	1608.110855	18.289639	-0.040192	2.272436
210.348630	1600.083756	18.294643	-0.040195	2.267450
210.527340	1592.143854	18.299648	-0.040223	2.262519
210.259035	1584.235773	18.304653	-0.040168	2.257559
210.264096	1576.282791	18.309658	-0.040164	2.252583
210.221726	1568.337063	18.314663	-0.040151	2.247597
210.212949	1560.381968	18.319667	-0.040144	2.242596
210.186609	1552.474538	18.324672	-0.040134	2.237613
210.102962	1544.518151	18.329677	-0.040113	2.232583
210.038767	1536.565185	18.334682	-0.040096	2.227545
210.062723	1528.621810	18.339687	-0.040095	2.222510
209.897527	1520.693534	18.344691	-0.040059	2.217456
210.106645	1512.718792	18.349696	-0.040093	2.212395
209.880849	1504.787497	18.354701	-0.040046	2.207310
209.721204	1496.871138	18.359706	-0.040011	2.202230
209.716435	1488.942278	18.364711	-0.040005	2.197143
209.559129	1480.967736	18.369715	-0.039970	2.192001
209.594778	1473.003062	18.374720	-0.039972	2.186872
209.505611	1465.055667	18.379725	-0.039950	2.181730
209.525674	1457.105284	18.384730	-0.039949	2.176583
209.656141	1449.146684	18.389735	-0.039968	2.171430
209.355953	1441.238227	18.394739	-0.039907	2.166257
209.426110	1433.302276	18.399744	-0.039915	2.161088
209.376204	1425.372571	18.404749	-0.039900	2.155899
209.253564	1417.437634	18.409754	-0.039872	2.150688
209.121437	1409.507458	18.414759	-0.039843	2.145467
209.343649	1401.526459	18.419763	-0.039879	2.140232
209.428495	1393.600345	18.424768	-0.039889	2.135008
209.250884	1385.656113	18.429773	-0.039851	2.129734
209.024213	1377.757767	18.434778	-0.039804	2.124473
209.097465	1369.820910	18.439783	-0.039812	2.119202
208.982177	1361.881123	18.444787	-0.039786	2.113897
208.954831	1353.886810	18.449792	-0.039775	2.108552
208.855765	1345.941993	18.454797	-0.039752	2.103218
208.836348	1338.029050	18.459802	-0.039743	2.097901
208.788151	1330.097513	18.464807	-0.039729	2.092554
208.733267	1322.145673	18.469811	-0.039713	2.087180
208.706687	1314.243150	18.474816	-0.039703	2.081828
208.525698	1306.332213	18.479821	-0.039665	2.076441
208.703303	1298.352512	18.484826	-0.039692	2.071028
208.686395	1290.437683	18.489831	-0.039684	2.065627
208.292741	1282.549178	18.494835	-0.039606	2.060191
208.410212	1274.613075	18.499840	-0.039622	2.054760
208.557046	1266.626208	18.504845	-0.039645	2.049283
208.516928	1258.714679	18.509850	-0.039632	2.043823
208.417604	1250.817214	18.514855	-0.039608	2.038353
208.328892	1242.878048	18.519859	-0.039587	2.032841
208.202752	1234.951401	18.524864	-0.039558	2.027318
208.008205	1227.036617	18.529869	-0.039517	2.021781
207.832035	1219.137357	18.534874	-0.039479	2.016242
208.147714	1211.140225	18.539879	-0.039532	2.010670
208.059132	1203.212447	18.544883	-0.039511	2.005089
208.125199	1195.307293	18.549888	-0.039518	1.999525
208.048670	1187.401791	18.554893	-0.039498	1.993930
207.908479	1179.477392	18.559898	-0.039467	1.988299
207.804850	1171.571180	18.564903	-0.039443	1.982668
207.873176	1163.630790	18.569907	-0.039450	1.977016
207.957908	1155.703380	18.574912	-0.039461	1.971358
207.642408	1147.809964	18.579917	-0.039397	1.965666
207.652525	1139.890908	18.584922	-0.039394	1.959974
207.722039	1131.981380	18.589927	-0.039401	1.954278
207.380260	1124.036048	18.594931	-0.039333	1.948495
207.445085	1116.107624	18.599936	-0.039340	1.942752
207.582821	1108.164168	18.604941	-0.039360	1.936988
207.452982	1100.264858	18.609946	-0.039331	1.931210
207.410691	1092.345179	18.614951	-0.039318	1.925410
207.362984	1084.442330	18.619955	-0.039304	1.919603
207.459451	1076.541814	18.624960	-0.039317	1.913797
207.054294	1068.650135	18.629965	-0.039236	1.907924
207.127899	1060.720808	18.634970	-0.039245	1.902058
207.051285	1052.835706	18.639975	-0.039225	1.896190
206.838421	1044.925910	18.644979	-0.039180	1.890270
207.015433	1036.992354	18.649984	-0.039208	1.884358
207.078234	1029.088440	18.654989	-0.039215	1.878436
207.053092	1021.168093	18.659994	-0.039205	1.872474
207.047893	1013.249887	18.664999	-0.039199	1.866496
206.935938	1005.349467	18.670003	-0.039173	1.860500
206.814653	997.480312	18.675008	-0.039145	1.854507
206.473069	989.591507	18.680013	-0.039076	1.848454
206.607914	981.665668	18.685018	-0.039096	1.842409
206.633896	973.775710	18.690023	-0.039096	1.836358
206.745905	965.835899	18.695027	-0.039112	1.830260
206.400307	957.997346	18.700032	-0.039042	1.824165
206.380901	950.088695	18.705037	-0.039033	1.818033
206.622662	942.140312	18.710042	-0.039073	1.811882
206.418462	934.281425	18.715047	-0.039030	1.805726
206.226686	926.413322	18.720051	-0.038989	1.799543
206.397143	918.492441	18.725056	-0.039016	1.793341
206.143217	910.574287	18.730061	-0.038964	1.787067
206.017259	902.700287	18.735066	-0.038935	1.780823
206.027938	894.818782	18.740071	-0.038932	1.774567
205.980753	886.905180	18.745075	-0.038918	1.768256
205.970543	879.030038	18.750080	-0.038911	1.761959
206.028742	871.138739	18.755085	-0.038917	1.755634
205.882358	863.265965	18.760090	-0.038884	1.749275
205.851839	855.388540	18.765095	-0.038873	1.742904
205.672001	847.526612	18.770099	-0.038835	1.736504
205.824985	839.609038	18.775104	-0.038858	1.730076
205.408745	831.781326	18.780109	-0.038776	1.723625
205.459866	823.906147	18.785114	-0.038780	1.717172
205.635960	815.976458	18.790119	-0.038808	1.710665
205.440064	808.106526	18.795123	-0.038766	1.704134
205.269885	800.273168	18.800128	-0.038729	1.697612
205.301945	792.368482	18.805133	-0.038730	1.691032
205.397278	784.477754	18.810138	-0.038743	1.684446
205.108718	776.671688	18.815143	-0.038684	1.677854
205.165431	768.766713	18.820147	-0.038689	1.671199
205.267491	760.881304	18.825152	-0.038703	1.664540
205.185867	753.035402	18.830157	-0.038683	1.657863
204.842750	745.206692	18.835162	-0.038614	1.651138
205.011261	737.314070	18.840167	-0.038640	1.644401
204.773366	729.493592	18.845171	-0.038591	1.637642
204.716143	721.592481	18.850176	-0.038575	1.630811
204.541804	713.720212	18.855181	-0.038537	1.623959
204.840845	705.828544	18.860186	-0.038588	1.617128
204.865290	697.966135	18.865191	-0.038587	1.610255
204.631853	690.144724	18.870195	-0.038539	1.603352
204.721686	682.301866	18.875200	-0.038550	1.596446
204.507714	674.472921	18.880205	-0.038505	1.589479
204.311726	666.648259	18.885210	-0.038464	1.582487
204.365839	658.801249	18.890215	-0.038469	1.575481
204.304692	650.943437	18.895219	-0.038452	1.568417
204.239267	643.128614	18.900224	-0.038435	1.561359
204.038964	635.316629	18.905229	-0.038393	1.554251
204.043687	627.445527	18.910234	-0.038388	1.547088
204.256148	619.585777	18.915239	-0.038423	1.539932
204.088290	611.766708	18.920243	-0.038387	1.532724
203.954494	603.950306	18.925248	-0.038357	1.525489
203.986667	596.129256	18.930253	-0.038358	1.518240
203.905526	588.306247	18.935258	-0.038337	1.510938
203.800225	580.499726	18.940263	-0.038313	1.503611
203.801503	572.669689	18.945267	-0.038308	1.496244
203.942544	564.825790	18.950272	-0.038329	1.488848
203.527626	557.073295	18.955277	-0.038247	1.481415
203.507861	549.259629	18.960282	-0.038238	1.473949
203.539850	541.397678	18.965287	-0.038239	1.466406
203.298217	533.623734	18.970291	-0.038189	1.458866
203.221649	525.830278	18.975296	-0.038169	1.451293
203.134695	518.028900	18.980301	-0.038148	1.443672
203.148963	510.229793	18.985306	-0.038146	1.436029
203.225422	502.417108	18.990311	-0.038155	1.428342
203.153838	494.625487	18.995315	-0.038136	1.420609
202.918088	486.892326	19.000320	-0.038088	1.412866
202.670703	479.118671	19.005325	-0.038036	1.405037
202.731459	471.335130	19.010330	-0.038043	1.397206
202.865040	463.511796	19.015335	-0.038062	1.389303
202.584523	455.765743	19.020339	-0.038005	1.381363
202.601941	447.998800	19.025344	-0.038003	1.373407
202.458974	440.227621	19.030349	-0.037972	1.365372
202.489699	432.475981	19.035354	-0.037972	1.357340
202.390605	424.726060	19.040359	-0.037949	1.349239
202.387262	416.951204	19.045363	-0.037943	1.341080
202.353070	409.213795	19.050368	-0.037932	1.332905
202.212973	401.472272	19.055373	-0.037901	1.324657
202.042872	393.762644	19.060378	-0.037864	1.316385
202.134529	385.881506	19.065383	-0.037876	1.307924
201.997192	378.156088	19.070387	-0.037845	1.299534
202.051653	370.426834	19.075392	-0.037850	1.291122
201.880596	362.732005	19.080397	-0.037814	1.282650
201.752630	355.046237	19.085402	-0.037785	1.274140
201.671401	347.331027	19.090407	-0.037765	1.265548
201.519475	339.652991	19.095411	-0.037731	1.256926
201.582674	331.934832	19.100416	-0.037738	1.248240
201.269950	324.284769	19.105421	-0.037675	1.239499
201.253478	316.578378	19.110426	-0.037667	1.230688
201.319736	308.865530	19.115431	-0.037674	1.221822
200.970047	301.234159	19.120435	-0.037604	1.212904
201.093618	293.531499	19.125440	-0.037622	1.203931
201.041652	285.872394	19.130445	-0.037607	1.194907
200.878784	278.221925	19.135450	-0.037572	1.185801
200.783418	270.589463	19.140455	-0.037549	1.176661
200.725687	262.930856	19.145459	-0.037534	1.167425
200.719122	255.305453	19.150464	-0.037527	1.158166
200.530692	247.660446	19.155469	-0.037487	1.148771
200.442431	240.026551	19.160474	-0.037466	1.139333
200.564531	232.381037	19.165479	-0.037484	1.129846
200.383356	224.796571	19.170483	-0.037445	1.120291
200.363804	217.202828	19.175488	-0.037437	1.110677
200.252363	209.612416	19.180493	-0.037411	1.100963
200.088631	202.051575	19.185498	-0.037375	1.091189
199.988482	194.487303	19.190503	-0.037352	1.081336
199.774059	186.947952	19.195507	-0.037307	1.071400
199.747887	179.381888	19.200512	-0.037297	1.061378
199.678982	171.835561	19.205517	-0.037280	1.051277
199.463424	164.328751	19.210522	-0.037235	1.041097
199.423187	156.810260	19.215527	-0.037222	1.030842
199.020086	149.349267	19.220531	-0.037142	1.020477
198.676673	141.896869	19.225536	-0.037073	1.010031
198.394218	134.438786	19.230541	-0.037016	0.999483
197.968416	126.988638	19.235546	-0.036932	0.988799
197.491332	119.572172	19.240551	-0.036838	0.978032
197.091860	112.151939	19.245555	-0.036759	0.967160
196.706921	104.763879	19.250560	-0.036683	0.956216
196.160904	97.393560	19.255565	-0.036576	0.945129
195.778363	90.020249	19.260570	-0.036500	0.933948
195.395563	82.660885	19.265575	-0.036424	0.922654
194.989647	75.315423	19.270579	-0.036344	0.911234
194.498172	68.005928	19.275584	-0.036247	0.899702
193.833997	60.958404	19.280589	-0.036119	0.888388