Fri Mar 12 13:24:59 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.684313	0.013524	0.000000	0.000007	0.721133

0.564784	0.029831	0.005005	0.000030	0.721124
0.618062	0.024927	0.010010	0.000020	0.721133
0.706021	0.005515	0.015014	0.000003	0.721125
0.424120	0.055735	0.020019	0.000056	0.721125
0.312472	0.077344	0.025024	0.000077	0.721129
0.421872	0.052765	0.030029	0.000056	0.721119
0.662733	0.015966	0.035034	0.000011	0.721131
0.521579	0.036599	0.040038	0.000038	0.721122
0.562630	0.030183	0.045043	0.000030	0.721124
0.593528	0.026050	0.050048	0.000024	0.721127
0.634780	0.015591	0.055053	0.000016	0.721120
0.748150	0.000423	0.060058	-0.000005	0.721130
0.537794	0.033776	0.065062	0.000034	0.721122
0.473617	0.045027	0.070067	0.000046	0.721122
0.500537	0.044222	0.075072	0.000041	0.721130
0.479419	0.044789	0.080077	0.000045	0.721124
0.624532	-0.087789	0.085082	0.000018	0.720914
0.531691	-0.090433	0.090086	0.000036	0.720876
0.353689	-0.057762	0.095091	0.000069	0.720878
0.517893	-0.086189	0.100096	0.000038	0.720880
0.384212	-0.065496	0.105101	0.000063	0.720874
0.459939	-0.074479	0.110106	0.000049	0.720882
0.395999	-0.092620	0.115110	0.000061	0.720824
0.356585	-0.228888	0.120115	0.000068	0.720542
0.356164	-0.226810	0.125120	0.000068	0.720546
0.269148	-0.215456	0.130125	0.000084	0.720538
0.401624	-0.235776	0.135130	0.000060	0.720545
0.431039	-0.243610	0.140134	0.000054	0.720540
0.394241	-0.391027	0.145139	0.000061	0.720236
0.407351	-0.396274	0.150144	0.000059	0.720231
0.275176	-0.377509	0.155149	0.000083	0.720221
0.302280	-0.376569	0.160154	0.000078	0.720233
0.432041	-0.501370	0.165158	0.000054	0.720033
0.332430	-0.549844	0.170163	0.000073	0.719902
0.351140	-0.552482	0.175168	0.000069	0.719904
0.368722	-0.559118	0.180173	0.000066	0.719897
0.386296	-0.681395	0.185178	0.000063	0.719662
0.247669	-0.687728	0.190182	0.000088	0.719601
0.250608	-0.688508	0.195187	0.000088	0.719600
0.331330	-0.758410	0.200192	0.000073	0.719491
0.213503	-0.850370	0.205197	0.000095	0.719268
0.248879	-0.854157	0.210202	0.000088	0.719273
0.386670	-0.909702	0.215206	0.000063	0.719212
0.334090	-1.027956	0.220211	0.000072	0.718960
0.534412	-1.060923	0.225216	0.000035	0.718966
0.402106	-1.090976	0.230221	0.000060	0.718860
0.453150	-1.207220	0.235226	0.000050	0.718649
0.389037	-1.197402	0.240230	0.000062	0.718645
0.343231	-1.281461	0.245235	0.000071	0.718463
0.419186	-1.349715	0.250240	0.000057	0.718355
0.274325	-1.334170	0.255245	0.000084	0.718335
0.170755	-1.474239	0.260250	0.000103	0.718022
-0.027011	-1.440574	0.265254	0.000140	0.718019
-0.044711	-1.514786	0.270259	0.000143	0.717866
0.006084	-1.601892	0.275264	0.000134	0.717712
-0.174910	-1.573345	0.280269	0.000167	0.717705
-0.276816	-1.715463	0.285274	0.000186	0.717388
-0.109569	-1.747838	0.290278	0.000155	0.717383
-0.022298	-1.854135	0.295283	0.000139	0.717203
-0.106051	-1.896411	0.300288	0.000155	0.717090
-0.199193	-1.937873	0.305293	0.000172	0.716976
-0.181129	-2.050406	0.310298	0.000169	0.716759
-0.454413	-2.015193	0.315302	0.000220	0.716733
-0.411189	-2.166191	0.320307	0.000212	0.716449
-0.648958	-2.120900	0.325312	0.000256	0.716455
-1.360015	-2.133616	0.330317	0.000388	0.716179
-1.854914	-2.066045	0.335322	0.000480	0.716138
-2.084250	-2.061694	0.340326	0.000523	0.716066
-2.559539	-2.070798	0.345331	0.000611	0.715880
-2.253004	-2.123020	0.350336	0.000554	0.715885
-3.008298	-2.087732	0.355341	0.000695	0.715688
-3.867498	-2.004221	0.360346	0.000855	0.715550
-3.368612	-2.096420	0.365350	0.000762	0.715544
-3.657711	-2.110635	0.370355	0.000816	0.715414
-4.680050	-2.017902	0.375360	0.001006	0.715236
-4.555952	-2.045144	0.380365	0.000983	0.715226
-4.428276	-2.063698	0.385370	0.000959	0.715234
-5.086908	-2.099613	0.390374	0.001082	0.714930
-5.739579	-1.994567	0.395379	0.001203	0.714908
-5.577782	-2.020146	0.400384	0.001173	0.714915
-5.463192	-2.045063	0.405389	0.001152	0.714906
-6.049631	-2.076504	0.410394	0.001261	0.714636
-6.284300	-2.049459	0.415398	0.001305	0.714607
-6.474930	-2.015791	0.420403	0.001340	0.714606
-6.196259	-2.060935	0.425408	0.001288	0.714615
-6.532038	-2.101800	0.430413	0.001351	0.714415
-7.471971	-2.002427	0.435418	0.001526	0.714280
-7.357051	-2.023430	0.440422	0.001504	0.714279
-7.797202	-1.946329	0.445427	0.001586	0.714277
-7.367867	-2.021345	0.450432	0.001506	0.714280
-7.471000	-2.094650	0.455437	0.001526	0.714097
-8.736474	-1.931390	0.460442	0.001761	0.713974
-8.337778	-2.003777	0.465446	0.001687	0.713971
-8.077708	-2.053233	0.470451	0.001638	0.713965
-8.599542	-1.955528	0.475456	0.001736	0.713975
-8.465483	-1.984576	0.480461	0.001711	0.713964
-8.741101	-2.078737	0.485466	0.001762	0.713680
-9.355754	-1.982358	0.490470	0.001876	0.713654
-9.388979	-1.976457	0.495475	0.001882	0.713654
-8.754663	-2.085093	0.500480	0.001764	0.713662
-9.392144	-1.976756	0.505485	0.001883	0.713652
-9.339265	-2.001624	0.510490	0.001873	0.713621
-9.634391	-2.078816	0.515494	0.001928	0.713363
-10.029946	-2.009183	0.520499	0.002002	0.713362
-10.047606	-2.003347	0.525504	0.002005	0.713367
-9.893284	-2.034668	0.530509	0.001976	0.713359
-10.007489	-2.011514	0.535514	0.001997	0.713365
-10.249753	-1.998190	0.540518	0.002043	0.713306
-10.976088	-2.011747	0.545523	0.002178	0.713021
-10.553093	-2.081485	0.550528	0.002099	0.713032
-11.248833	-1.962640	0.555533	0.002228	0.713022
-11.028513	-1.997051	0.560538	0.002187	0.713032
-10.931517	-2.016195	0.565542	0.002169	0.713028
-11.013630	-2.003898	0.570547	0.002185	0.713024
-11.031400	-2.107024	0.575552	0.002188	0.712812
-12.341862	-1.925182	0.580557	0.002432	0.712709
-12.091917	-1.966678	0.585562	0.002385	0.712715
-11.857284	-2.009092	0.590566	0.002342	0.712714
-12.420878	-1.911395	0.595571	0.002447	0.712709
-11.856739	-2.009226	0.600576	0.002342	0.712714
-12.097041	-1.968898	0.605581	0.002386	0.712709
-12.447587	-1.993790	0.610586	0.002452	0.712536
-13.168989	-1.938434	0.615590	0.002586	0.712390
-12.841757	-1.999072	0.620595	0.002525	0.712385
-12.998372	-1.965385	0.625600	0.002554	0.712397
-13.375233	-1.903583	0.630605	0.002624	0.712386
-13.037493	-1.960020	0.635610	0.002561	0.712394
-12.997883	-1.969212	0.640614	0.002554	0.712389
-13.415617	-1.895308	0.645619	0.002632	0.712388
-13.248200	-2.059064	0.650624	0.002600	0.712122
-13.851515	-1.969520	0.655629	0.002713	0.712086
-14.384386	-1.870671	0.660634	0.002812	0.712094
-13.862839	-1.964680	0.665638	0.002715	0.712092
-13.581479	-2.017262	0.670643	0.002662	0.712087
-13.893473	-1.956283	0.675648	0.002720	0.712097
-14.068116	-1.931802	0.680653	0.002753	0.712084
-14.034102	-2.072120	0.685658	0.002747	0.711817
-14.779680	-1.966650	0.690662	0.002885	0.711762
-15.207783	-1.892225	0.695667	0.002965	0.711759
-14.776206	-1.965115	0.700672	0.002885	0.711767
-14.911906	-1.946160	0.705677	0.002910	0.711756
-14.945372	-1.937592	0.710682	0.002916	0.711761
-14.833649	-1.959477	0.715686	0.002895	0.711758
-15.229294	-1.979102	0.720691	0.002969	0.711578
-16.004074	-1.901600	0.725696	0.003113	0.711457
-16.056013	-1.896277	0.730701	0.003123	0.711449
-15.526515	-1.988302	0.735706	0.003024	0.711454
-15.444190	-2.003617	0.740710	0.003009	0.711453
-16.057869	-1.896355	0.745715	0.003123	0.711449
-15.438277	-2.002830	0.750720	0.003008	0.711456
-15.580290	-2.022110	0.755725	0.003034	0.711368
-16.855969	-1.910012	0.760730	0.003272	0.711138
-16.729199	-1.932699	0.765734	0.003248	0.711138
-16.708779	-1.938156	0.770739	0.003244	0.711134
-16.223139	-2.021352	0.775744	0.003154	0.711141
-16.731879	-1.934312	0.780749	0.003249	0.711134
-16.720514	-1.932875	0.785754	0.003246	0.711140
-16.387640	-2.006683	0.790758	0.003184	0.711112
-17.614496	-1.911096	0.795763	0.003413	0.710866
-17.377848	-1.948556	0.800768	0.003369	0.710875
-17.532654	-1.925328	0.805773	0.003398	0.710867
-17.288961	-1.964707	0.810778	0.003352	0.710875
-17.389091	-1.947352	0.815782	0.003371	0.710874
-17.479246	-1.933572	0.820787	0.003388	0.710869
-17.173990	-2.020554	0.825792	0.003331	0.710804
-18.533242	-1.916945	0.830797	0.003584	0.710528
-18.226057	-1.967642	0.835802	0.003527	0.710536
-18.183186	-1.974754	0.840806	0.003519	0.710537
-18.679155	-1.889358	0.845811	0.003611	0.710531
-18.313878	-1.951267	0.850816	0.003543	0.710537
-18.120488	-1.989305	0.855821	0.003507	0.710530
-18.339542	-1.982876	0.860826	0.003548	0.710465
-19.075153	-1.975370	0.865830	0.003685	0.710218
-19.263463	-1.944995	0.870835	0.003720	0.710212
-19.096698	-1.969303	0.875840	0.003689	0.710223
-19.482934	-1.904045	0.880845	0.003760	0.710216
-19.256976	-1.940973	0.885850	0.003718	0.710222
-19.117081	-1.968305	0.890854	0.003692	0.710218
-19.382935	-1.932078	0.895859	0.003742	0.710195
-20.036476	-1.964094	0.900864	0.003863	0.709899
-20.219855	-1.936000	0.905869	0.003898	0.709890
-20.160197	-1.944191	0.910874	0.003886	0.709894
-20.295429	-1.919368	0.915878	0.003912	0.709896
-20.444856	-1.895685	0.920883	0.003939	0.709890
-19.885293	-1.993161	0.925888	0.003835	0.709895
-20.293430	-1.924153	0.930893	0.003911	0.709887
-20.567985	-1.971346	0.935898	0.003962	0.709695
-20.992876	-1.944737	0.940902	0.004041	0.709597
-21.011555	-1.945017	0.945907	0.004045	0.709590
-20.921490	-1.954999	0.950912	0.004028	0.709602
-21.054340	-1.937195	0.955917	0.004053	0.709590
-20.888591	-1.964295	0.960922	0.004022	0.709595
-21.191934	-1.909629	0.965926	0.004078	0.709596
-21.497133	-1.968365	0.970931	0.004135	0.709370
-21.704326	-1.982597	0.975936	0.004174	0.709268
-21.949052	-1.942550	0.980941	0.004219	0.709261
-22.075195	-1.918098	0.985946	0.004243	0.709265
-22.007461	-1.930968	0.990950	0.004230	0.709263
-21.791089	-1.971422	0.995955	0.004190	0.709259
-21.760453	-1.972805	1.000960	0.004184	0.709267
-22.164468	-2.009391	1.005965	0.004259	0.709050
-22.948358	-1.917970	1.010970	0.004405	0.708954
-22.645974	-1.969542	1.015974	0.004349	0.708958
-22.791810	-1.947468	1.020979	0.004376	0.708950
-22.835124	-1.934270	1.025984	0.004384	0.708961
-22.850733	-1.936887	1.030989	0.004387	0.708951
-22.928315	-1.919609	1.035994	0.004401	0.708958
-22.973556	-2.000637	1.040998	0.004410	0.708779
-24.183087	-1.858818	1.046003	0.004635	0.708632
-23.621183	-1.953257	1.051008	0.004530	0.708643
-23.641760	-1.954051	1.056013	0.004534	0.708634
-23.677939	-1.944192	1.061018	0.004541	0.708641
-23.472828	-1.980261	1.066022	0.004503	0.708642
-24.168530	-1.860260	1.071027	0.004632	0.708634
-23.660848	-2.003872	1.076032	0.004538	0.708528
-24.289034	-1.983983	1.081037	0.004655	0.708343
-24.434354	-1.955920	1.086042	0.004682	0.708348
-24.406913	-1.959427	1.091046	0.004676	0.708350
-24.379104	-1.966857	1.096051	0.004671	0.708346
-24.404745	-1.958021	1.101056	0.004676	0.708354
-24.584987	-1.929927	1.106061	0.004710	0.708346
-24.646126	-2.052236	1.111066	0.004721	0.708079
-25.393341	-1.950728	1.116070	0.004860	0.708016
-25.745750	-1.892606	1.121075	0.004926	0.708006
-25.057437	-2.009001	1.126080	0.004797	0.708019
-25.274188	-1.974085	1.131085	0.004838	0.708012
-25.473779	-1.938997	1.136090	0.004875	0.708011
-25.032561	-2.023186	1.141094	0.004793	0.708000
-25.975446	-2.005700	1.146099	0.004968	0.707698
-26.307460	-1.943583	1.151104	0.005030	0.707704
-26.628362	-1.890918	1.156109	0.005090	0.707695
-25.980806	-2.003984	1.161114	0.004969	0.707699
-26.107520	-1.979043	1.166118	0.004993	0.707704
-26.580239	-1.900136	1.171123	0.005081	0.707693
-26.123200	-1.975975	1.176128	0.004996	0.707705
-26.857745	-2.007262	1.181133	0.005132	0.707379
-27.518224	-1.890643	1.186138	0.005255	0.707377
-27.262876	-1.935710	1.191142	0.005208	0.707378
-27.090043	-1.969414	1.196147	0.005176	0.707372
-26.917707	-1.995016	1.201152	0.005144	0.707383
-27.160027	-1.955538	1.206157	0.005189	0.707375
-27.200851	-1.947347	1.211162	0.005196	0.707377
-27.152515	-2.078636	1.216166	0.005187	0.707131
-28.123577	-1.933442	1.221171	0.005368	0.707075
-27.810852	-1.983100	1.226176	0.005310	0.707087
-27.805047	-1.988663	1.231181	0.005309	0.707078
-28.359641	-1.889321	1.236186	0.005412	0.707079
-27.748346	-1.996009	1.241190	0.005298	0.707084
-27.655597	-2.052720	1.246195	0.005281	0.707003
-28.744957	-1.983478	1.251200	0.005484	0.706752
-28.784124	-1.979041	1.256205	0.005491	0.706747
-28.898583	-1.956326	1.261210	0.005512	0.706752
-28.767576	-1.978648	1.266214	0.005488	0.706754
-29.210285	-1.903289	1.271219	0.005570	0.706747
-29.008923	-1.935820	1.276224	0.005533	0.706754
-28.577215	-2.044423	1.281229	0.005452	0.706690
-29.724347	-1.962684	1.286234	0.005666	0.706444
-29.495116	-2.002710	1.291238	0.005623	0.706445
-29.849803	-1.942922	1.296243	0.005689	0.706438
-29.807751	-1.946086	1.301248	0.005681	0.706447
-29.890688	-1.934506	1.306253	0.005697	0.706441
-30.067091	-1.903002	1.311258	0.005729	0.706441
-29.726711	-1.970183	1.316262	0.005666	0.706428
-30.548776	-1.976854	1.321267	0.005819	0.706120
-30.322317	-2.012894	1.326272	0.005777	0.706129
-30.354743	-2.010587	1.331277	0.005783	0.706122
-30.641400	-1.957992	1.336282	0.005836	0.706125
-30.581371	-1.968285	1.341286	0.005825	0.706126
-30.797984	-1.931399	1.346291	0.005865	0.706122
-30.706321	-1.971594	1.351296	0.005848	0.706074
-31.668315	-1.908766	1.356301	0.006027	0.705856
-31.169703	-1.994759	1.361306	0.005935	0.705862
-31.181278	-1.991705	1.366310	0.005937	0.705864
-31.739239	-1.894317	1.371315	0.006041	0.705860
-31.305558	-1.968424	1.376320	0.005960	0.705866
-31.335683	-1.965867	1.381325	0.005965	0.705860
-31.619909	-1.968809	1.386330	0.006018	0.705753
-32.530088	-1.919584	1.391334	0.006188	0.705525
-32.149687	-1.990403	1.396339	0.006117	0.705519
-31.982545	-2.015137	1.401344	0.006086	0.705530
-32.521876	-1.922928	1.406349	0.006186	0.705522
-32.372645	-1.949123	1.411354	0.006158	0.705522
-32.040049	-2.008860	1.416358	0.006096	0.705522
-32.462476	-2.014244	1.421363	0.006175	0.705359
-33.364268	-1.926708	1.426368	0.006343	0.705212
-32.976038	-1.999000	1.431373	0.006271	0.705206
-33.335871	-1.935181	1.436378	0.006338	0.705205
-33.310755	-1.936769	1.441382	0.006333	0.705211
-33.234653	-1.953689	1.446387	0.006319	0.705204
-33.148925	-1.965347	1.451392	0.006303	0.705212
-33.379109	-1.988335	1.456397	0.006346	0.705083
-34.059241	-1.966168	1.461402	0.006472	0.704883
-33.613551	-2.043279	1.466406	0.006389	0.704888
-34.389587	-1.906461	1.471411	0.006534	0.704885
-34.509544	-1.882808	1.476416	0.006556	0.704890
-34.070373	-1.964143	1.481421	0.006474	0.704883
-34.301972	-1.923610	1.486426	0.006517	0.704882
-34.243733	-1.964895	1.491430	0.006506	0.704820
-34.960336	-1.954042	1.496435	0.006640	0.704584
-34.611380	-2.012438	1.501440	0.006575	0.704592
-35.359874	-1.881417	1.506445	0.006714	0.704587
-35.236454	-1.903285	1.511450	0.006691	0.704588
-34.631741	-2.009213	1.516454	0.006579	0.704591
-35.052593	-1.939509	1.521459	0.006657	0.704581
-34.882730	-2.011797	1.526464	0.006625	0.704496
-35.681764	-1.988475	1.531469	0.006774	0.704256
-35.615603	-1.999205	1.536474	0.006762	0.704258
-36.074461	-1.913971	1.541478	0.006847	0.704265
-35.926005	-1.945142	1.546483	0.006819	0.704256
-35.542259	-2.009860	1.551488	0.006748	0.704263
-35.793070	-1.967680	1.556493	0.006795	0.704258
-36.135528	-1.980041	1.561498	0.006858	0.704110
-36.573843	-1.978469	1.566502	0.006940	0.703956
-36.786833	-1.944694	1.571507	0.006980	0.703947
-36.818535	-1.934107	1.576512	0.006986	0.703957
-36.465830	-2.000879	1.581517	0.006920	0.703949
-36.354144	-2.022319	1.586522	0.006899	0.703946
-36.731564	-1.950753	1.591526	0.006969	0.703955
-37.144767	-1.976273	1.596531	0.007046	0.703755
-37.542105	-1.964017	1.601536	0.007120	0.703637
-37.661114	-1.943901	1.606541	0.007142	0.703635
-38.033312	-1.877250	1.611546	0.007212	0.703635
-37.775279	-1.922346	1.616550	0.007164	0.703637
-37.659585	-1.946589	1.621555	0.007142	0.703630
-37.826331	-1.912933	1.626560	0.007173	0.703638
-37.761109	-1.942605	1.631565	0.007161	0.703602
-38.380739	-1.960690	1.636570	0.007276	0.703342
-38.401387	-1.955171	1.641574	0.007280	0.703346
-38.844886	-1.879712	1.646579	0.007363	0.703339
-38.082932	-2.013148	1.651584	0.007221	0.703343
-38.366261	-1.964700	1.656589	0.007273	0.703339
-38.748811	-1.896241	1.661594	0.007345	0.703340
-38.275615	-2.021261	1.666598	0.007257	0.703258
-39.345670	-1.958775	1.671603	0.007456	0.702999
-39.139845	-1.989232	1.676608	0.007417	0.703011
-39.489433	-1.930397	1.681613	0.007482	0.703004
-39.203090	-1.982708	1.686618	0.007429	0.703002
-39.282903	-1.966255	1.691622	0.007444	0.703006
-39.758233	-1.884923	1.696627	0.007532	0.703000
-39.347997	-1.995453	1.701632	0.007456	0.702924
-40.090690	-1.977170	1.706637	0.007594	0.702694
-40.220336	-1.956004	1.711642	0.007618	0.702690
-40.231020	-1.951066	1.716646	0.007620	0.702696
-40.223600	-1.955807	1.721651	0.007619	0.702689
-40.204709	-1.954714	1.726656	0.007615	0.702698
-40.382126	-1.925416	1.731661	0.007648	0.702693
-40.266860	-1.999789	1.736666	0.007627	0.702585
-41.158921	-1.945353	1.741670	0.007793	0.702373
-41.036410	-1.971270	1.746675	0.007770	0.702365
-40.985578	-1.975488	1.751680	0.007761	0.702375
-41.056167	-1.964078	1.756685	0.007774	0.702372
-41.347093	-1.914810	1.761690	0.007828	0.702367
-41.139616	-1.947615	1.766694	0.007789	0.702376
-41.166137	-1.996990	1.771699	0.007794	0.702266
-41.923752	-1.953855	1.776704	0.007935	0.702080
-41.811367	-1.976885	1.781709	0.007914	0.702074
-42.051352	-1.935308	1.786714	0.007959	0.702072
-41.687261	-1.997354	1.791718	0.007891	0.702078
-42.175282	-1.913055	1.796723	0.007982	0.702072
-42.014951	-1.936762	1.801728	0.007952	0.702082
-41.825023	-2.049402	1.806733	0.007917	0.701923
-43.299036	-1.875503	1.811738	0.008191	0.701743
-42.847465	-1.951685	1.816742	0.008107	0.701752
-42.867722	-1.952103	1.821747	0.008111	0.701744
-42.824135	-1.957001	1.826752	0.008103	0.701750
-42.766908	-1.969500	1.831757	0.008092	0.701745
-42.765564	-1.970144	1.836762	0.008092	0.701744
-42.784451	-2.042001	1.841766	0.008095	0.701592
-44.210830	-1.867178	1.846771	0.008361	0.701431
-43.597409	-1.972186	1.851776	0.008247	0.701440
-43.507562	-1.990270	1.856781	0.008230	0.701436
-43.952182	-1.912586	1.861786	0.008313	0.701433
-43.423171	-2.003775	1.866790	0.008214	0.701439
-43.734535	-1.952667	1.871795	0.008272	0.701430
-44.059635	-1.978750	1.876800	0.008333	0.701260
-44.913367	-1.892895	1.881805	0.008492	0.701126
-44.361149	-1.993082	1.886810	0.008389	0.701122
-44.178545	-2.022003	1.891814	0.008355	0.701130
-44.985966	-1.883320	1.896819	0.008505	0.701119
-44.619084	-1.943675	1.901824	0.008437	0.701129
-44.326057	-1.997913	1.906829	0.008382	0.701125
-44.733410	-2.003240	1.911834	0.008458	0.700967
-45.318461	-1.940921	1.916838	0.008567	0.700882
-45.222408	-1.962807	1.921843	0.008549	0.700873
-44.866503	-2.023095	1.926848	0.008483	0.700879
-45.078902	-1.987203	1.931853	0.008522	0.700875
-45.386598	-1.933970	1.936858	0.008579	0.700872
-45.078692	-2.043977	1.941862	0.008522	0.700760
-46.516908	-1.900351	1.946867	0.008790	0.700532
-45.900646	-2.006802	1.951872	0.008675	0.700539
-46.032047	-1.983812	1.956877	0.008700	0.700538
-46.333121	-1.932681	1.961882	0.008756	0.700533
-45.837556	-2.018340	1.966886	0.008663	0.700538
-46.020361	-1.990726	1.971891	0.008697	0.700528
-46.504522	-2.021967	1.976896	0.008788	0.700290
-47.437574	-1.889691	1.981901	0.008961	0.700221
-47.317646	-1.913906	1.986906	0.008939	0.700215
-46.567672	-2.043514	1.991910	0.008799	0.700223
-47.398835	-1.899426	1.996915	0.008954	0.700215
-47.107080	-1.949509	2.001920	0.008900	0.700219

-47.380612	-1.983832	2.011917	0.008951	0.700050
-48.053591	-1.940929	2.021914	0.009076	0.699894
-47.992504	-1.952631	2.031910	0.009064	0.699893
-48.016415	-1.947172	2.041907	0.009069	0.699895
-48.003491	-1.949091	2.051904	0.009066	0.699896
-48.024379	-1.945327	2.061901	0.009070	0.699896
-47.749718	-1.994655	2.071898	0.009019	0.699895
-47.991438	-1.952009	2.081894	0.009064	0.699895
-47.367225	-1.933471	2.091891	0.008948	0.700158
-47.134963	-1.944682	2.101888	0.008904	0.700219
-46.960197	-1.975770	2.111885	0.008872	0.700220
-46.959356	-1.976767	2.121882	0.008872	0.700218
-47.249870	-1.925729	2.131878	0.008926	0.700217
-46.876041	-1.991277	2.141875	0.008856	0.700219
-46.999685	-1.969187	2.151872	0.008879	0.700219
-47.008212	-1.920383	2.161869	0.008881	0.700315
-46.015733	-1.990834	2.171866	0.008696	0.700531
-46.320531	-1.936093	2.181862	0.008752	0.700532
-46.075683	-1.977713	2.191859	0.008707	0.700536
-46.254590	-1.944574	2.201856	0.008740	0.700539
-45.597016	-1.937525	2.211853	0.008618	0.700791
-45.579821	-1.900286	2.221850	0.008614	0.700873
-45.298827	-1.950818	2.231846	0.008562	0.700872
-45.091370	-1.985536	2.241843	0.008523	0.700876
-44.991909	-1.911963	2.251840	0.008505	0.701062
-44.552406	-1.959353	2.261837	0.008423	0.701124
-44.384966	-1.990522	2.271834	0.008392	0.701122
-44.690479	-1.920569	2.281830	0.008449	0.701153
-43.629635	-1.969793	2.291827	0.008251	0.701437
-43.878288	-1.924989	2.301824	0.008297	0.701438
-43.514411	-1.989527	2.311821	0.008229	0.701438
-43.431151	-1.924300	2.321818	0.008214	0.701601
-42.836726	-1.961480	2.331814	0.008103	0.701740
-42.993957	-1.932709	2.341811	0.008132	0.701742
-42.779621	-1.956367	2.351808	0.008092	0.701771
-41.923517	-1.960445	2.361805	0.007933	0.702072
-42.060859	-1.936998	2.371802	0.007959	0.702070
-41.942934	-1.959879	2.381798	0.007937	0.702066
-41.679609	-1.927264	2.391795	0.007887	0.702227
-41.191954	-1.943134	2.401792	0.007797	0.702371
-41.033565	-1.970949	2.411789	0.007767	0.702372
-41.278432	-1.911553	2.421786	0.007813	0.702404
-40.343798	-1.936218	2.431782	0.007639	0.702691
-40.308376	-1.941759	2.441779	0.007632	0.702692
-40.110820	-1.977176	2.451776	0.007595	0.702692
-39.621209	-1.967036	2.461773	0.007504	0.702889
-39.611983	-1.912889	2.471770	0.007502	0.703002
-39.456669	-1.940039	2.481766	0.007473	0.703003
-39.306293	-1.929780	2.491763	0.007445	0.703078
-38.493956	-1.943677	2.501760	0.007294	0.703342
-38.399405	-1.960224	2.511757	0.007276	0.703343
-38.599928	-1.925206	2.521754	0.007314	0.703342
-38.071376	-1.919859	2.531750	0.007215	0.703543
-37.826394	-1.917103	2.541747	0.007169	0.703636
-37.681327	-1.941533	2.551744	0.007142	0.703639
-37.535847	-1.924283	2.561741	0.007115	0.703727
-36.997816	-1.909407	2.571738	0.007015	0.703950
-36.828687	-1.938552	2.581734	0.006983	0.703952
-36.859345	-1.932504	2.591731	0.006989	0.703954
-36.143911	-1.916928	2.601728	0.006856	0.704242
-35.932549	-1.944026	2.611725	0.006817	0.704264
-35.936231	-1.945307	2.621722	0.006817	0.704260
-35.596777	-1.941313	2.631718	0.006754	0.704390
-34.997607	-1.949556	2.641715	0.006642	0.704589
-35.100499	-1.929970	2.651712	0.006661	0.704591
-34.857035	-1.974382	2.661709	0.006616	0.704589
-34.636027	-1.892597	2.671706	0.006575	0.704834
-34.204254	-1.944545	2.681702	0.006494	0.704884
-34.225397	-1.941124	2.691699	0.006498	0.704883
-33.958054	-1.913655	2.701696	0.006448	0.705035
-33.271798	-1.948855	2.711693	0.006321	0.705210
-33.511640	-1.906873	2.721690	0.006365	0.705209
-33.317530	-1.933790	2.731686	0.006329	0.705224
-32.644499	-1.904974	2.741683	0.006204	0.705524
-32.402594	-1.947942	2.751680	0.006159	0.705524
-32.433080	-1.943438	2.761677	0.006164	0.705522
-32.237876	-1.875220	2.771674	0.006128	0.705730
-31.526507	-1.936601	2.781670	0.005995	0.705861
-31.749737	-1.894630	2.791667	0.006037	0.705866
-31.523169	-1.914889	2.801664	0.005995	0.705907
-30.866823	-1.922401	2.811661	0.005872	0.706127
-30.744274	-1.945179	2.821658	0.005850	0.706125
-30.880784	-1.919560	2.831654	0.005875	0.706128
-30.415090	-1.880607	2.841651	0.005788	0.706373
-30.266222	-1.870275	2.851648	0.005760	0.706447
-30.050540	-1.909187	2.861645	0.005720	0.706446
-29.750345	-1.871251	2.871642	0.005664	0.706630
-29.095271	-1.928416	2.881638	0.005542	0.706750
-29.522691	-1.850981	2.891635	0.005622	0.706752
-28.828218	-1.927416	2.901632	0.005493	0.706848
-28.390033	-1.887667	2.911629	0.005411	0.707084
-28.205591	-1.921788	2.921626	0.005377	0.707082
-28.427302	-1.882890	2.931622	0.005418	0.707081
-27.458634	-1.926441	2.941619	0.005237	0.707340
-27.291331	-1.937957	2.951616	0.005206	0.707377
-27.385395	-1.920722	2.961613	0.005224	0.707378
-27.289629	-1.902387	2.971610	0.005206	0.707449
-26.511269	-1.916111	2.981606	0.005061	0.707700
-26.472451	-1.922600	2.991603	0.005054	0.707701
-26.417993	-1.932500	3.001600	0.005043	0.707700
-26.138687	-1.866111	3.011597	0.004991	0.707933
-25.388859	-1.961207	3.021594	0.004852	0.708011
-25.737382	-1.898034	3.031590	0.004916	0.708013
-25.413024	-1.920135	3.041587	0.004856	0.708085
-24.703815	-1.913259	3.051584	0.004724	0.708352
-24.694174	-1.915639	3.061581	0.004722	0.708350
-24.514428	-1.947479	3.071578	0.004689	0.708351
-24.424601	-1.869170	3.081574	0.004672	0.708540
-23.853531	-1.920816	3.091571	0.004565	0.708641
-23.828970	-1.924295	3.101568	0.004561	0.708642
-23.931394	-1.871701	3.111565	0.004580	0.708711
-22.947867	-1.925337	3.121562	0.004397	0.708955
-23.132482	-1.893369	3.131558	0.004431	0.708953
-22.853338	-1.942806	3.141555	0.004379	0.708954
-22.365103	-1.912339	3.151552	0.004288	0.709189
-22.213605	-1.900365	3.161549	0.004260	0.709267
-22.094887	-1.923005	3.171546	0.004238	0.709264
-22.221411	-1.850071	3.181542	0.004261	0.709365
-21.058482	-1.942627	3.191539	0.004045	0.709595
-21.195913	-1.917234	3.201536	0.004070	0.709597
-21.302689	-1.898086	3.211533	0.004090	0.709597
-20.697927	-1.886044	3.221530	0.003977	0.709837
-20.511726	-1.892372	3.231526	0.003943	0.709890
-20.197930	-1.946339	3.241523	0.003884	0.709894
-20.439836	-1.841146	3.251520	0.003929	0.710018
-19.419231	-1.921633	3.261517	0.003739	0.710221
-19.545460	-1.900974	3.271514	0.003763	0.710218
-19.630042	-1.886369	3.281510	0.003778	0.710217
-18.663237	-1.908213	3.291507	0.003598	0.710517
-18.566604	-1.916472	3.301504	0.003580	0.710535
-18.218579	-1.978569	3.311501	0.003515	0.710535
-18.581754	-1.884971	3.321498	0.003583	0.710593
-17.684074	-1.906701	3.331494	0.003416	0.710869
-17.429545	-1.951509	3.341491	0.003368	0.710870
-17.619063	-1.916482	3.351488	0.003404	0.710873
-17.320938	-1.897256	3.361485	0.003348	0.711017
-16.707872	-1.945650	3.371482	0.003234	0.711139
-17.045947	-1.886383	3.381478	0.003297	0.711137
-16.807638	-1.905310	3.391475	0.003252	0.711184
-16.243887	-1.868820	3.401472	0.003147	0.711457
-15.800699	-1.947165	3.411469	0.003065	0.711459
-16.252440	-1.868193	3.421466	0.003149	0.711456
-15.497341	-1.875738	3.431462	0.003008	0.711709
-15.178630	-1.906188	3.441459	0.002949	0.711762
-15.243730	-1.894155	3.451456	0.002961	0.711763
-14.912190	-1.872590	3.461453	0.002899	0.711923
-14.200216	-1.915657	3.471450	0.002767	0.712091
-14.386735	-1.881205	3.481446	0.002801	0.712093
-14.271683	-1.901390	3.491443	0.002780	0.712094
-13.720683	-1.850628	3.501440	0.002677	0.712391
-13.431520	-1.900149	3.511437	0.002623	0.712395
-13.358426	-1.916075	3.521434	0.002610	0.712389
-12.992731	-1.892395	3.531430	0.002541	0.712566
-12.446414	-1.916538	3.541427	0.002440	0.712712
-12.634881	-1.882916	3.551424	0.002475	0.712712
-12.573765	-1.882146	3.561421	0.002463	0.712735
-12.115031	-1.819080	3.571418	0.002378	0.713023
-11.723664	-1.889281	3.581414	0.002305	0.713023
-11.871897	-1.862083	3.591411	0.002332	0.713024
-11.154460	-1.847248	3.601408	0.002199	0.713308
-10.733288	-1.894195	3.611405	0.002120	0.713364
-10.713214	-1.899970	3.621402	0.002117	0.713360
-10.750498	-1.865507	3.631398	0.002124	0.713415
-10.076313	-1.867173	3.641395	0.001998	0.713651
-9.683713	-1.935390	3.651392	0.001925	0.713654
-9.946836	-1.887644	3.661389	0.001974	0.713656
-9.542361	-1.846089	3.671386	0.001898	0.713882
-9.263080	-1.852236	3.681382	0.001846	0.713969
-8.953869	-1.905043	3.691379	0.001789	0.713973
-9.058977	-1.840065	3.701376	0.001808	0.714065
-8.144284	-1.895202	3.711373	0.001638	0.714280
-8.299730	-1.867664	3.721370	0.001667	0.714280
-8.089942	-1.905667	3.731366	0.001628	0.714278
-7.705424	-1.839432	3.741363	0.001556	0.714546
-6.888081	-1.952926	3.751360	0.001404	0.714610
-6.993657	-1.935139	3.761357	0.001424	0.714608
-7.135491	-1.910893	3.771354	0.001450	0.714606
-6.146867	-1.940912	3.781350	0.001266	0.714896
-5.936279	-1.972677	3.791347	0.001227	0.714908
-5.832305	-1.989663	3.801344	0.001207	0.714911
-5.861142	-1.985232	3.811341	0.001213	0.714909
-5.486602	-1.935054	3.821338	0.001143	0.715141
-5.101096	-1.959567	3.831334	0.001071	0.715229
-5.196517	-1.940675	3.841331	0.001089	0.715233
-4.754549	-2.017359	3.851328	0.001006	0.715237
-4.298366	-1.965468	3.861325	0.000921	0.715501
-3.990503	-1.995597	3.871322	0.000864	0.715550
-3.921647	-2.008373	3.881318	0.000851	0.715549
-3.950944	-2.003113	3.891315	0.000857	0.715549
-3.231581	-1.996347	3.901312	0.000723	0.715817
-3.057495	-1.991550	3.911309	0.000690	0.715888
-3.060647	-1.991617	3.921306	0.000691	0.715887
-2.863791	-2.026959	3.931302	0.000654	0.715886
-2.659906	-1.970115	3.941299	0.000616	0.716071
-2.230435	-2.011428	3.951296	0.000536	0.716141
-2.316110	-1.996401	3.961293	0.000552	0.716140
-2.245397	-1.966465	3.971290	0.000539	0.716225
-1.514913	-1.981670	3.981286	0.000403	0.716452
-1.626363	-1.959092	3.991283	0.000423	0.716458
-1.523309	-1.978040	4.001280	0.000404	0.716457
-1.500823	-1.839253	4.011277	0.000400	0.716740
-1.380186	-1.851422	4.021274	0.000377	0.716758
-1.260968	-1.835655	4.031270	0.000355	0.716831
-0.779397	-1.791288	4.041267	0.000265	0.717089
-0.942668	-1.762124	4.051264	0.000296	0.717089
-0.783943	-1.687865	4.061261	0.000266	0.717292
-1.007935	-1.603190	4.071258	0.000308	0.717381
-1.076351	-1.497325	4.081254	0.000320	0.717566
-0.820701	-1.471577	4.091251	0.000273	0.717707
-0.661839	-1.393336	4.101248	0.000243	0.717918
-0.675461	-1.341387	4.111245	0.000245	0.718015
-0.650801	-1.189892	4.121242	0.000241	0.718323
-0.750257	-1.114473	4.131238	0.000259	0.718437
-0.655987	-1.025133	4.141235	0.000241	0.718647
-0.510097	-0.921589	4.151232	0.000214	0.718903
-0.255446	-0.880748	4.161229	0.000167	0.719073
-0.240377	-0.782398	4.171226	0.000164	0.719272
-0.383289	-0.599159	4.181222	0.000190	0.719583
-0.359012	-0.494802	4.191219	0.000186	0.719798
-0.289516	-0.387479	4.201216	0.000172	0.720034
-0.028985	-0.307866	4.211213	0.000124	0.720282
-0.102204	-0.161390	4.221210	0.000137	0.720545
-0.019052	-0.006852	4.231206	0.000122	0.720878
-0.008173	0.101080	4.241203	0.000120	0.721094
0.000000	0.249072	4.251200	0.000118	0.721388

-0.253684	0.924040	4.256205	0.000165	0.722626
-0.001093	2.144751	4.261210	0.000117	0.725106
0.464356	3.919480	4.266214	0.000029	0.728731
0.521224	6.316973	4.271219	0.000017	0.733403
1.088926	9.138435	4.276224	-0.000091	0.739034
1.344075	12.491703	4.281229	-0.000140	0.745528
1.510997	16.318354	4.286234	-0.000174	0.752830
1.914782	20.503267	4.291238	-0.000252	0.760808
2.444847	25.064018	4.296243	-0.000354	0.769438
2.872004	30.019140	4.301248	-0.000436	0.778657
3.250193	35.323211	4.306253	-0.000510	0.788380
3.567274	40.957501	4.311258	-0.000573	0.798552
4.112063	46.856105	4.316262	-0.000678	0.809131
4.525522	53.055678	4.321267	-0.000759	0.820053
4.754178	59.565596	4.326272	-0.000806	0.831305
5.219946	66.246366	4.331277	-0.000897	0.842765
5.653046	73.162742	4.336282	-0.000982	0.854452
6.031643	80.289862	4.341286	-0.001058	0.866311
6.452360	87.591173	4.346291	-0.001141	0.878303
11.069226	94.362219	4.351296	-0.002005	0.890463
13.077028	101.817912	4.356301	-0.002384	0.902813
13.310326	109.731921	4.361306	-0.002432	0.915222
14.136880	117.646260	4.366310	-0.002591	0.927625
14.826227	125.702842	4.371315	-0.002725	0.940042
15.529774	133.867900	4.376320	-0.002861	0.952462
16.520803	142.062585	4.381325	-0.003051	0.964839
17.265587	150.390156	4.386330	-0.003195	0.977189
17.955357	158.811339	4.391334	-0.003329	0.989505
19.187274	167.180740	4.396339	-0.003564	1.001730
19.971999	175.666842	4.401344	-0.003716	1.013860
20.681772	184.185309	4.406349	-0.003853	1.025874
21.471546	192.737221	4.411354	-0.004006	1.037812
22.368891	201.303890	4.416358	-0.004179	1.049660
23.110006	209.913408	4.421363	-0.004322	1.061396
23.778047	218.580090	4.426368	-0.004452	1.073062
24.508381	227.210442	4.431373	-0.004594	1.084569
25.329549	235.850734	4.436378	-0.004753	1.095987
25.843825	244.541732	4.441382	-0.004854	1.107285
26.372784	253.224835	4.446387	-0.004958	1.118461
27.117299	261.863327	4.451392	-0.005103	1.129517
27.775648	270.518247	4.456397	-0.005231	1.140468
28.484447	279.182277	4.461402	-0.005368	1.151336
29.260734	287.811347	4.466406	-0.005519	1.162073
30.456461	296.350032	4.471411	-0.005747	1.172689
31.176703	304.974475	4.476416	-0.005887	1.183214
31.871386	313.595710	4.481421	-0.006022	1.193638
32.258706	322.234097	4.486426	-0.006099	1.203929
33.264996	330.770303	4.491430	-0.006292	1.214137
33.839082	339.353172	4.496435	-0.006405	1.224228
34.569740	347.932789	4.501440	-0.006546	1.234263
35.281085	356.461588	4.506445	-0.006685	1.244155
35.898922	365.007047	4.511450	-0.006805	1.253970
36.492613	373.545274	4.516454	-0.006921	1.263695
36.963022	382.086164	4.521459	-0.007014	1.273326
37.540341	390.584678	4.526464	-0.007127	1.282857
38.026286	399.101073	4.531469	-0.007224	1.292320
38.674819	407.557332	4.536474	-0.007350	1.301679
39.377934	416.077707	4.541478	-0.007486	1.311050
39.899267	424.573387	4.546483	-0.007589	1.320294
40.588371	432.966992	4.551488	-0.007723	1.329396
40.959860	441.419396	4.556493	-0.007797	1.338441
41.276914	449.848918	4.561498	-0.007862	1.347392
41.749923	458.268306	4.566502	-0.007956	1.356300
42.427681	466.607362	4.571507	-0.008087	1.365101
43.163099	474.977101	4.576512	-0.008230	1.373888
43.639860	483.355380	4.581517	-0.008324	1.382583
44.256982	491.718549	4.586522	-0.008444	1.391232
44.841024	500.085359	4.591526	-0.008559	1.399825
45.172804	508.444844	4.596531	-0.008626	1.408316
45.961807	516.750845	4.601536	-0.008778	1.416779
46.350093	525.092754	4.606541	-0.008856	1.425160
46.705292	533.451970	4.611546	-0.008927	1.433505
47.467046	541.718653	4.616550	-0.009075	1.441775
47.800509	550.058752	4.621555	-0.009142	1.450001
48.328605	558.372502	4.626560	-0.009246	1.458186
48.791154	566.673278	4.631565	-0.009338	1.466302
49.237779	575.030510	4.636570	-0.009426	1.474425
50.248533	583.227588	4.641574	-0.009620	1.482439
50.663122	591.515239	4.646579	-0.009702	1.490402
51.408243	599.766249	4.651584	-0.009847	1.498340
52.008435	608.017815	4.656589	-0.009964	1.506213
52.167711	616.359074	4.661594	-0.009999	1.514062
52.625767	624.616436	4.666598	-0.010089	1.521838
52.947417	632.882727	4.671603	-0.010155	1.529562
53.288215	641.173254	4.676608	-0.010224	1.537272
54.048112	649.360619	4.681613	-0.010370	1.544911
54.733107	657.597697	4.686618	-0.010503	1.552546
55.353478	665.828048	4.691622	-0.010624	1.560128
55.761221	674.066576	4.696627	-0.010706	1.567650
56.360415	682.302169	4.701632	-0.010823	1.575161
57.053865	690.498461	4.706637	-0.010957	1.582614
57.221732	698.781906	4.711642	-0.010994	1.590034
57.967855	706.983329	4.716646	-0.011138	1.597430
58.572569	715.161316	4.721651	-0.011256	1.604750
58.855349	723.427076	4.726656	-0.011314	1.612069
59.320204	731.646106	4.731661	-0.011406	1.619339
59.682688	739.868296	4.736666	-0.011479	1.626565
60.102995	748.152124	4.741670	-0.011563	1.633821
60.336015	756.345475	4.746675	-0.011611	1.640940
61.068125	764.487894	4.751680	-0.011753	1.648053
61.957452	772.629272	4.756685	-0.011924	1.655156
62.326674	780.824661	4.761690	-0.011998	1.662203
62.947290	789.008550	4.766694	-0.012119	1.669245
63.401778	797.213228	4.771699	-0.012209	1.676253
63.774587	805.409120	4.776704	-0.012284	1.683212
64.235256	813.594550	4.781709	-0.012375	1.690146
64.518238	821.813018	4.786714	-0.012433	1.697056
65.094497	829.969456	4.791718	-0.012545	1.703924
65.678666	838.132363	4.796723	-0.012660	1.710771
66.081423	846.329153	4.801728	-0.012740	1.717594
66.658854	854.459873	4.806733	-0.012853	1.724359
66.970603	862.655326	4.811738	-0.012916	1.731117
67.251494	870.864624	4.816742	-0.012974	1.737855
67.623803	879.020248	4.821747	-0.013049	1.744535
68.016380	887.204567	4.826752	-0.013127	1.751215
68.369424	895.379459	4.831757	-0.013198	1.757857
68.742434	903.516213	4.836762	-0.013273	1.764446
69.285384	911.685421	4.841766	-0.013379	1.771057
69.750936	919.832510	4.846771	-0.013471	1.777616
70.232663	927.976590	4.851776	-0.013566	1.784151
70.906475	936.130099	4.856781	-0.013697	1.790693
71.382904	944.303894	4.861786	-0.013791	1.797202
71.756820	952.443748	4.866790	-0.013866	1.803649
72.137474	960.570963	4.871795	-0.013942	1.810064
72.574258	968.713126	4.876800	-0.014029	1.816474
72.893683	976.863808	4.881805	-0.014094	1.822854
73.110666	985.029310	4.886810	-0.014140	1.829211
73.774672	993.147803	4.891814	-0.014268	1.835563
74.278539	1001.251840	4.896819	-0.014368	1.841862
74.879818	1009.369172	4.901824	-0.014485	1.848162
75.453899	1017.513636	4.906829	-0.014597	1.854457
75.606925	1025.683069	4.911834	-0.014631	1.860701
76.045288	1033.824972	4.916838	-0.014718	1.866937
76.303842	1041.999664	4.921843	-0.014771	1.873155
76.732510	1050.119691	4.926848	-0.014856	1.879331
77.119230	1058.231441	4.931853	-0.014934	1.885476
77.250297	1066.398679	4.936858	-0.014964	1.891613
77.810333	1074.504633	4.941862	-0.015073	1.897733
78.145857	1082.610237	4.946867	-0.015141	1.903808
78.234638	1090.792692	4.951872	-0.015163	1.909892
78.608752	1098.915296	4.956877	-0.015238	1.915945
79.056928	1106.991287	4.961882	-0.015326	1.921952
79.424581	1115.120205	4.966886	-0.015400	1.927971
79.567458	1123.285064	4.971891	-0.015432	1.933972
80.324304	1131.338334	4.976896	-0.015578	1.939941
80.762205	1139.457072	4.981901	-0.015665	1.945904
81.090828	1147.619882	4.986906	-0.015732	1.951868
81.456231	1155.761215	4.991910	-0.015805	1.957803
81.714084	1163.842552	4.996915	-0.015858	1.963665
81.895875	1171.978328	5.001920	-0.015898	1.969540
82.170737	1180.098972	5.006925	-0.015954	1.975397
82.643060	1188.162308	5.011930	-0.016047	1.981217
83.154783	1196.257927	5.016934	-0.016148	1.987046
83.434873	1204.379905	5.021939	-0.016205	1.992853
83.749248	1212.495165	5.026944	-0.016269	1.998641
84.193175	1220.561301	5.031949	-0.016357	2.004392
84.561281	1228.669311	5.036954	-0.016431	2.010148
84.832337	1236.808790	5.041958	-0.016487	2.015899
85.322327	1244.878768	5.046963	-0.016583	2.021607
85.534692	1253.003539	5.051968	-0.016628	2.027309
85.966871	1261.132671	5.056973	-0.016714	2.033021
86.126814	1269.249310	5.061978	-0.016749	2.038680
86.548154	1277.322284	5.066982	-0.016833	2.044319
86.915286	1285.415008	5.071987	-0.016906	2.049951
87.309238	1293.520929	5.076992	-0.016985	2.055580
87.710637	1301.606251	5.081997	-0.017065	2.061179
87.785928	1309.726220	5.087002	-0.017084	2.066754
88.206941	1317.836481	5.092006	-0.017168	2.072343
88.918561	1325.875058	5.097011	-0.017306	2.077895
89.239317	1333.978358	5.102016	-0.017371	2.083439
89.300274	1342.122147	5.107021	-0.017388	2.088969
89.822647	1350.182252	5.112026	-0.017490	2.094473
90.220209	1358.274665	5.117030	-0.017569	2.099973
90.186886	1366.412440	5.122035	-0.017569	2.105446
90.599243	1374.531170	5.127040	-0.017651	2.110936
90.940113	1382.653208	5.132045	-0.017719	2.116407
91.049166	1390.726977	5.137050	-0.017745	2.121809
91.249247	1398.824505	5.142054	-0.017788	2.127222
91.580713	1406.888178	5.147059	-0.017855	2.132611
91.812380	1414.973165	5.152064	-0.017903	2.137991
92.248818	1423.027121	5.157069	-0.017990	2.143356
92.754395	1431.087909	5.162074	-0.018089	2.148719
93.335300	1439.187927	5.167078	-0.018202	2.154101
93.261876	1447.302279	5.172083	-0.018194	2.159418
93.624776	1455.365533	5.177088	-0.018267	2.164729
94.253426	1463.420604	5.182093	-0.018389	2.170046
94.320378	1471.558037	5.187098	-0.018407	2.175352
94.639052	1479.638757	5.192102	-0.018472	2.180631
95.009432	1487.699902	5.197107	-0.018546	2.185889
95.550378	1495.784631	5.202112	-0.018652	2.191166
95.939198	1503.882183	5.207117	-0.018730	2.196424
96.309917	1511.917708	5.212122	-0.018804	2.201628
96.701370	1520.005883	5.217126	-0.018882	2.206855
96.686073	1528.135677	5.222131	-0.018885	2.212059
97.136208	1536.192498	5.227136	-0.018974	2.217247
97.307082	1544.287151	5.232141	-0.019011	2.222422
97.622781	1552.341910	5.237146	-0.019075	2.227572
97.912616	1560.464254	5.242150	-0.019134	2.232750
98.303677	1568.507323	5.247155	-0.019212	2.237876
98.524913	1576.589872	5.252160	-0.019259	2.242999
98.896590	1584.658433	5.257165	-0.019333	2.248115
99.245689	1592.740345	5.262170	-0.019403	2.253226
99.708476	1600.795903	5.267174	-0.019495	2.258319
99.686038	1608.909401	5.272179	-0.019496	2.263394
99.919830	1616.990055	5.277184	-0.019545	2.268460
100.397357	1625.130955	5.282189	-0.019639	2.273572
100.765525	1633.154044	5.287194	-0.019713	2.278591
101.117566	1641.211176	5.292198	-0.019784	2.283618
101.576168	1649.253696	5.297203	-0.019874	2.288634
101.789875	1657.344877	5.302208	-0.019919	2.293648
101.915346	1665.435873	5.307213	-0.019948	2.298643
102.064338	1673.489231	5.312218	-0.019981	2.303607
102.574312	1681.538345	5.317222	-0.020081	2.308587
103.049997	1689.597134	5.322227	-0.020175	2.313560
103.384879	1697.654220	5.327232	-0.020243	2.318509
103.878717	1705.711934	5.332237	-0.020340	2.323461
103.774085	1713.824326	5.337242	-0.020326	2.328386
104.309201	1721.892752	5.342246	-0.020431	2.333327
104.467619	1729.975418	5.347251	-0.020465	2.338235
104.913325	1738.010591	5.352256	-0.020554	2.343128
105.322901	1746.085648	5.357261	-0.020635	2.348031
105.473996	1754.200394	5.362266	-0.020669	2.352927
106.015195	1762.237280	5.367270	-0.020775	2.357797
105.973995	1770.331168	5.372275	-0.020772	2.362645
106.299365	1778.375804	5.377280	-0.020838	2.367482
106.813851	1786.438116	5.382285	-0.020939	2.372335
107.277363	1794.464591	5.387290	-0.021031	2.377153
107.455805	1802.563531	5.392294	-0.021069	2.381982
107.631633	1810.642243	5.397299	-0.021107	2.386788
108.069047	1818.694189	5.402304	-0.021194	2.391589
108.499954	1826.767718	5.407309	-0.021280	2.396393
108.971753	1834.767487	5.412314	-0.021373	2.401147
109.471014	1842.830756	5.417318	-0.021471	2.405931
109.950528	1850.882974	5.422323	-0.021565	2.410698
110.276514	1858.983307	5.427328	-0.021631	2.415471
110.597288	1867.066653	5.432333	-0.021696	2.420224
110.740160	1875.120614	5.437338	-0.021728	2.424937
110.747778	1883.239872	5.442342	-0.021735	2.429669
111.211485	1891.365815	5.447347	-0.021827	2.434430
111.279259	1899.408600	5.452352	-0.021845	2.439103
111.579321	1907.432782	5.457357	-0.021906	2.443774
111.595800	1915.499523	5.462362	-0.021914	2.448439
111.998051	1923.551079	5.467366	-0.021994	2.453116
112.440311	1931.569622	5.472371	-0.022082	2.457768
112.865302	1939.592862	5.477376	-0.022166	2.462412
113.169639	1947.675615	5.482381	-0.022228	2.467072
113.443512	1955.736362	5.487386	-0.022284	2.471709
113.704510	1963.822580	5.492390	-0.022338	2.476351
114.207647	1971.832132	5.497395	-0.022437	2.480958
114.399955	1979.889858	5.502400	-0.022478	2.485561
114.559223	1987.975183	5.507405	-0.022513	2.490169
114.960139	1996.035495	5.512410	-0.022593	2.494771
115.244955	2004.100306	5.517414	-0.022652	2.499359
115.599030	2012.123091	5.522419	-0.022723	2.503920
115.657850	2020.242819	5.527424	-0.022739	2.508506
115.921129	2028.345592	5.532429	-0.022793	2.513089
116.224257	2036.358159	5.537434	-0.022855	2.517615
116.541172	2044.402785	5.542438	-0.022919	2.522152
117.006167	2052.415242	5.547443	-0.023011	2.526674
117.294965	2060.476344	5.552448	-0.023070	2.531202
117.572429	2068.571993	5.557453	-0.023127	2.535740
117.711165	2076.613644	5.562458	-0.023158	2.540230
118.211345	2084.652254	5.567462	-0.023257	2.544737
118.588362	2092.699419	5.572467	-0.023332	2.549231
118.731617	2100.797463	5.577472	-0.023364	2.553729
119.150174	2108.847880	5.582477	-0.023447	2.558211
119.266059	2116.883932	5.587482	-0.023474	2.562657
119.501465	2124.952361	5.592486	-0.023523	2.567122
120.011431	2132.986727	5.597491	-0.023623	2.571578
120.261607	2141.060677	5.602496	-0.023675	2.576031
120.411814	2149.126290	5.607501	-0.023708	2.580465
120.589127	2157.145680	5.612506	-0.023747	2.584867
120.797894	2165.224084	5.617510	-0.023791	2.589297
121.018226	2173.471365	5.622515	-0.023837	2.593811
121.291219	2181.463526	5.627520	-0.023893	2.598183
121.679233	2189.441463	5.632525	-0.023971	2.602547
121.939162	2197.430856	5.637530	-0.024024	2.606901
122.436637	2205.475147	5.642534	-0.024122	2.611294
122.494570	2213.537628	5.647539	-0.024138	2.615659
122.976183	2221.540259	5.652544	-0.024233	2.620013
123.207233	2229.573321	5.657549	-0.024282	2.624360
123.386586	2237.638718	5.662554	-0.024320	2.628713
123.538779	2245.739268	5.667558	-0.024354	2.633076
123.680261	2253.789735	5.672563	-0.024386	2.637405
123.957028	2261.807709	5.677568	-0.024442	2.641717
124.282589	2269.851954	5.682573	-0.024508	2.646040
124.491332	2277.888765	5.687578	-0.024552	2.650345
124.713067	2285.982028	5.692582	-0.024599	2.654673
124.914937	2294.010035	5.697587	-0.024642	2.658957
125.176799	2302.046149	5.702592	-0.024696	2.663244
125.387391	2310.123416	5.707597	-0.024740	2.667541
125.519189	2318.186254	5.712602	-0.024770	2.671820
126.033171	2326.241095	5.717606	-0.024871	2.676111
126.279735	2334.250443	5.722611	-0.024922	2.680354
126.631410	2342.240345	5.727616	-0.024993	2.684588
126.794797	2350.316305	5.732621	-0.025029	2.688847
127.178752	2358.353578	5.737626	-0.025105	2.693094
127.561490	2366.409276	5.742630	-0.025182	2.697343
127.486999	2374.488158	5.747635	-0.025173	2.701569
127.795037	2382.505033	5.752640	-0.025236	2.705780
128.282645	2390.553752	5.757645	-0.025332	2.710012
128.337050	2398.628833	5.762650	-0.025347	2.714224
128.840989	2406.633958	5.767654	-0.025446	2.718422
128.926208	2414.696298	5.772659	-0.025468	2.722616
128.975983	2422.750659	5.777664	-0.025482	2.726798
129.302977	2430.815818	5.782669	-0.025548	2.730996
129.462987	2438.868704	5.787674	-0.025583	2.735170
129.826939	2446.887434	5.792678	-0.025656	2.739333
130.010178	2454.927844	5.797683	-0.025696	2.743490
130.516355	2462.959403	5.802688	-0.025795	2.747656
130.927436	2471.049916	5.807693	-0.025877	2.751840
130.946944	2479.158915	5.812698	-0.025886	2.756003
130.966645	2487.197870	5.817702	-0.025895	2.760124
131.242747	2495.169923	5.822707	-0.025952	2.764220
131.403239	2503.231102	5.827712	-0.025987	2.768349
131.819986	2511.274441	5.832717	-0.026070	2.772477
132.029012	2519.308884	5.837722	-0.026114	2.776583
132.064535	2527.370657	5.842726	-0.026126	2.780686
132.252241	2535.381135	5.847731	-0.026166	2.784765
132.417023	2543.428930	5.852736	-0.026202	2.788857
132.679376	2551.511874	5.857741	-0.026256	2.792966
132.770957	2559.545715	5.862746	-0.026278	2.797034
133.326049	2567.527827	5.867750	-0.026387	2.801097
133.487278	2575.565443	5.872755	-0.026422	2.805159
133.896926	2583.597355	5.877760	-0.026504	2.809226
134.112686	2591.683954	5.882765	-0.026549	2.813304
134.362457	2599.701338	5.887770	-0.026601	2.817344
134.777479	2607.728883	5.892774	-0.026683	2.821392
134.908792	2615.788177	5.897779	-0.026713	2.825433
135.288323	2623.824487	5.902784	-0.026789	2.829472
135.843095	2631.875672	5.907789	-0.026898	2.833522
135.952096	2639.924877	5.912794	-0.026923	2.837540
136.233401	2647.974764	5.917798	-0.026981	2.841563
136.441268	2655.981063	5.922803	-0.027025	2.845553
136.684504	2664.024303	5.927808	-0.027075	2.849559
136.905907	2672.100383	5.932813	-0.027122	2.853574
137.093345	2680.142561	5.937818	-0.027162	2.857564
137.472273	2688.171353	5.942822	-0.027238	2.861553
137.616699	2696.208188	5.947827	-0.027270	2.865528
137.848880	2704.236270	5.952832	-0.027318	2.869497
138.080496	2712.332164	5.957837	-0.027367	2.873494
138.401545	2720.318212	5.962842	-0.027432	2.877437
138.758825	2728.353361	5.967846	-0.027504	2.881400
138.953240	2736.393074	5.972851	-0.027545	2.885350
139.219816	2744.399502	5.977856	-0.027600	2.889284
139.384209	2752.498659	5.982861	-0.027636	2.893251
139.588049	2760.547687	5.987866	-0.027679	2.897191
140.089090	2768.546039	5.992870	-0.027778	2.901116
140.355243	2776.594944	5.997875	-0.027832	2.905048
140.520746	2784.639016	6.002880	-0.027868	2.908967
140.920682	2792.769899	6.007885	-0.027948	2.912936
141.053940	2800.793833	6.012890	-0.027978	2.916833
141.227677	2808.831879	6.017894	-0.028016	2.920733
141.463629	2816.808044	6.022899	-0.028065	2.924602
141.673168	2824.841791	6.027904	-0.028109	2.928492
142.023956	2832.886471	6.032909	-0.028180	2.932390
142.132420	2840.932123	6.037914	-0.028205	2.936270
142.545366	2848.961211	6.042918	-0.028288	2.940153
142.736441	2856.974492	6.047923	-0.028328	2.944011
142.743195	2865.026188	6.052928	-0.028335	2.947873
143.290877	2873.082110	6.057933	-0.028442	2.951760
143.499311	2881.135955	6.062938	-0.028486	2.955624
143.553881	2889.160150	6.067942	-0.028502	2.959460
143.670845	2897.194627	6.072947	-0.028529	2.963300
143.759363	2905.235438	6.077952	-0.028550	2.967136
144.037325	2913.270993	6.082957	-0.028607	2.970974
144.261531	2921.313644	6.087962	-0.028654	2.974808
144.551473	2929.320942	6.092966	-0.028714	2.978623
144.664493	2937.374666	6.097971	-0.028740	2.982447
144.770008	2945.413197	6.102976	-0.028765	2.986258
144.968697	2953.466696	6.107981	-0.028807	2.990076
145.308355	2961.510360	6.112986	-0.028876	2.993891
145.591868	2969.513447	6.117990	-0.028934	2.997680
145.709281	2977.547015	6.122995	-0.028961	3.001469
145.932385	2985.552432	6.128000	-0.029008	3.005246
146.122072	2993.599489	6.133005	-0.029048	3.009036
146.310252	3001.657622	6.138010	-0.029088	3.012827
146.615619	3009.704387	6.143014	-0.029151	3.016613
146.660321	3017.744662	6.148019	-0.029164	3.020378
146.720846	3025.755257	6.153024	-0.029181	3.024126
147.066574	3033.816340	6.158029	-0.029250	3.027906
147.379643	3041.832799	6.163034	-0.029314	3.031660
147.589179	3049.878839	6.168038	-0.029358	3.035417
147.841096	3057.896989	6.173043	-0.029410	3.039159
148.240914	3065.885641	6.178048	-0.029490	3.042889
148.408957	3073.967504	6.183053	-0.029527	3.046647
148.494605	3082.004570	6.188058	-0.029548	3.050376
148.868390	3090.058312	6.193062	-0.029623	3.054121
149.325547	3098.079789	6.198067	-0.029713	3.057851
149.284291	3106.113014	6.203072	-0.029711	3.061558
149.548027	3114.145072	6.208077	-0.029765	3.065275
149.848295	3122.158872	6.213082	-0.029826	3.068980
150.050930	3130.297728	6.218086	-0.029869	3.072733
150.144717	3138.344860	6.223091	-0.029892	3.076435
150.331635	3146.299705	6.228096	-0.029932	3.080094
150.780291	3154.309822	6.233101	-0.030021	3.083787
150.800618	3162.330804	6.238106	-0.030030	3.087460
151.203090	3170.358293	6.243110	-0.030110	3.091149
151.348865	3178.417351	6.248115	-0.030142	3.094837
151.613216	3186.415967	6.253120	-0.030197	3.098497
151.776429	3194.485758	6.258125	-0.030232	3.102182
151.998028	3202.509274	6.263130	-0.030279	3.105843
152.003224	3210.549586	6.268134	-0.030285	3.109498
152.284304	3218.615180	6.273139	-0.030343	3.113173
152.505579	3226.630280	6.278144	-0.030389	3.116817
152.859367	3234.637568	6.283149	-0.030460	3.120460
152.765267	3242.675362	6.288154	-0.030448	3.124092
153.017958	3250.719237	6.293158	-0.030500	3.127738
153.573191	3258.732352	6.298163	-0.030609	3.131380
153.606199	3266.783032	6.303168	-0.030620	3.135011
154.033411	3274.793165	6.308173	-0.030705	3.138637
154.394236	3282.803331	6.313178	-0.030778	3.142255
154.520721	3290.861193	6.318182	-0.030806	3.145881
154.562282	3298.897053	6.323187	-0.030819	3.149489
154.982608	3306.965798	6.328192	-0.030903	3.153124
155.347353	3314.982507	6.333197	-0.030976	3.156729
155.455069	3323.002136	6.338202	-0.031001	3.160320
155.792340	3330.990480	6.343206	-0.031069	3.163902
156.048197	3339.047053	6.348211	-0.031122	3.167508
156.123655	3347.076409	6.353216	-0.031142	3.171090
156.534674	3355.158299	6.358221	-0.031223	3.174705
156.685125	3363.150355	6.363226	-0.031257	3.178265
156.647121	3371.223719	6.368230	-0.031255	3.181849
156.676049	3379.246243	6.373235	-0.031266	3.185409
156.964504	3387.244465	6.378240	-0.031324	3.188966
157.344666	3395.310050	6.383245	-0.031401	3.192552
157.371409	3403.354295	6.388250	-0.031411	3.196110
157.863350	3411.321543	6.393254	-0.031508	3.199649
158.368578	3419.339795	6.398259	-0.031607	3.203208
158.500966	3427.361426	6.403264	-0.031637	3.206748
158.770323	3435.437948	6.408269	-0.031692	3.210314
158.874613	3443.497248	6.413274	-0.031717	3.213862
159.177285	3451.497758	6.418278	-0.031779	3.217389
159.377945	3459.545980	6.423283	-0.031821	3.220928
159.796012	3467.507931	6.428288	-0.031904	3.224434
160.158877	3475.590252	6.433293	-0.031977	3.227987
160.102785	3483.685775	6.438298	-0.031972	3.231524
160.400264	3491.732891	6.443302	-0.032033	3.235051
160.684267	3499.700700	6.448307	-0.032091	3.238539
160.864346	3507.696921	6.453312	-0.032129	3.242031
160.919841	3515.744965	6.458317	-0.032145	3.245538
161.061086	3523.755035	6.463322	-0.032177	3.249027
161.592083	3531.791067	6.468326	-0.032281	3.252539
161.633663	3539.866685	6.473331	-0.032294	3.256045
161.684852	3547.865119	6.478336	-0.032308	3.259514
162.150403	3555.883199	6.483341	-0.032400	3.263004
162.193131	3563.929976	6.488346	-0.032414	3.266487
162.334284	3571.969883	6.493350	-0.032445	3.269966
162.723446	3580.027697	6.498355	-0.032523	3.273459
162.727489	3588.038011	6.503360	-0.032529	3.276913
162.905472	3596.056975	6.508365	-0.032567	3.280374
163.082077	3604.031626	6.513370	-0.032605	3.283812
163.338245	3612.088946	6.518374	-0.032658	3.287285
163.556258	3620.111790	6.523379	-0.032704	3.290738
163.919951	3628.144648	6.528384	-0.032777	3.294197
163.941204	3636.208090	6.533389	-0.032786	3.297652
164.119096	3644.222931	6.538394	-0.032825	3.301089
164.271476	3652.202466	6.543398	-0.032858	3.304507
164.651490	3660.273187	6.548403	-0.032934	3.307968
164.921973	3668.316164	6.553408	-0.032990	3.311410
165.103697	3676.381381	6.558413	-0.033029	3.314854
165.060636	3684.383998	6.563418	-0.033026	3.318260
165.365286	3692.388355	6.568422	-0.033088	3.321675
165.512902	3700.411999	6.573427	-0.033121	3.325090
165.660557	3708.424094	6.578432	-0.033154	3.328496
166.092275	3716.475547	6.583437	-0.033239	3.331926
166.292721	3724.521091	6.588442	-0.033282	3.335341
166.465181	3732.527228	6.593446	-0.033319	3.338735
166.871340	3740.549320	6.598451	-0.033400	3.342141
167.205892	3748.569748	6.603456	-0.033468	3.345540
167.564878	3756.588974	6.608461	-0.033540	3.348935
167.694004	3764.648273	6.613466	-0.033569	3.352336
167.923325	3772.684911	6.618470	-0.033617	3.355728
168.015850	3780.718557	6.623475	-0.033640	3.359109
168.019655	3788.736748	6.628480	-0.033646	3.362478
168.547081	3796.779108	6.633485	-0.033749	3.365872
168.728004	3804.777544	6.638490	-0.033788	3.369232
168.728882	3812.835226	6.643494	-0.033793	3.372607
168.855958	3820.892476	6.648499	-0.033822	3.375983
169.083427	3828.867126	6.653504	-0.033870	3.379324
169.443649	3836.881164	6.658509	-0.033942	3.382684
169.526147	3844.927589	6.663514	-0.033963	3.386043
169.656792	3852.938265	6.668518	-0.033992	3.389386
169.838455	3861.077164	6.673523	-0.034032	3.392781
169.936781	3869.103640	6.678528	-0.034055	3.396123
170.227640	3877.039996	6.683533	-0.034114	3.399431
170.323985	3885.071225	6.688538	-0.034138	3.402768
170.607345	3893.080476	6.693542	-0.034196	3.406099
170.745945	3901.090155	6.698547	-0.034227	3.409422
170.887892	3909.124046	6.703552	-0.034258	3.412752
171.195977	3917.164936	6.708557	-0.034321	3.416087
171.297068	3925.165157	6.713562	-0.034345	3.419395
171.636236	3933.195178	6.718566	-0.034414	3.422721
172.061799	3941.208642	6.723571	-0.034498	3.426039
171.971603	3949.257241	6.728576	-0.034486	3.429350
172.369919	3957.304713	6.733581	-0.034566	3.432675
172.519602	3965.332617	6.738586	-0.034599	3.435980
172.640156	3973.333431	6.743590	-0.034627	3.439270
172.853744	3981.336690	6.748595	-0.034672	3.442560
172.945460	3989.395700	6.753600	-0.034694	3.445866
173.238090	3997.417260	6.758605	-0.034754	3.449161
173.413372	4005.496570	6.763610	-0.034792	3.452472
173.482017	4013.522762	6.768614	-0.034810	3.455754
173.879768	4021.537076	6.773619	-0.034889	3.459039
173.886985	4029.546080	6.778624	-0.034896	3.462307
173.950213	4037.600337	6.783629	-0.034913	3.465591
174.220787	4045.587433	6.788634	-0.034968	3.468852
174.550606	4053.638897	6.793638	-0.035035	3.472137
174.675083	4061.705217	6.798643	-0.035063	3.475419
174.840520	4069.678274	6.803648	-0.035099	3.478661
175.164101	4077.693343	6.808653	-0.035165	3.481922
175.148215	4085.705048	6.813658	-0.035167	3.485168
175.553208	4093.719704	6.818662	-0.035248	3.488426
175.748420	4101.782426	6.823667	-0.035289	3.491693
175.762831	4109.798135	6.828672	-0.035297	3.494932
175.934603	4117.795096	6.833677	-0.035335	3.498166
176.302819	4125.826857	6.838682	-0.035408	3.501417
176.379374	4133.842381	6.843686	-0.035428	3.504649
176.471898	4141.891266	6.848691	-0.035450	3.507893
176.953704	4149.909831	6.853696	-0.035545	3.511133
177.230935	4157.944789	6.858701	-0.035602	3.514370
177.219557	4165.959664	6.863706	-0.035605	3.517587
177.442344	4173.995867	6.868710	-0.035652	3.520817
177.750169	4181.980056	6.873715	-0.035715	3.524026
177.685282	4190.032068	6.878720	-0.035708	3.527247
178.059091	4198.075245	6.883725	-0.035783	3.530476
178.256393	4206.109647	6.888730	-0.035825	3.533692
178.196859	4214.144295	6.893734	-0.035819	3.536898
178.560170	4222.159009	6.898739	-0.035892	3.540106
178.714051	4230.170278	6.903744	-0.035926	3.543304
178.910095	4238.231195	6.908749	-0.035967	3.546519
179.105533	4246.255600	6.913754	-0.036009	3.549717
179.282308	4254.350031	6.918758	-0.036047	3.552939
179.622945	4262.401938	6.923763	-0.036116	3.556146
179.545964	4270.327744	6.928768	-0.036107	3.559288
179.665828	4278.375966	6.933773	-0.036134	3.562482
179.838060	4286.376335	6.938778	-0.036172	3.565655
180.132054	4294.344944	6.943782	-0.036232	3.568816
180.337429	4302.415769	6.948787	-0.036275	3.572013
180.513938	4310.417744	6.953792	-0.036313	3.575178
180.737422	4318.434546	6.958797	-0.036360	3.578348
181.003804	4326.466529	6.963802	-0.036415	3.581522
181.269457	4334.448724	6.968806	-0.036470	3.584673
181.516663	4342.517983	6.973811	-0.036521	3.587856
181.542163	4350.558133	6.978816	-0.036531	3.591018
181.927635	4358.569881	6.983821	-0.036608	3.594176
182.042380	4366.594805	6.988826	-0.036635	3.597329
182.296103	4374.572253	6.993830	-0.036687	3.600465
182.458345	4382.593615	6.998835	-0.036723	3.603612
182.714614	4390.618553	7.003840	-0.036776	3.606760
183.174311	4398.651322	7.008845	-0.036866	3.609915
183.420507	4406.687302	7.013850	-0.036917	3.613062
183.277153	4414.758775	7.018854	-0.036896	3.616209
183.620971	4422.762804	7.023859	-0.036965	3.619341
183.669847	4430.785870	7.028864	-0.036980	3.622469
183.888392	4438.795170	7.033869	-0.037026	3.625594
184.026781	4446.816292	7.038874	-0.037057	3.628718
184.166205	4454.845127	7.043878	-0.037088	3.631843
184.409960	4462.934804	7.048883	-0.037138	3.634992
184.776368	4470.887878	7.053888	-0.037212	3.638088
184.983428	4478.945124	7.058893	-0.037256	3.641217
185.197313	4486.923466	7.063898	-0.037301	3.644314
185.429817	4494.956639	7.068902	-0.037349	3.647429
186.056679	4502.980228	7.073907	-0.037471	3.650549
186.121653	4511.007385	7.078912	-0.037489	3.653652
186.242339	4519.078862	7.083917	-0.037516	3.656771
186.363464	4527.069812	7.088922	-0.037544	3.659857
186.660933	4535.075051	7.093926	-0.037605	3.662950
186.938120	4543.133991	7.098931	-0.037662	3.666060
187.046655	4551.129291	7.103936	-0.037687	3.669139
187.400145	4559.188010	7.108941	-0.037758	3.672246
187.664368	4567.204409	7.113946	-0.037813	3.675332
187.750054	4575.185895	7.118950	-0.037834	3.678397
188.213037	4583.249115	7.123955	-0.037925	3.681501
188.298331	4591.204241	7.128960	-0.037946	3.684550
188.597925	4599.275819	7.133965	-0.038007	3.687648
188.550473	4607.324180	7.138970	-0.038004	3.690725
188.893304	4615.318381	7.143974	-0.038073	3.693788
189.055277	4623.382795	7.148979	-0.038108	3.696872
189.008580	4631.372724	7.153984	-0.038105	3.699919
189.420023	4639.367160	7.158989	-0.038187	3.702976
189.602532	4647.417743	7.163994	-0.038226	3.706047
189.728732	4655.403242	7.168998	-0.038255	3.709089
190.145572	4663.498934	7.174003	-0.038338	3.712178
190.212337	4671.583049	7.179008	-0.038355	3.715251
190.265815	4679.556271	7.184013	-0.038371	3.718279
190.363231	4687.554614	7.189018	-0.038394	3.721315
190.581546	4695.502360	7.194022	-0.038440	3.724333
190.772936	4703.575491	7.199027	-0.038481	3.727394
190.938126	4711.562914	7.204032	-0.038517	3.730420
191.322730	4719.613221	7.209037	-0.038594	3.733473
191.408305	4727.682569	7.214042	-0.038615	3.736523
191.430628	4735.638415	7.219046	-0.038624	3.739527
191.796503	4743.669375	7.224051	-0.038698	3.742564
191.930127	4751.685922	7.229056	-0.038728	3.745588
192.140803	4759.724115	7.234061	-0.038772	3.748620
192.207011	4767.772919	7.239066	-0.038790	3.751649
192.476518	4775.784088	7.244070	-0.038845	3.754667
192.645506	4783.798061	7.249075	-0.038882	3.757681
192.918670	4791.786333	7.254080	-0.038938	3.760685
192.995982	4799.847285	7.259085	-0.038958	3.763710
193.176786	4807.868417	7.264090	-0.038997	3.766719
193.314303	4815.854478	7.269094	-0.039027	3.769712
193.536986	4823.942793	7.274099	-0.039074	3.772743
193.558192	4831.952175	7.279104	-0.039083	3.775738
193.788487	4839.957801	7.284109	-0.039131	3.778733
193.973177	4847.995231	7.289114	-0.039171	3.781737
194.238466	4855.968968	7.294118	-0.039226	3.784716
194.402776	4864.050714	7.299123	-0.039262	3.787731
194.573079	4872.037114	7.304128	-0.039298	3.790708
195.124837	4880.137321	7.309133	-0.039407	3.793733
195.197970	4888.149939	7.314138	-0.039425	3.796713
195.060009	4896.106523	7.319142	-0.039405	3.799666
195.229765	4904.129385	7.324147	-0.039442	3.802647
195.594325	4912.086551	7.329152	-0.039515	3.805605
195.646584	4920.168647	7.334157	-0.039530	3.808601
195.721502	4928.202672	7.339162	-0.039549	3.811578
195.822489	4936.239813	7.344166	-0.039573	3.814553
195.989590	4944.254105	7.349171	-0.039609	3.817519
196.341018	4952.213339	7.354176	-0.039680	3.820467
196.651893	4960.261600	7.359181	-0.039743	3.823444
196.747974	4968.289635	7.364186	-0.039766	3.826407
196.824507	4976.285225	7.369190	-0.039786	3.829355
197.055337	4984.358807	7.374195	-0.039834	3.832333
196.951984	4992.375403	7.379200	-0.039820	3.835280
197.319435	5000.374901	7.384205	-0.039894	3.838229
197.430708	5008.400255	7.389210	-0.039920	3.841179
197.848569	5016.349955	7.394214	-0.040003	3.844106
198.044753	5024.423038	7.399219	-0.040045	3.847072
198.098814	5032.443051	7.404224	-0.040060	3.850012
198.292057	5040.465755	7.409229	-0.040101	3.852954
198.407490	5048.556171	7.414234	-0.040128	3.855917
198.496864	5056.505694	7.419238	-0.040150	3.858826
198.583031	5064.585374	7.424243	-0.040171	3.861780
198.842418	5072.535194	7.429248	-0.040225	3.864688
199.149007	5080.614381	7.434253	-0.040287	3.867642
199.276868	5088.660776	7.439258	-0.040316	3.870578
199.409135	5096.844282	7.444262	-0.040346	3.873561
199.649651	5104.871296	7.449267	-0.040396	3.876488
199.735008	5112.703324	7.454272	-0.040417	3.879338
200.006976	5120.786359	7.459277	-0.040473	3.882282
200.156476	5128.720523	7.464282	-0.040506	3.885166
200.213530	5136.738728	7.469286	-0.040522	3.888077
200.519282	5144.791121	7.474291	-0.040584	3.891003
200.599882	5152.818518	7.479296	-0.040604	3.893913
200.852259	5160.832567	7.484301	-0.040657	3.896820
200.902988	5168.808912	7.489306	-0.040671	3.899707
201.022706	5176.842876	7.494310	-0.040699	3.902614
201.300443	5184.864286	7.499315	-0.040756	3.905517
201.311304	5192.895255	7.504320	-0.040763	3.908416
201.555327	5200.915819	7.509325	-0.040814	3.911314
201.914705	5208.953832	7.514330	-0.040886	3.914218
201.883211	5216.959931	7.519334	-0.040885	3.917101
202.039944	5224.976188	7.524339	-0.040920	3.919989
202.392934	5232.949363	7.529344	-0.040991	3.922864
202.686807	5240.971515	7.534349	-0.041051	3.925752
202.658438	5249.020336	7.539354	-0.041051	3.928642
202.682349	5257.065485	7.544358	-0.041060	3.931530
202.882397	5265.119930	7.549363	-0.041103	3.934421
203.064533	5273.086287	7.554368	-0.041142	3.937279
203.172304	5281.090126	7.559373	-0.041167	3.940147
203.460763	5289.090896	7.564378	-0.041226	3.943015
203.827190	5297.117358	7.569382	-0.041300	3.945891
203.780165	5305.185898	7.574387	-0.041296	3.948773
203.778122	5313.187260	7.579392	-0.041301	3.951630
203.895433	5321.246376	7.584397	-0.041328	3.954507
204.064792	5329.232673	7.589402	-0.041365	3.957357
204.227886	5337.197933	7.594406	-0.041401	3.960198
204.495084	5345.228892	7.599411	-0.041456	3.963061
204.531036	5353.235614	7.604416	-0.041467	3.965910
204.664274	5361.227651	7.609421	-0.041497	3.968753
205.014808	5369.318888	7.614426	-0.041568	3.971633
205.295229	5377.303336	7.619430	-0.041625	3.974472
205.521011	5385.378084	7.624435	-0.041673	3.977340
205.452682	5393.354519	7.629440	-0.041665	3.980166
205.726338	5401.392894	7.634445	-0.041722	3.983018
205.917764	5409.414514	7.639450	-0.041762	3.985860
206.052484	5417.413675	7.644454	-0.041793	3.988691
206.537172	5425.499607	7.649459	-0.041888	3.991557
206.628811	5433.486739	7.654464	-0.041911	3.994379
206.720424	5441.541513	7.659469	-0.041933	3.997223
206.881206	5449.512126	7.664474	-0.041968	4.000037
206.954684	5457.538477	7.669478	-0.041987	4.002867
207.318257	5465.568057	7.674483	-0.042060	4.005700
207.190744	5473.575030	7.679488	-0.042041	4.008516
207.574492	5481.630363	7.684493	-0.042118	4.011355
207.739208	5489.678251	7.689498	-0.042154	4.014186
207.950317	5497.667578	7.694502	-0.042199	4.016994
208.284395	5505.696306	7.699507	-0.042266	4.019817
208.313078	5513.698870	7.704512	-0.042277	4.022624
208.254776	5521.710860	7.709517	-0.042271	4.025430
208.732635	5529.737991	7.714522	-0.042365	4.028249
208.674555	5537.757678	7.719526	-0.042360	4.031054
208.819551	5545.900962	7.724531	-0.042392	4.033904
208.984540	5553.897273	7.729536	-0.042428	4.036700
209.198012	5561.788011	7.734541	-0.042473	4.039459
209.348633	5569.847127	7.739546	-0.042506	4.042274
209.239784	5577.798477	7.744550	-0.042491	4.045045
209.680860	5585.852051	7.749555	-0.042579	4.047858
209.830244	5593.842098	7.754560	-0.042612	4.050642
209.899274	5601.896729	7.759565	-0.042630	4.053446
209.963061	5609.967071	7.764570	-0.042647	4.056253
210.055457	5617.921419	7.769574	-0.042669	4.059019
210.240390	5625.949357	7.774579	-0.042709	4.061809
210.223405	5633.957016	7.779584	-0.042711	4.064588
210.544773	5641.967995	7.784589	-0.042776	4.067370
210.669885	5650.006125	7.789594	-0.042805	4.070158
210.897058	5658.016823	7.794598	-0.042852	4.072935
211.165794	5666.035021	7.799603	-0.042907	4.075714
211.242057	5674.036747	7.804608	-0.042927	4.078482
211.304480	5682.062577	7.809613	-0.042944	4.081256
211.396759	5690.039358	7.814618	-0.042966	4.084013
211.834850	5698.107414	7.819622	-0.043053	4.086803
212.037375	5706.105340	7.824627	-0.043096	4.089564
212.074342	5714.181407	7.829632	-0.043108	4.092348
212.206958	5722.197602	7.834637	-0.043138	4.095111
212.417406	5730.222602	7.839642	-0.043182	4.097876
212.284741	5738.185562	7.844646	-0.043163	4.100613
212.644709	5746.231167	7.849651	-0.043235	4.103383
213.035118	5754.262107	7.854656	-0.043313	4.106146
213.153685	5762.258021	7.859661	-0.043341	4.108892
213.292293	5770.328689	7.864666	-0.043372	4.111663
213.478080	5778.348422	7.869670	-0.043411	4.114414
213.656086	5786.405809	7.874675	-0.043450	4.117176
213.577987	5794.385180	7.879680	-0.043441	4.119907
213.866801	5802.415552	7.884685	-0.043500	4.122658
214.020970	5810.366855	7.889690	-0.043534	4.125378
213.854186	5818.377306	7.894694	-0.043508	4.128112
214.247144	5826.465879	7.899699	-0.043586	4.130879
214.364003	5834.485855	7.904704	-0.043613	4.133617
214.472446	5842.484944	7.909709	-0.043639	4.136345
214.533009	5850.488338	7.914714	-0.043655	4.139073
214.781151	5858.522443	7.919718	-0.043707	4.141811
215.061490	5866.496586	7.924723	-0.043764	4.144528
214.941845	5874.571956	7.929728	-0.043747	4.147273
215.284592	5882.560106	7.934733	-0.043816	4.149991
215.651823	5890.626358	7.939738	-0.043890	4.152735
215.667691	5898.637614	7.944742	-0.043898	4.155454
215.844937	5906.620007	7.949747	-0.043936	4.158163
215.983060	5914.634833	7.954752	-0.043967	4.160881
216.308084	5922.619070	7.959757	-0.044033	4.163589
216.234904	5930.712598	7.964762	-0.044024	4.166328
216.543235	5938.653586	7.969766	-0.044087	4.169018
216.810753	5946.720387	7.974771	-0.044142	4.171747
216.771780	5954.711299	7.979776	-0.044140	4.174446
216.958350	5962.754467	7.984781	-0.044180	4.177164
217.322240	5970.779517	7.989786	-0.044253	4.179875
217.437765	5978.768988	7.994790	-0.044280	4.182570
217.461921	5986.814846	7.999795	-0.044290	4.185281
217.665033	5994.839732	8.004800	-0.044333	4.187986
217.840777	6002.802097	8.009805	-0.044371	4.190667
218.036206	6010.978900	8.014810	-0.044412	4.193418
218.332435	6018.933986	8.019814	-0.044473	4.196095
218.324768	6026.895524	8.024819	-0.044477	4.198769
218.476967	6034.908292	8.029824	-0.044510	4.201460
218.651280	6042.852949	8.034829	-0.044548	4.204126
218.944016	6050.975146	8.039834	-0.044608	4.206852
219.066027	6058.885180	8.044838	-0.044635	4.209502
218.979426	6066.996035	8.049843	-0.044625	4.212217
218.990905	6074.996150	8.054848	-0.044632	4.214893
219.487811	6083.004415	8.059853	-0.044730	4.217576
219.598298	6091.003439	8.064858	-0.044756	4.220249
219.733258	6098.978798	8.069862	-0.044786	4.222914
220.021739	6107.037058	8.074867	-0.044845	4.225605
220.195503	6115.048711	8.079872	-0.044883	4.228279
220.472720	6123.061544	8.084877	-0.044939	4.230952
220.599475	6131.150522	8.089882	-0.044968	4.233647
220.529494	6139.138744	8.094886	-0.044960	4.236305
220.654770	6147.141376	8.099891	-0.044989	4.238968
220.977622	6155.154738	8.104896	-0.045054	4.241635
221.147094	6163.105241	8.109901	-0.045091	4.244278
221.262870	6171.194921	8.114906	-0.045118	4.246965
221.492214	6179.187772	8.119910	-0.045166	4.249619
221.840675	6187.242695	8.124915	-0.045236	4.252293
222.045982	6195.276623	8.129920	-0.045280	4.254957
221.904056	6203.258217	8.134925	-0.045258	4.257598
222.087909	6211.291545	8.139930	-0.045298	4.260259
222.293130	6219.275580	8.144934	-0.045341	4.262901
222.572075	6227.333548	8.149939	-0.045398	4.265567
222.875656	6235.336461	8.154944	-0.045460	4.268213
222.905455	6243.409401	8.159949	-0.045471	4.270878
222.920661	6251.437615	8.164954	-0.045479	4.273527
222.986954	6259.480862	8.169958	-0.045497	4.276180
223.356575	6267.418003	8.174963	-0.045571	4.278798
223.444870	6275.492552	8.179968	-0.045592	4.281458
223.301466	6283.402492	8.184973	-0.045571	4.284060
223.892712	6291.485729	8.189978	-0.045686	4.286723
223.964011	6299.460878	8.194982	-0.045705	4.289345
224.130991	6307.546952	8.199987	-0.045741	4.292002
223.963370	6315.564539	8.204992	-0.045715	4.294633
224.321577	6323.581750	8.209997	-0.045787	4.297266
224.443206	6331.585951	8.215002	-0.045815	4.299891
224.378224	6339.605306	8.220006	-0.045808	4.302518
224.759336	6347.597924	8.225011	-0.045884	4.305139
224.792418	6355.653427	8.230016	-0.045896	4.307775
224.796894	6363.603796	8.235021	-0.045902	4.310376
225.161322	6371.714933	8.240026	-0.045975	4.313030
225.285570	6379.681887	8.245030	-0.046003	4.315633
225.355548	6387.719999	8.250035	-0.046022	4.318258
225.516818	6395.715980	8.255040	-0.046057	4.320868
225.973320	6403.703524	8.260045	-0.046147	4.323475
226.118920	6411.752847	8.265050	-0.046180	4.326100
225.945214	6419.712532	8.270054	-0.046152	4.328690
226.308590	6427.802371	8.275059	-0.046225	4.331326
226.512056	6435.808592	8.280064	-0.046268	4.333932
226.582688	6443.824500	8.285069	-0.046287	4.336538
226.941714	6451.794900	8.290074	-0.046359	4.339130
226.854280	6459.814274	8.295078	-0.046348	4.341733
227.014719	6467.838058	8.300083	-0.046383	4.344338
227.394791	6475.858324	8.305088	-0.046459	4.346941
227.366633	6483.888088	8.310093	-0.046459	4.349543
227.537136	6491.970681	8.315098	-0.046496	4.352162
227.613770	6500.015732	8.320102	-0.046516	4.354767
227.778588	6507.971206	8.325107	-0.046552	4.357342
227.958540	6515.951443	8.330112	-0.046590	4.359923
228.033786	6523.966566	8.335117	-0.046609	4.362513
228.249759	6531.954752	8.340122	-0.046655	4.365094
228.506475	6539.956655	8.345126	-0.046708	4.367678
228.762976	6547.997299	8.350131	-0.046761	4.370273
228.614921	6556.061091	8.355136	-0.046739	4.372872
228.799294	6564.020692	8.360141	-0.046778	4.375437
228.974475	6572.054081	8.365146	-0.046816	4.378025
229.004233	6580.063890	8.370150	-0.046827	4.380602
229.178742	6588.087483	8.375155	-0.046865	4.383183
229.351619	6596.082875	8.380160	-0.046902	4.385754
229.557813	6604.110643	8.385165	-0.046946	4.388334
229.571456	6612.173820	8.390170	-0.046954	4.390922
229.585926	6620.150253	8.395174	-0.046961	4.393481
229.863946	6628.233024	8.400179	-0.047018	4.396075
229.809683	6636.206411	8.405184	-0.047014	4.398629
230.056461	6644.210613	8.410189	-0.047065	4.401194
230.271277	6652.192795	8.415194	-0.047110	4.403750
230.306430	6660.225585	8.420198	-0.047122	4.406320
230.554206	6668.221573	8.425203	-0.047173	4.408877
230.825482	6676.322612	8.430208	-0.047229	4.411467
230.796780	6684.320760	8.435213	-0.047229	4.414021
230.833887	6692.379274	8.440218	-0.047241	4.416593
230.931860	6700.330935	8.445222	-0.047264	4.419129
231.088645	6708.402908	8.450227	-0.047299	4.421703
231.207530	6716.338079	8.455232	-0.047326	4.424232
231.503641	6724.401767	8.460237	-0.047387	4.426800
231.805547	6732.441720	8.465242	-0.047448	4.429360
231.476694	6740.468965	8.470246	-0.047392	4.431911
231.752662	6748.494138	8.475251	-0.047449	4.434463
231.847231	6756.490202	8.480256	-0.047472	4.437004
232.124677	6764.445101	8.485261	-0.047529	4.439530
232.223429	6772.555690	8.490266	-0.047552	4.442104
232.517269	6780.467522	8.495270	-0.047612	4.444614
232.733992	6788.563321	8.500275	-0.047658	4.447181
232.653173	6796.556329	8.505280	-0.047648	4.449712
232.780505	6804.600536	8.510285	-0.047677	4.452259
233.053850	6812.574527	8.515290	-0.047733	4.454783
233.098450	6820.610307	8.520294	-0.047747	4.457324
233.327026	6828.598058	8.525299	-0.047794	4.459849
233.644176	6836.676388	8.530304	-0.047859	4.462402
233.756336	6844.631295	8.535309	-0.047885	4.464913
233.829021	6852.697113	8.540314	-0.047904	4.467458
233.887950	6860.688483	8.545318	-0.047920	4.469977
234.152049	6868.736604	8.550323	-0.047974	4.472514
234.112471	6876.728293	8.555328	-0.047972	4.475031
234.008323	6884.740053	8.560333	-0.047958	4.477552
234.424748	6892.740842	8.565338	-0.048041	4.480070
234.571845	6900.729245	8.570343	-0.048073	4.482582
234.656565	6908.739729	8.575347	-0.048094	4.485100
234.809851	6916.823677	8.580352	-0.048128	4.487639
234.755429	6924.804864	8.585357	-0.048123	4.490144
234.882663	6932.854450	8.590362	-0.048152	4.492669
235.180180	6940.838281	8.595367	-0.048213	4.495173
235.490883	6948.902315	8.600371	-0.048276	4.497700
235.566374	6956.847493	8.605376	-0.048295	4.500189
235.556886	6964.887660	8.610381	-0.048299	4.502705
235.821374	6972.906992	8.615386	-0.048353	4.505214
235.766274	6980.939608	8.620391	-0.048348	4.507725
235.979174	6988.937490	8.625395	-0.048393	4.510225
236.271162	6997.019264	8.630400	-0.048453	4.512749
236.492817	7005.023191	8.635405	-0.048499	4.515248
236.638457	7013.016211	8.640410	-0.048532	4.517741
236.686541	7020.947329	8.645415	-0.048546	4.520214
236.873028	7029.014106	8.650419	-0.048586	4.522728
236.921002	7037.014232	8.655424	-0.048600	4.525219
236.987476	7044.975519	8.660429	-0.048617	4.527697
237.450673	7053.033910	8.665434	-0.048709	4.530205
237.458304	7061.070798	8.670439	-0.048716	4.532703
237.618879	7069.145336	8.675443	-0.048751	4.535212
237.680926	7077.114402	8.680448	-0.048768	4.537687
237.544488	7085.085006	8.685453	-0.048747	4.540161
237.793631	7093.117090	8.690458	-0.048799	4.542653
237.877939	7101.088125	8.695463	-0.048820	4.545124
238.153129	7109.141127	8.700467	-0.048877	4.547620
238.107574	7117.164024	8.705472	-0.048873	4.550104
238.222552	7125.204623	8.710477	-0.048900	4.552593
238.597372	7133.243386	8.715482	-0.048975	4.555080
238.510840	7141.222148	8.720487	-0.048964	4.557547
238.669271	7149.228385	8.725491	-0.048999	4.560021
238.929711	7157.274004	8.730496	-0.049053	4.562506
238.996814	7165.227767	8.735501	-0.049070	4.564961
239.003428	7173.293377	8.740506	-0.049077	4.567450
239.104271	7181.277977	8.745511	-0.049101	4.569912
239.413015	7189.355398	8.750515	-0.049164	4.572401
239.620902	7197.370755	8.755520	-0.049208	4.574870
239.683031	7205.390972	8.760525	-0.049224	4.577339
239.884167	7213.396886	8.765530	-0.049267	4.579802
240.090443	7221.423434	8.770535	-0.049311	4.582270
239.968086	7229.405408	8.775539	-0.049293	4.584723
240.120230	7237.448952	8.780544	-0.049327	4.587194
240.070101	7245.408816	8.785549	-0.049323	4.589638
240.206342	7253.527266	8.790554	-0.049353	4.592129
240.316497	7261.553486	8.795559	-0.049379	4.594590
240.656519	7269.631613	8.800563	-0.049448	4.597066
240.789020	7277.486144	8.805568	-0.049477	4.599472
240.787809	7285.564287	8.810573	-0.049482	4.601946
241.088292	7293.546504	8.815578	-0.049544	4.604388
241.122704	7301.551648	8.820583	-0.049555	4.606837
241.149830	7309.520209	8.825587	-0.049566	4.609272
241.541463	7317.598178	8.830592	-0.049644	4.611740
241.687456	7325.587592	8.835597	-0.049676	4.614180
241.869199	7333.684653	8.840602	-0.049715	4.616651
241.601300	7341.609907	8.845607	-0.049671	4.619068
242.107252	7349.675825	8.850611	-0.049770	4.621527
242.199860	7357.655773	8.855616	-0.049793	4.623959
242.307963	7365.669717	8.860621	-0.049818	4.626399
242.496508	7373.679819	8.865626	-0.049858	4.628837
242.532544	7381.729963	8.870631	-0.049870	4.631286
242.980356	7389.767527	8.875635	-0.049959	4.633730
242.886726	7397.805541	8.880640	-0.049947	4.636172
243.042074	7405.726899	8.885645	-0.049981	4.638578
243.104385	7413.777752	8.890650	-0.049998	4.641022
243.135869	7421.765909	8.895655	-0.050009	4.643446
243.534796	7429.780776	8.900659	-0.050088	4.645876
243.709515	7437.789111	8.905664	-0.050126	4.648303
243.476217	7445.821178	8.910669	-0.050088	4.650736
243.808131	7453.895169	8.915674	-0.050155	4.653180
243.963082	7461.855329	8.920679	-0.050189	4.655589
244.176701	7469.879765	8.925683	-0.050234	4.658016
244.157156	7477.919002	8.930688	-0.050236	4.660446
244.359983	7485.935370	8.935693	-0.050279	4.662867
244.588545	7493.927138	8.940698	-0.050326	4.665280
244.576185	7501.934551	8.945703	-0.050329	4.667697
244.990252	7509.942803	8.950707	-0.050412	4.670112
245.093596	7518.051315	8.955712	-0.050436	4.672557
244.996347	7526.060569	8.960717	-0.050423	4.674971
245.420731	7534.070297	8.965722	-0.050508	4.677382
245.699103	7542.015110	8.970727	-0.050565	4.679773
245.694114	7550.012408	8.975731	-0.050569	4.682180
246.044303	7557.970100	8.980736	-0.050639	4.684572
246.206051	7566.076384	8.985741	-0.050675	4.687008
246.446863	7574.026294	8.990746	-0.050725	4.689396
246.379520	7582.113681	8.995751	-0.050718	4.691824
246.453243	7590.099986	9.000755	-0.050737	4.694221
246.394888	7598.164512	9.005760	-0.050731	4.696639
246.627764	7606.084088	9.010765	-0.050780	4.699013
246.887991	7614.183050	9.015770	-0.050833	4.701439
247.001120	7622.100688	9.020775	-0.050860	4.703810
247.102090	7630.176693	9.025779	-0.050884	4.706227
247.115322	7638.192565	9.030784	-0.050891	4.708625
247.354732	7646.198607	9.035789	-0.050941	4.711018
247.652376	7654.243763	9.040794	-0.051002	4.713422
247.485469	7662.251761	9.045799	-0.050976	4.715814
247.684003	7670.289802	9.050803	-0.051018	4.718214
247.892712	7678.272453	9.055808	-0.051062	4.720595
248.089080	7686.263304	9.060813	-0.051104	4.722978
248.202953	7694.327734	9.065818	-0.051131	4.725382
248.191623	7702.317626	9.070823	-0.051134	4.727762
248.449532	7710.345497	9.075827	-0.051187	4.730152
248.507874	7718.399783	9.080832	-0.051203	4.732549
248.508449	7726.364202	9.085837	-0.051208	4.734918
248.875662	7734.465401	9.090842	-0.051282	4.737326
248.963187	7742.430414	9.095847	-0.051304	4.739693
248.962434	7750.437447	9.100851	-0.051309	4.742071
249.245511	7758.437787	9.105856	-0.051367	4.744445
249.216864	7766.405270	9.110861	-0.051367	4.746810
249.475713	7774.478800	9.115866	-0.051420	4.749203
249.599315	7782.503405	9.120871	-0.051448	4.751582
249.642906	7790.453196	9.125875	-0.051462	4.753937
249.861627	7798.547089	9.130880	-0.051508	4.756333
249.954238	7806.488602	9.135885	-0.051530	4.758683
250.100752	7814.583556	9.140890	-0.051563	4.761078
250.116805	7822.526895	9.145895	-0.051571	4.763426
250.435683	7830.530682	9.150899	-0.051635	4.765791
250.734533	7838.642987	9.155904	-0.051696	4.768186
250.581351	7846.591992	9.160909	-0.051673	4.770533
250.861101	7854.727103	9.165914	-0.051730	4.772933
251.018142	7862.628731	9.170919	-0.051765	4.775263
251.248092	7870.665535	9.175923	-0.051813	4.777631
251.205621	7878.645562	9.180928	-0.051810	4.779983
251.257645	7886.663659	9.185933	-0.051825	4.782344
251.608880	7894.629380	9.190938	-0.051896	4.784687
251.591125	7902.666190	9.195943	-0.051898	4.787052
251.881733	7910.752741	9.200947	-0.051957	4.789428
251.948424	7918.787103	9.205952	-0.051975	4.791790
251.835530	7926.782464	9.210957	-0.051959	4.794139
252.003294	7934.801788	9.215962	-0.051996	4.796493
252.123492	7942.765893	9.220967	-0.052023	4.798830
252.320642	7950.757449	9.225971	-0.052065	4.801173
252.353907	7958.790964	9.230976	-0.052077	4.803528
252.544671	7966.780794	9.235981	-0.052117	4.805869
252.766047	7974.849708	9.240986	-0.052164	4.808231
252.855693	7982.852329	9.245991	-0.052186	4.810574
253.081650	7990.285875	9.250995	-0.052233	4.812748
253.330905	7994.835531	9.256000	-0.052282	4.814078

253.239746	7997.339560	9.261005	-0.052267	4.814810
253.392806	7998.721464	9.266010	-0.052296	4.815214
253.408615	7999.181911	9.271015	-0.052299	4.815348
253.849358	8000.114843	9.276019	-0.052382	4.815619
253.834047	8000.170122	9.281024	-0.052379	4.815635
253.761095	8000.084579	9.286029	-0.052366	4.815611
253.880874	8000.144192	9.291034	-0.052388	4.815627
253.928855	8000.163128	9.296039	-0.052397	4.815633
254.005509	8000.155835	9.301043	-0.052411	4.815630
254.174590	8000.193828	9.306048	-0.052443	4.815641
254.137348	8000.130222	9.311053	-0.052436	4.815622
254.063839	8000.151451	9.316058	-0.052422	4.815629
254.223990	8000.150857	9.321063	-0.052452	4.815628
254.297168	8000.118948	9.326067	-0.052466	4.815618
254.057291	8000.150282	9.331072	-0.052421	4.815628
253.971300	8000.144612	9.336077	-0.052405	4.815627
254.285163	8000.082452	9.341082	-0.052463	4.815607
254.234823	8000.115804	9.346087	-0.052454	4.815617
254.192338	8000.105504	9.351091	-0.052446	4.815615
254.385270	8000.185531	9.356096	-0.052482	4.815637
254.481542	8000.134777	9.361101	-0.052500	4.815622
254.315888	8000.195082	9.366106	-0.052469	4.815640
254.207488	8000.139928	9.371111	-0.052449	4.815625
254.548090	8000.147612	9.376115	-0.052513	4.815625
254.471932	8000.244614	9.381120	-0.052498	4.815654
254.486563	8000.158359	9.386125	-0.052501	4.815629
254.701496	8000.165065	9.391130	-0.052541	4.815630
254.602033	8000.153836	9.396135	-0.052523	4.815627
254.553628	8000.135964	9.401139	-0.052514	4.815622
254.586807	8000.169609	9.406144	-0.052520	4.815631
254.433865	8000.145764	9.411149	-0.052491	4.815625
254.630273	8000.153235	9.416154	-0.052528	4.815626
254.691131	8000.048513	9.421159	-0.052539	4.815596
254.742782	8000.051492	9.426163	-0.052549	4.815596
254.782185	8000.095916	9.431168	-0.052556	4.815609
254.608443	8000.086681	9.436173	-0.052524	4.815607
254.757420	8000.149976	9.441178	-0.052552	4.815625
254.823720	8000.167075	9.446183	-0.052564	4.815630
254.716469	8000.120481	9.451187	-0.052544	4.815616
254.861561	8000.140999	9.456192	-0.052571	4.815622
254.910256	8000.142861	9.461197	-0.052580	4.815622
254.953824	8000.142505	9.466202	-0.052588	4.815622
254.852265	8000.123767	9.471207	-0.052570	4.815617
255.105756	8000.087320	9.476211	-0.052617	4.815605
255.272446	8000.127411	9.481216	-0.052648	4.815616
254.831750	8000.130913	9.486221	-0.052566	4.815619
255.061173	8000.091938	9.491226	-0.052609	4.815606
255.169193	8000.075546	9.496231	-0.052629	4.815601
255.209561	8000.061255	9.501235	-0.052636	4.815597
255.213378	8000.175579	9.506240	-0.052637	4.815630
255.007032	8000.080385	9.511245	-0.052599	4.815603
255.093769	8000.126648	9.516250	-0.052615	4.815616
255.171445	8000.164222	9.521255	-0.052629	4.815627
255.157155	8000.107395	9.526259	-0.052627	4.815611
255.074837	8000.153041	9.531264	-0.052611	4.815624
255.018516	8000.061359	9.536269	-0.052601	4.815598
255.189255	8000.134620	9.541274	-0.052633	4.815618
255.283233	8000.117999	9.546279	-0.052650	4.815613
255.218369	8000.124419	9.551283	-0.052638	4.815615
255.047572	8000.194252	9.556288	-0.052606	4.815636
255.094407	8000.151235	9.561293	-0.052615	4.815624
255.403974	8000.163755	9.566298	-0.052673	4.815626
254.990823	8000.186925	9.571303	-0.052596	4.815635
255.132475	8000.097400	9.576307	-0.052622	4.815608
255.267688	8000.118826	9.581312	-0.052647	4.815613
255.158128	8000.110635	9.586317	-0.052627	4.815611
255.164317	8000.116077	9.591322	-0.052628	4.815613
255.230215	8000.082981	9.596327	-0.052640	4.815603
255.202412	8000.077191	9.601331	-0.052635	4.815601
255.207767	8000.118926	9.606336	-0.052636	4.815614
255.299757	8000.071305	9.611341	-0.052653	4.815599
255.415502	8000.100956	9.616346	-0.052675	4.815607
255.302080	8000.110857	9.621351	-0.052654	4.815611
255.289538	8000.108519	9.626355	-0.052652	4.815610
255.367682	8000.147168	9.631360	-0.052666	4.815621
255.232932	8000.090514	9.636365	-0.052641	4.815605
255.183344	8000.133490	9.641370	-0.052632	4.815618
255.171038	8000.183480	9.646375	-0.052630	4.815633
255.296992	8000.140684	9.651379	-0.052653	4.815620
255.181534	8000.193265	9.656384	-0.052632	4.815636
255.205289	8000.119972	9.661389	-0.052636	4.815614
255.464027	8000.141275	9.666394	-0.052684	4.815619
255.347439	8000.105206	9.671399	-0.052663	4.815609
255.386209	8000.090889	9.676403	-0.052670	4.815605
255.469772	8000.123220	9.681408	-0.052685	4.815614
255.443705	8000.115322	9.686413	-0.052681	4.815611
255.659806	8000.147677	9.691418	-0.052721	4.815620
255.367901	8000.193112	9.696423	-0.052667	4.815635
255.512780	8000.110046	9.701427	-0.052693	4.815610
255.392888	8000.209540	9.706432	-0.052671	4.815639
255.364552	8000.116177	9.711437	-0.052666	4.815612
255.610390	8000.192798	9.716442	-0.052712	4.815633
255.373450	8000.170786	9.721447	-0.052668	4.815628
255.452758	8000.079177	9.726451	-0.052682	4.815601
255.646520	8000.131456	9.731456	-0.052718	4.815615
255.526679	8000.103877	9.736461	-0.052696	4.815608
255.415795	8000.159736	9.741466	-0.052676	4.815625
255.706478	8000.155931	9.746471	-0.052730	4.815622
255.657062	8000.127363	9.751475	-0.052721	4.815614
255.564010	8000.155749	9.756480	-0.052703	4.815623
255.470995	8000.180932	9.761485	-0.052686	4.815631
255.524496	8000.172194	9.766490	-0.052696	4.815628
255.499690	8000.125874	9.771495	-0.052691	4.815614
255.540477	8000.104116	9.776499	-0.052699	4.815608
255.541180	8000.164996	9.781504	-0.052699	4.815626
255.476974	8000.088134	9.786509	-0.052687	4.815603
255.469129	8000.091212	9.791514	-0.052686	4.815604
255.529785	8000.081523	9.796519	-0.052697	4.815601
255.522075	8000.113435	9.801523	-0.052696	4.815611
255.474399	8000.134017	9.806528	-0.052687	4.815617
255.455282	8000.071772	9.811533	-0.052683	4.815599
255.630208	8000.108795	9.816538	-0.052716	4.815609
255.675977	8000.205649	9.821543	-0.052724	4.815637
255.546878	8000.136273	9.826547	-0.052700	4.815617
255.632039	8000.108830	9.831552	-0.052716	4.815609
255.641424	8000.061999	9.836557	-0.052718	4.815595
255.439775	8000.091819	9.841562	-0.052680	4.815605
255.443351	8000.095082	9.846567	-0.052681	4.815606
255.612054	8000.083950	9.851571	-0.052713	4.815601
255.710356	8000.254276	9.856576	-0.052731	4.815651
255.695815	8000.209190	9.861581	-0.052728	4.815638
255.823512	8000.154676	9.866586	-0.052752	4.815621
255.602324	8000.153209	9.871591	-0.052711	4.815622
255.494242	8000.119414	9.876595	-0.052691	4.815612
255.646666	8000.156071	9.881600	-0.052719	4.815622
255.765363	8000.128107	9.886605	-0.052741	4.815614
255.719019	8000.157253	9.891610	-0.052733	4.815622
255.444214	8000.167728	9.896615	-0.052682	4.815627
255.565392	8000.112039	9.901619	-0.052704	4.815610
255.329166	8000.155178	9.906624	-0.052660	4.815624
255.397363	8000.116780	9.911629	-0.052673	4.815612
255.404577	8000.121171	9.916634	-0.052674	4.815613
255.542971	8000.139445	9.921639	-0.052700	4.815618
255.371668	8000.099281	9.926643	-0.052668	4.815607
255.615631	8000.180143	9.931648	-0.052714	4.815630
255.528148	8000.129598	9.936653	-0.052697	4.815615
255.623297	8000.130082	9.941658	-0.052715	4.815615
255.641761	8000.153878	9.946663	-0.052718	4.815622
255.808702	8000.129903	9.951667	-0.052750	4.815614
255.966275	8000.169848	9.956672	-0.052779	4.815625
255.633664	8000.183651	9.961677	-0.052717	4.815631
255.564428	8000.181457	9.966682	-0.052704	4.815630
255.665939	8000.070988	9.971687	-0.052723	4.815597
255.563490	7999.999910	9.976691	-0.052704	4.815577
255.719607	8000.096426	9.981696	-0.052733	4.815605
255.692897	8000.107739	9.986701	-0.052728	4.815608
255.792968	8000.101896	9.991706	-0.052747	4.815606
255.597606	8000.161718	9.996711	-0.052710	4.815624
255.530384	8000.100825	10.001715	-0.052698	4.815607
255.654204	8000.135948	10.006720	-0.052721	4.815616
255.648761	8000.096350	10.011725	-0.052720	4.815605
255.915044	8000.102826	10.016730	-0.052770	4.815606
255.780151	8000.094223	10.021735	-0.052744	4.815604
255.869736	8000.067920	10.026739	-0.052761	4.815596
255.868673	8000.176826	10.031744	-0.052761	4.815627
255.857485	8000.124320	10.036749	-0.052759	4.815612
256.082646	8000.165366	10.041754	-0.052801	4.815623
256.051785	8000.120015	10.046759	-0.052795	4.815610
256.055190	8000.097647	10.051763	-0.052796	4.815603
256.060249	8000.134038	10.056768	-0.052797	4.815614
255.942976	8000.121450	10.061773	-0.052775	4.815611
255.951519	8000.120524	10.066778	-0.052777	4.815611
256.075346	8000.146036	10.071783	-0.052800	4.815617
255.912543	8000.072906	10.076787	-0.052769	4.815597
255.992558	8000.100908	10.081792	-0.052784	4.815605
255.999881	8000.066858	10.086797	-0.052786	4.815595
256.037061	8000.140080	10.091802	-0.052793	4.815616
255.813261	8000.196235	10.096807	-0.052751	4.815633
255.844295	8000.139078	10.101811	-0.052757	4.815616
256.080044	8000.216604	10.106816	-0.052801	4.815638
255.977089	8000.147652	10.111821	-0.052782	4.815618
255.942560	8000.094766	10.116826	-0.052775	4.815603
255.980594	8000.141306	10.121831	-0.052782	4.815616
255.850020	8000.074040	10.126835	-0.052758	4.815597
256.024000	8000.179392	10.131840	-0.052790	4.815627
256.114632	8000.138156	10.136845	-0.052807	4.815615
255.964014	8000.131432	10.141850	-0.052779	4.815614
255.966929	8000.121870	10.146855	-0.052780	4.815611
255.862077	8000.108417	10.151859	-0.052760	4.815607
255.997049	8000.160808	10.156864	-0.052785	4.815622
255.696152	8000.193281	10.161869	-0.052729	4.815633
255.984828	8000.148865	10.166874	-0.052783	4.815619
256.076782	8000.104447	10.171879	-0.052800	4.815605
255.992820	8000.080656	10.176883	-0.052785	4.815599
256.102468	8000.108073	10.181888	-0.052805	4.815606
256.113387	8000.094370	10.186893	-0.052807	4.815602
256.231380	8000.095227	10.191898	-0.052829	4.815602
256.113760	8000.189420	10.196903	-0.052807	4.815630
256.042364	8000.108168	10.201907	-0.052794	4.815606
256.169714	8000.175385	10.206912	-0.052818	4.815626
256.299825	8000.149743	10.211917	-0.052842	4.815617
256.216657	8000.116353	10.216922	-0.052827	4.815608
256.231303	8000.108050	10.221927	-0.052829	4.815606
256.240205	8000.109265	10.226931	-0.052831	4.815606
256.282774	8000.117436	10.231936	-0.052839	4.815608
256.137411	8000.166326	10.236941	-0.052812	4.815623
256.103522	8000.125197	10.241946	-0.052806	4.815611
256.112271	8000.155241	10.246951	-0.052807	4.815620
256.017119	8000.087485	10.251955	-0.052790	4.815601
256.054228	8000.091295	10.256960	-0.052796	4.815601
255.973548	8000.072896	10.261965	-0.052781	4.815596
255.930801	8000.077540	10.266970	-0.052774	4.815598
256.215564	8000.155865	10.271975	-0.052827	4.815620
256.072749	8000.112961	10.276979	-0.052800	4.815608
256.071625	8000.149252	10.281984	-0.052800	4.815618
256.314798	8000.156420	10.286989	-0.052845	4.815619
256.371839	8000.079397	10.291994	-0.052856	4.815596
256.427203	8000.106998	10.296999	-0.052866	4.815604
256.336295	8000.069210	10.302003	-0.052849	4.815594
256.415854	8000.115359	10.307008	-0.052864	4.815607
256.184513	8000.125473	10.312013	-0.052821	4.815611
256.179688	8000.104038	10.317018	-0.052820	4.815605
256.205360	8000.149309	10.322023	-0.052825	4.815618
256.109575	8000.075135	10.327027	-0.052807	4.815596
256.171571	8000.139151	10.332032	-0.052819	4.815615
256.018529	8000.174034	10.337037	-0.052790	4.815626
255.968308	8000.120892	10.342042	-0.052781	4.815611
256.290824	8000.168864	10.347047	-0.052841	4.815623
256.078939	8000.151531	10.352051	-0.052801	4.815619
256.184583	8000.215191	10.357056	-0.052821	4.815637
256.218637	8000.170897	10.362061	-0.052828	4.815624
256.387958	8000.125604	10.367066	-0.052859	4.815610
256.363395	8000.151902	10.372071	-0.052855	4.815618
256.304885	8000.109303	10.377075	-0.052844	4.815606
256.301019	8000.165839	10.382080	-0.052843	4.815622
256.177945	8000.118984	10.387085	-0.052820	4.815609
256.259659	8000.095757	10.392090	-0.052835	4.815602
256.210906	8000.094964	10.397095	-0.052826	4.815602
256.020300	8000.128167	10.402099	-0.052791	4.815612
256.234249	8000.139130	10.407104	-0.052831	4.815615
256.233144	8000.072906	10.412109	-0.052830	4.815595
256.247229	8000.052848	10.417114	-0.052833	4.815589
256.402669	8000.118387	10.422119	-0.052862	4.815608
256.386370	8000.104241	10.427123	-0.052859	4.815604
256.352223	8000.159216	10.432128	-0.052853	4.815620
256.261364	8000.122497	10.437133	-0.052836	4.815610
256.405442	8000.088539	10.442138	-0.052863	4.815599
256.349271	8000.155969	10.447143	-0.052852	4.815619
255.998188	8000.103263	10.452147	-0.052787	4.815605
256.210999	8000.132362	10.457152	-0.052826	4.815613
256.362486	8000.114543	10.462157	-0.052855	4.815607
256.498795	8000.099680	10.467162	-0.052880	4.815602
256.376313	8000.153215	10.472167	-0.052857	4.815618
256.256431	8000.092530	10.477171	-0.052835	4.815601
256.164420	8000.182869	10.482176	-0.052818	4.815628
255.994296	8000.135248	10.487181	-0.052786	4.815615
256.282247	8000.141010	10.492186	-0.052840	4.815615
256.415233	8000.229677	10.497191	-0.052865	4.815640
256.410987	8000.102532	10.502195	-0.052864	4.815603
256.288846	8000.163548	10.507200	-0.052841	4.815621
256.234845	8000.149855	10.512205	-0.052831	4.815618
256.275704	8000.115283	10.517210	-0.052839	4.815607
256.320331	8000.164066	10.522215	-0.052847	4.815621
256.319754	8000.134158	10.527219	-0.052847	4.815613
256.380122	8000.154366	10.532224	-0.052858	4.815618
256.384989	8000.118139	10.537229	-0.052859	4.815608
256.195189	8000.131065	10.542234	-0.052824	4.815612
256.446692	8000.145845	10.547239	-0.052871	4.815616
256.477304	8000.082273	10.552243	-0.052876	4.815597
256.258002	8000.155587	10.557248	-0.052836	4.815619
256.380606	8000.163995	10.562253	-0.052858	4.815621
256.518621	8000.155567	10.567258	-0.052884	4.815618
256.233568	8000.144516	10.572263	-0.052831	4.815616
256.266410	8000.072437	10.577267	-0.052837	4.815595
256.271544	8000.117373	10.582272	-0.052838	4.815608
256.152670	8000.128252	10.587277	-0.052816	4.815612
256.365974	8000.091151	10.592282	-0.052856	4.815600
256.506568	8000.109462	10.597287	-0.052882	4.815605
256.315469	8000.096739	10.602291	-0.052846	4.815602
256.256158	8000.103249	10.607296	-0.052835	4.815604
256.295755	8000.092149	10.612301	-0.052843	4.815601
256.512458	8000.102090	10.617306	-0.052883	4.815602
256.324839	8000.127867	10.622311	-0.052848	4.815611
256.218737	8000.127207	10.627315	-0.052829	4.815611
256.534019	8000.206031	10.632320	-0.052887	4.815633
256.405822	8000.170839	10.637325	-0.052863	4.815623
256.383378	8000.145914	10.642330	-0.052859	4.815616
256.636139	8000.160714	10.647335	-0.052906	4.815619
256.450844	8000.136338	10.652339	-0.052872	4.815613
256.485341	8000.190296	10.657344	-0.052878	4.815628
256.438245	8000.142543	10.662349	-0.052870	4.815615
256.470429	8000.153748	10.667354	-0.052876	4.815618
256.382897	8000.184360	10.672359	-0.052859	4.815627
256.323507	8000.146018	10.677363	-0.052848	4.815616
256.381379	8000.145895	10.682368	-0.052859	4.815616
256.170512	8000.137120	10.687373	-0.052820	4.815614
256.314537	8000.088212	10.692378	-0.052847	4.815599
256.454675	8000.117194	10.697383	-0.052873	4.815607
256.408372	8000.082269	10.702387	-0.052864	4.815597
256.485222	8000.146528	10.707392	-0.052879	4.815616
256.396747	8000.109848	10.712397	-0.052862	4.815605
256.302452	8000.096566	10.717402	-0.052844	4.815602
256.426983	8000.160534	10.722407	-0.052868	4.815620
256.347003	8000.069531	10.727411	-0.052853	4.815594
256.418557	8000.134771	10.732416	-0.052866	4.815612
256.204097	8000.089631	10.737421	-0.052826	4.815600
256.467839	8000.073641	10.742426	-0.052875	4.815594
256.566027	8000.111551	10.747431	-0.052894	4.815605
256.240912	8000.049657	10.752435	-0.052833	4.815588
256.413971	8000.073836	10.757440	-0.052865	4.815595
256.453531	8000.065940	10.762445	-0.052873	4.815592
256.493956	8000.102908	10.767450	-0.052880	4.815603
256.337919	8000.147353	10.772455	-0.052851	4.815616
256.447297	8000.124577	10.777459	-0.052872	4.815609
256.551541	8000.146567	10.782464	-0.052891	4.815615
256.475367	8000.143191	10.787469	-0.052877	4.815615
256.484535	8000.120917	10.792474	-0.052879	4.815608
256.680225	8000.206336	10.797479	-0.052915	4.815632
256.535530	8000.071562	10.802483	-0.052888	4.815593
256.649703	8000.086239	10.807488	-0.052909	4.815597
256.737813	8000.099423	10.812493	-0.052926	4.815601
256.628320	8000.109387	10.817498	-0.052906	4.815604
256.689867	8000.144564	10.822503	-0.052917	4.815614
256.494359	8000.096528	10.827507	-0.052881	4.815601
256.651356	8000.151415	10.832512	-0.052910	4.815616
256.571192	8000.120209	10.837517	-0.052895	4.815607
256.401709	8000.099295	10.842522	-0.052863	4.815602
256.692115	8000.189461	10.847527	-0.052918	4.815627
256.598693	8000.159106	10.852531	-0.052900	4.815619
256.507792	8000.164034	10.857536	-0.052883	4.815621
256.621938	8000.171236	10.862541	-0.052905	4.815622
256.821853	8000.149935	10.867546	-0.052942	4.815615
256.753022	8000.144543	10.872551	-0.052929	4.815614
256.671181	8000.090884	10.877555	-0.052914	4.815598
256.796293	8000.116419	10.882560	-0.052937	4.815605
256.655697	8000.135486	10.887565	-0.052911	4.815611
256.547567	8000.115572	10.892570	-0.052891	4.815606
256.757313	8000.204423	10.897575	-0.052930	4.815631
256.480830	8000.155067	10.902579	-0.052878	4.815618
256.580785	8000.137476	10.907584	-0.052897	4.815612
256.522186	8000.135455	10.912589	-0.052886	4.815612
256.637192	8000.106362	10.917594	-0.052908	4.815603
256.528950	8000.155858	10.922599	-0.052888	4.815618
256.576144	8000.159833	10.927603	-0.052896	4.815619
256.843351	8000.156715	10.932608	-0.052946	4.815617
256.695248	8000.105180	10.937613	-0.052918	4.815602
256.748865	8000.138092	10.942618	-0.052929	4.815612
256.934076	8000.208390	10.947623	-0.052963	4.815631
256.925036	8000.140967	10.952627	-0.052961	4.815612
256.928516	8000.142094	10.957632	-0.052962	4.815612
256.798301	8000.114343	10.962637	-0.052938	4.815605
257.030094	8000.117056	10.967642	-0.052981	4.815604
256.674902	8000.242617	10.972647	-0.052915	4.815643
256.658164	8000.181477	10.977651	-0.052912	4.815625
256.631746	8000.184251	10.982656	-0.052907	4.815626
256.586106	8000.132251	10.987661	-0.052898	4.815611
256.569043	8000.089259	10.992666	-0.052895	4.815598
256.752884	8000.116819	10.997671	-0.052929	4.815606
256.797234	8000.125019	11.002675	-0.052938	4.815608
256.821042	8000.119001	11.007680	-0.052942	4.815606
256.630860	8000.098817	11.012685	-0.052907	4.815601
256.570292	8000.127732	11.017690	-0.052896	4.815610
256.912575	8000.171757	11.022695	-0.052959	4.815621
256.701581	8000.139486	11.027699	-0.052920	4.815612
256.704080	8000.128850	11.032704	-0.052921	4.815609
256.703810	8000.190785	11.037709	-0.052921	4.815627
256.626266	8000.122246	11.042714	-0.052906	4.815608
256.765887	8000.186461	11.047719	-0.052932	4.815626
256.701868	8000.086106	11.052723	-0.052920	4.815597
256.749294	8000.143478	11.057728	-0.052929	4.815613
256.642919	8000.123592	11.062733	-0.052909	4.815608
256.813564	8000.156276	11.067738	-0.052941	4.815617
256.852556	8000.183611	11.072743	-0.052948	4.815625
256.746139	8000.145569	11.077747	-0.052929	4.815614
256.722794	8000.235961	11.082752	-0.052924	4.815641
256.669343	8000.207326	11.087757	-0.052914	4.815632
256.615811	8000.149857	11.092762	-0.052904	4.815616
256.636105	8000.167276	11.097767	-0.052908	4.815621
256.570743	8000.128836	11.102771	-0.052896	4.815610
256.677108	8000.165812	11.107776	-0.052916	4.815620
256.520368	8000.186752	11.112781	-0.052887	4.815627
256.719467	8000.203882	11.117786	-0.052924	4.815631
256.758087	8000.172477	11.122791	-0.052931	4.815622
256.646035	8000.127937	11.127795	-0.052910	4.815609
256.770061	8000.134232	11.132800	-0.052933	4.815611
256.859051	8000.143159	11.137805	-0.052950	4.815613
256.693519	8000.138327	11.142810	-0.052919	4.815612
256.784455	8000.182526	11.147815	-0.052936	4.815625
256.978580	8000.093854	11.152819	-0.052972	4.815598
256.700690	8000.109616	11.157824	-0.052920	4.815604
256.770268	8000.163078	11.162829	-0.052933	4.815619
256.866458	8000.135815	11.167834	-0.052951	4.815611
257.071036	8000.189343	11.172839	-0.052989	4.815625
256.942727	8000.178710	11.177843	-0.052966	4.815623
256.943979	8000.142423	11.182848	-0.052966	4.815612
256.917003	8000.147325	11.187853	-0.052961	4.815614
256.933180	8000.158269	11.192858	-0.052964	4.815617
256.922139	8000.168770	11.197863	-0.052962	4.815620
256.976354	8000.120532	11.202867	-0.052972	4.815606
257.039668	8000.197387	11.207872	-0.052984	4.815628
257.038024	8000.202701	11.212877	-0.052983	4.815629
257.034284	8000.140704	11.217882	-0.052983	4.815611
257.191572	8000.164628	11.222887	-0.053012	4.815617
256.855238	8000.149535	11.227891	-0.052949	4.815615
256.886171	8000.143634	11.232896	-0.052955	4.815613
256.953519	8000.198128	11.237901	-0.052968	4.815628
256.932594	8000.128376	11.242906	-0.052964	4.815608
256.657623	8000.140981	11.247911	-0.052913	4.815613
256.853249	8000.124950	11.252915	-0.052949	4.815607
256.848462	8000.137688	11.257920	-0.052948	4.815611
256.570913	8000.131030	11.262925	-0.052897	4.815611
256.766583	8000.102185	11.267930	-0.052933	4.815601
257.079500	8000.145732	11.272935	-0.052991	4.815612
256.824274	8000.093518	11.277939	-0.052944	4.815598
256.956264	8000.114893	11.282944	-0.052968	4.815604
256.989402	8000.100485	11.287949	-0.052975	4.815600
256.897315	8000.092578	11.292954	-0.052958	4.815598
256.969947	8000.111918	11.297959	-0.052971	4.815603
257.065830	8000.112415	11.302963	-0.052989	4.815603
256.935709	8000.132721	11.307968	-0.052965	4.815609
256.873532	8000.179764	11.312973	-0.052953	4.815623
256.737446	8000.123085	11.317978	-0.052928	4.815607
257.116779	8000.120727	11.322983	-0.052999	4.815605
257.153308	8000.118121	11.327987	-0.053005	4.815604
256.848877	8000.127042	11.332992	-0.052949	4.815608
256.973693	8000.139758	11.337997	-0.052972	4.815611
256.899184	8000.139613	11.343002	-0.052958	4.815611
256.873986	8000.220363	11.348007	-0.052953	4.815635
256.942908	8000.146736	11.353011	-0.052966	4.815613
257.012700	8000.154283	11.358016	-0.052979	4.815615
256.952146	8000.163976	11.363021	-0.052968	4.815618
256.894164	8000.180119	11.368026	-0.052957	4.815623
257.132671	8000.173331	11.373031	-0.053002	4.815620
257.051553	8000.137837	11.378035	-0.052987	4.815610
256.916751	8000.170882	11.383040	-0.052962	4.815621
256.998529	8000.189303	11.388045	-0.052977	4.815626
256.980961	8000.170864	11.393050	-0.052974	4.815620
256.944419	8000.176677	11.398055	-0.052967	4.815622
256.778540	8000.173975	11.403059	-0.052936	4.815622
257.161211	8000.138567	11.408064	-0.053007	4.815610
256.939802	8000.237477	11.413069	-0.052966	4.815640
256.845061	8000.119534	11.418074	-0.052948	4.815606
257.027641	8000.215419	11.423079	-0.052982	4.815633
256.949057	8000.219479	11.428083	-0.052968	4.815635
256.867337	8000.191451	11.433088	-0.052953	4.815627
256.935934	8000.180824	11.438093	-0.052965	4.815623
256.933089	8000.117774	11.443098	-0.052965	4.815605
256.938956	8000.207574	11.448103	-0.052966	4.815631
256.819367	8000.145825	11.453107	-0.052944	4.815614
256.909658	8000.112058	11.458112	-0.052960	4.815603
256.884377	8000.111647	11.463117	-0.052956	4.815603
257.154301	8000.133136	11.468122	-0.053006	4.815608
257.260042	8000.169034	11.473127	-0.053026	4.815618
257.176372	8000.136703	11.478131	-0.053010	4.815609
257.113618	8000.146360	11.483136	-0.052999	4.815612
257.082589	8000.193912	11.488141	-0.052993	4.815626
257.213860	8000.151202	11.493146	-0.053017	4.815613
257.062232	8000.178633	11.498151	-0.052989	4.815622
257.060161	8000.126274	11.503155	-0.052989	4.815607
257.186148	8000.118718	11.508160	-0.053012	4.815604
257.244001	8000.138886	11.513165	-0.053023	4.815610
257.105445	8000.084302	11.518170	-0.052997	4.815594
256.968779	8000.118384	11.523175	-0.052972	4.815605
256.885109	8000.101003	11.528179	-0.052956	4.815600
256.953164	8000.140558	11.533184	-0.052969	4.815611
257.119685	8000.191330	11.538189	-0.053000	4.815626
257.065891	8000.163757	11.543194	-0.052990	4.815618
257.047709	8000.170938	11.548199	-0.052987	4.815620
256.924542	8000.150777	11.553203	-0.052964	4.815615
257.105186	8000.111008	11.558208	-0.052997	4.815602
257.184352	8000.134727	11.563213	-0.053012	4.815609
257.014760	8000.084976	11.568218	-0.052980	4.815595
257.160624	8000.147158	11.573223	-0.053008	4.815612
257.188320	8000.138000	11.578227	-0.053013	4.815610
257.158766	8000.183440	11.583232	-0.053007	4.815623
257.072352	8000.171353	11.588237	-0.052991	4.815620
257.111459	8000.143160	11.593242	-0.052999	4.815611
257.137700	8000.115824	11.598247	-0.053003	4.815603
256.981297	8000.175213	11.603251	-0.052974	4.815621
257.032065	8000.168568	11.608256	-0.052984	4.815619
257.026263	8000.156728	11.613261	-0.052983	4.815616
256.849613	8000.072690	11.618266	-0.052950	4.815592
257.100383	8000.132310	11.623271	-0.052997	4.815608
256.913677	8000.084417	11.628275	-0.052962	4.815595
257.038538	8000.121695	11.633280	-0.052985	4.815606
257.065718	8000.140294	11.638285	-0.052990	4.815611
257.179595	8000.104776	11.643290	-0.053011	4.815600
257.149037	8000.174760	11.648295	-0.053006	4.815621
256.952736	8000.188648	11.653299	-0.052969	4.815626
257.043425	8000.183721	11.658304	-0.052986	4.815624
256.982097	8000.160297	11.663309	-0.052975	4.815617
256.977859	8000.120717	11.668314	-0.052974	4.815606
257.001993	8000.156353	11.673319	-0.052979	4.815616
256.972326	8000.136649	11.678323	-0.052973	4.815610
257.137949	8000.114789	11.683328	-0.053004	4.815603
256.894040	8000.115086	11.688333	-0.052958	4.815604
257.113437	8000.088764	11.693338	-0.052999	4.815596
257.245981	8000.138982	11.698343	-0.053024	4.815610
257.295956	8000.126983	11.703347	-0.053033	4.815606
257.292759	8000.082081	11.708352	-0.053033	4.815593
257.452137	8000.190404	11.713357	-0.053063	4.815624
257.228691	8000.130163	11.718362	-0.053021	4.815607
257.065346	8000.152064	11.723367	-0.052991	4.815614
257.146626	8000.133100	11.728371	-0.053006	4.815608
257.233812	8000.133456	11.733376	-0.053022	4.815608
257.237785	8000.173035	11.738381	-0.053023	4.815620
256.945315	8000.088176	11.743386	-0.052968	4.815596
257.096249	8000.168594	11.748391	-0.052996	4.815619
257.065171	8000.095473	11.753395	-0.052991	4.815598
257.010374	8000.122346	11.758400	-0.052980	4.815606
257.135182	8000.167099	11.763405	-0.053004	4.815618
257.056931	8000.098547	11.768410	-0.052989	4.815599
257.136007	8000.140418	11.773415	-0.053004	4.815611
257.240853	8000.087667	11.778419	-0.053023	4.815595
257.248356	8000.107013	11.783424	-0.053025	4.815600
257.233164	8000.075798	11.788429	-0.053022	4.815591
257.180556	8000.061059	11.793434	-0.053012	4.815587
257.175196	8000.087671	11.798439	-0.053011	4.815595
257.091953	8000.068162	11.803443	-0.052996	4.815590
257.227483	8000.125903	11.808448	-0.053021	4.815606
257.362014	8000.139845	11.813453	-0.053046	4.815609
257.023849	8000.101229	11.818458	-0.052983	4.815600
257.192313	8000.113588	11.823463	-0.053015	4.815602
257.227648	8000.152610	11.828467	-0.053021	4.815614
257.208205	8000.153363	11.833472	-0.053018	4.815614
257.124224	8000.142384	11.838477	-0.053002	4.815611
257.046463	8000.090927	11.843482	-0.052987	4.815596
257.279176	8000.077637	11.848487	-0.053031	4.815592
257.169444	8000.066238	11.853491	-0.053010	4.815589
257.166367	8000.114245	11.858496	-0.053010	4.815603
257.269881	8000.142632	11.863501	-0.053029	4.815611
257.207711	8000.075411	11.868506	-0.053018	4.815591
257.091479	8000.124776	11.873511	-0.052996	4.815606
257.134631	8000.085969	11.878515	-0.053004	4.815595
256.999799	8000.060280	11.883520	-0.052979	4.815588
257.126235	8000.111465	11.888525	-0.053002	4.815602
256.987701	8000.072900	11.893530	-0.052977	4.815592
257.139013	8000.090319	11.898535	-0.053005	4.815596
257.165722	8000.131336	11.903539	-0.053010	4.815608
257.234742	8000.112173	11.908544	-0.053023	4.815602
257.196415	8000.163877	11.913549	-0.053016	4.815617
257.076406	8000.079695	11.918554	-0.052993	4.815593
257.021123	8000.133257	11.923559	-0.052983	4.815609
257.023913	8000.091657	11.928563	-0.052984	4.815597
257.235579	8000.081227	11.933568	-0.053023	4.815593
257.180145	8000.110226	11.938573	-0.053013	4.815601
257.143327	8000.105356	11.943578	-0.053006	4.815600
257.231351	8000.165527	11.948583	-0.053022	4.815617
257.082211	8000.110770	11.953587	-0.052995	4.815602
257.104728	8000.091917	11.958592	-0.052999	4.815596
257.335664	8000.122381	11.963597	-0.053042	4.815604
257.322448	8000.050618	11.968602	-0.053039	4.815583
257.282643	8000.075601	11.973607	-0.053032	4.815591
257.135513	8000.097765	11.978611	-0.053005	4.815598
257.194253	8000.089113	11.983616	-0.053016	4.815595
257.165106	8000.205041	11.988621	-0.053010	4.815629
257.067900	8000.118026	11.993626	-0.052992	4.815604
257.385528	8000.155243	11.998631	-0.053051	4.815614
257.131855	8000.071017	12.003635	-0.053004	4.815590
256.906487	8000.081227	12.008640	-0.052962	4.815594
257.316706	8000.154126	12.013645	-0.053038	4.815614
257.216584	8000.099101	12.018650	-0.053020	4.815598
257.275152	8000.147045	12.023655	-0.053031	4.815612
257.142176	8000.129928	12.028659	-0.053006	4.815607
257.094197	8000.102450	12.033664	-0.052997	4.815600
257.160077	8000.149445	12.038669	-0.053009	4.815613
257.007689	8000.102111	12.043674	-0.052981	4.815600
257.255559	8000.144598	12.048679	-0.053027	4.815611
257.129626	8000.158565	12.053683	-0.053004	4.815616
257.042498	8000.126177	12.058688	-0.052988	4.815607
257.224199	8000.136617	12.063693	-0.053021	4.815609
257.071503	8000.072191	12.068698	-0.052993	4.815591
257.129693	8000.145758	12.073703	-0.053004	4.815612
257.186124	8000.175513	12.078707	-0.053014	4.815621
257.133441	8000.137280	12.083712	-0.053005	4.815610
257.081821	8000.124693	12.088717	-0.052995	4.815606
257.108256	8000.116582	12.093722	-0.053000	4.815604
257.194252	8000.142548	12.098727	-0.053016	4.815611
257.373359	8000.115569	12.103731	-0.053049	4.815602
257.163270	8000.093991	12.108736	-0.053010	4.815597
257.522612	8000.144703	12.113741	-0.053077	4.815610
257.475239	8000.131118	12.118746	-0.053068	4.815606
257.433982	8000.151805	12.123751	-0.053061	4.815612
257.404143	8000.128894	12.128755	-0.053055	4.815606
257.317194	8000.090102	12.133760	-0.053039	4.815595
257.481567	8000.140839	12.138765	-0.053070	4.815609
257.174663	8000.070695	12.143770	-0.053012	4.815590
257.348182	8000.150414	12.148775	-0.053045	4.815612
257.465154	8000.098928	12.153779	-0.053067	4.815597
257.305928	8000.073908	12.158784	-0.053037	4.815590
257.202020	8000.120271	12.163789	-0.053018	4.815604
257.228286	8000.070510	12.168794	-0.053023	4.815590
257.258206	8000.114783	12.173799	-0.053028	4.815602
257.220646	8000.134463	12.178803	-0.053021	4.815608
257.262594	8000.095636	12.183808	-0.053029	4.815597
257.203171	8000.171557	12.188813	-0.053018	4.815619
256.962986	8000.133471	12.193818	-0.052973	4.815609
257.243086	8000.174348	12.198823	-0.053026	4.815620
257.377684	8000.184019	12.203827	-0.053051	4.815622
257.241852	8000.084628	12.208832	-0.053025	4.815594
257.216987	8000.100242	12.213837	-0.053021	4.815598
257.464415	8000.119229	12.218842	-0.053067	4.815603
257.512354	8000.127488	12.223847	-0.053076	4.815605
257.331352	8000.179001	12.228851	-0.053042	4.815621
257.326777	8000.115922	12.233856	-0.053041	4.815602
257.462678	8000.150177	12.238861	-0.053067	4.815612
257.244652	8000.106043	12.243866	-0.053026	4.815600
257.252188	8000.138205	12.248871	-0.053027	4.815609
257.402965	8000.113967	12.253875	-0.053055	4.815601
257.495540	8000.086645	12.258880	-0.053073	4.815593
257.455330	8000.122300	12.263885	-0.053065	4.815604
257.405020	8000.094784	12.268890	-0.053056	4.815596
257.380757	8000.110408	12.273895	-0.053051	4.815601
257.562536	8000.090948	12.278899	-0.053085	4.815594
257.402038	8000.077654	12.283904	-0.053055	4.815591
257.603139	8000.136466	12.288909	-0.053093	4.815607
257.421620	8000.081180	12.293914	-0.053059	4.815592
257.396976	8000.116021	12.298919	-0.053055	4.815602
257.574526	8000.152023	12.303923	-0.053088	4.815612
257.450108	8000.084854	12.308928	-0.053064	4.815593
257.334837	8000.061618	12.313933	-0.053043	4.815587
257.327191	8000.105279	12.318938	-0.053042	4.815599
257.544620	8000.109894	12.323943	-0.053082	4.815600
257.174188	8000.068615	12.328947	-0.053013	4.815589
257.255588	8000.045383	12.333952	-0.053028	4.815582
257.521268	8000.096703	12.338957	-0.053078	4.815596
257.161685	8000.099386	12.343962	-0.053011	4.815598
257.232884	8000.116567	12.348967	-0.053024	4.815603
257.306679	8000.125247	12.353971	-0.053038	4.815605
257.349031	8000.113124	12.358976	-0.053046	4.815601
257.379081	8000.149924	12.363981	-0.053051	4.815612
257.354942	8000.100409	12.368986	-0.053047	4.815598
257.449500	8000.179910	12.373991	-0.053065	4.815621
257.394463	8000.148045	12.378995	-0.053054	4.815611
257.453338	8000.108426	12.384000	-0.053065	4.815600
257.780988	8000.126586	12.389005	-0.053126	4.815603
257.446768	8000.098711	12.394010	-0.053064	4.815597
257.425521	8000.158169	12.399015	-0.053060	4.815614
257.459048	8000.114934	12.404019	-0.053066	4.815601
257.560661	8000.125135	12.409024	-0.053085	4.815604
257.320147	8000.136166	12.414029	-0.053041	4.815608
257.174173	8000.082529	12.419034	-0.053013	4.815593
257.352288	8000.091842	12.424039	-0.053047	4.815595
257.246527	8000.128563	12.429043	-0.053027	4.815606
257.203971	8000.101174	12.434048	-0.053019	4.815599
257.322444	8000.099904	12.439053	-0.053041	4.815598
257.358785	8000.098362	12.444058	-0.053048	4.815597
257.305972	8000.157305	12.449063	-0.053038	4.815615
257.243626	8000.132796	12.454067	-0.053027	4.815608
257.357981	8000.154953	12.459072	-0.053048	4.815614
257.370046	8000.143404	12.464077	-0.053050	4.815610
257.375340	8000.134949	12.469082	-0.053051	4.815608
257.607230	8000.139800	12.474087	-0.053094	4.815608
257.591649	8000.137412	12.479091	-0.053091	4.815607
257.450694	8000.057158	12.484096	-0.053065	4.815585
257.616841	8000.139962	12.489101	-0.053096	4.815608
257.436696	8000.171199	12.494106	-0.053063	4.815618
257.495589	8000.163618	12.499111	-0.053074	4.815616
257.529846	8000.151363	12.504115	-0.053080	4.815612
257.438347	8000.110361	12.509120	-0.053063	4.815600
257.293260	8000.125083	12.514125	-0.053036	4.815605
257.186301	8000.062471	12.519130	-0.053016	4.815587
257.335701	8000.102285	12.524135	-0.053044	4.815598
257.498262	8000.086783	12.529139	-0.053074	4.815593
257.311250	8000.089075	12.534144	-0.053039	4.815595
257.680871	8000.166653	12.539149	-0.053108	4.815616
257.495711	8000.126259	12.544154	-0.053074	4.815605
257.427213	8000.130483	12.549159	-0.053061	4.815606
257.452230	8000.138368	12.554163	-0.053066	4.815608
257.471584	8000.124803	12.559168	-0.053069	4.815604
257.447954	8000.139370	12.564173	-0.053065	4.815609
257.336332	8000.129008	12.569178	-0.053044	4.815606
257.478423	8000.153753	12.574183	-0.053071	4.815613
257.465387	8000.135387	12.579187	-0.053068	4.815607
257.265852	8000.092623	12.584192	-0.053031	4.815596
257.540084	8000.215634	12.589197	-0.053082	4.815631
257.379365	8000.145737	12.594202	-0.053052	4.815611
257.321319	8000.105280	12.599207	-0.053042	4.815599
257.399553	8000.125779	12.604211	-0.053056	4.815605
257.510099	8000.083800	12.609216	-0.053077	4.815592
257.657609	8000.162028	12.614221	-0.053104	4.815614
257.485674	8000.137868	12.619226	-0.053072	4.815608
257.576606	8000.138284	12.624231	-0.053089	4.815608
257.537115	8000.170747	12.629235	-0.053082	4.815617
257.425747	8000.087772	12.634240	-0.053061	4.815594
257.643798	8000.161811	12.639245	-0.053102	4.815614
257.655926	8000.147060	12.644250	-0.053104	4.815610
257.425120	8000.161453	12.649255	-0.053061	4.815615
257.456064	8000.129922	12.654259	-0.053067	4.815606
257.610430	8000.113218	12.659264	-0.053096	4.815600
257.646573	8000.145847	12.664269	-0.053102	4.815610
257.425811	8000.089921	12.669274	-0.053061	4.815594
257.535433	8000.162192	12.674279	-0.053082	4.815615
257.541996	8000.150554	12.679283	-0.053083	4.815611
257.440872	8000.112598	12.684288	-0.053064	4.815601
257.446132	8000.113753	12.689293	-0.053065	4.815601
257.643476	8000.071053	12.694298	-0.053102	4.815588
257.669634	8000.134488	12.699303	-0.053107	4.815606
257.419734	8000.132550	12.704307	-0.053060	4.815607
257.604159	8000.128084	12.709312	-0.053095	4.815605
257.474921	8000.128114	12.714317	-0.053071	4.815605
257.170689	8000.117816	12.719322	-0.053014	4.815604
257.452061	8000.124541	12.724327	-0.053066	4.815604
257.637777	8000.170288	12.729331	-0.053101	4.815617
257.532809	8000.122658	12.734336	-0.053082	4.815603
257.545592	8000.182670	12.739341	-0.053084	4.815621
257.671616	8000.142011	12.744346	-0.053107	4.815608
257.578261	8000.152237	12.749351	-0.053090	4.815612
257.423710	8000.146515	12.754355	-0.053061	4.815611
257.532059	8000.095956	12.759360	-0.053081	4.815596
257.488867	8000.160396	12.764365	-0.053073	4.815615
257.531181	8000.106625	12.769370	-0.053081	4.815599
257.499025	8000.109306	12.774375	-0.053075	4.815600
257.525132	8000.142838	12.779379	-0.053080	4.815609
257.562057	8000.131695	12.784384	-0.053087	4.815606
257.509666	8000.152200	12.789389	-0.053077	4.815612
257.559319	8000.187185	12.794394	-0.053087	4.815622
257.465459	8000.184588	12.799399	-0.053069	4.815622
257.383941	8000.173649	12.804403	-0.053054	4.815619
257.538546	8000.118505	12.809408	-0.053083	4.815602
257.679327	8000.195556	12.814413	-0.053109	4.815624
257.331140	8000.175997	12.819418	-0.053044	4.815620
257.465439	8000.181393	12.824423	-0.053069	4.815621
257.743746	8000.240397	12.829427	-0.053121	4.815637
257.476698	8000.197598	12.834432	-0.053072	4.815626
257.468138	8000.255128	12.839437	-0.053070	4.815642
257.608035	8000.180521	12.844442	-0.053096	4.815620
257.630317	8000.161664	12.849447	-0.053100	4.815614
257.552474	8000.148649	12.854451	-0.053086	4.815611
257.506156	8000.110519	12.859456	-0.053077	4.815600
257.691835	8000.151993	12.864461	-0.053112	4.815611
257.481099	8000.150694	12.869466	-0.053072	4.815612
257.555056	8000.143359	12.874471	-0.053086	4.815609
257.721262	8000.156750	12.879475	-0.053117	4.815612
257.609285	8000.098327	12.884480	-0.053096	4.815596
257.640017	8000.209892	12.889485	-0.053102	4.815628
257.452843	8000.138495	12.894490	-0.053067	4.815608
257.473414	8000.144172	12.899495	-0.053071	4.815610
257.486683	8000.177495	12.904499	-0.053074	4.815620
257.515791	8000.109626	12.909504	-0.053079	4.815600
257.725323	8000.192069	12.914509	-0.053118	4.815623
257.491388	8000.104960	12.919514	-0.053075	4.815598
257.484976	8000.132622	12.924519	-0.053073	4.815606
257.711645	8000.132049	12.929523	-0.053116	4.815605
257.656253	8000.126875	12.934528	-0.053105	4.815604
257.553332	8000.138014	12.939533	-0.053086	4.815608
257.605541	8000.123916	12.944538	-0.053096	4.815603
257.821178	8000.124231	12.949543	-0.053136	4.815602
257.717385	8000.189818	12.954547	-0.053117	4.815622
257.604139	8000.119627	12.959552	-0.053096	4.815602
257.580359	8000.161957	12.964557	-0.053091	4.815615
257.449553	8000.145943	12.969562	-0.053067	4.815611
257.490352	8000.120980	12.974567	-0.053075	4.815603
257.542168	8000.136777	12.979571	-0.053084	4.815607
257.742191	8000.106936	12.984576	-0.053121	4.815598
257.541608	8000.101531	12.989581	-0.053084	4.815597
257.676181	8000.141104	12.994586	-0.053109	4.815608
257.708353	8000.148038	12.999591	-0.053115	4.815610
257.525165	8000.098064	13.004595	-0.053081	4.815596
257.424864	8000.124196	13.009600	-0.053063	4.815604
257.570850	8000.151140	13.014605	-0.053090	4.815611
257.540536	8000.129289	13.019610	-0.053084	4.815605
257.561294	8000.096525	13.024615	-0.053088	4.815596
257.740214	8000.122938	13.029619	-0.053121	4.815602
257.835468	8000.108474	13.034624	-0.053139	4.815598
257.577424	8000.135237	13.039629	-0.053091	4.815607
257.598153	8000.148392	13.044634	-0.053095	4.815611
257.766021	8000.173557	13.049639	-0.053126	4.815617
257.749980	8000.153007	13.054643	-0.053123	4.815611
257.635663	8000.089206	13.059648	-0.053102	4.815593
257.813004	8000.162582	13.064653	-0.053135	4.815614
257.618151	8000.107078	13.069658	-0.053099	4.815598
257.623681	8000.106102	13.074663	-0.053100	4.815598
257.718943	8000.164257	13.079667	-0.053118	4.815615
257.711330	8000.131029	13.084672	-0.053116	4.815605
257.649991	8000.133234	13.089677	-0.053105	4.815606
257.717944	8000.134344	13.094682	-0.053117	4.815606
257.837667	8000.142706	13.099687	-0.053140	4.815608
257.645190	8000.156655	13.104691	-0.053104	4.815613
257.544612	8000.119776	13.109696	-0.053085	4.815602
257.771940	8000.140571	13.114701	-0.053128	4.815607
257.562933	8000.116874	13.119706	-0.053089	4.815601
257.617182	8000.141254	13.124711	-0.053099	4.815608
257.660521	8000.123809	13.129715	-0.053107	4.815603
257.697252	8000.085965	13.134720	-0.053114	4.815592
257.815919	8000.133822	13.139725	-0.053136	4.815605
257.644078	8000.120342	13.144730	-0.053104	4.815602
257.605792	8000.100497	13.149735	-0.053097	4.815596
257.770629	8000.145903	13.154739	-0.053127	4.815609
257.742657	8000.135837	13.159744	-0.053122	4.815606
257.796884	8000.166625	13.164749	-0.053132	4.815615
257.838360	8000.157692	13.169754	-0.053140	4.815612
257.750974	8000.131707	13.174759	-0.053124	4.815605
257.677947	8000.127314	13.179763	-0.053110	4.815604
257.595026	8000.113148	13.184768	-0.053095	4.815600
257.660936	8000.181503	13.189773	-0.053107	4.815620
257.737834	8000.187031	13.194778	-0.053122	4.815621
257.881990	8000.145599	13.199783	-0.053148	4.815608
257.876481	8000.252303	13.204787	-0.053147	4.815640
257.864661	8000.155999	13.209792	-0.053145	4.815611
257.905385	8000.159869	13.214797	-0.053153	4.815612
258.021758	8000.174583	13.219802	-0.053175	4.815616
257.802991	8000.140048	13.224807	-0.053134	4.815607
257.808169	8000.142270	13.229811	-0.053135	4.815608
257.723526	8000.110989	13.234816	-0.053119	4.815599
257.719663	8000.173935	13.239821	-0.053118	4.815617
257.680393	8000.158345	13.244826	-0.053111	4.815613
257.675527	8000.141181	13.249831	-0.053110	4.815608
257.764259	8000.216316	13.254835	-0.053127	4.815630
257.500051	8000.170360	13.259840	-0.053078	4.815617
257.664057	8000.206142	13.264845	-0.053108	4.815627
257.680122	8000.159417	13.269850	-0.053111	4.815613
257.700813	8000.115972	13.274855	-0.053115	4.815601
257.874658	8000.170069	13.279859	-0.053147	4.815616
257.678611	8000.126293	13.284864	-0.053111	4.815604
257.908630	8000.179170	13.289869	-0.053154	4.815618
257.896758	8000.120243	13.294874	-0.053152	4.815601
257.887243	8000.106206	13.299879	-0.053150	4.815597
257.804954	8000.150786	13.304883	-0.053134	4.815610
257.622096	8000.133923	13.309888	-0.053100	4.815606
257.718039	8000.192089	13.314893	-0.053118	4.815623
257.707701	8000.158817	13.319898	-0.053116	4.815613
257.533226	8000.157041	13.324903	-0.053084	4.815613
257.816660	8000.248166	13.329907	-0.053137	4.815639
257.754302	8000.137156	13.334912	-0.053125	4.815606
257.810965	8000.190409	13.339917	-0.053136	4.815622
257.847726	8000.151498	13.344922	-0.053143	4.815610
257.829784	8000.157614	13.349927	-0.053139	4.815612
257.866923	8000.197735	13.354931	-0.053146	4.815624
257.771325	8000.159868	13.359936	-0.053128	4.815613
257.836626	8000.192972	13.364941	-0.053141	4.815622
257.764711	8000.222771	13.369946	-0.053127	4.815631
257.779975	8000.142928	13.374951	-0.053130	4.815608
257.561362	8000.214118	13.379955	-0.053089	4.815630
257.750643	8000.124298	13.384960	-0.053125	4.815603
257.665338	8000.139995	13.389965	-0.053109	4.815608
257.593591	8000.114265	13.394970	-0.053095	4.815601
257.641112	8000.137468	13.399975	-0.053104	4.815607
257.798516	8000.165667	13.404979	-0.053134	4.815615
257.778643	8000.132239	13.409984	-0.053130	4.815605
257.738366	8000.157214	13.414989	-0.053123	4.815612
257.880461	8000.210793	13.419994	-0.053149	4.815627
257.624745	8000.156432	13.424999	-0.053101	4.815613
257.682052	8000.205424	13.430003	-0.053112	4.815627
257.763160	8000.213156	13.435008	-0.053127	4.815629
257.712191	8000.149320	13.440013	-0.053118	4.815610
257.739374	8000.159376	13.445018	-0.053123	4.815613
257.747798	8000.155244	13.450023	-0.053124	4.815612
257.834108	8000.188691	13.455027	-0.053141	4.815621
257.671697	8000.130512	13.460032	-0.053110	4.815605
257.880470	8000.168092	13.465037	-0.053149	4.815615
257.823794	8000.125521	13.470042	-0.053139	4.815603
257.874177	8000.146634	13.475047	-0.053148	4.815609
257.956700	8000.221668	13.480051	-0.053163	4.815630
257.854284	8000.118548	13.485056	-0.053144	4.815601
257.798514	8000.213752	13.490061	-0.053134	4.815629
257.630131	8000.155476	13.495066	-0.053103	4.815612
257.848612	8000.151566	13.500071	-0.053143	4.815610
258.022505	8000.191781	13.505075	-0.053176	4.815621
257.793065	8000.130373	13.510080	-0.053133	4.815604
257.685788	8000.143576	13.515085	-0.053113	4.815609
257.693897	8000.146913	13.520090	-0.053115	4.815610
257.994332	8000.148611	13.525095	-0.053171	4.815609
257.842783	8000.190994	13.530099	-0.053142	4.815622
257.768566	8000.137457	13.535104	-0.053129	4.815606
257.908692	8000.169646	13.540109	-0.053155	4.815615
257.862858	8000.188123	13.545114	-0.053146	4.815621
257.816005	8000.190564	13.550119	-0.053138	4.815622
257.627417	8000.171471	13.555123	-0.053102	4.815617
257.650439	8000.113113	13.560128	-0.053107	4.815600
257.647482	8000.119474	13.565133	-0.053106	4.815602
257.732441	8000.127269	13.570138	-0.053122	4.815604
257.737095	8000.144433	13.575143	-0.053123	4.815609
257.969981	8000.171727	13.580147	-0.053166	4.815616
257.778885	8000.150458	13.585152	-0.053131	4.815610
257.949100	8000.216243	13.590157	-0.053162	4.815629
257.941973	8000.096522	13.595162	-0.053161	4.815594
257.847806	8000.129161	13.600167	-0.053144	4.815604
257.833303	8000.095821	13.605171	-0.053141	4.815594
257.893947	8000.074385	13.610176	-0.053152	4.815587
257.853820	8000.146351	13.615181	-0.053145	4.815609
257.849055	8000.152682	13.620186	-0.053144	4.815611
257.747882	8000.143558	13.625191	-0.053125	4.815608
257.781290	8000.186822	13.630195	-0.053131	4.815621
257.693335	8000.158691	13.635200	-0.053115	4.815613
257.837162	8000.188804	13.640205	-0.053142	4.815621
257.807446	8000.145605	13.645210	-0.053136	4.815609
257.899246	8000.144968	13.650215	-0.053153	4.815608
257.847843	8000.182576	13.655219	-0.053144	4.815619
257.939801	8000.204368	13.660224	-0.053161	4.815625
257.845731	8000.231669	13.665229	-0.053144	4.815634
257.899022	8000.222929	13.670234	-0.053153	4.815631
257.722057	8000.176260	13.675239	-0.053121	4.815618
257.828026	8000.244201	13.680243	-0.053140	4.815637
257.648135	8000.232725	13.685248	-0.053107	4.815635
257.858008	8000.217995	13.690253	-0.053146	4.815630
257.790996	8000.239330	13.695258	-0.053133	4.815636
257.637474	8000.209062	13.700263	-0.053105	4.815628
257.780339	8000.199647	13.705267	-0.053131	4.815625
258.066086	8000.169068	13.710272	-0.053185	4.815614
257.968322	8000.211260	13.715277	-0.053167	4.815627
257.642747	8000.161099	13.720282	-0.053106	4.815614
257.820708	8000.169343	13.725287	-0.053139	4.815616
257.860886	8000.172136	13.730291	-0.053147	4.815616
257.827072	8000.117122	13.735296	-0.053140	4.815600
258.059613	8000.167905	13.740301	-0.053184	4.815614
257.997596	8000.176506	13.745306	-0.053172	4.815617
257.681302	8000.131837	13.750311	-0.053113	4.815605
257.867430	8000.202153	13.755315	-0.053148	4.815625
257.772611	8000.144008	13.760320	-0.053130	4.815608
257.840101	8000.180352	13.765325	-0.053143	4.815619
257.717064	8000.130291	13.770330	-0.053120	4.815605
257.827625	8000.106466	13.775335	-0.053141	4.815597
258.061427	8000.178628	13.780339	-0.053184	4.815617
257.592114	8000.147481	13.785344	-0.053097	4.815610
257.949078	8000.181070	13.790349	-0.053163	4.815618
258.066084	8000.164826	13.795354	-0.053185	4.815613
257.967739	8000.095945	13.800359	-0.053167	4.815593
257.838072	8000.173925	13.805363	-0.053143	4.815617
257.812106	8000.107293	13.810368	-0.053138	4.815597
257.856243	8000.131508	13.815373	-0.053146	4.815604
257.740239	8000.160588	13.820378	-0.053124	4.815613
257.901999	8000.149345	13.825383	-0.053155	4.815609
257.918686	8000.142143	13.830387	-0.053158	4.815607
258.029022	8000.130062	13.835392	-0.053178	4.815603
258.083769	8000.146975	13.840397	-0.053188	4.815608
258.082989	8000.122402	13.845402	-0.053188	4.815601
258.005262	8000.128611	13.850407	-0.053174	4.815603
258.053033	8000.147547	13.855411	-0.053183	4.815608
258.062126	8000.146629	13.860416	-0.053185	4.815608
257.800220	8000.131680	13.865421	-0.053136	4.815605
257.795781	8000.179665	13.870426	-0.053135	4.815619
257.789432	8000.114421	13.875431	-0.053134	4.815600
257.915794	8000.157064	13.880435	-0.053157	4.815611
257.831724	8000.179189	13.885440	-0.053142	4.815618
257.866086	8000.264117	13.890445	-0.053148	4.815643
257.831553	8000.204819	13.895450	-0.053142	4.815626
257.929412	8000.149818	13.900455	-0.053160	4.815609
257.874541	8000.235426	13.905459	-0.053150	4.815635
257.721366	8000.150700	13.910464	-0.053121	4.815611
257.905016	8000.180395	13.915469	-0.053156	4.815618
257.957012	8000.204739	13.920474	-0.053165	4.815625
257.906017	8000.155852	13.925479	-0.053156	4.815611
258.105981	8000.210376	13.930483	-0.053193	4.815626
257.857323	8000.160401	13.935488	-0.053147	4.815613
257.799228	8000.133825	13.940493	-0.053136	4.815605
257.877185	8000.128691	13.945498	-0.053150	4.815603
257.644119	8000.115281	13.950503	-0.053107	4.815601
257.745840	8000.161794	13.955507	-0.053126	4.815614
257.869799	8000.112557	13.960512	-0.053149	4.815599
257.903236	8000.124851	13.965517	-0.053155	4.815602
257.920529	8000.124067	13.970522	-0.053159	4.815602
257.887714	8000.150231	13.975527	-0.053153	4.815610
258.006213	8000.208766	13.980531	-0.053175	4.815626
257.750875	8000.151207	13.985536	-0.053127	4.815611
257.817343	8000.180058	13.990541	-0.053139	4.815619
257.796669	8000.158365	13.995546	-0.053136	4.815612
257.800829	8000.159502	14.000551	-0.053136	4.815613
257.691266	8000.159853	14.005555	-0.053116	4.815613
257.686373	8000.090361	14.010560	-0.053115	4.815593
257.846248	8000.138890	14.015565	-0.053145	4.815606
257.723938	8000.120878	14.020570	-0.053122	4.815602
257.811849	8000.093480	14.025575	-0.053139	4.815593
257.886603	8000.165183	14.030579	-0.053153	4.815614
257.782473	8000.147468	14.035584	-0.053133	4.815609
257.993555	8000.206444	14.040589	-0.053173	4.815626
258.071905	8000.201316	14.045594	-0.053187	4.815624
257.983759	8000.182793	14.050599	-0.053171	4.815619
257.941144	8000.217341	14.055603	-0.053163	4.815629
257.885673	8000.182265	14.060608	-0.053152	4.815619
257.915820	8000.109072	14.065613	-0.053158	4.815597
257.936298	8000.163872	14.070618	-0.053162	4.815613
258.024707	8000.151432	14.075623	-0.053178	4.815609
258.037704	8000.173004	14.080627	-0.053181	4.815616
258.032572	8000.141953	14.085632	-0.053180	4.815606
258.041179	8000.152774	14.090637	-0.053182	4.815610
258.175878	8000.141090	14.095642	-0.053207	4.815606
258.034923	8000.135589	14.100647	-0.053180	4.815605
258.023556	8000.156764	14.105651	-0.053178	4.815611
258.036755	8000.172999	14.110656	-0.053181	4.815616
257.984004	8000.139035	14.115661	-0.053171	4.815606
258.022105	8000.166356	14.120666	-0.053178	4.815614
258.008253	8000.134095	14.125671	-0.053176	4.815604
258.137822	8000.158636	14.130675	-0.053200	4.815611
257.957152	8000.115110	14.135680	-0.053166	4.815599
257.833034	8000.104544	14.140685	-0.053143	4.815596
258.011221	8000.168323	14.145690	-0.053176	4.815614
257.904078	8000.120657	14.150695	-0.053156	4.815601
257.851302	8000.206299	14.155699	-0.053146	4.815626
257.881985	8000.137387	14.160704	-0.053152	4.815606
257.974635	8000.148511	14.165709	-0.053169	4.815609
258.074766	8000.155485	14.170714	-0.053188	4.815610
257.868075	8000.128622	14.175719	-0.053150	4.815603
258.012894	8000.197196	14.180723	-0.053177	4.815623
257.957258	8000.156778	14.185728	-0.053166	4.815611
257.867006	8000.133949	14.190733	-0.053150	4.815605
258.014160	8000.216445	14.195738	-0.053177	4.815628
258.087832	8000.118332	14.200743	-0.053191	4.815599
258.042671	8000.131480	14.205747	-0.053182	4.815603
257.815798	8000.137393	14.210752	-0.053140	4.815606
258.229539	8000.154822	14.215757	-0.053217	4.815609
257.986693	8000.150862	14.220762	-0.053172	4.815609
257.800107	8000.151025	14.225767	-0.053137	4.815610
257.914092	8000.166768	14.230771	-0.053158	4.815614
257.870728	8000.100920	14.235776	-0.053150	4.815595
257.802443	8000.111555	14.240781	-0.053138	4.815599
257.766986	8000.144084	14.245786	-0.053131	4.815608
257.874673	8000.095650	14.250791	-0.053151	4.815594
257.843288	8000.169894	14.255795	-0.053145	4.815616
257.769625	7999.224686	14.260800	-0.053131	4.815340

258.024484	7996.042659	14.265805	-0.053176	4.814408
258.173899	7990.583868	14.270810	-0.053201	4.812811
257.763711	7983.884602	14.275815	-0.053120	4.810853
257.863216	7976.607576	14.280819	-0.053134	4.808722
258.008689	7968.981650	14.285824	-0.053156	4.806488
257.812902	7961.168602	14.290829	-0.053114	4.804200
257.766646	7953.365886	14.295834	-0.053101	4.801913
258.005089	7945.352988	14.300839	-0.053140	4.799563
257.846678	7937.460403	14.305843	-0.053105	4.797248
257.482580	7929.381553	14.310848	-0.053032	4.794878
257.575907	7921.377198	14.315853	-0.053044	4.792526
257.724252	7913.364780	14.320858	-0.053067	4.790172
257.583666	7905.439267	14.325863	-0.053036	4.787842
257.551986	7897.364241	14.330867	-0.053024	4.785467
257.536096	7889.433469	14.335872	-0.053016	4.783134
257.411883	7881.381089	14.340877	-0.052988	4.780763
257.435425	7873.412068	14.345882	-0.052987	4.778416
257.559196	7865.384723	14.350887	-0.053005	4.776050
257.501565	7857.388627	14.355891	-0.052989	4.773692
257.262264	7849.365643	14.360896	-0.052939	4.771326
257.354223	7841.332891	14.365901	-0.052951	4.768955
257.453449	7833.446892	14.370906	-0.052965	4.766626
257.229472	7825.334726	14.375911	-0.052918	4.764230
257.348603	7817.443059	14.380915	-0.052935	4.761897
257.376869	7809.336742	14.385920	-0.052935	4.759500
257.235663	7801.408726	14.390925	-0.052903	4.757155
257.083088	7793.398095	14.395930	-0.052870	4.754784
257.172114	7785.335195	14.400935	-0.052881	4.752396
257.300083	7777.328361	14.405939	-0.052900	4.750023
257.104602	7769.315702	14.410944	-0.052858	4.747648
257.094812	7761.289099	14.415949	-0.052851	4.745267
257.156921	7753.364038	14.420954	-0.052857	4.742915
257.182109	7745.283787	14.425959	-0.052857	4.740515
257.089136	7737.370355	14.430963	-0.052834	4.738165
257.101970	7729.331708	14.435968	-0.052832	4.735776
256.965070	7721.318781	14.440973	-0.052801	4.733393
256.868209	7713.348092	14.445978	-0.052778	4.731022
256.863684	7705.254368	14.450983	-0.052772	4.728613
256.970281	7697.320883	14.455987	-0.052786	4.726250
256.494298	7689.277277	14.460992	-0.052692	4.723854
256.664888	7681.324112	14.465997	-0.052719	4.721483
256.913566	7673.321129	14.471002	-0.052760	4.719095
256.812056	7665.346428	14.476007	-0.052736	4.716715
256.557349	7657.346347	14.481011	-0.052683	4.714327
256.458905	7649.319258	14.486016	-0.052660	4.711930
256.534255	7641.233925	14.491021	-0.052669	4.709513
256.567858	7633.287056	14.496026	-0.052670	4.707137
256.439619	7625.291907	14.501031	-0.052641	4.704745
256.619885	7617.336420	14.506035	-0.052669	4.702363
256.540176	7609.300791	14.511040	-0.052649	4.699957
256.574272	7601.325281	14.516045	-0.052650	4.697567
256.491506	7593.332247	14.521050	-0.052630	4.695171
256.318366	7585.261604	14.526055	-0.052592	4.692750
256.301371	7577.264790	14.531059	-0.052584	4.690350
256.375316	7569.296528	14.536064	-0.052592	4.687957
256.314849	7561.272328	14.541069	-0.052576	4.685547
256.285962	7553.357343	14.546074	-0.052565	4.683168
256.332185	7545.270357	14.551079	-0.052569	4.680736
256.278486	7537.318798	14.556083	-0.052554	4.678344
256.091686	7529.303287	14.561088	-0.052514	4.675931
256.121343	7521.233949	14.566093	-0.052514	4.673500
256.355416	7513.122086	14.571098	-0.052552	4.671056
256.134284	7505.185295	14.576103	-0.052506	4.668663
256.149242	7497.236054	14.581107	-0.052503	4.666265
255.819648	7489.224392	14.586112	-0.052437	4.663847
256.095771	7481.224460	14.591117	-0.052483	4.661431
255.849824	7473.244282	14.596122	-0.052432	4.659020
255.792326	7465.270005	14.601127	-0.052416	4.656610
255.795034	7457.257767	14.606131	-0.052412	4.654186
255.841444	7449.184860	14.611136	-0.052415	4.651743
255.678113	7441.185701	14.616141	-0.052379	4.649322
255.709038	7433.277833	14.621146	-0.052380	4.646926
255.732490	7425.177327	14.626151	-0.052379	4.644471
255.820697	7417.251077	14.631155	-0.052390	4.642067
255.718445	7409.204045	14.636160	-0.052366	4.639626
255.747195	7401.266412	14.641165	-0.052366	4.637216
255.541551	7393.230782	14.646170	-0.052323	4.634776
255.517185	7385.184326	14.651175	-0.052313	4.632331
255.605790	7377.144329	14.656179	-0.052324	4.629886
255.616591	7369.215177	14.661184	-0.052321	4.627474
255.491624	7361.183399	14.666189	-0.052293	4.625030
255.517013	7353.255441	14.671194	-0.052292	4.622616
255.495141	7345.162576	14.676199	-0.052283	4.620150
255.360882	7337.218381	14.681203	-0.052253	4.617728
255.326328	7329.193486	14.686208	-0.052241	4.615280
255.353807	7321.169794	14.691213	-0.052241	4.612832
255.280817	7313.160614	14.696218	-0.052222	4.610386
255.207592	7305.136309	14.701223	-0.052203	4.607935
255.395356	7297.164120	14.706227	-0.052233	4.605498
255.269425	7289.175956	14.711232	-0.052205	4.603055
255.126692	7281.145186	14.716237	-0.052173	4.600598
255.121027	7273.212388	14.721242	-0.052167	4.598169
255.055982	7265.201344	14.726247	-0.052149	4.595715
255.114268	7257.170983	14.731251	-0.052155	4.593254
255.178697	7249.091971	14.736256	-0.052162	4.590777
255.280216	7241.104716	14.741261	-0.052175	4.588327
255.126606	7233.135490	14.746266	-0.052142	4.585880
254.800319	7225.122228	14.751271	-0.052076	4.583419
255.046817	7217.165724	14.756275	-0.052116	4.580974
254.982340	7209.164520	14.761280	-0.052099	4.578514
254.969783	7201.142129	14.766285	-0.052092	4.576046
254.972039	7193.176760	14.771290	-0.052087	4.573594
254.780614	7185.068363	14.776295	-0.052046	4.571097
254.707980	7177.137262	14.781299	-0.052027	4.568653
254.671537	7169.097929	14.786304	-0.052015	4.566174
254.857934	7161.082329	14.791309	-0.052045	4.563702
254.783299	7153.138848	14.796314	-0.052026	4.561250
254.629699	7145.129269	14.801319	-0.051992	4.558777
254.691404	7137.199894	14.806323	-0.051998	4.556327
254.644895	7129.139993	14.811328	-0.051984	4.553835
254.562186	7121.085718	14.816333	-0.051964	4.551344
254.617223	7113.122926	14.821338	-0.051969	4.548880
254.700590	7105.104812	14.826343	-0.051979	4.546397
254.456365	7097.141227	14.831347	-0.051928	4.543929
254.246943	7089.144618	14.836352	-0.051884	4.541450
254.529347	7081.109295	14.841357	-0.051932	4.538959
254.332073	7073.189843	14.846362	-0.051890	4.536501
254.064524	7065.086232	14.851367	-0.051835	4.533984
254.393902	7057.080796	14.856371	-0.051891	4.531498
254.377042	7049.067899	14.861376	-0.051883	4.529007
254.319975	7041.097837	14.866381	-0.051867	4.526528
254.412152	7033.115065	14.871386	-0.051879	4.524044
254.365595	7025.113602	14.876391	-0.051865	4.521553
254.130146	7017.112978	14.881395	-0.051816	4.519060
254.078832	7009.168527	14.886400	-0.051801	4.516584
254.233715	7001.054704	14.891405	-0.051825	4.514053
254.182216	6993.073070	14.896410	-0.051810	4.511563
254.082255	6985.030294	14.901415	-0.051786	4.509051
254.044955	6977.071446	14.906419	-0.051774	4.506565
254.024447	6969.037981	14.911424	-0.051765	4.504054
253.915026	6961.070677	14.916429	-0.051739	4.501562
253.958496	6953.081518	14.921434	-0.051742	4.499062
253.860154	6945.100093	14.926439	-0.051719	4.496563
253.949290	6937.080537	14.931443	-0.051730	4.494051
253.805407	6929.056724	14.936448	-0.051698	4.491536
253.789836	6921.012327	14.941453	-0.051690	4.489013
253.611285	6913.110364	14.946458	-0.051652	4.486533
253.600197	6905.020276	14.951463	-0.051644	4.483993
253.649472	6897.094115	14.956467	-0.051648	4.481503
253.662716	6889.073432	14.961472	-0.051646	4.478982
253.641918	6881.100308	14.966477	-0.051637	4.476474
253.659316	6873.067770	14.971482	-0.051635	4.473947
253.638682	6865.025328	14.976487	-0.051626	4.471414
253.631591	6856.998202	14.981491	-0.051619	4.468886
253.412683	6849.009763	14.986496	-0.051573	4.466367
253.700689	6840.998201	14.991501	-0.051621	4.463841
253.634745	6833.056614	14.996506	-0.051604	4.461335
253.458257	6825.022014	15.001511	-0.051566	4.458797
253.211412	6817.013681	15.006515	-0.051515	4.456266
253.317413	6809.033232	15.011520	-0.051529	4.453744
253.401077	6801.005254	15.016525	-0.051540	4.451205
253.156416	6793.039325	15.021530	-0.051489	4.448683
253.106670	6785.013367	15.026535	-0.051475	4.446141
253.627220	6777.021882	15.031539	-0.051566	4.443612
253.419116	6769.008146	15.036544	-0.051522	4.441070
253.334652	6761.043644	15.041549	-0.051501	4.438544
253.387119	6753.073952	15.046554	-0.051506	4.436015
253.375661	6744.984869	15.051559	-0.051499	4.433446
253.182805	6736.948258	15.056563	-0.051457	4.430891
253.183905	6728.976393	15.061568	-0.051453	4.428357
253.092563	6720.948640	15.066573	-0.051430	4.425803
253.036274	6712.995648	15.071578	-0.051415	4.423271
253.064292	6704.952871	15.076583	-0.051415	4.420710
253.130365	6697.017993	15.081587	-0.051422	4.418182
252.940019	6688.982937	15.086592	-0.051381	4.415619
252.817618	6680.974070	15.091597	-0.051353	4.413063
252.751235	6672.970969	15.096602	-0.051336	4.410508
252.638849	6664.975230	15.101607	-0.051309	4.407954
252.584418	6656.993006	15.106611	-0.051294	4.405402
252.853085	6649.019902	15.111616	-0.051339	4.402854
252.755043	6640.997892	15.116621	-0.051316	4.400287
252.755033	6633.051108	15.121626	-0.051310	4.397743
252.536431	6624.997669	15.126631	-0.051264	4.395162
252.570521	6616.978800	15.131635	-0.051266	4.392592
252.700043	6608.932794	15.136640	-0.051284	4.390012
252.549247	6600.975175	15.141645	-0.051251	4.387458
252.473491	6592.992737	15.146650	-0.051232	4.384894
252.409288	6585.003141	15.151655	-0.051215	4.382327
252.544498	6577.001052	15.156659	-0.051235	4.379756
252.442014	6569.012824	15.161664	-0.051211	4.377185
252.239437	6560.999187	15.166669	-0.051168	4.374605
252.415315	6552.964873	15.171674	-0.051195	4.372019
252.131670	6544.939094	15.176679	-0.051137	4.369431
252.439796	6536.994980	15.181683	-0.051189	4.366872
252.214550	6529.005716	15.186688	-0.051142	4.364293
252.093334	6521.002807	15.191693	-0.051114	4.361709
252.244077	6513.031234	15.196698	-0.051137	4.359135
252.055639	6505.019872	15.201703	-0.051097	4.356545
251.910391	6496.989329	15.206707	-0.051065	4.353947
252.035781	6488.918614	15.211712	-0.051083	4.351336
251.911518	6480.887690	15.216717	-0.051055	4.348735
251.925373	6472.961863	15.221722	-0.051052	4.346168
251.723285	6464.943161	15.226727	-0.051009	4.343567
251.843818	6456.972601	15.231731	-0.051026	4.340983
251.791679	6448.934439	15.236736	-0.051011	4.338374
251.817930	6440.969624	15.241741	-0.051011	4.335787
251.699656	6432.994432	15.246746	-0.050984	4.333195
251.429910	6424.957294	15.251751	-0.050929	4.330580
251.466939	6416.959630	15.256755	-0.050930	4.327979
251.501708	6408.934219	15.261760	-0.050932	4.325366
251.591941	6400.960319	15.266765	-0.050943	4.322770
251.522178	6393.002456	15.271770	-0.050925	4.320176
251.381760	6384.984024	15.276775	-0.050894	4.317560
251.402084	6376.961084	15.281779	-0.050892	4.314942
251.439130	6368.906302	15.286784	-0.050894	4.312312
251.379544	6360.907404	15.291789	-0.050878	4.309699
251.438197	6352.959297	15.296794	-0.050883	4.307101
251.432739	6344.884865	15.301799	-0.050877	4.304460
251.230791	6336.953602	15.306803	-0.050834	4.301862
251.344031	6328.963385	15.311808	-0.050850	4.299246
251.241546	6320.975622	15.316813	-0.050826	4.296628
251.195454	6312.983780	15.321818	-0.050812	4.294007
251.086699	6304.878538	15.326823	-0.050787	4.291347
251.174883	6296.943633	15.331827	-0.050798	4.288742
251.213313	6288.934963	15.336832	-0.050800	4.286112
251.044196	6280.897524	15.341837	-0.050763	4.283468
251.270491	6272.934751	15.346842	-0.050800	4.280851
251.286993	6264.911029	15.351847	-0.050798	4.278211
251.079234	6256.948293	15.356851	-0.050754	4.275586
251.047066	6248.877987	15.361856	-0.050743	4.272927
251.014145	6240.850607	15.366861	-0.050732	4.270280
251.125445	6232.898197	15.371866	-0.050747	4.267657
250.999392	6224.862424	15.376871	-0.050718	4.265003
250.946850	6216.962010	15.381875	-0.050704	4.262393
250.835546	6208.903761	15.386880	-0.050678	4.259728
250.983199	6200.917158	15.391885	-0.050700	4.257088
251.116490	6192.894358	15.396890	-0.050720	4.254434
250.952642	6184.900746	15.401895	-0.050684	4.251785
250.745973	6176.866287	15.406899	-0.050640	4.249121
250.788660	6168.891158	15.411904	-0.050643	4.246477
250.845346	6160.876380	15.416909	-0.050648	4.243818
250.802354	6152.964387	15.421914	-0.050635	4.241191
250.597906	6144.893768	15.426919	-0.050592	4.238508
250.523560	6136.965440	15.431923	-0.050573	4.235871
250.565067	6128.938330	15.436928	-0.050575	4.233202
250.414493	6120.932191	15.441933	-0.050542	4.230536
250.427560	6112.931987	15.446938	-0.050539	4.227871
250.418440	6104.900961	15.451943	-0.050532	4.225195
250.475898	6096.934825	15.456947	-0.050538	4.222539
250.374122	6088.924202	15.461952	-0.050514	4.219865
250.498633	6080.939931	15.466957	-0.050532	4.217200
250.495795	6072.962657	15.471962	-0.050526	4.214535
250.245166	6064.935451	15.476967	-0.050474	4.211849
250.371463	6056.889771	15.481971	-0.050493	4.209159
250.295004	6048.988786	15.486976	-0.050473	4.206513
250.089365	6040.929108	15.491981	-0.050430	4.203811
250.111886	6032.967198	15.496986	-0.050429	4.201143
250.237891	6024.968004	15.501991	-0.050447	4.198461
250.229667	6016.950228	15.506995	-0.050440	4.195771
250.093859	6008.849666	15.512000	-0.050410	4.193049
250.038138	6000.802012	15.517005	-0.050394	4.190344
250.135379	5992.914296	15.522010	-0.050407	4.187693
249.865933	5984.851434	15.527015	-0.050352	4.184977
249.892898	5976.937197	15.532019	-0.050351	4.182313
249.928384	5968.946198	15.537024	-0.050353	4.179621
249.840279	5960.921837	15.542029	-0.050331	4.176915
249.867329	5952.946078	15.547034	-0.050331	4.174224
249.930616	5944.886411	15.552039	-0.050338	4.171505
249.575809	5936.915334	15.557043	-0.050266	4.168808
249.723008	5928.908588	15.562048	-0.050289	4.166103
249.782304	5920.888753	15.567053	-0.050295	4.163392
249.842352	5912.931277	15.572058	-0.050301	4.160699
249.608136	5904.930072	15.577063	-0.050252	4.157987
249.682167	5896.937346	15.582067	-0.050260	4.155279
249.955680	5888.874764	15.587072	-0.050306	4.152548
249.634665	5880.844608	15.592077	-0.050241	4.149820
249.675937	5872.914676	15.597082	-0.050244	4.147128
249.450149	5864.856032	15.602087	-0.050196	4.144387
249.611056	5856.922173	15.607091	-0.050221	4.141691
249.552778	5848.938876	15.612096	-0.050205	4.138974
249.437466	5840.903313	15.617101	-0.050178	4.136237
249.659075	5832.909507	15.622106	-0.050214	4.133517
249.358877	5824.860182	15.627111	-0.050153	4.130769
249.370577	5816.928468	15.632115	-0.050150	4.128064
249.395226	5808.889935	15.637120	-0.050150	4.125320
249.513092	5800.888028	15.642125	-0.050166	4.122588
249.215222	5792.929633	15.647130	-0.050106	4.119864
248.989492	5784.973942	15.652135	-0.050059	4.117140
249.055626	5776.886837	15.657139	-0.050066	4.114373
248.866289	5768.870365	15.662144	-0.050025	4.111625
248.770419	5760.863994	15.667149	-0.050002	4.108880
249.039693	5752.904634	15.672154	-0.050047	4.106154
248.952560	5744.879514	15.677159	-0.050026	4.103399
248.803984	5736.923990	15.682163	-0.049993	4.100665
248.887496	5728.946707	15.687168	-0.050003	4.097925
248.926589	5720.875714	15.692173	-0.050005	4.095150
248.835544	5712.920472	15.697178	-0.049983	4.092411
248.789154	5704.856459	15.702183	-0.049969	4.089634
248.726285	5696.957107	15.707187	-0.049952	4.086911
248.729139	5688.918340	15.712192	-0.049948	4.084140
248.711673	5680.943736	15.717197	-0.049939	4.081388
248.855994	5672.950878	15.722202	-0.049961	4.078630
248.630362	5664.967403	15.727207	-0.049914	4.075869
248.448926	5656.938909	15.732211	-0.049875	4.073091
248.712461	5648.927687	15.737216	-0.049919	4.070323
248.614831	5640.907692	15.742221	-0.049895	4.067545
248.897554	5632.908271	15.747226	-0.049943	4.064777
248.430030	5624.940566	15.752231	-0.049851	4.062008
248.430868	5616.960926	15.757235	-0.049846	4.059240
248.297264	5608.994120	15.762240	-0.049815	4.056472
248.328885	5600.932486	15.767245	-0.049816	4.053672
248.528380	5592.939402	15.772250	-0.049848	4.050897
248.452882	5584.950746	15.777255	-0.049829	4.048116
248.441838	5576.915579	15.782259	-0.049822	4.045319
248.399727	5568.991229	15.787264	-0.049809	4.042558
248.353509	5560.938198	15.792269	-0.049795	4.039750
248.275823	5553.005766	15.797274	-0.049775	4.036982
248.212244	5544.935159	15.802279	-0.049758	4.034164
248.372549	5536.814076	15.807283	-0.049783	4.031329
248.198347	5528.859608	15.812288	-0.049745	4.028546
248.014593	5520.864742	15.817293	-0.049706	4.025746
248.025968	5512.921344	15.822298	-0.049703	4.022966
248.089284	5504.950860	15.827303	-0.049709	4.020175
247.921122	5496.924912	15.832307	-0.049673	4.017359
248.041576	5488.909634	15.837312	-0.049690	4.014549
248.077274	5480.895706	15.842317	-0.049691	4.011736
247.999854	5472.887132	15.847322	-0.049672	4.008922
247.747879	5464.900072	15.852327	-0.049620	4.006110
247.930814	5456.930115	15.857331	-0.049649	4.003309
248.019616	5448.946005	15.862336	-0.049660	4.000500
247.713380	5440.952710	15.867341	-0.049598	3.997680
247.892008	5432.963347	15.872346	-0.049626	3.994866
247.821151	5424.883973	15.877351	-0.049607	3.992015
247.721834	5416.896592	15.882355	-0.049584	3.989193
247.765213	5408.925959	15.887360	-0.049587	3.986378
247.621965	5400.922851	15.892365	-0.049555	3.983547
247.664671	5392.957383	15.897370	-0.049557	3.980729
247.499022	5384.969421	15.902375	-0.049521	3.977898
247.424292	5376.963555	15.907379	-0.049502	3.975061
247.548764	5368.938167	15.912384	-0.049520	3.972218
247.396473	5360.891175	15.917389	-0.049487	3.969360
247.521330	5352.965154	15.922394	-0.049505	3.966548
247.422497	5344.936847	15.927399	-0.049481	3.963694
247.425771	5336.972656	15.932403	-0.049477	3.960862
247.288334	5329.030613	15.937408	-0.049446	3.958034
247.359025	5320.996566	15.942413	-0.049454	3.955175
247.378597	5312.948900	15.947418	-0.049452	3.952307
247.266610	5304.906504	15.952423	-0.049426	3.949438
247.376472	5296.930831	15.957427	-0.049441	3.946594
247.553892	5288.972397	15.962432	-0.049469	3.943755
247.179071	5281.000663	15.967437	-0.049394	3.940899
247.122514	5272.997246	15.972442	-0.049379	3.938036
247.135097	5264.977920	15.977447	-0.049376	3.935166
247.090784	5256.994308	15.982451	-0.049362	3.932306
246.982232	5248.965770	15.987456	-0.049337	3.929427
246.855379	5241.001522	15.992461	-0.049308	3.926568
247.131105	5233.002750	15.997466	-0.049354	3.923702
246.870845	5225.024793	16.002471	-0.049301	3.920832
247.021974	5217.017914	16.007475	-0.049324	3.917956
247.038754	5209.027206	16.012480	-0.049321	3.915082
246.760667	5201.000308	16.017485	-0.049264	3.912188
246.757118	5192.986966	16.022490	-0.049259	3.909301
246.842219	5185.012183	16.027495	-0.049269	3.906427
246.853277	5176.979617	16.032499	-0.049266	3.903529
246.692558	5169.057927	16.037504	-0.049231	3.900666
246.577869	5161.016204	16.042509	-0.049205	3.897758
246.528182	5153.018548	16.047514	-0.049190	3.894865
246.446633	5144.992322	16.052519	-0.049170	3.891959
246.540694	5137.010229	16.057523	-0.049182	3.889071
246.628527	5128.980975	16.062528	-0.049193	3.886163
246.266504	5121.005792	16.067533	-0.049121	3.883263
246.486153	5113.025360	16.072538	-0.049156	3.880371
246.511781	5105.051766	16.077543	-0.049156	3.877475
246.169310	5097.021551	16.082547	-0.049087	3.874550
246.024047	5088.770693	16.087552	-0.049054	3.871545
246.183001	5080.826104	16.092557	-0.049079	3.868656
246.207658	5072.912698	16.097562	-0.049078	3.865774
246.147091	5064.939663	16.102567	-0.049062	3.862865
246.190936	5056.978053	16.107571	-0.049065	3.859961
246.415274	5049.005642	16.112576	-0.049102	3.857055
246.205513	5040.978600	16.117581	-0.049057	3.854117
246.073733	5033.037079	16.122586	-0.049028	3.851210
245.908334	5024.992634	16.127591	-0.048992	3.848263
246.177082	5016.966817	16.132595	-0.049036	3.845329
245.851053	5009.081676	16.137600	-0.048971	3.842432
246.028139	5001.001622	16.142605	-0.048998	3.839472
246.064406	4993.086998	16.147610	-0.049000	3.836567
245.850825	4985.036207	16.152615	-0.048955	3.833605
245.812191	4977.024235	16.157619	-0.048942	3.830658
245.977089	4969.073002	16.162624	-0.048968	3.827736
245.828922	4961.030427	16.167629	-0.048935	3.824771
245.908509	4953.074238	16.172634	-0.048945	3.821841
245.640275	4945.054460	16.177639	-0.048890	3.818878
245.756790	4937.101656	16.182643	-0.048906	3.815945
245.695913	4929.082410	16.187648	-0.048890	3.812982
245.624510	4921.054003	16.192653	-0.048871	3.810012
245.770534	4913.106088	16.197658	-0.048893	3.807075
245.616148	4905.058779	16.202663	-0.048859	3.804092
245.555332	4897.134483	16.207667	-0.048843	3.801155
245.843557	4889.120024	16.212672	-0.048891	3.798189
245.586244	4881.108653	16.217677	-0.048838	3.795210
245.421149	4873.067128	16.222682	-0.048802	3.792220
245.512338	4865.082256	16.227687	-0.048814	3.789254
245.384751	4857.088145	16.232691	-0.048785	3.786278
245.505414	4849.088021	16.237696	-0.048802	3.783302
245.400525	4841.068336	16.242701	-0.048778	3.780312
245.615817	4833.142871	16.247706	-0.048812	3.777362
245.413924	4825.128322	16.252711	-0.048770	3.774366
245.268271	4817.108459	16.257715	-0.048737	3.771368
245.201764	4809.126129	16.262720	-0.048720	3.768383
244.945969	4801.092473	16.267725	-0.048667	3.765372
245.022487	4793.145036	16.272730	-0.048676	3.762399
244.929464	4785.125979	16.277735	-0.048654	3.759392
245.050717	4777.144284	16.282739	-0.048671	3.756402
244.902071	4769.156485	16.287744	-0.048638	3.753402
245.007365	4761.093741	16.292749	-0.048652	3.750376
245.040220	4753.128324	16.297754	-0.048653	3.747383
244.891762	4745.094301	16.302759	-0.048621	3.744357
244.828869	4737.141894	16.307763	-0.048604	3.741362
244.935390	4729.147972	16.312768	-0.048618	3.738353
244.920303	4721.137487	16.317773	-0.048610	3.735332
244.675352	4713.172007	16.322778	-0.048559	3.732320
244.632645	4705.125881	16.327783	-0.048546	3.729280
244.781290	4697.155082	16.332787	-0.048569	3.726271
244.804030	4689.175596	16.337792	-0.048568	3.723253
244.634006	4681.187708	16.342797	-0.048531	3.720225
244.664091	4673.250392	16.347802	-0.048531	3.717218
244.422262	4665.201209	16.352807	-0.048481	3.714160
244.370983	4657.097133	16.357811	-0.048466	3.711082
244.284018	4649.136033	16.362816	-0.048445	3.708056
244.328851	4641.124482	16.367821	-0.048448	3.705012
244.336821	4633.195725	16.372826	-0.048445	3.701995
244.381250	4625.202209	16.377831	-0.048448	3.698953
244.443434	4617.225557	16.382835	-0.048454	3.695914
244.390074	4609.229491	16.387840	-0.048439	3.692863
244.016470	4601.217026	16.392845	-0.048364	3.689795
244.297178	4593.231853	16.397850	-0.048411	3.686751
244.175436	4585.221893	16.402855	-0.048383	3.683686
243.934218	4577.245362	16.407859	-0.048333	3.680627
244.111241	4569.272940	16.412864	-0.048361	3.677578
244.053682	4561.234008	16.417869	-0.048345	3.674495
244.000644	4553.243037	16.422874	-0.048330	3.671428
243.864535	4545.228600	16.427879	-0.048299	3.668347
244.124897	4537.203147	16.432883	-0.048343	3.665270
244.140649	4529.266597	16.437888	-0.048341	3.662218
243.998521	4521.250088	16.442893	-0.048309	3.659128
243.970810	4513.283666	16.447898	-0.048299	3.656058
243.933781	4505.262270	16.452903	-0.048286	3.652964
243.753219	4497.246192	16.457907	-0.048248	3.649866
243.861633	4489.310093	16.462912	-0.048263	3.646804
243.756876	4481.245134	16.467917	-0.048238	3.643683
243.712078	4473.287854	16.472922	-0.048224	3.640604
243.491047	4465.322128	16.477927	-0.048178	3.637513
243.732178	4457.259541	16.482931	-0.048218	3.634395
243.615313	4449.256038	16.487936	-0.048191	3.631287
243.462365	4441.254727	16.492941	-0.048157	3.628177
243.608596	4433.269937	16.497946	-0.048179	3.625078
243.661660	4425.316908	16.502951	-0.048184	3.621987
243.419583	4417.293602	16.507955	-0.048134	3.618857
243.519689	4409.335718	16.512960	-0.048147	3.615760
243.424487	4401.280776	16.517965	-0.048124	3.612617
243.253521	4393.322234	16.522970	-0.048087	3.609506
243.184533	4385.345004	16.527975	-0.048069	3.606389
243.411334	4377.320081	16.532979	-0.048106	3.603258
243.455200	4369.352609	16.537984	-0.048109	3.600142
243.310474	4361.382435	16.542989	-0.048077	3.597017
243.286128	4353.405028	16.547994	-0.048067	3.593889
243.223605	4345.354601	16.552999	-0.048050	3.590730
243.095258	4337.382817	16.558003	-0.048021	3.587596
243.057079	4329.398025	16.563008	-0.048009	3.584457
242.967510	4321.402563	16.568013	-0.047987	3.581310
243.117154	4313.430830	16.573018	-0.048010	3.578176
243.062175	4305.425528	16.578023	-0.047994	3.575020
242.984978	4297.406005	16.583027	-0.047975	3.571855
243.015764	4289.433135	16.588032	-0.047975	3.568709
242.812838	4281.429205	16.593037	-0.047932	3.565542
242.757887	4273.446025	16.598042	-0.047917	3.562383
242.992394	4265.442218	16.603047	-0.047955	3.559223
242.798979	4257.490575	16.608051	-0.047914	3.556067
242.809674	4249.426995	16.613056	-0.047911	3.552871
242.659703	4241.353565	16.618061	-0.047878	3.549662
242.564035	4233.409154	16.623066	-0.047855	3.546504
242.575477	4225.423801	16.628071	-0.047852	3.543330
242.476485	4217.403714	16.633075	-0.047828	3.540136
242.506031	4209.455664	16.638080	-0.047829	3.536971
242.535376	4201.452888	16.643085	-0.047829	3.533782
242.571321	4193.450572	16.648090	-0.047830	3.530591
242.674344	4185.437881	16.653095	-0.047844	3.527394
242.383641	4177.460057	16.658099	-0.047785	3.524197
242.533611	4169.507446	16.663104	-0.047808	3.521020
242.391410	4161.511837	16.668109	-0.047776	3.517814
242.486327	4153.502276	16.673114	-0.047789	3.514606
242.161193	4145.511301	16.678119	-0.047723	3.511391
242.406305	4137.486928	16.683123	-0.047763	3.508176
242.484582	4129.508326	16.688128	-0.047773	3.504972
242.335259	4121.549201	16.693133	-0.047740	3.501766
242.307689	4113.564727	16.698138	-0.047729	3.498550
242.271812	4105.573546	16.703143	-0.047717	3.495329
242.197451	4097.581929	16.708147	-0.047698	3.492103
242.213127	4089.569820	16.713152	-0.047696	3.488868
242.077466	4081.577015	16.718157	-0.047666	3.485634
241.978579	4073.638948	16.723162	-0.047642	3.482420
242.069231	4065.597740	16.728167	-0.047654	3.479167
242.009413	4057.635203	16.733171	-0.047637	3.475938
242.012088	4049.617447	16.738176	-0.047633	3.472686
241.687869	4041.582450	16.743181	-0.047567	3.469413
241.914491	4033.593481	16.748186	-0.047604	3.466174
241.845251	4025.613254	16.753191	-0.047586	3.462925
241.655069	4017.621106	16.758195	-0.047546	3.459665
241.839926	4009.648613	16.763200	-0.047575	3.456422
241.765879	4001.627080	16.768205	-0.047556	3.453147
241.831766	3993.625607	16.773210	-0.047563	3.449882
241.629644	3985.654102	16.778215	-0.047520	3.446618
241.519497	3977.662203	16.783219	-0.047494	3.443344
241.608806	3969.683105	16.788224	-0.047506	3.440080
241.362308	3961.732780	16.793229	-0.047455	3.436813
241.463390	3953.683439	16.798234	-0.047468	3.433514
241.514696	3945.678537	16.803239	-0.047473	3.430229
241.425808	3937.660892	16.808243	-0.047451	3.426930
241.321473	3929.692477	16.813248	-0.047426	3.423648
241.356432	3921.680130	16.818253	-0.047428	3.420349
241.423138	3913.744034	16.823258	-0.047435	3.417080
241.349993	3905.749185	16.828263	-0.047416	3.413778
241.249878	3897.712974	16.833267	-0.047392	3.410455
241.433077	3889.757705	16.838272	-0.047421	3.407173
241.276396	3881.744840	16.843277	-0.047387	3.403851
240.971017	3873.835904	16.848282	-0.047325	3.400564
240.993174	3865.828331	16.853287	-0.047324	3.397245
240.859028	3857.799591	16.858291	-0.047294	3.393908
240.831302	3849.739824	16.863296	-0.047283	3.390558
240.970549	3841.736995	16.868301	-0.047304	3.387235
241.082182	3833.749539	16.873306	-0.047319	3.383913
241.023482	3825.812005	16.878311	-0.047303	3.380604
240.753082	3817.826925	16.883315	-0.047248	3.377264
240.748368	3809.861659	16.888320	-0.047242	3.373938
240.754754	3801.809233	16.893325	-0.047238	3.370572
240.743208	3793.835004	16.898330	-0.047230	3.367236
240.921533	3785.872548	16.903335	-0.047258	3.363908
240.786901	3777.885199	16.908339	-0.047228	3.360555
240.564607	3769.928302	16.913344	-0.047182	3.357208
240.417896	3761.896415	16.918349	-0.047149	3.353829
240.638647	3753.855789	16.923354	-0.047185	3.350456
240.525328	3745.886935	16.928359	-0.047159	3.347098
240.267557	3737.901639	16.933363	-0.047106	3.343725
240.609734	3729.929319	16.938368	-0.047164	3.340375
240.407085	3721.936196	16.943373	-0.047121	3.336993
240.408760	3713.942288	16.948378	-0.047116	3.333615
240.502965	3705.918876	16.953383	-0.047129	3.330225
240.427488	3697.924381	16.958387	-0.047109	3.326837
240.305837	3689.970841	16.963392	-0.047082	3.323461
240.051649	3681.987117	16.968397	-0.047029	3.320064
240.163272	3674.024926	16.973402	-0.047045	3.316686
240.193872	3666.000175	16.978407	-0.047045	3.313276
239.958900	3657.990376	16.983411	-0.046996	3.309858
239.998143	3650.011459	16.988416	-0.046998	3.306460
240.034384	3642.014659	16.993421	-0.047000	3.303050
239.939885	3634.035584	16.998426	-0.046977	3.299640
239.924492	3626.082551	17.003431	-0.046969	3.296241
239.975607	3618.050081	17.008435	-0.046973	3.292806
239.885506	3610.056878	17.013440	-0.046951	3.289379
239.694371	3602.082608	17.018445	-0.046911	3.285953
239.809388	3594.108746	17.023450	-0.046927	3.282536
239.767435	3586.109400	17.028455	-0.046914	3.279097
239.502950	3578.163309	17.033459	-0.046860	3.275670
239.747148	3570.122923	17.038464	-0.046900	3.272218
239.801971	3562.086427	17.043469	-0.046905	3.268756
239.799998	3554.109167	17.048474	-0.046899	3.265315
239.581266	3546.175312	17.053479	-0.046853	3.261880
239.674469	3538.183815	17.058483	-0.046865	3.258428
239.733058	3530.171479	17.063488	-0.046871	3.254963
239.588364	3522.169789	17.068493	-0.046839	3.251490
239.556654	3514.208031	17.073498	-0.046828	3.248036
239.472809	3506.201368	17.078503	-0.046807	3.244556
239.526671	3498.230074	17.083507	-0.046812	3.241093
239.534599	3490.245721	17.088512	-0.046808	3.237619
239.452171	3482.231058	17.093517	-0.046788	3.234125
239.209404	3474.217857	17.098522	-0.046737	3.230621
239.026816	3466.234301	17.103527	-0.046698	3.227128
239.173410	3458.205838	17.108531	-0.046720	3.223626
239.113717	3450.267421	17.113536	-0.046704	3.220150
239.087212	3442.263244	17.118541	-0.046694	3.216644
239.140153	3434.285242	17.123546	-0.046699	3.213148
239.071459	3426.313866	17.128551	-0.046681	3.209646
238.900979	3418.313977	17.133555	-0.046644	3.206124
238.910475	3410.353447	17.138560	-0.046640	3.202623
238.823679	3402.373915	17.143565	-0.046619	3.199105
238.750935	3394.406822	17.148570	-0.046600	3.195590
238.707533	3386.379990	17.153575	-0.046587	3.192045
238.547927	3378.364717	17.158579	-0.046552	3.188497
238.745588	3370.379292	17.163584	-0.046584	3.184973
238.597514	3362.422365	17.168589	-0.046551	3.181444
238.705007	3354.412492	17.173594	-0.046566	3.177897
238.740678	3346.443733	17.178599	-0.046567	3.174362
238.586917	3338.419939	17.183603	-0.046533	3.170791
238.530530	3330.442854	17.188608	-0.046518	3.167240
238.678818	3322.454227	17.193613	-0.046540	3.163689
238.824900	3314.474713	17.198618	-0.046562	3.160138
238.404971	3306.568910	17.203623	-0.046479	3.156592
238.329716	3298.510834	17.208627	-0.046459	3.152988
238.473480	3290.482487	17.213632	-0.046481	3.149403
238.287674	3282.519829	17.218637	-0.046441	3.145829
238.237118	3274.568373	17.223642	-0.046427	3.142262
238.350688	3266.573713	17.228647	-0.046443	3.138678
238.271440	3258.578629	17.233651	-0.046423	3.135082
238.019020	3250.613991	17.238656	-0.046371	3.131488
238.152581	3242.566472	17.243661	-0.046390	3.127869
238.157154	3234.590095	17.248666	-0.046386	3.124272
237.960138	3226.671918	17.253671	-0.046344	3.120689
238.054269	3218.654623	17.258675	-0.046356	3.117070
238.180951	3210.664044	17.263680	-0.046375	3.113460
238.041037	3202.636248	17.268685	-0.046343	3.109817
237.968868	3194.677207	17.273690	-0.046325	3.106203
238.014266	3186.698517	17.278695	-0.046328	3.102583
237.972791	3178.697340	17.283699	-0.046315	3.098943
237.769270	3170.773971	17.288704	-0.046272	3.095328
237.726660	3162.752695	17.293709	-0.046259	3.091671
237.797295	3154.749342	17.298714	-0.046267	3.088022
237.734977	3146.782514	17.303719	-0.046250	3.084381
237.561814	3138.800875	17.308723	-0.046213	3.080723
237.683710	3130.837714	17.313728	-0.046230	3.077082
237.574505	3122.801224	17.318733	-0.046205	3.073393
237.535655	3114.731245	17.323738	-0.046192	3.069688
237.713307	3106.781349	17.328743	-0.046220	3.066043
237.688666	3098.813346	17.333747	-0.046210	3.062376
237.538790	3090.862309	17.338752	-0.046177	3.058707
237.486914	3082.883771	17.343757	-0.046163	3.055025
237.559726	3074.872327	17.348762	-0.046171	3.051330
237.353613	3066.903333	17.353767	-0.046127	3.047636
237.152838	3058.936141	17.358771	-0.046085	3.043939
237.335696	3050.966001	17.363776	-0.046114	3.040255
237.313084	3042.972244	17.368781	-0.046104	3.036545
237.130917	3034.980648	17.373786	-0.046065	3.032824
237.188155	3026.980101	17.378791	-0.046071	3.029105
237.305176	3018.965034	17.383795	-0.046087	3.025379
237.141247	3011.054683	17.388800	-0.046052	3.021682
236.854657	3003.069339	17.393805	-0.045993	3.017941
236.989362	2995.061937	17.398810	-0.046013	3.014205
236.954217	2987.063550	17.403815	-0.046001	3.010460
236.829466	2979.089883	17.408819	-0.045973	3.006717
236.992585	2971.100546	17.413824	-0.045998	3.002977
236.861153	2963.142195	17.418829	-0.045968	2.999232
236.876469	2955.173035	17.423834	-0.045966	2.995485
236.820104	2947.151864	17.428839	-0.045950	2.991705
236.688475	2939.144877	17.433843	-0.045921	2.987923
236.649646	2931.158721	17.438848	-0.045908	2.984151
236.604989	2923.198486	17.443853	-0.045895	2.980385
236.684518	2915.206743	17.448858	-0.045904	2.976607
236.624247	2907.253872	17.453863	-0.045888	2.972835
236.580216	2899.234432	17.458867	-0.045875	2.969027
236.670772	2891.258150	17.463872	-0.045886	2.965242
236.609130	2883.285405	17.468877	-0.045870	2.961446
236.453143	2875.336345	17.473882	-0.045835	2.957652
236.490439	2867.359721	17.478887	-0.045837	2.953849
236.370899	2859.334508	17.483891	-0.045810	2.950010
236.261588	2851.365675	17.488896	-0.045784	2.946194
236.130644	2843.387417	17.493901	-0.045755	2.942367
236.158972	2835.398407	17.498906	-0.045755	2.938538
236.190638	2827.443478	17.503911	-0.045755	2.934721
236.179395	2819.412694	17.508915	-0.045748	2.930860
236.011164	2811.473809	17.513920	-0.045712	2.927030
235.967244	2803.482611	17.518925	-0.045698	2.923176
235.932275	2795.508753	17.523930	-0.045687	2.919326
235.858561	2787.556787	17.528935	-0.045668	2.915479
235.934772	2779.457668	17.533939	-0.045677	2.911564
236.058966	2771.451687	17.538944	-0.045694	2.907692
235.967872	2763.487776	17.543949	-0.045672	2.903823
235.956073	2755.533470	17.548954	-0.045665	2.899958
235.927837	2747.589671	17.553959	-0.045655	2.896092
235.786807	2739.611363	17.558963	-0.045623	2.892198
235.650316	2731.631219	17.563968	-0.045593	2.888298
235.623375	2723.631850	17.568973	-0.045582	2.884389
235.480377	2715.706669	17.573978	-0.045551	2.880505
235.404508	2707.756729	17.578983	-0.045531	2.876607
235.466952	2699.706075	17.583987	-0.045538	2.872662
235.442516	2691.724463	17.588992	-0.045528	2.868741
235.177753	2683.738254	17.593997	-0.045473	2.864799
235.345984	2675.777837	17.599002	-0.045500	2.860888
235.392542	2667.812188	17.604007	-0.045503	2.856962
235.352279	2659.801554	17.609011	-0.045490	2.853004
235.337436	2651.826314	17.614016	-0.045482	2.849060
235.278860	2643.838098	17.619021	-0.045466	2.845101
235.106488	2635.914833	17.624026	-0.045429	2.841162
235.265446	2627.931708	17.629031	-0.045454	2.837207
235.233680	2619.911065	17.634035	-0.045442	2.833216
235.068306	2611.926995	17.639040	-0.045406	2.829231
234.879723	2603.971929	17.644045	-0.045366	2.825253
234.969723	2595.997552	17.649050	-0.045378	2.821276
235.087676	2588.000599	17.654055	-0.045395	2.817284
234.699379	2580.046855	17.659059	-0.045317	2.813278
234.775115	2572.053171	17.664064	-0.045326	2.809274
234.706763	2564.066315	17.669069	-0.045308	2.805259
234.725789	2556.100081	17.674074	-0.045306	2.801253
234.731985	2548.154145	17.679079	-0.045302	2.797251
234.860069	2540.121969	17.684083	-0.045321	2.793207
234.762877	2532.149087	17.689088	-0.045298	2.789174
234.504508	2524.199720	17.694093	-0.045245	2.785138
234.545820	2516.221005	17.699098	-0.045247	2.781098
234.663543	2508.244956	17.704103	-0.045264	2.777059
234.517259	2500.270730	17.709107	-0.045231	2.772999
234.648759	2492.280697	17.714112	-0.045251	2.768941
234.473936	2484.301433	17.719117	-0.045213	2.764865
234.240495	2476.378199	17.724122	-0.045164	2.760807
234.360766	2468.392838	17.729127	-0.045182	2.756733
234.184121	2460.357846	17.734131	-0.045143	2.752610
234.158216	2452.347047	17.739136	-0.045133	2.748502
234.069737	2444.376893	17.744141	-0.045112	2.744405
234.080258	2436.437928	17.749146	-0.045109	2.740324
234.023144	2428.481229	17.754151	-0.045093	2.736224
233.932209	2420.479398	17.759155	-0.045071	2.732092
233.991368	2412.499070	17.764160	-0.045076	2.727974
233.967294	2404.526188	17.769165	-0.045067	2.723848
233.955947	2396.562674	17.774170	-0.045060	2.719722
233.925323	2388.627381	17.779175	-0.045049	2.715603
233.793631	2380.615966	17.784179	-0.045019	2.711432
233.982776	2372.638466	17.789184	-0.045049	2.707293
233.911618	2364.667179	17.794189	-0.045031	2.703134
233.803102	2356.710894	17.799194	-0.045005	2.698973
233.772486	2348.765914	17.804199	-0.044994	2.694818
233.697274	2340.748025	17.809203	-0.044975	2.690615
233.649902	2332.800016	17.814208	-0.044961	2.686443
233.564763	2324.833904	17.819213	-0.044940	2.682254
233.370201	2316.880493	17.824218	-0.044899	2.678057
233.390308	2308.904734	17.829223	-0.044897	2.673856
233.283362	2300.866496	17.834227	-0.044872	2.669607
233.351738	2292.910071	17.839232	-0.044880	2.665405
233.394135	2284.928069	17.844237	-0.044882	2.661182
233.271914	2276.979986	17.849242	-0.044855	2.656960
233.345960	2268.983013	17.854247	-0.044863	2.652717
233.215777	2261.004450	17.859251	-0.044834	2.648464
233.022644	2253.069331	17.864256	-0.044793	2.644224
233.062605	2245.094737	17.869261	-0.044795	2.639971
233.111659	2237.142062	17.874266	-0.044799	2.635723
233.302538	2229.125849	17.879271	-0.044829	2.631443
233.228852	2221.136024	17.884275	-0.044810	2.627154
233.143743	2213.205997	17.889280	-0.044789	2.622889
233.268967	2205.220256	17.894285	-0.044807	2.618600
232.915033	2197.291605	17.899290	-0.044736	2.614304
232.821690	2189.318975	17.904295	-0.044714	2.609994
232.821710	2181.326316	17.909299	-0.044709	2.605672
232.951981	2173.373018	17.914304	-0.044728	2.601374
232.832345	2165.419982	17.919309	-0.044700	2.597051
232.821203	2157.322896	17.924314	-0.044693	2.592650
232.765622	2149.272630	17.929319	-0.044677	2.588264
232.890177	2141.312998	17.934323	-0.044695	2.583933
232.851542	2133.406259	17.939328	-0.044683	2.579612
232.750328	2125.481883	17.944333	-0.044659	2.575270
232.657061	2117.525244	17.949338	-0.044637	2.570903
232.689960	2109.547223	17.954343	-0.044637	2.566526
232.499167	2101.587506	17.959347	-0.044597	2.562136
232.639905	2093.645182	17.964352	-0.044618	2.557771
232.473759	2085.694441	17.969357	-0.044582	2.553372
232.348983	2077.705686	17.974362	-0.044553	2.548948
232.335008	2069.744112	17.979367	-0.044546	2.544538
232.148028	2061.810209	17.984371	-0.044506	2.540125
232.123969	2053.863258	17.989376	-0.044496	2.535708
232.190054	2045.857568	17.994381	-0.044503	2.531256
231.980133	2037.891138	17.999386	-0.044459	2.526800
232.259000	2029.915660	18.004391	-0.044506	2.522365
232.190279	2021.959590	18.009395	-0.044488	2.517908
231.939372	2014.011550	18.014400	-0.044436	2.513435
231.819952	2006.011734	18.019405	-0.044408	2.508934
231.957214	1998.014618	18.024410	-0.044429	2.504445
231.948439	1990.087122	18.029415	-0.044422	2.499977
231.821263	1982.132743	18.034419	-0.044393	2.495477
232.068915	1974.130766	18.039424	-0.044434	2.490969
231.795326	1966.196080	18.044429	-0.044378	2.486453
231.566971	1958.272025	18.049434	-0.044330	2.481938
231.617393	1950.310105	18.054439	-0.044334	2.477414
231.654469	1942.306669	18.059443	-0.044336	2.472857
231.676783	1934.321794	18.064448	-0.044335	2.468301
231.459864	1926.393511	18.069453	-0.044290	2.463751
231.519544	1918.443835	18.074458	-0.044295	2.459202
231.584782	1910.485547	18.079463	-0.044302	2.454639
231.368942	1902.503743	18.084467	-0.044257	2.450033
231.256824	1894.565955	18.089472	-0.044231	2.445451
231.417405	1886.575896	18.094477	-0.044256	2.440852
231.147450	1878.658308	18.099482	-0.044200	2.436252
231.144288	1870.638814	18.104487	-0.044195	2.431606
231.049081	1862.645191	18.109491	-0.044172	2.426958
230.811831	1854.724872	18.114496	-0.044122	2.422333
230.804952	1846.771905	18.119501	-0.044116	2.417698
230.698589	1838.806784	18.124506	-0.044091	2.413040
230.771011	1830.824551	18.129511	-0.044099	2.408376
230.709375	1822.872370	18.134515	-0.044083	2.403710
230.812421	1814.935490	18.139520	-0.044097	2.399057
230.649002	1806.999136	18.144525	-0.044061	2.394375
230.494896	1799.029016	18.149530	-0.044027	2.389664
230.593157	1791.044624	18.154535	-0.044040	2.384955
230.672291	1783.075856	18.159539	-0.044050	2.380245
230.733249	1775.127607	18.164544	-0.044056	2.375536
230.339521	1767.206060	18.169549	-0.043978	2.370797
230.373350	1759.224715	18.174554	-0.043979	2.366048
230.405230	1751.275833	18.179559	-0.043979	2.361308
230.460645	1743.309705	18.184563	-0.043985	2.356550
230.500650	1735.352592	18.189568	-0.043987	2.351786
230.301890	1727.401020	18.194573	-0.043945	2.346997
230.408936	1719.414231	18.199578	-0.043959	2.342202
230.347917	1711.488008	18.204583	-0.043943	2.337420
230.296482	1703.525609	18.209587	-0.043928	2.332606
230.286400	1695.559610	18.214592	-0.043921	2.327784
229.892544	1687.659605	18.219597	-0.043843	2.322961
230.155867	1679.664216	18.224602	-0.043887	2.318124
230.191287	1671.729545	18.229607	-0.043888	2.313294
229.928056	1663.777174	18.234611	-0.043834	2.308419
230.026605	1655.830159	18.239616	-0.043847	2.303567
229.875118	1647.898007	18.244621	-0.043814	2.298693
229.777477	1639.940837	18.249626	-0.043790	2.293798
229.894923	1631.961467	18.254631	-0.043807	2.288897
230.062273	1623.975783	18.259635	-0.043833	2.283985
229.824887	1616.086993	18.264640	-0.043784	2.279089
229.855008	1608.139305	18.269645	-0.043784	2.274168
229.782151	1600.107254	18.274650	-0.043765	2.269175
229.671727	1592.172056	18.279655	-0.043740	2.264229
229.502195	1584.238210	18.284659	-0.043703	2.259267
229.562868	1576.296631	18.289664	-0.043709	2.254309
229.516094	1568.334892	18.294669	-0.043695	2.249319
229.377474	1560.394205	18.299674	-0.043664	2.244322
229.289579	1552.482049	18.304679	-0.043643	2.239337
229.287524	1544.513238	18.309683	-0.043637	2.234312
229.268258	1536.551424	18.314688	-0.043628	2.229280
229.131417	1528.611515	18.319693	-0.043598	2.224239
229.185913	1520.668233	18.324698	-0.043603	2.219201
229.238137	1512.745459	18.329703	-0.043607	2.214165
228.986231	1504.783706	18.334707	-0.043555	2.209065
228.931882	1496.852907	18.339712	-0.043540	2.203991
229.006094	1488.905457	18.344717	-0.043549	2.198906
229.001437	1480.953959	18.349722	-0.043543	2.193800
228.797121	1473.010701	18.354727	-0.043499	2.188669
228.701931	1465.041734	18.359731	-0.043476	2.183519
228.941017	1457.092165	18.364736	-0.043516	2.178400
228.821542	1449.168023	18.369741	-0.043488	2.173253
228.631916	1441.226634	18.374746	-0.043448	2.168075
228.734480	1433.292626	18.379751	-0.043462	2.162917
228.537535	1425.369076	18.384755	-0.043420	2.157726
228.417689	1417.431072	18.389760	-0.043393	2.152520
228.485321	1409.462470	18.394765	-0.043400	2.147299
228.479813	1401.522236	18.399770	-0.043394	2.142077
228.329371	1393.620720	18.404775	-0.043361	2.136854
228.309522	1385.653564	18.409779	-0.043352	2.131587
228.356664	1377.715758	18.414784	-0.043355	2.126332
228.212264	1369.794585	18.419789	-0.043323	2.121058
228.082859	1361.878160	18.424794	-0.043294	2.115775
228.053429	1353.878623	18.429799	-0.043284	2.110433
227.993998	1345.902981	18.434803	-0.043267	2.105090
228.130642	1337.992659	18.439808	-0.043288	2.099797
228.139447	1330.072247	18.444813	-0.043284	2.094471
228.011640	1322.133518	18.449818	-0.043255	2.089105
227.820123	1314.230746	18.454823	-0.043214	2.083744
227.772985	1306.298208	18.459827	-0.043200	2.078363
227.867694	1298.355461	18.464832	-0.043213	2.072976
227.702146	1290.428457	18.469837	-0.043177	2.067559
227.537672	1282.509167	18.474842	-0.043141	2.062133
227.908655	1274.555468	18.479847	-0.043205	2.056723
227.762527	1266.626409	18.484851	-0.043173	2.051263
227.543682	1258.717216	18.489856	-0.043127	2.045795
227.461876	1250.816636	18.494861	-0.043106	2.040333
227.440158	1242.882024	18.499866	-0.043097	2.034838
227.199556	1234.953908	18.504871	-0.043047	2.029311
227.283482	1226.985590	18.509875	-0.043058	2.023773
227.412662	1219.059558	18.514880	-0.043077	2.018255
227.361062	1211.144382	18.519885	-0.043062	2.012710
227.220636	1203.210647	18.524890	-0.043031	2.007128
227.239115	1195.295671	18.529895	-0.043029	2.001560
227.201529	1187.381179	18.534899	-0.043017	1.995971
227.015313	1179.468432	18.539904	-0.042977	1.990352
227.062786	1171.533276	18.544909	-0.042981	1.984726
226.993368	1163.626362	18.549914	-0.042963	1.979091
226.792091	1155.742883	18.554919	-0.042920	1.973443
226.858439	1147.774403	18.559923	-0.042927	1.967747
226.900174	1139.854311	18.564928	-0.042930	1.962066
226.807010	1131.965388	18.569933	-0.042907	1.956376
226.776882	1124.008406	18.574938	-0.042897	1.950628
226.763593	1116.075576	18.579943	-0.042889	1.944881
226.810581	1108.159254	18.584947	-0.042893	1.939137
226.569848	1100.268550	18.589952	-0.042843	1.933362
226.381294	1092.361299	18.594957	-0.042802	1.927564
226.397287	1084.427109	18.599962	-0.042800	1.921751
226.264801	1076.552671	18.604967	-0.042770	1.915948
226.116456	1068.639462	18.609971	-0.042738	1.910096
226.256536	1060.698262	18.614976	-0.042759	1.904239
226.291580	1052.792233	18.619981	-0.042760	1.898377
226.155790	1044.877650	18.624986	-0.042730	1.892472
226.104224	1036.971286	18.629991	-0.042715	1.886564
226.271041	1029.040843	18.634995	-0.042741	1.880644
226.174716	1021.164098	18.640000	-0.042718	1.874716
225.923278	1013.266917	18.645005	-0.042666	1.868736
225.884007	1005.343191	18.650010	-0.042653	1.862740
225.788891	997.465639	18.655015	-0.042630	1.856754
225.647040	989.557204	18.660019	-0.042599	1.850720
225.594063	981.646319	18.665024	-0.042584	1.844675
225.630258	973.752156	18.670029	-0.042586	1.838632
225.462279	965.864973	18.675034	-0.042549	1.832551
225.526134	957.946152	18.680039	-0.042556	1.826453
225.502056	950.042053	18.685043	-0.042546	1.820336
225.466449	942.153235	18.690048	-0.042535	1.814208
225.415148	934.249867	18.695053	-0.042520	1.808046
225.262574	926.358806	18.700058	-0.042486	1.801861
225.490424	918.464220	18.705063	-0.042524	1.795698
225.062798	910.568249	18.710067	-0.042439	1.789432
225.309246	902.625990	18.715072	-0.042480	1.783190
225.376249	894.739757	18.720077	-0.042487	1.776949
225.088318	886.875636	18.725082	-0.042428	1.770659
224.917682	879.025300	18.730087	-0.042391	1.764373
224.992191	871.127640	18.735091	-0.042400	1.758057
224.899304	863.238264	18.740096	-0.042378	1.751703
224.805702	855.362210	18.745101	-0.042355	1.745337
224.732857	847.483969	18.750106	-0.042336	1.738949
224.707577	839.604807	18.755111	-0.042327	1.732542
224.544327	831.721414	18.760115	-0.042291	1.726091
224.581867	823.843457	18.765120	-0.042293	1.719645
224.512848	815.979869	18.770125	-0.042275	1.713173
224.362475	808.084797	18.775130	-0.042242	1.706640
224.337764	800.215461	18.780135	-0.042232	1.700120
224.361779	792.331853	18.785139	-0.042232	1.693569
224.338868	784.442407	18.790144	-0.042222	1.686982
224.160265	776.611368	18.795149	-0.042184	1.680397
224.029069	768.761217	18.800154	-0.042154	1.673776
224.182915	760.850097	18.805159	-0.042178	1.667116
223.953540	753.011615	18.810163	-0.042130	1.660439
224.099965	745.136075	18.815168	-0.042152	1.653754
224.055705	737.264584	18.820173	-0.042139	1.647020
223.937253	729.411146	18.825178	-0.042112	1.640263
223.827422	721.579710	18.830183	-0.042086	1.633499
223.849765	713.642634	18.835187	-0.042085	1.626633
223.814224	705.794841	18.840192	-0.042073	1.619808
223.693135	697.965068	18.845197	-0.042046	1.612957
223.560972	690.110681	18.850202	-0.042016	1.606054
223.879394	682.233859	18.855207	-0.042070	1.599166
223.675182	674.417703	18.860211	-0.042027	1.592226
223.599008	666.566212	18.865216	-0.042008	1.585244
223.728588	658.716681	18.870221	-0.042027	1.578262
223.506182	650.892926	18.875226	-0.041980	1.571220
223.532243	643.053705	18.880231	-0.041980	1.564170
223.429764	635.236401	18.885235	-0.041956	1.557088
223.179152	627.413680	18.890240	-0.041904	1.549948
222.972901	619.600043	18.895245	-0.041861	1.542789
222.984524	611.746676	18.900250	-0.041858	1.535592
223.044873	603.897583	18.905255	-0.041864	1.528373
223.007773	596.064917	18.910259	-0.041852	1.521121
222.890922	588.266808	18.915264	-0.041825	1.513853
222.903075	580.430474	18.920269	-0.041822	1.506535
222.592420	572.647826	18.925274	-0.041760	1.499181
222.723227	564.811004	18.930279	-0.041779	1.491809
222.693496	556.983593	18.935283	-0.041768	1.484383
222.845238	549.157056	18.940288	-0.041791	1.476950
222.747456	541.322604	18.945293	-0.041768	1.469432
222.740095	533.500150	18.950298	-0.041762	1.461901
222.681076	525.717227	18.955303	-0.041746	1.454361
222.494573	517.927578	18.960307	-0.041706	1.446755
222.329545	510.159235	18.965312	-0.041670	1.439134
222.243752	502.383432	18.970317	-0.041649	1.431477
222.283633	494.562782	18.975322	-0.041651	1.423754
222.198740	486.799540	18.980327	-0.041630	1.416027
222.215705	478.991846	18.985331	-0.041629	1.408229
222.166612	471.217281	18.990336	-0.041614	1.400410
222.100781	463.460811	18.995341	-0.041597	1.392563
221.713759	455.711592	19.000346	-0.041520	1.384625
221.884741	447.915935	19.005351	-0.041547	1.376688
221.931155	440.118677	19.010355	-0.041550	1.368681
221.681087	432.387500	19.015360	-0.041499	1.360646
221.567280	424.655219	19.020365	-0.041473	1.352584
221.366120	416.903014	19.025370	-0.041430	1.344439
221.381789	409.147326	19.030375	-0.041428	1.336278
221.430369	401.367582	19.035379	-0.041432	1.328047
221.365494	393.644859	19.040384	-0.041415	1.319806
221.363821	385.843695	19.045389	-0.041409	1.311439
221.251692	378.043884	19.050394	-0.041384	1.303001
221.252122	370.330744	19.055399	-0.041379	1.294622
220.973297	362.638247	19.060403	-0.041322	1.286160
220.876273	354.942796	19.065408	-0.041299	1.277672
220.900111	347.222032	19.070413	-0.041298	1.269122
220.802964	339.513130	19.075418	-0.041275	1.260505
220.642539	331.836583	19.080423	-0.041240	1.251852
220.525633	324.140263	19.085427	-0.041213	1.243125
220.616357	316.437866	19.090432	-0.041225	1.234370
220.542087	308.742039	19.095437	-0.041206	1.225527
220.292215	301.089696	19.100442	-0.041155	1.216636
220.346683	293.397846	19.105447	-0.041160	1.207694
220.265897	285.737342	19.110451	-0.041140	1.198694
220.048293	278.102440	19.115456	-0.041095	1.189630
219.993962	270.443486	19.120461	-0.041080	1.180500
220.050358	262.769654	19.125466	-0.041085	1.171304
219.886080	255.161073	19.130471	-0.041049	1.162068
219.922104	247.503044	19.135475	-0.041051	1.152740
219.820882	239.854043	19.140480	-0.041027	1.143318
219.698585	232.253496	19.145485	-0.041000	1.133873
219.567788	224.637574	19.150490	-0.040970	1.124328
219.665759	217.027665	19.155495	-0.040984	1.114758
219.567748	209.430828	19.160499	-0.040961	1.105080
219.317971	201.886154	19.165504	-0.040909	1.095349
219.193443	194.312814	19.170509	-0.040881	1.085521
219.020343	186.769712	19.175514	-0.040844	1.075633
218.917922	179.205016	19.180519	-0.040820	1.065640
218.804703	171.664191	19.185523	-0.040794	1.055582
218.689352	164.126261	19.190528	-0.040768	1.045430
218.731357	156.596979	19.195533	-0.040771	1.035228
218.541829	149.091712	19.200538	-0.040730	1.024902
218.464750	141.599571	19.205543	-0.040711	1.014516
218.301992	134.114222	19.210547	-0.040676	1.004011
218.135158	126.652022	19.215552	-0.040640	0.993427
217.647427	119.229190	19.220557	-0.040544	0.982705
217.509298	111.773115	19.225562	-0.040514	0.971905
217.039050	104.400335	19.230567	-0.040422	0.961021
216.707935	97.006709	19.235571	-0.040355	0.950017
216.057635	89.679872	19.240576	-0.040229	0.938900
215.726302	82.310900	19.245581	-0.040163	0.927670
215.301813	74.978362	19.250586	-0.040079	0.916334
214.833880	67.651236	19.255591	-0.039987	0.904852
214.441422	60.568024	19.260595	-0.039909	0.893628