Fri Mar 12 13:27:56 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.771532	-0.064578	0.000000	0.000016	0.721130

0.944436	-0.098771	0.005005	-0.000017	0.721124
0.907017	-0.089837	0.010010	-0.000010	0.721128
0.917338	-0.090556	0.015014	-0.000012	0.721130
0.892263	-0.089613	0.020019	-0.000007	0.721124
0.979787	-0.101063	0.025024	-0.000023	0.721132
0.890576	-0.088224	0.030029	-0.000007	0.721126
0.917942	-0.093286	0.035034	-0.000012	0.721126
0.781234	-0.065640	0.040038	0.000014	0.721132
0.683912	-0.052903	0.045043	0.000032	0.721123
0.923342	-0.092396	0.050048	-0.000013	0.721129
0.806636	-0.073708	0.055053	0.000009	0.721125
0.719133	-0.057800	0.060058	0.000025	0.721126
0.836556	-0.076082	0.065062	0.000003	0.721131
0.787622	-0.071645	0.070067	0.000012	0.721123
1.025521	-0.147725	0.075072	-0.000032	0.721057
0.885733	-0.211208	0.080077	-0.000006	0.720883
1.082534	-0.247435	0.085082	-0.000043	0.720881
0.919881	-0.215527	0.090086	-0.000012	0.720886
0.640958	-0.170647	0.095091	0.000039	0.720877
0.747004	-0.185279	0.100096	0.000020	0.720885
0.609807	-0.165678	0.105101	0.000045	0.720876
0.847630	-0.330643	0.110106	0.000001	0.720635
0.767005	-0.360485	0.115110	0.000016	0.720548
0.782005	-0.367390	0.120115	0.000013	0.720540
0.840465	-0.373470	0.125120	0.000002	0.720548
0.757918	-0.362211	0.130125	0.000018	0.720541
0.773392	-0.471987	0.135130	0.000015	0.720331
0.766674	-0.522145	0.140134	0.000016	0.720230
0.611494	-0.498266	0.145139	0.000045	0.720222
0.723870	-0.513752	0.150144	0.000024	0.720231
0.871104	-0.597620	0.155149	-0.000004	0.720118
0.776004	-0.691048	0.160154	0.000014	0.719900
0.855520	-0.701516	0.165158	-0.000001	0.719908
0.537206	-0.649929	0.170163	0.000059	0.719898
0.592750	-0.743263	0.175168	0.000048	0.719733
0.353721	-0.767131	0.180173	0.000093	0.719603
0.468391	-0.788494	0.185178	0.000071	0.719601
0.664229	-0.819997	0.190182	0.000035	0.719607
0.610640	-0.980782	0.195187	0.000045	0.719272
0.484226	-0.955370	0.200192	0.000068	0.719277
0.617867	-0.981537	0.205197	0.000044	0.719273
0.662554	-1.117771	0.210202	0.000035	0.719020
0.664428	-1.144048	0.215206	0.000035	0.718969
0.496456	-1.118554	0.220211	0.000066	0.718960
0.633788	-1.274832	0.225216	0.000041	0.718700
0.298882	-1.240166	0.230221	0.000103	0.718651
0.169720	-1.221226	0.235226	0.000127	0.718643
0.283977	-1.381833	0.240230	0.000106	0.718366
0.247208	-1.381995	0.245235	0.000113	0.718353
0.772096	-1.519700	0.250240	0.000015	0.718266
0.588933	-1.613119	0.255245	0.000049	0.718017
0.539602	-1.606694	0.260250	0.000058	0.718012
0.540222	-1.731301	0.265254	0.000058	0.717766
0.381011	-1.736620	0.270259	0.000088	0.717700
0.424318	-1.810820	0.275264	0.000080	0.717568
0.095225	-1.845558	0.280269	0.000141	0.717384
-0.117189	-1.808701	0.285274	0.000180	0.717382
0.121547	-1.997666	0.290278	0.000136	0.717092
0.033947	-1.985803	0.295283	0.000152	0.717085
-0.549075	-1.989048	0.300288	0.000261	0.716873
-0.499094	-2.054934	0.305293	0.000252	0.716760
-0.228265	-2.145600	0.310298	0.000201	0.716677
-0.705796	-2.173525	0.315302	0.000290	0.716453
-1.610808	-2.016247	0.320307	0.000458	0.716445
-1.670005	-2.120423	0.325312	0.000469	0.716218
-2.204972	-2.066886	0.330317	0.000569	0.716135
-2.212267	-2.066209	0.335322	0.000570	0.716134
-2.461336	-2.134068	0.340326	0.000617	0.715912
-3.201535	-2.017562	0.345331	0.000754	0.715882
-2.814457	-2.081545	0.350336	0.000682	0.715892
-3.155754	-2.168802	0.355341	0.000746	0.715598
-4.347886	-1.981778	0.360346	0.000968	0.715548
-3.770183	-2.083817	0.365350	0.000860	0.715550
-3.589451	-2.191149	0.370355	0.000827	0.715401
-5.201278	-1.985976	0.375360	0.001127	0.715238
-4.975497	-2.028118	0.380365	0.001085	0.715235
-4.942613	-2.035226	0.385370	0.001078	0.715232
-4.713597	-2.158640	0.390374	0.001036	0.715068
-5.777351	-2.047991	0.395379	0.001234	0.714912
-5.622243	-2.073531	0.400384	0.001205	0.714916
-5.723012	-2.057576	0.405389	0.001224	0.714912
-5.994332	-2.056504	0.410394	0.001274	0.714818
-6.730257	-2.027028	0.415398	0.001411	0.714617
-6.557704	-2.061142	0.420403	0.001379	0.714610
-6.906483	-1.997149	0.425408	0.001444	0.714614
-6.680647	-2.039143	0.430413	0.001402	0.714610
-6.647995	-2.111896	0.435418	0.001396	0.714478
-7.536143	-2.048606	0.440422	0.001561	0.714289
-7.635456	-2.036956	0.445427	0.001579	0.714277
-7.723083	-2.017092	0.450432	0.001596	0.714286
-7.591395	-2.041174	0.455437	0.001571	0.714285
-7.707904	-2.040526	0.460442	0.001593	0.714245
-8.100457	-2.103833	0.465446	0.001666	0.713980
-8.366446	-2.060638	0.470451	0.001715	0.713972
-8.695741	-1.998388	0.475456	0.001777	0.713979
-8.636924	-2.011097	0.480461	0.001766	0.713975
-8.611068	-2.015891	0.485466	0.001761	0.713974
-8.269268	-2.139577	0.490470	0.001697	0.713849
-9.950258	-1.938272	0.495475	0.002010	0.713654
-9.490613	-2.016467	0.500480	0.001924	0.713662
-9.445156	-2.026363	0.505485	0.001916	0.713658
-9.809429	-1.963220	0.510490	0.001984	0.713655
-9.352731	-2.040537	0.515494	0.001899	0.713663
-9.628424	-1.996002	0.520499	0.001950	0.713654
-10.011201	-2.062501	0.525504	0.002021	0.713386
-10.457651	-1.994015	0.530509	0.002104	0.713364
-10.326560	-2.018501	0.535514	0.002080	0.713362
-10.004604	-2.072324	0.540518	0.002020	0.713369
-10.435248	-2.000297	0.545523	0.002100	0.713360
-10.544421	-1.975696	0.550528	0.002120	0.713370
-10.163115	-2.143677	0.555533	0.002049	0.713171
-11.815461	-1.919753	0.560538	0.002357	0.713031
-11.262064	-2.015169	0.565542	0.002254	0.713037
-10.967863	-2.072169	0.570547	0.002199	0.713028
-11.242064	-2.019893	0.575552	0.002250	0.713035
-11.404132	-1.992185	0.580557	0.002280	0.713033
-11.365907	-2.001027	0.585562	0.002273	0.713029
-11.493680	-2.112169	0.590566	0.002297	0.712762
-12.472649	-1.962664	0.595571	0.002479	0.712713
-12.426332	-1.968713	0.600576	0.002470	0.712717
-11.886349	-2.064644	0.605581	0.002370	0.712718
-12.231292	-2.005016	0.610586	0.002434	0.712714
-12.320185	-1.986425	0.615590	0.002451	0.712720
-12.229742	-2.005237	0.620595	0.002434	0.712715
-12.668624	-2.073109	0.625600	0.002515	0.712424
-13.291517	-1.975201	0.630605	0.002631	0.712398
-13.183841	-1.997082	0.635610	0.002611	0.712393
-12.780698	-2.066947	0.640614	0.002536	0.712397
-13.315326	-1.975792	0.645619	0.002636	0.712388
-13.361390	-1.964324	0.650624	0.002644	0.712395
-12.922666	-2.043821	0.655629	0.002563	0.712392
-13.750169	-2.024162	0.660634	0.002717	0.712138
-14.293584	-1.945852	0.665638	0.002818	0.712101
-14.094859	-1.986267	0.670643	0.002781	0.712091
-13.718956	-2.048618	0.675648	0.002711	0.712100
-14.191221	-1.966182	0.680653	0.002799	0.712097
-14.294040	-1.950125	0.685658	0.002818	0.712093
-13.527563	-2.081522	0.690662	0.002675	0.712103
-14.348713	-2.050801	0.695667	0.002828	0.711873
-15.429533	-1.910978	0.700672	0.003029	0.711768
-14.718420	-2.038858	0.705677	0.002897	0.711765
-15.030028	-1.982893	0.710682	0.002955	0.711766
-15.145483	-1.958828	0.715686	0.002976	0.711773
-14.910548	-2.005224	0.720691	0.002932	0.711764
-14.963626	-1.991921	0.725696	0.002942	0.711772
-15.166313	-2.000188	0.730701	0.002980	0.711684
-16.143420	-1.939095	0.735706	0.003162	0.711458
-15.607857	-2.031625	0.740710	0.003062	0.711464
-16.297936	-1.913345	0.745715	0.003190	0.711455
-16.183626	-1.930849	0.750720	0.003169	0.711461
-15.672208	-2.021699	0.755725	0.003074	0.711461
-16.028049	-1.959456	0.760730	0.003140	0.711459
-16.032343	-1.956217	0.765734	0.003141	0.711464
-16.119562	-2.054090	0.770739	0.003157	0.711238
-16.900425	-1.959721	0.775744	0.003302	0.711148
-16.581374	-2.017037	0.780749	0.003243	0.711148
-17.005325	-1.943320	0.785754	0.003322	0.711144
-16.590528	-2.014842	0.790758	0.003245	0.711149
-16.508634	-2.033064	0.795763	0.003229	0.711142
-17.012176	-1.941096	0.800768	0.003323	0.711146
-16.862064	-2.066271	0.805773	0.003295	0.710950
-17.587813	-1.976464	0.810778	0.003430	0.710871
-17.322595	-2.018087	0.815782	0.003381	0.710882
-17.600950	-1.972933	0.820787	0.003433	0.710873
-17.528793	-1.983164	0.825792	0.003419	0.710879
-17.205318	-2.041347	0.830797	0.003359	0.710878
-17.653518	-2.004199	0.835802	0.003442	0.710792
-18.280717	-2.016128	0.840806	0.003559	0.710546
-18.115628	-2.050698	0.845811	0.003528	0.710535
-18.770821	-1.931078	0.850816	0.003650	0.710541
-18.470921	-1.986624	0.855821	0.003594	0.710537
-18.401071	-2.001291	0.860826	0.003581	0.710533
-18.554601	-1.969858	0.865830	0.003610	0.710541
-18.686645	-1.970625	0.870835	0.003634	0.710492
-19.233134	-2.007503	0.875840	0.003736	0.710224
-19.188874	-2.016906	0.880845	0.003728	0.710221
-19.767928	-1.915423	0.885850	0.003836	0.710218
-19.231124	-2.007876	0.890854	0.003736	0.710224
-19.307431	-1.997316	0.895859	0.003750	0.710218
-19.732023	-1.918985	0.900864	0.003829	0.710224
-19.670199	-1.930737	0.905869	0.003817	0.710222
-19.691738	-2.053069	0.910874	0.003821	0.709970
-20.041786	-2.026285	0.915878	0.003886	0.709899
-20.261896	-1.991188	0.920883	0.003927	0.709891
-20.084999	-2.020871	0.925888	0.003894	0.709895
-20.116179	-2.014837	0.930893	0.003900	0.709896
-20.626663	-1.927095	0.935898	0.003995	0.709889
-20.167934	-2.003646	0.940902	0.003910	0.709900
-20.725705	-2.043310	0.945907	0.004014	0.709622
-21.116584	-1.983240	0.950912	0.004086	0.709603
-21.221499	-1.966213	0.955917	0.004106	0.709599
-20.899233	-2.026253	0.960922	0.004046	0.709594
-20.878381	-2.025512	0.965926	0.004042	0.709603
-21.375872	-1.941096	0.970931	0.004134	0.709595
-21.148065	-1.978994	0.975936	0.004092	0.709600
-21.288806	-2.110978	0.980941	0.004118	0.709286
-22.203161	-1.958310	0.985946	0.004288	0.709265
-22.305443	-1.934573	0.990950	0.004307	0.709277
-21.763215	-2.035960	0.995955	0.004206	0.709267
-21.930174	-2.005846	1.000960	0.004237	0.709268
-22.134204	-1.967330	1.005965	0.004275	0.709272
-22.100929	-1.977425	1.010970	0.004269	0.709264
-22.258305	-2.085975	1.015974	0.004299	0.708991
-22.879948	-1.991823	1.020979	0.004414	0.708957
-22.775546	-2.008082	1.025984	0.004395	0.708962
-22.524260	-2.053289	1.030989	0.004348	0.708961
-23.059697	-1.960113	1.035994	0.004448	0.708957
-22.812721	-1.999639	1.040998	0.004402	0.708966
-22.686123	-2.054981	1.046003	0.004378	0.708900
-23.684590	-2.006654	1.051008	0.004564	0.708641
-23.713941	-1.998375	1.056013	0.004569	0.708647
-23.835004	-1.980414	1.061018	0.004592	0.708640
-23.567558	-2.024331	1.066022	0.004542	0.708647
-24.004022	-1.951365	1.071027	0.004623	0.708638
-24.051675	-1.940720	1.076032	0.004632	0.708642
-23.560979	-2.029688	1.081037	0.004541	0.708639
-24.424763	-2.019725	1.086042	0.004701	0.708351
-24.625408	-1.978969	1.091046	0.004739	0.708361
-24.428560	-2.019382	1.096051	0.004702	0.708350
-24.592262	-1.987899	1.101056	0.004733	0.708355
-24.717981	-1.965523	1.106061	0.004756	0.708355
-24.664071	-1.978551	1.111066	0.004746	0.708348
-24.299909	-2.060548	1.116070	0.004678	0.708314
-25.415712	-2.011005	1.121075	0.004886	0.708015
-25.734543	-1.952729	1.126080	0.004945	0.708018
-25.472772	-1.997665	1.131085	0.004896	0.708021
-25.599614	-1.978981	1.136090	0.004920	0.708013
-25.482244	-1.994403	1.141094	0.004898	0.708025
-25.598478	-1.978934	1.146099	0.004920	0.708014
-25.318140	-2.025467	1.151104	0.004867	0.708021
-25.961921	-2.062867	1.156109	0.004987	0.707716
-26.425929	-1.987976	1.161114	0.005074	0.707700
-26.228960	-2.018017	1.166118	0.005037	0.707711
-26.537806	-1.968174	1.171123	0.005094	0.707700
-26.664916	-1.941230	1.176128	0.005118	0.707709
-26.255460	-2.014982	1.181133	0.005042	0.707707
-26.643951	-1.948803	1.186138	0.005114	0.707701
-26.828108	-2.038723	1.191142	0.005148	0.707455
-27.319393	-1.988878	1.196147	0.005240	0.707380
-27.068179	-2.032286	1.201152	0.005193	0.707382
-27.209411	-2.004926	1.206157	0.005219	0.707387
-27.647484	-1.929906	1.211162	0.005301	0.707381
-26.907499	-2.058102	1.216166	0.005163	0.707388
-27.126379	-2.023358	1.221171	0.005204	0.707380
-28.301297	-1.951899	1.226176	0.005422	0.707103
-28.027632	-2.008020	1.231181	0.005371	0.707088
-28.244080	-1.972346	1.236186	0.005412	0.707082
-28.020846	-2.007231	1.241190	0.005370	0.707092
-28.186834	-1.982340	1.246195	0.005401	0.707083
-28.245941	-1.969930	1.251200	0.005412	0.707087
-28.213422	-1.975563	1.256205	0.005406	0.707087
-28.432856	-2.045674	1.261210	0.005447	0.706868
-29.280571	-1.947685	1.266214	0.005604	0.706761
-29.254882	-1.957308	1.271219	0.005600	0.706751
-29.414324	-1.927636	1.276224	0.005629	0.706754
-29.095282	-1.982399	1.281229	0.005570	0.706758
-29.226960	-1.962378	1.286234	0.005594	0.706751
-29.413989	-1.924135	1.291238	0.005629	0.706761
-29.516368	-1.910308	1.296243	0.005648	0.706752
-29.545145	-2.055796	1.301248	0.005653	0.706450
-29.972690	-1.979536	1.306253	0.005733	0.706450
-30.547279	-1.879940	1.311258	0.005840	0.706444
-29.825634	-2.004103	1.316262	0.005706	0.706453
-29.646467	-2.040461	1.321267	0.005672	0.706445
-30.548753	-1.877905	1.326272	0.005840	0.706448
-29.972874	-1.979037	1.331277	0.005733	0.706451
-30.437213	-2.038895	1.336282	0.005819	0.706165
-30.932619	-1.965407	1.341286	0.005912	0.706135
-30.968101	-1.962490	1.346291	0.005918	0.706128
-30.837349	-1.984820	1.351296	0.005894	0.706130
-30.941517	-1.965001	1.356301	0.005913	0.706133
-31.384673	-1.889800	1.361306	0.005996	0.706125
-30.793511	-1.991524	1.366310	0.005885	0.706133
-30.942978	-2.063083	1.371315	0.005913	0.705935
-32.141240	-1.886261	1.376320	0.006136	0.705861
-31.617969	-1.975691	1.381325	0.006039	0.705869
-31.624395	-1.979040	1.386330	0.006040	0.705860
-31.867643	-1.930469	1.391334	0.006085	0.705871
-31.929040	-1.924251	1.396339	0.006097	0.705861
-31.746831	-1.956065	1.401344	0.006063	0.705863
-32.008683	-2.044133	1.406349	0.006112	0.705592
-32.957689	-1.908890	1.411354	0.006288	0.705523
-32.451443	-1.993776	1.416358	0.006194	0.705534
-32.168440	-2.046779	1.421363	0.006141	0.705529
-32.918930	-1.912905	1.426368	0.006281	0.705529
-32.738951	-1.945719	1.431373	0.006247	0.705528
-32.454351	-2.000170	1.436378	0.006194	0.705521
-33.138567	-2.027142	1.441382	0.006322	0.705221
-33.826135	-1.910260	1.446387	0.006450	0.705209
-33.684548	-1.932895	1.451392	0.006423	0.705215
-33.259706	-2.006880	1.456397	0.006344	0.705218
-33.898736	-1.899077	1.461402	0.006463	0.705206
-33.694788	-1.930193	1.466406	0.006425	0.705217
-33.417180	-1.983630	1.471411	0.006373	0.705209
-34.049383	-1.993333	1.476416	0.006491	0.704962
-34.696694	-1.912029	1.481421	0.006611	0.704894
-34.212575	-2.002010	1.486426	0.006521	0.704886
-34.364181	-1.973036	1.491430	0.006550	0.704890
-34.885553	-1.881514	1.496435	0.006647	0.704888
-34.321780	-1.981122	1.501440	0.006542	0.704889
-34.027336	-2.032599	1.506445	0.006487	0.704892
-35.079599	-1.955811	1.511450	0.006683	0.704668
-35.554945	-1.907898	1.516454	0.006771	0.704594
-34.724194	-2.059909	1.521459	0.006616	0.704587
-35.092860	-1.992626	1.526464	0.006685	0.704590
-35.459191	-1.924365	1.531469	0.006753	0.704596
-35.439577	-1.930294	1.536474	0.006749	0.704591
-34.990676	-2.007721	1.541478	0.006666	0.704596
-35.703006	-2.020602	1.546483	0.006798	0.704314
-36.283493	-1.944438	1.551488	0.006906	0.704259
-36.139540	-1.968585	1.556493	0.006880	0.704262
-36.420682	-1.920583	1.561498	0.006932	0.704258
-36.147584	-1.966283	1.566502	0.006881	0.704264
-35.944391	-2.004282	1.571507	0.006843	0.704261
-36.007196	-1.993542	1.576512	0.006855	0.704260
-36.717199	-1.999606	1.581517	0.006987	0.703993
-37.088999	-1.956453	1.586522	0.007056	0.703946
-36.856540	-1.993285	1.591526	0.007013	0.703955
-37.108004	-1.950495	1.596531	0.007060	0.703951
-37.135241	-1.944625	1.601536	0.007065	0.703953
-36.845212	-1.994197	1.606541	0.007011	0.703958
-37.038001	-1.963649	1.611546	0.007047	0.703950
-37.526149	-2.016514	1.616550	0.007137	0.703668
-37.780640	-1.987417	1.621555	0.007185	0.703635
-37.820858	-1.977996	1.626560	0.007192	0.703640
-37.601149	-2.016193	1.631565	0.007151	0.703642
-37.744330	-1.995492	1.636570	0.007178	0.703632
-37.729970	-1.994370	1.641574	0.007175	0.703640
-37.861894	-2.014277	1.646579	0.007200	0.703552
-38.783321	-1.952846	1.651584	0.007371	0.703344
-38.115292	-2.069160	1.656589	0.007247	0.703350
-38.773097	-1.957321	1.661594	0.007369	0.703339
-38.876068	-1.933386	1.666598	0.007388	0.703351
-38.652605	-1.974767	1.671603	0.007347	0.703348
-38.690367	-1.968955	1.676608	0.007354	0.703346
-38.841718	-2.025272	1.681613	0.007382	0.703178
-40.094688	-1.887121	1.686618	0.007615	0.703006
-39.295176	-2.023908	1.691622	0.007466	0.703017
-39.760262	-1.945149	1.696627	0.007553	0.703009
-39.846039	-1.929190	1.701632	0.007569	0.703010
-39.416597	-2.003588	1.706637	0.007489	0.703015
-39.759628	-1.947480	1.711642	0.007553	0.703005
-39.862152	-1.959488	1.716646	0.007572	0.702943
-40.428514	-1.979922	1.721651	0.007677	0.702698
-40.254657	-2.011222	1.726656	0.007645	0.702698
-40.719038	-1.926367	1.731661	0.007731	0.702702
-40.519047	-1.967310	1.736666	0.007694	0.702691
-40.155501	-2.026754	1.741670	0.007626	0.702702
-40.481325	-1.972784	1.746675	0.007687	0.702694
-40.778430	-1.957846	1.751680	0.007742	0.702617
-41.279021	-1.986742	1.756685	0.007835	0.702378
-41.039267	-2.033615	1.761690	0.007791	0.702370
-41.434836	-1.961260	1.766694	0.007864	0.702374
-41.353676	-1.975646	1.771699	0.007849	0.702374
-41.262647	-1.991175	1.776704	0.007832	0.702376
-41.526314	-1.940563	1.781709	0.007881	0.702383
-41.562088	-1.987336	1.786714	0.007888	0.702276
-42.067276	-1.992080	1.791718	0.007982	0.702084
-42.162892	-1.980426	1.796723	0.008000	0.702073
-42.778327	-1.870795	1.801728	0.008114	0.702073
-42.129816	-1.982256	1.806733	0.007993	0.702081
-42.297149	-1.956695	1.811738	0.008025	0.702073
-42.700144	-1.882012	1.816742	0.008100	0.702079
-42.537819	-1.911797	1.821747	0.008069	0.702077
-42.761890	-2.022304	1.826752	0.008111	0.701773
-43.349804	-1.927607	1.831757	0.008220	0.701752
-43.552126	-1.895958	1.836762	0.008258	0.701743
-42.778982	-2.028490	1.841766	0.008114	0.701754
-43.127123	-1.968256	1.846771	0.008179	0.701750
-43.602018	-1.885341	1.851776	0.008267	0.701747
-43.128532	-1.967835	1.856781	0.008179	0.701751
-43.677347	-1.985853	1.861786	0.008281	0.701516
-44.395245	-1.892493	1.866790	0.008415	0.701446
-43.911148	-1.982625	1.871795	0.008325	0.701439
-43.972726	-1.972524	1.876800	0.008336	0.701437
-44.100531	-1.946372	1.881805	0.008360	0.701444
-44.253518	-1.922593	1.886810	0.008388	0.701437
-43.864429	-1.987379	1.891814	0.008316	0.701446
-44.324139	-2.013099	1.896819	0.008401	0.701228
-45.421941	-1.869781	1.901824	0.008606	0.701122
-44.879918	-1.964039	1.906829	0.008505	0.701127
-44.772418	-1.985898	1.911834	0.008485	0.701122
-45.182945	-1.908484	1.916838	0.008561	0.701130
-45.048352	-1.935406	1.921843	0.008536	0.701124
-44.849583	-1.970535	1.926848	0.008499	0.701125
-45.064100	-1.999936	1.931853	0.008539	0.700988
-46.010470	-1.886296	1.936858	0.008715	0.700876
-45.453897	-1.981418	1.941862	0.008612	0.700885
-45.314518	-2.009655	1.946867	0.008586	0.700878
-45.901392	-1.906187	1.951872	0.008695	0.700876
-45.816601	-1.918179	1.956877	0.008679	0.700882
-45.753811	-1.933837	1.961882	0.008667	0.700873
-46.157922	-2.012966	1.966886	0.008742	0.700567
-46.548947	-1.957127	1.971891	0.008815	0.700539
-46.751699	-1.921617	1.976896	0.008853	0.700537
-46.408556	-1.979606	1.981901	0.008789	0.700544
-46.963441	-1.885728	1.986906	0.008892	0.700534
-46.669862	-1.933493	1.991910	0.008838	0.700543
-46.345505	-2.013620	1.996915	0.008777	0.700498
-47.504385	-1.940929	2.001920	0.008993	0.700226

-47.610216	-1.924276	2.011917	0.009013	0.700222
-47.587173	-1.929025	2.021914	0.009008	0.700221
-47.385661	-1.963905	2.031910	0.008971	0.700223
-47.261920	-1.985572	2.041907	0.008948	0.700224
-47.465022	-1.949105	2.051904	0.008985	0.700225
-47.563358	-1.933981	2.061901	0.009004	0.700220
-47.626875	-1.921483	2.071898	0.009015	0.700222
-47.491322	-1.945410	2.081894	0.008990	0.700223
-47.360586	-1.968246	2.091891	0.008966	0.700224
-47.424667	-1.955763	2.101888	0.008977	0.700226
-47.371171	-1.967600	2.111885	0.008967	0.700222
-47.636956	-1.921111	2.121882	0.009017	0.700220
-47.133488	-1.931994	2.131878	0.008923	0.700380
-46.515814	-1.964805	2.141875	0.008808	0.700537
-46.664126	-1.937339	2.151872	0.008835	0.700539
-46.326256	-1.999580	2.161869	0.008773	0.700535
-46.594466	-1.951928	2.171866	0.008822	0.700535
-46.462715	-1.938589	2.181862	0.008798	0.700610
-45.435057	-1.990217	2.191859	0.008606	0.700877
-45.549695	-1.969913	2.201856	0.008628	0.700877
-45.575875	-1.965460	2.211853	0.008632	0.700876
-45.663363	-1.950615	2.221850	0.008649	0.700875
-45.111911	-1.951879	2.231846	0.008546	0.701072
-44.946017	-1.954283	2.241843	0.008515	0.701127
-44.981757	-1.948744	2.251840	0.008522	0.701125
-44.943583	-1.929605	2.261837	0.008514	0.701178
-44.295947	-1.915318	2.271834	0.008394	0.701441
-44.148145	-1.942701	2.281830	0.008366	0.701439
-44.170741	-1.937305	2.291827	0.008370	0.701442
-43.607189	-1.928438	2.301824	0.008265	0.701663
-43.290145	-1.943596	2.311821	0.008206	0.701747
-43.346662	-1.933928	2.321818	0.008217	0.701747
-42.997610	-1.966491	2.331814	0.008152	0.701807
-42.521646	-1.919147	2.341811	0.008063	0.702074
-42.250043	-1.966943	2.351808	0.008012	0.702076
-42.515687	-1.919831	2.361805	0.008062	0.702075
-42.016316	-1.897132	2.371802	0.007969	0.702301
-41.613153	-1.936766	2.381798	0.007894	0.702367
-41.588949	-1.938940	2.391795	0.007889	0.702371
-41.386879	-1.919555	2.401792	0.007851	0.702483
-40.682093	-1.941804	2.411789	0.007720	0.702693
-40.879878	-1.907915	2.421786	0.007757	0.702690
-40.582453	-1.959385	2.431782	0.007701	0.702693
-40.143565	-1.894301	2.441779	0.007619	0.702983
-39.763988	-1.950510	2.451776	0.007549	0.703006
-39.887149	-1.927916	2.461773	0.007572	0.703008
-39.720716	-1.875497	2.471770	0.007541	0.703173
-38.990296	-1.921910	2.481766	0.007404	0.703343
-38.992075	-1.921190	2.491763	0.007405	0.703344
-38.938769	-1.917903	2.501760	0.007395	0.703370
-38.336111	-1.893063	2.511757	0.007282	0.703637
-38.126030	-1.932904	2.521754	0.007243	0.703632
-38.040900	-1.947795	2.531750	0.007227	0.703633
-37.663857	-1.915376	2.541747	0.007157	0.703834
-37.145439	-1.947928	2.551744	0.007061	0.703955
-37.423473	-1.900202	2.561741	0.007112	0.703951
-37.194313	-1.916204	2.571738	0.007069	0.704002
-36.479591	-1.915479	2.581734	0.006936	0.704260
-36.316612	-1.944946	2.591731	0.006906	0.704259
-36.345945	-1.938460	2.601728	0.006911	0.704262
-35.882331	-1.900011	2.611725	0.006825	0.704506
-35.476225	-1.932528	2.621722	0.006749	0.704587
-35.338179	-1.956697	2.631718	0.006724	0.704588
-35.256125	-1.956649	2.641715	0.006708	0.704617
-34.560339	-1.946526	2.651712	0.006579	0.704888
-34.665060	-1.928229	2.661709	0.006598	0.704887
-34.447242	-1.966889	2.671706	0.006557	0.704888
-34.332434	-1.906856	2.681702	0.006536	0.705050
-33.627903	-1.951897	2.691699	0.006405	0.705212
-33.595373	-1.957680	2.701696	0.006399	0.705212
-33.736896	-1.932512	2.711693	0.006425	0.705212
-32.959719	-1.916891	2.721690	0.006280	0.705523
-32.919115	-1.923065	2.731686	0.006272	0.705525
-32.735741	-1.954573	2.741683	0.006238	0.705528
-32.583500	-1.886063	2.751680	0.006210	0.705720
-31.984148	-1.920156	2.761677	0.006098	0.705867
-31.900047	-1.936181	2.771674	0.006082	0.705865
-32.039053	-1.897474	2.781670	0.006108	0.705893
-31.276381	-1.915804	2.791667	0.005966	0.706129
-31.105198	-1.947313	2.801664	0.005934	0.706128
-31.368991	-1.900624	2.811661	0.005983	0.706127
-30.531120	-1.922126	2.821658	0.005827	0.706384
-30.594856	-1.880960	2.831654	0.005839	0.706444
-30.190023	-1.951630	2.841651	0.005764	0.706447
-30.235852	-1.875688	2.851648	0.005772	0.706584
-29.589657	-1.906048	2.861645	0.005652	0.706754
-29.611614	-1.903480	2.871642	0.005656	0.706751
-29.709837	-1.851208	2.881638	0.005674	0.706821
-28.449970	-1.945379	2.891635	0.005439	0.707083
-28.653173	-1.908053	2.901632	0.005477	0.707086
-28.632013	-1.913482	2.911629	0.005473	0.707083
-28.006277	-1.916375	2.921626	0.005356	0.707301
-28.066922	-1.866333	2.931622	0.005368	0.707380
-27.627505	-1.944719	2.941619	0.005286	0.707380
-27.672598	-1.886967	2.951616	0.005294	0.707479
-26.742161	-1.943402	2.961613	0.005121	0.707699
-26.842554	-1.924089	2.971610	0.005139	0.707702
-26.921916	-1.909615	2.981606	0.005154	0.707703
-26.156524	-1.932033	2.991603	0.005012	0.707932
-26.089812	-1.901225	3.001600	0.004999	0.708017
-25.938382	-1.928004	3.011597	0.004971	0.708018
-26.050306	-1.870731	3.021594	0.004992	0.708093
-25.182577	-1.895915	3.031590	0.004830	0.708352
-24.781450	-1.966690	3.041587	0.004755	0.708354
-25.036378	-1.922057	3.051584	0.004803	0.708352
-24.379596	-1.948370	3.061581	0.004680	0.708534
-24.361128	-1.898702	3.071578	0.004677	0.708641
-24.252496	-1.917696	3.081574	0.004656	0.708641
-24.202145	-1.902110	3.091571	0.004647	0.708691
-23.330944	-1.923458	3.101568	0.004485	0.708959
-23.234381	-1.941862	3.111565	0.004467	0.708957
-23.504642	-1.894537	3.121562	0.004517	0.708955
-22.844269	-1.916133	3.131558	0.004394	0.709148
-22.094391	-1.990951	3.141555	0.004254	0.709266
-22.498123	-1.918395	3.151552	0.004329	0.709267
-22.181822	-1.974125	3.161549	0.004270	0.709268
-21.821766	-1.884134	3.171546	0.004203	0.709577
-21.503385	-1.932029	3.181542	0.004144	0.709595
-21.449261	-1.939353	3.191539	0.004134	0.709599
-21.290855	-1.895430	3.201536	0.004104	0.709744
-20.596723	-1.942978	3.211533	0.003975	0.709896
-20.812493	-1.905134	3.221530	0.004015	0.709895
-20.691585	-1.920410	3.231526	0.003992	0.709908
-19.939166	-1.897418	3.241523	0.003852	0.710222
-19.878775	-1.909845	3.251520	0.003841	0.710219
-19.700631	-1.942241	3.261517	0.003808	0.710217
-19.368025	-1.909931	3.271514	0.003746	0.710401
-18.737496	-1.954399	3.281510	0.003628	0.710536
-18.950731	-1.917713	3.291507	0.003668	0.710534
-18.818372	-1.940501	3.301504	0.003643	0.710536
-18.068065	-1.914084	3.311501	0.003503	0.710855
-17.980517	-1.920743	3.321498	0.003487	0.710873
-17.741694	-1.962150	3.331494	0.003443	0.710876
-17.842958	-1.908619	3.341491	0.003461	0.710947
-17.152755	-1.934330	3.351488	0.003333	0.711141
-17.365610	-1.894739	3.361485	0.003372	0.711145
-17.339729	-1.900900	3.371482	0.003367	0.711142
-16.564737	-1.881006	3.381478	0.003223	0.711457
-16.409393	-1.906516	3.391475	0.003194	0.711461
-16.415410	-1.906524	3.401472	0.003195	0.711459
-15.719204	-1.921823	3.411469	0.003065	0.711676
-15.749102	-1.872697	3.421466	0.003071	0.711764
-15.385687	-1.938456	3.431462	0.003003	0.711762
-15.416133	-1.886954	3.441459	0.003009	0.711854
-14.463196	-1.935774	3.451456	0.002831	0.712095
-14.743467	-1.886209	3.461453	0.002883	0.712095
-14.771457	-1.882382	3.471450	0.002889	0.712092
-13.765286	-1.936837	3.481446	0.002701	0.712341
-13.748765	-1.914302	3.491443	0.002698	0.712392
-13.676503	-1.925081	3.501440	0.002684	0.712396
-13.682157	-1.884153	3.511437	0.002685	0.712476
-12.931276	-1.899798	3.521434	0.002546	0.712711
-12.702674	-1.938511	3.531430	0.002503	0.712715
-12.953463	-1.893927	3.541427	0.002550	0.712715
-12.220166	-1.900465	3.551424	0.002413	0.712963
-12.051954	-1.897707	3.561421	0.002382	0.713028
-12.065399	-1.897141	3.571418	0.002384	0.713024
-11.861412	-1.864463	3.581414	0.002346	0.713162
-11.057054	-1.905266	3.591411	0.002196	0.713366
-10.940000	-1.925162	3.601408	0.002174	0.713368
-11.141569	-1.889821	3.611405	0.002212	0.713367
-10.399466	-1.896349	3.621402	0.002074	0.713617
-10.279820	-1.897249	3.631398	0.002051	0.713658
-10.226779	-1.905699	3.641395	0.002041	0.713660
-9.914573	-1.915078	3.651392	0.001983	0.713752
-9.442339	-1.885051	3.661389	0.001895	0.713979
-9.315521	-1.909870	3.671386	0.001871	0.713975
-9.640043	-1.853058	3.681382	0.001932	0.713973
-8.730531	-1.865453	3.691379	0.001762	0.714270
-8.489433	-1.900954	3.701376	0.001717	0.714285
-8.627373	-1.877227	3.711373	0.001743	0.714283
-8.245738	-1.853047	3.721370	0.001672	0.714467
-7.458642	-1.920206	3.731366	0.001525	0.714612
-7.605787	-1.893896	3.741363	0.001553	0.714612
-6.985208	-2.003532	3.751360	0.001437	0.714614
-6.781190	-1.933801	3.761357	0.001399	0.714825
-6.276866	-1.979291	3.771354	0.001305	0.714913
-6.480971	-1.942046	3.781350	0.001343	0.714915
-6.064121	-2.015936	3.791347	0.001265	0.714916
-5.822551	-1.953083	3.801344	0.001220	0.715126
-5.592148	-1.938130	3.811341	0.001177	0.715237
-5.455292	-1.962888	3.821338	0.001152	0.715237
-5.413567	-1.970382	3.831334	0.001144	0.715237
-4.633854	-1.974890	3.841331	0.000999	0.715503
-4.383353	-1.994508	3.851328	0.000952	0.715553
-4.454564	-1.982475	3.861325	0.000965	0.715552
-4.383682	-1.996662	3.871322	0.000952	0.715549
-3.919917	-1.925263	3.881318	0.000865	0.715854
-3.400973	-2.000929	3.891315	0.000769	0.715888
-3.386295	-2.003014	3.901312	0.000766	0.715889
-3.492633	-1.972736	3.911309	0.000786	0.715911
-2.833717	-1.977126	3.921306	0.000663	0.716135
-2.829541	-1.976788	3.931302	0.000662	0.716138
-2.657586	-2.006494	3.941299	0.000630	0.716139
-2.704549	-1.903494	3.951296	0.000639	0.716327
-1.962350	-1.971042	3.961293	0.000500	0.716455
-1.872504	-1.986990	3.971290	0.000484	0.716455
-1.919353	-1.937300	3.981286	0.000492	0.716537
-1.079264	-1.973380	3.991283	0.000336	0.716762
-1.629726	-1.873218	4.001280	0.000438	0.716767
-1.429687	-1.882099	4.011277	0.000401	0.716820
-1.215006	-1.783660	4.021274	0.000361	0.717090
-1.241672	-1.779604	4.031270	0.000366	0.717089
-0.520427	-1.828997	4.041267	0.000231	0.717246
-0.925228	-1.684202	4.051264	0.000306	0.717389
-0.969628	-1.649559	4.061261	0.000315	0.717442
-0.793680	-1.545759	4.071258	0.000282	0.717710
-1.226266	-1.437849	4.081254	0.000362	0.717771
-0.500053	-1.439553	4.091251	0.000227	0.718023
-0.380946	-1.419251	4.101248	0.000205	0.718105
-0.251037	-1.314604	4.111245	0.000180	0.718358
-0.223786	-1.260665	4.121242	0.000175	0.718474
-0.411774	-1.138688	4.131238	0.000210	0.718649
-0.461706	-1.006547	4.141235	0.000219	0.718892
-0.364490	-0.941178	4.151232	0.000201	0.719055
-0.155068	-0.866649	4.161229	0.000162	0.719276
-0.031301	-0.751024	4.171226	0.000139	0.719548
-0.071100	-0.649400	4.181222	0.000146	0.719734
-0.122019	-0.532127	4.191219	0.000155	0.719947
-0.012781	-0.407794	4.201216	0.000135	0.720231
-0.018445	-0.266513	4.211213	0.000136	0.720507
-0.073907	-0.120481	4.221210	0.000146	0.720775
-0.058152	-0.000467	4.231206	0.000143	0.721017
0.000000	0.142447	4.241203	0.000132	0.721319

0.080755	0.761457	4.246208	0.000116	0.722563
0.490005	1.962876	4.251213	0.000039	0.725061
0.671400	3.791081	4.256218	0.000004	0.728691
0.904819	6.165205	4.261222	-0.000041	0.733379
1.399077	9.003094	4.266227	-0.000135	0.739016
1.687646	12.352480	4.271232	-0.000191	0.745515
1.864880	16.182424	4.276237	-0.000226	0.752826
2.142033	20.392716	4.281242	-0.000281	0.760810
2.612622	24.963964	4.286246	-0.000371	0.769439
3.118949	29.908455	4.291251	-0.000469	0.778664
3.294038	35.246906	4.296256	-0.000505	0.788384
3.694144	40.866971	4.301261	-0.000583	0.798558
4.208296	46.768026	4.306266	-0.000683	0.809131
4.595173	52.968841	4.311270	-0.000759	0.820047
5.280786	59.406479	4.316275	-0.000891	0.831313
5.568317	66.121224	4.321280	-0.000949	0.842777
5.993494	73.041373	4.326285	-0.001032	0.854468
6.473166	80.154085	4.331290	-0.001126	0.866332
7.586801	87.342982	4.336294	-0.001338	0.878339
12.332370	94.123745	4.341299	-0.002226	0.890549
12.978502	101.811209	4.346304	-0.002352	0.902886
13.381889	109.691138	4.351309	-0.002432	0.915288
13.774183	117.669490	4.356314	-0.002510	0.927671
14.945056	125.634449	4.361318	-0.002734	0.940076
16.121103	133.727694	4.366323	-0.002958	0.952512
17.142330	141.919588	4.371328	-0.003153	0.964892
18.141202	150.218568	4.376333	-0.003345	0.977263
18.840285	158.642131	4.381338	-0.003480	0.989584
19.477911	167.111333	4.386342	-0.003605	1.001802
20.393661	175.572574	4.391347	-0.003781	1.013928
21.280828	184.060880	4.396352	-0.003952	1.025942
22.325924	192.581364	4.401357	-0.004152	1.037897
23.151990	201.163242	4.406362	-0.004311	1.049747
23.979794	209.767030	4.411366	-0.004471	1.061494
24.523591	218.461674	4.416371	-0.004578	1.073167
25.330792	227.083438	4.421376	-0.004734	1.084679
25.939714	235.770005	4.426381	-0.004853	1.096108
26.631825	244.421938	4.431386	-0.004987	1.107394
27.094530	253.121901	4.436390	-0.005079	1.118576
27.694188	261.792350	4.441395	-0.005197	1.129639
28.373771	270.437358	4.446400	-0.005329	1.140580
29.037494	279.114422	4.451405	-0.005458	1.151454
29.969870	287.712124	4.456410	-0.005637	1.162184
30.563129	296.352577	4.461414	-0.005754	1.172797
31.025020	305.003230	4.466419	-0.005845	1.183300
31.820480	313.586144	4.471424	-0.005999	1.193698
32.846393	322.114034	4.476429	-0.006196	1.203986
33.503446	330.710210	4.481434	-0.006324	1.214194
33.905880	339.318703	4.486438	-0.006404	1.224280
34.765266	347.873013	4.491443	-0.006570	1.234311
35.651992	356.364613	4.496448	-0.006740	1.244194
36.264146	364.921123	4.501453	-0.006860	1.254019
37.047978	373.421389	4.506458	-0.007012	1.263738
37.536633	381.968726	4.511462	-0.007108	1.273378
38.248047	390.454730	4.516467	-0.007246	1.282920
38.499475	399.000276	4.521472	-0.007299	1.292372
39.230033	407.456307	4.526477	-0.007440	1.301744
39.701894	416.014179	4.531482	-0.007534	1.311113
40.335250	424.489811	4.536486	-0.007657	1.320356
41.016477	432.891591	4.541491	-0.007789	1.329464
41.626671	441.296921	4.546496	-0.007909	1.338501
41.933389	449.738183	4.551501	-0.007971	1.347461
42.606318	458.125756	4.556506	-0.008102	1.356370
43.140360	466.503287	4.561510	-0.008207	1.365186
44.067963	474.846931	4.566515	-0.008385	1.373978
44.790259	483.190535	4.571520	-0.008525	1.382679
45.216635	491.605738	4.576525	-0.008610	1.391348
45.384729	500.023220	4.581530	-0.008647	1.399921
45.988741	508.337598	4.586534	-0.008765	1.408412
46.700532	516.659680	4.591539	-0.008903	1.416877
47.268344	524.968488	4.596544	-0.009014	1.425254
47.669991	533.333329	4.601549	-0.009094	1.433611
48.174967	541.641951	4.606554	-0.009194	1.441880
48.695119	549.955177	4.611558	-0.009296	1.450109
49.030477	558.302459	4.616563	-0.009364	1.458295
49.443716	566.605546	4.621568	-0.009446	1.466405
50.130260	574.926170	4.626573	-0.009580	1.474529
50.643105	583.204022	4.631578	-0.009680	1.482541
51.016641	591.485651	4.636582	-0.009755	1.490492
51.423810	599.786590	4.641587	-0.009837	1.498424
51.804921	608.044412	4.646592	-0.009913	1.506269
52.188041	616.333841	4.651597	-0.009990	1.514103
52.862172	624.541904	4.656602	-0.010121	1.521866
53.279426	632.799999	4.661606	-0.010204	1.529596
53.982690	641.033172	4.666611	-0.010340	1.537307
54.525078	649.265926	4.671616	-0.010447	1.544955
55.137420	657.524421	4.676621	-0.010566	1.552599
55.579407	665.769972	4.681626	-0.010654	1.560168
55.966645	674.002641	4.686630	-0.010731	1.567681
56.866851	682.202256	4.691635	-0.010904	1.575203
57.482181	690.402468	4.696640	-0.011024	1.582648
57.940242	698.655302	4.701645	-0.011115	1.590083
58.051015	706.948971	4.706650	-0.011141	1.597469
58.504771	715.146010	4.711654	-0.011231	1.604785
58.979138	723.373103	4.716659	-0.011325	1.612096
59.521018	731.560932	4.721664	-0.011431	1.619350
59.926797	739.789268	4.726669	-0.011512	1.626587
60.215455	748.078880	4.731674	-0.011571	1.633829
60.609705	756.258027	4.736678	-0.011650	1.640958
61.097108	764.438763	4.741683	-0.011746	1.648070
61.801664	772.594761	4.746688	-0.011882	1.655160
62.135101	780.795353	4.751693	-0.011950	1.662208
62.486228	789.003876	4.756698	-0.012021	1.669234
62.837958	797.205559	4.761702	-0.012091	1.676225
63.451043	805.352825	4.766707	-0.012211	1.683176
63.761062	813.544218	4.771712	-0.012274	1.690095
64.429823	821.703516	4.776717	-0.012404	1.697006
64.963182	829.876491	4.781722	-0.012509	1.703883
65.063080	838.115568	4.786726	-0.012533	1.710730
65.365430	846.319961	4.791731	-0.012594	1.717547
65.845702	854.435624	4.796736	-0.012689	1.724287
66.067829	862.641086	4.801741	-0.012736	1.731041
66.547322	870.799616	4.806746	-0.012830	1.737764
67.171462	878.915494	4.811750	-0.012952	1.744444
67.567645	887.111348	4.816755	-0.013031	1.751134
67.847973	895.286351	4.821760	-0.013089	1.757767
67.994750	903.464760	4.826765	-0.013121	1.764362
68.671473	911.592544	4.831770	-0.013253	1.770957
68.993967	919.764125	4.836774	-0.013318	1.777518
69.621317	927.890743	4.841779	-0.013440	1.784058
70.171006	936.046256	4.846784	-0.013548	1.790586
70.505709	944.253145	4.851789	-0.013616	1.797105
70.911640	952.382923	4.856794	-0.013696	1.803548
71.322716	960.496498	4.861798	-0.013778	1.809956
71.897362	968.640023	4.866803	-0.013891	1.816384
72.188191	976.771538	4.871808	-0.013950	1.822747
72.486819	984.938835	4.876813	-0.014011	1.829115
73.114102	993.051161	4.881818	-0.014133	1.835458
73.158809	1001.227858	4.886822	-0.014147	1.841760
73.676591	1009.349039	4.891827	-0.014249	1.848053
74.081400	1017.496299	4.896832	-0.014329	1.854331
74.424514	1025.625830	4.901837	-0.014399	1.860568
74.572256	1033.796169	4.906842	-0.014431	1.866791
74.798627	1041.973468	4.911846	-0.014479	1.873009
75.402284	1050.069266	4.916851	-0.014597	1.879187
75.762504	1058.158247	4.921856	-0.014669	1.885312
76.153247	1066.300944	4.926861	-0.014747	1.891461
76.465780	1074.434684	4.931866	-0.014811	1.897575
76.942636	1082.527005	4.936870	-0.014905	1.903656
77.314400	1090.671044	4.941875	-0.014979	1.909744
77.809286	1098.776959	4.946880	-0.015077	1.915799
78.312470	1106.875298	4.951885	-0.015176	1.921830
78.478182	1115.029407	4.956890	-0.015212	1.927845
78.715169	1123.177089	4.961894	-0.015261	1.933844
79.029780	1131.306321	4.966899	-0.015325	1.939820
79.200945	1139.431407	4.971904	-0.015363	1.945759
79.881740	1147.535346	4.976909	-0.015495	1.951720
80.693251	1155.609886	4.981914	-0.015651	1.957655
81.028150	1163.710180	4.986918	-0.015719	1.963540
81.295038	1171.844160	4.991923	-0.015774	1.969423
81.594379	1179.953864	4.996928	-0.015835	1.975275
81.890881	1188.071711	5.001933	-0.015895	1.981115
82.264918	1196.189527	5.006938	-0.015970	1.986947
82.265439	1204.344873	5.011942	-0.015976	1.992748
82.897480	1212.420522	5.016947	-0.016099	1.998542
83.119799	1220.522340	5.021952	-0.016145	2.004295
83.752302	1228.578460	5.026957	-0.016269	2.010042
84.046127	1236.722279	5.031962	-0.016329	2.015799
84.372007	1244.809546	5.036966	-0.016395	2.021503
84.920440	1252.889792	5.041971	-0.016502	2.027209
85.285721	1261.029670	5.046976	-0.016575	2.032921
85.568940	1269.134905	5.051981	-0.016633	2.038585
86.156991	1277.194692	5.056986	-0.016748	2.044233
86.246165	1285.327852	5.061990	-0.016770	2.049865
86.568413	1293.453625	5.066995	-0.016835	2.055500
86.648671	1301.563047	5.072000	-0.016856	2.061084
87.098606	1309.637553	5.077005	-0.016945	2.066666
87.505236	1317.748813	5.082010	-0.017026	2.072254
87.701963	1325.855374	5.087014	-0.017068	2.077802
88.049454	1333.939541	5.092019	-0.017138	2.083335
88.391326	1342.014280	5.097024	-0.017207	2.088847
88.832322	1350.127660	5.102029	-0.017294	2.094380
89.379113	1358.190307	5.107034	-0.017401	2.099874
89.582969	1366.288625	5.112038	-0.017444	2.105344
90.176579	1374.393746	5.117043	-0.017560	2.110843
90.260098	1382.563305	5.122048	-0.017581	2.116321
90.289652	1390.653294	5.127053	-0.017592	2.121726
90.812538	1398.693391	5.132058	-0.017695	2.127132
91.335086	1406.751581	5.137062	-0.017797	2.132536
91.700903	1414.856430	5.142067	-0.017871	2.137942
92.124570	1422.907352	5.147072	-0.017955	2.143304
92.138630	1431.037901	5.152077	-0.017963	2.148666
92.475581	1439.143327	5.157082	-0.018031	2.154029
92.807947	1447.209371	5.162086	-0.018098	2.159353
93.369937	1455.258060	5.167091	-0.018208	2.164673
93.744348	1463.349390	5.172096	-0.018283	2.169990
93.895900	1471.471676	5.177101	-0.018317	2.175294
94.502516	1479.522823	5.182106	-0.018435	2.180581
94.481727	1487.628694	5.187110	-0.018436	2.185832
95.044755	1495.726973	5.192115	-0.018546	2.191120
95.300887	1503.840912	5.197120	-0.018599	2.196376
95.534470	1511.892664	5.202125	-0.018648	2.201578
96.094867	1519.941654	5.207130	-0.018758	2.206796
96.194727	1528.036418	5.212134	-0.018782	2.211989
96.481603	1536.133285	5.217139	-0.018840	2.217188
96.790612	1544.186686	5.222144	-0.018903	2.222348
96.907105	1552.293664	5.227149	-0.018930	2.227514
97.401655	1560.368088	5.232154	-0.019028	2.232681
97.556366	1568.444673	5.237158	-0.019062	2.237806
97.770733	1576.528103	5.242163	-0.019107	2.242930
97.857066	1584.623485	5.247168	-0.019128	2.248038
98.442211	1592.667885	5.252173	-0.019243	2.253147
98.705333	1600.760556	5.257178	-0.019297	2.258245
98.828877	1608.832914	5.262182	-0.019325	2.263308
99.227545	1616.913824	5.267187	-0.019405	2.268388
99.644486	1625.047237	5.272192	-0.019488	2.273491
99.764268	1633.116379	5.277197	-0.019515	2.278517
100.091899	1641.157849	5.282202	-0.019581	2.283532
100.713695	1649.157482	5.287206	-0.019703	2.288536
100.987117	1657.260242	5.292211	-0.019759	2.293562
101.063019	1665.356908	5.297216	-0.019778	2.298557
101.345868	1673.406741	5.302221	-0.019836	2.303530
101.764618	1681.470571	5.307226	-0.019919	2.308512
101.843797	1689.592746	5.312230	-0.019939	2.313491
102.372534	1697.604245	5.317235	-0.020043	2.318429
102.556933	1705.667903	5.322240	-0.020083	2.323359
102.888111	1713.731129	5.327245	-0.020150	2.328291
103.073833	1721.836126	5.332250	-0.020190	2.333225
103.309746	1729.890189	5.337254	-0.020239	2.338122
103.751327	1737.941147	5.342259	-0.020326	2.343024
103.846921	1746.047885	5.347264	-0.020349	2.347921
104.366840	1754.108478	5.352269	-0.020452	2.352815
104.696146	1762.182578	5.357274	-0.020518	2.357691
104.922781	1770.215263	5.362278	-0.020566	2.362524
105.391714	1778.277101	5.367283	-0.020658	2.367383
105.541539	1786.368667	5.372288	-0.020691	2.372225
105.622129	1794.462046	5.377293	-0.020712	2.377052
106.021923	1802.507557	5.382298	-0.020791	2.381867
106.271715	1810.565225	5.387302	-0.020843	2.386667
106.798887	1818.636493	5.392307	-0.020947	2.391488
107.124176	1826.694252	5.397312	-0.021013	2.396274
107.369520	1834.748275	5.402317	-0.021064	2.401043
107.650572	1842.817707	5.407322	-0.021121	2.405814
107.747907	1850.892937	5.412326	-0.021145	2.410564
107.809913	1859.001925	5.417331	-0.021161	2.415322
107.992674	1867.052981	5.422336	-0.021201	2.420046
108.204789	1875.098618	5.427341	-0.021245	2.424760
108.584840	1883.163596	5.432346	-0.021322	2.429490
108.876108	1891.291195	5.437350	-0.021381	2.434239
109.239524	1899.310952	5.442355	-0.021454	2.438922
109.450963	1907.353428	5.447360	-0.021499	2.443597
109.797740	1915.364481	5.452365	-0.021569	2.448256
110.155424	1923.455653	5.457370	-0.021640	2.452953
110.220168	1931.516061	5.462374	-0.021658	2.457601
110.701071	1939.552543	5.467379	-0.021753	2.462257
111.115200	1947.596672	5.472384	-0.021835	2.466904
111.362527	1955.672003	5.477389	-0.021886	2.471548
111.779487	1963.743872	5.482394	-0.021969	2.476194
112.522451	1971.731816	5.487398	-0.022113	2.480807
112.888185	1979.790961	5.492403	-0.022186	2.485424
112.883575	1987.890820	5.497408	-0.022191	2.490028
113.022730	1995.980730	5.502413	-0.022222	2.494628
113.325373	2004.035844	5.507418	-0.022283	2.499213
113.552297	2012.077861	5.512422	-0.022331	2.503776
113.717028	2020.171512	5.517427	-0.022367	2.508355
114.100633	2028.263271	5.522432	-0.022444	2.512940
114.604018	2036.257405	5.527437	-0.022543	2.517471
114.843040	2044.310206	5.532442	-0.022592	2.522008
115.065189	2052.344686	5.537446	-0.022639	2.526525
115.471206	2060.406773	5.542451	-0.022720	2.531062
115.276270	2068.537112	5.547456	-0.022689	2.535587
115.599117	2076.566200	5.552461	-0.022754	2.540083
116.045378	2084.578841	5.557466	-0.022843	2.544572
116.124371	2092.660487	5.562470	-0.022863	2.549065
116.315411	2100.758293	5.567475	-0.022904	2.553566
116.640673	2108.774999	5.572480	-0.022969	2.558024
116.724956	2116.823665	5.577485	-0.022990	2.562476
117.035635	2124.886402	5.582490	-0.023054	2.566943
117.290564	2132.937771	5.587494	-0.023106	2.571392
117.698070	2140.997395	5.592499	-0.023187	2.575848
117.914450	2149.044567	5.597504	-0.023233	2.580276
118.121680	2157.082600	5.602509	-0.023277	2.584692
118.656836	2165.142561	5.607514	-0.023382	2.589134
118.916260	2173.373195	5.612518	-0.023436	2.593643
119.178968	2181.413971	5.617523	-0.023490	2.598040
119.410475	2189.394570	5.622528	-0.023538	2.602396
119.933730	2197.374208	5.627533	-0.023641	2.606763
120.186989	2205.434866	5.632538	-0.023693	2.611148
120.294328	2213.490686	5.637542	-0.023718	2.615514
120.803763	2221.489061	5.642547	-0.023819	2.619868
120.791061	2229.544842	5.647552	-0.023821	2.624211
121.030798	2237.587988	5.652557	-0.023871	2.628557
121.297382	2245.670352	5.657562	-0.023926	2.632918
121.625486	2253.679795	5.662566	-0.023993	2.637238
121.776888	2261.736270	5.667571	-0.024026	2.641563
121.986301	2269.779058	5.672576	-0.024070	2.645878
122.107313	2277.831904	5.677581	-0.024098	2.650185
122.322982	2285.928839	5.682586	-0.024144	2.654516
122.463155	2293.952364	5.687590	-0.024175	2.658795
122.900363	2301.980291	5.692595	-0.024262	2.663088
123.009364	2310.029038	5.697600	-0.024287	2.667365
123.254055	2318.101405	5.702605	-0.024338	2.671656
123.845928	2326.150640	5.707610	-0.024454	2.675950
124.036020	2334.171327	5.712614	-0.024494	2.680196
124.179152	2342.206389	5.717619	-0.024526	2.684440
124.515225	2350.244591	5.722624	-0.024594	2.688691
124.873341	2358.301980	5.727629	-0.024666	2.692947
125.165773	2366.364760	5.732634	-0.024726	2.697195
125.041289	2374.422573	5.737638	-0.024708	2.701407
125.608377	2382.423581	5.742643	-0.024819	2.705626
125.740495	2390.510517	5.747648	-0.024849	2.709857
125.778052	2398.593325	5.752653	-0.024861	2.714072
126.177578	2406.608847	5.757658	-0.024941	2.718269
126.360695	2414.627343	5.762662	-0.024980	2.722447
126.799342	2422.670585	5.767667	-0.025067	2.726648
126.904689	2430.734165	5.772672	-0.025092	2.730831
127.179404	2438.794902	5.777677	-0.025148	2.735018
127.373073	2446.841464	5.782682	-0.025190	2.739185
127.658488	2454.839253	5.787686	-0.025248	2.743327
128.021205	2462.880821	5.792691	-0.025321	2.747489
128.368768	2470.985814	5.797696	-0.025391	2.751677
128.300622	2479.096318	5.802701	-0.025383	2.755836
128.527173	2487.111859	5.807706	-0.025431	2.759958
129.005576	2495.065392	5.812710	-0.025525	2.764058
129.283607	2503.133360	5.817715	-0.025582	2.768197
129.400453	2511.208545	5.822720	-0.025609	2.772324
129.643897	2519.240579	5.827725	-0.025660	2.776431
130.113400	2527.277948	5.832730	-0.025753	2.780548
129.946810	2535.311125	5.837734	-0.025727	2.784618
130.386243	2543.358234	5.842739	-0.025814	2.788726
130.745385	2551.407038	5.847744	-0.025886	2.792824
130.657431	2559.469609	5.852749	-0.025875	2.796896
130.997172	2567.511147	5.857754	-0.025943	2.800977
131.019022	2575.530669	5.862758	-0.025953	2.805022
131.355625	2583.570815	5.867763	-0.026021	2.809090
131.541319	2591.635199	5.872768	-0.026061	2.813155
131.844832	2599.660494	5.877773	-0.026122	2.817202
132.035264	2607.714830	5.882778	-0.026163	2.821251
132.143833	2615.748406	5.887782	-0.026189	2.825279
132.336720	2623.801381	5.892787	-0.026230	2.829316
132.768827	2631.860593	5.897792	-0.026316	2.833364
132.689629	2639.898913	5.902797	-0.026306	2.837366
132.978859	2647.911064	5.907802	-0.026365	2.841371
133.450470	2655.896391	5.912806	-0.026458	2.845366
133.591353	2663.960256	5.917811	-0.026490	2.849377
133.683431	2672.042347	5.922816	-0.026512	2.853388
133.853041	2680.065260	5.927821	-0.026549	2.857369
134.170367	2688.107465	5.932826	-0.026613	2.861361
134.396150	2696.136571	5.937830	-0.026661	2.865337
134.915832	2704.156631	5.942835	-0.026763	2.869319
135.212873	2712.238472	5.947840	-0.026823	2.873313
135.290579	2720.280001	5.952845	-0.026843	2.877270
135.507238	2728.326037	5.957850	-0.026889	2.881231
135.944578	2736.297474	5.962854	-0.026975	2.885162
136.070975	2744.383573	5.967859	-0.027004	2.889127
136.400151	2752.438510	5.972864	-0.027071	2.893082
136.607432	2760.469538	5.977869	-0.027115	2.897014
136.895364	2768.537913	5.982874	-0.027174	2.900963
136.934003	2776.535905	5.987878	-0.027186	2.904858
137.355412	2784.605241	5.992883	-0.027270	2.908804
137.698772	2792.683428	5.997888	-0.027339	2.912744
137.664496	2800.769165	6.002893	-0.027338	2.916663
137.816288	2808.762752	6.007898	-0.027371	2.920541
138.072211	2816.751122	6.012902	-0.027424	2.924417
138.352889	2824.770170	6.017907	-0.027482	2.928305
138.373087	2832.860861	6.022912	-0.027491	2.932207
138.568350	2840.882295	6.027917	-0.027532	2.936081
139.299471	2848.863284	6.032922	-0.027674	2.939958
139.273751	2856.899670	6.037926	-0.027674	2.943817
139.262554	2864.978233	6.042931	-0.027678	2.947691
139.545450	2873.025825	6.047936	-0.027735	2.951561
139.902236	2881.063097	6.052941	-0.027807	2.955425
140.234381	2889.070588	6.057946	-0.027874	2.959268
140.359506	2897.086074	6.062950	-0.027903	2.963100
141.002472	2905.103577	6.067955	-0.028028	2.966953
141.302062	2913.160796	6.072960	-0.028089	2.970803
141.277116	2921.234451	6.077965	-0.028090	2.974640
141.600563	2929.294463	6.082970	-0.028155	2.978482
141.802359	2937.283148	6.087974	-0.028198	2.982280
142.119302	2945.345087	6.092979	-0.028262	2.986113
142.219497	2953.375847	6.097984	-0.028286	2.989916
142.640879	2961.445668	6.102989	-0.028370	2.993748
142.732735	2969.508617	6.107994	-0.028392	2.997556
142.774249	2977.508940	6.112998	-0.028405	3.001326
143.089471	2985.523684	6.118003	-0.028469	3.005113
143.181762	2993.570849	6.123008	-0.028492	3.008898
143.295321	3001.615983	6.128013	-0.028518	3.012679
143.726039	3009.660688	6.133018	-0.028603	3.016471
143.912321	3017.657916	6.138022	-0.028643	3.020224
144.095012	3025.682275	6.143027	-0.028683	3.023984
144.510841	3033.710472	6.148032	-0.028765	3.027753
144.817458	3041.754906	6.153037	-0.028828	3.031520
144.981438	3049.829028	6.158042	-0.028864	3.035288
145.149339	3057.816168	6.163046	-0.028900	3.039012
145.490988	3065.859087	6.168051	-0.028969	3.042765
145.726241	3073.903591	6.173056	-0.029018	3.046509
145.766536	3081.933740	6.178061	-0.029031	3.050233
145.968243	3090.015154	6.183066	-0.029074	3.053983
146.276961	3098.020616	6.188070	-0.029136	3.057699
146.489875	3106.062720	6.193075	-0.029181	3.061423
146.572328	3114.091509	6.198080	-0.029202	3.065129
146.757146	3122.129102	6.203085	-0.029242	3.068841
147.059603	3130.224285	6.208090	-0.029303	3.072579
147.161173	3138.285351	6.213094	-0.029327	3.076288
147.546129	3146.260718	6.218099	-0.029404	3.079966
147.653433	3154.281466	6.223104	-0.029430	3.083648
147.651511	3162.288799	6.228109	-0.029435	3.087314
148.105792	3170.326529	6.233114	-0.029524	3.091011
148.225623	3178.364744	6.238118	-0.029552	3.094688
148.406922	3186.405035	6.243123	-0.029591	3.098365
148.668629	3194.417424	6.248128	-0.029645	3.102028
148.974664	3202.444590	6.253133	-0.029707	3.105695
149.189834	3210.485686	6.258138	-0.029753	3.109360
149.173902	3218.551198	6.263142	-0.029755	3.113022
149.562165	3226.592137	6.268147	-0.029832	3.116686
149.707671	3234.611712	6.273152	-0.029865	3.120326
149.987780	3242.598376	6.278157	-0.029922	3.123952
150.503772	3250.602210	6.283162	-0.030024	3.127592
150.623244	3258.664521	6.288166	-0.030051	3.131237
150.784703	3266.737000	6.293171	-0.030086	3.134883
150.922945	3274.754663	6.298176	-0.030117	3.138500
151.071924	3282.773652	6.303181	-0.030150	3.142114
151.194591	3290.821221	6.308186	-0.030179	3.145735
151.263532	3298.852067	6.313190	-0.030197	3.149342
151.661189	3306.918592	6.318195	-0.030276	3.152976
151.912445	3314.978900	6.323200	-0.030328	3.156596
151.891117	3322.954278	6.328205	-0.030329	3.160162
152.139588	3330.979593	6.333210	-0.030381	3.163758
152.292423	3338.989835	6.338214	-0.030415	3.167339
152.561817	3347.047714	6.343219	-0.030470	3.170942
152.716332	3355.086695	6.348224	-0.030504	3.174527
152.866130	3363.103692	6.353229	-0.030537	3.178099
153.144318	3371.145579	6.358234	-0.030594	3.181683
153.369723	3379.151756	6.363238	-0.030641	3.185245
153.575330	3387.204151	6.368243	-0.030685	3.188822
153.793752	3395.274352	6.373248	-0.030731	3.192404
154.087381	3403.290756	6.378253	-0.030791	3.195961
154.276313	3411.294380	6.383258	-0.030831	3.199505
154.287154	3419.341587	6.388262	-0.030839	3.203055
154.575964	3427.376359	6.393267	-0.030898	3.206609
154.843282	3435.387456	6.398272	-0.030953	3.210146
155.066132	3443.423802	6.403277	-0.030999	3.213690
155.243765	3451.493304	6.408282	-0.031038	3.217242
155.203614	3459.509701	6.413286	-0.031036	3.220757
155.392722	3467.500516	6.418291	-0.031076	3.224267
155.887528	3475.554295	6.423296	-0.031173	3.227814
155.875682	3483.605212	6.428301	-0.031177	3.231334
156.238110	3491.695817	6.433306	-0.031249	3.234883
156.431973	3499.652966	6.438310	-0.031291	3.238363
156.963963	3507.636844	6.443315	-0.031395	3.241865
157.089100	3515.660125	6.448320	-0.031423	3.245363
157.091376	3523.680505	6.453325	-0.031429	3.248852
157.414431	3531.740323	6.458330	-0.031495	3.252367
157.257236	3539.813635	6.463334	-0.031471	3.255864
157.575977	3547.799977	6.468339	-0.031535	3.259339
158.004588	3555.813787	6.473344	-0.031620	3.262827
158.193203	3563.848224	6.478349	-0.031661	3.266310
158.403886	3571.910286	6.483354	-0.031705	3.269802
158.639893	3579.937525	6.488358	-0.031754	3.273277
158.921475	3587.978691	6.493363	-0.031812	3.276755
159.147257	3595.989371	6.498368	-0.031859	3.280215
159.319190	3603.999703	6.503373	-0.031897	3.283668
159.698192	3612.033293	6.508378	-0.031973	3.287136
159.708548	3620.054205	6.513382	-0.031980	3.290581
160.086471	3628.111667	6.518387	-0.032055	3.294052
160.498040	3636.136893	6.523392	-0.032137	3.297506
160.576127	3644.181609	6.528397	-0.032157	3.300952
160.774647	3652.200647	6.533402	-0.032199	3.304389
160.942951	3660.214739	6.538406	-0.032236	3.307818
161.196976	3668.266218	6.543411	-0.032288	3.311263
161.528574	3676.317865	6.548416	-0.032355	3.314708
161.480274	3684.300909	6.553421	-0.032352	3.318105
161.917972	3692.342455	6.558426	-0.032438	3.321542
161.906782	3700.329193	6.563430	-0.032442	3.324936
162.009345	3708.383260	6.568435	-0.032466	3.328358
162.179922	3716.440442	6.573440	-0.032503	3.331781
162.258795	3724.477896	6.578445	-0.032523	3.335189
162.709813	3732.485942	6.583450	-0.032612	3.338594
162.980243	3740.498914	6.588454	-0.032668	3.341992
163.212968	3748.505704	6.593459	-0.032716	3.345382
163.352452	3756.553997	6.598464	-0.032748	3.348782
163.501477	3764.597119	6.603469	-0.032781	3.352177
163.889979	3772.663401	6.608474	-0.032858	3.355587
163.823038	3780.650334	6.613478	-0.032851	3.358944
163.897011	3788.695562	6.618483	-0.032870	3.362327
164.207904	3796.712238	6.623488	-0.032933	3.365703
164.384961	3804.706858	6.628493	-0.032972	3.369062
164.665165	3812.801404	6.633498	-0.033029	3.372463
164.768937	3820.817034	6.638502	-0.033054	3.375821
164.961777	3828.842096	6.643507	-0.033095	3.379183
165.270954	3836.847430	6.648512	-0.033158	3.382537
165.309509	3844.880770	6.653517	-0.033170	3.385890
165.666232	3852.924463	6.658522	-0.033242	3.389255
165.840976	3860.999908	6.663526	-0.033280	3.392624
165.994300	3869.064994	6.668531	-0.033313	3.395984
166.276200	3877.015372	6.673536	-0.033371	3.399298
166.377956	3885.012040	6.678541	-0.033395	3.402621
166.362265	3893.061026	6.683546	-0.033398	3.405959
166.636786	3901.053789	6.688550	-0.033454	3.409280
166.764109	3909.088593	6.693555	-0.033483	3.412610
166.835079	3917.168462	6.698560	-0.033501	3.415954
167.035176	3925.126152	6.703565	-0.033544	3.419248
167.391219	3933.165787	6.708570	-0.033616	3.422578
167.392199	3941.208554	6.713574	-0.033621	3.425895
167.561892	3949.226315	6.718579	-0.033658	3.429203
167.743911	3957.300232	6.723584	-0.033697	3.432532
168.016433	3965.317703	6.728589	-0.033753	3.435837
168.287736	3973.302061	6.733594	-0.033809	3.439125
168.278509	3981.323095	6.738598	-0.033812	3.442416
168.378046	3989.336126	6.743603	-0.033836	3.445704
168.655676	3997.395079	6.748608	-0.033893	3.449014
168.818747	4005.414665	6.753613	-0.033929	3.452301
169.024320	4013.480581	6.758618	-0.033972	3.455604
169.216674	4021.457475	6.763622	-0.034013	3.458868
169.308368	4029.522035	6.768627	-0.034036	3.462161
169.584318	4037.510621	6.773632	-0.034092	3.465426
169.820717	4045.526906	6.778637	-0.034142	3.468698
170.129557	4053.587342	6.783642	-0.034204	3.471987
170.228084	4061.656894	6.788646	-0.034228	3.475270
170.139722	4069.648920	6.793651	-0.034217	3.478512
170.403599	4077.681378	6.798656	-0.034271	3.481779
170.620311	4085.637365	6.803661	-0.034317	3.485010
170.860930	4093.709279	6.808666	-0.034367	3.488286
170.864651	4101.751102	6.813670	-0.034373	3.491539
171.051465	4109.757521	6.818675	-0.034413	3.494781
171.306008	4117.773145	6.823680	-0.034465	3.498025
171.401381	4125.797106	6.828685	-0.034489	3.501265
171.538808	4133.785759	6.833690	-0.034519	3.504489
171.942818	4141.818604	6.838694	-0.034600	3.507735
172.071888	4149.863236	6.843699	-0.034629	3.510975
172.367249	4157.927427	6.848704	-0.034689	3.514226
172.345144	4165.952828	6.853709	-0.034691	3.517447
172.444002	4173.961519	6.858714	-0.034714	3.520663
172.538892	4181.943596	6.863718	-0.034737	3.523865
172.855988	4189.995606	6.868723	-0.034801	3.527098
173.062672	4198.036228	6.873728	-0.034845	3.530321
173.201511	4206.062877	6.878733	-0.034876	3.533534
173.234959	4214.136945	6.883738	-0.034888	3.536759
173.317262	4222.126248	6.888742	-0.034908	3.539948
173.354348	4230.148930	6.893747	-0.034921	3.543147
173.854326	4238.158248	6.898752	-0.035019	3.546352
173.677022	4246.202217	6.903757	-0.034991	3.549547
174.256337	4254.306852	6.908762	-0.035104	3.552785
174.259563	4262.359043	6.913766	-0.035110	3.555983
174.251709	4270.287065	6.918771	-0.035114	3.559129
174.621803	4278.287065	6.923776	-0.035188	3.562311
174.722149	4286.274903	6.928781	-0.035212	3.565478
175.004947	4294.335374	6.933786	-0.035270	3.568675
175.124124	4302.407343	6.938790	-0.035298	3.571870
175.273338	4310.392672	6.943795	-0.035331	3.575029
175.530390	4318.421570	6.948800	-0.035384	3.578205
175.675071	4326.429484	6.953805	-0.035416	3.581366
175.967827	4334.425847	6.958810	-0.035476	3.584525
176.380785	4342.439726	6.963814	-0.035558	3.587691
176.530462	4350.495020	6.968819	-0.035591	3.590863
176.515789	4358.548703	6.973824	-0.035593	3.594027
176.722464	4366.539448	6.978829	-0.035637	3.597169
177.034466	4374.553611	6.983834	-0.035701	3.600321
176.979962	4382.576472	6.988838	-0.035696	3.603464
177.069972	4390.616744	6.993843	-0.035718	3.606614
177.529580	4398.625804	6.998848	-0.035808	3.609760
177.544108	4406.660079	7.003853	-0.035816	3.612900
177.712853	4414.735231	7.008858	-0.035853	3.616058
177.862269	4422.700407	7.013862	-0.035886	3.619170
177.800136	4430.732279	7.018867	-0.035880	3.622299
178.045076	4438.755928	7.023872	-0.035931	3.625431
178.471938	4446.757037	7.028877	-0.036016	3.628556
178.649270	4454.834082	7.033882	-0.036054	3.631701
178.770453	4462.871471	7.038886	-0.036082	3.634826
178.861772	4470.878481	7.043891	-0.036104	3.637936
179.337870	4478.906824	7.048896	-0.036198	3.641062
179.136222	4486.892351	7.053901	-0.036166	3.644151
179.539739	4494.938910	7.058906	-0.036246	3.647277
179.765536	4502.949045	7.063910	-0.036293	3.650381
179.719029	4511.011421	7.068915	-0.036290	3.653496
179.979856	4519.039459	7.073920	-0.036344	3.656602
180.197918	4527.010163	7.078925	-0.036390	3.659683
180.689409	4535.049344	7.083930	-0.036486	3.662795
180.734523	4543.083633	7.088934	-0.036500	3.665890
180.874830	4551.091529	7.093939	-0.036531	3.668975
181.145601	4559.152696	7.098944	-0.036587	3.672082
181.287140	4567.141681	7.103949	-0.036619	3.675154
181.539397	4575.170699	7.108954	-0.036671	3.678243
181.675219	4583.213538	7.113958	-0.036701	3.681331
181.775230	4591.166139	7.118963	-0.036725	3.684381
182.039428	4599.237673	7.123968	-0.036780	3.687478
182.127351	4607.242046	7.128973	-0.036801	3.690542
182.431483	4615.292793	7.133978	-0.036863	3.693627
182.418335	4623.326290	7.138982	-0.036866	3.696694
182.468499	4631.309928	7.143987	-0.036881	3.699742
183.045118	4639.350150	7.148992	-0.036993	3.702822
183.159273	4647.352032	7.153997	-0.037020	3.705873
183.380020	4655.397953	7.159002	-0.037066	3.708941
183.261343	4663.469339	7.164006	-0.037049	3.712008
183.572840	4671.549168	7.169011	-0.037113	3.715086
183.687406	4679.508677	7.174016	-0.037139	3.718111
183.646951	4687.525839	7.179021	-0.037137	3.721151
184.063346	4695.463462	7.184026	-0.037220	3.724170
184.298482	4703.507514	7.189030	-0.037269	3.727223
184.365277	4711.545044	7.194035	-0.037286	3.730266
184.541938	4719.600379	7.199040	-0.037325	3.733316
184.672364	4727.613231	7.204045	-0.037354	3.736347
185.049088	4735.586521	7.209050	-0.037430	3.739366
185.084856	4743.644979	7.214054	-0.037442	3.742406
185.182831	4751.636508	7.219059	-0.037465	3.745420
185.097795	4759.692395	7.224064	-0.037454	3.748452
185.384112	4767.758222	7.229069	-0.037513	3.751494
185.837361	4775.746440	7.234074	-0.037603	3.754508
185.908536	4783.756599	7.239078	-0.037621	3.757519
185.795820	4791.790384	7.244083	-0.037605	3.760532
186.316187	4799.816642	7.249088	-0.037708	3.763554
186.573397	4807.826541	7.254093	-0.037761	3.766562
186.829191	4815.840546	7.259098	-0.037814	3.769569
186.846398	4823.861402	7.264102	-0.037822	3.772570
187.157086	4831.891738	7.269107	-0.037885	3.775580
187.410434	4839.957174	7.274112	-0.037938	3.778598
187.439208	4847.910512	7.279117	-0.037948	3.781568
187.878369	4855.964370	7.284122	-0.038035	3.784581
187.973211	4863.990159	7.289126	-0.038058	3.787574
188.131572	4872.026940	7.294131	-0.038093	3.790571
188.355443	4880.097316	7.299136	-0.038140	3.793578
188.342192	4888.115179	7.304141	-0.038143	3.796559
188.757886	4896.084560	7.309146	-0.038225	3.799528
188.716464	4904.071312	7.314150	-0.038223	3.802492
189.136498	4912.084338	7.319155	-0.038306	3.805473
189.339035	4920.130895	7.324160	-0.038349	3.808460
189.522966	4928.130129	7.329165	-0.038389	3.811426
189.802012	4936.195988	7.334170	-0.038446	3.814417
190.006040	4944.216901	7.339174	-0.038489	3.817387
190.087293	4952.184462	7.344179	-0.038510	3.820332
190.394124	4960.216296	7.349184	-0.038572	3.823303
190.383991	4968.219360	7.354189	-0.038575	3.826255
190.706330	4976.273998	7.359194	-0.038641	3.829231
190.799838	4984.314166	7.364198	-0.038663	3.832194
190.949625	4992.326857	7.369203	-0.038697	3.835146
191.066280	5000.351914	7.374208	-0.038724	3.838099
191.067923	5008.354846	7.379213	-0.038729	3.841040
191.378772	5016.346542	7.384218	-0.038792	3.843980
191.519863	5024.381248	7.389222	-0.038824	3.846931
191.535954	5032.429167	7.394227	-0.038832	3.849882
191.838694	5040.480974	7.399232	-0.038894	3.852837
191.694982	5048.508383	7.404237	-0.038872	3.855773
192.208801	5056.489315	7.409242	-0.038973	3.858702
192.254809	5064.492885	7.414246	-0.038987	3.861628
192.487319	5072.516271	7.419251	-0.039036	3.864563
192.575779	5080.569141	7.424256	-0.039057	3.867503
192.616430	5088.583678	7.429261	-0.039070	3.870426
192.946004	5096.846643	7.434266	-0.039137	3.873443
193.261531	5104.830431	7.439270	-0.039201	3.876356
193.357970	5112.725711	7.444275	-0.039224	3.879230
193.716091	5120.752033	7.449280	-0.039296	3.882155
194.091612	5128.679602	7.454285	-0.039371	3.885042
194.411197	5136.720330	7.459290	-0.039436	3.887966
194.545991	5144.723678	7.464294	-0.039466	3.890872
194.933904	5152.786042	7.469299	-0.039544	3.893801
195.296628	5160.825795	7.474304	-0.039617	3.896720
195.326068	5168.764951	7.479309	-0.039627	3.899593
195.725401	5176.824513	7.484314	-0.039707	3.902515
195.853870	5184.793768	7.489318	-0.039736	3.905397
196.217648	5192.812981	7.494323	-0.039809	3.908299
196.231863	5200.940366	7.499328	-0.039817	3.911232
196.488726	5208.918422	7.504333	-0.039870	3.914113
196.769052	5216.936813	7.509338	-0.039927	3.917006
196.953185	5224.882022	7.514342	-0.039967	3.919870
197.067844	5232.923488	7.519347	-0.039994	3.922765
197.327117	5240.968826	7.524352	-0.040047	3.925661
197.270230	5248.998816	7.529357	-0.040042	3.928544
197.590046	5257.014849	7.534362	-0.040107	3.931427
197.772478	5265.056863	7.539366	-0.040146	3.934315
197.577807	5273.077525	7.544371	-0.040115	3.937186
197.943327	5281.070852	7.549376	-0.040188	3.940055
197.982151	5289.064547	7.554381	-0.040201	3.942916
198.240405	5297.105638	7.559386	-0.040254	3.945796
198.402536	5305.109378	7.564390	-0.040289	3.948659
198.477462	5313.170507	7.569395	-0.040309	3.951539
198.829010	5321.225808	7.574400	-0.040379	3.954419
198.834672	5329.214604	7.579405	-0.040386	3.957268
199.083413	5337.214931	7.584410	-0.040437	3.960122
199.303284	5345.174289	7.589414	-0.040483	3.962960
199.548458	5353.187395	7.594419	-0.040534	3.965815
199.617279	5361.244689	7.599424	-0.040552	3.968681
199.791335	5369.262392	7.604429	-0.040590	3.971532
200.163119	5377.314388	7.609434	-0.040665	3.974397
200.156607	5385.338287	7.614438	-0.040669	3.977243
200.066336	5393.348091	7.619443	-0.040657	3.980081
200.428450	5401.363545	7.624448	-0.040730	3.982926
200.312008	5409.369282	7.629453	-0.040713	3.985758
200.659155	5417.409457	7.634458	-0.040783	3.988608
201.125789	5425.454427	7.639462	-0.040875	3.991460
200.988289	5433.481020	7.644467	-0.040855	3.994292
201.247039	5441.541092	7.649472	-0.040909	3.997142
201.369420	5449.476017	7.654477	-0.040937	3.999942
201.703591	5457.503510	7.659482	-0.041004	4.002777
201.829051	5465.509053	7.664486	-0.041033	4.005599
202.039332	5473.532448	7.669491	-0.041077	4.008426
202.089830	5481.641592	7.674496	-0.041092	4.011279
202.448730	5489.636118	7.679501	-0.041164	4.014094
202.782555	5497.646423	7.684506	-0.041231	4.016913
202.810206	5505.628908	7.689510	-0.041242	4.019715
202.787289	5513.665518	7.694515	-0.041243	4.022533
203.009474	5521.693431	7.699520	-0.041289	4.025350
203.056508	5529.695491	7.704525	-0.041303	4.028153
203.460795	5537.739355	7.709530	-0.041384	4.030975
203.386724	5545.866025	7.714534	-0.041375	4.033816
203.628612	5553.840893	7.719539	-0.041426	4.036607
203.938373	5561.769289	7.724544	-0.041489	4.039380
204.104036	5569.804289	7.729549	-0.041525	4.042187
204.091665	5577.769248	7.734554	-0.041528	4.044964
204.366941	5585.845781	7.739558	-0.041584	4.047783
204.503223	5593.820941	7.744563	-0.041615	4.050563
204.544490	5601.895368	7.749568	-0.041628	4.053374
204.548607	5609.898852	7.754573	-0.041634	4.056157
205.015225	5617.888606	7.759578	-0.041726	4.058941
205.238806	5625.948062	7.764582	-0.041773	4.061743
205.576043	5633.900518	7.769587	-0.041841	4.064508
205.768162	5641.951835	7.774592	-0.041882	4.067303
205.805874	5649.975432	7.779597	-0.041894	4.070084
205.848998	5658.016944	7.784602	-0.041907	4.072870
205.897599	5666.016845	7.789606	-0.041922	4.075640
206.240649	5673.981474	7.794611	-0.041991	4.078399
206.311047	5682.067378	7.799616	-0.042009	4.081195
206.491724	5690.019744	7.804621	-0.042048	4.083944
206.682421	5698.099303	7.809626	-0.042089	4.086736
207.004611	5706.084216	7.814630	-0.042154	4.089494
206.868567	5714.125268	7.819635	-0.042134	4.092264
207.202791	5722.148815	7.824640	-0.042202	4.095032
207.067697	5730.135393	7.829645	-0.042182	4.097780
207.246596	5738.191400	7.834650	-0.042220	4.100553
207.396319	5746.195922	7.839654	-0.042253	4.103307
207.686167	5754.195980	7.844659	-0.042313	4.106059
207.962803	5762.258440	7.849664	-0.042369	4.108830
207.943446	5770.303089	7.854669	-0.042371	4.111590
208.433741	5778.332106	7.859674	-0.042468	4.114349
208.485464	5786.345797	7.864678	-0.042482	4.117095
208.482090	5794.307630	7.869683	-0.042487	4.119821
208.875772	5802.342157	7.874688	-0.042566	4.122575
208.969436	5810.322971	7.879693	-0.042588	4.125304
209.294271	5818.379233	7.884698	-0.042654	4.128061
209.379309	5826.399477	7.889702	-0.042675	4.130801
209.578535	5834.441075	7.894707	-0.042718	4.133547
209.498639	5842.488125	7.899712	-0.042708	4.136290
209.464676	5850.461855	7.904717	-0.042707	4.139007
209.882622	5858.540213	7.909722	-0.042790	4.141763
209.917418	5866.479913	7.914726	-0.042802	4.144465
209.977792	5874.547882	7.919731	-0.042818	4.147210
210.245854	5882.548680	7.924736	-0.042873	4.149932
210.392982	5890.598620	7.929741	-0.042906	4.152668
210.769948	5898.596256	7.934746	-0.042981	4.155387
210.833198	5906.613825	7.939750	-0.042998	4.158107
210.960058	5914.616063	7.944755	-0.043027	4.160821
211.173653	5922.613244	7.949760	-0.043072	4.163533
211.243368	5930.647380	7.954765	-0.043091	4.166253
211.427843	5938.663537	7.959770	-0.043130	4.168967
211.559806	5946.742192	7.964774	-0.043160	4.171700
211.462708	5954.741424	7.969779	-0.043147	4.174401
211.853982	5962.812827	7.974784	-0.043225	4.177131
211.892976	5970.739337	7.979789	-0.043238	4.179806
211.997109	5978.775319	7.984794	-0.043262	4.182517
211.993788	5986.785781	7.989798	-0.043267	4.185216
212.266665	5994.784113	7.994803	-0.043323	4.187913
212.601358	6002.853468	7.999808	-0.043391	4.190632
212.696153	6010.945187	8.004813	-0.043414	4.193354
212.776088	6018.971135	8.009818	-0.043434	4.196053
212.927664	6026.925637	8.014822	-0.043467	4.198726
212.716894	6034.886448	8.019827	-0.043433	4.201396
213.193136	6042.866131	8.024832	-0.043527	4.204078
213.283865	6050.899428	8.029837	-0.043549	4.206772
213.359866	6058.874053	8.034842	-0.043569	4.209444
213.477990	6066.999872	8.039846	-0.043596	4.212166
213.708673	6074.987560	8.044851	-0.043644	4.214841
213.801205	6083.014499	8.049856	-0.043667	4.217526
213.779912	6090.994885	8.054861	-0.043668	4.220192
214.228004	6099.008357	8.059866	-0.043757	4.222873
214.256902	6107.012433	8.064870	-0.043767	4.225544
214.351040	6115.014986	8.069875	-0.043790	4.228214
214.496720	6123.082033	8.074880	-0.043823	4.230904
214.794551	6131.084219	8.079885	-0.043883	4.233573
214.866979	6139.151583	8.084890	-0.043902	4.236259
214.914775	6147.123425	8.089894	-0.043916	4.238911
215.006950	6155.110292	8.094899	-0.043939	4.241568
215.424952	6163.097669	8.099904	-0.044022	4.244225
215.353741	6171.163264	8.104909	-0.044014	4.246903
215.687294	6179.206607	8.109914	-0.044081	4.249575
215.926539	6187.218222	8.114918	-0.044131	4.252234
216.003916	6195.248845	8.119923	-0.044151	4.254896
215.987413	6203.320109	8.124928	-0.044153	4.257569
216.227956	6211.267743	8.129933	-0.044203	4.260202
216.314977	6219.252867	8.134938	-0.044224	4.262844
216.594022	6227.315305	8.139942	-0.044281	4.265512
216.724231	6235.326373	8.144947	-0.044311	4.268160
217.015007	6243.420528	8.149952	-0.044370	4.270834
217.019483	6251.441259	8.154957	-0.044376	4.273481
217.164326	6259.448166	8.159962	-0.044409	4.276123
217.472239	6267.414181	8.164966	-0.044471	4.278750
217.666763	6275.395717	8.169971	-0.044513	4.281381
217.952477	6283.409342	8.174976	-0.044571	4.284021
218.168482	6291.444035	8.179981	-0.044617	4.286665
218.584553	6299.481623	8.184986	-0.044699	4.289311
218.714608	6307.514347	8.189990	-0.044729	4.291951
218.897288	6315.556488	8.194995	-0.044768	4.294593
219.076314	6323.579956	8.200000	-0.044807	4.297227
219.181559	6331.530217	8.205005	-0.044832	4.299834
219.383067	6339.605017	8.210010	-0.044874	4.302482
219.548478	6347.551290	8.215014	-0.044910	4.305086
219.660818	6355.615340	8.220019	-0.044937	4.307726
219.839980	6363.652268	8.225024	-0.044975	4.310357
219.869051	6371.651828	8.230029	-0.044986	4.312972
220.106384	6379.678216	8.235034	-0.045035	4.315596
220.157356	6387.670819	8.240038	-0.045050	4.318206
220.377252	6395.686462	8.245043	-0.045096	4.320823
220.635925	6403.693739	8.250048	-0.045150	4.323436
220.744359	6411.683453	8.255053	-0.045175	4.326041
220.916998	6419.742771	8.260058	-0.045213	4.328667
220.931386	6427.768318	8.265062	-0.045220	4.331280
221.132292	6435.783149	8.270067	-0.045263	4.333888
221.309726	6443.857196	8.275072	-0.045301	4.336515
221.326917	6451.800270	8.280077	-0.045310	4.339096
221.762495	6459.803673	8.285082	-0.045396	4.341697
221.760498	6467.817381	8.290086	-0.045401	4.344298
221.819377	6475.841374	8.295091	-0.045417	4.346901
222.207884	6483.879806	8.300096	-0.045495	4.349509
222.254085	6491.895496	8.305101	-0.045509	4.352106
222.462102	6500.034278	8.310106	-0.045553	4.354742
222.713411	6508.012166	8.315110	-0.045605	4.357325
222.776405	6515.923289	8.320115	-0.045622	4.359883
222.763399	6523.983603	8.325120	-0.045625	4.362488
222.913004	6531.924714	8.330125	-0.045658	4.365054
222.982578	6539.946600	8.335130	-0.045676	4.367643
223.251725	6548.000467	8.340134	-0.045731	4.370243
223.593036	6556.020110	8.345139	-0.045800	4.372831
223.697278	6564.084924	8.350144	-0.045825	4.375430
223.810159	6572.046772	8.355149	-0.045851	4.377994
223.802411	6580.079587	8.360154	-0.045855	4.380579
224.065017	6588.055957	8.365158	-0.045909	4.383146
224.350449	6596.037679	8.370163	-0.045967	4.385713
224.393245	6604.135418	8.375168	-0.045981	4.388315
224.182675	6612.114012	8.380173	-0.045947	4.390875
224.586603	6620.178066	8.385178	-0.046027	4.393465
224.803588	6628.217128	8.390182	-0.046073	4.396044
224.726212	6636.180221	8.395187	-0.046064	4.398596
224.932432	6644.270911	8.400192	-0.046107	4.401188
225.074978	6652.192880	8.405197	-0.046139	4.403725
225.273454	6660.213257	8.410202	-0.046181	4.406292
225.348687	6668.250149	8.415206	-0.046201	4.408862
225.549841	6676.283902	8.420211	-0.046243	4.411430
225.794487	6684.331520	8.425216	-0.046294	4.414001
225.595824	6692.343846	8.430221	-0.046262	4.416557
225.946974	6700.307287	8.435226	-0.046333	4.419099
225.995392	6708.363303	8.440230	-0.046347	4.421668
226.153073	6716.309681	8.445235	-0.046382	4.424200
226.346233	6724.426883	8.450240	-0.046423	4.426786
226.368476	6732.423831	8.455245	-0.046433	4.429331
226.479839	6740.489902	8.460250	-0.046459	4.431897
226.554890	6748.518969	8.465254	-0.046478	4.434450
226.933173	6756.484572	8.470259	-0.046554	4.436982
227.123868	6764.475169	8.475264	-0.046594	4.439520
226.921900	6772.488542	8.480269	-0.046562	4.442062
227.178459	6780.455989	8.485274	-0.046615	4.444590
227.345669	6788.554389	8.490278	-0.046651	4.447157
227.347367	6796.530546	8.495283	-0.046657	4.449684
227.660964	6804.594061	8.500288	-0.046721	4.452238
227.692443	6812.549427	8.505293	-0.046732	4.454755
227.738878	6820.610844	8.510298	-0.046746	4.457305
227.766865	6828.568436	8.515302	-0.046756	4.459820
228.073302	6836.619140	8.520307	-0.046818	4.462364
228.474804	6844.642779	8.525312	-0.046898	4.464898
228.393364	6852.681704	8.530317	-0.046889	4.467434
228.420582	6860.679365	8.535322	-0.046899	4.469956
228.672211	6868.745433	8.540326	-0.046951	4.472499
228.584637	6876.725749	8.545331	-0.046940	4.475012
228.913078	6884.792325	8.550336	-0.047006	4.477553
229.108313	6892.728054	8.555341	-0.047048	4.480050
229.275850	6900.733142	8.560346	-0.047084	4.482567
229.427020	6908.721109	8.565351	-0.047118	4.485078
229.628395	6916.773768	8.570355	-0.047161	4.487608
229.634797	6924.798161	8.575360	-0.047167	4.490127
229.590704	6932.840500	8.580365	-0.047164	4.492650
230.049059	6940.810874	8.585370	-0.047255	4.495150
230.123040	6948.876145	8.590375	-0.047274	4.497678
230.190679	6956.852317	8.595379	-0.047291	4.500176
230.368859	6964.907797	8.600384	-0.047330	4.502698
230.708399	6972.849671	8.605389	-0.047398	4.505183
230.723063	6980.923687	8.610394	-0.047406	4.507708
230.740087	6988.952254	8.615399	-0.047415	4.510217
230.821217	6996.995785	8.620403	-0.047435	4.512729
231.185913	7005.048596	8.625408	-0.047508	4.515243
231.265993	7012.973104	8.630413	-0.047529	4.517716
231.442557	7020.966369	8.635418	-0.047567	4.520208
231.448462	7029.005462	8.640423	-0.047573	4.522713
231.552092	7036.983147	8.645427	-0.047598	4.525198
231.961387	7045.003272	8.650432	-0.047679	4.527695
231.873152	7053.022320	8.655437	-0.047668	4.530190
231.920038	7061.082037	8.660442	-0.047682	4.532696
232.086974	7069.079150	8.665447	-0.047718	4.535181
232.390622	7077.080884	8.670451	-0.047780	4.537667
232.638792	7085.087465	8.675456	-0.047831	4.540153
232.558070	7093.108493	8.680461	-0.047822	4.542641
232.621182	7101.112949	8.685466	-0.047839	4.545123
232.913974	7109.169952	8.690471	-0.047898	4.547620
232.933794	7117.148229	8.695475	-0.047907	4.550091
233.019756	7125.248563	8.700480	-0.047929	4.552599
233.183347	7133.205659	8.705485	-0.047964	4.555061
233.188036	7141.262799	8.710490	-0.047971	4.557552
233.219893	7149.230262	8.715495	-0.047982	4.560015
233.445894	7157.230551	8.720499	-0.048029	4.562486
233.936328	7165.242300	8.725504	-0.048126	4.564960
233.592991	7173.316451	8.730509	-0.048067	4.567451
233.877010	7181.268035	8.735514	-0.048125	4.569903
234.012033	7189.363338	8.740519	-0.048155	4.572398
234.281808	7197.357249	8.745523	-0.048211	4.574861
234.468564	7205.440027	8.750528	-0.048251	4.577349
234.667184	7213.366893	8.755533	-0.048293	4.579788
234.716608	7221.427433	8.760538	-0.048308	4.582267
234.700324	7229.406165	8.765543	-0.048310	4.584720
234.673715	7237.430873	8.770547	-0.048310	4.587185
235.048785	7245.438715	8.775552	-0.048385	4.589644
235.002245	7253.491492	8.780557	-0.048382	4.592115
235.218902	7261.519640	8.785562	-0.048428	4.594577
235.612978	7269.621199	8.790567	-0.048506	4.597061
235.691059	7277.488170	8.795571	-0.048526	4.599471
235.770792	7285.609171	8.800576	-0.048546	4.601958
235.880903	7293.479471	8.805581	-0.048572	4.604366
236.151613	7301.558017	8.810586	-0.048627	4.606837
236.257183	7309.572660	8.815591	-0.048652	4.609287
236.383208	7317.596720	8.820595	-0.048681	4.611739
236.733674	7325.680298	8.825600	-0.048752	4.614208
236.688406	7333.639407	8.830605	-0.048748	4.616637
236.703030	7341.597595	8.835610	-0.048756	4.619065
237.054245	7349.699431	8.840615	-0.048827	4.621535
237.154747	7357.620097	8.845619	-0.048851	4.623948
237.301506	7365.678280	8.850624	-0.048884	4.626402
237.303469	7373.683209	8.855629	-0.048889	4.628839
237.416933	7381.740743	8.860634	-0.048916	4.631291
237.646735	7389.755522	8.865639	-0.048964	4.633728
237.663682	7397.760917	8.870643	-0.048972	4.636161
237.978595	7405.733031	8.875648	-0.049036	4.638582
238.031160	7413.794290	8.880653	-0.049051	4.641029
238.058012	7421.739365	8.885658	-0.049061	4.643440
238.250172	7429.835199	8.890663	-0.049102	4.645895
238.176390	7437.789446	8.895667	-0.049094	4.648306
238.322450	7445.875199	8.900672	-0.049126	4.650756
238.272894	7453.891474	8.905677	-0.049122	4.653183
238.661105	7461.857590	8.910682	-0.049200	4.655594
238.872442	7469.893472	8.915687	-0.049244	4.658024
238.954154	7477.890828	8.920691	-0.049265	4.660442
239.297946	7485.950202	8.925696	-0.049334	4.662877
239.169886	7493.910732	8.930701	-0.049316	4.665281
239.412122	7501.905828	8.935706	-0.049366	4.667694
239.585873	7509.991815	8.940711	-0.049404	4.670133
239.543484	7518.026236	8.945715	-0.049401	4.672556
239.681897	7526.141315	8.950720	-0.049432	4.675001
239.752101	7534.065462	8.955725	-0.049450	4.677388
240.017912	7542.001953	8.960730	-0.049505	4.679777
240.084073	7550.041178	8.965735	-0.049523	4.682196
240.069380	7557.947088	8.970739	-0.049525	4.684574
240.426347	7566.089765	8.975744	-0.049597	4.687021
240.663261	7574.018896	8.980749	-0.049646	4.689403
240.774738	7582.082429	8.985754	-0.049672	4.691824
241.009188	7590.161356	8.990759	-0.049721	4.694248
241.267520	7598.168716	8.995763	-0.049775	4.696649
241.248680	7606.091980	9.000768	-0.049776	4.699025
241.368285	7614.146301	9.005773	-0.049804	4.701438
241.397313	7622.158298	9.010778	-0.049814	4.703838
241.576791	7630.217224	9.015783	-0.049853	4.706250
241.393263	7638.186853	9.020787	-0.049824	4.708635
241.693978	7646.225773	9.025792	-0.049885	4.711038
241.728505	7654.238626	9.030797	-0.049897	4.713433
242.028047	7662.253523	9.035802	-0.049958	4.715827
242.284102	7670.282717	9.040807	-0.050011	4.718223
242.407576	7678.234409	9.045811	-0.050039	4.720596
242.350540	7686.299577	9.050816	-0.050034	4.723002
242.420187	7694.308159	9.055821	-0.050052	4.725389
242.585587	7702.317496	9.060826	-0.050088	4.727775
242.761712	7710.361457	9.065831	-0.050126	4.730171
242.799378	7718.383092	9.070835	-0.050139	4.732558
242.994424	7726.417658	9.075840	-0.050180	4.734948
243.122741	7734.437861	9.080845	-0.050209	4.737333
243.251487	7742.418037	9.085850	-0.050239	4.739704
243.191185	7750.465519	9.090855	-0.050233	4.742095
243.397994	7758.417798	9.095859	-0.050276	4.744456
243.495388	7766.478196	9.100864	-0.050300	4.746847
243.637197	7774.461063	9.105869	-0.050331	4.749215
243.784713	7782.497545	9.110874	-0.050364	4.751597
244.130119	7790.589863	9.115879	-0.050434	4.753994
244.085940	7798.581818	9.120883	-0.050431	4.756361
244.260563	7806.523304	9.125888	-0.050468	4.758711
244.180854	7814.561852	9.130893	-0.050459	4.761090
244.480155	7822.503320	9.135898	-0.050520	4.763437
244.508767	7830.574440	9.140903	-0.050530	4.765823
244.418968	7838.561488	9.145907	-0.050519	4.768183
244.611895	7846.587730	9.150912	-0.050560	4.770552
244.635216	7854.628587	9.155917	-0.050570	4.772925
244.834820	7862.640801	9.160922	-0.050612	4.775288
244.937572	7870.674865	9.165927	-0.050637	4.777656
245.068678	7878.631744	9.170931	-0.050666	4.780000
245.149385	7886.684145	9.175936	-0.050687	4.782372
245.477103	7894.672891	9.180941	-0.050753	4.784722
245.666595	7902.685007	9.185946	-0.050793	4.787079
245.676958	7910.752783	9.190951	-0.050801	4.789452
245.854839	7918.751536	9.195955	-0.050839	4.791802
246.084431	7926.803931	9.200960	-0.050887	4.794167
246.100817	7934.812613	9.205965	-0.050895	4.796519
246.259325	7942.784793	9.210970	-0.050930	4.798859
246.618688	7950.804401	9.215975	-0.051002	4.801210
246.658979	7958.772106	9.220979	-0.051015	4.803546
246.721880	7966.814383	9.225984	-0.051032	4.805903
247.126824	7974.857457	9.230989	-0.051113	4.808257
247.127864	7982.826788	9.235994	-0.051118	4.810590
247.194904	7990.323021	9.240999	-0.051135	4.812784
247.307393	7994.758903	9.246003	-0.051159	4.814081

247.553273	7997.364127	9.251008	-0.051207	4.814842
247.537183	7998.648106	9.256013	-0.051205	4.815217
247.633776	7999.100196	9.261018	-0.051223	4.815349
247.646969	8000.094380	9.266023	-0.051226	4.815640
247.605052	8000.067011	9.271027	-0.051218	4.815632
247.651158	8000.070965	9.276032	-0.051227	4.815633
248.175247	8000.076278	9.281037	-0.051324	4.815632
247.975218	8000.028189	9.286042	-0.051287	4.815619
247.996623	8000.097938	9.291047	-0.051291	4.815639
247.859616	8000.067956	9.296051	-0.051266	4.815631
248.196948	8000.070235	9.301056	-0.051329	4.815630
248.168534	8000.024934	9.306061	-0.051323	4.815617
248.133231	7999.994469	9.311066	-0.051317	4.815608
248.333033	8000.075657	9.316071	-0.051354	4.815631
248.497316	8000.050569	9.321075	-0.051385	4.815623
248.398594	8000.085270	9.326080	-0.051366	4.815634
248.183105	8000.082839	9.331085	-0.051326	4.815634
248.414863	8000.016140	9.336090	-0.051369	4.815613
248.391431	8000.059537	9.341095	-0.051365	4.815626
248.311978	8000.037963	9.346099	-0.051350	4.815620
248.490419	8000.077166	9.351104	-0.051384	4.815631
248.586979	8000.081941	9.356109	-0.051402	4.815632
248.283192	8000.030031	9.361114	-0.051345	4.815618
248.517862	8000.089365	9.366119	-0.051389	4.815634
248.581613	8000.126705	9.371123	-0.051401	4.815645
248.480129	8000.119721	9.376128	-0.051382	4.815643
248.459346	8000.124724	9.381133	-0.051378	4.815645
248.569169	8000.030420	9.386138	-0.051398	4.815617
248.797971	8000.037343	9.391143	-0.051441	4.815618
248.709047	8000.027359	9.396147	-0.051425	4.815615
248.850033	8000.018976	9.401152	-0.051451	4.815612
248.667549	8000.025623	9.406157	-0.051417	4.815615
248.648435	7999.987946	9.411162	-0.051413	4.815604
248.762046	8000.076278	9.416167	-0.051435	4.815629
248.972521	7999.990014	9.421171	-0.051474	4.815603
248.899932	8000.035816	9.426176	-0.051460	4.815617
248.859184	8000.034089	9.431181	-0.051453	4.815616
249.099755	7999.986751	9.436186	-0.051498	4.815601
249.087356	8000.066630	9.441191	-0.051495	4.815625
248.784796	8000.000858	9.446195	-0.051439	4.815607
249.126114	8000.084349	9.451200	-0.051503	4.815630
249.068453	8000.079144	9.456205	-0.051492	4.815629
248.949836	8000.049459	9.461210	-0.051470	4.815621
249.212649	8000.084696	9.466215	-0.051519	4.815630
249.145090	8000.070788	9.471219	-0.051506	4.815626
249.039044	8000.042375	9.476224	-0.051487	4.815618
249.048358	8000.048936	9.481229	-0.051488	4.815620
249.234313	8000.007117	9.486234	-0.051523	4.815607
249.287611	8000.074183	9.491239	-0.051533	4.815626
249.087818	8000.048518	9.496243	-0.051496	4.815620
249.425573	8000.072160	9.501248	-0.051559	4.815625
249.397365	8000.080246	9.506253	-0.051554	4.815627
249.242693	8000.022215	9.511258	-0.051525	4.815611
249.488475	8000.080665	9.516263	-0.051571	4.815627
249.447251	8000.109894	9.521267	-0.051563	4.815636
249.228937	8000.106348	9.526272	-0.051522	4.815636
249.327024	8000.131435	9.531277	-0.051541	4.815643
249.302229	8000.070176	9.536282	-0.051536	4.815625
249.469361	8000.151905	9.541287	-0.051567	4.815648
249.484699	8000.076350	9.546291	-0.051570	4.815626
249.501812	8000.144965	9.551296	-0.051573	4.815646
249.396492	8000.126172	9.556301	-0.051554	4.815641
249.231252	8000.086119	9.561306	-0.051523	4.815630
249.434337	8000.157756	9.566311	-0.051561	4.815650
249.558029	8000.052998	9.571315	-0.051584	4.815619
249.330579	8000.047169	9.576320	-0.051542	4.815618
249.155643	8000.030449	9.581325	-0.051509	4.815614
249.347571	8000.011149	9.586330	-0.051545	4.815607
249.287542	8000.068900	9.591335	-0.051534	4.815625
249.446530	8000.104586	9.596339	-0.051563	4.815634
249.723938	8000.109098	9.601344	-0.051615	4.815634
249.532438	8000.116665	9.606349	-0.051579	4.815637
249.404686	8000.114591	9.611354	-0.051556	4.815637
249.597195	8000.198870	9.616359	-0.051592	4.815661
249.361515	8000.104286	9.621363	-0.051548	4.815635
249.481091	8000.097691	9.626368	-0.051570	4.815632
249.463459	8000.100610	9.631373	-0.051567	4.815633
249.683758	8000.074298	9.636378	-0.051608	4.815624
249.907362	8000.076867	9.641383	-0.051649	4.815624
249.573640	8000.097071	9.646387	-0.051587	4.815631
249.753891	8000.082920	9.651392	-0.051621	4.815626
249.881892	8000.154406	9.656397	-0.051645	4.815647
249.582827	8000.115380	9.661402	-0.051589	4.815637
249.522270	8000.136820	9.666407	-0.051578	4.815643
249.592312	8000.083508	9.671411	-0.051591	4.815627
249.781560	8000.073774	9.676416	-0.051626	4.815624
249.543246	8000.088055	9.681421	-0.051582	4.815629
249.619994	8000.064748	9.686426	-0.051596	4.815622
249.864582	8000.157347	9.691431	-0.051642	4.815648
249.604544	8000.150987	9.696435	-0.051593	4.815647
249.719730	8000.141117	9.701440	-0.051615	4.815644
249.999193	8000.164883	9.706445	-0.051667	4.815649
249.867979	8000.111501	9.711450	-0.051642	4.815634
250.031409	8000.165412	9.716455	-0.051673	4.815649
249.822974	8000.071270	9.721459	-0.051634	4.815623
249.921709	8000.098503	9.726464	-0.051653	4.815630
249.771982	8000.177219	9.731469	-0.051625	4.815654
249.648979	8000.143190	9.736474	-0.051602	4.815645
249.830151	8000.113039	9.741479	-0.051636	4.815635
249.792348	8000.070786	9.746483	-0.051629	4.815623
249.745698	8000.138365	9.751488	-0.051620	4.815643
249.839885	8000.117476	9.756493	-0.051638	4.815636
249.850875	8000.056798	9.761498	-0.051640	4.815618
249.794633	8000.132762	9.766503	-0.051629	4.815641
249.861359	8000.083667	9.771507	-0.051642	4.815626
249.852271	8000.100605	9.776512	-0.051640	4.815631
249.816991	8000.160895	9.781517	-0.051633	4.815649
250.013192	8000.088279	9.786522	-0.051670	4.815627
250.197857	8000.160687	9.791527	-0.051704	4.815647
249.857607	8000.077214	9.796531	-0.051641	4.815624
249.935234	8000.087020	9.801536	-0.051656	4.815627
249.963949	8000.126996	9.806541	-0.051661	4.815638
249.890952	8000.064951	9.811546	-0.051647	4.815621
250.024008	8000.114097	9.816551	-0.051672	4.815634
250.051607	8000.046214	9.821555	-0.051677	4.815614
250.148493	8000.055266	9.826560	-0.051695	4.815616
249.974103	8000.099414	9.831565	-0.051663	4.815630
249.970764	8000.045976	9.836570	-0.051662	4.815615
250.094932	8000.089639	9.841575	-0.051686	4.815627
249.975675	8000.055671	9.846579	-0.051663	4.815617
250.085813	8000.103377	9.851584	-0.051684	4.815631
250.096418	8000.092875	9.856589	-0.051686	4.815628
250.013904	8000.032811	9.861594	-0.051671	4.815611
249.916963	8000.052593	9.866599	-0.051653	4.815617
250.027100	7999.988187	9.871603	-0.051673	4.815597
250.108332	8000.023678	9.876608	-0.051688	4.815607
250.013038	8000.104346	9.881613	-0.051671	4.815631
250.034518	8000.063057	9.886618	-0.051675	4.815619
250.216705	8000.102324	9.891623	-0.051709	4.815630
249.970865	8000.051350	9.896627	-0.051663	4.815616
250.106268	8000.163530	9.901632	-0.051688	4.815648
250.127363	8000.135047	9.906637	-0.051692	4.815640
250.026511	8000.089634	9.911642	-0.051673	4.815627
250.014089	8000.153498	9.916647	-0.051671	4.815646
249.967566	8000.110036	9.921651	-0.051662	4.815633
250.126961	8000.111562	9.926656	-0.051692	4.815633
250.045432	8000.144407	9.931661	-0.051677	4.815643
249.868261	8000.055044	9.936666	-0.051644	4.815618
250.125431	8000.130765	9.941671	-0.051692	4.815639
250.087897	8000.093855	9.946675	-0.051685	4.815628
249.992240	8000.083761	9.951680	-0.051667	4.815626
250.108717	8000.116621	9.956685	-0.051689	4.815635
250.178089	8000.082517	9.961690	-0.051702	4.815624
250.041520	8000.047200	9.966695	-0.051676	4.815615
250.043465	8000.070724	9.971699	-0.051677	4.815621
250.356216	8000.082218	9.976704	-0.051735	4.815623
250.171610	8000.088829	9.981709	-0.051701	4.815626
250.208887	8000.062745	9.986714	-0.051708	4.815618
250.414845	8000.151515	9.991719	-0.051746	4.815643
250.198911	8000.104230	9.996723	-0.051706	4.815631
250.360095	8000.155969	10.001728	-0.051736	4.815645
250.375082	8000.143403	10.006733	-0.051739	4.815641
250.145211	8000.088417	10.011738	-0.051696	4.815626
250.319895	8000.153188	10.016743	-0.051729	4.815644
250.056944	8000.147848	10.021747	-0.051680	4.815644
250.353155	8000.154803	10.026752	-0.051735	4.815645
250.379631	8000.138152	10.031757	-0.051740	4.815640
250.031877	8000.020389	10.036762	-0.051675	4.815607
250.453455	8000.129749	10.041767	-0.051754	4.815637
250.559057	8000.081285	10.046771	-0.051773	4.815622
250.572603	8000.113540	10.051776	-0.051776	4.815631
250.290354	8000.158069	10.056781	-0.051723	4.815646
250.305288	8000.063287	10.061786	-0.051726	4.815618
250.371909	8000.111353	10.066791	-0.051739	4.815632
250.545974	8000.075747	10.071795	-0.051771	4.815621
250.223823	8000.098273	10.076800	-0.051711	4.815629
250.348901	8000.159035	10.081805	-0.051734	4.815646
250.271817	8000.089450	10.086810	-0.051720	4.815626
250.597780	8000.166292	10.091815	-0.051781	4.815647
250.497037	8000.104862	10.096819	-0.051762	4.815629
250.304470	8000.057957	10.101824	-0.051726	4.815616
250.304768	8000.125232	10.106829	-0.051726	4.815636
250.383575	8000.112636	10.111834	-0.051741	4.815632
250.450974	8000.125480	10.116839	-0.051754	4.815636
250.411543	8000.106690	10.121843	-0.051746	4.815630
250.509301	8000.083724	10.126848	-0.051765	4.815623
250.710125	8000.112618	10.131853	-0.051802	4.815631
250.614418	8000.049136	10.136858	-0.051784	4.815612
250.448487	8000.146808	10.141863	-0.051753	4.815642
250.577123	8000.133954	10.146867	-0.051777	4.815637
250.578799	8000.092342	10.151872	-0.051778	4.815625
250.313266	8000.106179	10.156877	-0.051728	4.815631
250.420665	8000.135689	10.161882	-0.051748	4.815639
250.457605	8000.168325	10.166887	-0.051755	4.815648
250.477873	8000.136625	10.171891	-0.051759	4.815639
250.474039	8000.179275	10.176896	-0.051758	4.815651
250.462706	8000.201517	10.181901	-0.051756	4.815658
250.547926	8000.092928	10.186906	-0.051772	4.815626
250.514468	8000.104132	10.191911	-0.051766	4.815629
250.374198	8000.055941	10.196915	-0.051740	4.815616
250.512258	8000.157489	10.201920	-0.051766	4.815645
250.442790	8000.164904	10.206925	-0.051753	4.815647
250.590150	8000.094696	10.211930	-0.051780	4.815626
250.616342	8000.114344	10.216935	-0.051785	4.815631
250.463591	8000.121473	10.221939	-0.051757	4.815634
250.700431	8000.122124	10.226944	-0.051801	4.815633
250.676254	8000.161240	10.231949	-0.051796	4.815645
250.455331	8000.087179	10.236954	-0.051755	4.815624
250.683186	8000.147478	10.241959	-0.051798	4.815641
250.625148	8000.108098	10.246963	-0.051787	4.815630
250.612216	8000.077994	10.251968	-0.051785	4.815621
250.563833	8000.056923	10.256973	-0.051776	4.815615
250.353805	8000.058849	10.261978	-0.051736	4.815616
250.501954	8000.062329	10.266983	-0.051764	4.815617
250.409407	8000.114214	10.271987	-0.051747	4.815632
250.585097	8000.093583	10.276992	-0.051780	4.815626
250.584134	8000.146957	10.281997	-0.051780	4.815641
250.630340	8000.069766	10.287002	-0.051788	4.815618
250.519609	8000.107475	10.292007	-0.051768	4.815630
250.625888	8000.104935	10.297011	-0.051787	4.815629
250.559246	8000.120938	10.302016	-0.051775	4.815634
250.501944	8000.087977	10.307021	-0.051764	4.815624
250.653222	8000.058407	10.312026	-0.051793	4.815615
250.597523	8000.129043	10.317031	-0.051782	4.815636
250.465538	8000.056429	10.322035	-0.051758	4.815615
250.495585	8000.067598	10.327040	-0.051763	4.815618
250.611000	8000.127135	10.332045	-0.051785	4.815635
250.559069	8000.086787	10.337050	-0.051775	4.815624
250.419274	8000.164597	10.342055	-0.051749	4.815647
250.484488	8000.120815	10.347059	-0.051761	4.815634
250.577643	8000.155433	10.352064	-0.051779	4.815644
250.453899	8000.183320	10.357069	-0.051756	4.815652
250.499517	8000.116797	10.362074	-0.051764	4.815633
250.731014	8000.169681	10.367079	-0.051807	4.815647
250.603116	8000.097133	10.372083	-0.051784	4.815626
250.455016	8000.085118	10.377088	-0.051756	4.815624
250.639527	8000.148982	10.382093	-0.051790	4.815641
250.478752	8000.053477	10.387098	-0.051761	4.815614
250.517638	8000.128854	10.392103	-0.051768	4.815636
250.588967	8000.074494	10.397107	-0.051781	4.815620
250.706369	8000.060390	10.402112	-0.051803	4.815615
250.605293	8000.116407	10.407117	-0.051784	4.815632
250.404804	8000.087524	10.412122	-0.051747	4.815625
250.901353	8000.154328	10.417127	-0.051839	4.815642
250.883253	8000.096378	10.422131	-0.051836	4.815625
250.739861	8000.101523	10.427136	-0.051809	4.815627
250.736522	8000.107878	10.432141	-0.051809	4.815629
250.659184	8000.095946	10.437146	-0.051794	4.815626
250.767874	8000.160713	10.442151	-0.051815	4.815644
250.699109	8000.086991	10.447155	-0.051802	4.815623
250.663518	8000.093889	10.452160	-0.051795	4.815625
250.667948	8000.133471	10.457165	-0.051796	4.815637
250.514148	8000.050892	10.462170	-0.051768	4.815613
250.722393	8000.100194	10.467175	-0.051806	4.815627
250.814957	8000.101702	10.472179	-0.051824	4.815627
250.669888	8000.047026	10.477184	-0.051797	4.815611
250.726899	8000.108818	10.482189	-0.051807	4.815629
250.776234	8000.065845	10.487194	-0.051817	4.815616
250.761814	8000.109391	10.492199	-0.051814	4.815629
250.706548	8000.101021	10.497203	-0.051804	4.815627
250.849410	8000.103347	10.502208	-0.051830	4.815627
250.860202	8000.144100	10.507213	-0.051832	4.815639
250.844284	8000.098998	10.512218	-0.051829	4.815626
250.823082	8000.201160	10.517223	-0.051826	4.815656
250.670376	8000.150631	10.522227	-0.051797	4.815642
250.736899	8000.121818	10.527232	-0.051810	4.815633
250.799737	8000.187976	10.532237	-0.051821	4.815652
251.034250	8000.120254	10.537242	-0.051865	4.815631
250.858573	8000.187871	10.542247	-0.051832	4.815652
250.811518	8000.124111	10.547251	-0.051824	4.815633
250.832733	8000.113781	10.552256	-0.051828	4.815630
250.818982	8000.153067	10.557261	-0.051825	4.815642
250.715858	8000.075583	10.562266	-0.051806	4.815620
250.806349	8000.115496	10.567271	-0.051823	4.815631
250.902138	8000.086092	10.572275	-0.051841	4.815622
250.718838	8000.093792	10.577280	-0.051806	4.815625
250.665455	8000.183685	10.582285	-0.051797	4.815651
250.591676	8000.083187	10.587290	-0.051783	4.815622
250.708071	8000.147012	10.592295	-0.051805	4.815641
250.683714	8000.140212	10.597299	-0.051800	4.815639
250.908976	8000.170573	10.602304	-0.051842	4.815646
250.769619	8000.153360	10.607309	-0.051816	4.815642
250.628409	8000.133983	10.612314	-0.051790	4.815637
250.796438	8000.161277	10.617319	-0.051821	4.815644
250.812323	8000.094270	10.622323	-0.051824	4.815625
250.800447	8000.099418	10.627328	-0.051822	4.815626
250.727560	8000.178316	10.632333	-0.051809	4.815650
250.785161	8000.131207	10.637338	-0.051819	4.815636
250.898727	8000.180038	10.642343	-0.051840	4.815649
250.718671	8000.136538	10.647347	-0.051807	4.815637
250.763841	8000.078550	10.652352	-0.051815	4.815620
250.828220	8000.160748	10.657357	-0.051827	4.815644
250.789219	8000.071494	10.662362	-0.051820	4.815618
250.872924	8000.066451	10.667367	-0.051836	4.815616
250.750157	8000.024951	10.672371	-0.051813	4.815605
250.805383	8000.110204	10.677376	-0.051823	4.815629
250.757625	8000.187376	10.682381	-0.051814	4.815652
250.863725	8000.206188	10.687386	-0.051834	4.815657
250.874472	8000.207434	10.692391	-0.051836	4.815657
250.627539	8000.161778	10.697395	-0.051790	4.815645
251.012729	8000.180859	10.702400	-0.051862	4.815649
250.932854	8000.205188	10.707405	-0.051847	4.815656
250.831160	8000.108507	10.712410	-0.051828	4.815629
250.671833	8000.160374	10.717415	-0.051799	4.815645
250.856029	8000.082224	10.722419	-0.051833	4.815621
250.790794	8000.092911	10.727424	-0.051821	4.815624
250.792691	8000.190110	10.732429	-0.051821	4.815653
250.892286	8000.106312	10.737434	-0.051840	4.815628
251.030919	8000.179042	10.742439	-0.051866	4.815648
250.943786	8000.128511	10.747443	-0.051849	4.815634
250.854144	8000.181511	10.752448	-0.051833	4.815650
251.059278	8000.153885	10.757453	-0.051871	4.815641
250.972704	8000.093754	10.762458	-0.051855	4.815624
250.964402	8000.163025	10.767463	-0.051853	4.815644
250.815872	8000.101886	10.772467	-0.051826	4.815627
250.841986	8000.129007	10.777472	-0.051831	4.815635
250.716491	8000.200644	10.782477	-0.051807	4.815656
250.850538	8000.071494	10.787482	-0.051832	4.815618
251.036318	8000.132176	10.792487	-0.051867	4.815635
250.877728	8000.108245	10.797491	-0.051838	4.815628
250.925817	8000.054575	10.802496	-0.051846	4.815612
251.036700	8000.181308	10.807501	-0.051867	4.815649
250.908184	8000.105545	10.812506	-0.051843	4.815627
251.113297	8000.166543	10.817511	-0.051882	4.815644
251.217600	8000.137278	10.822515	-0.051901	4.815635
251.241108	8000.062920	10.827520	-0.051905	4.815613
251.104850	8000.140788	10.832525	-0.051880	4.815637
250.993127	8000.095196	10.837530	-0.051859	4.815624
251.130738	8000.175383	10.842535	-0.051885	4.815647
251.019977	8000.184262	10.847539	-0.051864	4.815650
250.889941	8000.093526	10.852544	-0.051840	4.815624
251.007403	8000.174453	10.857549	-0.051862	4.815647
250.861975	8000.072790	10.862554	-0.051835	4.815618
250.857861	8000.090877	10.867559	-0.051834	4.815623
251.116113	8000.134587	10.872563	-0.051882	4.815635
251.067752	8000.099635	10.877568	-0.051873	4.815625
251.052632	8000.193355	10.882573	-0.051871	4.815652
250.792627	8000.132538	10.887578	-0.051822	4.815636
250.920152	8000.182663	10.892583	-0.051846	4.815650
250.861889	8000.169973	10.897587	-0.051835	4.815646
251.085470	8000.134106	10.902592	-0.051877	4.815635
251.292873	8000.139618	10.907597	-0.051916	4.815636
251.112566	8000.137755	10.912602	-0.051882	4.815636
250.854638	8000.112208	10.917607	-0.051834	4.815630
250.792461	8000.072761	10.922611	-0.051822	4.815618
251.005215	8000.076224	10.927616	-0.051862	4.815618
250.917642	8000.159154	10.932621	-0.051846	4.815643
250.931607	8000.079303	10.937626	-0.051848	4.815620
251.152262	8000.115995	10.942631	-0.051890	4.815629
251.156250	8000.049862	10.947635	-0.051890	4.815610
250.959166	8000.021034	10.952640	-0.051854	4.815602
250.974887	8000.015953	10.957645	-0.051857	4.815601
250.993856	8000.040823	10.962650	-0.051860	4.815608
251.075567	8000.119033	10.967655	-0.051875	4.815631
250.972387	8000.109883	10.972659	-0.051856	4.815628
251.053720	8000.109073	10.977664	-0.051871	4.815628
251.025161	8000.127831	10.982669	-0.051866	4.815633
250.824259	8000.059434	10.987674	-0.051829	4.815614
251.045098	8000.111077	10.992679	-0.051870	4.815628
250.850693	8000.050260	10.997683	-0.051834	4.815611
251.081452	8000.074303	11.002688	-0.051877	4.815617
251.279365	8000.089270	11.007693	-0.051914	4.815621
250.892799	8000.064834	11.012698	-0.051842	4.815616
251.038362	8000.073610	11.017703	-0.051869	4.815617
250.875728	8000.112610	11.022707	-0.051839	4.815630
251.193726	8000.099633	11.027712	-0.051898	4.815624
251.083021	8000.152291	11.032717	-0.051877	4.815640
250.916097	8000.091920	11.037722	-0.051846	4.815623
251.009742	8000.151105	11.042727	-0.051864	4.815640
250.971576	8000.145148	11.047731	-0.051857	4.815639
250.943024	8000.064605	11.052736	-0.051851	4.815615
251.137722	8000.152127	11.057741	-0.051888	4.815640
251.332445	8000.127536	11.062746	-0.051924	4.815632
251.249696	8000.134735	11.067751	-0.051909	4.815634
251.283343	8000.180131	11.072755	-0.051915	4.815647
251.329870	8000.123231	11.077760	-0.051924	4.815631
251.097268	8000.145077	11.082765	-0.051880	4.815638
251.012744	8000.090317	11.087770	-0.051865	4.815622
251.166137	8000.160084	11.092775	-0.051893	4.815642
251.132199	8000.158467	11.097779	-0.051887	4.815642
251.077746	8000.075366	11.102784	-0.051877	4.815618
251.170691	8000.154827	11.107789	-0.051894	4.815641
251.157715	8000.115112	11.112794	-0.051892	4.815629
250.952027	8000.126718	11.117799	-0.051853	4.815633
251.035909	8000.138762	11.122803	-0.051869	4.815636
250.988540	8000.164689	11.127808	-0.051860	4.815644
251.071725	8000.158570	11.132813	-0.051876	4.815642
251.088964	8000.063823	11.137818	-0.051879	4.815614
251.347815	8000.190829	11.142823	-0.051927	4.815650
251.127760	8000.175507	11.147827	-0.051886	4.815647
251.164090	8000.113103	11.152832	-0.051893	4.815628
251.313370	8000.145431	11.157837	-0.051921	4.815637
251.166408	8000.107807	11.162842	-0.051894	4.815627
251.094459	8000.135469	11.167847	-0.051880	4.815635
251.122900	8000.126325	11.172851	-0.051886	4.815632
251.233539	8000.120653	11.177856	-0.051906	4.815630
251.280333	8000.159856	11.182861	-0.051915	4.815641
251.188564	8000.131672	11.187866	-0.051898	4.815634
251.115534	8000.146504	11.192871	-0.051884	4.815638
251.179644	8000.111246	11.197875	-0.051896	4.815628
251.235509	8000.073718	11.202880	-0.051907	4.815616
251.197444	8000.113676	11.207885	-0.051900	4.815628
251.092599	8000.131193	11.212890	-0.051880	4.815634
251.259940	8000.197984	11.217895	-0.051911	4.815653
251.290806	8000.139762	11.222899	-0.051917	4.815636
251.304752	8000.072723	11.227904	-0.051920	4.815616
251.274008	8000.184340	11.232909	-0.051914	4.815649
251.116870	8000.142280	11.237914	-0.051885	4.815637
251.204969	8000.206714	11.242919	-0.051901	4.815656
251.457337	8000.164908	11.247923	-0.051948	4.815642
251.334592	8000.176795	11.252928	-0.051926	4.815646
251.290292	8000.186755	11.257933	-0.051917	4.815649
251.431971	8000.145284	11.262938	-0.051944	4.815636
251.470640	8000.140577	11.267943	-0.051951	4.815635
251.413234	8000.122562	11.272947	-0.051940	4.815630
251.474874	8000.119296	11.277952	-0.051952	4.815629
251.365355	8000.192261	11.282957	-0.051931	4.815651
251.233202	8000.190114	11.287962	-0.051907	4.815651
251.153185	8000.195222	11.292967	-0.051892	4.815652
251.217118	8000.127928	11.297971	-0.051904	4.815632
251.181003	8000.089972	11.302976	-0.051897	4.815621
251.251977	8000.174414	11.307981	-0.051911	4.815646
251.222534	8000.176074	11.312986	-0.051905	4.815646
251.382143	8000.184012	11.317991	-0.051935	4.815648
251.234504	8000.175206	11.322995	-0.051907	4.815646
251.259917	8000.155335	11.328000	-0.051912	4.815640
251.431812	8000.200845	11.333005	-0.051944	4.815653
251.209250	8000.123551	11.338010	-0.051903	4.815631
251.266665	8000.159724	11.343015	-0.051913	4.815641
251.533025	8000.176874	11.348019	-0.051963	4.815645
251.488736	8000.093938	11.353024	-0.051955	4.815621
251.370270	8000.178502	11.358029	-0.051933	4.815646
251.344775	8000.100144	11.363034	-0.051928	4.815624
251.455717	8000.179898	11.368039	-0.051949	4.815646
251.272466	8000.196140	11.373043	-0.051915	4.815652
251.199936	8000.097796	11.378048	-0.051901	4.815624
251.313866	8000.200022	11.383053	-0.051923	4.815653
251.268892	8000.148041	11.388058	-0.051914	4.815638
251.417838	8000.140857	11.393063	-0.051942	4.815635
251.328943	8000.122329	11.398067	-0.051925	4.815630
251.304036	8000.122994	11.403072	-0.051921	4.815631
251.288871	8000.207104	11.408077	-0.051918	4.815655
251.261277	8000.152202	11.413082	-0.051913	4.815639
251.560414	8000.153868	11.418087	-0.051969	4.815638
251.544908	8000.155754	11.423091	-0.051966	4.815639
251.397452	8000.072208	11.428096	-0.051938	4.815615
251.592199	8000.205647	11.433101	-0.051975	4.815653
251.395511	8000.175755	11.438106	-0.051938	4.815646
251.490990	8000.152753	11.443111	-0.051956	4.815638
251.537324	8000.181271	11.448115	-0.051965	4.815646
251.338814	8000.192993	11.453120	-0.051928	4.815651
251.269395	8000.231374	11.458125	-0.051915	4.815662
251.206491	8000.129984	11.463130	-0.051903	4.815633
251.420990	8000.151628	11.468135	-0.051943	4.815638
251.283998	8000.147266	11.473139	-0.051918	4.815638
251.322678	8000.154305	11.478144	-0.051925	4.815640
251.525201	8000.176823	11.483149	-0.051963	4.815645
251.502345	8000.130540	11.488154	-0.051958	4.815632
251.397380	8000.152326	11.493159	-0.051939	4.815639
251.304089	8000.162556	11.498163	-0.051921	4.815642
251.384908	8000.083791	11.503168	-0.051936	4.815619
251.225264	8000.174093	11.508173	-0.051907	4.815646
251.253229	8000.128637	11.513178	-0.051912	4.815632
251.587125	8000.124461	11.518183	-0.051974	4.815630
251.536310	8000.169552	11.523187	-0.051965	4.815643
251.302977	8000.108099	11.528192	-0.051921	4.815626
251.388415	8000.176761	11.533197	-0.051937	4.815646
251.591537	8000.110663	11.538202	-0.051975	4.815626
251.367107	8000.140116	11.543207	-0.051933	4.815635
251.450984	8000.123331	11.548211	-0.051949	4.815630
251.423289	8000.097257	11.553216	-0.051944	4.815622
251.394113	8000.180071	11.558221	-0.051939	4.815647
251.373883	8000.086849	11.563226	-0.051935	4.815620
251.405087	8000.141816	11.568231	-0.051941	4.815636
251.321162	8000.125504	11.573235	-0.051925	4.815631
251.379134	8000.114705	11.578240	-0.051936	4.815628
251.608210	8000.200653	11.583245	-0.051979	4.815652
251.488900	8000.159207	11.588250	-0.051956	4.815640
251.571928	8000.168035	11.593255	-0.051972	4.815642
251.523587	8000.202488	11.598259	-0.051963	4.815653
251.529580	8000.102218	11.603264	-0.051964	4.815623
251.469409	8000.163172	11.608269	-0.051953	4.815641
251.491488	8000.122959	11.613274	-0.051957	4.815630
251.587023	8000.151210	11.618279	-0.051975	4.815637
251.358963	8000.125080	11.623283	-0.051932	4.815631
251.417964	8000.074790	11.628288	-0.051943	4.815616
251.415983	8000.089709	11.633293	-0.051943	4.815620
251.441127	8000.071969	11.638298	-0.051948	4.815615
251.270072	8000.136458	11.643303	-0.051916	4.815635
251.368897	8000.190389	11.648307	-0.051934	4.815650
251.597448	8000.119367	11.653312	-0.051977	4.815628
251.568368	8000.166946	11.658317	-0.051972	4.815642
251.366124	8000.175404	11.663322	-0.051934	4.815646
251.424414	8000.133644	11.668327	-0.051945	4.815633
251.544541	8000.164431	11.673331	-0.051967	4.815641
251.554981	8000.148587	11.678336	-0.051969	4.815637
251.552824	8000.191266	11.683341	-0.051969	4.815649
251.389164	8000.178996	11.688346	-0.051939	4.815646
251.413181	8000.153763	11.693351	-0.051943	4.815639
251.474499	8000.190000	11.698355	-0.051954	4.815649
251.646941	8000.161843	11.703360	-0.051987	4.815640
251.677871	8000.220009	11.708365	-0.051992	4.815657
251.573329	8000.188413	11.713370	-0.051973	4.815648
251.634665	8000.137093	11.718375	-0.051984	4.815633
251.677395	8000.177299	11.723379	-0.051992	4.815645
251.588841	8000.203623	11.728384	-0.051976	4.815653
251.621156	8000.225507	11.733389	-0.051982	4.815659
251.665596	8000.181386	11.738394	-0.051990	4.815646
251.799210	8000.183563	11.743399	-0.052015	4.815646
251.687063	8000.168928	11.748403	-0.051994	4.815642
251.663938	8000.169622	11.753408	-0.051990	4.815642
251.774996	8000.163958	11.758413	-0.052011	4.815640
251.429369	8000.187167	11.763418	-0.051946	4.815649
251.680734	8000.147481	11.768423	-0.051993	4.815636
251.644102	8000.189598	11.773427	-0.051987	4.815648
251.544601	8000.154881	11.778432	-0.051968	4.815639
251.573727	8000.204476	11.783437	-0.051974	4.815653
251.661373	8000.136499	11.788442	-0.051990	4.815633
251.690630	8000.126300	11.793447	-0.051995	4.815630
251.610114	8000.094028	11.798451	-0.051980	4.815621
251.712067	8000.055114	11.803456	-0.051999	4.815609
251.806809	8000.137809	11.808461	-0.052017	4.815632
251.701249	8000.067757	11.813466	-0.051997	4.815612
251.723003	8000.112960	11.818471	-0.052001	4.815626
251.612118	8000.164548	11.823475	-0.051981	4.815641
251.499463	8000.138159	11.828480	-0.051960	4.815634
251.745446	8000.116537	11.833485	-0.052006	4.815626
251.633659	8000.036774	11.838490	-0.051985	4.815604
251.792209	8000.070322	11.843495	-0.052015	4.815613
251.791725	8000.136519	11.848499	-0.052014	4.815632
251.564885	8000.083713	11.853504	-0.051972	4.815618
251.592919	8000.183475	11.858509	-0.051978	4.815647
251.501640	8000.090164	11.863514	-0.051961	4.815620
251.544867	8000.107955	11.868519	-0.051969	4.815625
251.787034	8000.128982	11.873523	-0.052014	4.815630
251.669771	8000.071553	11.878528	-0.051992	4.815614
251.593414	8000.146125	11.883533	-0.051978	4.815636
251.657685	8000.117276	11.888538	-0.051990	4.815627
251.646277	8000.130974	11.893543	-0.051988	4.815631
251.668154	8000.088622	11.898547	-0.051992	4.815619
251.598293	8000.073607	11.903552	-0.051979	4.815615
251.726271	8000.121606	11.908557	-0.052003	4.815628
251.641298	8000.090329	11.913562	-0.051987	4.815619
251.649036	8000.082984	11.918567	-0.051988	4.815617
251.545337	8000.095180	11.923571	-0.051969	4.815621
251.646455	8000.047711	11.928576	-0.051988	4.815607
251.706969	8000.119171	11.933581	-0.051999	4.815627
251.538537	8000.107891	11.938586	-0.051968	4.815625
251.712127	8000.080821	11.943591	-0.052000	4.815616
251.768513	8000.141536	11.948595	-0.052011	4.815634
251.633695	8000.092364	11.953600	-0.051986	4.815620
251.915415	8000.182372	11.958605	-0.052038	4.815645
251.565248	8000.140373	11.963610	-0.051973	4.815634
251.534073	8000.195393	11.968615	-0.051967	4.815651
251.641262	8000.135209	11.973619	-0.051987	4.815632
251.521477	8000.154618	11.978624	-0.051965	4.815639
251.498105	8000.136089	11.983629	-0.051961	4.815633
251.470308	8000.079048	11.988634	-0.051956	4.815617
251.554092	8000.066533	11.993639	-0.051971	4.815613
251.443990	8000.178995	11.998643	-0.051951	4.815646
251.539737	8000.071643	12.003648	-0.051969	4.815614
251.690013	8000.171258	12.008653	-0.051997	4.815643
251.489377	8000.086846	12.013658	-0.051959	4.815619
251.645940	8000.141717	12.018663	-0.051988	4.815634
251.621636	8000.149866	12.023667	-0.051984	4.815637
251.579865	8000.073378	12.028672	-0.051976	4.815615
251.693004	8000.116865	12.033677	-0.051997	4.815627
251.621216	8000.038820	12.038682	-0.051984	4.815604
251.823103	8000.085886	12.043687	-0.052022	4.815617
251.562245	8000.096594	12.048691	-0.051973	4.815621
251.653966	8000.099156	12.053696	-0.051990	4.815622
251.782296	8000.129009	12.058701	-0.052014	4.815630
251.694325	8000.078463	12.063706	-0.051998	4.815616
251.622915	8000.079440	12.068711	-0.051984	4.815616
251.769373	8000.064741	12.073715	-0.052012	4.815611
251.949685	8000.048458	12.078720	-0.052045	4.815606
251.713078	8000.106542	12.083725	-0.052001	4.815624
251.517270	8000.132189	12.088730	-0.051965	4.815632
251.583989	8000.107650	12.093735	-0.051977	4.815625
251.784356	8000.139743	12.098739	-0.052015	4.815633
251.695603	8000.065693	12.103744	-0.051998	4.815612
251.726544	8000.128130	12.108749	-0.052004	4.815630
251.705342	8000.050909	12.113754	-0.052000	4.815607
251.643992	8000.037100	12.118759	-0.051989	4.815604
251.570217	8000.085020	12.123763	-0.051975	4.815618
251.892747	8000.087067	12.128768	-0.052035	4.815617
251.778273	8000.093750	12.133773	-0.052014	4.815620
251.549177	8000.109245	12.138778	-0.051971	4.815625
251.689127	8000.112592	12.143783	-0.051997	4.815626
251.558534	8000.046405	12.148787	-0.051973	4.815607
251.544701	8000.026963	12.153792	-0.051970	4.815601
251.867206	8000.118702	12.158797	-0.052031	4.815626
251.750250	8000.123208	12.163802	-0.052009	4.815628
251.719262	8000.132317	12.168807	-0.052003	4.815631
251.604047	8000.148597	12.173811	-0.051982	4.815636
251.679534	8000.096440	12.178816	-0.051996	4.815621
251.766608	8000.161925	12.183821	-0.052012	4.815640
251.703068	8000.100031	12.188826	-0.052000	4.815622
251.856812	8000.144179	12.193831	-0.052029	4.815634
251.845191	8000.129044	12.198835	-0.052027	4.815630
251.765023	8000.049795	12.203840	-0.052012	4.815607
251.859342	8000.141025	12.208845	-0.052029	4.815633
251.786371	8000.123824	12.213850	-0.052016	4.815628
251.630865	8000.087128	12.218855	-0.051987	4.815618
251.670119	8000.125142	12.223859	-0.051994	4.815629
251.861137	8000.103694	12.228864	-0.052030	4.815622
251.960856	8000.186470	12.233869	-0.052048	4.815646
251.597161	8000.132505	12.238874	-0.051981	4.815632
251.600692	8000.106939	12.243879	-0.051981	4.815624
251.697047	8000.118119	12.248883	-0.051999	4.815627
251.849260	8000.045855	12.253888	-0.052028	4.815605
251.826913	8000.123441	12.258893	-0.052024	4.815628
251.911101	8000.100255	12.263898	-0.052039	4.815621
251.846880	8000.105620	12.268903	-0.052027	4.815623
251.708653	8000.169575	12.273907	-0.052002	4.815642
251.692406	8000.083892	12.278912	-0.051999	4.815617
251.766640	8000.187609	12.283917	-0.052013	4.815647
251.579795	8000.204859	12.288922	-0.051978	4.815653
251.761660	8000.246261	12.293927	-0.052012	4.815664
251.900034	8000.198330	12.298931	-0.052038	4.815650
251.813661	8000.088015	12.303936	-0.052021	4.815618
251.908575	8000.158967	12.308941	-0.052039	4.815638
251.835840	8000.134295	12.313946	-0.052026	4.815631
252.116509	8000.173034	12.318951	-0.052078	4.815641
251.844431	8000.185694	12.323955	-0.052027	4.815646
251.859186	8000.134684	12.328960	-0.052030	4.815631
252.035868	8000.204832	12.333965	-0.052063	4.815651
251.795278	8000.128311	12.338970	-0.052018	4.815630
251.885184	8000.118031	12.343975	-0.052035	4.815626
251.887163	8000.154370	12.348979	-0.052035	4.815637
251.877087	8000.131786	12.353984	-0.052034	4.815630
251.912152	8000.153715	12.358989	-0.052040	4.815636
251.920235	8000.152781	12.363994	-0.052042	4.815636
252.063759	8000.167933	12.368999	-0.052069	4.815640
251.802298	8000.148732	12.374003	-0.052020	4.815636
251.872134	8000.146668	12.379008	-0.052033	4.815635
251.967654	8000.179191	12.384013	-0.052051	4.815644
251.672818	8000.144498	12.389018	-0.051996	4.815635
251.843946	8000.199607	12.394023	-0.052028	4.815650
251.844491	8000.203890	12.399027	-0.052028	4.815651
251.846844	8000.096085	12.404032	-0.052028	4.815620
251.811791	8000.143568	12.409037	-0.052022	4.815634
251.777109	8000.100295	12.414042	-0.052015	4.815621
252.001865	8000.102887	12.419047	-0.052057	4.815621
251.823715	8000.143770	12.424051	-0.052024	4.815634
251.815791	8000.120153	12.429056	-0.052023	4.815627
251.848731	8000.187962	12.434061	-0.052029	4.815647
251.689598	8000.184307	12.439066	-0.051999	4.815646
251.819234	8000.103133	12.444071	-0.052023	4.815622
251.736675	8000.160520	12.449075	-0.052008	4.815639
251.766505	8000.114026	12.454080	-0.052014	4.815626
251.799811	8000.129520	12.459085	-0.052020	4.815630
251.869328	8000.076197	12.464090	-0.052033	4.815614
251.807705	8000.147806	12.469095	-0.052021	4.815635
251.741347	8000.105086	12.474099	-0.052009	4.815623
251.830789	8000.070240	12.479104	-0.052026	4.815612
251.897385	8000.170629	12.484109	-0.052038	4.815641
251.780781	8000.186887	12.489114	-0.052017	4.815647
251.771765	8000.198489	12.494119	-0.052015	4.815650
251.939176	8000.222571	12.499123	-0.052046	4.815656
252.013439	8000.086039	12.504128	-0.052060	4.815616
251.911311	8000.113210	12.509133	-0.052041	4.815625
251.922339	8000.101647	12.514138	-0.052043	4.815621
252.031485	8000.140798	12.519143	-0.052063	4.815632
251.840127	8000.190008	12.524147	-0.052028	4.815647
251.920505	8000.110168	12.529152	-0.052043	4.815624
252.026283	8000.175958	12.534157	-0.052063	4.815642
251.909841	8000.153779	12.539162	-0.052041	4.815636
251.816137	8000.161867	12.544167	-0.052024	4.815639
252.026594	8000.185582	12.549171	-0.052063	4.815645
251.905186	8000.197490	12.554176	-0.052040	4.815649
251.987559	8000.221257	12.559181	-0.052056	4.815656
252.013867	8000.215281	12.564186	-0.052061	4.815654
251.965925	8000.180335	12.569191	-0.052052	4.815644
251.893654	8000.172755	12.574195	-0.052038	4.815642
251.925953	8000.146589	12.579200	-0.052044	4.815634
252.175085	8000.228594	12.584205	-0.052091	4.815657
251.853405	8000.161431	12.589210	-0.052031	4.815639
251.858523	8000.146568	12.594215	-0.052032	4.815635
252.062120	8000.176578	12.599219	-0.052070	4.815642
252.076800	8000.131973	12.604224	-0.052072	4.815629
251.932784	8000.203309	12.609229	-0.052046	4.815651
251.877784	8000.193875	12.614234	-0.052035	4.815648
251.971620	8000.138812	12.619239	-0.052053	4.815632
252.024664	8000.188796	12.624243	-0.052063	4.815646
251.907245	8000.198634	12.629248	-0.052041	4.815650
252.186992	8000.186105	12.634253	-0.052093	4.815645
252.005331	8000.189558	12.639258	-0.052059	4.815646
251.836524	8000.172933	12.644263	-0.052028	4.815642
251.838465	8000.175103	12.649267	-0.052028	4.815643
251.919862	8000.208463	12.654272	-0.052044	4.815652
251.979376	8000.236129	12.659277	-0.052055	4.815660
251.914912	8000.206253	12.664282	-0.052043	4.815652
251.750372	8000.213188	12.669287	-0.052012	4.815655
251.967397	8000.209248	12.674291	-0.052053	4.815652
251.813735	8000.094634	12.679296	-0.052024	4.815620
252.147606	8000.165204	12.684301	-0.052086	4.815639
251.849492	8000.109102	12.689306	-0.052031	4.815624
251.728465	8000.086848	12.694311	-0.052008	4.815618
251.861110	8000.193652	12.699315	-0.052033	4.815648
252.027028	8000.135491	12.704320	-0.052064	4.815631
252.052037	8000.171137	12.709325	-0.052069	4.815641
252.077915	8000.138460	12.714330	-0.052073	4.815631
252.130854	8000.136121	12.719335	-0.052083	4.815630
252.156275	8000.173910	12.724339	-0.052088	4.815641
251.942604	8000.101030	12.729344	-0.052048	4.815621
252.286493	8000.213408	12.734349	-0.052112	4.815652
252.023371	8000.242229	12.739354	-0.052063	4.815662
251.946471	8000.217489	12.744359	-0.052049	4.815655
252.075381	8000.201438	12.749363	-0.052073	4.815650
252.104132	8000.155994	12.754368	-0.052079	4.815636
252.234558	8000.208305	12.759373	-0.052103	4.815651
251.923435	8000.148788	12.764378	-0.052045	4.815635
252.276414	8000.134247	12.769383	-0.052111	4.815629
252.175750	8000.252204	12.774387	-0.052092	4.815664
251.966177	8000.183661	12.779392	-0.052053	4.815645
251.968122	8000.229610	12.784397	-0.052053	4.815658
252.055289	8000.171235	12.789402	-0.052070	4.815641
252.052077	8000.126339	12.794407	-0.052069	4.815628
251.822483	8000.171724	12.799411	-0.052026	4.815642
252.103289	8000.133585	12.804416	-0.052079	4.815630
252.007014	8000.127750	12.809421	-0.052061	4.815628
251.753319	8000.097998	12.814426	-0.052014	4.815621
251.970857	8000.157065	12.819431	-0.052054	4.815637
251.982962	8000.144451	12.824435	-0.052056	4.815633
251.917903	8000.119905	12.829440	-0.052044	4.815626
252.095240	8000.197538	12.834445	-0.052077	4.815648
251.920138	8000.145573	12.839450	-0.052045	4.815634
251.991400	8000.117906	12.844455	-0.052058	4.815626
251.997720	8000.208773	12.849459	-0.052059	4.815652
251.995309	8000.204465	12.854464	-0.052059	4.815651
252.148039	8000.209089	12.859469	-0.052087	4.815651
252.004913	8000.168322	12.864474	-0.052061	4.815640
252.061789	8000.119065	12.869479	-0.052071	4.815626
251.955335	8000.162182	12.874483	-0.052052	4.815639
251.951000	8000.093777	12.879488	-0.052051	4.815619
251.988164	8000.129621	12.884493	-0.052058	4.815629
251.901310	8000.171990	12.889498	-0.052042	4.815642
251.932108	8000.162883	12.894503	-0.052047	4.815639
251.806928	8000.182205	12.899507	-0.052024	4.815645
251.844728	8000.058961	12.904512	-0.052031	4.815609
252.144846	8000.236828	12.909517	-0.052087	4.815660
251.779077	8000.191370	12.914522	-0.052019	4.815648
251.922567	8000.126438	12.919527	-0.052046	4.815628
252.063441	8000.127665	12.924531	-0.052072	4.815628
252.064113	8000.110594	12.929536	-0.052072	4.815623
252.004855	8000.187581	12.934541	-0.052061	4.815646
251.982010	8000.145569	12.939546	-0.052057	4.815634
251.986788	8000.108277	12.944551	-0.052058	4.815623
252.185257	8000.128594	12.949555	-0.052095	4.815628
252.105172	8000.115548	12.954560	-0.052080	4.815624
252.159186	8000.187971	12.959565	-0.052090	4.815645
251.930789	8000.153291	12.964570	-0.052048	4.815636
251.876399	8000.096885	12.969575	-0.052037	4.815620
252.076643	8000.186636	12.974579	-0.052075	4.815645
251.979912	8000.094304	12.979584	-0.052057	4.815619
251.985682	8000.140315	12.984589	-0.052058	4.815632
252.204222	8000.144942	12.989594	-0.052099	4.815632
252.051628	8000.092276	12.994599	-0.052070	4.815618
252.005547	8000.184426	12.999603	-0.052062	4.815645
252.036708	8000.109123	13.004608	-0.052068	4.815623
252.095373	8000.199774	13.009613	-0.052079	4.815649
252.043113	8000.178639	13.014618	-0.052069	4.815643
251.917651	8000.098652	13.019623	-0.052045	4.815620
252.053982	8000.117958	13.024627	-0.052071	4.815625
251.895505	8000.121788	13.029632	-0.052041	4.815627
251.950547	8000.199567	13.034637	-0.052052	4.815650
252.159986	8000.192301	13.039642	-0.052091	4.815646
251.924999	8000.161785	13.044647	-0.052047	4.815639
251.743327	8000.183390	13.049651	-0.052013	4.815646
251.937788	8000.084051	13.054656	-0.052049	4.815616
252.092255	8000.168786	13.059661	-0.052078	4.815640
251.963204	8000.133588	13.064666	-0.052054	4.815630
252.094423	8000.116506	13.069671	-0.052079	4.815625
252.072289	8000.185554	13.074675	-0.052075	4.815645
252.068370	8000.163070	13.079680	-0.052074	4.815638
252.185816	8000.143628	13.084685	-0.052096	4.815632
252.329475	8000.127817	13.089690	-0.052123	4.815627
252.262993	8000.127805	13.094695	-0.052110	4.815627
252.234011	8000.184997	13.099699	-0.052105	4.815644
251.925220	8000.073197	13.104704	-0.052047	4.815613
252.183800	8000.105169	13.109709	-0.052096	4.815621
252.000638	8000.103259	13.114714	-0.052062	4.815621
252.053753	8000.132957	13.119719	-0.052071	4.815630
252.126138	8000.143747	13.124723	-0.052085	4.815632
252.020570	8000.120677	13.129728	-0.052065	4.815626
252.061751	8000.132027	13.134733	-0.052073	4.815629
251.972048	8000.149790	13.139738	-0.052056	4.815635
252.210730	8000.096017	13.144743	-0.052101	4.815618
252.107060	8000.166942	13.149747	-0.052082	4.815639
251.899344	8000.181717	13.154752	-0.052043	4.815645
252.151862	8000.156999	13.159757	-0.052090	4.815636
252.047582	8000.155305	13.164762	-0.052071	4.815636
252.112654	8000.129672	13.169767	-0.052083	4.815628
252.201037	8000.180231	13.174771	-0.052099	4.815643
252.019829	8000.136709	13.179776	-0.052066	4.815631
252.010109	8000.214502	13.184781	-0.052064	4.815654
252.077471	8000.223076	13.189786	-0.052076	4.815656
251.906999	8000.150899	13.194791	-0.052045	4.815636
251.924247	8000.196029	13.199795	-0.052048	4.815649
251.815169	8000.105631	13.204800	-0.052028	4.815623
252.015881	8000.166560	13.209805	-0.052065	4.815640
251.830155	8000.200913	13.214810	-0.052030	4.815651
251.913763	8000.163836	13.219815	-0.052046	4.815639
252.023609	8000.175237	13.224819	-0.052067	4.815642
252.118597	8000.105244	13.229824	-0.052084	4.815621
252.052490	8000.110577	13.234829	-0.052072	4.815623
251.956620	8000.213663	13.239834	-0.052054	4.815654
252.048566	8000.159637	13.244839	-0.052071	4.815637
252.221142	8000.220109	13.249843	-0.052104	4.815654
252.066935	8000.104417	13.254848	-0.052075	4.815621
252.102547	8000.179744	13.259853	-0.052081	4.815643
252.048531	8000.121208	13.264858	-0.052071	4.815626
251.935213	8000.104418	13.269863	-0.052050	4.815622
252.006371	8000.166442	13.274867	-0.052064	4.815640
252.142503	8000.085373	13.279872	-0.052089	4.815615
251.997719	8000.106511	13.284877	-0.052062	4.815622
252.169360	8000.105036	13.289882	-0.052094	4.815621
252.162195	8000.088905	13.294887	-0.052093	4.815616
251.983480	8000.186371	13.299891	-0.052060	4.815646
251.907769	8000.061280	13.304896	-0.052045	4.815609
252.111078	8000.158556	13.309901	-0.052083	4.815637
251.994363	8000.154523	13.314906	-0.052062	4.815636
251.906400	8000.131739	13.319911	-0.052045	4.815630
251.988402	8000.171517	13.324915	-0.052061	4.815641
252.064608	8000.123642	13.329920	-0.052075	4.815627
251.954299	8000.190187	13.334925	-0.052054	4.815647
251.968935	8000.210716	13.339930	-0.052057	4.815653
252.151933	8000.190206	13.344935	-0.052091	4.815646
251.989186	8000.208916	13.349939	-0.052061	4.815652
251.894648	8000.171076	13.354944	-0.052043	4.815641
251.898131	8000.181813	13.359949	-0.052044	4.815645
251.924794	8000.171572	13.364954	-0.052049	4.815641
251.941585	8000.160102	13.369959	-0.052052	4.815638
252.015703	8000.237124	13.374963	-0.052066	4.815660
252.176284	8000.101996	13.379968	-0.052096	4.815620
252.155407	8000.103795	13.384973	-0.052092	4.815621
252.080442	8000.125001	13.389978	-0.052078	4.815627
252.154208	8000.182797	13.394983	-0.052092	4.815644
252.021508	8000.179572	13.399987	-0.052067	4.815643
251.999221	8000.157857	13.404992	-0.052063	4.815637
252.354857	8000.140156	13.409997	-0.052129	4.815630
252.218816	8000.178521	13.415002	-0.052104	4.815642
252.023475	8000.100600	13.420007	-0.052068	4.815620
251.987065	8000.154467	13.425011	-0.052061	4.815636
252.133780	8000.110942	13.430016	-0.052088	4.815623
252.304040	8000.069937	13.435021	-0.052120	4.815610
252.311243	8000.080735	13.440026	-0.052121	4.815613
252.195669	8000.102348	13.445031	-0.052100	4.815620
252.388641	8000.151406	13.450035	-0.052136	4.815633
252.159357	8000.085746	13.455040	-0.052093	4.815615
252.243620	8000.145848	13.460045	-0.052109	4.815632
252.289071	8000.179692	13.465050	-0.052118	4.815642
252.113206	8000.143732	13.470055	-0.052085	4.815632
252.321803	8000.159943	13.475059	-0.052124	4.815636
252.251901	8000.126774	13.480064	-0.052111	4.815627
252.235509	8000.187374	13.485069	-0.052108	4.815645
252.209505	8000.164530	13.490074	-0.052103	4.815638
252.487591	8000.125280	13.495079	-0.052155	4.815625
252.389291	8000.158920	13.500083	-0.052136	4.815636
252.290760	8000.124217	13.505088	-0.052118	4.815626
252.278390	8000.113341	13.510093	-0.052116	4.815623
252.324394	8000.153601	13.515098	-0.052124	4.815634
252.233831	8000.110486	13.520103	-0.052108	4.815622
252.264229	8000.110983	13.525107	-0.052113	4.815622
252.343118	8000.104796	13.530112	-0.052128	4.815620
252.340325	8000.142125	13.535117	-0.052128	4.815631
252.219197	8000.133750	13.540122	-0.052105	4.815629
252.200480	8000.109957	13.545127	-0.052102	4.815622
252.133415	8000.149444	13.550131	-0.052089	4.815634
252.053914	8000.141747	13.555136	-0.052074	4.815632
252.129172	8000.117348	13.560141	-0.052088	4.815625
252.096646	8000.176617	13.565146	-0.052082	4.815642
252.183554	8000.094747	13.570151	-0.052099	4.815618
252.124973	8000.150389	13.575155	-0.052088	4.815634
252.166879	8000.104091	13.580160	-0.052095	4.815621
252.156605	8000.130621	13.585165	-0.052094	4.815628
252.067048	8000.106744	13.590170	-0.052077	4.815622
251.894088	8000.027052	13.595175	-0.052045	4.815599
252.204040	8000.097233	13.600179	-0.052103	4.815618
252.082052	8000.110199	13.605184	-0.052080	4.815623
252.014807	8000.141141	13.610189	-0.052067	4.815632
252.103984	8000.122308	13.615194	-0.052084	4.815626
252.161129	8000.085868	13.620199	-0.052095	4.815615
252.177628	8000.172630	13.625203	-0.052098	4.815641
252.234800	8000.136191	13.630208	-0.052108	4.815630
252.410291	8000.127304	13.635213	-0.052141	4.815626
252.366440	8000.188525	13.640218	-0.052133	4.815644
252.114762	8000.143856	13.645223	-0.052086	4.815632
252.254087	8000.183498	13.650227	-0.052112	4.815643
252.230927	8000.096634	13.655232	-0.052108	4.815618
252.284185	8000.145554	13.660237	-0.052118	4.815632
252.252811	8000.167469	13.665242	-0.052112	4.815639
252.298317	8000.162874	13.670247	-0.052121	4.815637
252.248580	8000.184491	13.675251	-0.052111	4.815644
252.163689	8000.137197	13.680256	-0.052096	4.815630
252.118779	8000.141808	13.685261	-0.052087	4.815632
252.171887	8000.196064	13.690266	-0.052097	4.815647
252.021407	8000.160517	13.695271	-0.052069	4.815638
252.342800	8000.150801	13.700275	-0.052129	4.815633
252.246162	8000.136418	13.705280	-0.052111	4.815630
252.133844	8000.208270	13.710285	-0.052090	4.815651
252.259427	8000.192164	13.715290	-0.052114	4.815646
252.221889	8000.216115	13.720295	-0.052107	4.815653
252.183843	8000.258211	13.725299	-0.052100	4.815665
252.031571	8000.233311	13.730304	-0.052071	4.815659
252.405582	8000.227656	13.735309	-0.052141	4.815656
252.331429	8000.233927	13.740314	-0.052127	4.815658
252.277065	8000.132672	13.745319	-0.052117	4.815628
252.039911	8000.182205	13.750323	-0.052073	4.815644
252.075242	8000.203071	13.755328	-0.052080	4.815650
252.167675	8000.182154	13.760333	-0.052097	4.815643
252.233195	8000.170410	13.765338	-0.052109	4.815640
252.385675	8000.141928	13.770343	-0.052137	4.815631
252.365337	8000.184312	13.775347	-0.052134	4.815643
252.239265	8000.136348	13.780352	-0.052110	4.815630
252.222143	8000.158496	13.785357	-0.052107	4.815636
252.318411	8000.149387	13.790362	-0.052125	4.815633
252.289425	8000.132902	13.795367	-0.052120	4.815628
252.436287	8000.115007	13.800371	-0.052147	4.815622
252.303849	8000.119261	13.805376	-0.052122	4.815624
252.110299	8000.166300	13.810381	-0.052086	4.815639
252.299386	8000.180058	13.815386	-0.052122	4.815642
252.331229	8000.172036	13.820391	-0.052128	4.815640
252.576857	8000.214478	13.825395	-0.052173	4.815651
252.331534	8000.180589	13.830400	-0.052128	4.815642
252.439546	8000.191960	13.835405	-0.052148	4.815645
252.495584	8000.202486	13.840410	-0.052158	4.815648
252.244036	8000.142869	13.845415	-0.052112	4.815631
252.295419	8000.203504	13.850419	-0.052121	4.815649
252.189380	8000.172951	13.855424	-0.052101	4.815641
252.364156	8000.158714	13.860429	-0.052134	4.815636
252.198573	8000.164564	13.865434	-0.052103	4.815638
252.333986	8000.139008	13.870439	-0.052128	4.815630
252.495298	8000.236670	13.875443	-0.052159	4.815658
252.150105	8000.143496	13.880448	-0.052094	4.815632
252.193471	8000.226424	13.885453	-0.052102	4.815656
252.189458	8000.200734	13.890458	-0.052102	4.815649
251.984021	8000.170699	13.895463	-0.052064	4.815641
252.171933	8000.183370	13.900467	-0.052099	4.815644
252.317571	8000.125947	13.905472	-0.052126	4.815626
252.337970	8000.183943	13.910477	-0.052130	4.815643
252.270086	8000.218078	13.915482	-0.052117	4.815653
252.219966	8000.154265	13.920487	-0.052108	4.815635
252.288133	8000.187411	13.925491	-0.052120	4.815644
252.145658	8000.147723	13.930496	-0.052094	4.815633
252.347983	8000.219357	13.935501	-0.052132	4.815653
252.369414	8000.214370	13.940506	-0.052136	4.815652
252.173109	8000.165262	13.945511	-0.052099	4.815638
252.276080	8000.224602	13.950515	-0.052118	4.815655
252.273901	8000.198942	13.955520	-0.052118	4.815648
252.260516	8000.185914	13.960525	-0.052115	4.815644
252.158381	8000.215220	13.965530	-0.052096	4.815653
252.246525	8000.169675	13.970535	-0.052113	4.815639
252.325769	8000.233967	13.975539	-0.052128	4.815658
252.106789	8000.196236	13.980544	-0.052087	4.815648
252.267194	8000.200985	13.985549	-0.052117	4.815648
252.422750	8000.236622	13.990554	-0.052146	4.815658
252.224476	8000.210974	13.995559	-0.052109	4.815651
252.261753	8000.259634	14.000563	-0.052116	4.815665
252.238695	8000.196262	14.005568	-0.052112	4.815647
252.371553	8000.219783	14.010573	-0.052136	4.815653
252.274159	8000.241692	14.015578	-0.052118	4.815660
252.304662	8000.174920	14.020583	-0.052124	4.815641
252.483462	8000.268596	14.025587	-0.052157	4.815667
252.213491	8000.225764	14.030592	-0.052107	4.815656
252.164409	8000.239917	14.035597	-0.052098	4.815660
252.127952	8000.224377	14.040602	-0.052091	4.815656
252.334809	8000.213866	14.045607	-0.052130	4.815652
252.340874	8000.242798	14.050611	-0.052131	4.815660
252.174673	8000.208061	14.055616	-0.052100	4.815651
252.241275	8000.246521	14.060621	-0.052113	4.815662
252.357760	8000.232403	14.065626	-0.052134	4.815657
252.152121	8000.177805	14.070631	-0.052096	4.815642
252.310016	8000.218818	14.075635	-0.052125	4.815653
252.423682	8000.193976	14.080640	-0.052147	4.815646
252.447446	8000.226400	14.085645	-0.052151	4.815655
252.315944	8000.210381	14.090650	-0.052127	4.815651
252.153616	8000.191724	14.095655	-0.052096	4.815646
252.317667	8000.232838	14.100659	-0.052127	4.815657
252.517323	8000.213667	14.105664	-0.052164	4.815651
252.417560	8000.246215	14.110669	-0.052146	4.815661
252.362018	8000.219687	14.115674	-0.052135	4.815653
252.211055	8000.120064	14.120679	-0.052107	4.815625
252.568638	8000.212378	14.125683	-0.052174	4.815650
252.349534	8000.232306	14.130688	-0.052133	4.815657
252.271050	8000.233167	14.135693	-0.052119	4.815658
252.441628	8000.206048	14.140698	-0.052150	4.815649
252.197595	8000.162570	14.145703	-0.052105	4.815637
252.232462	8000.226140	14.150707	-0.052111	4.815656
252.252565	8000.121827	14.155712	-0.052115	4.815625
252.292144	8000.186541	14.160717	-0.052123	4.815644
252.141163	8000.174477	14.165722	-0.052095	4.815641
252.169431	8000.154652	14.170727	-0.052100	4.815635
252.396201	8000.188243	14.175731	-0.052142	4.815644
252.291383	8000.160913	14.180736	-0.052123	4.815636
252.288638	8000.176888	14.185741	-0.052122	4.815641
252.372931	8000.213500	14.190746	-0.052138	4.815651
252.250920	8000.180551	14.195751	-0.052115	4.815642
252.314649	8000.224303	14.200755	-0.052127	4.815655
252.361296	8000.185557	14.205760	-0.052136	4.815643
252.406529	8000.169211	14.210765	-0.052144	4.815638
252.253692	8000.230794	14.215770	-0.052116	4.815657
252.279035	8000.178887	14.220775	-0.052121	4.815642
252.447880	8000.227553	14.225779	-0.052152	4.815655
252.240538	8000.202825	14.230784	-0.052113	4.815649
252.359448	8000.184476	14.235789	-0.052136	4.815643
252.394749	8000.258731	14.240794	-0.052142	4.815665
252.223503	8000.258082	14.245799	-0.052110	4.815665
252.383570	7999.251651	14.250803	-0.052140	4.815370

252.162910	7996.025981	14.255808	-0.052096	4.814428
252.424502	7990.579270	14.260813	-0.052142	4.812834
252.304643	7983.898242	14.265818	-0.052115	4.810879
252.139657	7976.629613	14.270823	-0.052080	4.808752
252.144183	7968.969365	14.275827	-0.052075	4.806509
252.156386	7961.174334	14.280832	-0.052073	4.804225
252.259767	7953.406755	14.285837	-0.052087	4.801947
252.216417	7945.397992	14.290842	-0.052074	4.799598
252.125990	7937.419072	14.295847	-0.052052	4.797258
252.035930	7929.454726	14.300851	-0.052030	4.794920
251.871986	7921.401857	14.305856	-0.051994	4.792555
251.969236	7913.380104	14.310861	-0.052007	4.790197
251.930691	7905.435746	14.315866	-0.051995	4.787862
251.703248	7897.351560	14.320871	-0.051947	4.785485
251.901213	7889.439534	14.325875	-0.051979	4.783155
252.155080	7881.379399	14.330880	-0.052021	4.780781
251.932230	7873.412240	14.335885	-0.051974	4.778435
251.994729	7865.453860	14.340890	-0.051981	4.776089
252.109131	7857.351855	14.345895	-0.051997	4.773700
252.079096	7849.379000	14.350899	-0.051986	4.771347
251.883660	7841.334021	14.355904	-0.051944	4.768973
252.140397	7833.389559	14.360909	-0.051987	4.766626
251.958275	7825.343278	14.365914	-0.051948	4.764250
251.628560	7817.429209	14.370919	-0.051881	4.761911
251.644245	7809.417657	14.375923	-0.051879	4.759542
251.480269	7801.381669	14.380928	-0.051843	4.757164
251.387612	7793.395906	14.385933	-0.051821	4.754800
251.495773	7785.333139	14.390938	-0.051836	4.752412
251.622519	7777.327254	14.395943	-0.051854	4.750038
251.588858	7769.364670	14.400947	-0.051843	4.747678
251.394752	7761.299170	14.405952	-0.051801	4.745286
251.508824	7753.351413	14.410957	-0.051818	4.742926
251.483288	7745.343100	14.415962	-0.051808	4.740548
251.269208	7737.377926	14.420967	-0.051763	4.738182
251.506956	7729.364511	14.425971	-0.051802	4.735800
251.427319	7721.289054	14.430976	-0.051782	4.733398
251.339456	7713.311014	14.435981	-0.051760	4.731025
251.108148	7705.350388	14.440986	-0.051712	4.728655
251.397237	7697.316768	14.445991	-0.051760	4.726262
251.340991	7689.324940	14.450995	-0.051745	4.723880
251.016933	7681.299287	14.456000	-0.051679	4.721488
251.159509	7673.314174	14.461005	-0.051701	4.719106
251.243044	7665.430867	14.466010	-0.051711	4.716753
251.036714	7657.302480	14.471015	-0.051667	4.714326
251.034943	7649.330395	14.476019	-0.051662	4.711944
251.081589	7641.253081	14.481024	-0.051665	4.709530
250.916409	7633.321310	14.486029	-0.051629	4.707158
250.996246	7625.304623	14.491034	-0.051639	4.704759
250.966370	7617.330852	14.496039	-0.051628	4.702372
250.982478	7609.295815	14.501043	-0.051626	4.699965
250.912633	7601.319526	14.506048	-0.051608	4.697575
250.985567	7593.313898	14.511053	-0.051616	4.695174
250.914464	7585.337458	14.516058	-0.051598	4.692782
250.718035	7577.239576	14.521063	-0.051556	4.690351
250.918815	7569.309399	14.526067	-0.051588	4.687970
250.989944	7561.250519	14.531072	-0.051596	4.685548
250.994992	7553.313791	14.536077	-0.051592	4.683162
250.806970	7545.336510	14.541082	-0.051552	4.680763
250.677011	7537.274492	14.546087	-0.051523	4.678338
250.907255	7529.316959	14.551091	-0.051560	4.675942
250.573783	7521.218828	14.556096	-0.051493	4.673503
250.568670	7513.168997	14.561101	-0.051487	4.671076
250.545915	7505.196774	14.566106	-0.051477	4.668673
250.472383	7497.180876	14.571111	-0.051459	4.666254
250.391703	7489.253931	14.576115	-0.051438	4.663862
250.414454	7481.281871	14.581120	-0.051438	4.661454
250.409367	7473.209506	14.586125	-0.051431	4.659015
250.320864	7465.279441	14.591130	-0.051410	4.656617
250.243250	7457.217332	14.596135	-0.051390	4.654179
250.258400	7449.246390	14.601139	-0.051388	4.651766
250.097419	7441.155408	14.606144	-0.051353	4.649316
250.155783	7433.233128	14.611149	-0.051358	4.646916
250.311145	7425.210128	14.616154	-0.051382	4.644484
250.213133	7417.264828	14.621159	-0.051359	4.642075
250.073686	7409.234128	14.626163	-0.051327	4.639638
250.247968	7401.254532	14.631168	-0.051355	4.637215
250.193993	7393.220114	14.636173	-0.051339	4.634775
250.037794	7385.200086	14.641178	-0.051305	4.632337
249.900740	7377.144339	14.646183	-0.051274	4.629888
250.020444	7369.196791	14.651187	-0.051292	4.627470
249.953957	7361.174255	14.656192	-0.051274	4.625028
250.134304	7353.236080	14.661197	-0.051302	4.622610
250.165593	7345.197455	14.666202	-0.051303	4.620161
249.967965	7337.187606	14.671207	-0.051261	4.617719
250.025342	7329.217901	14.676211	-0.051267	4.615288
249.850103	7321.196172	14.681216	-0.051229	4.612839
249.909779	7313.145989	14.686221	-0.051235	4.610381
249.842610	7305.168598	14.691226	-0.051217	4.607944
249.849421	7297.147419	14.696231	-0.051213	4.605492
249.890610	7289.207022	14.701235	-0.051216	4.603063
249.662684	7281.178296	14.706240	-0.051168	4.600606
249.691581	7273.194393	14.711245	-0.051168	4.598161
249.958120	7265.166490	14.716250	-0.051213	4.595702
249.752800	7257.093695	14.721255	-0.051169	4.593228
249.776223	7249.109378	14.726259	-0.051168	4.590779
249.683359	7241.115322	14.731264	-0.051146	4.588326
249.860605	7233.097519	14.736269	-0.051174	4.585865
249.845908	7225.143370	14.741274	-0.051166	4.583422
249.335049	7217.097308	14.746279	-0.051065	4.580948
249.657149	7209.145777	14.751283	-0.051120	4.578503
249.468919	7201.160373	14.756288	-0.051080	4.576046
249.555944	7193.140930	14.761293	-0.051091	4.573578
249.437784	7185.091030	14.766298	-0.051064	4.571098
249.514154	7177.084344	14.771303	-0.051073	4.568631
249.301020	7169.118501	14.776307	-0.051028	4.566175
249.184263	7161.102015	14.781312	-0.051001	4.563701
249.298287	7153.145580	14.786317	-0.051017	4.561246
249.431662	7145.146820	14.791322	-0.051037	4.558776
249.133688	7137.161409	14.796327	-0.050976	4.556308
249.252632	7129.139076	14.801331	-0.050993	4.553827
249.162401	7121.103959	14.806336	-0.050971	4.551342
249.187145	7113.093856	14.811341	-0.050971	4.548863
249.489862	7105.156165	14.816346	-0.051022	4.546405
249.156451	7097.093236	14.821351	-0.050954	4.543906
249.253846	7089.157235	14.826355	-0.050967	4.541446
249.153492	7081.109962	14.831360	-0.050944	4.538950
249.297516	7073.160192	14.836365	-0.050965	4.536483
249.007583	7065.107896	14.841370	-0.050906	4.533982
248.992508	7057.104576	14.846375	-0.050898	4.531495
249.063714	7049.121146	14.851379	-0.050906	4.529013
248.892399	7041.130708	14.856384	-0.050869	4.526527
248.702325	7033.125814	14.861389	-0.050828	4.524036
248.733877	7025.176914	14.866394	-0.050829	4.521561
248.854079	7017.079426	14.871399	-0.050846	4.519038
248.951926	7009.126763	14.876403	-0.050859	4.516559
248.666744	7001.034364	14.881408	-0.050801	4.514034
248.515461	6992.994535	14.886413	-0.050768	4.511525
248.508377	6985.051008	14.891418	-0.050761	4.509045
248.448171	6977.045382	14.896423	-0.050745	4.506543
248.655389	6969.086842	14.901427	-0.050778	4.504056
248.422374	6961.097612	14.906432	-0.050730	4.501556
248.307808	6953.068960	14.911437	-0.050703	4.499044
248.526208	6945.089611	14.916442	-0.050739	4.496546
248.583147	6937.050393	14.921447	-0.050744	4.494027
248.590738	6929.075883	14.926451	-0.050740	4.491527
248.291334	6921.042166	14.931456	-0.050679	4.489007
248.427710	6913.054465	14.936461	-0.050700	4.486500
248.347847	6905.058483	14.941466	-0.050680	4.483989
248.127600	6897.051594	14.946471	-0.050633	4.481473
248.210342	6889.072889	14.951475	-0.050644	4.478965
248.351747	6881.093034	14.956480	-0.050665	4.476456
247.985490	6873.013106	14.961485	-0.050591	4.473911
248.241006	6865.028102	14.966490	-0.050634	4.471398
248.011195	6857.006463	14.971495	-0.050586	4.468870
248.188545	6849.026330	14.976499	-0.050614	4.466355
248.057838	6841.028529	14.981504	-0.050584	4.463831
248.109155	6833.016321	14.986509	-0.050588	4.461303
248.342828	6825.037066	14.991514	-0.050627	4.458784
247.914975	6817.032869	14.996519	-0.050542	4.456253
247.926941	6809.020968	15.001523	-0.050539	4.453720
247.926282	6800.978269	15.006528	-0.050534	4.451176
248.016819	6793.025774	15.011533	-0.050545	4.448660
248.012154	6785.019869	15.016538	-0.050539	4.446124
247.952671	6776.979871	15.021543	-0.050523	4.443576
247.980825	6769.035867	15.026547	-0.050523	4.441058
247.793695	6761.020609	15.031552	-0.050483	4.438514
247.934081	6753.062505	15.036557	-0.050504	4.435989
247.863042	6745.015558	15.041562	-0.050486	4.433433
247.657198	6736.942803	15.046567	-0.050442	4.430867
247.713761	6728.966228	15.051571	-0.050447	4.428331
247.718419	6720.939052	15.056576	-0.050443	4.425777
247.511645	6712.982409	15.061581	-0.050399	4.423243
247.539352	6705.023942	15.066586	-0.050399	4.420708
247.486304	6696.979213	15.071591	-0.050384	4.418144
247.585409	6688.988706	15.076595	-0.050398	4.415597
247.411586	6680.981616	15.081600	-0.050360	4.413041
247.493810	6672.911641	15.086605	-0.050370	4.410465
247.722808	6664.972974	15.091610	-0.050408	4.407930
247.629479	6656.947347	15.096615	-0.050385	4.405365
247.532306	6649.046543	15.101619	-0.050362	4.402837
247.439396	6641.005897	15.106624	-0.050339	4.400264
247.498666	6633.026905	15.111629	-0.050345	4.397710
247.417459	6625.003287	15.116634	-0.050325	4.395139
247.264308	6616.958380	15.121639	-0.050291	4.392559
247.377470	6608.926288	15.126643	-0.050307	4.389983
247.303358	6600.978992	15.131648	-0.050288	4.387432
247.308771	6592.967879	15.136653	-0.050284	4.384860
247.307454	6585.038332	15.141658	-0.050279	4.382312
247.336373	6576.980828	15.146663	-0.050279	4.379721
247.282664	6569.027595	15.151667	-0.050264	4.377163
247.018928	6561.013123	15.156672	-0.050209	4.374581
247.118100	6552.973436	15.161677	-0.050223	4.371993
247.102577	6544.956147	15.166682	-0.050214	4.369409
247.027828	6536.973785	15.171687	-0.050195	4.366834
247.151291	6528.970089	15.176691	-0.050213	4.364253
247.118097	6521.008949	15.181696	-0.050202	4.361683
247.019670	6512.972648	15.186701	-0.050178	4.359086
246.921039	6505.061888	15.191706	-0.050155	4.356528
246.798069	6496.934350	15.196711	-0.050127	4.353899
246.717727	6488.895786	15.201715	-0.050106	4.351297
246.745576	6480.904193	15.206720	-0.050106	4.348710
246.823188	6472.931737	15.211725	-0.050116	4.346127
246.508719	6464.951000	15.216730	-0.050052	4.343538
246.605875	6456.955900	15.221735	-0.050065	4.340945
246.836775	6448.990590	15.226739	-0.050103	4.338361
246.665028	6440.966502	15.231744	-0.050066	4.335754
246.643328	6432.932545	15.236749	-0.050056	4.333143
246.581787	6424.926393	15.241754	-0.050040	4.330539
246.486306	6416.939266	15.246759	-0.050017	4.327940
246.547718	6408.946785	15.251763	-0.050023	4.325338
246.369071	6400.985557	15.256768	-0.049985	4.322744
246.453114	6392.957179	15.261773	-0.049995	4.320127
246.360893	6385.018998	15.266778	-0.049973	4.317538
246.370440	6376.919746	15.271783	-0.049969	4.314895
246.439959	6368.916781	15.276787	-0.049977	4.312282
246.411352	6360.879866	15.281792	-0.049967	4.309656
246.336037	6352.939660	15.286797	-0.049947	4.307059
246.407929	6344.939723	15.291802	-0.049956	4.304443
246.330067	6336.955845	15.296807	-0.049936	4.301828
246.163641	6328.923732	15.301811	-0.049900	4.299196
246.209395	6320.943822	15.306816	-0.049903	4.296581
246.405273	6312.946991	15.311821	-0.049934	4.293960
246.333604	6304.893111	15.316826	-0.049916	4.291317
246.069255	6296.881352	15.321831	-0.049861	4.288684
246.146995	6288.917329	15.326835	-0.049871	4.286068
246.095208	6280.886424	15.331840	-0.049856	4.283428
245.932756	6272.916455	15.336845	-0.049820	4.280805
246.172905	6264.958162	15.341850	-0.049860	4.278187
246.041162	6256.919521	15.346855	-0.049830	4.275538
246.013541	6248.907829	15.351859	-0.049820	4.272898
245.887927	6240.877184	15.356864	-0.049791	4.270248
246.094407	6232.890079	15.361869	-0.049825	4.267615
245.943755	6224.902231	15.366874	-0.049791	4.264976
245.792034	6216.875025	15.371879	-0.049758	4.262323
246.061916	6208.865078	15.376883	-0.049803	4.259677
245.995606	6200.926724	15.381888	-0.049785	4.257051
245.827076	6192.866930	15.386893	-0.049749	4.254381
245.611220	6184.892733	15.391898	-0.049704	4.251738
245.702442	6176.849120	15.396903	-0.049715	4.249073
245.617479	6168.955693	15.401907	-0.049694	4.246455
245.395415	6160.883876	15.406912	-0.049648	4.243774
245.683725	6152.930587	15.411917	-0.049696	4.241136
245.752560	6144.980902	15.416922	-0.049704	4.238496
245.518314	6136.961328	15.421927	-0.049655	4.235827
245.810979	6128.939138	15.426931	-0.049704	4.233161
245.405432	6120.879453	15.431936	-0.049624	4.230474
245.255212	6112.887833	15.436941	-0.049591	4.227811
245.579212	6104.924746	15.441946	-0.049646	4.225160
245.543645	6096.952907	15.446951	-0.049634	4.222501
245.331147	6088.925012	15.451955	-0.049589	4.219820
245.499825	6080.967458	15.456960	-0.049615	4.217164
245.388011	6072.915954	15.461965	-0.049589	4.214473
245.267891	6064.932441	15.466970	-0.049562	4.211802
245.028159	6056.878433	15.471975	-0.049512	4.209105
245.244102	6048.934924	15.476979	-0.049547	4.206448
245.245405	6040.922913	15.481984	-0.049542	4.203764
245.087060	6032.924751	15.486989	-0.049508	4.201081
245.025538	6024.973380	15.491994	-0.049491	4.198414
245.111246	6016.933161	15.496999	-0.049502	4.195716
245.204056	6008.862547	15.502003	-0.049514	4.193006
244.959876	6000.807007	15.507008	-0.049463	4.190296
245.235207	5992.834673	15.512013	-0.049509	4.187618
245.115810	5984.891285	15.517018	-0.049482	4.184944
244.967687	5976.906699	15.522023	-0.049449	4.182254
244.896751	5968.920150	15.527027	-0.049431	4.179562
244.825417	5960.912877	15.532032	-0.049412	4.176862
244.708010	5952.872574	15.537037	-0.049385	4.174148
244.854055	5944.891607	15.542042	-0.049407	4.171455
244.950354	5936.864755	15.547047	-0.049420	4.168744
244.828886	5928.906779	15.552051	-0.049392	4.166053
244.700076	5920.928417	15.557056	-0.049363	4.163353
244.612429	5912.888417	15.562061	-0.049341	4.160630
244.797293	5904.917139	15.567066	-0.049371	4.157933
244.607797	5896.896700	15.572071	-0.049330	4.155212
244.769142	5888.885953	15.577075	-0.049355	4.152497
244.640113	5880.842726	15.582080	-0.049326	4.149766
244.416865	5872.869747	15.587085	-0.049279	4.147056
244.509729	5864.873443	15.592090	-0.049291	4.144340
244.461649	5856.921325	15.597095	-0.049277	4.141635
244.514382	5848.893775	15.602099	-0.049282	4.138904
244.424534	5840.936217	15.607104	-0.049260	4.136194
244.334447	5832.867593	15.612109	-0.049238	4.133444
244.417959	5824.841098	15.617114	-0.049248	4.130708
243.970624	5816.849357	15.622119	-0.049160	4.127976
244.359205	5808.870782	15.627123	-0.049227	4.125257
244.306751	5800.880714	15.632128	-0.049212	4.122527
244.351000	5792.859512	15.637133	-0.049215	4.119785
244.169486	5784.931439	15.642138	-0.049176	4.117071
244.231571	5776.889214	15.647143	-0.049182	4.114319
244.348636	5768.834790	15.652147	-0.049199	4.111562
244.087695	5760.837386	15.657152	-0.049145	4.108817
244.014411	5752.885609	15.662157	-0.049126	4.106089
243.923774	5744.854343	15.667162	-0.049104	4.103331
243.798177	5736.863488	15.672167	-0.049076	4.100585
243.781454	5728.941942	15.677171	-0.049068	4.097862
243.994795	5720.903297	15.682176	-0.049102	4.095101
244.088431	5712.881017	15.687181	-0.049114	4.092341
243.975382	5704.905762	15.692186	-0.049088	4.089593
243.724682	5696.924144	15.697191	-0.049036	4.086839
243.741409	5688.929271	15.702195	-0.049034	4.084083
243.814995	5680.939340	15.707200	-0.049043	4.081326
243.781629	5672.937373	15.712205	-0.049031	4.078563
243.697544	5664.972696	15.717210	-0.049010	4.075810
243.532427	5656.895771	15.722215	-0.048974	4.073014
243.717281	5648.912177	15.727219	-0.049004	4.070255
243.887718	5640.901167	15.732224	-0.049030	4.067483
243.735876	5632.886246	15.737229	-0.048997	4.064704
243.534851	5624.956314	15.742234	-0.048954	4.061952
243.436660	5616.912454	15.747239	-0.048931	4.059159
243.683071	5608.961426	15.752243	-0.048972	4.056402
243.509914	5600.936218	15.757248	-0.048934	4.053611
243.480643	5592.894422	15.762253	-0.048923	4.050815
243.662416	5584.915682	15.767258	-0.048952	4.048042
243.385021	5576.941168	15.772263	-0.048895	4.045261
243.368232	5568.971027	15.777267	-0.048887	4.042484
243.530392	5560.914583	15.782272	-0.048912	4.039678
243.499872	5552.945302	15.787277	-0.048901	4.036897
243.253860	5544.941657	15.792282	-0.048850	4.034099
243.445342	5536.748744	15.797287	-0.048880	4.031240
243.573801	5528.844614	15.802291	-0.048899	4.028478
243.315114	5520.877137	15.807296	-0.048846	4.025687
243.086660	5512.909516	15.812301	-0.048798	4.022894
243.142323	5504.905608	15.817306	-0.048803	4.020091
243.058863	5496.941914	15.822311	-0.048783	4.017298
242.998838	5488.929384	15.827315	-0.048766	4.014486
242.987067	5480.880342	15.832320	-0.048759	4.011660
243.137266	5472.880352	15.837325	-0.048782	4.008851
243.084644	5464.923456	15.842330	-0.048767	4.006053
242.752935	5456.890748	15.847335	-0.048700	4.003222
242.848671	5448.904723	15.852339	-0.048712	4.000412
242.755061	5440.966578	15.857344	-0.048690	3.997613
242.619000	5432.919137	15.862349	-0.048659	3.994774
242.805183	5424.877689	15.867354	-0.048689	3.991940
242.734980	5416.861686	15.872359	-0.048671	3.989108
242.680350	5408.931952	15.877363	-0.048655	3.986306
242.715888	5400.899466	15.882368	-0.048657	3.983466
242.630591	5392.891585	15.887373	-0.048636	3.980632
242.634524	5384.944313	15.892378	-0.048631	3.977818
242.530354	5376.932023	15.897383	-0.048607	3.974977
242.726029	5368.918346	15.902387	-0.048638	3.972139
242.713180	5360.892976	15.907392	-0.048630	3.969291
242.519036	5352.950592	15.912397	-0.048589	3.966467
242.460942	5344.962635	15.917402	-0.048573	3.963628
242.595406	5336.929913	15.922407	-0.048593	3.960774
242.321956	5328.988427	15.927411	-0.048537	3.957943
242.441827	5320.993340	15.932416	-0.048554	3.955098
242.185622	5312.930337	15.937421	-0.048501	3.952220
242.257929	5304.916756	15.942426	-0.048509	3.949363
242.295628	5296.940382	15.947431	-0.048511	3.946517
242.449157	5288.924718	15.952435	-0.048534	3.943657
242.242803	5280.952710	15.957440	-0.048491	3.940804
242.102774	5272.953606	15.962445	-0.048460	3.937941
242.378781	5265.005025	15.967450	-0.048506	3.935101
242.241790	5256.953805	15.972455	-0.048475	3.932215
242.135960	5248.959234	15.977459	-0.048450	3.929347
242.108759	5240.984853	15.982464	-0.048440	3.926486
242.060848	5232.946931	15.987469	-0.048426	3.923600
242.009113	5225.013314	15.992474	-0.048411	3.920749
241.753833	5217.022966	15.997479	-0.048358	3.917871
241.837558	5209.003014	16.002483	-0.048369	3.914988
241.982024	5200.912139	16.007488	-0.048390	3.912077
241.822617	5192.925206	16.012493	-0.048356	3.909197
241.905034	5184.987097	16.017498	-0.048366	3.906336
241.660584	5176.993936	16.022503	-0.048315	3.903447
241.835259	5168.977142	16.027507	-0.048342	3.900556
241.789501	5160.997640	16.032512	-0.048329	3.897671
241.718838	5152.985684	16.037517	-0.048310	3.894772
241.662483	5144.979837	16.042522	-0.048295	3.891874
241.703259	5136.940372	16.047527	-0.048297	3.888963
241.675784	5128.976844	16.052531	-0.048287	3.886076
241.725109	5121.002248	16.057536	-0.048291	3.883184
241.655336	5112.975475	16.062541	-0.048273	3.880269
241.540132	5105.031955	16.067546	-0.048246	3.877382
241.517153	5096.966674	16.072551	-0.048237	3.874449
241.438199	5088.748423	16.077555	-0.048217	3.871458
241.389838	5080.809187	16.082560	-0.048202	3.868566
241.321081	5072.851330	16.087565	-0.048184	3.865665
241.604630	5064.940969	16.092570	-0.048232	3.862786
241.445401	5056.933280	16.097575	-0.048197	3.859861
241.383853	5048.974208	16.102579	-0.048181	3.856953
241.267529	5040.946495	16.107584	-0.048154	3.854017
241.285948	5032.969527	16.112589	-0.048152	3.851100
241.198285	5024.986606	16.117594	-0.048131	3.848176
241.272758	5016.953024	16.122599	-0.048139	3.845235
241.392945	5009.002172	16.127603	-0.048157	3.842322
241.087888	5001.026790	16.132608	-0.048095	3.839390
241.170113	4993.061270	16.137613	-0.048105	3.836467
241.153306	4985.013973	16.142618	-0.048096	3.833510
240.911056	4976.990809	16.147623	-0.048046	3.830555
241.101881	4969.015390	16.152627	-0.048076	3.827624
241.078839	4961.005707	16.157632	-0.048067	3.824674
240.946290	4953.047460	16.162637	-0.048037	3.821738
240.933274	4945.107119	16.167642	-0.048030	3.818809
240.885222	4937.086981	16.172647	-0.048015	3.815847
240.790397	4929.054691	16.177651	-0.047993	3.812878
240.635439	4921.061750	16.182656	-0.047959	3.809919
240.595095	4913.054903	16.187661	-0.047946	3.806956
240.794089	4905.043661	16.192666	-0.047978	3.803994
240.485139	4897.072651	16.197671	-0.047915	3.801033
240.705307	4889.112126	16.202675	-0.047951	3.798086
240.612913	4881.088741	16.207680	-0.047928	3.795106
240.502341	4873.049259	16.212685	-0.047903	3.792117
240.446156	4865.039794	16.217690	-0.047887	3.789138
240.672316	4857.029015	16.222695	-0.047924	3.786163
240.644168	4849.070698	16.227699	-0.047914	3.783199
240.318585	4841.106373	16.232704	-0.047848	3.780225
240.512065	4833.061079	16.237709	-0.047879	3.777229
240.572351	4825.083669	16.242714	-0.047885	3.774253
240.369415	4817.070861	16.247719	-0.047842	3.771255
240.373028	4809.080323	16.252723	-0.047837	3.768268
240.334616	4801.082843	16.257728	-0.047825	3.765276
240.257109	4793.057466	16.262733	-0.047805	3.762269
240.125856	4785.118472	16.267738	-0.047776	3.759291
240.256742	4777.097260	16.272743	-0.047795	3.756287
240.110214	4769.091267	16.277747	-0.047762	3.753279
240.096430	4761.078537	16.282752	-0.047755	3.750269
240.045093	4753.136026	16.287757	-0.047740	3.747282
240.067481	4745.118124	16.292762	-0.047739	3.744266
239.938672	4737.131900	16.297767	-0.047710	3.741256
239.809412	4729.109956	16.302771	-0.047680	3.738230
240.007247	4721.137669	16.307776	-0.047712	3.735228
239.950445	4713.102646	16.312781	-0.047696	3.732194
239.841605	4705.122102	16.317786	-0.047671	3.729177
239.661994	4697.129459	16.322791	-0.047632	3.726151
239.964083	4689.131625	16.327795	-0.047683	3.723133
239.754787	4681.177005	16.332800	-0.047639	3.720116
239.689189	4673.214769	16.337805	-0.047622	3.717097
239.765366	4665.165979	16.342810	-0.047631	3.714046
239.499631	4657.048848	16.347815	-0.047576	3.710958
239.495910	4649.094948	16.352819	-0.047570	3.707936
239.497036	4641.103723	16.357824	-0.047565	3.704898
239.367978	4633.143946	16.362829	-0.047536	3.701866
239.328104	4625.189840	16.367834	-0.047523	3.698836
239.341874	4617.178989	16.372839	-0.047521	3.695783
239.267589	4609.183820	16.377843	-0.047502	3.692731
239.063334	4601.166270	16.382848	-0.047459	3.689665
238.916253	4593.190901	16.387853	-0.047426	3.686614
239.079795	4585.226083	16.392858	-0.047451	3.683572
239.209415	4577.199914	16.397863	-0.047470	3.680503
238.965365	4569.241978	16.402867	-0.047420	3.677449
238.988496	4561.198816	16.407872	-0.047419	3.674366
239.259054	4553.167757	16.412877	-0.047464	3.671291
238.970642	4545.227249	16.417882	-0.047405	3.668235
238.930437	4537.188238	16.422887	-0.047392	3.665144
239.121274	4529.232069	16.427891	-0.047423	3.662088
239.006882	4521.205908	16.432896	-0.047396	3.658995
238.861134	4513.238938	16.437901	-0.047364	3.655922
238.978641	4505.238111	16.442906	-0.047381	3.652839
238.822481	4497.177020	16.447911	-0.047346	3.649724
239.041732	4489.231218	16.452915	-0.047382	3.646660
239.121413	4481.228965	16.457920	-0.047392	3.643569
238.910268	4473.248713	16.462925	-0.047347	3.640475
238.902616	4465.310410	16.467930	-0.047341	3.637400
238.732413	4457.264516	16.472935	-0.047304	3.634277
238.669384	4449.249531	16.477939	-0.047287	3.631166
238.530068	4441.241149	16.482944	-0.047256	3.628053
238.523406	4433.207136	16.487949	-0.047249	3.624930
238.656998	4425.273709	16.492954	-0.047269	3.621848
238.531446	4417.262611	16.497959	-0.047240	3.618726
238.378560	4409.291655	16.502963	-0.047207	3.615617
238.358469	4401.291823	16.507968	-0.047198	3.612496
238.450531	4393.270170	16.512973	-0.047210	3.609368
238.307374	4385.326497	16.517978	-0.047178	3.606261
238.194418	4377.309364	16.522983	-0.047152	3.603124
238.212459	4369.328176	16.527987	-0.047150	3.600001
238.145011	4361.363232	16.532992	-0.047132	3.596880
238.006616	4353.353818	16.537997	-0.047101	3.593736
238.194110	4345.327179	16.543002	-0.047131	3.590592
238.313672	4337.337835	16.548007	-0.047148	3.587458
238.113522	4329.337319	16.553011	-0.047106	3.584308
238.118023	4321.377444	16.558016	-0.047101	3.581177
238.036021	4313.386454	16.563021	-0.047081	3.578029
238.131827	4305.387961	16.568026	-0.047094	3.574879
237.968259	4297.362475	16.573031	-0.047058	3.571709
238.019136	4289.401163	16.578035	-0.047062	3.568568
237.999078	4281.407051	16.583040	-0.047053	3.565409
237.859286	4273.392584	16.588045	-0.047022	3.562235
238.077913	4265.415548	16.593050	-0.047058	3.559084
238.020256	4257.437641	16.598055	-0.047042	3.555922
237.816145	4249.363652	16.603059	-0.046999	3.552714
237.716444	4241.324642	16.608064	-0.046975	3.549521
237.762336	4233.335440	16.613069	-0.046978	3.546349
237.825495	4225.390536	16.618074	-0.046985	3.543192
237.619272	4217.396103	16.623079	-0.046941	3.540004
237.695523	4209.415872	16.628083	-0.046950	3.536828
237.669098	4201.429410	16.633088	-0.046940	3.533643
237.497889	4193.408742	16.638093	-0.046903	3.530437
237.684748	4185.421363	16.643098	-0.046933	3.527253
237.607376	4177.417533	16.648103	-0.046913	3.524051
237.453505	4169.480675	16.653107	-0.046879	3.520871
237.380221	4161.484115	16.658112	-0.046860	3.517666
237.324685	4153.476391	16.663117	-0.046845	3.514454
237.414504	4145.481943	16.668122	-0.046856	3.511250
237.232857	4137.449652	16.673127	-0.046817	3.508018
237.311414	4129.469160	16.678131	-0.046827	3.504813
237.344868	4121.507969	16.683136	-0.046828	3.501611
237.380674	4113.488772	16.688141	-0.046829	3.498383
237.278413	4105.537274	16.693146	-0.046805	3.495175
237.242043	4097.502897	16.698151	-0.046793	3.491932
237.257579	4089.511352	16.703155	-0.046791	3.488706
237.036991	4081.541874	16.708160	-0.046745	3.485477
237.027613	4073.580233	16.713165	-0.046738	3.482256
237.105496	4065.575160	16.718170	-0.046747	3.479017
236.886291	4057.592536	16.723175	-0.046701	3.475775
236.847331	4049.579334	16.728179	-0.046689	3.472522
236.976153	4041.511916	16.733184	-0.046707	3.469251
236.771449	4033.540042	16.738189	-0.046664	3.466004
236.643610	4025.598746	16.743194	-0.046635	3.462769
236.625056	4017.586453	16.748199	-0.046627	3.459505
236.667322	4009.615133	16.753203	-0.046629	3.456257
236.552872	4001.613417	16.758208	-0.046603	3.452989
236.496436	3993.571103	16.763213	-0.046587	3.449703
236.473627	3985.636823	16.768218	-0.046578	3.446459
236.255327	3977.612230	16.773223	-0.046532	3.443168
236.428980	3969.640539	16.778227	-0.046559	3.439909
236.733186	3961.636773	16.783232	-0.046611	3.436638
236.509344	3953.646315	16.788237	-0.046564	3.433352
236.343226	3945.630783	16.793242	-0.046528	3.430054
236.445294	3937.624585	16.798247	-0.046541	3.426766
236.646288	3929.640649	16.803251	-0.046574	3.423487
236.305469	3921.717991	16.808256	-0.046505	3.420212
236.157227	3913.707718	16.813261	-0.046472	3.416905
236.422160	3905.696791	16.818266	-0.046516	3.413607
236.322269	3897.682201	16.823271	-0.046493	3.410293
236.334882	3889.709869	16.828275	-0.046490	3.406997
236.311926	3881.742937	16.833280	-0.046480	3.403698
236.224070	3873.755272	16.838285	-0.046459	3.400386
236.016951	3865.807241	16.843290	-0.046415	3.397083
235.951788	3857.750646	16.848295	-0.046398	3.393736
235.922222	3849.665998	16.853299	-0.046387	3.390375
235.854880	3841.715602	16.858304	-0.046369	3.387066
235.819899	3833.726059	16.863309	-0.046358	3.383738
236.066915	3825.759449	16.868314	-0.046398	3.380427
235.859862	3817.800179	16.873319	-0.046355	3.377099
235.892242	3809.801587	16.878323	-0.046356	3.373760
235.788915	3801.795598	16.883328	-0.046331	3.370410
235.957168	3793.779635	16.888333	-0.046357	3.367062
235.814775	3785.842134	16.893338	-0.046326	3.363732
235.700537	3777.831997	16.898343	-0.046299	3.360370
235.750206	3769.856727	16.903347	-0.046303	3.357025
235.622379	3761.859384	16.908352	-0.046274	3.353660
235.399763	3753.825637	16.913357	-0.046228	3.350274
235.417911	3745.843761	16.918362	-0.046226	3.346915
235.524170	3737.845212	16.923367	-0.046240	3.343548
235.567249	3729.851293	16.928371	-0.046243	3.340178
235.485683	3721.915464	16.933376	-0.046223	3.336824
235.587637	3713.859396	16.938381	-0.046237	3.333423
235.539087	3705.884429	16.943386	-0.046223	3.330047
235.435550	3697.915771	16.948391	-0.046198	3.326669
235.696602	3689.920982	16.953395	-0.046242	3.323289
235.545629	3681.957294	16.958400	-0.046208	3.319904
235.251676	3673.998278	16.963405	-0.046148	3.316512
235.373728	3665.971088	16.968410	-0.046166	3.313103
235.166993	3657.928504	16.973415	-0.046122	3.309672
234.971034	3649.973224	16.978419	-0.046081	3.306274
235.012424	3641.990432	16.983424	-0.046083	3.302871
235.132445	3633.974485	16.988429	-0.046100	3.299452
235.190699	3626.031450	16.993434	-0.046106	3.296059
234.880891	3618.043537	16.998439	-0.046043	3.292629
235.028845	3610.004006	17.003443	-0.046065	3.289192
235.144497	3602.016476	17.008448	-0.046082	3.285771
234.827902	3594.051522	17.013453	-0.046018	3.282340
234.992453	3586.075482	17.018458	-0.046043	3.278919
235.174416	3578.072017	17.023463	-0.046072	3.275484
234.919488	3570.070908	17.028467	-0.046019	3.272029
234.922710	3562.072244	17.033472	-0.046015	3.268581
234.935440	3554.066691	17.038477	-0.046012	3.265127
234.877474	3546.146864	17.043482	-0.045996	3.261704
234.662761	3538.130681	17.048487	-0.045951	3.258229
234.639823	3530.135821	17.053491	-0.045941	3.254767
234.575675	3522.156155	17.058496	-0.045924	3.251307
234.418478	3514.151880	17.063501	-0.045890	3.247828
234.565969	3506.139599	17.068506	-0.045912	3.244355
234.594754	3498.172664	17.073511	-0.045912	3.240893
234.447459	3490.191137	17.078515	-0.045880	3.237413
234.442907	3482.182790	17.083520	-0.045874	3.233924
234.575172	3474.082343	17.088525	-0.045893	3.230396
234.429508	3466.150992	17.093530	-0.045861	3.226928
234.283098	3458.186193	17.098535	-0.045828	3.223440
234.559306	3450.187610	17.103539	-0.045875	3.219952
234.620118	3442.247008	17.108544	-0.045881	3.216476
234.205134	3434.248753	17.113549	-0.045798	3.212952
234.211742	3426.263066	17.118554	-0.045794	3.209446
234.201949	3418.277713	17.123559	-0.045787	3.205936
234.044179	3410.287471	17.128563	-0.045753	3.202415
234.176406	3402.279989	17.133568	-0.045772	3.198893
234.263190	3394.306816	17.138573	-0.045783	3.195381
234.269322	3386.337331	17.143578	-0.045779	3.191864
234.061547	3378.329980	17.148583	-0.045735	3.188316
234.193942	3370.334360	17.153587	-0.045755	3.184785
234.169528	3362.379492	17.158592	-0.045745	3.181261
234.014200	3354.372841	17.163597	-0.045711	3.177704
234.084256	3346.395714	17.168602	-0.045719	3.174166
234.148835	3338.389357	17.173607	-0.045726	3.170611
233.943942	3330.396957	17.178611	-0.045682	3.167047
233.787408	3322.442604	17.183616	-0.045648	3.163498
233.880358	3314.444355	17.188621	-0.045660	3.159935
234.003973	3306.464683	17.193626	-0.045678	3.156379
233.739664	3298.464015	17.198631	-0.045624	3.152792
233.721313	3290.438811	17.203635	-0.045615	3.149201
233.855004	3282.462238	17.208640	-0.045635	3.145634
233.809941	3274.478768	17.213645	-0.045621	3.142052
233.682777	3266.546546	17.218650	-0.045592	3.138485
233.558350	3258.543300	17.223655	-0.045564	3.134883
233.536266	3250.544083	17.228659	-0.045555	3.131283
233.466538	3242.534543	17.233664	-0.045537	3.127671
233.390843	3234.552870	17.238669	-0.045517	3.124068
233.487480	3226.601363	17.243674	-0.045530	3.120482
233.394946	3218.640474	17.248679	-0.045508	3.116879
233.559715	3210.601862	17.253683	-0.045533	3.113249
233.517363	3202.600093	17.258688	-0.045520	3.109621
233.284982	3194.631491	17.263693	-0.045472	3.105996
233.396394	3186.665368	17.268698	-0.045487	3.102383
233.375294	3178.654515	17.273703	-0.045478	3.098740
233.270958	3170.682027	17.278707	-0.045454	3.095106
233.420044	3162.678372	17.283712	-0.045476	3.091465
233.164640	3154.693434	17.288717	-0.045423	3.087810
233.239082	3146.713421	17.293722	-0.045432	3.084168
233.122843	3138.758702	17.298727	-0.045405	3.080524
233.096772	3130.790679	17.303731	-0.045395	3.076874
233.178497	3122.743581	17.308736	-0.045405	3.073189
233.082094	3114.682779	17.313741	-0.045382	3.069484
232.925440	3106.740427	17.318746	-0.045348	3.065827
233.059283	3098.757585	17.323751	-0.045368	3.062160
233.174493	3090.784116	17.328755	-0.045384	3.058492
232.821714	3082.858042	17.333760	-0.045313	3.054820
232.856688	3074.836944	17.338765	-0.045314	3.051117
233.112740	3066.848679	17.343770	-0.045357	3.047436
232.729943	3058.875891	17.348775	-0.045280	3.043727
232.696124	3050.891067	17.353779	-0.045269	3.040025
232.820161	3042.933253	17.358784	-0.045287	3.036338
232.678816	3034.905813	17.363789	-0.045255	3.032602
232.488897	3026.946378	17.368794	-0.045215	3.028890
232.500471	3018.934274	17.373799	-0.045212	3.025159
232.697193	3010.958221	17.378803	-0.045243	3.021449
232.454042	3003.013138	17.383808	-0.045193	3.017727
232.538842	2995.000242	17.388813	-0.045203	3.013986
232.377718	2987.017734	17.393818	-0.045168	3.010242
232.384715	2979.048203	17.398823	-0.045164	3.006507
232.316835	2971.079171	17.403827	-0.045147	3.002764
232.377883	2963.101193	17.408832	-0.045153	2.999019
232.155046	2955.130664	17.413837	-0.045106	2.995259
232.134150	2947.113764	17.418842	-0.045097	2.991482
232.008540	2939.096942	17.423847	-0.045069	2.987695
232.175257	2931.108170	17.428851	-0.045094	2.983931
231.976283	2923.161080	17.433856	-0.045052	2.980164
231.853633	2915.188978	17.438861	-0.045024	2.976383
232.080555	2907.169958	17.443866	-0.045061	2.972594
231.791443	2899.190007	17.448871	-0.045002	2.968792
231.806712	2891.207476	17.453875	-0.045000	2.964999
231.751676	2883.259099	17.458880	-0.044985	2.961215
231.715993	2875.282813	17.463885	-0.044973	2.957413
231.702036	2867.289608	17.468890	-0.044965	2.953599
231.638825	2859.274173	17.473895	-0.044948	2.949767
231.875798	2851.287579	17.478899	-0.044987	2.945959
231.614687	2843.339134	17.483904	-0.044933	2.942139
231.526379	2835.353101	17.488909	-0.044912	2.938305
231.669092	2827.373845	17.493914	-0.044933	2.934481
231.790467	2819.345592	17.498919	-0.044950	2.930628
231.476666	2811.405816	17.503923	-0.044887	2.926789
231.486457	2803.446402	17.508928	-0.044883	2.922952
231.477983	2795.450957	17.513933	-0.044877	2.919093
231.629865	2787.471728	17.518938	-0.044900	2.915244
231.409484	2779.413028	17.523943	-0.044854	2.911332
231.693813	2771.399806	17.528947	-0.044901	2.907464
231.465846	2763.465206	17.533952	-0.044854	2.903602
231.335819	2755.512481	17.538957	-0.044824	2.899730
231.414363	2747.550554	17.543962	-0.044834	2.895861
231.291213	2739.556927	17.548967	-0.044806	2.891959
231.100099	2731.579787	17.553971	-0.044765	2.888057
231.218696	2723.581609	17.558976	-0.044782	2.884156
231.186945	2715.619882	17.563981	-0.044771	2.880260
231.098499	2707.681012	17.568986	-0.044749	2.876366
230.954082	2699.663163	17.573991	-0.044717	2.872425
230.907906	2691.675871	17.578995	-0.044703	2.868499
230.965302	2683.678395	17.584000	-0.044709	2.864569
230.891905	2675.736345	17.589005	-0.044690	2.860653
230.991353	2667.745254	17.594010	-0.044703	2.856717
230.754104	2659.782909	17.599015	-0.044654	2.852771
230.797873	2651.763984	17.604019	-0.044657	2.848807
230.851347	2643.779032	17.609024	-0.044662	2.844855
230.738147	2635.846699	17.614029	-0.044636	2.840915
230.660905	2627.895593	17.619034	-0.044616	2.836961
230.644169	2619.880352	17.624039	-0.044608	2.832974
230.628226	2611.870676	17.629043	-0.044600	2.828984
230.904261	2603.868985	17.634048	-0.044646	2.825008
230.655988	2595.927772	17.639053	-0.044594	2.821028
230.494065	2587.971166	17.644058	-0.044559	2.817039
230.573796	2579.969527	17.649063	-0.044569	2.813036
230.394487	2572.002800	17.654067	-0.044530	2.809029
230.376261	2564.024015	17.659072	-0.044522	2.805020
230.519253	2556.032465	17.664077	-0.044543	2.801008
230.364355	2548.089806	17.669082	-0.044509	2.796998
230.216339	2540.104643	17.674087	-0.044476	2.792961
230.409963	2532.077909	17.679091	-0.044507	2.788917
230.494449	2524.095116	17.684096	-0.044518	2.784883
230.232054	2516.169121	17.689101	-0.044464	2.780852
230.213686	2508.208499	17.694106	-0.044455	2.776811
230.339843	2500.191035	17.699111	-0.044474	2.772745
230.036597	2492.237303	17.704115	-0.044412	2.768679
230.064138	2484.266478	17.709120	-0.044412	2.764618
230.003016	2476.305525	17.714125	-0.044395	2.760551
229.935011	2468.349820	17.719130	-0.044378	2.756480
229.771751	2460.303767	17.724135	-0.044342	2.752351
229.730159	2452.301780	17.729139	-0.044329	2.748246
229.967252	2444.311068	17.734144	-0.044368	2.744158
229.714045	2436.371915	17.739149	-0.044316	2.740060
229.674032	2428.428005	17.744154	-0.044303	2.735966
229.728449	2420.420688	17.749159	-0.044308	2.731839
229.538267	2412.461753	17.754163	-0.044267	2.727716
229.559745	2404.493983	17.759168	-0.044266	2.723596
229.551440	2396.502672	17.764173	-0.044260	2.719455
229.530078	2388.559362	17.769178	-0.044250	2.715332
229.354976	2380.558278	17.774183	-0.044213	2.711162
229.255494	2372.583914	17.779187	-0.044189	2.707005
229.268608	2364.625695	17.784192	-0.044186	2.702858
228.987679	2356.665433	17.789197	-0.044129	2.698684
229.100392	2348.701874	17.794202	-0.044145	2.694526
229.320508	2340.666111	17.799207	-0.044180	2.690332
229.244023	2332.700576	17.804211	-0.044161	2.686149
229.372422	2324.761305	17.809216	-0.044180	2.681986
229.281679	2316.790283	17.814221	-0.044158	2.677786
229.223923	2308.825445	17.819226	-0.044142	2.673584
229.112180	2300.798753	17.824231	-0.044116	2.669340
228.924367	2292.851384	17.829235	-0.044076	2.665127
229.269323	2284.867049	17.834240	-0.044135	2.660921
228.886437	2276.942254	17.839245	-0.044058	2.656693
228.895007	2268.942483	17.844250	-0.044055	2.652444
229.046510	2260.936547	17.849255	-0.044078	2.648194
229.031113	2252.972921	17.854259	-0.044070	2.643949
229.008296	2245.025925	17.859264	-0.044060	2.639706
228.819732	2237.076234	17.864269	-0.044020	2.635443
228.822021	2229.074625	17.869274	-0.044015	2.631158
228.933804	2221.077180	17.874279	-0.044031	2.626876
228.838174	2213.140128	17.879283	-0.044008	2.622606
228.784808	2205.200967	17.884288	-0.043993	2.618330
228.658536	2197.216136	17.889293	-0.043964	2.614017
228.682371	2189.218681	17.894298	-0.043964	2.609701
228.670993	2181.259585	17.899303	-0.043956	2.605396
228.536857	2173.320884	17.904307	-0.043926	2.601086
228.465998	2165.379755	17.909312	-0.043908	2.596773
228.552998	2157.239860	17.914317	-0.043919	2.592354
228.592362	2149.207124	17.919322	-0.043921	2.587984
228.390497	2141.277663	17.924327	-0.043878	2.583646
228.337488	2133.356362	17.929331	-0.043863	2.579315
228.493125	2125.411888	17.934336	-0.043887	2.574978
228.223278	2117.459175	17.939341	-0.043832	2.570601
228.323418	2109.480022	17.944346	-0.043845	2.566227
228.223550	2101.541098	17.949351	-0.043821	2.561853
228.333500	2093.580741	17.954355	-0.043837	2.557475
228.233499	2085.635118	17.959360	-0.043813	2.553083
228.029818	2077.647828	17.964365	-0.043770	2.548653
227.996829	2069.673121	17.969370	-0.043758	2.544235
228.003277	2061.733127	17.974375	-0.043755	2.539830
227.853234	2053.795698	17.979379	-0.043721	2.535408
228.025773	2045.790105	17.984384	-0.043748	2.530964
228.046067	2037.794164	17.989389	-0.043747	2.526506
227.824154	2029.888843	17.994394	-0.043701	2.522074
227.800109	2021.918382	17.999399	-0.043691	2.517611
227.763310	2013.931988	18.004403	-0.043679	2.513131
227.585919	2005.963502	18.009408	-0.043641	2.508643
227.496197	1997.985055	18.014413	-0.043619	2.504147
227.733102	1990.010654	18.019418	-0.043658	2.499669
227.694704	1982.061664	18.024423	-0.043645	2.495178
227.564932	1974.096100	18.029427	-0.043616	2.490662
227.372117	1966.148273	18.034432	-0.043575	2.486144
227.387202	1958.180878	18.039437	-0.043573	2.481621
227.369581	1950.231421	18.044442	-0.043564	2.477098
227.437416	1942.245403	18.049447	-0.043572	2.472553
227.433362	1934.251980	18.054451	-0.043566	2.467989
227.395410	1926.317848	18.059456	-0.043554	2.463448
227.210533	1918.377567	18.064461	-0.043514	2.458884
227.193346	1910.416319	18.069466	-0.043506	2.454313
227.053921	1902.446624	18.074471	-0.043475	2.449718
226.996382	1894.487429	18.079475	-0.043459	2.445127
226.965056	1886.538953	18.084480	-0.043448	2.440536
226.855568	1878.579073	18.089485	-0.043422	2.435924
226.921224	1870.549330	18.094490	-0.043429	2.431275
226.864586	1862.572002	18.099495	-0.043414	2.426639
226.854457	1854.607814	18.104499	-0.043406	2.422005
226.904015	1846.679051	18.109504	-0.043411	2.417388
226.708764	1838.723643	18.114509	-0.043369	2.412727
226.701433	1830.753419	18.119514	-0.043363	2.408063
226.858544	1822.777014	18.124519	-0.043387	2.403399
226.680414	1814.862787	18.129523	-0.043348	2.398737
226.549256	1806.933934	18.134528	-0.043319	2.394060
226.549791	1798.924503	18.139533	-0.043314	2.389337
226.607631	1790.957276	18.144538	-0.043319	2.384634
226.381718	1783.049551	18.149543	-0.043272	2.379935
226.468648	1775.079569	18.154547	-0.043283	2.375214
226.538811	1767.101908	18.159552	-0.043291	2.370478
226.307395	1759.157168	18.164557	-0.043243	2.365728
226.499566	1751.201472	18.169562	-0.043273	2.360996
226.318506	1743.271035	18.174567	-0.043235	2.356239
226.306321	1735.280536	18.179571	-0.043227	2.351451
226.272815	1727.326080	18.184576	-0.043216	2.346672
226.223163	1719.351407	18.189581	-0.043201	2.341870
226.138933	1711.428070	18.194586	-0.043181	2.337087
226.087913	1703.462535	18.199591	-0.043166	2.332270
226.009092	1695.490729	18.204595	-0.043146	2.327438
226.022219	1687.573881	18.209600	-0.043143	2.322637
225.767832	1679.627821	18.214605	-0.043091	2.317786
225.996547	1671.657842	18.219610	-0.043128	2.312950
226.018666	1663.686672	18.224615	-0.043127	2.308086
225.702730	1655.758241	18.229619	-0.043063	2.303209
225.691421	1647.809296	18.234624	-0.043056	2.298336
225.660518	1639.859595	18.239629	-0.043045	2.293449
225.611077	1631.899509	18.244634	-0.043031	2.288545
225.472351	1623.962249	18.249639	-0.043000	2.283636
225.568080	1616.000683	18.254643	-0.043012	2.278722
225.686553	1608.038222	18.259648	-0.043029	2.273798
225.324645	1600.033124	18.264653	-0.042957	2.268796
225.395405	1592.086894	18.269658	-0.042965	2.263857
225.205355	1584.172657	18.274663	-0.042924	2.258904
225.400328	1576.187186	18.279667	-0.042955	2.253930
225.198073	1568.272015	18.284672	-0.042913	2.248954
225.212096	1560.308572	18.289677	-0.042910	2.243955
225.073838	1552.409633	18.294682	-0.042879	2.238972
225.113088	1544.454340	18.299687	-0.042881	2.233959
225.094594	1536.469692	18.304691	-0.042873	2.228910
224.941212	1528.558223	18.309696	-0.042839	2.223885
224.906573	1520.605577	18.314701	-0.042827	2.218832
224.813821	1512.676775	18.319706	-0.042805	2.213778
224.752823	1504.717905	18.324711	-0.042789	2.208696
224.680662	1496.785782	18.329715	-0.042770	2.203618
224.617145	1488.853969	18.334720	-0.042753	2.198529
224.702031	1480.880248	18.339725	-0.042764	2.193415
224.467308	1472.940978	18.344730	-0.042715	2.188283
224.454009	1464.976782	18.349735	-0.042707	2.183142
224.455401	1457.044438	18.354739	-0.042702	2.178011
224.533545	1449.088359	18.359744	-0.042712	2.172860
224.397619	1441.155628	18.364749	-0.042681	2.167692
224.469794	1433.217029	18.369754	-0.042690	2.162527
224.350546	1425.298616	18.374759	-0.042662	2.157345
224.270530	1417.353916	18.379763	-0.042642	2.152136
224.164807	1409.426227	18.384768	-0.042617	2.146924
224.093155	1401.472199	18.389773	-0.042599	2.141685
224.198291	1393.543752	18.394778	-0.042613	2.136467
224.320041	1385.569218	18.399783	-0.042631	2.131208
224.090891	1377.647089	18.404787	-0.042583	2.125936
224.094530	1369.734935	18.409792	-0.042579	2.120680
223.912749	1361.823230	18.414797	-0.042540	2.115394
223.985768	1353.812189	18.419802	-0.042548	2.110053
224.096549	1345.835229	18.424807	-0.042563	2.104724
223.937654	1337.934376	18.429811	-0.042529	2.099407
223.838673	1330.026410	18.434816	-0.042505	2.094077
223.924743	1322.047503	18.439821	-0.042516	2.088704
223.889698	1314.136159	18.444826	-0.042504	2.083351
223.738169	1306.234054	18.449831	-0.042471	2.077979
223.485781	1298.322909	18.454835	-0.042419	2.072577
223.658595	1290.366157	18.459840	-0.042446	2.067172
223.566927	1282.438595	18.464845	-0.042424	2.061746
223.466191	1274.526676	18.469850	-0.042400	2.056316
223.691187	1266.552806	18.474855	-0.042437	2.050862
223.482688	1258.635936	18.479859	-0.042393	2.045388
223.281661	1250.758938	18.484864	-0.042350	2.039928
223.482790	1242.800102	18.489869	-0.042382	2.034438
223.546032	1234.823828	18.494874	-0.042389	2.028907
223.300629	1226.942068	18.499879	-0.042338	2.023394
223.156422	1219.021233	18.504883	-0.042306	2.017850
223.163983	1211.081554	18.509888	-0.042303	2.012293
223.133254	1203.141909	18.514893	-0.042292	2.006716
223.145425	1195.228823	18.519898	-0.042289	2.001147
223.070520	1187.332103	18.524903	-0.042270	1.995565
222.864099	1179.401746	18.529907	-0.042226	1.989930
223.006298	1171.468241	18.534912	-0.042248	1.984313
222.834288	1163.560522	18.539917	-0.042210	1.978665
222.914627	1155.632383	18.544922	-0.042220	1.973014
222.879160	1147.703020	18.549927	-0.042208	1.967333
222.707397	1139.807181	18.554931	-0.042171	1.961645
222.796079	1131.886688	18.559936	-0.042183	1.955950
222.778478	1123.912730	18.564941	-0.042174	1.950189
222.567633	1116.026409	18.569946	-0.042130	1.944453
222.560169	1108.101601	18.574951	-0.042123	1.938695
222.619046	1100.167653	18.579955	-0.042129	1.932920
222.471377	1092.266505	18.584960	-0.042097	1.927128
222.344572	1084.370103	18.589965	-0.042068	1.921326
222.507107	1076.446064	18.594970	-0.042093	1.915517
222.321981	1068.539537	18.599975	-0.042053	1.909665
222.316618	1060.617073	18.604979	-0.042047	1.903803
222.352669	1052.722360	18.609984	-0.042049	1.897948
222.248923	1044.805966	18.614989	-0.042024	1.892043
222.001965	1036.919421	18.619994	-0.041973	1.886126
221.967454	1029.016090	18.624999	-0.041962	1.880202
221.938380	1021.112777	18.630003	-0.041951	1.874259
221.716518	1013.211847	18.635008	-0.041905	1.868278
221.737643	1005.270184	18.640013	-0.041904	1.862274
221.717243	997.381175	18.645018	-0.041895	1.856286
221.724285	989.454842	18.650023	-0.041891	1.850253
221.483026	981.579140	18.655027	-0.041841	1.844210
221.547349	973.683302	18.660032	-0.041848	1.838168
221.764557	965.741365	18.665037	-0.041883	1.832089
221.591262	957.860428	18.670042	-0.041846	1.825990
221.456468	949.978453	18.675047	-0.041816	1.819874
221.371984	942.090198	18.680051	-0.041795	1.813739
221.501574	934.166181	18.685056	-0.041814	1.807581
221.428593	926.281417	18.690061	-0.041795	1.801408
221.442864	918.404224	18.695066	-0.041793	1.795230
221.265683	910.473130	18.700071	-0.041754	1.788965
221.164913	902.571087	18.705075	-0.041731	1.782711
221.078802	894.709876	18.710080	-0.041709	1.776468
221.128401	886.784295	18.715085	-0.041713	1.770169
221.105407	878.910442	18.720090	-0.041704	1.763880
220.912461	871.060055	18.725095	-0.041663	1.757566
220.996978	863.150666	18.730099	-0.041674	1.751216
220.755736	855.296281	18.735104	-0.041624	1.744847
220.664544	847.423398	18.740109	-0.041602	1.738458
220.865038	839.511128	18.745114	-0.041634	1.732051
220.824673	831.622561	18.750119	-0.041621	1.725609
220.517073	823.797275	18.755123	-0.041559	1.719160
220.476447	815.923756	18.760128	-0.041546	1.712681
220.467797	808.004746	18.765133	-0.041539	1.706144
220.583084	800.113971	18.770138	-0.041556	1.699622
220.267795	792.292488	18.775143	-0.041492	1.693076
220.136653	784.403899	18.780147	-0.041463	1.686472
220.276824	776.525805	18.785152	-0.041484	1.679888
220.070562	768.688707	18.790157	-0.041440	1.673266
220.179480	760.783700	18.795162	-0.041455	1.666602
220.241282	752.908441	18.800167	-0.041462	1.659930
220.081184	745.074235	18.805171	-0.041427	1.653237
220.077521	737.197565	18.810176	-0.041421	1.646501
220.054907	729.342301	18.815181	-0.041412	1.639753
219.936202	721.493117	18.820186	-0.041384	1.632969
219.728398	713.606287	18.825191	-0.041341	1.626112
219.618674	705.762436	18.830195	-0.041315	1.619277
219.660306	697.908583	18.835200	-0.041318	1.612426
219.608468	690.034602	18.840205	-0.041303	1.605514
219.567347	682.212600	18.845210	-0.041290	1.598620
219.578141	674.352034	18.850215	-0.041287	1.591669
219.489887	666.500640	18.855219	-0.041266	1.584682
219.575810	658.657387	18.860224	-0.041277	1.577696
219.479018	650.812503	18.865229	-0.041254	1.570651
219.490498	642.976872	18.870234	-0.041251	1.563598
219.279048	635.181050	18.875239	-0.041206	1.556517
219.181866	627.320410	18.880243	-0.041183	1.549361
219.300937	619.471452	18.885248	-0.041200	1.542215
219.227999	611.645160	18.890253	-0.041181	1.535028
219.186405	603.812222	18.895258	-0.041169	1.527805
219.139421	595.995964	18.900263	-0.041155	1.520563
218.960516	588.194533	18.905267	-0.041116	1.513280
218.996677	580.354711	18.910272	-0.041118	1.505958
218.953566	572.535979	18.915277	-0.041105	1.498609
218.915101	564.725926	18.920282	-0.041093	1.491232
218.789420	556.923597	18.925287	-0.041064	1.483812
218.646775	549.140421	18.930291	-0.041033	1.476370
218.620634	541.282540	18.935296	-0.041023	1.468837
218.306676	533.500038	18.940301	-0.040959	1.461293
218.429111	525.677891	18.945306	-0.040977	1.453740
218.336788	517.869889	18.950311	-0.040955	1.446128
218.357240	510.072008	18.955315	-0.040954	1.438503
218.202165	502.310892	18.960320	-0.040920	1.430845
218.092914	494.518967	18.965325	-0.040894	1.423123
218.204503	486.719372	18.970330	-0.040910	1.415387
217.942013	478.962570	18.975335	-0.040856	1.407590
217.887177	471.177692	18.980339	-0.040841	1.399756
217.902219	463.398572	18.985344	-0.040839	1.391895
217.657481	455.629846	18.990349	-0.040788	1.383956
217.624055	447.858267	18.995354	-0.040777	1.376004
217.793318	440.047985	19.000359	-0.040803	1.368001
217.447815	432.337096	19.005363	-0.040734	1.359965
217.530528	424.568804	19.010368	-0.040744	1.351896
217.502029	416.789545	19.015373	-0.040734	1.343747
217.436229	409.057030	19.020378	-0.040717	1.335591
217.242248	401.330299	19.025383	-0.040676	1.327369
217.264982	393.576497	19.030387	-0.040675	1.319105
217.291246	385.760729	19.035392	-0.040675	1.310723
217.101182	377.992628	19.040397	-0.040634	1.302299
216.896227	370.302310	19.045402	-0.040591	1.293902
216.960337	362.557158	19.050407	-0.040598	1.285440
217.045118	354.834392	19.055411	-0.040609	1.276951
216.958065	347.141230	19.060416	-0.040588	1.268405
216.619072	339.475245	19.065421	-0.040519	1.259784
216.579624	331.774110	19.070426	-0.040507	1.251121
216.508931	324.084948	19.075431	-0.040489	1.242406
216.316946	316.412553	19.080435	-0.040448	1.233624
216.398264	308.687346	19.085440	-0.040458	1.224772
216.390859	300.996675	19.090445	-0.040452	1.215878
216.377044	293.314631	19.095450	-0.040444	1.206927
216.431348	285.646574	19.100455	-0.040450	1.197939
216.311872	277.991515	19.105459	-0.040422	1.188864
216.362623	270.331969	19.110464	-0.040427	1.179748
216.155636	262.709339	19.115469	-0.040383	1.170553
215.966678	255.096613	19.120474	-0.040343	1.161301
215.759305	247.483236	19.125479	-0.040300	1.151969
215.697793	239.820904	19.130483	-0.040283	1.142532
215.795369	232.181336	19.135488	-0.040297	1.133078
215.635229	224.579908	19.140493	-0.040262	1.123538
215.625617	216.980770	19.145498	-0.040255	1.113951
215.567221	209.385967	19.150503	-0.040239	1.104275
215.514744	201.806932	19.155507	-0.040225	1.094536
215.159656	194.281925	19.160512	-0.040154	1.084711
215.147243	186.708462	19.165517	-0.040146	1.074811
215.179490	179.122309	19.170522	-0.040148	1.064812
215.077209	171.588094	19.175527	-0.040124	1.054757
214.799987	164.073421	19.180531	-0.040067	1.044590
214.980633	156.524991	19.185536	-0.040096	1.034385
215.010069	148.989590	19.190541	-0.040097	1.024061
214.793406	141.526779	19.195546	-0.040051	1.013673
214.751465	134.036179	19.200551	-0.040039	1.003181
214.489618	126.585907	19.205555	-0.039985	0.992580
214.425668	119.095942	19.210560	-0.039968	0.981858
214.075854	111.688786	19.215565	-0.039898	0.971065
213.970889	104.259207	19.220570	-0.039874	0.960181
213.886825	96.842246	19.225575	-0.039854	0.949196
213.596056	89.466577	19.230579	-0.039795	0.938090
213.562922	82.064707	19.235584	-0.039784	0.926879
213.026299	74.773949	19.240589	-0.039679	0.915567
212.524646	67.465822	19.245594	-0.039581	0.904095
212.226482	60.384055	19.250599	-0.039521	0.892890