Fri Mar 12 13:30:51 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.192764	0.146611	0.000000	0.000050	0.721337

0.389908	0.164264	0.005005	0.000013	0.721441
0.244350	0.122674	0.010010	0.000040	0.721308
0.183859	0.037936	0.015014	0.000052	0.721120
0.453655	-0.006292	0.020019	0.000001	0.721128
0.444200	-0.008291	0.025024	0.000003	0.721121
0.485560	-0.013388	0.030029	-0.000005	0.721125
0.526008	-0.020544	0.035034	-0.000012	0.721125
0.215068	0.031024	0.040038	0.000046	0.721118
0.191431	0.041628	0.045043	0.000050	0.721131
0.177446	0.039959	0.050048	0.000053	0.721122
0.325836	0.016239	0.055053	0.000025	0.721128
0.236113	0.032739	0.060058	0.000042	0.721129
0.180775	0.039148	0.065062	0.000052	0.721122
0.254727	0.029002	0.070067	0.000038	0.721128
0.288808	0.019329	0.075072	0.000032	0.721121
0.455160	-0.007986	0.080077	0.000001	0.721126
0.444281	-0.128151	0.085082	0.000003	0.720886
0.323613	-0.113241	0.090086	0.000025	0.720873
0.305953	-0.105369	0.095091	0.000028	0.720882
0.346956	-0.116829	0.100096	0.000021	0.720874
0.410677	-0.124957	0.105101	0.000009	0.720880
0.355307	-0.116081	0.110106	0.000019	0.720879
0.472136	-0.250382	0.115110	-0.000003	0.720655
0.591631	-0.327045	0.120115	-0.000025	0.720546
0.427743	-0.301699	0.125120	0.000006	0.720539
0.456194	-0.304895	0.130125	0.000000	0.720543
0.409436	-0.296800	0.135130	0.000009	0.720542
0.245826	-0.409998	0.140134	0.000040	0.720262
0.356894	-0.446891	0.145139	0.000019	0.720228
0.101849	-0.405070	0.150144	0.000066	0.720221
0.176205	-0.418068	0.155149	0.000052	0.720222
0.190355	-0.505494	0.160154	0.000050	0.720055
0.197340	-0.586199	0.165158	0.000049	0.719898
0.324364	-0.602911	0.170163	0.000025	0.719910
0.240979	-0.593402	0.175168	0.000040	0.719899
0.106620	-0.684320	0.180173	0.000065	0.719673
0.217303	-0.738513	0.185178	0.000045	0.719605
0.279399	-0.753881	0.190182	0.000033	0.719597
0.305710	-0.813433	0.195187	0.000028	0.719489
0.111425	-0.890328	0.200192	0.000064	0.719269
0.034641	-0.874905	0.205197	0.000079	0.719272
-0.111755	-0.869760	0.210202	0.000106	0.719231
-0.212624	-0.990111	0.215206	0.000125	0.718958
-0.004926	-1.019857	0.220211	0.000086	0.718973
-0.243105	-0.986608	0.225216	0.000130	0.718955
-0.017428	-1.181870	0.230221	0.000088	0.718649
-0.115177	-1.163781	0.235226	0.000107	0.718650
-0.090138	-1.197889	0.240230	0.000102	0.718592
-0.061303	-1.321970	0.245235	0.000097	0.718357
0.039556	-1.342417	0.250240	0.000078	0.718352
0.227880	-1.465704	0.255245	0.000043	0.718175
0.126377	-1.525653	0.260250	0.000062	0.718021
0.054848	-1.529617	0.265254	0.000075	0.717988
0.037373	-1.667505	0.270259	0.000078	0.717709
-0.026871	-1.660438	0.275264	0.000090	0.717701
-0.221854	-1.737992	0.280269	0.000127	0.717479
-0.158218	-1.797597	0.285274	0.000115	0.717384
-0.248536	-1.835654	0.290278	0.000131	0.717277
-0.244204	-1.930375	0.295283	0.000131	0.717091
-0.308389	-1.933731	0.300288	0.000143	0.717062
-0.227281	-2.102049	0.305293	0.000128	0.716757
-0.674805	-2.020946	0.310298	0.000211	0.716760
-1.091013	-2.077786	0.315302	0.000288	0.716501
-0.719396	-2.167235	0.320307	0.000219	0.716455
-0.798846	-2.241681	0.325312	0.000234	0.716279
-0.800397	-2.313394	0.330317	0.000234	0.716137
-0.765707	-2.363380	0.335322	0.000228	0.716050
-0.974833	-2.410382	0.340326	0.000267	0.715883
-2.955152	-2.051579	0.345331	0.000635	0.715895
-2.957191	-2.221440	0.350336	0.000636	0.715558
-3.574501	-2.115795	0.355341	0.000751	0.715549
-4.058954	-2.028069	0.360346	0.000841	0.715552
-3.810420	-2.218715	0.365350	0.000794	0.715262
-4.446320	-2.117624	0.370355	0.000913	0.715238
-4.947312	-2.032539	0.375360	0.001006	0.715230
-4.337748	-2.222293	0.380365	0.000893	0.715069
-5.059879	-2.171052	0.385370	0.001027	0.714915
-5.609438	-2.077939	0.390374	0.001129	0.714906
-5.694249	-2.057829	0.395379	0.001145	0.714916
-5.635409	-2.176527	0.400384	0.001134	0.714701
-6.302772	-2.104256	0.405389	0.001258	0.714609
-6.408070	-2.082975	0.410394	0.001278	0.714614
-6.288553	-2.108703	0.415398	0.001255	0.714605
-6.210036	-2.204722	0.420403	0.001241	0.714442
-7.554558	-2.048807	0.425408	0.001491	0.714276
-7.339803	-2.087650	0.430413	0.001451	0.714275
-6.994606	-2.147494	0.435418	0.001387	0.714279
-7.458836	-2.066627	0.440422	0.001473	0.714275
-7.402461	-2.186749	0.445427	0.001463	0.714056
-8.265817	-2.079550	0.450432	0.001623	0.713964
-8.199703	-2.088220	0.455437	0.001611	0.713970
-8.129328	-2.099848	0.460442	0.001598	0.713972
-8.310538	-2.070621	0.465446	0.001632	0.713966
-7.910369	-2.226933	0.470451	0.001557	0.713797
-9.321587	-2.049898	0.475456	0.001820	0.713649
-9.174080	-2.074877	0.480461	0.001792	0.713652
-8.856795	-2.130576	0.485466	0.001733	0.713654
-9.223677	-2.069129	0.490470	0.001801	0.713646
-9.122473	-2.082364	0.495475	0.001783	0.713655
-9.394393	-2.164145	0.500480	0.001833	0.713396
-9.923662	-2.088400	0.505485	0.001932	0.713360
-9.929061	-2.086451	0.510490	0.001933	0.713362
-9.841427	-2.104845	0.515494	0.001916	0.713356
-9.776937	-2.112483	0.520499	0.001904	0.713364
-10.040519	-2.070694	0.525504	0.001953	0.713354
-10.609614	-2.134298	0.530509	0.002059	0.713026
-10.351600	-2.178655	0.535514	0.002011	0.713029
-10.765312	-2.109486	0.540518	0.002088	0.713020
-10.706204	-2.115814	0.545523	0.002077	0.713028
-10.829978	-2.097520	0.550528	0.002100	0.713021
-10.701273	-2.120171	0.555533	0.002076	0.713021
-11.345872	-2.152716	0.560538	0.002196	0.712728
-12.056726	-2.036871	0.565542	0.002328	0.712707
-11.790903	-2.080740	0.570547	0.002279	0.712714
-11.623079	-2.114164	0.575552	0.002248	0.712707
-11.768839	-2.087520	0.580557	0.002275	0.712708
-11.493389	-2.132242	0.585562	0.002223	0.712717
-11.870916	-2.114087	0.590566	0.002294	0.712619
-12.980576	-2.030252	0.595571	0.002500	0.712392
-12.611729	-2.100318	0.600576	0.002432	0.712384
-12.658527	-2.090915	0.605581	0.002440	0.712386
-12.587420	-2.101110	0.610586	0.002427	0.712391
-12.930030	-2.044876	0.615590	0.002491	0.712382
-12.400928	-2.134484	0.620595	0.002392	0.712391
-12.574110	-2.141901	0.625600	0.002424	0.712315
-13.695733	-2.056311	0.630605	0.002633	0.712087
-13.126620	-2.153169	0.635610	0.002527	0.712096
-13.404474	-2.109254	0.640614	0.002579	0.712085
-13.349053	-2.114932	0.645619	0.002569	0.712094
-13.351520	-2.117776	0.650624	0.002569	0.712087
-13.571918	-2.077480	0.655629	0.002610	0.712089
-13.709019	-2.158820	0.660634	0.002635	0.711878
-15.141506	-1.965185	0.665638	0.002902	0.711756
-14.238908	-2.121707	0.670643	0.002734	0.711764
-14.196479	-2.131845	0.675648	0.002726	0.711759
-14.624930	-2.056393	0.680653	0.002806	0.711758
-14.169213	-2.135595	0.685658	0.002721	0.711762
-14.320116	-2.112458	0.690662	0.002749	0.711754
-14.455202	-2.181659	0.695667	0.002774	0.711568
-15.407251	-2.071450	0.700672	0.002951	0.711450
-15.380518	-2.075737	0.705677	0.002946	0.711451
-15.104526	-2.122798	0.710682	0.002895	0.711455
-15.867435	-1.991072	0.715686	0.003037	0.711447
-15.154857	-2.111078	0.720691	0.002904	0.711461
-15.172735	-2.111212	0.725696	0.002908	0.711454
-15.523977	-2.127379	0.730701	0.002973	0.711297
-16.161190	-2.094015	0.735706	0.003092	0.711137
-15.932355	-2.136273	0.740710	0.003049	0.711134
-16.421844	-2.045129	0.745715	0.003140	0.711142
-16.558565	-2.025375	0.750720	0.003165	0.711133
-16.124227	-2.102258	0.755725	0.003085	0.711134
-16.129731	-2.098260	0.760730	0.003085	0.711140
-16.634315	-2.040291	0.765734	0.003179	0.711077
-16.877589	-2.097977	0.770739	0.003225	0.710875
-16.811520	-2.112599	0.775744	0.003212	0.710869
-17.506866	-1.988603	0.780749	0.003342	0.710870
-17.139288	-2.051285	0.785754	0.003273	0.710875
-16.878229	-2.102022	0.790758	0.003225	0.710867
-17.061869	-2.065381	0.795763	0.003259	0.710875
-17.055528	-2.114670	0.800768	0.003258	0.710779
-18.174663	-2.040693	0.805773	0.003466	0.710528
-17.532204	-2.152597	0.810778	0.003346	0.710534
-18.168073	-2.042910	0.815782	0.003465	0.710526
-17.868399	-2.092282	0.820787	0.003409	0.710534
-17.784935	-2.110393	0.825792	0.003393	0.710528
-18.393069	-2.002561	0.830797	0.003506	0.710527
-17.985858	-2.106188	0.835802	0.003431	0.710465
-18.720288	-2.103128	0.840806	0.003567	0.710210
-18.689517	-2.104582	0.845811	0.003562	0.710218
-19.236004	-2.009765	0.850816	0.003663	0.710213
-18.949688	-2.060002	0.855821	0.003610	0.710214
-18.665880	-2.108464	0.860826	0.003557	0.710219
-19.251336	-2.006428	0.865830	0.003666	0.710214
-18.904209	-2.065549	0.870835	0.003601	0.710220
-19.328646	-2.151887	0.875840	0.003680	0.709896
-20.051004	-2.024513	0.880845	0.003815	0.709893
-20.034842	-2.026099	0.885850	0.003812	0.709896
-19.820317	-2.067799	0.890854	0.003772	0.709889
-19.861365	-2.055558	0.895859	0.003779	0.709899
-19.963363	-2.041669	0.900864	0.003798	0.709891
-19.877277	-2.057434	0.905869	0.003782	0.709890
-19.894636	-2.141307	0.910874	0.003786	0.709716
-21.371558	-1.941235	0.915878	0.004060	0.709590
-20.720564	-2.052447	0.920883	0.003939	0.709600
-20.411552	-2.109932	0.925888	0.003882	0.709595
-20.948826	-2.014330	0.930893	0.003982	0.709595
-20.439605	-2.103749	0.935898	0.003887	0.709597
-20.471590	-2.102179	0.940902	0.003893	0.709589
-20.740152	-2.149633	0.945907	0.003943	0.709398
-21.895667	-2.012151	0.950912	0.004158	0.709262
-21.710613	-2.045827	0.955917	0.004123	0.709260
-21.253756	-2.124941	0.960922	0.004038	0.709265
-21.854931	-2.020133	0.965926	0.004150	0.709260
-21.540769	-2.072256	0.970931	0.004092	0.709268
-21.307932	-2.117452	0.975936	0.004048	0.709261
-21.834643	-2.099275	0.980941	0.004146	0.709109
-22.666529	-2.024584	0.985946	0.004301	0.708962
-22.562537	-2.048765	0.990950	0.004282	0.708951
-22.499785	-2.054952	0.995955	0.004270	0.708961
-22.758797	-2.012566	1.000960	0.004318	0.708953
-22.726040	-2.019294	1.005965	0.004312	0.708952
-22.396917	-2.075880	1.010970	0.004251	0.708956
-22.823794	-2.003731	1.015974	0.004330	0.708948
-23.051187	-2.110535	1.020979	0.004372	0.708653
-23.235874	-2.086186	1.025984	0.004407	0.708636
-23.461494	-2.045266	1.030989	0.004449	0.708638
-23.260310	-2.079675	1.035994	0.004411	0.708641
-23.292897	-2.078343	1.040998	0.004417	0.708632
-23.202766	-2.089763	1.046003	0.004401	0.708641
-23.319196	-2.098972	1.051008	0.004422	0.708581
-24.297153	-2.040644	1.056013	0.004604	0.708349
-23.566540	-2.167507	1.061018	0.004468	0.708356
-24.197984	-2.059748	1.066022	0.004586	0.708346
-24.444153	-2.012712	1.071027	0.004631	0.708352
-24.091875	-2.077168	1.076032	0.004566	0.708349
-24.442248	-2.014909	1.081037	0.004631	0.708349
-24.206825	-2.110379	1.086042	0.004587	0.708242
-25.236138	-2.043264	1.091046	0.004779	0.708009
-24.618887	-2.147240	1.096051	0.004664	0.708021
-25.282693	-2.032929	1.101056	0.004787	0.708013
-25.168536	-2.055100	1.106061	0.004766	0.708009
-24.707614	-2.133705	1.111066	0.004680	0.708016
-25.293173	-2.032990	1.116070	0.004789	0.708009
-25.460718	-2.056883	1.121075	0.004820	0.707901
-25.769968	-2.102522	1.126080	0.004878	0.707699
-25.472905	-2.157177	1.131085	0.004823	0.707696
-26.007757	-2.056663	1.136090	0.004922	0.707707
-26.023008	-2.059892	1.141094	0.004925	0.707695
-25.557084	-2.140637	1.146099	0.004838	0.707699
-25.911020	-2.079296	1.151104	0.004904	0.707696
-26.320837	-2.117132	1.156109	0.004980	0.707474
-26.696951	-2.097699	1.161114	0.005050	0.707378
-26.669030	-2.106715	1.166118	0.005045	0.707370
-26.745961	-2.090429	1.171123	0.005059	0.707375
-26.717983	-2.096772	1.176128	0.005054	0.707373
-26.902383	-2.063664	1.181133	0.005088	0.707373
-27.008192	-2.043164	1.186138	0.005108	0.707377
-27.075290	-2.133208	1.191142	0.005121	0.707172
-27.526904	-2.099089	1.196147	0.005205	0.707079
-27.371976	-2.129498	1.201152	0.005176	0.707073
-27.704339	-2.069860	1.206157	0.005238	0.707074
-27.331162	-2.132446	1.211162	0.005168	0.707082
-27.317289	-2.140589	1.216166	0.005166	0.707071
-27.513875	-2.138937	1.221171	0.005202	0.707004
-28.396398	-2.108834	1.226176	0.005366	0.706748
-28.098400	-2.162064	1.231181	0.005311	0.706748
-28.375230	-2.109603	1.236186	0.005362	0.706755
-28.676712	-2.061725	1.241190	0.005418	0.706743
-28.467917	-2.095246	1.246195	0.005380	0.706750
-28.520340	-2.088149	1.251200	0.005389	0.706746
-28.748220	-2.103399	1.256205	0.005432	0.706634
-29.107843	-2.131242	1.261210	0.005499	0.706449
-28.954964	-2.163188	1.266214	0.005470	0.706440
-29.512072	-2.061466	1.271219	0.005574	0.706445
-29.472130	-2.072154	1.276224	0.005566	0.706438
-29.549899	-2.058557	1.281229	0.005581	0.706437
-29.486676	-2.065509	1.286234	0.005569	0.706446
-29.847712	-2.024723	1.291238	0.005636	0.706399
-29.976132	-2.135990	1.296243	0.005660	0.706129
-29.715076	-2.185781	1.301248	0.005611	0.706123
-30.604372	-2.027948	1.306253	0.005777	0.706121
-30.108903	-2.112654	1.311258	0.005685	0.706129
-30.167809	-2.107505	1.316262	0.005696	0.706118
-30.450018	-2.052689	1.321267	0.005748	0.706127
-30.187952	-2.133796	1.326272	0.005699	0.706058
-30.649953	-2.150178	1.331277	0.005785	0.705859
-30.768064	-2.127370	1.336282	0.005807	0.705863
-31.456073	-2.008482	1.341286	0.005935	0.705856
-31.042450	-2.078446	1.346291	0.005858	0.705863
-30.625703	-2.155486	1.351296	0.005781	0.705858
-31.170821	-2.058810	1.356301	0.005882	0.705857
-31.202873	-2.158866	1.361306	0.005888	0.705644
-31.797501	-2.115121	1.366310	0.005999	0.705519
-31.855511	-2.101322	1.371315	0.006009	0.705526
-31.916325	-2.091095	1.376320	0.006021	0.705525
-32.173542	-2.047020	1.381325	0.006069	0.705521
-31.730195	-2.123179	1.386330	0.005986	0.705527
-32.170625	-2.048537	1.391334	0.006068	0.705519
-32.172084	-2.159966	1.396339	0.006068	0.705295
-32.799807	-2.090823	1.401344	0.006185	0.705209
-32.751301	-2.101403	1.406349	0.006176	0.705205
-32.698002	-2.107836	1.411354	0.006166	0.705211
-32.765055	-2.100335	1.416358	0.006178	0.705202
-32.800131	-2.090626	1.421363	0.006185	0.705209
-32.803703	-2.089401	1.426368	0.006186	0.705210
-33.112481	-2.179169	1.431373	0.006243	0.704919
-33.573317	-2.112199	1.436378	0.006329	0.704888
-34.071814	-2.026772	1.441382	0.006422	0.704882
-33.537397	-2.118281	1.446387	0.006322	0.704889
-33.382348	-2.147932	1.451392	0.006293	0.704885
-34.024864	-2.035318	1.456397	0.006413	0.704881
-33.765170	-2.077812	1.461402	0.006364	0.704889
-33.743208	-2.207723	1.466406	0.006360	0.704635
-34.466846	-2.101370	1.471411	0.006495	0.704590
-34.671894	-2.067093	1.476416	0.006533	0.704585
-34.420709	-2.113999	1.481421	0.006486	0.704581
-34.293622	-2.133745	1.486426	0.006463	0.704587
-34.585060	-2.085191	1.491430	0.006517	0.704580
-34.474327	-2.123596	1.496435	0.006496	0.704543
-35.194666	-2.138372	1.501440	0.006630	0.704254
-35.476426	-2.088211	1.506445	0.006683	0.704254
-35.510144	-2.077896	1.511450	0.006689	0.704263
-35.384088	-2.106288	1.516454	0.006665	0.704251
-35.169909	-2.141795	1.521459	0.006626	0.704256
-35.635490	-2.057855	1.526464	0.006712	0.704258
-35.365181	-2.124973	1.531469	0.006662	0.704220
-35.591668	-2.217353	1.536474	0.006704	0.703953
-36.311519	-2.092568	1.541478	0.006838	0.703945
-36.644236	-2.030688	1.546483	0.006900	0.703951
-36.087321	-2.129703	1.551488	0.006796	0.703951
-36.373119	-2.080329	1.556493	0.006849	0.703948
-36.518902	-2.052049	1.561498	0.006876	0.703953
-36.271758	-2.111044	1.566502	0.006830	0.703923
-36.717452	-2.172714	1.571507	0.006913	0.703638
-37.323001	-2.066253	1.576512	0.007026	0.703635
-37.582833	-2.022668	1.581517	0.007074	0.703630
-36.998913	-2.121780	1.586522	0.006966	0.703640
-37.322919	-2.070428	1.591526	0.007026	0.703627
-37.341127	-2.063153	1.596531	0.007029	0.703635
-37.095363	-2.107971	1.601536	0.006984	0.703633
-37.636680	-2.139887	1.606541	0.007084	0.703374
-38.120098	-2.068267	1.611546	0.007174	0.703345
-38.293547	-2.041899	1.616550	0.007206	0.703336
-37.822229	-2.121906	1.621555	0.007119	0.703344
-38.214060	-2.053237	1.626560	0.007192	0.703342
-38.457233	-2.012620	1.631565	0.007237	0.703336
-37.615376	-2.158924	1.636570	0.007080	0.703344
-38.444881	-2.149835	1.641574	0.007235	0.703064
-39.202375	-2.042904	1.646579	0.007375	0.703007
-38.663978	-2.138391	1.651584	0.007275	0.703008
-38.804259	-2.114804	1.656589	0.007301	0.703005
-39.304600	-2.024003	1.661594	0.007394	0.703008
-39.162751	-2.053695	1.666598	0.007368	0.703000
-38.640163	-2.143079	1.671603	0.007271	0.703007
-39.318049	-2.148976	1.676608	0.007397	0.702751
-40.043026	-2.050955	1.681613	0.007532	0.702688
-39.655244	-2.114337	1.686618	0.007460	0.702700
-39.754146	-2.102529	1.691622	0.007478	0.702688
-40.138698	-2.031060	1.696627	0.007549	0.702694
-39.858487	-2.081943	1.701632	0.007497	0.702692
-39.914088	-2.073569	1.706637	0.007508	0.702689
-40.219055	-2.120063	1.711642	0.007564	0.702486
-41.058964	-2.030723	1.716646	0.007721	0.702363
-40.560477	-2.117594	1.721651	0.007628	0.702368
-40.473035	-2.132639	1.726656	0.007612	0.702369
-41.150780	-2.013871	1.731661	0.007738	0.702365
-40.513549	-2.124516	1.736666	0.007619	0.702371
-40.718345	-2.090194	1.741670	0.007657	0.702366
-41.336057	-2.060494	1.746675	0.007772	0.702204
-41.907444	-2.023868	1.751680	0.007878	0.702072
-41.430627	-2.111701	1.756685	0.007790	0.702066
-41.627493	-2.073158	1.761690	0.007826	0.702073
-41.961980	-2.016597	1.766694	0.007888	0.702067
-41.615224	-2.077186	1.771699	0.007824	0.702070
-41.501823	-2.096745	1.776704	0.007803	0.702071
-41.938205	-2.049452	1.781709	0.007884	0.702009
-42.136874	-2.146118	1.786714	0.007921	0.701742
-42.430213	-2.098974	1.791718	0.007976	0.701732
-42.967501	-1.999498	1.796723	0.008076	0.701739
-42.300969	-2.118962	1.801728	0.007951	0.701738
-42.340115	-2.113982	1.806733	0.007959	0.701734
-42.706244	-2.043020	1.811738	0.008027	0.701746
-42.881837	-2.033650	1.816742	0.008059	0.701701
-43.173858	-2.114032	1.821747	0.008114	0.701433
-43.149230	-2.118610	1.826752	0.008109	0.701433
-43.859541	-1.993987	1.831757	0.008241	0.701429
-43.288557	-2.092136	1.836762	0.008135	0.701437
-43.291113	-2.095761	1.841766	0.008136	0.701428
-43.816249	-1.999646	1.846771	0.008233	0.701433
-43.346068	-2.087107	1.851776	0.008146	0.701426
-43.818057	-2.156807	1.856781	0.008234	0.701115
-43.899268	-2.137580	1.861786	0.008249	0.701124
-44.467642	-2.041500	1.866790	0.008354	0.701114
-44.210488	-2.085232	1.871795	0.008306	0.701118
-44.146748	-2.095590	1.876800	0.008295	0.701120
-44.736447	-1.993049	1.881805	0.008404	0.701115
-43.925414	-2.166800	1.886810	0.008253	0.701056
-44.576426	-2.143978	1.891814	0.008375	0.700867
-44.995249	-2.066782	1.896819	0.008452	0.700872
-44.978659	-2.069042	1.901824	0.008449	0.700874
-44.712403	-2.118673	1.906829	0.008400	0.700870
-44.434402	-2.165199	1.911834	0.008348	0.700876
-44.943929	-2.099525	1.916838	0.008443	0.700825
-45.600516	-2.126693	1.921843	0.008565	0.700533
-45.226836	-2.192671	1.926848	0.008495	0.700534
-46.173251	-2.026626	1.931853	0.008672	0.700528
-45.895670	-2.070923	1.936858	0.008620	0.700539
-45.738835	-2.104469	1.941862	0.008591	0.700528
-45.908994	-2.069268	1.946867	0.008622	0.700538
-45.867691	-2.154163	1.951872	0.008615	0.700381
-46.968958	-2.040286	1.956877	0.008819	0.700213
-46.385043	-2.139871	1.961882	0.008711	0.700223
-46.882180	-2.055135	1.966886	0.008803	0.700215
-47.017631	-2.029434	1.971891	0.008828	0.700218
-46.403424	-2.138654	1.976896	0.008714	0.700219
-46.934798	-2.047428	1.981901	0.008813	0.700212
-46.864242	-2.140542	1.986906	0.008800	0.700048
-47.422463	-2.118387	1.991910	0.008904	0.699891
-47.432423	-2.113951	1.996915	0.008906	0.699897
-47.616582	-2.083498	2.001920	0.008940	0.699892

-47.601113	-2.085475	2.011917	0.008937	0.699894
-47.442348	-2.115087	2.021914	0.008907	0.699891
-48.361604	-2.087759	2.031910	0.009078	0.699614
-48.316644	-2.104813	2.041907	0.009070	0.699596
-48.381318	-2.094192	2.051904	0.009082	0.699594
-48.168460	-2.066651	2.061901	0.009042	0.699727
-47.555475	-2.094895	2.071898	0.008928	0.699892
-47.832249	-2.046334	2.081894	0.008979	0.699890
-47.517856	-2.102390	2.091891	0.008921	0.699891
-47.732049	-2.064450	2.101888	0.008961	0.699890
-47.404974	-2.121998	2.111885	0.008900	0.699892
-47.737047	-2.063421	2.121882	0.008961	0.699891
-47.651508	-2.080013	2.131878	0.008945	0.699888
-47.551184	-2.097546	2.141875	0.008927	0.699889
-47.159492	-2.082375	2.151872	0.008854	0.700062
-46.590432	-2.108793	2.161869	0.008748	0.700214
-46.927655	-2.049761	2.171866	0.008810	0.700212
-46.623358	-2.103130	2.181862	0.008754	0.700214
-46.534375	-2.119989	2.191859	0.008737	0.700212
-46.320888	-2.026548	2.201856	0.008697	0.700479
-45.810842	-2.092706	2.211853	0.008602	0.700529
-45.711062	-2.108214	2.221850	0.008584	0.700534
-45.906874	-2.073900	2.231846	0.008620	0.700533
-45.313061	-2.039348	2.241843	0.008509	0.700818
-45.113464	-2.048934	2.251840	0.008472	0.700871
-44.672504	-2.126979	2.261837	0.008390	0.700872
-45.049164	-2.057524	2.271834	0.008460	0.700877
-44.406022	-2.052029	2.281830	0.008340	0.701120
-44.394140	-2.055101	2.291827	0.008338	0.701118
-44.307697	-2.069578	2.301824	0.008322	0.701120
-43.675359	-2.094147	2.311821	0.008204	0.701299
-43.368231	-2.081121	2.321818	0.008147	0.701437
-43.462631	-2.065357	2.331814	0.008164	0.701435
-43.444584	-2.052659	2.341811	0.008161	0.701467
-42.786342	-2.034182	2.351808	0.008038	0.701742
-42.318306	-2.115543	2.361805	0.007951	0.701746
-42.709006	-2.046134	2.371802	0.008023	0.701746
-42.071952	-2.041902	2.381798	0.007905	0.701984
-41.721078	-2.061027	2.391795	0.007839	0.702072
-41.700299	-2.063445	2.401792	0.007835	0.702075
-41.359360	-2.095902	2.411789	0.007772	0.702133
-40.856808	-2.067925	2.421786	0.007678	0.702371
-40.597061	-2.114073	2.431782	0.007630	0.702371
-41.127280	-2.020757	2.441779	0.007728	0.702369
-40.253738	-2.052429	2.451776	0.007566	0.702620
-39.859641	-2.086604	2.461773	0.007492	0.702693
-40.100749	-2.041088	2.471770	0.007537	0.702698
-39.885750	-2.027427	2.481766	0.007497	0.702803
-39.334084	-2.026814	2.491763	0.007394	0.703003
-39.086906	-2.071067	2.501760	0.007348	0.703003
-39.127973	-2.056149	2.511757	0.007356	0.703018
-38.400358	-2.026564	2.521754	0.007220	0.703340
-38.109479	-2.078686	2.531750	0.007166	0.703340
-38.304615	-2.044308	2.541747	0.007202	0.703339
-37.919752	-2.047368	2.551744	0.007130	0.703472
-37.347874	-2.070473	2.561741	0.007024	0.703631
-37.501372	-2.042281	2.571738	0.007052	0.703633
-37.063063	-2.119099	2.581734	0.006971	0.703635
-36.627436	-2.041061	2.591731	0.006890	0.703950
-36.443837	-2.074248	2.601728	0.006855	0.703949
-36.487392	-2.067052	2.611725	0.006863	0.703948
-36.128762	-2.056691	2.621722	0.006796	0.704098
-35.401625	-2.106855	2.631718	0.006661	0.704258
-35.712483	-2.052818	2.641715	0.006719	0.704256
-35.499881	-2.090671	2.651712	0.006679	0.704256
-34.911146	-2.037727	2.661709	0.006569	0.704574
-34.692551	-2.070714	2.671706	0.006529	0.704586
-34.605155	-2.086632	2.681702	0.006512	0.704586
-34.695977	-1.998824	2.691699	0.006529	0.704730
-33.604013	-2.117479	2.701696	0.006326	0.704884
-33.805506	-2.081585	2.711693	0.006363	0.704884
-33.818633	-2.078224	2.721690	0.006366	0.704886
-33.038668	-2.065392	2.731686	0.006220	0.705192
-33.266345	-2.018115	2.741683	0.006263	0.705205
-32.712838	-2.117282	2.751680	0.006160	0.705204
-32.838124	-2.020585	2.761677	0.006183	0.705354
-31.929008	-2.097361	2.771674	0.006013	0.705526
-32.035428	-2.080048	2.781670	0.006033	0.705523
-32.057117	-2.076286	2.791667	0.006037	0.705523
-31.387053	-2.034853	2.801664	0.005912	0.705847
-31.279388	-2.048244	2.811661	0.005892	0.705858
-30.924341	-2.110280	2.821658	0.005826	0.705861
-30.965843	-2.045471	2.831654	0.005834	0.705977
-30.366684	-2.078803	2.841651	0.005722	0.706124
-30.554090	-2.045772	2.851648	0.005757	0.706124
-30.512276	-2.034438	2.861645	0.005749	0.706162
-29.716949	-2.036801	2.871642	0.005601	0.706442
-29.688697	-2.041164	2.881638	0.005596	0.706444
-29.706894	-2.038181	2.891635	0.005599	0.706443
-28.962394	-2.035119	2.901632	0.005460	0.706716
-29.088032	-1.996098	2.911629	0.005483	0.706750
-28.723074	-2.060596	2.921626	0.005415	0.706751
-28.428223	-2.008224	2.931622	0.005360	0.706962
-27.937096	-2.037134	2.941619	0.005269	0.707080
-27.809607	-2.060820	2.951616	0.005245	0.707078
-27.968700	-2.000410	2.961613	0.005275	0.707142
-26.872239	-2.079021	2.971610	0.005071	0.707377
-27.038800	-2.050995	2.981606	0.005101	0.707374
-26.965250	-2.064638	2.991603	0.005088	0.707373
-26.565560	-2.022284	3.001600	0.005013	0.707601
-26.352381	-2.011606	3.011597	0.004973	0.707698
-25.958717	-2.082112	3.021594	0.004900	0.707698
-26.124334	-2.009015	3.031590	0.004931	0.707785
-25.091716	-2.079713	3.041587	0.004739	0.708013
-25.278508	-2.047187	3.051584	0.004773	0.708011
-25.115294	-2.075681	3.061581	0.004743	0.708013
-24.678154	-2.039422	3.071578	0.004661	0.708242
-24.555291	-2.007139	3.081574	0.004638	0.708350
-24.246167	-2.064173	3.091571	0.004581	0.708347
-24.449507	-1.992465	3.101568	0.004618	0.708418
-23.495339	-2.052773	3.111565	0.004441	0.708638
-23.379906	-2.072984	3.121562	0.004419	0.708639
-23.553359	-2.042252	3.131558	0.004451	0.708639
-22.738658	-2.072357	3.141555	0.004300	0.708869
-22.751520	-2.029183	3.151552	0.004302	0.708951
-22.346840	-2.100436	3.161549	0.004227	0.708953
-22.595992	-2.034860	3.171546	0.004273	0.708996
-21.997221	-2.007827	3.181542	0.004161	0.709263
-21.725515	-2.058074	3.191539	0.004111	0.709260
-21.884156	-2.029515	3.201536	0.004140	0.709261
-20.944503	-2.065836	3.211533	0.003965	0.709523
-20.900769	-2.037946	3.221530	0.003957	0.709595
-20.920924	-2.034029	3.231526	0.003961	0.709595
-20.947387	-1.992921	3.241523	0.003965	0.709668
-20.077401	-2.038400	3.251520	0.003803	0.709887
-19.917300	-2.065552	3.261517	0.003774	0.709890
-20.223534	-2.009948	3.271514	0.003830	0.709893
-19.431844	-2.007491	3.281510	0.003683	0.710180
-19.161429	-2.039127	3.291507	0.003633	0.710213
-19.362349	-2.002995	3.301504	0.003670	0.710214
-18.790071	-2.025058	3.311501	0.003563	0.710373
-18.173164	-2.054506	3.321498	0.003448	0.710534
-18.315018	-2.030192	3.331494	0.003475	0.710533
-18.243048	-2.044610	3.341491	0.003461	0.710529
-17.647456	-1.991956	3.351488	0.003350	0.710847
-17.072105	-2.081789	3.361485	0.003243	0.710872
-17.490899	-2.006833	3.371482	0.003321	0.710873
-17.248423	-1.997334	3.381478	0.003276	0.710978
-16.615358	-2.031112	3.391475	0.003158	0.711136
-16.869224	-1.986174	3.401472	0.003205	0.711136
-16.696931	-1.992426	3.411469	0.003173	0.711185
-15.931075	-1.993582	3.421466	0.003030	0.711455
-15.707772	-2.033635	3.431462	0.002989	0.711454
-15.723645	-2.033340	3.441459	0.002991	0.711449
-15.235894	-2.004286	3.451456	0.002901	0.711681
-14.836096	-2.036474	3.461453	0.002826	0.711759
-14.868489	-2.029631	3.471450	0.002832	0.711761
-14.481012	-2.074085	3.481446	0.002760	0.711810
-13.990740	-2.022983	3.491443	0.002668	0.712086
-13.892821	-2.042026	3.501440	0.002650	0.712083
-13.750061	-2.065961	3.511437	0.002623	0.712086
-13.523672	-2.029334	3.521434	0.002581	0.712240
-12.822067	-2.081916	3.531430	0.002451	0.712384
-12.922322	-2.065217	3.541427	0.002469	0.712382
-12.867464	-2.074429	3.551424	0.002459	0.712383
-12.293600	-2.036296	3.561421	0.002352	0.712663
-12.109478	-2.045343	3.571418	0.002318	0.712710
-11.650118	-2.126864	3.581414	0.002232	0.712711
-12.125677	-2.025355	3.591411	0.002320	0.712745
-11.208115	-2.050308	3.601408	0.002150	0.713021
-11.014509	-2.083220	3.611405	0.002113	0.713024
-10.912799	-2.100898	3.621402	0.002094	0.713025
-10.543129	-2.097939	3.631398	0.002026	0.713162
-10.149197	-2.068878	3.641395	0.001952	0.713360
-9.861405	-2.120259	3.651392	0.001898	0.713360
-9.887960	-2.115004	3.661389	0.001903	0.713361
-9.807934	-2.062919	3.671386	0.001888	0.713493
-8.920113	-2.138549	3.681382	0.001723	0.713657
-9.222432	-2.086010	3.691379	0.001779	0.713655
-8.916585	-2.141000	3.701376	0.001722	0.713654
-8.586485	-2.092313	3.711373	0.001661	0.713867
-8.310299	-2.088812	3.721370	0.001609	0.713972
-8.166077	-2.115123	3.731366	0.001582	0.713971
-8.182418	-2.108227	3.741363	0.001585	0.713979
-7.453028	-2.089002	3.751360	0.001449	0.714276
-7.301453	-2.115639	3.761357	0.001421	0.714277
-7.249199	-2.123677	3.771354	0.001411	0.714279
-7.110209	-2.071341	3.781350	0.001385	0.714433
-6.427424	-2.106382	3.791347	0.001258	0.714605
-6.211592	-2.144152	3.801344	0.001218	0.714606
-6.328151	-2.123491	3.811341	0.001239	0.714606
-5.861459	-2.103001	3.821338	0.001153	0.714812
-5.612594	-2.097549	3.831334	0.001106	0.714911
-5.681447	-2.086530	3.841331	0.001119	0.714909
-5.501420	-2.082239	3.851328	0.001085	0.714981
-4.736935	-2.091180	3.861325	0.000943	0.715233
-4.547286	-2.125071	3.871322	0.000907	0.715233
-4.563788	-2.122788	3.881318	0.000910	0.715232
-4.303502	-2.070394	3.891315	0.000862	0.715428
-3.634840	-2.131481	3.901312	0.000737	0.715543
-3.728840	-2.113343	3.911309	0.000755	0.715546
-3.524179	-2.150025	3.921306	0.000717	0.715546
-3.127147	-2.051202	3.931302	0.000643	0.715882
-2.683454	-2.130109	3.941299	0.000560	0.715883
-2.646521	-2.137188	3.951296	0.000553	0.715882
-2.742692	-2.076857	3.961293	0.000571	0.715967
-2.303629	-2.071469	3.971290	0.000489	0.716133
-2.180017	-2.093003	3.981286	0.000466	0.716134
-2.261328	-2.048481	3.991283	0.000481	0.716194
-1.780002	-2.007456	4.001280	0.000391	0.716445
-1.303366	-2.091281	4.011277	0.000302	0.716447
-1.886986	-1.945546	4.021274	0.000411	0.716530
-1.381149	-1.920236	4.031270	0.000317	0.716759
-1.514420	-1.896918	4.041267	0.000341	0.716758
-1.373805	-1.798456	4.051264	0.000315	0.717003
-1.231888	-1.783508	4.061261	0.000289	0.717082
-1.307538	-1.683020	4.071258	0.000303	0.717255
-0.750492	-1.718881	4.081254	0.000199	0.717380
-1.175702	-1.564276	4.091251	0.000278	0.717536
-1.192692	-1.478214	4.101248	0.000281	0.717700
-0.895338	-1.417432	4.111245	0.000225	0.717925
-0.599586	-1.422947	4.121242	0.000170	0.718019
-0.552655	-1.270537	4.131238	0.000161	0.718336
-0.693040	-1.192724	4.141235	0.000187	0.718441
-0.725759	-1.085662	4.151232	0.000193	0.718641
-0.758209	-0.947294	4.161229	0.000199	0.718902
-0.979696	-0.805994	4.171226	0.000240	0.719103
-0.428151	-0.799686	4.181222	0.000137	0.719310
-0.614655	-0.620160	4.191219	0.000172	0.719598
-0.276499	-0.550709	4.201216	0.000109	0.719854
-0.143549	-0.455457	4.211213	0.000084	0.720089
-0.134684	-0.329178	4.221210	0.000082	0.720341
-0.228360	-0.179791	4.231206	0.000100	0.720602
-0.419469	0.004231	4.241203	0.000135	0.720897
-0.154421	0.074148	4.251200	0.000085	0.721128
0.000000	0.255839	4.261197	0.000057	0.721539

0.148193	0.852654	4.266202	0.000029	0.722764
0.366472	2.087985	4.271206	-0.000013	0.725260
0.692964	3.886336	4.276211	-0.000075	0.728882
0.919199	6.259946	4.281216	-0.000119	0.733565
1.324824	9.115190	4.286221	-0.000196	0.739204
1.390852	12.501295	4.291226	-0.000211	0.745695
1.821376	16.284775	4.296230	-0.000293	0.753002
2.226707	20.468432	4.301235	-0.000372	0.760977
2.559806	25.067645	4.306240	-0.000437	0.769611
2.811715	30.053519	4.311245	-0.000487	0.778827
3.260076	35.340712	4.316250	-0.000574	0.788540
3.910117	40.923037	4.321254	-0.000698	0.798723
4.271326	46.849164	4.326259	-0.000770	0.809290
4.703279	53.048843	4.331264	-0.000854	0.820216
5.240025	59.510749	4.336269	-0.000958	0.831477
5.579435	66.215983	4.341274	-0.001026	0.842938
5.864729	73.161553	4.346278	-0.001084	0.854628
6.648083	80.218376	4.351283	-0.001234	0.866486
8.264332	87.326751	4.356288	-0.001540	0.878503
11.564897	94.363861	4.361293	-0.002159	0.890715
12.085093	102.054005	4.366298	-0.002261	0.903019
13.784195	109.706631	4.371302	-0.002582	0.915419
14.465569	117.643788	4.376307	-0.002714	0.927815
15.386646	125.669794	4.381312	-0.002891	0.940245
16.296383	133.812407	4.386317	-0.003066	0.952682
17.115897	142.039814	4.391322	-0.003224	0.965060
17.871412	150.371178	4.396326	-0.003370	0.977415
18.682619	158.773367	4.401331	-0.003526	0.989731
19.684827	167.175081	4.406336	-0.003719	1.001941
20.618166	175.632715	4.411341	-0.003898	1.014065
21.028148	184.207191	4.416346	-0.003980	1.026082
22.019649	192.731977	4.421350	-0.004170	1.038029
22.809833	201.307693	4.426355	-0.004323	1.049861
23.380068	209.948354	4.431360	-0.004435	1.061596
24.133079	218.595819	4.436365	-0.004581	1.073254
24.802437	227.234932	4.441370	-0.004711	1.084756
25.503561	235.897553	4.446374	-0.004847	1.096175
26.329209	244.519808	4.451379	-0.005006	1.107451
26.925844	253.194490	4.456384	-0.005123	1.118629
27.316882	261.907413	4.461389	-0.005202	1.129701
27.659246	270.603720	4.466394	-0.005271	1.140634
28.471908	279.250526	4.471398	-0.005428	1.151501
29.208170	287.866450	4.476403	-0.005571	1.162212
29.864462	296.488756	4.481408	-0.005699	1.172816
30.543515	305.096815	4.486413	-0.005831	1.183313
30.906735	313.750472	4.491418	-0.005904	1.193707
31.282140	322.367586	4.496422	-0.005980	1.203970
31.820686	330.959119	4.501427	-0.006086	1.214149
32.502558	339.502851	4.506432	-0.006218	1.224216
32.729343	348.146132	4.511437	-0.006266	1.234227
33.343818	356.649114	4.516442	-0.006386	1.244071
34.196274	365.135540	4.521446	-0.006550	1.253865
34.784293	373.639000	4.526451	-0.006665	1.263552
35.179743	382.185036	4.531456	-0.006745	1.273175
35.626440	390.688355	4.536461	-0.006833	1.282689
36.121285	399.165581	4.541466	-0.006931	1.292113
36.413080	407.678177	4.546470	-0.006991	1.301469
36.953657	416.195750	4.551475	-0.007097	1.310809
37.466392	424.688979	4.556480	-0.007198	1.320052
37.868631	433.111437	4.561485	-0.007279	1.329135
38.119129	441.552592	4.566490	-0.007331	1.338149
38.772302	449.906981	4.571494	-0.007458	1.347082
39.067734	458.335835	4.576499	-0.007519	1.355972
39.225085	466.743171	4.581504	-0.007553	1.364757
39.892863	475.088154	4.586509	-0.007683	1.373509
40.281776	483.448118	4.591514	-0.007761	1.382174
40.618093	491.842691	4.596518	-0.007829	1.390810
41.036835	500.190822	4.601523	-0.007913	1.399360
41.455838	508.521353	4.606528	-0.007996	1.407840
42.176201	516.829397	4.611533	-0.008136	1.416297
42.391599	525.175446	4.616538	-0.008181	1.424658
42.840616	533.520846	4.621542	-0.008270	1.433007
43.122547	541.840925	4.626547	-0.008328	1.441256
43.406599	550.169042	4.631552	-0.008387	1.449466
44.008014	558.458465	4.636557	-0.008504	1.457643
44.502956	566.721739	4.641562	-0.008602	1.465732
44.927257	575.078877	4.646566	-0.008686	1.473855
45.186637	583.369381	4.651571	-0.008740	1.481844
45.460303	591.650841	4.656576	-0.008796	1.489784
46.017981	599.904429	4.661581	-0.008906	1.497699
46.368592	608.151504	4.666586	-0.008976	1.505534
46.854777	616.427965	4.671590	-0.009072	1.513377
47.275712	624.664144	4.676595	-0.009156	1.521132
47.478376	632.946777	4.681600	-0.009199	1.528857
47.911541	641.201175	4.686605	-0.009285	1.536552
48.175017	649.446815	4.691610	-0.009340	1.544175
48.709007	657.697454	4.696614	-0.009445	1.551805
49.204568	665.913846	4.701619	-0.009542	1.559361
49.430739	674.152650	4.706624	-0.009590	1.566861
50.029439	682.375985	4.711629	-0.009707	1.574366
50.000867	690.650345	4.716634	-0.009707	1.581790
50.341738	698.882404	4.721638	-0.009776	1.589194
50.618516	707.122277	4.726643	-0.009832	1.596562
50.962123	715.312976	4.731648	-0.009902	1.603862
51.266204	723.538549	4.736653	-0.009964	1.611154
51.582077	731.744079	4.741658	-0.010028	1.618396
51.854499	739.961845	4.746662	-0.010084	1.625612
52.041251	748.237012	4.751667	-0.010124	1.632833
52.584418	756.381395	4.756672	-0.010231	1.639958
53.233276	764.521944	4.761677	-0.010357	1.647063
53.352916	772.754786	4.766682	-0.010385	1.654145
53.785413	780.927752	4.771686	-0.010471	1.661188
54.435503	789.064403	4.776691	-0.010597	1.668199
54.706981	797.280586	4.781696	-0.010653	1.675198
54.809095	805.496195	4.786701	-0.010677	1.682144
55.152217	813.662360	4.791706	-0.010747	1.689051
55.498624	821.864087	4.796710	-0.010816	1.695961
55.681696	830.053013	4.801715	-0.010856	1.702811
56.105704	838.219641	4.806720	-0.010940	1.709646
56.374764	846.429641	4.811725	-0.010996	1.716469
56.673807	854.566877	4.816730	-0.011057	1.723209
56.886288	862.748006	4.821734	-0.011102	1.729948
57.317323	870.902702	4.826739	-0.011187	1.736667
57.893130	879.012590	4.831744	-0.011300	1.743342
58.239240	887.186641	4.836749	-0.011370	1.750014
58.571900	895.351778	4.841754	-0.011437	1.756651
59.243278	903.456826	4.846758	-0.011567	1.763258
59.290066	911.663597	4.851763	-0.011581	1.769844
59.617552	919.828738	4.856768	-0.011648	1.776406
60.265051	927.943039	4.861773	-0.011774	1.782944
60.217747	936.169828	4.866778	-0.011770	1.789461
60.646803	944.360253	4.871782	-0.011855	1.795984
60.995256	952.471202	4.876787	-0.011926	1.802411
61.214492	960.611515	4.881792	-0.011972	1.808822
61.540613	968.768642	4.886797	-0.012038	1.815237
61.971490	976.872140	4.891802	-0.012123	1.821599
62.207667	985.030982	4.896806	-0.012173	1.827959
62.220077	993.231090	4.901811	-0.012180	1.834303
62.409382	1001.355141	4.906816	-0.012221	1.840587
63.017269	1009.448001	4.911821	-0.012339	1.846874
63.250051	1017.601814	4.916826	-0.012388	1.853143
63.725550	1025.710044	4.921830	-0.012482	1.859384
63.943063	1033.849230	4.926835	-0.012528	1.865598
64.211615	1042.013763	4.931840	-0.012583	1.871816
64.684486	1050.124252	4.936845	-0.012677	1.877996
64.972979	1058.229344	4.941850	-0.012736	1.884131
65.736463	1066.299931	4.946854	-0.012883	1.890274
65.985231	1074.476715	4.951859	-0.012935	1.896417
66.078880	1082.617598	4.956864	-0.012958	1.902497
66.621284	1090.734732	4.961869	-0.013064	1.908590
66.928928	1098.865917	4.966874	-0.013126	1.914647
67.134817	1106.995755	4.971878	-0.013170	1.920673
67.349089	1115.129037	4.976883	-0.013215	1.926684
67.589546	1123.273753	4.981888	-0.013265	1.932687
68.264555	1131.354888	4.986893	-0.013396	1.938672
68.529801	1139.456960	4.991898	-0.013451	1.944610
69.005388	1147.598055	4.996902	-0.013545	1.950580
69.461399	1155.727555	5.001907	-0.013635	1.956522
69.332432	1163.870901	5.006912	-0.013617	1.962392
69.604201	1171.976881	5.011917	-0.013673	1.968261
70.011854	1180.062201	5.016922	-0.013754	1.974112
70.267517	1188.155251	5.021926	-0.013807	1.979936
70.424512	1196.277646	5.026931	-0.013841	1.985752
70.750474	1204.381307	5.031936	-0.013907	1.991556
71.119267	1212.495049	5.036941	-0.013981	1.997355
71.342592	1220.575876	5.041946	-0.014028	2.003098
71.540572	1228.708218	5.046950	-0.014070	2.008858
72.053522	1236.791935	5.051955	-0.014171	2.014601
72.310928	1244.877221	5.056960	-0.014224	2.020301
72.793697	1252.965048	5.061965	-0.014320	2.026011
72.956584	1261.116302	5.066970	-0.014355	2.031716
73.064439	1269.256934	5.071974	-0.014381	2.037391
73.168911	1277.353966	5.076979	-0.014405	2.043021
73.655040	1285.409728	5.081984	-0.014501	2.048644
73.976692	1293.533891	5.086989	-0.014566	2.054283
74.221400	1301.613102	5.091994	-0.014617	2.059868
74.495893	1309.707820	5.096998	-0.014674	2.065451
75.024161	1317.782827	5.102003	-0.014777	2.071031
75.544660	1325.861488	5.107008	-0.014880	2.076598
75.782853	1333.983157	5.112013	-0.014929	2.082151
75.924059	1342.071523	5.117018	-0.014961	2.087657
76.064651	1350.215388	5.122022	-0.014992	2.093185
76.280939	1358.311847	5.127027	-0.015038	2.098675
76.872614	1366.339822	5.132032	-0.015153	2.104141
77.121983	1374.479365	5.137037	-0.015205	2.109634
77.161342	1382.652006	5.142042	-0.015218	2.115114
77.575635	1390.691025	5.147046	-0.015300	2.120527
77.835096	1398.761733	5.152051	-0.015354	2.125933
77.988255	1406.855796	5.157056	-0.015388	2.131330
78.456357	1414.934692	5.162061	-0.015480	2.136734
78.684720	1423.000058	5.167066	-0.015528	2.142091
78.890970	1431.099393	5.172070	-0.015572	2.147456
79.217070	1439.197260	5.177075	-0.015638	2.152818
79.464660	1447.278240	5.182080	-0.015689	2.158148
79.842134	1455.352038	5.187085	-0.015765	2.163472
79.963083	1463.438083	5.192090	-0.015793	2.168767
80.157545	1471.551997	5.197094	-0.015834	2.174074
80.504616	1479.629603	5.202099	-0.015904	2.179359
80.833747	1487.673496	5.207104	-0.015971	2.184607
81.242934	1495.780952	5.212109	-0.016052	2.189891
81.478921	1503.878099	5.217114	-0.016101	2.195140
81.824093	1511.936675	5.222118	-0.016171	2.200361
82.112910	1520.007042	5.227123	-0.016230	2.205572
82.518515	1528.060027	5.232128	-0.016311	2.210771
82.695765	1536.189091	5.237133	-0.016349	2.215985
82.921625	1544.254671	5.242138	-0.016396	2.221150
83.270524	1552.326359	5.247142	-0.016467	2.226319
83.738251	1560.407556	5.252147	-0.016559	2.231492
83.646358	1568.521775	5.257152	-0.016547	2.236624
84.317530	1576.535346	5.262157	-0.016678	2.241748
84.746636	1584.584174	5.267162	-0.016763	2.246862
84.912672	1592.707935	5.272166	-0.016799	2.251987
85.061855	1600.807371	5.277171	-0.016832	2.257085
85.383379	1608.861617	5.282176	-0.016897	2.262157
85.549374	1616.965263	5.287181	-0.016933	2.267236
85.604428	1625.109097	5.292186	-0.016949	2.272318
86.114700	1633.160757	5.297190	-0.017049	2.277371
86.685780	1641.167133	5.302195	-0.017161	2.282390
86.490447	1649.276339	5.307200	-0.017130	2.287396
87.038712	1657.326533	5.312205	-0.017237	2.292417
87.128957	1665.412676	5.317210	-0.017259	2.297411
87.474997	1673.451633	5.322214	-0.017329	2.302387
87.815690	1681.524745	5.327219	-0.017398	2.307372
87.967092	1689.615478	5.332224	-0.017431	2.312342
88.410208	1697.666190	5.337229	-0.017519	2.317300
88.609392	1705.720392	5.342234	-0.017561	2.322230
88.877107	1713.794575	5.347238	-0.017617	2.327167
88.999771	1721.895822	5.352243	-0.017645	2.332098
89.317845	1729.953189	5.357248	-0.017709	2.337009
89.656670	1738.015610	5.362253	-0.017778	2.341913
90.120615	1746.041702	5.367258	-0.017869	2.346796
90.494587	1754.156168	5.372262	-0.017944	2.351714
90.544553	1762.254747	5.377267	-0.017959	2.356586
90.801199	1770.291424	5.382272	-0.018012	2.361427
91.266495	1778.330218	5.387277	-0.018104	2.366277
91.333192	1786.431645	5.392282	-0.018122	2.371121
91.302397	1794.528207	5.397286	-0.018121	2.375946
91.671074	1802.572091	5.402291	-0.018195	2.380761
91.817192	1810.624978	5.407296	-0.018228	2.385554
92.147913	1818.710598	5.412301	-0.018294	2.390371
92.540968	1826.763733	5.417306	-0.018373	2.395164
92.718114	1834.832698	5.422310	-0.018411	2.399940
92.763583	1842.910208	5.427315	-0.018425	2.404701
93.064439	1850.942934	5.432320	-0.018486	2.409446
93.692631	1859.009201	5.437325	-0.018608	2.414227
93.763233	1867.078595	5.442330	-0.018627	2.418957
93.926662	1875.142450	5.447334	-0.018663	2.423682
94.149018	1883.208199	5.452339	-0.018709	2.428403
94.257890	1891.348279	5.457344	-0.018735	2.433150
94.462700	1899.419328	5.462349	-0.018778	2.437854
94.770040	1907.399902	5.467354	-0.018841	2.442505
94.998795	1915.450510	5.472358	-0.018889	2.447181
95.233353	1923.519969	5.477363	-0.018938	2.451860
95.466415	1931.573217	5.482368	-0.018986	2.456520
95.942930	1939.608142	5.487373	-0.019080	2.461179
96.010619	1947.671244	5.492378	-0.019098	2.465815
96.225403	1955.752178	5.497382	-0.019144	2.470463
96.729084	1963.789522	5.502387	-0.019243	2.475099
96.954017	1971.827927	5.507392	-0.019290	2.479706
97.199628	1979.890533	5.512397	-0.019341	2.484320
97.445088	1987.943872	5.517402	-0.019392	2.488920
97.773806	1996.023498	5.522406	-0.019458	2.493532
97.876170	2004.093833	5.527411	-0.019483	2.498114
98.003388	2012.138569	5.532416	-0.019512	2.502675
98.492246	2020.189330	5.537421	-0.019608	2.507258
98.563818	2028.294183	5.542426	-0.019627	2.511832
98.722668	2036.386260	5.547430	-0.019661	2.516396
98.930161	2044.405669	5.552435	-0.019705	2.520916
99.093320	2052.426897	5.557440	-0.019741	2.525425
99.498982	2060.474803	5.562445	-0.019822	2.529958
99.683404	2068.549459	5.567450	-0.019861	2.534482
99.909724	2076.593815	5.572454	-0.019909	2.538984
100.234457	2084.648200	5.577459	-0.019975	2.543491
100.435514	2092.694855	5.582464	-0.020017	2.547976
100.925537	2100.742216	5.587469	-0.020114	2.552474
101.095348	2108.801523	5.592474	-0.020151	2.556949
101.113909	2116.862839	5.597478	-0.020159	2.561406
101.378291	2124.904871	5.602483	-0.020214	2.565862
101.847096	2132.940353	5.607488	-0.020307	2.570321
102.187389	2141.026740	5.612493	-0.020375	2.574790
102.432525	2149.058536	5.617498	-0.020426	2.579216
102.740917	2157.108881	5.622502	-0.020489	2.583649
102.781771	2165.208240	5.627507	-0.020502	2.588082
102.927846	2173.376149	5.632512	-0.020534	2.592552
103.573568	2181.437874	5.637517	-0.020660	2.596991
103.630634	2189.433701	5.642522	-0.020676	2.601346
104.076177	2197.425309	5.647526	-0.020764	2.605718
104.223412	2205.476965	5.652531	-0.020797	2.610095
104.694370	2213.495940	5.657536	-0.020890	2.614468
104.910939	2221.557022	5.662541	-0.020935	2.618840
104.891154	2229.604541	5.667546	-0.020937	2.623182
105.507616	2237.612786	5.672550	-0.021057	2.627537
105.711342	2245.694383	5.677555	-0.021100	2.631897
105.703836	2253.766679	5.682560	-0.021104	2.636231
106.316411	2261.762809	5.687565	-0.021223	2.640558
106.644071	2269.787013	5.692570	-0.021289	2.644874
106.854925	2277.852896	5.697574	-0.021334	2.649198
106.952603	2285.956207	5.702579	-0.021358	2.653527
107.199304	2293.973037	5.707584	-0.021409	2.657812
107.630815	2302.002718	5.712589	-0.021494	2.662110
107.671137	2310.063319	5.717594	-0.021507	2.666391
107.930909	2318.136722	5.722598	-0.021561	2.670687
108.172079	2326.214326	5.727603	-0.021611	2.674976
108.281737	2334.229331	5.732608	-0.021637	2.679218
108.588997	2342.266341	5.737613	-0.021699	2.683476
108.911140	2350.291367	5.742618	-0.021764	2.687723
109.242475	2358.351346	5.747622	-0.021831	2.691982
109.508414	2366.414319	5.752627	-0.021886	2.696231
109.700423	2374.435883	5.757632	-0.021927	2.700447
110.085085	2382.460085	5.762637	-0.022004	2.704670
110.119166	2390.542712	5.767642	-0.022016	2.708895
110.403983	2398.614540	5.772646	-0.022074	2.713124
110.695545	2406.655133	5.777651	-0.022134	2.717330
110.805349	2414.686203	5.782656	-0.022159	2.721513
111.150682	2422.725092	5.787661	-0.022229	2.725708
111.367051	2430.755158	5.792666	-0.022274	2.729885
111.541967	2438.858714	5.797670	-0.022312	2.734090
111.880973	2446.871360	5.802675	-0.022381	2.738252
112.067150	2454.887856	5.807680	-0.022421	2.742400
112.567933	2462.941260	5.812685	-0.022519	2.746580
112.611940	2471.030169	5.817690	-0.022533	2.750744
112.893823	2479.150781	5.822694	-0.022591	2.754933
113.203078	2487.145467	5.827699	-0.022653	2.759052
113.228552	2495.174023	5.832704	-0.022663	2.763165
113.505947	2503.203354	5.837709	-0.022720	2.767288
114.067645	2511.202977	5.842714	-0.022830	2.771406
114.050950	2519.292222	5.847718	-0.022832	2.775529
114.239051	2527.320504	5.852723	-0.022873	2.779628
114.489201	2535.338156	5.857728	-0.022924	2.783718
114.789023	2543.400752	5.862733	-0.022986	2.787828
114.853766	2551.471273	5.867738	-0.023003	2.791922
115.305599	2559.505122	5.872742	-0.023092	2.796015
115.638058	2567.517208	5.877747	-0.023159	2.800083
115.892081	2575.543388	5.882752	-0.023212	2.804148
116.115035	2583.599207	5.887757	-0.023259	2.808220
116.366283	2591.658627	5.892762	-0.023311	2.812289
116.437837	2599.736837	5.897766	-0.023330	2.816352
116.687213	2607.765881	5.902771	-0.023381	2.820394
116.745941	2615.777284	5.907776	-0.023397	2.824411
117.162109	2623.847328	5.912781	-0.023480	2.828472
117.274886	2631.914424	5.917786	-0.023506	2.832508
117.487918	2639.964137	5.922790	-0.023551	2.836535
117.942036	2647.970396	5.927795	-0.023641	2.840549
117.719857	2655.984002	5.932800	-0.023605	2.844522
118.080795	2664.025628	5.937805	-0.023678	2.848537
118.323798	2672.082701	5.942810	-0.023728	2.852547
118.651229	2680.124054	5.947814	-0.023794	2.856548
119.067236	2688.146668	5.952819	-0.023877	2.860539
118.810487	2696.190671	5.957824	-0.023835	2.864498
119.216847	2704.233859	5.962829	-0.023916	2.868488
119.292077	2712.298347	5.967834	-0.023935	2.872464
119.666124	2720.318362	5.972838	-0.024010	2.876429
120.177388	2728.333679	5.977843	-0.024110	2.880394
120.152530	2736.371112	5.982848	-0.024111	2.884335
120.536166	2744.405915	5.987853	-0.024188	2.888291
120.916024	2752.445984	5.992858	-0.024264	2.892245
121.375136	2760.499983	5.997862	-0.024354	2.896204
121.518710	2768.551551	6.002867	-0.024386	2.900139
121.522866	2776.593007	6.007872	-0.024392	2.904057
121.958042	2784.647827	6.012877	-0.024479	2.907998
122.108225	2792.738804	6.017882	-0.024512	2.911937
122.209678	2800.803686	6.022886	-0.024536	2.915855
122.556686	2808.794473	6.027891	-0.024606	2.919745
122.876456	2816.775207	6.032896	-0.024671	2.923624
122.918335	2824.835924	6.037901	-0.024684	2.927521
123.380130	2832.838227	6.042906	-0.024775	2.931407
123.428509	2840.928257	6.047910	-0.024789	2.935308
123.648732	2848.940918	6.052915	-0.024836	2.939176
123.730313	2856.957227	6.057920	-0.024856	2.943033
124.200449	2864.994020	6.062925	-0.024949	2.946915
124.222431	2873.047184	6.067930	-0.024958	2.950777
124.355241	2881.105464	6.072934	-0.024988	2.954642
124.737389	2889.116107	6.077939	-0.025065	2.958492
124.882388	2897.127604	6.082944	-0.025097	2.962324
124.873605	2905.205401	6.087949	-0.025101	2.966176
125.095103	2913.224383	6.092954	-0.025147	2.970006
125.491171	2921.262729	6.097958	-0.025226	2.973850
125.709814	2929.326058	6.102963	-0.025272	2.977691
125.877627	2937.323690	6.107968	-0.025309	2.981494
126.314917	2945.366220	6.112973	-0.025395	2.985326
126.372835	2953.418070	6.117978	-0.025411	2.989139
126.668493	2961.480126	6.122982	-0.025472	2.992964
127.015487	2969.523390	6.127987	-0.025542	2.996778
127.181582	2977.525305	6.132992	-0.025578	3.000558
127.425665	2985.539789	6.137997	-0.025629	3.004343
127.719850	2993.569869	6.143002	-0.025689	3.008133
128.100536	3001.601805	6.148006	-0.025765	3.011923
128.421346	3009.678328	6.153011	-0.025830	3.015727
128.372084	3017.697283	6.158016	-0.025826	3.019480
128.638803	3025.726543	6.163021	-0.025881	3.023250
128.830200	3033.745080	6.168026	-0.025922	3.027005
129.061472	3041.808357	6.173030	-0.025970	3.030779
129.472574	3049.855067	6.178035	-0.026052	3.034549
129.753766	3057.869786	6.183040	-0.026109	3.038294
129.734770	3065.931692	6.188045	-0.026111	3.042041
129.944574	3073.957001	6.193050	-0.026156	3.045777
130.301924	3081.975704	6.198054	-0.026227	3.049513
130.588647	3090.049478	6.203059	-0.026286	3.053266
130.595323	3098.074351	6.208064	-0.026293	3.056979
130.912373	3106.113646	6.213069	-0.026357	3.060708
131.197016	3114.070789	6.218074	-0.026415	3.064394
131.285342	3122.139744	6.223078	-0.026437	3.068117
131.626686	3130.244307	6.228083	-0.026506	3.071864
132.028477	3138.282813	6.233088	-0.026586	3.075579
132.317377	3146.277425	6.238093	-0.026645	3.079264
132.436471	3154.290823	6.243098	-0.026672	3.082945
132.701878	3162.298369	6.248102	-0.026727	3.086626
132.987182	3170.347057	6.253107	-0.026785	3.090322
132.940937	3178.417106	6.258112	-0.026782	3.094008
133.239022	3186.433354	6.263117	-0.026843	3.097681
133.606504	3194.442711	6.268122	-0.026916	3.101350
133.714060	3202.474094	6.273126	-0.026942	3.105012
134.087120	3210.525532	6.278131	-0.027016	3.108692
134.358036	3218.549466	6.283136	-0.027072	3.112349
134.729835	3226.620426	6.288141	-0.027147	3.116029
134.839931	3234.622402	6.293146	-0.027172	3.119661
135.110010	3242.623396	6.298150	-0.027228	3.123295
135.624485	3250.668351	6.303155	-0.027329	3.126956
135.555172	3258.730952	6.308160	-0.027321	3.130594
135.789589	3266.774997	6.313165	-0.027370	3.134233
136.229492	3274.774299	6.318170	-0.027458	3.137857
136.238861	3282.823334	6.323174	-0.027465	3.141481
136.375002	3290.820590	6.328179	-0.027495	3.145082
136.551875	3298.890577	6.333184	-0.027533	3.148713
136.975782	3306.954187	6.338189	-0.027618	3.152349
137.026280	3315.022615	6.343194	-0.027632	3.155965
137.555537	3322.942025	6.348198	-0.027736	3.159532
137.730543	3331.002920	6.353203	-0.027774	3.163143
137.778888	3339.009138	6.358208	-0.027788	3.166719
137.967994	3347.075959	6.363213	-0.027829	3.170325
138.194815	3355.119670	6.368218	-0.027876	3.173918
138.419913	3363.150317	6.373222	-0.027923	3.177501
138.657961	3371.182575	6.378227	-0.027973	3.181081
138.659067	3379.193276	6.383232	-0.027978	3.184637
139.135380	3387.227993	6.388237	-0.028072	3.188220
139.247352	3395.304008	6.393242	-0.028099	3.191802
139.422534	3403.337234	6.398246	-0.028136	3.195363
139.703163	3411.336962	6.403251	-0.028194	3.198911
139.775345	3419.374014	6.408256	-0.028213	3.202462
140.007241	3427.408426	6.413261	-0.028261	3.206014
140.365104	3435.411583	6.418266	-0.028333	3.209554
140.236740	3443.496659	6.423270	-0.028314	3.213106
140.617089	3451.516382	6.428275	-0.028390	3.216646
140.725930	3459.510189	6.433280	-0.028416	3.220160
141.212502	3467.547856	6.438285	-0.028512	3.223705
141.401020	3475.595436	6.443290	-0.028552	3.227238
141.741506	3483.597037	6.448294	-0.028621	3.230753
142.240688	3491.722085	6.453299	-0.028719	3.234325
142.248452	3499.724667	6.458304	-0.028726	3.237819
142.373619	3507.732162	6.463309	-0.028754	3.241316
142.557963	3515.718509	6.468314	-0.028794	3.244803
142.821934	3523.716945	6.473318	-0.028848	3.248294
142.852254	3531.794553	6.478323	-0.028859	3.251806
143.001895	3539.841871	6.483328	-0.028892	3.255307
143.432267	3547.824600	6.488333	-0.028978	3.258787
143.512319	3555.843883	6.493338	-0.028998	3.262265
143.764421	3563.869013	6.498342	-0.029050	3.265748
144.065330	3571.950402	6.503347	-0.029112	3.269254
144.012466	3579.999090	6.508352	-0.029107	3.272728
144.229169	3588.036867	6.513357	-0.029153	3.276205
144.450570	3596.004591	6.518362	-0.029199	3.279647
144.556652	3604.015910	6.523366	-0.029224	3.283101
144.791739	3612.093067	6.528371	-0.029273	3.286583
144.999160	3620.095612	6.533376	-0.029317	3.290029
145.579085	3628.145929	6.538381	-0.029430	3.293507
145.498346	3636.190756	6.543386	-0.029420	3.296953
145.898824	3644.189194	6.548390	-0.029500	3.300393
146.175949	3652.232030	6.553395	-0.029557	3.303845
146.144156	3660.263457	6.558400	-0.029557	3.307276
146.200115	3668.317357	6.563405	-0.029572	3.310716
146.398061	3676.380979	6.568410	-0.029614	3.314163
146.682295	3684.346469	6.573414	-0.029673	3.317567
146.965617	3692.377613	6.578419	-0.029731	3.320995
147.245785	3700.325638	6.583424	-0.029788	3.324385
147.606230	3708.388114	6.588429	-0.029860	3.327823
147.786840	3716.460911	6.593434	-0.029899	3.331254
148.058102	3724.475961	6.598438	-0.029955	3.334661
148.262137	3732.528830	6.603443	-0.029998	3.338078
148.407032	3740.532440	6.608448	-0.030031	3.341469
148.435265	3748.558845	6.613453	-0.030041	3.344861
148.377910	3756.606772	6.618458	-0.030036	3.348256
148.688827	3764.662049	6.623462	-0.030099	3.351664
148.949801	3772.715909	6.628467	-0.030153	3.355066
149.074772	3780.685887	6.633472	-0.030181	3.358424
149.339597	3788.709828	6.638477	-0.030236	3.361807
149.723238	3796.716905	6.643482	-0.030312	3.365184
149.793563	3804.753101	6.648486	-0.030331	3.368558
150.077045	3812.820911	6.653491	-0.030389	3.371949
150.084783	3820.838436	6.658496	-0.030396	3.375306
150.404369	3828.860570	6.663501	-0.030460	3.378673
150.543410	3836.893483	6.668506	-0.030492	3.382034
150.617703	3844.904028	6.673510	-0.030511	3.385381
150.893484	3852.956448	6.678515	-0.030567	3.388748
150.892645	3861.047836	6.683520	-0.030572	3.392119
151.385927	3869.080949	6.688525	-0.030670	3.395480
151.415266	3877.053012	6.693530	-0.030680	3.398795
151.663199	3885.049170	6.698534	-0.030732	3.402125
152.128726	3893.036615	6.703539	-0.030824	3.405456
152.145988	3901.064943	6.708544	-0.030832	3.408785
152.417244	3909.123006	6.713549	-0.030888	3.412131
152.508366	3917.160268	6.718554	-0.030910	3.415459
152.535563	3925.168391	6.723558	-0.030920	3.418770
152.760980	3933.208779	6.728563	-0.030968	3.422098
152.880124	3941.181813	6.733568	-0.030995	3.425391
153.086543	3949.242571	6.738573	-0.031039	3.428720
153.282669	3957.294661	6.743578	-0.031081	3.432042
153.306070	3965.331568	6.748582	-0.031090	3.435348
153.743096	3973.344769	6.753587	-0.031177	3.438656
153.923800	3981.345672	6.758592	-0.031216	3.441946
154.075602	3989.377996	6.763597	-0.031249	3.445246
154.190853	3997.370744	6.768602	-0.031276	3.448525
154.508904	4005.427261	6.773606	-0.031340	3.451833
155.098709	4013.468994	6.778611	-0.031456	3.455141
155.209332	4021.473917	6.783616	-0.031481	3.458415
155.378370	4029.540724	6.788621	-0.031518	3.461713
155.542642	4037.558241	6.793626	-0.031554	3.464988
155.545927	4045.567910	6.798630	-0.031560	3.468251
155.796942	4053.656727	6.803635	-0.031612	3.471551
156.177392	4061.658584	6.808640	-0.031688	3.474817
156.210289	4069.677242	6.813645	-0.031699	3.478076
156.202713	4077.709720	6.818650	-0.031703	3.481335
156.596187	4085.661867	6.823654	-0.031782	3.484572
156.656242	4093.739584	6.828659	-0.031798	3.487846
156.576133	4101.776496	6.833664	-0.031789	3.491096
157.039229	4109.799977	6.838669	-0.031880	3.494355
157.310416	4117.802852	6.843674	-0.031936	3.497596
157.278572	4125.841530	6.848678	-0.031935	3.500839
157.450317	4133.842399	6.853683	-0.031972	3.504071
157.716214	4141.848094	6.858688	-0.032027	3.507304
158.137619	4149.878001	6.863693	-0.032111	3.510548
158.218335	4157.939479	6.868698	-0.032131	3.513792
158.439143	4165.953355	6.873702	-0.032178	3.517018
158.658130	4173.989623	6.878707	-0.032224	3.520250
158.724122	4181.991342	6.883712	-0.032241	3.523460
159.092584	4189.982766	6.888717	-0.032315	3.526673
159.250296	4198.044524	6.893722	-0.032350	3.529904
159.538115	4206.100744	6.898726	-0.032409	3.533134
159.871136	4214.143070	6.903731	-0.032476	3.536357
160.058276	4222.124089	6.908736	-0.032516	3.539548
160.348799	4230.171193	6.913741	-0.032575	3.542766
160.561995	4238.189227	6.918746	-0.032620	3.545966
160.494945	4246.223064	6.923750	-0.032613	3.549162
160.873704	4254.333677	6.928755	-0.032689	3.552399
160.718899	4262.391031	6.933760	-0.032665	3.555595
160.951955	4270.344889	6.938765	-0.032714	3.558759
161.257410	4278.336008	6.943770	-0.032776	3.561938
161.336188	4286.303886	6.948774	-0.032796	3.565097
161.529338	4294.364322	6.953779	-0.032837	3.568294
161.740982	4302.384129	6.958784	-0.032882	3.571472
162.142592	4310.399609	6.963789	-0.032962	3.574651
162.065604	4318.469321	6.968794	-0.032953	3.577835
162.203437	4326.447367	6.973798	-0.032984	3.580986
162.584755	4334.452026	6.978803	-0.033060	3.584151
162.682730	4342.492453	6.983808	-0.033084	3.587320
162.817862	4350.530998	6.988813	-0.033114	3.590487
163.095041	4358.591874	6.993818	-0.033171	3.593663
163.105141	4366.589385	6.998822	-0.033178	3.596804
163.363671	4374.596745	7.003827	-0.033231	3.599953
163.607163	4382.589213	7.008832	-0.033282	3.603093
163.976052	4390.630844	7.013837	-0.033356	3.606253
163.943064	4398.655667	7.018842	-0.033355	3.609393
164.106369	4406.695086	7.023846	-0.033391	3.612541
164.558010	4414.720362	7.028851	-0.033480	3.615688
164.636997	4422.740772	7.033856	-0.033500	3.618821
164.877911	4430.751154	7.038861	-0.033550	3.621951
164.931663	4438.788151	7.043866	-0.033565	3.625084
165.075812	4446.806539	7.048870	-0.033598	3.628210
165.159676	4454.889126	7.053875	-0.033618	3.631356
165.313801	4462.912788	7.058880	-0.033652	3.634478
165.551433	4470.925555	7.063885	-0.033702	3.637596
165.553929	4478.924575	7.068890	-0.033708	3.640699
165.667326	4486.892948	7.073894	-0.033734	3.643791
166.136309	4494.959767	7.078899	-0.033827	3.646927
166.294625	4502.968736	7.083904	-0.033861	3.650031
166.380536	4511.024300	7.088909	-0.033883	3.653147
166.816677	4519.069320	7.093914	-0.033969	3.656267
166.987531	4527.021342	7.098918	-0.034006	3.659340
167.045143	4535.097170	7.103923	-0.034022	3.662456
167.189964	4543.076722	7.108928	-0.034054	3.665534
167.373037	4551.119696	7.113933	-0.034094	3.668635
167.454568	4559.206449	7.118938	-0.034114	3.671748
167.602320	4567.202199	7.123942	-0.034147	3.674825
167.679732	4575.234650	7.128947	-0.034167	3.677911
167.991786	4583.219143	7.133952	-0.034230	3.680983
168.200934	4591.196119	7.138957	-0.034274	3.684046
168.477531	4599.243853	7.143962	-0.034331	3.687135
168.621457	4607.262364	7.148966	-0.034363	3.690208
168.867568	4615.348678	7.153971	-0.034414	3.693306
168.887962	4623.365196	7.158976	-0.034423	3.696369
169.089320	4631.356051	7.163981	-0.034466	3.699425
169.243763	4639.359954	7.168986	-0.034500	3.702482
169.217535	4647.384791	7.173990	-0.034500	3.705539
169.488639	4655.441204	7.178995	-0.034556	3.708614
169.624249	4663.459038	7.184000	-0.034587	3.711668
169.914145	4671.539294	7.189005	-0.034646	3.714747
170.120435	4679.554487	7.194010	-0.034690	3.717796
170.379999	4687.543309	7.199014	-0.034743	3.720835
170.573410	4695.487839	7.204019	-0.034784	3.723852
170.732254	4703.529311	7.209024	-0.034819	3.726903
170.989715	4711.538996	7.214029	-0.034872	3.729942
171.277265	4719.597182	7.219034	-0.034931	3.732997
170.988032	4727.655639	7.224038	-0.034883	3.736036
171.406462	4735.626268	7.229043	-0.034966	3.739056
171.636467	4743.658424	7.234048	-0.035014	3.742092
171.749966	4751.642391	7.239053	-0.035040	3.745105
171.799910	4759.685730	7.244058	-0.035055	3.748137
171.964286	4767.718522	7.249062	-0.035091	3.751165
172.268968	4775.777400	7.254067	-0.035153	3.754203
172.272882	4783.794260	7.259072	-0.035159	3.757216
172.601765	4791.802493	7.264077	-0.035225	3.760231
172.702368	4799.822196	7.269082	-0.035249	3.763242
172.730797	4807.841139	7.274086	-0.035260	3.766249
172.960735	4815.862526	7.279091	-0.035308	3.769260
173.110943	4823.916153	7.284096	-0.035341	3.772278
173.246145	4831.942142	7.289101	-0.035372	3.775283
173.444107	4839.974969	7.294106	-0.035414	3.778289
173.398928	4847.983802	7.299110	-0.035411	3.781279
173.701414	4855.999802	7.304115	-0.035472	3.784277
173.646339	4864.040394	7.309120	-0.035467	3.787273
173.952709	4872.054829	7.314125	-0.035529	3.790266
174.310921	4880.100339	7.319130	-0.035601	3.793268
174.345897	4888.138836	7.324134	-0.035613	3.796259
174.747446	4896.100645	7.329139	-0.035693	3.799227
174.862096	4904.092518	7.334144	-0.035720	3.802197
174.979884	4912.101454	7.339149	-0.035747	3.805171
175.180551	4920.128705	7.344154	-0.035790	3.808152
175.484985	4928.190843	7.349158	-0.035852	3.811145
175.599851	4936.207218	7.354163	-0.035878	3.814115
175.573144	4944.249092	7.359168	-0.035878	3.817089
175.823926	4952.224566	7.364173	-0.035930	3.820042
176.099819	4960.248856	7.369178	-0.035987	3.823012
176.021478	4968.226230	7.374182	-0.035978	3.825954
176.313877	4976.313847	7.379187	-0.036037	3.828942
176.332512	4984.327751	7.384192	-0.036046	3.831895
176.466823	4992.346365	7.389197	-0.036076	3.834850
176.662145	5000.373714	7.394202	-0.036118	3.837807
176.882313	5008.371958	7.399206	-0.036164	3.840752
177.116479	5016.368001	7.404211	-0.036213	3.843694
177.161472	5024.396207	7.409216	-0.036227	3.846641
177.375423	5032.430520	7.414221	-0.036272	3.849592
177.625776	5040.480150	7.419226	-0.036324	3.852547
177.579044	5048.521008	7.424230	-0.036320	3.855491
177.820638	5056.501689	7.429235	-0.036371	3.858416
178.018199	5064.529404	7.434240	-0.036413	3.861355
178.215801	5072.534259	7.439245	-0.036455	3.864283
178.418314	5080.606609	7.444250	-0.036498	3.867234
178.530121	5088.617390	7.449254	-0.036524	3.870158
178.854004	5096.837832	7.454259	-0.036589	3.873161
178.734916	5104.858968	7.459264	-0.036573	3.876080
179.150347	5112.743138	7.464269	-0.036655	3.878958
179.182874	5120.788759	7.469274	-0.036666	3.881884
179.409556	5128.703736	7.474278	-0.036714	3.884765
179.538968	5136.740833	7.479283	-0.036743	3.887686
179.679741	5144.761916	7.484288	-0.036775	3.890599
179.837180	5152.785611	7.489293	-0.036809	3.893511
180.059549	5160.832649	7.494298	-0.036856	3.896431
180.102122	5168.815051	7.499302	-0.036869	3.899322
180.477175	5176.850733	7.504307	-0.036944	3.902236
180.392937	5184.847444	7.509312	-0.036934	3.905125
180.418822	5192.863343	7.514317	-0.036944	3.908021
180.910488	5200.916452	7.519322	-0.037041	3.910937
180.980085	5208.958608	7.524326	-0.037059	3.913839
181.247487	5216.983600	7.529331	-0.037114	3.916736
181.534435	5224.929535	7.534336	-0.037173	3.919603
181.717578	5232.944860	7.539341	-0.037212	3.922491
181.809385	5240.981241	7.544346	-0.037234	3.925382
181.824746	5248.987486	7.549350	-0.037242	3.928260
182.023707	5257.041670	7.554355	-0.037285	3.931155
182.121444	5265.064320	7.559360	-0.037308	3.934036
182.255332	5273.072797	7.564365	-0.037338	3.936909
182.650329	5281.057608	7.569370	-0.037417	3.939777
182.620186	5289.078252	7.574374	-0.037417	3.942648
182.720099	5297.145442	7.579379	-0.037441	3.945536
182.856848	5305.137279	7.584384	-0.037471	3.948396
183.144958	5313.185245	7.589389	-0.037530	3.951276
183.252888	5321.244523	7.594394	-0.037556	3.954154
183.261902	5329.230492	7.599398	-0.037563	3.957003
183.663619	5337.204056	7.604403	-0.037643	3.959852
183.762086	5345.205204	7.609408	-0.037666	3.962704
183.971245	5353.231407	7.614413	-0.037711	3.965564
184.131928	5361.264068	7.619418	-0.037746	3.968424
184.183989	5369.290208	7.624422	-0.037761	3.971278
184.405162	5377.319389	7.629427	-0.037807	3.974133
184.607202	5385.362391	7.634432	-0.037850	3.976991
184.894886	5393.326216	7.639437	-0.037909	3.979820
184.935262	5401.382353	7.644442	-0.037922	3.982676
185.074485	5409.385880	7.649446	-0.037953	3.985512
185.284054	5417.448382	7.654451	-0.037997	3.988369
185.445480	5425.463353	7.659456	-0.038032	3.991206
185.414604	5433.506237	7.664461	-0.038032	3.994048
185.766361	5441.558480	7.669466	-0.038103	3.996897
185.929527	5449.525245	7.674470	-0.038138	3.999711
185.934480	5457.559820	7.679475	-0.038144	4.002544
186.117728	5465.511350	7.684480	-0.038184	4.005349
186.323596	5473.575723	7.689485	-0.038227	4.008192
186.588930	5481.641465	7.694490	-0.038282	4.011034
186.332443	5489.655599	7.699494	-0.038240	4.013848
186.818039	5497.699039	7.704499	-0.038335	4.016682
187.120485	5505.647990	7.709504	-0.038397	4.019477
187.014642	5513.672288	7.714509	-0.038382	4.022291
187.279839	5521.713446	7.719514	-0.038437	4.025115
187.578563	5529.745530	7.724518	-0.038498	4.027934
187.600854	5537.777595	7.729523	-0.038507	4.030746
187.754560	5545.880096	7.734528	-0.038541	4.033583
187.877880	5553.895004	7.739533	-0.038570	4.036388
188.046853	5561.823299	7.744538	-0.038606	4.039160
188.236674	5569.805422	7.749542	-0.038647	4.041950
188.583040	5577.799894	7.754547	-0.038717	4.044745
188.469492	5585.843764	7.759552	-0.038701	4.047548
188.547415	5593.853703	7.764557	-0.038720	4.050340
188.786043	5601.910883	7.769562	-0.038770	4.053148
188.749127	5609.927854	7.774566	-0.038769	4.055937
189.011542	5617.914503	7.779571	-0.038823	4.058718
189.074463	5625.962661	7.784576	-0.038840	4.061515
189.499553	5633.882716	7.789581	-0.038924	4.064272
189.665369	5641.949499	7.794586	-0.038960	4.067073
189.666104	5649.969229	7.799590	-0.038966	4.069854
190.010762	5658.017402	7.804595	-0.039035	4.072647
190.105522	5666.063340	7.809600	-0.039058	4.075435
190.109087	5674.015619	7.814605	-0.039064	4.078186
190.497233	5682.068030	7.819610	-0.039141	4.080976
190.803265	5690.029078	7.824614	-0.039204	4.083731
190.925754	5698.113271	7.829619	-0.039232	4.086525
191.043840	5706.115439	7.834624	-0.039259	4.089288
191.316532	5714.129670	7.839629	-0.039315	4.092055
191.708484	5722.153840	7.844634	-0.039393	4.094825
191.554295	5730.165898	7.849638	-0.039370	4.097582
191.661207	5738.183156	7.854643	-0.039395	4.100343
191.837526	5746.183212	7.859648	-0.039433	4.103096
191.790242	5754.220931	7.864653	-0.039429	4.105858
192.130935	5762.245598	7.869658	-0.039498	4.108619
192.260164	5770.297493	7.874662	-0.039527	4.111384
192.669156	5778.359776	7.879667	-0.039609	4.114154
192.734221	5786.353129	7.884672	-0.039626	4.116895
192.948285	5794.332591	7.889677	-0.039671	4.119631
193.181573	5802.392468	7.894682	-0.039720	4.122392
193.279575	5810.354212	7.899686	-0.039744	4.125117
193.457674	5818.395977	7.904691	-0.039782	4.127868
193.846741	5826.413518	7.909696	-0.039860	4.130612
193.901743	5834.486240	7.914701	-0.039875	4.133368
194.030747	5842.531488	7.919706	-0.039905	4.136114
194.175876	5850.449645	7.924710	-0.039937	4.138815
194.390497	5858.524555	7.929715	-0.039982	4.141569
194.653287	5866.471125	7.934720	-0.040036	4.144278
194.906351	5874.561960	7.939725	-0.040089	4.147033
194.990134	5882.566894	7.944730	-0.040109	4.149756
195.016180	5890.596616	7.949734	-0.040120	4.152485
195.271466	5898.643877	7.954739	-0.040172	4.155220
195.456885	5906.618906	7.959744	-0.040212	4.157928
195.517595	5914.591547	7.964749	-0.040229	4.160633
195.623364	5922.636057	7.969754	-0.040254	4.163360
195.771018	5930.655877	7.974758	-0.040286	4.166078
195.999704	5938.657032	7.979763	-0.040334	4.168788
195.955829	5946.697615	7.984768	-0.040331	4.171507
195.978111	5954.769859	7.989773	-0.040341	4.174236
196.470182	5962.767027	7.994778	-0.040438	4.176943
196.529021	5970.758038	7.999782	-0.040454	4.179641
196.455886	5978.812285	8.004787	-0.040446	4.182357
196.635635	5986.779166	8.009792	-0.040484	4.185045
196.659061	5994.820298	8.014797	-0.040494	4.187754
196.825232	6002.830499	8.019802	-0.040530	4.190453
197.158443	6010.904615	8.024806	-0.040597	4.193173
197.371786	6018.959156	8.029811	-0.040642	4.195883
197.472013	6026.884110	8.034816	-0.040666	4.198547
197.673979	6034.873244	8.039821	-0.040709	4.201232
198.080196	6042.878852	8.044826	-0.040790	4.203923
198.072238	6050.911989	8.049830	-0.040794	4.206617
198.217420	6058.919444	8.054835	-0.040826	4.209302
198.176849	6066.966704	8.059840	-0.040824	4.211997
198.303681	6074.992527	8.064845	-0.040853	4.214685
198.514322	6083.025652	8.069850	-0.040897	4.217374
198.801664	6090.967327	8.074854	-0.040956	4.220032
199.034310	6099.015798	8.079859	-0.041004	4.222723
199.123913	6107.015776	8.084864	-0.041026	4.225395
199.257555	6115.042021	8.089869	-0.041057	4.228074
199.590275	6123.076927	8.094874	-0.041124	4.230757
199.833505	6131.114069	8.099878	-0.041174	4.233437
200.110776	6139.133853	8.104883	-0.041231	4.236111
200.212958	6147.087864	8.109888	-0.041255	4.238759
200.358304	6155.127354	8.114893	-0.041288	4.241434
200.498412	6163.106363	8.119898	-0.041319	4.244087
200.545698	6171.153225	8.124902	-0.041333	4.246761
200.860398	6179.205206	8.129907	-0.041397	4.249437
200.829586	6187.248493	8.134912	-0.041397	4.252105
200.849770	6195.242666	8.139917	-0.041406	4.254755
201.258501	6203.300910	8.144922	-0.041487	4.257429
201.186942	6211.245459	8.149926	-0.041479	4.260059
201.419724	6219.326323	8.154931	-0.041528	4.262735
201.705683	6227.292895	8.159936	-0.041586	4.265372
201.870825	6235.361295	8.164941	-0.041622	4.268040
201.828424	6243.395880	8.169946	-0.041619	4.270694
202.036174	6251.427924	8.174950	-0.041663	4.273347
202.211620	6259.467789	8.179955	-0.041701	4.276000
202.387642	6267.433139	8.184960	-0.041739	4.278628
202.152985	6275.433937	8.189965	-0.041701	4.281262
202.413754	6283.415541	8.194970	-0.041755	4.283892
202.668642	6291.464001	8.199974	-0.041807	4.286543
202.959274	6299.457777	8.204979	-0.041867	4.289174
202.970745	6307.534820	8.209984	-0.041874	4.291829
203.092493	6315.520014	8.214989	-0.041902	4.294452
203.280741	6323.599851	8.219994	-0.041942	4.297106
203.523026	6331.540649	8.224998	-0.041993	4.299713
203.769950	6339.596759	8.230003	-0.042044	4.302356
203.891747	6347.586583	8.235008	-0.042072	4.304975
203.913721	6355.600870	8.240013	-0.042081	4.307599
204.292336	6363.651731	8.245018	-0.042157	4.310237
204.322414	6371.678595	8.250022	-0.042168	4.312862
204.313160	6379.715104	8.255027	-0.042172	4.315488
204.434815	6387.689443	8.260032	-0.042199	4.318094
204.429142	6395.668690	8.265037	-0.042204	4.320699
204.793702	6403.697032	8.270042	-0.042277	4.323321
205.028872	6411.705526	8.275046	-0.042326	4.325933
205.328045	6419.725209	8.280051	-0.042387	4.328549
205.433979	6427.763717	8.285056	-0.042412	4.331167
205.433361	6435.773003	8.290061	-0.042417	4.333774
205.738354	6443.847717	8.295066	-0.042479	4.336402
205.935187	6451.791429	8.300070	-0.042521	4.338986
205.874216	6459.843498	8.305075	-0.042515	4.341601
205.994695	6467.828288	8.310080	-0.042542	4.344194
206.151597	6475.859495	8.315085	-0.042577	4.346801
206.459195	6483.889589	8.320090	-0.042639	4.349407
206.573229	6491.930521	8.325094	-0.042666	4.352013
206.856693	6500.029784	8.330099	-0.042724	4.354638
206.903602	6507.996974	8.335104	-0.042738	4.357217
207.074669	6515.922033	8.340109	-0.042775	4.359782
207.350645	6523.963753	8.345114	-0.042832	4.362384
207.518688	6531.903275	8.350118	-0.042868	4.364950
207.769001	6539.967816	8.355123	-0.042920	4.367556
207.775803	6548.016774	8.360128	-0.042927	4.370153
208.061913	6556.018769	8.365133	-0.042985	4.372736
208.062202	6564.087163	8.370138	-0.042991	4.375336
208.138636	6572.039711	8.375142	-0.043010	4.377899
208.245812	6580.078845	8.380147	-0.043035	4.380487
208.378096	6588.100005	8.385152	-0.043065	4.383069
208.384917	6596.083532	8.390157	-0.043072	4.385636
208.711710	6604.131175	8.395162	-0.043138	4.388224
208.829532	6612.137787	8.400166	-0.043165	4.390796
209.012357	6620.180127	8.405171	-0.043204	4.393379
209.110584	6628.223864	8.410176	-0.043228	4.395960
209.226162	6636.167856	8.415181	-0.043255	4.398508
209.460011	6644.220758	8.420186	-0.043303	4.401089
209.416588	6652.203120	8.425190	-0.043301	4.403645
209.478972	6660.284978	8.430195	-0.043317	4.406232
209.587158	6668.230282	8.435200	-0.043343	4.408774
209.622228	6676.256615	8.440205	-0.043355	4.411340
209.754591	6684.375055	8.445210	-0.043385	4.413934
209.903643	6692.373859	8.450214	-0.043418	4.416489
210.010723	6700.328097	8.455219	-0.043443	4.419028
210.181772	6708.374114	8.460224	-0.043480	4.421595
210.507420	6716.337319	8.465229	-0.043546	4.424134
210.617296	6724.435882	8.470234	-0.043572	4.426715
210.712641	6732.411915	8.475238	-0.043594	4.429255
210.981154	6740.486256	8.480243	-0.043650	4.431825
211.155149	6748.544159	8.485248	-0.043687	4.434388
211.325786	6756.513498	8.490253	-0.043724	4.436922
211.558718	6764.454159	8.495258	-0.043773	4.439445
211.655320	6772.497708	8.500262	-0.043796	4.441999
211.855090	6780.452015	8.505267	-0.043839	4.444523
212.064098	6788.543770	8.510272	-0.043883	4.447090
212.048116	6796.485558	8.515277	-0.043885	4.449606
212.233254	6804.615612	8.520282	-0.043925	4.452182
212.409585	6812.574951	8.525286	-0.043963	4.454702
212.456333	6820.648096	8.530291	-0.043977	4.457256
212.454251	6828.593153	8.535296	-0.043982	4.459768
212.651641	6836.598591	8.540301	-0.044024	4.462298
212.578895	6844.627699	8.545306	-0.044016	4.464834
212.743036	6852.656594	8.550310	-0.044051	4.467369
213.073246	6860.701078	8.555315	-0.044118	4.469907
213.129600	6868.739510	8.560320	-0.044134	4.472442
213.260554	6876.744038	8.565325	-0.044164	4.474964
213.359639	6884.774316	8.570330	-0.044187	4.477494
213.271004	6892.709990	8.575335	-0.044176	4.479991
213.621778	6900.695066	8.580339	-0.044247	4.482504
213.696911	6908.727359	8.585344	-0.044266	4.485029
213.791374	6916.761039	8.590349	-0.044289	4.487554
214.069755	6924.815355	8.595354	-0.044346	4.490084
214.184123	6932.828172	8.600359	-0.044372	4.492599
214.322660	6940.844306	8.605363	-0.044403	4.495114
214.349686	6948.856075	8.610368	-0.044414	4.497625
214.307045	6956.832115	8.615373	-0.044411	4.500124
214.497044	6964.868329	8.620378	-0.044452	4.502641
214.530641	6972.866594	8.625383	-0.044463	4.505144
214.971168	6980.919739	8.630387	-0.044550	4.507664
214.960740	6988.936413	8.635392	-0.044554	4.510170
215.165076	6997.000763	8.640397	-0.044597	4.512690
215.174370	7005.071275	8.645402	-0.044604	4.515210
215.221342	7013.012925	8.650407	-0.044618	4.517689
215.379455	7020.960115	8.655411	-0.044653	4.520168
215.523873	7028.972947	8.660416	-0.044685	4.522666
215.872807	7036.944689	8.665421	-0.044755	4.525151
215.896817	7045.054627	8.670426	-0.044765	4.527676
215.995798	7053.025104	8.675431	-0.044789	4.530157
216.198207	7061.048502	8.680435	-0.044831	4.532653
216.359993	7069.061605	8.685440	-0.044867	4.535144
216.468275	7077.091582	8.690445	-0.044892	4.537640
216.541474	7085.100095	8.695450	-0.044911	4.540127
216.684672	7093.094512	8.700455	-0.044943	4.542608
217.116528	7101.124945	8.705459	-0.045029	4.545100
216.995556	7109.190198	8.710464	-0.045012	4.547600
216.981920	7117.135311	8.715469	-0.045014	4.550061
217.397070	7125.230779	8.720474	-0.045097	4.552569
217.338517	7133.217174	8.725479	-0.045091	4.555041
217.494469	7141.250290	8.730483	-0.045125	4.557526
217.690016	7149.243235	8.735488	-0.045167	4.559997
217.875222	7157.241656	8.740493	-0.045207	4.562469
218.091231	7165.249423	8.745498	-0.045252	4.564942
218.010680	7173.293147	8.750503	-0.045243	4.567425
218.359310	7181.276852	8.755507	-0.045313	4.569888
218.208311	7189.373135	8.760512	-0.045290	4.572384
218.625604	7197.327977	8.765517	-0.045373	4.574836
218.804824	7205.419826	8.770522	-0.045412	4.577328
218.717046	7213.357674	8.775527	-0.045400	4.579771
218.818820	7221.390565	8.780531	-0.045425	4.582243
218.954312	7229.386113	8.785536	-0.045455	4.584701
219.173104	7237.407155	8.790541	-0.045501	4.587166
219.269592	7245.468458	8.795546	-0.045524	4.589642
219.323107	7253.472191	8.800551	-0.045540	4.592099
219.670033	7261.523479	8.805555	-0.045609	4.594570
219.716372	7269.571578	8.810560	-0.045623	4.597038
219.811488	7277.478252	8.815565	-0.045646	4.599461
220.089768	7285.554073	8.820570	-0.045703	4.601935
220.232328	7293.498830	8.825575	-0.045735	4.604367
220.224335	7301.553095	8.830579	-0.045739	4.606832
220.602970	7309.557314	8.835584	-0.045815	4.609280
220.756894	7317.600778	8.840589	-0.045849	4.611738
220.782986	7325.670100	8.845594	-0.045859	4.614204
220.672058	7333.642508	8.850599	-0.045843	4.616638
220.727991	7341.613996	8.855603	-0.045859	4.619070
220.942740	7349.645058	8.860608	-0.045904	4.621520
220.864869	7357.611681	8.865613	-0.045895	4.623949
221.127683	7365.697512	8.870618	-0.045949	4.626412
221.537675	7373.672018	8.875623	-0.046031	4.628840
221.501027	7381.732462	8.880627	-0.046029	4.631294
221.756935	7389.785239	8.885632	-0.046082	4.633743
221.830298	7397.791780	8.890637	-0.046101	4.636177
221.779596	7405.758164	8.895642	-0.046097	4.638598
221.702530	7413.801650	8.900647	-0.046088	4.641041
222.094129	7421.761860	8.905651	-0.046166	4.643457
222.148349	7429.781186	8.910656	-0.046181	4.645890
222.333352	7437.792710	8.915661	-0.046221	4.648320
222.324249	7445.834776	8.920666	-0.046225	4.650757
222.729215	7453.853388	8.925671	-0.046305	4.653186
222.685771	7461.879105	8.930675	-0.046302	4.655615
222.906854	7469.889228	8.935680	-0.046349	4.658039
222.977790	7477.848373	8.940685	-0.046367	4.660446
223.315906	7485.916984	8.945690	-0.046436	4.662885
223.056417	7493.849155	8.950695	-0.046392	4.665281
223.314359	7501.979757	8.955699	-0.046446	4.667736
223.477039	7509.969483	8.960704	-0.046481	4.670147
223.405882	7518.016207	8.965709	-0.046473	4.672575
223.883396	7526.063417	8.970714	-0.046568	4.675000
223.906883	7534.030941	8.975719	-0.046577	4.677401
224.038209	7541.974083	8.980723	-0.046607	4.679793
224.093108	7550.053739	8.985728	-0.046622	4.682225
224.303026	7557.945402	8.990733	-0.046667	4.684599
224.402329	7566.078351	8.995738	-0.046690	4.687045
224.359974	7574.047490	9.000743	-0.046688	4.689440
224.600598	7582.103474	9.005747	-0.046738	4.691859
224.788678	7590.104107	9.010752	-0.046778	4.694261
224.790458	7598.135828	9.015757	-0.046784	4.696671
225.067423	7606.100607	9.020762	-0.046840	4.699060
225.205871	7614.112368	9.025767	-0.046872	4.701461
225.489218	7622.125126	9.030771	-0.046930	4.703861
225.590836	7630.217961	9.035776	-0.046954	4.706285
225.784202	7638.197791	9.040781	-0.046995	4.708673
225.967715	7646.268322	9.045786	-0.047034	4.711087
225.924923	7654.265079	9.050791	-0.047032	4.713478
225.950103	7662.220449	9.055795	-0.047042	4.715855
226.245501	7670.278230	9.060800	-0.047102	4.718261
226.187398	7678.255716	9.065805	-0.047096	4.720643
226.391818	7686.250963	9.070810	-0.047140	4.723028
226.625653	7694.263159	9.075815	-0.047188	4.725417
226.816926	7702.309510	9.080819	-0.047229	4.727815
226.775227	7710.368390	9.085824	-0.047227	4.730216
226.943350	7718.367239	9.090829	-0.047263	4.732598
227.243759	7726.415512	9.095834	-0.047325	4.734992
227.185404	7734.382629	9.100839	-0.047319	4.737363
227.351882	7742.387450	9.105843	-0.047355	4.739742
227.785235	7750.416916	9.110848	-0.047441	4.742127
227.682246	7758.396732	9.115853	-0.047427	4.744498
227.688412	7766.470006	9.120858	-0.047434	4.746894
227.798707	7774.426401	9.125863	-0.047459	4.749255
227.964099	7782.509543	9.130867	-0.047496	4.751652
227.873816	7790.579266	9.135872	-0.047484	4.754044
228.050603	7798.558006	9.140877	-0.047522	4.756407
228.304177	7806.521631	9.145882	-0.047575	4.758765
228.658991	7814.520029	9.150887	-0.047646	4.761131
228.622221	7822.525310	9.155891	-0.047644	4.763499
229.081063	7830.555309	9.160896	-0.047735	4.765872
228.805687	7838.580529	9.165901	-0.047689	4.768245
228.950044	7846.595826	9.170906	-0.047721	4.770612
229.181693	7854.618383	9.175911	-0.047770	4.772980
229.555140	7862.607679	9.180915	-0.047844	4.775336
229.467543	7870.666021	9.185920	-0.047833	4.777713
229.716686	7878.675588	9.190925	-0.047885	4.780073
229.919888	7886.689663	9.195930	-0.047928	4.782434
229.846496	7894.611778	9.200935	-0.047920	4.784767
230.163454	7902.729827	9.205939	-0.047984	4.787155
230.428689	7910.737767	9.210944	-0.048039	4.789510
230.279510	7918.777873	9.215949	-0.048016	4.791875
230.218407	7926.766855	9.220954	-0.048010	4.794224
230.390380	7934.796082	9.225959	-0.048047	4.796582
230.605363	7942.729997	9.230963	-0.048092	4.798910
230.641260	7950.812018	9.235968	-0.048104	4.801282
230.772142	7958.724906	9.240973	-0.048134	4.803603
231.071927	7966.809354	9.245978	-0.048195	4.805972
231.032892	7974.795684	9.250983	-0.048193	4.808312
231.204320	7982.883026	9.255987	-0.048230	4.810680
231.246429	7990.328115	9.260992	-0.048243	4.812860
231.372017	7994.933264	9.265997	-0.048269	4.814207

231.697802	7997.265636	9.271002	-0.048332	4.814888
231.497487	7998.688106	9.276007	-0.048295	4.815305
231.874675	7999.118926	9.281011	-0.048366	4.815429
231.890833	7999.718974	9.286016	-0.048369	4.815605
231.984362	7999.710880	9.291021	-0.048387	4.815602
232.305152	7999.750209	9.296026	-0.048447	4.815612
232.319821	7999.780332	9.301031	-0.048449	4.815621
232.218539	7999.734944	9.306035	-0.048431	4.815608
232.343388	7999.775382	9.311040	-0.048454	4.815619
232.247644	7999.719410	9.316045	-0.048436	4.815603
232.266007	7999.794418	9.321050	-0.048439	4.815625
232.240602	7999.717168	9.326055	-0.048435	4.815602
232.470590	7999.726216	9.331059	-0.048478	4.815604
232.488114	7999.756386	9.336064	-0.048481	4.815613
232.761421	7999.776806	9.341069	-0.048532	4.815617
233.158489	7999.819503	9.346074	-0.048606	4.815628
233.157837	7999.878197	9.351079	-0.048606	4.815645
233.278651	7999.784093	9.356083	-0.048628	4.815617
233.410498	7999.793694	9.361088	-0.048653	4.815619
233.553805	7999.852577	9.366093	-0.048680	4.815636
233.542494	7999.812907	9.371098	-0.048678	4.815624
233.358478	7999.849431	9.376103	-0.048643	4.815636
233.433688	7999.798350	9.381107	-0.048657	4.815621
233.704992	7999.792058	9.386112	-0.048708	4.815617
233.400804	7999.836248	9.391117	-0.048651	4.815632
233.726711	7999.895943	9.396122	-0.048712	4.815648
233.708341	7999.792121	9.401127	-0.048709	4.815617
233.698714	7999.839997	9.406131	-0.048707	4.815631
233.851283	7999.812578	9.411136	-0.048735	4.815623
233.755876	7999.757676	9.416141	-0.048718	4.815607
233.759449	7999.799362	9.421146	-0.048718	4.815619
233.773347	7999.847618	9.426151	-0.048721	4.815633
233.886908	7999.782213	9.431155	-0.048742	4.815614
234.033209	7999.831539	9.436160	-0.048769	4.815627
233.870682	7999.761679	9.441165	-0.048739	4.815608
233.938856	7999.841763	9.446170	-0.048752	4.815631
233.899110	7999.789893	9.451175	-0.048744	4.815616
233.828617	7999.862403	9.456179	-0.048731	4.815637
233.992193	7999.871450	9.461184	-0.048762	4.815639
234.013321	7999.874996	9.466189	-0.048766	4.815640
234.077453	7999.837611	9.471194	-0.048778	4.815629
233.848038	7999.821103	9.476199	-0.048735	4.815625
233.942442	7999.779938	9.481203	-0.048753	4.815613
234.113761	7999.799783	9.486208	-0.048785	4.815618
234.166318	7999.858269	9.491213	-0.048795	4.815635
234.410209	7999.817382	9.496218	-0.048840	4.815621
234.441864	7999.792280	9.501223	-0.048846	4.815614
234.300691	7999.766523	9.506227	-0.048820	4.815607
234.492635	7999.821924	9.511232	-0.048855	4.815622
234.399514	7999.757452	9.516237	-0.048838	4.815604
234.457116	7999.774394	9.521242	-0.048849	4.815609
234.260818	7999.869422	9.526247	-0.048812	4.815637
234.319725	7999.760442	9.531251	-0.048823	4.815605
234.386826	7999.833038	9.536256	-0.048836	4.815626
234.260979	7999.882241	9.541261	-0.048813	4.815641
234.358875	7999.861411	9.546266	-0.048831	4.815635
234.397274	7999.825745	9.551271	-0.048838	4.815624
234.306332	7999.797597	9.556275	-0.048821	4.815616
234.447872	7999.807356	9.561280	-0.048847	4.815618
234.287313	7999.803699	9.566285	-0.048818	4.815618
234.410464	7999.872932	9.571290	-0.048841	4.815638
234.336565	7999.840789	9.576295	-0.048827	4.815629
234.424831	7999.771774	9.581299	-0.048843	4.815608
234.510344	7999.898035	9.586304	-0.048859	4.815645
234.286109	7999.823974	9.591309	-0.048818	4.815624
234.373893	7999.855279	9.596314	-0.048834	4.815633
234.341187	7999.880370	9.601319	-0.048828	4.815640
234.477502	7999.848419	9.606323	-0.048853	4.815630
234.329253	7999.868443	9.611328	-0.048826	4.815637
234.443256	7999.819055	9.616333	-0.048847	4.815622
234.558120	7999.830518	9.621338	-0.048868	4.815625
234.486002	7999.783462	9.626343	-0.048855	4.815611
234.526614	7999.796928	9.631347	-0.048863	4.815615
234.626628	7999.784671	9.636352	-0.048881	4.815611
234.489254	7999.863572	9.641357	-0.048856	4.815635
234.449340	7999.799959	9.646362	-0.048848	4.815616
234.534100	7999.819475	9.651367	-0.048864	4.815621
234.492673	7999.731289	9.656371	-0.048856	4.815596
234.757387	7999.759046	9.661376	-0.048906	4.815603
234.557172	7999.865751	9.666381	-0.048869	4.815635
234.796171	7999.785294	9.671386	-0.048913	4.815610
234.571475	7999.790208	9.676391	-0.048871	4.815613
234.479242	7999.794059	9.681395	-0.048854	4.815614
234.696731	7999.796506	9.686400	-0.048895	4.815614
234.659661	7999.840738	9.691405	-0.048888	4.815627
234.706346	7999.810542	9.696410	-0.048896	4.815618
234.727818	7999.783141	9.701415	-0.048900	4.815610
234.653931	7999.822510	9.706419	-0.048887	4.815622
234.673072	7999.877256	9.711424	-0.048890	4.815638
234.651652	7999.784055	9.716429	-0.048886	4.815611
234.768474	7999.782742	9.721434	-0.048908	4.815610
234.798876	7999.823795	9.726439	-0.048914	4.815621
234.655559	7999.849234	9.731443	-0.048887	4.815630
234.854931	7999.945315	9.736448	-0.048925	4.815657
234.700349	7999.843559	9.741453	-0.048896	4.815628
234.711638	7999.828802	9.746458	-0.048898	4.815623
234.619517	7999.800634	9.751463	-0.048881	4.815616
234.679559	7999.779193	9.756467	-0.048892	4.815609
234.756194	7999.792174	9.761472	-0.048906	4.815612
234.826804	7999.752758	9.766477	-0.048919	4.815601
235.041378	7999.817064	9.771482	-0.048959	4.815618
234.765448	7999.789130	9.776487	-0.048908	4.815611
234.750335	7999.825178	9.781491	-0.048905	4.815622
234.959711	7999.855246	9.786496	-0.048944	4.815630
234.878723	7999.819786	9.791501	-0.048929	4.815620
234.921984	7999.787400	9.796506	-0.048937	4.815610
234.749368	7999.830511	9.801511	-0.048905	4.815624
234.859928	7999.873926	9.806515	-0.048926	4.815636
234.860349	7999.783212	9.811520	-0.048926	4.815609
234.739296	7999.825021	9.816525	-0.048903	4.815622
234.945902	7999.800610	9.821530	-0.048942	4.815614
234.903005	7999.795651	9.826535	-0.048934	4.815613
234.809226	7999.874189	9.831539	-0.048917	4.815636
234.881524	7999.749414	9.836544	-0.048930	4.815599
234.818763	7999.888225	9.841549	-0.048918	4.815640
234.651416	7999.848169	9.846554	-0.048887	4.815629
234.822464	7999.795432	9.851559	-0.048919	4.815613
235.021809	7999.734614	9.856563	-0.048956	4.815594
235.006775	7999.808020	9.861568	-0.048954	4.815616
234.801567	7999.889029	9.866573	-0.048915	4.815641
234.984512	7999.783118	9.871578	-0.048949	4.815609
234.896287	7999.764619	9.876583	-0.048933	4.815604
234.869131	7999.843166	9.881587	-0.048928	4.815627
234.896928	7999.820137	9.886592	-0.048933	4.815620
234.854491	7999.781031	9.891597	-0.048925	4.815609
234.959737	7999.785935	9.896602	-0.048945	4.815610
234.997295	7999.811093	9.901607	-0.048952	4.815617
234.988510	7999.820560	9.906611	-0.048950	4.815620
235.036700	7999.869372	9.911616	-0.048960	4.815634
234.892458	7999.837160	9.916621	-0.048933	4.815625
235.081587	7999.828476	9.921626	-0.048968	4.815621
234.836955	7999.825596	9.926631	-0.048922	4.815622
234.737918	7999.774903	9.931635	-0.048904	4.815607
235.037389	7999.880071	9.936640	-0.048960	4.815637
234.988567	7999.793899	9.941645	-0.048951	4.815612
234.981331	7999.772438	9.946650	-0.048949	4.815606
234.908327	7999.776599	9.951655	-0.048936	4.815607
235.043576	7999.809739	9.956659	-0.048961	4.815616
235.030791	7999.869306	9.961664	-0.048959	4.815634
235.089245	7999.747509	9.966669	-0.048970	4.815598
235.261312	7999.792984	9.971674	-0.049002	4.815610
235.336017	7999.908400	9.976679	-0.049016	4.815644
235.091287	7999.731541	9.981683	-0.048970	4.815593
235.239400	7999.802246	9.986688	-0.048998	4.815613
235.150714	7999.750652	9.991693	-0.048981	4.815598
235.140336	7999.878568	9.996698	-0.048979	4.815636
235.102176	7999.777624	10.001703	-0.048972	4.815606
234.956430	7999.771005	10.006707	-0.048945	4.815605
235.045520	7999.788456	10.011712	-0.048962	4.815610
234.960357	7999.756131	10.016717	-0.048946	4.815601
235.045244	7999.784188	10.021722	-0.048962	4.815609
234.997577	7999.907233	10.026727	-0.048953	4.815645
234.971097	7999.762718	10.031731	-0.048948	4.815603
235.071965	7999.820918	10.036736	-0.048967	4.815619
235.102063	7999.761636	10.041741	-0.048973	4.815602
235.297587	7999.774403	10.046746	-0.049009	4.815605
235.227431	7999.795687	10.051751	-0.048996	4.815611
235.261014	7999.788761	10.056755	-0.049002	4.815609
235.344674	7999.838146	10.061760	-0.049018	4.815623
235.228205	7999.872557	10.066765	-0.048996	4.815634
235.237155	7999.747826	10.071770	-0.048998	4.815597
235.289570	7999.794571	10.076775	-0.049008	4.815611
235.070084	7999.845464	10.081779	-0.048967	4.815626
235.111694	7999.790637	10.086784	-0.048975	4.815610
235.259278	7999.832515	10.091789	-0.049002	4.815622
235.312396	7999.760797	10.096794	-0.049012	4.815601
235.232042	7999.813936	10.101799	-0.048997	4.815616
235.075720	7999.902139	10.106803	-0.048968	4.815643
235.425977	7999.741293	10.111808	-0.049033	4.815594
235.179872	7999.807766	10.116813	-0.048988	4.815615
235.254999	7999.862349	10.121818	-0.049002	4.815631
235.426486	7999.774398	10.126823	-0.049034	4.815604
235.276713	7999.802935	10.131827	-0.049006	4.815613
235.390598	7999.892300	10.136832	-0.049027	4.815639
235.373912	7999.808780	10.141837	-0.049024	4.815614
235.207449	7999.868000	10.146842	-0.048993	4.815632
235.019593	7999.789188	10.151847	-0.048958	4.815610
235.172981	7999.744706	10.156851	-0.048986	4.815596
235.228368	7999.892896	10.161856	-0.048997	4.815640
235.173135	7999.737243	10.166861	-0.048987	4.815594
235.369648	7999.864231	10.171866	-0.049023	4.815631
235.408938	7999.776279	10.176871	-0.049031	4.815605
235.325518	7999.844312	10.181875	-0.049015	4.815625
235.363655	7999.763813	10.186880	-0.049022	4.815601
235.304888	7999.877073	10.191885	-0.049011	4.815635
235.424489	7999.792552	10.196890	-0.049034	4.815609
235.325306	7999.761068	10.201895	-0.049015	4.815601
235.252927	7999.863434	10.206899	-0.049002	4.815631
235.305641	7999.757554	10.211904	-0.049012	4.815600
235.200051	7999.812421	10.216909	-0.048992	4.815616
235.165481	7999.838549	10.221914	-0.048986	4.815624
235.226043	7999.863012	10.226919	-0.048997	4.815631
235.228534	7999.832102	10.231923	-0.048997	4.815622
235.226339	7999.785107	10.236928	-0.048997	4.815608
235.341526	7999.839270	10.241933	-0.049019	4.815623
235.470682	7999.749567	10.246938	-0.049043	4.815596
235.366005	7999.775630	10.251943	-0.049023	4.815605
235.338407	7999.800804	10.256947	-0.049018	4.815612
235.468159	7999.795431	10.261952	-0.049042	4.815610
235.344655	7999.886298	10.266957	-0.049019	4.815637
235.314133	7999.796151	10.271962	-0.049014	4.815611
235.424458	7999.824620	10.276967	-0.049034	4.815619
235.508316	7999.802496	10.281971	-0.049050	4.815612
235.602669	7999.858458	10.286976	-0.049067	4.815628
235.536752	7999.850992	10.291981	-0.049055	4.815626
235.493006	7999.864164	10.296986	-0.049047	4.815630
235.322414	7999.852872	10.301991	-0.049015	4.815627
235.386161	7999.805874	10.306995	-0.049027	4.815613
235.602714	7999.813644	10.312000	-0.049068	4.815615
235.488737	7999.794729	10.317005	-0.049046	4.815610
235.481726	7999.806359	10.322010	-0.049045	4.815613
235.490594	7999.839593	10.327015	-0.049047	4.815623
235.458194	7999.777167	10.332019	-0.049041	4.815605
235.560634	7999.835394	10.337024	-0.049060	4.815621
235.493951	7999.859936	10.342029	-0.049048	4.815629
235.623691	7999.842823	10.347034	-0.049072	4.815623
235.346194	7999.881037	10.352039	-0.049020	4.815636
235.325882	7999.808133	10.357043	-0.049016	4.815614
235.417674	7999.809618	10.362048	-0.049034	4.815614
235.311762	7999.747072	10.367053	-0.049014	4.815596
235.269318	7999.777342	10.372058	-0.049006	4.815606
235.413374	7999.854386	10.377063	-0.049033	4.815627
235.471204	7999.895883	10.382067	-0.049044	4.815639
235.486239	7999.873714	10.387072	-0.049046	4.815633
235.312863	7999.789798	10.392077	-0.049014	4.815609
235.669326	7999.794491	10.397082	-0.049081	4.815609
235.631141	7999.835504	10.402087	-0.049074	4.815621
235.402403	7999.782715	10.407091	-0.049031	4.815606
235.572528	7999.844170	10.412096	-0.049063	4.815624
235.759590	7999.789557	10.417101	-0.049098	4.815607
235.609735	7999.819160	10.422106	-0.049070	4.815616
235.509943	7999.827157	10.427111	-0.049051	4.815619
235.529091	7999.819998	10.432115	-0.049055	4.815617
235.500831	7999.862239	10.437120	-0.049050	4.815629
235.435693	7999.804620	10.442125	-0.049037	4.815613
235.590638	7999.816732	10.447130	-0.049066	4.815616
235.603769	7999.852170	10.452135	-0.049069	4.815626
235.265539	7999.779467	10.457139	-0.049006	4.815606
235.392746	7999.805006	10.462144	-0.049030	4.815613
235.626680	7999.936870	10.467149	-0.049073	4.815651
235.623388	7999.806602	10.472154	-0.049073	4.815612
235.438736	7999.800421	10.477159	-0.049038	4.815611
235.529671	7999.762401	10.482163	-0.049055	4.815600
235.507788	7999.764185	10.487168	-0.049051	4.815601
235.612518	7999.864076	10.492173	-0.049071	4.815629
235.724785	7999.794380	10.497178	-0.049092	4.815608
235.563721	7999.785377	10.502183	-0.049062	4.815606
235.571185	7999.748143	10.507187	-0.049063	4.815596
235.529138	7999.814710	10.512192	-0.049055	4.815615
235.523318	7999.860515	10.517197	-0.049054	4.815629
235.421900	7999.756415	10.522202	-0.049035	4.815599
235.438830	7999.814328	10.527207	-0.049039	4.815616
235.452506	7999.776127	10.532211	-0.049041	4.815604
235.520991	7999.767630	10.537216	-0.049054	4.815601
235.512910	7999.778176	10.542221	-0.049052	4.815605
235.699587	7999.758780	10.547226	-0.049087	4.815598
235.653547	7999.858370	10.552231	-0.049079	4.815627
235.535846	7999.795633	10.557235	-0.049057	4.815610
235.637923	7999.837844	10.562240	-0.049076	4.815621
235.592811	7999.844590	10.567245	-0.049068	4.815624
235.517403	7999.824163	10.572250	-0.049054	4.815618
235.595787	7999.831836	10.577255	-0.049068	4.815620
235.614740	7999.797990	10.582259	-0.049072	4.815610
235.619642	7999.849305	10.587264	-0.049073	4.815625
235.549810	7999.815092	10.592269	-0.049060	4.815615
235.692563	7999.852623	10.597274	-0.049086	4.815626
235.634692	7999.799391	10.602279	-0.049076	4.815610
235.418260	7999.793764	10.607283	-0.049035	4.815610
235.560429	7999.818477	10.612288	-0.049062	4.815616
235.628352	7999.828116	10.617293	-0.049074	4.815619
235.512430	7999.796361	10.622298	-0.049053	4.815610
235.610943	7999.838515	10.627303	-0.049071	4.815622
235.597626	7999.810551	10.632307	-0.049069	4.815614
235.794049	7999.798784	10.637312	-0.049105	4.815609
235.665604	7999.849013	10.642317	-0.049082	4.815625
235.654701	7999.737835	10.647322	-0.049080	4.815592
235.889401	7999.830219	10.652327	-0.049123	4.815618
235.538137	7999.821346	10.657331	-0.049058	4.815617
235.570205	7999.858157	10.662336	-0.049064	4.815628
235.669160	7999.864028	10.667341	-0.049082	4.815629
235.620126	7999.883519	10.672346	-0.049073	4.815635
235.754843	7999.836599	10.677351	-0.049098	4.815621
235.723888	7999.788071	10.682355	-0.049093	4.815606
235.715290	7999.856246	10.687360	-0.049091	4.815626
235.489640	7999.804573	10.692365	-0.049049	4.815612
235.660004	7999.820136	10.697370	-0.049081	4.815616
235.986506	7999.867041	10.702375	-0.049142	4.815628
235.741369	7999.866286	10.707379	-0.049096	4.815629
235.713123	7999.844485	10.712384	-0.049091	4.815623
235.866444	7999.774385	10.717389	-0.049119	4.815602
235.760776	7999.769479	10.722394	-0.049100	4.815601
235.730139	7999.831961	10.727399	-0.049094	4.815619
235.735051	7999.782945	10.732403	-0.049095	4.815605
235.743519	7999.840722	10.737408	-0.049097	4.815622
235.631766	7999.822909	10.742413	-0.049076	4.815617
235.703293	7999.813394	10.747418	-0.049089	4.815614
235.837442	7999.853989	10.752423	-0.049114	4.815625
235.774519	7999.822022	10.757427	-0.049103	4.815616
235.715028	7999.812525	10.762432	-0.049092	4.815614
235.738660	7999.856672	10.767437	-0.049096	4.815626
235.786906	7999.852117	10.772442	-0.049105	4.815625
235.618481	7999.872881	10.777447	-0.049074	4.815632
235.855434	7999.838287	10.782451	-0.049118	4.815621
235.841096	7999.952266	10.787456	-0.049115	4.815654
235.660152	7999.874631	10.792461	-0.049082	4.815632
235.613995	7999.805577	10.797466	-0.049073	4.815612
235.656894	7999.899133	10.802471	-0.049081	4.815639
235.669949	7999.776601	10.807475	-0.049084	4.815603
235.866929	7999.844895	10.812480	-0.049120	4.815622
235.633776	7999.833660	10.817485	-0.049077	4.815620
235.753318	7999.796102	10.822490	-0.049099	4.815609
235.846776	7999.853117	10.827495	-0.049117	4.815625
235.742241	7999.793794	10.832499	-0.049097	4.815608
235.924255	7999.834095	10.837504	-0.049131	4.815619
235.722714	7999.803091	10.842509	-0.049094	4.815611
235.709543	7999.838104	10.847514	-0.049091	4.815621
235.833146	7999.867855	10.852519	-0.049114	4.815629
235.798403	7999.793649	10.857523	-0.049108	4.815608
235.738860	7999.843923	10.862528	-0.049097	4.815623
235.889086	7999.782312	10.867533	-0.049125	4.815604
235.830370	7999.783501	10.872538	-0.049114	4.815605
235.895827	7999.801639	10.877543	-0.049126	4.815610
235.899872	7999.865749	10.882547	-0.049127	4.815628
235.959506	7999.878456	10.887552	-0.049138	4.815632
235.940040	7999.848259	10.892557	-0.049134	4.815623
235.966665	7999.808132	10.897562	-0.049139	4.815611
235.865267	7999.855595	10.902567	-0.049121	4.815626
235.707553	7999.810356	10.907571	-0.049091	4.815613
235.798601	7999.837447	10.912576	-0.049108	4.815621
235.791200	7999.795703	10.917581	-0.049107	4.815608
235.953937	7999.797268	10.922586	-0.049137	4.815608
235.895218	7999.844353	10.927591	-0.049126	4.815622
235.853889	7999.810600	10.932595	-0.049119	4.815612
235.933208	7999.835367	10.937600	-0.049133	4.815619
235.852830	7999.820196	10.942605	-0.049119	4.815615
235.839779	7999.783698	10.947610	-0.049116	4.815605
235.957132	7999.869918	10.952615	-0.049138	4.815629
235.913434	7999.779557	10.957619	-0.049130	4.815603
235.850444	7999.811630	10.962624	-0.049118	4.815613
235.801324	7999.818311	10.967629	-0.049109	4.815615
235.869277	7999.774583	10.972634	-0.049122	4.815602
235.900476	7999.804976	10.977639	-0.049128	4.815611
235.766545	7999.880732	10.982643	-0.049103	4.815633
235.988816	7999.804274	10.987648	-0.049144	4.815610
235.923098	7999.792542	10.992653	-0.049132	4.815607
235.593573	7999.755202	10.997658	-0.049071	4.815597
235.911509	7999.831853	11.002663	-0.049130	4.815618
235.844286	7999.800884	11.007667	-0.049117	4.815610
235.748550	7999.839900	11.012672	-0.049100	4.815621
235.722745	7999.832015	11.017677	-0.049095	4.815619
235.871054	7999.793854	11.022682	-0.049122	4.815607
235.860103	7999.838509	11.027687	-0.049120	4.815621
235.710835	7999.820090	11.032691	-0.049093	4.815616
235.796764	7999.857772	11.037696	-0.049109	4.815626
235.885371	7999.848532	11.042701	-0.049125	4.815623
235.902300	7999.809317	11.047706	-0.049128	4.815612
236.069798	7999.835507	11.052711	-0.049160	4.815619
235.718264	7999.813821	11.057715	-0.049094	4.815614
235.746814	7999.852710	11.062720	-0.049100	4.815625
235.668701	7999.879202	11.067725	-0.049085	4.815633
235.795203	7999.791591	11.072730	-0.049109	4.815607
235.983707	7999.849075	11.077735	-0.049144	4.815623
235.677453	7999.780089	11.082739	-0.049087	4.815604
235.941344	7999.781152	11.087744	-0.049136	4.815603
235.888601	7999.849682	11.092749	-0.049126	4.815624
235.987167	7999.809650	11.097754	-0.049145	4.815611
236.026517	7999.936238	11.102759	-0.049152	4.815648
236.059744	7999.881275	11.107763	-0.049158	4.815632
236.081688	7999.853881	11.112768	-0.049162	4.815624
235.895068	7999.856205	11.117773	-0.049128	4.815626
235.959137	7999.911679	11.122778	-0.049140	4.815641
236.028448	7999.913869	11.127783	-0.049153	4.815642
235.911683	7999.786037	11.132787	-0.049131	4.815605
235.962953	7999.867988	11.137792	-0.049140	4.815629
236.036565	7999.846765	11.142797	-0.049154	4.815622
235.964361	7999.809311	11.147802	-0.049141	4.815611
235.894126	7999.920253	11.152807	-0.049128	4.815644
235.981663	7999.805328	11.157811	-0.049144	4.815610
235.795263	7999.826869	11.162816	-0.049109	4.815617
235.864085	7999.849330	11.167821	-0.049122	4.815624
235.962519	7999.764468	11.172826	-0.049141	4.815598
236.119639	7999.806501	11.177831	-0.049170	4.815610
236.160108	7999.815697	11.182835	-0.049177	4.815612
236.067699	7999.794994	11.187840	-0.049160	4.815607
235.978628	7999.793558	11.192845	-0.049144	4.815607
236.189272	7999.760674	11.197850	-0.049183	4.815596
236.165372	7999.896914	11.202855	-0.049179	4.815636
236.060849	7999.856803	11.207859	-0.049159	4.815625
236.071154	7999.868713	11.212864	-0.049161	4.815628
235.904124	7999.797707	11.217869	-0.049130	4.815608
235.848339	7999.800010	11.222874	-0.049120	4.815609
235.887169	7999.835864	11.227879	-0.049127	4.815620
235.845911	7999.826661	11.232883	-0.049119	4.815617
235.958526	7999.829551	11.237888	-0.049140	4.815617
236.028144	7999.833881	11.242893	-0.049153	4.815618
236.049354	7999.746703	11.247898	-0.049157	4.815593
236.066685	7999.899619	11.252903	-0.049161	4.815637
235.931545	7999.826992	11.257907	-0.049135	4.815617
235.961939	7999.855238	11.262912	-0.049141	4.815625
235.975463	7999.890682	11.267917	-0.049144	4.815635
235.892686	7999.805026	11.272922	-0.049128	4.815611
236.028505	7999.832840	11.277927	-0.049154	4.815618
235.966248	7999.782739	11.282931	-0.049142	4.815604
235.990179	7999.846103	11.287936	-0.049146	4.815622
236.049686	7999.842797	11.292941	-0.049158	4.815621
235.941529	7999.793022	11.297946	-0.049137	4.815607
235.898467	7999.842495	11.302951	-0.049130	4.815621
235.898188	7999.779519	11.307955	-0.049129	4.815603
236.058961	7999.855768	11.312960	-0.049159	4.815625
235.878314	7999.820831	11.317965	-0.049126	4.815615
235.716846	7999.815024	11.322970	-0.049096	4.815614
235.901843	7999.901270	11.327975	-0.049130	4.815639
235.887137	7999.791097	11.332979	-0.049128	4.815606
235.956693	7999.888286	11.337984	-0.049141	4.815635
235.939955	7999.864536	11.342989	-0.049138	4.815628
235.936844	7999.847411	11.347994	-0.049137	4.815623
236.045110	7999.835288	11.352999	-0.049157	4.815619
235.904435	7999.854365	11.358003	-0.049131	4.815625
236.046896	7999.863074	11.363008	-0.049158	4.815627
236.007386	7999.841091	11.368013	-0.049150	4.815621
235.890277	7999.826394	11.373018	-0.049128	4.815617
236.094169	7999.843567	11.378023	-0.049166	4.815621
235.947529	7999.837999	11.383027	-0.049139	4.815620
236.025321	7999.849932	11.388032	-0.049154	4.815623
236.082054	7999.823100	11.393037	-0.049164	4.815615
236.030823	7999.789187	11.398042	-0.049155	4.815605
235.922483	7999.844010	11.403047	-0.049135	4.815622
235.905056	7999.814913	11.408051	-0.049131	4.815613
236.149737	7999.795387	11.413056	-0.049177	4.815606
236.005822	7999.857107	11.418061	-0.049150	4.815625
236.114709	7999.787355	11.423066	-0.049171	4.815604
236.241212	7999.864118	11.428071	-0.049194	4.815626
236.116458	7999.855701	11.433075	-0.049171	4.815624
235.999217	7999.781229	11.438080	-0.049149	4.815603
236.084823	7999.768739	11.443085	-0.049165	4.815599
236.024584	7999.763500	11.448090	-0.049154	4.815598
236.140830	7999.814479	11.453095	-0.049176	4.815612
235.905924	7999.764791	11.458099	-0.049132	4.815599
235.960480	7999.836121	11.463104	-0.049142	4.815619
236.064682	7999.854885	11.468109	-0.049162	4.815624
235.989148	7999.825916	11.473114	-0.049148	4.815616
236.225270	7999.819061	11.478119	-0.049192	4.815613
235.805969	7999.802683	11.483123	-0.049114	4.815610
236.002957	7999.876315	11.488128	-0.049150	4.815631
235.925742	7999.825971	11.493133	-0.049136	4.815616
236.117992	7999.883516	11.498138	-0.049172	4.815632
236.025388	7999.791297	11.503143	-0.049154	4.815606
235.907496	7999.790463	11.508147	-0.049133	4.815606
236.105951	7999.841703	11.513152	-0.049170	4.815620
235.992918	7999.845217	11.518157	-0.049149	4.815622
235.888394	7999.760277	11.523162	-0.049129	4.815597
236.379827	7999.788499	11.528167	-0.049221	4.815603
236.095130	7999.885302	11.533171	-0.049168	4.815633
236.089949	7999.815843	11.538176	-0.049167	4.815613
236.021398	7999.805132	11.543181	-0.049154	4.815610
236.111435	7999.814061	11.548186	-0.049171	4.815612
236.078766	7999.798593	11.553191	-0.049165	4.815608
236.055011	7999.796078	11.558195	-0.049160	4.815607
236.255513	7999.838813	11.563200	-0.049198	4.815619
236.064529	7999.807979	11.568205	-0.049162	4.815611
236.241595	7999.757474	11.573210	-0.049195	4.815595
236.232324	7999.763731	11.578215	-0.049194	4.815597
236.219334	7999.926832	11.583219	-0.049191	4.815645
236.069860	7999.817683	11.588224	-0.049163	4.815613
236.098982	7999.812820	11.593229	-0.049169	4.815612
236.182192	7999.781079	11.598234	-0.049184	4.815602
236.279655	7999.899000	11.603239	-0.049203	4.815636
236.063892	7999.859226	11.608243	-0.049162	4.815626
236.127781	7999.831442	11.613248	-0.049174	4.815617
236.036113	7999.838503	11.618253	-0.049157	4.815620
235.866520	7999.781331	11.623258	-0.049126	4.815604
236.082037	7999.868070	11.628263	-0.049166	4.815628
236.120485	7999.796113	11.633267	-0.049173	4.815607
236.098418	7999.820309	11.638272	-0.049169	4.815614
236.114651	7999.807766	11.643277	-0.049172	4.815610
236.179255	7999.860046	11.648282	-0.049184	4.815625
236.240846	7999.852505	11.653287	-0.049196	4.815623
236.030158	7999.792534	11.658291	-0.049156	4.815606
236.119252	7999.816391	11.663296	-0.049173	4.815613
236.185211	7999.833470	11.668301	-0.049185	4.815617
236.434891	7999.822564	11.673306	-0.049232	4.815613
236.168431	7999.888708	11.678311	-0.049182	4.815634
236.262445	7999.741866	11.683315	-0.049200	4.815590
236.135394	7999.858294	11.688320	-0.049176	4.815625
236.260946	7999.847517	11.693325	-0.049200	4.815621
236.049869	7999.793944	11.698330	-0.049160	4.815606
236.178180	7999.863264	11.703335	-0.049184	4.815626
236.093476	7999.781846	11.708339	-0.049169	4.815603
236.175254	7999.800248	11.713344	-0.049184	4.815608
236.070315	7999.863665	11.718349	-0.049164	4.815627
236.157620	7999.792497	11.723354	-0.049181	4.815606
235.895093	7999.857637	11.728359	-0.049132	4.815626
236.007749	7999.796486	11.733363	-0.049153	4.815607
235.967168	7999.795834	11.738368	-0.049145	4.815607
236.040297	7999.755391	11.743373	-0.049159	4.815595
236.202226	7999.733460	11.748378	-0.049189	4.815588
236.369249	7999.910143	11.753383	-0.049220	4.815639
236.279141	7999.800886	11.758387	-0.049204	4.815607
236.235525	7999.776702	11.763392	-0.049195	4.815601
236.377136	7999.751241	11.768397	-0.049222	4.815592
236.309113	7999.776829	11.773402	-0.049209	4.815600
236.210095	7999.810456	11.778407	-0.049191	4.815611
236.284773	7999.791385	11.783411	-0.049205	4.815605
236.356244	7999.797880	11.788416	-0.049218	4.815606
236.153015	7999.837294	11.793421	-0.049180	4.815619
236.275065	7999.884099	11.798426	-0.049203	4.815632
236.304456	7999.817332	11.803431	-0.049209	4.815612
236.265328	7999.798558	11.808435	-0.049201	4.815607
236.447016	7999.789755	11.813440	-0.049235	4.815603
236.341846	7999.889459	11.818445	-0.049216	4.815633
236.061014	7999.750436	11.823450	-0.049163	4.815594
236.145000	7999.804097	11.828455	-0.049179	4.815609
236.206246	7999.767732	11.833459	-0.049190	4.815598
236.200369	7999.807132	11.838464	-0.049189	4.815610
236.191940	7999.842222	11.843469	-0.049188	4.815620
236.226025	7999.894010	11.848474	-0.049194	4.815635
236.276007	7999.820104	11.853479	-0.049204	4.815613
236.189387	7999.792024	11.858483	-0.049187	4.815605
236.131573	7999.775082	11.863488	-0.049177	4.815601
236.313999	7999.824997	11.868493	-0.049211	4.815614
236.097027	7999.778800	11.873498	-0.049170	4.815602
236.302046	7999.781047	11.878503	-0.049209	4.815601
236.124404	7999.815538	11.883507	-0.049176	4.815612
236.173802	7999.818474	11.888512	-0.049185	4.815613
236.127522	7999.807056	11.893517	-0.049176	4.815610
236.193893	7999.886049	11.898522	-0.049189	4.815633
236.342202	7999.803059	11.903527	-0.049216	4.815608
236.235609	7999.770386	11.908531	-0.049196	4.815599
236.257486	7999.762203	11.913536	-0.049201	4.815596
236.190207	7999.799544	11.918541	-0.049188	4.815607
236.355505	7999.878002	11.923546	-0.049219	4.815630
236.184602	7999.835750	11.928551	-0.049187	4.815618
236.385620	7999.805913	11.933555	-0.049225	4.815608
236.487592	7999.773408	11.938560	-0.049244	4.815598
236.314411	7999.902967	11.943565	-0.049211	4.815637
236.070711	7999.768813	11.948570	-0.049166	4.815599
236.268271	7999.776277	11.953575	-0.049203	4.815600
236.106246	7999.765124	11.958579	-0.049173	4.815598
236.345886	7999.771133	11.963584	-0.049217	4.815598
236.217452	7999.810688	11.968589	-0.049193	4.815611
236.159081	7999.833230	11.973594	-0.049183	4.815617
236.095428	7999.762826	11.978599	-0.049171	4.815597
236.088593	7999.836367	11.983603	-0.049170	4.815619
236.408294	7999.760415	11.988608	-0.049229	4.815595
236.248443	7999.824012	11.993613	-0.049199	4.815614
236.171505	7999.776875	11.998618	-0.049185	4.815601
236.370346	7999.830257	12.003623	-0.049222	4.815616
236.209686	7999.795643	12.008627	-0.049192	4.815606
236.268362	7999.820077	12.013632	-0.049203	4.815613
236.164210	7999.838677	12.018637	-0.049184	4.815619
236.244393	7999.796213	12.023642	-0.049199	4.815606
236.318442	7999.844377	12.028647	-0.049213	4.815620
236.082198	7999.810676	12.033651	-0.049169	4.815611
236.358431	7999.893061	12.038656	-0.049220	4.815634
236.243886	7999.857057	12.043661	-0.049199	4.815624
236.109441	7999.750286	12.048666	-0.049174	4.815593
236.331552	7999.816852	12.053671	-0.049215	4.815612
236.370824	7999.853780	12.058675	-0.049223	4.815622
236.297179	7999.838717	12.063680	-0.049209	4.815618
236.369443	7999.843090	12.068685	-0.049222	4.815619
236.302475	7999.821731	12.073690	-0.049210	4.815613
236.464561	7999.844633	12.078695	-0.049240	4.815619
236.208582	7999.782862	12.083699	-0.049193	4.815602
236.601519	7999.838313	12.088704	-0.049266	4.815617
236.310878	7999.821879	12.093709	-0.049212	4.815613
236.124655	7999.875443	12.098714	-0.049177	4.815630
236.373811	7999.827171	12.103719	-0.049224	4.815615
236.265202	7999.816880	12.108723	-0.049203	4.815612
236.297111	7999.793917	12.113728	-0.049209	4.815605
236.292084	7999.815186	12.118733	-0.049208	4.815611
236.184477	7999.802776	12.123738	-0.049188	4.815608
236.304765	7999.889045	12.128743	-0.049211	4.815633
236.106737	7999.834615	12.133747	-0.049174	4.815618
236.297302	7999.789665	12.138752	-0.049209	4.815604
236.299999	7999.812126	12.143757	-0.049210	4.815611
236.280077	7999.792595	12.148762	-0.049206	4.815605
236.411966	7999.842761	12.153767	-0.049231	4.815619
236.380629	7999.820910	12.158771	-0.049225	4.815613
236.226500	7999.799210	12.163776	-0.049196	4.815607
236.176142	7999.979852	12.168781	-0.049187	4.815660
236.296256	7999.876126	12.173786	-0.049210	4.815629
236.260642	7999.878756	12.178791	-0.049203	4.815630
236.195398	7999.836077	12.183795	-0.049191	4.815618
236.238700	7999.836780	12.188800	-0.049199	4.815618
236.304843	7999.891220	12.193805	-0.049211	4.815634
236.206389	7999.875756	12.198810	-0.049193	4.815630
236.288081	7999.896292	12.203815	-0.049208	4.815635
236.556421	7999.816309	12.208819	-0.049258	4.815611
236.350475	7999.793771	12.213824	-0.049220	4.815605
236.216566	7999.840709	12.218829	-0.049195	4.815619
236.416896	7999.790581	12.223834	-0.049232	4.815604
236.366649	7999.901846	12.228839	-0.049223	4.815636
236.327955	7999.871337	12.233843	-0.049216	4.815628
236.262222	7999.856402	12.238848	-0.049204	4.815624
236.389739	7999.905430	12.243853	-0.049228	4.815637
236.142319	7999.793631	12.248858	-0.049181	4.815606
236.505770	7999.897705	12.253863	-0.049249	4.815635
236.405292	7999.854457	12.258867	-0.049230	4.815622
236.356931	7999.816320	12.263872	-0.049221	4.815611
236.212229	7999.855612	12.268877	-0.049195	4.815624
236.315978	7999.779374	12.273882	-0.049214	4.815601
236.396308	7999.867132	12.278887	-0.049229	4.815626
236.212243	7999.850285	12.283891	-0.049195	4.815622
236.478836	7999.857798	12.288896	-0.049244	4.815623
236.548174	7999.897347	12.293901	-0.049257	4.815634
236.483488	7999.815184	12.298906	-0.049245	4.815611
236.233056	7999.822881	12.303911	-0.049199	4.815614
236.384918	7999.840281	12.308915	-0.049227	4.815618
236.406671	7999.815019	12.313920	-0.049231	4.815611
236.337510	7999.851262	12.318925	-0.049218	4.815622
236.324485	7999.792350	12.323930	-0.049216	4.815605
236.529538	7999.874652	12.328935	-0.049254	4.815628
236.312368	7999.914908	12.333939	-0.049214	4.815641
236.465618	7999.872557	12.338944	-0.049242	4.815627
236.603090	7999.906804	12.343949	-0.049268	4.815637
236.428970	7999.908262	12.348954	-0.049236	4.815638
236.433133	7999.878446	12.353959	-0.049236	4.815629
236.447065	7999.872269	12.358963	-0.049239	4.815627
236.315390	7999.827450	12.363968	-0.049214	4.815615
236.277759	7999.867405	12.368973	-0.049207	4.815627
236.372620	7999.808100	12.373978	-0.049225	4.815609
236.441243	7999.819886	12.378983	-0.049238	4.815612
236.303887	7999.758964	12.383987	-0.049212	4.815595
236.339686	7999.807577	12.388992	-0.049219	4.815609
236.411300	7999.863173	12.393997	-0.049233	4.815625
236.322756	7999.815849	12.399002	-0.049216	4.815611
236.359236	7999.819643	12.404007	-0.049223	4.815612
236.559606	7999.810075	12.409011	-0.049260	4.815609
236.598268	7999.819242	12.414016	-0.049267	4.815611
236.544151	7999.838651	12.419021	-0.049257	4.815617
236.557293	7999.781228	12.424026	-0.049260	4.815600
236.515702	7999.867016	12.429031	-0.049252	4.815626
236.387658	7999.825457	12.434035	-0.049228	4.815614
236.325502	7999.783896	12.439040	-0.049217	4.815602
236.394709	7999.786084	12.444045	-0.049230	4.815602
236.588479	7999.843655	12.449050	-0.049266	4.815618
236.581766	7999.762428	12.454055	-0.049265	4.815595
236.414034	7999.780001	12.459059	-0.049233	4.815601
236.421417	7999.796134	12.464064	-0.049235	4.815605
236.495444	7999.820816	12.469069	-0.049249	4.815612
236.460301	7999.793566	12.474074	-0.049242	4.815604
236.437194	7999.830554	12.479079	-0.049238	4.815615
236.338834	7999.810822	12.484083	-0.049220	4.815610
236.448994	7999.811538	12.489088	-0.049240	4.815610
236.536420	7999.937837	12.494093	-0.049257	4.815646
236.412746	7999.815228	12.499098	-0.049233	4.815611
236.686468	7999.791902	12.504103	-0.049284	4.815603
236.439318	7999.797518	12.509107	-0.049238	4.815606
236.549669	7999.825988	12.514112	-0.049259	4.815613
236.599955	7999.867364	12.519117	-0.049269	4.815625
236.429449	7999.809108	12.524122	-0.049237	4.815609
236.571827	7999.811412	12.529127	-0.049263	4.815609
236.452547	7999.773197	12.534131	-0.049241	4.815598
236.533790	7999.794793	12.539136	-0.049256	4.815604
236.545147	7999.813125	12.544141	-0.049258	4.815610
236.467262	7999.841755	12.549146	-0.049244	4.815618
236.539474	7999.861071	12.554151	-0.049257	4.815624
236.608846	7999.898486	12.559155	-0.049270	4.815634
236.754566	7999.821858	12.564160	-0.049298	4.815611
236.482638	7999.840948	12.569165	-0.049247	4.815618
236.391429	7999.761559	12.574170	-0.049230	4.815595
236.508858	7999.871265	12.579175	-0.049252	4.815627
236.473408	7999.811989	12.584179	-0.049245	4.815610
236.372137	7999.808221	12.589184	-0.049227	4.815609
236.369190	7999.796435	12.594189	-0.049226	4.815606
236.602763	7999.761787	12.599194	-0.049270	4.815594
236.579836	7999.792373	12.604199	-0.049265	4.815603
236.480354	7999.808914	12.609203	-0.049247	4.815609
236.687495	7999.908329	12.614208	-0.049285	4.815637
236.491934	7999.793097	12.619213	-0.049249	4.815604
236.344623	7999.776844	12.624218	-0.049222	4.815600
236.662326	7999.792654	12.629223	-0.049281	4.815603
236.472046	7999.770369	12.634227	-0.049245	4.815597
236.408944	7999.782161	12.639232	-0.049234	4.815601
236.530672	7999.823624	12.644237	-0.049256	4.815613
236.615159	7999.861283	12.649242	-0.049272	4.815623
236.499554	7999.791106	12.654247	-0.049251	4.815603
236.484969	7999.833568	12.659251	-0.049248	4.815616
236.498185	7999.807100	12.664256	-0.049251	4.815608
236.520814	7999.838423	12.669261	-0.049255	4.815617
236.588584	7999.802163	12.674266	-0.049267	4.815606
236.614173	7999.833533	12.679271	-0.049272	4.815615
236.598102	7999.851422	12.684275	-0.049269	4.815621
236.375947	7999.766715	12.689280	-0.049228	4.815597
236.577362	7999.810533	12.694285	-0.049265	4.815609
236.740829	7999.798234	12.699290	-0.049296	4.815604
236.759756	7999.786802	12.704295	-0.049299	4.815601
236.529398	7999.800160	12.709299	-0.049257	4.815606
236.655041	7999.898258	12.714304	-0.049280	4.815634
236.838429	7999.823306	12.719309	-0.049314	4.815611
236.558001	7999.852933	12.724314	-0.049262	4.815621
236.710851	7999.835126	12.729319	-0.049291	4.815615
236.558922	7999.731273	12.734323	-0.049262	4.815586
236.474901	7999.866542	12.739328	-0.049247	4.815626
236.446052	7999.822316	12.744333	-0.049241	4.815613
236.373201	7999.812603	12.749338	-0.049228	4.815610
236.632092	7999.879765	12.754343	-0.049276	4.815629
236.488292	7999.796324	12.759347	-0.049249	4.815605
236.570185	7999.759224	12.764352	-0.049265	4.815594
236.527820	7999.804440	12.769357	-0.049257	4.815607
236.706874	7999.769978	12.774362	-0.049290	4.815596
236.667589	7999.818446	12.779367	-0.049283	4.815611
236.627270	7999.795382	12.784371	-0.049275	4.815604
236.680456	7999.786638	12.789376	-0.049285	4.815601
236.663584	7999.846142	12.794381	-0.049282	4.815619
236.538174	7999.755526	12.799386	-0.049259	4.815593
236.676372	7999.799390	12.804391	-0.049285	4.815605
236.537370	7999.782203	12.809395	-0.049259	4.815601
236.648249	7999.779728	12.814400	-0.049279	4.815599
236.647593	7999.839494	12.819405	-0.049279	4.815617
236.553473	7999.783540	12.824410	-0.049262	4.815601
236.761718	7999.829603	12.829415	-0.049301	4.815613
236.645874	7999.865092	12.834419	-0.049279	4.815624
236.655633	7999.846040	12.839424	-0.049281	4.815619
236.547341	7999.894460	12.844429	-0.049261	4.815633
236.689267	7999.854061	12.849434	-0.049287	4.815621
236.605779	7999.844176	12.854439	-0.049272	4.815618
236.535036	7999.928426	12.859443	-0.049259	4.815643
236.652609	7999.847074	12.864448	-0.049281	4.815619
236.769513	7999.904470	12.869453	-0.049303	4.815635
236.454532	7999.828935	12.874458	-0.049244	4.815615
236.476940	7999.848513	12.879463	-0.049248	4.815620
236.654029	7999.903680	12.884467	-0.049281	4.815636
236.546186	7999.831493	12.889472	-0.049261	4.815615
236.503439	7999.806255	12.894477	-0.049253	4.815608
236.572945	7999.775360	12.899482	-0.049266	4.815598
236.603796	7999.807883	12.904487	-0.049272	4.815608
236.693844	7999.828554	12.909491	-0.049289	4.815613
236.499878	7999.841433	12.914496	-0.049253	4.815618
236.638319	7999.890638	12.919501	-0.049278	4.815632
236.466960	7999.814223	12.924506	-0.049247	4.815610
236.682641	7999.846531	12.929511	-0.049287	4.815619
236.627563	7999.804016	12.934515	-0.049276	4.815606
236.893927	7999.816862	12.939520	-0.049326	4.815609
236.666204	7999.855880	12.944525	-0.049284	4.815621
236.614733	7999.785672	12.949530	-0.049274	4.815601
236.639817	7999.826640	12.954535	-0.049279	4.815613
236.768671	7999.890634	12.959539	-0.049303	4.815631
236.472098	7999.802589	12.964544	-0.049248	4.815607
236.627964	7999.836064	12.969549	-0.049277	4.815616
236.397284	7999.814194	12.974554	-0.049234	4.815611
236.603384	7999.791911	12.979559	-0.049272	4.815603
236.442314	7999.844814	12.984563	-0.049242	4.815619
236.656288	7999.743672	12.989568	-0.049282	4.815589
236.536454	7999.788703	12.994573	-0.049260	4.815602
236.430521	7999.844633	12.999578	-0.049240	4.815619
236.805695	7999.765308	13.004583	-0.049310	4.815594
236.708654	7999.877953	13.009587	-0.049292	4.815628
236.720002	7999.778873	13.014592	-0.049294	4.815599
236.991864	7999.800347	13.019597	-0.049345	4.815604
236.739434	7999.772788	13.024602	-0.049298	4.815597
236.638346	7999.798910	13.029607	-0.049279	4.815605
236.645264	7999.775542	13.034611	-0.049280	4.815598
236.531815	7999.785453	13.039616	-0.049259	4.815601
236.674284	7999.799499	13.044621	-0.049286	4.815605
236.590980	7999.759731	13.049626	-0.049270	4.815594
236.746817	7999.883933	13.054631	-0.049300	4.815629
236.797883	7999.769484	13.059635	-0.049309	4.815596
236.558409	7999.752809	13.064640	-0.049264	4.815592
236.840630	7999.793664	13.069645	-0.049317	4.815602
236.695517	7999.778513	13.074650	-0.049290	4.815599
236.722031	7999.845122	13.079655	-0.049295	4.815618
236.638360	7999.797875	13.084659	-0.049280	4.815605
236.893250	7999.788122	13.089664	-0.049327	4.815601
236.667686	7999.816501	13.094669	-0.049285	4.815610
236.387858	7999.854677	13.099674	-0.049233	4.815622
236.573565	7999.790436	13.104679	-0.049268	4.815603
236.738952	7999.805920	13.109683	-0.049298	4.815606
236.665835	7999.804742	13.114688	-0.049285	4.815606
236.644424	7999.881250	13.119693	-0.049281	4.815629
236.813425	7999.822076	13.124698	-0.049312	4.815611
236.728426	7999.824975	13.129703	-0.049297	4.815612
236.422457	7999.801888	13.134707	-0.049240	4.815607
236.471799	7999.783476	13.139712	-0.049249	4.815601
236.598676	7999.835696	13.144717	-0.049273	4.815616
236.456834	7999.776836	13.149722	-0.049246	4.815599
236.744545	7999.858339	13.154727	-0.049300	4.815622
236.756489	7999.821177	13.159731	-0.049302	4.815611
236.693818	7999.874604	13.164736	-0.049290	4.815627
236.639660	7999.816093	13.169741	-0.049280	4.815610
236.510111	7999.762768	13.174746	-0.049256	4.815595
236.755884	7999.797697	13.179751	-0.049302	4.815604
236.600057	7999.804788	13.184755	-0.049273	4.815607
236.813136	7999.794358	13.189760	-0.049313	4.815603
236.847349	7999.906990	13.194765	-0.049319	4.815636
236.678785	7999.780452	13.199770	-0.049288	4.815599
236.811725	7999.837040	13.204775	-0.049313	4.815615
236.733186	7999.880604	13.209779	-0.049298	4.815628
236.482746	7999.785832	13.214784	-0.049251	4.815602
236.578647	7999.795924	13.219789	-0.049269	4.815604
236.831928	7999.759459	13.224794	-0.049316	4.815592
236.598759	7999.782379	13.229799	-0.049273	4.815600
236.578119	7999.915471	13.234803	-0.049269	4.815639
236.507771	7999.752095	13.239808	-0.049256	4.815592
236.561604	7999.760440	13.244813	-0.049266	4.815594
236.433597	7999.753038	13.249818	-0.049242	4.815592
236.691108	7999.900231	13.254823	-0.049291	4.815634
236.773225	7999.791620	13.259827	-0.049306	4.815602
236.654949	7999.781173	13.264832	-0.049284	4.815600
236.754338	7999.827612	13.269837	-0.049302	4.815613
236.599379	7999.856065	13.274842	-0.049274	4.815622
236.615073	7999.802952	13.279847	-0.049277	4.815606
236.687513	7999.779576	13.284851	-0.049290	4.815599
236.845026	7999.761845	13.289856	-0.049319	4.815593
236.942522	7999.787973	13.294861	-0.049338	4.815600
236.542363	7999.751623	13.299866	-0.049263	4.815592
236.551770	7999.788069	13.304871	-0.049265	4.815602
236.799603	7999.915893	13.309875	-0.049311	4.815638
236.687815	7999.788138	13.314880	-0.049290	4.815601
236.484859	7999.764581	13.319885	-0.049253	4.815596
236.509699	7999.747908	13.324890	-0.049257	4.815591
236.645985	7999.791741	13.329895	-0.049283	4.815603
236.629952	7999.851258	13.334899	-0.049280	4.815620
236.504329	7999.799064	13.339904	-0.049256	4.815606
236.610399	7999.882969	13.344909	-0.049276	4.815630
236.411462	7999.863747	13.349914	-0.049239	4.815625
236.526228	7999.805831	13.354919	-0.049260	4.815607
236.535381	7999.787837	13.359923	-0.049262	4.815602
236.411169	7999.759148	13.364928	-0.049239	4.815594
236.490656	7999.795659	13.369933	-0.049254	4.815605
236.572647	7999.783111	13.374938	-0.049269	4.815601
236.706074	7999.820494	13.379943	-0.049294	4.815611
236.620143	7999.842590	13.384947	-0.049278	4.815618
236.660903	7999.776007	13.389952	-0.049286	4.815598
236.788911	7999.827178	13.394957	-0.049310	4.815612
236.607945	7999.763416	13.399962	-0.049276	4.815595
236.849255	7999.816418	13.404967	-0.049321	4.815609
236.696500	7999.926028	13.409971	-0.049293	4.815642
236.521648	7999.762031	13.414976	-0.049260	4.815595
236.539906	7999.769800	13.419981	-0.049263	4.815597
236.632193	7999.854550	13.424986	-0.049281	4.815621
236.568031	7999.817225	13.429991	-0.049269	4.815611
236.671957	7999.825312	13.434995	-0.049288	4.815612
236.612125	7999.793394	13.440000	-0.049277	4.815603
236.712514	7999.838782	13.445005	-0.049296	4.815616
236.433759	7999.794787	13.450010	-0.049244	4.815605
236.585157	7999.832460	13.455015	-0.049272	4.815615
236.735634	7999.788998	13.460019	-0.049300	4.815601
236.637237	7999.787410	13.465024	-0.049282	4.815601
236.586170	7999.773780	13.470029	-0.049272	4.815598
236.524509	7999.822953	13.475034	-0.049261	4.815612
236.478925	7999.792333	13.480039	-0.049253	4.815604
236.469511	7999.809262	13.485043	-0.049251	4.815609
236.466658	7999.755850	13.490048	-0.049250	4.815593
236.831849	7999.879166	13.495053	-0.049318	4.815627
236.726629	7999.850784	13.500058	-0.049299	4.815620
236.819031	7999.820259	13.505063	-0.049316	4.815610
236.622961	7999.850182	13.510067	-0.049280	4.815620
236.642847	7999.871854	13.515072	-0.049283	4.815626
236.581968	7999.824976	13.520077	-0.049272	4.815613
236.584357	7999.800468	13.525082	-0.049272	4.815606
236.713222	7999.816429	13.530087	-0.049297	4.815610
236.660823	7999.801709	13.535091	-0.049287	4.815606
236.674930	7999.752841	13.540096	-0.049289	4.815591
236.715545	7999.817543	13.545101	-0.049297	4.815610
236.638847	7999.754399	13.550106	-0.049283	4.815592
236.756503	7999.761640	13.555111	-0.049305	4.815593
236.807818	7999.883086	13.560115	-0.049314	4.815629
236.696060	7999.769208	13.565120	-0.049294	4.815596
236.703716	7999.819502	13.570125	-0.049295	4.815611
236.680328	7999.772162	13.575130	-0.049291	4.815597
236.954222	7999.804343	13.580135	-0.049342	4.815605
236.564872	7999.816199	13.585139	-0.049269	4.815610
236.738480	7999.758167	13.590144	-0.049302	4.815592
236.836317	7999.836603	13.595149	-0.049320	4.815615
236.632616	7999.771406	13.600154	-0.049282	4.815597
236.773083	7999.900698	13.605159	-0.049308	4.815634
236.847195	7999.841057	13.610163	-0.049322	4.815616
236.680743	7999.777529	13.615168	-0.049291	4.815598
236.592589	7999.828409	13.620173	-0.049275	4.815614
236.422083	7999.770154	13.625178	-0.049243	4.815597
236.652131	7999.769604	13.630183	-0.049286	4.815596
236.501535	7999.756500	13.635187	-0.049258	4.815593
236.611310	7999.740132	13.640192	-0.049278	4.815588
236.601654	7999.878738	13.645197	-0.049277	4.815628
236.680388	7999.726310	13.650202	-0.049291	4.815583
236.572377	7999.859058	13.655207	-0.049271	4.815623
236.751689	7999.795781	13.660211	-0.049305	4.815603
236.736636	7999.889470	13.665216	-0.049302	4.815631
236.971987	7999.833504	13.670221	-0.049346	4.815613
236.746820	7999.801048	13.675226	-0.049304	4.815605
236.582605	7999.779184	13.680231	-0.049273	4.815599
236.658477	7999.800694	13.685235	-0.049287	4.815605
236.656907	7999.777189	13.690240	-0.049287	4.815598
236.803346	7999.764615	13.695245	-0.049314	4.815594
236.703996	7999.863346	13.700250	-0.049296	4.815623
236.727275	7999.791144	13.705255	-0.049300	4.815602
236.770978	7999.812133	13.710259	-0.049309	4.815608
236.738615	7999.776390	13.715264	-0.049303	4.815598
236.635863	7999.859055	13.720269	-0.049283	4.815622
236.568749	7999.804604	13.725274	-0.049271	4.815607
236.784164	7999.785674	13.730279	-0.049311	4.815600
236.620635	7999.882300	13.735283	-0.049281	4.815629
236.443707	7999.825008	13.740288	-0.049248	4.815613
236.736283	7999.893782	13.745293	-0.049302	4.815632
236.644604	7999.881629	13.750298	-0.049285	4.815629
236.677696	7999.850146	13.755303	-0.049291	4.815620
236.535779	7999.864933	13.760307	-0.049265	4.815625
236.831031	7999.768306	13.765312	-0.049320	4.815595
236.829372	7999.837663	13.770317	-0.049320	4.815615
236.622333	7999.820444	13.775322	-0.049281	4.815611
236.766706	7999.836656	13.780327	-0.049308	4.815615
236.884972	7999.856716	13.785331	-0.049330	4.815621
236.681308	7999.758430	13.790336	-0.049292	4.815593
236.819810	7999.805501	13.795341	-0.049318	4.815606
236.751318	7999.777713	13.800346	-0.049305	4.815598
236.763648	7999.832352	13.805351	-0.049308	4.815614
236.592319	7999.792228	13.810355	-0.049276	4.815603
236.701304	7999.769442	13.815360	-0.049296	4.815596
236.874048	7999.793584	13.820365	-0.049328	4.815602
236.739714	7999.887481	13.825370	-0.049304	4.815630
236.868765	7999.797775	13.830375	-0.049328	4.815603
236.956695	7999.750099	13.835379	-0.049344	4.815589
236.596787	7999.853158	13.840384	-0.049277	4.815621
236.638078	7999.791921	13.845389	-0.049285	4.815603
236.854571	7999.771940	13.850394	-0.049325	4.815596
236.707516	7999.795183	13.855399	-0.049298	4.815603
236.638961	7999.807955	13.860403	-0.049285	4.815607
236.700773	7999.767329	13.865408	-0.049296	4.815595
236.959503	7999.880387	13.870413	-0.049345	4.815627
236.600881	7999.773192	13.875418	-0.049278	4.815597
236.840727	7999.780273	13.880423	-0.049323	4.815598
236.794103	7999.822218	13.885427	-0.049314	4.815611
236.572558	7999.787687	13.890432	-0.049273	4.815602
236.617065	7999.758522	13.895437	-0.049281	4.815593
236.791142	7999.836055	13.900442	-0.049314	4.815615
236.732130	7999.757185	13.905447	-0.049303	4.815592
236.579154	7999.847578	13.910451	-0.049274	4.815619
236.831263	7999.771602	13.915456	-0.049321	4.815596
236.828919	7999.804656	13.920461	-0.049321	4.815606
236.788866	7999.750643	13.925466	-0.049313	4.815590
236.645228	7999.860399	13.930471	-0.049287	4.815623
236.874359	7999.785119	13.935475	-0.049329	4.815600
236.630719	7999.731018	13.940480	-0.049284	4.815585
236.540469	7999.819222	13.945485	-0.049267	4.815611
236.581373	7999.861514	13.950490	-0.049275	4.815623
236.685675	7999.784216	13.955495	-0.049294	4.815600
236.663321	7999.793465	13.960499	-0.049290	4.815603
236.713441	7999.769728	13.965504	-0.049300	4.815596
236.779680	7999.788947	13.970509	-0.049312	4.815601
236.621162	7999.778916	13.975514	-0.049282	4.815599
236.660168	7999.839323	13.980519	-0.049290	4.815616
236.661895	7999.861769	13.985523	-0.049290	4.815623
236.603740	7999.807463	13.990528	-0.049279	4.815607
236.577553	7999.848671	13.995533	-0.049274	4.815620
236.820479	7999.836589	14.000538	-0.049320	4.815615
236.767754	7999.854953	14.005543	-0.049310	4.815621
236.921124	7999.793391	14.010547	-0.049339	4.815602
236.744601	7999.874865	14.015552	-0.049306	4.815626
236.927431	7999.816982	14.020557	-0.049340	4.815609
236.948649	7999.794913	14.025562	-0.049344	4.815602
236.893480	7999.770541	14.030567	-0.049334	4.815595
236.854161	7999.798728	14.035571	-0.049326	4.815604
236.811976	7999.852486	14.040576	-0.049318	4.815620
236.989102	7999.777433	14.045581	-0.049351	4.815597
236.815977	7999.786379	14.050586	-0.049319	4.815600
236.682974	7999.806648	14.055591	-0.049295	4.815607
236.508977	7999.802771	14.060595	-0.049262	4.815606
236.644652	7999.759070	14.065600	-0.049287	4.815593
236.832190	7999.778114	14.070605	-0.049322	4.815598
236.697661	7999.852794	14.075610	-0.049297	4.815620
236.546301	7999.780972	14.080615	-0.049269	4.815600
236.694555	7999.773764	14.085619	-0.049297	4.815597
236.629952	7999.765251	14.090624	-0.049285	4.815595
236.829717	7999.816515	14.095629	-0.049322	4.815609
236.957485	7999.786561	14.100634	-0.049346	4.815600
236.994316	7999.794631	14.105639	-0.049353	4.815602
236.832886	7999.867809	14.110643	-0.049323	4.815624
236.658564	7999.889545	14.115648	-0.049290	4.815631
237.031627	7999.821928	14.120653	-0.049360	4.815610
236.853959	7999.804116	14.125658	-0.049327	4.815605
236.729683	7999.793571	14.130663	-0.049304	4.815603
236.755145	7999.823872	14.135667	-0.049309	4.815611
236.628568	7999.774865	14.140672	-0.049285	4.815598
236.883368	7999.798199	14.145677	-0.049332	4.815603
236.760324	7999.832504	14.150682	-0.049310	4.815614
236.935231	7999.800110	14.155687	-0.049342	4.815604
236.830821	7999.884884	14.160691	-0.049323	4.815629
236.792691	7999.767926	14.165696	-0.049316	4.815595
236.877433	7999.830139	14.170701	-0.049332	4.815613
236.786506	7999.812662	14.175706	-0.049315	4.815608
236.819288	7999.817464	14.180711	-0.049321	4.815609
236.918909	7999.842560	14.185715	-0.049339	4.815616
236.885585	7999.797194	14.190720	-0.049333	4.815603
236.678681	7999.831212	14.195725	-0.049295	4.815614
236.534160	7999.908933	14.200730	-0.049268	4.815637
236.719583	7999.806261	14.205735	-0.049302	4.815606
236.778464	7999.794407	14.210739	-0.049313	4.815603
236.830141	7999.774965	14.215744	-0.049323	4.815597
236.799239	7999.793682	14.220749	-0.049317	4.815602
236.810405	7999.776787	14.225754	-0.049319	4.815597
236.634701	7999.788894	14.230759	-0.049287	4.815602
236.889962	7999.793022	14.235763	-0.049334	4.815602
236.746742	7999.865427	14.240768	-0.049308	4.815624
236.846584	7999.790192	14.245773	-0.049326	4.815601
236.849576	7999.773166	14.250778	-0.049327	4.815596
236.913653	7999.804091	14.255783	-0.049339	4.815605
236.926761	7999.838462	14.260787	-0.049341	4.815615
236.770821	7999.780441	14.265792	-0.049312	4.815599
236.842549	7999.638574	14.270797	-0.049326	4.815557

236.667396	7996.372055	14.275802	-0.049291	4.814602
236.649196	7990.725341	14.280807	-0.049284	4.812950
236.622810	7983.967139	14.285811	-0.049275	4.810972
236.563699	7976.670814	14.290816	-0.049259	4.808835
236.681884	7969.078989	14.295821	-0.049276	4.806611
236.569823	7961.177257	14.300826	-0.049250	4.804295
236.674362	7953.390142	14.305831	-0.049264	4.802011
236.747451	7945.404104	14.310835	-0.049273	4.799668
236.605008	7937.447498	14.315840	-0.049241	4.797333
236.574891	7929.427371	14.320845	-0.049230	4.794978
236.424508	7921.419049	14.325850	-0.049197	4.792625
236.493091	7913.358349	14.330855	-0.049205	4.790255
236.492349	7905.425882	14.335859	-0.049199	4.787922
236.424683	7897.362727	14.340864	-0.049182	4.785550
236.552935	7889.462093	14.345869	-0.049200	4.783223
236.445791	7881.390468	14.350874	-0.049175	4.780846
236.398606	7873.426428	14.355879	-0.049161	4.778499
236.440558	7865.436778	14.360883	-0.049164	4.776143
236.282431	7857.410428	14.365888	-0.049129	4.773776
236.291378	7849.374357	14.370893	-0.049126	4.771405
236.205059	7841.341113	14.375898	-0.049104	4.769033
236.243743	7833.416959	14.380903	-0.049107	4.766692
236.108330	7825.360505	14.385907	-0.049076	4.764311
236.191282	7817.431024	14.390912	-0.049086	4.761965
236.128689	7809.385594	14.395917	-0.049070	4.759585
235.940248	7801.427142	14.400922	-0.049029	4.757230
235.931304	7793.383030	14.405927	-0.049022	4.754848
235.954063	7785.338044	14.410931	-0.049021	4.752464
235.706843	7777.264706	14.415936	-0.048970	4.750071
235.738541	7769.293194	14.420941	-0.048971	4.747706
235.719779	7761.314609	14.425946	-0.048962	4.745339
235.902836	7753.347336	14.430951	-0.048991	4.742972
235.866263	7745.397541	14.435955	-0.048979	4.740611
235.944073	7737.342584	14.440960	-0.048989	4.738217
235.859834	7729.328956	14.445965	-0.048968	4.735834
235.588355	7721.330226	14.450970	-0.048912	4.733455
235.793787	7713.302283	14.455975	-0.048945	4.731065
235.894502	7705.327687	14.460979	-0.048959	4.728690
235.554814	7697.340602	14.465984	-0.048890	4.726311
235.654970	7689.286100	14.470989	-0.048904	4.723909
235.461385	7681.330500	14.475994	-0.048862	4.721537
235.519309	7673.336083	14.480999	-0.048868	4.719151
235.552392	7665.358041	14.486003	-0.048869	4.716769
235.507110	7657.276832	14.491008	-0.048855	4.714355
235.517619	7649.310915	14.496013	-0.048852	4.711974
235.410003	7641.322049	14.501018	-0.048827	4.709585
235.482545	7633.312518	14.506023	-0.048835	4.707189
235.837269	7625.318436	14.511027	-0.048896	4.704795
235.476082	7617.328559	14.516032	-0.048824	4.702403
235.269520	7609.323101	14.521037	-0.048780	4.700005
235.431086	7601.335669	14.526042	-0.048805	4.697610
235.375071	7593.296770	14.531047	-0.048789	4.695199
235.353035	7585.325681	14.536051	-0.048780	4.692807
235.243152	7577.265635	14.541056	-0.048754	4.690387
235.365756	7569.317112	14.546061	-0.048772	4.687999
235.045729	7561.259028	14.551066	-0.048707	4.685578
235.179575	7553.257492	14.556071	-0.048727	4.683171
235.199017	7545.321679	14.561075	-0.048725	4.680783
235.184302	7537.279840	14.566080	-0.048718	4.678363
235.009345	7529.301518	14.571085	-0.048680	4.675960
234.913018	7521.223120	14.576090	-0.048657	4.673526
234.926198	7513.138071	14.581095	-0.048654	4.671088
234.839844	7505.212030	14.586099	-0.048633	4.668697
234.900013	7497.204843	14.591104	-0.048639	4.666280
235.061812	7489.233184	14.596109	-0.048664	4.663873
234.821205	7481.253802	14.601114	-0.048614	4.661463
234.581019	7473.251805	14.606119	-0.048564	4.659044
234.727498	7465.300719	14.611123	-0.048586	4.656639
234.597031	7457.231140	14.616128	-0.048556	4.654197
234.582911	7449.213607	14.621133	-0.048549	4.651770
234.669642	7441.214965	14.626138	-0.048560	4.649347
234.698097	7433.249160	14.631143	-0.048560	4.646933
234.515021	7425.225257	14.636147	-0.048520	4.644500
234.541479	7417.223558	14.641152	-0.048520	4.642072
234.812115	7409.189485	14.646157	-0.048565	4.639633
234.674575	7401.284233	14.651162	-0.048535	4.637232
234.452394	7393.205313	14.656167	-0.048488	4.634778
234.465106	7385.209093	14.661171	-0.048485	4.632346
234.301435	7377.134797	14.666176	-0.048449	4.629890
234.429465	7369.223049	14.671181	-0.048468	4.627482
234.336379	7361.154300	14.676186	-0.048446	4.625025
234.245515	7353.222035	14.681191	-0.048424	4.622609
234.207104	7345.176232	14.686195	-0.048411	4.620156
234.324850	7337.185912	14.691200	-0.048428	4.617719
234.241708	7329.202854	14.696205	-0.048407	4.615283
234.127877	7321.178057	14.701210	-0.048381	4.612833
234.156481	7313.169774	14.706215	-0.048381	4.610386
234.147868	7305.210693	14.711219	-0.048374	4.607954
233.970777	7297.138597	14.716224	-0.048336	4.605485
233.862738	7289.195284	14.721229	-0.048311	4.603055
233.785030	7281.186851	14.726234	-0.048291	4.600603
233.888158	7273.203867	14.731239	-0.048305	4.598158
233.789245	7265.190796	14.736243	-0.048282	4.595702
233.786156	7257.120809	14.741248	-0.048276	4.593227
233.867221	7249.108931	14.746253	-0.048286	4.590770
233.678268	7241.094796	14.751258	-0.048245	4.588309
233.881233	7233.098332	14.756263	-0.048278	4.585854
233.766346	7225.150578	14.761267	-0.048251	4.583411
233.925546	7217.150518	14.766272	-0.048276	4.580952
233.829260	7209.187927	14.771277	-0.048253	4.578502
233.818135	7201.115797	14.776282	-0.048246	4.576018
233.751250	7193.136428	14.781287	-0.048228	4.573560
233.722005	7185.128833	14.786291	-0.048217	4.571093
233.520605	7177.108001	14.791296	-0.048175	4.568620
233.782726	7169.119119	14.796301	-0.048218	4.566156
233.703484	7161.114627	14.801306	-0.048198	4.563686
233.503960	7153.171632	14.806311	-0.048156	4.561233
233.569859	7145.211593	14.811315	-0.048163	4.558774
233.571500	7137.167281	14.816320	-0.048158	4.556287
233.607136	7129.148394	14.821325	-0.048160	4.553807
233.360520	7121.081855	14.826330	-0.048108	4.551310
233.243884	7113.125000	14.831335	-0.048082	4.548846
233.245278	7105.106378	14.836339	-0.048077	4.546362
233.184055	7097.088473	14.841344	-0.048060	4.543877
233.354209	7089.124954	14.846349	-0.048087	4.541407
233.221628	7081.135358	14.851354	-0.048057	4.538928
233.067674	7073.144291	14.856359	-0.048023	4.536446
233.127071	7065.133179	14.861363	-0.048029	4.533958
233.059117	7057.107213	14.866368	-0.048011	4.531463
232.959651	7049.110005	14.871373	-0.047987	4.528976
232.946620	7041.125656	14.876378	-0.047980	4.526491
233.054156	7033.088693	14.881383	-0.047994	4.523989
232.976078	7025.185769	14.886387	-0.047975	4.521527
232.986204	7017.097253	14.891392	-0.047971	4.519006
233.053503	7009.178946	14.896397	-0.047979	4.516537
233.036856	7001.112580	14.901402	-0.047971	4.514020
232.821545	6992.964382	14.906407	-0.047925	4.511476
232.978924	6985.050548	14.911411	-0.047949	4.509004
232.722253	6977.042697	14.916416	-0.047896	4.506500
232.687088	6969.042451	14.921421	-0.047885	4.503998
232.712852	6961.111959	14.926426	-0.047884	4.501517
232.687571	6953.064680	14.931431	-0.047874	4.498998
232.862210	6945.114712	14.936435	-0.047902	4.496508
232.637952	6937.030494	14.941440	-0.047855	4.493973
232.396814	6929.075505	14.946445	-0.047805	4.491478
232.449541	6921.076363	14.951450	-0.047809	4.488968
232.222241	6913.052707	14.956455	-0.047762	4.486448
232.313531	6905.061166	14.961459	-0.047774	4.483938
232.487952	6897.076178	14.966464	-0.047801	4.481429
232.438360	6889.081130	14.971469	-0.047787	4.478915
232.199943	6881.097617	14.976474	-0.047737	4.476402
232.265042	6873.043944	14.981479	-0.047744	4.473866
232.537393	6865.043999	14.986483	-0.047789	4.471347
232.228996	6857.031369	14.991488	-0.047727	4.468821
232.338933	6849.034349	14.996493	-0.047742	4.466299
232.322194	6841.016608	15.001498	-0.047734	4.463769
232.087937	6833.049548	15.006503	-0.047685	4.461253
232.055665	6825.083619	15.011507	-0.047674	4.458736
232.139988	6817.046700	15.016512	-0.047684	4.456196
232.157149	6809.014201	15.021517	-0.047682	4.453656
232.000668	6801.004297	15.026522	-0.047648	4.451120
231.893698	6793.010210	15.031527	-0.047623	4.448589
232.064635	6785.010151	15.036531	-0.047650	4.446055
231.874774	6777.023375	15.041536	-0.047609	4.443522
231.894372	6769.043303	15.046541	-0.047608	4.440991
232.009284	6761.046795	15.051546	-0.047624	4.438454
231.798744	6753.010235	15.056551	-0.047579	4.435901
231.926491	6745.044318	15.061555	-0.047598	4.433371
231.821040	6736.960596	15.066560	-0.047573	4.430800
231.908779	6728.980842	15.071565	-0.047584	4.428262
231.877326	6720.960326	15.076570	-0.047573	4.425710
231.769284	6712.980888	15.081575	-0.047548	4.423168
231.782388	6704.984660	15.086579	-0.047545	4.420620
231.542632	6697.001823	15.091584	-0.047495	4.418074
231.575583	6689.039017	15.096589	-0.047496	4.415534
231.665943	6680.984059	15.101594	-0.047508	4.412963
231.554996	6672.958476	15.106599	-0.047482	4.410399
231.564183	6664.996226	15.111603	-0.047479	4.407855
231.810256	6656.943933	15.116608	-0.047519	4.405281
231.717650	6649.045254	15.121613	-0.047497	4.402754
231.550134	6641.066609	15.126618	-0.047461	4.400199
231.457546	6633.050482	15.131623	-0.047438	4.397631
231.506362	6625.008424	15.136627	-0.047442	4.395053
231.215169	6616.998363	15.141632	-0.047383	4.392483
231.258720	6608.956136	15.146637	-0.047386	4.389903
231.264034	6600.999988	15.151642	-0.047381	4.387348
231.294324	6592.944079	15.156647	-0.047382	4.384760
231.290692	6585.044033	15.161651	-0.047376	4.382221
231.242100	6577.002868	15.166656	-0.047362	4.379634
231.194003	6569.037268	15.171661	-0.047348	4.377071
231.170480	6560.981886	15.176666	-0.047338	4.374477
231.097820	6552.968068	15.181671	-0.047319	4.371894
231.137559	6544.982052	15.186675	-0.047322	4.369320
230.936925	6537.004389	15.191680	-0.047279	4.366745
230.924677	6528.991117	15.196685	-0.047272	4.364158
230.918665	6521.037569	15.201690	-0.047265	4.361590
230.806211	6513.030945	15.206695	-0.047239	4.359001
231.023393	6505.037015	15.211699	-0.047274	4.356418
230.990835	6496.950539	15.216704	-0.047263	4.353801
230.907334	6488.868056	15.221709	-0.047242	4.351184
230.886479	6480.896135	15.226714	-0.047233	4.348602
230.803832	6472.921584	15.231719	-0.047213	4.346016
230.895389	6464.951052	15.236723	-0.047225	4.343432
230.749801	6456.987369	15.241728	-0.047192	4.340847
230.349507	6449.003178	15.246733	-0.047113	4.338251
230.390414	6440.982725	15.251738	-0.047115	4.335646
230.500707	6432.951176	15.256743	-0.047131	4.333035
230.560109	6424.961046	15.261747	-0.047136	4.330437
230.470266	6416.946398	15.266752	-0.047114	4.327827
230.591260	6408.941504	15.271757	-0.047132	4.325221
230.444687	6400.997220	15.276762	-0.047099	4.322631
230.057608	6392.934972	15.281767	-0.047022	4.319999
230.225194	6385.031532	15.286771	-0.047048	4.317422
230.251808	6376.955332	15.291776	-0.047048	4.314785
230.215334	6368.939991	15.296781	-0.047036	4.312166
230.102317	6360.937068	15.301786	-0.047010	4.309549
230.185284	6352.913426	15.306791	-0.047020	4.306926
230.063741	6344.921464	15.311795	-0.046992	4.304309
230.033240	6336.936039	15.316800	-0.046981	4.301694
229.986285	6328.943507	15.321805	-0.046967	4.299075
229.946838	6321.021370	15.326810	-0.046955	4.296477
229.927734	6312.916139	15.331815	-0.046946	4.293817
230.051522	6304.935988	15.336819	-0.046964	4.291199
229.994466	6296.925289	15.341824	-0.046948	4.288567
229.964579	6288.921700	15.346829	-0.046937	4.285936
229.850371	6280.982128	15.351834	-0.046911	4.283324
229.994704	6272.910901	15.356839	-0.046933	4.280669
229.780146	6264.974264	15.361843	-0.046888	4.278053
229.616107	6256.922860	15.366848	-0.046852	4.275399
229.804039	6248.925052	15.371853	-0.046882	4.272764
229.728285	6240.874740	15.376858	-0.046862	4.270107
229.405729	6232.903163	15.381863	-0.046797	4.267473
229.577198	6224.900740	15.386867	-0.046824	4.264831
229.619138	6216.929371	15.391872	-0.046827	4.262197
229.582961	6208.949000	15.396877	-0.046815	4.259557
229.384243	6200.955411	15.401882	-0.046772	4.256910
229.503105	6192.900640	15.406887	-0.046789	4.254244
229.434013	6184.922968	15.411891	-0.046771	4.251600
229.363971	6176.909844	15.416896	-0.046753	4.248942
229.277529	6168.934216	15.421901	-0.046732	4.246296
229.341915	6160.927366	15.426906	-0.046739	4.243638
229.303755	6152.921861	15.431911	-0.046726	4.240978
229.410865	6144.976385	15.436915	-0.046741	4.238338
229.404725	6136.947135	15.441920	-0.046735	4.235668
229.274728	6128.937818	15.446925	-0.046705	4.233001
229.212541	6120.903506	15.451930	-0.046689	4.230325
229.191262	6112.933047	15.456935	-0.046680	4.227669
229.106545	6104.958265	15.461939	-0.046659	4.225009
228.977715	6096.944964	15.466944	-0.046629	4.222334
229.217984	6088.926639	15.471949	-0.046669	4.219659
229.093641	6080.956104	15.476954	-0.046641	4.216995
228.998841	6072.950553	15.481959	-0.046618	4.214318
228.999690	6064.945336	15.486963	-0.046613	4.211640
228.817408	6056.941542	15.491968	-0.046574	4.208959
228.697601	6048.947513	15.496973	-0.046546	4.206281
228.922250	6040.968364	15.501978	-0.046583	4.203609
228.937742	6032.963550	15.506983	-0.046581	4.200925
228.895133	6024.994521	15.511987	-0.046567	4.198250
228.656668	6016.949457	15.516992	-0.046518	4.195546
228.906324	6008.861553	15.521997	-0.046559	4.192831
228.905794	6000.831405	15.527002	-0.046554	4.190131
228.787098	5992.864072	15.532007	-0.046527	4.187450
228.934138	5984.895095	15.537011	-0.046549	4.184768
228.739105	5976.941457	15.542016	-0.046507	4.182087
228.907886	5968.891204	15.547021	-0.046533	4.179375
228.799779	5960.952450	15.552026	-0.046508	4.176696
228.652417	5952.919360	15.557031	-0.046476	4.173983
228.802676	5944.906527	15.562035	-0.046498	4.171278
228.651948	5936.921921	15.567040	-0.046465	4.168578
228.404357	5928.924619	15.572045	-0.046414	4.165871
228.450855	5920.916132	15.577050	-0.046417	4.163161
228.407142	5912.910414	15.582055	-0.046404	4.160450
228.534702	5904.923371	15.587059	-0.046423	4.157745
228.487371	5896.888641	15.592064	-0.046409	4.155020
228.379674	5888.892592	15.597069	-0.046383	4.152306
228.279142	5880.900651	15.602074	-0.046359	4.149591
228.420794	5872.846649	15.607079	-0.046381	4.146857
228.481915	5864.911850	15.612083	-0.046387	4.144160
228.267425	5856.933314	15.617088	-0.046342	4.141443
228.182751	5848.931615	15.622093	-0.046321	4.138718
228.205705	5840.950587	15.627098	-0.046320	4.136000
228.243479	5832.867140	15.632103	-0.046322	4.133245
228.037407	5824.901358	15.637107	-0.046278	4.130525
228.176315	5816.898097	15.642112	-0.046299	4.127796
228.111715	5808.909406	15.647117	-0.046282	4.125066
227.908465	5800.953086	15.652122	-0.046239	4.122345
227.739611	5792.907748	15.657127	-0.046202	4.119591
228.078741	5784.967416	15.662131	-0.046260	4.116878
227.943022	5776.908782	15.667136	-0.046230	4.114116
227.852658	5768.841158	15.672141	-0.046207	4.111351
227.801553	5760.866709	15.677146	-0.046193	4.108616
227.806008	5752.886381	15.682151	-0.046188	4.105877
227.744166	5744.925744	15.687155	-0.046172	4.103143
227.826782	5736.904924	15.692160	-0.046182	4.100388
227.727183	5728.938287	15.697165	-0.046158	4.097648
227.488151	5720.980646	15.702170	-0.046109	4.094906
227.391437	5712.953068	15.707175	-0.046085	4.092141
227.606797	5704.903283	15.712179	-0.046120	4.089371
227.302321	5696.938270	15.717184	-0.046058	4.086621
227.239964	5688.907615	15.722189	-0.046042	4.083849
227.280675	5680.950650	15.727194	-0.046044	4.081103
227.186347	5672.937599	15.732199	-0.046021	4.078333
227.274176	5664.976859	15.737203	-0.046033	4.075583
227.194922	5656.946137	15.742208	-0.046013	4.072803
227.278306	5648.908004	15.747213	-0.046023	4.070022
227.352810	5640.936967	15.752218	-0.046032	4.067262
227.106744	5632.907962	15.757223	-0.045981	4.064475
227.181347	5624.990995	15.762227	-0.045989	4.061730
227.111326	5616.949591	15.767232	-0.045971	4.058938
227.214214	5608.945186	15.772237	-0.045985	4.056159
227.330993	5600.961812	15.777242	-0.046002	4.053385
227.237331	5592.915547	15.782247	-0.045979	4.050585
227.166170	5584.952846	15.787251	-0.045961	4.047813
227.075568	5576.945389	15.792256	-0.045939	4.045022
227.099382	5568.995929	15.797261	-0.045938	4.042252
227.105844	5560.973919	15.802266	-0.045934	4.039454
226.902430	5552.974549	15.807271	-0.045891	4.036659
227.109408	5544.931802	15.812275	-0.045924	4.033853
226.806516	5536.843490	15.817280	-0.045863	4.031021
226.770311	5528.863576	15.822285	-0.045851	4.028229
226.857175	5520.901659	15.827290	-0.045862	4.025444
226.724605	5512.923691	15.832295	-0.045832	4.022647
226.714794	5504.947689	15.837299	-0.045825	4.019852
226.679937	5496.941878	15.842304	-0.045813	4.017043
226.723649	5488.906175	15.847309	-0.045816	4.014223
226.654134	5480.906945	15.852314	-0.045798	4.011413
226.659045	5472.878933	15.857319	-0.045794	4.008591
226.800070	5464.929402	15.862323	-0.045815	4.005797
226.593945	5456.963868	15.867328	-0.045771	4.002990
226.284806	5448.953770	15.872333	-0.045708	4.000164
226.461849	5440.983016	15.877338	-0.045736	3.997357
226.272985	5432.943466	15.882343	-0.045696	3.994518
226.429025	5424.910609	15.887347	-0.045720	3.991685
226.220063	5416.917088	15.892352	-0.045676	3.988858
226.298635	5408.899180	15.897357	-0.045685	3.986025
226.268128	5400.922921	15.902362	-0.045674	3.983203
226.003402	5392.948330	15.907367	-0.045620	3.980376
226.226570	5385.003242	15.912371	-0.045656	3.977565
226.171408	5376.952709	15.917376	-0.045641	3.974711
226.161776	5368.963012	15.922381	-0.045634	3.971876
226.264265	5360.960499	15.927386	-0.045648	3.969037
226.127957	5352.965441	15.932391	-0.045617	3.966194
226.013396	5344.976890	15.937395	-0.045591	3.963352
225.886411	5336.990337	15.942400	-0.045562	3.960509
226.000428	5329.010178	15.947405	-0.045578	3.957670
225.889964	5320.988809	15.952410	-0.045552	3.954810
225.670348	5312.947989	15.957415	-0.045506	3.951939
225.786247	5304.961390	15.962419	-0.045522	3.949092
225.797475	5296.955070	15.967424	-0.045519	3.946233
225.721866	5288.975438	15.972429	-0.045500	3.943381
225.832640	5280.986265	15.977434	-0.045516	3.940526
225.794279	5273.023349	15.982439	-0.045503	3.937676
225.676966	5265.020493	15.987443	-0.045476	3.934808
225.449169	5256.989011	15.992448	-0.045429	3.931926
225.607249	5248.994556	15.997453	-0.045453	3.929062
225.579783	5241.032646	16.002458	-0.045443	3.926204
225.419994	5232.994634	16.007463	-0.045408	3.923314
225.418396	5225.030103	16.012467	-0.045402	3.920451
225.369358	5217.011348	16.017472	-0.045388	3.917566
225.354767	5209.023639	16.022477	-0.045380	3.914691
225.500814	5200.986746	16.027482	-0.045402	3.911799
225.489289	5192.983806	16.032487	-0.045395	3.908914
225.225160	5185.025855	16.037491	-0.045340	3.906038
225.268197	5177.003413	16.042496	-0.045343	3.903143
225.161425	5169.005116	16.047501	-0.045318	3.900251
225.336589	5161.024758	16.052506	-0.045346	3.897369
225.293508	5152.988419	16.057511	-0.045332	3.894461
225.460314	5145.015960	16.062515	-0.045358	3.891577
225.377980	5137.004005	16.067520	-0.045338	3.888673
225.282484	5128.995337	16.072525	-0.045315	3.885767
225.254417	5121.040700	16.077530	-0.045304	3.882879
225.300490	5113.003805	16.082535	-0.045308	3.879962
225.208528	5105.078268	16.087539	-0.045285	3.877079
225.106835	5097.021050	16.092544	-0.045261	3.874147
225.220104	5088.775699	16.097549	-0.045277	3.871148
225.181155	5080.861115	16.102554	-0.045265	3.868264
225.047644	5072.889990	16.107559	-0.045235	3.865356
224.853545	5064.991554	16.112563	-0.045193	3.862470
224.846968	5056.989635	16.117568	-0.045187	3.859549
224.713873	5049.019560	16.122573	-0.045157	3.856634
224.768559	5041.014445	16.127578	-0.045162	3.853708
224.756575	5032.985837	16.132583	-0.045155	3.850770
224.781777	5025.036288	16.137587	-0.045154	3.847859
224.726935	5016.999303	16.142592	-0.045139	3.844913
224.570051	5009.059331	16.147597	-0.045104	3.841997
224.645095	5001.053717	16.152602	-0.045113	3.839061
224.493552	4993.084863	16.157607	-0.045080	3.836130
224.601840	4985.057334	16.162611	-0.045095	3.833181
224.413041	4977.036744	16.167616	-0.045054	3.830227
224.421021	4969.052720	16.172621	-0.045051	3.827287
224.235209	4961.076628	16.177626	-0.045011	3.824345
224.215051	4953.130237	16.182631	-0.045002	3.821414
224.369185	4945.102941	16.187635	-0.045026	3.818455
224.275068	4937.089425	16.192640	-0.045003	3.815493
224.479710	4929.063128	16.197645	-0.045036	3.812531
224.368443	4921.076592	16.202650	-0.045010	3.809575
224.202710	4913.075049	16.207655	-0.044974	3.806609
224.440688	4905.120147	16.212659	-0.045013	3.803667
224.168911	4897.139031	16.217664	-0.044957	3.800702
223.999296	4889.146456	16.222669	-0.044920	3.797733
224.004489	4881.112873	16.227674	-0.044916	3.794750
223.898492	4873.057793	16.232679	-0.044891	3.791754
224.038749	4865.050660	16.237683	-0.044912	3.788779
223.752826	4857.084492	16.242688	-0.044854	3.785808
223.869612	4849.106392	16.247693	-0.044870	3.782838
223.858639	4841.148068	16.252698	-0.044863	3.779871
223.836468	4833.118055	16.257703	-0.044854	3.776875
223.764586	4825.114160	16.262707	-0.044835	3.773884
223.906069	4817.071100	16.267712	-0.044856	3.770882
223.781900	4809.088150	16.272717	-0.044828	3.767894
223.675918	4801.111313	16.277722	-0.044803	3.764905
223.471847	4793.120224	16.282727	-0.044760	3.761907
223.553103	4785.158818	16.287731	-0.044770	3.758925
223.527776	4777.154556	16.292736	-0.044760	3.755921
223.386911	4769.128970	16.297741	-0.044729	3.752904
223.379018	4761.121568	16.302746	-0.044722	3.749895
223.405353	4753.087767	16.307751	-0.044722	3.746874
223.399747	4745.130425	16.312755	-0.044716	3.743879
223.431861	4737.137327	16.317760	-0.044716	3.740869
223.296627	4729.149600	16.322765	-0.044686	3.737854
223.227184	4721.182425	16.327770	-0.044668	3.734846
223.099285	4713.172515	16.332775	-0.044639	3.731818
223.222943	4705.154839	16.337779	-0.044657	3.728791
223.101729	4697.158403	16.342784	-0.044629	3.725764
223.098384	4689.191497	16.347789	-0.044623	3.722748
223.187923	4681.191326	16.352794	-0.044635	3.719719
223.001104	4673.233515	16.357799	-0.044595	3.716698
223.110511	4665.200657	16.362803	-0.044610	3.713652
223.095828	4657.074728	16.367808	-0.044602	3.710566
223.091444	4649.112544	16.372813	-0.044596	3.707539
222.978662	4641.154899	16.377818	-0.044570	3.704509
222.949353	4633.210667	16.382823	-0.044559	3.701484
223.063120	4625.219357	16.387827	-0.044575	3.698442
222.865815	4617.226357	16.392832	-0.044533	3.695389
222.924495	4609.240371	16.397837	-0.044539	3.692343
222.986726	4601.228043	16.402842	-0.044546	3.689284
222.923931	4593.217558	16.407847	-0.044529	3.686220
222.848684	4585.254560	16.412851	-0.044510	3.683171
222.741516	4577.257128	16.417856	-0.044484	3.680106
222.612922	4569.280872	16.422861	-0.044455	3.677046
222.724434	4561.283028	16.427866	-0.044471	3.673981
222.664292	4553.210676	16.432871	-0.044454	3.670880
222.581763	4545.254712	16.437875	-0.044434	3.667821
222.445338	4537.248204	16.442880	-0.044403	3.664739
222.606649	4529.273727	16.447885	-0.044428	3.661674
222.529152	4521.287255	16.452890	-0.044409	3.658596
222.437611	4513.278551	16.457895	-0.044386	3.655506
222.312990	4505.290250	16.462899	-0.044358	3.652421
222.326873	4497.236233	16.467904	-0.044355	3.649311
222.346986	4489.266165	16.472909	-0.044354	3.646231
222.208093	4481.298462	16.477914	-0.044323	3.643145
222.207948	4473.285264	16.482919	-0.044318	3.640043
222.290273	4465.355335	16.487923	-0.044328	3.636972
222.143824	4457.300716	16.492928	-0.044295	3.633845
222.154700	4449.252589	16.497933	-0.044292	3.630721
221.994075	4441.273985	16.502938	-0.044257	3.627617
222.080626	4433.214331	16.507943	-0.044268	3.624486
222.077138	4425.317897	16.512947	-0.044262	3.621413
221.935201	4417.344185	16.517952	-0.044231	3.618303
221.975589	4409.337294	16.522957	-0.044233	3.615183
222.001322	4401.340740	16.527962	-0.044233	3.612064
221.920859	4393.303494	16.532967	-0.044212	3.608923
222.023803	4385.343256	16.537971	-0.044226	3.605815
222.016632	4377.368990	16.542976	-0.044220	3.602696
221.761039	4369.374800	16.547981	-0.044167	3.599559
221.775364	4361.441577	16.552986	-0.044165	3.596450
221.961669	4353.354827	16.557991	-0.044194	3.593284
221.703179	4345.387543	16.562995	-0.044141	3.590149
221.588986	4337.398622	16.568000	-0.044114	3.587007
221.735628	4329.378773	16.573005	-0.044137	3.583858
221.717921	4321.435759	16.578010	-0.044128	3.580731
221.484377	4313.437024	16.583015	-0.044080	3.577573
221.572033	4305.443324	16.588019	-0.044091	3.574424
221.482125	4297.417473	16.593024	-0.044069	3.571255
221.494085	4289.418952	16.598029	-0.044066	3.568096
221.510760	4281.427955	16.603034	-0.044064	3.564937
221.517007	4273.459795	16.608039	-0.044060	3.561785
221.408361	4265.458357	16.613043	-0.044034	3.558613
221.234737	4257.480747	16.618048	-0.043997	3.555445
221.209679	4249.377338	16.623053	-0.043987	3.552230
221.228282	4241.374682	16.628058	-0.043985	3.549052
221.138069	4233.398333	16.633063	-0.043963	3.545879
221.291234	4225.408535	16.638067	-0.043987	3.542706
221.282078	4217.447462	16.643072	-0.043980	3.539536
221.091928	4209.475876	16.648077	-0.043939	3.536353
221.224405	4201.453494	16.653082	-0.043959	3.533157
221.126212	4193.437064	16.658087	-0.043935	3.529954
221.073978	4185.493184	16.663091	-0.043920	3.526778
220.931374	4177.500186	16.668096	-0.043889	3.523576
220.969612	4169.524078	16.673101	-0.043890	3.520384
221.010432	4161.565896	16.678106	-0.043893	3.517197
220.863771	4153.542180	16.683111	-0.043860	3.513974
221.176019	4145.467995	16.688115	-0.043913	3.510743
221.038159	4137.511985	16.693120	-0.043883	3.507542
220.932498	4129.495634	16.698125	-0.043858	3.504314
220.994217	4121.562103	16.703130	-0.043864	3.501123
220.644828	4113.577159	16.708135	-0.043794	3.497895
220.832356	4105.582625	16.713139	-0.043824	3.494676
220.469619	4097.601302	16.718144	-0.043751	3.491443
220.496055	4089.576178	16.723149	-0.043751	3.488202
220.548269	4081.588889	16.728154	-0.043755	3.484973
220.473215	4073.622865	16.733159	-0.043736	3.481746
220.537638	4065.627833	16.738163	-0.043743	3.478509
220.428067	4057.650917	16.743168	-0.043717	3.475271
220.452271	4049.574780	16.748173	-0.043716	3.471993
220.486971	4041.591447	16.753178	-0.043718	3.468751
220.346520	4033.589636	16.758183	-0.043686	3.465492
220.391984	4025.637286	16.763187	-0.043690	3.462256
220.304582	4017.628713	16.768192	-0.043668	3.458990
220.278635	4009.629698	16.773197	-0.043658	3.455727
220.250199	4001.660624	16.778202	-0.043648	3.452473
220.192342	3993.624322	16.783207	-0.043632	3.449188
220.206714	3985.677607	16.788211	-0.043629	3.445938
220.360332	3977.663064	16.793216	-0.043653	3.442662
220.218915	3969.675500	16.798221	-0.043621	3.439384
220.138899	3961.742351	16.803226	-0.043601	3.436128
220.099636	3953.662943	16.808231	-0.043589	3.432809
220.187168	3945.659958	16.813235	-0.043600	3.429523
219.961448	3937.731282	16.818240	-0.043553	3.426254
219.846826	3929.715503	16.823245	-0.043526	3.422950
219.676539	3921.765112	16.828250	-0.043489	3.419668
219.631460	3913.745526	16.833255	-0.043476	3.416358
219.438083	3905.767938	16.838259	-0.043435	3.413057
219.549540	3897.695846	16.843264	-0.043450	3.409724
219.530882	3889.747262	16.848269	-0.043441	3.406435
219.332070	3881.780712	16.853274	-0.043399	3.403128
219.364419	3873.780089	16.858279	-0.043400	3.399813
219.736523	3865.827969	16.863283	-0.043464	3.396526
219.413499	3857.780248	16.868288	-0.043399	3.393172
219.276907	3849.709183	16.873293	-0.043368	3.389812
219.323898	3841.769406	16.878298	-0.043372	3.386509
219.214910	3833.760666	16.883303	-0.043346	3.383169
219.423816	3825.810763	16.888307	-0.043380	3.379861
219.335169	3817.858697	16.893312	-0.043358	3.376538
219.347977	3809.805042	16.898317	-0.043356	3.373174
219.156782	3801.847712	16.903322	-0.043315	3.369839
219.195761	3793.854066	16.908327	-0.043317	3.366494
219.200488	3785.863842	16.913331	-0.043313	3.363145
219.162881	3777.880008	16.918336	-0.043301	3.359795
219.102173	3769.917297	16.923341	-0.043284	3.356449
219.076801	3761.918679	16.928346	-0.043274	3.353086
218.940999	3753.868685	16.933351	-0.043244	3.349694
218.903932	3745.902811	16.938355	-0.043232	3.346337
218.789197	3737.911735	16.943360	-0.043205	3.342964
218.677964	3729.930696	16.948365	-0.043179	3.339592
218.597964	3721.963175	16.953370	-0.043159	3.336223
218.787496	3713.904901	16.958375	-0.043189	3.332822
218.997184	3705.911232	16.963379	-0.043223	3.329446
218.984986	3697.950964	16.968384	-0.043216	3.326072
218.680129	3689.989979	16.973389	-0.043154	3.322684
218.840832	3682.002055	16.978394	-0.043178	3.319298
218.644414	3674.032506	16.983399	-0.043137	3.315903
218.418700	3666.012212	16.988403	-0.043090	3.312482
218.468808	3657.997790	16.993408	-0.043094	3.309070
218.567412	3649.990225	16.998413	-0.043107	3.305660
218.512742	3642.046227	17.003418	-0.043092	3.302267
218.262363	3634.051967	17.008423	-0.043040	3.298842
218.469950	3626.074708	17.013427	-0.043073	3.295438
218.372406	3618.074692	17.018432	-0.043050	3.292009
218.273879	3610.056211	17.023437	-0.043026	3.288569
218.162706	3602.095315	17.028442	-0.043000	3.285149
218.222733	3594.106224	17.033447	-0.043006	3.281720
218.235367	3586.139911	17.038451	-0.043004	3.278295
218.019685	3578.142466	17.043456	-0.042958	3.274845
218.132449	3570.123684	17.048461	-0.042974	3.271395
218.079687	3562.143592	17.053466	-0.042959	3.267951
217.830284	3554.124859	17.058471	-0.042908	3.264479
217.919034	3546.185622	17.063475	-0.042919	3.261051
217.946206	3538.189666	17.068480	-0.042919	3.257592
217.946407	3530.175136	17.073485	-0.042914	3.254121
218.004315	3522.177518	17.078490	-0.042919	3.250655
217.799552	3514.189648	17.083495	-0.042876	3.247180
217.601099	3506.224928	17.088499	-0.042834	3.243711
217.539686	3498.253974	17.093504	-0.042817	3.240241
217.442114	3490.280618	17.098509	-0.042794	3.236765
217.657268	3482.255991	17.103514	-0.042829	3.233276
217.591201	3474.188937	17.108519	-0.042811	3.229753
217.705560	3466.219562	17.113523	-0.042827	3.226276
217.566566	3458.258197	17.118528	-0.042796	3.222788
217.563594	3450.259260	17.123533	-0.042791	3.219286
217.624684	3442.307145	17.128538	-0.042797	3.215803
217.512475	3434.290348	17.133543	-0.042771	3.212281
217.365116	3426.312715	17.138547	-0.042738	3.208770
217.284735	3418.341807	17.143552	-0.042718	3.205262
217.442851	3410.340753	17.148557	-0.042742	3.201746
217.472191	3402.369144	17.153562	-0.042743	3.198234
217.293342	3394.394983	17.158567	-0.042704	3.194708
217.344097	3386.401453	17.163571	-0.042708	3.191180
217.218414	3378.409617	17.168576	-0.042680	3.187641
217.106096	3370.375395	17.173581	-0.042654	3.184080
217.226319	3362.422249	17.178586	-0.042671	3.180560
217.043095	3354.447954	17.183591	-0.042632	3.177015
217.176902	3346.427517	17.188595	-0.042651	3.173458
217.188566	3338.423592	17.193600	-0.042648	3.169899
217.090967	3330.446933	17.198605	-0.042625	3.166344
217.162943	3322.483150	17.203610	-0.042633	3.162798
216.814604	3314.516640	17.208615	-0.042563	3.159229
216.884298	3306.561235	17.213619	-0.042571	3.155679
216.858757	3298.517279	17.218624	-0.042561	3.152081
216.922725	3290.491202	17.223629	-0.042568	3.148490
216.664921	3282.548918	17.228634	-0.042515	3.144919
216.765880	3274.549298	17.233639	-0.042528	3.141334
216.503231	3266.595198	17.238643	-0.042474	3.137750
216.534003	3258.581183	17.243648	-0.042475	3.134147
216.429442	3250.580023	17.248653	-0.042450	3.130540
216.507589	3242.601224	17.253658	-0.042460	3.126947
216.387114	3234.614592	17.258663	-0.042432	3.123337
216.498575	3226.638405	17.263667	-0.042448	3.119738
216.548616	3218.676788	17.268672	-0.042452	3.116139
216.368293	3210.667376	17.273677	-0.042413	3.112504
216.228736	3202.698443	17.278682	-0.042382	3.108885
216.169869	3194.692297	17.283687	-0.042366	3.105248
216.200614	3186.701000	17.288691	-0.042366	3.101618
216.107357	3178.748642	17.293696	-0.042344	3.097995
216.103229	3170.702142	17.298701	-0.042338	3.094330
216.445093	3162.714456	17.303706	-0.042396	3.090702
216.173002	3154.744681	17.308711	-0.042340	3.087051
216.208404	3146.781345	17.313715	-0.042342	3.083412
216.366935	3138.781507	17.318720	-0.042366	3.079758
216.200312	3130.847262	17.323725	-0.042330	3.076115
215.911947	3122.815194	17.328730	-0.042271	3.072417
216.068429	3114.779517	17.333735	-0.042295	3.068733
216.104528	3106.792847	17.338739	-0.042297	3.065062
216.086783	3098.853090	17.343744	-0.042288	3.061405
215.865165	3090.890264	17.348749	-0.042242	3.057724
215.879927	3082.910830	17.353754	-0.042239	3.054042
215.591597	3074.891185	17.358759	-0.042180	3.050322
215.860643	3066.892108	17.363763	-0.042225	3.046634
215.836697	3058.938913	17.368768	-0.042216	3.042949
215.751962	3050.943130	17.373773	-0.042195	3.039237
215.827028	3043.002408	17.378778	-0.042204	3.035553
215.596163	3034.994351	17.383783	-0.042155	3.031819
215.714754	3026.968623	17.388787	-0.042172	3.028089
215.552563	3019.014137	17.393792	-0.042137	3.024374
215.690369	3011.018781	17.398797	-0.042157	3.020649
215.851220	3003.044828	17.403802	-0.042182	3.016932
215.753180	2995.051742	17.408807	-0.042159	3.013188
215.590418	2987.066115	17.413811	-0.042123	3.009439
215.645292	2979.108204	17.418816	-0.042128	3.005710
215.641953	2971.117108	17.423821	-0.042123	3.001958
215.557055	2963.167849	17.428826	-0.042102	2.998216
215.405663	2955.185882	17.433831	-0.042068	2.994452
215.582449	2947.120327	17.438835	-0.042096	2.990659
215.243579	2939.195047	17.443840	-0.042028	2.986902
215.081546	2931.195732	17.448845	-0.041992	2.983114
215.217609	2923.211818	17.453850	-0.042013	2.979344
215.042092	2915.254747	17.458855	-0.041975	2.975565
215.016636	2907.257618	17.463859	-0.041965	2.971771
214.883959	2899.273011	17.468864	-0.041935	2.967972
214.830862	2891.265222	17.473869	-0.041920	2.964161
214.895917	2883.329095	17.478874	-0.041927	2.960386
214.670090	2875.374849	17.483879	-0.041880	2.956582
214.878324	2867.347507	17.488883	-0.041913	2.952761
214.861783	2859.333214	17.493888	-0.041905	2.948929
214.712683	2851.347617	17.498893	-0.041872	2.945099
214.870428	2843.407547	17.503898	-0.041896	2.941302
214.655481	2835.432338	17.508903	-0.041851	2.937464
214.651819	2827.436217	17.513907	-0.041845	2.933622
214.616176	2819.437852	17.518912	-0.041833	2.929772
214.641860	2811.466632	17.523917	-0.041833	2.925933
214.614216	2803.499410	17.528922	-0.041823	2.922088
214.430703	2795.540407	17.533927	-0.041783	2.918234
214.373832	2787.551655	17.538931	-0.041768	2.914367
214.350144	2779.479697	17.543936	-0.041758	2.910457
214.096149	2771.523123	17.548941	-0.041706	2.906584
214.172127	2763.557548	17.553946	-0.041715	2.902720
214.140679	2755.577211	17.558951	-0.041704	2.898838
214.112388	2747.622610	17.563955	-0.041693	2.894963
214.115028	2739.603573	17.568960	-0.041688	2.891054
213.980288	2731.635583	17.573965	-0.041658	2.887156
214.188626	2723.649775	17.578970	-0.041692	2.883263
213.905688	2715.695054	17.583975	-0.041634	2.879354
214.052685	2707.719772	17.588979	-0.041656	2.875452
213.973868	2699.736035	17.593984	-0.041636	2.871529
213.844940	2691.728254	17.598989	-0.041607	2.867585
213.847674	2683.775706	17.603994	-0.041603	2.863671
213.804120	2675.777213	17.608999	-0.041589	2.859726
213.632096	2667.836501	17.614003	-0.041552	2.855797
213.688252	2659.830542	17.619008	-0.041557	2.851843
213.741970	2651.817651	17.624013	-0.041562	2.847880
213.802628	2643.861677	17.629018	-0.041568	2.843940
213.639205	2635.907565	17.634023	-0.041533	2.839983
213.747309	2627.943790	17.639027	-0.041548	2.836031
213.652808	2619.953964	17.644032	-0.041525	2.832049
213.464366	2611.943584	17.649037	-0.041485	2.828045
213.456685	2603.983991	17.654042	-0.041478	2.824072
213.456743	2595.991651	17.659047	-0.041473	2.820077
213.292586	2588.041310	17.664051	-0.041437	2.816088
213.396635	2580.042261	17.669056	-0.041451	2.812084
213.457522	2572.028438	17.674061	-0.041458	2.808065
213.389533	2564.094901	17.679066	-0.041440	2.804073
213.295060	2556.104490	17.684071	-0.041417	2.800045
213.295365	2548.161078	17.689075	-0.041412	2.796040
213.193462	2540.190214	17.694080	-0.041388	2.792010
213.113458	2532.186416	17.699085	-0.041368	2.787959
213.166063	2524.207224	17.704090	-0.041372	2.783922
213.075210	2516.234130	17.709095	-0.041350	2.779873
212.914409	2508.294371	17.714099	-0.041315	2.775832
212.873326	2500.289709	17.719104	-0.041302	2.771759
213.064603	2492.264135	17.724109	-0.041333	2.767682
213.009705	2484.329281	17.729114	-0.041317	2.763632
212.887220	2476.348063	17.734119	-0.041289	2.759548
212.784991	2468.414156	17.739123	-0.041265	2.755483
212.670566	2460.360703	17.744128	-0.041239	2.751350
212.459690	2452.375175	17.749133	-0.041194	2.747240
212.724156	2444.400795	17.754138	-0.041238	2.743158
212.660475	2436.423019	17.759143	-0.041221	2.739049
212.695409	2428.466140	17.764147	-0.041223	2.734950
212.367674	2420.518296	17.769152	-0.041157	2.730827
212.478866	2412.503282	17.774157	-0.041172	2.726691
212.401598	2404.567403	17.779162	-0.041153	2.722577
212.275875	2396.616853	17.784167	-0.041124	2.718447
212.268156	2388.634318	17.789171	-0.041117	2.714301
212.223457	2380.652215	17.794176	-0.041104	2.710146
212.151982	2372.659234	17.799181	-0.041085	2.705978
212.114577	2364.711589	17.804186	-0.041073	2.701829
212.095280	2356.725036	17.809191	-0.041064	2.697655
212.117526	2348.751811	17.814195	-0.041063	2.693483
211.996623	2340.756415	17.819200	-0.041036	2.689285
211.842664	2332.807872	17.824205	-0.041002	2.685102
211.978868	2324.847357	17.829210	-0.041022	2.680925
211.778387	2316.893187	17.834215	-0.040980	2.676724
211.771314	2308.890874	17.839219	-0.040973	2.672503
211.899845	2300.877035	17.844224	-0.040992	2.668277
211.875622	2292.894421	17.849229	-0.040982	2.664052
211.851309	2284.956280	17.854234	-0.040973	2.659844
211.817196	2276.999587	17.859239	-0.040961	2.655618
211.767078	2269.008833	17.864243	-0.040947	2.651366
211.890890	2261.022196	17.869248	-0.040964	2.647122
211.759273	2253.075269	17.874253	-0.040935	2.642874
211.692081	2245.127135	17.879258	-0.040917	2.638624
211.528724	2237.165503	17.884263	-0.040882	2.634353
211.541052	2229.166683	17.889267	-0.040879	2.630067
211.544550	2221.197961	17.894272	-0.040874	2.625789
211.531569	2213.203359	17.899277	-0.040867	2.621490
211.455453	2205.286462	17.904282	-0.040847	2.617221
211.298685	2197.305797	17.909287	-0.040813	2.612905
211.388139	2189.281243	17.914291	-0.040824	2.608574
211.165365	2181.356666	17.919296	-0.040778	2.604270
210.877400	2173.416337	17.924301	-0.040719	2.599946
211.228095	2165.435467	17.929306	-0.040779	2.595635
211.049172	2157.306524	17.934311	-0.040741	2.591201
210.912508	2149.319398	17.939315	-0.040710	2.586840
211.217705	2141.366100	17.944320	-0.040762	2.582519
210.760691	2133.467794	17.949325	-0.040671	2.578170
210.843843	2125.503424	17.954330	-0.040682	2.573813
210.841516	2117.511231	17.959335	-0.040676	2.569429
210.729933	2109.570311	17.964339	-0.040650	2.565057
210.778207	2101.642044	17.969344	-0.040654	2.560696
210.627645	2093.681151	17.974349	-0.040621	2.556296
210.796853	2085.692086	17.979354	-0.040647	2.551895
210.713377	2077.707355	17.984359	-0.040627	2.547471
210.581225	2069.770870	17.989363	-0.040597	2.543062
210.666292	2061.802290	17.994368	-0.040607	2.538644
210.462003	2053.847153	17.999373	-0.040564	2.534204
210.524468	2045.864990	18.004378	-0.040571	2.529761
210.404205	2037.911530	18.009383	-0.040543	2.525313
210.333619	2029.956580	18.014387	-0.040525	2.520860
210.518825	2021.996254	18.019392	-0.040554	2.516414
210.258533	2014.001255	18.024397	-0.040501	2.511909
210.416359	2006.008260	18.029402	-0.040525	2.507427
210.457714	1998.043363	18.034407	-0.040527	2.502944
210.173081	1990.131481	18.039411	-0.040469	2.498460
210.233094	1982.168706	18.044416	-0.040475	2.493964
210.204801	1974.166406	18.049421	-0.040465	2.489431
210.247419	1966.211010	18.054426	-0.040468	2.484921
209.967450	1958.291343	18.059431	-0.040410	2.480400
209.903590	1950.326942	18.064435	-0.040393	2.475861
210.013915	1942.342454	18.069440	-0.040409	2.471315
209.864459	1934.361172	18.074445	-0.040376	2.466743
210.003712	1926.405265	18.079450	-0.040396	2.462199
209.926748	1918.446021	18.084455	-0.040377	2.457628
209.747623	1910.505786	18.089459	-0.040338	2.453052
209.730326	1902.542979	18.094464	-0.040330	2.448466
209.813253	1894.545687	18.099469	-0.040340	2.443860
209.784510	1886.611847	18.104474	-0.040330	2.439273
209.542895	1878.688407	18.109479	-0.040280	2.434668
209.614872	1870.616110	18.114483	-0.040288	2.429991
209.537077	1862.673554	18.119488	-0.040268	2.425369
209.294762	1854.736895	18.124493	-0.040218	2.420729
209.294338	1846.799833	18.129498	-0.040213	2.416098
209.079962	1838.837288	18.134503	-0.040168	2.411427
209.092614	1830.858246	18.139507	-0.040165	2.406755
209.348112	1822.882538	18.144512	-0.040207	2.402095
209.409101	1814.918103	18.149517	-0.040214	2.397417
209.201978	1807.012914	18.154522	-0.040170	2.392744
209.029932	1799.048852	18.159527	-0.040133	2.388029
208.922960	1791.089002	18.164531	-0.040108	2.383313
209.055925	1783.133048	18.169536	-0.040127	2.378609
208.873995	1775.181982	18.174541	-0.040088	2.373874
209.034158	1767.195107	18.179546	-0.040113	2.369134
208.891076	1759.245330	18.184551	-0.040081	2.364384
208.825219	1751.312683	18.189555	-0.040064	2.359640
208.895845	1743.371592	18.194560	-0.040072	2.354892
208.703952	1735.385512	18.199565	-0.040031	2.350087
208.855216	1727.399750	18.204570	-0.040054	2.345300
208.606075	1719.474665	18.209575	-0.040002	2.340507
208.468708	1711.546390	18.214579	-0.039972	2.335711
208.535698	1703.562579	18.219584	-0.039979	2.330889
208.577100	1695.572987	18.224589	-0.039981	2.326051
208.633952	1687.645378	18.229594	-0.039987	2.321242
208.440416	1679.724282	18.234599	-0.039946	2.316406
208.516499	1671.743829	18.239603	-0.039955	2.311546
208.583470	1663.784151	18.244608	-0.039962	2.306688
208.303104	1655.865668	18.249613	-0.039905	2.301815
208.243250	1647.924683	18.254618	-0.039888	2.296937
208.090520	1639.976859	18.259623	-0.039855	2.292037
208.351497	1631.977737	18.264627	-0.039898	2.287129
208.419398	1624.036877	18.269632	-0.039906	2.282231
208.238844	1616.115841	18.274637	-0.039867	2.277313
208.139969	1608.133101	18.279642	-0.039843	2.272353
207.998587	1600.146644	18.284647	-0.039812	2.267376
207.962408	1592.192993	18.289651	-0.039800	2.262418
207.966882	1584.267375	18.294656	-0.039796	2.257470
207.898226	1576.310980	18.299661	-0.039778	2.252485
207.843117	1568.372581	18.304666	-0.039762	2.247502
207.826926	1560.430506	18.309671	-0.039754	2.242509
207.769174	1552.502764	18.314675	-0.039738	2.237510
207.764903	1544.549471	18.319680	-0.039732	2.232488
207.450353	1536.618101	18.324685	-0.039669	2.227442
207.566962	1528.649591	18.329690	-0.039685	2.222399
207.653282	1520.697195	18.334695	-0.039696	2.217351
207.318574	1512.777021	18.339699	-0.039629	2.212276
207.317020	1504.829539	18.344704	-0.039623	2.207200
207.158582	1496.891999	18.349709	-0.039589	2.202106
207.525670	1488.920575	18.354714	-0.039652	2.197025
207.337115	1480.972425	18.359719	-0.039612	2.191897
207.157948	1473.025455	18.364723	-0.039573	2.186759
207.144973	1465.096394	18.369728	-0.039566	2.181635
207.110622	1457.148057	18.374733	-0.039554	2.176485
207.111132	1449.202534	18.379738	-0.039549	2.171328
206.942342	1441.273379	18.384743	-0.039512	2.166153
206.850430	1433.337255	18.389747	-0.039490	2.160968
206.980012	1425.397425	18.394752	-0.039509	2.155790
206.807282	1417.448887	18.399757	-0.039472	2.150564
206.780334	1409.507449	18.404762	-0.039462	2.145345
206.671990	1401.587774	18.409767	-0.039436	2.140119
206.680958	1393.650827	18.414771	-0.039433	2.134880
206.680677	1385.695324	18.419776	-0.039428	2.129615
206.539005	1377.761730	18.424781	-0.039396	2.124338
206.491018	1369.843340	18.429786	-0.039382	2.119067
206.525318	1361.895382	18.434791	-0.039383	2.113771
206.276624	1353.906265	18.439795	-0.039332	2.108407
206.544042	1345.945789	18.444800	-0.039377	2.103098
206.296850	1338.051672	18.449805	-0.039325	2.097771
206.326228	1330.121447	18.454810	-0.039326	2.092432
206.160931	1322.197447	18.459815	-0.039290	2.087065
206.260203	1314.246010	18.464819	-0.039303	2.081692
206.235063	1306.345529	18.469824	-0.039293	2.076327
206.103122	1298.397654	18.474829	-0.039264	2.070905
206.025926	1290.475016	18.479834	-0.039244	2.065491
206.110620	1282.534244	18.484839	-0.039255	2.060068
206.180644	1274.600535	18.489843	-0.039263	2.054633
206.058566	1266.671475	18.494848	-0.039235	2.049167
205.891881	1258.769962	18.499853	-0.039199	2.043702
205.854570	1250.858725	18.504858	-0.039187	2.038228
205.759381	1242.927121	18.509863	-0.039164	2.032719
205.658442	1234.972619	18.514867	-0.039140	2.027179
205.849763	1227.013113	18.519872	-0.039170	2.021651
205.764894	1219.104417	18.524877	-0.039149	2.016114
205.474450	1211.217433	18.529882	-0.039090	2.010555
205.414222	1203.289528	18.534887	-0.039074	2.004977
205.511282	1195.352195	18.539891	-0.039087	1.999393
205.405196	1187.461371	18.544896	-0.039062	1.993804
205.269107	1179.512080	18.549901	-0.039031	1.988155
205.350320	1171.581614	18.554906	-0.039041	1.982527
205.282535	1163.671955	18.559911	-0.039024	1.976881
205.193998	1155.748332	18.564915	-0.039002	1.971207
205.232534	1147.817918	18.569920	-0.039004	1.965526
205.167204	1139.910527	18.574925	-0.038987	1.959833
204.980090	1132.037252	18.579930	-0.038947	1.954135
204.878173	1124.059195	18.584935	-0.038923	1.948354
204.895867	1116.125146	18.589939	-0.038921	1.942601
204.892117	1108.221425	18.594944	-0.038915	1.936850
204.770052	1100.300018	18.599949	-0.038887	1.931056
204.890230	1092.367197	18.604954	-0.038904	1.925263
204.846217	1084.477181	18.609959	-0.038891	1.919466
204.792156	1076.557702	18.614963	-0.038876	1.913629
204.621696	1068.667994	18.619968	-0.038839	1.907782
204.754846	1060.730263	18.624973	-0.038859	1.901916
204.700880	1052.835835	18.629978	-0.038844	1.896043
204.531925	1044.935266	18.634983	-0.038807	1.890135
204.523545	1037.018408	18.639987	-0.038800	1.884213
204.540324	1029.132547	18.644992	-0.038798	1.878299
204.231420	1021.242451	18.649997	-0.038736	1.872326
204.221323	1013.314377	18.655002	-0.038729	1.866340
204.286842	1005.391712	18.660007	-0.038736	1.860347
204.114216	997.510843	18.665011	-0.038699	1.854338
204.225828	989.574236	18.670016	-0.038714	1.848301
204.146593	981.679877	18.675021	-0.038694	1.842254
203.793832	973.842740	18.680026	-0.038624	1.836199
203.678752	965.927547	18.685031	-0.038597	1.830091
203.761549	958.001090	18.690035	-0.038607	1.823978
203.786052	950.112897	18.695040	-0.038607	1.817868
203.668818	942.210734	18.700045	-0.038580	1.811708
203.772143	934.295012	18.705050	-0.038594	1.805544
203.808084	926.409851	18.710055	-0.038595	1.799374
203.610503	918.529150	18.715059	-0.038554	1.793158
203.447948	910.604267	18.720064	-0.038518	1.786890
203.320770	902.713613	18.725069	-0.038489	1.780631
203.259838	894.848711	18.730074	-0.038473	1.774379
203.308255	886.931926	18.735079	-0.038477	1.768077
203.178395	879.059195	18.740083	-0.038448	1.761765
203.259476	871.177733	18.745088	-0.038458	1.755450
202.955008	863.311274	18.750093	-0.038396	1.749076
203.052560	855.416966	18.755098	-0.038409	1.742706
203.114627	847.526212	18.760103	-0.038415	1.736312
202.902049	839.664079	18.765107	-0.038371	1.729882
202.852488	831.798665	18.770112	-0.038356	1.723447
202.783992	823.916419	18.775117	-0.038338	1.716971
202.593450	816.045687	18.780122	-0.038298	1.710464
202.547188	808.161933	18.785127	-0.038284	1.703940
202.492509	800.288100	18.790131	-0.038269	1.697398
202.548457	792.401326	18.795136	-0.038274	1.690835
202.382991	784.533159	18.800141	-0.038238	1.684232
202.378227	776.683292	18.805146	-0.038232	1.677641
202.417230	768.799064	18.810151	-0.038234	1.671000
202.253473	760.933000	18.815155	-0.038199	1.664320
202.054492	753.111735	18.820160	-0.038157	1.657647
201.866366	745.243141	18.825165	-0.038117	1.650908
201.988420	737.361911	18.830170	-0.038134	1.644173
201.958247	729.510999	18.835175	-0.038124	1.637416
201.919847	721.604327	18.840179	-0.038111	1.630581
202.009553	713.721062	18.845184	-0.038123	1.623755
201.636917	705.914784	18.850189	-0.038048	1.616903
201.434395	698.076182	18.855194	-0.038006	1.610018
201.650536	690.184902	18.860199	-0.038041	1.603115
201.634826	682.341088	18.865203	-0.038033	1.596192
201.537250	674.507337	18.870208	-0.038010	1.589236
201.470609	666.656559	18.875213	-0.037992	1.582238
201.395156	658.830779	18.880218	-0.037973	1.575231
201.280906	650.993196	18.885223	-0.037947	1.568176
201.193640	643.163087	18.890227	-0.037925	1.561099
201.282294	635.325760	18.895232	-0.037937	1.554010
200.915541	627.504065	18.900237	-0.037863	1.546835
200.912566	619.666953	18.905242	-0.037858	1.539667
200.978724	611.816389	18.910247	-0.037865	1.532463
200.751514	603.998836	18.915251	-0.037818	1.525211
200.621188	596.210752	18.920256	-0.037788	1.517967
200.711318	588.352469	18.925261	-0.037800	1.510656
200.855099	580.502495	18.930266	-0.037822	1.503325
200.641247	572.727136	18.935271	-0.037777	1.495974
200.338943	564.938936	18.940275	-0.037716	1.488560
200.600112	557.083115	18.945280	-0.037759	1.481133
200.289056	549.306640	18.950285	-0.037696	1.473655
200.210753	541.456805	18.955290	-0.037676	1.466104
200.271896	533.642875	18.960295	-0.037683	1.458571
200.120599	525.850804	18.965299	-0.037650	1.450987
200.169732	518.047550	18.970304	-0.037654	1.443384
200.050720	510.268031	18.975309	-0.037626	1.435736
200.127436	502.454733	18.980314	-0.037636	1.428047
199.814935	494.709146	18.985319	-0.037573	1.420318
199.843324	486.915545	18.990323	-0.037573	1.412556
199.864448	479.117051	18.995328	-0.037572	1.404745
199.756764	471.364448	19.000333	-0.037547	1.396915
199.628329	463.582584	19.005338	-0.037518	1.389008
199.475752	455.815486	19.010343	-0.037484	1.381066
199.407295	448.045736	19.015347	-0.037466	1.373090
199.364577	440.276043	19.020352	-0.037453	1.365072
199.159163	432.545138	19.025357	-0.037410	1.357018
199.045739	424.793147	19.030362	-0.037384	1.348911
198.985182	417.030384	19.035367	-0.037368	1.340752
199.036228	409.264527	19.040371	-0.037372	1.332560
199.038152	401.509693	19.045376	-0.037368	1.324320
198.888075	393.795711	19.050381	-0.037335	1.316044
198.719266	385.939609	19.055386	-0.037298	1.307560
198.775372	378.202579	19.060391	-0.037304	1.299191
198.645600	370.488340	19.065395	-0.037274	1.290758
198.635975	362.777144	19.070400	-0.037268	1.282295
198.386197	355.097821	19.075405	-0.037216	1.273766
198.436944	347.364831	19.080410	-0.037221	1.265177
198.297490	339.692272	19.085415	-0.037190	1.256560
198.054852	332.008754	19.090419	-0.037139	1.247852
198.207080	324.290252	19.095424	-0.037163	1.239119
198.033917	316.607843	19.100429	-0.037126	1.230302
197.859402	308.937179	19.105434	-0.037088	1.221435
197.788181	301.264647	19.110439	-0.037070	1.212521
197.735948	293.578798	19.115443	-0.037055	1.203529
197.610005	285.941805	19.120448	-0.037027	1.194512
197.495743	278.276050	19.125453	-0.037001	1.185395
197.517303	270.622183	19.130458	-0.037000	1.176249
197.442326	262.974829	19.135463	-0.036981	1.167019
197.212816	255.373065	19.140467	-0.036933	1.157740
197.315767	247.684043	19.145472	-0.036947	1.148347
197.195995	240.061654	19.150477	-0.036920	1.138913
197.045173	232.459490	19.155482	-0.036887	1.129418
196.856495	224.875929	19.160487	-0.036847	1.119858
196.732811	217.285915	19.165491	-0.036819	1.110222
196.606316	209.705633	19.170496	-0.036791	1.100513
196.416751	202.135929	19.175501	-0.036750	1.090717
196.479800	194.548450	19.180506	-0.036757	1.080866
196.221905	187.017503	19.185511	-0.036704	1.070925
196.086264	179.456743	19.190515	-0.036674	1.060880
196.135142	171.902295	19.195520	-0.036678	1.050790
196.007356	164.372596	19.200525	-0.036650	1.040595
195.824743	156.878926	19.205530	-0.036611	1.030335
195.881467	149.346843	19.210535	-0.036617	1.019976
195.688675	141.868373	19.215539	-0.036576	1.009525
195.458857	134.421983	19.220544	-0.036528	0.999000
195.271733	126.929550	19.225549	-0.036489	0.988309
195.274788	119.450475	19.230554	-0.036484	0.977567
195.281854	111.989311	19.235559	-0.036481	0.966734
194.875287	104.622191	19.240563	-0.036400	0.955809
194.606421	97.239206	19.245568	-0.036345	0.944771
194.014132	89.917125	19.250573	-0.036230	0.933608
193.463475	82.602188	19.255578	-0.036123	0.922332
193.330774	75.230576	19.260583	-0.036094	0.910942
192.760262	67.933205	19.265587	-0.035983	0.899403
192.342242	60.870195	19.270592	-0.035900	0.888130