Fri Mar 12 13:33:49 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
-0.075143	0.034796	0.000000	0.000041	0.720870

0.166870	-0.002782	0.005005	-0.000005	0.720881
0.000020	0.022572	0.010010	0.000027	0.720873
-0.302416	0.079013	0.015014	0.000083	0.720878
-0.188765	0.059811	0.020019	0.000062	0.720880
-0.315925	-0.046383	0.025024	0.000085	0.720626
-0.464929	-0.060561	0.030029	0.000113	0.720546
-0.299994	-0.094962	0.035034	0.000083	0.720536
-0.114269	-0.127753	0.040038	0.000048	0.720537
0.177950	-0.177725	0.045043	-0.000006	0.720541
0.060719	-0.162234	0.050048	0.000015	0.720530
0.150229	-0.173094	0.055053	-0.000001	0.720540
-0.053517	-0.139739	0.060058	0.000037	0.720534
0.096177	-0.164409	0.065062	0.000009	0.720538
0.006997	-0.145906	0.070067	0.000025	0.720543
0.083966	-0.163730	0.075072	0.000011	0.720535
0.087015	-0.158797	0.080077	0.000011	0.720546
-0.105750	-0.169418	0.085082	0.000046	0.720458
0.010910	-0.311785	0.090086	0.000025	0.720218
0.029262	-0.311402	0.095091	0.000021	0.720225
-0.228344	-0.269603	0.100096	0.000069	0.720217
-0.091078	-0.289524	0.105101	0.000044	0.720226
0.003291	-0.309693	0.110106	0.000026	0.720220
-0.255380	-0.262829	0.115110	0.000074	0.720221
-0.134847	-0.416265	0.120115	0.000052	0.719961
-0.226164	-0.434696	0.125120	0.000069	0.719893
-0.159936	-0.441415	0.130125	0.000057	0.719903
-0.254010	-0.430003	0.135130	0.000074	0.719892
0.016255	-0.476148	0.140134	0.000024	0.719896
-0.100780	-0.566388	0.145139	0.000046	0.719677
-0.518371	-0.532598	0.150144	0.000124	0.719597
-0.206645	-0.583041	0.155149	0.000066	0.719607
-0.096055	-0.607957	0.160154	0.000045	0.719597
-0.295036	-0.646625	0.165158	0.000082	0.719451
-0.538987	-0.695116	0.170163	0.000128	0.719269
-0.389070	-0.724739	0.175168	0.000100	0.719264
-0.047443	-0.778770	0.180173	0.000036	0.719277
-0.333832	-0.819958	0.185178	0.000089	0.719095
-0.425507	-0.873728	0.190182	0.000107	0.718957
-0.393582	-0.876837	0.195187	0.000101	0.718962
-0.637327	-0.836466	0.200192	0.000146	0.718956
-0.383668	-1.036275	0.205197	0.000099	0.718651
-0.336389	-1.051096	0.210202	0.000090	0.718638
-0.652981	-0.994071	0.215206	0.000149	0.718639
-1.039662	-1.027352	0.220211	0.000221	0.718438
-0.925101	-1.096012	0.225216	0.000200	0.718342
-0.463259	-1.172652	0.230221	0.000114	0.718354
-0.892555	-1.187948	0.235226	0.000194	0.718172
-0.689370	-1.306668	0.240230	0.000156	0.718009
-0.504413	-1.335102	0.245235	0.000122	0.718018
-0.589371	-1.425390	0.250240	0.000138	0.717810
-0.599232	-1.477258	0.255245	0.000139	0.717704
-0.579728	-1.484122	0.260250	0.000136	0.717697
-0.806376	-1.598073	0.265254	0.000178	0.717392
-1.333583	-1.509095	0.270259	0.000276	0.717382
-1.469271	-1.513535	0.275264	0.000301	0.717326
-1.127375	-1.696875	0.280269	0.000238	0.717083
-1.316189	-1.665604	0.285274	0.000273	0.717079
-1.303280	-1.750346	0.290278	0.000271	0.716916
-1.273302	-1.836020	0.295283	0.000265	0.716757
-1.272356	-1.840324	0.300288	0.000265	0.716749
-1.031739	-2.027603	0.305293	0.000220	0.716463
-1.188654	-2.007450	0.310298	0.000250	0.716447
-1.341302	-2.078038	0.315302	0.000278	0.716254
-3.243398	-1.799057	0.320307	0.000632	0.716135
-2.985136	-1.849943	0.325312	0.000584	0.716125
-3.000394	-1.929634	0.330317	0.000587	0.715962
-4.047504	-1.784770	0.335322	0.000782	0.715879
-3.861540	-1.817340	0.340326	0.000747	0.715881
-3.857030	-1.882803	0.345331	0.000746	0.715752
-5.040673	-1.780607	0.350336	0.000967	0.715537
-4.077907	-1.946915	0.355341	0.000788	0.715547
-4.633231	-1.852470	0.360346	0.000891	0.715538
-5.270615	-1.867462	0.365350	0.001010	0.715283
-5.649950	-1.827030	0.370355	0.001080	0.715230
-5.810855	-1.802767	0.375360	0.001110	0.715221
-5.141230	-1.916151	0.380365	0.000986	0.715233
-5.805145	-1.916839	0.385370	0.001109	0.714997
-6.623762	-1.816857	0.390374	0.001262	0.714906
-5.992791	-1.927136	0.395379	0.001144	0.714910
-6.579253	-1.826742	0.400384	0.001253	0.714902
-6.444925	-1.905684	0.405389	0.001228	0.714792
-7.303220	-1.849568	0.410394	0.001388	0.714600
-7.451304	-1.821726	0.415398	0.001416	0.714603
-7.448091	-1.820524	0.420403	0.001415	0.714607
-7.274195	-1.854015	0.425408	0.001383	0.714602
-7.143434	-1.951597	0.430413	0.001358	0.714454
-8.617361	-1.781192	0.435418	0.001633	0.714271
-8.015308	-1.889037	0.440422	0.001521	0.714270
-7.770325	-1.927491	0.445427	0.001475	0.714280
-8.589126	-1.786363	0.450432	0.001628	0.714271
-7.936179	-1.932704	0.455437	0.001506	0.714211
-8.809203	-1.900270	0.460442	0.001669	0.713966
-9.070008	-1.853917	0.465446	0.001717	0.713966
-9.194618	-1.829668	0.470451	0.001740	0.713970
-9.020380	-1.864751	0.475456	0.001708	0.713962
-8.772847	-1.905115	0.480461	0.001662	0.713970
-9.391513	-1.895455	0.485466	0.001777	0.713770
-10.370627	-1.783663	0.490470	0.001959	0.713645
-9.646644	-1.909978	0.495475	0.001825	0.713651
-10.482036	-1.765687	0.500480	0.001980	0.713641
-10.282353	-1.796155	0.505485	0.001943	0.713652
-9.827303	-1.880365	0.510490	0.001858	0.713645
-10.143375	-1.860553	0.515494	0.001917	0.713573
-11.072355	-1.800996	0.520499	0.002090	0.713362
-10.800216	-1.853323	0.525504	0.002039	0.713354
-10.772764	-1.856403	0.530509	0.002034	0.713358
-10.802402	-1.854767	0.535514	0.002040	0.713351
-10.705317	-1.872333	0.540518	0.002022	0.713350
-10.501323	-1.909458	0.545523	0.001984	0.713349
-11.672660	-1.867911	0.550528	0.002202	0.713016
-11.529245	-1.889693	0.555533	0.002175	0.713024
-11.645307	-1.870381	0.560538	0.002197	0.713021
-11.583847	-1.881797	0.565542	0.002185	0.713020
-11.780029	-1.844366	0.570547	0.002222	0.713025
-12.008432	-1.810450	0.575552	0.002264	0.713011
-11.510539	-1.986057	0.580557	0.002172	0.712838
-12.771927	-1.829088	0.585562	0.002407	0.712703
-12.723404	-1.835494	0.590566	0.002398	0.712708
-12.158648	-1.933842	0.595571	0.002292	0.712712
-12.711469	-1.840549	0.600576	0.002395	0.712702
-12.722985	-1.834023	0.605581	0.002397	0.712711
-12.275548	-1.925972	0.610586	0.002314	0.712687
-13.092546	-1.933284	0.615590	0.002466	0.712382
-13.446787	-1.866240	0.620595	0.002532	0.712390
-14.026825	-1.768329	0.625600	0.002640	0.712379
-13.307208	-1.892863	0.630605	0.002506	0.712386
-13.502636	-1.860230	0.635610	0.002543	0.712382
-13.875995	-1.795031	0.640614	0.002612	0.712379
-13.249277	-1.922565	0.645619	0.002496	0.712348
-14.246505	-1.878530	0.650624	0.002681	0.712081
-14.408851	-1.845054	0.655629	0.002711	0.712090
-14.277631	-1.869448	0.660634	0.002687	0.712088
-14.369455	-1.853668	0.665638	0.002704	0.712087
-14.307850	-1.862329	0.670643	0.002693	0.712092
-14.424114	-1.845328	0.675648	0.002714	0.712084
-14.072172	-1.962823	0.680653	0.002649	0.711975
-15.135843	-1.881310	0.685658	0.002847	0.711760
-15.258372	-1.860684	0.690662	0.002870	0.711758
-14.897388	-1.921010	0.695667	0.002802	0.711765
-15.451709	-1.828023	0.700672	0.002906	0.711754
-15.350924	-1.840535	0.705677	0.002887	0.711765
-15.250049	-1.859483	0.710682	0.002868	0.711763
-15.258916	-1.940842	0.715686	0.002870	0.711597
-15.911740	-1.896985	0.720691	0.002991	0.711453
-16.217179	-1.845408	0.725696	0.003048	0.711447
-16.001340	-1.879873	0.730701	0.003008	0.711455
-16.154875	-1.854308	0.735706	0.003037	0.711452
-16.289493	-1.831019	0.740710	0.003062	0.711450
-15.844698	-1.908356	0.745715	0.002979	0.711454
-16.132599	-1.965657	0.750720	0.003033	0.711237
-17.506849	-1.769657	0.755725	0.003288	0.711140
-16.914994	-1.877270	0.760730	0.003178	0.711135
-16.867104	-1.886033	0.765734	0.003169	0.711135
-16.961332	-1.868023	0.770739	0.003187	0.711137
-17.368902	-1.797736	0.775744	0.003263	0.711133
-17.094691	-1.845070	0.780749	0.003212	0.711136
-17.065259	-1.902949	0.785754	0.003206	0.711031
-17.953804	-1.828749	0.790758	0.003372	0.710863
-17.364942	-1.929301	0.795763	0.003262	0.710871
-17.846394	-1.847801	0.800768	0.003352	0.710863
-17.980765	-1.821191	0.805773	0.003377	0.710868
-17.538940	-1.899255	0.810778	0.003294	0.710870
-17.629675	-1.885778	0.815782	0.003311	0.710864
-17.849545	-1.984456	0.820787	0.003352	0.710589
-18.948318	-1.821704	0.825792	0.003557	0.710523
-18.830551	-1.838777	0.830797	0.003535	0.710531
-18.187401	-1.953580	0.835802	0.003415	0.710530
-18.965091	-1.816823	0.840806	0.003560	0.710527
-18.453743	-1.904152	0.845811	0.003465	0.710534
-18.573780	-1.897252	0.850816	0.003487	0.710505
-19.307807	-1.910205	0.855821	0.003624	0.710218
-19.356307	-1.902259	0.860826	0.003633	0.710217
-19.475035	-1.882892	0.865830	0.003655	0.710213
-19.416549	-1.889677	0.870835	0.003644	0.710220
-19.756114	-1.833454	0.875840	0.003707	0.710212
-19.475034	-1.880181	0.880845	0.003655	0.710218
-19.292708	-1.959730	0.885850	0.003621	0.710124
-20.868339	-1.796420	0.890854	0.003914	0.709889
-20.389745	-1.879949	0.895859	0.003825	0.709893
-20.637950	-1.838873	0.900864	0.003872	0.709887
-20.480871	-1.865611	0.905869	0.003842	0.709889
-20.318445	-1.895099	0.910874	0.003812	0.709888
-20.657831	-1.834844	0.915878	0.003875	0.709888
-20.258073	-1.909556	0.920883	0.003801	0.709881
-21.101395	-1.905117	0.925888	0.003958	0.709589
-21.253659	-1.874151	0.930893	0.003986	0.709597
-21.212024	-1.881019	0.935898	0.003979	0.709598
-21.599035	-1.813407	0.940902	0.004051	0.709595
-21.281602	-1.866345	0.945907	0.003991	0.709602
-21.369403	-1.855647	0.950912	0.004008	0.709592
-21.037186	-1.926985	0.955917	0.003946	0.709568
-21.860615	-1.929609	0.960922	0.004099	0.709269
-22.080058	-1.894004	0.965926	0.004140	0.709262
-22.008472	-1.902584	0.970931	0.004127	0.709271
-22.282315	-1.856816	0.975936	0.004178	0.709264
-22.243257	-1.862055	0.980941	0.004171	0.709268
-21.910283	-1.922251	0.985946	0.004109	0.709266
-22.206693	-1.916532	0.990950	0.004164	0.709172
-23.165705	-1.849016	0.995955	0.004342	0.708965
-22.734641	-1.930827	1.000960	0.004262	0.708955
-23.179662	-1.848389	1.005965	0.004345	0.708961
-23.053255	-1.873213	1.010970	0.004321	0.708957
-22.908537	-1.901378	1.015974	0.004295	0.708952
-22.823924	-1.910838	1.020979	0.004279	0.708963
-23.171172	-1.914475	1.025984	0.004343	0.708832
-24.018702	-1.857809	1.030989	0.004501	0.708643
-23.221736	-2.001171	1.035994	0.004353	0.708640
-24.154581	-1.836815	1.040998	0.004527	0.708636
-24.009919	-1.858423	1.046003	0.004500	0.708645
-23.688325	-1.920645	1.051008	0.004440	0.708635
-24.026106	-1.858606	1.056013	0.004503	0.708638
-23.807711	-1.972140	1.061018	0.004462	0.708489
-24.917671	-1.846527	1.066022	0.004669	0.708344
-24.233475	-1.964222	1.071027	0.004541	0.708353
-24.880207	-1.852492	1.076032	0.004662	0.708346
-24.973108	-1.834526	1.081037	0.004679	0.708349
-24.354776	-1.944261	1.086042	0.004564	0.708349
-24.789089	-1.869884	1.091046	0.004645	0.708343
-25.077176	-1.943269	1.096051	0.004698	0.708093
-25.623571	-1.889754	1.101056	0.004800	0.708005
-25.352900	-1.936941	1.106061	0.004750	0.708008
-25.399521	-1.927926	1.111066	0.004758	0.708009
-25.737444	-1.869364	1.116070	0.004821	0.708006
-25.170312	-1.964408	1.121075	0.004716	0.708018
-25.816659	-1.857025	1.126080	0.004836	0.708002
-26.399917	-1.903923	1.131085	0.004945	0.707699
-26.326183	-1.916282	1.136090	0.004931	0.707701
-26.755427	-1.842530	1.141094	0.005011	0.707695
-26.618943	-1.862960	1.146099	0.004986	0.707703
-26.580918	-1.874986	1.151104	0.004978	0.707693
-26.701881	-1.851785	1.156109	0.005001	0.707696
-26.614737	-1.865017	1.161114	0.004985	0.707701
-26.865618	-1.911495	1.166118	0.005032	0.707518
-27.495020	-1.868077	1.171123	0.005149	0.707380
-27.463693	-1.876883	1.176128	0.005143	0.707373
-27.610345	-1.849493	1.181133	0.005170	0.707376
-27.425978	-1.883517	1.186138	0.005136	0.707373
-27.385102	-1.892431	1.191142	0.005128	0.707370
-27.508386	-1.866406	1.196147	0.005151	0.707378
-27.340639	-1.945188	1.201152	0.005120	0.707280
-28.321725	-1.871560	1.206157	0.005303	0.707077
-28.044513	-1.917391	1.211162	0.005251	0.707084
-28.609179	-1.821477	1.216166	0.005356	0.707075
-28.316078	-1.869751	1.221171	0.005302	0.707082
-28.263132	-1.883265	1.226176	0.005292	0.707074
-28.491743	-1.840372	1.231181	0.005334	0.707079
-28.144144	-1.949209	1.236186	0.005270	0.706984
-29.186768	-1.884655	1.241190	0.005464	0.706741
-29.189327	-1.878209	1.246195	0.005464	0.706753
-29.464811	-1.833100	1.251200	0.005516	0.706745
-29.098207	-1.895722	1.256205	0.005447	0.706750
-28.870868	-1.937212	1.261210	0.005405	0.706748
-29.445017	-1.836961	1.266214	0.005512	0.706744
-29.002896	-1.963092	1.271219	0.005430	0.706649
-29.804936	-1.926134	1.276224	0.005579	0.706436
-30.001495	-1.888371	1.281229	0.005616	0.706442
-30.090360	-1.872059	1.286234	0.005632	0.706442
-30.237546	-1.849817	1.291238	0.005659	0.706434
-30.068384	-1.874606	1.296243	0.005628	0.706445
-30.235937	-1.848345	1.301248	0.005659	0.706438
-29.931930	-1.954263	1.306253	0.005603	0.706334
-30.831422	-1.896192	1.311258	0.005770	0.706128
-31.087142	-1.854329	1.316262	0.005818	0.706121
-30.790285	-1.903553	1.321267	0.005762	0.706128
-30.773759	-1.907153	1.326272	0.005759	0.706127
-31.195559	-1.830870	1.331277	0.005838	0.706129
-30.904917	-1.883335	1.336282	0.005784	0.706128
-31.066369	-1.894418	1.341286	0.005814	0.706048
-31.828307	-1.848518	1.346291	0.005956	0.705867
-31.635888	-1.888208	1.351296	0.005920	0.705856
-31.701518	-1.873825	1.356301	0.005932	0.705861
-31.569730	-1.895799	1.361306	0.005908	0.705864
-31.961805	-1.830713	1.366310	0.005981	0.705855
-31.752279	-1.862742	1.371315	0.005942	0.705865
-31.577642	-1.976985	1.376320	0.005909	0.705698
-32.872354	-1.833306	1.381325	0.006150	0.705523
-32.544036	-1.890277	1.386330	0.006089	0.705526
-32.658012	-1.873793	1.391334	0.006110	0.705518
-32.315975	-1.931814	1.396339	0.006047	0.705524
-32.462741	-1.908128	1.401344	0.006074	0.705519
-32.528177	-1.894750	1.406349	0.006086	0.705523
-32.830961	-1.966458	1.411354	0.006143	0.705270
-33.804791	-1.824988	1.416358	0.006324	0.705205
-33.517741	-1.872899	1.421363	0.006270	0.705212
-33.231810	-1.926426	1.426368	0.006217	0.705206
-33.806112	-1.823573	1.431373	0.006324	0.705207
-33.440472	-1.887665	1.436378	0.006256	0.705210
-33.246505	-1.925806	1.441382	0.006220	0.705202
-33.547022	-2.008864	1.446387	0.006276	0.704927
-34.821466	-1.803706	1.451392	0.006513	0.704883
-34.523752	-1.856505	1.456397	0.006458	0.704883
-33.972280	-1.954232	1.461402	0.006355	0.704885
-34.485835	-1.867284	1.466406	0.006451	0.704875
-34.221778	-1.909277	1.471411	0.006402	0.704886
-34.132876	-1.933491	1.476416	0.006385	0.704869
-35.081541	-1.904879	1.481421	0.006562	0.704586
-35.037384	-1.909066	1.486426	0.006553	0.704593
-35.206212	-1.883610	1.491430	0.006585	0.704584
-35.025535	-1.912097	1.496435	0.006551	0.704591
-35.436655	-1.843717	1.501440	0.006628	0.704581
-35.315398	-1.863160	1.506445	0.006605	0.704586
-34.804114	-1.986493	1.511450	0.006510	0.704521
-36.213762	-1.869890	1.516454	0.006773	0.704249
-35.994536	-1.903394	1.521459	0.006732	0.704260
-36.000795	-1.905757	1.526464	0.006733	0.704253
-36.306949	-1.849001	1.531469	0.006790	0.704258
-36.141933	-1.876480	1.536474	0.006759	0.704262
-35.927837	-1.919174	1.541478	0.006719	0.704253
-35.796001	-1.982160	1.546483	0.006695	0.704173
-37.129742	-1.856145	1.551488	0.006943	0.703948
-36.940537	-1.888905	1.556493	0.006908	0.703949
-36.772103	-1.918929	1.561498	0.006877	0.703949
-37.341153	-1.821417	1.566502	0.006982	0.703941
-37.086095	-1.862434	1.571507	0.006935	0.703950
-36.890577	-1.901041	1.576512	0.006899	0.703943
-36.845582	-1.925001	1.581517	0.006890	0.703911
-37.519722	-1.940017	1.586522	0.007016	0.703638
-37.687953	-1.913808	1.591526	0.007047	0.703630
-37.718860	-1.904154	1.596531	0.007053	0.703639
-37.814634	-1.891018	1.601536	0.007071	0.703631
-38.004580	-1.856451	1.606541	0.007106	0.703632
-37.564392	-1.931832	1.611546	0.007024	0.703638
-37.914685	-1.927194	1.616550	0.007089	0.703522
-38.363288	-1.933552	1.621555	0.007173	0.703347
-38.105249	-1.984348	1.626560	0.007125	0.703338
-38.667178	-1.884269	1.631565	0.007229	0.703337
-38.793633	-1.859050	1.636570	0.007253	0.703343
-38.669089	-1.885735	1.641574	0.007230	0.703334
-38.349121	-1.937288	1.646579	0.007170	0.703345
-38.833175	-1.986156	1.651584	0.007260	0.703072
-39.704350	-1.862742	1.656589	0.007423	0.703007
-39.427124	-1.911625	1.661594	0.007371	0.703009
-39.566126	-1.891395	1.666598	0.007397	0.702999
-39.697052	-1.862945	1.671603	0.007421	0.703010
-39.625139	-1.880862	1.676608	0.007408	0.702999
-39.218232	-1.951901	1.681613	0.007332	0.703002
-39.731141	-1.988484	1.686618	0.007428	0.702744
-40.566836	-1.869099	1.691622	0.007583	0.702684
-40.145668	-1.939824	1.696627	0.007505	0.702693
-40.357229	-1.902908	1.701632	0.007544	0.702691
-40.493322	-1.879332	1.706637	0.007570	0.702690
-40.189447	-1.932504	1.711642	0.007513	0.702692
-40.478605	-1.885267	1.716646	0.007567	0.702683
-41.006699	-1.940622	1.721651	0.007665	0.702381
-40.957434	-1.956775	1.726656	0.007656	0.702366
-41.204956	-1.912287	1.731661	0.007702	0.702367
-41.075166	-1.931524	1.736666	0.007678	0.702374
-41.424080	-1.875598	1.741670	0.007743	0.702362
-40.977696	-1.949125	1.746675	0.007660	0.702374
-41.137384	-1.954541	1.751680	0.007690	0.702305
-42.266870	-1.870626	1.756685	0.007900	0.702068
-41.493742	-2.004850	1.761690	0.007756	0.702075
-42.083887	-1.903860	1.766694	0.007866	0.702067
-42.163896	-1.885768	1.771699	0.007881	0.702074
-41.940473	-1.927569	1.776704	0.007839	0.702070
-41.844723	-1.946335	1.781709	0.007821	0.702067
-42.204230	-1.964720	1.786714	0.007888	0.701900
-43.333736	-1.843197	1.791718	0.008099	0.701738
-42.695463	-1.953997	1.796723	0.007980	0.701744
-42.732520	-1.949042	1.801728	0.007987	0.701741
-43.369827	-1.835472	1.806733	0.008105	0.701741
-42.909422	-1.916214	1.811738	0.008020	0.701744
-43.017306	-1.900173	1.816742	0.008040	0.701737
-43.161447	-1.918895	1.821747	0.008067	0.701647
-43.859427	-1.900697	1.826752	0.008197	0.701432
-43.509171	-1.963149	1.831757	0.008131	0.701432
-43.662914	-1.932412	1.836762	0.008160	0.701439
-43.957000	-1.884168	1.841766	0.008215	0.701430
-43.484467	-1.965263	1.846771	0.008127	0.701437
-43.458353	-1.970762	1.851776	0.008122	0.701435
-44.252422	-1.937283	1.856781	0.008270	0.701216
-44.553892	-1.928724	1.861786	0.008326	0.701125
-44.577597	-1.928538	1.866790	0.008330	0.701116
-44.616199	-1.916562	1.871795	0.008337	0.701127
-44.641035	-1.914979	1.876800	0.008342	0.701121
-44.506664	-1.939976	1.881805	0.008317	0.701119
-44.429229	-1.951466	1.886810	0.008303	0.701124
-45.231177	-1.922770	1.891814	0.008452	0.700892
-45.077836	-1.959431	1.896819	0.008424	0.700873
-44.927081	-1.987002	1.901824	0.008395	0.700872
-45.281903	-1.924570	1.906829	0.008461	0.700870
-45.014069	-1.968667	1.911834	0.008412	0.700877
-45.204110	-1.939703	1.916838	0.008447	0.700867
-45.274957	-2.048691	1.921843	0.008460	0.700621
-46.154254	-1.934428	1.926848	0.008624	0.700535
-46.317572	-1.905761	1.931853	0.008654	0.700534
-45.796855	-1.995611	1.936858	0.008557	0.700540
-46.436986	-1.885609	1.941862	0.008677	0.700531
-46.015834	-1.955587	1.946867	0.008598	0.700542
-46.049910	-1.990276	1.951872	0.008605	0.700459
-47.507383	-1.848329	1.956877	0.008876	0.700220
-46.652511	-1.998582	1.961882	0.008717	0.700224
-47.158367	-1.913369	1.966886	0.008811	0.700214
-47.414194	-1.863469	1.971891	0.008859	0.700223
-47.266108	-1.891951	1.976896	0.008831	0.700219
-47.035311	-1.932488	1.981901	0.008788	0.700220
-46.743105	-2.021958	1.986906	0.008734	0.700144
-48.290960	-1.873141	1.991910	0.009022	0.699886
-47.935889	-1.931227	1.996915	0.008956	0.699897
-48.124706	-1.898595	2.001920	0.008991	0.699894

-47.881377	-1.941709	2.011917	0.008946	0.699895
-48.115722	-1.900907	2.021914	0.008989	0.699893
-47.917979	-1.935776	2.031910	0.008952	0.699894
-48.411353	-1.916594	2.041907	0.009044	0.699754
-48.904540	-1.870597	2.051904	0.009136	0.699669
-47.995317	-1.922104	2.061901	0.008967	0.699893
-48.077229	-1.950580	2.071898	0.008982	0.699806
-47.782459	-1.959927	2.081894	0.008927	0.699894
-48.068474	-1.909795	2.091891	0.008981	0.699892
-47.842785	-1.951073	2.101888	0.008939	0.699890
-47.913667	-1.938074	2.111885	0.008952	0.699890
-48.097514	-1.903197	2.121882	0.008986	0.699895
-47.981475	-1.923687	2.131878	0.008964	0.699895
-48.159122	-1.893459	2.141875	0.008997	0.699892
-47.433205	-1.902643	2.151872	0.008862	0.700136
-47.211119	-1.904054	2.161869	0.008821	0.700214
-46.943755	-1.952417	2.171866	0.008771	0.700212
-47.133210	-1.917541	2.181862	0.008807	0.700214
-47.437838	-1.827522	2.191859	0.008863	0.700287
-46.336177	-1.903793	2.201856	0.008658	0.700530
-46.220645	-1.923768	2.211853	0.008637	0.700532
-46.223785	-1.923197	2.221850	0.008637	0.700532
-46.242602	-1.863696	2.231846	0.008641	0.700645
-45.471743	-1.891784	2.241843	0.008497	0.700867
-45.451683	-1.894579	2.251840	0.008493	0.700869
-45.401981	-1.902814	2.261837	0.008484	0.700870
-45.092274	-1.894771	2.271834	0.008427	0.700998
-44.799223	-1.887101	2.281830	0.008372	0.701119
-44.722281	-1.902354	2.291827	0.008358	0.701116
-44.638082	-1.907557	2.301824	0.008342	0.701136
-44.076909	-1.860186	2.311821	0.008238	0.701435
-43.526169	-1.959231	2.321818	0.008135	0.701433
-43.952208	-1.883327	2.331814	0.008214	0.701433
-43.468286	-1.880656	2.341811	0.008124	0.701613
-42.918062	-1.916354	2.351808	0.008022	0.701739
-43.136184	-1.876174	2.361805	0.008062	0.701742
-42.936389	-1.886686	2.371802	0.008025	0.701792
-42.397996	-1.845459	2.381798	0.007925	0.702070
-42.194272	-1.883281	2.391795	0.007887	0.702067
-42.234001	-1.875839	2.401792	0.007895	0.702068
-41.559477	-1.868646	2.411789	0.007769	0.702325
-41.143580	-1.923233	2.421786	0.007692	0.702365
-41.297863	-1.895325	2.431782	0.007720	0.702366
-41.093248	-1.881310	2.441779	0.007682	0.702468
-40.323901	-1.909238	2.451776	0.007539	0.702689
-40.428229	-1.891360	2.461773	0.007558	0.702687
-40.451580	-1.885523	2.471770	0.007563	0.702690
-39.834749	-1.856158	2.481766	0.007448	0.702972
-39.642326	-1.875791	2.491763	0.007412	0.703002
-39.643727	-1.876653	2.501760	0.007412	0.702999
-39.387781	-1.836175	2.511757	0.007365	0.703173
-38.633418	-1.887752	2.521754	0.007224	0.703341
-38.633325	-1.889190	2.531750	0.007224	0.703338
-38.511921	-1.908773	2.541747	0.007202	0.703342
-38.096100	-1.838782	2.551744	0.007124	0.703633
-37.833220	-1.886879	2.561741	0.007075	0.703630
-37.395742	-1.963628	2.571738	0.006994	0.703633
-37.388302	-1.890691	2.581734	0.006992	0.703783
-36.535231	-1.961296	2.591731	0.006834	0.703947
-37.008693	-1.876292	2.601728	0.006922	0.703948
-36.697685	-1.930683	2.611725	0.006864	0.703950
-36.109799	-1.927942	2.621722	0.006754	0.704167
-36.155294	-1.875088	2.631718	0.006763	0.704257
-35.966303	-1.908810	2.641715	0.006728	0.704257
-36.056769	-1.846653	2.651712	0.006745	0.704350
-35.170389	-1.885698	2.661709	0.006580	0.704590
-35.202202	-1.878270	2.671706	0.006585	0.704593
-35.339070	-1.854091	2.681702	0.006611	0.704593
-34.581461	-1.847669	2.691699	0.006470	0.704878
-34.478622	-1.863624	2.701696	0.006451	0.704883
-34.165826	-1.918330	2.711693	0.006393	0.704885
-34.043896	-1.834539	2.721690	0.006370	0.705097
-33.543992	-1.867285	2.731686	0.006277	0.705211
-33.277447	-1.915102	2.741683	0.006227	0.705210
-33.598977	-1.831179	2.751680	0.006287	0.705263
-32.590985	-1.881906	2.761677	0.006099	0.705523
-32.172891	-1.955107	2.771674	0.006022	0.705526
-32.395885	-1.915887	2.781670	0.006063	0.705525
-32.141610	-1.878392	2.791667	0.006016	0.705691
-31.596646	-1.892850	2.801664	0.005914	0.705858
-31.639251	-1.884273	2.811661	0.005922	0.705859
-31.777510	-1.857906	2.821658	0.005948	0.705863
-30.893215	-1.884944	2.831654	0.005783	0.706125
-30.955172	-1.874588	2.841651	0.005795	0.706124
-31.083043	-1.850306	2.851648	0.005819	0.706127
-30.370133	-1.867116	2.861645	0.005686	0.706349
-30.404152	-1.813208	2.871642	0.005692	0.706445
-30.064563	-1.873381	2.881638	0.005629	0.706446
-29.961885	-1.806997	2.891635	0.005610	0.706616
-29.420739	-1.835092	2.901632	0.005509	0.706753
-29.206004	-1.871996	2.911629	0.005469	0.706756
-29.153413	-1.840152	2.921626	0.005459	0.706838
-28.258560	-1.876347	2.931622	0.005293	0.707086
-28.434632	-1.843706	2.941619	0.005326	0.707089
-28.483169	-1.836834	2.951616	0.005335	0.707085
-27.660111	-1.868751	2.961613	0.005181	0.707315
-27.682357	-1.832102	2.971610	0.005186	0.707381
-27.324244	-1.896546	2.981606	0.005119	0.707380
-27.424036	-1.821844	2.991603	0.005138	0.707494
-26.440246	-1.895000	3.001600	0.004954	0.707699
-26.712535	-1.844937	3.011597	0.005005	0.707702
-26.672260	-1.852377	3.021594	0.004998	0.707701
-25.997044	-1.835030	3.031590	0.004872	0.707977
-25.880411	-1.837877	3.041587	0.004850	0.708013
-25.654643	-1.879275	3.051584	0.004808	0.708011
-25.538918	-1.823166	3.061581	0.004787	0.708165
-24.690572	-1.880380	3.071578	0.004629	0.708353
-24.739316	-1.871603	3.081574	0.004638	0.708353
-24.900522	-1.844225	3.091571	0.004668	0.708351
-24.227884	-1.845476	3.101568	0.004543	0.708588
-24.159823	-1.831221	3.111565	0.004530	0.708641
-23.976037	-1.865020	3.121562	0.004496	0.708639
-23.850339	-1.811163	3.131558	0.004472	0.708792
-23.391763	-1.810527	3.141555	0.004387	0.708957
-23.232313	-1.839324	3.151552	0.004357	0.708956
-23.185517	-1.816697	3.161549	0.004349	0.709018
-22.487915	-1.815402	3.171546	0.004219	0.709269
-22.226560	-1.862321	3.181542	0.004170	0.709268
-22.514632	-1.812961	3.191539	0.004224	0.709264
-21.749429	-1.811906	3.201536	0.004081	0.709539
-21.526204	-1.822726	3.211533	0.004040	0.709597
-21.392914	-1.845259	3.221530	0.004015	0.709600
-21.255951	-1.821047	3.231526	0.003989	0.709697
-20.683365	-1.824079	3.241523	0.003883	0.709895
-20.470859	-1.863073	3.251520	0.003843	0.709893
-20.592943	-1.842165	3.261517	0.003866	0.709891
-19.761989	-1.859342	3.271514	0.003711	0.710153
-19.660827	-1.843179	3.281510	0.003692	0.710221
-19.559686	-1.862366	3.291507	0.003674	0.710219
-19.532008	-1.850470	3.301504	0.003668	0.710252
-18.794196	-1.841585	3.311501	0.003531	0.710533
-18.447856	-1.900750	3.321498	0.003467	0.710538
-18.655455	-1.864487	3.331494	0.003505	0.710536
-18.734290	-1.769503	3.341491	0.003520	0.710698
-17.681281	-1.870757	3.351488	0.003324	0.710870
-17.848034	-1.838877	3.361485	0.003355	0.710875
-17.615035	-1.879526	3.371482	0.003312	0.710876
-17.079419	-1.855582	3.381478	0.003212	0.711115
-17.159954	-1.828571	3.391475	0.003227	0.711140
-16.981190	-1.861590	3.401472	0.003194	0.711137
-17.011776	-1.778541	3.411469	0.003199	0.711292
-16.041684	-1.868931	3.421466	0.003019	0.711457
-16.303681	-1.822900	3.431462	0.003067	0.711455
-16.190204	-1.820345	3.441459	0.003046	0.711501
-15.194426	-1.866056	3.451456	0.002861	0.711763
-15.344540	-1.838786	3.461453	0.002889	0.711764
-15.035924	-1.894552	3.471450	0.002831	0.711763
-15.019261	-1.797148	3.481446	0.002828	0.711963
-14.485368	-1.827883	3.491443	0.002729	0.712091
-14.521376	-1.822514	3.501440	0.002736	0.712089
-14.144593	-1.863835	3.511437	0.002666	0.712141
-13.327875	-1.884962	3.521434	0.002513	0.712388
-13.700242	-1.818954	3.531430	0.002583	0.712388
-13.744474	-1.811140	3.541427	0.002591	0.712388
-12.908324	-1.832621	3.551424	0.002435	0.712641
-12.865169	-1.805563	3.561421	0.002427	0.712711
-12.552597	-1.860774	3.571418	0.002369	0.712712
-12.646726	-1.796257	3.581414	0.002387	0.712807
-11.296911	-1.927988	3.591411	0.002135	0.713023
-11.696345	-1.858418	3.601408	0.002210	0.713020
-11.830560	-1.833826	3.611405	0.002235	0.713021
-11.342197	-1.822363	3.621402	0.002144	0.713217
-10.955656	-1.819723	3.631398	0.002072	0.713359
-10.645520	-1.875086	3.641395	0.002014	0.713359
-10.741989	-1.857652	3.651392	0.002032	0.713360
-9.898908	-1.864098	3.661389	0.001875	0.713645
-9.744332	-1.887343	3.671386	0.001846	0.713654
-9.814572	-1.874542	3.681382	0.001859	0.713655
-9.771463	-1.853634	3.691379	0.001851	0.713711
-9.060935	-1.850032	3.701376	0.001719	0.713970
-8.805096	-1.895484	3.711373	0.001672	0.713970
-9.003247	-1.860367	3.721370	0.001708	0.713970
-8.791555	-1.795811	3.731366	0.001669	0.714173
-8.029996	-1.878370	3.741363	0.001527	0.714279
-8.190428	-1.850445	3.751360	0.001557	0.714277
-7.923067	-1.870958	3.761357	0.001507	0.714331
-7.118266	-1.875997	3.771354	0.001358	0.714606
-7.114036	-1.876583	3.781350	0.001357	0.714606
-7.040439	-1.891297	3.791347	0.001343	0.714603
-7.139151	-1.801778	3.801344	0.001361	0.714746
-6.199591	-1.889458	3.811341	0.001187	0.714904
-6.473285	-1.839624	3.821338	0.001237	0.714906
-6.335305	-1.853483	3.831334	0.001212	0.714927
-5.326565	-1.883184	3.841331	0.001024	0.715225
-5.417001	-1.867810	3.851328	0.001041	0.715223
-5.262503	-1.893432	3.861325	0.001012	0.715227
-5.219200	-1.839471	3.871322	0.001004	0.715349
-4.175161	-1.929288	3.881318	0.000810	0.715540
-4.510226	-1.869469	3.891315	0.000872	0.715540
-4.500615	-1.870697	3.901312	0.000870	0.715541
-3.736978	-1.897167	3.911309	0.000728	0.715758
-3.595438	-1.860145	3.921306	0.000702	0.715882
-3.345252	-1.904110	3.931302	0.000655	0.715883
-3.395165	-1.895484	3.941299	0.000664	0.715882
-2.947508	-1.866436	3.951296	0.000581	0.716098
-2.663286	-1.903248	3.961293	0.000528	0.716125
-2.679077	-1.897307	3.971290	0.000531	0.716132
-2.644521	-1.836222	3.981286	0.000525	0.716265
-2.628945	-1.748142	3.991283	0.000522	0.716445
-1.911955	-1.875416	4.001280	0.000388	0.716445
-2.412576	-1.707678	4.011277	0.000481	0.716601
-1.066312	-1.869381	4.021274	0.000231	0.716756
-1.809315	-1.736073	4.031270	0.000369	0.716757
-1.257332	-1.737000	4.041267	0.000266	0.716950
-1.331641	-1.655969	4.051264	0.000280	0.717084
-2.133594	-1.483127	4.061261	0.000429	0.717144
-0.914030	-1.581648	4.071258	0.000202	0.717378
-0.736473	-1.612591	4.081254	0.000169	0.717380
-0.974379	-1.441541	4.091251	0.000214	0.717634
-0.729239	-1.452932	4.101248	0.000168	0.717698
-1.185802	-1.257474	4.111245	0.000253	0.717923
-1.307498	-1.180966	4.121242	0.000276	0.718032
-1.052901	-1.064717	4.131238	0.000228	0.718351
-0.642943	-1.079068	4.141235	0.000152	0.718467
-0.305850	-1.050938	4.151232	0.000089	0.718641
-0.670150	-0.873905	4.161229	0.000157	0.718862
-0.383977	-0.844023	4.171226	0.000103	0.719021
-0.409150	-0.713938	4.181222	0.000108	0.719269
-0.968019	-0.486700	4.191219	0.000212	0.719521
-0.490171	-0.453607	4.201216	0.000123	0.719754
-0.215692	-0.397464	4.211213	0.000072	0.719961
0.017429	-0.305118	4.221210	0.000028	0.720225
0.021773	-0.163129	4.231206	0.000027	0.720506
-0.003479	-0.031499	4.241203	0.000032	0.720756
0.102335	0.066985	4.251200	0.000012	0.720987
0.000000	0.234155	4.261197	0.000031	0.721280

-0.057248	0.871131	4.266202	0.000042	0.722511
0.574646	2.032795	4.271206	-0.000077	0.725009
0.682735	3.871400	4.276211	-0.000098	0.728635
1.215006	6.192244	4.281216	-0.000199	0.733322
1.793192	9.018856	4.286221	-0.000308	0.738967
2.292016	12.335824	4.291226	-0.000403	0.745476
2.867400	16.108733	4.296230	-0.000513	0.752813
3.679664	20.234342	4.301235	-0.000667	0.760815
5.828545	24.539814	4.306240	-0.001070	0.769504
8.039827	29.241519	4.311245	-0.001485	0.778836
9.199668	34.481100	4.316250	-0.001704	0.788689
10.899710	39.968336	4.321254	-0.002024	0.799030
12.114352	45.845911	4.326259	-0.002254	0.809771
12.905219	52.085686	4.331264	-0.002405	0.820867
13.856594	58.575225	4.336269	-0.002587	0.832289
14.465717	65.336082	4.341274	-0.002705	0.843910
15.269857	72.298125	4.346278	-0.002859	0.855763
15.866998	79.485730	4.351283	-0.002975	0.867763
16.639975	86.834982	4.356288	-0.003123	0.879909
17.573649	94.325054	4.361293	-0.003302	0.892159
17.918644	102.070243	4.366298	-0.003371	0.904479
18.551375	109.917246	4.371302	-0.003494	0.916870
19.835431	117.756495	4.376307	-0.003739	0.929257
20.634778	125.791408	4.381312	-0.003893	0.941647
21.494810	133.926422	4.386317	-0.004058	0.954040
22.525295	142.098876	4.391322	-0.004255	0.966373
23.333492	150.415261	4.396326	-0.004411	0.978701
23.991190	158.835950	4.401331	-0.004539	0.990988
24.829855	167.264325	4.406336	-0.004701	1.003179
25.960059	175.692912	4.411341	-0.004917	1.015294
26.236295	184.290843	4.416346	-0.004974	1.027295
26.991178	192.856842	4.421350	-0.005120	1.039227
27.799585	201.419772	4.426355	-0.005276	1.051031
28.635194	210.011400	4.431360	-0.005437	1.062749
29.185630	218.690156	4.436365	-0.005545	1.074387
29.746151	227.335802	4.441370	-0.005655	1.085860
30.331161	236.014088	4.446374	-0.005770	1.097261
30.853281	244.684961	4.451379	-0.005873	1.108520
31.501290	253.343040	4.456384	-0.005999	1.119677
32.259576	261.981072	4.461389	-0.006146	1.130722
32.762228	270.647229	4.466394	-0.006245	1.141641
33.240790	279.355831	4.471398	-0.006340	1.152502
33.601001	288.018356	4.476403	-0.006413	1.163182
34.204800	296.627733	4.481408	-0.006531	1.173750
34.581016	305.268650	4.486413	-0.006606	1.184214
34.874903	313.910705	4.491418	-0.006667	1.194572
35.597820	322.458975	4.496422	-0.006807	1.204816
36.168379	331.024860	4.501427	-0.006919	1.214963
36.597598	339.605604	4.506432	-0.007004	1.225016
37.555386	348.119602	4.511437	-0.007188	1.235013
37.938559	356.671144	4.516442	-0.007265	1.244861
38.710726	365.173613	4.521446	-0.007414	1.254650
39.331388	373.675340	4.526451	-0.007535	1.264334
39.781582	382.203646	4.531456	-0.007625	1.273942
40.436154	390.671585	4.536461	-0.007752	1.283448
40.807431	399.180761	4.541466	-0.007827	1.292878
41.194591	407.680242	4.546470	-0.007904	1.302231
41.756913	416.200452	4.551475	-0.008015	1.311571
42.080094	424.709153	4.556480	-0.008080	1.320790
42.617066	433.116321	4.561485	-0.008186	1.329875
43.087276	441.517245	4.566490	-0.008279	1.338880
43.711403	449.901623	4.571494	-0.008400	1.347833
43.948600	458.335064	4.576499	-0.008450	1.356712
44.353404	466.714924	4.581504	-0.008531	1.365505
44.678965	475.129570	4.586509	-0.008597	1.374265
45.127615	483.476882	4.591514	-0.008686	1.382921
45.678806	491.840007	4.596518	-0.008794	1.391556
45.987098	500.206036	4.601523	-0.008857	1.400100
46.046051	508.593634	4.606528	-0.008873	1.408572
46.617886	516.903213	4.611533	-0.008985	1.417001
47.223131	525.177246	4.616538	-0.009103	1.425349
47.687947	533.518532	4.621542	-0.009195	1.433692
47.987827	541.834811	4.626547	-0.009257	1.441935
48.534676	550.120981	4.631552	-0.009364	1.450142
48.802019	558.463279	4.636557	-0.009419	1.458312
49.209870	566.742648	4.641562	-0.009500	1.466398
49.766308	575.080041	4.646566	-0.009609	1.474519
50.209198	583.343149	4.651571	-0.009697	1.482506
50.488659	591.628784	4.656576	-0.009755	1.490446
50.832239	599.919510	4.661581	-0.009824	1.498359
51.222197	608.168840	4.666586	-0.009902	1.506198
51.606908	616.456901	4.671590	-0.009979	1.514032
51.875558	624.716624	4.676595	-0.010034	1.521781
52.305825	632.949094	4.681600	-0.010120	1.529491
52.717178	641.208649	4.686605	-0.010202	1.537183
53.164831	649.432936	4.691610	-0.010291	1.544810
53.713681	657.677808	4.696614	-0.010398	1.552433
54.166777	665.898288	4.701619	-0.010488	1.559983
54.487818	674.137180	4.706624	-0.010553	1.567493
55.006777	682.371242	4.711629	-0.010655	1.574992
55.576492	690.556121	4.716634	-0.010766	1.582418
55.904296	698.810714	4.721638	-0.010833	1.589837
56.145003	707.066209	4.726643	-0.010883	1.597209
56.575024	715.255159	4.731648	-0.010968	1.604516
57.035898	723.486805	4.736653	-0.011060	1.611831
57.325758	731.704421	4.741658	-0.011119	1.619077
57.515356	739.951435	4.746662	-0.011160	1.626302
58.058341	748.174058	4.751667	-0.011266	1.633523
58.320788	756.366388	4.756672	-0.011320	1.640647
58.924941	764.522943	4.761677	-0.011438	1.647757
59.210379	772.720580	4.766682	-0.011497	1.654827
59.480789	780.922691	4.771686	-0.011552	1.661869
59.780110	789.113403	4.776691	-0.011613	1.668875
59.891522	797.342666	4.781696	-0.011639	1.675859
60.522070	805.469470	4.786701	-0.011762	1.682797
60.863062	813.642256	4.791706	-0.011831	1.689707
61.354447	821.819712	4.796710	-0.011928	1.696612
61.842498	829.977304	4.801715	-0.012024	1.703472
61.954060	838.203355	4.806720	-0.012050	1.710312
61.961390	846.443701	4.811725	-0.012057	1.717123
62.464634	854.548587	4.816730	-0.012156	1.723859
62.768751	862.725773	4.821734	-0.012218	1.730603
63.114297	870.901131	4.826739	-0.012287	1.737325
63.435787	879.056365	4.831744	-0.012353	1.744001
63.943980	887.204160	4.836749	-0.012452	1.750669
64.174030	895.377044	4.841754	-0.012501	1.757296
64.521703	903.523613	4.846758	-0.012571	1.763893
65.045301	911.652759	4.851763	-0.012673	1.770472
65.251877	919.840488	4.856768	-0.012717	1.777035
65.547226	928.003832	4.861773	-0.012778	1.783564
65.864459	936.168561	4.866778	-0.012842	1.790074
66.537792	944.310914	4.871782	-0.012973	1.796586
66.762298	952.452615	4.876787	-0.013020	1.803019
67.222640	960.568618	4.881792	-0.013111	1.809438
67.582104	968.731692	4.886797	-0.013183	1.815858
67.560152	976.900702	4.891802	-0.013184	1.822214
67.699885	985.078581	4.896806	-0.013216	1.828575
68.311926	993.178241	4.901811	-0.013335	1.834909
68.556089	1001.310040	4.906816	-0.013386	1.841202
68.798322	1009.469603	4.911821	-0.013436	1.847495
69.073394	1017.612150	4.916826	-0.013492	1.853757
69.501834	1025.729714	4.921830	-0.013577	1.859997
69.826529	1033.860162	4.926835	-0.013643	1.866214
70.188531	1042.012968	4.931840	-0.013716	1.872431
70.735960	1050.122081	4.936845	-0.013823	1.878616
71.126159	1058.197807	4.941850	-0.013901	1.884737
71.327124	1066.370012	4.946854	-0.013944	1.890889
71.730252	1074.485000	4.951859	-0.014024	1.897001
71.930465	1082.604450	4.956864	-0.014067	1.903074
72.225523	1090.759245	4.961869	-0.014127	1.909165
72.618118	1098.863528	4.966874	-0.014205	1.915209
73.084087	1106.962361	4.971878	-0.014297	1.921239
73.267549	1115.095911	4.976883	-0.014337	1.927244
73.559226	1123.224848	4.981888	-0.014396	1.933238
73.865547	1131.356136	4.986893	-0.014459	1.939217
73.969861	1139.483119	4.991898	-0.014483	1.945153
74.518209	1147.614207	4.996902	-0.014591	1.951122
74.954123	1155.733164	5.001907	-0.014677	1.957051
75.428514	1163.789347	5.006912	-0.014771	1.962921
75.826703	1171.900567	5.011917	-0.014850	1.968806
76.013860	1180.026553	5.016922	-0.014890	1.974660
76.366901	1188.129166	5.021926	-0.014961	1.980498
76.595374	1196.254624	5.026931	-0.015009	1.986322
76.962883	1204.364572	5.031936	-0.015083	1.992132
77.582628	1212.439687	5.036941	-0.015204	1.997927
77.709028	1220.541923	5.041946	-0.015232	2.003673
77.950084	1228.676259	5.046950	-0.015283	2.009437
78.157607	1236.812465	5.051955	-0.015327	2.015182
78.521364	1244.879244	5.056960	-0.015400	2.020878
78.838078	1252.995706	5.061965	-0.015464	2.026588
79.051858	1261.127421	5.066970	-0.015509	2.032282
79.451099	1269.228324	5.071974	-0.015589	2.037958
79.763057	1277.304129	5.076979	-0.015652	2.043591
79.887671	1285.415294	5.081984	-0.015680	2.049214
80.288570	1293.523317	5.086989	-0.015760	2.054848
80.654256	1301.585464	5.091994	-0.015834	2.060431
80.700988	1309.715497	5.096998	-0.015848	2.066013
80.915982	1317.846668	5.102003	-0.015893	2.071598
81.464662	1325.895886	5.107008	-0.016000	2.077145
81.798643	1333.987533	5.112013	-0.016068	2.082684
82.038924	1342.072020	5.117018	-0.016118	2.088195
82.662232	1350.158246	5.122022	-0.016239	2.093730
83.214272	1358.222532	5.127027	-0.016347	2.099229
83.299114	1366.343791	5.132032	-0.016368	2.104705
83.786299	1374.440209	5.137037	-0.016464	2.110190
84.008910	1382.591859	5.142042	-0.016511	2.115672
84.345715	1390.658772	5.147046	-0.016579	2.121094
84.716636	1398.718468	5.152051	-0.016653	2.126501
85.220642	1406.788299	5.157056	-0.016752	2.131913
85.465516	1414.903996	5.162061	-0.016803	2.137317
85.375019	1423.012202	5.167066	-0.016792	2.142671
85.921760	1431.063579	5.172070	-0.016899	2.148034
86.213981	1439.183311	5.177075	-0.016958	2.153405
86.340979	1447.277622	5.182080	-0.016987	2.158730
86.819479	1455.323512	5.187085	-0.017082	2.164043
86.978948	1463.429488	5.192090	-0.017117	2.169353
87.519201	1471.487618	5.197094	-0.017223	2.174653
87.648948	1479.606825	5.202099	-0.017252	2.179942
87.877377	1487.677390	5.207104	-0.017300	2.185196
88.302550	1495.779558	5.212109	-0.017384	2.190476
88.490717	1503.878696	5.217114	-0.017424	2.195720
88.899027	1511.916722	5.222118	-0.017506	2.200931
89.265579	1519.985842	5.227123	-0.017579	2.206146
89.177969	1528.115145	5.232128	-0.017568	2.211347
89.406022	1536.220106	5.237133	-0.017616	2.216548
89.576346	1544.280586	5.242138	-0.017653	2.221703
90.043298	1552.334279	5.247142	-0.017745	2.226869
90.125424	1560.460686	5.252147	-0.017766	2.232034
90.195224	1568.542071	5.257152	-0.017784	2.237158
90.836820	1576.549303	5.262157	-0.017909	2.242274
90.979341	1584.641692	5.267162	-0.017940	2.247387
91.435861	1592.715595	5.272166	-0.018031	2.252505
91.729996	1600.799158	5.277171	-0.018091	2.257603
91.799391	1608.885758	5.282176	-0.018109	2.262672
92.190850	1616.958886	5.287181	-0.018187	2.267749
92.372240	1625.106323	5.292186	-0.018226	2.272843
92.506344	1633.193280	5.297190	-0.018256	2.277884
92.614156	1641.244970	5.302195	-0.018282	2.282889
92.807161	1649.283233	5.307200	-0.018323	2.287882
93.266753	1657.351303	5.312205	-0.018414	2.292906
93.436042	1665.423077	5.317210	-0.018450	2.297896
93.752351	1673.466420	5.322214	-0.018515	2.302870
94.160287	1681.521436	5.327219	-0.018596	2.307848
94.186793	1689.638724	5.332224	-0.018606	2.312822
94.641717	1697.678100	5.337229	-0.018696	2.317773
95.104380	1705.692420	5.342234	-0.018787	2.322698
95.577310	1713.756065	5.347238	-0.018881	2.327644
95.975608	1721.832433	5.352243	-0.018960	2.332581
96.156744	1729.912140	5.357248	-0.018999	2.337492
96.582868	1737.974674	5.362253	-0.019084	2.342402
96.604527	1746.076894	5.367258	-0.019093	2.347292
96.907343	1754.161603	5.372262	-0.019155	2.352185
97.183764	1762.250027	5.377267	-0.019211	2.357068
97.045662	1770.325383	5.382272	-0.019191	2.361899
97.294902	1778.389522	5.387277	-0.019243	2.366744
97.496114	1786.446215	5.392282	-0.019285	2.371572
97.872566	1794.503257	5.397286	-0.019361	2.376403
98.138634	1802.553677	5.402291	-0.019415	2.381213
98.464586	1810.590682	5.407296	-0.019481	2.386009
98.675028	1818.693839	5.412301	-0.019526	2.390825
98.969681	1826.749102	5.417306	-0.019586	2.395610
99.473574	1834.776334	5.422310	-0.019685	2.400386
99.915974	1842.821984	5.427315	-0.019773	2.405158
99.937261	1850.927710	5.432320	-0.019782	2.409922
100.312382	1859.016616	5.437325	-0.019857	2.414695
100.583252	1867.048047	5.442330	-0.019913	2.419417
100.892095	1875.100488	5.447334	-0.019975	2.424144
100.982127	1883.206110	5.452339	-0.019997	2.428877
101.334067	1891.325784	5.457344	-0.020068	2.433628
101.862311	1899.332574	5.462349	-0.020172	2.438319
102.052273	1907.365977	5.467354	-0.020212	2.442989
102.306164	1915.424578	5.472358	-0.020265	2.447670
102.371549	1923.524611	5.477363	-0.020282	2.452352
102.466125	1931.582121	5.482368	-0.020305	2.457003
102.851888	1939.617125	5.487373	-0.020382	2.461653
103.264450	1947.636046	5.492378	-0.020464	2.466288
103.772536	1955.681580	5.497382	-0.020564	2.470936
104.027713	1963.774734	5.502387	-0.020617	2.475584
104.259363	1971.814074	5.507392	-0.020665	2.480191
104.574985	1979.888868	5.512397	-0.020729	2.484815
104.917405	1987.930932	5.517402	-0.020798	2.489414
105.216691	1996.009920	5.522406	-0.020859	2.494022
105.461473	2004.075252	5.527411	-0.020910	2.498610
105.696898	2012.115618	5.532416	-0.020959	2.503175
105.845352	2020.193380	5.537421	-0.020992	2.507746
106.164257	2028.271524	5.542426	-0.021057	2.512321
106.239436	2036.365380	5.547430	-0.021076	2.516879
106.518516	2044.390191	5.552435	-0.021133	2.521405
106.927932	2052.407883	5.557440	-0.021215	2.525928
107.420892	2060.448510	5.562445	-0.021312	2.530462
107.561281	2068.536328	5.567450	-0.021343	2.534988
107.943459	2076.559087	5.572454	-0.021419	2.539488
108.164750	2084.616250	5.577459	-0.021466	2.543987
108.221187	2092.688819	5.582464	-0.021482	2.548475
108.773074	2100.749942	5.587469	-0.021590	2.552983
108.966111	2108.792126	5.592474	-0.021631	2.557448
109.325094	2116.817306	5.597478	-0.021703	2.561908
109.923026	2124.851988	5.602483	-0.021819	2.566381
110.109088	2132.925802	5.607488	-0.021859	2.570839
110.524151	2140.993712	5.612493	-0.021942	2.575303
110.525848	2149.065811	5.617498	-0.021947	2.579732
110.793792	2157.111503	5.622502	-0.022003	2.584157
111.168707	2165.184601	5.627507	-0.022078	2.588597
111.410702	2173.369156	5.632512	-0.022128	2.593082
111.426516	2181.458977	5.637517	-0.022136	2.597491
111.484081	2189.445060	5.642522	-0.022152	2.601839
112.234165	2197.409150	5.647526	-0.022297	2.606215
112.560697	2205.444979	5.652531	-0.022363	2.610594
112.730869	2213.505849	5.657536	-0.022400	2.614968
113.189229	2221.516242	5.662541	-0.022491	2.619327
113.483178	2229.559468	5.667546	-0.022551	2.623686
113.799649	2237.594030	5.672550	-0.022615	2.628034
114.076360	2245.666764	5.677555	-0.022671	2.632393
114.783413	2253.666241	5.682560	-0.022808	2.636733
114.891127	2261.748134	5.687565	-0.022834	2.641071
115.285994	2269.779485	5.692570	-0.022912	2.645393
115.510235	2277.821161	5.697574	-0.022959	2.649703
115.865679	2285.910686	5.702579	-0.023031	2.654040
115.879141	2293.970966	5.707584	-0.023039	2.658332
116.321069	2302.014902	5.712589	-0.023126	2.662636
116.621987	2310.050448	5.717594	-0.023187	2.666919
116.758272	2318.139188	5.722598	-0.023218	2.671213
116.900301	2326.237379	5.727603	-0.023250	2.675506
117.277344	2334.218982	5.732608	-0.023325	2.679745
117.609008	2342.261614	5.737613	-0.023392	2.684006
117.697490	2350.313991	5.742618	-0.023414	2.688251
117.834288	2358.368565	5.747622	-0.023445	2.692492
118.155935	2366.439848	5.752627	-0.023510	2.696748
118.427563	2374.456740	5.757632	-0.023565	2.700965
118.903751	2382.491617	5.762637	-0.023659	2.705198
119.158055	2390.536662	5.767642	-0.023712	2.709416
119.445247	2398.609034	5.772646	-0.023771	2.713643
119.681323	2406.660070	5.777651	-0.023820	2.717849
119.860505	2414.667403	5.782656	-0.023858	2.722023
120.196180	2422.705208	5.787661	-0.023926	2.726215
120.456889	2430.754256	5.792666	-0.023980	2.730402
120.642516	2438.832586	5.797670	-0.024020	2.734594
121.043657	2446.860373	5.802675	-0.024100	2.738766
121.095162	2454.912350	5.807680	-0.024115	2.742922
121.254176	2462.963266	5.812685	-0.024149	2.747079
121.663956	2471.011465	5.817690	-0.024231	2.751242
121.797134	2479.149709	5.822694	-0.024261	2.755429
122.145098	2487.123419	5.827699	-0.024331	2.759538
122.341606	2495.135544	5.832704	-0.024373	2.763652
122.792381	2503.155593	5.837709	-0.024462	2.767779
122.949214	2511.211864	5.842714	-0.024496	2.771900
123.170619	2519.270227	5.847718	-0.024543	2.776020
123.350953	2527.326452	5.852723	-0.024582	2.780131
123.502709	2535.351307	5.857728	-0.024615	2.784217
123.715896	2543.407383	5.862733	-0.024660	2.788317
123.999791	2551.445040	5.867738	-0.024718	2.792406
124.394381	2559.473175	5.872742	-0.024797	2.796491
124.667776	2567.531622	5.877747	-0.024853	2.800577
124.793818	2575.541590	5.882752	-0.024882	2.804625
125.243263	2583.578656	5.887757	-0.024971	2.808699
125.345030	2591.641565	5.892762	-0.024995	2.812760
125.847641	2599.664549	5.897766	-0.025094	2.816819
126.140961	2607.726506	5.902771	-0.025154	2.820879
126.023821	2615.776738	5.907776	-0.025137	2.824903
126.266775	2623.845972	5.912781	-0.025187	2.828952
126.554008	2631.903087	5.917786	-0.025246	2.832992
126.742487	2639.929858	5.922790	-0.025287	2.837005
127.064711	2647.971096	5.927795	-0.025352	2.841027
127.308940	2655.956736	5.932800	-0.025402	2.845011
127.650939	2664.003041	5.937805	-0.025471	2.849025
127.722977	2672.083234	5.942810	-0.025490	2.853036
128.104577	2680.087514	5.947814	-0.025566	2.857020
128.358472	2688.144751	5.952819	-0.025619	2.861018
128.550695	2696.150105	5.957824	-0.025660	2.864981
128.963480	2704.215385	5.962829	-0.025742	2.868980
129.211715	2712.269359	5.967834	-0.025793	2.872959
129.395397	2720.315815	5.972838	-0.025833	2.876925
129.696225	2728.358484	5.977843	-0.025894	2.880890
129.689302	2736.363262	5.982848	-0.025898	2.884815
130.078881	2744.423481	5.987853	-0.025976	2.888782
130.147145	2752.481520	5.992858	-0.025994	2.892726
130.241611	2760.553452	5.997862	-0.026017	2.896673
130.713187	2768.588270	6.002867	-0.026110	2.900616
130.843401	2776.585421	6.007872	-0.026139	2.904517
131.026052	2784.671771	6.012877	-0.026178	2.908460
131.467241	2792.709834	6.017882	-0.026266	2.912387
131.690677	2800.782942	6.022886	-0.026313	2.916314
131.961911	2808.770216	6.027891	-0.026368	2.920197
132.134750	2816.778411	6.032896	-0.026406	2.924079
132.442948	2824.810997	6.037901	-0.026468	2.927975
132.244189	2832.898165	6.042906	-0.026437	2.931866
132.418662	2840.948154	6.047910	-0.026474	2.935753
132.878643	2848.909011	6.052915	-0.026565	2.939607
133.146622	2856.931985	6.057920	-0.026620	2.943476
133.407186	2864.988605	6.062925	-0.026674	2.947356
133.742927	2873.034159	6.067930	-0.026742	2.951228
133.932702	2881.102322	6.072934	-0.026782	2.955099
134.294245	2889.099897	6.077939	-0.026855	2.958940
134.394369	2897.115915	6.082944	-0.026879	2.962772
134.822864	2905.161479	6.087949	-0.026964	2.966629
134.928294	2913.226152	6.092954	-0.026989	2.970474
135.127299	2921.254523	6.097958	-0.027031	2.974301
135.645462	2929.302661	6.102963	-0.027133	2.978149
135.673872	2937.332706	6.107968	-0.027143	2.981958
135.855628	2945.379140	6.112973	-0.027182	2.985778
136.022237	2953.415796	6.117978	-0.027218	2.989588
136.185946	2961.472365	6.122982	-0.027254	2.993402
136.221229	2969.537012	6.127987	-0.027266	2.997209
136.611612	2977.506114	6.132992	-0.027344	3.000984
136.808165	2985.539102	6.137997	-0.027386	3.004774
137.018225	2993.582915	6.143002	-0.027430	3.008565
137.288443	3001.613363	6.148006	-0.027486	3.012348
137.481335	3009.696818	6.153011	-0.027527	3.016147
137.683420	3017.687531	6.158016	-0.027570	3.019898
137.801799	3025.731111	6.163021	-0.027597	3.023666
138.122871	3033.753610	6.168026	-0.027662	3.027428
138.361452	3041.803560	6.173030	-0.027712	3.031195
138.438186	3049.881820	6.178035	-0.027731	3.034962
138.505546	3057.872447	6.183040	-0.027749	3.038684
139.006382	3065.885829	6.188045	-0.027847	3.042432
139.629661	3073.898050	6.193050	-0.027969	3.046181
139.832220	3081.940291	6.198054	-0.028012	3.049919
140.420017	3090.000071	6.203059	-0.028126	3.053679
140.571850	3098.040594	6.208064	-0.028160	3.057404
140.721519	3106.089203	6.213069	-0.028193	3.061129
140.896788	3114.106478	6.218074	-0.028231	3.064835
141.171354	3122.133579	6.223078	-0.028287	3.068547
141.170347	3130.267216	6.228083	-0.028292	3.072290
141.288479	3138.325247	6.233088	-0.028319	3.075999
141.591400	3146.308972	6.238093	-0.028381	3.079678
141.808849	3154.311074	6.243098	-0.028427	3.083358
141.984740	3162.315463	6.248102	-0.028465	3.087032
142.378726	3170.347743	6.253107	-0.028543	3.090724
142.508971	3178.410960	6.258112	-0.028573	3.094414
142.612060	3186.451695	6.263117	-0.028597	3.098088
142.808377	3194.454976	6.268122	-0.028639	3.101745
143.243554	3202.466507	6.273126	-0.028725	3.105412
143.592832	3210.525186	6.278131	-0.028796	3.109092
143.418683	3218.594277	6.283136	-0.028768	3.112749
143.796964	3226.622542	6.288141	-0.028844	3.116408
144.054671	3234.631067	6.293146	-0.028897	3.120048
144.178585	3242.635444	6.298150	-0.028925	3.123676
144.284956	3250.685488	6.303155	-0.028951	3.127320
144.584684	3258.720327	6.308160	-0.029012	3.130961
144.818023	3266.763610	6.313165	-0.029060	3.134599
144.840911	3274.803108	6.318170	-0.029070	3.138221
145.175813	3282.814996	6.323174	-0.029137	3.141841
145.587390	3290.836424	6.328179	-0.029219	3.145464
145.540468	3298.880888	6.333184	-0.029216	3.149073
146.038491	3306.919636	6.338189	-0.029314	3.152699
146.333408	3314.974450	6.343194	-0.029374	3.156319
146.399009	3322.973696	6.348198	-0.029391	3.159901
146.748094	3331.001363	6.353203	-0.029461	3.163503
146.859965	3339.014462	6.358208	-0.029487	3.167084
146.992880	3347.078100	6.363213	-0.029517	3.170685
147.142462	3355.140250	6.368218	-0.029551	3.174281
147.522531	3363.125510	6.373222	-0.029627	3.177849
147.712560	3371.177587	6.378227	-0.029667	3.181435
147.973357	3379.182787	6.383232	-0.029721	3.184999
148.182940	3387.231590	6.388237	-0.029765	3.188576
148.548741	3395.285196	6.393242	-0.029839	3.192157
148.568819	3403.341457	6.398246	-0.029848	3.195721
148.711693	3411.344133	6.403251	-0.029879	3.199263
148.867739	3419.341055	6.408256	-0.029914	3.202799
149.120002	3427.393050	6.413261	-0.029966	3.206359
149.318638	3435.396062	6.418266	-0.030008	3.209891
149.688316	3443.460736	6.423270	-0.030082	3.213453
150.127187	3451.491062	6.428275	-0.030169	3.217000
149.986229	3459.530884	6.433280	-0.030148	3.220522
150.413862	3467.519693	6.438285	-0.030233	3.224042
150.381166	3475.579091	6.443290	-0.030232	3.227570
150.554938	3483.623724	6.448294	-0.030270	3.231096
150.671701	3491.736170	6.453299	-0.030297	3.234645
151.138072	3499.667615	6.458304	-0.030389	3.238126
151.366359	3507.672203	6.463309	-0.030436	3.241625
151.627755	3515.686078	6.468314	-0.030490	3.245126
151.892331	3523.715627	6.473318	-0.030545	3.248630
152.375123	3531.764759	6.478323	-0.030640	3.252147
152.309019	3539.836680	6.483328	-0.030633	3.255648
152.716142	3547.813283	6.488333	-0.030714	3.259123
153.153496	3555.839102	6.493338	-0.030801	3.262617
153.124882	3563.873774	6.498342	-0.030800	3.266092
153.238128	3571.946688	6.503347	-0.030827	3.269586
153.491999	3579.973530	6.508352	-0.030879	3.273062
153.748652	3588.024715	6.513357	-0.030932	3.276545
153.786397	3596.007300	6.518362	-0.030944	3.279985
153.977958	3604.025741	6.523366	-0.030985	3.283444
154.389919	3612.090957	6.528371	-0.031067	3.286927
154.705612	3620.081969	6.533376	-0.031131	3.290372
154.869851	3628.155563	6.538381	-0.031167	3.293842
155.123362	3636.176541	6.543386	-0.031220	3.297289
155.411530	3644.172297	6.548390	-0.031278	3.300723
155.549231	3652.208226	6.553395	-0.031309	3.304165
155.690334	3660.253036	6.558400	-0.031341	3.307608
156.058081	3668.308102	6.563405	-0.031415	3.311059
156.096113	3676.369513	6.568410	-0.031427	3.314498
156.296250	3684.344288	6.573414	-0.031469	3.317901
156.622939	3692.389593	6.578419	-0.031535	3.321337
156.933502	3700.345594	6.583424	-0.031598	3.324730
157.167286	3708.377696	6.588429	-0.031647	3.328149
157.518221	3716.434407	6.593434	-0.031718	3.331579
157.787401	3724.435982	6.598438	-0.031773	3.334979
157.961084	3732.491102	6.603443	-0.031811	3.338395
158.096184	3740.521728	6.608448	-0.031841	3.341795
158.559685	3748.520945	6.613453	-0.031933	3.345191
158.769128	3756.576480	6.618458	-0.031977	3.348598
158.864936	3764.642755	6.623462	-0.032000	3.352001
159.030689	3772.703078	6.628467	-0.032036	3.355401
159.038800	3780.667934	6.633472	-0.032043	3.358752
159.191232	3788.709357	6.638477	-0.032076	3.362137
159.561556	3796.743241	6.643482	-0.032151	3.365523
159.561372	3804.768712	6.648486	-0.032156	3.368889
159.739710	3812.833934	6.653491	-0.032194	3.372275
159.988766	3820.855055	6.658496	-0.032246	3.375641
160.097563	3828.867102	6.663501	-0.032271	3.378995
160.314552	3836.892195	6.668506	-0.032317	3.382355
160.569970	3844.903412	6.673510	-0.032370	3.385707
161.054580	3852.912331	6.678515	-0.032465	3.389063
161.064390	3861.031683	6.683520	-0.032472	3.392444
161.108070	3869.107501	6.688525	-0.032486	3.395806
161.588494	3877.017193	6.693530	-0.032580	3.399110
161.808402	3885.020554	6.698534	-0.032626	3.402441
162.096021	3893.053322	6.703539	-0.032685	3.405783
162.067643	3901.065420	6.708544	-0.032685	3.409102
162.305124	3909.122832	6.713549	-0.032735	3.412446
162.684084	3917.166721	6.718554	-0.032810	3.415786
162.931270	3925.104834	6.723558	-0.032862	3.419075
163.184134	3933.183420	6.728563	-0.032914	3.422418
163.423457	3941.186313	6.733568	-0.032964	3.425726
163.791814	3949.213003	6.738573	-0.033037	3.429046
164.136432	3957.274639	6.743578	-0.033107	3.432375
164.322672	3965.304799	6.748582	-0.033147	3.435683
164.526135	3973.336067	6.753587	-0.033190	3.438989
164.547589	3981.339734	6.758592	-0.033199	3.442275
164.828988	3989.379492	6.763597	-0.033257	3.445580
164.956195	3997.415951	6.768602	-0.033286	3.448876
165.161808	4005.469099	6.773606	-0.033329	3.452178
165.484730	4013.505330	6.778611	-0.033395	3.455474
165.620777	4021.512403	6.783616	-0.033425	3.458749
165.823877	4029.542428	6.788621	-0.033468	3.462032
166.033217	4037.563587	6.793626	-0.033512	3.465308
166.452280	4045.575711	6.798630	-0.033596	3.468585
166.474704	4053.657886	6.803635	-0.033605	3.471874
166.533123	4061.688022	6.808640	-0.033621	3.475140
166.710805	4069.678612	6.813645	-0.033659	3.478391
167.053716	4077.699897	6.818650	-0.033728	3.481656
167.063806	4085.679587	6.823654	-0.033736	3.484891
167.494176	4093.698455	6.828659	-0.033821	3.488151
167.425628	4101.750260	6.833664	-0.033813	3.491407
167.784279	4109.799321	6.838669	-0.033885	3.494671
168.119373	4117.797588	6.843674	-0.033953	3.497912
168.292334	4125.823020	6.848678	-0.033990	3.501155
168.271732	4133.847759	6.853683	-0.033992	3.504389
168.307163	4141.851523	6.858688	-0.034004	3.507613
168.736950	4149.883452	6.863693	-0.034089	3.510857
168.969909	4157.915647	6.868698	-0.034137	3.514093
169.036504	4165.937811	6.873702	-0.034155	3.517317
169.339545	4173.984279	6.878707	-0.034217	3.520554
169.616259	4181.936672	6.883712	-0.034273	3.523750
169.865301	4190.003045	6.888717	-0.034325	3.526988
169.963523	4198.057199	6.893722	-0.034349	3.530213
170.149780	4206.094118	6.898726	-0.034389	3.533431
170.322169	4214.155930	6.903731	-0.034426	3.536656
170.371589	4222.137399	6.908736	-0.034440	3.539842
170.813157	4230.152974	6.913741	-0.034528	3.543051
170.794348	4238.208248	6.918746	-0.034529	3.546258
171.073558	4246.195895	6.923750	-0.034587	3.549445
171.400461	4254.318502	6.928755	-0.034653	3.552684
171.774409	4262.379901	6.933760	-0.034728	3.555896
171.854823	4270.327330	6.938765	-0.034748	3.559052
171.997694	4278.360734	6.943770	-0.034780	3.562242
172.082664	4286.327627	6.948774	-0.034801	3.565400
172.218044	4294.368153	6.953779	-0.034831	3.568586
172.532078	4302.387785	6.958784	-0.034895	3.571766
172.665923	4310.432675	6.963789	-0.034925	3.574948
173.063749	4318.456784	6.968794	-0.035004	3.578126
173.312475	4326.445234	6.973798	-0.035056	3.581284
173.933136	4334.408239	6.978803	-0.035177	3.584439
174.423800	4342.449875	6.983808	-0.035273	3.587618
174.566072	4350.489939	6.988813	-0.035305	3.590784
174.859784	4358.559626	6.993818	-0.035365	3.593963
175.100428	4366.555288	6.998822	-0.035415	3.597109
175.448156	4374.570286	7.003827	-0.035485	3.600263
175.528121	4382.586142	7.008832	-0.035505	3.603406
176.045766	4390.595340	7.013837	-0.035606	3.606557
176.465563	4398.625935	7.018842	-0.035690	3.609710
176.457218	4406.662985	7.023846	-0.035694	3.612851
176.665250	4414.750897	7.028851	-0.035738	3.616015
177.035004	4422.719299	7.033856	-0.035812	3.619134
177.120507	4430.750821	7.038861	-0.035833	3.622267
177.242822	4438.766709	7.043866	-0.035861	3.625393
177.265201	4446.782931	7.048870	-0.035870	3.628513
177.762665	4454.858041	7.053875	-0.035968	3.631666
177.817716	4462.903675	7.058880	-0.035983	3.634793
177.788932	4470.919443	7.063885	-0.035983	3.637904
178.281778	4478.936545	7.068890	-0.036080	3.641026
178.351353	4486.893257	7.073894	-0.036098	3.644111
178.552264	4494.968721	7.078899	-0.036141	3.647242
178.680174	4502.987601	7.083904	-0.036170	3.650348
179.025048	4511.017104	7.088909	-0.036240	3.653460
179.221233	4519.076710	7.093914	-0.036281	3.656577
179.446585	4527.014204	7.098918	-0.036328	3.659646
179.676083	4535.073238	7.103923	-0.036376	3.662758
179.847820	4543.111521	7.108928	-0.036414	3.665859
179.980999	4551.114656	7.113933	-0.036444	3.668942
180.554086	4559.163217	7.118938	-0.036556	3.672051
180.605967	4567.193678	7.123942	-0.036571	3.675138
180.726295	4575.189725	7.128947	-0.036598	3.678210
180.662480	4583.243894	7.133952	-0.036591	3.681298
180.949065	4591.194281	7.138957	-0.036650	3.684352
181.193903	4599.245529	7.143962	-0.036701	3.687440
181.174258	4607.281133	7.148966	-0.036702	3.690514
181.659795	4615.317085	7.153971	-0.036798	3.693598
181.630341	4623.366848	7.158976	-0.036798	3.696672
181.812884	4631.330835	7.163981	-0.036837	3.699715
182.291390	4639.358305	7.168986	-0.036931	3.702788
182.303954	4647.386952	7.173990	-0.036939	3.705847
182.543613	4655.432107	7.178995	-0.036989	3.708915
182.705980	4663.498077	7.184000	-0.037024	3.711987
182.950166	4671.567168	7.189005	-0.037075	3.715059
183.059544	4679.536574	7.194010	-0.037101	3.718088
183.252861	4687.487387	7.199014	-0.037142	3.721109
183.585312	4695.503410	7.204019	-0.037209	3.724156
183.433123	4703.544703	7.209024	-0.037186	3.727198
183.626080	4711.564776	7.214029	-0.037227	3.730238
183.988608	4719.606334	7.219034	-0.037300	3.733287
184.253962	4727.604567	7.224038	-0.037354	3.736316
184.210474	4735.614813	7.229043	-0.037351	3.739339
184.435781	4743.658524	7.234048	-0.037399	3.742378
185.010949	4751.621504	7.239053	-0.037511	3.745393
185.246409	4759.706086	7.244058	-0.037560	3.748443
185.476474	4767.745409	7.249062	-0.037608	3.751474
185.604292	4775.794362	7.254067	-0.037637	3.754503
185.693316	4783.800735	7.259072	-0.037659	3.757513
185.770586	4791.789338	7.264077	-0.037678	3.760514
186.194655	4799.797186	7.269082	-0.037763	3.763527
186.138835	4807.827714	7.274086	-0.037757	3.766535
186.530539	4815.875679	7.279091	-0.037836	3.769558
186.621726	4823.907677	7.284096	-0.037858	3.772566
186.705572	4831.937387	7.289101	-0.037879	3.775570
187.146000	4839.956983	7.294106	-0.037966	3.778575
187.074259	4847.963006	7.299110	-0.037958	3.781562
187.435355	4855.994540	7.304115	-0.038030	3.784566
187.695066	4864.021932	7.309120	-0.038084	3.787563
187.870502	4872.036512	7.314125	-0.038122	3.790552
188.002663	4880.117155	7.319130	-0.038151	3.793561
188.254328	4888.126627	7.324134	-0.038204	3.796545
188.183395	4896.118712	7.329139	-0.038196	3.799512
188.075711	4904.113298	7.334144	-0.038181	3.802478
188.473622	4912.102069	7.339149	-0.038260	3.805449
188.679416	4920.148119	7.344154	-0.038304	3.808436
188.535879	4928.183857	7.349158	-0.038282	3.811409
189.231183	4936.198132	7.354163	-0.038417	3.814389
189.291938	4944.208461	7.359168	-0.038433	3.817352
189.410194	4952.212426	7.364173	-0.038461	3.820312
189.809095	4960.232726	7.369178	-0.038540	3.823281
190.007054	4968.253191	7.374182	-0.038582	3.826244
190.205159	4976.291819	7.379187	-0.038624	3.829211
190.350269	4984.333012	7.384192	-0.038656	3.832176
190.502976	4992.352065	7.389197	-0.038690	3.835130
190.726213	5000.373382	7.394202	-0.038737	3.838085
190.752807	5008.372126	7.399206	-0.038747	3.841024
190.913865	5016.389023	7.404211	-0.038782	3.843971
191.268787	5024.399587	7.409216	-0.038854	3.846917
191.299185	5032.422640	7.414221	-0.038864	3.849859
191.467363	5040.490226	7.419226	-0.038901	3.852818
191.673524	5048.517619	7.424230	-0.038945	3.855760
191.910119	5056.513696	7.429235	-0.038994	3.858690
192.219248	5064.523929	7.434240	-0.039057	3.861624
192.244571	5072.533724	7.439245	-0.039067	3.864549
192.423056	5080.597723	7.444250	-0.039105	3.867495
192.553555	5088.599477	7.449254	-0.039135	3.870416
192.856291	5096.868007	7.454259	-0.039196	3.873434
193.142913	5104.871199	7.459264	-0.039255	3.876354
193.201777	5112.714257	7.464269	-0.039271	3.879208
193.324671	5120.755567	7.469274	-0.039299	3.882134
193.729231	5128.693364	7.474278	-0.039380	3.885025
193.852747	5136.725366	7.479283	-0.039408	3.887943
193.951053	5144.763078	7.484288	-0.039431	3.890860
194.010625	5152.796856	7.489293	-0.039448	3.893773
194.488873	5160.845665	7.494298	-0.039542	3.896697
194.670662	5168.792884	7.499302	-0.039581	3.899577
194.904512	5176.843524	7.504307	-0.039630	3.902492
195.238189	5184.819894	7.509312	-0.039697	3.905381
195.415370	5192.845042	7.514317	-0.039735	3.908282
195.676480	5200.906520	7.519322	-0.039789	3.911195
195.796347	5208.929430	7.524326	-0.039817	3.914090
195.926924	5216.964723	7.529331	-0.039846	3.916987
195.990332	5224.947000	7.534336	-0.039863	3.919862
196.261957	5232.938453	7.539341	-0.039919	3.922741
196.568856	5240.990586	7.544346	-0.039981	3.925641
196.920796	5248.958716	7.549350	-0.040052	3.928510
196.834884	5257.068865	7.554355	-0.040041	3.931419
196.962626	5265.087197	7.559360	-0.040070	3.934298
197.195078	5273.087929	7.564365	-0.040119	3.937169
197.291607	5281.090910	7.569370	-0.040142	3.940037
197.608178	5289.059187	7.574374	-0.040206	3.942894
197.779469	5297.090342	7.579379	-0.040243	3.945769
197.921066	5305.132390	7.584384	-0.040275	3.948646
197.927900	5313.188723	7.589389	-0.040281	3.951523
198.438249	5321.231615	7.594394	-0.040382	3.954401
198.575422	5329.219901	7.599398	-0.040413	3.957252
198.718306	5337.219872	7.604403	-0.040444	3.960105
198.808611	5345.222951	7.609408	-0.040466	3.962956
198.892228	5353.232160	7.614413	-0.040487	3.965807
199.029869	5361.251619	7.619418	-0.040518	3.968660
199.299677	5369.317210	7.624422	-0.040573	3.971531
199.661985	5377.339504	7.629427	-0.040646	3.974385
199.610972	5385.377569	7.634432	-0.040642	3.977235
199.925357	5393.341644	7.639437	-0.040706	3.980064
200.099640	5401.393908	7.644442	-0.040743	3.982919
199.842967	5409.376858	7.649446	-0.040701	3.985741
200.047055	5417.446367	7.654451	-0.040744	3.988599
200.456603	5425.482210	7.659456	-0.040825	3.991446
200.883117	5433.476330	7.664461	-0.040910	3.994277
201.039964	5441.536460	7.669466	-0.040945	3.997124
201.023186	5449.486384	7.674470	-0.040947	3.999928
201.168825	5457.533735	7.679475	-0.040979	4.002767
201.316315	5465.561070	7.684480	-0.041012	4.005597
201.383100	5473.555200	7.689485	-0.041029	4.008412
201.967169	5481.616996	7.694490	-0.041143	4.011256
201.951519	5489.634278	7.699494	-0.041146	4.014074
201.967373	5497.692249	7.704499	-0.041154	4.016904
202.370231	5505.671136	7.709504	-0.041234	4.019711
202.551446	5513.688710	7.714509	-0.041273	4.022526
202.396505	5521.726751	7.719514	-0.041249	4.025341
202.469318	5529.723839	7.724518	-0.041268	4.028143
202.850261	5537.739885	7.729523	-0.041344	4.030954
203.197207	5545.877469	7.734528	-0.041414	4.033805
203.241673	5553.904445	7.739533	-0.041428	4.036612
203.562823	5561.784753	7.744538	-0.041493	4.039369
203.778942	5569.803933	7.749542	-0.041538	4.042171
203.720282	5577.781374	7.754547	-0.041532	4.044952
203.746527	5585.861051	7.759552	-0.041542	4.047768
204.151779	5593.844301	7.764557	-0.041623	4.050555
204.132398	5601.950659	7.769562	-0.041625	4.053376
204.304545	5609.902006	7.774566	-0.041662	4.056144
204.503583	5617.909862	7.779571	-0.041704	4.058930
204.789644	5625.957473	7.784576	-0.041763	4.061729
204.772917	5633.911663	7.789581	-0.041765	4.064489
205.347162	5641.958675	7.794586	-0.041877	4.067289
205.491640	5649.963244	7.799590	-0.041909	4.070065
205.607281	5658.033128	7.804595	-0.041936	4.072862
206.044104	5666.016225	7.809600	-0.042022	4.075631
206.080936	5674.023743	7.814605	-0.042034	4.078401
206.333197	5682.068762	7.819610	-0.042087	4.081185
206.284075	5690.038267	7.824614	-0.042083	4.083937
206.628646	5698.090716	7.829619	-0.042152	4.086722
206.813128	5706.091745	7.834624	-0.042192	4.089484
206.925980	5714.139134	7.839629	-0.042218	4.092259
207.505493	5722.159303	7.844634	-0.042331	4.095030
207.506567	5730.162274	7.849638	-0.042336	4.097785
207.507942	5738.187876	7.854643	-0.042342	4.100545
207.654578	5746.216030	7.859648	-0.042375	4.103307
208.082534	5754.206161	7.864653	-0.042459	4.106058
208.232076	5762.246101	7.869658	-0.042492	4.108820
208.313985	5770.290442	7.874662	-0.042513	4.111580
208.508674	5778.350554	7.879667	-0.042554	4.114346
208.824109	5786.344193	7.884672	-0.042618	4.117089
208.846152	5794.299516	7.889677	-0.042628	4.119813
209.188321	5802.353209	7.894682	-0.042697	4.122573
209.179874	5810.329486	7.899686	-0.042700	4.125300
209.514043	5818.382550	7.904691	-0.042768	4.128056
209.435563	5826.442498	7.909696	-0.042758	4.130807
209.643276	5834.471767	7.914701	-0.042802	4.133549
209.694583	5842.509367	7.919706	-0.042817	4.136291
209.750865	5850.465085	7.924710	-0.042833	4.139002
210.033837	5858.527076	7.929715	-0.042891	4.141751
210.315478	5866.486309	7.934720	-0.042948	4.144463
210.359709	5874.528147	7.939725	-0.042962	4.147199
210.589009	5882.565135	7.944730	-0.043010	4.149933
210.800855	5890.626526	7.949734	-0.043054	4.152674
211.084866	5898.631020	7.954739	-0.043112	4.155394
211.345044	5906.633421	7.959744	-0.043166	4.158111
211.391995	5914.642976	7.964749	-0.043180	4.160827
211.795338	5922.625320	7.969754	-0.043260	4.163535
211.646639	5930.665018	7.974758	-0.043238	4.166255
212.068021	5938.665717	7.979763	-0.043322	4.168967
212.521550	5946.740932	7.984768	-0.043411	4.171702
212.596110	5954.714136	7.989773	-0.043430	4.174396
212.674365	5962.814504	7.994778	-0.043450	4.177132
212.788933	5970.771855	7.999782	-0.043477	4.179818
213.090245	5978.788449	8.004787	-0.043538	4.182525
212.985541	5986.795815	8.009792	-0.043524	4.185222
213.240603	5994.807766	8.014797	-0.043576	4.187923
213.336652	6002.861682	8.019802	-0.043600	4.190634
213.531262	6010.952060	8.024806	-0.043641	4.193357
213.924637	6018.968045	8.029811	-0.043720	4.196056
214.221254	6026.926406	8.034816	-0.043780	4.198732
214.238714	6034.895966	8.039821	-0.043788	4.201407
214.440165	6042.865796	8.044826	-0.043831	4.204083
214.491777	6050.935815	8.049830	-0.043846	4.206788
214.729437	6058.882262	8.054835	-0.043895	4.209453
214.772966	6066.986256	8.059840	-0.043909	4.212167
214.864502	6074.959627	8.064845	-0.043931	4.214835
215.034284	6083.017917	8.069850	-0.043968	4.217532
215.245490	6090.969910	8.074854	-0.044012	4.220191
215.569458	6098.995649	8.079859	-0.044078	4.222874
215.835414	6107.023678	8.084864	-0.044133	4.225556
215.745661	6115.011241	8.089869	-0.044121	4.228219
215.978768	6123.075859	8.094874	-0.044170	4.230909
215.956672	6131.134397	8.099878	-0.044171	4.233593
216.137534	6139.133067	8.104883	-0.044210	4.236258
216.472951	6147.136167	8.109888	-0.044277	4.238923
216.533866	6155.153225	8.114893	-0.044294	4.241589
216.619317	6163.143644	8.119898	-0.044315	4.244245
216.902524	6171.160816	8.124902	-0.044373	4.246909
217.094465	6179.167816	8.129907	-0.044414	4.249568
217.350299	6187.191327	8.134912	-0.044467	4.252231
217.269227	6195.243405	8.139917	-0.044457	4.254899
217.315864	6203.282871	8.144922	-0.044471	4.257562
217.545273	6211.311104	8.149926	-0.044519	4.260221
217.934177	6219.279725	8.154931	-0.044597	4.262861
217.866155	6227.330881	8.159936	-0.044589	4.265521
218.057797	6235.303565	8.164941	-0.044630	4.268157
218.448408	6243.420731	8.169946	-0.044708	4.270840
218.483317	6251.435127	8.174950	-0.044720	4.273485
218.684837	6259.474798	8.179955	-0.044762	4.276138
219.026311	6267.439174	8.184960	-0.044831	4.278765
219.127775	6275.472588	8.189965	-0.044855	4.281412
219.362107	6283.419396	8.194970	-0.044904	4.284029
219.560466	6291.456576	8.199974	-0.044946	4.286675
219.707679	6299.465887	8.204979	-0.044979	4.289309
219.892777	6307.534384	8.209984	-0.045019	4.291961
219.897000	6315.565804	8.214989	-0.045025	4.294598
220.086891	6323.582399	8.219994	-0.045065	4.297229
220.155549	6331.565029	8.224998	-0.045083	4.299848
220.587984	6339.566674	8.230003	-0.045169	4.302473
220.884683	6347.569001	8.235008	-0.045229	4.305096
220.834522	6355.621763	8.240013	-0.045225	4.307732
220.885027	6363.626477	8.245018	-0.045240	4.310350
221.148258	6371.684630	8.250022	-0.045294	4.312987
221.463630	6379.673975	8.255027	-0.045358	4.315599
221.603517	6387.702921	8.260032	-0.045389	4.318221
221.741919	6395.662194	8.265037	-0.045420	4.320820
222.003704	6403.661848	8.270042	-0.045474	4.323430
222.111889	6411.713959	8.275046	-0.045500	4.326055
222.331978	6419.725388	8.280051	-0.045546	4.328666
222.505776	6427.751400	8.285056	-0.045583	4.331280
222.532048	6435.800904	8.290061	-0.045594	4.333899
222.506391	6443.836241	8.295066	-0.045594	4.336511
222.623756	6451.795513	8.300070	-0.045621	4.339098
223.093511	6459.845425	8.305075	-0.045714	4.341715
223.161650	6467.827009	8.310080	-0.045732	4.344305
223.260069	6475.847429	8.315085	-0.045755	4.346907
223.208110	6483.912406	8.320090	-0.045751	4.349521
223.451435	6491.939570	8.325094	-0.045801	4.352123
223.404512	6500.018016	8.330099	-0.045798	4.354738
223.706148	6508.009401	8.335104	-0.045859	4.357326
223.896780	6515.948946	8.340109	-0.045900	4.359894
224.176638	6523.957223	8.345114	-0.045957	4.362484
224.217960	6531.920855	8.350118	-0.045970	4.365056
224.271018	6539.981866	8.355123	-0.045985	4.367658
224.421525	6548.038117	8.360128	-0.046018	4.370258
224.458636	6556.051962	8.365133	-0.046031	4.372842
224.703388	6564.075427	8.370138	-0.046081	4.375428
224.987348	6572.049681	8.375142	-0.046139	4.377998
225.041643	6580.049424	8.380147	-0.046155	4.380572
225.426864	6588.089687	8.385152	-0.046232	4.383160
225.708790	6596.068697	8.390157	-0.046289	4.385727
225.748566	6604.174405	8.395162	-0.046302	4.388331
225.517899	6612.152515	8.400166	-0.046264	4.390891
226.093992	6620.172858	8.405171	-0.046377	4.393467
226.096994	6628.208900	8.410176	-0.046383	4.396044
226.068445	6636.157625	8.415181	-0.046382	4.398592
226.242055	6644.237261	8.420186	-0.046420	4.401180
226.450371	6652.199209	8.425190	-0.046464	4.403730
226.599265	6660.237114	8.430195	-0.046497	4.406302
226.762186	6668.257091	8.435200	-0.046533	4.408867
226.822199	6676.269765	8.440205	-0.046549	4.411428
227.159349	6684.309178	8.445210	-0.046617	4.413997
227.179103	6692.349532	8.450214	-0.046626	4.416563
227.347249	6700.328669	8.455219	-0.046662	4.419109
227.439897	6708.395910	8.460224	-0.046685	4.421682
227.484580	6716.327463	8.465229	-0.046698	4.424209
227.741324	6724.420314	8.470234	-0.046751	4.426787
227.889455	6732.406720	8.475238	-0.046784	4.429329
227.989879	6740.445595	8.480243	-0.046808	4.431886
228.106894	6748.527242	8.485248	-0.046835	4.434456
228.196152	6756.507850	8.490253	-0.046857	4.436992
228.305979	6764.457375	8.495258	-0.046883	4.439516
228.527065	6772.513302	8.500262	-0.046929	4.442073
228.739385	6780.453948	8.505267	-0.046974	4.444592
228.920737	6788.574981	8.510272	-0.047013	4.447167
228.951815	6796.531208	8.515277	-0.047024	4.449687
229.106281	6804.593965	8.520282	-0.047058	4.452241
229.296754	6812.593849	8.525286	-0.047098	4.454773
229.344532	6820.613962	8.530291	-0.047113	4.457309
229.730835	6828.592050	8.535296	-0.047190	4.459832
229.667017	6836.624711	8.540301	-0.047183	4.462369
230.064920	6844.649548	8.545306	-0.047262	4.464903
229.956788	6852.648364	8.550310	-0.047247	4.467427
230.112822	6860.667468	8.555315	-0.047282	4.469956
230.568818	6868.726463	8.560320	-0.047372	4.472497
230.591279	6876.749402	8.565325	-0.047381	4.475024
230.774071	6884.802934	8.570330	-0.047421	4.477560
230.825598	6892.717580	8.575335	-0.047435	4.480050
230.769925	6900.736104	8.580339	-0.047430	4.482571
230.975747	6908.759429	8.585344	-0.047474	4.485093
231.152511	6916.768758	8.590349	-0.047512	4.487609
231.458668	6924.793322	8.595354	-0.047574	4.490129
231.492488	6932.842079	8.600359	-0.047586	4.492654
231.680298	6940.824203	8.605363	-0.047626	4.495157
231.930940	6948.879041	8.610368	-0.047678	4.497682
231.951210	6956.861828	8.615373	-0.047687	4.500182
232.030541	6964.886459	8.620378	-0.047707	4.502694
232.213477	6972.876774	8.625383	-0.047746	4.505194
232.256772	6980.912748	8.630387	-0.047759	4.507706
232.359580	6988.966727	8.635392	-0.047784	4.510223
232.432581	6997.003496	8.640397	-0.047802	4.512733
232.844822	7004.996067	8.645402	-0.047884	4.515229
232.882823	7013.055184	8.650407	-0.047897	4.517743
232.943172	7020.979417	8.655411	-0.047913	4.520214
233.146645	7029.000170	8.660416	-0.047956	4.522714
233.053417	7036.992471	8.665421	-0.047944	4.525203
233.285060	7045.041064	8.670426	-0.047992	4.527708
233.393215	7053.026787	8.675431	-0.048018	4.530193
233.567379	7061.030572	8.680435	-0.048055	4.532682
233.715671	7069.098290	8.685440	-0.048088	4.535189
233.945795	7077.079537	8.690445	-0.048136	4.537668
234.281047	7085.099832	8.695450	-0.048204	4.540158
234.468903	7093.106394	8.700455	-0.048244	4.542643
234.898679	7101.066718	8.705459	-0.048329	4.545111
235.158107	7109.178588	8.710464	-0.048383	4.547626
235.434302	7117.155822	8.715469	-0.048440	4.550097
235.532304	7125.250384	8.720474	-0.048463	4.552602
235.634526	7133.254544	8.725479	-0.048487	4.555079
235.684652	7141.255268	8.730483	-0.048502	4.557553
235.922914	7149.239325	8.735488	-0.048551	4.560020
235.844839	7157.280708	8.740493	-0.048542	4.562504
236.194890	7165.272122	8.745498	-0.048612	4.564971
236.420113	7173.298847	8.750503	-0.048660	4.567448
236.313320	7181.274517	8.755507	-0.048645	4.569907
236.724506	7189.381359	8.760512	-0.048727	4.572406
236.793812	7197.328652	8.765517	-0.048745	4.574854
236.821684	7205.422381	8.770522	-0.048755	4.577346
237.050176	7213.353512	8.775527	-0.048803	4.579786
237.347285	7221.425882	8.780531	-0.048864	4.582269
237.489154	7229.397465	8.785536	-0.048895	4.584719
237.455307	7237.444936	8.790541	-0.048894	4.587191
237.555261	7245.460865	8.795546	-0.048918	4.589652
237.632767	7253.505610	8.800551	-0.048938	4.592120
237.779298	7261.530168	8.805555	-0.048970	4.594581
238.104854	7269.581241	8.810560	-0.049036	4.597049
238.135112	7277.487311	8.815565	-0.049047	4.599471
238.147278	7285.569951	8.820570	-0.049054	4.601946
238.303853	7293.524164	8.825575	-0.049089	4.604381
238.443428	7301.544948	8.830579	-0.049120	4.606834
238.798823	7309.536247	8.835584	-0.049191	4.609277
238.903484	7317.599471	8.840589	-0.049216	4.611740
239.021713	7325.648646	8.845594	-0.049243	4.614198
239.032669	7333.665325	8.850599	-0.049251	4.616645
239.089429	7341.604380	8.855603	-0.049266	4.619067
239.302613	7349.650132	8.860608	-0.049311	4.621520
239.390773	7357.622280	8.865613	-0.049333	4.623949
239.623732	7365.669535	8.870618	-0.049381	4.626400
239.656755	7373.691197	8.875623	-0.049393	4.628841
239.902441	7381.717377	8.880627	-0.049444	4.631283
240.126197	7389.788946	8.885632	-0.049491	4.633737
239.998109	7397.770808	8.890637	-0.049472	4.636163
240.378350	7405.744369	8.895642	-0.049548	4.638585
240.496797	7413.806073	8.900647	-0.049575	4.641032
240.620087	7421.741390	8.905651	-0.049603	4.643440
240.773353	7429.795253	8.910656	-0.049637	4.645882
240.524611	7437.780258	8.915661	-0.049596	4.648303
240.880996	7445.825658	8.920666	-0.049668	4.650740
241.037115	7453.872764	8.925671	-0.049702	4.653176
241.341801	7461.853427	8.930675	-0.049764	4.655591
241.468236	7469.893510	8.935680	-0.049793	4.658023
241.423599	7477.887657	8.940685	-0.049790	4.660440
241.777463	7485.942221	8.945690	-0.049861	4.662873
241.912778	7493.929955	8.950695	-0.049891	4.665285
241.909321	7501.925445	8.955699	-0.049896	4.667698
242.175914	7509.981117	8.960704	-0.049951	4.670128
242.560256	7518.040596	8.965709	-0.050027	4.672558
242.714349	7526.112661	8.970714	-0.050061	4.674990
242.706108	7534.082443	8.975719	-0.050065	4.677390
242.781547	7541.984141	8.980723	-0.050084	4.679769
243.039797	7550.043434	8.985728	-0.050137	4.682194
243.066395	7557.969702	8.990733	-0.050148	4.684577
243.321049	7566.083142	8.995738	-0.050200	4.687016
243.435310	7574.053518	9.000743	-0.050227	4.689410
243.691213	7582.087123	9.005747	-0.050280	4.691822
243.941720	7590.128057	9.010752	-0.050332	4.694234
243.774347	7598.128875	9.015757	-0.050306	4.696634
243.845846	7606.063455	9.020762	-0.050324	4.699013
244.155475	7614.166305	9.025767	-0.050387	4.701440
244.418666	7622.131335	9.030771	-0.050441	4.703825
244.561292	7630.193530	9.035776	-0.050473	4.706238
244.458144	7638.175633	9.040781	-0.050459	4.708627
244.701326	7646.213492	9.045786	-0.050509	4.711030
244.728763	7654.244459	9.050791	-0.050520	4.713430
244.776318	7662.246247	9.055795	-0.050534	4.715820
245.041613	7670.261237	9.060800	-0.050588	4.718212
245.319097	7678.221907	9.065805	-0.050645	4.720587
245.517072	7686.286524	9.070810	-0.050687	4.722992
245.474269	7694.302929	9.075815	-0.050685	4.725382
245.668868	7702.299324	9.080819	-0.050726	4.727764
245.949138	7710.384512	9.085824	-0.050784	4.730171
245.881579	7718.385681	9.090829	-0.050776	4.732553
246.092161	7726.418726	9.095834	-0.050821	4.734942
246.304899	7734.442287	9.100839	-0.050865	4.737328
246.297770	7742.416297	9.105843	-0.050869	4.739697
246.550039	7750.499970	9.110848	-0.050922	4.742098
246.684608	7758.446733	9.115853	-0.050952	4.744457
246.704537	7766.452070	9.120858	-0.050961	4.746833
246.910644	7774.476073	9.125863	-0.051004	4.749212
247.113735	7782.486246	9.130867	-0.051047	4.751586
247.146659	7790.551307	9.135872	-0.051059	4.753975
247.240826	7798.566311	9.140877	-0.051082	4.756349
247.596397	7806.477609	9.145882	-0.051153	4.758689
247.652403	7814.564641	9.150887	-0.051169	4.761082
247.680124	7822.544547	9.155891	-0.051179	4.763441
247.912563	7830.582686	9.160896	-0.051227	4.765816
248.118596	7838.590777	9.165901	-0.051271	4.768181
248.309771	7846.599573	9.170906	-0.051312	4.770545
248.251027	7854.642045	9.175911	-0.051306	4.772919
248.311453	7862.619113	9.180915	-0.051323	4.775271
248.756685	7870.684634	9.185920	-0.051411	4.777648
248.831310	7878.616947	9.190925	-0.051430	4.779985
249.019099	7886.672398	9.195930	-0.051470	4.782357
249.144820	7894.669550	9.200935	-0.051499	4.784710
249.272132	7902.676024	9.205939	-0.051528	4.787065
249.525543	7910.725440	9.210944	-0.051580	4.789432
249.728719	7918.711293	9.215949	-0.051623	4.791778
249.978673	7926.752843	9.220954	-0.051675	4.794140
249.973346	7934.766004	9.225959	-0.051679	4.796493
250.025776	7942.752044	9.230963	-0.051694	4.798836
250.354541	7950.784500	9.235968	-0.051760	4.801191
250.381165	7958.755718	9.240973	-0.051771	4.803528
250.460339	7966.803039	9.245978	-0.051790	4.805886
250.760133	7974.879124	9.250983	-0.051852	4.808251
250.573600	7982.852409	9.255987	-0.051822	4.810586
250.706034	7990.293598	9.260992	-0.051852	4.812763
250.821238	7994.760745	9.265997	-0.051876	4.814069

251.007739	7997.308590	9.271002	-0.051912	4.814813
250.983490	7998.699270	9.276007	-0.051909	4.815220
251.148952	7999.151438	9.281011	-0.051940	4.815352
251.365082	8000.090259	9.286016	-0.051981	4.815625
251.334788	8000.034243	9.291021	-0.051975	4.815609
251.447013	8000.030729	9.296026	-0.051996	4.815607
251.471549	8000.087717	9.301031	-0.052000	4.815624
251.692958	8000.027253	9.306035	-0.052042	4.815605
251.718392	8000.052224	9.311040	-0.052046	4.815612
251.735867	8000.053575	9.316045	-0.052050	4.815613
251.979386	8000.030842	9.321050	-0.052095	4.815605
252.294109	8000.098958	9.326055	-0.052154	4.815623
252.014667	7999.998314	9.331059	-0.052101	4.815595
252.119190	8000.061943	9.336064	-0.052121	4.815613
252.176529	8000.073553	9.341069	-0.052132	4.815616
251.978212	8000.036159	9.346074	-0.052095	4.815606
252.167743	8000.056325	9.351079	-0.052130	4.815611
252.258015	8000.022557	9.356083	-0.052147	4.815601
252.034669	8000.085124	9.361088	-0.052105	4.815621
252.301930	8000.038219	9.366093	-0.052155	4.815606
252.287946	8000.030516	9.371098	-0.052152	4.815603
252.273464	8000.037755	9.376103	-0.052150	4.815606
252.286574	7999.998460	9.381107	-0.052152	4.815594
252.251367	8000.073698	9.386112	-0.052146	4.815616
252.283810	8000.034718	9.391117	-0.052152	4.815605
252.261615	8000.015137	9.396122	-0.052147	4.815599
252.221509	8000.067872	9.401127	-0.052140	4.815615
252.302140	8000.004050	9.406131	-0.052155	4.815596
252.351062	8000.077453	9.411136	-0.052164	4.815617
252.325985	8000.065299	9.416141	-0.052159	4.815613
252.378095	8000.058672	9.421146	-0.052169	4.815611
252.322843	8000.074856	9.426151	-0.052159	4.815616
252.334876	8000.029138	9.431155	-0.052161	4.815603
252.576341	8000.106741	9.436160	-0.052206	4.815624
252.662369	8000.087853	9.441165	-0.052222	4.815618
252.691238	8000.074441	9.446170	-0.052227	4.815614
252.689949	8000.137418	9.451175	-0.052227	4.815633
252.807071	8000.066715	9.456179	-0.052249	4.815611
252.849103	8000.072737	9.461184	-0.052257	4.815613
252.762756	8000.065993	9.466189	-0.052241	4.815611
252.889504	8000.037089	9.471194	-0.052264	4.815602
252.741456	8000.136118	9.476199	-0.052237	4.815632
252.861925	8000.097502	9.481203	-0.052259	4.815620
252.997940	8000.123206	9.486208	-0.052284	4.815627
252.972710	8000.072609	9.491213	-0.052280	4.815612
252.868661	8000.070916	9.496218	-0.052260	4.815612
252.809801	8000.107330	9.501223	-0.052249	4.815623
252.787217	8000.138995	9.506227	-0.052245	4.815633
252.874431	8000.147888	9.511232	-0.052261	4.815635
252.626703	8000.140653	9.516237	-0.052215	4.815634
252.765027	8000.135429	9.521242	-0.052241	4.815632
253.133783	8000.147836	9.526247	-0.052310	4.815634
252.966662	8000.022322	9.531251	-0.052278	4.815598
252.868493	8000.092265	9.536256	-0.052260	4.815619
252.929031	8000.110334	9.541261	-0.052272	4.815624
252.906589	8000.131323	9.546266	-0.052267	4.815630
252.888357	8000.132094	9.551271	-0.052264	4.815630
253.040381	8000.067297	9.556275	-0.052292	4.815611
253.140803	8000.142608	9.561280	-0.052311	4.815632
253.048796	8000.046078	9.566285	-0.052294	4.815604
252.991860	8000.071845	9.571290	-0.052283	4.815612
253.164450	8000.126974	9.576295	-0.052315	4.815627
253.156839	8000.064919	9.581299	-0.052314	4.815609
253.105404	8000.075827	9.586304	-0.052304	4.815613
253.148712	8000.128852	9.591309	-0.052312	4.815628
253.181426	8000.147537	9.596314	-0.052318	4.815633
253.073204	8000.110538	9.601319	-0.052298	4.815623
253.264232	8000.054918	9.606323	-0.052334	4.815606
253.178906	8000.137884	9.611328	-0.052318	4.815631
253.104235	8000.066195	9.616333	-0.052304	4.815610
253.053863	8000.080323	9.621338	-0.052295	4.815614
253.355989	8000.139697	9.626343	-0.052351	4.815630
253.451787	8000.106018	9.631347	-0.052369	4.815620
253.253295	8000.156177	9.636352	-0.052332	4.815636
253.407124	8000.159748	9.641357	-0.052360	4.815636
253.416518	8000.089426	9.646362	-0.052362	4.815615
253.218666	8000.196188	9.651367	-0.052325	4.815647
253.467436	8000.125491	9.656371	-0.052372	4.815626
253.420814	8000.123664	9.661376	-0.052363	4.815625
253.200125	8000.085902	9.666381	-0.052322	4.815615
253.277429	8000.051923	9.671386	-0.052336	4.815605
253.472211	8000.158668	9.676391	-0.052373	4.815635
253.497514	8000.101418	9.681395	-0.052377	4.815618
253.399711	8000.133995	9.686400	-0.052359	4.815628
253.389743	8000.184019	9.691405	-0.052357	4.815643
253.391439	8000.134928	9.696410	-0.052357	4.815629
253.322029	8000.124187	9.701415	-0.052345	4.815626
253.357025	8000.082045	9.706419	-0.052351	4.815613
253.402804	8000.140450	9.711424	-0.052360	4.815630
253.297680	8000.071468	9.716429	-0.052340	4.815611
253.410485	8000.074371	9.721434	-0.052361	4.815611
253.379158	8000.126182	9.726439	-0.052355	4.815626
253.490709	8000.083150	9.731443	-0.052376	4.815613
253.278748	8000.059412	9.736448	-0.052336	4.815607
253.484405	8000.105470	9.741453	-0.052375	4.815620
253.460309	8000.082654	9.746458	-0.052370	4.815613
253.411112	8000.097870	9.751463	-0.052361	4.815618
253.469876	8000.068927	9.756467	-0.052372	4.815609
253.675234	8000.095761	9.761472	-0.052410	4.815616
253.387523	8000.104959	9.766477	-0.052357	4.815620
253.574131	8000.084504	9.771482	-0.052391	4.815613
253.805814	8000.157681	9.776487	-0.052435	4.815633
253.640303	8000.081309	9.781491	-0.052404	4.815612
253.600227	8000.147927	9.786496	-0.052396	4.815631
253.746600	8000.133224	9.791501	-0.052423	4.815626
253.605078	8000.096751	9.796506	-0.052397	4.815616
253.518884	8000.113500	9.801511	-0.052381	4.815622
253.550516	8000.037133	9.806515	-0.052387	4.815599
253.775930	8000.187090	9.811520	-0.052429	4.815642
253.542865	8000.122431	9.816525	-0.052386	4.815624
253.473975	8000.060445	9.821530	-0.052373	4.815606
253.659881	8000.091233	9.826535	-0.052407	4.815615
253.675502	8000.060521	9.831539	-0.052410	4.815606
253.686555	8000.092734	9.836544	-0.052412	4.815615
253.438326	8000.108981	9.841549	-0.052366	4.815621
253.745062	8000.108634	9.846554	-0.052423	4.815619
253.722657	8000.118947	9.851559	-0.052419	4.815622
253.560121	8000.060776	9.856563	-0.052389	4.815606
253.704478	8000.090888	9.861568	-0.052416	4.815614
253.613348	8000.073387	9.866573	-0.052399	4.815610
253.764849	8000.060903	9.871578	-0.052427	4.815605
253.756545	8000.084259	9.876583	-0.052425	4.815612
253.934011	8000.048706	9.881587	-0.052458	4.815601
253.889796	8000.092834	9.886592	-0.052450	4.815614
253.856744	8000.143550	9.891597	-0.052444	4.815629
253.760217	8000.073639	9.896602	-0.052426	4.815609
253.866772	8000.095661	9.901607	-0.052446	4.815615
253.788051	8000.095447	9.906611	-0.052431	4.815615
253.947898	8000.086302	9.911616	-0.052461	4.815612
253.940874	8000.148120	9.916621	-0.052460	4.815630
253.957926	8000.172957	9.921626	-0.052463	4.815637
253.883640	8000.237951	9.926631	-0.052449	4.815656
253.661230	8000.153177	9.931635	-0.052407	4.815633
253.750513	8000.117256	9.936640	-0.052424	4.815622
253.829498	8000.104660	9.941645	-0.052439	4.815618
253.858835	8000.062425	9.946650	-0.052444	4.815605
253.881804	8000.140748	9.951655	-0.052448	4.815628
253.909431	8000.085672	9.956659	-0.052454	4.815612
254.040944	8000.155084	9.961664	-0.052478	4.815631
253.880594	8000.205863	9.966669	-0.052448	4.815647
253.697224	8000.097165	9.971674	-0.052414	4.815616
253.803383	8000.150147	9.976679	-0.052434	4.815631
253.856196	8000.122176	9.981683	-0.052444	4.815623
254.143809	8000.188790	9.986688	-0.052497	4.815641
253.956226	8000.183600	9.991693	-0.052462	4.815640
254.160591	8000.089756	9.996698	-0.052500	4.815612
254.050098	8000.110381	10.001703	-0.052480	4.815618
253.865696	8000.102039	10.006707	-0.052445	4.815617
254.015737	8000.102346	10.011712	-0.052473	4.815616
253.962405	8000.049155	10.016717	-0.052463	4.815601
253.831852	8000.044894	10.021722	-0.052439	4.815600
253.895841	8000.110003	10.026727	-0.052451	4.815619
253.911511	8000.035511	10.031731	-0.052454	4.815597
254.015835	8000.066040	10.036736	-0.052473	4.815606
253.908755	8000.129432	10.041741	-0.052453	4.815625
254.014629	8000.091646	10.046746	-0.052473	4.815613
254.046448	8000.111384	10.051751	-0.052479	4.815619
254.095609	8000.108981	10.056755	-0.052488	4.815618
254.079068	8000.142881	10.061760	-0.052485	4.815628
254.228137	8000.121815	10.066765	-0.052513	4.815621
253.977468	8000.079293	10.071770	-0.052466	4.815610
254.048099	8000.117815	10.076775	-0.052479	4.815621
254.185532	8000.105103	10.081779	-0.052505	4.815616
254.120670	8000.164912	10.086784	-0.052493	4.815634
253.910314	8000.131588	10.091789	-0.052454	4.815625
254.042403	8000.118788	10.096794	-0.052478	4.815621
254.160571	8000.191187	10.101799	-0.052500	4.815641
254.065904	8000.158679	10.106803	-0.052483	4.815632
254.145315	8000.166378	10.111808	-0.052497	4.815634
254.185352	8000.136063	10.116813	-0.052505	4.815625
254.247769	8000.096502	10.121818	-0.052516	4.815613
254.127684	8000.185310	10.126823	-0.052494	4.815640
254.219527	8000.136618	10.131827	-0.052511	4.815625
254.279987	8000.132263	10.136832	-0.052522	4.815624
254.112777	8000.114591	10.141837	-0.052491	4.815619
254.092280	8000.058730	10.146842	-0.052487	4.815603
254.159967	8000.137782	10.151847	-0.052500	4.815626
254.130818	8000.106340	10.156851	-0.052495	4.815617
254.278468	8000.123693	10.161856	-0.052522	4.815621
254.436672	8000.134811	10.166861	-0.052552	4.815624
253.999792	8000.082850	10.171866	-0.052470	4.815611
254.018861	8000.145092	10.176871	-0.052474	4.815629
253.963028	8000.080115	10.181875	-0.052463	4.815610
254.047028	8000.124194	10.186880	-0.052479	4.815622
253.986925	8000.081570	10.191885	-0.052468	4.815610
254.049893	8000.139189	10.196890	-0.052480	4.815627
254.217078	8000.136571	10.201895	-0.052511	4.815625
254.098452	8000.048147	10.206899	-0.052488	4.815600
254.133149	8000.083949	10.211904	-0.052495	4.815610
254.208559	8000.096922	10.216909	-0.052509	4.815614
254.287057	8000.013842	10.221914	-0.052524	4.815589
254.360406	8000.054545	10.226919	-0.052537	4.815601
254.239643	8000.015205	10.231923	-0.052515	4.815590
254.451258	8000.088057	10.236928	-0.052554	4.815610
254.183797	8000.097584	10.241933	-0.052504	4.815614
254.127430	8000.058225	10.246938	-0.052494	4.815603
254.361818	8000.129312	10.251943	-0.052538	4.815622
254.186550	8000.063457	10.256947	-0.052505	4.815604
254.181997	8000.070857	10.261952	-0.052504	4.815606
254.404290	8000.147087	10.266957	-0.052545	4.815627
254.268374	8000.050906	10.271962	-0.052520	4.815600
254.336681	8000.102205	10.276967	-0.052533	4.815615
254.277425	8000.072409	10.281971	-0.052522	4.815606
254.477790	8000.095959	10.286976	-0.052559	4.815612
254.223866	8000.122791	10.291981	-0.052512	4.815621
254.126055	8000.067808	10.296986	-0.052494	4.815606
254.199583	8000.057258	10.301991	-0.052507	4.815602
254.265278	8000.046581	10.306995	-0.052519	4.815599
254.186890	8000.063457	10.312000	-0.052505	4.815604
254.297139	8000.078065	10.317005	-0.052525	4.815608
254.318943	8000.047453	10.322010	-0.052529	4.815599
254.420423	8000.089682	10.327015	-0.052548	4.815611
254.360856	8000.021440	10.332019	-0.052537	4.815591
254.418808	8000.067231	10.337024	-0.052548	4.815604
254.401733	8000.126750	10.342029	-0.052545	4.815621
254.355781	8000.045915	10.347034	-0.052536	4.815598
254.450738	8000.102987	10.352039	-0.052554	4.815614
254.479372	8000.059672	10.357043	-0.052559	4.815601
254.586960	8000.063559	10.362048	-0.052579	4.815602
254.608667	8000.120506	10.367053	-0.052583	4.815619
254.551083	8000.099279	10.372058	-0.052573	4.815613
254.545351	8000.129085	10.377063	-0.052572	4.815621
254.413245	8000.044711	10.382067	-0.052547	4.815597
254.591938	8000.055095	10.387072	-0.052580	4.815600
254.320113	8000.053872	10.392077	-0.052530	4.815601
254.358021	8000.070506	10.397082	-0.052537	4.815605
254.526943	8000.140528	10.402087	-0.052568	4.815625
254.593233	8000.102098	10.407091	-0.052580	4.815613
254.426323	8000.118600	10.412096	-0.052549	4.815619
254.482486	8000.106701	10.417101	-0.052560	4.815615
254.440546	8000.054762	10.422106	-0.052552	4.815600
254.470041	8000.079802	10.427111	-0.052557	4.815607
254.246695	8000.119945	10.432115	-0.052516	4.815620
254.611802	8000.112008	10.437120	-0.052584	4.815616
254.488460	8000.120677	10.442125	-0.052561	4.815619
254.357967	8000.047008	10.447130	-0.052537	4.815598
254.459238	8000.096708	10.452135	-0.052555	4.815612
254.413727	8000.039373	10.457139	-0.052547	4.815596
254.381693	8000.046325	10.462144	-0.052541	4.815598
254.556607	8000.118581	10.467149	-0.052574	4.815618
254.662907	8000.048767	10.472154	-0.052593	4.815597
254.610743	8000.088494	10.477159	-0.052584	4.815609
254.340595	8000.139622	10.482163	-0.052533	4.815626
254.707688	8000.177633	10.487168	-0.052602	4.815635
254.535104	8000.175890	10.492173	-0.052570	4.815635
254.536984	8000.096902	10.497178	-0.052570	4.815612
254.372966	8000.110248	10.502183	-0.052539	4.815617
254.429904	8000.101564	10.507187	-0.052550	4.815614
254.411380	8000.103398	10.512192	-0.052546	4.815615
254.451526	8000.101915	10.517197	-0.052554	4.815614
254.543167	8000.118356	10.522202	-0.052571	4.815618
254.584545	8000.161742	10.527207	-0.052579	4.815631
254.574714	8000.090038	10.532211	-0.052577	4.815610
254.458667	8000.110572	10.537216	-0.052555	4.815616
254.650754	8000.111563	10.542221	-0.052591	4.815616
254.644677	8000.045259	10.547226	-0.052590	4.815596
254.601270	8000.097943	10.552231	-0.052582	4.815612
254.804177	8000.076686	10.557235	-0.052619	4.815605
254.622821	8000.081208	10.562240	-0.052586	4.815607
254.608571	8000.096992	10.567245	-0.052583	4.815612
254.725919	8000.081818	10.572250	-0.052605	4.815607
254.780701	8000.112608	10.577255	-0.052615	4.815616
254.630856	8000.088811	10.582259	-0.052587	4.815609
254.693134	8000.081282	10.587264	-0.052599	4.815607
254.589669	8000.092411	10.592269	-0.052580	4.815611
254.468764	8000.041322	10.597274	-0.052557	4.815596
254.547337	8000.153654	10.602279	-0.052572	4.815629
254.533124	8000.136337	10.607283	-0.052569	4.815624
254.540389	8000.098013	10.612288	-0.052570	4.815612
254.534503	8000.089374	10.617293	-0.052569	4.815610
254.509381	8000.030235	10.622298	-0.052564	4.815593
254.759087	8000.066335	10.627303	-0.052611	4.815602
254.606630	8000.062784	10.632307	-0.052583	4.815602
254.564825	8000.099477	10.637312	-0.052575	4.815613
254.742328	8000.172843	10.642317	-0.052608	4.815633
254.626280	8000.081255	10.647322	-0.052586	4.815607
254.672467	8000.098024	10.652327	-0.052595	4.815612
254.671004	8000.038202	10.657331	-0.052595	4.815594
254.581405	8000.107219	10.662336	-0.052578	4.815615
254.452798	8000.123277	10.667341	-0.052554	4.815620
254.438884	8000.065388	10.672346	-0.052551	4.815603
254.633468	8000.116608	10.677351	-0.052588	4.815617
254.620629	8000.066210	10.682355	-0.052585	4.815603
254.688225	8000.051293	10.687360	-0.052598	4.815598
254.671123	8000.118287	10.692365	-0.052595	4.815618
254.643471	8000.055903	10.697370	-0.052589	4.815600
254.773506	8000.128496	10.702375	-0.052614	4.815620
254.819917	8000.096149	10.707379	-0.052622	4.815611
254.863150	8000.103259	10.712384	-0.052630	4.815612
254.816517	8000.149483	10.717389	-0.052622	4.815626
254.622953	8000.064109	10.722394	-0.052586	4.815602
254.539510	8000.065953	10.727399	-0.052570	4.815603
254.660169	8000.062578	10.732403	-0.052592	4.815601
254.934481	8000.096943	10.737408	-0.052644	4.815610
254.839040	8000.098592	10.742413	-0.052626	4.815611
254.823850	8000.038546	10.747418	-0.052623	4.815594
254.716156	8000.075234	10.752423	-0.052603	4.815605
254.818179	8000.067284	10.757427	-0.052622	4.815602
254.751909	8000.065137	10.762432	-0.052610	4.815602
254.625746	8000.056675	10.767437	-0.052586	4.815600
254.663811	8000.065837	10.772442	-0.052593	4.815602
254.863432	8000.107528	10.777447	-0.052630	4.815614
254.692525	8000.068439	10.782451	-0.052598	4.815603
254.658661	8000.051870	10.787456	-0.052592	4.815598
254.814398	8000.064015	10.792461	-0.052621	4.815601
254.800631	8000.039231	10.797466	-0.052619	4.815594
254.745622	8000.038335	10.802471	-0.052608	4.815594
254.757180	8000.075896	10.807475	-0.052610	4.815605
254.865194	8000.100079	10.812480	-0.052631	4.815611
254.698606	8000.092026	10.817485	-0.052600	4.815610
254.794071	8000.056207	10.822490	-0.052617	4.815599
254.934098	8000.103335	10.827495	-0.052643	4.815612
254.785290	8000.060334	10.832499	-0.052616	4.815600
254.660351	8000.016654	10.837504	-0.052592	4.815588
254.830418	8000.081356	10.842509	-0.052624	4.815606
254.730384	8000.055167	10.847514	-0.052605	4.815599
254.593297	8000.083901	10.852519	-0.052580	4.815608
254.731386	8000.071200	10.857523	-0.052606	4.815604
254.788555	8000.071062	10.862528	-0.052616	4.815603
254.799918	8000.059501	10.867533	-0.052618	4.815600
254.660702	8000.075386	10.872538	-0.052592	4.815605
254.838871	8000.085762	10.877543	-0.052626	4.815607
255.037938	8000.053765	10.882547	-0.052663	4.815597
254.837983	8000.095357	10.887552	-0.052625	4.815610
254.874596	8000.100224	10.892557	-0.052632	4.815611
254.896033	8000.069605	10.897562	-0.052636	4.815602
254.905667	8000.125289	10.902567	-0.052638	4.815619
254.805259	8000.071330	10.907571	-0.052619	4.815603
254.757571	8000.082299	10.912576	-0.052610	4.815607
254.847741	8000.099784	10.917581	-0.052627	4.815611
254.641794	8000.109244	10.922586	-0.052589	4.815615
254.807307	8000.105531	10.927591	-0.052620	4.815613
254.909232	8000.073020	10.932595	-0.052639	4.815603
255.119069	8000.062555	10.937600	-0.052678	4.815599
255.095232	8000.152932	10.942605	-0.052673	4.815626
254.832145	8000.050407	10.947610	-0.052624	4.815597
254.887256	8000.061982	10.952615	-0.052634	4.815600
254.774005	8000.069748	10.957619	-0.052613	4.815603
255.033313	8000.109208	10.962624	-0.052662	4.815613
254.993488	8000.126712	10.967629	-0.052654	4.815619
255.036470	8000.078292	10.972634	-0.052662	4.815604
254.895281	8000.103756	10.977639	-0.052636	4.815612
254.836930	8000.017379	10.982643	-0.052625	4.815587
254.911166	8000.014316	10.987648	-0.052639	4.815586
254.788229	8000.049687	10.992653	-0.052616	4.815597
254.938431	8000.056404	10.997658	-0.052644	4.815598
255.161506	8000.156141	11.002663	-0.052686	4.815626
255.063104	8000.082993	11.007667	-0.052667	4.815606
255.056721	8000.104245	11.012672	-0.052666	4.815612
255.101451	8000.125262	11.017677	-0.052674	4.815618
255.071131	8000.054291	11.022682	-0.052669	4.815597
255.138768	8000.079952	11.027687	-0.052681	4.815604
254.873717	8000.059618	11.032691	-0.052632	4.815600
254.868595	8000.049924	11.037696	-0.052631	4.815597
254.753476	8000.119593	11.042701	-0.052610	4.815618
254.969192	8000.038747	11.047706	-0.052650	4.815593
254.987554	8000.056131	11.052711	-0.052653	4.815598
254.890121	8000.057747	11.057715	-0.052635	4.815599
254.994853	8000.054113	11.062720	-0.052654	4.815597
254.938715	8000.106589	11.067725	-0.052644	4.815613
254.969702	8000.049431	11.072730	-0.052650	4.815596
254.884175	8000.062987	11.077735	-0.052634	4.815601
254.932355	8000.078721	11.082739	-0.052643	4.815605
254.833078	8000.076036	11.087744	-0.052624	4.815605
254.856405	8000.066805	11.092749	-0.052629	4.815602
255.056636	8000.068997	11.097754	-0.052666	4.815601
255.280497	8000.086524	11.102759	-0.052708	4.815606
254.904846	8000.093220	11.107763	-0.052638	4.815609
255.085104	8000.053442	11.112768	-0.052671	4.815597
254.952481	8000.049146	11.117773	-0.052646	4.815596
254.899366	8000.038670	11.122778	-0.052637	4.815593
254.940189	8000.068166	11.127783	-0.052644	4.815602
255.174660	8000.100815	11.132787	-0.052688	4.815610
255.151933	8000.053460	11.137792	-0.052684	4.815596
255.264603	8000.072380	11.142797	-0.052705	4.815601
255.264458	8000.047817	11.147802	-0.052705	4.815594
255.232712	8000.099623	11.152807	-0.052699	4.815610
255.195622	8000.084069	11.157811	-0.052692	4.815605
255.161069	8000.077098	11.162816	-0.052685	4.815603
255.070100	8000.066006	11.167821	-0.052668	4.815601
254.936025	8000.012567	11.172826	-0.052643	4.815586
255.022843	8000.052421	11.177831	-0.052659	4.815597
254.960989	8000.016176	11.182835	-0.052648	4.815587
254.859762	8000.054036	11.187840	-0.052629	4.815598
254.977940	8000.063435	11.192845	-0.052651	4.815600
255.069649	8000.045707	11.197850	-0.052668	4.815595
255.084657	8000.100410	11.202855	-0.052671	4.815611
254.857307	8000.049723	11.207859	-0.052629	4.815597
254.946014	8000.028743	11.212864	-0.052645	4.815590
254.970138	8000.031270	11.217869	-0.052650	4.815591
254.933325	8000.018925	11.222874	-0.052643	4.815587
254.892261	8000.075918	11.227879	-0.052635	4.815604
255.126166	8000.127779	11.232883	-0.052679	4.815618
254.865947	8000.111794	11.237888	-0.052630	4.815615
254.985885	8000.157528	11.242893	-0.052653	4.815628
255.002311	8000.099064	11.247898	-0.052656	4.815611
255.150732	8000.083328	11.252903	-0.052683	4.815605
254.948160	8000.071486	11.257907	-0.052645	4.815603
255.095989	8000.045061	11.262912	-0.052673	4.815594
255.297059	8000.107066	11.267917	-0.052710	4.815611
255.326325	8000.040269	11.272922	-0.052716	4.815592
255.423330	8000.088833	11.277927	-0.052734	4.815606
255.143481	8000.037290	11.282931	-0.052682	4.815592
254.889271	8000.018201	11.287936	-0.052634	4.815587
255.020051	8000.050229	11.292941	-0.052659	4.815596
254.941409	8000.042541	11.297946	-0.052644	4.815594
255.204284	8000.066042	11.302951	-0.052693	4.815600
255.140821	8000.070347	11.307955	-0.052681	4.815601
255.127821	8000.080813	11.312960	-0.052679	4.815605
255.477269	8000.130286	11.317965	-0.052744	4.815617
255.253396	8000.066840	11.322970	-0.052702	4.815600
255.244445	8000.080575	11.327975	-0.052701	4.815604
255.102193	8000.043020	11.332979	-0.052674	4.815594
255.175863	8000.036744	11.337984	-0.052688	4.815592
255.022078	8000.128208	11.342989	-0.052659	4.815619
255.187804	8000.071108	11.347994	-0.052690	4.815601
255.247320	8000.111587	11.352999	-0.052701	4.815613
255.109002	8000.102927	11.358003	-0.052675	4.815611
255.113370	8000.076301	11.363008	-0.052676	4.815603
255.304455	8000.131737	11.368013	-0.052712	4.815619
255.226696	8000.081350	11.373018	-0.052697	4.815604
255.208123	8000.097064	11.378023	-0.052694	4.815609
255.110372	8000.054894	11.383027	-0.052676	4.815597
255.265013	8000.051005	11.388032	-0.052704	4.815595
255.075503	8000.094903	11.393037	-0.052669	4.815609
254.896022	8000.042859	11.398042	-0.052636	4.815595
255.222248	8000.087681	11.403047	-0.052696	4.815606
255.042629	8000.060195	11.408051	-0.052663	4.815599
255.022147	8000.067336	11.413056	-0.052659	4.815601
255.023911	8000.118620	11.418061	-0.052659	4.815616
255.034368	8000.066466	11.423066	-0.052661	4.815601
255.021963	8000.123926	11.428071	-0.052659	4.815618
255.132096	8000.066989	11.433075	-0.052680	4.815601
255.160883	8000.106967	11.438080	-0.052685	4.815612
255.060079	8000.143767	11.443085	-0.052666	4.815623
255.085049	8000.099324	11.448090	-0.052671	4.815610
255.325186	8000.152355	11.453095	-0.052716	4.815625
255.156565	8000.118641	11.458099	-0.052684	4.815616
255.081822	8000.089659	11.463104	-0.052670	4.815607
255.291028	8000.147526	11.468109	-0.052709	4.815623
255.201304	8000.072383	11.473114	-0.052692	4.815602
255.158343	8000.087701	11.478119	-0.052684	4.815606
255.117787	8000.066751	11.483123	-0.052677	4.815601
255.087744	8000.058786	11.488128	-0.052671	4.815598
255.356689	8000.069573	11.493133	-0.052721	4.815600
255.051384	8000.030430	11.498138	-0.052664	4.815590
255.271031	8000.084194	11.503143	-0.052705	4.815605
255.303505	8000.118893	11.508147	-0.052711	4.815615
255.334385	8000.092700	11.513152	-0.052717	4.815607
255.562856	8000.102828	11.518157	-0.052760	4.815609
255.288718	8000.096226	11.523162	-0.052709	4.815608
255.180002	8000.102998	11.528167	-0.052688	4.815611
255.414611	8000.133515	11.533171	-0.052732	4.815619
255.179450	8000.083767	11.538176	-0.052688	4.815605
255.396825	8000.142835	11.543181	-0.052729	4.815621
255.289879	8000.130414	11.548186	-0.052709	4.815618
255.433772	8000.113536	11.553191	-0.052736	4.815613
255.252918	8000.131946	11.558195	-0.052702	4.815619
255.205453	8000.086324	11.563200	-0.052693	4.815606
255.434396	8000.156258	11.568205	-0.052736	4.815625
255.357835	8000.122975	11.573210	-0.052721	4.815616
255.273550	8000.110924	11.578215	-0.052706	4.815613
255.475019	8000.133426	11.583219	-0.052743	4.815618
255.575234	8000.065648	11.588224	-0.052762	4.815598
255.577821	8000.098793	11.593229	-0.052762	4.815608
255.230897	8000.071785	11.598234	-0.052698	4.815601
255.343174	8000.098173	11.603239	-0.052719	4.815609
255.491161	8000.071751	11.608243	-0.052746	4.815600
255.235302	8000.134857	11.613248	-0.052699	4.815620
255.255628	8000.159748	11.618253	-0.052702	4.815627
255.389251	8000.060480	11.623258	-0.052727	4.815597
255.434045	8000.130618	11.628263	-0.052736	4.815618
255.392090	8000.187598	11.633267	-0.052728	4.815635
255.492529	8000.115552	11.638272	-0.052746	4.815613
255.600948	8000.144014	11.643277	-0.052767	4.815621
255.498456	8000.109241	11.648282	-0.052748	4.815611
255.424443	8000.126188	11.653287	-0.052734	4.815616
255.528962	8000.116144	11.658291	-0.052753	4.815613
255.639483	8000.075230	11.663296	-0.052774	4.815601
255.552507	8000.090898	11.668301	-0.052758	4.815606
255.436419	8000.078328	11.673306	-0.052736	4.815602
255.380520	8000.144691	11.678311	-0.052726	4.815622
255.530355	8000.114028	11.683315	-0.052753	4.815612
255.440954	8000.081604	11.688320	-0.052737	4.815603
255.450015	8000.121261	11.693325	-0.052738	4.815615
255.246320	8000.063483	11.698330	-0.052701	4.815599
255.419011	8000.097263	11.703335	-0.052733	4.815608
255.324950	8000.071170	11.708339	-0.052715	4.815601
255.375227	8000.057039	11.713344	-0.052724	4.815596
255.486437	8000.088749	11.718349	-0.052745	4.815605
255.526126	8000.068038	11.723354	-0.052753	4.815599
255.468150	8000.099128	11.728359	-0.052742	4.815608
255.401638	8000.151436	11.733363	-0.052729	4.815624
255.335252	8000.085217	11.738368	-0.052717	4.815605
255.567432	8000.150933	11.743373	-0.052760	4.815623
255.504736	8000.115740	11.748378	-0.052749	4.815613
255.379273	8000.116899	11.753383	-0.052725	4.815614
255.628664	8000.093197	11.758387	-0.052772	4.815606
255.452128	8000.060422	11.763392	-0.052739	4.815597
255.494433	8000.100620	11.768397	-0.052747	4.815609
255.641851	8000.101953	11.773402	-0.052774	4.815608
255.683307	8000.100492	11.778407	-0.052782	4.815608
255.617955	8000.188059	11.783411	-0.052770	4.815634
255.521802	8000.130964	11.788416	-0.052752	4.815617
255.496647	8000.186081	11.793421	-0.052747	4.815634
255.282866	8000.075815	11.798426	-0.052707	4.815602
255.497778	8000.127367	11.803431	-0.052747	4.815616
255.380186	8000.140401	11.808435	-0.052725	4.815621
255.343279	8000.124850	11.813440	-0.052718	4.815616
255.353845	8000.191227	11.818445	-0.052720	4.815636
255.363962	8000.198867	11.823450	-0.052722	4.815638
255.367821	8000.182911	11.828455	-0.052723	4.815633
255.335375	8000.172772	11.833459	-0.052717	4.815631
255.372759	8000.129599	11.838464	-0.052724	4.815618
255.698027	8000.141304	11.843469	-0.052784	4.815620
255.424507	8000.122966	11.848474	-0.052734	4.815616
255.424837	8000.119767	11.853479	-0.052734	4.815615
255.522354	8000.119219	11.858483	-0.052752	4.815614
255.554525	8000.090911	11.863488	-0.052758	4.815606
255.624401	8000.218055	11.868493	-0.052771	4.815642
255.486669	8000.079126	11.873498	-0.052745	4.815602
255.609616	8000.111028	11.878503	-0.052768	4.815611
255.498980	8000.112429	11.883507	-0.052747	4.815612
255.507312	8000.091207	11.888512	-0.052749	4.815606
255.481434	8000.180484	11.893517	-0.052744	4.815632
255.437877	8000.118907	11.898522	-0.052736	4.815614
255.531711	8000.092671	11.903527	-0.052753	4.815606
255.755770	8000.120881	11.908531	-0.052795	4.815613
255.575900	8000.120086	11.913536	-0.052762	4.815614
255.559876	8000.133707	11.918541	-0.052759	4.815618
255.486545	8000.143190	11.923546	-0.052745	4.815621
255.548729	8000.102556	11.928551	-0.052757	4.815609
255.418903	8000.122866	11.933555	-0.052732	4.815616
255.568892	8000.115698	11.938560	-0.052760	4.815613
255.580734	8000.131908	11.943565	-0.052763	4.815617
255.382907	8000.156449	11.948570	-0.052726	4.815626
255.443240	8000.143549	11.953575	-0.052737	4.815621
255.483341	8000.147406	11.958579	-0.052744	4.815622
255.349663	8000.085429	11.963584	-0.052719	4.815605
255.528207	8000.160950	11.968589	-0.052753	4.815626
255.602415	8000.113037	11.973594	-0.052767	4.815612
255.589415	8000.138453	11.978599	-0.052764	4.815619
255.447115	8000.182052	11.983603	-0.052738	4.815633
255.304725	8000.116729	11.988608	-0.052711	4.815614
255.333037	8000.135343	11.993613	-0.052716	4.815620
255.200037	8000.074445	11.998618	-0.052692	4.815602
255.206168	8000.105512	12.003623	-0.052693	4.815611
255.487658	8000.102621	12.008627	-0.052745	4.815609
255.575032	8000.088027	12.013632	-0.052761	4.815605
255.622517	8000.152870	12.018637	-0.052770	4.815623
255.627379	8000.074996	12.023642	-0.052771	4.815601
255.585466	8000.127705	12.028647	-0.052763	4.815616
255.356346	8000.193382	12.033651	-0.052721	4.815636
255.446609	8000.131849	12.038656	-0.052737	4.815618
255.493896	8000.141162	12.043661	-0.052746	4.815621
255.301043	8000.136952	12.048666	-0.052710	4.815620
255.421703	8000.141053	12.053671	-0.052733	4.815621
255.561947	8000.156151	12.058675	-0.052759	4.815625
255.615198	8000.107897	12.063680	-0.052769	4.815610
255.583389	8000.125532	12.068685	-0.052763	4.815616
255.351143	8000.051271	12.073690	-0.052720	4.815595
255.539215	8000.076758	12.078695	-0.052755	4.815601
255.541420	8000.054369	12.083699	-0.052755	4.815595
255.367845	8000.059016	12.088704	-0.052723	4.815597
255.638107	8000.060214	12.093709	-0.052773	4.815596
255.683350	8000.069493	12.098714	-0.052781	4.815599
255.487702	8000.078052	12.103719	-0.052745	4.815602
255.499305	8000.132701	12.108723	-0.052747	4.815618
255.446785	8000.079521	12.113728	-0.052737	4.815603
255.554750	8000.102635	12.118733	-0.052757	4.815609
255.418674	8000.186914	12.123738	-0.052732	4.815634
255.552095	8000.107930	12.128743	-0.052757	4.815611
255.649343	8000.116989	12.133747	-0.052775	4.815613
255.555432	8000.085559	12.138752	-0.052758	4.815604
255.524098	8000.132033	12.143757	-0.052752	4.815618
255.468782	8000.061722	12.148762	-0.052741	4.815597
255.499669	8000.070767	12.153767	-0.052747	4.815600
255.553763	8000.133583	12.158771	-0.052757	4.815618
255.622552	8000.039665	12.163776	-0.052770	4.815590
255.572222	8000.086897	12.168781	-0.052761	4.815604
255.303418	8000.143385	12.173786	-0.052711	4.815622
255.334765	8000.103317	12.178791	-0.052716	4.815610
255.431802	8000.082473	12.183795	-0.052734	4.815604
255.401479	8000.064893	12.188800	-0.052729	4.815599
255.536607	8000.111943	12.193805	-0.052754	4.815612
255.513521	8000.084870	12.198810	-0.052750	4.815604
255.487089	8000.055608	12.203815	-0.052745	4.815596
255.372123	8000.096448	12.208819	-0.052723	4.815608
255.465688	8000.049919	12.213824	-0.052741	4.815594
255.494978	8000.141162	12.218829	-0.052746	4.815621
255.360375	8000.081306	12.223834	-0.052721	4.815604
255.401610	8000.120419	12.228839	-0.052729	4.815615
255.470595	8000.165324	12.233843	-0.052742	4.815628
255.457340	8000.083951	12.238848	-0.052739	4.815604
255.583427	8000.124447	12.243853	-0.052763	4.815615
255.429723	8000.095247	12.248858	-0.052734	4.815607
255.539264	8000.109844	12.253863	-0.052754	4.815611
255.477688	8000.129130	12.258867	-0.052743	4.815617
255.554164	8000.039609	12.263872	-0.052757	4.815591
255.478753	8000.104586	12.268877	-0.052743	4.815610
255.314320	8000.124332	12.273882	-0.052713	4.815616
255.457823	8000.098905	12.278887	-0.052739	4.815608
255.556530	8000.147497	12.283891	-0.052758	4.815622
255.435999	8000.101752	12.288896	-0.052735	4.815609
255.514134	8000.107295	12.293901	-0.052750	4.815611
255.628952	8000.126251	12.298906	-0.052771	4.815616
255.527553	8000.108581	12.303911	-0.052752	4.815611
255.343450	8000.111989	12.308915	-0.052718	4.815613
255.378585	8000.097611	12.313920	-0.052724	4.815608
255.461372	8000.136333	12.318925	-0.052740	4.815619
255.310198	8000.140277	12.323930	-0.052712	4.815621
255.429821	8000.126207	12.328935	-0.052734	4.815616
255.605427	8000.157899	12.333939	-0.052767	4.815625
255.472801	8000.117296	12.338944	-0.052742	4.815614
255.467387	8000.168464	12.343949	-0.052741	4.815629
255.492919	8000.188100	12.348954	-0.052746	4.815634
255.600315	8000.119372	12.353959	-0.052766	4.815614
255.594586	8000.140635	12.358963	-0.052765	4.815620
255.758886	8000.116615	12.363968	-0.052795	4.815612
255.817033	8000.144258	12.368973	-0.052806	4.815620
255.483350	8000.129211	12.373978	-0.052744	4.815617
255.589025	8000.148017	12.378983	-0.052764	4.815622
255.658358	8000.153417	12.383987	-0.052776	4.815623
255.649527	8000.095609	12.388992	-0.052775	4.815606
255.437413	8000.220295	12.393997	-0.052735	4.815644
255.377266	8000.197958	12.399002	-0.052724	4.815638
255.398007	8000.126750	12.404007	-0.052728	4.815617
255.440342	8000.173356	12.409011	-0.052736	4.815630
255.367804	8000.188191	12.414016	-0.052722	4.815635
255.632984	8000.189307	12.419021	-0.052772	4.815634
255.572665	8000.178714	12.424026	-0.052761	4.815631
255.567531	8000.119898	12.429031	-0.052760	4.815614
255.576271	8000.169161	12.434035	-0.052761	4.815628
255.475474	8000.158975	12.439040	-0.052742	4.815626
255.490822	8000.138936	12.444045	-0.052745	4.815620
255.713684	8000.135091	12.449050	-0.052787	4.815618
255.687259	8000.073793	12.454055	-0.052782	4.815600
255.581036	8000.154286	12.459059	-0.052762	4.815624
255.785784	8000.175775	12.464064	-0.052800	4.815629
255.819774	8000.219042	12.469069	-0.052806	4.815642
255.833921	8000.175490	12.474074	-0.052809	4.815629
255.682088	8000.113216	12.479079	-0.052781	4.815611
255.889898	8000.128348	12.484083	-0.052819	4.815615
255.714563	8000.081709	12.489088	-0.052787	4.815602
255.772100	8000.133902	12.494093	-0.052798	4.815617
255.658100	8000.168351	12.499098	-0.052776	4.815628
255.708709	8000.118987	12.504103	-0.052786	4.815613
255.587980	8000.152258	12.509107	-0.052763	4.815623
255.447087	8000.138216	12.514112	-0.052737	4.815620
255.629721	8000.167887	12.519117	-0.052771	4.815628
255.607945	8000.103461	12.524122	-0.052767	4.815609
255.766160	8000.118852	12.529127	-0.052796	4.815613
255.840268	8000.144620	12.534131	-0.052810	4.815620
255.529732	8000.133153	12.539136	-0.052752	4.815618
255.590461	8000.134142	12.544141	-0.052764	4.815618
255.728770	8000.185516	12.549146	-0.052789	4.815632
255.760346	8000.147587	12.554151	-0.052795	4.815621
255.719506	8000.222738	12.559155	-0.052788	4.815643
255.712168	8000.135055	12.564160	-0.052786	4.815618
255.869706	8000.186742	12.569165	-0.052816	4.815632
255.752501	8000.096200	12.574170	-0.052794	4.815606
255.581741	8000.164964	12.579175	-0.052762	4.815627
255.724297	8000.170489	12.584179	-0.052789	4.815628
255.811462	8000.073667	12.589184	-0.052805	4.815599
255.959595	8000.132676	12.594189	-0.052832	4.815616
255.884172	8000.103682	12.599194	-0.052818	4.815608
255.884064	8000.135715	12.604199	-0.052818	4.815617
255.878362	8000.156979	12.609203	-0.052817	4.815623
255.814027	8000.126031	12.614208	-0.052805	4.815615
255.976063	8000.127602	12.619213	-0.052835	4.815614
255.953164	8000.121889	12.624218	-0.052831	4.815613
255.521284	8000.108446	12.629223	-0.052751	4.815611
255.553010	8000.162354	12.634227	-0.052757	4.815626
255.888326	8000.102678	12.639232	-0.052819	4.815607
255.828501	8000.138010	12.644237	-0.052808	4.815618
255.593487	8000.158741	12.649242	-0.052764	4.815625
255.634564	8000.123103	12.654247	-0.052772	4.815615
255.762219	8000.164692	12.659251	-0.052796	4.815626
255.734036	8000.156758	12.664256	-0.052790	4.815624
255.813574	8000.187953	12.669261	-0.052805	4.815633
255.561153	8000.166754	12.674266	-0.052758	4.815628
255.614614	8000.125979	12.679271	-0.052768	4.815616
255.695025	8000.147577	12.684275	-0.052783	4.815621
255.512991	8000.098694	12.689280	-0.052749	4.815608
255.548755	8000.151601	12.694285	-0.052756	4.815623
255.567981	8000.213849	12.699290	-0.052759	4.815641
255.585275	8000.139380	12.704295	-0.052763	4.815620
255.560487	8000.209454	12.709299	-0.052758	4.815640
255.506140	8000.131683	12.714304	-0.052748	4.815618
255.894367	8000.134804	12.719309	-0.052820	4.815617
255.827828	8000.149737	12.724314	-0.052808	4.815621
255.591709	8000.111719	12.729319	-0.052764	4.815611
255.542067	8000.134402	12.734323	-0.052754	4.815618
255.603081	8000.084139	12.739328	-0.052766	4.815603
255.660610	8000.123518	12.744333	-0.052776	4.815615
255.546367	8000.167574	12.749338	-0.052755	4.815628
255.777113	8000.141433	12.754343	-0.052798	4.815619
255.883305	8000.177334	12.759347	-0.052818	4.815629
255.726802	8000.199344	12.764352	-0.052789	4.815636
255.847380	8000.174612	12.769357	-0.052811	4.815629
255.595247	8000.116043	12.774362	-0.052764	4.815613
255.695837	8000.120885	12.779367	-0.052783	4.815614
255.826515	8000.174270	12.784371	-0.052807	4.815629
255.889609	8000.150737	12.789376	-0.052819	4.815621
255.890969	8000.152894	12.794381	-0.052819	4.815622
255.621026	8000.145293	12.799386	-0.052769	4.815621
255.944539	8000.134545	12.804391	-0.052829	4.815616
255.707133	8000.164848	12.809395	-0.052785	4.815626
255.610943	8000.088531	12.814400	-0.052767	4.815605
255.559845	8000.100512	12.819405	-0.052758	4.815608
255.651075	8000.144712	12.824410	-0.052775	4.815621
255.476350	8000.095948	12.829415	-0.052742	4.815607
255.503503	8000.154053	12.834419	-0.052747	4.815624
255.547286	8000.131273	12.839424	-0.052755	4.815617
255.755713	8000.142143	12.844429	-0.052794	4.815620
255.605314	8000.149303	12.849434	-0.052766	4.815622
255.765089	8000.145498	12.854439	-0.052796	4.815621
255.781594	8000.154309	12.859443	-0.052799	4.815623
255.701373	8000.148731	12.864448	-0.052784	4.815622
255.788857	8000.148020	12.869453	-0.052800	4.815621
255.905423	8000.184090	12.874458	-0.052822	4.815631
255.706043	8000.143466	12.879463	-0.052785	4.815620
255.682987	8000.167650	12.884467	-0.052781	4.815627
255.774908	8000.059159	12.889472	-0.052798	4.815595
255.947506	8000.119634	12.894477	-0.052830	4.815612
255.561710	8000.113349	12.899482	-0.052758	4.815612
255.624729	8000.156021	12.904487	-0.052770	4.815624
255.806080	8000.245471	12.909491	-0.052803	4.815650
255.720020	8000.171454	12.914496	-0.052787	4.815628
255.675562	8000.187815	12.919501	-0.052779	4.815633
255.730598	8000.213272	12.924506	-0.052789	4.815641
255.798060	8000.117196	12.929511	-0.052802	4.815612
255.529221	8000.183294	12.934515	-0.052752	4.815633
255.416527	8000.144083	12.939520	-0.052731	4.815622
255.649385	8000.195929	12.944525	-0.052774	4.815636
255.666466	8000.182325	12.949530	-0.052777	4.815632
255.577375	8000.136023	12.954535	-0.052761	4.815619
255.834614	8000.227777	12.959539	-0.052809	4.815644
255.766739	8000.138039	12.964544	-0.052796	4.815618
255.782360	8000.107325	12.969549	-0.052799	4.815609
255.721585	8000.159727	12.974554	-0.052788	4.815625
255.738808	8000.127972	12.979559	-0.052791	4.815616
255.573586	8000.186147	12.984563	-0.052760	4.815633
255.752171	8000.130324	12.989568	-0.052793	4.815616
255.954725	8000.097317	12.994573	-0.052831	4.815606
255.673915	8000.140795	12.999578	-0.052779	4.815620
255.701707	8000.106008	13.004583	-0.052784	4.815609
255.834859	8000.178655	13.009587	-0.052809	4.815630
255.754922	8000.136774	13.014592	-0.052794	4.815618
255.632513	8000.171086	13.019597	-0.052771	4.815629
255.841494	8000.210797	13.024602	-0.052810	4.815639
255.829733	8000.181773	13.029607	-0.052808	4.815631
255.808720	8000.168616	13.034611	-0.052804	4.815627
255.855086	8000.178981	13.039616	-0.052812	4.815630
255.944010	8000.200719	13.044621	-0.052829	4.815636
255.839089	8000.223570	13.049626	-0.052809	4.815643
255.787396	8000.143706	13.054631	-0.052800	4.815620
255.731789	8000.216481	13.059635	-0.052789	4.815641
255.632129	8000.143311	13.064640	-0.052771	4.815621
255.754776	8000.118612	13.069645	-0.052794	4.815613
255.646824	8000.146753	13.074650	-0.052774	4.815621
255.722874	8000.104210	13.079655	-0.052788	4.815609
255.768338	8000.199988	13.084659	-0.052796	4.815636
255.778600	8000.158509	13.089664	-0.052798	4.815624
255.845381	8000.114747	13.094669	-0.052810	4.815611
255.866436	8000.133243	13.099674	-0.052814	4.815616
255.663700	8000.108582	13.104679	-0.052777	4.815610
255.979594	8000.178867	13.109683	-0.052835	4.815629
256.027468	8000.155086	13.114688	-0.052844	4.815622
255.912293	8000.240773	13.119693	-0.052823	4.815648
255.797945	8000.239977	13.124698	-0.052802	4.815648
255.822888	8000.128259	13.129703	-0.052806	4.815615
255.949009	8000.196520	13.134707	-0.052830	4.815635
255.805537	8000.125839	13.139712	-0.052803	4.815615
255.824070	8000.131480	13.144717	-0.052806	4.815616
255.965268	8000.188241	13.149722	-0.052833	4.815632
256.001769	8000.120492	13.154727	-0.052840	4.815612
255.963249	8000.101710	13.159731	-0.052832	4.815607
255.906560	8000.101854	13.164736	-0.052822	4.815607
255.810198	8000.149405	13.169741	-0.052804	4.815621
255.979842	8000.162847	13.174746	-0.052835	4.815625
255.769011	8000.130580	13.179751	-0.052796	4.815616
255.842206	8000.215064	13.184755	-0.052810	4.815641
255.912606	8000.207668	13.189760	-0.052823	4.815638
255.960180	8000.209510	13.194765	-0.052832	4.815638
255.932805	8000.202657	13.199770	-0.052827	4.815636
255.809643	8000.130171	13.204775	-0.052804	4.815616
256.027389	8000.240504	13.209779	-0.052844	4.815647
256.066607	8000.174935	13.214784	-0.052852	4.815628
255.979705	8000.139347	13.219789	-0.052835	4.815618
255.809150	8000.149382	13.224794	-0.052804	4.815621
255.945314	8000.139854	13.229799	-0.052829	4.815618
256.124621	8000.147046	13.234803	-0.052862	4.815619
255.860768	8000.136340	13.239808	-0.052813	4.815617
255.950456	8000.179447	13.244813	-0.052830	4.815630
255.834528	8000.150861	13.249818	-0.052808	4.815622
255.704432	8000.150877	13.254823	-0.052784	4.815622
255.776385	8000.208645	13.259827	-0.052797	4.815639
255.842094	8000.141372	13.264832	-0.052810	4.815619
255.774403	8000.171237	13.269837	-0.052797	4.815628
255.716179	8000.138252	13.274842	-0.052786	4.815619
255.861977	8000.071217	13.279847	-0.052813	4.815598
255.975466	8000.117915	13.284851	-0.052834	4.815611
255.705557	8000.123128	13.289856	-0.052784	4.815614
255.866867	8000.152451	13.294861	-0.052814	4.815622
256.073461	8000.223092	13.299866	-0.052853	4.815642
255.723977	8000.164004	13.304871	-0.052788	4.815626
255.855472	8000.261185	13.309875	-0.052812	4.815654
255.806402	8000.240096	13.314880	-0.052803	4.815648
255.964385	8000.179666	13.319885	-0.052832	4.815630
256.008617	8000.155826	13.324890	-0.052841	4.815622
256.065225	8000.099083	13.329895	-0.052851	4.815606
256.115962	8000.177863	13.334899	-0.052861	4.815628
256.014723	8000.099327	13.339904	-0.052842	4.815606
256.201777	8000.138682	13.344909	-0.052877	4.815616
256.253139	8000.173690	13.349914	-0.052886	4.815626
255.898907	8000.146560	13.354919	-0.052820	4.815620
256.245084	8000.202390	13.359923	-0.052885	4.815635
256.175573	8000.175628	13.364928	-0.052872	4.815627
256.177202	8000.175654	13.369933	-0.052872	4.815627
256.148518	8000.153829	13.374938	-0.052867	4.815621
256.191504	8000.096864	13.379943	-0.052875	4.815604
256.231219	8000.150904	13.384947	-0.052882	4.815620
255.846875	8000.163862	13.389952	-0.052810	4.815626
256.022653	8000.153912	13.394957	-0.052843	4.815622
256.139642	8000.136596	13.399962	-0.052865	4.815616
255.918302	8000.060375	13.404967	-0.052824	4.815595
255.900489	8000.135902	13.409971	-0.052820	4.815617
256.050759	8000.108450	13.414976	-0.052848	4.815608
256.042605	8000.118995	13.419981	-0.052847	4.815611
255.923257	8000.176850	13.424986	-0.052825	4.815629
256.033311	8000.112435	13.429991	-0.052845	4.815610
256.126341	8000.121426	13.434995	-0.052862	4.815612
255.896281	8000.088845	13.440000	-0.052820	4.815603
255.884647	8000.113215	13.445005	-0.052817	4.815611
255.882743	8000.142016	13.450010	-0.052817	4.815619
255.917106	8000.071029	13.455015	-0.052823	4.815598
255.941418	8000.132292	13.460019	-0.052828	4.815616
256.104850	8000.124276	13.465024	-0.052858	4.815613
256.140056	8000.126985	13.470029	-0.052865	4.815613
255.968715	8000.159432	13.475034	-0.052833	4.815624
256.001663	8000.103372	13.480039	-0.052839	4.815607
256.067202	8000.219768	13.485043	-0.052851	4.815641
255.883271	8000.166581	13.490048	-0.052817	4.815626
255.841361	8000.121048	13.495053	-0.052809	4.815613
255.985998	8000.145829	13.500058	-0.052836	4.815620
255.945330	8000.141962	13.505063	-0.052829	4.815619
255.797903	8000.183342	13.510067	-0.052801	4.815631
255.990769	8000.126684	13.515072	-0.052837	4.815614
255.998629	8000.127879	13.520077	-0.052839	4.815614
255.937685	8000.146107	13.525082	-0.052827	4.815620
255.999761	8000.128964	13.530087	-0.052839	4.815615
256.160738	8000.156148	13.535091	-0.052869	4.815622
255.982581	8000.069952	13.540096	-0.052835	4.815597
255.904471	8000.090036	13.545101	-0.052821	4.815604
256.160299	8000.135850	13.550106	-0.052869	4.815616
256.196616	8000.142848	13.555111	-0.052875	4.815618
256.292977	8000.158300	13.560115	-0.052893	4.815622
256.192704	8000.155598	13.565120	-0.052875	4.815621
256.155127	8000.144306	13.570125	-0.052868	4.815618
256.251383	8000.174706	13.575130	-0.052886	4.815627
256.099988	8000.114575	13.580135	-0.052857	4.815610
256.347872	8000.162396	13.585139	-0.052904	4.815623
256.148477	8000.140992	13.590144	-0.052866	4.815617
256.213476	8000.127101	13.595149	-0.052878	4.815613
256.025489	8000.192380	13.600154	-0.052843	4.815633
255.939586	8000.103416	13.605159	-0.052827	4.815607
256.093756	8000.159320	13.610163	-0.052856	4.815623
256.102353	8000.151985	13.615168	-0.052858	4.815621
256.247911	8000.123388	13.620173	-0.052885	4.815612
256.018017	8000.200799	13.625178	-0.052842	4.815636
255.990297	8000.075408	13.630183	-0.052837	4.815599
256.077204	8000.134487	13.635187	-0.052853	4.815616
256.028973	8000.090987	13.640192	-0.052844	4.815603
256.098141	8000.135895	13.645197	-0.052857	4.815616
256.097319	8000.132678	13.650202	-0.052857	4.815615
256.017749	8000.075852	13.655207	-0.052842	4.815599
256.218028	8000.153865	13.660211	-0.052879	4.815621
256.069224	8000.147168	13.665216	-0.052852	4.815620
256.198398	8000.136458	13.670221	-0.052876	4.815616
256.268135	8000.161087	13.675226	-0.052889	4.815623
256.115879	8000.084923	13.680231	-0.052860	4.815601
256.243354	8000.155343	13.685235	-0.052884	4.815621
256.151210	8000.158112	13.690240	-0.052867	4.815622
256.223432	8000.138999	13.695245	-0.052880	4.815616
256.387040	8000.155547	13.700250	-0.052911	4.815621
256.203625	8000.126929	13.705255	-0.052876	4.815613
256.210070	8000.105677	13.710259	-0.052878	4.815607
256.063624	8000.143868	13.715264	-0.052850	4.815619
256.243874	8000.180977	13.720269	-0.052884	4.815629
256.195127	8000.195132	13.725274	-0.052875	4.815633
256.149657	8000.148472	13.730279	-0.052866	4.815620
256.310896	8000.130810	13.735283	-0.052896	4.815614
256.342034	8000.128113	13.740288	-0.052902	4.815613
256.401670	8000.149374	13.745293	-0.052913	4.815619
256.284148	8000.142119	13.750298	-0.052891	4.815617
256.336426	8000.109867	13.755303	-0.052901	4.815607
256.296242	8000.117754	13.760307	-0.052894	4.815610
256.196507	8000.118264	13.765312	-0.052875	4.815611
256.184300	8000.074283	13.770317	-0.052873	4.815598
256.363713	8000.126327	13.775322	-0.052906	4.815612
256.126419	8000.079746	13.780327	-0.052862	4.815600
256.153114	8000.103673	13.785331	-0.052867	4.815606
256.242607	8000.067756	13.790336	-0.052884	4.815596
256.326285	8000.128919	13.795341	-0.052899	4.815613
256.451795	8000.169407	13.800346	-0.052923	4.815624
256.401109	8000.146155	13.805351	-0.052913	4.815618
256.236141	8000.139195	13.810355	-0.052882	4.815616
256.132163	8000.109736	13.815360	-0.052863	4.815608
256.214624	8000.144183	13.820365	-0.052878	4.815618
256.274575	8000.157973	13.825370	-0.052890	4.815622
256.200356	8000.121524	13.830375	-0.052876	4.815611
256.302506	8000.114645	13.835379	-0.052895	4.815609
256.171470	8000.083677	13.840384	-0.052870	4.815601
256.061115	8000.079743	13.845389	-0.052850	4.815600
256.205629	8000.087436	13.850394	-0.052877	4.815601
256.198025	8000.045666	13.855399	-0.052875	4.815589
256.263878	8000.057417	13.860403	-0.052887	4.815592
256.165948	8000.081449	13.865408	-0.052869	4.815600
256.378712	8000.110544	13.870413	-0.052909	4.815607
256.427439	8000.164731	13.875418	-0.052918	4.815623
256.255675	8000.108538	13.880423	-0.052886	4.815607
256.286584	8000.118652	13.885427	-0.052892	4.815610
256.391844	8000.128910	13.890432	-0.052911	4.815613
256.268054	8000.108738	13.895437	-0.052888	4.815607
256.199947	8000.100153	13.900442	-0.052876	4.815605
256.125073	8000.048744	13.905447	-0.052862	4.815591
256.233679	8000.120991	13.910451	-0.052882	4.815611
256.189606	8000.102119	13.915456	-0.052874	4.815606
256.058398	8000.082895	13.920461	-0.052849	4.815601
256.087455	8000.120743	13.925466	-0.052855	4.815612
256.049500	8000.082749	13.930471	-0.052847	4.815601
256.446391	8000.118048	13.935475	-0.052921	4.815609
256.166217	8000.122025	13.940480	-0.052869	4.815612
256.153247	8000.108998	13.945485	-0.052867	4.815608
256.180679	8000.109445	13.950490	-0.052872	4.815608
256.080986	8000.060834	13.955495	-0.052853	4.815594
256.110148	8000.113634	13.960499	-0.052859	4.815610
256.140668	8000.100249	13.965504	-0.052864	4.815606
256.278132	8000.101420	13.970509	-0.052890	4.815605
256.261011	8000.113955	13.975514	-0.052887	4.815609
256.216679	8000.071586	13.980519	-0.052879	4.815597
256.213331	8000.116381	13.985523	-0.052878	4.815610
256.253290	8000.123438	13.990528	-0.052885	4.815612
256.231525	8000.115608	13.995533	-0.052881	4.815610
256.120051	8000.139420	14.000538	-0.052861	4.815617
256.083657	8000.059805	14.005543	-0.052854	4.815594
256.202947	8000.118345	14.010547	-0.052876	4.815611
256.091900	8000.125078	14.015552	-0.052855	4.815613
256.376305	8000.105150	14.020557	-0.052908	4.815606
256.148854	8000.150565	14.025562	-0.052866	4.815620
256.084874	8000.070501	14.030567	-0.052854	4.815597
256.084838	8000.089721	14.035571	-0.052854	4.815603
256.218207	8000.092962	14.040576	-0.052879	4.815603
256.282304	8000.097209	14.045581	-0.052891	4.815604
256.283132	8000.176244	14.050586	-0.052891	4.815627
256.373370	8000.092285	14.055591	-0.052908	4.815602
256.394332	8000.070201	14.060595	-0.052912	4.815596
256.377421	8000.052839	14.065600	-0.052908	4.815591
256.070665	8000.076673	14.070605	-0.052851	4.815599
256.289780	8000.125092	14.075610	-0.052892	4.815612
256.202605	8000.092703	14.080615	-0.052876	4.815603
256.193381	8000.132063	14.085619	-0.052874	4.815615
256.239840	8000.153109	14.090624	-0.052883	4.815621
256.231387	8000.114528	14.095629	-0.052881	4.815609
256.283745	8000.194402	14.100634	-0.052891	4.815632
256.291301	8000.095214	14.105639	-0.052892	4.815603
256.314734	8000.138310	14.110643	-0.052897	4.815616
256.113232	8000.157451	14.115648	-0.052859	4.815622
256.167704	8000.127370	14.120653	-0.052869	4.815613
256.510404	8000.151108	14.125658	-0.052933	4.815619
256.386887	8000.135212	14.130663	-0.052910	4.815615
256.376765	8000.139318	14.135667	-0.052908	4.815616
256.189597	8000.187525	14.140672	-0.052873	4.815631
256.316934	8000.162903	14.145677	-0.052897	4.815623
256.331856	8000.227217	14.150682	-0.052900	4.815642
256.321629	8000.201421	14.155687	-0.052898	4.815634
256.318666	8000.233409	14.160691	-0.052897	4.815644
256.333513	8000.199478	14.165696	-0.052900	4.815634
256.012628	8000.142992	14.170701	-0.052840	4.815619
256.404238	8000.137626	14.175706	-0.052913	4.815615
256.443228	8000.122243	14.180711	-0.052921	4.815611
256.311515	8000.112621	14.185715	-0.052896	4.815608
256.248643	8000.172464	14.190720	-0.052884	4.815626
256.168703	8000.116700	14.195725	-0.052869	4.815610
256.360465	8000.188168	14.200730	-0.052905	4.815630
256.175624	8000.125355	14.205735	-0.052871	4.815613
256.390159	8000.165157	14.210739	-0.052911	4.815623
256.191184	8000.196086	14.215744	-0.052874	4.815633
256.169074	8000.129518	14.220749	-0.052869	4.815614
256.329823	8000.199412	14.225754	-0.052899	4.815634
256.232664	8000.138028	14.230759	-0.052881	4.815616
256.187734	8000.214182	14.235763	-0.052873	4.815639
256.386883	8000.203544	14.240768	-0.052910	4.815635
256.396745	8000.164193	14.245773	-0.052912	4.815623
256.411783	8000.217831	14.250778	-0.052915	4.815639
256.251451	8000.113771	14.255783	-0.052885	4.815609
256.383701	8000.107382	14.260787	-0.052909	4.815606
256.429386	8000.147637	14.265792	-0.052918	4.815618
256.293039	7999.201452	14.270797	-0.052892	4.815342

256.159105	7996.068787	14.275802	-0.052865	4.814427
256.195706	7990.567915	14.280807	-0.052868	4.812818
256.108369	7983.920050	14.285811	-0.052848	4.810873
256.158977	7976.647931	14.290816	-0.052852	4.808744
256.046238	7968.964002	14.295821	-0.052826	4.806494
256.120607	7961.205628	14.300826	-0.052835	4.804221
255.854659	7953.342460	14.305831	-0.052780	4.801917
256.110804	7945.348374	14.310835	-0.052823	4.799572
256.012927	7937.490104	14.315840	-0.052799	4.797266
255.893398	7929.410993	14.320845	-0.052772	4.794895
255.895657	7921.401450	14.325850	-0.052767	4.792543
255.692796	7913.320706	14.330855	-0.052724	4.790169
255.659608	7905.423727	14.335859	-0.052713	4.787848
255.603011	7897.350942	14.340864	-0.052697	4.785473
255.742716	7889.390929	14.345869	-0.052718	4.783130
255.755752	7881.408689	14.350874	-0.052715	4.780780
255.567006	7873.367313	14.355879	-0.052675	4.778412
255.565015	7865.419280	14.360883	-0.052669	4.776069
255.677667	7857.359131	14.365888	-0.052685	4.773692
255.586418	7849.328950	14.370893	-0.052663	4.771324
255.630188	7841.353126	14.375898	-0.052665	4.768969
255.581261	7833.424487	14.380903	-0.052651	4.766628
255.564274	7825.367047	14.385907	-0.052643	4.764248
255.374673	7817.427748	14.390912	-0.052602	4.761901
255.343650	7809.376094	14.395917	-0.052591	4.759520
255.391861	7801.433828	14.400922	-0.052595	4.757170
255.188902	7793.351364	14.405927	-0.052552	4.754778
255.245853	7785.329680	14.410931	-0.052557	4.752402
255.205122	7777.289865	14.415936	-0.052545	4.750019
255.097516	7769.314450	14.420941	-0.052519	4.747655
255.293746	7761.357826	14.425946	-0.052551	4.745294
255.142675	7753.345772	14.430951	-0.052517	4.742917
255.244656	7745.333007	14.435955	-0.052531	4.740537
255.226307	7737.350355	14.440960	-0.052522	4.738166
255.032103	7729.296497	14.445965	-0.052481	4.735773
255.097905	7721.313298	14.450970	-0.052488	4.733398
254.870850	7713.311418	14.455975	-0.052441	4.731018
254.824314	7705.260792	14.460979	-0.052427	4.728622
254.874912	7697.325179	14.465984	-0.052431	4.726258
254.705668	7689.273239	14.470989	-0.052394	4.723859
254.939590	7681.340938	14.475994	-0.052432	4.721493
254.959655	7673.304008	14.480999	-0.052431	4.719096
254.944712	7665.351406	14.486003	-0.052423	4.716723
254.674135	7657.276386	14.491008	-0.052367	4.714312
254.653456	7649.285916	14.496013	-0.052358	4.711925
254.800542	7641.275726	14.501018	-0.052380	4.709531
254.631322	7633.314184	14.506023	-0.052344	4.707150
254.638162	7625.313157	14.511027	-0.052340	4.704756
254.625204	7617.354648	14.516032	-0.052332	4.702374
254.447848	7609.337577	14.521037	-0.052294	4.699973
254.324777	7601.402116	14.526042	-0.052266	4.697595
254.316885	7593.298658	14.531047	-0.052259	4.695166
254.482466	7585.296218	14.536051	-0.052285	4.692765
254.516462	7577.246061	14.541056	-0.052286	4.690349
254.567400	7569.258356	14.546061	-0.052290	4.687950
254.622838	7561.257093	14.551066	-0.052295	4.685546
254.557393	7553.294565	14.556071	-0.052278	4.683153
254.371187	7545.320973	14.561075	-0.052238	4.680755
254.408116	7537.293557	14.566080	-0.052240	4.678340
254.348008	7529.288468	14.571085	-0.052223	4.675930
254.434991	7521.271650	14.576090	-0.052234	4.673515
254.432873	7513.135303	14.581095	-0.052228	4.671063
254.214195	7505.150327	14.586099	-0.052182	4.668655
254.185029	7497.241732	14.591104	-0.052172	4.666270
254.021426	7489.202243	14.596109	-0.052136	4.663843
254.201699	7481.268547	14.601114	-0.052165	4.661447
253.908783	7473.228729	14.606119	-0.052105	4.659018
254.202501	7465.293272	14.611123	-0.052154	4.656619
254.019709	7457.227179	14.616128	-0.052115	4.654179
254.098961	7449.158951	14.621133	-0.052124	4.651738
253.830002	7441.198089	14.626138	-0.052069	4.649327
254.022043	7433.240591	14.631143	-0.052100	4.646917
254.028781	7425.231110	14.636147	-0.052096	4.644489
253.770998	7417.258179	14.641152	-0.052043	4.642071
253.925652	7409.174091	14.646157	-0.052066	4.639618
253.950973	7401.282144	14.651162	-0.052066	4.637222
253.918875	7393.230792	14.656167	-0.052054	4.634777
253.774677	7385.223607	14.661171	-0.052022	4.632344
253.936625	7377.151265	14.666176	-0.052047	4.629889
253.963765	7369.211257	14.671181	-0.052047	4.627474
253.819918	7361.186038	14.676186	-0.052015	4.625031
253.620610	7353.213257	14.681191	-0.051973	4.622603
253.747018	7345.152704	14.686195	-0.051991	4.620147
253.496340	7337.178206	14.691200	-0.051939	4.617716
253.346252	7329.177322	14.696205	-0.051906	4.615275
253.613667	7321.204201	14.701210	-0.051951	4.612842
253.681073	7313.137130	14.706215	-0.051958	4.610379
253.651007	7305.148982	14.711219	-0.051947	4.607938
253.515161	7297.173331	14.716224	-0.051917	4.605500
253.336044	7289.142813	14.721229	-0.051878	4.603044
253.165032	7281.199268	14.726234	-0.051841	4.600614
253.026502	7273.196749	14.731239	-0.051810	4.598163
253.180447	7265.187932	14.736243	-0.051833	4.595710
253.142653	7257.162278	14.741248	-0.051821	4.593250
252.942561	7249.068989	14.746253	-0.051779	4.590768
253.190994	7241.122663	14.751258	-0.051820	4.588330
253.074977	7233.087763	14.756263	-0.051793	4.585864
253.033630	7225.178995	14.761267	-0.051780	4.583434
252.883410	7217.155905	14.766272	-0.051747	4.580969
253.005182	7209.169925	14.771277	-0.051764	4.578513
253.110698	7201.180123	14.776282	-0.051779	4.576055
252.788541	7193.141211	14.781287	-0.051713	4.573580
252.922674	7185.089003	14.786291	-0.051733	4.571101
252.860467	7177.099567	14.791296	-0.051716	4.568639
252.745512	7169.098475	14.796301	-0.051690	4.566172
252.840012	7161.164661	14.801306	-0.051702	4.563724
252.673724	7153.151228	14.806311	-0.051666	4.561251
252.747385	7145.168448	14.811315	-0.051674	4.558786
252.723568	7137.176271	14.816320	-0.051665	4.556316
252.633873	7129.136262	14.821325	-0.051643	4.553830
252.725733	7121.126017	14.826330	-0.051655	4.551353
252.736674	7113.113466	14.831335	-0.051652	4.548873
252.660663	7105.115834	14.836339	-0.051632	4.546396
252.584439	7097.111518	14.841344	-0.051613	4.543916
252.552720	7089.094238	14.846349	-0.051602	4.541431
252.766395	7081.101041	14.851354	-0.051636	4.538952
252.619855	7073.141501	14.856359	-0.051604	4.536481
252.708253	7065.087373	14.861363	-0.051615	4.533981
252.678290	7057.099717	14.866368	-0.051604	4.531499
252.496307	7049.057235	14.871373	-0.051565	4.528999
252.456377	7041.132690	14.876378	-0.051552	4.526534
252.378895	7033.091396	14.881383	-0.051533	4.524031
252.378658	7025.166293	14.886387	-0.051528	4.521563
252.413381	7017.118030	14.891392	-0.051529	4.519056
252.236749	7009.140936	14.896397	-0.051491	4.516569
252.370014	7001.104826	14.901402	-0.051510	4.514063
252.203831	6993.001541	14.906407	-0.051474	4.511534
252.057601	6985.013665	14.911411	-0.051442	4.509040
252.025055	6977.060283	14.916416	-0.051430	4.506555
252.015756	6969.022242	14.921421	-0.051423	4.504042
252.252431	6961.104277	14.926426	-0.051462	4.501566
252.084431	6953.093507	14.931431	-0.051426	4.499059
252.033434	6945.105136	14.936435	-0.051411	4.496558
251.983503	6937.096321	14.941440	-0.051396	4.494049
251.862993	6929.072773	14.946445	-0.051369	4.491533
251.917213	6921.053054	14.951450	-0.051374	4.489018
251.919553	6913.035352	14.956455	-0.051369	4.486502
251.878227	6905.045464	14.961459	-0.051356	4.483993
251.737568	6897.112766	14.966464	-0.051325	4.481501
251.736013	6889.069878	14.971469	-0.051319	4.478972
251.785530	6881.106409	14.976474	-0.051323	4.476468
251.729601	6873.022584	14.981479	-0.051307	4.473924
251.699134	6865.006542	14.986483	-0.051297	4.471400
251.674635	6856.999933	14.991488	-0.051287	4.468877
251.491330	6849.005639	14.996493	-0.051247	4.466356
251.327480	6841.059250	15.001498	-0.051212	4.463849
251.381089	6833.026779	15.006503	-0.051216	4.461315
251.352158	6825.051261	15.011507	-0.051206	4.458796
251.307066	6817.059722	15.016512	-0.051192	4.456271
251.219753	6809.005145	15.021517	-0.051171	4.453725
251.286031	6801.013454	15.026522	-0.051178	4.451197
251.201489	6793.020343	15.031527	-0.051157	4.448667
251.124891	6784.988350	15.036531	-0.051137	4.446123
251.257012	6777.032093	15.041536	-0.051157	4.443603
251.129925	6769.031628	15.046541	-0.051128	4.441066
251.176889	6761.026522	15.051546	-0.051131	4.438527
251.194135	6753.031316	15.056551	-0.051129	4.435989
251.277405	6744.982755	15.061555	-0.051140	4.433433
251.083873	6736.961424	15.066560	-0.051098	4.430884
250.940859	6728.930320	15.071565	-0.051067	4.428330
250.980196	6720.993463	15.076570	-0.051069	4.425805
251.034001	6712.987374	15.081575	-0.051073	4.423257
251.000536	6704.959759	15.086579	-0.051062	4.420700
251.097774	6697.029819	15.091584	-0.051075	4.418173
250.989528	6688.952902	15.096589	-0.051050	4.415597
251.076433	6680.973568	15.101594	-0.051061	4.413052
250.927375	6672.947795	15.106599	-0.051028	4.410489
250.856919	6664.972396	15.111603	-0.051009	4.407941
250.823554	6656.983466	15.116608	-0.050998	4.405387
250.945329	6648.974196	15.121613	-0.051015	4.402827
251.099867	6641.012897	15.126618	-0.051039	4.400280
250.679286	6633.018040	15.131623	-0.050955	4.397718
250.781875	6624.966522	15.136627	-0.050969	4.395140
250.950958	6616.988662	15.141632	-0.050995	4.392583
250.808202	6608.943925	15.146637	-0.050964	4.390002
250.628407	6600.987303	15.151642	-0.050925	4.387448
250.789235	6592.995325	15.156647	-0.050950	4.384882
250.914980	6585.019285	15.161651	-0.050968	4.382321
250.621230	6576.985576	15.166656	-0.050908	4.379736
250.452137	6569.002962	15.171661	-0.050871	4.377167
250.471473	6560.994466	15.176666	-0.050870	4.374590
250.217526	6553.025851	15.181671	-0.050817	4.372022
250.317409	6544.961383	15.186675	-0.050830	4.369424
250.218652	6537.017762	15.191680	-0.050807	4.366862
250.023154	6528.974303	15.196685	-0.050765	4.364266
250.244892	6521.012660	15.201690	-0.050801	4.361697
250.251012	6512.985473	15.206695	-0.050797	4.359104
250.421816	6505.039944	15.211699	-0.050824	4.356537
250.203578	6496.951467	15.216704	-0.050778	4.353920
250.106862	6488.836551	15.221709	-0.050755	4.351293
250.458570	6480.882235	15.226714	-0.050815	4.348720
250.236421	6472.953022	15.231719	-0.050768	4.346150
250.060881	6464.940973	15.236723	-0.050730	4.343552
250.000441	6456.970824	15.241728	-0.050714	4.340966
249.966591	6448.955848	15.246733	-0.050702	4.338364
249.925742	6440.987177	15.251738	-0.050690	4.335776
250.061584	6432.948391	15.256743	-0.050710	4.333165
249.979382	6424.960438	15.261747	-0.050689	4.330567
249.772284	6416.967598	15.266752	-0.050645	4.327965
249.606399	6408.891495	15.271757	-0.050609	4.325335
249.817687	6400.981522	15.276762	-0.050643	4.322760
249.718320	6392.912757	15.281767	-0.050620	4.320129
249.731797	6384.976533	15.286771	-0.050617	4.317541
249.714023	6376.972144	15.291776	-0.050608	4.314929
249.699415	6368.916150	15.296781	-0.050601	4.312298
249.703167	6360.914329	15.301786	-0.050596	4.309684
249.674123	6352.933418	15.306791	-0.050585	4.307075
249.792642	6344.888979	15.311795	-0.050602	4.304444
249.651304	6336.977692	15.316800	-0.050571	4.301853
249.565622	6328.921233	15.321805	-0.050550	4.299214
249.534153	6321.004629	15.326810	-0.050538	4.296619
249.363478	6312.957286	15.331815	-0.050501	4.293979
249.261562	6304.868564	15.336819	-0.050477	4.291324
249.353451	6296.932160	15.341824	-0.050489	4.288719
249.355341	6288.885958	15.346829	-0.050484	4.286076
249.260748	6280.912680	15.351834	-0.050461	4.283454
249.177750	6272.927903	15.356839	-0.050441	4.280827
249.308758	6264.930243	15.361843	-0.050460	4.278196
249.271513	6256.987302	15.366848	-0.050448	4.275579
249.147676	6248.896182	15.371853	-0.050419	4.272912
249.288863	6240.879875	15.376858	-0.050441	4.270270
249.081462	6232.913651	15.381863	-0.050397	4.267639
248.953782	6224.865227	15.386867	-0.050368	4.264981
248.988358	6216.963954	15.391872	-0.050369	4.262371
248.960241	6208.860555	15.396877	-0.050358	4.259692
248.902492	6200.981984	15.401882	-0.050343	4.257085
248.898343	6192.909718	15.406887	-0.050337	4.254414
248.955202	6184.899273	15.411891	-0.050342	4.251761
248.797168	6176.870597	15.416896	-0.050307	4.249099
248.675442	6168.940125	15.421901	-0.050279	4.246468
248.808062	6160.901161	15.426906	-0.050299	4.243802
248.577649	6152.960237	15.431911	-0.050251	4.241163
248.466598	6144.913847	15.436915	-0.050225	4.238489
248.455432	6137.012415	15.441920	-0.050218	4.235862
248.548249	6128.923358	15.446925	-0.050230	4.233172
248.636917	6120.926734	15.451930	-0.050241	4.230511
248.467868	6112.901453	15.456935	-0.050204	4.227837
248.503896	6104.877136	15.461939	-0.050206	4.225163
248.601969	6096.940273	15.466944	-0.050219	4.222517
248.449144	6088.920470	15.471949	-0.050185	4.219839
248.543073	6080.977837	15.476954	-0.050197	4.217188
248.413766	6072.922707	15.481959	-0.050168	4.214495
248.428986	6064.915047	15.486963	-0.050166	4.211818
248.491928	6056.925940	15.491968	-0.050172	4.209146
248.381377	6048.946320	15.496973	-0.050146	4.206473
248.338144	6040.939915	15.501978	-0.050133	4.203791
248.280864	6032.950258	15.506983	-0.050117	4.201112
248.256807	6024.951655	15.511987	-0.050107	4.198429
248.479124	6016.981991	15.516992	-0.050144	4.195757
248.056986	6008.892898	15.521997	-0.050060	4.193036
248.015813	6000.829519	15.527002	-0.050047	4.190326
248.073217	5992.858227	15.532007	-0.050052	4.187646
247.999673	5984.844333	15.537011	-0.050033	4.184948
248.050165	5976.939114	15.542016	-0.050038	4.182287
247.858626	5968.924590	15.547021	-0.049997	4.179585
247.876186	5960.937123	15.552026	-0.049995	4.176892
247.897739	5952.924146	15.557031	-0.049994	4.174189
247.847373	5944.897498	15.562035	-0.049979	4.171479
248.007718	5936.893955	15.567040	-0.050004	4.168777
247.677840	5928.875191	15.572045	-0.049937	4.166063
247.829842	5920.934907	15.577050	-0.049960	4.163379
247.815281	5912.895654	15.582055	-0.049952	4.160657
247.545428	5904.943257	15.587059	-0.049897	4.157961
247.569429	5896.934399	15.592064	-0.049896	4.155247
247.804565	5888.849802	15.597069	-0.049934	4.152508
247.816275	5880.872075	15.602074	-0.049931	4.149801
247.573598	5872.887366	15.607079	-0.049881	4.147087
247.674908	5864.886640	15.612083	-0.049895	4.144369
247.623460	5856.929604	15.617088	-0.049880	4.141663
247.508972	5848.877315	15.622093	-0.049853	4.138922
247.486810	5840.936180	15.627098	-0.049844	4.136218
247.312313	5832.865603	15.632103	-0.049806	4.133466
247.232448	5824.853798	15.637107	-0.049786	4.130734
247.190234	5816.908170	15.642112	-0.049773	4.128023
247.223744	5808.877237	15.647117	-0.049774	4.125282
247.245499	5800.918765	15.652122	-0.049773	4.122563
247.306190	5792.876445	15.657127	-0.049779	4.119815
247.201187	5784.935986	15.662131	-0.049754	4.117098
247.260616	5776.902559	15.667136	-0.049760	4.114349
247.003343	5768.836307	15.672141	-0.049707	4.111583
247.019606	5760.852649	15.677146	-0.049705	4.108847
246.904856	5752.890219	15.682151	-0.049678	4.106114
246.993555	5744.877159	15.687155	-0.049690	4.103365
247.080980	5736.914019	15.692160	-0.049701	4.100632
246.891118	5728.906942	15.697165	-0.049660	4.097877
246.960681	5720.889809	15.702170	-0.049668	4.095121
246.859212	5712.890173	15.707175	-0.049644	4.092367
246.632823	5704.870058	15.712179	-0.049596	4.089602
246.891351	5696.898839	15.717184	-0.049639	4.086859
246.709793	5688.877000	15.722189	-0.049600	4.084090
246.621333	5680.985412	15.727194	-0.049579	4.081366
246.763399	5672.949812	15.732199	-0.049600	4.078593
246.858808	5664.958535	15.737203	-0.049612	4.075834
246.686145	5656.962707	15.742208	-0.049575	4.073067
246.573608	5648.906810	15.747213	-0.049549	4.070278
246.545545	5640.915240	15.752218	-0.049538	4.067510
246.334197	5632.924028	15.757223	-0.049494	4.064739
246.317668	5624.952844	15.762227	-0.049485	4.061975
246.374482	5616.948083	15.767232	-0.049491	4.059198
246.256759	5608.951542	15.772237	-0.049464	4.056420
246.248502	5600.952372	15.777242	-0.049457	4.053641
246.102213	5592.921399	15.782247	-0.049424	4.050847
246.310621	5584.928632	15.787251	-0.049458	4.048069
246.318572	5576.969481	15.792256	-0.049454	4.045298
246.294185	5568.945495	15.797261	-0.049445	4.042503
246.456005	5560.917331	15.802266	-0.049469	4.039706
246.267516	5552.966955	15.807271	-0.049429	4.036930
246.068238	5544.955550	15.812275	-0.049387	4.034130
246.107700	5536.848337	15.817280	-0.049389	4.031298
246.106234	5528.870003	15.822285	-0.049383	4.028509
245.942150	5520.900738	15.827290	-0.049348	4.025719
245.907934	5512.893041	15.832295	-0.049336	4.022915
245.935399	5504.905157	15.837299	-0.049336	4.020117
245.875242	5496.958757	15.842304	-0.049320	4.017330
245.846425	5488.920430	15.847309	-0.049309	4.014510
245.887830	5480.894415	15.852314	-0.049311	4.011693
245.778032	5472.909237	15.857319	-0.049286	4.008886
245.804864	5464.907570	15.862323	-0.049286	4.006073
245.787651	5456.944561	15.867328	-0.049277	4.003272
245.769262	5448.913615	15.872333	-0.049268	4.000444
245.727920	5440.973567	15.877338	-0.049256	3.997646
245.465427	5432.946547	15.882343	-0.049201	3.994812
245.629740	5424.902163	15.887347	-0.049227	3.991977
245.596929	5416.912321	15.892352	-0.049216	3.989155
245.289380	5408.906450	15.897357	-0.049153	3.986322
245.404341	5400.920264	15.902362	-0.049169	3.983500
245.382808	5392.941671	15.907367	-0.049160	3.980677
245.340764	5384.962666	15.912371	-0.049147	3.977851
245.390677	5376.968283	15.917376	-0.049151	3.975019
245.489533	5368.905086	15.922381	-0.049164	3.972162
245.350991	5360.906445	15.927386	-0.049133	3.969322
245.188864	5352.954273	15.932391	-0.049098	3.966495
245.193059	5344.900620	15.937395	-0.049093	3.963634
245.226418	5336.987425	15.942400	-0.049094	3.960821
245.117189	5328.989384	15.947405	-0.049069	3.957973
245.099237	5321.020769	15.952410	-0.049060	3.955135
245.235049	5312.953184	15.957415	-0.049080	3.952262
244.962217	5304.938532	15.962419	-0.049024	3.949399
244.944266	5296.999501	15.967424	-0.049016	3.946566
244.899444	5288.923321	15.972429	-0.049002	3.943681
244.806156	5280.974236	15.977434	-0.048980	3.940838
244.892309	5273.015036	15.982439	-0.048990	3.937993
244.989093	5264.967727	15.987443	-0.049003	3.935115
245.118015	5256.982172	15.992448	-0.049022	3.932257
244.905424	5248.956850	15.997453	-0.048977	3.929376
244.964582	5241.030816	16.002458	-0.048983	3.926534
244.817175	5233.012286	16.007463	-0.048950	3.923653
244.613072	5225.009548	16.012467	-0.048907	3.920775
244.765079	5217.038012	16.017472	-0.048930	3.917912
244.603527	5209.018909	16.022477	-0.048895	3.915024
244.467539	5200.986280	16.027482	-0.048864	3.912130
244.432777	5192.970027	16.032487	-0.048853	3.909241
244.512153	5184.971119	16.037491	-0.048862	3.906358
244.620405	5177.037997	16.042496	-0.048877	3.903498
244.389656	5168.990923	16.047501	-0.048829	3.900588
244.579164	5161.001351	16.052506	-0.048859	3.897705
244.588702	5153.000328	16.057511	-0.048856	3.894811
244.251385	5144.981305	16.062515	-0.048788	3.891903
244.442809	5136.990397	16.067520	-0.048818	3.889013
244.339114	5128.960770	16.072525	-0.048793	3.886100
244.315155	5121.001793	16.077530	-0.048784	3.883213
244.173850	5113.013767	16.082535	-0.048752	3.880311
244.278793	5105.030576	16.087539	-0.048767	3.877413
244.230492	5097.042696	16.092544	-0.048752	3.874508
244.013929	5088.730238	16.097549	-0.048707	3.871480
243.984251	5080.825672	16.102554	-0.048696	3.868602
244.019011	5072.886663	16.107559	-0.048697	3.865710
244.033428	5064.958980	16.112563	-0.048695	3.862819
244.101640	5056.968422	16.117568	-0.048702	3.859905
244.120418	5048.984891	16.122573	-0.048701	3.856990
244.204013	5040.970507	16.127578	-0.048711	3.854063
244.059939	5032.995294	16.132583	-0.048679	3.851143
243.852708	5024.965766	16.137587	-0.048635	3.848200
243.903654	5017.005582	16.142592	-0.048639	3.845285
243.740220	5009.022574	16.147597	-0.048604	3.842355
243.853211	5001.000404	16.152602	-0.048619	3.839415
243.779506	4993.084984	16.157607	-0.048601	3.836507
243.740536	4984.998658	16.162611	-0.048588	3.833536
243.576496	4977.061535	16.167616	-0.048552	3.830614
243.621330	4969.036365	16.172621	-0.048555	3.827661
243.647054	4961.021858	16.177626	-0.048555	3.824711
243.466497	4953.103281	16.182631	-0.048516	3.821788
243.402325	4945.061450	16.187635	-0.048499	3.818821
243.543649	4937.118017	16.192640	-0.048520	3.815892
243.314981	4929.075368	16.197645	-0.048472	3.812916
243.324110	4921.056497	16.202650	-0.048469	3.809952
243.233391	4913.099466	16.207655	-0.048447	3.807006
243.284302	4905.051845	16.212659	-0.048451	3.804027
243.374367	4897.120220	16.217664	-0.048463	3.801090
243.308029	4889.091152	16.222669	-0.048445	3.798111
243.330736	4881.107716	16.227674	-0.048444	3.795148
243.238057	4873.074344	16.232679	-0.048421	3.792162
243.153592	4865.044338	16.237683	-0.048401	3.789176
243.196497	4857.106213	16.242688	-0.048403	3.786223
243.199163	4849.062681	16.247693	-0.048399	3.783229
242.989461	4841.087708	16.252698	-0.048354	3.780253
242.958081	4833.100824	16.257703	-0.048343	3.777274
242.963291	4825.093796	16.262707	-0.048339	3.774286
242.966165	4817.095762	16.267712	-0.048334	3.771298
242.873142	4809.100727	16.272717	-0.048312	3.768308
243.151244	4801.023505	16.277722	-0.048358	3.765293
243.017552	4793.121252	16.282727	-0.048328	3.762331
242.768729	4785.125752	16.287731	-0.048277	3.759330
242.742137	4777.177974	16.292736	-0.048267	3.756349
242.671951	4769.132777	16.297741	-0.048248	3.753328
242.794485	4761.086288	16.302746	-0.048266	3.750309
243.007459	4753.098718	16.307751	-0.048300	3.747311
242.754138	4745.086014	16.312755	-0.048248	3.744291
242.735086	4737.139818	16.317760	-0.048239	3.741299
242.603521	4729.130865	16.322765	-0.048209	3.738278
242.573563	4721.141908	16.327770	-0.048199	3.735265
242.603429	4713.126693	16.332775	-0.048199	3.732240
242.422849	4705.132140	16.337779	-0.048160	3.729216
242.723231	4697.141632	16.342784	-0.048211	3.726203
242.674002	4689.141824	16.347789	-0.048196	3.723175
242.503132	4681.187656	16.352794	-0.048159	3.720159
242.576460	4673.232579	16.357799	-0.048168	3.717147
242.450233	4665.165939	16.362803	-0.048139	3.714084
242.302508	4657.095891	16.367808	-0.048106	3.711018
242.268462	4649.114767	16.372813	-0.048095	3.707985
242.094356	4641.127130	16.377818	-0.048057	3.704944
242.034537	4633.181334	16.382823	-0.048041	3.701919
242.144317	4625.178536	16.387827	-0.048056	3.698874
242.241817	4617.210929	16.392832	-0.048069	3.695840
242.148752	4609.182998	16.397837	-0.048046	3.692775
241.872608	4601.208999	16.402842	-0.047990	3.689724
242.146951	4593.202873	16.407847	-0.048036	3.686672
241.913018	4585.227177	16.412851	-0.047987	3.683616
241.949373	4577.244308	16.417856	-0.047989	3.680562
241.763570	4569.260062	16.422861	-0.047949	3.677499
241.680595	4561.261024	16.427866	-0.047928	3.674430
241.743002	4553.245131	16.432871	-0.047934	3.671356
241.544070	4545.209629	16.437875	-0.047892	3.668265
242.018410	4537.211077	16.442880	-0.047975	3.665204
241.860193	4529.242340	16.447885	-0.047941	3.662134
241.713449	4521.243913	16.452890	-0.047908	3.659051
241.453307	4513.301324	16.457895	-0.047854	3.655984
241.614870	4505.256621	16.462899	-0.047879	3.652886
241.514546	4497.259243	16.467904	-0.047855	3.649797
241.338067	4489.260987	16.472909	-0.047817	3.646703
241.323433	4481.242319	16.477914	-0.047809	3.643603
241.270481	4473.296043	16.482919	-0.047794	3.640526
241.165830	4465.292401	16.487923	-0.047770	3.637424
241.376561	4457.301929	16.492928	-0.047804	3.634333
241.280088	4449.244625	16.497933	-0.047780	3.631204
241.260120	4441.260508	16.502938	-0.047771	3.628104
241.239233	4433.269643	16.507943	-0.047762	3.624998
241.184477	4425.307275	16.512947	-0.047747	3.621900
240.986932	4417.332138	16.517952	-0.047705	3.618790
240.980010	4409.303239	16.522957	-0.047698	3.615662
240.921906	4401.324134	16.527962	-0.047682	3.612549
240.932255	4393.308700	16.532967	-0.047679	3.609421
240.841834	4385.333750	16.537971	-0.047657	3.606303
240.914712	4377.350100	16.542976	-0.047665	3.603184
240.779495	4369.366690	16.547981	-0.047635	3.600057
240.722126	4361.402231	16.552986	-0.047619	3.596936
240.849429	4353.362965	16.557991	-0.047638	3.593788
240.656591	4345.352984	16.562995	-0.047597	3.590640
240.800715	4337.365489	16.568000	-0.047618	3.587508
240.678702	4329.359742	16.573005	-0.047590	3.584358
240.584938	4321.419333	16.578010	-0.047568	3.581232
240.550576	4313.445906	16.583015	-0.047556	3.578092
240.523625	4305.406098	16.588019	-0.047546	3.574923
240.689093	4297.390987	16.593024	-0.047571	3.571767
240.646835	4289.398154	16.598029	-0.047558	3.568610
240.601555	4281.407900	16.603034	-0.047545	3.565452
240.473173	4273.455353	16.608039	-0.047515	3.562304
240.495764	4265.430126	16.613043	-0.047514	3.559128
240.315311	4257.489364	16.618048	-0.047476	3.555977
240.147477	4249.386364	16.623053	-0.047439	3.552759
240.275184	4241.321413	16.628058	-0.047458	3.549562
240.350351	4233.379949	16.633063	-0.047466	3.546410
240.167769	4225.388716	16.638067	-0.047427	3.543227
240.165691	4217.428034	16.643072	-0.047422	3.540059
239.976401	4209.459611	16.648077	-0.047381	3.536880
240.089676	4201.453653	16.653082	-0.047397	3.533692
240.101585	4193.426582	16.658087	-0.047394	3.530489
240.014892	4185.411942	16.663091	-0.047373	3.527286
240.191931	4177.451674	16.668096	-0.047400	3.524109
240.059033	4169.487081	16.673101	-0.047371	3.520918
240.060405	4161.506246	16.678106	-0.047366	3.517722
240.114439	4153.502157	16.683111	-0.047370	3.514516
239.911542	4145.476899	16.688115	-0.047327	3.511290
239.934112	4137.487571	16.693120	-0.047326	3.508082
239.858330	4129.484424	16.698125	-0.047307	3.504863
239.769855	4121.544727	16.703130	-0.047285	3.501666
239.743469	4113.553253	16.708135	-0.047275	3.498448
239.488512	4105.551346	16.713139	-0.047223	3.495214
239.646015	4097.536351	16.718144	-0.047247	3.491986
239.448022	4089.539536	16.723149	-0.047205	3.488751
239.440104	4081.570830	16.728154	-0.047198	3.485530
239.519431	4073.615748	16.733159	-0.047207	3.482314
239.407703	4065.590574	16.738163	-0.047181	3.479061
239.492309	4057.624423	16.743168	-0.047192	3.475835
239.513991	4049.582161	16.748173	-0.047191	3.472573
239.419984	4041.568939	16.753178	-0.047168	3.469316
239.223375	4033.618298	16.758183	-0.047126	3.466078
239.275421	4025.620809	16.763187	-0.047131	3.462826
239.354382	4017.627893	16.768192	-0.047140	3.459574
239.260901	4009.651704	16.773197	-0.047118	3.456320
239.034210	4001.657839	16.778202	-0.047070	3.453051
239.077981	3993.599415	16.783207	-0.047073	3.449762
238.964764	3985.633110	16.788211	-0.047047	3.446502
238.899870	3977.655231	16.793216	-0.047030	3.443236
239.105662	3969.646214	16.798221	-0.047063	3.439963
239.001984	3961.716354	16.803226	-0.047038	3.436709
238.817671	3953.695684	16.808231	-0.046999	3.433412
238.720952	3945.641456	16.813235	-0.046975	3.430100
239.000581	3937.697039	16.818240	-0.047022	3.426844
238.780506	3929.669158	16.823245	-0.046976	3.423533
238.749865	3921.695671	16.828250	-0.046965	3.420248
238.767400	3913.715292	16.833255	-0.046963	3.416958
238.656718	3905.720690	16.838259	-0.046937	3.413655
238.645322	3897.727914	16.843264	-0.046930	3.410353
238.730475	3889.725052	16.848269	-0.046941	3.407047
238.616852	3881.754780	16.853274	-0.046914	3.403744
238.552352	3873.791966	16.858279	-0.046897	3.400443
238.524956	3865.789417	16.863283	-0.046887	3.397123
238.587102	3857.772912	16.868288	-0.046893	3.393797
238.354611	3849.699653	16.873293	-0.046845	3.390435
238.424352	3841.744083	16.878298	-0.046852	3.387128
238.504037	3833.746696	16.883303	-0.046862	3.383801
238.429956	3825.788882	16.888307	-0.046843	3.380482
238.288985	3817.847591	16.893312	-0.046812	3.377165
238.091819	3809.838995	16.898317	-0.046770	3.373813
238.086784	3801.825058	16.903322	-0.046763	3.370464
238.060511	3793.846269	16.908327	-0.046753	3.367124
237.919868	3785.833797	16.913331	-0.046722	3.363763
238.101637	3777.862018	16.918336	-0.046751	3.360428
238.141216	3769.863461	16.923341	-0.046753	3.357073
238.009035	3761.881011	16.928346	-0.046723	3.353715
238.028127	3753.860156	16.933351	-0.046721	3.350343
237.908166	3745.859416	16.938355	-0.046694	3.346970
237.831440	3737.916369	16.943360	-0.046674	3.343621
237.711839	3729.925125	16.948365	-0.046647	3.340246
237.960332	3721.901794	16.953370	-0.046688	3.336868
237.861288	3713.935303	16.958375	-0.046664	3.333497
237.724103	3705.907977	16.963379	-0.046633	3.330096
237.693779	3697.956173	16.968384	-0.046622	3.326727
237.742679	3689.951739	16.973389	-0.046626	3.323336
237.614766	3681.985015	16.978394	-0.046597	3.319950
237.693191	3674.033229	16.983399	-0.046607	3.316576
237.831914	3665.964551	16.988403	-0.046627	3.313150
237.762875	3657.958512	16.993408	-0.046609	3.309739
237.454695	3649.998139	16.998413	-0.046547	3.306336
237.457945	3642.019823	17.003418	-0.046542	3.302933
237.526760	3634.021952	17.008423	-0.046550	3.299520
237.190478	3626.059095	17.013427	-0.046482	3.296104
237.285377	3618.071086	17.018432	-0.046494	3.292690
237.242384	3610.033779	17.023437	-0.046481	3.289246
237.239375	3602.069722	17.028442	-0.046475	3.285831
237.081581	3594.122108	17.033447	-0.046441	3.282413
237.066757	3586.090756	17.038451	-0.046433	3.278962
237.043847	3578.146229	17.043456	-0.046423	3.275544
237.078848	3570.108361	17.048461	-0.046425	3.272085
237.123153	3562.062207	17.053466	-0.046428	3.268618
237.191432	3554.104826	17.058471	-0.046435	3.265187
237.042653	3546.141672	17.063475	-0.046402	3.261742
237.067596	3538.163152	17.068480	-0.046402	3.258293
237.048585	3530.167551	17.073485	-0.046393	3.254831
236.686177	3522.199107	17.078490	-0.046320	3.251364
236.697819	3514.188305	17.083495	-0.046317	3.247890
236.617309	3506.196026	17.088499	-0.046297	3.244416
236.769436	3498.257564	17.093504	-0.046320	3.240971
236.691578	3490.241257	17.098509	-0.046300	3.237479
236.748211	3482.213256	17.103514	-0.046306	3.233984
236.808908	3474.169205	17.108519	-0.046312	3.230479
236.613186	3466.182102	17.113523	-0.046270	3.226983
236.578405	3458.238667	17.118528	-0.046258	3.223510
236.628294	3450.243815	17.123533	-0.046262	3.220014
236.651268	3442.273689	17.128538	-0.046262	3.216524
236.704909	3434.277297	17.133543	-0.046266	3.213020
236.343502	3426.284689	17.138547	-0.046194	3.209496
236.516220	3418.308771	17.143552	-0.046221	3.205999
236.513299	3410.319813	17.148557	-0.046215	3.202484
236.288478	3402.338021	17.153562	-0.046168	3.198959
236.293933	3394.388531	17.158567	-0.046164	3.195454
236.065917	3386.368925	17.163571	-0.046116	3.191905
236.282558	3378.366734	17.168576	-0.046151	3.188378
236.293441	3370.340786	17.173581	-0.046148	3.184828
236.193159	3362.406309	17.178586	-0.046124	3.181310
236.081120	3354.432527	17.183591	-0.046098	3.177770
236.106062	3346.409511	17.188595	-0.046097	3.174210
235.988590	3338.430992	17.193600	-0.046070	3.170659
235.795377	3330.453360	17.198605	-0.046029	3.167102
235.782978	3322.439955	17.203610	-0.046022	3.163533
235.823250	3314.505373	17.208615	-0.046024	3.159997
235.699976	3306.485809	17.213619	-0.045996	3.156412
236.031110	3298.459078	17.218624	-0.046052	3.152839
235.801603	3290.476485	17.223629	-0.046004	3.149258
235.521874	3282.516361	17.228634	-0.045947	3.145681
235.692069	3274.542911	17.233639	-0.045974	3.142113
235.595422	3266.512891	17.238643	-0.045950	3.138504
235.576543	3258.554628	17.243648	-0.045942	3.134926
235.362681	3250.570593	17.248653	-0.045897	3.131324
235.529924	3242.549897	17.253658	-0.045922	3.127719
235.548271	3234.591851	17.258663	-0.045921	3.124131
235.384534	3226.620914	17.263667	-0.045885	3.120524
235.341002	3218.662519	17.268672	-0.045872	3.116925
235.261754	3210.661740	17.273677	-0.045852	3.113301
235.479094	3202.616635	17.278682	-0.045887	3.109665
235.354543	3194.677592	17.283687	-0.045859	3.106059
235.143349	3186.687119	17.288691	-0.045814	3.102420
235.169741	3178.713861	17.293696	-0.045814	3.098796
235.190526	3170.718268	17.298701	-0.045812	3.095157
235.140677	3162.715904	17.303706	-0.045798	3.091508
235.282206	3154.729009	17.308711	-0.045819	3.087870
235.020739	3146.723213	17.313715	-0.045765	3.084201
234.919831	3138.802913	17.318720	-0.045741	3.080574
235.043552	3130.814007	17.323725	-0.045759	3.076922
235.012989	3122.765820	17.328730	-0.045748	3.073230
234.946940	3114.743851	17.333735	-0.045731	3.069545
234.815872	3106.780282	17.338739	-0.045701	3.065879
234.937446	3098.798439	17.343744	-0.045718	3.062213
234.626713	3090.856160	17.348749	-0.045655	3.058539
234.668434	3082.859673	17.353754	-0.045658	3.054853
234.848538	3074.861966	17.358759	-0.045686	3.051168
234.598612	3066.889789	17.363763	-0.045634	3.047471
234.595913	3058.912011	17.368768	-0.045629	3.043778
234.503475	3050.944446	17.373773	-0.045606	3.040081
234.657105	3042.965837	17.378778	-0.045630	3.036386
234.607721	3034.972939	17.383783	-0.045615	3.032670
234.412983	3026.966746	17.388787	-0.045574	3.028936
234.574752	3018.975591	17.393792	-0.045599	3.025222
234.353281	3011.024801	17.398797	-0.045552	3.021504
234.296292	3003.033969	17.403802	-0.045536	3.017771
234.210177	2995.071460	17.408807	-0.045515	3.014044
234.208258	2987.028015	17.413811	-0.045510	3.010279
234.073228	2979.081200	17.418816	-0.045479	3.006548
234.229982	2971.092972	17.423821	-0.045503	3.002808
234.139497	2963.121449	17.428826	-0.045481	2.999058
233.947027	2955.170726	17.433831	-0.045440	2.995309
233.802975	2947.136826	17.438835	-0.045408	2.991518
233.870621	2939.150930	17.443840	-0.045416	2.987755
233.715190	2931.157145	17.448845	-0.045381	2.983973
233.583057	2923.198154	17.453850	-0.045352	2.980203
233.745285	2915.233057	17.458855	-0.045377	2.976441
233.755752	2907.213861	17.463859	-0.045373	2.972641
233.635046	2899.238683	17.468864	-0.045346	2.968850
233.747599	2891.252019	17.473869	-0.045361	2.965060
233.840788	2883.273654	17.478874	-0.045374	2.961269
233.750589	2875.325201	17.483879	-0.045352	2.957477
233.522273	2867.324053	17.488883	-0.045304	2.953649
233.504331	2859.322429	17.493888	-0.045295	2.949826
233.537657	2851.351733	17.498893	-0.045296	2.946016
233.551882	2843.358875	17.503898	-0.045294	2.942189
233.539720	2835.405302	17.508903	-0.045286	2.938374
233.464680	2827.407175	17.513907	-0.045267	2.934530
233.341491	2819.422869	17.518912	-0.045239	2.930685
233.293149	2811.446769	17.523917	-0.045225	2.926843
233.542520	2803.419475	17.528922	-0.045266	2.922987
233.456926	2795.487830	17.533927	-0.045245	2.919154
233.335300	2787.506049	17.538931	-0.045217	2.915290
233.430783	2779.433680	17.543936	-0.045229	2.911388
233.360489	2771.486915	17.548941	-0.045211	2.907533
233.137375	2763.489151	17.553946	-0.045164	2.903640
233.205559	2755.551575	17.558951	-0.045172	2.899787
233.188633	2747.574304	17.563955	-0.045164	2.895905
233.059256	2739.591397	17.568960	-0.045134	2.892009
232.997279	2731.611189	17.573965	-0.045118	2.888112
232.960194	2723.622408	17.578970	-0.045105	2.884208
233.124693	2715.681939	17.583975	-0.045131	2.880332
232.686723	2707.722554	17.588979	-0.045044	2.876409
232.793301	2699.713967	17.593984	-0.045059	2.872487
232.675310	2691.719203	17.598989	-0.045032	2.868553
232.529251	2683.727202	17.603994	-0.044999	2.864614
232.563215	2675.791267	17.608999	-0.045000	2.860708
232.448366	2667.796895	17.614003	-0.044974	2.856758
232.493912	2659.815119	17.619008	-0.044977	2.852819
232.415872	2651.821098	17.624013	-0.044957	2.848861
232.660956	2643.798488	17.629018	-0.044998	2.844901
232.768968	2635.866626	17.634023	-0.045013	2.840973
232.413381	2627.902871	17.639027	-0.044941	2.836998
232.553862	2619.900907	17.644032	-0.044962	2.833026
232.320043	2611.930214	17.649037	-0.044913	2.829043
232.241679	2603.931226	17.654042	-0.044894	2.825049
232.225804	2595.990163	17.659047	-0.044885	2.821082
232.118370	2588.010889	17.664051	-0.044860	2.817085
232.165370	2580.025271	17.669056	-0.044864	2.813088
232.129258	2572.035655	17.674061	-0.044852	2.809078
232.212899	2564.030629	17.679066	-0.044862	2.805062
232.238228	2556.091504	17.684071	-0.044862	2.801070
232.032807	2548.120985	17.689075	-0.044818	2.797043
231.979386	2540.151265	17.694080	-0.044803	2.793019
232.009779	2532.149994	17.699085	-0.044804	2.788979
231.879000	2524.141406	17.704090	-0.044774	2.784919
232.019421	2516.216459	17.709095	-0.044795	2.780912
232.002635	2508.221570	17.714099	-0.044787	2.776854
231.818024	2500.256122	17.719104	-0.044747	2.772796
231.801491	2492.271140	17.724109	-0.044739	2.768731
231.866547	2484.269362	17.729114	-0.044746	2.764657
231.890992	2476.350729	17.734119	-0.044745	2.760617
231.720694	2468.382937	17.739123	-0.044708	2.756534
231.586486	2460.358199	17.744128	-0.044678	2.752418
231.560942	2452.343075	17.749133	-0.044668	2.748307
231.470939	2444.360933	17.754138	-0.044646	2.744203
231.807991	2436.410047	17.759143	-0.044703	2.740135
231.511034	2428.454403	17.764147	-0.044643	2.736020
231.612336	2420.448522	17.769152	-0.044657	2.731897
231.269202	2412.504462	17.774157	-0.044588	2.727773
231.385846	2404.501601	17.779162	-0.044604	2.723640
231.273531	2396.591704	17.784167	-0.044578	2.719535
231.139592	2388.617637	17.789171	-0.044548	2.715389
231.169836	2380.591764	17.794176	-0.044548	2.711220
231.399472	2372.604077	17.799181	-0.044586	2.707076
231.026460	2364.678656	17.804186	-0.044511	2.702922
231.016583	2356.708246	17.809191	-0.044504	2.698760
230.977494	2348.723224	17.814195	-0.044492	2.694582
230.867895	2340.748386	17.819200	-0.044466	2.690398
230.924427	2332.764166	17.824205	-0.044471	2.686214
230.754181	2324.811469	17.829210	-0.044434	2.682025
230.722738	2316.872261	17.834215	-0.044423	2.677846
230.621174	2308.877611	17.839219	-0.044399	2.673626
230.742775	2300.843103	17.844224	-0.044417	2.669393
230.793163	2292.870060	17.849229	-0.044421	2.665181
230.582476	2284.929636	17.854234	-0.044376	2.660963
230.452808	2276.992616	17.859239	-0.044347	2.656745
230.547707	2268.967400	17.864243	-0.044360	2.652488
230.473037	2261.005683	17.869248	-0.044340	2.648247
230.461514	2253.041694	17.874253	-0.044333	2.644002
230.383171	2245.081469	17.879258	-0.044313	2.639748
230.516885	2237.111812	17.884263	-0.044333	2.635496
230.228640	2229.129471	17.889267	-0.044274	2.631203
230.203297	2221.161599	17.894272	-0.044264	2.626927
230.256880	2213.189111	17.899277	-0.044269	2.622648
229.983274	2205.246066	17.904282	-0.044213	2.618355
230.256692	2197.257033	17.909287	-0.044259	2.614067
230.137407	2189.257796	17.914291	-0.044231	2.609740
230.006494	2181.317465	17.919296	-0.044202	2.605437
229.973944	2173.372595	17.924301	-0.044190	2.601132
229.800294	2165.411940	17.929306	-0.044153	2.596800
230.101958	2157.294480	17.934311	-0.044204	2.592409
229.966532	2149.243878	17.939315	-0.044173	2.588017
229.801235	2141.336604	17.944320	-0.044137	2.583693
229.927537	2133.403470	17.949325	-0.044156	2.579368
229.621132	2125.482403	17.954330	-0.044093	2.575013
229.709959	2117.500373	17.959335	-0.044105	2.570644
229.562791	2109.533506	17.964339	-0.044072	2.566260
229.558423	2101.590936	17.969344	-0.044066	2.561891
229.611506	2093.648980	17.974349	-0.044071	2.557519
229.498080	2085.659711	17.979354	-0.044045	2.553102
229.826153	2077.646914	17.984359	-0.044100	2.548696
229.445331	2069.714791	17.989363	-0.044024	2.544276
229.241654	2061.807580	17.994368	-0.043981	2.539875
229.302524	2053.833872	17.999373	-0.043987	2.535448
229.320218	2045.838098	18.004378	-0.043985	2.530998
229.335579	2037.880160	18.009383	-0.043983	2.526562
229.212304	2029.905645	18.014387	-0.043955	2.522098
229.183216	2021.967234	18.019392	-0.043944	2.517653
229.291346	2013.971816	18.024397	-0.043959	2.513178
229.003245	2005.993226	18.029402	-0.043900	2.508676
229.095168	1998.032274	18.034407	-0.043912	2.504204
229.118430	1990.062522	18.039411	-0.043911	2.499713
229.013492	1982.118392	18.044416	-0.043887	2.495220
228.956692	1974.148489	18.049421	-0.043871	2.490707
228.863569	1966.167221	18.054426	-0.043848	2.486177
228.894987	1958.239871	18.059431	-0.043849	2.481678
228.730346	1950.294778	18.064435	-0.043813	2.477147
228.667312	1942.317151	18.069440	-0.043796	2.472597
228.747870	1934.324867	18.074445	-0.043806	2.468040
228.658289	1926.349597	18.079450	-0.043784	2.463472
228.578390	1918.429817	18.084455	-0.043764	2.458928
228.498392	1910.463336	18.089459	-0.043744	2.454348
228.462098	1902.480818	18.094464	-0.043732	2.449754
228.430827	1894.529949	18.099469	-0.043721	2.445171
228.620492	1886.547650	18.104474	-0.043751	2.440577
228.627305	1878.621867	18.109479	-0.043747	2.435993
228.403409	1870.600410	18.114483	-0.043700	2.431327
228.396087	1862.610994	18.119488	-0.043694	2.426688
228.329603	1854.676048	18.124493	-0.043676	2.422067
228.140234	1846.737510	18.129498	-0.043636	2.417426
228.455944	1838.761461	18.134503	-0.043689	2.412792
228.393201	1830.782848	18.139507	-0.043673	2.408119
228.168790	1822.863880	18.144512	-0.043626	2.403460
228.123218	1814.919578	18.149517	-0.043612	2.398790
227.876255	1806.969153	18.154522	-0.043561	2.394092
227.993805	1798.999252	18.159527	-0.043577	2.389401
227.889543	1791.026567	18.164531	-0.043553	2.384683
227.843134	1783.089625	18.169536	-0.043539	2.379980
227.859748	1775.140476	18.174541	-0.043537	2.375266
227.477224	1767.185441	18.179546	-0.043460	2.370508
227.491629	1759.223821	18.184551	-0.043458	2.365767
227.601748	1751.258703	18.189555	-0.043473	2.361023
227.414477	1743.327235	18.194560	-0.043433	2.356265
227.389958	1735.348513	18.199565	-0.043423	2.351482
227.535125	1727.340199	18.204570	-0.043445	2.346686
227.519072	1719.397744	18.209575	-0.043437	2.341906
227.254077	1711.471936	18.214579	-0.043383	2.337107
227.446928	1703.507550	18.219584	-0.043413	2.332311
227.419946	1695.536271	18.224589	-0.043403	2.327484
227.131107	1687.604131	18.229594	-0.043344	2.322648
227.192313	1679.684250	18.234599	-0.043350	2.317839
226.982140	1671.746436	18.239603	-0.043306	2.312986
227.100259	1663.748781	18.244608	-0.043323	2.308114
227.026241	1655.810327	18.249613	-0.043304	2.303252
227.150453	1647.823298	18.254618	-0.043322	2.298366
227.009115	1639.912262	18.259623	-0.043290	2.293495
226.802994	1631.962194	18.264627	-0.043247	2.288583
226.788794	1623.999320	18.269632	-0.043239	2.283669
226.937424	1616.056822	18.274637	-0.043261	2.278771
226.695947	1608.110988	18.279642	-0.043211	2.273827
226.941237	1600.066975	18.284647	-0.043252	2.268853
226.646022	1592.144930	18.289651	-0.043192	2.263898
226.597345	1584.204689	18.294656	-0.043177	2.258941
226.770936	1576.248995	18.299661	-0.043204	2.253983
226.586448	1568.308258	18.304666	-0.043165	2.248993
226.513373	1560.377673	18.309671	-0.043146	2.244007
226.385748	1552.463197	18.314675	-0.043117	2.239016
226.287127	1544.518379	18.319680	-0.043094	2.233997
226.665751	1536.508620	18.324685	-0.043159	2.228968
226.449849	1528.576133	18.329690	-0.043114	2.223923
226.482763	1520.655583	18.334695	-0.043114	2.218897
226.444568	1512.699478	18.339699	-0.043102	2.213831
226.502658	1504.734355	18.344704	-0.043108	2.208755
226.295678	1496.834846	18.349709	-0.043064	2.203687
226.225704	1488.886371	18.354714	-0.043046	2.198587
226.134779	1480.965643	18.359719	-0.043024	2.193491
225.970209	1472.993144	18.364723	-0.042988	2.188344
225.937920	1465.041295	18.369728	-0.042977	2.183210
225.998377	1457.095718	18.374733	-0.042983	2.178076
225.962426	1449.149570	18.379738	-0.042971	2.172920
225.991139	1441.201811	18.384743	-0.042971	2.167758
225.853331	1433.273938	18.389747	-0.042940	2.162581
225.839730	1425.345738	18.394752	-0.042933	2.157402
225.862774	1417.408227	18.399757	-0.042932	2.152209
225.656657	1409.468215	18.404762	-0.042888	2.146979
225.710076	1401.538942	18.409767	-0.042893	2.141769
225.337371	1393.638018	18.414771	-0.042818	2.136524
225.224724	1385.680713	18.419776	-0.042792	2.131253
225.457926	1377.699998	18.424781	-0.042830	2.125987
225.351570	1369.779087	18.429786	-0.042805	2.120715
225.441114	1361.854363	18.434791	-0.042817	2.115446
225.336074	1353.853161	18.439795	-0.042792	2.110094
225.195112	1345.920836	18.444800	-0.042761	2.104771
225.164400	1338.005012	18.449805	-0.042750	2.099457
225.015375	1330.085601	18.454810	-0.042717	2.094115
225.045463	1322.141762	18.459815	-0.042717	2.088760
224.992872	1314.207903	18.464819	-0.042702	2.083390
224.970631	1306.285962	18.469824	-0.042693	2.078017
225.003878	1298.356230	18.474829	-0.042694	2.072631
224.970536	1290.398448	18.479834	-0.042683	2.067205
224.609021	1282.526406	18.484839	-0.042610	2.061790
224.616404	1274.579899	18.489843	-0.042606	2.056347
224.651039	1266.631573	18.494848	-0.042608	2.050891
224.628802	1258.697074	18.499853	-0.042598	2.045424
224.483727	1250.794376	18.504858	-0.042566	2.039952
224.509432	1242.878844	18.509863	-0.042566	2.034474
224.436064	1234.912062	18.514867	-0.042547	2.028935
224.367528	1226.979565	18.519872	-0.042529	2.023406
224.425892	1219.055624	18.524877	-0.042535	2.017880
224.215053	1211.132328	18.529882	-0.042490	2.012312
224.202279	1203.218656	18.534887	-0.042483	2.006756
224.233869	1195.283548	18.539891	-0.042483	2.001173
224.288184	1187.367598	18.544896	-0.042488	1.995591
224.283021	1179.438744	18.549901	-0.042482	1.989978
224.030534	1171.532153	18.554906	-0.042430	1.984339
224.094095	1163.613162	18.559911	-0.042437	1.978708
223.988010	1155.700896	18.564915	-0.042412	1.973048
223.955142	1147.761267	18.569920	-0.042401	1.967360
224.199468	1139.824407	18.574925	-0.042441	1.961687
223.916254	1131.946649	18.579930	-0.042383	1.955984
223.645923	1124.025827	18.584935	-0.042327	1.950234
223.582354	1116.085031	18.589939	-0.042310	1.944474
223.697668	1108.151399	18.594944	-0.042327	1.938723
223.776473	1100.229568	18.599949	-0.042336	1.932959
223.636969	1092.303398	18.604954	-0.042305	1.927150
223.655202	1084.404404	18.609959	-0.042303	1.921362
223.535834	1076.514774	18.614963	-0.042276	1.915547
223.394231	1068.597164	18.619968	-0.042244	1.909692
223.522812	1060.671630	18.624973	-0.042263	1.903843
223.377427	1052.786454	18.629978	-0.042231	1.897975
223.173454	1044.900314	18.634983	-0.042188	1.892081
223.214156	1036.958890	18.639987	-0.042190	1.886156
223.190705	1029.056905	18.644992	-0.042181	1.880234
223.142098	1021.178865	18.649997	-0.042167	1.874308
222.811602	1013.265608	18.655002	-0.042100	1.868305
222.951324	1005.327190	18.660007	-0.042121	1.862317
223.003226	997.408068	18.665011	-0.042125	1.856315
222.937385	989.498939	18.670016	-0.042108	1.850287
222.852974	981.625798	18.675021	-0.042087	1.844264
222.849231	973.718015	18.680026	-0.042081	1.838205
222.600190	965.863450	18.685031	-0.042030	1.832138
222.554252	957.941579	18.690035	-0.042016	1.826023
222.550887	950.038071	18.695040	-0.042010	1.819906
222.598861	942.152167	18.700045	-0.042014	1.813789
222.363369	934.259185	18.705050	-0.041965	1.807611
222.538317	926.349778	18.710055	-0.041992	1.801449
222.450278	918.469042	18.715059	-0.041971	1.795256
222.256253	910.528642	18.720064	-0.041929	1.788981
222.372600	902.621682	18.725069	-0.041946	1.782750
222.247837	894.746686	18.730074	-0.041918	1.776492
222.421108	886.829992	18.735079	-0.041945	1.770215
222.334561	878.964689	18.740083	-0.041923	1.763925
221.984689	871.123454	18.745088	-0.041853	1.757599
222.042048	863.239537	18.750093	-0.041859	1.751266
221.844819	855.353779	18.755098	-0.041817	1.744877
222.128231	847.447527	18.760103	-0.041864	1.738509
221.891528	839.597065	18.765107	-0.041815	1.732097
221.550545	831.731125	18.770112	-0.041747	1.725634
221.704057	823.845907	18.775117	-0.041770	1.719196
221.648788	815.962628	18.780122	-0.041755	1.712707
221.629489	808.064474	18.785127	-0.041746	1.706186
221.580328	800.194983	18.790131	-0.041732	1.699660
221.499578	792.323606	18.795136	-0.041711	1.693104
221.585867	784.426839	18.800141	-0.041722	1.686522
221.459473	776.568596	18.805146	-0.041694	1.679919
221.352392	768.739181	18.810151	-0.041669	1.673317
221.284338	760.855962	18.815155	-0.041651	1.666648
221.225589	752.989967	18.820160	-0.041635	1.659968
221.236479	745.137966	18.825165	-0.041632	1.653282
221.077662	737.269263	18.830170	-0.041597	1.646532
221.009682	729.432227	18.835175	-0.041579	1.639794
220.862751	721.569731	18.840179	-0.041547	1.632995
220.952931	713.635225	18.845184	-0.041558	1.626138
221.063719	705.778560	18.850189	-0.041574	1.619323
220.745350	697.963438	18.855194	-0.041509	1.612455
220.808798	690.091662	18.860199	-0.041516	1.605561
220.586767	682.285970	18.865203	-0.041470	1.598656
220.547589	674.431047	18.870208	-0.041457	1.591703
220.497838	666.584061	18.875213	-0.041443	1.584725
220.604215	658.726373	18.880218	-0.041458	1.577730
220.527740	650.887670	18.885223	-0.041438	1.570693
220.283343	643.079746	18.890227	-0.041388	1.563629
220.328238	635.238973	18.895232	-0.041391	1.556544
220.352909	627.375669	18.900237	-0.041390	1.549404
220.329052	619.525997	18.905242	-0.041381	1.542236
220.285496	611.709336	18.910247	-0.041368	1.535062
220.255082	603.865513	18.915251	-0.041357	1.527831
220.163427	596.052416	18.920256	-0.041335	1.520585
220.014549	588.267147	18.925261	-0.041302	1.513322
220.089758	580.403144	18.930266	-0.041311	1.505984
219.924213	572.622901	18.935271	-0.041275	1.498651
219.636974	564.836052	18.940275	-0.041216	1.491258
219.659189	556.997031	18.945280	-0.041215	1.483826
219.721955	549.192637	18.950285	-0.041222	1.476397
219.448315	541.352689	18.955290	-0.041166	1.468842
219.491119	533.533344	18.960295	-0.041169	1.461318
219.482305	525.730753	18.965299	-0.041162	1.453764
219.354895	517.931025	18.970304	-0.041133	1.446154
219.225630	510.170640	18.975309	-0.041104	1.438542
219.061904	502.379814	18.980314	-0.041068	1.430853
219.178748	494.566821	18.985319	-0.041085	1.423147
219.065019	486.795330	18.990323	-0.041059	1.415403
218.890737	479.015067	18.995328	-0.041021	1.407596
218.905024	471.240465	19.000333	-0.041019	1.399784
218.762468	463.467700	19.005338	-0.040987	1.391903
218.650705	455.692101	19.010343	-0.040961	1.383980
218.621895	447.914067	19.015347	-0.040951	1.376022
218.502829	440.144046	19.020352	-0.040924	1.368011
218.369742	432.409413	19.025357	-0.040894	1.359987
218.386078	424.629429	19.030362	-0.040892	1.351894
218.423694	416.862283	19.035367	-0.040894	1.343769
218.329087	409.125388	19.040371	-0.040871	1.335604
218.158521	401.380002	19.045376	-0.040834	1.327366
218.232515	393.638878	19.050381	-0.040843	1.319125
218.176230	385.821268	19.055386	-0.040827	1.310726
218.089389	378.047364	19.060391	-0.040806	1.302314
217.917006	370.357068	19.065395	-0.040769	1.293924
217.883680	362.615255	19.070400	-0.040758	1.285447
217.850460	354.929522	19.075405	-0.040747	1.276977
217.610142	347.236289	19.080410	-0.040697	1.268402
217.694340	339.513682	19.085415	-0.040707	1.259798
217.511528	331.831512	19.090419	-0.040668	1.251129
217.169691	324.183211	19.095424	-0.040600	1.242407
217.370580	316.455963	19.100429	-0.040632	1.233639
217.198382	308.761684	19.105434	-0.040595	1.224773
217.250050	301.070502	19.110439	-0.040600	1.215890
217.083513	293.412584	19.115443	-0.040564	1.206937
217.002262	285.751967	19.120448	-0.040544	1.197931
217.008106	278.088062	19.125453	-0.040540	1.188870
216.820755	270.448739	19.130458	-0.040500	1.179730
216.769130	262.804344	19.135463	-0.040485	1.170540
216.792806	255.150363	19.140467	-0.040485	1.161282
216.464591	247.551216	19.145472	-0.040418	1.151942
216.487533	239.882442	19.150477	-0.040418	1.142514
216.403879	232.260658	19.155482	-0.040397	1.133044
216.310417	224.656806	19.160487	-0.040375	1.123514
216.064624	217.094497	19.165491	-0.040324	1.113921
215.956433	209.496062	19.170496	-0.040299	1.104230
215.763375	201.941684	19.175501	-0.040258	1.094491
215.642313	194.356579	19.180506	-0.040231	1.084640
215.796815	186.764967	19.185511	-0.040254	1.074753
215.550101	179.226221	19.190515	-0.040204	1.064752
215.127876	171.734732	19.195520	-0.040120	1.054679
215.062387	164.189005	19.200525	-0.040103	1.044518
214.724461	156.710773	19.205530	-0.040035	1.034286
214.527856	149.207928	19.210535	-0.039994	1.023951
214.100653	141.757901	19.215539	-0.039909	1.013528
213.706974	134.302854	19.220544	-0.039831	1.002998
213.116087	126.896643	19.225549	-0.039716	0.992376
212.775059	119.413969	19.230554	-0.039648	0.981592
212.275110	112.010361	19.235559	-0.039550	0.970763
212.029339	104.576437	19.240563	-0.039499	0.959831
211.255259	97.238078	19.245568	-0.039350	0.948779
210.755804	89.880380	19.250573	-0.039253	0.937639
210.085696	82.544425	19.255578	-0.039123	0.926352
209.494752	75.229437	19.260583	-0.039008	0.914980
208.893375	67.901012	19.265587	-0.038891	0.903440
208.470345	60.804188	19.270592	-0.038808	0.892166