Fri Mar 12 13:37:04 2021

Number of Points = 3628
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
-0.008967	-0.064980	0.000000	-0.000062	0.721749

0.153276	-0.094276	0.005005	-0.000093	0.721748
0.066234	-0.081248	0.010010	-0.000076	0.721744
0.137293	-0.090375	0.015014	-0.000090	0.721751
-0.009941	-0.068456	0.020019	-0.000062	0.721742
-0.004291	-0.065301	0.025024	-0.000063	0.721751
0.060043	-0.077877	0.030029	-0.000075	0.721749
-0.019076	-0.065029	0.035034	-0.000061	0.721746
0.077384	-0.077647	0.040038	-0.000079	0.721755
-0.008871	-0.068452	0.045043	-0.000063	0.721743
0.302302	-0.120733	0.050048	-0.000121	0.721749
0.124288	-0.088368	0.055053	-0.000088	0.721751
-0.045928	-0.134748	0.060058	-0.000056	0.721600
0.129464	-0.246584	0.065062	-0.000089	0.721442
-0.112536	-0.206636	0.070067	-0.000044	0.721436
-0.141047	-0.198432	0.075072	-0.000038	0.721442
-0.035126	-0.218731	0.080077	-0.000058	0.721439
0.049101	-0.235525	0.085082	-0.000074	0.721436
0.000356	-0.223598	0.090086	-0.000065	0.721442
-0.212927	-0.314067	0.095091	-0.000025	0.721190
0.064834	-0.395640	0.100096	-0.000077	0.721127
-0.025808	-0.379230	0.105101	-0.000060	0.721127
-0.229516	-0.345940	0.110106	-0.000022	0.721122
0.025322	-0.385615	0.115110	-0.000070	0.721133
-0.036546	-0.459434	0.120115	-0.000058	0.720966
-0.092338	-0.490724	0.125120	-0.000048	0.720885
-0.008169	-0.505920	0.130125	-0.000063	0.720885
-0.043003	-0.503534	0.135130	-0.000057	0.720877
-0.006923	-0.574182	0.140134	-0.000064	0.720751
-0.241565	-0.641810	0.145139	-0.000020	0.720536
0.000616	-0.680506	0.150144	-0.000065	0.720545
-0.132313	-0.657002	0.155149	-0.000041	0.720544
-0.205831	-0.740607	0.160154	-0.000027	0.720354
-0.129377	-0.815942	0.165158	-0.000041	0.720233
-0.278565	-0.793425	0.170163	-0.000013	0.720225
-0.250644	-0.812435	0.175168	-0.000019	0.720197
-0.113096	-0.985756	0.180173	-0.000044	0.719904
-0.158294	-0.979538	0.185178	-0.000036	0.719901
-0.048797	-0.995086	0.190182	-0.000056	0.719909
-0.301777	-1.101372	0.195187	-0.000009	0.719610
-0.044866	-1.149312	0.200192	-0.000057	0.719606
-0.020567	-1.161766	0.205197	-0.000061	0.719590
-0.122611	-1.305670	0.210202	-0.000042	0.719271
0.072408	-1.336335	0.215206	-0.000079	0.719279
0.028035	-1.392869	0.220211	-0.000071	0.719152
0.005545	-1.482408	0.225216	-0.000066	0.718968
-0.150210	-1.454717	0.230221	-0.000037	0.718968
-0.159122	-1.592170	0.235226	-0.000036	0.718693
0.016358	-1.644827	0.240230	-0.000068	0.718651
-0.250688	-1.661092	0.245235	-0.000019	0.718525
-0.144162	-1.764199	0.250240	-0.000039	0.718359
-0.156384	-1.769976	0.255245	-0.000036	0.718344
-0.579372	-1.860148	0.260250	0.000042	0.718017
-0.312395	-1.902375	0.265254	-0.000007	0.718027
-0.412968	-2.001518	0.270259	0.000011	0.717796
-0.490955	-2.030409	0.275264	0.000026	0.717712
-0.446271	-2.112101	0.280269	0.000018	0.717566
-0.349062	-2.224450	0.285274	-0.000000	0.717378
-0.494678	-2.239928	0.290278	0.000027	0.717297
-0.821663	-2.288836	0.295283	0.000087	0.717085
-0.679195	-2.335331	0.300288	0.000061	0.717043
-1.946780	-2.252821	0.305293	0.000297	0.716760
-3.372684	-2.002820	0.310298	0.000562	0.716752
-2.772556	-2.164818	0.315302	0.000450	0.716643
-3.540552	-2.125246	0.320307	0.000593	0.716451
-3.787912	-2.080287	0.325312	0.000639	0.716452
-4.030219	-2.074106	0.330317	0.000684	0.716379
-4.532320	-2.109047	0.335322	0.000778	0.716133
-4.537452	-2.106369	0.340326	0.000779	0.716137
-4.986162	-2.030387	0.345331	0.000862	0.716129
-4.854445	-2.142421	0.350336	0.000838	0.715953
-5.640784	-2.036149	0.355341	0.000984	0.715887
-5.833035	-2.004314	0.360346	0.001020	0.715882
-4.859045	-2.174244	0.365350	0.000838	0.715889
-5.975388	-2.133491	0.370355	0.001046	0.715576
-6.728041	-2.013712	0.375360	0.001186	0.715548
-6.205599	-2.104271	0.380365	0.001089	0.715553
-6.164814	-2.115010	0.385370	0.001081	0.715546
-6.721126	-2.116012	0.390374	0.001185	0.715347
-7.679996	-2.005529	0.395379	0.001363	0.715228
-7.047745	-2.114473	0.400384	0.001246	0.715235
-7.450724	-2.041827	0.405389	0.001321	0.715237
-7.665621	-2.006701	0.410394	0.001360	0.715231
-7.426053	-2.158840	0.415398	0.001316	0.715014
-8.461394	-2.026442	0.420403	0.001509	0.714911
-8.803254	-1.965430	0.425408	0.001572	0.714911
-8.077592	-2.094088	0.430413	0.001437	0.714912
-8.214497	-2.072342	0.435418	0.001462	0.714907
-8.117462	-2.149101	0.440422	0.001444	0.714789
-9.584340	-1.979786	0.445427	0.001717	0.714607
-9.172044	-2.049984	0.450432	0.001641	0.714613
-9.079315	-2.065413	0.455437	0.001623	0.714615
-9.446057	-2.004449	0.460442	0.001691	0.714607
-8.966470	-2.086164	0.465446	0.001602	0.714614
-9.358083	-2.100212	0.470451	0.001675	0.714448
-10.751639	-1.935497	0.475456	0.001934	0.714282
-9.813855	-2.100773	0.480461	0.001760	0.714286
-10.180923	-2.038491	0.485466	0.001828	0.714280
-10.393148	-1.997822	0.490470	0.001868	0.714286
-10.396784	-2.000602	0.495475	0.001868	0.714279
-10.088308	-2.062681	0.500480	0.001811	0.714265
-10.616236	-2.113635	0.505485	0.001909	0.713977
-11.274335	-1.999734	0.510490	0.002031	0.713970
-11.255351	-1.998216	0.515494	0.002028	0.713980
-10.865286	-2.071687	0.520499	0.001955	0.713972
-11.258848	-1.998672	0.525504	0.002028	0.713978
-11.089578	-2.027818	0.530509	0.001997	0.713980
-11.171100	-2.104020	0.535514	0.002012	0.713800
-12.187261	-1.992008	0.540518	0.002201	0.713663
-12.173269	-1.998593	0.545523	0.002198	0.713655
-11.985300	-2.030483	0.550528	0.002163	0.713658
-11.971297	-2.032594	0.555533	0.002161	0.713659
-12.247148	-1.986283	0.560538	0.002212	0.713653
-11.751060	-2.071616	0.565542	0.002120	0.713660
-11.961326	-2.141636	0.570547	0.002159	0.713446
-12.995110	-1.999251	0.575552	0.002351	0.713363
-12.851357	-2.021615	0.580557	0.002324	0.713369
-12.893836	-2.020492	0.585562	0.002332	0.713357
-13.015700	-1.992078	0.590566	0.002355	0.713370
-13.263572	-1.951063	0.595571	0.002401	0.713364
-12.927922	-2.009345	0.600576	0.002338	0.713367
-12.924839	-2.136434	0.605581	0.002338	0.713116
-14.173781	-1.959376	0.610586	0.002570	0.713025
-13.987167	-1.987458	0.615590	0.002535	0.713036
-13.360724	-2.104221	0.620595	0.002419	0.713025
-13.920665	-2.004110	0.625600	0.002523	0.713026
-13.692704	-2.041716	0.630605	0.002481	0.713032
-13.758651	-2.034604	0.635610	0.002493	0.713023
-14.101752	-2.113199	0.640614	0.002557	0.712745
-14.900477	-1.986222	0.645619	0.002705	0.712715
-14.920811	-1.983235	0.650624	0.002709	0.712713
-14.524156	-2.052470	0.655629	0.002635	0.712716
-15.070109	-1.958573	0.660634	0.002737	0.712710
-14.648914	-2.027358	0.665638	0.002658	0.712722
-14.367504	-2.083781	0.670643	0.002606	0.712710
-15.296009	-2.056122	0.675648	0.002779	0.712436
-15.759599	-1.994297	0.680653	0.002865	0.712394
-15.664345	-2.015315	0.685658	0.002847	0.712386
-15.288474	-2.079124	0.690662	0.002777	0.712393
-15.917305	-1.969163	0.695667	0.002894	0.712389
-15.503493	-2.043220	0.700672	0.002817	0.712388
-15.165854	-2.101079	0.705677	0.002754	0.712393
-16.321860	-2.022239	0.710682	0.002969	0.712140
-16.678413	-1.980337	0.715686	0.003036	0.712097
-16.354442	-2.040267	0.720691	0.002975	0.712092
-16.338320	-2.043384	0.725696	0.002972	0.712092
-16.565459	-2.000492	0.730701	0.003014	0.712097
-16.358499	-2.040082	0.735706	0.002976	0.712092
-15.931742	-2.111198	0.740710	0.002896	0.712102
-17.044477	-2.059939	0.745715	0.003103	0.711809
-17.715097	-1.961474	0.750720	0.003228	0.711767
-17.189057	-2.053457	0.755725	0.003130	0.711770
-17.300321	-2.037829	0.760730	0.003151	0.711762
-17.315717	-2.030319	0.765734	0.003154	0.711772
-17.249057	-2.046161	0.770739	0.003141	0.711764
-17.472222	-2.005660	0.775744	0.003183	0.711765
-17.688518	-2.065182	0.780749	0.003223	0.711570
-18.531024	-1.973685	0.785754	0.003380	0.711453
-18.119030	-2.041827	0.790758	0.003303	0.711464
-18.439468	-1.988766	0.795763	0.003363	0.711456
-18.563550	-1.966430	0.800768	0.003386	0.711456
-17.951788	-2.072048	0.805773	0.003272	0.711463
-18.441197	-1.988487	0.810778	0.003363	0.711456
-18.405814	-2.043790	0.815782	0.003356	0.711358
-19.135220	-2.022886	0.820787	0.003492	0.711141
-18.947633	-2.054172	0.825792	0.003457	0.711145
-19.238353	-2.000850	0.830797	0.003511	0.711148
-19.224414	-2.010775	0.835802	0.003508	0.711134
-18.816522	-2.077603	0.840806	0.003432	0.711145
-19.155623	-2.020940	0.845811	0.003496	0.711138
-19.273060	-2.057748	0.850816	0.003517	0.711023
-19.600929	-2.070067	0.855821	0.003578	0.710882
-19.844818	-2.032284	0.860826	0.003624	0.710871
-19.873902	-2.022028	0.865830	0.003629	0.710881
-19.942424	-2.012916	0.870835	0.003642	0.710875
-19.773083	-2.042437	0.875840	0.003610	0.710876
-19.963459	-2.007505	0.880845	0.003646	0.710878
-20.334564	-2.075383	0.885850	0.003715	0.710611
-20.797036	-2.028814	0.890854	0.003801	0.710539
-21.019833	-1.990801	0.895859	0.003842	0.710536
-20.802573	-2.027729	0.900864	0.003802	0.710540
-20.360615	-2.106147	0.905869	0.003719	0.710540
-20.843109	-2.023260	0.910874	0.003809	0.710534
-20.958327	-1.999025	0.915878	0.003830	0.710542
-21.243647	-2.085052	0.920883	0.003884	0.710268
-21.762772	-2.015712	0.925888	0.003980	0.710222
-21.877401	-1.993927	0.930893	0.004001	0.710225
-22.091922	-1.957972	0.935898	0.004041	0.710221
-21.635104	-2.035993	0.940902	0.003956	0.710227
-21.733739	-2.020924	0.945907	0.003975	0.710223
-21.713290	-2.026062	0.950912	0.003971	0.710220
-21.608347	-2.144831	0.955917	0.003951	0.710020
-22.799113	-1.996508	0.960922	0.004173	0.709892
-22.500456	-2.045253	0.965926	0.004117	0.709901
-22.547992	-2.040226	0.970931	0.004126	0.709894
-22.658886	-2.020668	0.975936	0.004147	0.709894
-22.554631	-2.035548	0.980941	0.004127	0.709902
-22.746509	-2.005384	0.985946	0.004163	0.709894
-22.567750	-2.145573	0.990950	0.004129	0.709677
-23.338084	-2.047011	0.995955	0.004273	0.709600
-23.978597	-1.934236	1.000960	0.004392	0.709597
-23.406942	-2.032768	1.005965	0.004285	0.709604
-23.300007	-2.056440	1.010970	0.004266	0.709595
-23.450715	-2.026039	1.015974	0.004294	0.709602
-23.355321	-2.045782	1.020979	0.004276	0.709597
-23.716578	-2.127990	1.025984	0.004343	0.709303
-24.144467	-2.067773	1.030989	0.004423	0.709271
-24.631062	-1.984688	1.035994	0.004513	0.709264
-24.179625	-2.061916	1.040998	0.004429	0.709271
-24.125167	-2.073659	1.046003	0.004419	0.709267
-24.731907	-1.964677	1.051008	0.004532	0.709269
-24.086165	-2.079772	1.056013	0.004411	0.709269
-25.001342	-2.074103	1.061018	0.004582	0.708954
-25.299528	-2.018161	1.066022	0.004637	0.708959
-25.476054	-1.988152	1.071027	0.004670	0.708957
-25.237044	-2.030135	1.076032	0.004626	0.708958
-25.297002	-2.016379	1.081037	0.004637	0.708964
-25.603125	-1.966625	1.086042	0.004694	0.708955
-25.115270	-2.049060	1.091046	0.004603	0.708964
-25.337220	-2.104200	1.096051	0.004644	0.708774
-26.838654	-1.903956	1.101056	0.004923	0.708639
-26.178033	-2.018395	1.106061	0.004800	0.708646
-26.172610	-2.024086	1.111066	0.004799	0.708637
-26.469061	-1.966233	1.116070	0.004855	0.708647
-26.063097	-2.039805	1.121075	0.004779	0.708645
-25.925722	-2.065702	1.126080	0.004753	0.708642
-26.132491	-2.072735	1.131085	0.004792	0.708554
-27.354574	-1.956027	1.136090	0.005019	0.708352
-26.789818	-2.052410	1.141094	0.004914	0.708360
-26.923922	-2.032686	1.146099	0.004939	0.708352
-27.168519	-1.988009	1.151104	0.004984	0.708354
-26.789502	-2.051521	1.156109	0.004914	0.708362
-26.918942	-2.034070	1.161114	0.004938	0.708351
-26.833329	-2.127740	1.166118	0.004922	0.708194
-27.896955	-2.027965	1.171123	0.005120	0.708014
-27.631750	-2.075556	1.176128	0.005070	0.708014
-27.603130	-2.078214	1.181133	0.005065	0.708019
-28.320927	-1.953322	1.186138	0.005199	0.708013
-27.670863	-2.064603	1.191142	0.005078	0.708022
-27.387069	-2.117298	1.196147	0.005025	0.708018
-28.658999	-2.026411	1.201152	0.005261	0.707746
-28.806806	-2.017665	1.206157	0.005289	0.707711
-28.657881	-2.048967	1.211162	0.005261	0.707701
-28.688673	-2.040103	1.216166	0.005267	0.707708
-28.920669	-2.001874	1.221171	0.005310	0.707702
-28.980653	-1.991932	1.226176	0.005321	0.707700
-28.354670	-2.099781	1.231181	0.005205	0.707708
-29.059599	-2.077370	1.236186	0.005336	0.707501
-30.039132	-1.961522	1.241190	0.005518	0.707383
-29.487640	-2.062205	1.246195	0.005415	0.707379
-29.627851	-2.038818	1.251200	0.005441	0.707375
-29.920548	-1.982105	1.256205	0.005496	0.707385
-29.769026	-2.013245	1.261210	0.005468	0.707376
-29.778512	-2.007363	1.266214	0.005469	0.707385
-29.759853	-2.049515	1.271219	0.005466	0.707307
-30.540999	-2.022550	1.276224	0.005611	0.707082
-30.245007	-2.073221	1.281229	0.005556	0.707086
-31.092952	-1.925623	1.286234	0.005714	0.707079
-30.543347	-2.020295	1.291238	0.005611	0.707086
-30.227059	-2.078471	1.296243	0.005552	0.707082
-30.876663	-1.964439	1.301248	0.005673	0.707079
-30.563953	-2.043321	1.306253	0.005615	0.707033
-31.157826	-2.079380	1.311258	0.005726	0.706748
-31.213410	-2.065207	1.316262	0.005736	0.706756
-31.828228	-1.956207	1.321267	0.005850	0.706755
-31.771118	-1.967990	1.326272	0.005840	0.706752
-31.108073	-2.083741	1.331277	0.005716	0.706757
-31.650060	-1.991492	1.336282	0.005817	0.706748
-31.766117	-1.965957	1.341286	0.005839	0.706758
-31.669723	-2.127368	1.346291	0.005821	0.706469
-32.319563	-2.024669	1.351296	0.005942	0.706442
-32.379515	-2.009719	1.356301	0.005953	0.706451
-32.135907	-2.057698	1.361306	0.005907	0.706442
-32.146544	-2.053908	1.366310	0.005909	0.706446
-32.384632	-2.012720	1.371315	0.005953	0.706443
-32.323245	-2.055328	1.376320	0.005942	0.706380
-32.680650	-2.112588	1.381325	0.006009	0.706137
-33.063828	-2.049806	1.386330	0.006080	0.706126
-33.276461	-2.008456	1.391334	0.006119	0.706133
-32.831941	-2.089065	1.396339	0.006037	0.706130
-33.073156	-2.048017	1.401344	0.006081	0.706126
-33.378141	-1.989234	1.406349	0.006138	0.706135
-33.349305	-2.053741	1.411354	0.006133	0.706016
-33.881267	-2.032706	1.416358	0.006232	0.705868
-33.749915	-2.057490	1.421363	0.006207	0.705865
-33.954175	-2.023610	1.426368	0.006245	0.705860
-33.735553	-2.058362	1.431373	0.006204	0.705869
-33.898993	-2.033932	1.436378	0.006235	0.705859
-34.320174	-1.954436	1.441382	0.006313	0.705868
-33.993839	-2.132054	1.446387	0.006252	0.705628
-35.078088	-1.990565	1.451392	0.006454	0.705524
-34.940195	-2.011782	1.456397	0.006428	0.705531
-34.829846	-2.035071	1.461402	0.006408	0.705524
-34.810904	-2.035471	1.466406	0.006404	0.705530
-34.742254	-2.050939	1.471411	0.006391	0.705523
-35.014089	-2.002993	1.476416	0.006442	0.705522
-34.921914	-2.136791	1.481421	0.006425	0.705286
-35.883074	-2.005623	1.486426	0.006604	0.705206
-35.933804	-1.992673	1.491430	0.006613	0.705214
-35.530589	-2.064681	1.496435	0.006538	0.705213
-35.732764	-2.030742	1.501440	0.006576	0.705209
-35.716580	-2.028946	1.506445	0.006572	0.705219
-35.713500	-2.034390	1.511450	0.006572	0.705209
-35.935340	-2.135989	1.516454	0.006613	0.704925
-36.697456	-2.018424	1.521459	0.006755	0.704888
-37.101022	-1.947224	1.526464	0.006830	0.704887
-36.395862	-2.069924	1.531469	0.006699	0.704893
-36.464018	-2.062317	1.536474	0.006711	0.704884
-36.858913	-1.987587	1.541478	0.006785	0.704893
-36.500681	-2.053050	1.546483	0.006718	0.704890
-36.773619	-2.134469	1.551488	0.006769	0.704628
-37.501029	-2.019556	1.556493	0.006904	0.704598
-37.668939	-1.994202	1.561498	0.006935	0.704589
-37.245175	-2.065306	1.566502	0.006857	0.704598
-37.450406	-2.030974	1.571507	0.006895	0.704593
-37.749899	-1.978791	1.576512	0.006950	0.704591
-37.409251	-2.035309	1.581517	0.006887	0.704600
-38.130116	-2.066938	1.586522	0.007021	0.704277
-38.627001	-1.984711	1.591526	0.007114	0.704264
-38.458814	-2.013893	1.596531	0.007082	0.704266
-38.290981	-2.045876	1.601536	0.007051	0.704262
-38.352373	-2.031302	1.606541	0.007062	0.704269
-38.774624	-1.960793	1.611546	0.007141	0.704260
-38.260342	-2.050323	1.616550	0.007045	0.704264
-38.497263	-2.107852	1.621555	0.007089	0.704063
-39.987908	-1.898605	1.626560	0.007366	0.703949
-39.003828	-2.068955	1.631565	0.007183	0.703960
-38.842910	-2.103228	1.636570	0.007153	0.703949
-39.344516	-2.010866	1.641574	0.007247	0.703955
-39.326072	-2.014861	1.646579	0.007243	0.703953
-39.444157	-1.994863	1.651584	0.007265	0.703951
-39.471022	-2.084417	1.656589	0.007270	0.703761
-40.481828	-1.966995	1.661594	0.007458	0.703634
-39.912973	-2.067537	1.666598	0.007352	0.703636
-39.831757	-2.081253	1.671603	0.007337	0.703638
-40.342074	-1.992676	1.676608	0.007432	0.703633
-39.905699	-2.066542	1.681613	0.007351	0.703641
-40.058155	-2.043858	1.686618	0.007379	0.703632
-40.695955	-2.043776	1.691622	0.007498	0.703403
-40.942681	-2.029028	1.696627	0.007544	0.703344
-40.937855	-2.031715	1.701632	0.007543	0.703341
-40.910832	-2.032793	1.706637	0.007538	0.703348
-41.413629	-1.948260	1.711642	0.007631	0.703338
-41.016405	-2.016271	1.716646	0.007557	0.703344
-40.536154	-2.101675	1.721651	0.007468	0.703344
-41.685812	-2.036407	1.726656	0.007682	0.703062
-42.137690	-1.981625	1.731661	0.007766	0.703010
-41.634694	-2.073907	1.736666	0.007672	0.703005
-41.574469	-2.081061	1.741670	0.007661	0.703012
-42.091681	-1.990244	1.746675	0.007757	0.703010
-41.843512	-2.037787	1.751680	0.007711	0.703003
-41.479729	-2.099684	1.756685	0.007643	0.703009
-42.429293	-2.076779	1.761690	0.007820	0.702714
-42.724576	-2.033641	1.766694	0.007875	0.702694
-42.556729	-2.061956	1.771699	0.007843	0.702698
-42.761312	-2.029429	1.776704	0.007881	0.702690
-42.701878	-2.035323	1.781709	0.007870	0.702700
-42.712372	-2.037750	1.786714	0.007872	0.702691
-42.740085	-2.035754	1.791718	0.007877	0.702685
-43.420098	-2.066009	1.796723	0.008004	0.702379
-43.409818	-2.071250	1.801728	0.008002	0.702372
-43.569874	-2.038590	1.806733	0.008032	0.702381
-44.035927	-1.958858	1.811738	0.008118	0.702374
-43.727178	-2.012801	1.816742	0.008061	0.702376
-43.093094	-2.125100	1.821747	0.007943	0.702378
-43.608972	-2.050537	1.826752	0.008039	0.702343
-44.361640	-2.044372	1.831757	0.008179	0.702084
-44.169923	-2.083314	1.836762	0.008143	0.702074
-44.452958	-2.031544	1.841766	0.008196	0.702077
-44.338871	-2.051434	1.846771	0.008175	0.702078
-44.448942	-2.034287	1.851776	0.008195	0.702073
-44.358813	-2.045775	1.856781	0.008178	0.702083
-44.546758	-2.061434	1.861786	0.008213	0.701983
-45.468671	-2.012946	1.866790	0.008385	0.701749
-45.102565	-2.077891	1.871795	0.008316	0.701750
-45.462127	-2.015560	1.876800	0.008383	0.701746
-45.298044	-2.041858	1.881805	0.008353	0.701752
-45.293280	-2.046537	1.886810	0.008352	0.701745
-45.429242	-2.019024	1.891814	0.008377	0.701751
-45.400711	-2.054284	1.896819	0.008372	0.701690
-46.073809	-2.059825	1.901824	0.008497	0.701436
-45.812393	-2.101824	1.906829	0.008448	0.701446
-46.685733	-1.949109	1.911834	0.008611	0.701440
-46.613199	-1.962593	1.916838	0.008597	0.701439
-45.877381	-2.091615	1.921843	0.008460	0.701443
-46.327362	-2.013544	1.926848	0.008544	0.701439
-46.526885	-1.974621	1.931853	0.008581	0.701446
-46.725197	-2.098229	1.936858	0.008618	0.701124
-46.748958	-2.092230	1.941862	0.008622	0.701128
-47.404831	-1.975977	1.946867	0.008744	0.701126
-47.243566	-2.009330	1.951872	0.008714	0.701117
-46.538359	-2.128620	1.956877	0.008583	0.701130
-46.942959	-2.060527	1.961882	0.008658	0.701122
-47.149528	-2.067013	1.966886	0.008697	0.701035
-47.714396	-2.042075	1.971891	0.008802	0.700881
-47.730627	-2.044853	1.976896	0.008805	0.700870
-47.775362	-2.032379	1.981901	0.008813	0.700879
-47.860949	-2.021403	1.986906	0.008829	0.700870
-47.514780	-2.079946	1.991910	0.008764	0.700877
-47.811214	-2.026748	1.996915	0.008820	0.700878
-48.356454	-2.080503	2.001920	0.008921	0.700572

-48.807956	-2.017202	2.011917	0.009005	0.700537
-48.575081	-2.058789	2.021914	0.008962	0.700537
-48.899912	-2.000419	2.031910	0.009022	0.700538
-48.552871	-2.062365	2.041907	0.008957	0.700538
-48.859667	-2.007675	2.051904	0.009014	0.700539
-48.694668	-2.037774	2.061901	0.008983	0.700537
-48.699804	-2.035645	2.071898	0.008984	0.700540
-48.756275	-2.024399	2.081894	0.008995	0.700543
-48.676647	-2.039853	2.091891	0.008980	0.700540
-48.882327	-2.003541	2.101888	0.009018	0.700540
-48.630405	-2.049835	2.111885	0.008971	0.700537
-48.590418	-2.056408	2.121882	0.008963	0.700538
-48.182286	-1.974928	2.131878	0.008887	0.700851
-47.699743	-2.048385	2.141875	0.008797	0.700877
-47.902976	-2.012511	2.151872	0.008835	0.700876
-47.641679	-2.059744	2.161869	0.008786	0.700875
-47.628697	-2.060922	2.171866	0.008784	0.700878
-47.501133	-2.034430	2.181862	0.008760	0.700978
-46.879583	-2.071558	2.191859	0.008644	0.701127
-47.269526	-2.002351	2.201856	0.008717	0.701127
-47.215307	-2.013004	2.211853	0.008706	0.701125
-46.771984	-2.012621	2.221850	0.008624	0.701286
-46.112339	-2.051410	2.231846	0.008501	0.701446
-46.130723	-2.049117	2.241843	0.008504	0.701444
-46.373216	-2.006359	2.251840	0.008549	0.701443
-45.647756	-2.033889	2.261837	0.008414	0.701650
-45.644857	-1.985342	2.271834	0.008413	0.701749
-45.398209	-2.029381	2.281830	0.008367	0.701749
-45.176091	-2.055451	2.291827	0.008326	0.701777
-44.742273	-1.984133	2.301824	0.008245	0.702078
-44.499603	-2.029549	2.311821	0.008200	0.702074
-44.410567	-2.044208	2.321818	0.008183	0.702076
-44.305992	-1.994359	2.331814	0.008163	0.702215
-43.607769	-2.041765	2.341811	0.008033	0.702371
-43.717199	-2.022079	2.351808	0.008054	0.702372
-43.621768	-2.033317	2.361805	0.008036	0.702384
-42.921233	-2.005125	2.371802	0.007905	0.702693
-42.754399	-2.033035	2.381798	0.007874	0.702697
-42.583639	-2.062303	2.391795	0.007842	0.702700
-42.526775	-1.998737	2.401792	0.007831	0.702849
-41.727019	-2.062156	2.411789	0.007682	0.703009
-42.009982	-2.011607	2.421786	0.007735	0.703009
-41.858808	-2.039742	2.431782	0.007707	0.703007
-41.101776	-2.014430	2.441779	0.007566	0.703331
-41.020480	-2.021937	2.451776	0.007550	0.703345
-40.919603	-2.039710	2.461773	0.007532	0.703346
-41.028287	-1.960380	2.471770	0.007552	0.703467
-39.874420	-2.080930	2.481766	0.007337	0.703639
-40.107943	-2.037920	2.491763	0.007380	0.703642
-40.175413	-2.027188	2.501760	0.007393	0.703640
-39.457843	-2.014368	2.511757	0.007259	0.703924
-39.505085	-1.991357	2.521754	0.007268	0.703953
-38.979566	-2.083016	2.531750	0.007170	0.703958
-39.136944	-1.988478	2.541747	0.007199	0.704092
-38.531050	-2.010973	2.551744	0.007086	0.704265
-38.448158	-2.026895	2.561741	0.007070	0.704263
-38.557502	-1.993193	2.571738	0.007091	0.704291
-37.594424	-2.014187	2.581734	0.006911	0.704595
-37.586977	-2.015418	2.591731	0.006910	0.704596
-37.594591	-2.015438	2.601728	0.006911	0.704593
-37.269309	-1.972514	2.611725	0.006850	0.704797
-36.948542	-1.982810	2.621722	0.006791	0.704891
-36.746793	-2.018331	2.631718	0.006753	0.704892
-36.677442	-1.966102	2.641715	0.006740	0.705023
-35.832167	-2.022101	2.651712	0.006582	0.705213
-36.143371	-1.967380	2.661709	0.006640	0.705212
-35.997227	-1.985067	2.671706	0.006613	0.705229
-35.142718	-1.990447	2.681702	0.006454	0.705525
-35.000385	-2.014519	2.691699	0.006427	0.705528
-34.855656	-2.040378	2.701696	0.006400	0.705528
-34.829564	-1.966662	2.711693	0.006395	0.705686
-34.091969	-2.011022	2.721690	0.006258	0.705861
-33.887993	-2.044799	2.731686	0.006220	0.705867
-34.178490	-1.992800	2.741683	0.006274	0.705867
-33.401054	-2.008358	2.751680	0.006129	0.706115
-33.562799	-1.972198	2.761677	0.006159	0.706130
-33.009964	-2.069949	2.771674	0.006056	0.706132
-33.009589	-1.992784	2.781670	0.006055	0.706287
-32.455234	-2.011474	2.791667	0.005952	0.706448
-32.494021	-2.005085	2.801664	0.005959	0.706447
-32.548110	-1.979322	2.811661	0.005969	0.706480
-31.763357	-1.982954	2.821658	0.005823	0.706754
-31.368600	-2.052445	2.831654	0.005749	0.706756
-31.591951	-2.013196	2.841651	0.005791	0.706755
-30.887116	-2.028526	2.851648	0.005660	0.706977
-30.894230	-1.973871	2.861645	0.005661	0.707084
-30.579614	-2.031332	2.871642	0.005602	0.707081
-30.712696	-1.980496	2.881638	0.005627	0.707136
-29.905493	-2.001856	2.891635	0.005476	0.707382
-29.698941	-2.039081	2.901632	0.005438	0.707382
-30.038037	-1.979943	2.911629	0.005501	0.707379
-29.306349	-1.985381	2.921626	0.005365	0.707630
-28.899074	-2.020901	2.931622	0.005289	0.707705
-28.868080	-2.026835	2.941619	0.005283	0.707704
-28.886233	-1.981690	2.951616	0.005286	0.707788
-28.180980	-1.995668	2.961613	0.005155	0.708012
-27.630248	-2.093303	2.971610	0.005052	0.708014
-28.130444	-2.003311	2.981606	0.005145	0.708016
-27.466214	-2.018361	2.991603	0.005021	0.708223
-27.006872	-2.033953	3.001600	0.004936	0.708356
-27.439074	-1.959474	3.011597	0.005016	0.708351
-27.015498	-2.017437	3.021594	0.004937	0.708386
-26.359025	-2.005527	3.031590	0.004815	0.708645
-26.207940	-2.031772	3.041587	0.004786	0.708646
-26.303041	-2.016480	3.051584	0.004804	0.708643
-26.110568	-1.944461	3.061581	0.004768	0.708856
-25.564965	-1.989454	3.071578	0.004666	0.708961
-25.673169	-1.970696	3.081574	0.004686	0.708960
-25.310004	-1.974576	3.091571	0.004619	0.709082
-24.537954	-2.019801	3.101568	0.004475	0.709267
-24.808744	-1.971637	3.111565	0.004525	0.709267
-24.562512	-2.014564	3.121562	0.004479	0.709269
-24.094821	-1.933044	3.131558	0.004392	0.709599
-23.680647	-2.006017	3.141555	0.004315	0.709601
-23.757877	-1.992037	3.151552	0.004329	0.709602
-23.512349	-1.946283	3.161549	0.004283	0.709781
-22.609625	-2.049448	3.171546	0.004115	0.709897
-23.085788	-1.964686	3.181542	0.004204	0.709897
-22.743602	-2.011888	3.191539	0.004140	0.709925
-22.351655	-1.933368	3.201536	0.004067	0.710221
-21.892768	-2.015712	3.211533	0.003981	0.710220
-21.831969	-2.026097	3.221530	0.003970	0.710221
-21.614946	-1.977526	3.231526	0.003929	0.710396
-20.758096	-2.057901	3.241523	0.003770	0.710541
-21.161009	-1.986353	3.251520	0.003844	0.710540
-20.860702	-2.040279	3.261517	0.003789	0.710540
-20.414677	-1.974037	3.271514	0.003705	0.710831
-20.112883	-2.003918	3.281510	0.003649	0.710879
-20.010778	-2.022093	3.291507	0.003630	0.710879
-20.270703	-1.938796	3.301504	0.003678	0.710953
-19.391320	-2.002992	3.311501	0.003514	0.711138
-19.483514	-1.987522	3.321498	0.003531	0.711136
-19.569936	-1.963837	3.331494	0.003547	0.711153
-18.465780	-2.008311	3.341491	0.003342	0.711457
-18.775306	-1.953527	3.351488	0.003399	0.711456
-18.488862	-2.005176	3.361485	0.003346	0.711455
-18.190036	-1.955421	3.371482	0.003290	0.711661
-17.701548	-1.991490	3.381478	0.003199	0.711763
-17.735794	-1.983447	3.391475	0.003205	0.711767
-17.619954	-1.963377	3.401472	0.003184	0.711848
-16.599264	-2.022188	3.411469	0.002994	0.712094
-16.726956	-2.000434	3.421466	0.003017	0.712092
-16.903990	-1.967652	3.431462	0.003050	0.712094
-16.090582	-2.007645	3.441459	0.002898	0.712304
-16.171987	-1.950121	3.451456	0.002913	0.712390
-15.932714	-1.993911	3.461453	0.002869	0.712387
-16.045744	-1.914305	3.471450	0.002890	0.712506
-14.936246	-2.008126	3.481446	0.002683	0.712713
-15.261094	-1.948380	3.491443	0.002743	0.712717
-15.016300	-1.993821	3.501440	0.002698	0.712714
-14.336166	-1.969087	3.511437	0.002571	0.713004
-14.066894	-2.004516	3.521434	0.002521	0.713029
-14.062870	-2.005134	3.531430	0.002520	0.713030
-13.953425	-1.976973	3.541427	0.002499	0.713125
-13.057904	-2.015710	3.551424	0.002333	0.713365
-13.035373	-2.019153	3.561421	0.002328	0.713367
-13.442841	-1.947241	3.571418	0.002404	0.713366
-12.555180	-2.024582	3.581414	0.002239	0.713526
-12.413624	-1.983711	3.591411	0.002212	0.713658
-12.384907	-1.989239	3.601408	0.002207	0.713657
-12.311259	-1.994635	3.611405	0.002193	0.713673
-11.712602	-1.950727	3.621402	0.002081	0.713972
-11.433686	-1.999691	3.631398	0.002029	0.713974
-11.581184	-1.974099	3.641395	0.002057	0.713973
-11.188913	-1.941230	3.651392	0.001984	0.714177
-10.801351	-1.959232	3.661389	0.001911	0.714279
-10.654181	-1.984132	3.671386	0.001884	0.714282
-10.398395	-1.986243	3.681382	0.001836	0.714368
-9.620841	-2.001327	3.691379	0.001691	0.714614
-9.628511	-2.000097	3.701376	0.001693	0.714613
-9.684208	-1.990980	3.711373	0.001703	0.714612
-9.458191	-1.950993	3.721370	0.001661	0.714772
-8.642167	-2.025431	3.731366	0.001509	0.714913
-8.746955	-2.007963	3.741363	0.001528	0.714910
-8.637306	-2.028027	3.751360	0.001508	0.714909
-7.682676	-2.041617	3.761357	0.001330	0.715220
-7.799368	-2.014149	3.771354	0.001351	0.715234
-7.527598	-2.061321	3.781350	0.001301	0.715236
-7.712543	-2.023270	3.791347	0.001335	0.715247
-6.745663	-2.043691	3.801344	0.001155	0.715548
-6.805001	-2.033966	3.811341	0.001166	0.715546
-6.754593	-2.042176	3.821338	0.001156	0.715548
-6.743472	-2.001602	3.831334	0.001154	0.715633
-5.766768	-2.046872	3.841331	0.000972	0.715888
-5.618887	-2.073786	3.851328	0.000945	0.715887
-5.961039	-2.013011	3.861325	0.001008	0.715887
-5.576096	-2.037469	3.871322	0.000936	0.715974
-4.791570	-2.095151	3.881318	0.000790	0.716137
-5.045766	-2.048073	3.891315	0.000837	0.716141
-4.945232	-2.067854	3.901312	0.000819	0.716137
-4.489662	-2.021375	3.911309	0.000734	0.716390
-4.005970	-2.076927	3.921306	0.000643	0.716451
-4.010326	-2.074709	3.931302	0.000644	0.716454
-4.133676	-2.016282	3.941299	0.000667	0.716527
-3.079101	-2.085945	3.951296	0.000471	0.716761
-3.320328	-2.043547	3.961293	0.000515	0.716760
-3.183967	-2.069513	3.971290	0.000490	0.716757
-2.930222	-1.995299	3.981286	0.000443	0.716993
-2.220313	-2.074444	3.991283	0.000310	0.717087
-2.221579	-2.073327	4.001280	0.000310	0.717089
-2.389139	-2.016554	4.011277	0.000341	0.717142
-1.601712	-2.034921	4.021274	0.000195	0.717384
-1.769113	-2.004450	4.031270	0.000226	0.717385
-1.454760	-2.060184	4.041267	0.000167	0.717386
-1.661740	-1.883512	4.051264	0.000206	0.717662
-1.314892	-1.921664	4.061261	0.000141	0.717709
-1.295900	-1.904068	4.071258	0.000137	0.717751
-1.643090	-1.704726	4.081254	0.000202	0.718023
-1.037137	-1.812315	4.091251	0.000089	0.718024
-1.182849	-1.642792	4.101248	0.000116	0.718307
-0.812347	-1.683549	4.111245	0.000047	0.718357
-0.723672	-1.594424	4.121242	0.000030	0.718565
-0.802170	-1.537108	4.131238	0.000044	0.718651
-0.788257	-1.426307	4.141235	0.000042	0.718874
-1.132697	-1.313369	4.151232	0.000106	0.718976
-0.826438	-1.216979	4.161229	0.000048	0.719274
-0.818699	-1.145927	4.171226	0.000047	0.719417
-0.591206	-1.089852	4.181222	0.000004	0.719608
-0.599382	-0.948552	4.191219	0.000006	0.719884
-0.480957	-0.881956	4.201216	-0.000016	0.720057
-0.436809	-0.789174	4.211213	-0.000025	0.720255
-0.206403	-0.682573	4.221210	-0.000068	0.720546
-0.192320	-0.562209	4.231206	-0.000071	0.720788
-0.202635	-0.456050	4.241203	-0.000069	0.720993
-0.279017	-0.336745	4.251200	-0.000055	0.721201
-0.389340	-0.180522	4.261197	-0.000035	0.721470
-0.330215	-0.050406	4.271194	-0.000046	0.721747
0.000000	0.100974	4.281190	-0.000107	0.722160

-0.031254	0.723652	4.286195	-0.000102	0.723371
0.237057	1.948851	4.291200	-0.000153	0.725863
0.414107	3.779412	4.296205	-0.000187	0.729493
0.653994	6.150268	4.301210	-0.000233	0.734171
1.000624	9.015108	4.306214	-0.000300	0.739803
1.067032	12.404433	4.311219	-0.000314	0.746296
1.540374	16.175721	4.316224	-0.000405	0.753587
1.932200	20.369906	4.321229	-0.000481	0.761570
1.966615	25.017678	4.326234	-0.000490	0.770189
2.501113	29.952374	4.331238	-0.000593	0.779396
2.793595	35.271247	4.336243	-0.000651	0.789109
3.386179	40.858574	4.341248	-0.000765	0.799275
4.429691	46.669642	4.346253	-0.000963	0.809845
6.120121	52.669204	4.351258	-0.001282	0.820801
6.869144	59.124950	4.356262	-0.001426	0.832106
7.358833	65.835483	4.361267	-0.001521	0.843611
8.070847	72.744358	4.366272	-0.001658	0.855354
9.046191	79.804540	4.371277	-0.001845	0.867262
9.636778	87.129193	4.376282	-0.001960	0.879325
10.299910	94.614292	4.381286	-0.002088	0.891499
10.855795	102.272645	4.386291	-0.002196	0.903752
11.610431	110.047109	4.391296	-0.002342	0.916074
12.117341	117.972244	4.396301	-0.002442	0.928397
13.175653	125.925684	4.401306	-0.002644	0.940745
13.916118	134.059485	4.406310	-0.002787	0.953119
14.782611	142.238862	4.411315	-0.002954	0.965432
16.192818	150.434982	4.416320	-0.003222	0.977752
16.798846	158.855095	4.421325	-0.003340	0.990038
17.484860	167.286745	4.426330	-0.003474	1.002209
18.260951	175.741854	4.431334	-0.003624	1.014288
19.066869	184.224577	4.436339	-0.003779	1.026270
19.861910	192.766902	4.441344	-0.003933	1.038192
20.286179	201.388633	4.446349	-0.004018	1.049999
20.852870	210.001484	4.451354	-0.004129	1.061695
21.790072	218.602948	4.456358	-0.004309	1.073333
22.552635	227.208574	4.461363	-0.004457	1.084811
23.640604	235.795283	4.466368	-0.004665	1.096217
24.544181	244.406994	4.471373	-0.004839	1.107496
25.155130	253.083745	4.476378	-0.004958	1.118680
25.659126	261.772369	4.481382	-0.005058	1.129745
26.354884	270.412327	4.486387	-0.005193	1.140682
26.796609	279.127979	4.491392	-0.005281	1.151555
27.393965	287.773953	4.496397	-0.005398	1.162273
27.945178	296.402359	4.501402	-0.005506	1.172862
28.637930	305.009275	4.506406	-0.005641	1.183359
29.142060	313.635331	4.511411	-0.005740	1.193749
30.107386	322.163600	4.516416	-0.005926	1.204025
31.003210	330.708201	4.521421	-0.006098	1.214220
31.668905	339.268896	4.526426	-0.006228	1.224302
32.111013	347.898528	4.531430	-0.006316	1.234338
32.680299	356.429867	4.536435	-0.006427	1.244204
33.452128	364.940298	4.541440	-0.006577	1.254008
34.113331	373.450851	4.546445	-0.006705	1.263715
34.777562	381.959919	4.551450	-0.006835	1.273347
35.336837	390.466712	4.556454	-0.006944	1.282883
35.921791	398.949898	4.561459	-0.007059	1.292328
36.610198	407.421112	4.566464	-0.007193	1.301710
37.219047	415.952281	4.571469	-0.007312	1.311075
37.822718	424.439640	4.576474	-0.007430	1.320325
38.554237	432.835080	4.581478	-0.007571	1.329436
39.001201	441.275296	4.586483	-0.007660	1.338481
39.656008	449.667173	4.591488	-0.007788	1.347451
40.260809	458.069244	4.596493	-0.007906	1.356363
40.823934	466.441776	4.601498	-0.008016	1.365179
41.436323	474.831535	4.606502	-0.008136	1.373964
42.093400	483.189385	4.611507	-0.008263	1.382669
42.336783	491.630589	4.616512	-0.008314	1.391333
42.847438	499.990336	4.621517	-0.008415	1.399906
43.470710	508.295850	4.626522	-0.008536	1.408391
44.165871	516.624313	4.631526	-0.008671	1.416859
44.569102	524.955348	4.636531	-0.008752	1.425232
44.910233	533.330491	4.641536	-0.008821	1.433589
45.395286	541.640483	4.646541	-0.008917	1.441857
45.863635	549.949274	4.651546	-0.009009	1.450073
46.482370	558.257895	4.656550	-0.009130	1.458267
46.693867	566.586684	4.661555	-0.009175	1.466370
46.959531	574.967163	4.666560	-0.009230	1.474486
47.782023	583.184936	4.671565	-0.009388	1.482489
48.076279	591.476720	4.676570	-0.009449	1.490438
48.701749	599.736981	4.681574	-0.009571	1.498365
49.248343	607.977395	4.686579	-0.009678	1.506220
49.700684	616.266112	4.691584	-0.009767	1.514064
50.041888	624.535053	4.696589	-0.009836	1.521833
50.348831	632.805965	4.701594	-0.009899	1.529558
51.008201	641.032774	4.706598	-0.010027	1.537257
51.416936	649.279024	4.711603	-0.010109	1.544898
52.047827	657.524003	4.716608	-0.010232	1.552533
53.088466	665.674639	4.721613	-0.010431	1.560104
53.293126	673.949617	4.726618	-0.010474	1.567629
53.653121	682.227097	4.731622	-0.010547	1.575143
54.119727	690.445604	4.736627	-0.010639	1.582584
54.549312	698.685349	4.741632	-0.010725	1.590003
54.944888	706.926828	4.746637	-0.010804	1.597384
55.553505	715.102338	4.751642	-0.010922	1.604703
56.317497	723.290113	4.756646	-0.011070	1.612021
57.004912	731.470463	4.761651	-0.011203	1.619289
57.511009	739.683881	4.766656	-0.011303	1.626528
58.052408	747.953898	4.771661	-0.011409	1.633788
59.085913	756.048617	4.776666	-0.011607	1.640932
59.932586	764.218120	4.781670	-0.011770	1.648084
60.305111	772.458705	4.786675	-0.011845	1.655201
60.895590	780.645226	4.791680	-0.011960	1.662270
61.083046	788.900189	4.796685	-0.012000	1.669313
61.174876	797.150000	4.801690	-0.012023	1.676310
62.210891	805.239778	4.806694	-0.012221	1.683268
62.682418	813.426645	4.811699	-0.012314	1.690204
63.103801	821.639706	4.816704	-0.012398	1.697127
63.777067	829.793507	4.821709	-0.012529	1.704005
64.297104	837.971764	4.826714	-0.012631	1.710856
64.781173	846.179198	4.831718	-0.012727	1.717698
65.093808	854.358450	4.836723	-0.012790	1.724468
65.710511	862.515786	4.841728	-0.012911	1.731233
66.136291	870.711490	4.846733	-0.012995	1.737978
66.597658	878.859494	4.851738	-0.013086	1.744662
66.843134	887.089233	4.856742	-0.013138	1.751359
67.392092	895.224860	4.861747	-0.013245	1.757994
67.781394	903.385971	4.866752	-0.013323	1.764603
68.209690	911.551523	4.871757	-0.013408	1.771196
68.573505	919.711345	4.876762	-0.013481	1.777753
69.008240	927.859969	4.881766	-0.013568	1.784284
69.272660	936.064359	4.886771	-0.013622	1.790815
69.916481	944.206093	4.891776	-0.013747	1.797319
70.487587	952.316441	4.896781	-0.013859	1.803766
70.625832	960.486390	4.901786	-0.013890	1.810184
71.100120	968.636611	4.906790	-0.013984	1.816605
71.669539	976.725697	4.911795	-0.014095	1.822966
71.889040	984.908395	4.916800	-0.014141	1.829336
72.190839	993.071366	4.921805	-0.014203	1.835678
72.811441	1001.157238	4.926810	-0.014324	1.841977
73.344635	1009.294585	4.931814	-0.014429	1.848284
73.614982	1017.461875	4.936819	-0.014484	1.854560
74.234867	1025.556017	4.941824	-0.014605	1.860801
74.701458	1033.699091	4.946829	-0.014697	1.867040
74.841191	1041.893103	4.951834	-0.014729	1.873258
75.512611	1049.973552	4.956838	-0.014859	1.879432
76.127183	1058.056796	4.961843	-0.014979	1.885581
76.446314	1066.226735	4.966848	-0.015044	1.891741
76.790571	1074.370201	4.971853	-0.015113	1.897864
77.165226	1082.475849	4.976858	-0.015188	1.903942
77.719531	1090.601611	4.981862	-0.015297	1.910036
78.108510	1098.731303	4.986867	-0.015374	1.916095
78.411448	1106.866812	4.991872	-0.015436	1.922129
78.840748	1114.988487	4.996877	-0.015521	1.928148
79.055919	1123.146872	5.001882	-0.015567	1.934152
79.499541	1131.248728	5.006886	-0.015655	1.940121
79.955329	1139.359089	5.011891	-0.015745	1.946079
80.154566	1147.543339	5.016896	-0.015788	1.952044
80.646603	1155.656464	5.021901	-0.015884	1.957971
80.828389	1163.747919	5.026906	-0.015924	1.963831
81.215148	1171.853500	5.031910	-0.016001	1.969706
81.591399	1179.952080	5.036915	-0.016076	1.975557
82.142008	1188.020386	5.041920	-0.016184	1.981388
82.488127	1196.148208	5.046925	-0.016254	1.987222
82.592606	1204.287138	5.051930	-0.016279	1.993021
83.092949	1212.379193	5.056934	-0.016377	1.998812
83.535453	1220.448897	5.061939	-0.016465	2.004564
83.981261	1228.549213	5.066944	-0.016553	2.010322
84.146804	1236.711923	5.071949	-0.016590	2.016077
84.600217	1244.772862	5.076954	-0.016679	2.021775
85.350203	1252.840911	5.081958	-0.016824	2.027492
85.617040	1261.007798	5.086963	-0.016879	2.033212
85.943082	1269.110273	5.091968	-0.016945	2.038877
86.242380	1277.203862	5.096973	-0.017006	2.044518
86.293212	1285.342723	5.101978	-0.017021	2.050149
86.795164	1293.433385	5.106982	-0.017120	2.055777
86.993290	1301.531066	5.111987	-0.017162	2.061363
87.382481	1309.609746	5.116992	-0.017240	2.066941
87.859735	1317.709611	5.121997	-0.017334	2.072527
88.227247	1325.786282	5.127002	-0.017408	2.078070
88.616726	1333.872667	5.132006	-0.017486	2.083608
88.985197	1341.976567	5.137011	-0.017560	2.089141
89.097809	1350.129227	5.142016	-0.017586	2.094667
89.530043	1358.195102	5.147021	-0.017672	2.100151
89.943485	1366.263066	5.152026	-0.017754	2.105620
90.152970	1374.425377	5.157030	-0.017799	2.111119
90.373939	1382.566628	5.162035	-0.017845	2.116590
90.836472	1390.591069	5.167040	-0.017936	2.121992
91.333221	1398.652760	5.172045	-0.018034	2.127409
91.934876	1406.715838	5.177050	-0.018152	2.132822
92.175795	1414.832562	5.182054	-0.018202	2.138223
92.229580	1422.934405	5.187059	-0.018217	2.143583
92.566843	1431.017416	5.192064	-0.018285	2.148944
93.184660	1439.105483	5.197069	-0.018406	2.154321
93.282440	1447.191757	5.202074	-0.018429	2.159634
93.685227	1455.265051	5.207078	-0.018509	2.164954
94.147046	1463.327129	5.212083	-0.018601	2.170260
94.375486	1471.435280	5.217088	-0.018649	2.175560
94.605521	1479.527312	5.222093	-0.018697	2.180838
94.758626	1487.607831	5.227098	-0.018731	2.186088
95.323494	1495.696496	5.232102	-0.018841	2.191368
95.383865	1503.813918	5.237107	-0.018858	2.196609
95.643991	1511.879088	5.242112	-0.018911	2.201821
96.113052	1519.935813	5.247117	-0.019004	2.207034
96.213919	1528.032796	5.252122	-0.019028	2.212227
96.806938	1536.093138	5.257126	-0.019144	2.217429
96.962174	1544.180380	5.262131	-0.019178	2.222597
97.102602	1552.271440	5.267136	-0.019210	2.227754
97.362793	1560.381592	5.272141	-0.019263	2.232921
97.609127	1568.461551	5.277146	-0.019315	2.238057
98.046240	1576.502924	5.282150	-0.019401	2.243173
98.257567	1584.567674	5.287155	-0.019446	2.248272
98.302032	1592.691787	5.292160	-0.019459	2.253382
98.805900	1600.729133	5.297165	-0.019559	2.258466
99.007133	1608.807254	5.302170	-0.019601	2.263538
99.149235	1616.910096	5.307174	-0.019633	2.268608
99.454758	1625.059231	5.312179	-0.019695	2.273711
99.886391	1633.073928	5.317184	-0.019781	2.278729
100.306744	1641.111692	5.322189	-0.019865	2.283749
100.632019	1649.150756	5.327194	-0.019930	2.288751
101.120901	1657.234981	5.332198	-0.020027	2.293784
101.306173	1665.298137	5.337203	-0.020067	2.298767
101.397692	1673.380362	5.342208	-0.020089	2.303743
101.704510	1681.458770	5.347213	-0.020151	2.308723
102.043841	1689.518226	5.352218	-0.020220	2.313685
102.298017	1697.603030	5.357222	-0.020273	2.318643
102.558613	1705.657528	5.362227	-0.020326	2.323574
103.109272	1713.692864	5.367232	-0.020434	2.328506
103.412042	1721.786322	5.372237	-0.020496	2.333442
103.345983	1729.889725	5.377242	-0.020489	2.338344
103.882907	1737.938338	5.382246	-0.020594	2.343251
104.335975	1745.976177	5.387251	-0.020684	2.348135
104.623567	1754.094494	5.392256	-0.020743	2.353044
105.018513	1762.156910	5.397261	-0.020822	2.357917
105.241385	1770.207352	5.402266	-0.020868	2.362760
105.448885	1778.289344	5.407270	-0.020912	2.367609
105.813212	1786.349675	5.412275	-0.020985	2.372449
106.204709	1794.392897	5.417280	-0.021064	2.377271
106.351893	1802.478925	5.422285	-0.021096	2.382088
106.269705	1810.562899	5.427290	-0.021086	2.386877
106.846141	1818.615607	5.432294	-0.021199	2.391689
107.428576	1826.651594	5.437299	-0.021313	2.396483
107.435156	1834.737144	5.442304	-0.021319	2.401250
108.004535	1842.773914	5.447309	-0.021431	2.406024
108.336826	1850.831152	5.452314	-0.021498	2.410781
108.855900	1858.901062	5.457318	-0.021600	2.415551
109.072572	1866.973141	5.462323	-0.021645	2.420290
109.343064	1875.027567	5.467328	-0.021701	2.425012
109.659095	1883.117875	5.472333	-0.021765	2.429750
109.637017	1891.290322	5.477338	-0.021767	2.434501
109.770209	1899.336029	5.482342	-0.021797	2.439180
110.104021	1907.347949	5.487347	-0.021864	2.443847
110.270243	1915.389594	5.492352	-0.021900	2.448508
111.290923	1923.380857	5.497357	-0.022096	2.453197
111.593851	1931.440343	5.502362	-0.022157	2.457861
112.009577	1939.492159	5.507366	-0.022240	2.462521
112.306562	1947.554317	5.512371	-0.022301	2.467169
112.677758	1955.626290	5.517376	-0.022375	2.471819
113.189475	1963.689121	5.522381	-0.022476	2.476465
113.174081	1971.763403	5.527386	-0.022478	2.481070
113.328965	1979.825911	5.532390	-0.022512	2.485673
113.692706	1987.879688	5.537395	-0.022585	2.490277
113.933249	1995.963735	5.542400	-0.022635	2.494881
114.328787	2004.012213	5.547405	-0.022714	2.499467
114.535607	2012.052822	5.552410	-0.022758	2.504027
114.846406	2020.138859	5.557414	-0.022821	2.508612
115.069407	2028.234823	5.562419	-0.022868	2.513187
115.325580	2036.276667	5.567424	-0.022921	2.517727
115.492544	2044.334613	5.572429	-0.022958	2.522260
115.472725	2052.374470	5.577434	-0.022959	2.526762
115.902430	2060.448016	5.582438	-0.023044	2.531306
116.474937	2068.474440	5.587443	-0.023156	2.535827
116.580780	2076.532425	5.592448	-0.023181	2.540323
116.777196	2084.592670	5.597453	-0.023223	2.544820
116.922260	2092.646528	5.602458	-0.023256	2.549301
117.154759	2100.749515	5.607462	-0.023304	2.553808
117.655617	2108.763480	5.612467	-0.023403	2.558276
118.135078	2116.745813	5.617472	-0.023497	2.562717
118.416149	2124.818661	5.622477	-0.023555	2.567187
118.579216	2132.893388	5.627482	-0.023591	2.571641
118.894942	2140.967833	5.632486	-0.023655	2.576099
119.218671	2149.012436	5.637491	-0.023720	2.580532
119.453538	2157.045136	5.642496	-0.023769	2.584946
119.685619	2165.121512	5.647501	-0.023818	2.589375
120.063028	2173.346036	5.652506	-0.023893	2.593888
120.535530	2181.336561	5.657510	-0.023987	2.598272
120.605836	2189.357145	5.662515	-0.024005	2.602637
120.782879	2197.364709	5.667520	-0.024043	2.606995
121.220845	2205.402061	5.672525	-0.024130	2.611380
121.105627	2213.486366	5.677530	-0.024114	2.615745
121.642251	2221.468867	5.682534	-0.024219	2.620092
121.847275	2229.510061	5.687539	-0.024263	2.624441
121.881939	2237.578814	5.692544	-0.024274	2.628786
122.096782	2245.662554	5.697549	-0.024320	2.633144
122.496484	2253.662783	5.702554	-0.024399	2.637462
122.667434	2261.734554	5.707558	-0.024437	2.641796
122.990842	2269.762399	5.712563	-0.024502	2.646110
123.262622	2277.795242	5.717568	-0.024558	2.650416
123.745341	2285.853307	5.722573	-0.024653	2.654742
123.797803	2293.900766	5.727578	-0.024668	2.659027
123.958154	2301.976902	5.732582	-0.024703	2.663328
124.068787	2310.051044	5.737587	-0.024729	2.667617
124.185817	2318.120364	5.742592	-0.024756	2.671897
124.547808	2326.176496	5.747597	-0.024829	2.676179
124.478687	2334.211598	5.752602	-0.024821	2.680416
124.736871	2342.195447	5.757606	-0.024875	2.684640
124.936067	2350.254979	5.762611	-0.024917	2.688893
125.306634	2358.297199	5.767616	-0.024991	2.693141
125.777424	2366.342651	5.772621	-0.025084	2.697390
125.879667	2374.381556	5.777626	-0.025109	2.701606
126.320843	2382.403740	5.782630	-0.025196	2.705828
126.607575	2390.472197	5.787635	-0.025255	2.710058
126.831108	2398.520832	5.792640	-0.025302	2.714267
126.921260	2406.593233	5.797645	-0.025324	2.718473
127.196963	2414.601939	5.802650	-0.025381	2.722651
127.495262	2422.658967	5.807654	-0.025441	2.726849
127.525549	2430.754430	5.812659	-0.025452	2.731044
127.712937	2438.811696	5.817664	-0.025493	2.735223
128.359317	2446.787668	5.822669	-0.025618	2.739381
128.330009	2454.851242	5.827674	-0.025618	2.743537
128.553945	2462.919572	5.832678	-0.025665	2.747704
128.821094	2471.010386	5.837683	-0.025720	2.751879
129.071050	2479.084627	5.842688	-0.025772	2.756038
129.328096	2487.097830	5.847693	-0.025825	2.760160
129.375240	2495.096509	5.852698	-0.025839	2.764256
129.970260	2503.094262	5.857702	-0.025955	2.768378
130.191870	2511.157141	5.862707	-0.026002	2.772504
130.278399	2519.205620	5.867712	-0.026023	2.776610
130.791843	2527.235341	5.872717	-0.026124	2.780724
130.829332	2535.275436	5.877722	-0.026136	2.784810
131.088032	2543.328772	5.882726	-0.026190	2.788910
131.284187	2551.396431	5.887731	-0.026232	2.793007
131.588679	2559.424583	5.892736	-0.026294	2.797084
131.918453	2567.459849	5.897741	-0.026360	2.801160
132.231928	2575.454981	5.902746	-0.026424	2.805210
132.699562	2583.500561	5.907750	-0.026516	2.809287
132.902096	2591.582995	5.912755	-0.026559	2.813362
132.865644	2599.644336	5.917760	-0.026558	2.817407
133.286224	2607.690418	5.922765	-0.026641	2.821464
133.491810	2615.716749	5.927770	-0.026685	2.825493
133.545749	2623.783857	5.932774	-0.026700	2.829528
133.700400	2631.864179	5.937779	-0.026734	2.833570
134.214242	2639.855064	5.942784	-0.026835	2.837582
134.378842	2647.903514	5.947789	-0.026871	2.841597
134.609205	2655.905695	5.952794	-0.026919	2.845587
134.979256	2663.945598	5.957798	-0.026994	2.849598
135.226562	2672.005875	5.962803	-0.027045	2.853606
135.451022	2680.029071	5.967808	-0.027092	2.857589
135.851120	2688.084896	5.972813	-0.027172	2.861592
136.191938	2696.086092	5.977818	-0.027241	2.865560
136.500058	2704.125699	5.982822	-0.027303	2.869539
136.748377	2712.222069	5.987827	-0.027355	2.873537
137.158851	2720.213814	5.992832	-0.027437	2.877487
137.450741	2728.264392	5.997837	-0.027496	2.881454
137.656516	2736.285470	6.002842	-0.027540	2.885396
137.927849	2744.356303	6.007846	-0.027596	2.889360
138.069150	2752.422140	6.012851	-0.027627	2.893310
138.117879	2760.488227	6.017856	-0.027642	2.897249
138.665774	2768.476729	6.022861	-0.027749	2.901172
139.071333	2776.495288	6.027866	-0.027830	2.905097
139.570938	2784.530610	6.032870	-0.027928	2.909030
139.878928	2792.689580	6.037875	-0.027991	2.913006
140.184969	2800.709276	6.042880	-0.028053	2.916910
140.273361	2808.741828	6.047885	-0.028075	2.920803
140.527760	2816.710747	6.052890	-0.028127	2.924669
140.951831	2824.739743	6.057894	-0.028212	2.928568
141.262553	2832.795286	6.062899	-0.028275	2.932468
141.245354	2840.865016	6.067904	-0.028277	2.936353
141.460511	2848.892873	6.072909	-0.028322	2.940225
141.682399	2856.891020	6.077914	-0.028369	2.944077
142.024467	2864.939508	6.082918	-0.028438	2.947955
142.281146	2873.001498	6.087923	-0.028491	2.951830
142.266242	2881.074162	6.092928	-0.028493	2.955690
142.717417	2889.065289	6.097933	-0.028583	2.959531
142.719654	2897.102249	6.102938	-0.028588	2.963366
143.055391	2905.125612	6.107942	-0.028656	2.967206
143.489892	2913.157501	6.112947	-0.028742	2.971050
143.376828	2921.225097	6.117952	-0.028727	2.974878
143.753371	2929.244156	6.122957	-0.028802	2.978703
144.019812	2937.260421	6.127962	-0.028857	2.982516
144.219429	2945.326541	6.132966	-0.028899	2.986345
144.270141	2953.391191	6.137971	-0.028914	2.990160
144.551137	2961.444404	6.142976	-0.028972	2.993977
145.119466	2969.433254	6.147981	-0.029083	2.997773
144.911057	2977.492037	6.152986	-0.029049	3.001558
145.107828	2985.499571	6.157990	-0.029091	3.005334
145.318644	2993.525118	6.162995	-0.029136	3.009115
145.434470	3001.601483	6.168000	-0.029163	3.012910
146.019155	3009.617601	6.173005	-0.029277	3.016695
146.044979	3017.648526	6.178010	-0.029287	3.020455
146.394255	3025.658360	6.183014	-0.029357	3.024216
146.453826	3033.721947	6.188019	-0.029374	3.027983
146.610066	3041.774833	6.193024	-0.029408	3.031746
147.197620	3049.809775	6.198029	-0.029523	3.035516
147.309268	3057.815034	6.203034	-0.029549	3.039244
147.344422	3065.871057	6.208038	-0.029561	3.042988
147.662599	3073.896343	6.213043	-0.029625	3.046727
147.859370	3081.915188	6.218048	-0.029667	3.050452
148.367828	3089.973292	6.223053	-0.029767	3.054206
148.627530	3097.984005	6.228058	-0.029821	3.057921
148.745922	3106.030590	6.233062	-0.029848	3.061641
149.067960	3114.060774	6.238067	-0.029913	3.065359
149.371151	3122.082455	6.243072	-0.029975	3.069068
149.666992	3130.213227	6.248077	-0.030035	3.072822
149.720505	3138.267241	6.253082	-0.030051	3.076524
149.741042	3146.262860	6.258086	-0.030060	3.080194
150.114499	3154.254074	6.263091	-0.030134	3.083874
150.352791	3162.270069	6.268096	-0.030184	3.087555
150.579080	3170.328398	6.273101	-0.030232	3.091250
150.658119	3178.372338	6.278106	-0.030252	3.094927
150.942846	3186.381236	6.283110	-0.030310	3.098593
151.578588	3194.368652	6.288115	-0.030433	3.102261
151.673301	3202.417993	6.293120	-0.030456	3.105928
152.040565	3210.449651	6.298125	-0.030530	3.109595
152.077965	3218.503946	6.303130	-0.030542	3.113253
152.213044	3226.558701	6.308134	-0.030573	3.116912
152.665135	3234.587345	6.313139	-0.030662	3.120568
152.974855	3242.558971	6.318144	-0.030725	3.124188
152.954724	3250.654245	6.323149	-0.030727	3.127845
153.252791	3258.680480	6.328154	-0.030788	3.131480
153.435254	3266.733837	6.333158	-0.030827	3.135119
153.614748	3274.763639	6.338163	-0.030866	3.138742
153.975241	3282.757254	6.343168	-0.030938	3.142353
154.327948	3290.812475	6.348173	-0.031009	3.145987
154.410562	3298.819380	6.353178	-0.031030	3.149583
154.661112	3306.911092	6.358182	-0.031082	3.153221
154.985283	3314.930440	6.363187	-0.031147	3.156825
155.238429	3322.905249	6.368192	-0.031200	3.160402
155.579762	3330.924031	6.373197	-0.031268	3.163998
155.613546	3338.974903	6.378202	-0.031280	3.167591
156.004139	3347.021477	6.383206	-0.031358	3.171194
156.103353	3355.087268	6.388211	-0.031382	3.174788
156.349269	3363.065927	6.393216	-0.031433	3.178346
156.655585	3371.115379	6.398221	-0.031495	3.181934
156.776334	3379.136237	6.403226	-0.031523	3.185497
156.921028	3387.198396	6.408230	-0.031555	3.189075
157.446940	3395.217757	6.413235	-0.031658	3.192647
157.595315	3403.287294	6.418240	-0.031691	3.196220
157.794946	3411.286087	6.423245	-0.031734	3.199761
157.910600	3419.306773	6.428250	-0.031761	3.203304
158.083994	3427.350075	6.433254	-0.031798	3.206855
158.174874	3435.398120	6.438259	-0.031820	3.210401
158.297847	3443.427220	6.443264	-0.031848	3.213936
158.760780	3451.446029	6.448269	-0.031940	3.217477
158.779431	3459.486447	6.453274	-0.031949	3.221005
158.911924	3467.482965	6.458278	-0.031979	3.224514
159.098038	3475.537488	6.463283	-0.032019	3.228047
159.241585	3483.597764	6.468288	-0.032051	3.231577
159.645524	3491.667706	6.473293	-0.032131	3.235118
159.821316	3499.636160	6.478298	-0.032169	3.238602
159.829112	3507.663994	6.483302	-0.032176	3.242101
160.285766	3515.669002	6.488307	-0.032266	3.245604
160.252876	3523.700819	6.493312	-0.032265	3.249095
160.475053	3531.755145	6.498317	-0.032312	3.252603
160.781644	3539.786040	6.503322	-0.032374	3.256100
160.916494	3547.790324	6.508326	-0.032405	3.259575
161.375472	3555.797338	6.513331	-0.032495	3.263060
161.547692	3563.839355	6.518336	-0.032533	3.266545
161.630560	3571.882296	6.523341	-0.032554	3.270023
161.907787	3579.953069	6.528346	-0.032610	3.273517
161.985052	3587.968897	6.533350	-0.032630	3.276976
162.147307	3595.998591	6.538355	-0.032666	3.280441
162.119859	3604.002465	6.543360	-0.032666	3.283883
162.684982	3612.012862	6.548365	-0.032776	3.287347
163.001703	3620.053630	6.553370	-0.032841	3.290812
163.251340	3628.084295	6.558374	-0.032892	3.294265
163.287912	3636.150637	6.563379	-0.032904	3.297722
163.687176	3644.160177	6.568384	-0.032984	3.301165
163.900034	3652.163498	6.573389	-0.033029	3.304595
163.802981	3660.222596	6.578394	-0.033016	3.308033
164.292052	3668.262109	6.583398	-0.033113	3.311481
164.335476	3676.346833	6.588403	-0.033126	3.314928
164.445612	3684.315966	6.593408	-0.033152	3.318325
164.868811	3692.339867	6.598413	-0.033236	3.321753
165.017289	3700.323679	6.603418	-0.033269	3.325150
165.122926	3708.369549	6.608422	-0.033294	3.328569
165.207755	3716.439572	6.613427	-0.033315	3.331993
165.631286	3724.432253	6.618432	-0.033399	3.335394
165.864835	3732.459487	6.623437	-0.033448	3.338799
166.044219	3740.498276	6.628442	-0.033486	3.342203
166.229112	3748.501226	6.633446	-0.033526	3.345589
166.370302	3756.561343	6.638451	-0.033558	3.348994
166.606001	3764.558547	6.643456	-0.033607	3.352372
166.809552	3772.627562	6.648461	-0.033650	3.355776
167.172837	3780.605690	6.653466	-0.033723	3.359144
167.346559	3788.656630	6.658470	-0.033761	3.362532
167.395906	3796.733146	6.663475	-0.033775	3.365923
167.629198	3804.717906	6.668480	-0.033824	3.369279
167.945503	3812.780476	6.673485	-0.033888	3.372667
168.015606	3820.828980	6.678490	-0.033906	3.376037
168.235387	3828.792884	6.683494	-0.033952	3.379374
168.532625	3836.853954	6.688499	-0.034013	3.382750
168.727630	3844.856992	6.693504	-0.034055	3.386095
168.877640	3852.886083	6.698509	-0.034088	3.389447
169.168529	3860.975863	6.703514	-0.034147	3.392825
169.309663	3869.051882	6.708518	-0.034179	3.396188
169.669867	3876.989815	6.713523	-0.034251	3.399499
169.886722	3884.985274	6.718528	-0.034297	3.402825
170.002839	3893.042267	6.723533	-0.034324	3.406170
170.110622	3901.017451	6.728538	-0.034349	3.409477
170.349396	3909.060509	6.733542	-0.034399	3.412814
170.720517	3917.139126	6.738547	-0.034473	3.416167
170.878008	3925.081679	6.743552	-0.034508	3.419453
171.404884	3933.105960	6.748557	-0.034611	3.422782
171.798962	3941.118923	6.753562	-0.034690	3.426098
172.249619	3949.145819	6.758566	-0.034779	3.429419
172.413424	3957.264173	6.763571	-0.034815	3.432765
172.546270	3965.264628	6.768576	-0.034845	3.436057
173.025152	3973.277344	6.773581	-0.034939	3.439364
173.208095	3981.306064	6.778586	-0.034979	3.442663
173.255457	3989.336042	6.783590	-0.034993	3.445956
173.542564	3997.349761	6.788595	-0.035052	3.449246
173.666411	4005.391319	6.793600	-0.035080	3.452540
173.948285	4013.459239	6.798605	-0.035138	3.455846
173.965085	4021.448432	6.803610	-0.035146	3.459108
174.330749	4029.476969	6.808614	-0.035219	3.462395
174.355647	4037.529044	6.813619	-0.035229	3.465676
174.452418	4045.551582	6.818624	-0.035253	3.468946
174.825774	4053.594307	6.823629	-0.035327	3.472229
174.870831	4061.657798	6.828634	-0.035341	3.475506
175.242612	4069.611511	6.833638	-0.035416	3.478747
175.488644	4077.638969	6.838643	-0.035467	3.482010
175.433100	4085.646173	6.843648	-0.035462	3.485253
175.581289	4093.667963	6.848653	-0.035495	3.488505
175.934877	4101.718292	6.853658	-0.035566	3.491772
176.287661	4109.740060	6.858662	-0.035637	3.495024
176.466260	4117.759836	6.863667	-0.035675	3.498267
176.512572	4125.790460	6.868672	-0.035689	3.501507
176.889338	4133.768030	6.873677	-0.035764	3.504733
177.110368	4141.831914	6.878682	-0.035811	3.507986
177.056478	4149.890437	6.883686	-0.035806	3.511225
177.516847	4157.908242	6.888691	-0.035897	3.514460
177.646638	4165.898346	6.893696	-0.035927	3.517672
177.833656	4173.967761	6.898701	-0.035967	3.520913
178.017704	4181.935015	6.903706	-0.036006	3.524111
178.249651	4189.959786	6.908710	-0.036055	3.527331
178.363576	4198.032993	6.913715	-0.036081	3.530563
178.534609	4206.024905	6.918720	-0.036118	3.533761
178.849289	4214.102475	6.923725	-0.036182	3.536996
178.871635	4222.101568	6.928730	-0.036192	3.540187
178.992787	4230.127111	6.933734	-0.036220	3.543388
179.381123	4238.171310	6.938739	-0.036297	3.546602
179.343836	4246.179459	6.943744	-0.036295	3.549786
179.530809	4254.314023	6.948749	-0.036336	3.553025
179.553589	4262.361334	6.953754	-0.036345	3.556220
179.874719	4270.261463	6.958758	-0.036410	3.559363
180.292190	4278.286112	6.963763	-0.036493	3.562556
180.380041	4286.282555	6.968768	-0.036515	3.565725
180.688078	4294.304675	6.973773	-0.036577	3.568907
180.888012	4302.362594	6.978778	-0.036620	3.572098
181.023248	4310.387473	6.983782	-0.036650	3.575271
181.016116	4318.429163	6.988787	-0.036654	3.578444
181.064245	4326.438309	6.993792	-0.036669	3.581602
181.142377	4334.438098	6.998797	-0.036688	3.584755
181.452426	4342.476576	7.003802	-0.036751	3.587927
181.623851	4350.498972	7.008806	-0.036789	3.591086
181.888160	4358.544083	7.013811	-0.036843	3.594253
181.864508	4366.526399	7.018816	-0.036844	3.597385
182.206071	4374.535673	7.023821	-0.036913	3.600535
182.341192	4382.559714	7.028826	-0.036943	3.603683
182.561427	4390.551252	7.033830	-0.036990	3.606817
182.975167	4398.601571	7.038835	-0.037072	3.609977
183.139063	4406.637695	7.043840	-0.037108	3.613121
183.276363	4414.697984	7.048845	-0.037139	3.616272
183.572420	4422.684502	7.053850	-0.037199	3.619395
183.701024	4430.695452	7.058854	-0.037228	3.622520
183.841671	4438.757461	7.063859	-0.037260	3.625663
183.843883	4446.779221	7.068864	-0.037265	3.628784
184.254098	4454.826029	7.073869	-0.037347	3.631923
184.425730	4462.878900	7.078874	-0.037384	3.635055
184.566721	4470.872505	7.083878	-0.037416	3.638160
184.697756	4478.907536	7.088883	-0.037446	3.641279
184.738585	4486.854148	7.093888	-0.037458	3.644358
185.094395	4494.924639	7.098893	-0.037530	3.647491
185.037681	4502.974001	7.103898	-0.037525	3.650602
185.506525	4510.973235	7.108902	-0.037617	3.653705
185.592346	4519.033127	7.113907	-0.037639	3.656819
185.823489	4527.010687	7.118912	-0.037687	3.659902
186.067050	4535.055839	7.123917	-0.037737	3.663008
186.212274	4543.104854	7.128922	-0.037770	3.666111
186.605297	4551.082347	7.133926	-0.037848	3.669190
186.614040	4559.180321	7.138931	-0.037855	3.672303
186.810362	4567.144108	7.143936	-0.037897	3.675367
186.984390	4575.174726	7.148941	-0.037935	3.678453
187.132412	4583.199244	7.153946	-0.037967	3.681534
187.450738	4591.159719	7.158950	-0.038032	3.684591
187.670036	4599.242859	7.163955	-0.038078	3.687691
187.545372	4607.252734	7.168960	-0.038060	3.690751
187.802128	4615.307832	7.173965	-0.038113	3.693836
188.209223	4623.321460	7.178970	-0.038194	3.696905
188.086919	4631.319301	7.183974	-0.038177	3.699953
188.289054	4639.354944	7.188979	-0.038220	3.703021
188.365954	4647.370239	7.193984	-0.038239	3.706076
188.660099	4655.356746	7.198989	-0.038299	3.709122
188.760720	4663.465982	7.203994	-0.038323	3.712208
188.982401	4671.549543	7.208998	-0.038370	3.715285
189.218609	4679.524605	7.214003	-0.038419	3.718318
189.383222	4687.505941	7.219008	-0.038455	3.721349
189.714988	4695.428781	7.224013	-0.038522	3.724359
189.679463	4703.528417	7.229018	-0.038521	3.727426
189.957754	4711.527267	7.234022	-0.038578	3.730459
190.100894	4719.576845	7.239027	-0.038610	3.733505
190.347034	4727.573644	7.244032	-0.038661	3.736531
190.563756	4735.592134	7.249037	-0.038707	3.739563
190.786014	4743.611916	7.254042	-0.038753	3.742593
190.944558	4751.601674	7.259046	-0.038788	3.745607
191.149012	4759.689650	7.264051	-0.038832	3.748657
191.367595	4767.737769	7.269056	-0.038878	3.751689
191.676407	4775.717944	7.274061	-0.038940	3.754696
191.781764	4783.776274	7.279066	-0.038965	3.757725
191.895589	4791.788206	7.284070	-0.038992	3.760734
192.139594	4799.803615	7.289075	-0.039042	3.763746
192.243394	4807.831639	7.294080	-0.039067	3.766756
192.619541	4815.825326	7.299085	-0.039142	3.769757
192.722057	4823.905654	7.304090	-0.039167	3.772782
192.833351	4831.918452	7.309094	-0.039193	3.775779
193.166596	4839.935133	7.314099	-0.039260	3.778781
193.202024	4847.950334	7.319104	-0.039272	3.781773
193.388595	4855.945240	7.324109	-0.039312	3.784758
193.714763	4863.981783	7.329114	-0.039378	3.787759
193.732936	4872.013021	7.334118	-0.039387	3.790750
194.145512	4880.085099	7.339123	-0.039469	3.793762
194.606728	4888.107959	7.344128	-0.039560	3.796754
194.564840	4896.064476	7.349133	-0.039557	3.799708
194.657984	4904.109277	7.354138	-0.039580	3.802695
194.814950	4912.078375	7.359142	-0.039614	3.805654
195.285407	4920.099477	7.364147	-0.039707	3.808636
195.313123	4928.128422	7.369152	-0.039718	3.811609
195.404170	4936.173483	7.374157	-0.039740	3.814587
195.764760	4944.177165	7.379162	-0.039812	3.817553
195.949462	4952.189774	7.384166	-0.039852	3.820516
196.379913	4960.188635	7.389171	-0.039937	3.823478
196.279243	4968.240424	7.394176	-0.039924	3.826445
196.580512	4976.242411	7.399181	-0.039985	3.829400
196.751175	4984.314136	7.404186	-0.040022	3.832375
196.846681	4992.327719	7.409190	-0.040045	3.835326
197.211850	5000.317832	7.414195	-0.040119	3.838271
197.262135	5008.328587	7.419200	-0.040133	3.841214
197.223398	5016.331796	7.424205	-0.040131	3.844151
197.530779	5024.410307	7.429210	-0.040194	3.847121
197.691884	5032.413024	7.434214	-0.040229	3.850057
197.865293	5040.478385	7.439219	-0.040267	3.853014
197.832716	5048.495710	7.444224	-0.040266	3.855947
198.136198	5056.490341	7.449229	-0.040328	3.858877
198.303135	5064.522626	7.454234	-0.040364	3.861815
198.283625	5072.500320	7.459238	-0.040366	3.864727
198.551963	5080.577041	7.464243	-0.040421	3.867679
198.676274	5088.613057	7.469248	-0.040450	3.870611
198.957077	5096.841381	7.474253	-0.040507	3.873613
199.087890	5104.842338	7.479258	-0.040537	3.876528
199.497190	5112.697857	7.484262	-0.040618	3.879393
199.527784	5120.731777	7.489267	-0.040629	3.882313
199.586912	5128.674780	7.494272	-0.040645	3.885199
199.894005	5136.723269	7.499277	-0.040708	3.888126
200.091591	5144.748455	7.504282	-0.040750	3.891039
200.237092	5152.763537	7.509286	-0.040782	3.893946
200.373432	5160.847269	7.514291	-0.040813	3.896876
200.470554	5168.773459	7.519296	-0.040836	3.899745
200.635881	5176.790089	7.524301	-0.040872	3.902646
200.946200	5184.822506	7.529306	-0.040935	3.905554
201.200595	5192.870871	7.534310	-0.040988	3.908464
201.384560	5200.877039	7.539315	-0.041028	3.911355
201.726083	5208.894104	7.544320	-0.041097	3.914251
202.008386	5216.914226	7.549325	-0.041154	3.917145
202.293826	5224.891650	7.554330	-0.041213	3.920021
202.370217	5232.910017	7.559334	-0.041232	3.922906
202.499729	5240.964658	7.564339	-0.041262	3.925803
202.624025	5248.975131	7.569344	-0.041290	3.928682
202.704812	5257.002432	7.574349	-0.041310	3.931564
202.927145	5265.075607	7.579354	-0.041357	3.934463
203.295597	5273.029871	7.584358	-0.041431	3.937319
203.550616	5281.049797	7.589363	-0.041484	3.940195
203.684270	5289.036317	7.594368	-0.041514	3.943055
203.945800	5297.104506	7.599373	-0.041568	3.945944
204.208123	5305.103506	7.604378	-0.041622	3.948806
204.180779	5313.133978	7.609382	-0.041622	3.951673
204.540855	5321.190789	7.614387	-0.041695	3.954553
204.608596	5329.165319	7.619392	-0.041712	3.957397
204.756439	5337.166297	7.624397	-0.041745	3.960250
204.971023	5345.204118	7.629402	-0.041790	3.963114
205.233573	5353.198138	7.634406	-0.041845	3.965962
205.561585	5361.205440	7.639411	-0.041911	3.968814
205.380208	5369.280693	7.644416	-0.041882	3.971679
205.659263	5377.319653	7.649421	-0.041940	3.974537
206.048571	5385.344351	7.654426	-0.042018	3.977389
206.066204	5393.323713	7.659430	-0.042026	3.980218
206.288704	5401.352971	7.664435	-0.042073	3.983065
206.559209	5409.349656	7.669440	-0.042128	3.985899
206.558133	5417.378888	7.674445	-0.042133	3.988739
206.663212	5425.468155	7.679450	-0.042158	3.991599
206.690680	5433.466912	7.684454	-0.042169	3.994424
207.017030	5441.533766	7.689459	-0.042235	3.997276
207.084411	5449.476638	7.694464	-0.042253	4.000078
207.301238	5457.502520	7.699469	-0.042298	4.002910
207.511888	5465.556638	7.704474	-0.042343	4.005749
207.524985	5473.559786	7.709478	-0.042350	4.008566
207.749664	5481.617706	7.714483	-0.042398	4.011403
207.896936	5489.605785	7.719488	-0.042430	4.014212
208.016833	5497.622982	7.724493	-0.042458	4.017029
208.171999	5505.649643	7.729498	-0.042492	4.019848
208.168118	5513.675661	7.734502	-0.042497	4.022662
208.426890	5521.682409	7.739507	-0.042550	4.025471
208.480624	5529.695797	7.744512	-0.042565	4.028278
208.648201	5537.735737	7.749517	-0.042602	4.031094
209.100613	5545.863725	7.754522	-0.042691	4.033943
209.154419	5553.863777	7.759526	-0.042707	4.036739
209.144968	5561.778203	7.764531	-0.042710	4.039502
209.355126	5569.815771	7.769536	-0.042755	4.042309
209.529978	5577.768267	7.774541	-0.042792	4.045085
209.602575	5585.848946	7.779546	-0.042811	4.047902
209.924888	5593.834180	7.784550	-0.042876	4.050687
210.196347	5601.902580	7.789555	-0.042932	4.053498
210.332235	5609.909608	7.794560	-0.042963	4.056284
210.455349	5617.853526	7.799565	-0.042991	4.059046
210.767231	5625.937219	7.804570	-0.043054	4.061858
210.669421	5633.916603	7.809574	-0.043041	4.064625
210.968820	5641.958977	7.814579	-0.043103	4.067418
211.016718	5649.970396	7.819584	-0.043117	4.070195
211.183028	5658.035722	7.824589	-0.043153	4.072990
211.389113	5666.091522	7.829594	-0.043197	4.075780
211.406726	5674.035873	7.834598	-0.043205	4.078528
211.742676	5682.076800	7.839603	-0.043273	4.081311
211.733758	5690.018610	7.844608	-0.043277	4.084053
211.880439	5698.048291	7.849613	-0.043309	4.086826
212.383037	5706.096638	7.854618	-0.043408	4.089608
212.413795	5714.117528	7.859622	-0.043419	4.092373
212.603990	5722.184798	7.864627	-0.043460	4.095154
212.677734	5730.192282	7.869632	-0.043479	4.097910
212.902730	5738.144869	7.874637	-0.043526	4.100648
213.008868	5746.208305	7.879642	-0.043551	4.103421
213.355146	5754.195319	7.884646	-0.043621	4.106169
213.478618	5762.239077	7.889651	-0.043649	4.108931
213.601878	5770.283761	7.894656	-0.043677	4.111692
213.627322	5778.333038	7.899661	-0.043687	4.114451
213.844350	5786.354119	7.904666	-0.043733	4.117201
214.122408	5794.303570	7.909670	-0.043790	4.119926
214.236604	5802.340258	7.914675	-0.043817	4.122676
214.280790	5810.342009	7.919680	-0.043830	4.125412
214.572306	5818.323570	7.924685	-0.043890	4.128142
214.639359	5826.423939	7.929690	-0.043907	4.130908
214.743483	5834.441458	7.934694	-0.043932	4.133645
215.109650	5842.472289	7.939699	-0.044005	4.136387
215.190961	5850.450999	7.944704	-0.044026	4.139107
215.545351	5858.493127	7.949709	-0.044097	4.141849
215.745983	5866.490206	7.954714	-0.044140	4.144572
215.810375	5874.504794	7.959718	-0.044157	4.147298
215.830873	5882.560238	7.964723	-0.044166	4.150035
215.965175	5890.608765	7.969728	-0.044196	4.152770
216.226116	5898.613165	7.974733	-0.044250	4.155489
216.448441	5906.625178	7.979738	-0.044297	4.158209
216.368358	5914.637253	7.984742	-0.044287	4.160923
216.590113	5922.617486	7.989747	-0.044334	4.163628
216.832285	5930.640146	7.994752	-0.044384	4.166346
216.940663	5938.655126	7.999757	-0.044410	4.169058
217.117582	5946.758082	8.004762	-0.044448	4.171799
217.247001	5954.682191	8.009766	-0.044477	4.174477
217.499062	5962.746157	8.014771	-0.044530	4.177202
217.577272	5970.727729	8.019776	-0.044549	4.179896
217.684188	5978.756160	8.024781	-0.044575	4.182603
217.906410	5986.752717	8.029786	-0.044621	4.185300
217.858776	5994.782750	8.034790	-0.044618	4.188003
218.379309	6002.804305	8.039795	-0.044720	4.190707
218.584533	6010.934236	8.044800	-0.044763	4.193443
218.713076	6018.943748	8.049805	-0.044793	4.196136
218.977470	6026.882560	8.054810	-0.044847	4.198805
218.885569	6034.873094	8.059814	-0.044835	4.201485
219.095922	6042.847158	8.064819	-0.044880	4.204162
219.104013	6050.922126	8.069824	-0.044886	4.206868
219.489367	6058.882513	8.074829	-0.044963	4.209538
219.611920	6066.956936	8.079834	-0.044992	4.212242
219.689623	6074.963282	8.084838	-0.045011	4.214921
219.845077	6082.978949	8.089843	-0.045045	4.217602
220.050603	6090.955281	8.094848	-0.045089	4.220269
220.317670	6098.961103	8.099853	-0.045144	4.222945
220.682003	6106.984208	8.104858	-0.045217	4.225625
220.863811	6115.022628	8.109862	-0.045256	4.228307
221.020494	6123.068843	8.114867	-0.045291	4.230990
221.133947	6131.130873	8.119872	-0.045317	4.233676
221.472927	6139.137134	8.124877	-0.045386	4.236344
221.542851	6147.135649	8.129882	-0.045404	4.239005
221.324799	6155.120185	8.134886	-0.045368	4.241657
221.697368	6163.110782	8.139891	-0.045443	4.244314
221.866254	6171.173422	8.144896	-0.045480	4.246992
221.900805	6179.188496	8.149901	-0.045492	4.249652
222.026987	6187.251286	8.154906	-0.045520	4.252326
222.231812	6195.240700	8.159910	-0.045564	4.254975
222.430736	6203.261752	8.164915	-0.045606	4.257633
222.362584	6211.308364	8.169920	-0.045599	4.260295
222.670535	6219.279976	8.174925	-0.045661	4.262934
222.807460	6227.342498	8.179930	-0.045692	4.265600
222.893132	6235.310318	8.184934	-0.045713	4.268232
223.244189	6243.383959	8.189939	-0.045784	4.270900
223.444134	6251.405218	8.194944	-0.045826	4.273548
223.749576	6259.479955	8.199949	-0.045889	4.276213
223.843080	6267.418399	8.204954	-0.045911	4.278829
223.895839	6275.448152	8.209958	-0.045926	4.281473
224.236409	6283.404412	8.214963	-0.045995	4.284094
224.224831	6291.484719	8.219968	-0.045998	4.286751
224.515255	6299.434212	8.224973	-0.046058	4.289366
225.034696	6307.513265	8.229978	-0.046160	4.292024
224.804727	6315.541771	8.234982	-0.046122	4.294658
225.026269	6323.567906	8.239987	-0.046169	4.297292
225.199250	6331.553563	8.244992	-0.046206	4.299912
225.317181	6339.563599	8.249997	-0.046233	4.302537
225.505145	6347.587406	8.255002	-0.046274	4.305166
225.667794	6355.583396	8.260006	-0.046309	4.307783
225.751306	6363.629150	8.265011	-0.046330	4.310415
225.967700	6371.681552	8.270016	-0.046375	4.313049
225.889877	6379.706550	8.275021	-0.046366	4.315669
226.403583	6387.695141	8.280026	-0.046467	4.318281
226.438403	6395.670914	8.285030	-0.046479	4.320883
226.675434	6403.665173	8.290035	-0.046528	4.323491
226.694424	6411.695096	8.295040	-0.046537	4.326108
226.945569	6419.698877	8.300045	-0.046589	4.328716
227.122416	6427.747605	8.305050	-0.046627	4.331336
227.313714	6435.769286	8.310054	-0.046668	4.333947
227.423160	6443.853372	8.315059	-0.046694	4.336575
227.404358	6451.804786	8.320064	-0.046696	4.339158
227.533180	6459.839587	8.325069	-0.046725	4.341767
227.838180	6467.823622	8.330074	-0.046787	4.344360
227.886233	6475.813062	8.335078	-0.046801	4.346951
228.088577	6483.897608	8.340083	-0.046844	4.349572
228.196989	6491.955280	8.345088	-0.046870	4.352182
228.355160	6499.995612	8.350093	-0.046904	4.354786
228.440711	6508.027792	8.355098	-0.046926	4.357385
228.425174	6515.929631	8.360102	-0.046928	4.359939
228.719418	6523.992437	8.365107	-0.046988	4.362546
228.684005	6531.899250	8.370112	-0.046987	4.365099
228.960862	6539.975025	8.375117	-0.047044	4.367706
229.109331	6547.995239	8.380122	-0.047076	4.370294
229.300231	6556.010756	8.385126	-0.047117	4.372879
229.312379	6564.026664	8.390131	-0.047125	4.375461
229.625587	6572.053428	8.395136	-0.047188	4.378047
229.761550	6580.046557	8.400141	-0.047219	4.380619
229.819013	6588.049742	8.405146	-0.047235	4.383193
229.891174	6596.082667	8.410150	-0.047254	4.385775
230.211470	6604.127664	8.415155	-0.047319	4.388361
230.283549	6612.146835	8.420160	-0.047337	4.390935
230.510976	6620.145686	8.425165	-0.047385	4.393502
230.617925	6628.202015	8.430170	-0.047410	4.396086
230.853328	6636.175204	8.435174	-0.047459	4.398642
230.845383	6644.220567	8.440179	-0.047463	4.401218
230.897296	6652.177939	8.445184	-0.047478	4.403765
231.086108	6660.191424	8.450189	-0.047518	4.406329
231.269678	6668.265430	8.455194	-0.047558	4.408911
231.426390	6676.295800	8.460198	-0.047592	4.411477
231.555555	6684.322544	8.465203	-0.047622	4.414041
231.858360	6692.357202	8.470208	-0.047683	4.416606
231.965367	6700.277243	8.475213	-0.047708	4.419132
232.302057	6708.391427	8.480218	-0.047777	4.421720
232.234163	6716.334172	8.485222	-0.047769	4.424250
232.604137	6724.407445	8.490227	-0.047843	4.426822
232.743882	6732.442771	8.495232	-0.047875	4.429379
232.767773	6740.471691	8.500237	-0.047884	4.431932
232.994142	6748.525990	8.505242	-0.047932	4.434493
233.087017	6756.486607	8.510246	-0.047954	4.437022
233.362570	6764.485707	8.515251	-0.048011	4.439562
233.281279	6772.520903	8.520256	-0.048001	4.442111
233.355487	6780.463082	8.525261	-0.048020	4.444630
233.724914	6788.580363	8.530266	-0.048094	4.447203
233.679483	6796.512619	8.535270	-0.048091	4.449715
233.969045	6804.596039	8.540275	-0.048150	4.452275
234.128834	6812.593062	8.545280	-0.048185	4.454805
234.458434	6820.599522	8.550285	-0.048252	4.457338
234.457486	6828.614688	8.555290	-0.048257	4.459870
234.497657	6836.640848	8.560295	-0.048270	4.462405
234.851888	6844.660978	8.565299	-0.048341	4.464938
234.890024	6852.699363	8.570304	-0.048353	4.467474
235.074889	6860.635667	8.575309	-0.048393	4.469976
235.344833	6868.740082	8.580314	-0.048449	4.472531
235.536832	6876.711258	8.585319	-0.048490	4.475041
235.553316	6884.753385	8.590323	-0.048498	4.477572
235.840322	6892.743599	8.595328	-0.048557	4.480086
236.094853	6900.730811	8.600333	-0.048609	4.482598
236.171901	6908.737343	8.605338	-0.048629	4.485114
236.200499	6916.768785	8.610343	-0.048640	4.487636
236.520884	6924.781004	8.615347	-0.048704	4.490151
236.914395	6932.850915	8.620352	-0.048783	4.492683
236.921892	6940.848480	8.625357	-0.048790	4.495190
237.201057	6948.870943	8.630362	-0.048847	4.497704
237.398228	6956.823949	8.635367	-0.048889	4.500195
237.526662	6964.909789	8.640371	-0.048918	4.502726
237.767615	6972.891427	8.645376	-0.048968	4.505223
237.778671	6980.897519	8.650381	-0.048976	4.507725
237.959914	6988.947653	8.655386	-0.049015	4.510241
237.870804	6997.016540	8.660391	-0.049003	4.512760
238.088603	7005.041463	8.665395	-0.049049	4.515265
238.219184	7013.000512	8.670400	-0.049079	4.517747
238.214710	7020.914915	8.675405	-0.049083	4.520214
238.576736	7029.013416	8.680410	-0.049156	4.522738
238.616466	7036.978459	8.685415	-0.049168	4.525218
238.754528	7045.030510	8.690419	-0.049199	4.527724
238.879810	7053.051022	8.695424	-0.049228	4.530219
239.251845	7061.059341	8.700429	-0.049303	4.532709
239.392929	7069.108854	8.705434	-0.049334	4.535210
239.330489	7077.087680	8.710439	-0.049328	4.537688
239.441860	7085.070827	8.715443	-0.049354	4.540165
239.559194	7093.116751	8.720448	-0.049381	4.542661
239.619951	7101.107021	8.725453	-0.049398	4.545138
239.801315	7109.182683	8.730458	-0.049437	4.547640
239.947924	7117.180353	8.735463	-0.049469	4.550117
240.144323	7125.241734	8.740467	-0.049511	4.552612
240.377291	7133.304422	8.745472	-0.049560	4.555106
240.545177	7141.248679	8.750477	-0.049596	4.557562
240.609698	7149.218971	8.755482	-0.049613	4.560025
240.727724	7157.231811	8.760487	-0.049641	4.562499
241.017788	7165.239266	8.765491	-0.049700	4.564971
241.194237	7173.304255	8.770496	-0.049738	4.567459
241.254831	7181.296136	8.775501	-0.049755	4.569923
241.479821	7189.385048	8.780506	-0.049802	4.572416
241.529979	7197.342128	8.785511	-0.049816	4.574866
241.732004	7205.405524	8.790515	-0.049859	4.577348
242.086566	7213.346060	8.795520	-0.049931	4.579791
242.281605	7221.391953	8.800525	-0.049972	4.582265
242.383364	7229.419128	8.805530	-0.049997	4.584732
242.420539	7237.403026	8.810535	-0.050009	4.587184
242.599095	7245.427559	8.815539	-0.050047	4.589647
242.843259	7253.502167	8.820544	-0.050098	4.592124
242.981467	7261.505026	8.825549	-0.050129	4.594578
243.144243	7269.584540	8.830554	-0.050165	4.597054
243.345470	7277.516517	8.835559	-0.050207	4.599484
243.547990	7285.573147	8.840563	-0.050250	4.601950
243.668255	7293.530147	8.845568	-0.050278	4.604385
243.569969	7301.533426	8.850573	-0.050265	4.606832
243.766634	7309.556120	8.855578	-0.050307	4.609284
243.801013	7317.590371	8.860583	-0.050318	4.611738
244.105615	7325.643224	8.865587	-0.050381	4.614197
244.504441	7333.706652	8.870592	-0.050460	4.616657
244.460249	7341.599304	8.875597	-0.050457	4.619064
244.693806	7349.680617	8.880602	-0.050506	4.621527
244.854181	7357.652507	8.885607	-0.050541	4.623956
245.077206	7365.718968	8.890611	-0.050588	4.626412
245.030608	7373.729997	8.895616	-0.050584	4.628850
245.176624	7381.747542	8.900621	-0.050617	4.631289
245.298957	7389.772424	8.905626	-0.050645	4.633728
245.297450	7397.767465	8.910631	-0.050650	4.636158
245.394162	7405.747353	8.915635	-0.050673	4.638581
245.673227	7413.783280	8.920640	-0.050730	4.641020
245.761270	7421.739735	8.925645	-0.050752	4.643433
245.840864	7429.819825	8.930650	-0.050772	4.645883
245.937142	7437.758964	8.935655	-0.050795	4.648289
246.159376	7445.841808	8.940659	-0.050842	4.650737
246.506434	7453.912882	8.945664	-0.050912	4.653180
246.695821	7461.904226	8.950669	-0.050952	4.655598
246.863882	7469.918320	8.955674	-0.050989	4.658021
246.734543	7477.908717	8.960679	-0.050970	4.660436
246.987567	7485.892274	8.965683	-0.051023	4.662848
247.207208	7493.915101	8.970688	-0.051069	4.665270
247.175804	7501.926645	8.975693	-0.051068	4.667687
247.249972	7509.992502	8.980698	-0.051087	4.670120
247.441709	7518.061071	8.985703	-0.051128	4.672552
247.791855	7526.118104	8.990707	-0.051199	4.674979
247.820979	7534.104235	8.995712	-0.051209	4.677384
248.002389	7541.964557	9.000717	-0.051248	4.679749
248.077806	7550.040128	9.005722	-0.051268	4.682179
248.216536	7557.961375	9.010727	-0.051299	4.684560
248.316568	7566.107830	9.015731	-0.051323	4.687008
248.652288	7574.057257	9.020736	-0.051391	4.689395
248.797605	7582.064829	9.025741	-0.051423	4.691799
248.692708	7590.115572	9.030746	-0.051409	4.694215
248.890609	7598.129720	9.035751	-0.051451	4.696618
249.183551	7606.108065	9.040755	-0.051511	4.699008
249.301707	7614.173815	9.045760	-0.051538	4.701425
249.363093	7622.089010	9.050765	-0.051555	4.703794
249.643073	7630.163217	9.055770	-0.051612	4.706210
249.619056	7638.212258	9.060775	-0.051613	4.708618
249.931545	7646.234590	9.065779	-0.051676	4.711016
249.951493	7654.297490	9.070784	-0.051685	4.713425
250.124932	7662.249714	9.075789	-0.051723	4.715799
250.207779	7670.253390	9.080794	-0.051743	4.718188
250.375927	7678.257701	9.085799	-0.051780	4.720576
250.470825	7686.291680	9.090803	-0.051803	4.722972
250.627028	7694.317755	9.095808	-0.051837	4.725363
250.562635	7702.308223	9.100813	-0.051831	4.727744
250.884503	7710.368164	9.105818	-0.051896	4.730143
250.776530	7718.414616	9.110823	-0.051881	4.732538
250.961467	7726.412298	9.115827	-0.051921	4.734916
251.257045	7734.430928	9.120832	-0.051981	4.737299
251.234187	7742.388509	9.125837	-0.051982	4.739664
251.385644	7750.430710	9.130842	-0.052016	4.742052
251.493397	7758.392415	9.135847	-0.052041	4.744415
251.750758	7766.476560	9.140851	-0.052094	4.746813
252.051458	7774.499026	9.145856	-0.052155	4.749191
251.953193	7782.481200	9.150861	-0.052142	4.751557
252.175434	7790.592146	9.155866	-0.052189	4.753959
252.173536	7798.586604	9.160871	-0.052194	4.756326
252.467721	7806.516738	9.165875	-0.052254	4.758672
252.709059	7814.598083	9.170880	-0.052304	4.761061
252.738863	7822.524723	9.175885	-0.052315	4.763405
252.863824	7830.629758	9.180890	-0.052344	4.765799
252.879417	7838.589546	9.185895	-0.052352	4.768150
253.310735	7846.591302	9.190899	-0.052437	4.770511
253.210426	7854.641201	9.195904	-0.052424	4.772886
253.244274	7862.609991	9.200909	-0.052435	4.775236
253.602679	7870.687648	9.205914	-0.052508	4.777616
253.750466	7878.625687	9.210919	-0.052540	4.779954
253.606190	7886.669765	9.215923	-0.052519	4.782323
253.925168	7894.672168	9.220928	-0.052583	4.784677
254.204265	7902.714177	9.225933	-0.052641	4.787042
254.271843	7910.746665	9.230938	-0.052658	4.789403
254.501188	7918.744030	9.235943	-0.052706	4.791753
254.524046	7926.806201	9.240947	-0.052716	4.794121
254.582749	7934.784621	9.245952	-0.052732	4.796463
254.727858	7942.776773	9.250957	-0.052764	4.798807
255.054603	7950.798001	9.255962	-0.052831	4.801158
255.196100	7958.841763	9.260967	-0.052862	4.803516
255.164326	7966.786670	9.265971	-0.052862	4.805844
255.358316	7974.862658	9.270976	-0.052903	4.808208
255.450988	7982.836546	9.275981	-0.052925	4.810542
255.699353	7990.324822	9.280986	-0.052977	4.812732
255.758040	7994.857084	9.285991	-0.052991	4.814057

255.916897	7997.409284	9.290995	-0.053022	4.814803
256.146340	7998.806517	9.296000	-0.053066	4.815210
255.975056	7999.252238	9.301005	-0.053034	4.815341
255.935575	8000.229811	9.306010	-0.053027	4.815627
255.909042	8000.255013	9.311015	-0.053022	4.815635
255.852349	8000.237005	9.316019	-0.053012	4.815630
255.902345	8000.321126	9.321024	-0.053021	4.815654
256.017450	8000.238640	9.326029	-0.053043	4.815629
256.137455	8000.305749	9.331034	-0.053065	4.815648
256.089987	8000.256920	9.336039	-0.053056	4.815634
256.170501	8000.206977	9.341043	-0.053071	4.815619
256.290839	8000.216421	9.346048	-0.053094	4.815621
256.160458	8000.166240	9.351053	-0.053070	4.815607
256.475213	8000.198080	9.356058	-0.053128	4.815615
256.585570	8000.244741	9.361063	-0.053149	4.815628
256.568782	8000.247675	9.366067	-0.053146	4.815629
256.510854	8000.238190	9.371072	-0.053135	4.815627
256.478367	8000.257956	9.376077	-0.053129	4.815633
256.407932	8000.266422	9.381082	-0.053116	4.815636
256.530054	8000.274828	9.386087	-0.053139	4.815637
256.609188	8000.222726	9.391091	-0.053154	4.815622
256.682528	8000.231403	9.396096	-0.053167	4.815624
256.506149	8000.164451	9.401101	-0.053135	4.815605
256.483939	8000.189724	9.406106	-0.053130	4.815613
256.723262	8000.253441	9.411111	-0.053175	4.815630
256.745224	8000.263416	9.416115	-0.053179	4.815633
256.841879	8000.279950	9.421120	-0.053197	4.815637
256.726991	8000.226816	9.426125	-0.053176	4.815622
256.818640	8000.244336	9.431130	-0.053193	4.815627
256.742647	8000.216401	9.436135	-0.053179	4.815619
256.819947	8000.261454	9.441139	-0.053193	4.815632
257.120081	8000.309078	9.446144	-0.053249	4.815645
256.996971	8000.254741	9.451149	-0.053226	4.815629
256.965117	8000.273449	9.456154	-0.053221	4.815635
257.089321	8000.323541	9.461159	-0.053244	4.815649
257.128276	8000.343405	9.466163	-0.053251	4.815655
257.178458	8000.306850	9.471168	-0.053260	4.815644
257.146798	8000.232646	9.476173	-0.053255	4.815622
257.188706	8000.292074	9.481178	-0.053262	4.815639
256.886803	8000.294625	9.486183	-0.053206	4.815641
257.004184	8000.288002	9.491187	-0.053228	4.815639
257.113549	8000.356007	9.496192	-0.053249	4.815658
257.136056	8000.284824	9.501197	-0.053253	4.815637
257.195591	8000.300753	9.506202	-0.053264	4.815642
257.177403	8000.291916	9.511207	-0.053261	4.815639
257.262712	8000.339237	9.516211	-0.053277	4.815653
257.112493	8000.320769	9.521216	-0.053249	4.815648
257.029786	8000.287383	9.526221	-0.053233	4.815639
257.218561	8000.317170	9.531226	-0.053269	4.815646
257.163017	8000.330151	9.536231	-0.053258	4.815651
257.019825	8000.249855	9.541235	-0.053232	4.815628
257.340850	8000.317044	9.546240	-0.053291	4.815646
257.270807	8000.318041	9.551245	-0.053279	4.815646
257.245794	8000.320841	9.556250	-0.053274	4.815647
257.377736	8000.337952	9.561255	-0.053299	4.815652
257.454056	8000.303959	9.566259	-0.053313	4.815641
257.475953	8000.354517	9.571264	-0.053317	4.815656
257.109531	8000.242807	9.576269	-0.053249	4.815625
257.368880	8000.311125	9.581274	-0.053297	4.815644
257.317015	8000.298535	9.586279	-0.053287	4.815641
257.357490	8000.303472	9.591283	-0.053295	4.815642
257.512074	8000.363673	9.596288	-0.053324	4.815659
257.356349	8000.293850	9.601293	-0.053295	4.815639
257.258812	8000.358477	9.606298	-0.053277	4.815658
257.508607	8000.334794	9.611303	-0.053323	4.815650
257.642076	8000.334842	9.616307	-0.053348	4.815650
257.531863	8000.360814	9.621312	-0.053328	4.815658
257.395240	8000.364995	9.626317	-0.053302	4.815660
257.577136	8000.391467	9.631322	-0.053336	4.815666
257.428271	8000.345252	9.636327	-0.053309	4.815654
257.455868	8000.339299	9.641331	-0.053314	4.815652
257.467571	8000.375806	9.646336	-0.053316	4.815662
257.456513	8000.298735	9.651341	-0.053314	4.815640
257.304452	8000.312276	9.656346	-0.053286	4.815645
257.369166	8000.330425	9.661351	-0.053298	4.815650
257.505387	8000.323042	9.666355	-0.053323	4.815647
257.458959	8000.351124	9.671360	-0.053315	4.815655
257.204712	8000.308529	9.676365	-0.053267	4.815644
257.465333	8000.342693	9.681370	-0.053316	4.815653
257.490891	8000.313211	9.686375	-0.053321	4.815644
257.414157	8000.302351	9.691379	-0.053307	4.815641
257.507583	8000.358349	9.696384	-0.053324	4.815657
257.588401	8000.296661	9.701389	-0.053339	4.815639
257.569439	8000.336940	9.706394	-0.053336	4.815651
257.660028	8000.320268	9.711399	-0.053353	4.815645
257.816042	8000.301461	9.716403	-0.053382	4.815639
257.903424	8000.332797	9.721408	-0.053398	4.815648
257.639843	8000.277232	9.726413	-0.053349	4.815633
257.728995	8000.319276	9.731418	-0.053366	4.815645
257.735702	8000.301234	9.736423	-0.053367	4.815639
257.563765	8000.304839	9.741427	-0.053335	4.815641
257.510725	8000.358444	9.746432	-0.053325	4.815657
257.459742	8000.273245	9.751437	-0.053316	4.815632
257.611295	8000.286404	9.756442	-0.053344	4.815636
257.421339	8000.318550	9.761447	-0.053309	4.815646
257.401692	8000.285126	9.766451	-0.053305	4.815636
257.509006	8000.325331	9.771456	-0.053325	4.815647
257.417448	8000.245877	9.776461	-0.053308	4.815625
257.554773	8000.297251	9.781466	-0.053334	4.815639
257.726827	8000.313950	9.786471	-0.053366	4.815643
257.652103	8000.320210	9.791475	-0.053352	4.815645
257.748392	8000.344215	9.796480	-0.053370	4.815652
257.722379	8000.318163	9.801485	-0.053365	4.815644
257.706845	8000.299757	9.806490	-0.053362	4.815639
257.599562	8000.274514	9.811495	-0.053342	4.815632
257.587242	8000.318105	9.816499	-0.053340	4.815645
257.708137	8000.280568	9.821504	-0.053363	4.815633
257.638031	8000.232436	9.826509	-0.053350	4.815620
257.659158	8000.271233	9.831514	-0.053354	4.815631
257.853083	8000.334213	9.836519	-0.053390	4.815648
257.636503	8000.353108	9.841523	-0.053350	4.815655
257.694080	8000.366868	9.846528	-0.053360	4.815659
257.608417	8000.294986	9.851533	-0.053344	4.815638
257.773020	8000.314767	9.856538	-0.053375	4.815643
257.836140	8000.346774	9.861543	-0.053387	4.815652
257.715669	8000.294615	9.866547	-0.053365	4.815637
257.913014	8000.353379	9.871552	-0.053401	4.815654
257.832014	8000.289048	9.876557	-0.053386	4.815635
257.938445	8000.327103	9.881562	-0.053406	4.815646
257.944931	8000.312262	9.886567	-0.053407	4.815641
257.800736	8000.316319	9.891571	-0.053381	4.815643
257.863523	8000.316281	9.896576	-0.053392	4.815643
257.750331	8000.257832	9.901581	-0.053371	4.815626
258.071254	8000.338907	9.906586	-0.053431	4.815649
257.730857	8000.314127	9.911591	-0.053368	4.815643
257.586726	8000.292553	9.916595	-0.053341	4.815637
257.776792	8000.357606	9.921600	-0.053377	4.815656
257.787443	8000.297977	9.926605	-0.053378	4.815638
257.698375	8000.308274	9.931610	-0.053362	4.815641
257.914866	8000.353467	9.936615	-0.053402	4.815654
258.097627	8000.305193	9.941619	-0.053436	4.815639
258.066738	8000.347413	9.946624	-0.053431	4.815651
257.825645	8000.289011	9.951629	-0.053386	4.815635
258.003634	8000.279107	9.956634	-0.053419	4.815631
258.007845	8000.278112	9.961639	-0.053420	4.815631
258.032197	8000.263562	9.966643	-0.053424	4.815627
258.099438	8000.315929	9.971648	-0.053437	4.815642
257.986564	8000.263894	9.976653	-0.053416	4.815627
257.979267	8000.324655	9.981658	-0.053415	4.815645
257.912821	8000.308622	9.986663	-0.053402	4.815641
257.699586	8000.262424	9.991667	-0.053363	4.815628
257.695186	8000.356340	9.996672	-0.053362	4.815656
257.723719	8000.292731	10.001677	-0.053367	4.815637
257.945079	8000.346547	10.006682	-0.053409	4.815651
257.974529	8000.365189	10.011687	-0.053414	4.815657
257.751934	8000.313497	10.016691	-0.053373	4.815643
257.954175	8000.313601	10.021696	-0.053411	4.815642
257.897377	8000.295589	10.026701	-0.053400	4.815637
257.979504	8000.271303	10.031706	-0.053415	4.815629
258.160068	8000.274257	10.036711	-0.053449	4.815629
258.037236	8000.290411	10.041715	-0.053426	4.815635
258.035242	8000.363008	10.046720	-0.053426	4.815656
257.959952	8000.321198	10.051725	-0.053412	4.815644
258.155988	8000.350037	10.056730	-0.053448	4.815651
258.108534	8000.289458	10.061735	-0.053440	4.815634
258.028687	8000.240098	10.066739	-0.053425	4.815620
258.058122	8000.322820	10.071744	-0.053430	4.815644
257.953713	8000.284806	10.076749	-0.053411	4.815633
258.247937	8000.261849	10.081754	-0.053466	4.815625
258.330668	8000.342238	10.086759	-0.053481	4.815648
258.224242	8000.274287	10.091763	-0.053461	4.815629
258.104691	8000.333215	10.096768	-0.053439	4.815647
258.081986	8000.230320	10.101773	-0.053435	4.815617
258.201041	8000.307029	10.106778	-0.053457	4.815639
258.144059	8000.311443	10.111783	-0.053447	4.815640
258.230771	8000.257328	10.116787	-0.053463	4.815624
258.370573	8000.334377	10.121792	-0.053489	4.815646
258.126569	8000.314375	10.126797	-0.053444	4.815641
258.137860	8000.326312	10.131802	-0.053446	4.815645
258.289791	8000.283942	10.136807	-0.053474	4.815631
258.357275	8000.259416	10.141811	-0.053487	4.815624
258.247324	8000.315297	10.146816	-0.053466	4.815641
258.162484	8000.247699	10.151821	-0.053451	4.815621
258.067304	8000.282461	10.156826	-0.053433	4.815632
258.199310	8000.311322	10.161831	-0.053458	4.815640
258.023100	8000.286020	10.166835	-0.053425	4.815633
258.113805	8000.333430	10.171840	-0.053442	4.815647
258.142154	8000.307198	10.176845	-0.053447	4.815639
258.060402	8000.278098	10.181850	-0.053432	4.815631
258.214298	8000.317997	10.186855	-0.053461	4.815642
258.199834	8000.323106	10.191859	-0.053458	4.815643
258.336245	8000.336019	10.196864	-0.053483	4.815646
258.280312	8000.318021	10.201869	-0.053473	4.815641
258.506170	8000.299287	10.206874	-0.053515	4.815635
258.465547	8000.285812	10.211879	-0.053508	4.815631
258.330042	8000.322051	10.216883	-0.053482	4.815642
258.415808	8000.336273	10.221888	-0.053499	4.815646
258.293821	8000.320400	10.226893	-0.053476	4.815642
258.371416	8000.333421	10.231898	-0.053490	4.815646
258.296408	8000.331132	10.236903	-0.053476	4.815645
258.418819	8000.347020	10.241907	-0.053499	4.815649
258.332131	8000.358424	10.246912	-0.053483	4.815653
258.323433	8000.265370	10.251917	-0.053482	4.815626
258.519776	8000.326255	10.256922	-0.053518	4.815643
258.406430	8000.378876	10.261927	-0.053497	4.815659
258.186437	8000.295185	10.266931	-0.053456	4.815635
258.514598	8000.277055	10.271936	-0.053517	4.815628
258.474502	8000.284948	10.276941	-0.053510	4.815631
258.277050	8000.273183	10.281946	-0.053473	4.815628
258.445679	8000.340023	10.286951	-0.053505	4.815647
258.397736	8000.322156	10.291955	-0.053496	4.815642
258.432616	8000.383607	10.296960	-0.053502	4.815660
258.304462	8000.333457	10.301965	-0.053479	4.815646
258.538972	8000.312729	10.306970	-0.053522	4.815639
258.353821	8000.326796	10.311975	-0.053488	4.815644
258.367796	8000.298193	10.316979	-0.053491	4.815635
258.374724	8000.381616	10.321984	-0.053492	4.815660
258.473479	8000.299928	10.326989	-0.053510	4.815635
258.373493	8000.322863	10.331994	-0.053492	4.815642
258.423646	8000.287375	10.336999	-0.053501	4.815632
258.456961	8000.256951	10.342003	-0.053507	4.815623
258.479675	8000.366265	10.347008	-0.053512	4.815655
258.264891	8000.298679	10.352013	-0.053472	4.815636
258.374888	8000.253488	10.357018	-0.053492	4.815622
258.495443	8000.305658	10.362023	-0.053515	4.815637
258.352356	8000.292645	10.367027	-0.053488	4.815634
258.494329	8000.340894	10.372032	-0.053515	4.815647
258.348933	8000.276578	10.377037	-0.053488	4.815629
258.387896	8000.294307	10.382042	-0.053495	4.815634
258.432772	8000.336697	10.387047	-0.053503	4.815646
258.473729	8000.323487	10.392051	-0.053511	4.815642
258.630121	8000.361291	10.397056	-0.053540	4.815652
258.275709	8000.306376	10.402061	-0.053474	4.815638
258.389265	8000.254835	10.407066	-0.053495	4.815622
258.562996	8000.361276	10.412071	-0.053528	4.815653
258.418925	8000.300185	10.417075	-0.053501	4.815636
258.430639	8000.333489	10.422080	-0.053503	4.815645
258.458318	8000.356375	10.427085	-0.053509	4.815652
258.493026	8000.369762	10.432090	-0.053515	4.815656
258.529803	8000.390660	10.437095	-0.053522	4.815661
258.420907	8000.347233	10.442099	-0.053502	4.815649
258.589548	8000.380965	10.447104	-0.053533	4.815658
258.445885	8000.308133	10.452109	-0.053506	4.815638
258.480177	8000.365303	10.457114	-0.053513	4.815654
258.577664	8000.383989	10.462119	-0.053531	4.815659
258.596986	8000.324499	10.467123	-0.053535	4.815642
258.685442	8000.340902	10.472128	-0.053551	4.815646
258.461718	8000.327638	10.477133	-0.053510	4.815643
258.714893	8000.393725	10.482138	-0.053557	4.815661
258.526699	8000.349001	10.487143	-0.053522	4.815649
258.413634	8000.291621	10.492147	-0.053501	4.815633
258.654144	8000.345753	10.497152	-0.053546	4.815648
258.666539	8000.326735	10.502157	-0.053548	4.815642
258.703159	8000.355107	10.507162	-0.053555	4.815650
258.860060	8000.359811	10.512167	-0.053584	4.815651
258.683232	8000.331293	10.517171	-0.053551	4.815643
258.776407	8000.346705	10.522176	-0.053569	4.815647
258.664761	8000.348089	10.527181	-0.053548	4.815648
258.719527	8000.319084	10.532186	-0.053558	4.815640
258.693283	8000.336816	10.537191	-0.053553	4.815645
258.810776	8000.305631	10.542195	-0.053575	4.815635
258.822629	8000.366707	10.547200	-0.053578	4.815653
258.643465	8000.346695	10.552205	-0.053544	4.815648
258.949456	8000.352768	10.557210	-0.053601	4.815648
258.745447	8000.395364	10.562215	-0.053563	4.815662
258.612712	8000.299213	10.567219	-0.053539	4.815634
258.724401	8000.361920	10.572224	-0.053560	4.815652
258.758573	8000.333646	10.577229	-0.053566	4.815644
258.821091	8000.388074	10.582234	-0.053578	4.815659
258.993998	8000.363135	10.587239	-0.053610	4.815651
258.839531	8000.345663	10.592243	-0.053581	4.815647
259.004452	8000.371859	10.597248	-0.053612	4.815654
258.815513	8000.352755	10.602253	-0.053577	4.815649
258.784792	8000.361870	10.607258	-0.053571	4.815652
258.872058	8000.381457	10.612263	-0.053587	4.815657
258.849080	8000.326617	10.617267	-0.053583	4.815641
259.006663	8000.391142	10.622272	-0.053613	4.815659
258.893426	8000.412793	10.627277	-0.053592	4.815666
258.765870	8000.333814	10.632282	-0.053568	4.815644
258.613513	8000.356962	10.637287	-0.053540	4.815651
258.620142	8000.309013	10.642291	-0.053541	4.815637
258.966577	8000.369149	10.647296	-0.053605	4.815653
259.046249	8000.350163	10.652301	-0.053620	4.815647
258.868556	8000.284249	10.657306	-0.053587	4.815629
258.703817	8000.342439	10.662311	-0.053557	4.815646
258.698623	8000.341291	10.667315	-0.053556	4.815646
258.864083	8000.385652	10.672320	-0.053587	4.815658
258.806495	8000.361219	10.677325	-0.053576	4.815651
258.734540	8000.384612	10.682330	-0.053563	4.815659
258.698640	8000.413935	10.687335	-0.053556	4.815667
258.570055	8000.359505	10.692339	-0.053532	4.815652
258.943623	8000.399791	10.697344	-0.053602	4.815662
258.614864	8000.395491	10.702349	-0.053540	4.815662
258.767417	8000.385172	10.707354	-0.053569	4.815659
258.917645	8000.387632	10.712359	-0.053597	4.815659
258.895322	8000.355230	10.717363	-0.053593	4.815649
258.779222	8000.408875	10.722368	-0.053571	4.815665
258.608632	8000.416772	10.727373	-0.053540	4.815669
258.615811	8000.346404	10.732378	-0.053541	4.815648
258.722664	8000.368447	10.737383	-0.053561	4.815654
258.712972	8000.305279	10.742387	-0.053559	4.815636
258.872724	8000.311098	10.747392	-0.053589	4.815636
258.740922	8000.360214	10.752397	-0.053564	4.815651
258.782990	8000.351294	10.757402	-0.053572	4.815649
258.855699	8000.398412	10.762407	-0.053586	4.815662
258.916423	8000.388729	10.767411	-0.053597	4.815659
258.955304	8000.370144	10.772416	-0.053605	4.815653
258.683722	8000.399887	10.777421	-0.053554	4.815663
258.796099	8000.400660	10.782426	-0.053575	4.815663
259.016277	8000.410671	10.787431	-0.053616	4.815665
258.693109	8000.350924	10.792435	-0.053556	4.815649
258.865186	8000.368693	10.797440	-0.053588	4.815653
258.704802	8000.357532	10.802445	-0.053558	4.815651
258.884456	8000.328432	10.807450	-0.053592	4.815641
258.960345	8000.335017	10.812455	-0.053606	4.815643
259.041799	8000.293631	10.817459	-0.053621	4.815631
259.040416	8000.431390	10.822464	-0.053621	4.815671
258.773234	8000.378966	10.827469	-0.053571	4.815657
259.126997	8000.359119	10.832474	-0.053637	4.815649
259.000366	8000.360258	10.837479	-0.053614	4.815650
258.898217	8000.297715	10.842483	-0.053595	4.815632
259.009869	8000.363626	10.847488	-0.053615	4.815651
258.941178	8000.375325	10.852493	-0.053603	4.815655
258.905693	8000.360865	10.857498	-0.053596	4.815651
258.798481	8000.375137	10.862503	-0.053576	4.815656
258.616499	8000.329447	10.867507	-0.053542	4.815643
258.794923	8000.330231	10.872512	-0.053576	4.815642
258.950368	8000.346660	10.877517	-0.053605	4.815646
258.943531	8000.358301	10.882522	-0.053603	4.815650
258.983613	8000.370709	10.887527	-0.053611	4.815653
258.998755	8000.375233	10.892531	-0.053614	4.815655
258.895948	8000.373557	10.897536	-0.053595	4.815655
258.795001	8000.312102	10.902541	-0.053576	4.815637
258.905844	8000.279741	10.907546	-0.053597	4.815627
259.047989	8000.361103	10.912551	-0.053623	4.815650
259.080496	8000.352027	10.917555	-0.053629	4.815647
258.977139	8000.372771	10.922560	-0.053610	4.815654
258.731873	8000.361290	10.927565	-0.053565	4.815652
258.902999	8000.291465	10.932570	-0.053596	4.815631
259.113749	8000.352588	10.937575	-0.053636	4.815647
258.719282	8000.326921	10.942579	-0.053562	4.815642
258.935227	8000.371040	10.947584	-0.053603	4.815654
258.994638	8000.325022	10.952589	-0.053614	4.815640
258.965515	8000.349115	10.957594	-0.053608	4.815647
259.103326	8000.381277	10.962599	-0.053634	4.815656
259.068679	8000.344402	10.967603	-0.053628	4.815645
259.131006	8000.363582	10.972608	-0.053639	4.815651
258.933815	8000.351819	10.977613	-0.053603	4.815648
258.992115	8000.316463	10.982618	-0.053614	4.815637
259.086484	8000.432290	10.987623	-0.053631	4.815671
258.813386	8000.333844	10.992627	-0.053580	4.815643
259.013187	8000.387311	10.997632	-0.053618	4.815658
259.343660	8000.322227	11.002637	-0.053679	4.815637
259.055323	8000.318586	11.007642	-0.053626	4.815638
259.085042	8000.365002	11.012647	-0.053631	4.815651
259.194957	8000.350783	11.017651	-0.053652	4.815646
259.164023	8000.360962	11.022656	-0.053646	4.815650
259.100564	8000.374881	11.027661	-0.053634	4.815654
258.850643	8000.316332	11.032666	-0.053588	4.815638
259.225232	8000.341683	11.037671	-0.053658	4.815644
259.124913	8000.280238	11.042675	-0.053639	4.815626
259.091157	8000.280758	11.047680	-0.053633	4.815626
259.031328	8000.305418	11.052685	-0.053622	4.815634
259.053499	8000.307921	11.057690	-0.053626	4.815635
259.044503	8000.360112	11.062695	-0.053624	4.815650
259.010302	8000.368102	11.067699	-0.053618	4.815652
259.059814	8000.373187	11.072704	-0.053627	4.815654
258.891526	8000.352285	11.077709	-0.053596	4.815648
258.948250	8000.377781	11.082714	-0.053606	4.815656
259.103561	8000.342943	11.087719	-0.053635	4.815645
259.019286	8000.308461	11.092723	-0.053620	4.815635
259.013849	8000.324397	11.097728	-0.053619	4.815640
259.044451	8000.358011	11.102733	-0.053625	4.815649
259.051761	8000.347454	11.107738	-0.053626	4.815646
259.041391	8000.380398	11.112743	-0.053624	4.815656
258.823340	8000.295669	11.117747	-0.053583	4.815632
259.112943	8000.335651	11.122752	-0.053637	4.815642
258.885544	8000.346891	11.127757	-0.053595	4.815647
258.871581	8000.321035	11.132762	-0.053593	4.815639
259.090326	8000.381220	11.137767	-0.053633	4.815656
259.015100	8000.313777	11.142771	-0.053619	4.815636
258.916402	8000.328189	11.147776	-0.053601	4.815641
258.979881	8000.332435	11.152781	-0.053613	4.815642
258.925917	8000.343306	11.157786	-0.053603	4.815646
259.047841	8000.385888	11.162791	-0.053626	4.815657
258.960677	8000.368448	11.167795	-0.053610	4.815653
259.133648	8000.385164	11.172800	-0.053642	4.815657
259.141459	8000.358595	11.177805	-0.053643	4.815649
258.952326	8000.297834	11.182810	-0.053608	4.815632
259.087087	8000.392960	11.187815	-0.053633	4.815659
259.234777	8000.312072	11.192819	-0.053661	4.815635
259.083285	8000.290376	11.197824	-0.053633	4.815629
259.056752	8000.345484	11.202829	-0.053628	4.815646
258.847336	8000.353815	11.207834	-0.053589	4.815649
258.965865	8000.340804	11.212839	-0.053611	4.815645
258.862879	8000.360486	11.217843	-0.053592	4.815651
259.083008	8000.421762	11.222848	-0.053633	4.815668
259.073121	8000.376747	11.227853	-0.053631	4.815655
259.026652	8000.289481	11.232858	-0.053622	4.815629
259.181146	8000.337936	11.237863	-0.053651	4.815643
259.211745	8000.312808	11.242867	-0.053657	4.815635
258.959956	8000.331126	11.247872	-0.053610	4.815642
258.946017	8000.343719	11.252877	-0.053608	4.815646
259.085182	8000.340658	11.257882	-0.053634	4.815644
258.976792	8000.414721	11.262887	-0.053614	4.815666
258.816280	8000.342680	11.267891	-0.053584	4.815646
259.144636	8000.351255	11.272896	-0.053645	4.815647
259.144715	8000.333104	11.277901	-0.053645	4.815641
258.951996	8000.316075	11.282906	-0.053609	4.815637
259.066620	8000.378831	11.287911	-0.053631	4.815655
258.999043	8000.311512	11.292915	-0.053618	4.815636
258.959345	8000.370678	11.297920	-0.053611	4.815653
258.864517	8000.402242	11.302925	-0.053593	4.815663
259.029916	8000.336595	11.307930	-0.053624	4.815643
259.204257	8000.351197	11.312935	-0.053656	4.815646
259.027956	8000.373953	11.317939	-0.053624	4.815654
259.304008	8000.438280	11.322944	-0.053675	4.815671
259.346627	8000.391988	11.327949	-0.053683	4.815658
259.089427	8000.302345	11.332954	-0.053635	4.815633
259.320203	8000.353115	11.337959	-0.053678	4.815646
259.257163	8000.344613	11.342963	-0.053667	4.815644
259.265561	8000.344754	11.347968	-0.053668	4.815644
259.014308	8000.315019	11.352973	-0.053621	4.815637
259.094258	8000.374004	11.357978	-0.053636	4.815654
259.112042	8000.364687	11.362983	-0.053640	4.815651
259.071389	8000.359755	11.367987	-0.053632	4.815650
259.342545	8000.333219	11.372992	-0.053683	4.815641
259.352055	8000.375032	11.377997	-0.053685	4.815653
259.027500	8000.360119	11.383002	-0.053624	4.815650
259.139869	8000.333123	11.388007	-0.053645	4.815641
259.268467	8000.325617	11.393011	-0.053669	4.815639
259.330060	8000.359738	11.398016	-0.053681	4.815648
259.296745	8000.331429	11.403021	-0.053675	4.815640
259.146675	8000.330048	11.408026	-0.053647	4.815641
259.214133	8000.357856	11.413031	-0.053659	4.815648
259.237022	8000.312309	11.418035	-0.053664	4.815635
259.086511	8000.392092	11.423040	-0.053636	4.815659
259.080029	8000.391991	11.428045	-0.053634	4.815659
258.861548	8000.302982	11.433050	-0.053594	4.815634
259.082942	8000.384571	11.438055	-0.053635	4.815657
259.007219	8000.347025	11.443059	-0.053621	4.815646
259.128267	8000.347940	11.448064	-0.053644	4.815646
259.083366	8000.336530	11.453069	-0.053635	4.815643
259.304498	8000.305971	11.458074	-0.053677	4.815633
259.350545	8000.357995	11.463079	-0.053685	4.815648
259.331998	8000.302158	11.468083	-0.053682	4.815631
259.462227	8000.300019	11.473088	-0.053706	4.815630
259.349634	8000.347313	11.478093	-0.053685	4.815645
259.391875	8000.319170	11.483098	-0.053693	4.815636
259.231589	8000.377433	11.488103	-0.053663	4.815654
259.263553	8000.321354	11.493107	-0.053669	4.815637
259.246192	8000.345640	11.498112	-0.053666	4.815645
259.284227	8000.374035	11.503117	-0.053673	4.815653
259.182479	8000.331791	11.508122	-0.053654	4.815641
259.228395	8000.398764	11.513127	-0.053663	4.815660
259.232288	8000.301640	11.518131	-0.053664	4.815632
259.271116	8000.290531	11.523136	-0.053671	4.815628
259.306100	8000.359462	11.528141	-0.053678	4.815648
259.362937	8000.315538	11.533146	-0.053688	4.815635
259.328182	8000.369444	11.538151	-0.053682	4.815651
259.307195	8000.337064	11.543155	-0.053678	4.815642
259.522241	8000.338448	11.548160	-0.053718	4.815641
259.332686	8000.346034	11.553165	-0.053683	4.815644
259.469508	8000.301281	11.558170	-0.053708	4.815631
259.502869	8000.347757	11.563175	-0.053715	4.815644
259.351193	8000.333534	11.568179	-0.053686	4.815641
259.405403	8000.366466	11.573184	-0.053697	4.815650
259.402615	8000.336519	11.578189	-0.053696	4.815641
259.175822	8000.256986	11.583194	-0.053654	4.815619
259.274641	8000.388906	11.588199	-0.053672	4.815657
259.322863	8000.358726	11.593203	-0.053681	4.815648
259.407587	8000.348367	11.598208	-0.053697	4.815645
259.288684	8000.357108	11.603213	-0.053675	4.815648
259.293778	8000.283501	11.608218	-0.053676	4.815626
259.444759	8000.355396	11.613223	-0.053704	4.815646
259.260135	8000.338498	11.618227	-0.053670	4.815642
259.337858	8000.404924	11.623232	-0.053684	4.815661
259.367693	8000.373375	11.628237	-0.053690	4.815652
259.267576	8000.299116	11.633242	-0.053671	4.815631
259.325120	8000.329966	11.638247	-0.053682	4.815640
259.379786	8000.299891	11.643251	-0.053692	4.815631
259.397462	8000.314068	11.648256	-0.053696	4.815635
259.391224	8000.334264	11.653261	-0.053695	4.815641
259.329325	8000.299079	11.658266	-0.053683	4.815631
259.535731	8000.366540	11.663271	-0.053722	4.815649
259.274856	8000.331307	11.668275	-0.053673	4.815640
259.241818	8000.298730	11.673280	-0.053667	4.815631
259.267900	8000.366448	11.678285	-0.053672	4.815651
259.375101	8000.304122	11.683290	-0.053692	4.815632
259.370368	8000.373472	11.688295	-0.053691	4.815652
259.317320	8000.324547	11.693299	-0.053681	4.815638
259.380642	8000.381125	11.698304	-0.053693	4.815654
259.413793	8000.375263	11.703309	-0.053699	4.815652
259.336958	8000.310997	11.708314	-0.053685	4.815634
259.329036	8000.340777	11.713319	-0.053684	4.815643
259.345581	8000.281242	11.718323	-0.053687	4.815625
259.405700	8000.302522	11.723328	-0.053698	4.815631
259.536079	8000.369808	11.728333	-0.053722	4.815650
259.482656	8000.323013	11.733338	-0.053712	4.815637
259.489427	8000.354102	11.738343	-0.053714	4.815646
259.303048	8000.307270	11.743347	-0.053679	4.815633
259.357392	8000.309230	11.748352	-0.053689	4.815633
259.517976	8000.302247	11.753357	-0.053719	4.815631
259.491682	8000.318911	11.758362	-0.053714	4.815636
259.673972	8000.367821	11.763367	-0.053748	4.815649
259.512708	8000.316059	11.768371	-0.053718	4.815635
259.510295	8000.328841	11.773376	-0.053718	4.815638
259.468193	8000.288639	11.778381	-0.053710	4.815627
259.467565	8000.285430	11.783386	-0.053710	4.815626
259.461765	8000.345150	11.788391	-0.053709	4.815643
259.400506	8000.299295	11.793395	-0.053698	4.815630
259.661442	8000.266183	11.798400	-0.053746	4.815619
259.633685	8000.281755	11.803405	-0.053741	4.815624
259.338952	8000.241696	11.808410	-0.053686	4.815614
259.459361	8000.320568	11.813415	-0.053709	4.815636
259.354728	8000.286820	11.818419	-0.053690	4.815627
259.466417	8000.274766	11.823424	-0.053710	4.815623
259.479213	8000.313429	11.828429	-0.053713	4.815634
259.636012	8000.294636	11.833434	-0.053742	4.815628
259.591437	8000.302456	11.838439	-0.053734	4.815630
259.517720	8000.283099	11.843443	-0.053720	4.815625
259.443767	8000.271214	11.848448	-0.053706	4.815622
259.454456	8000.327999	11.853453	-0.053708	4.815638
259.486285	8000.302891	11.858458	-0.053714	4.815631
259.597129	8000.337817	11.863463	-0.053735	4.815641
259.576359	8000.318257	11.868467	-0.053731	4.815635
259.594128	8000.275830	11.873472	-0.053735	4.815622
259.507313	8000.323545	11.878477	-0.053719	4.815637
259.520280	8000.260747	11.883482	-0.053721	4.815618
259.611992	8000.304973	11.888487	-0.053738	4.815631
259.533017	8000.305822	11.893491	-0.053723	4.815631
259.518823	8000.278894	11.898496	-0.053721	4.815624
259.555611	8000.304064	11.903501	-0.053728	4.815631
259.507319	8000.228516	11.908506	-0.053719	4.815609
259.504042	8000.263713	11.913511	-0.053718	4.815619
259.417323	8000.223850	11.918515	-0.053702	4.815608
259.434752	8000.263657	11.923520	-0.053705	4.815620
259.457832	8000.275787	11.928525	-0.053710	4.815623
259.354640	8000.279445	11.933530	-0.053691	4.815625
259.538771	8000.378584	11.938535	-0.053725	4.815653
259.306091	8000.349151	11.943539	-0.053682	4.815645
259.495659	8000.287104	11.948544	-0.053717	4.815626
259.586784	8000.319571	11.953549	-0.053734	4.815635
259.476982	8000.295352	11.958554	-0.053714	4.815629
259.599771	8000.322997	11.963559	-0.053737	4.815636
259.472769	8000.205576	11.968563	-0.053713	4.815602
259.606572	8000.260102	11.973568	-0.053738	4.815618
259.495614	8000.311695	11.978573	-0.053717	4.815633
259.629241	8000.289319	11.983578	-0.053742	4.815626
259.600406	8000.335846	11.988583	-0.053737	4.815640
259.294233	8000.308416	11.993587	-0.053680	4.815633
259.310386	8000.353543	11.998592	-0.053683	4.815646
259.581487	8000.402837	12.003597	-0.053734	4.815660
259.509824	8000.372833	12.008602	-0.053720	4.815651
259.690182	8000.434529	12.013607	-0.053754	4.815668
259.599916	8000.382859	12.018611	-0.053737	4.815654
259.512939	8000.356876	12.023616	-0.053721	4.815646
259.417946	8000.420479	12.028621	-0.053703	4.815665
259.501690	8000.308639	12.033626	-0.053719	4.815632
259.598952	8000.368976	12.038631	-0.053737	4.815650
259.258809	8000.338855	12.043635	-0.053674	4.815642
259.307255	8000.356740	12.048640	-0.053683	4.815647
259.444759	8000.304522	12.053645	-0.053709	4.815631
259.545371	8000.298695	12.058650	-0.053727	4.815629
259.541801	8000.297573	12.063655	-0.053727	4.815629
259.609038	8000.343535	12.068659	-0.053739	4.815642
259.610183	8000.275203	12.073664	-0.053740	4.815622
259.579690	8000.249076	12.078669	-0.053734	4.815615
259.586491	8000.286573	12.083674	-0.053735	4.815626
259.479493	8000.322210	12.088679	-0.053716	4.815636
259.127640	8000.321803	12.093683	-0.053650	4.815638
259.410854	8000.278375	12.098688	-0.053703	4.815624
259.477283	8000.338208	12.103693	-0.053715	4.815641
259.313545	8000.289610	12.108698	-0.053685	4.815628
259.680088	8000.308423	12.113703	-0.053753	4.815631
259.730200	8000.344492	12.118707	-0.053763	4.815642
259.673458	8000.295506	12.123712	-0.053752	4.815628
259.582979	8000.349570	12.128717	-0.053735	4.815644
259.643610	8000.284347	12.133722	-0.053746	4.815625
259.668539	8000.374475	12.138727	-0.053751	4.815651
259.555582	8000.353408	12.143731	-0.053730	4.815645
259.484660	8000.306327	12.148736	-0.053717	4.815632
259.657770	8000.335863	12.153741	-0.053749	4.815640
259.779361	8000.309018	12.158746	-0.053772	4.815631
259.782239	8000.336838	12.163751	-0.053773	4.815639
259.447452	8000.318553	12.168755	-0.053710	4.815636
259.493001	8000.325711	12.173760	-0.053719	4.815637
259.428232	8000.339609	12.178765	-0.053707	4.815642
259.494088	8000.346030	12.183770	-0.053719	4.815643
259.649907	8000.375283	12.188775	-0.053748	4.815651
259.581769	8000.296206	12.193779	-0.053736	4.815628
259.631915	8000.330140	12.198784	-0.053745	4.815638
259.720419	8000.362565	12.203789	-0.053762	4.815647
259.576678	8000.334586	12.208794	-0.053735	4.815640
259.501475	8000.410261	12.213799	-0.053721	4.815662
259.495035	8000.301219	12.218803	-0.053720	4.815630
259.544289	8000.282804	12.223808	-0.053729	4.815625
259.435236	8000.351516	12.228813	-0.053709	4.815645
259.363408	8000.331122	12.233818	-0.053695	4.815640
259.705843	8000.374106	12.238823	-0.053759	4.815651
259.393981	8000.355128	12.243827	-0.053701	4.815646
259.390191	8000.327301	12.248832	-0.053701	4.815638
259.545662	8000.366161	12.253837	-0.053730	4.815649
259.363456	8000.279879	12.258842	-0.053696	4.815625
259.381413	8000.296198	12.263847	-0.053699	4.815629
259.396783	8000.325290	12.268851	-0.053702	4.815638
259.631339	8000.299224	12.273856	-0.053746	4.815629
259.471326	8000.324382	12.278861	-0.053716	4.815637
259.578116	8000.252437	12.283866	-0.053736	4.815616
259.727824	8000.261297	12.288871	-0.053764	4.815617
259.583671	8000.298462	12.293875	-0.053737	4.815629
259.561621	8000.330148	12.298880	-0.053733	4.815638
259.442430	8000.323932	12.303885	-0.053711	4.815637
259.575428	8000.271640	12.308890	-0.053736	4.815621
259.633713	8000.337748	12.313895	-0.053747	4.815640
259.583692	8000.224790	12.318899	-0.053737	4.815607
259.653032	8000.291079	12.323904	-0.053750	4.815626
259.606675	8000.343728	12.328909	-0.053742	4.815642
259.515365	8000.261068	12.333914	-0.053725	4.815618
259.636331	8000.322860	12.338919	-0.053747	4.815636
259.591064	8000.296492	12.343923	-0.053739	4.815628
259.521433	8000.284678	12.348928	-0.053726	4.815625
259.558637	8000.348305	12.353933	-0.053733	4.815644
259.657714	8000.339249	12.358938	-0.053751	4.815641
259.707440	8000.343270	12.363943	-0.053761	4.815641
259.654425	8000.314639	12.368947	-0.053751	4.815633
259.717796	8000.267617	12.373952	-0.053763	4.815619
259.618024	8000.311916	12.378957	-0.053744	4.815633
259.526006	8000.304008	12.383962	-0.053727	4.815631
259.766719	8000.367759	12.388967	-0.053772	4.815648
259.709988	8000.315569	12.393971	-0.053762	4.815633
259.639467	8000.288788	12.398976	-0.053748	4.815626
259.614094	8000.349256	12.403981	-0.053744	4.815644
259.695806	8000.323895	12.408986	-0.053759	4.815636
259.708767	8000.345473	12.413991	-0.053762	4.815642
259.503103	8000.329298	12.418995	-0.053723	4.815638
259.546576	8000.308652	12.424000	-0.053731	4.815632
259.589397	8000.391597	12.429005	-0.053739	4.815656
259.496391	8000.336678	12.434010	-0.053722	4.815641
259.560544	8000.320643	12.439015	-0.053734	4.815636
259.523057	8000.316830	12.444019	-0.053727	4.815635
259.509936	8000.289919	12.449024	-0.053725	4.815627
259.811324	8000.338641	12.454029	-0.053781	4.815640
259.771921	8000.268577	12.459034	-0.053774	4.815619
259.668452	8000.336314	12.464039	-0.053755	4.815640
259.645942	8000.357311	12.469043	-0.053750	4.815646
259.554668	8000.301353	12.474048	-0.053733	4.815630
259.576312	8000.364726	12.479053	-0.053738	4.815648
259.467457	8000.324501	12.484058	-0.053717	4.815637
259.569004	8000.313349	12.489063	-0.053736	4.815633
259.499305	8000.275901	12.494067	-0.053723	4.815623
259.426195	8000.330248	12.499072	-0.053710	4.815639
259.538445	8000.344904	12.504077	-0.053731	4.815643
259.619326	8000.242630	12.509082	-0.053746	4.815612
259.884177	8000.333477	12.514087	-0.053795	4.815638
259.685744	8000.362279	12.519091	-0.053758	4.815647
259.710680	8000.315696	12.524096	-0.053763	4.815633
259.698638	8000.355022	12.529101	-0.053761	4.815645
259.549960	8000.292785	12.534106	-0.053733	4.815627
259.912375	8000.293374	12.539111	-0.053801	4.815626
259.828763	8000.316577	12.544115	-0.053785	4.815633
259.787817	8000.275326	12.549120	-0.053778	4.815621
259.698641	8000.376405	12.554125	-0.053761	4.815651
259.862708	8000.294716	12.559130	-0.053792	4.815626
259.766499	8000.339074	12.564135	-0.053774	4.815640
259.556393	8000.327099	12.569139	-0.053735	4.815637
259.723316	8000.305267	12.574144	-0.053766	4.815630
259.886774	8000.292991	12.579149	-0.053796	4.815626
259.736453	8000.258497	12.584154	-0.053768	4.815616
259.965991	8000.356243	12.589159	-0.053811	4.815644
259.833982	8000.344476	12.594163	-0.053787	4.815641
259.680858	8000.302459	12.599168	-0.053758	4.815630
259.724701	8000.325609	12.604173	-0.053766	4.815636
259.668685	8000.308677	12.609178	-0.053756	4.815631
259.631842	8000.345461	12.614183	-0.053749	4.815642
259.714152	8000.336131	12.619187	-0.053765	4.815639
259.630338	8000.319812	12.624192	-0.053749	4.815635
259.799791	8000.331132	12.629197	-0.053781	4.815637
259.664564	8000.355627	12.634202	-0.053756	4.815645
259.674137	8000.356856	12.639207	-0.053757	4.815646
259.837962	8000.359539	12.644211	-0.053788	4.815646
259.666684	8000.354607	12.649216	-0.053756	4.815645
259.790158	8000.426054	12.654221	-0.053779	4.815665
259.754134	8000.378474	12.659226	-0.053772	4.815651
259.804159	8000.326962	12.664231	-0.053782	4.815636
259.704072	8000.296493	12.669235	-0.053763	4.815628
259.949040	8000.349633	12.674240	-0.053809	4.815642
259.926938	8000.381318	12.679245	-0.053805	4.815651
259.706574	8000.306159	12.684250	-0.053764	4.815631
259.957424	8000.250454	12.689255	-0.053811	4.815613
259.823656	8000.329444	12.694259	-0.053786	4.815637
259.729004	8000.355670	12.699264	-0.053768	4.815645
259.711176	8000.416262	12.704269	-0.053765	4.815663
259.723971	8000.335304	12.709274	-0.053767	4.815639
259.779502	8000.387483	12.714279	-0.053778	4.815654
259.834471	8000.383046	12.719283	-0.053788	4.815652
259.688076	8000.304825	12.724288	-0.053761	4.815630
259.935090	8000.356930	12.729293	-0.053807	4.815644
259.711662	8000.349009	12.734298	-0.053765	4.815643
259.677318	8000.345248	12.739303	-0.053759	4.815642
259.780497	8000.391798	12.744307	-0.053778	4.815655
259.682765	8000.332529	12.749312	-0.053760	4.815638
259.706253	8000.407682	12.754317	-0.053765	4.815660
259.581770	8000.386426	12.759322	-0.053741	4.815655
259.868221	8000.323826	12.764327	-0.053795	4.815635
259.730509	8000.347213	12.769331	-0.053769	4.815642
259.622721	8000.339047	12.774336	-0.053749	4.815641
259.949890	8000.379646	12.779341	-0.053810	4.815651
259.826110	8000.292182	12.784346	-0.053787	4.815626
259.644956	8000.331947	12.789351	-0.053753	4.815638
259.769302	8000.356414	12.794355	-0.053777	4.815645
259.796236	8000.322681	12.799360	-0.053782	4.815635
259.763019	8000.371273	12.804365	-0.053776	4.815649
259.699182	8000.358485	12.809370	-0.053764	4.815646
259.824632	8000.344519	12.814375	-0.053787	4.815641
259.886445	8000.353011	12.819379	-0.053799	4.815643
259.873823	8000.333584	12.824384	-0.053796	4.815638
259.827975	8000.375561	12.829389	-0.053788	4.815650
259.888337	8000.342375	12.834394	-0.053799	4.815640
259.964129	8000.346823	12.839399	-0.053813	4.815641
259.885501	8000.367971	12.844403	-0.053799	4.815648
259.764712	8000.369204	12.849408	-0.053776	4.815649
259.672833	8000.411497	12.854413	-0.053759	4.815661
259.686415	8000.330551	12.859418	-0.053762	4.815638
259.895548	8000.359608	12.864423	-0.053801	4.815645
259.805817	8000.372030	12.869427	-0.053784	4.815649
259.666061	8000.298190	12.874432	-0.053758	4.815628
259.893784	8000.383090	12.879437	-0.053801	4.815652
259.772156	8000.317022	12.884442	-0.053778	4.815633
259.848135	8000.297976	12.889447	-0.053792	4.815627
259.898306	8000.361816	12.894451	-0.053802	4.815646
260.045402	8000.323639	12.899456	-0.053829	4.815634
260.076030	8000.372208	12.904461	-0.053835	4.815648
260.002369	8000.284495	12.909466	-0.053821	4.815623
259.804774	8000.320787	12.914471	-0.053784	4.815634
259.823708	8000.320033	12.919475	-0.053788	4.815634
259.699093	8000.231488	12.924480	-0.053765	4.815609
259.858341	8000.359058	12.929485	-0.053795	4.815645
259.879673	8000.316689	12.934490	-0.053799	4.815633
259.920612	8000.308818	12.939495	-0.053806	4.815630
259.867695	8000.327182	12.944499	-0.053796	4.815636
259.945934	8000.291084	12.949504	-0.053811	4.815625
259.916033	8000.357887	12.954509	-0.053806	4.815645
259.957656	8000.296625	12.959514	-0.053813	4.815626
260.029893	8000.336261	12.964519	-0.053827	4.815638
259.970980	8000.286171	12.969523	-0.053816	4.815623
259.714364	8000.306545	12.974528	-0.053768	4.815631
259.810863	8000.412797	12.979533	-0.053786	4.815661
259.887920	8000.370271	12.984538	-0.053801	4.815648
259.876487	8000.385041	12.989543	-0.053799	4.815653
259.832968	8000.405696	12.994547	-0.053791	4.815659
259.941202	8000.399993	12.999552	-0.053811	4.815657
259.935818	8000.415931	13.004557	-0.053810	4.815661
259.851940	8000.395339	13.009562	-0.053794	4.815656
259.712300	8000.430442	13.014567	-0.053768	4.815667
259.821163	8000.409797	13.019571	-0.053789	4.815660
259.790842	8000.327065	13.024576	-0.053783	4.815636
259.972196	8000.366349	13.029581	-0.053817	4.815647
259.881825	8000.359535	13.034586	-0.053800	4.815645
259.955008	8000.315878	13.039591	-0.053814	4.815632
259.757777	8000.345767	13.044595	-0.053777	4.815642
259.784158	8000.320570	13.049600	-0.053782	4.815634
259.876820	8000.392581	13.054605	-0.053799	4.815655
259.572301	8000.379062	13.059610	-0.053743	4.815652
259.719640	8000.368659	13.064615	-0.053770	4.815649
259.820349	8000.372446	13.069619	-0.053789	4.815649
259.721004	8000.362282	13.074624	-0.053771	4.815647
259.925493	8000.363494	13.079629	-0.053809	4.815646
259.802960	8000.324113	13.084634	-0.053786	4.815635
259.853318	8000.319600	13.089639	-0.053795	4.815634
259.765208	8000.370499	13.094643	-0.053779	4.815649
259.806037	8000.303883	13.099648	-0.053787	4.815629
260.010175	8000.353152	13.104653	-0.053825	4.815643
259.790298	8000.303635	13.109658	-0.053784	4.815629
259.700488	8000.286150	13.114663	-0.053767	4.815625
259.830875	8000.396160	13.119667	-0.053791	4.815656
259.819996	8000.320155	13.124672	-0.053789	4.815634
259.738292	8000.359409	13.129677	-0.053774	4.815646
259.726025	8000.320763	13.134682	-0.053772	4.815635
259.875374	8000.334958	13.139687	-0.053800	4.815638
260.017855	8000.320203	13.144691	-0.053826	4.815633
259.855881	8000.291926	13.149696	-0.053796	4.815626
259.809139	8000.320004	13.154701	-0.053788	4.815634
259.763665	8000.322469	13.159706	-0.053779	4.815635
260.017266	8000.356526	13.164711	-0.053827	4.815644
260.071408	8000.371300	13.169715	-0.053837	4.815648
259.941907	8000.346758	13.174720	-0.053813	4.815641
259.909715	8000.371869	13.179725	-0.053807	4.815649
259.863081	8000.346546	13.184730	-0.053798	4.815641
259.876914	8000.366002	13.189735	-0.053801	4.815647
259.741960	8000.357391	13.194739	-0.053776	4.815645
259.664133	8000.299516	13.199744	-0.053761	4.815629
260.025123	8000.400480	13.204749	-0.053828	4.815656
259.901548	8000.299135	13.209754	-0.053805	4.815627
259.823120	8000.330967	13.214759	-0.053791	4.815637
260.061751	8000.367983	13.219763	-0.053835	4.815647
259.858891	8000.336901	13.224768	-0.053798	4.815639
259.807759	8000.361702	13.229773	-0.053788	4.815646
259.757300	8000.291458	13.234778	-0.053779	4.815626
260.038880	8000.348401	13.239783	-0.053831	4.815641
259.841764	8000.375088	13.244787	-0.053795	4.815650
259.789861	8000.335794	13.249792	-0.053785	4.815639
259.784663	8000.343190	13.254797	-0.053784	4.815641
259.651790	8000.316457	13.259802	-0.053759	4.815634
259.682695	8000.330851	13.264807	-0.053765	4.815638
259.765246	8000.365315	13.269811	-0.053781	4.815647
259.891294	8000.344951	13.274816	-0.053804	4.815641
259.923356	8000.410632	13.279821	-0.053810	4.815660
259.883586	8000.355515	13.284826	-0.053803	4.815644
259.892086	8000.326821	13.289831	-0.053805	4.815636
259.664294	8000.397865	13.294835	-0.053762	4.815657
259.506844	8000.334416	13.299840	-0.053733	4.815640
259.806199	8000.342519	13.304845	-0.053789	4.815641
259.819852	8000.383333	13.309850	-0.053791	4.815652
259.661627	8000.346572	13.314855	-0.053762	4.815642
259.846784	8000.384850	13.319859	-0.053796	4.815653
259.773934	8000.334533	13.324864	-0.053783	4.815638
259.774302	8000.368721	13.329869	-0.053783	4.815648
259.875938	8000.339413	13.334874	-0.053802	4.815639
259.953074	8000.326794	13.339879	-0.053816	4.815635
259.836734	8000.374027	13.344883	-0.053795	4.815650
259.627253	8000.310796	13.349888	-0.053756	4.815632
259.794476	8000.338099	13.354893	-0.053787	4.815639
259.804049	8000.294470	13.359898	-0.053789	4.815626
259.742342	8000.294534	13.364903	-0.053777	4.815627
259.944747	8000.367271	13.369907	-0.053815	4.815647
259.898693	8000.340889	13.374912	-0.053807	4.815640
259.986491	8000.373303	13.379917	-0.053823	4.815649
259.756745	8000.336441	13.384922	-0.053780	4.815639
259.923406	8000.314605	13.389927	-0.053811	4.815632
259.787437	8000.356177	13.394931	-0.053786	4.815645
259.724019	8000.335920	13.399936	-0.053774	4.815639
260.094641	8000.394319	13.404941	-0.053843	4.815654
259.991992	8000.377692	13.409946	-0.053824	4.815650
259.754009	8000.403711	13.414951	-0.053780	4.815659
259.931137	8000.400203	13.419955	-0.053813	4.815657
259.935355	8000.292403	13.424960	-0.053814	4.815625
260.086108	8000.384589	13.429965	-0.053842	4.815651
259.933283	8000.346849	13.434970	-0.053814	4.815641
260.035818	8000.315420	13.439975	-0.053833	4.815631
259.979219	8000.367902	13.444979	-0.053822	4.815647
259.838250	8000.311130	13.449984	-0.053796	4.815631
259.974460	8000.351812	13.454989	-0.053822	4.815642
259.793620	8000.316818	13.459994	-0.053788	4.815633
259.981601	8000.318828	13.464999	-0.053823	4.815633
260.027236	8000.271516	13.470003	-0.053831	4.815619
260.201895	8000.292533	13.475008	-0.053864	4.815624
260.043233	8000.358299	13.480013	-0.053835	4.815644
259.903989	8000.280195	13.485018	-0.053809	4.815622
259.858157	8000.287994	13.490023	-0.053800	4.815624
260.012113	8000.318285	13.495027	-0.053829	4.815632
259.770852	8000.337842	13.500032	-0.053784	4.815639
259.840292	8000.345391	13.505037	-0.053797	4.815641
259.874237	8000.337406	13.510042	-0.053803	4.815639
259.884046	8000.338638	13.515047	-0.053805	4.815639
259.851783	8000.354136	13.520051	-0.053799	4.815644
259.842140	8000.329418	13.525056	-0.053798	4.815636
259.927909	8000.409861	13.530061	-0.053814	4.815660
259.932801	8000.341590	13.535066	-0.053815	4.815640
260.036275	8000.303768	13.540071	-0.053834	4.815628
260.101199	8000.396687	13.545075	-0.053846	4.815655
259.961312	8000.330320	13.550080	-0.053820	4.815636
260.014519	8000.410232	13.555085	-0.053830	4.815659
260.038983	8000.393547	13.560090	-0.053835	4.815654
259.949779	8000.330145	13.565095	-0.053818	4.815636
259.882323	8000.355748	13.570099	-0.053806	4.815644
259.923108	8000.331854	13.575104	-0.053813	4.815637
259.868818	8000.368353	13.580109	-0.053803	4.815648
259.765337	8000.334624	13.585114	-0.053784	4.815638
260.043657	8000.290048	13.590119	-0.053836	4.815624
259.998876	8000.341655	13.595123	-0.053828	4.815639
259.867342	8000.283970	13.600128	-0.053803	4.815623
259.933160	8000.368359	13.605133	-0.053815	4.815647
259.806585	8000.346001	13.610138	-0.053792	4.815641
259.871898	8000.320372	13.615143	-0.053804	4.815634
259.852072	8000.353162	13.620147	-0.053800	4.815643
259.855657	8000.291278	13.625152	-0.053801	4.815625
259.987656	8000.374613	13.630157	-0.053826	4.815649
259.791686	8000.313738	13.635162	-0.053789	4.815632
259.778876	8000.362664	13.640167	-0.053787	4.815646
259.951158	8000.388983	13.645171	-0.053819	4.815653
259.694782	8000.326052	13.650176	-0.053771	4.815636
259.837941	8000.379664	13.655181	-0.053798	4.815651
259.814607	8000.381423	13.660186	-0.053794	4.815652
259.710139	8000.375447	13.665191	-0.053774	4.815651
259.886223	8000.400760	13.670195	-0.053807	4.815657
259.756568	8000.337765	13.675200	-0.053783	4.815639
259.979556	8000.383070	13.680205	-0.053825	4.815651
259.694082	8000.362386	13.685210	-0.053772	4.815647
259.876113	8000.350413	13.690215	-0.053806	4.815642
260.003225	8000.393083	13.695219	-0.053829	4.815654
259.883300	8000.349472	13.700224	-0.053807	4.815642
259.999292	8000.387687	13.705229	-0.053829	4.815653
260.038802	8000.369112	13.710234	-0.053836	4.815647
260.004694	8000.380308	13.715239	-0.053830	4.815651
259.772688	8000.375451	13.720243	-0.053787	4.815650
259.904136	8000.339154	13.725248	-0.053811	4.815639
260.077392	8000.364421	13.730253	-0.053844	4.815646
259.767027	8000.351874	13.735258	-0.053786	4.815643
259.755194	8000.353821	13.740263	-0.053784	4.815644
260.030205	8000.378616	13.745267	-0.053835	4.815650
259.951787	8000.332479	13.750272	-0.053820	4.815637
259.941141	8000.384645	13.755277	-0.053818	4.815652
259.967989	8000.330617	13.760282	-0.053823	4.815636
260.119595	8000.313875	13.765287	-0.053852	4.815631
260.099080	8000.386173	13.770291	-0.053848	4.815652
259.958527	8000.315523	13.775296	-0.053822	4.815632
260.041549	8000.372424	13.780301	-0.053837	4.815648
259.933622	8000.329009	13.785306	-0.053817	4.815636
259.922867	8000.277571	13.790311	-0.053815	4.815621
260.078795	8000.313235	13.795315	-0.053844	4.815631
260.026102	8000.274996	13.800320	-0.053835	4.815620
260.164302	8000.353092	13.805325	-0.053860	4.815642
260.136317	8000.366524	13.810330	-0.053855	4.815646
260.198760	8000.322691	13.815335	-0.053867	4.815633
260.213992	8000.324012	13.820339	-0.053870	4.815633
260.119268	8000.325672	13.825344	-0.053852	4.815634
260.307782	8000.370414	13.830349	-0.053887	4.815646
260.125950	8000.326858	13.835354	-0.053854	4.815634
259.959320	8000.348704	13.840359	-0.053823	4.815641
260.227805	8000.404366	13.845363	-0.053873	4.815656
259.965211	8000.313563	13.850368	-0.053824	4.815631
259.793092	8000.376973	13.855373	-0.053792	4.815651
259.956774	8000.390334	13.860378	-0.053822	4.815654
260.027236	8000.345564	13.865383	-0.053836	4.815640
260.191442	8000.411270	13.870387	-0.053866	4.815659
259.949178	8000.335752	13.875392	-0.053821	4.815638
260.130352	8000.403871	13.880397	-0.053855	4.815657
259.959127	8000.376510	13.885402	-0.053823	4.815650
259.989534	8000.338562	13.890407	-0.053829	4.815638
260.098974	8000.415120	13.895411	-0.053849	4.815660
260.048254	8000.382253	13.900416	-0.053840	4.815651
259.846973	8000.356537	13.905421	-0.053802	4.815644
259.896119	8000.361617	13.910426	-0.053812	4.815646
260.048349	8000.323525	13.915431	-0.053840	4.815634
260.152755	8000.333781	13.920435	-0.053859	4.815636
260.049140	8000.323546	13.925440	-0.053840	4.815634
260.247379	8000.373788	13.930445	-0.053877	4.815647
260.061049	8000.350452	13.935450	-0.053843	4.815641
259.918303	8000.397253	13.940455	-0.053816	4.815656
260.291414	8000.425789	13.945459	-0.053886	4.815662
260.176096	8000.375844	13.950464	-0.053864	4.815648
260.155869	8000.410764	13.955469	-0.053860	4.815659
259.941864	8000.427562	13.960474	-0.053821	4.815665
260.004729	8000.390144	13.965479	-0.053832	4.815653
259.964488	8000.417260	13.970483	-0.053825	4.815661
259.712744	8000.325567	13.975488	-0.053778	4.815636
260.102760	8000.397101	13.980493	-0.053851	4.815655
260.088112	8000.379777	13.985498	-0.053848	4.815650
259.742476	8000.347428	13.990503	-0.053784	4.815642
259.760747	8000.393658	13.995507	-0.053787	4.815656
259.903108	8000.323362	14.000512	-0.053814	4.815634
259.988559	8000.345056	14.005517	-0.053830	4.815640
259.958198	8000.371266	14.010522	-0.053824	4.815648
259.955676	8000.362685	14.015527	-0.053824	4.815646
260.200160	8000.359211	14.020531	-0.053869	4.815643
259.853580	8000.356752	14.025536	-0.053805	4.815644
259.970179	8000.371480	14.030541	-0.053827	4.815648
259.963728	8000.370311	14.035546	-0.053825	4.815648
259.797464	8000.302445	14.040551	-0.053794	4.815629
260.057674	8000.312044	14.045555	-0.053843	4.815630
260.053457	8000.286346	14.050560	-0.053842	4.815623
260.156756	8000.321150	14.055565	-0.053862	4.815632
259.996102	8000.334548	14.060570	-0.053832	4.815637
260.105138	8000.361969	14.065575	-0.053852	4.815645
260.027233	8000.386333	14.070579	-0.053838	4.815652
259.819942	8000.378676	14.075584	-0.053799	4.815651
260.052843	8000.353651	14.080589	-0.053842	4.815642
259.945811	8000.346565	14.085594	-0.053823	4.815641
259.945127	8000.329469	14.090599	-0.053823	4.815636
260.216276	8000.297593	14.095603	-0.053873	4.815625
259.839839	8000.292511	14.100608	-0.053803	4.815626
259.890310	8000.353152	14.105613	-0.053812	4.815643
259.865521	8000.374112	14.110618	-0.053808	4.815649
260.034906	8000.322415	14.115623	-0.053839	4.815633
259.971825	8000.392948	14.120627	-0.053828	4.815654
259.742532	8000.309099	14.125632	-0.053785	4.815631
260.055207	8000.351598	14.130637	-0.053843	4.815642
260.036465	8000.366249	14.135642	-0.053840	4.815646
259.876792	8000.301695	14.140647	-0.053810	4.815628
260.122987	8000.370877	14.145651	-0.053856	4.815647
260.001801	8000.373172	14.150656	-0.053834	4.815648
260.089572	8000.353250	14.155661	-0.053850	4.815642
260.121155	8000.353771	14.160666	-0.053856	4.815642
260.106556	8000.337516	14.165671	-0.053853	4.815637
260.252571	8000.406129	14.170675	-0.053881	4.815657
260.117534	8000.346249	14.175680	-0.053855	4.815640
260.140992	8000.347705	14.180685	-0.053860	4.815640
260.089366	8000.341525	14.185690	-0.053850	4.815639
260.037508	8000.274462	14.190695	-0.053841	4.815619
259.929608	8000.335717	14.195699	-0.053821	4.815638
260.015526	8000.261294	14.200704	-0.053837	4.815616
260.049796	8000.309922	14.205709	-0.053843	4.815630
260.152739	8000.304133	14.210714	-0.053862	4.815627
260.411639	8000.291282	14.215719	-0.053911	4.815622
260.267583	8000.345539	14.220723	-0.053884	4.815639
260.121488	8000.316452	14.225728	-0.053857	4.815631
260.183189	8000.312125	14.230733	-0.053868	4.815630
260.123596	8000.366695	14.235738	-0.053857	4.815646
259.951577	8000.386316	14.240743	-0.053825	4.815652
259.816978	8000.418297	14.245747	-0.053800	4.815662
259.962420	8000.336303	14.250752	-0.053827	4.815638
260.093917	8000.316028	14.255757	-0.053852	4.815631
260.041262	8000.326920	14.260762	-0.053842	4.815635
259.914369	8000.335531	14.265767	-0.053819	4.815638
260.058018	8000.428670	14.270771	-0.053845	4.815664
259.945847	8000.317897	14.275776	-0.053825	4.815632
260.002875	8000.361557	14.280781	-0.053835	4.815645
260.072323	8000.314634	14.285786	-0.053848	4.815631
260.004151	7999.317053	14.290791	-0.053835	4.815340

259.948484	7996.124221	14.295795	-0.053822	4.814406
260.089610	7990.628314	14.300800	-0.053845	4.812799
260.182264	7983.958626	14.305805	-0.053858	4.810847
259.857990	7976.639779	14.310810	-0.053793	4.808707
260.019526	7968.972637	14.315815	-0.053818	4.806461
260.111081	7961.247214	14.320819	-0.053830	4.804197
259.748629	7953.391762	14.325824	-0.053758	4.801897
259.765829	7945.427764	14.330829	-0.053756	4.799562
260.065184	7937.471829	14.335834	-0.053806	4.797226
259.998540	7929.390947	14.340839	-0.053789	4.794855
259.913232	7921.432873	14.345843	-0.053768	4.792518
259.712307	7913.348525	14.350848	-0.053725	4.790144
259.686173	7905.400274	14.355853	-0.053715	4.787808
259.607700	7897.360736	14.360858	-0.053695	4.785444
259.526749	7889.430195	14.365863	-0.053675	4.783111
259.701220	7881.450810	14.370867	-0.053702	4.780761
259.594935	7873.407974	14.375872	-0.053677	4.778393
259.554787	7865.451602	14.380877	-0.053665	4.776049
259.574621	7857.386651	14.385882	-0.053663	4.773671
259.503929	7849.339384	14.390887	-0.053645	4.771297
259.428779	7841.338408	14.395891	-0.053626	4.768937
259.512438	7833.361357	14.400896	-0.053636	4.766581
259.762428	7825.384959	14.405901	-0.053678	4.764224
259.380121	7817.453462	14.410906	-0.053601	4.761881
259.287362	7809.363696	14.415911	-0.053579	4.759489
259.473610	7801.380431	14.420915	-0.053608	4.757127
259.285382	7793.366242	14.425920	-0.053568	4.754756
259.227561	7785.361801	14.430925	-0.053552	4.752385
259.206188	7777.340714	14.435930	-0.053543	4.750009
259.233696	7769.328396	14.440935	-0.053543	4.747634
259.108945	7761.299534	14.445939	-0.053515	4.745253
259.073623	7753.356678	14.450944	-0.053503	4.742896
259.188690	7745.365705	14.455949	-0.053519	4.740523
259.098347	7737.349326	14.460954	-0.053497	4.738142
259.004860	7729.332786	14.465959	-0.053475	4.735760
259.064237	7721.346986	14.470963	-0.053481	4.733386
259.290490	7713.303796	14.475968	-0.053517	4.730992
259.230973	7705.304961	14.480973	-0.053501	4.728612
258.947978	7697.322844	14.485978	-0.053443	4.726236
258.732824	7689.306696	14.490983	-0.053398	4.723848
258.817712	7681.345446	14.495987	-0.053409	4.721475
258.720923	7673.276754	14.500992	-0.053386	4.719069
258.886377	7665.418361	14.505997	-0.053411	4.716723
258.721245	7657.324874	14.511002	-0.053375	4.714307
258.755385	7649.251804	14.516007	-0.053377	4.711896
258.815882	7641.290640	14.521011	-0.053383	4.709517
258.575671	7633.285307	14.526016	-0.053333	4.707124
258.588114	7625.280767	14.531021	-0.053330	4.704729
258.319746	7617.326288	14.536026	-0.053275	4.702349
258.462823	7609.281847	14.541031	-0.053296	4.699940
258.558596	7601.369306	14.546035	-0.053309	4.697569
258.206663	7593.270398	14.551040	-0.053238	4.695142
258.412122	7585.277161	14.556045	-0.053271	4.692744
258.418203	7577.256557	14.561050	-0.053267	4.690337
258.169024	7569.268713	14.566055	-0.053216	4.687940
258.358645	7561.302120	14.571059	-0.053246	4.685546
258.293353	7553.291388	14.576064	-0.053229	4.683139
258.352105	7545.349827	14.581069	-0.053234	4.680751
258.164437	7537.287577	14.586074	-0.053194	4.678326
258.231929	7529.288920	14.591079	-0.053202	4.675918
258.159850	7521.219080	14.596083	-0.053183	4.673488
258.037804	7513.091095	14.601088	-0.053155	4.671039
258.473902	7505.205919	14.606093	-0.053231	4.668661
258.358521	7497.209505	14.611098	-0.053204	4.666250
258.322981	7489.246556	14.616103	-0.053193	4.663847
258.422471	7481.267570	14.621107	-0.053206	4.661437
258.326610	7473.203121	14.626112	-0.053183	4.659001
258.407698	7465.257131	14.631117	-0.053193	4.656599
258.147694	7457.240841	14.636122	-0.053139	4.654176
258.168293	7449.233809	14.641127	-0.053138	4.651753
258.077057	7441.225479	14.646131	-0.053116	4.649329
257.662084	7433.225671	14.651136	-0.053034	4.646906
257.694845	7425.202454	14.656141	-0.053034	4.644475
257.933942	7417.246690	14.661146	-0.053074	4.642062
257.940785	7409.173096	14.666151	-0.053070	4.639613
257.829934	7401.259859	14.671155	-0.053044	4.637211
257.679569	7393.214011	14.676160	-0.053011	4.634768
257.807262	7385.193424	14.681165	-0.053030	4.632331
257.871230	7377.168722	14.686170	-0.053036	4.629891
257.672030	7369.182840	14.691175	-0.052994	4.627462
257.701905	7361.182977	14.696179	-0.052994	4.625028
257.505345	7353.206644	14.701184	-0.052953	4.622599
257.580780	7345.176323	14.706189	-0.052962	4.620153
257.677826	7337.199392	14.711194	-0.052974	4.617721
257.621761	7329.149859	14.716199	-0.052959	4.615267
257.600809	7321.195674	14.721203	-0.052950	4.612840
257.552107	7313.138351	14.726208	-0.052936	4.610380
257.500930	7305.151775	14.731213	-0.052921	4.607940
257.469094	7297.178635	14.736218	-0.052910	4.605503
257.539093	7289.204544	14.741223	-0.052918	4.603065
257.649945	7281.197890	14.746227	-0.052933	4.600616
257.314310	7273.210296	14.751232	-0.052865	4.598171
257.302223	7265.208280	14.756237	-0.052858	4.595720
257.395341	7257.163521	14.761242	-0.052870	4.593255
257.105772	7249.113573	14.766247	-0.052811	4.590786
257.010001	7241.135852	14.771251	-0.052788	4.588339
257.101794	7233.087783	14.776256	-0.052800	4.585869
257.352240	7225.115802	14.781261	-0.052842	4.583421
257.134518	7217.145146	14.786266	-0.052796	4.580972
257.085172	7209.151979	14.791271	-0.052781	4.578514
257.077904	7201.180254	14.796275	-0.052775	4.576062
256.904339	7193.138294	14.801280	-0.052737	4.573587
256.971925	7185.097922	14.806285	-0.052745	4.571112
257.162311	7177.122233	14.811290	-0.052775	4.568654
256.922898	7169.098723	14.816295	-0.052725	4.566181
257.038966	7161.151118	14.821299	-0.052742	4.563730
257.035368	7153.126316	14.826304	-0.052736	4.561253
256.721838	7145.155751	14.831309	-0.052673	4.558792
256.765707	7137.192040	14.836314	-0.052676	4.556332
256.808027	7129.139729	14.841319	-0.052678	4.553843
256.871430	7121.096755	14.846323	-0.052685	4.551356
256.622137	7113.073883	14.851328	-0.052633	4.548873
256.521406	7105.106122	14.856333	-0.052609	4.546406
256.688481	7097.098940	14.861338	-0.052635	4.543926
256.525566	7089.113060	14.866343	-0.052600	4.541450
256.517369	7081.107545	14.871347	-0.052593	4.538968
256.412653	7073.133162	14.876352	-0.052568	4.536493
256.604894	7065.114062	14.881357	-0.052599	4.534004
256.518716	7057.120194	14.886362	-0.052578	4.531521
256.594842	7049.057360	14.891367	-0.052587	4.529015
256.451401	7041.083781	14.896371	-0.052555	4.526535
256.316762	7033.058398	14.901376	-0.052525	4.524038
256.311669	7025.153870	14.906381	-0.052519	4.521577
256.445856	7017.134378	14.911386	-0.052539	4.519080
256.450440	7009.167335	14.916391	-0.052534	4.516597
256.364688	7001.126313	14.921395	-0.052513	4.514089
256.306187	6993.009553	14.926400	-0.052497	4.511557
256.357007	6984.998464	14.931405	-0.052501	4.509056
256.093238	6977.062402	14.936410	-0.052447	4.506576
255.931996	6969.025075	14.941415	-0.052412	4.504064
256.257790	6961.082840	14.946419	-0.052467	4.501581
256.087195	6953.045582	14.951424	-0.052430	4.499066
255.966134	6945.115132	14.956429	-0.052403	4.496583
256.115444	6937.064016	14.961434	-0.052425	4.494062
256.127012	6929.032630	14.966439	-0.052422	4.491545
255.946734	6921.037483	14.971443	-0.052384	4.489037
256.144212	6913.064010	14.976448	-0.052415	4.486536
256.148524	6905.047164	14.981453	-0.052411	4.484020
255.951865	6897.091557	14.986458	-0.052369	4.481520
255.902966	6889.060459	14.991463	-0.052355	4.478996
255.989931	6881.096974	14.996467	-0.052366	4.476492
255.760352	6873.018370	15.001472	-0.052318	4.473950
255.730570	6865.034438	15.006477	-0.052307	4.471436
255.760135	6856.995882	15.011482	-0.052308	4.468904
255.584158	6849.006828	15.016487	-0.052270	4.466386
255.516420	6841.043854	15.021491	-0.052252	4.463874
255.644904	6833.044483	15.026496	-0.052271	4.461351
255.847024	6825.024979	15.031501	-0.052303	4.458820
255.545187	6817.051717	15.036506	-0.052242	4.456300
255.422708	6809.017655	15.041511	-0.052214	4.453760
255.697921	6800.997995	15.046515	-0.052260	4.451225
255.516629	6793.000514	15.051520	-0.052221	4.448694
255.428984	6784.991655	15.056525	-0.052199	4.446158
255.312206	6777.035085	15.061530	-0.052172	4.443637
255.367352	6769.015784	15.066535	-0.052178	4.441095
255.395702	6761.025044	15.071539	-0.052178	4.438561
255.193444	6752.999762	15.076544	-0.052135	4.436014
255.281393	6744.994767	15.081549	-0.052146	4.433472
255.154936	6736.944334	15.086554	-0.052117	4.430914
255.110987	6728.951421	15.091559	-0.052104	4.428373
255.399841	6720.964146	15.096563	-0.052153	4.425834
255.114623	6712.958464	15.101568	-0.052094	4.423285
255.108707	6704.967051	15.106573	-0.052088	4.420740
255.119607	6696.977056	15.111578	-0.052085	4.418195
255.013213	6688.950397	15.116583	-0.052060	4.415635
254.976600	6681.009545	15.121587	-0.052048	4.413102
254.993662	6672.958016	15.126592	-0.052046	4.410532
254.874479	6664.947562	15.131597	-0.052019	4.407973
254.882694	6656.908500	15.136602	-0.052015	4.405405
254.841751	6648.977434	15.141607	-0.052002	4.402869
254.961008	6641.009286	15.146611	-0.052019	4.400320
254.953265	6633.008840	15.151616	-0.052013	4.397759
254.891192	6624.969159	15.156621	-0.051996	4.395184
254.850388	6616.998136	15.161626	-0.051983	4.392629
254.733032	6608.929928	15.166631	-0.051956	4.390041
254.885622	6600.989235	15.171635	-0.051979	4.387494
254.728499	6592.942893	15.176640	-0.051945	4.384910
254.796599	6585.010041	15.181645	-0.051953	4.382362
254.865348	6577.004088	15.186650	-0.051960	4.379790
254.745916	6568.997526	15.191655	-0.051933	4.377214
254.751396	6560.991485	15.196659	-0.051929	4.374638
254.611338	6552.987067	15.201664	-0.051897	4.372059
254.550858	6544.949121	15.206669	-0.051881	4.369469
254.553529	6536.997064	15.211674	-0.051876	4.366906
254.506963	6528.973222	15.216679	-0.051862	4.364318
254.718135	6521.046825	15.221683	-0.051897	4.361761
254.271375	6512.974591	15.226688	-0.051808	4.359151
254.335262	6505.047925	15.231693	-0.051815	4.356590
254.322175	6496.979752	15.236698	-0.051807	4.353981
254.186081	6488.823410	15.241703	-0.051777	4.351342
254.399005	6480.890560	15.246707	-0.051811	4.348775
254.412865	6472.923059	15.251712	-0.051809	4.346194
254.182049	6464.943233	15.256717	-0.051761	4.343606
254.183544	6456.952798	15.261722	-0.051756	4.341015
253.914827	6448.933433	15.266727	-0.051701	4.338411
254.161017	6440.972391	15.271731	-0.051741	4.335828
254.057807	6432.896733	15.276736	-0.051717	4.333204
253.989873	6424.900135	15.281741	-0.051699	4.330604
254.004898	6416.973719	15.286746	-0.051697	4.328026
253.882444	6408.902603	15.291751	-0.051669	4.325398
253.947428	6400.969303	15.296755	-0.051676	4.322815
253.963037	6392.958513	15.301760	-0.051673	4.320204
254.040606	6384.947329	15.306765	-0.051683	4.317593
253.912481	6376.961948	15.311770	-0.051654	4.314986
253.734819	6368.900377	15.316775	-0.051615	4.312353
253.866458	6360.905389	15.321779	-0.051635	4.309743
253.681731	6352.931233	15.326784	-0.051595	4.307135
253.693580	6344.901980	15.331789	-0.051592	4.304509
253.704842	6336.928189	15.336794	-0.051589	4.301900
253.516279	6328.889711	15.341799	-0.051549	4.299266
253.662958	6320.953831	15.346803	-0.051571	4.296667
253.620858	6312.926416	15.351808	-0.051558	4.294035
253.598305	6304.875875	15.356813	-0.051549	4.291393
253.680699	6296.900909	15.361818	-0.051559	4.288776
253.568738	6288.900498	15.366823	-0.051533	4.286148
253.760121	6280.894538	15.371827	-0.051563	4.283518
253.587264	6272.919778	15.376832	-0.051526	4.280894
253.411575	6264.923501	15.381837	-0.051488	4.278261
253.556690	6256.962798	15.386842	-0.051510	4.275641
253.426605	6248.886204	15.391847	-0.051481	4.272979
253.396390	6240.876461	15.396851	-0.051470	4.270338
253.331413	6232.902885	15.401856	-0.051453	4.267707
253.397867	6224.819192	15.406861	-0.051460	4.265039
253.312822	6216.950592	15.411866	-0.051439	4.262440
253.189198	6208.816850	15.416871	-0.051410	4.259750
253.338882	6200.928131	15.421875	-0.051433	4.257143
253.089869	6192.877796	15.426880	-0.051382	4.254477
253.034304	6184.902686	15.431885	-0.051366	4.251836
253.054226	6176.872062	15.436890	-0.051365	4.249175
252.983881	6168.890413	15.441895	-0.051346	4.246528
253.143089	6160.893201	15.446899	-0.051371	4.243877
252.928977	6152.946302	15.451904	-0.051326	4.241237
252.967086	6144.861940	15.456909	-0.051328	4.238552
252.750007	6136.954357	15.461914	-0.051282	4.235921
252.751916	6128.890602	15.466919	-0.051277	4.233240
253.109043	6120.895707	15.471923	-0.051339	4.230582
252.991843	6112.880240	15.476928	-0.051312	4.227912
252.945624	6104.869671	15.481933	-0.051298	4.225243
252.919793	6096.909453	15.486938	-0.051288	4.222588
252.890425	6088.919751	15.491943	-0.051277	4.219922
252.825732	6080.947399	15.496947	-0.051260	4.217260
252.857531	6072.937018	15.501952	-0.051261	4.214585
252.621322	6064.896004	15.506957	-0.051212	4.211894
252.572474	6056.895540	15.511962	-0.051198	4.209218
252.590473	6048.920508	15.516967	-0.051196	4.206549
252.568415	6040.930349	15.521971	-0.051187	4.203873
252.574732	6032.962103	15.526976	-0.051183	4.201203
252.383282	6024.925105	15.531981	-0.051142	4.198505
252.561663	6016.958855	15.536986	-0.051170	4.195834
252.461140	6008.849403	15.541991	-0.051146	4.193110
252.406423	6000.826476	15.546995	-0.051131	4.190414
252.416659	5992.883699	15.552000	-0.051127	4.187744
252.379571	5984.846404	15.557005	-0.051115	4.185040
252.423665	5976.885849	15.562010	-0.051118	4.182360
252.119829	5968.892693	15.567015	-0.051057	4.179664
252.377382	5960.926115	15.572019	-0.051099	4.176982
252.225855	5952.882826	15.577024	-0.051066	4.174267
251.941619	5944.865915	15.582029	-0.051008	4.171559
252.044152	5936.885705	15.587034	-0.051022	4.168865
251.955460	5928.876443	15.592039	-0.051000	4.166157
251.940686	5920.908683	15.597043	-0.050992	4.163462
251.934599	5912.876625	15.602048	-0.050986	4.160744
252.025219	5904.909179	15.607053	-0.050998	4.158047
252.071115	5896.883019	15.612058	-0.051001	4.155328
252.059404	5888.848453	15.617063	-0.050994	4.152604
252.323840	5880.846322	15.622067	-0.051038	4.149892
251.890342	5872.877513	15.627072	-0.050952	4.147182
251.873087	5864.877349	15.632077	-0.050943	4.144464
252.051452	5856.930586	15.637082	-0.050972	4.141765
251.821989	5848.886061	15.642087	-0.050924	4.139025
251.990900	5840.893176	15.647091	-0.050950	4.136307
251.660629	5832.870357	15.652096	-0.050883	4.133570
251.845984	5824.835200	15.657101	-0.050913	4.130834
251.883130	5816.853713	15.662106	-0.050914	4.128112
251.500024	5808.836199	15.667111	-0.050838	4.125371
251.682275	5800.902029	15.672115	-0.050867	4.122663
251.625317	5792.853103	15.677120	-0.050851	4.119912
251.640381	5784.908203	15.682125	-0.050849	4.117195
251.819605	5776.873022	15.687130	-0.050877	4.114448
251.765127	5768.811837	15.692135	-0.050861	4.111687
251.627533	5760.859429	15.697139	-0.050831	4.108960
251.404094	5752.845544	15.702144	-0.050784	4.106209
251.278656	5744.840659	15.707149	-0.050755	4.103461
251.371029	5736.889185	15.712154	-0.050767	4.100732
251.138901	5728.887375	15.717159	-0.050719	4.097979
251.322931	5720.893958	15.722163	-0.050748	4.095234
251.395211	5712.859392	15.727168	-0.050756	4.092470
251.246676	5704.837071	15.732173	-0.050724	4.089706
251.064941	5696.921198	15.737178	-0.050685	4.086977
250.916218	5688.892607	15.742183	-0.050652	4.084207
251.083670	5680.957376	15.747187	-0.050678	4.081472
250.873344	5672.916834	15.752192	-0.050633	4.078693
250.907092	5664.933499	15.757197	-0.050635	4.075936
251.044524	5656.899914	15.762202	-0.050655	4.073161
250.767861	5648.845237	15.767207	-0.050598	4.070371
250.852927	5640.907693	15.772211	-0.050609	4.067624
250.972203	5632.934438	15.777216	-0.050626	4.064864
251.011152	5624.932044	15.782221	-0.050628	4.062091
250.829861	5616.934308	15.787226	-0.050589	4.059314
250.898674	5608.939838	15.792231	-0.050597	4.056540
250.824455	5600.919940	15.797235	-0.050578	4.053753
250.702289	5592.886054	15.802240	-0.050550	4.050959
250.670075	5584.893464	15.807245	-0.050539	4.048179
250.725303	5576.917931	15.812250	-0.050544	4.045404
250.551557	5568.912779	15.817255	-0.050506	4.042613
250.536222	5560.918115	15.822259	-0.050498	4.039826
250.622341	5552.956846	15.827264	-0.050509	4.037051
250.545526	5544.892688	15.832269	-0.050490	4.034235
250.436705	5536.818607	15.837274	-0.050464	4.031413
250.475851	5528.842025	15.842279	-0.050466	4.028626
250.432696	5520.869192	15.847283	-0.050453	4.025837
250.262067	5512.894122	15.852288	-0.050416	4.023043
250.257603	5504.892404	15.857293	-0.050410	4.020240
250.504902	5496.891375	15.862298	-0.050451	4.017440
250.347893	5488.849719	15.867303	-0.050417	4.014617
250.563054	5480.869215	15.872307	-0.050452	4.011819
250.398458	5472.869445	15.877312	-0.050416	4.009007
250.403484	5464.881052	15.882317	-0.050412	4.006199
250.457145	5456.919137	15.887322	-0.050417	4.003400
250.329238	5448.893872	15.892327	-0.050388	4.000573
250.363085	5440.949373	15.897331	-0.050389	3.997776
249.984340	5432.913317	15.902336	-0.050313	3.994937
249.873072	5424.864652	15.907341	-0.050287	3.992096
250.021693	5416.838067	15.912346	-0.050310	3.989266
249.965162	5408.876996	15.917351	-0.050294	3.986453
250.067694	5400.889450	15.922355	-0.050308	3.983631
249.971107	5392.890363	15.927360	-0.050285	3.980800
249.745333	5384.914540	15.932365	-0.050238	3.977973
249.831319	5376.946536	15.937370	-0.050248	3.975152
249.841364	5368.923483	15.942375	-0.050245	3.972308
249.777436	5360.882419	15.947379	-0.050228	3.969455
249.980188	5352.929398	15.952384	-0.050261	3.966635
249.785721	5344.908734	15.957389	-0.050219	3.963782
249.906357	5336.950766	15.962394	-0.050237	3.960955
249.530074	5328.975057	15.967399	-0.050161	3.958112
249.612360	5320.963729	15.972403	-0.050171	3.955261
249.728801	5312.879400	15.977408	-0.050188	3.952383
249.714981	5304.856303	15.982413	-0.050180	3.949522
249.525120	5296.934264	15.987418	-0.050140	3.946692
249.478608	5288.932266	15.992423	-0.050126	3.943834
249.459676	5280.969669	15.997427	-0.050117	3.940989
249.457202	5272.968380	16.002432	-0.050112	3.938128
249.402890	5264.949331	16.007437	-0.050096	3.935258
249.557708	5256.933545	16.012442	-0.050120	3.932390
249.371409	5248.899745	16.017447	-0.050080	3.929508
249.260175	5240.976054	16.022451	-0.050054	3.926664
249.321719	5232.947666	16.027456	-0.050061	3.923784
249.271712	5225.001208	16.032461	-0.050046	3.920929
249.336796	5216.986965	16.037466	-0.050053	3.918050
249.431039	5208.964951	16.042471	-0.050065	3.915167
249.506309	5200.944587	16.047475	-0.050074	3.912281
249.292035	5192.946779	16.052480	-0.050029	3.909397
249.104871	5184.995127	16.057485	-0.049989	3.906527
249.234720	5176.980159	16.062490	-0.050008	3.903638
249.098476	5168.956423	16.067495	-0.049978	3.900739
249.107409	5160.996772	16.072499	-0.049974	3.897864
249.139341	5152.963235	16.077504	-0.049975	3.894960
249.035464	5144.943706	16.082509	-0.049950	3.892057
248.991539	5136.951174	16.087514	-0.049937	3.889162
248.837119	5128.955846	16.092519	-0.049903	3.886262
248.882475	5120.979145	16.097523	-0.049907	3.883370
248.839291	5112.976989	16.102528	-0.049893	3.880465
248.655048	5105.021941	16.107533	-0.049854	3.877573
248.849822	5096.975203	16.112538	-0.049885	3.874652
248.714829	5088.713754	16.117543	-0.049854	3.871645
248.895019	5080.806927	16.122547	-0.049883	3.868770
248.688722	5072.872985	16.127552	-0.049839	3.865876
248.720564	5064.879837	16.132557	-0.049840	3.862963
248.707148	5056.920858	16.137562	-0.049833	3.860059
248.335812	5048.998698	16.142567	-0.049758	3.857160
248.464145	5040.952555	16.147571	-0.049777	3.854223
248.616597	5032.961518	16.152576	-0.049800	3.851304
248.620462	5024.937838	16.157581	-0.049796	3.848368
248.550378	5016.986627	16.162586	-0.049778	3.845455
248.532863	5009.001063	16.167591	-0.049769	3.842528
248.331701	5001.021710	16.172595	-0.049727	3.839597
248.233735	4993.064828	16.177600	-0.049703	3.836675
248.500276	4984.993172	16.182605	-0.049748	3.833715
248.352891	4977.001237	16.187610	-0.049715	3.830774
248.216482	4969.009794	16.192615	-0.049684	3.827832
248.215327	4961.005808	16.197619	-0.049679	3.824885
248.215700	4953.029085	16.202624	-0.049674	3.821946
248.054222	4945.006885	16.207629	-0.049639	3.818984
248.021372	4937.068969	16.212634	-0.049628	3.816054
248.178045	4929.017177	16.217639	-0.049651	3.813084
248.306456	4921.016304	16.222643	-0.049670	3.810130
247.924982	4913.056397	16.227648	-0.049594	3.807177
247.877026	4905.040317	16.232653	-0.049580	3.804209
248.054071	4897.096494	16.237658	-0.049608	3.801270
247.907253	4889.070083	16.242663	-0.049575	3.798291
247.901374	4881.105629	16.247667	-0.049569	3.795335
247.877190	4873.041740	16.252672	-0.049559	3.792340
247.743985	4864.995764	16.257677	-0.049529	3.789347
247.606442	4857.073941	16.262682	-0.049499	3.786398
247.741385	4849.033041	16.267687	-0.049519	3.783408
247.633176	4841.083426	16.272691	-0.049493	3.780444
247.503483	4833.089493	16.277696	-0.049464	3.777461
247.390055	4825.036548	16.282701	-0.049438	3.774454
247.562657	4817.059645	16.287706	-0.049465	3.771479
247.349260	4809.043143	16.292711	-0.049420	3.768479
247.395338	4801.062344	16.297715	-0.049423	3.765495
247.446346	4793.087555	16.302720	-0.049428	3.762512
247.322741	4785.053157	16.307725	-0.049399	3.759499
247.296269	4777.134151	16.312730	-0.049389	3.756530
247.251135	4769.075350	16.317735	-0.049376	3.753505
247.341980	4761.058688	16.322739	-0.049387	3.750497
247.355809	4753.047401	16.327744	-0.049385	3.747487
247.494173	4745.017356	16.332749	-0.049405	3.744470
247.505306	4737.132692	16.337754	-0.049402	3.741503
247.271310	4729.073332	16.342759	-0.049354	3.738461
247.319921	4721.102173	16.347763	-0.049358	3.735457
247.343939	4713.129040	16.352768	-0.049357	3.732449
247.155295	4705.069195	16.357773	-0.049317	3.729401
247.420172	4697.158134	16.362778	-0.049361	3.726418
247.242001	4689.114875	16.367783	-0.049322	3.723372
247.098404	4681.126362	16.372787	-0.049290	3.720344
247.016859	4673.178333	16.377792	-0.049270	3.717331
246.911416	4665.134620	16.382797	-0.049245	3.714279
247.067575	4657.050262	16.387802	-0.049269	3.711215
246.874454	4649.064149	16.392807	-0.049228	3.708177
247.009258	4641.078161	16.397811	-0.049248	3.705145
246.935430	4633.133571	16.402816	-0.049229	3.702121
246.723860	4625.134011	16.407821	-0.049185	3.699070
246.759802	4617.189642	16.412826	-0.049186	3.696044
246.709198	4609.151888	16.417831	-0.049172	3.692978
246.692072	4601.144798	16.422835	-0.049163	3.689921
246.738472	4593.191629	16.427840	-0.049167	3.686884
246.517451	4585.182721	16.432845	-0.049120	3.683817
246.687873	4577.214927	16.437850	-0.049147	3.680773
246.726883	4569.217594	16.442855	-0.049149	3.677711
246.679659	4561.194402	16.447859	-0.049135	3.674635
246.622094	4553.184343	16.452864	-0.049119	3.671561
246.473720	4545.175750	16.457869	-0.049086	3.668483
246.700083	4537.168175	16.462874	-0.049123	3.665412
246.486099	4529.214847	16.467879	-0.049078	3.662348
246.630825	4521.185569	16.472883	-0.049100	3.659262
246.470433	4513.257482	16.477888	-0.049065	3.656204
246.260267	4505.201078	16.482893	-0.049021	3.653093
246.331379	4497.208425	16.487898	-0.049029	3.650010
246.017987	4489.235940	16.492903	-0.048965	3.646923
246.067654	4481.225193	16.497907	-0.048970	3.643829
246.288833	4473.239255	16.502912	-0.049006	3.640745
246.184970	4465.238140	16.507917	-0.048981	3.637645
246.087559	4457.272443	16.512922	-0.048958	3.634556
245.973911	4449.214919	16.517927	-0.048931	3.631428
246.200934	4441.213794	16.522931	-0.048969	3.628328
246.106147	4433.224246	16.527936	-0.048946	3.625222
246.018140	4425.258776	16.532941	-0.048924	3.622122
246.225173	4417.235314	16.537946	-0.048958	3.619006
245.996285	4409.273456	16.542951	-0.048910	3.615898
245.928519	4401.273533	16.547955	-0.048892	3.612778
245.949524	4393.240672	16.552960	-0.048891	3.609644
245.910833	4385.286952	16.557965	-0.048878	3.606537
245.859965	4377.317025	16.562970	-0.048864	3.603421
245.661531	4369.329469	16.567975	-0.048822	3.600291
245.646970	4361.353309	16.572979	-0.048814	3.597167
245.621437	4353.315594	16.577984	-0.048804	3.594017
245.488958	4345.279125	16.582989	-0.048774	3.590861
245.708114	4337.317386	16.587994	-0.048810	3.587742
245.399903	4329.331588	16.592999	-0.048747	3.584596
245.457514	4321.378744	16.598003	-0.048753	3.581470
245.434434	4313.388749	16.603008	-0.048743	3.578325
245.412754	4305.373215	16.608013	-0.048734	3.575166
245.469413	4297.378037	16.613018	-0.048740	3.572016
245.239222	4289.361927	16.618023	-0.048691	3.568846
245.236519	4281.358425	16.623027	-0.048686	3.565684
245.407879	4273.384701	16.628032	-0.048713	3.562537
245.292755	4265.382368	16.633037	-0.048686	3.559367
245.435432	4257.444526	16.638042	-0.048707	3.556228
245.391422	4249.326770	16.643047	-0.048694	3.553009
245.168898	4241.298141	16.648051	-0.048647	3.549817
245.048391	4233.321861	16.653056	-0.048620	3.546646
245.119669	4225.326620	16.658061	-0.048628	3.543470
245.086696	4217.401265	16.663066	-0.048617	3.540316
244.768990	4209.440967	16.668071	-0.048552	3.537137
245.075251	4201.390723	16.673075	-0.048604	3.533938
245.112554	4193.386781	16.678080	-0.048606	3.530746
244.934996	4185.407943	16.683085	-0.048568	3.527555
245.050260	4177.390693	16.688090	-0.048584	3.524355
244.740936	4169.468475	16.693095	-0.048521	3.521177
244.657379	4161.481718	16.698099	-0.048501	3.517977
244.720295	4153.465338	16.703104	-0.048507	3.514766
244.694807	4145.414818	16.708109	-0.048497	3.511537
244.805584	4137.429621	16.713114	-0.048513	3.508334
244.448976	4129.438866	16.718119	-0.048441	3.505112
244.571127	4121.482155	16.723123	-0.048459	3.501916
244.675680	4113.493715	16.728128	-0.048473	3.498704
244.375037	4105.501525	16.733133	-0.048412	3.495474
244.550988	4097.510612	16.738138	-0.048440	3.492257
244.592226	4089.498104	16.743143	-0.048442	3.489023
244.540485	4081.530423	16.748147	-0.048427	3.485802
244.517926	4073.556267	16.753152	-0.048418	3.482577
244.553131	4065.515580	16.758157	-0.048419	3.479323
244.395822	4057.612373	16.763162	-0.048385	3.476116
244.254098	4049.567567	16.768167	-0.048353	3.472849
244.294861	4041.525904	16.773171	-0.048356	3.469586
244.405011	4033.540029	16.778176	-0.048371	3.466344
244.329731	4025.538778	16.783181	-0.048352	3.463088
244.347518	4017.556812	16.788186	-0.048350	3.459839
244.101999	4009.601156	16.793191	-0.048299	3.456589
244.053452	4001.604368	16.798195	-0.048285	3.453326
244.055634	3993.567508	16.803200	-0.048280	3.450045
244.066165	3985.570460	16.808205	-0.048277	3.446778
244.276859	3977.586153	16.813210	-0.048311	3.443519
243.874846	3969.611015	16.818215	-0.048231	3.440241
243.906029	3961.626706	16.823219	-0.048232	3.436970
244.070862	3953.631484	16.828224	-0.048257	3.433696
243.821421	3945.561393	16.833229	-0.048206	3.430374
243.903057	3937.630806	16.838234	-0.048216	3.427117
243.827817	3929.603030	16.843239	-0.048197	3.423812
243.931903	3921.643308	16.848243	-0.048211	3.420538
243.892790	3913.660581	16.853248	-0.048198	3.417247
243.695386	3905.670673	16.858253	-0.048156	3.413944
243.605397	3897.672890	16.863258	-0.048134	3.410638
243.608021	3889.666910	16.868263	-0.048130	3.407328
243.761980	3881.671945	16.873267	-0.048153	3.404026
243.754182	3873.732079	16.878272	-0.048147	3.400737
243.774694	3865.735060	16.883277	-0.048145	3.397422
243.621143	3857.746148	16.888282	-0.048112	3.394102
243.707539	3849.645804	16.893287	-0.048123	3.390740
243.598707	3841.686976	16.898291	-0.048097	3.387427
243.593863	3833.696472	16.903296	-0.048091	3.384101
243.389849	3825.738924	16.908301	-0.048048	3.380779
243.411808	3817.785096	16.913306	-0.048047	3.377462
243.316336	3809.759354	16.918311	-0.048024	3.374109
243.218436	3801.768733	16.923315	-0.048001	3.370766
243.353499	3793.783351	16.928320	-0.048021	3.367431
243.308481	3785.751178	16.933325	-0.048007	3.364067
243.324247	3777.852892	16.938330	-0.048005	3.360757
243.236479	3769.856738	16.943335	-0.047983	3.357399
243.095194	3761.836087	16.948339	-0.047952	3.354026
243.057469	3753.816118	16.953344	-0.047940	3.350653
243.032806	3745.806823	16.958349	-0.047930	3.347282
243.105759	3737.842334	16.963354	-0.047938	3.343930
242.962474	3729.861677	16.968359	-0.047906	3.340560
242.847991	3721.893291	16.973363	-0.047880	3.337192
242.897241	3713.874393	16.978368	-0.047884	3.333806
242.906799	3705.856029	16.983373	-0.047881	3.330415
243.021122	3697.883077	16.988378	-0.047897	3.327044
243.132560	3689.866130	16.993383	-0.047912	3.323651
242.976603	3681.920601	16.998387	-0.047878	3.320275
242.837818	3673.949385	17.003392	-0.047847	3.316884
242.580521	3665.945492	17.008397	-0.047794	3.313472
242.643178	3657.913528	17.013402	-0.047801	3.310057
242.478168	3649.934971	17.018407	-0.047765	3.306652
242.452768	3641.956669	17.023411	-0.047755	3.303249
242.460134	3633.988066	17.028416	-0.047751	3.299848
242.446943	3625.994465	17.033421	-0.047743	3.296432
242.325237	3618.023996	17.038426	-0.047716	3.293018
242.347404	3609.965851	17.043431	-0.047715	3.289568
242.364009	3602.014930	17.048435	-0.047713	3.286161
242.380227	3594.039561	17.053440	-0.047710	3.282740
242.170725	3586.040608	17.058445	-0.047666	3.279296
242.314035	3578.094390	17.063450	-0.047688	3.275885
242.328625	3570.052806	17.068455	-0.047685	3.272424
242.118965	3562.046652	17.073459	-0.047641	3.268966
242.238760	3554.059539	17.078464	-0.047658	3.265526
242.098377	3546.073493	17.083469	-0.047627	3.262072
242.183738	3538.089018	17.088474	-0.047638	3.258624
242.125538	3530.118200	17.093479	-0.047622	3.255172
242.128442	3522.107027	17.098483	-0.047617	3.251702
241.975186	3514.131033	17.103488	-0.047583	3.248237
241.770880	3506.129527	17.108493	-0.047540	3.244756
241.901692	3498.191142	17.113498	-0.047559	3.241311
241.929826	3490.179565	17.118503	-0.047560	3.237827
241.749784	3482.184486	17.123507	-0.047521	3.234338
241.597516	3474.143291	17.128512	-0.047487	3.230826
241.651587	3466.116685	17.133517	-0.047492	3.227325
241.712085	3458.147441	17.138522	-0.047498	3.223846
241.572923	3450.194070	17.143527	-0.047467	3.220361
241.702856	3442.214846	17.148531	-0.047486	3.216873
241.799600	3434.219579	17.153536	-0.047499	3.213372
241.422971	3426.237795	17.158541	-0.047424	3.209854
241.574563	3418.275417	17.163546	-0.047447	3.206362
241.386251	3410.270100	17.168551	-0.047407	3.202833
241.236505	3402.301934	17.173555	-0.047374	3.199319
241.376551	3394.315053	17.178560	-0.047395	3.195805
241.258587	3386.285803	17.183565	-0.047367	3.192257
241.436526	3378.295926	17.188570	-0.047395	3.188735
241.395338	3370.299765	17.193575	-0.047383	3.185197
241.507433	3362.319670	17.198579	-0.047398	3.181669
241.487173	3354.362493	17.203584	-0.047389	3.178141
241.282321	3346.344724	17.208589	-0.047346	3.174575
241.459366	3338.348420	17.213594	-0.047374	3.171031
241.143634	3330.393140	17.218599	-0.047310	3.167479
241.101471	3322.398734	17.223603	-0.047297	3.163918
241.177068	3314.427132	17.228608	-0.047306	3.160369
241.114109	3306.461135	17.233613	-0.047289	3.156811
241.240798	3298.420725	17.238618	-0.047307	3.153225
240.974473	3290.413794	17.243623	-0.047253	3.149633
241.189381	3282.408114	17.248627	-0.047288	3.146058
241.091904	3274.476138	17.253632	-0.047264	3.142498
241.081970	3266.465343	17.258637	-0.047257	3.138903
240.923495	3258.528347	17.263642	-0.047223	3.135330
240.806869	3250.490911	17.268647	-0.047196	3.131710
240.882939	3242.504090	17.273651	-0.047205	3.128116
240.682444	3234.544077	17.278656	-0.047162	3.124519
240.685024	3226.573208	17.283661	-0.047158	3.120922
240.645345	3218.595012	17.288666	-0.047145	3.117315
240.641261	3210.589425	17.293671	-0.047139	3.113693
240.843867	3202.558084	17.298675	-0.047172	3.110064
240.771223	3194.597228	17.303680	-0.047153	3.106451
240.515001	3186.622806	17.308685	-0.047100	3.102820
240.630269	3178.641883	17.313690	-0.047116	3.099197
240.573548	3170.660087	17.318695	-0.047101	3.095563
240.612519	3162.643820	17.323699	-0.047103	3.091912
240.370952	3154.689238	17.328704	-0.047053	3.088273
240.380009	3146.679203	17.333709	-0.047049	3.084616
240.246946	3138.757204	17.338714	-0.047019	3.080988
240.176816	3130.744156	17.343719	-0.047001	3.077316
240.307105	3122.723064	17.348723	-0.047020	3.073647
240.153622	3114.684621	17.353728	-0.046986	3.069951
240.102382	3106.671316	17.358733	-0.046972	3.066267
240.210299	3098.724667	17.363738	-0.046987	3.062617
239.999842	3090.781417	17.368743	-0.046942	3.058950
240.068399	3082.792787	17.373747	-0.046950	3.055270
240.048587	3074.797145	17.378752	-0.046941	3.051578
240.007429	3066.785036	17.383757	-0.046928	3.047873
240.041095	3058.817452	17.388762	-0.046929	3.044188
239.718477	3050.898347	17.393767	-0.046864	3.040504
239.847825	3042.906554	17.398771	-0.046883	3.036803
240.133299	3034.882041	17.403776	-0.046931	3.033090
239.914221	3026.879392	17.408781	-0.046885	3.029358
239.918731	3018.911017	17.413786	-0.046881	3.025649
239.753550	3010.951376	17.418791	-0.046845	3.021930
239.702075	3002.975026	17.423795	-0.046830	3.018205
239.623645	2994.990676	17.428800	-0.046811	3.014470
239.863248	2986.942889	17.433805	-0.046850	3.010717
240.022061	2978.983440	17.438810	-0.046874	3.006996
239.660256	2971.032700	17.443815	-0.046802	3.003249
239.761001	2963.039295	17.448819	-0.046815	2.999500
239.830880	2955.092272	17.453824	-0.046823	2.995767
239.681917	2947.064965	17.458829	-0.046790	2.991980
239.640991	2939.068872	17.463834	-0.046778	2.988209
239.554153	2931.083808	17.468839	-0.046756	2.984435
239.554134	2923.129357	17.473843	-0.046751	2.980676
239.318123	2915.189008	17.478848	-0.046702	2.976907
239.445982	2907.136336	17.483853	-0.046721	2.973098
239.366781	2899.154880	17.488858	-0.046701	2.969308
239.334855	2891.177276	17.493863	-0.046690	2.965517
239.391597	2883.203647	17.498867	-0.046695	2.961727
239.270562	2875.265876	17.503872	-0.046668	2.957941
239.069776	2867.269067	17.508877	-0.046625	2.954117
239.126587	2859.267969	17.513882	-0.046630	2.950300
239.276748	2851.242953	17.518887	-0.046653	2.946471
239.122428	2843.286706	17.523891	-0.046619	2.942655
238.796887	2835.356850	17.528896	-0.046554	2.938837
238.731965	2827.360370	17.533901	-0.046536	2.934995
238.836405	2819.344256	17.538906	-0.046551	2.931148
238.767281	2811.373116	17.543911	-0.046533	2.927309
238.575896	2803.399939	17.548915	-0.046492	2.923457
238.689727	2795.425281	17.553920	-0.046508	2.919615
238.692420	2787.459692	17.558925	-0.046503	2.915767
238.664155	2779.401607	17.563930	-0.046493	2.911868
238.674726	2771.385480	17.568935	-0.046490	2.907985
238.648523	2763.427205	17.573939	-0.046480	2.904123
238.373530	2755.508947	17.578944	-0.046423	2.900263
238.320774	2747.517121	17.583949	-0.046408	2.896373
238.376040	2739.523440	17.588954	-0.046413	2.892483
238.145099	2731.549244	17.593959	-0.046365	2.888582
237.945635	2723.579248	17.598963	-0.046323	2.884679
238.149582	2715.606443	17.603968	-0.046356	2.880791
238.017190	2707.642341	17.608973	-0.046326	2.876885
238.225691	2699.610913	17.613978	-0.046360	2.872958
238.085794	2691.628118	17.618983	-0.046328	2.869031
238.146402	2683.635094	17.623987	-0.046335	2.865104
238.272559	2675.686814	17.628992	-0.046353	2.861198
238.081260	2667.704072	17.633997	-0.046312	2.857252
238.047758	2659.742466	17.639002	-0.046301	2.853319
237.895831	2651.753489	17.644007	-0.046267	2.849361
237.809959	2643.777041	17.649011	-0.046246	2.845408
238.055100	2635.808803	17.654016	-0.046287	2.841471
237.922772	2627.826478	17.659021	-0.046257	2.837501
237.735242	2619.882386	17.664026	-0.046217	2.833541
237.684125	2611.841209	17.669031	-0.046202	2.829535
237.630168	2603.870594	17.674035	-0.046187	2.825558
237.526045	2595.928838	17.679040	-0.046162	2.821587
237.395753	2587.933924	17.684045	-0.046133	2.817582
237.692306	2579.925149	17.689050	-0.046183	2.813590
237.503033	2571.939860	17.694055	-0.046143	2.809575
237.355544	2563.992966	17.699059	-0.046110	2.805576
237.489627	2556.033077	17.704064	-0.046130	2.801582
237.478139	2548.031889	17.709069	-0.046123	2.797552
237.482964	2540.063239	17.714074	-0.046118	2.793534
237.435692	2532.061430	17.719079	-0.046104	2.789491
237.252545	2524.092574	17.724083	-0.046065	2.785450
237.399793	2516.128994	17.729088	-0.046087	2.781425
237.299921	2508.155204	17.734093	-0.046064	2.777375
237.277465	2500.181610	17.739098	-0.046054	2.773324
237.132836	2492.195933	17.744103	-0.046022	2.769253
237.022851	2484.229657	17.749107	-0.045997	2.765188
237.156057	2476.273547	17.754112	-0.046016	2.761137
237.046678	2468.291583	17.759117	-0.045991	2.757052
237.101660	2460.274130	17.764122	-0.045996	2.752953
236.878284	2452.256944	17.769127	-0.045949	2.748831
236.974848	2444.253050	17.774131	-0.045962	2.744729
236.757768	2436.360657	17.779136	-0.045916	2.740659
236.725435	2428.372175	17.784141	-0.045905	2.736545
236.932389	2420.370976	17.789146	-0.045939	2.732433
236.645610	2412.422227	17.794151	-0.045880	2.728311
236.556251	2404.453714	17.799155	-0.045858	2.724185
236.696237	2396.491675	17.804160	-0.045879	2.720070
236.680664	2388.519874	17.809165	-0.045871	2.715934
236.628858	2380.526120	17.814170	-0.045856	2.711779
236.354530	2372.567697	17.819175	-0.045800	2.707621
236.656472	2364.553727	17.824179	-0.045851	2.703464
236.562014	2356.627628	17.829184	-0.045829	2.699322
236.356330	2348.668041	17.834189	-0.045785	2.695149
236.438520	2340.654023	17.839194	-0.045795	2.690959
236.300273	2332.686187	17.844199	-0.045764	2.686772
236.302259	2324.712702	17.849203	-0.045760	2.682585
236.208100	2316.768643	17.854208	-0.045737	2.678401
236.224593	2308.782174	17.859213	-0.045735	2.674195
236.237633	2300.764331	17.864218	-0.045732	2.669966
236.026323	2292.817768	17.869223	-0.045688	2.665753
236.106249	2284.829532	17.874227	-0.045697	2.661530
236.101036	2276.891975	17.879232	-0.045691	2.657322
235.892486	2268.897847	17.884237	-0.045647	2.653064
236.189520	2260.909020	17.889242	-0.045697	2.648835
236.102341	2252.938903	17.894247	-0.045676	2.644584
235.939175	2244.987474	17.899251	-0.045640	2.640331
236.133530	2237.023060	17.904256	-0.045672	2.636088
235.803662	2229.049692	17.909261	-0.045605	2.631798
235.822903	2221.086576	17.914266	-0.045603	2.627530
235.617324	2213.126994	17.919271	-0.045560	2.623242
235.608758	2205.144265	17.924275	-0.045553	2.618948
235.780489	2197.176593	17.929280	-0.045580	2.614667
235.515543	2189.195168	17.934285	-0.045526	2.610342
235.540659	2181.222496	17.939290	-0.045525	2.606034
235.572847	2173.258075	17.944295	-0.045526	2.601724
235.552357	2165.299022	17.949299	-0.045517	2.597406
235.388222	2157.287325	17.954304	-0.045481	2.593042
235.415266	2149.175857	17.959309	-0.045481	2.588630
235.402461	2141.236844	17.964314	-0.045474	2.584302
235.367271	2133.330799	17.969319	-0.045462	2.579983
235.144515	2125.391152	17.974323	-0.045415	2.575625
235.170511	2117.429194	17.979328	-0.045415	2.571265
235.091824	2109.435660	17.984333	-0.045395	2.566873
235.128369	2101.513645	17.989338	-0.045397	2.562520
235.303430	2093.545338	17.994343	-0.045424	2.558145
235.031856	2085.608683	17.999347	-0.045369	2.553748
235.003230	2077.608740	18.004352	-0.045358	2.549325
234.940434	2069.626188	18.009357	-0.045341	2.544902
234.780688	2061.715451	18.014362	-0.045307	2.540505
234.838840	2053.735415	18.019367	-0.045312	2.536076
234.942450	2045.731800	18.024371	-0.045326	2.531630
234.933579	2037.761593	18.029376	-0.045320	2.527187
234.797226	2029.799100	18.034381	-0.045289	2.522731
234.871844	2021.867754	18.039386	-0.045298	2.518300
234.814605	2013.906574	18.044391	-0.045282	2.513835
234.849827	2005.876276	18.049395	-0.045283	2.509329
234.675948	1997.946375	18.054400	-0.045246	2.504857
234.614823	1989.987956	18.059405	-0.045229	2.500369
234.592818	1982.034934	18.064410	-0.045220	2.495879
234.561004	1974.070193	18.069415	-0.045209	2.491373
234.307633	1966.104804	18.074419	-0.045157	2.486843
234.474262	1958.135306	18.079424	-0.045183	2.482333
234.373458	1950.188603	18.084429	-0.045159	2.477807
234.267693	1942.236854	18.089434	-0.045134	2.473271
234.224005	1934.243833	18.094439	-0.045121	2.468707
234.417975	1926.239773	18.099443	-0.045152	2.464146
234.177234	1918.341272	18.104448	-0.045102	2.459604
234.197843	1910.376536	18.109453	-0.045100	2.455036
234.307656	1902.382082	18.114458	-0.045116	2.450448
234.178248	1894.433932	18.119463	-0.045086	2.445861
234.050230	1886.500315	18.124467	-0.045057	2.441274
234.140780	1878.545347	18.129472	-0.045069	2.436682
233.964755	1870.532762	18.134477	-0.045031	2.432027
233.865981	1862.544766	18.139482	-0.045008	2.427384
233.824525	1854.602614	18.144487	-0.044995	2.422763
233.946887	1846.630910	18.149491	-0.045012	2.418129
233.860443	1838.698092	18.154496	-0.044991	2.413493
233.753516	1830.719016	18.159501	-0.044966	2.408818
233.757762	1822.758530	18.164506	-0.044962	2.404154
233.879135	1814.807438	18.169511	-0.044979	2.399496
233.587529	1806.890211	18.174515	-0.044920	2.394817
233.725779	1798.899981	18.179520	-0.044940	2.390118
233.568375	1790.941418	18.184525	-0.044906	2.385406
233.338942	1783.023085	18.189530	-0.044858	2.380703
233.457010	1775.043132	18.194535	-0.044875	2.375981
233.497738	1767.063621	18.199539	-0.044877	2.371245
233.460725	1759.117292	18.204544	-0.044865	2.366512
233.364476	1751.171325	18.209549	-0.044842	2.361765
233.398083	1743.235603	18.214554	-0.044844	2.357025
233.212553	1735.273815	18.219559	-0.044804	2.352242
233.097042	1727.292347	18.224563	-0.044777	2.347444
233.245581	1719.326489	18.229568	-0.044800	2.342666
233.194338	1711.381371	18.234573	-0.044785	2.337875
232.960106	1703.456772	18.239578	-0.044736	2.333071
232.789580	1695.504656	18.244583	-0.044699	2.328246
232.909669	1687.516140	18.249587	-0.044717	2.323413
232.939560	1679.586754	18.254592	-0.044717	2.318598
232.701638	1671.638439	18.259597	-0.044668	2.313740
232.761129	1663.657821	18.264602	-0.044674	2.308876
232.818741	1655.689889	18.269607	-0.044679	2.304009
232.669718	1647.762015	18.274611	-0.044646	2.299140
232.738443	1639.822617	18.279616	-0.044654	2.294271
232.565229	1631.852722	18.284621	-0.044617	2.289353
232.476187	1623.913492	18.289626	-0.044595	2.284450
232.501863	1615.983090	18.294631	-0.044595	2.279552
232.579847	1608.010600	18.299635	-0.044604	2.274622
232.534416	1599.984471	18.304640	-0.044590	2.269637
232.435974	1592.036240	18.309645	-0.044567	2.264685
232.639329	1584.097829	18.314650	-0.044600	2.259754
232.407226	1576.186196	18.319655	-0.044551	2.254792
232.272220	1568.220582	18.324659	-0.044521	2.249793
232.262752	1560.286316	18.329664	-0.044514	2.244814
232.132647	1552.350036	18.334669	-0.044485	2.239812
232.170654	1544.414497	18.339674	-0.044487	2.234814
232.160304	1536.432596	18.344679	-0.044480	2.229771
232.087253	1528.483196	18.349683	-0.044461	2.224731
232.079052	1520.575915	18.354688	-0.044454	2.219713
232.121868	1512.606524	18.359693	-0.044457	2.214648
232.045095	1504.649888	18.364698	-0.044438	2.209569
232.047871	1496.712822	18.369703	-0.044433	2.204498
231.848750	1488.801793	18.374707	-0.044391	2.199414
231.896383	1480.870673	18.379712	-0.044395	2.194328
231.844417	1472.870201	18.384717	-0.044380	2.189176
231.628423	1464.944462	18.389722	-0.044334	2.184045
231.678734	1457.011765	18.394727	-0.044339	2.178921
231.650717	1449.054898	18.399731	-0.044328	2.173763
231.727626	1441.105115	18.404736	-0.044338	2.168607
231.356013	1433.194951	18.409741	-0.044263	2.163423
231.330091	1425.268306	18.414746	-0.044253	2.158248
231.552139	1417.296180	18.419751	-0.044289	2.153053
231.205987	1409.364228	18.424755	-0.044220	2.147819
231.307831	1401.423735	18.429760	-0.044234	2.142609
231.255703	1393.491893	18.434765	-0.044219	2.137377
231.038696	1385.578622	18.439770	-0.044173	2.132130
231.196474	1377.600477	18.444775	-0.044198	2.126861
231.268327	1369.658328	18.449779	-0.044206	2.121596
231.322726	1361.732718	18.454784	-0.044211	2.116326
231.098389	1353.757899	18.459789	-0.044164	2.110984
230.928627	1345.819766	18.464794	-0.044127	2.105658
230.934427	1337.901752	18.469799	-0.044123	2.100349
230.782406	1329.977213	18.474803	-0.044090	2.095007
230.982502	1322.011698	18.479808	-0.044122	2.089658
230.968555	1314.076979	18.484813	-0.044114	2.084295
230.829600	1306.184314	18.489818	-0.044083	2.078934
230.680153	1298.272762	18.494823	-0.044050	2.073546
230.796552	1290.290657	18.499827	-0.044067	2.068122
230.900973	1282.354647	18.504832	-0.044081	2.062714
230.473733	1274.484101	18.509837	-0.043997	2.057283
230.552290	1266.542613	18.514842	-0.044006	2.051840
230.598043	1258.594533	18.519847	-0.044009	2.046374
230.331308	1250.704935	18.524851	-0.043955	2.040903
230.452076	1242.776765	18.529856	-0.043972	2.035430
230.647760	1234.769568	18.534861	-0.044003	2.029895
230.293876	1226.883656	18.539866	-0.043932	2.024372
230.229155	1218.979285	18.544871	-0.043915	2.018852
230.123846	1211.047071	18.549875	-0.043890	2.013292
230.209772	1203.103631	18.554880	-0.043901	2.007729
229.889102	1195.211564	18.559885	-0.043837	2.002144
230.023069	1187.285111	18.564890	-0.043856	1.996567
230.014932	1179.337215	18.569895	-0.043850	1.990945
229.853420	1171.414572	18.574899	-0.043815	1.985308
229.791442	1163.519864	18.579904	-0.043798	1.979685
229.728456	1155.599032	18.584909	-0.043781	1.974028
229.772114	1147.650796	18.589914	-0.043784	1.968346
229.601682	1139.761805	18.594919	-0.043747	1.962667
229.806713	1131.808562	18.599923	-0.043780	1.956966
229.757307	1123.869793	18.604928	-0.043766	1.951231
229.567453	1115.945956	18.609933	-0.043725	1.945475
229.748966	1108.020364	18.614938	-0.043754	1.939741
229.740592	1100.117706	18.619943	-0.043748	1.933986
229.580812	1092.201816	18.624947	-0.043713	1.928187
229.266298	1084.340207	18.629952	-0.043649	1.922394
229.359384	1076.409132	18.634957	-0.043661	1.916577
229.389495	1068.476865	18.639962	-0.043662	1.910734
229.350959	1060.561276	18.644967	-0.043649	1.904879
229.195144	1052.680244	18.649971	-0.043615	1.899017
229.436315	1044.738430	18.654976	-0.043655	1.893137
229.327743	1036.817821	18.659981	-0.043630	1.887215
229.124075	1028.955763	18.664986	-0.043587	1.881307
229.193895	1021.047799	18.669991	-0.043595	1.875378
229.062724	1013.116793	18.674995	-0.043565	1.869389
228.826877	1005.242123	18.680000	-0.043516	1.863411
228.902227	997.318556	18.685005	-0.043525	1.857413
228.997891	989.392369	18.690010	-0.043538	1.851396
228.917933	981.492411	18.695015	-0.043518	1.845359
228.861491	973.610452	18.700019	-0.043502	1.839318
228.870857	965.714247	18.705024	-0.043499	1.833255
228.522685	957.835654	18.710029	-0.043429	1.827142
228.706361	949.905958	18.715034	-0.043458	1.821033
228.726059	942.029176	18.720039	-0.043457	1.814925
228.512314	934.134642	18.725043	-0.043412	1.808754
228.383018	926.251941	18.730048	-0.043383	1.802581
228.272798	918.382823	18.735053	-0.043357	1.796400
228.194659	910.427491	18.740058	-0.043337	1.790134
228.307457	902.508302	18.745063	-0.043353	1.783897
228.173563	894.636708	18.750067	-0.043323	1.777647
228.242347	886.733101	18.755072	-0.043331	1.771373
227.976402	878.864615	18.760077	-0.043276	1.765064
227.781347	871.019437	18.765082	-0.043235	1.758759
228.021283	863.093644	18.770087	-0.043274	1.752422
228.036949	855.178954	18.775091	-0.043272	1.746042
227.991139	847.320658	18.780096	-0.043259	1.739677
227.825179	839.456433	18.785101	-0.043223	1.733269
227.727524	831.575322	18.790106	-0.043199	1.726831
227.765105	823.701814	18.795111	-0.043201	1.720393
227.603697	815.839303	18.800115	-0.043166	1.713914
227.612442	807.940701	18.805120	-0.043163	1.707403
227.490713	800.066393	18.810125	-0.043135	1.700870
227.418500	792.206894	18.815130	-0.043116	1.694330
227.433894	784.317388	18.820135	-0.043114	1.687752
227.362413	776.450739	18.825139	-0.043096	1.681155
227.100705	768.636791	18.830144	-0.043042	1.674552
226.999013	760.741532	18.835149	-0.043018	1.667875
227.132372	752.846467	18.840154	-0.043038	1.661203
226.987442	745.014008	18.845159	-0.043006	1.654520
226.752190	737.148886	18.850163	-0.042957	1.647769
227.026662	729.258685	18.855168	-0.043003	1.641039
227.068797	721.393826	18.860173	-0.043006	1.634271
226.720701	713.523488	18.865178	-0.042936	1.627416
226.848579	705.644695	18.870183	-0.042954	1.620590
226.743765	697.803130	18.875187	-0.042930	1.613736
226.901115	689.932418	18.880192	-0.042954	1.606864
226.728975	682.111930	18.885197	-0.042917	1.599961
226.758237	674.264894	18.890202	-0.042917	1.593032
226.637458	666.426195	18.895207	-0.042890	1.586059
226.499586	658.598215	18.900211	-0.042859	1.579062
226.627320	650.738313	18.905216	-0.042878	1.572044
226.478506	642.900291	18.910221	-0.042845	1.564974
226.014474	635.152031	18.915226	-0.042754	1.557907
225.986482	627.292903	18.920231	-0.042743	1.550771
226.004425	619.423845	18.925235	-0.042742	1.543599
225.934549	611.600233	18.930240	-0.042724	1.536423
225.797597	603.771266	18.935245	-0.042693	1.529198
225.841963	595.927638	18.940250	-0.042696	1.521953
225.933342	588.102836	18.945255	-0.042708	1.514697
225.674508	580.291195	18.950259	-0.042655	1.507366
225.853706	572.450578	18.955264	-0.042683	1.500038
225.823054	564.633039	18.960269	-0.042673	1.492664
225.504637	556.845928	18.965274	-0.042608	1.485238
225.417441	549.064422	18.970279	-0.042587	1.477815
225.401340	541.202478	18.975283	-0.042579	1.470289
225.385084	533.384774	18.980288	-0.042571	1.462767
225.274286	525.594880	18.985293	-0.042545	1.455218
225.293078	517.782458	18.990298	-0.042544	1.447629
225.399721	509.967716	18.995303	-0.042558	1.440011
225.236540	502.204033	19.000307	-0.042523	1.432359
225.301597	494.395680	19.005312	-0.042530	1.424659
225.032140	486.651244	19.010317	-0.042475	1.416926
224.976604	478.854651	19.015322	-0.042460	1.409134
224.905533	471.084324	19.020327	-0.042441	1.401322
224.797905	463.316944	19.025331	-0.042416	1.393463
224.616431	455.547397	19.030336	-0.042377	1.385545
224.531911	447.775766	19.035341	-0.042357	1.377596
224.560971	439.986268	19.040346	-0.042357	1.369601
224.796635	432.180830	19.045351	-0.042396	1.361579
224.468112	424.474463	19.050355	-0.042330	1.353514
224.435735	416.715447	19.055360	-0.042319	1.345398
224.321137	408.981829	19.060365	-0.042292	1.337244
224.181522	401.236704	19.065370	-0.042261	1.329024
224.087136	393.503024	19.070375	-0.042239	1.320773
223.998126	385.723290	19.075379	-0.042217	1.312422
223.989078	377.904794	19.080384	-0.042211	1.303989
223.706672	370.214648	19.085389	-0.042153	1.295592
223.620484	362.493011	19.090394	-0.042132	1.287141
223.736639	354.763680	19.095399	-0.042149	1.278663
223.548254	347.063973	19.100403	-0.042109	1.270105
223.504532	339.353798	19.105408	-0.042095	1.261504
223.479223	331.652770	19.110413	-0.042086	1.252858
223.110851	324.006508	19.115418	-0.042012	1.244148
222.735752	316.373616	19.120423	-0.041938	1.235390
222.657816	308.648131	19.125427	-0.041918	1.226521
222.554986	300.973236	19.130432	-0.041894	1.217642
222.030124	293.355274	19.135437	-0.041791	1.208679
221.848077	285.693501	19.140442	-0.041752	1.199667
221.761118	278.027334	19.145447	-0.041731	1.190600
221.227810	270.419716	19.150451	-0.041627	1.181443
220.835439	262.815191	19.155456	-0.041549	1.172246
220.569348	255.175579	19.160461	-0.041495	1.162960
220.173164	247.567310	19.165466	-0.041416	1.153611
219.918331	239.915035	19.170471	-0.041364	1.144160
219.408331	232.336026	19.175475	-0.041264	1.134668
219.024071	224.745473	19.180480	-0.041187	1.125107
218.620642	217.171437	19.185485	-0.041107	1.115481
218.010436	209.621603	19.190490	-0.040989	1.105757
217.855272	202.018766	19.195495	-0.040955	1.095979
217.535075	194.433384	19.200499	-0.040890	1.086098
217.177411	186.897715	19.205504	-0.040819	1.076183
216.524988	179.377328	19.210509	-0.040693	1.066129
216.191304	171.835624	19.215514	-0.040626	1.056023
215.656222	164.327010	19.220519	-0.040521	1.045818
215.324978	156.806334	19.225523	-0.040455	1.035543
214.876581	149.314128	19.230528	-0.040366	1.025177
214.254629	141.860820	19.235533	-0.040246	1.014716
213.807304	134.380225	19.240538	-0.040158	1.004151
213.481649	126.898604	19.245543	-0.040092	0.993501
212.792386	119.454781	19.250547	-0.039959	0.982699
212.206552	112.044848	19.255552	-0.039845	0.971852
211.636795	104.637894	19.260557	-0.039734	0.960891
211.330905	97.205032	19.265562	-0.039673	0.949833
210.774025	89.827723	19.270567	-0.039564	0.938662
210.391910	82.428990	19.275571	-0.039488	0.927371
209.880893	75.095830	19.280576	-0.039388	0.916006
209.294377	67.757474	19.285581	-0.039274	0.904469
208.922048	60.650524	19.290586	-0.039200	0.893208