Fri Mar 12 13:40:02 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.269908	-0.014435	0.000000	-0.000015	0.721434

0.166167	0.007925	0.005005	0.000004	0.721442
0.356011	-0.027670	0.010010	-0.000032	0.721439
0.079443	0.020027	0.015014	0.000020	0.721436
0.276843	-0.011118	0.020019	-0.000017	0.721444
0.283541	-0.015887	0.025024	-0.000018	0.721437
0.368225	-0.030612	0.030029	-0.000034	0.721437
0.300183	-0.016951	0.035034	-0.000021	0.721441
0.402876	-0.037702	0.040038	-0.000040	0.721436
0.373074	-0.027556	0.045043	-0.000035	0.721445
0.362976	-0.028619	0.050048	-0.000033	0.721440
0.304309	-0.016469	0.055053	-0.000022	0.721443
0.260899	-0.008781	0.060058	-0.000014	0.721443
0.221959	-0.005820	0.065062	-0.000007	0.721436
0.429840	-0.052566	0.070067	-0.000046	0.721417
0.319891	-0.184754	0.075072	-0.000025	0.721118
0.207497	-0.163116	0.080077	-0.000004	0.721121
0.326353	-0.183411	0.085082	-0.000027	0.721123
0.165667	-0.157539	0.090086	0.000003	0.721118
0.258213	-0.169340	0.095091	-0.000014	0.721127
0.053739	-0.137455	0.100096	0.000024	0.721118
0.111734	-0.201308	0.105101	0.000013	0.721013
0.160357	-0.276376	0.110106	0.000004	0.720883
0.327261	-0.309989	0.115110	-0.000027	0.720875
0.388807	-0.316351	0.120115	-0.000038	0.720884
0.232229	-0.293429	0.125120	-0.000009	0.720874
0.133597	-0.347655	0.130125	0.000009	0.720733
0.081881	-0.436271	0.135130	0.000019	0.720541
0.126751	-0.446842	0.140134	0.000010	0.720536
0.339318	-0.479267	0.145139	-0.000029	0.720547
0.422144	-0.524825	0.150144	-0.000045	0.720486
0.293029	-0.635055	0.155149	-0.000021	0.720224
0.236918	-0.624114	0.160154	-0.000010	0.720226
0.279126	-0.635716	0.165158	-0.000018	0.720218
0.149850	-0.684141	0.170163	0.000006	0.720077
0.017560	-0.750594	0.175168	0.000030	0.719900
0.159913	-0.775117	0.180173	0.000004	0.719902
0.115176	-0.770956	0.185178	0.000012	0.719894
-0.147471	-0.874002	0.190182	0.000061	0.719599
0.059825	-0.907756	0.195187	0.000023	0.719605
-0.029300	-0.894698	0.200192	0.000039	0.719600
0.031088	-1.034156	0.205197	0.000028	0.719346
0.097140	-1.083286	0.210202	0.000016	0.719273
-0.005570	-1.068084	0.215206	0.000035	0.719267
0.059615	-1.201849	0.220211	0.000023	0.719026
0.077235	-1.236640	0.225216	0.000019	0.718963
0.267008	-1.287334	0.230221	-0.000016	0.718930
0.012167	-1.383540	0.235226	0.000031	0.718651
-0.244482	-1.341906	0.240230	0.000079	0.718643
-0.003595	-1.446296	0.245235	0.000034	0.718521
-0.202655	-1.497852	0.250240	0.000071	0.718350
-0.131883	-1.506073	0.255245	0.000058	0.718359
-0.050525	-1.672989	0.260250	0.000043	0.718058
-0.061650	-1.693255	0.265254	0.000045	0.718014
-0.144998	-1.755089	0.270259	0.000061	0.717862
-0.198072	-1.827196	0.275264	0.000070	0.717701
-0.439677	-1.808806	0.280269	0.000115	0.717653
-0.558895	-1.923780	0.285274	0.000138	0.717383
-0.528914	-1.932164	0.290278	0.000132	0.717377
-0.520862	-2.048565	0.295283	0.000131	0.717150
-0.398246	-2.104659	0.300288	0.000108	0.717082
-0.676042	-2.149665	0.305293	0.000159	0.716896
-1.899831	-2.001765	0.310298	0.000387	0.716757
-2.531751	-1.893939	0.315302	0.000505	0.716748
-2.844222	-1.977659	0.320307	0.000563	0.716472
-3.607917	-1.854751	0.325312	0.000705	0.716446
-3.537717	-1.867890	0.330317	0.000692	0.716445
-2.893376	-2.090977	0.335322	0.000572	0.716230
-4.041082	-1.941147	0.340326	0.000786	0.716122
-4.202566	-1.907893	0.345331	0.000816	0.716131
-3.987167	-1.990866	0.350336	0.000775	0.716043
-4.729356	-1.939881	0.355341	0.000914	0.715882
-4.409567	-1.996418	0.360346	0.000854	0.715883
-5.060442	-1.884729	0.365350	0.000975	0.715875
-4.972230	-2.027087	0.370355	0.000959	0.715624
-5.833157	-1.917186	0.375360	0.001119	0.715538
-6.142648	-1.858907	0.380365	0.001176	0.715544
-5.579486	-1.957541	0.385370	0.001072	0.715547
-5.922821	-1.992974	0.390374	0.001135	0.715356
-7.131974	-1.838606	0.395379	0.001360	0.715235
-6.356539	-1.982654	0.400384	0.001216	0.715223
-6.739058	-1.913923	0.405389	0.001287	0.715225
-6.804538	-1.900412	0.410394	0.001299	0.715228
-7.058846	-2.003579	0.415398	0.001347	0.714934
-7.298589	-1.974677	0.420403	0.001391	0.714907
-7.606054	-1.921597	0.425408	0.001449	0.714903
-7.930170	-1.863426	0.430413	0.001509	0.714904
-7.673470	-1.907549	0.435418	0.001461	0.714908
-7.717521	-2.029429	0.440422	0.001469	0.714650
-8.422222	-1.925706	0.445427	0.001600	0.714607
-8.830706	-1.854273	0.450432	0.001676	0.714604
-8.356416	-1.939796	0.455437	0.001588	0.714602
-8.094541	-1.983348	0.460442	0.001539	0.714609
-8.597746	-1.973420	0.465446	0.001633	0.714450
-9.427230	-1.914615	0.470451	0.001787	0.714274
-9.151071	-1.965470	0.475456	0.001736	0.714271
-9.615598	-1.881535	0.480461	0.001822	0.714273
-9.243507	-1.945629	0.485466	0.001753	0.714277
-9.454545	-1.912436	0.490470	0.001792	0.714269
-9.576589	-1.961926	0.495475	0.001815	0.714127
-10.511717	-1.878010	0.500480	0.001989	0.713963
-10.100192	-1.950939	0.505485	0.001912	0.713964
-10.280929	-1.916818	0.510490	0.001946	0.713968
-10.846401	-1.819767	0.515494	0.002051	0.713961
-10.067573	-1.953463	0.520499	0.001906	0.713971
-10.296574	-1.919030	0.525504	0.001949	0.713958
-11.332130	-1.891322	0.530509	0.002141	0.713647
-11.140315	-1.922124	0.535514	0.002106	0.713653
-11.120345	-1.930279	0.540518	0.002102	0.713644
-10.789498	-1.985578	0.545523	0.002040	0.713652
-11.255513	-1.905144	0.550528	0.002127	0.713647
-11.337925	-1.890229	0.555533	0.002142	0.713647
-10.770402	-2.070873	0.560538	0.002037	0.713489
-12.290893	-1.870807	0.565542	0.002320	0.713348
-11.935403	-1.929832	0.570547	0.002253	0.713357
-11.795132	-1.957182	0.575552	0.002227	0.713352
-12.180887	-1.888259	0.580557	0.002299	0.713353
-11.943311	-1.928238	0.585562	0.002255	0.713358
-12.132380	-1.901971	0.590566	0.002290	0.713343
-12.717359	-1.957964	0.595571	0.002399	0.713024
-12.892748	-1.928404	0.600576	0.002431	0.713021
-13.138846	-1.885579	0.605581	0.002477	0.713019
-12.733019	-1.955224	0.610586	0.002402	0.713024
-13.339301	-1.851714	0.615590	0.002514	0.713016
-12.969128	-1.912535	0.620595	0.002445	0.713026
-12.563502	-2.016109	0.625600	0.002370	0.712964
-13.874612	-1.911622	0.630605	0.002614	0.712707
-13.892612	-1.905086	0.635610	0.002617	0.712713
-13.978247	-1.894889	0.640614	0.002633	0.712703
-13.504829	-1.973405	0.645619	0.002545	0.712715
-14.051447	-1.879502	0.650624	0.002647	0.712708
-14.075025	-1.878401	0.655629	0.002651	0.712702
-13.260188	-2.058716	0.660634	0.002499	0.712632
-14.588086	-1.950152	0.665638	0.002746	0.712377
-14.685391	-1.928115	0.670643	0.002765	0.712387
-14.801101	-1.909265	0.675648	0.002786	0.712383
-14.691279	-1.928328	0.680653	0.002766	0.712384
-14.631584	-1.937087	0.685658	0.002754	0.712388
-14.942408	-1.885979	0.690662	0.002812	0.712380
-14.568760	-2.006747	0.695667	0.002743	0.712272
-15.738465	-1.892654	0.700672	0.002960	0.712084
-15.569510	-1.923781	0.705677	0.002929	0.712082
-15.458658	-1.939425	0.710682	0.002908	0.712090
-15.775533	-1.886961	0.715686	0.002967	0.712083
-15.924594	-1.856997	0.720691	0.002995	0.712089
-15.711273	-1.898106	0.725696	0.002955	0.712083
-15.498426	-1.966545	0.730701	0.002915	0.712023
-16.569917	-1.905854	0.735706	0.003115	0.711763
-16.602814	-1.905124	0.740710	0.003121	0.711753
-16.581911	-1.903802	0.745715	0.003117	0.711763
-16.772900	-1.872592	0.750720	0.003152	0.711758
-16.715247	-1.881891	0.755725	0.003142	0.711760
-16.322916	-1.951178	0.760730	0.003069	0.711761
-16.444059	-1.934411	0.765734	0.003091	0.711751
-16.961912	-1.978813	0.770739	0.003188	0.711479
-17.373894	-1.919452	0.775744	0.003264	0.711451
-17.528502	-1.893510	0.780749	0.003293	0.711448
-17.294283	-1.931299	0.785754	0.003249	0.711456
-17.492431	-1.901081	0.790758	0.003286	0.711446
-17.333000	-1.926364	0.795763	0.003256	0.711452
-17.463642	-1.903401	0.800768	0.003281	0.711452
-18.084307	-1.940215	0.805773	0.003396	0.711158
-18.027322	-1.958979	0.810778	0.003386	0.711140
-18.527420	-1.875889	0.815782	0.003479	0.711129
-18.349238	-1.901974	0.820787	0.003445	0.711140
-18.207656	-1.930493	0.825792	0.003419	0.711133
-18.362794	-1.902577	0.830797	0.003448	0.711134
-18.164249	-1.936436	0.835802	0.003411	0.711137
-18.855255	-1.932770	0.840806	0.003539	0.710899
-19.011978	-1.918960	0.845811	0.003569	0.710871
-19.221386	-1.884344	0.850816	0.003607	0.710865
-19.404234	-1.850592	0.855821	0.003641	0.710868
-19.341124	-1.859027	0.860826	0.003630	0.710874
-19.248201	-1.880399	0.865830	0.003612	0.710864
-19.354253	-1.857281	0.870835	0.003632	0.710873
-19.208451	-1.980214	0.875840	0.003605	0.710679
-20.406586	-1.841271	0.880845	0.003828	0.710530
-20.220480	-1.871822	0.885850	0.003793	0.710535
-20.260062	-1.868837	0.890854	0.003800	0.710527
-20.005610	-1.911606	0.895859	0.003753	0.710533
-19.904071	-1.932206	0.900864	0.003734	0.710528
-20.328673	-1.857286	0.905869	0.003813	0.710526
-20.150338	-1.950493	0.910874	0.003780	0.710404
-21.242712	-1.854268	0.915878	0.003983	0.710207
-20.691077	-1.946408	0.920883	0.003881	0.710220
-20.947289	-1.904385	0.925888	0.003928	0.710212
-21.176681	-1.864095	0.930893	0.003971	0.710211
-21.086428	-1.876628	0.935898	0.003954	0.710218
-21.287378	-1.844063	0.940902	0.003991	0.710212
-20.987348	-1.937138	0.945907	0.003935	0.710133
-22.034148	-1.869723	0.950912	0.004130	0.709895
-22.304817	-1.823364	0.955917	0.004181	0.709891
-22.078850	-1.862311	0.960922	0.004139	0.709894
-22.049325	-1.870973	0.965926	0.004133	0.709887
-22.262228	-1.827959	0.970931	0.004173	0.709897
-22.242525	-1.833817	0.975936	0.004169	0.709893
-22.023509	-1.875117	0.980941	0.004128	0.709888
-21.983417	-1.948198	0.985946	0.004121	0.709757
-23.174857	-1.820284	0.990950	0.004342	0.709588
-22.552391	-1.927632	0.995955	0.004226	0.709595
-22.615080	-1.917908	1.000960	0.004238	0.709592
-23.043921	-1.844529	1.005965	0.004318	0.709586
-22.413426	-1.951669	1.010970	0.004200	0.709597
-22.800826	-1.888212	1.015974	0.004272	0.709586
-23.227666	-1.923185	1.020979	0.004352	0.709364
-23.795527	-1.873746	1.025984	0.004458	0.709260
-23.667070	-1.897775	1.030989	0.004434	0.709258
-23.527166	-1.919241	1.035994	0.004408	0.709265
-24.107788	-1.821305	1.040998	0.004516	0.709254
-23.557428	-1.914207	1.046003	0.004413	0.709265
-23.471277	-1.932880	1.051008	0.004397	0.709258
-24.296145	-1.885631	1.056013	0.004551	0.709058
-24.721176	-1.859439	1.061018	0.004630	0.708959
-24.463867	-1.909396	1.066022	0.004582	0.708951
-24.719679	-1.861585	1.071027	0.004629	0.708956
-25.067588	-1.800947	1.076032	0.004694	0.708953
-24.674834	-1.873367	1.081037	0.004621	0.708948
-24.241807	-1.946337	1.086042	0.004540	0.708957
-24.848495	-1.885969	1.091046	0.004653	0.708861
-25.535893	-1.874692	1.096051	0.004781	0.708639
-24.950493	-1.980629	1.101056	0.004672	0.708636
-25.791883	-1.833167	1.106061	0.004829	0.708631
-25.360488	-1.905771	1.111066	0.004748	0.708639
-25.432030	-1.896882	1.116070	0.004762	0.708632
-25.643234	-1.855386	1.121075	0.004801	0.708639
-25.566260	-1.922413	1.126080	0.004786	0.708533
-26.244458	-1.895504	1.131085	0.004913	0.708345
-26.084237	-1.920091	1.136090	0.004883	0.708353
-26.954750	-1.769498	1.141094	0.005045	0.708344
-26.546359	-1.839954	1.146099	0.004969	0.708348
-26.069375	-1.925868	1.151104	0.004880	0.708347
-26.660313	-1.821249	1.156109	0.004990	0.708345
-26.509566	-1.880488	1.161114	0.004962	0.708280
-27.194880	-1.892842	1.166118	0.005089	0.708011
-27.015574	-1.922624	1.171123	0.005056	0.708015
-27.478566	-1.843221	1.176128	0.005142	0.708009
-27.248487	-1.884701	1.181133	0.005099	0.708008
-26.855410	-1.948965	1.186138	0.005026	0.708020
-27.495379	-1.840314	1.191142	0.005145	0.708009
-27.484582	-1.883079	1.196147	0.005143	0.707928
-27.941432	-1.914563	1.201152	0.005228	0.707701
-28.047699	-1.897533	1.206157	0.005248	0.707697
-28.173788	-1.872027	1.211162	0.005271	0.707704
-28.178375	-1.875689	1.216166	0.005272	0.707695
-28.083528	-1.888201	1.221171	0.005254	0.707704
-28.218110	-1.866163	1.226176	0.005279	0.707700
-28.303648	-1.890105	1.231181	0.005295	0.707621
-28.623179	-1.951574	1.236186	0.005355	0.707384
-28.972509	-1.895496	1.241190	0.005420	0.707371
-29.346684	-1.825771	1.246195	0.005489	0.707378
-28.555150	-1.967096	1.251200	0.005342	0.707377
-29.086464	-1.874341	1.256205	0.005441	0.707373
-29.412947	-1.812456	1.261210	0.005501	0.707381
-29.130538	-1.885590	1.266214	0.005449	0.707335
-29.609994	-1.925422	1.271219	0.005538	0.707084
-29.921268	-1.871964	1.276224	0.005596	0.707080
-30.326992	-1.800620	1.281229	0.005671	0.707078
-29.650997	-1.918087	1.286234	0.005546	0.707084
-29.882393	-1.880499	1.291238	0.005589	0.707077
-30.103502	-1.838525	1.296243	0.005630	0.707082
-29.609900	-1.952289	1.301248	0.005538	0.707030
-30.536662	-1.927680	1.306253	0.005710	0.706748
-30.734475	-1.888382	1.311258	0.005747	0.706756
-30.770350	-1.885450	1.316262	0.005754	0.706750
-30.349777	-1.958402	1.321267	0.005675	0.706754
-30.678083	-1.902527	1.326272	0.005736	0.706748
-31.014923	-1.842838	1.331277	0.005799	0.706748
-30.524406	-1.992836	1.336282	0.005708	0.706622
-31.951473	-1.830291	1.341286	0.005973	0.706438
-31.774754	-1.860281	1.346291	0.005940	0.706441
-31.382915	-1.929551	1.351296	0.005867	0.706442
-31.885600	-1.840803	1.356301	0.005961	0.706441
-31.876686	-1.838550	1.361306	0.005959	0.706448
-31.748616	-1.866161	1.366310	0.005935	0.706439
-31.535326	-1.931335	1.371315	0.005896	0.706384
-32.467680	-1.893203	1.376320	0.006069	0.706127
-32.764040	-1.842086	1.381325	0.006124	0.706124
-32.443226	-1.896833	1.386330	0.006065	0.706129
-32.538435	-1.884058	1.391334	0.006082	0.706120
-32.805573	-1.833064	1.396339	0.006132	0.706127
-32.643369	-1.862759	1.401344	0.006102	0.706126
-32.610995	-1.869816	1.406349	0.006096	0.706123
-32.875738	-1.939813	1.411354	0.006145	0.705888
-33.486950	-1.845568	1.416358	0.006259	0.705858
-33.366654	-1.864960	1.421363	0.006236	0.705862
-33.258748	-1.882958	1.426368	0.006216	0.705865
-33.598609	-1.825638	1.431373	0.006279	0.705858
-32.815160	-1.962159	1.436378	0.006133	0.705865
-33.037634	-1.979392	1.441382	0.006175	0.705750
-34.410609	-1.848194	1.446387	0.006430	0.705522
-33.798060	-1.955379	1.451392	0.006316	0.705526
-34.185770	-1.891038	1.456397	0.006388	0.705517
-34.072286	-1.905571	1.461402	0.006367	0.705528
-34.018575	-1.921667	1.466406	0.006357	0.705515
-34.157372	-1.892816	1.471411	0.006383	0.705524
-34.484316	-1.960111	1.476416	0.006444	0.705271
-35.494563	-1.813903	1.481421	0.006632	0.705203
-35.021925	-1.893358	1.486426	0.006544	0.705213
-34.934952	-1.912861	1.491430	0.006528	0.705205
-35.342485	-1.837422	1.496435	0.006603	0.705210
-35.066310	-1.887203	1.501440	0.006552	0.705209
-35.192066	-1.866184	1.506445	0.006575	0.705207
-35.182414	-1.968232	1.511450	0.006574	0.705005
-36.418367	-1.810292	1.516454	0.006804	0.704879
-35.886897	-1.901014	1.521459	0.006705	0.704887
-35.650711	-1.944093	1.526464	0.006661	0.704885
-36.518528	-1.790356	1.531469	0.006822	0.704883
-35.864426	-1.901855	1.536474	0.006700	0.704894
-35.820293	-1.916122	1.541478	0.006692	0.704881
-36.308787	-1.919589	1.546483	0.006783	0.704699
-36.891792	-1.870586	1.551488	0.006891	0.704588
-36.816648	-1.887279	1.556493	0.006877	0.704582
-36.811917	-1.882975	1.561498	0.006876	0.704592
-37.076729	-1.840805	1.566502	0.006926	0.704582
-36.735041	-1.898200	1.571507	0.006862	0.704589
-36.776015	-1.891364	1.576512	0.006870	0.704588
-37.261225	-1.905056	1.581517	0.006960	0.704386
-37.950132	-1.845276	1.586522	0.007088	0.704259
-37.573918	-1.916689	1.591526	0.007018	0.704251
-37.969664	-1.842383	1.596531	0.007092	0.704258
-37.611784	-1.905920	1.601536	0.007025	0.704259
-37.764153	-1.881508	1.606541	0.007053	0.704254
-37.643181	-1.899247	1.611546	0.007031	0.704261
-38.079930	-1.891415	1.616550	0.007112	0.704120
-38.798731	-1.847097	1.621555	0.007246	0.703951
-38.223752	-1.948065	1.626560	0.007139	0.703955
-38.931948	-1.826374	1.631565	0.007271	0.703945
-38.552002	-1.889977	1.636570	0.007200	0.703954
-38.464546	-1.909327	1.641574	0.007183	0.703946
-38.818982	-1.845521	1.646579	0.007249	0.703948
-38.644344	-1.951107	1.651584	0.007217	0.703798
-39.530814	-1.877626	1.656589	0.007382	0.703627
-39.212228	-1.930139	1.661594	0.007323	0.703636
-39.528270	-1.877857	1.666598	0.007381	0.703628
-39.464016	-1.886687	1.671603	0.007369	0.703633
-39.072716	-1.955992	1.676608	0.007296	0.703634
-39.604094	-1.863925	1.681613	0.007395	0.703629
-39.885098	-1.926096	1.686618	0.007448	0.703402
-40.216080	-1.901964	1.691622	0.007509	0.703332
-40.455690	-1.857468	1.696627	0.007554	0.703336
-40.167652	-1.907050	1.701632	0.007500	0.703339
-40.251214	-1.895558	1.706637	0.007516	0.703332
-39.996248	-1.934951	1.711642	0.007468	0.703345
-40.243243	-1.909939	1.716646	0.007514	0.703306
-41.000862	-1.925877	1.721651	0.007655	0.703002
-40.688220	-1.980929	1.726656	0.007597	0.703003
-41.550563	-1.831545	1.731661	0.007757	0.702994
-41.182665	-1.892276	1.736666	0.007689	0.703004
-41.050727	-1.921061	1.741670	0.007664	0.702994
-41.254688	-1.881183	1.746675	0.007702	0.703001
-41.374784	-1.878322	1.751680	0.007724	0.702964
-42.045628	-1.894935	1.756685	0.007849	0.702688
-41.763668	-1.941467	1.761690	0.007797	0.702696
-42.468986	-1.819457	1.766694	0.007928	0.702689
-42.209313	-1.863831	1.771699	0.007880	0.702693
-41.869249	-1.925165	1.776704	0.007816	0.702691
-42.308545	-1.850357	1.781709	0.007898	0.702684
-42.142594	-1.874543	1.786714	0.007867	0.702695
-42.468333	-1.962517	1.791718	0.007928	0.702400
-43.093329	-1.868223	1.796723	0.008044	0.702366
-43.336204	-1.822759	1.801728	0.008089	0.702370
-42.911956	-1.902656	1.806733	0.008010	0.702361
-42.895438	-1.900471	1.811738	0.008007	0.702372
-43.196969	-1.851228	1.816742	0.008063	0.702363
-43.237809	-1.841479	1.821747	0.008071	0.702368
-43.028116	-1.966886	1.826752	0.008032	0.702190
-44.164128	-1.825382	1.831757	0.008243	0.702067
-43.777052	-1.891165	1.836762	0.008171	0.702073
-43.647248	-1.916360	1.841766	0.008147	0.702069
-43.905649	-1.869324	1.846771	0.008195	0.702071
-43.975598	-1.856007	1.851776	0.008208	0.702073
-44.046851	-1.845390	1.856781	0.008221	0.702069
-43.944642	-1.968413	1.861786	0.008202	0.701857
-44.935701	-1.850523	1.866790	0.008386	0.701738
-44.929734	-1.851437	1.871795	0.008385	0.701738
-44.377280	-1.948294	1.876800	0.008282	0.701742
-44.755214	-1.884301	1.881805	0.008353	0.701735
-44.712472	-1.886527	1.886810	0.008345	0.701746
-44.677316	-1.895963	1.891814	0.008338	0.701740
-44.752452	-1.998031	1.896819	0.008352	0.701506
-45.598635	-1.881576	1.901824	0.008509	0.701437
-45.631513	-1.879766	1.906829	0.008516	0.701428
-45.400020	-1.916231	1.911834	0.008472	0.701438
-45.618104	-1.881511	1.916838	0.008513	0.701430
-45.771255	-1.854437	1.921843	0.008541	0.701430
-45.037751	-2.000158	1.926848	0.008405	0.701399
-46.171372	-1.939199	1.931853	0.008616	0.701114
-46.256428	-1.921185	1.936858	0.008632	0.701119
-46.581885	-1.864155	1.941862	0.008692	0.701117
-46.414171	-1.893488	1.946867	0.008661	0.701119
-46.292531	-1.914144	1.951872	0.008638	0.701121
-46.623926	-1.857712	1.956877	0.008700	0.701116
-45.980626	-2.014625	1.961882	0.008580	0.701030
-47.052300	-1.906430	1.966886	0.008780	0.700862
-47.246851	-1.869931	1.971891	0.008816	0.700866
-46.950245	-1.920555	1.976896	0.008760	0.700871
-47.007488	-1.912701	1.981901	0.008771	0.700866
-47.050117	-1.899942	1.986906	0.008779	0.700877
-46.961357	-1.920436	1.991910	0.008762	0.700867
-47.425836	-2.001746	1.996915	0.008849	0.700535
-48.011896	-1.900004	2.001920	0.008958	0.700529

-47.638361	-1.966317	2.011917	0.008888	0.700530
-47.985344	-1.903523	2.021914	0.008953	0.700532
-48.107261	-1.884181	2.031910	0.008975	0.700527
-47.971710	-1.908864	2.041907	0.008950	0.700526
-48.319281	-1.915811	2.051904	0.009015	0.700387
-48.325478	-1.903730	2.061901	0.009016	0.700409
-48.041888	-1.892752	2.071898	0.008963	0.700534
-47.869659	-1.924438	2.081894	0.008931	0.700532
-47.964575	-1.907983	2.091891	0.008948	0.700532
-48.083938	-1.887708	2.101888	0.008970	0.700530
-47.818767	-1.933463	2.111885	0.008921	0.700533
-48.034041	-1.896354	2.121882	0.008961	0.700531
-47.915254	-1.916698	2.131878	0.008939	0.700533
-47.904418	-1.920065	2.141875	0.008937	0.700530
-47.439625	-1.858364	2.151872	0.008850	0.700823
-46.942798	-1.921630	2.161869	0.008757	0.700875
-47.206175	-1.874904	2.171866	0.008806	0.700874
-47.061703	-1.902025	2.181862	0.008779	0.700872
-47.171972	-1.840134	2.191859	0.008800	0.700957
-46.338111	-1.909095	2.201856	0.008644	0.701119
-46.405592	-1.895296	2.211853	0.008657	0.701123
-46.444636	-1.889191	2.221850	0.008664	0.701121
-46.030170	-1.871997	2.231846	0.008587	0.701306
-45.543879	-1.896770	2.241843	0.008496	0.701431
-45.796021	-1.850389	2.251840	0.008543	0.701435
-45.538792	-1.890515	2.261837	0.008495	0.701446
-45.105527	-1.821985	2.271834	0.008414	0.701742
-44.690958	-1.895222	2.281830	0.008337	0.701743
-45.055267	-1.831273	2.291827	0.008405	0.701741
-44.307542	-1.850392	2.301824	0.008265	0.701973
-43.955303	-1.863755	2.311821	0.008200	0.702073
-43.962224	-1.862220	2.321818	0.008201	0.702073
-43.776234	-1.874218	2.331814	0.008166	0.702116
-43.052004	-1.882586	2.341811	0.008031	0.702361
-42.764204	-1.931476	2.351808	0.007978	0.702366
-42.952512	-1.896941	2.361805	0.008013	0.702368
-42.806665	-1.842115	2.371802	0.007985	0.702532
-41.950802	-1.916614	2.381798	0.007826	0.702690
-42.296593	-1.856746	2.391795	0.007890	0.702686
-41.963803	-1.915589	2.401792	0.007828	0.702687
-41.398612	-1.859006	2.411789	0.007723	0.703005
-41.117813	-1.909739	2.421786	0.007670	0.703004
-41.170508	-1.901551	2.431782	0.007680	0.703002
-41.161328	-1.830021	2.441779	0.007678	0.703150
-40.234361	-1.903608	2.451776	0.007506	0.703335
-40.303797	-1.891275	2.461773	0.007519	0.703335
-40.075518	-1.932372	2.471770	0.007476	0.703335
-39.539417	-1.908709	2.481766	0.007376	0.703576
-39.537317	-1.881169	2.491763	0.007376	0.703632
-39.260716	-1.929602	2.501760	0.007324	0.703634
-39.416739	-1.866122	2.511757	0.007353	0.703706
-38.634714	-1.885694	2.521754	0.007207	0.703948
-38.803829	-1.855474	2.531750	0.007239	0.703948
-38.878239	-1.844076	2.541747	0.007252	0.703945
-37.642838	-1.914586	2.551744	0.007022	0.704247
-37.675408	-1.903322	2.561741	0.007028	0.704258
-37.518186	-1.931826	2.571738	0.006999	0.704257
-37.713746	-1.847113	2.581734	0.007035	0.704358
-36.806545	-1.895938	2.591731	0.006866	0.704586
-36.746653	-1.906741	2.601728	0.006855	0.704586
-36.880336	-1.882567	2.611725	0.006880	0.704586
-36.068216	-1.906408	2.621722	0.006728	0.704830
-36.336243	-1.832366	2.631718	0.006778	0.704883
-36.099535	-1.874845	2.641715	0.006734	0.704883
-35.740066	-1.858222	2.651712	0.006667	0.705046
-35.309202	-1.853219	2.661709	0.006587	0.705211
-35.338335	-1.849509	2.671706	0.006592	0.705208
-35.424706	-1.784077	2.681702	0.006608	0.705309
-34.314206	-1.876781	2.691699	0.006401	0.705521
-34.474071	-1.849223	2.701696	0.006431	0.705519
-34.375367	-1.865934	2.711693	0.006412	0.705521
-33.524636	-1.856266	2.721690	0.006254	0.705846
-33.422626	-1.868552	2.731686	0.006235	0.705858
-33.358375	-1.881374	2.741683	0.006223	0.705855
-33.235937	-1.856227	2.751680	0.006200	0.705950
-32.545364	-1.892702	2.761677	0.006071	0.706124
-32.503197	-1.900888	2.771674	0.006063	0.706123
-32.793150	-1.848664	2.781670	0.006117	0.706124
-31.776109	-1.891126	2.791667	0.005928	0.706403
-31.883236	-1.854927	2.801664	0.005948	0.706438
-31.657168	-1.893716	2.811661	0.005905	0.706441
-31.465047	-1.859671	2.821658	0.005870	0.706579
-30.960591	-1.865374	2.831654	0.005776	0.706748
-30.939671	-1.870201	2.841651	0.005772	0.706746
-31.060813	-1.834335	2.851648	0.005794	0.706775
-30.209335	-1.834881	2.861645	0.005635	0.707079
-29.880275	-1.893894	2.871642	0.005574	0.707078
-30.308779	-1.816393	2.881638	0.005654	0.707080
-29.316476	-1.887571	2.891635	0.005469	0.707293
-29.448870	-1.824298	2.901632	0.005493	0.707373
-28.992756	-1.904127	2.911629	0.005408	0.707376
-29.035803	-1.869238	2.921626	0.005416	0.707430
-28.382395	-1.852678	2.931622	0.005295	0.707697
-28.142061	-1.897082	2.941619	0.005250	0.707695
-28.353448	-1.858204	2.951616	0.005289	0.707697
-27.852999	-1.835919	2.961613	0.005196	0.707921
-27.356669	-1.879138	2.971610	0.005103	0.708012
-27.447761	-1.864352	2.981606	0.005120	0.708009
-27.260169	-1.864660	2.991603	0.005085	0.708076
-26.504687	-1.865068	3.001600	0.004944	0.708345
-26.280007	-1.903639	3.011597	0.004902	0.708348
-26.601923	-1.845764	3.021594	0.004962	0.708349
-26.104699	-1.844445	3.031590	0.004870	0.708529
-25.916455	-1.825139	3.041587	0.004834	0.708636
-25.704552	-1.863851	3.051584	0.004795	0.708634
-25.506568	-1.849707	3.061581	0.004758	0.708733
-24.698883	-1.882041	3.071578	0.004607	0.708957
-24.811966	-1.865096	3.081574	0.004628	0.708950
-24.813973	-1.863848	3.091571	0.004629	0.708952
-24.441927	-1.806632	3.101568	0.004559	0.709200
-23.952292	-1.863013	3.111565	0.004468	0.709262
-23.993627	-1.855498	3.121562	0.004476	0.709262
-23.620615	-1.848126	3.131558	0.004406	0.709410
-22.876446	-1.890278	3.141555	0.004267	0.709591
-23.150428	-1.840715	3.151552	0.004318	0.709593
-22.836410	-1.896882	3.161549	0.004260	0.709593
-22.492045	-1.837700	3.171546	0.004196	0.709834
-22.112739	-1.874817	3.181542	0.004125	0.709895
-22.273089	-1.848280	3.191539	0.004155	0.709891
-22.146855	-1.813552	3.201536	0.004131	0.710006
-20.985129	-1.915954	3.211533	0.003915	0.710215
-21.596093	-1.807277	3.221530	0.004028	0.710215
-21.390325	-1.844268	3.231526	0.003990	0.710214
-20.748874	-1.806499	3.241523	0.003870	0.710518
-20.512548	-1.843105	3.251520	0.003826	0.710529
-20.132307	-1.910522	3.261517	0.003755	0.710530
-20.279037	-1.801266	3.271514	0.003783	0.710696
-19.212321	-1.905137	3.281510	0.003584	0.710869
-19.431495	-1.866792	3.291507	0.003625	0.710868
-19.385534	-1.874089	3.301504	0.003616	0.710870
-18.664806	-1.909741	3.311501	0.003482	0.711055
-18.793131	-1.844550	3.321498	0.003506	0.711140
-18.612117	-1.877479	3.331494	0.003472	0.711138
-18.797464	-1.813088	3.341491	0.003506	0.711201
-17.864508	-1.854384	3.351488	0.003332	0.711451
-17.849219	-1.855353	3.361485	0.003329	0.711454
-17.861805	-1.852648	3.371482	0.003332	0.711455
-17.070851	-1.857066	3.381478	0.003184	0.711728
-17.134310	-1.829734	3.391475	0.003196	0.711760
-16.723593	-1.903359	3.401472	0.003119	0.711759
-16.780379	-1.824253	3.411469	0.003130	0.711897
-15.928667	-1.880624	3.421466	0.002971	0.712087
-15.919870	-1.883218	3.431462	0.002970	0.712085
-16.325907	-1.812601	3.441459	0.003045	0.712082
-15.390778	-1.835790	3.451456	0.002871	0.712368
-15.233199	-1.854224	3.461453	0.002841	0.712387
-15.182400	-1.865598	3.471450	0.002832	0.712383
-14.898751	-1.825426	3.481446	0.002779	0.712564
-14.509854	-1.823060	3.491443	0.002706	0.712707
-14.276840	-1.864664	3.501440	0.002663	0.712707
-14.525648	-1.790427	3.511437	0.002709	0.712766
-13.393252	-1.861179	3.521434	0.002498	0.713027
-13.587267	-1.827207	3.531430	0.002534	0.713026
-13.431123	-1.855821	3.541427	0.002505	0.713025
-12.916124	-1.834469	3.551424	0.002409	0.713250
-12.430104	-1.866737	3.561421	0.002319	0.713358
-12.332603	-1.884352	3.571418	0.002300	0.713358
-12.414007	-1.870091	3.581414	0.002315	0.713358
-12.067977	-1.802816	3.591411	0.002251	0.713614
-11.339567	-1.914835	3.601408	0.002115	0.713650
-11.383035	-1.905250	3.611405	0.002123	0.713654
-11.256515	-1.906887	3.621402	0.002100	0.713695
-10.689012	-1.869959	3.631398	0.001994	0.713970
-10.393724	-1.923126	3.641395	0.001939	0.713969
-10.420832	-1.917439	3.651392	0.001944	0.713971
-10.302694	-1.887996	3.661389	0.001922	0.714071
-9.317279	-1.959635	3.671386	0.001738	0.714278
-9.445531	-1.938367	3.681382	0.001762	0.714275
-9.581442	-1.913727	3.691379	0.001787	0.714276
-9.245667	-1.924137	3.701376	0.001724	0.714374
-8.738640	-1.898099	3.711373	0.001630	0.714605
-8.379271	-1.961067	3.721370	0.001563	0.714608
-8.767212	-1.892393	3.731366	0.001635	0.714607
-8.137081	-1.906398	3.741363	0.001518	0.714802
-7.915429	-1.893482	3.751360	0.001476	0.714906
-7.916726	-1.893613	3.761357	0.001476	0.714906
-7.699550	-1.904270	3.771354	0.001436	0.714962
-6.945513	-1.903065	3.781350	0.001295	0.715231
-6.748033	-1.937622	3.791347	0.001259	0.715232
-6.889174	-1.913509	3.801344	0.001285	0.715230
-6.595146	-1.887209	3.811341	0.001230	0.715386
-5.662866	-1.974471	3.821338	0.001056	0.715543
-5.989470	-1.916099	3.831334	0.001117	0.715543
-5.795254	-1.950389	3.841331	0.001081	0.715544
-5.218589	-1.921920	3.851328	0.000973	0.715805
-5.080801	-1.905974	3.861325	0.000947	0.715885
-4.939450	-1.929426	3.871322	0.000921	0.715889
-5.107150	-1.884139	3.881318	0.000952	0.715919
-4.310473	-1.919800	3.891315	0.000804	0.716130
-4.337536	-1.915105	3.901312	0.000809	0.716130
-4.176922	-1.941001	3.911309	0.000779	0.716135
-3.556567	-1.932904	3.921306	0.000663	0.716370
-3.448774	-1.913475	3.931302	0.000643	0.716447
-3.380988	-1.924530	3.941299	0.000630	0.716449
-3.461747	-1.862944	3.951296	0.000645	0.716543
-2.452220	-1.934047	3.961293	0.000457	0.716758
-2.579532	-1.910784	3.971290	0.000481	0.716760
-2.427041	-1.939099	3.981286	0.000452	0.716758
-1.960641	-1.879528	3.991283	0.000365	0.717040
-1.502380	-1.938171	4.001280	0.000280	0.717086
-1.709053	-1.902786	4.011277	0.000318	0.717083
-1.526729	-1.873082	4.021274	0.000284	0.717206
-1.014700	-1.876168	4.031270	0.000189	0.717381
-1.399658	-1.809227	4.041267	0.000260	0.717378
-1.144619	-1.792211	4.051264	0.000213	0.717501
-1.441731	-1.637416	4.061261	0.000268	0.717703
-1.090548	-1.692462	4.071258	0.000202	0.717718
-0.856245	-1.584032	4.081254	0.000159	0.718015
-0.984372	-1.561811	4.091251	0.000182	0.718014
-0.674815	-1.472698	4.101248	0.000125	0.718299
-0.605997	-1.458169	4.111245	0.000112	0.718352
-0.453813	-1.369739	4.121242	0.000083	0.718580
-0.415965	-1.345249	4.131238	0.000076	0.718642
-0.492749	-1.190247	4.141235	0.000090	0.718921
-0.517102	-1.136799	4.151232	0.000095	0.719018
-0.372963	-1.033631	4.161229	0.000068	0.719272
-0.229295	-0.957645	4.171226	0.000041	0.719473
-0.243622	-0.873436	4.181222	0.000043	0.719634
-0.201611	-0.747922	4.191219	0.000035	0.719896
-0.337965	-0.606744	4.201216	0.000060	0.720127
-0.160448	-0.528369	4.211213	0.000027	0.720343
-0.218419	-0.396273	4.221210	0.000038	0.720583
-0.012507	-0.284281	4.231206	-0.000001	0.720876
0.080722	-0.190184	4.241203	-0.000018	0.721094
-0.064492	-0.037219	4.251200	0.000009	0.721344
-0.087428	0.106458	4.261197	0.000013	0.721619
0.000000	0.256984	4.271194	-0.000004	0.721945

0.054617	0.885144	4.276198	-0.000014	0.723198
0.160600	2.128596	4.281203	-0.000035	0.725669
0.400033	3.946009	4.286208	-0.000081	0.729296
0.501780	6.329565	4.291213	-0.000101	0.733953
0.838293	9.190507	4.296218	-0.000166	0.739576
1.284562	12.507895	4.301222	-0.000251	0.746062
1.598425	16.301976	4.306227	-0.000312	0.753346
1.986112	20.494935	4.311232	-0.000387	0.761328
2.281044	25.092521	4.316237	-0.000445	0.769943
2.971256	30.002110	4.321242	-0.000577	0.779158
3.299771	35.318567	4.326246	-0.000641	0.788881
3.450654	40.977766	4.331251	-0.000673	0.799039
4.173357	46.848394	4.336256	-0.000812	0.809616
4.804059	53.009148	4.341261	-0.000933	0.820531
5.144513	59.505760	4.346266	-0.001001	0.831787
6.582010	66.027193	4.351270	-0.001273	0.843260
9.319195	72.583876	4.356275	-0.001787	0.855017
9.797718	79.755690	4.361280	-0.001881	0.866969
10.252963	87.110147	4.366285	-0.001970	0.879046
11.463469	94.510135	4.371290	-0.002200	0.891242
12.556520	102.101892	4.376294	-0.002409	0.903542
13.219507	109.911569	4.381299	-0.002538	0.915897
14.315278	117.771429	4.386304	-0.002747	0.928279
15.220965	125.786422	4.391309	-0.002921	0.940681
16.042096	133.929661	4.396314	-0.003079	0.953091
16.886375	142.149210	4.401318	-0.003242	0.965458
17.697665	150.454371	4.406323	-0.003398	0.977784
18.290431	158.881656	4.411328	-0.003514	0.990076
19.155948	167.280429	4.416333	-0.003681	1.002245
20.355440	175.679795	4.421338	-0.003910	1.014348
21.109562	184.199155	4.426342	-0.004056	1.026367
21.676850	192.787329	4.431347	-0.004167	1.038297
22.735445	201.321984	4.436352	-0.004370	1.050133
23.276585	209.962958	4.441357	-0.004476	1.061859
23.844178	218.638850	4.446362	-0.004587	1.073509
24.617187	227.256114	4.451366	-0.004737	1.085003
25.227253	235.921153	4.456371	-0.004856	1.096401
25.837151	244.583489	4.461376	-0.004975	1.107679
26.826074	253.183010	4.466381	-0.005165	1.118845
27.877523	261.783168	4.471386	-0.005367	1.129915
28.184302	270.510383	4.476390	-0.005430	1.140876
28.840399	279.184618	4.481395	-0.005557	1.151741
29.465422	287.839812	4.486400	-0.005679	1.162474
30.129510	296.453738	4.491405	-0.005809	1.173067
30.938583	305.042550	4.496410	-0.005965	1.183565
31.621740	313.654842	4.501414	-0.006098	1.193972
32.529837	322.195548	4.506419	-0.006273	1.204249
33.056539	330.815739	4.511424	-0.006376	1.214457
33.694786	339.378185	4.516429	-0.006501	1.224534
34.170830	347.992061	4.521434	-0.006595	1.234556
35.189026	356.466163	4.526438	-0.006790	1.244442
35.785206	365.007889	4.531443	-0.006907	1.254246
36.360192	373.547625	4.536448	-0.007020	1.263967
37.020447	382.052577	4.541453	-0.007148	1.273591
37.887773	390.509058	4.546458	-0.007315	1.283127
38.538560	399.005089	4.551462	-0.007442	1.292596
39.068550	407.484942	4.556467	-0.007546	1.301957
39.806895	416.014484	4.561472	-0.007689	1.311341
40.195497	424.542642	4.566477	-0.007767	1.320595
40.922554	432.939140	4.571482	-0.007908	1.329703
41.674070	441.336948	4.576486	-0.008054	1.338755
42.014314	449.774901	4.581491	-0.008122	1.347716
42.718430	458.174664	4.586496	-0.008259	1.356642
43.018777	466.586760	4.591501	-0.008321	1.365451
43.423029	475.001647	4.596506	-0.008401	1.374225
43.842759	483.380857	4.601510	-0.008485	1.382909
44.546461	491.717264	4.606515	-0.008622	1.391542
45.171315	500.060575	4.611520	-0.008743	1.400117
45.456180	508.428235	4.616525	-0.008802	1.408606
46.108228	516.752737	4.621530	-0.008929	1.417062
46.691878	525.066255	4.626534	-0.009043	1.425446
47.141831	533.407143	4.631539	-0.009132	1.433785
47.499645	541.746878	4.636544	-0.009204	1.442060
48.075339	550.038194	4.641549	-0.009317	1.450276
48.630879	558.354353	4.646554	-0.009426	1.458465
49.046164	566.662749	4.651558	-0.009509	1.466580
49.377685	575.031374	4.656563	-0.009576	1.474693
50.055067	583.278209	4.661568	-0.009707	1.482701
50.462190	591.552055	4.666573	-0.009789	1.490648
51.029749	599.818358	4.671578	-0.009900	1.498571
51.671782	608.049661	4.676582	-0.010025	1.506430
52.059555	616.340421	4.681587	-0.010102	1.514266
52.252484	624.644349	4.686592	-0.010144	1.522043
52.628712	632.898721	4.691597	-0.010219	1.529763
53.678859	641.073005	4.696602	-0.010420	1.537471
53.998136	649.344185	4.701606	-0.010485	1.545120
54.526134	657.611020	4.706611	-0.010589	1.552758
55.176046	665.826287	4.711616	-0.010715	1.560330
55.639467	674.056799	4.716621	-0.010807	1.567851
56.099435	682.312380	4.721626	-0.010898	1.575358
56.659342	690.523980	4.726630	-0.011008	1.582805
57.347586	698.710138	4.731635	-0.011141	1.590212
57.947930	706.940829	4.736640	-0.011258	1.597612
58.328544	715.155681	4.741645	-0.011335	1.604932
58.898070	723.379475	4.746650	-0.011446	1.612253
59.181127	731.631194	4.751654	-0.011504	1.619525
59.465594	739.854351	4.756659	-0.011563	1.626740
60.050081	748.109130	4.761664	-0.011677	1.633992
60.338146	756.310212	4.766669	-0.011736	1.641125
60.666986	764.511775	4.771674	-0.011802	1.648232
61.179564	772.703662	4.776678	-0.011903	1.655326
61.741664	780.853976	4.781683	-0.012013	1.662360
62.059849	789.074888	4.786688	-0.012078	1.669392
62.089877	797.318902	4.791693	-0.012089	1.676375
62.468042	805.485819	4.796698	-0.012165	1.683311
62.970929	813.644216	4.801702	-0.012264	1.690227
63.389986	821.816176	4.806707	-0.012347	1.697115
63.892309	829.983698	4.811712	-0.012446	1.703983
64.233523	838.170900	4.816717	-0.012515	1.710818
64.255735	846.415702	4.821722	-0.012524	1.717631
64.817084	854.528717	4.826726	-0.012634	1.724380
65.296401	862.677271	4.831731	-0.012729	1.731120
65.578080	870.881055	4.836736	-0.012787	1.737854
65.851256	879.040235	4.841741	-0.012843	1.744524
66.427892	887.177698	4.846746	-0.012956	1.751190
66.916501	895.345222	4.851750	-0.013052	1.757843
67.426318	903.469711	4.856755	-0.013152	1.764439
67.761118	911.657489	4.861760	-0.013220	1.771039
68.011066	919.828826	4.866765	-0.013272	1.777591
68.496450	927.969216	4.871770	-0.013368	1.784124
68.944458	936.151869	4.876774	-0.013456	1.790661
69.150026	944.357105	4.881779	-0.013500	1.797162
69.471157	952.492269	4.886784	-0.013565	1.803599
70.256465	960.539163	4.891789	-0.013717	1.810000
70.823331	968.666675	4.896794	-0.013828	1.816415
71.307374	976.797071	4.901798	-0.013923	1.822799
71.637008	984.941320	4.906803	-0.013990	1.829153
72.006388	993.120460	4.911808	-0.014064	1.835517
72.304358	1001.258102	4.916813	-0.014125	1.841819
73.054785	1009.341860	4.921818	-0.014270	1.848110
73.436625	1017.518140	4.926822	-0.014346	1.854408
74.030213	1025.610176	4.931827	-0.014462	1.860644
74.477567	1033.760518	4.936832	-0.014551	1.866887
74.511432	1041.976706	4.941837	-0.014563	1.873111
74.938669	1050.098147	4.946842	-0.014647	1.879288
75.181903	1058.226919	4.951846	-0.014698	1.885430
75.394472	1066.374171	4.956851	-0.014743	1.891561
75.995764	1074.484651	4.961856	-0.014860	1.897690
76.275713	1082.589402	4.966861	-0.014918	1.903758
76.575452	1090.732660	4.971866	-0.014979	1.909837
76.856019	1098.881605	4.976870	-0.015037	1.915899
77.098150	1106.988684	4.981875	-0.015087	1.921907
77.903613	1115.057635	4.986880	-0.015242	1.927930
78.059814	1123.224354	4.991885	-0.015277	1.933934
78.493749	1131.325832	4.996890	-0.015363	1.939903
78.933210	1139.435304	5.001894	-0.015450	1.945859
79.005597	1147.629853	5.006899	-0.015469	1.951819
79.272339	1155.771180	5.011904	-0.015524	1.957743
79.511329	1163.858633	5.016909	-0.015574	1.963608
80.007661	1171.930281	5.021914	-0.015671	1.969471
80.171988	1180.078822	5.026918	-0.015707	1.975336
80.688546	1188.139360	5.031923	-0.015809	1.981159
80.957552	1196.268156	5.036928	-0.015864	1.986987
81.253425	1204.377948	5.041933	-0.015925	1.992787
81.622838	1212.476467	5.046938	-0.015999	1.998569
81.956694	1220.570884	5.051942	-0.016066	2.004329
82.142073	1228.688923	5.056947	-0.016106	2.010072
82.559898	1236.806867	5.061952	-0.016189	2.015824
82.915755	1244.880369	5.066957	-0.016261	2.021521
83.362442	1252.968701	5.071962	-0.016349	2.027223
83.493935	1261.147697	5.076966	-0.016379	2.032938
83.752189	1269.230683	5.081971	-0.016433	2.038584
84.055150	1277.315983	5.086976	-0.016494	2.044221
84.359756	1285.404627	5.091981	-0.016556	2.049844
84.449195	1293.549543	5.096986	-0.016578	2.055469
84.891798	1301.620393	5.101990	-0.016666	2.061063
85.043787	1309.719770	5.106995	-0.016700	2.066633
85.621401	1317.802327	5.112000	-0.016813	2.072218
85.991907	1325.882350	5.117005	-0.016887	2.077766
86.318385	1333.970233	5.122010	-0.016953	2.083300
86.679561	1342.069553	5.127014	-0.017026	2.088830
87.189871	1350.156052	5.132019	-0.017126	2.094351
87.496402	1358.259799	5.137024	-0.017188	2.099850
87.555679	1366.386468	5.142029	-0.017205	2.105326
88.016515	1374.485382	5.147034	-0.017296	2.110807
88.509208	1382.601357	5.152038	-0.017393	2.116289
88.632245	1390.658898	5.157043	-0.017421	2.121682
88.851267	1398.753263	5.162048	-0.017467	2.127095
89.312720	1406.822045	5.167053	-0.017558	2.132500
89.753088	1414.883799	5.172058	-0.017646	2.137885
89.955631	1422.997022	5.177062	-0.017689	2.143268
90.029388	1431.103270	5.182067	-0.017708	2.148620
90.444218	1439.200987	5.187072	-0.017790	2.153985
90.659832	1447.281214	5.192077	-0.017836	2.159307
90.905109	1455.342457	5.197082	-0.017887	2.164606
91.242148	1463.446491	5.202086	-0.017955	2.169929
91.432383	1471.539495	5.207091	-0.017996	2.175218
91.659617	1479.637956	5.212096	-0.018043	2.180500
91.842867	1487.716904	5.217101	-0.018083	2.185754
92.178598	1495.810762	5.222106	-0.018150	2.191018
92.516622	1503.915785	5.227110	-0.018219	2.196277
92.771974	1511.956239	5.232115	-0.018272	2.201474
93.418993	1519.994003	5.237120	-0.018397	2.206692
93.511392	1528.105238	5.242125	-0.018420	2.211896
93.786405	1536.196516	5.247130	-0.018476	2.217090
94.171171	1544.251605	5.252134	-0.018553	2.222259
94.390686	1552.334420	5.257139	-0.018600	2.227419
94.714052	1560.426283	5.262144	-0.018665	2.232582
95.141121	1568.481389	5.267149	-0.018750	2.237719
95.346382	1576.538546	5.272154	-0.018793	2.242825
95.941426	1584.598303	5.277158	-0.018909	2.247956
96.259329	1592.688416	5.282163	-0.018974	2.253070
96.645600	1600.770200	5.287168	-0.019051	2.258173
96.845412	1608.849501	5.292173	-0.019094	2.263247
97.208197	1616.923483	5.297178	-0.019167	2.268320
97.585228	1625.089088	5.302182	-0.019242	2.273439
97.845304	1633.136449	5.307187	-0.019296	2.278464
98.011373	1641.208201	5.312192	-0.019332	2.283485
98.457289	1649.232740	5.317197	-0.019420	2.288489
99.105625	1657.277912	5.322202	-0.019546	2.293512
99.796584	1665.312246	5.327206	-0.019680	2.298521
100.482078	1673.326966	5.332211	-0.019813	2.303506
101.003263	1681.407029	5.337216	-0.019916	2.308507
101.155708	1689.535305	5.342221	-0.019949	2.313495
101.239615	1697.631004	5.347226	-0.019970	2.318447
101.801475	1705.665495	5.352230	-0.020080	2.323391
102.280214	1713.709558	5.357235	-0.020175	2.328323
102.324545	1721.877017	5.362240	-0.020188	2.333284
102.588386	1729.941492	5.367245	-0.020243	2.338190
103.406917	1737.923753	5.372250	-0.020400	2.343081
103.905194	1746.012531	5.377254	-0.020498	2.348000
104.023008	1754.136362	5.382259	-0.020526	2.352898
104.453667	1762.200586	5.387264	-0.020611	2.357776
104.666190	1770.267708	5.392269	-0.020656	2.362628
104.869450	1778.335049	5.397274	-0.020699	2.367470
105.224806	1786.424504	5.402278	-0.020771	2.372326
105.470070	1794.472646	5.407283	-0.020822	2.377140
105.643690	1802.567392	5.412288	-0.020859	2.381965
105.775667	1810.639742	5.417293	-0.020889	2.386764
106.205530	1818.688323	5.422298	-0.020975	2.391563
106.365942	1826.795180	5.427302	-0.021010	2.396366
106.510777	1834.825889	5.432307	-0.021042	2.401112
107.002709	1842.854243	5.437312	-0.021139	2.405875
107.255826	1850.925016	5.442317	-0.021191	2.410635
107.390208	1859.023155	5.447322	-0.021222	2.415392
107.479342	1867.105429	5.452326	-0.021244	2.420127
107.926848	1875.111453	5.457331	-0.021332	2.424836
108.159139	1883.189147	5.462336	-0.021381	2.429561
108.597492	1891.323499	5.467341	-0.021468	2.434325
108.988126	1899.326391	5.472346	-0.021546	2.439001
109.572845	1907.353067	5.477350	-0.021660	2.443695
109.901119	1915.393600	5.482355	-0.021726	2.448369
110.246440	1923.474017	5.487360	-0.021796	2.453058
110.582199	1931.518753	5.492365	-0.021864	2.457717
110.670573	1939.586345	5.497370	-0.021885	2.462362
110.923596	1947.663246	5.502374	-0.021938	2.467015
111.126658	1955.738624	5.507379	-0.021981	2.471655
111.565653	1963.786558	5.512384	-0.022068	2.476289
111.801838	1971.837073	5.517389	-0.022117	2.480900
111.921567	1979.905777	5.522394	-0.022145	2.485504
112.271229	1987.971806	5.527398	-0.022215	2.490114
112.340537	1996.055995	5.532403	-0.022233	2.494706
112.613571	2004.102311	5.537408	-0.022290	2.499283
112.751202	2012.163073	5.542413	-0.022320	2.503850
113.172725	2020.195410	5.547418	-0.022404	2.508413
113.418963	2028.307926	5.552422	-0.022455	2.513001
113.705473	2036.332709	5.557427	-0.022514	2.517533
113.996671	2044.373211	5.562432	-0.022574	2.522066
114.081386	2052.458727	5.567437	-0.022595	2.526602
114.392810	2060.483733	5.572442	-0.022658	2.531111
114.905285	2068.537323	5.577446	-0.022759	2.535643
115.095976	2076.584152	5.582451	-0.022799	2.540140
115.353169	2084.624541	5.587456	-0.022853	2.544631
115.616170	2092.704450	5.592461	-0.022907	2.549135
115.585041	2100.803459	5.597466	-0.022906	2.553622
116.001482	2108.832018	5.602470	-0.022989	2.558093
116.334974	2116.850589	5.607475	-0.023057	2.562545
116.614809	2124.915318	5.612480	-0.023114	2.567010
116.814365	2132.996734	5.617485	-0.023156	2.571472
116.946335	2141.076658	5.622490	-0.023186	2.575920
117.225470	2149.112818	5.627494	-0.023244	2.580347
117.246554	2157.163115	5.632499	-0.023253	2.584756
117.377429	2165.241713	5.637504	-0.023283	2.589180
117.773860	2173.440711	5.642509	-0.023362	2.593681
118.144786	2181.445418	5.647514	-0.023436	2.598066
118.287373	2189.467379	5.652518	-0.023468	2.602438
118.706404	2197.425886	5.657523	-0.023551	2.606787
118.851860	2205.481270	5.662528	-0.023584	2.611162
119.054786	2213.513380	5.667533	-0.023627	2.615521
119.183383	2221.561296	5.672538	-0.023656	2.619877
119.514238	2229.596200	5.677542	-0.023723	2.624231
119.865352	2237.625319	5.682547	-0.023793	2.628577
120.096048	2245.701992	5.687552	-0.023842	2.632933
120.341439	2253.745826	5.692557	-0.023893	2.637265
120.840000	2261.732811	5.697562	-0.023991	2.641576
121.262003	2269.792798	5.702566	-0.024075	2.645914
121.575659	2277.827767	5.707571	-0.024138	2.650225
121.776105	2285.924459	5.712576	-0.024181	2.654554
122.082755	2293.962502	5.717581	-0.024243	2.658851
122.414495	2301.987741	5.722586	-0.024310	2.663136
123.016226	2310.023251	5.727590	-0.024428	2.667437
123.112886	2318.124101	5.732595	-0.024451	2.671734
123.225294	2326.216641	5.737600	-0.024477	2.676020
123.462057	2334.236712	5.742605	-0.024527	2.680268
123.543253	2342.264778	5.747610	-0.024547	2.684505
123.724282	2350.321419	5.752614	-0.024586	2.688755
123.923555	2358.371476	5.757619	-0.024628	2.692997
124.343307	2366.408379	5.762624	-0.024712	2.697239
124.749002	2374.441981	5.767629	-0.024793	2.701472
124.762854	2382.485293	5.772634	-0.024800	2.705679
125.153968	2390.530614	5.777638	-0.024879	2.709904
125.308470	2398.599068	5.782643	-0.024913	2.714119
125.711603	2406.616228	5.787648	-0.024993	2.718316
125.908565	2414.660398	5.792653	-0.025035	2.722509
126.071788	2422.714484	5.797658	-0.025071	2.726697
126.632721	2430.748233	5.802662	-0.025180	2.730894
126.548644	2438.851319	5.807667	-0.025170	2.735080
127.082054	2446.855470	5.812672	-0.025275	2.739246
127.277899	2454.889649	5.817677	-0.025316	2.743401
127.292088	2462.956375	5.822682	-0.025324	2.747555
127.734008	2471.048082	5.827686	-0.025412	2.751742
128.028233	2479.118027	5.832691	-0.025472	2.755902
128.004547	2487.160294	5.837696	-0.025473	2.760022
128.386118	2495.143812	5.842701	-0.025549	2.764131
128.501259	2503.185323	5.847706	-0.025576	2.768247
128.727297	2511.271829	5.852710	-0.025623	2.772386
128.976408	2519.304698	5.857715	-0.025675	2.776493
129.628496	2527.301400	5.862720	-0.025802	2.780600
129.409487	2535.358789	5.867725	-0.025766	2.784680
129.653877	2543.393131	5.872730	-0.025817	2.788769
130.092378	2551.466246	5.877734	-0.025904	2.792884
130.314870	2559.499310	5.882739	-0.025951	2.796959
130.437057	2567.529834	5.887744	-0.025979	2.801022
130.737564	2575.556468	5.892749	-0.026040	2.805087
131.079033	2583.564139	5.897754	-0.026109	2.809138
131.534101	2591.630780	5.902758	-0.026199	2.813220
131.441416	2599.696997	5.907763	-0.026187	2.817265
131.754917	2607.735054	5.912768	-0.026250	2.821312
132.138062	2615.766881	5.917773	-0.026327	2.825355
132.414963	2623.797569	5.922778	-0.026384	2.829385
132.654475	2631.900464	5.927782	-0.026434	2.833443
132.607792	2639.941146	5.932787	-0.026430	2.837449
132.854109	2647.967402	5.937792	-0.026482	2.841458
133.339661	2655.962277	5.942797	-0.026577	2.845459
133.624216	2663.980746	5.947802	-0.026635	2.849455
133.581406	2672.097448	5.952806	-0.026633	2.853475
133.800644	2680.101949	5.957811	-0.026679	2.857449
134.059657	2688.146109	5.962816	-0.026732	2.861439
134.438683	2696.160928	5.967821	-0.026808	2.865416
134.599396	2704.217316	5.972826	-0.026844	2.869396
134.706629	2712.321448	5.977830	-0.026869	2.873390
134.974672	2720.326761	5.982835	-0.026924	2.877340
135.190768	2728.375762	5.987840	-0.026969	2.881302
135.274425	2736.404207	5.992845	-0.026990	2.885242
135.346495	2744.438586	5.997850	-0.027009	2.889178
135.530957	2752.517498	6.002854	-0.027049	2.893137
135.793155	2760.534958	6.007859	-0.027103	2.897065
135.963164	2768.585194	6.012864	-0.027140	2.900999
136.155909	2776.602868	6.017869	-0.027181	2.904912
136.269770	2784.647240	6.022874	-0.027207	2.908829
136.631886	2792.754972	6.027878	-0.027280	2.912784
136.987384	2800.770268	6.032883	-0.027352	2.916689
136.894415	2808.808949	6.037888	-0.027340	2.920577
137.189697	2816.782808	6.042893	-0.027400	2.924448
137.587732	2824.782038	6.047898	-0.027479	2.928332
137.765655	2832.876386	6.052902	-0.027518	2.932245
137.797560	2840.919071	6.057907	-0.027529	2.936120
138.298989	2848.902492	6.062912	-0.027627	2.939986
138.398359	2856.955314	6.067917	-0.027651	2.943859
138.328296	2865.002651	6.072922	-0.027644	2.947715
138.640179	2873.083730	6.077926	-0.027707	2.951603
139.080831	2881.081413	6.082931	-0.027794	2.955452
139.455088	2889.085153	6.087936	-0.027869	2.959295
139.486196	2897.149526	6.092941	-0.027880	2.963145
139.781618	2905.177006	6.097946	-0.027941	2.966986
139.966562	2913.245278	6.102950	-0.027980	2.970835
140.177599	2921.283864	6.107955	-0.028025	2.974667
140.463599	2929.308472	6.112960	-0.028083	2.978491
140.567375	2937.363642	6.117965	-0.028108	2.982315
140.734275	2945.377628	6.122970	-0.028144	2.986118
141.091980	2953.428557	6.127974	-0.028216	2.989943
141.445912	2961.494362	6.132979	-0.028287	2.993770
141.626954	2969.510165	6.137984	-0.028326	2.997560
141.716921	2977.554459	6.142989	-0.028348	3.001353
142.121322	2985.538638	6.147994	-0.028429	3.005130
142.586773	2993.580505	6.152998	-0.028521	3.008932
142.625453	3001.633702	6.158003	-0.028533	3.012713
142.877152	3009.675368	6.163008	-0.028586	3.016494
143.448251	3017.645106	6.168013	-0.028697	3.020253
143.403246	3025.704157	6.173018	-0.028694	3.024018
143.507795	3033.796443	6.178022	-0.028719	3.027802
143.809139	3041.816127	6.183027	-0.028780	3.031556
144.036723	3049.883763	6.188032	-0.028828	3.035325
144.250805	3057.913256	6.193037	-0.028873	3.039070
144.342102	3065.918417	6.198042	-0.028895	3.042794
144.760538	3073.949454	6.203046	-0.028979	3.046540
144.758703	3081.987434	6.208051	-0.028983	3.050266
144.870702	3090.054574	6.213056	-0.029010	3.054005
145.420448	3098.050880	6.218061	-0.029117	3.057728
145.638974	3106.068185	6.223066	-0.029163	3.061440
145.837334	3114.117049	6.228070	-0.029205	3.065162
145.933891	3122.157719	6.233075	-0.029229	3.068870
146.322436	3130.225932	6.238080	-0.029306	3.072600
146.339046	3138.319572	6.243085	-0.029315	3.076320
146.376572	3146.301786	6.248090	-0.029327	3.079985
146.979227	3154.279176	6.253094	-0.029444	3.083670
147.035210	3162.328558	6.258099	-0.029460	3.087358
147.373565	3170.350206	6.263104	-0.029528	3.091042
147.683681	3178.415910	6.268109	-0.029591	3.094741
147.996762	3186.413069	6.273114	-0.029655	3.098403
148.183763	3194.462680	6.278118	-0.029695	3.102080
148.197253	3202.493343	6.283123	-0.029703	3.105735
148.521734	3210.507877	6.288128	-0.029769	3.109394
148.935004	3218.589207	6.293133	-0.029851	3.113082
149.072932	3226.602377	6.298138	-0.029882	3.116722
149.474505	3234.597400	6.303142	-0.029962	3.120361
149.816065	3242.586520	6.308147	-0.030031	3.123991
150.037258	3250.661318	6.313152	-0.030077	3.127650
150.263174	3258.726540	6.318157	-0.030125	3.131301
150.415383	3266.761450	6.323162	-0.030158	3.134930
150.677188	3274.779011	6.328166	-0.030212	3.138552
150.773650	3282.816663	6.333171	-0.030235	3.142172
150.970612	3290.841964	6.338176	-0.030277	3.145786
151.209066	3298.884373	6.343181	-0.030327	3.149406
151.143618	3306.967935	6.348186	-0.030320	3.153027
151.320284	3315.028790	6.353190	-0.030358	3.156643
151.684470	3322.979464	6.358195	-0.030431	3.160215
151.789731	3331.010611	6.363200	-0.030456	3.163807
152.132029	3339.020977	6.368205	-0.030525	3.167396
152.222840	3347.056515	6.373210	-0.030548	3.170982
152.403056	3355.139584	6.378214	-0.030586	3.174588
152.600968	3363.159288	6.383219	-0.030629	3.178162
152.871936	3371.171259	6.388224	-0.030684	3.181733
153.189834	3379.199135	6.393229	-0.030749	3.185308
153.297361	3387.215451	6.398234	-0.030774	3.188865
153.817767	3395.286016	6.403238	-0.030876	3.192460
154.020556	3403.338295	6.408243	-0.030919	3.196029
154.281164	3411.323457	6.413248	-0.030973	3.199567
154.488352	3419.376475	6.418253	-0.031017	3.203129
154.700420	3427.375019	6.423258	-0.031062	3.206662
155.082509	3435.394096	6.428262	-0.031138	3.210208
155.086621	3443.465715	6.433267	-0.031144	3.213758
155.356290	3451.474324	6.438272	-0.031200	3.217286
155.627936	3459.513038	6.443277	-0.031255	3.220825
155.885003	3467.514346	6.448282	-0.031309	3.224342
156.198009	3475.562815	6.453286	-0.031372	3.227878
156.340314	3483.624068	6.458291	-0.031404	3.231409
156.866817	3491.670572	6.463296	-0.031507	3.234945
157.287483	3499.670843	6.468301	-0.031591	3.238453
157.444269	3507.677971	6.473306	-0.031625	3.241950
157.539402	3515.717472	6.478310	-0.031648	3.245454
157.511509	3523.737580	6.483315	-0.031648	3.248941
158.093102	3531.748205	6.488320	-0.031762	3.252444
158.343982	3539.829141	6.493325	-0.031814	3.255961
158.382441	3547.814511	6.498330	-0.031826	3.259424
158.656042	3555.874858	6.503334	-0.031883	3.262926
158.938190	3563.881120	6.508339	-0.031940	3.266400
159.227244	3571.912770	6.513344	-0.032000	3.269882
159.265050	3580.002055	6.518349	-0.032012	3.273375
159.376232	3588.007133	6.523354	-0.032038	3.276832
159.693068	3596.042692	6.528358	-0.032102	3.280305
159.620774	3604.050257	6.533363	-0.032094	3.283748
159.947983	3612.067928	6.538368	-0.032160	3.287207
160.090709	3620.117372	6.543373	-0.032192	3.290668
160.260394	3628.162750	6.548378	-0.032229	3.294126
160.521100	3636.209965	6.553382	-0.032283	3.297583
160.840316	3644.209439	6.558387	-0.032347	3.301020
160.893622	3652.196586	6.563392	-0.032363	3.304437
161.043434	3660.272657	6.568397	-0.032396	3.307892
161.358553	3668.286184	6.573402	-0.032460	3.311323
161.642606	3676.350513	6.578406	-0.032518	3.314771
161.817393	3684.345751	6.583411	-0.032556	3.318182
162.041967	3692.360332	6.588416	-0.032603	3.321599
162.486734	3700.353586	6.593421	-0.032691	3.325012
162.365787	3708.395446	6.598426	-0.032674	3.328421
162.527980	3716.478121	6.603430	-0.032709	3.331854
162.671327	3724.511135	6.608435	-0.032741	3.335262
162.854394	3732.524612	6.613440	-0.032780	3.338660
162.977837	3740.570756	6.618445	-0.032809	3.342065
163.200700	3748.527766	6.623450	-0.032855	3.345434
163.642862	3756.580506	6.628454	-0.032943	3.348847
163.656725	3764.650588	6.633459	-0.032951	3.352248
163.981086	3772.676839	6.638464	-0.033017	3.355639
164.246696	3780.692665	6.643469	-0.033071	3.359020
164.404120	3788.704442	6.648474	-0.033106	3.362392
164.623565	3796.762187	6.653478	-0.033152	3.365782
164.769347	3804.762210	6.658483	-0.033185	3.369141
164.834490	3812.818194	6.663488	-0.033202	3.372518
165.060589	3820.890972	6.668493	-0.033249	3.375904
165.217868	3828.854529	6.673498	-0.033284	3.379239
165.619030	3836.880894	6.678502	-0.033364	3.382605
165.469914	3844.932063	6.683507	-0.033341	3.385959
165.904227	3852.940400	6.688512	-0.033428	3.389312
166.207707	3861.049672	6.693517	-0.033489	3.392699
166.364528	3869.084151	6.698522	-0.033524	3.396046
166.374848	3877.077282	6.703526	-0.033531	3.399368
166.751381	3885.040841	6.708531	-0.033606	3.402687
166.909744	3893.038850	6.713536	-0.033641	3.406009
167.080598	3901.072358	6.718541	-0.033678	3.409344
167.048645	3909.126134	6.723546	-0.033678	3.412676
167.497584	3917.158503	6.728550	-0.033766	3.416013
167.602310	3925.144225	6.733555	-0.033791	3.419315
167.769985	3933.187782	6.738560	-0.033828	3.422641
168.204845	3941.215750	6.743565	-0.033914	3.425965
168.282828	3949.199877	6.748570	-0.033934	3.429256
168.627000	3957.262528	6.753574	-0.034003	3.432586
168.772605	3965.312926	6.758579	-0.034035	3.435900
169.083579	3973.316626	6.763584	-0.034099	3.439198
169.025451	3981.382529	6.768589	-0.034093	3.442505
169.181592	3989.375542	6.773594	-0.034127	3.445787
169.530862	3997.385037	6.778598	-0.034198	3.449078
169.493630	4005.468670	6.783603	-0.034196	3.452384
169.853997	4013.473767	6.788608	-0.034268	3.455668
170.524454	4021.469394	6.793613	-0.034399	3.458954
170.569897	4029.517669	6.798618	-0.034412	3.462239
170.516925	4037.592213	6.803622	-0.034408	3.465528
170.618387	4045.593820	6.808627	-0.034432	3.468789
170.991914	4053.637423	6.813632	-0.034507	3.472073
171.152138	4061.706517	6.818637	-0.034542	3.475358
171.244591	4069.673292	6.823642	-0.034564	3.478595
171.557925	4077.684000	6.828646	-0.034628	3.481855
171.641844	4085.678816	6.833651	-0.034649	3.485097
171.840123	4093.702225	6.838656	-0.034691	3.488352
172.046363	4101.764263	6.843661	-0.034735	3.491619
172.495219	4109.771702	6.848666	-0.034824	3.494869
172.722976	4117.812564	6.853670	-0.034871	3.498123
172.792951	4125.812896	6.858675	-0.034890	3.501352
173.050180	4133.827825	6.863680	-0.034943	3.504590
173.349752	4141.867185	6.868685	-0.035004	3.507836
173.453551	4149.863246	6.873690	-0.035028	3.511055
173.783377	4157.948784	6.878694	-0.035095	3.514314
173.758510	4165.972764	6.883699	-0.035096	3.517535
174.005995	4173.972323	6.888704	-0.035147	3.520751
174.184780	4181.981450	6.893709	-0.035186	3.523966
174.499060	4189.987651	6.898714	-0.035249	3.527182
174.575356	4198.049858	6.903718	-0.035269	3.530409
174.662015	4206.103849	6.908723	-0.035290	3.533630
175.042506	4214.122667	6.913728	-0.035366	3.536843
175.154778	4222.179378	6.918733	-0.035393	3.540060
174.962548	4230.164511	6.923738	-0.035362	3.543237
175.235229	4238.229294	6.928742	-0.035418	3.546456
175.550007	4246.235574	6.933747	-0.035482	3.549651
175.890696	4254.331370	6.938752	-0.035551	3.552879
176.190247	4262.384269	6.943757	-0.035612	3.556085
176.286232	4270.284926	6.948762	-0.035635	3.559223
176.586561	4278.328756	6.953766	-0.035696	3.562420
176.826265	4286.335537	6.958771	-0.035746	3.565598
177.036036	4294.339153	6.963776	-0.035790	3.568771
177.353893	4302.405258	6.968781	-0.035855	3.571969
177.548992	4310.416570	6.973786	-0.035896	3.575138
177.729037	4318.440145	6.978790	-0.035935	3.578310
177.868514	4326.485769	6.983795	-0.035967	3.581486
177.887177	4334.456998	6.988800	-0.035975	3.584626
178.117603	4342.528600	6.993805	-0.036023	3.587809
178.177734	4350.545927	6.998810	-0.036040	3.590963
178.447912	4358.577445	7.003814	-0.036096	3.594126
178.834504	4366.560046	7.008819	-0.036173	3.597270
178.924527	4374.562333	7.013824	-0.036195	3.600411
179.159248	4382.597171	7.018829	-0.036244	3.603566
179.300975	4390.613887	7.023834	-0.036275	3.606708
179.557114	4398.629522	7.028838	-0.036328	3.609851
179.829932	4406.663069	7.033843	-0.036384	3.612998
180.012029	4414.710172	7.038848	-0.036424	3.616145
180.149515	4422.729893	7.043853	-0.036455	3.619277
180.026181	4430.754155	7.048858	-0.036437	3.622401
180.430325	4438.789172	7.053862	-0.036517	3.625541
180.588343	4446.814860	7.058867	-0.036552	3.628668
180.878476	4454.837522	7.063872	-0.036611	3.631795
181.115662	4462.923994	7.068877	-0.036661	3.634942
181.119356	4470.897781	7.073882	-0.036667	3.638037
181.349023	4478.950525	7.078886	-0.036715	3.641165
181.540070	4486.914612	7.083891	-0.036756	3.644256
181.783811	4494.943249	7.088896	-0.036806	3.647370
181.870442	4503.009031	7.093901	-0.036828	3.650492
181.995200	4511.027423	7.098906	-0.036856	3.653593
182.248841	4519.068165	7.103910	-0.036909	3.656704
182.344795	4527.060214	7.108915	-0.036932	3.659790
182.717971	4535.080762	7.113920	-0.037007	3.662891
182.914595	4543.124284	7.118925	-0.037049	3.665994
183.006435	4551.120092	7.123930	-0.037071	3.669072
183.269706	4559.186687	7.128934	-0.037125	3.672180
183.518220	4567.202686	7.133939	-0.037177	3.675266
183.722514	4575.180482	7.138944	-0.037220	3.678333
183.959096	4583.259806	7.143949	-0.037269	3.681437
184.076871	4591.199893	7.148954	-0.037297	3.684482
184.340893	4599.257658	7.153958	-0.037351	3.687574
184.371119	4607.282240	7.158963	-0.037362	3.690644
184.553496	4615.309217	7.163968	-0.037401	3.693716
184.893326	4623.373514	7.168973	-0.037470	3.696804
184.897780	4631.332436	7.173978	-0.037476	3.699841
185.279417	4639.353553	7.178982	-0.037552	3.702908
185.375945	4647.391049	7.183987	-0.037575	3.705972
185.457112	4655.393571	7.188992	-0.037596	3.709020
185.633253	4663.503341	7.193997	-0.037634	3.712108
185.977006	4671.558167	7.199002	-0.037703	3.715177
186.134229	4679.541319	7.204006	-0.037738	3.718212
186.109250	4687.560051	7.209011	-0.037738	3.721253
186.231807	4695.507506	7.214016	-0.037766	3.724268
186.492867	4703.573038	7.219021	-0.037820	3.727329
186.760909	4711.545005	7.224026	-0.037875	3.730352
187.080026	4719.583935	7.229030	-0.037940	3.733399
186.991644	4727.659463	7.234035	-0.037929	3.736448
187.344902	4735.618580	7.239040	-0.038000	3.739461
187.460477	4743.674561	7.244045	-0.038027	3.742502
187.641984	4751.658436	7.249050	-0.038066	3.745515
188.015746	4759.694889	7.254054	-0.038141	3.748550
188.063555	4767.755816	7.259059	-0.038155	3.751584
188.345360	4775.766413	7.264064	-0.038213	3.754602
188.528916	4783.819594	7.269069	-0.038252	3.757631
188.587327	4791.808020	7.274074	-0.038268	3.760631
188.740974	4799.828653	7.279078	-0.038302	3.763642
188.951870	4807.843944	7.284083	-0.038347	3.766650
189.156287	4815.857796	7.289088	-0.038390	3.769656
189.216979	4823.987900	7.294093	-0.038407	3.772699
189.413897	4831.940048	7.299098	-0.038449	3.775676
189.825000	4839.959199	7.304102	-0.038530	3.778680
189.824645	4847.989632	7.309107	-0.038536	3.781677
189.883817	4855.977642	7.314112	-0.038552	3.784658
190.353620	4864.018637	7.319117	-0.038645	3.787665
190.376255	4872.004007	7.324122	-0.038654	3.790638
190.577615	4880.127747	7.329126	-0.038697	3.793665
190.753997	4888.112521	7.334131	-0.038735	3.796637
190.926227	4896.089588	7.339136	-0.038772	3.799604
191.231256	4904.119004	7.344141	-0.038834	3.802591
191.339307	4912.109171	7.349146	-0.038860	3.805556
191.648212	4920.124213	7.354150	-0.038923	3.808533
191.850839	4928.196571	7.359155	-0.038966	3.811527
191.676617	4936.197665	7.364160	-0.038938	3.814483
192.054082	4944.209264	7.369165	-0.039014	3.817453
192.123890	4952.193464	7.374170	-0.039032	3.820404
192.226840	4960.256426	7.379174	-0.039057	3.823382
192.440735	4968.271944	7.384179	-0.039102	3.826343
192.763429	4976.273147	7.389184	-0.039167	3.829299
192.874062	4984.348732	7.394189	-0.039193	3.832275
192.931274	4992.369176	7.399194	-0.039209	3.835228
193.230403	5000.351568	7.404198	-0.039270	3.838169
193.390289	5008.397374	7.409203	-0.039305	3.841128
193.526076	5016.359786	7.414208	-0.039335	3.844054
193.864108	5024.398742	7.419213	-0.039404	3.847010
194.001581	5032.429661	7.424218	-0.039435	3.849957
194.216453	5040.480404	7.429222	-0.039480	3.852910
194.422566	5048.533642	7.434227	-0.039523	3.855861
194.588330	5056.498015	7.439232	-0.039560	3.858777
194.761205	5064.560406	7.444237	-0.039597	3.861727
194.720121	5072.524445	7.449242	-0.039595	3.864634
195.085442	5080.596389	7.454246	-0.039668	3.867587
195.131717	5088.661192	7.459251	-0.039682	3.870528
195.281846	5096.874838	7.464256	-0.039715	3.873523
195.494840	5104.882175	7.469261	-0.039760	3.876442
195.644855	5112.720448	7.474266	-0.039793	3.879296
195.945730	5120.765265	7.479270	-0.039855	3.882226
196.123659	5128.708502	7.484275	-0.039893	3.885115
196.412794	5136.709467	7.489280	-0.039952	3.888024
196.335385	5144.771315	7.494285	-0.039943	3.890946
196.424634	5152.800222	7.499290	-0.039965	3.893858
196.837575	5160.829346	7.504294	-0.040047	3.896773
196.926995	5168.805689	7.509299	-0.040069	3.899661
196.847758	5176.835678	7.514304	-0.040059	3.902563
197.151510	5184.833514	7.519309	-0.040121	3.905458
197.343898	5192.870884	7.524314	-0.040162	3.908363
197.506774	5200.919313	7.529318	-0.040198	3.911270
197.689570	5208.924264	7.534323	-0.040237	3.914159
198.015285	5216.904472	7.539328	-0.040303	3.917040
198.239608	5224.938398	7.544333	-0.040350	3.919936
198.075146	5232.953883	7.549338	-0.040325	3.922816
198.326835	5240.994925	7.554342	-0.040377	3.925710
198.497841	5249.014790	7.559347	-0.040414	3.928594
198.760217	5257.003829	7.564352	-0.040468	3.931466
198.979140	5265.087224	7.569357	-0.040514	3.934369
199.212051	5273.062693	7.574362	-0.040563	3.937231
199.437719	5281.082808	7.579366	-0.040610	3.940107
199.603945	5289.102231	7.584371	-0.040646	3.942980
199.666867	5297.111717	7.589376	-0.040663	3.945845
199.908857	5305.150595	7.594381	-0.040714	3.948721
200.117474	5313.165589	7.599386	-0.040758	3.951587
200.477003	5321.234284	7.604390	-0.040830	3.954472
200.772743	5329.242050	7.609395	-0.040890	3.957332
200.915031	5337.207063	7.614400	-0.040922	3.960172
201.037014	5345.202525	7.619405	-0.040950	3.963020
201.011461	5353.253899	7.624410	-0.040951	3.965884
201.324446	5361.259762	7.629414	-0.041014	3.968735
201.526314	5369.309344	7.634419	-0.041057	3.971598
201.622010	5377.315311	7.639424	-0.041080	3.974442
202.025783	5385.374145	7.644429	-0.041161	3.977307
201.883142	5393.334262	7.649434	-0.041139	3.980126
202.312189	5401.361369	7.654438	-0.041224	3.982977
202.432015	5409.377953	7.659443	-0.041252	3.985816
202.424196	5417.426549	7.664448	-0.041256	3.988663
202.632134	5425.500963	7.669453	-0.041300	3.991520
202.935298	5433.498175	7.674458	-0.041362	3.994350
203.061271	5441.528785	7.679462	-0.041390	3.997186
203.012004	5449.540397	7.684467	-0.041386	4.000011
203.299895	5457.511314	7.689472	-0.041445	4.002825
203.839016	5465.530687	7.694477	-0.041551	4.005657
203.698814	5473.553761	7.699482	-0.041530	4.008479
203.886254	5481.635221	7.704486	-0.041570	4.011324
204.066413	5489.659734	7.709491	-0.041609	4.014147
204.168105	5497.689024	7.714496	-0.041633	4.016968
204.296018	5505.689031	7.719501	-0.041662	4.019778
204.607432	5513.675915	7.724506	-0.041726	4.022583
204.912046	5521.670594	7.729510	-0.041788	4.025390
204.929541	5529.739723	7.734515	-0.041796	4.028216
205.138034	5537.749105	7.739520	-0.041840	4.031022
205.608180	5545.890361	7.744525	-0.041933	4.033876
205.730867	5553.879195	7.749530	-0.041961	4.036670
205.850670	5561.778945	7.754534	-0.041989	4.039430
206.031024	5569.848923	7.759539	-0.042028	4.042249
206.092798	5577.778311	7.764544	-0.042044	4.045015
206.280704	5585.872716	7.769549	-0.042085	4.047839
206.580478	5593.835413	7.774554	-0.042146	4.050616
206.795745	5601.881742	7.779558	-0.042191	4.053419
206.909637	5609.939769	7.784563	-0.042218	4.056223
207.035745	5617.890583	7.789568	-0.042246	4.058988
207.438859	5625.928044	7.794573	-0.042327	4.061785
207.505820	5633.921169	7.799578	-0.042344	4.064560
207.757402	5641.959053	7.804582	-0.042396	4.067351
208.098651	5649.980890	7.809587	-0.042465	4.070136
208.233898	5658.007716	7.814592	-0.042496	4.072917
208.483615	5666.028249	7.819597	-0.042548	4.075696
208.574845	5674.011073	7.824602	-0.042570	4.078459
208.835305	5682.038669	7.829606	-0.042624	4.081236
209.059109	5690.052511	7.834611	-0.042670	4.084007
209.129435	5698.057165	7.839616	-0.042689	4.086771
209.428185	5706.114409	7.844621	-0.042750	4.089554
209.479499	5714.154361	7.849626	-0.042765	4.092326
209.794638	5722.192214	7.854630	-0.042829	4.095098
209.985221	5730.195121	7.859635	-0.042869	4.097855
210.212481	5738.168492	7.864640	-0.042917	4.100601
210.355047	5746.222345	7.869645	-0.042949	4.103371
210.622356	5754.227836	7.874650	-0.043004	4.106124
210.655613	5762.262285	7.879654	-0.043015	4.108882
210.877949	5770.332323	7.884659	-0.043062	4.111654
211.124242	5778.346871	7.889664	-0.043113	4.114404
211.418725	5786.417965	7.894669	-0.043173	4.117173
211.585546	5794.346113	7.899674	-0.043209	4.119889
211.683578	5802.384366	7.904678	-0.043233	4.122640
211.821830	5810.383617	7.909683	-0.043264	4.125376
211.868381	5818.376984	7.914688	-0.043278	4.128108
212.308470	5826.471988	7.919693	-0.043365	4.130877
212.437484	5834.490544	7.924698	-0.043394	4.133614
212.773330	5842.510669	7.929702	-0.043462	4.136353
212.800408	5850.498768	7.934707	-0.043473	4.139075
212.968039	5858.517390	7.939712	-0.043509	4.141807
213.371192	5866.506398	7.944717	-0.043589	4.144531
213.225486	5874.541354	7.949722	-0.043568	4.147261
213.336848	5882.566085	7.954726	-0.043594	4.149990
213.586324	5890.621671	7.959731	-0.043645	4.152728
213.721771	5898.613950	7.964736	-0.043676	4.155442
214.071069	5906.607810	7.969741	-0.043746	4.158157
214.156924	5914.652035	7.974746	-0.043767	4.160885
214.190462	5922.643435	7.979750	-0.043779	4.163592
214.347290	5930.649708	7.984755	-0.043813	4.166304
214.410358	5938.669976	7.989760	-0.043830	4.169017
215.028548	5946.718434	7.994765	-0.043951	4.171745
215.170112	5954.714377	7.999770	-0.043982	4.174448
215.190226	5962.761229	8.004774	-0.043991	4.177164
215.321558	5970.754123	8.009779	-0.044021	4.179862
215.674727	5978.749596	8.014784	-0.044092	4.182562
215.758016	5986.786069	8.019789	-0.044113	4.185271
215.956126	5994.801807	8.024794	-0.044155	4.187972
216.147705	6002.811883	8.029798	-0.044196	4.190669
216.237135	6010.987430	8.034803	-0.044218	4.193419
216.328037	6018.944374	8.039808	-0.044240	4.196094
216.575314	6026.902423	8.044813	-0.044291	4.198770
216.880323	6034.907575	8.049818	-0.044353	4.201460
216.807819	6042.836674	8.054822	-0.044345	4.204118
216.757755	6050.986229	8.059827	-0.044341	4.206849
217.031477	6058.896133	8.064832	-0.044397	4.209502
217.432000	6066.992905	8.069837	-0.044477	4.212216
217.301110	6074.978704	8.074842	-0.044458	4.214887
217.774877	6082.980172	8.079846	-0.044552	4.217567
218.057107	6091.011387	8.084851	-0.044609	4.220253
218.072671	6098.980986	8.089856	-0.044618	4.222914
218.189989	6107.040580	8.094861	-0.044645	4.225604
218.507556	6115.035776	8.099866	-0.044709	4.228274
218.899991	6123.063020	8.104870	-0.044787	4.230953
218.835154	6131.144460	8.109875	-0.044781	4.233644
219.012668	6139.146138	8.114880	-0.044819	4.236309
219.334591	6147.139398	8.119885	-0.044884	4.238970
219.352340	6155.136162	8.124890	-0.044893	4.241629
219.437322	6163.107850	8.129894	-0.044914	4.244278
219.723167	6171.161689	8.134899	-0.044972	4.246954
219.859811	6179.193839	8.139904	-0.045003	4.249620
219.866757	6187.260125	8.144909	-0.045010	4.252295
220.146888	6195.262714	8.149914	-0.045067	4.254949
220.352966	6203.269619	8.154918	-0.045111	4.257603
220.606749	6211.285032	8.159923	-0.045163	4.260258
220.843019	6219.266369	8.164928	-0.045213	4.262900
220.844931	6227.348794	8.169933	-0.045218	4.265571
220.849423	6235.353028	8.174938	-0.045224	4.268215
221.191257	6243.398745	8.179942	-0.045293	4.270874
221.449096	6251.437622	8.184947	-0.045347	4.273528
221.474036	6259.475349	8.189952	-0.045356	4.276179
221.949415	6267.427794	8.194957	-0.045450	4.278803
222.035347	6275.435123	8.199962	-0.045471	4.281441
222.063016	6283.396717	8.204966	-0.045482	4.284061
222.245409	6291.486546	8.209971	-0.045521	4.286723
222.550092	6299.472959	8.214976	-0.045583	4.289350
222.988382	6307.535242	8.219981	-0.045670	4.292002
223.198195	6315.545534	8.224986	-0.045714	4.294633
223.308284	6323.567074	8.229990	-0.045740	4.297266
223.541558	6331.581075	8.234995	-0.045789	4.299895
223.730770	6339.563971	8.240000	-0.045829	4.302512
224.029580	6347.521541	8.245005	-0.045890	4.305121
224.312549	6355.611359	8.250010	-0.045948	4.307770
224.573746	6363.634220	8.255014	-0.046002	4.310396
224.707543	6371.730977	8.260019	-0.046032	4.313044
224.700027	6379.700270	8.265024	-0.046036	4.315647
225.082011	6387.697041	8.270029	-0.046113	4.318260
225.115779	6395.720114	8.275034	-0.046124	4.320878
225.199954	6403.682768	8.280038	-0.046145	4.323475
225.541869	6411.727886	8.285043	-0.046214	4.326099
225.637331	6419.744160	8.290048	-0.046237	4.328710
225.868427	6427.789219	8.295053	-0.046285	4.331330
225.816940	6435.813698	8.300058	-0.046281	4.333940
226.105530	6443.839529	8.305062	-0.046340	4.336551
226.220651	6451.793269	8.310067	-0.046367	4.339135
226.249853	6459.825759	8.315072	-0.046377	4.341744
226.603112	6467.840920	8.320077	-0.046448	4.344347
226.573443	6475.867048	8.325082	-0.046448	4.346949
226.964775	6483.887411	8.330086	-0.046526	4.349551
227.438462	6491.956385	8.335091	-0.046620	4.352168
227.417712	6499.971871	8.340096	-0.046621	4.354762
227.648891	6507.992904	8.345101	-0.046670	4.357358
227.716906	6515.962154	8.350106	-0.046687	4.359935
227.836501	6523.962207	8.355110	-0.046715	4.362521
228.012920	6531.947587	8.360115	-0.046753	4.365101
228.046488	6539.983086	8.365120	-0.046765	4.367694
228.120075	6547.999383	8.370125	-0.046784	4.370280
228.283716	6556.027495	8.375130	-0.046819	4.372869
228.314872	6564.048358	8.380134	-0.046830	4.375453
228.636819	6572.064754	8.385139	-0.046896	4.378036
228.609218	6580.039001	8.390144	-0.046896	4.380601
228.880258	6588.086349	8.395149	-0.046951	4.383191
228.972021	6596.089292	8.400154	-0.046974	4.385763
229.293639	6604.094874	8.405158	-0.047039	4.388336
229.421813	6612.151467	8.410163	-0.047068	4.390923
229.648401	6620.137193	8.415168	-0.047116	4.393486
229.677154	6628.215789	8.420173	-0.047126	4.396077
229.691159	6636.189289	8.425178	-0.047134	4.398632
229.795542	6644.239071	8.430182	-0.047159	4.401210
230.114438	6652.213987	8.435187	-0.047223	4.403764
230.183327	6660.187968	8.440192	-0.047241	4.406315
230.295858	6668.252846	8.445197	-0.047268	4.408894
230.507481	6676.307243	8.450202	-0.047312	4.411469
230.736653	6684.318238	8.455206	-0.047360	4.414028
230.894185	6692.370320	8.460211	-0.047395	4.416598
230.937395	6700.300637	8.465216	-0.047408	4.419127
231.181341	6708.416687	8.470221	-0.047459	4.421716
231.337102	6716.331081	8.475226	-0.047493	4.424238
231.341057	6724.406290	8.480230	-0.047499	4.426808
231.577882	6732.438661	8.485235	-0.047549	4.429365
231.924860	6740.451614	8.490240	-0.047619	4.431915
231.977595	6748.542259	8.495245	-0.047634	4.434487
231.995853	6756.513247	8.500250	-0.047642	4.437019
232.262726	6764.463749	8.505254	-0.047697	4.439544
232.524878	6772.542978	8.510259	-0.047751	4.442108
232.335348	6780.448835	8.515264	-0.047721	4.444614
232.761207	6788.559916	8.520269	-0.047806	4.447186
232.950050	6796.535966	8.525274	-0.047846	4.449713
233.155170	6804.592391	8.530278	-0.047890	4.452264
233.297683	6812.594096	8.535283	-0.047922	4.454796
233.485022	6820.610727	8.540288	-0.047962	4.457332
233.654065	6828.607521	8.545293	-0.047998	4.459859
233.671036	6836.654255	8.550298	-0.048007	4.462401
233.939589	6844.641285	8.555302	-0.048062	4.464923
234.150217	6852.725684	8.560307	-0.048107	4.467474
234.191451	6860.674084	8.565312	-0.048120	4.469980
234.561506	6868.763036	8.570317	-0.048194	4.472530
234.434073	6876.734301	8.575322	-0.048175	4.475039
234.504286	6884.741599	8.580327	-0.048194	4.477560
234.768307	6892.758340	8.585331	-0.048248	4.480082
234.977242	6900.727636	8.590336	-0.048292	4.482588
235.035163	6908.743775	8.595341	-0.048308	4.485107
235.268303	6916.818387	8.600346	-0.048357	4.487644
235.389143	6924.792299	8.605351	-0.048385	4.490146
235.501164	6932.868371	8.610355	-0.048411	4.492680
235.527363	6940.853234	8.615360	-0.048421	4.495183
235.797133	6948.904107	8.620365	-0.048477	4.497706
236.005801	6956.852459	8.625370	-0.048521	4.500196
236.057845	6964.863566	8.630375	-0.048536	4.502703
236.318401	6972.897330	8.635379	-0.048589	4.505217
236.396698	6980.915255	8.640384	-0.048609	4.507723
236.571792	6988.919890	8.645389	-0.048647	4.510225
236.688939	6997.020522	8.650394	-0.048674	4.512754
237.085085	7005.035499	8.655399	-0.048753	4.515257
237.264720	7013.037724	8.660403	-0.048792	4.517753
237.116087	7020.980794	8.665408	-0.048770	4.520229
237.358882	7029.006502	8.670413	-0.048820	4.522730
237.766527	7036.984438	8.675418	-0.048901	4.525215
237.585630	7044.968984	8.680423	-0.048873	4.527699
237.941534	7053.021518	8.685427	-0.048944	4.530205
238.180379	7061.053303	8.690432	-0.048994	4.532702
238.334228	7069.117294	8.695437	-0.049028	4.535208
238.404955	7077.104862	8.700442	-0.049046	4.537688
238.726771	7085.076228	8.705447	-0.049112	4.540163
238.996800	7093.127884	8.710451	-0.049167	4.542661
238.901034	7101.101493	8.715456	-0.049155	4.545132
238.946367	7109.173402	8.720461	-0.049168	4.547633
239.051095	7117.132493	8.725466	-0.049193	4.550098
239.171253	7125.203836	8.730471	-0.049221	4.552596
239.513197	7133.255392	8.735475	-0.049290	4.555088
239.692250	7141.251633	8.740480	-0.049328	4.557560
239.700908	7149.188355	8.745485	-0.049335	4.560012
239.963784	7157.262793	8.750490	-0.049389	4.562506
240.161248	7165.223640	8.755495	-0.049431	4.564963
240.327722	7173.325645	8.760499	-0.049468	4.567463
240.230904	7181.247747	8.765504	-0.049455	4.569905
240.615150	7189.384232	8.770509	-0.049532	4.572413
240.782656	7197.348585	8.775514	-0.049568	4.574866
240.939410	7205.398482	8.780519	-0.049603	4.577344
240.864022	7213.395603	8.785523	-0.049594	4.579804
241.004493	7221.366982	8.790528	-0.049625	4.582255
241.233854	7229.413611	8.795533	-0.049673	4.584728
241.302049	7237.488427	8.800538	-0.049691	4.587208
241.445375	7245.452538	8.805543	-0.049723	4.589653
241.773686	7253.529531	8.810547	-0.049790	4.592131
241.774345	7261.520922	8.815552	-0.049795	4.594581
242.015649	7269.561074	8.820557	-0.049845	4.597046
242.094470	7277.496757	8.825562	-0.049865	4.599476
242.241893	7285.547790	8.830567	-0.049898	4.601941
242.531075	7293.531640	8.835571	-0.049957	4.604384
242.512029	7301.546606	8.840576	-0.049959	4.606835
242.908079	7309.544189	8.845581	-0.050038	4.609280
242.899104	7317.615806	8.850586	-0.050041	4.611746
242.923727	7325.639582	8.855591	-0.050051	4.614195
243.277850	7333.647208	8.860595	-0.050122	4.616639
243.217688	7341.590496	8.865600	-0.050116	4.619062
243.408913	7349.656898	8.870605	-0.050157	4.621521
243.664464	7357.638549	8.875610	-0.050210	4.623952
243.801967	7365.657221	8.880615	-0.050241	4.626394
243.836089	7373.713940	8.885619	-0.050253	4.628846
243.964664	7381.760699	8.890624	-0.050282	4.631294
244.370522	7389.762878	8.895629	-0.050363	4.633726
244.346267	7397.813930	8.900634	-0.050363	4.636173
244.387049	7405.741849	8.905639	-0.050376	4.638580
244.604959	7413.826538	8.910643	-0.050422	4.641034
244.736006	7421.743501	8.915648	-0.050452	4.643436
244.844223	7429.828318	8.920653	-0.050477	4.645888
245.313634	7437.786512	8.925658	-0.050570	4.648299
245.109387	7445.848155	8.930663	-0.050537	4.650741
245.304745	7453.938900	8.935667	-0.050579	4.653190
245.558525	7461.887626	8.940672	-0.050631	4.655595
245.732464	7469.892957	8.945677	-0.050669	4.658016
245.793747	7477.928983	8.950682	-0.050686	4.660445
245.810756	7485.912212	8.955687	-0.050694	4.662857
246.340244	7493.936803	8.960691	-0.050798	4.665279
246.334296	7501.922139	8.965696	-0.050802	4.667689
246.485912	7509.950606	8.970701	-0.050836	4.670110
246.675015	7518.099495	8.975706	-0.050876	4.672567
246.732566	7526.079045	8.980711	-0.050892	4.674971
246.925019	7534.101771	8.985715	-0.050933	4.677387
246.972022	7542.003477	8.990720	-0.050947	4.679765
247.353681	7550.040775	8.995725	-0.051024	4.682182
247.516295	7558.010542	9.000730	-0.051059	4.684579
247.516062	7566.069768	9.005735	-0.051064	4.687001
247.815820	7574.048666	9.010739	-0.051125	4.689397
247.825010	7582.072630	9.015744	-0.051132	4.691806
247.999188	7590.106979	9.020749	-0.051170	4.694216
248.173808	7598.142412	9.025754	-0.051208	4.696626
248.457357	7606.058807	9.030759	-0.051266	4.698998
248.566759	7614.179281	9.035763	-0.051292	4.701431
248.498923	7622.092092	9.040768	-0.051284	4.703800
248.923131	7630.165852	9.045773	-0.051368	4.706216
249.268185	7638.212019	9.050778	-0.051438	4.708622
249.047696	7646.198551	9.055783	-0.051402	4.711010
249.320667	7654.307907	9.060787	-0.051458	4.713433
249.478676	7662.246012	9.065792	-0.051493	4.715804
249.451353	7670.313219	9.070797	-0.051493	4.718212
249.565055	7678.297826	9.075802	-0.051520	4.720594
249.827339	7686.227071	9.080807	-0.051574	4.722958
250.347223	7694.308312	9.085811	-0.051676	4.725365
250.499001	7702.320313	9.090816	-0.051709	4.727752
250.834989	7710.389525	9.095821	-0.051777	4.730154
250.941989	7718.410443	9.100826	-0.051802	4.732540
250.870130	7726.402237	9.105831	-0.051794	4.734918
251.337810	7734.435904	9.110835	-0.051887	4.737305
251.384951	7742.418092	9.115840	-0.051901	4.739677
251.597629	7750.440697	9.120845	-0.051945	4.742059
251.624346	7758.434978	9.125850	-0.051956	4.744432
251.737693	7766.468932	9.130855	-0.051982	4.746815
251.630560	7774.508802	9.135859	-0.051967	4.749200
251.545162	7782.513938	9.140864	-0.051957	4.751573
252.005787	7790.572389	9.145869	-0.052048	4.753958
252.004237	7798.596055	9.150874	-0.052053	4.756334
252.024310	7806.482600	9.155879	-0.052062	4.758668
252.282239	7814.600696	9.160883	-0.052115	4.761069
252.512348	7822.508252	9.165888	-0.052163	4.763406
252.738123	7830.546543	9.170893	-0.052210	4.765781
252.760078	7838.606502	9.175898	-0.052220	4.768161
252.861115	7846.572067	9.180903	-0.052244	4.770512
252.989825	7854.670019	9.185907	-0.052273	4.772901
253.011748	7862.611872	9.190912	-0.052282	4.775243
253.061796	7870.684077	9.195917	-0.052297	4.777623
253.440200	7878.648128	9.200922	-0.052373	4.779968
253.557171	7886.672084	9.205927	-0.052400	4.782330
253.726615	7894.689111	9.210931	-0.052437	4.784689
253.897558	7902.719742	9.215936	-0.052474	4.787051
254.075700	7910.714157	9.220941	-0.052512	4.789401
254.122568	7918.759571	9.225946	-0.052526	4.791765
254.262337	7926.744423	9.230951	-0.052558	4.794110
254.556469	7934.818478	9.235955	-0.052618	4.796479
254.627289	7942.764556	9.240960	-0.052636	4.798811
254.604888	7950.795103	9.245965	-0.052637	4.801166
254.905354	7958.818556	9.250970	-0.052698	4.803517
254.984695	7966.800007	9.255975	-0.052718	4.805856
254.955651	7974.879645	9.260979	-0.052718	4.808222
255.149812	7982.833460	9.265984	-0.052760	4.810549
255.148389	7990.319537	9.270989	-0.052764	4.812740
255.463725	7994.857864	9.275994	-0.052826	4.814066

255.447645	7997.362270	9.280999	-0.052825	4.814798
255.744232	7998.784016	9.286003	-0.052881	4.815212
255.576898	7999.218036	9.291008	-0.052850	4.815340
255.861413	8000.129297	9.296013	-0.052904	4.815605
256.146819	8000.164924	9.301018	-0.052957	4.815614
256.137629	8000.116722	9.306023	-0.052955	4.815600
256.331107	8000.219198	9.311027	-0.052991	4.815629
256.264415	8000.147631	9.316032	-0.052979	4.815609
256.416860	8000.146918	9.321037	-0.053007	4.815608
256.367223	8000.150384	9.326042	-0.052998	4.815609
256.343528	8000.107285	9.331047	-0.052994	4.815596
256.468796	8000.169135	9.336051	-0.053017	4.815614
256.437159	8000.171827	9.341056	-0.053011	4.815615
256.679059	8000.159758	9.346061	-0.053056	4.815610
256.695352	8000.188862	9.351066	-0.053059	4.815619
256.631890	8000.175015	9.356071	-0.053048	4.815615
256.548717	8000.171527	9.361075	-0.053032	4.815614
256.730271	8000.155269	9.366080	-0.053066	4.815609
256.871702	8000.202434	9.371085	-0.053093	4.815622
256.891341	8000.226252	9.376090	-0.053096	4.815629
256.837818	8000.164511	9.381095	-0.053086	4.815611
257.130813	8000.150072	9.386099	-0.053141	4.815605
257.012346	8000.155619	9.391104	-0.053119	4.815607
256.959685	8000.162239	9.396109	-0.053109	4.815610
257.095659	8000.181549	9.401114	-0.053134	4.815615
257.095459	8000.184753	9.406119	-0.053134	4.815616
257.160456	8000.198633	9.411123	-0.053147	4.815619
257.074809	8000.175881	9.416128	-0.053131	4.815613
257.211652	8000.209088	9.421133	-0.053156	4.815622
257.127963	8000.225881	9.426138	-0.053141	4.815627
257.155718	8000.161193	9.431143	-0.053146	4.815608
257.493585	8000.200885	9.436147	-0.053209	4.815618
257.303607	8000.180701	9.441152	-0.053174	4.815613
257.410949	8000.169642	9.446157	-0.053194	4.815610
257.614384	8000.188984	9.451162	-0.053232	4.815614
257.253035	8000.208722	9.456167	-0.053164	4.815622
257.213337	8000.268951	9.461171	-0.053157	4.815640
257.088189	8000.199633	9.466176	-0.053134	4.815620
257.334647	8000.187639	9.471181	-0.053180	4.815615
257.573841	8000.207566	9.476186	-0.053224	4.815620
257.436449	8000.201056	9.481191	-0.053199	4.815619
257.566559	8000.249105	9.486195	-0.053223	4.815632
257.492903	8000.213732	9.491200	-0.053209	4.815622
257.415474	8000.178298	9.496205	-0.053195	4.815612
257.511488	8000.185209	9.501210	-0.053213	4.815614
257.639473	8000.211864	9.506215	-0.053237	4.815621
257.575555	8000.253543	9.511219	-0.053225	4.815633
257.612423	8000.205023	9.516224	-0.053232	4.815619
257.593323	8000.173745	9.521229	-0.053228	4.815610
257.428491	8000.192418	9.526234	-0.053198	4.815616
257.324881	8000.159761	9.531239	-0.053178	4.815607
257.562515	8000.221311	9.536243	-0.053223	4.815624
257.489165	8000.173129	9.541248	-0.053209	4.815610
257.583375	8000.178942	9.546253	-0.053227	4.815611
257.539303	8000.246575	9.551258	-0.053218	4.815631
257.586972	8000.248425	9.556263	-0.053227	4.815632
257.750704	8000.226538	9.561267	-0.053258	4.815625
257.616503	8000.161343	9.566272	-0.053233	4.815606
257.828374	8000.225678	9.571277	-0.053272	4.815624
257.960270	8000.242786	9.576282	-0.053297	4.815628
257.735956	8000.197479	9.581287	-0.053255	4.815616
257.941278	8000.373844	9.586291	-0.053294	4.815667
257.826537	8000.310033	9.591296	-0.053272	4.815649
257.577598	8000.219469	9.596301	-0.053226	4.815623
257.578906	8000.248329	9.601306	-0.053226	4.815632
257.790489	8000.208000	9.606311	-0.053266	4.815619
257.829666	8000.210779	9.611315	-0.053273	4.815620
257.601920	8000.180367	9.616320	-0.053231	4.815612
257.778717	8000.220635	9.621325	-0.053264	4.815623
257.615438	8000.282051	9.626330	-0.053233	4.815641
257.624426	8000.235212	9.631335	-0.053235	4.815628
257.878489	8000.288489	9.636339	-0.053282	4.815642
257.807643	8000.228599	9.641344	-0.053269	4.815625
257.786815	8000.204768	9.646349	-0.053265	4.815618
257.871900	8000.212568	9.651354	-0.053281	4.815620
257.820253	8000.213865	9.656359	-0.053272	4.815621
257.920312	8000.247541	9.661363	-0.053290	4.815630
257.745073	8000.275655	9.666368	-0.053258	4.815639
257.803643	8000.284091	9.671373	-0.053269	4.815641
257.833618	8000.266429	9.676378	-0.053274	4.815636
257.837471	8000.241933	9.681383	-0.053275	4.815629
257.922137	8000.249726	9.686387	-0.053291	4.815631
257.954563	8000.197929	9.691392	-0.053297	4.815615
257.970950	8000.252667	9.696397	-0.053300	4.815631
257.794004	8000.319200	9.701402	-0.053267	4.815651
257.633969	8000.232223	9.706407	-0.053237	4.815627
257.783372	8000.292335	9.711411	-0.053265	4.815644
257.678111	8000.267126	9.716416	-0.053246	4.815637
257.858130	8000.240165	9.721421	-0.053279	4.815628
257.761106	8000.264217	9.726426	-0.053261	4.815636
257.666144	8000.185778	9.731431	-0.053244	4.815613
257.699390	8000.214091	9.736435	-0.053250	4.815621
257.843561	8000.219652	9.741440	-0.053277	4.815622
257.758636	8000.177688	9.746445	-0.053261	4.815610
257.784001	8000.227231	9.751450	-0.053266	4.815625
257.763363	8000.186316	9.756455	-0.053262	4.815613
257.911565	8000.290195	9.761459	-0.053290	4.815642
257.727609	8000.203896	9.766464	-0.053255	4.815618
257.977151	8000.261371	9.771469	-0.053302	4.815634
258.030400	8000.270788	9.776474	-0.053312	4.815636
257.709771	8000.183325	9.781479	-0.053252	4.815612
257.875689	8000.270406	9.786483	-0.053283	4.815637
257.865523	8000.276652	9.791488	-0.053281	4.815639
258.202023	8000.250110	9.796493	-0.053344	4.815629
257.886204	8000.240687	9.801498	-0.053285	4.815628
257.774944	8000.230331	9.806503	-0.053265	4.815626
258.156349	8000.255784	9.811507	-0.053336	4.815631
258.079280	8000.274821	9.816512	-0.053321	4.815637
257.971235	8000.266653	9.821517	-0.053301	4.815635
258.137254	8000.347329	9.826522	-0.053332	4.815658
257.898337	8000.245180	9.831527	-0.053288	4.815629
258.059851	8000.370637	9.836531	-0.053318	4.815665
258.013491	8000.298330	9.841536	-0.053309	4.815644
258.099000	8000.312546	9.846541	-0.053325	4.815648
258.273087	8000.333547	9.851546	-0.053358	4.815653
258.098491	8000.290118	9.856551	-0.053325	4.815641
258.137100	8000.335607	9.861555	-0.053333	4.815655
257.864344	8000.298051	9.866560	-0.053282	4.815645
258.002897	8000.246918	9.871565	-0.053308	4.815629
257.913448	8000.284977	9.876570	-0.053291	4.815641
258.066301	8000.280000	9.881575	-0.053320	4.815639
257.994599	8000.277766	9.886579	-0.053306	4.815638
257.926156	8000.220050	9.891584	-0.053294	4.815622
258.203564	8000.272641	9.896589	-0.053345	4.815636
258.079243	8000.273819	9.901594	-0.053322	4.815637
258.042405	8000.228368	9.906599	-0.053315	4.815624
258.188510	8000.279883	9.911603	-0.053343	4.815638
258.140542	8000.285512	9.916608	-0.053334	4.815640
258.195321	8000.194565	9.921613	-0.053344	4.815613
258.160699	8000.197207	9.926618	-0.053338	4.815614
258.056182	8000.146379	9.931623	-0.053318	4.815600
258.173678	8000.213447	9.936627	-0.053340	4.815619
258.287718	8000.227060	9.941632	-0.053361	4.815622
258.410056	8000.250420	9.946637	-0.053384	4.815628
258.382031	8000.291618	9.951642	-0.053379	4.815641
258.319793	8000.205168	9.956647	-0.053367	4.815616
258.425836	8000.295545	9.961651	-0.053387	4.815641
258.289629	8000.271966	9.966656	-0.053362	4.815635
258.382222	8000.200859	9.971661	-0.053379	4.815614
258.476780	8000.271825	9.976666	-0.053397	4.815634
258.392495	8000.256569	9.981671	-0.053381	4.815630
258.299746	8000.272146	9.986675	-0.053364	4.815635
258.542001	8000.255814	9.991680	-0.053409	4.815629
258.632210	8000.207096	9.996685	-0.053426	4.815615
258.706843	8000.289485	10.001690	-0.053440	4.815638
258.532127	8000.287704	10.006695	-0.053407	4.815639
258.696975	8000.328847	10.011699	-0.053438	4.815650
258.263112	8000.302543	10.016704	-0.053357	4.815644
258.468198	8000.239681	10.021709	-0.053396	4.815625
258.577620	8000.322638	10.026714	-0.053416	4.815649
258.508414	8000.303356	10.031719	-0.053403	4.815643
258.551761	8000.320088	10.036723	-0.053411	4.815648
258.534742	8000.278163	10.041728	-0.053408	4.815636
258.743211	8000.244191	10.046733	-0.053447	4.815625
258.471286	8000.291018	10.051738	-0.053397	4.815640
258.426061	8000.224069	10.056743	-0.053388	4.815621
258.683784	8000.287020	10.061747	-0.053436	4.815638
258.548113	8000.349955	10.066752	-0.053411	4.815657
258.472301	8000.286778	10.071757	-0.053397	4.815639
258.579904	8000.223393	10.076762	-0.053417	4.815620
258.612588	8000.210047	10.081767	-0.053423	4.815616
258.735641	8000.276139	10.086771	-0.053446	4.815634
258.405080	8000.226958	10.091776	-0.053385	4.815621
258.492332	8000.207027	10.096781	-0.053401	4.815615
258.455161	8000.204288	10.101786	-0.053394	4.815615
258.423502	8000.190960	10.106791	-0.053388	4.815611
258.501900	8000.312925	10.111795	-0.053403	4.815646
258.584359	8000.307867	10.116800	-0.053418	4.815644
258.455869	8000.235287	10.121805	-0.053394	4.815624
258.466709	8000.280323	10.126810	-0.053396	4.815637
258.401975	8000.255774	10.131815	-0.053384	4.815630
258.410071	8000.231347	10.136819	-0.053386	4.815623
258.491186	8000.288210	10.141824	-0.053401	4.815639
258.571549	8000.230787	10.146829	-0.053416	4.815622
258.558629	8000.297863	10.151834	-0.053414	4.815641
258.588367	8000.220390	10.156839	-0.053419	4.815619
258.859024	8000.278213	10.161843	-0.053470	4.815634
258.530114	8000.273914	10.166848	-0.053408	4.815635
258.418479	8000.198405	10.171853	-0.053388	4.815613
258.671637	8000.278368	10.176858	-0.053435	4.815635
258.658065	8000.269607	10.181863	-0.053432	4.815633
258.787929	8000.335811	10.186867	-0.053457	4.815651
258.690280	8000.298976	10.191872	-0.053439	4.815641
258.796701	8000.303922	10.196877	-0.053458	4.815642
258.723090	8000.315540	10.201882	-0.053445	4.815646
258.388753	8000.237462	10.206887	-0.053383	4.815625
258.600448	8000.299661	10.211891	-0.053422	4.815642
258.578949	8000.272614	10.216896	-0.053418	4.815634
258.498703	8000.218977	10.221901	-0.053403	4.815619
258.669434	8000.345655	10.226906	-0.053435	4.815655
258.631211	8000.291635	10.231911	-0.053428	4.815639
258.632646	8000.314090	10.236915	-0.053428	4.815646
258.660492	8000.313481	10.241920	-0.053433	4.815646
258.704051	8000.254389	10.246925	-0.053442	4.815628
258.702115	8000.304557	10.251930	-0.053441	4.815643
258.497549	8000.305492	10.256935	-0.053403	4.815644
258.682501	8000.283953	10.261939	-0.053438	4.815637
258.815849	8000.327786	10.266944	-0.053463	4.815649
258.806517	8000.312685	10.271949	-0.053461	4.815645
258.937043	8000.309481	10.276954	-0.053485	4.815643
259.008682	8000.281819	10.281959	-0.053499	4.815635
259.008385	8000.350170	10.286963	-0.053499	4.815655
258.895460	8000.321630	10.291968	-0.053478	4.815647
258.880410	8000.316048	10.296973	-0.053475	4.815645
259.033461	8000.344183	10.301978	-0.053503	4.815653
258.766529	8000.319536	10.306983	-0.053454	4.815647
258.642639	8000.377324	10.311987	-0.053431	4.815664
258.835726	8000.329218	10.316992	-0.053467	4.815649
258.788566	8000.320975	10.321997	-0.053458	4.815647
258.826658	8000.341893	10.327002	-0.053465	4.815653
258.826690	8000.361122	10.332007	-0.053465	4.815659
258.899714	8000.342026	10.337011	-0.053479	4.815653
258.858052	8000.334942	10.342016	-0.053471	4.815651
258.685394	8000.306494	10.347021	-0.053439	4.815643
258.713438	8000.338996	10.352026	-0.053444	4.815653
258.631223	8000.241539	10.357031	-0.053429	4.815625
258.663103	8000.293326	10.362035	-0.053435	4.815640
258.826023	8000.308807	10.367040	-0.053465	4.815643
258.984609	8000.304993	10.372045	-0.053495	4.815641
258.783371	8000.388217	10.377050	-0.053458	4.815667
258.826063	8000.360083	10.382055	-0.053466	4.815658
258.970930	8000.383813	10.387059	-0.053493	4.815665
258.797131	8000.367094	10.392064	-0.053460	4.815660
258.846663	8000.345479	10.397069	-0.053470	4.815654
258.922352	8000.433227	10.402074	-0.053484	4.815679
258.487269	8000.343890	10.407079	-0.053403	4.815655
258.613435	8000.366246	10.412083	-0.053426	4.815661
258.600582	8000.354292	10.417088	-0.053424	4.815658
258.810522	8000.379084	10.422093	-0.053463	4.815664
258.729748	8000.378837	10.427098	-0.053448	4.815664
258.708107	8000.310136	10.432103	-0.053444	4.815644
258.788481	8000.301841	10.437107	-0.053459	4.815641
258.585319	8000.313479	10.442112	-0.053421	4.815646
258.609493	8000.336305	10.447117	-0.053426	4.815652
258.727879	8000.358534	10.452122	-0.053448	4.815658
258.747569	8000.285169	10.457127	-0.053452	4.815637
258.905909	8000.321934	10.462131	-0.053481	4.815647
258.810592	8000.307566	10.467136	-0.053463	4.815643
258.797593	8000.314833	10.472141	-0.053461	4.815645
258.886413	8000.363279	10.477146	-0.053478	4.815659
258.768316	8000.345335	10.482151	-0.053456	4.815654
259.002660	8000.351302	10.487155	-0.053499	4.815655
258.808005	8000.365215	10.492160	-0.053463	4.815660
258.826284	8000.328137	10.497165	-0.053467	4.815649
258.935239	8000.387592	10.502170	-0.053487	4.815666
258.913793	8000.323166	10.507175	-0.053483	4.815647
258.865047	8000.319170	10.512179	-0.053474	4.815646
258.834806	8000.319748	10.517184	-0.053468	4.815646
258.849325	8000.309309	10.522189	-0.053471	4.815643
258.792529	8000.367125	10.527194	-0.053461	4.815660
258.761068	8000.319624	10.532199	-0.053455	4.815647
258.810256	8000.299071	10.537203	-0.053464	4.815641
258.756199	8000.292853	10.542208	-0.053454	4.815639
258.889008	8000.288617	10.547213	-0.053479	4.815637
258.961145	8000.388055	10.552218	-0.053492	4.815666
258.901089	8000.329406	10.557223	-0.053481	4.815649
258.746170	8000.330084	10.562227	-0.053452	4.815650
258.738321	8000.325688	10.567232	-0.053451	4.815649
258.787681	8000.360674	10.572237	-0.053460	4.815659
258.891670	8000.386940	10.577242	-0.053480	4.815666
258.730011	8000.277505	10.582247	-0.053449	4.815635
258.911535	8000.292221	10.587251	-0.053483	4.815638
258.822542	8000.319607	10.592256	-0.053467	4.815646
258.845137	8000.269785	10.597261	-0.053471	4.815632
258.940488	8000.286298	10.602266	-0.053489	4.815636
259.001656	8000.248853	10.607271	-0.053500	4.815625
258.945716	8000.241535	10.612275	-0.053490	4.815623
258.924349	8000.259346	10.617280	-0.053486	4.815628
258.889566	8000.270530	10.622285	-0.053480	4.815632
258.958622	8000.299429	10.627290	-0.053492	4.815640
258.927891	8000.215628	10.632295	-0.053487	4.815616
258.999445	8000.309716	10.637299	-0.053500	4.815643
258.886516	8000.297196	10.642304	-0.053479	4.815640
259.006990	8000.261787	10.647309	-0.053502	4.815629
259.018732	8000.348490	10.652314	-0.053504	4.815654
258.733177	8000.277615	10.657319	-0.053451	4.815635
259.010397	8000.271467	10.662323	-0.053502	4.815631
259.130538	8000.248869	10.667328	-0.053525	4.815624
259.259631	8000.243505	10.672333	-0.053549	4.815622
259.126392	8000.344929	10.677338	-0.053524	4.815652
259.127120	8000.277661	10.682343	-0.053524	4.815633
259.137960	8000.367554	10.687347	-0.053526	4.815659
258.898778	8000.363651	10.692352	-0.053482	4.815659
258.895767	8000.301662	10.697357	-0.053481	4.815641
258.990332	8000.325638	10.702362	-0.053499	4.815647
259.004630	8000.333352	10.707367	-0.053502	4.815650
258.846036	8000.306202	10.712371	-0.053472	4.815642
258.807050	8000.335472	10.717376	-0.053465	4.815651
258.926850	8000.312869	10.722381	-0.053487	4.815644
259.031969	8000.390418	10.727386	-0.053507	4.815666
258.845842	8000.355342	10.732391	-0.053472	4.815657
259.007378	8000.354780	10.737395	-0.053503	4.815656
258.996807	8000.349271	10.742400	-0.053501	4.815654
258.983161	8000.317013	10.747405	-0.053498	4.815645
259.041851	8000.336131	10.752410	-0.053509	4.815650
259.025835	8000.262182	10.757415	-0.053506	4.815629
258.955922	8000.280268	10.762419	-0.053493	4.815634
258.907748	8000.337156	10.767424	-0.053484	4.815651
259.122028	8000.214637	10.772429	-0.053524	4.815614
259.112091	8000.267878	10.777434	-0.053522	4.815630
258.916204	8000.304199	10.782439	-0.053486	4.815641
259.294107	8000.364843	10.787443	-0.053556	4.815657
259.173607	8000.344723	10.792448	-0.053534	4.815652
258.914354	8000.289228	10.797453	-0.053486	4.815637
258.887145	8000.329372	10.802458	-0.053481	4.815649
259.039096	8000.245350	10.807463	-0.053509	4.815624
259.149394	8000.325119	10.812467	-0.053530	4.815646
259.063624	8000.292750	10.817472	-0.053514	4.815637
259.109384	8000.211266	10.822477	-0.053522	4.815613
259.298362	8000.229308	10.827482	-0.053557	4.815618
259.145940	8000.197987	10.832487	-0.053529	4.815609
259.200005	8000.213826	10.837491	-0.053539	4.815614
259.182882	8000.328893	10.842496	-0.053536	4.815647
259.206525	8000.301516	10.847501	-0.053541	4.815639
259.197275	8000.315252	10.852506	-0.053539	4.815643
259.311278	8000.272263	10.857511	-0.053560	4.815630
259.236548	8000.289202	10.862515	-0.053546	4.815636
259.175284	8000.343741	10.867520	-0.053535	4.815652
259.207567	8000.287668	10.872525	-0.053541	4.815635
259.367774	8000.352233	10.877530	-0.053571	4.815653
259.058635	8000.327964	10.882535	-0.053513	4.815648
259.167092	8000.342555	10.887539	-0.053534	4.815651
259.217463	8000.320954	10.892544	-0.053543	4.815645
259.124851	8000.267113	10.897549	-0.053526	4.815630
259.286413	8000.318884	10.902554	-0.053556	4.815644
259.278549	8000.363615	10.907559	-0.053555	4.815657
259.376699	8000.381243	10.912563	-0.053573	4.815662
259.225564	8000.393730	10.917568	-0.053545	4.815666
259.248047	8000.338565	10.922573	-0.053549	4.815650
259.422546	8000.339283	10.927578	-0.053582	4.815649
259.324538	8000.285354	10.932583	-0.053563	4.815634
259.280990	8000.382903	10.937587	-0.053555	4.815663
259.234219	8000.375735	10.942592	-0.053547	4.815661
259.228113	8000.269907	10.947597	-0.053545	4.815630
259.152361	8000.309258	10.952602	-0.053531	4.815642
259.378925	8000.345003	10.957607	-0.053574	4.815651
259.412575	8000.295360	10.962611	-0.053580	4.815636
259.344877	8000.309210	10.967616	-0.053567	4.815641
259.139383	8000.268478	10.972621	-0.053529	4.815630
259.240797	8000.349170	10.977626	-0.053548	4.815653
259.339542	8000.301659	10.982631	-0.053567	4.815639
259.340166	8000.346529	10.987635	-0.053567	4.815652
259.263302	8000.291877	10.992640	-0.053552	4.815636
259.223765	8000.268808	10.997645	-0.053545	4.815630
259.127326	8000.358016	11.002650	-0.053527	4.815656
259.403514	8000.287771	11.007655	-0.053579	4.815634
259.513112	8000.283158	11.012659	-0.053599	4.815632
259.327884	8000.373052	11.017664	-0.053565	4.815660
259.427217	8000.314870	11.022669	-0.053583	4.815642
259.411205	8000.359469	11.027674	-0.053580	4.815655
259.355913	8000.339346	11.032679	-0.053570	4.815650
259.370555	8000.301141	11.037683	-0.053573	4.815638
259.494760	8000.344826	11.042688	-0.053596	4.815651
259.380738	8000.337627	11.047693	-0.053575	4.815649
259.186801	8000.310967	11.052698	-0.053539	4.815642
259.207985	8000.334813	11.057703	-0.053543	4.815649
259.545462	8000.268773	11.062707	-0.053606	4.815628
259.504766	8000.345009	11.067712	-0.053598	4.815651
259.474806	8000.340251	11.072717	-0.053593	4.815649
259.513887	8000.393226	11.077722	-0.053600	4.815665
259.424804	8000.326626	11.082727	-0.053583	4.815646
259.476964	8000.370203	11.087731	-0.053593	4.815658
259.670609	8000.364826	11.092736	-0.053629	4.815656
259.429705	8000.321378	11.097741	-0.053584	4.815644
259.336144	8000.411702	11.102746	-0.053567	4.815671
259.281184	8000.341388	11.107751	-0.053557	4.815651
259.598108	8000.316665	11.112755	-0.053616	4.815642
259.504591	8000.349318	11.117760	-0.053599	4.815652
259.231027	8000.235917	11.122765	-0.053548	4.815620
259.400425	8000.309176	11.127770	-0.053579	4.815641
259.332091	8000.310199	11.132775	-0.053567	4.815641
259.365059	8000.238118	11.137779	-0.053573	4.815620
259.458019	8000.271680	11.142784	-0.053590	4.815629
259.466628	8000.213085	11.147789	-0.053592	4.815612
259.428698	8000.277617	11.152794	-0.053585	4.815631
259.449769	8000.258741	11.157799	-0.053589	4.815626
259.595613	8000.287828	11.162803	-0.053616	4.815633
259.488410	8000.286080	11.167808	-0.053596	4.815633
259.511304	8000.255486	11.172813	-0.053600	4.815624
259.597210	8000.335926	11.177818	-0.053616	4.815647
259.640848	8000.321691	11.182823	-0.053624	4.815643
259.627168	8000.313995	11.187827	-0.053622	4.815641
259.624711	8000.363087	11.192832	-0.053622	4.815655
259.446683	8000.304646	11.197837	-0.053588	4.815639
259.452755	8000.342130	11.202842	-0.053590	4.815650
259.528477	8000.323079	11.207847	-0.053604	4.815644
259.619592	8000.292531	11.212851	-0.053621	4.815635
259.559988	8000.299037	11.217856	-0.053610	4.815637
259.502982	8000.289566	11.222861	-0.053599	4.815634
259.653792	8000.329414	11.227866	-0.053627	4.815645
259.500857	8000.317307	11.232871	-0.053599	4.815642
259.524092	8000.309146	11.237875	-0.053603	4.815640
259.469739	8000.334963	11.242880	-0.053593	4.815648
259.581717	8000.249219	11.247885	-0.053614	4.815622
259.615749	8000.352308	11.252890	-0.053620	4.815652
259.450412	8000.320775	11.257895	-0.053590	4.815644
259.748702	8000.305359	11.262899	-0.053645	4.815638
259.649501	8000.330443	11.267904	-0.053627	4.815646
259.691713	8000.341817	11.272909	-0.053635	4.815649
259.677285	8000.353333	11.277914	-0.053632	4.815652
259.626165	8000.263857	11.282919	-0.053623	4.815626
259.715259	8000.324057	11.287923	-0.053639	4.815643
259.625642	8000.410174	11.292928	-0.053623	4.815669
259.425496	8000.353507	11.297933	-0.053585	4.815653
259.556258	8000.417592	11.302938	-0.053610	4.815671
259.439515	8000.371900	11.307943	-0.053588	4.815659
259.707717	8000.322886	11.312947	-0.053638	4.815643
259.713134	8000.390263	11.317952	-0.053639	4.815663
259.669657	8000.370332	11.322957	-0.053631	4.815657
259.571600	8000.367666	11.327962	-0.053613	4.815657
259.533710	8000.360643	11.332967	-0.053606	4.815655
259.683341	8000.363091	11.337971	-0.053634	4.815655
259.637555	8000.359143	11.342976	-0.053625	4.815654
259.731229	8000.353202	11.347981	-0.053643	4.815652
259.676828	8000.348045	11.352986	-0.053633	4.815651
259.571257	8000.344188	11.357991	-0.053613	4.815650
259.701101	8000.273688	11.362995	-0.053637	4.815629
259.733082	8000.334023	11.368000	-0.053643	4.815646
259.588447	8000.240884	11.373005	-0.053616	4.815620
259.805730	8000.368327	11.378010	-0.053657	4.815656
259.535055	8000.335072	11.383015	-0.053607	4.815647
259.613063	8000.269066	11.388019	-0.053621	4.815628
259.396773	8000.341365	11.393024	-0.053581	4.815650
259.655840	8000.387254	11.398029	-0.053629	4.815662
259.719687	8000.407525	11.403034	-0.053641	4.815668
259.441864	8000.402990	11.408039	-0.053589	4.815668
259.457689	8000.341308	11.413043	-0.053592	4.815650
259.658699	8000.387316	11.418048	-0.053630	4.815662
259.693161	8000.337687	11.423053	-0.053636	4.815647
259.684893	8000.378140	11.428058	-0.053635	4.815659
259.655820	8000.337084	11.433063	-0.053630	4.815647
259.740333	8000.261572	11.438067	-0.053645	4.815625
259.606540	8000.334151	11.443072	-0.053620	4.815647
259.432733	8000.274711	11.448077	-0.053588	4.815630
259.542684	8000.356612	11.453082	-0.053609	4.815654
259.453160	8000.326317	11.458087	-0.053592	4.815645
259.539911	8000.344827	11.463091	-0.053608	4.815650
259.575488	8000.395608	11.468096	-0.053615	4.815665
259.487427	8000.321549	11.473101	-0.053599	4.815644
259.508840	8000.369963	11.478106	-0.053603	4.815658
259.801135	8000.360858	11.483111	-0.053657	4.815654
259.555598	8000.308790	11.488115	-0.053611	4.815640
259.680214	8000.377047	11.493120	-0.053635	4.815659
259.726704	8000.334022	11.498125	-0.053643	4.815646
259.815562	8000.349362	11.503130	-0.053660	4.815650
259.498021	8000.375150	11.508135	-0.053601	4.815659
259.551446	8000.364279	11.513139	-0.053611	4.815656
259.652841	8000.397980	11.518144	-0.053630	4.815665
259.600771	8000.310624	11.523149	-0.053620	4.815640
259.487697	8000.354705	11.528154	-0.053599	4.815653
259.586232	8000.329618	11.533159	-0.053617	4.815646
259.639934	8000.344384	11.538163	-0.053627	4.815650
259.673966	8000.342808	11.543168	-0.053634	4.815649
259.515383	8000.282548	11.548173	-0.053604	4.815632
259.788513	8000.322259	11.553178	-0.053655	4.815642
259.550873	8000.319448	11.558183	-0.053611	4.815643
259.565174	8000.341046	11.563187	-0.053614	4.815649
259.507327	8000.384961	11.568192	-0.053603	4.815662
259.593703	8000.413077	11.573197	-0.053619	4.815670
259.574402	8000.431990	11.578202	-0.053616	4.815675
259.682372	8000.376085	11.583207	-0.053636	4.815659
259.773326	8000.361555	11.588211	-0.053653	4.815654
259.870282	8000.338579	11.593216	-0.053671	4.815647
259.667000	8000.332057	11.598221	-0.053633	4.815646
259.859119	8000.373649	11.603226	-0.053669	4.815657
259.535859	8000.349147	11.608231	-0.053609	4.815651
259.504100	8000.334748	11.613235	-0.053603	4.815647
259.715282	8000.356358	11.618240	-0.053642	4.815653
259.360317	8000.318523	11.623245	-0.053576	4.815643
259.506972	8000.340146	11.628250	-0.053604	4.815649
259.540772	8000.315070	11.633255	-0.053610	4.815641
259.620891	8000.289683	11.638259	-0.053625	4.815634
259.567063	8000.367840	11.643264	-0.053615	4.815657
259.596090	8000.306374	11.648269	-0.053620	4.815639
259.976897	8000.353184	11.653274	-0.053691	4.815651
259.873946	8000.326941	11.658279	-0.053672	4.815643
259.712571	8000.270908	11.663283	-0.053642	4.815628
259.651685	8000.352154	11.668288	-0.053631	4.815652
259.672210	8000.347154	11.673293	-0.053635	4.815650
259.764679	8000.371097	11.678298	-0.053652	4.815657
259.679837	8000.343014	11.683303	-0.053636	4.815649
259.765967	8000.292092	11.688307	-0.053652	4.815634
259.608799	8000.388854	11.693312	-0.053623	4.815663
259.554334	8000.342043	11.698317	-0.053613	4.815649
259.801470	8000.361037	11.703322	-0.053659	4.815654
259.823514	8000.333633	11.708327	-0.053663	4.815646
259.739888	8000.272462	11.713331	-0.053648	4.815628
259.698589	8000.378592	11.718336	-0.053640	4.815659
259.866000	8000.316183	11.723341	-0.053671	4.815640
259.756260	8000.335754	11.728346	-0.053651	4.815646
259.646456	8000.328624	11.733351	-0.053630	4.815645
259.560188	8000.296246	11.738355	-0.053614	4.815636
259.663600	8000.382313	11.743360	-0.053634	4.815660
259.697991	8000.338022	11.748365	-0.053640	4.815647
259.812238	8000.345232	11.753370	-0.053662	4.815649
259.728279	8000.326776	11.758375	-0.053646	4.815644
259.771812	8000.275159	11.763379	-0.053654	4.815629
259.876549	8000.319595	11.768384	-0.053674	4.815641
259.830198	8000.304957	11.773389	-0.053665	4.815637
259.759468	8000.354002	11.778394	-0.053652	4.815652
259.455617	8000.338362	11.783399	-0.053595	4.815649
259.682330	8000.301485	11.788403	-0.053638	4.815637
259.847668	8000.367203	11.793408	-0.053668	4.815655
259.766171	8000.348787	11.798413	-0.053653	4.815650
259.846613	8000.366126	11.803418	-0.053668	4.815655
259.720589	8000.352322	11.808423	-0.053645	4.815651
259.712998	8000.363951	11.813427	-0.053644	4.815655
259.790288	8000.360945	11.818432	-0.053658	4.815654
259.711722	8000.373550	11.823437	-0.053643	4.815658
259.886524	8000.414859	11.828442	-0.053676	4.815669
259.664519	8000.383467	11.833447	-0.053635	4.815661
259.820800	8000.357188	11.838451	-0.053664	4.815652
259.755194	8000.394568	11.843456	-0.053652	4.815664
259.464920	8000.384489	11.848461	-0.053598	4.815662
259.702535	8000.406532	11.853466	-0.053642	4.815667
259.647588	8000.392822	11.858471	-0.053632	4.815664
259.658899	8000.340678	11.863475	-0.053634	4.815648
259.697706	8000.411805	11.868480	-0.053641	4.815669
259.692409	8000.381818	11.873485	-0.053640	4.815660
259.704211	8000.421531	11.878490	-0.053643	4.815672
259.671118	8000.361185	11.883495	-0.053636	4.815654
259.728031	8000.349303	11.888499	-0.053647	4.815651
259.849493	8000.405761	11.893504	-0.053670	4.815666
259.601377	8000.289569	11.898509	-0.053624	4.815634
259.612464	8000.316454	11.903514	-0.053626	4.815641
259.657932	8000.348174	11.908519	-0.053634	4.815651
259.720103	8000.316085	11.913523	-0.053646	4.815641
259.683119	8000.364613	11.918528	-0.053639	4.815655
259.777811	8000.359756	11.923533	-0.053657	4.815653
259.719619	8000.352401	11.928538	-0.053646	4.815651
259.547010	8000.339973	11.933543	-0.053614	4.815649
259.592553	8000.327905	11.938547	-0.053622	4.815645
259.824413	8000.392574	11.943552	-0.053666	4.815663
259.645797	8000.307422	11.948557	-0.053632	4.815639
259.695865	8000.319992	11.953562	-0.053642	4.815642
259.757714	8000.364795	11.958567	-0.053653	4.815655
259.786764	8000.274493	11.963571	-0.053659	4.815628
259.688049	8000.355121	11.968576	-0.053640	4.815652
259.711935	8000.310659	11.973581	-0.053645	4.815639
259.761771	8000.299729	11.978586	-0.053654	4.815636
259.806906	8000.344259	11.983591	-0.053663	4.815649
259.755727	8000.339154	11.988595	-0.053653	4.815647
259.847059	8000.358807	11.993600	-0.053670	4.815653
259.809655	8000.310139	11.998605	-0.053663	4.815639
259.783577	8000.319329	12.003610	-0.053658	4.815641
259.680756	8000.300565	12.008615	-0.053639	4.815636
259.731363	8000.293919	12.013619	-0.053649	4.815634
259.866451	8000.379436	12.018624	-0.053674	4.815659
259.867081	8000.295077	12.023629	-0.053674	4.815634
259.948398	8000.354082	12.028634	-0.053689	4.815651
259.921298	8000.318399	12.033639	-0.053684	4.815641
259.800783	8000.257693	12.038643	-0.053662	4.815623
259.844593	8000.254140	12.043648	-0.053670	4.815622
259.681913	8000.241875	12.048653	-0.053640	4.815619
259.862172	8000.318516	12.053658	-0.053673	4.815641
259.846991	8000.342837	12.058663	-0.053671	4.815648
259.719040	8000.310846	12.063667	-0.053647	4.815639
259.726778	8000.381465	12.068672	-0.053648	4.815660
259.701253	8000.314835	12.073677	-0.053644	4.815641
259.906414	8000.357708	12.078682	-0.053682	4.815652
259.766412	8000.295615	12.083687	-0.053656	4.815635
259.817715	8000.322090	12.088691	-0.053666	4.815642
259.904417	8000.347007	12.093696	-0.053682	4.815649
259.816214	8000.276148	12.098701	-0.053665	4.815629
259.916195	8000.347207	12.103706	-0.053684	4.815649
259.691604	8000.313637	12.108711	-0.053642	4.815640
259.805899	8000.299488	12.113715	-0.053664	4.815636
259.905913	8000.360935	12.118720	-0.053682	4.815653
259.826059	8000.299825	12.123725	-0.053667	4.815636
259.968539	8000.332062	12.128730	-0.053694	4.815644
259.831430	8000.341573	12.133735	-0.053668	4.815648
259.620614	8000.242012	12.138739	-0.053629	4.815620
259.847309	8000.359997	12.143744	-0.053672	4.815653
259.770210	8000.312817	12.148749	-0.053657	4.815640
259.901623	8000.340600	12.153754	-0.053682	4.815647
260.052212	8000.383650	12.158759	-0.053710	4.815659
259.858889	8000.391175	12.163763	-0.053674	4.815662
260.051565	8000.430640	12.168768	-0.053710	4.815673
260.022185	8000.342586	12.173773	-0.053704	4.815647
259.956074	8000.322285	12.178778	-0.053692	4.815641
259.833909	8000.298933	12.183783	-0.053669	4.815635
259.800599	8000.278100	12.188787	-0.053663	4.815629
259.942734	8000.318875	12.193792	-0.053690	4.815641
259.855815	8000.330275	12.198797	-0.053674	4.815644
259.968071	8000.374834	12.203802	-0.053695	4.815657
259.998966	8000.348642	12.208807	-0.053700	4.815649
259.969751	8000.348169	12.213811	-0.053695	4.815649
259.874752	8000.347688	12.218816	-0.053677	4.815649
259.738340	8000.330511	12.223821	-0.053652	4.815645
259.949672	8000.309404	12.228826	-0.053691	4.815638
259.768130	8000.319258	12.233831	-0.053658	4.815641
259.790496	8000.297199	12.238835	-0.053662	4.815635
259.998149	8000.376425	12.243840	-0.053701	4.815657
259.853534	8000.337753	12.248845	-0.053674	4.815646
260.005915	8000.370152	12.253850	-0.053702	4.815655
259.717464	8000.340878	12.258855	-0.053648	4.815648
260.108150	8000.229783	12.263859	-0.053721	4.815614
260.101558	8000.337550	12.268864	-0.053720	4.815645
260.018340	8000.279589	12.273869	-0.053705	4.815629
260.023466	8000.348030	12.278874	-0.053706	4.815649
259.877907	8000.361676	12.283879	-0.053679	4.815653
259.746509	8000.303996	12.288883	-0.053654	4.815637
259.852825	8000.338845	12.293888	-0.053674	4.815647
259.946997	8000.280579	12.298893	-0.053691	4.815629
259.827186	8000.258333	12.303898	-0.053669	4.815623
259.679082	8000.273006	12.308903	-0.053642	4.815628
259.899370	8000.327873	12.313907	-0.053683	4.815643
259.949685	8000.322291	12.318912	-0.053692	4.815641
259.872612	8000.327444	12.323917	-0.053678	4.815643
260.062320	8000.331616	12.328922	-0.053713	4.815644
259.890935	8000.388628	12.333927	-0.053681	4.815661
259.792246	8000.372067	12.338931	-0.053663	4.815657
259.956637	8000.364077	12.343936	-0.053694	4.815654
259.872761	8000.322126	12.348941	-0.053678	4.815642
259.985304	8000.351737	12.353946	-0.053699	4.815650
259.897824	8000.373808	12.358951	-0.053683	4.815657
260.124103	8000.341197	12.363955	-0.053725	4.815646
260.167221	8000.325885	12.368960	-0.053733	4.815641
259.965702	8000.294828	12.373965	-0.053696	4.815633
259.963313	8000.369554	12.378970	-0.053695	4.815655
260.049614	8000.344268	12.383975	-0.053711	4.815647
260.039781	8000.270418	12.388979	-0.053710	4.815626
259.939827	8000.345686	12.393984	-0.053691	4.815648
259.787480	8000.285528	12.398989	-0.053663	4.815631
259.911685	8000.276881	12.403994	-0.053686	4.815628
259.875857	8000.376693	12.408999	-0.053679	4.815658
259.958626	8000.350281	12.414003	-0.053695	4.815650
259.943981	8000.416263	12.419008	-0.053692	4.815669
259.869389	8000.341354	12.424013	-0.053678	4.815647
260.088108	8000.410082	12.429018	-0.053719	4.815666
260.040095	8000.391145	12.434023	-0.053710	4.815661
260.005270	8000.376695	12.439027	-0.053704	4.815657
259.919474	8000.411610	12.444032	-0.053688	4.815668
260.098265	8000.331230	12.449037	-0.053721	4.815643
260.022128	8000.278724	12.454042	-0.053707	4.815628
259.855634	8000.330477	12.459047	-0.053676	4.815644
260.010792	8000.310588	12.464051	-0.053705	4.815638
260.001884	8000.391616	12.469056	-0.053703	4.815661
259.762784	8000.379169	12.474061	-0.053659	4.815659
259.772082	8000.363304	12.479066	-0.053661	4.815654
259.762294	8000.351400	12.484071	-0.053659	4.815651
259.747030	8000.331930	12.489075	-0.053656	4.815645
259.752328	8000.366197	12.494080	-0.053657	4.815655
259.798642	8000.358414	12.499085	-0.053666	4.815653
259.970630	8000.395405	12.504090	-0.053698	4.815663
259.765294	8000.377101	12.509095	-0.053660	4.815658
259.800272	8000.284759	12.514099	-0.053666	4.815631
259.923991	8000.370090	12.519104	-0.053689	4.815656
259.849788	8000.303732	12.524109	-0.053675	4.815636
259.845239	8000.336770	12.529114	-0.053675	4.815646
260.038922	8000.305762	12.534119	-0.053711	4.815636
259.772184	8000.300340	12.539123	-0.053661	4.815636
259.911535	8000.410491	12.544128	-0.053687	4.815667
259.793105	8000.345547	12.549133	-0.053665	4.815649
260.014268	8000.374797	12.554138	-0.053706	4.815656
260.018955	8000.321476	12.559143	-0.053707	4.815641
259.899664	8000.307783	12.564147	-0.053685	4.815637
259.877376	8000.326647	12.569152	-0.053681	4.815643
259.826201	8000.298046	12.574157	-0.053671	4.815635
259.890352	8000.329003	12.579162	-0.053683	4.815644
259.854700	8000.341240	12.584167	-0.053677	4.815647
260.002366	8000.313753	12.589171	-0.053704	4.815639
260.101860	8000.381600	12.594176	-0.053723	4.815658
260.038649	8000.363483	12.599181	-0.053711	4.815653
260.055256	8000.362690	12.604186	-0.053714	4.815653
259.898893	8000.349458	12.609191	-0.053685	4.815650
259.846175	8000.327241	12.614195	-0.053676	4.815643
260.060236	8000.409776	12.619200	-0.053716	4.815666
260.104154	8000.330396	12.624205	-0.053724	4.815643
259.883527	8000.339611	12.629210	-0.053683	4.815647
260.045024	8000.274968	12.634215	-0.053713	4.815627
260.083046	8000.331131	12.639219	-0.053720	4.815643
260.039112	8000.396634	12.644224	-0.053712	4.815663
259.967252	8000.371967	12.649229	-0.053698	4.815656
259.985480	8000.342365	12.654234	-0.053702	4.815647
259.781233	8000.387092	12.659239	-0.053664	4.815661
259.699328	8000.357989	12.664243	-0.053649	4.815653
259.987896	8000.388341	12.669248	-0.053702	4.815660
259.862374	8000.321144	12.674253	-0.053679	4.815641
260.018909	8000.371767	12.679258	-0.053708	4.815656
260.038742	8000.355007	12.684263	-0.053712	4.815651
260.208066	8000.330009	12.689267	-0.053744	4.815642
260.101406	8000.397692	12.694272	-0.053724	4.815663
259.984476	8000.360540	12.699277	-0.053702	4.815652
260.033286	8000.365614	12.704282	-0.053711	4.815654
259.982089	8000.395754	12.709287	-0.053702	4.815663
259.918837	8000.381908	12.714291	-0.053690	4.815659
260.099241	8000.394472	12.719296	-0.053724	4.815662
259.869122	8000.308478	12.724301	-0.053681	4.815638
259.914019	8000.369025	12.729306	-0.053689	4.815655
259.988947	8000.404430	12.734311	-0.053703	4.815665
260.015161	8000.361073	12.739315	-0.053708	4.815652
260.130579	8000.407820	12.744320	-0.053730	4.815665
259.675736	8000.365147	12.749325	-0.053645	4.815655
259.789317	8000.360599	12.754330	-0.053666	4.815653
259.897467	8000.395478	12.759335	-0.053686	4.815663
259.867810	8000.378977	12.764339	-0.053681	4.815658
260.131453	8000.359793	12.769344	-0.053730	4.815651
260.009513	8000.369553	12.774349	-0.053707	4.815655
259.996716	8000.341579	12.779354	-0.053705	4.815647
259.949941	8000.387811	12.784359	-0.053696	4.815660
260.022935	8000.384736	12.789363	-0.053710	4.815659
260.017342	8000.409213	12.794368	-0.053709	4.815666
259.882097	8000.365354	12.799373	-0.053684	4.815654
259.958680	8000.392242	12.804378	-0.053698	4.815662
260.002483	8000.390826	12.809383	-0.053706	4.815661
259.739944	8000.360907	12.814387	-0.053658	4.815654
259.907041	8000.403158	12.819392	-0.053689	4.815665
259.865592	8000.372580	12.824397	-0.053681	4.815656
260.066340	8000.358776	12.829402	-0.053718	4.815651
260.114133	8000.362765	12.834407	-0.053727	4.815652
260.087908	8000.271559	12.839411	-0.053723	4.815626
260.228452	8000.362505	12.844416	-0.053749	4.815652
260.091928	8000.332510	12.849421	-0.053723	4.815644
260.179292	8000.347825	12.854426	-0.053740	4.815648
260.148824	8000.346263	12.859431	-0.053734	4.815647
260.082114	8000.339837	12.864435	-0.053722	4.815646
260.280920	8000.409308	12.869440	-0.053759	4.815665
260.079049	8000.373972	12.874445	-0.053721	4.815656
259.861670	8000.428097	12.879450	-0.053681	4.815673
259.914720	8000.389451	12.884455	-0.053691	4.815661
259.950335	8000.332363	12.889459	-0.053697	4.815644
260.098678	8000.380717	12.894464	-0.053725	4.815658
259.935126	8000.355619	12.899469	-0.053695	4.815651
260.042853	8000.339227	12.904474	-0.053715	4.815646
260.152418	8000.329273	12.909479	-0.053735	4.815642
259.982788	8000.348934	12.914483	-0.053704	4.815649
260.088532	8000.427564	12.919488	-0.053723	4.815671
260.095850	8000.386034	12.924493	-0.053725	4.815659
260.015151	8000.371903	12.929498	-0.053710	4.815656
259.918468	8000.388483	12.934503	-0.053692	4.815661
260.072432	8000.350418	12.939507	-0.053721	4.815649
260.143150	8000.361190	12.944512	-0.053734	4.815652
259.961680	8000.365705	12.949517	-0.053700	4.815654
260.225083	8000.399918	12.954522	-0.053749	4.815663
260.280735	8000.411512	12.959527	-0.053760	4.815666
259.916077	8000.380992	12.964531	-0.053692	4.815659
259.921240	8000.408849	12.969536	-0.053693	4.815667
260.066840	8000.365307	12.974541	-0.053720	4.815653
260.057167	8000.320296	12.979546	-0.053718	4.815640
259.979900	8000.380982	12.984551	-0.053704	4.815658
260.162764	8000.349798	12.989555	-0.053738	4.815648
260.275199	8000.387952	12.994560	-0.053759	4.815659
259.974461	8000.351001	12.999565	-0.053703	4.815650
260.009361	8000.370799	13.004570	-0.053709	4.815655
260.192026	8000.403693	13.009575	-0.053744	4.815664
259.883339	8000.369816	13.014579	-0.053686	4.815656
260.173382	8000.413009	13.019584	-0.053740	4.815667
260.332125	8000.364342	13.024589	-0.053770	4.815652
260.201315	8000.355800	13.029594	-0.053745	4.815650
260.066531	8000.397390	13.034599	-0.053720	4.815663
260.008256	8000.406054	13.039603	-0.053710	4.815665
260.074367	8000.348397	13.044608	-0.053722	4.815648
259.905183	8000.323208	13.049613	-0.053690	4.815642
259.984299	8000.344797	13.054618	-0.053705	4.815648
260.277339	8000.362406	13.059623	-0.053760	4.815651
260.212751	8000.370966	13.064627	-0.053748	4.815654
260.078614	8000.369846	13.069632	-0.053723	4.815655
260.156211	8000.346554	13.074637	-0.053737	4.815647
260.173521	8000.346841	13.079642	-0.053741	4.815647
260.049946	8000.382206	13.084647	-0.053718	4.815658
259.945212	8000.348458	13.089651	-0.053698	4.815649
260.116467	8000.370485	13.094656	-0.053730	4.815655
260.162732	8000.354156	13.099661	-0.053739	4.815650
260.093721	8000.384005	13.104666	-0.053726	4.815659
260.244856	8000.390751	13.109671	-0.053754	4.815660
260.083340	8000.337918	13.114675	-0.053724	4.815645
260.039522	8000.385267	13.119680	-0.053716	4.815659
259.933217	8000.366446	13.124685	-0.053696	4.815654
260.034593	8000.390535	13.129690	-0.053715	4.815661
260.001000	8000.391058	13.134695	-0.053709	4.815661
259.741200	8000.312055	13.139699	-0.053661	4.815639
260.115563	8000.411094	13.144704	-0.053731	4.815666
260.036416	8000.379900	13.149709	-0.053716	4.815658
260.015023	8000.390235	13.154714	-0.053712	4.815661
260.032079	8000.410810	13.159719	-0.053715	4.815667
260.031864	8000.403334	13.164723	-0.053715	4.815665
260.014868	8000.369952	13.169728	-0.053712	4.815655
260.042332	8000.321275	13.174733	-0.053717	4.815641
260.313216	8000.343862	13.179738	-0.053768	4.815646
260.092301	8000.368025	13.184743	-0.053727	4.815654
260.080724	8000.418037	13.189747	-0.053724	4.815669
260.210520	8000.443659	13.194752	-0.053749	4.815675
260.045070	8000.384353	13.199757	-0.053718	4.815659
260.128138	8000.347266	13.204762	-0.053733	4.815648
260.083018	8000.399934	13.209767	-0.053725	4.815663
259.971197	8000.355389	13.214771	-0.053704	4.815651
260.119585	8000.375974	13.219776	-0.053732	4.815656
259.976882	8000.314905	13.224781	-0.053705	4.815639
260.264634	8000.361264	13.229786	-0.053759	4.815651
260.272143	8000.392364	13.234791	-0.053760	4.815660
260.128777	8000.340895	13.239795	-0.053734	4.815646
260.324844	8000.392165	13.244800	-0.053770	4.815660
259.998635	8000.394314	13.249805	-0.053710	4.815662
259.857208	8000.365306	13.254810	-0.053683	4.815654
259.916325	8000.389773	13.259815	-0.053694	4.815661
259.996138	8000.332340	13.264819	-0.053709	4.815644
260.050738	8000.382365	13.269824	-0.053720	4.815658
259.922910	8000.322607	13.274829	-0.053696	4.815641
260.191441	8000.336611	13.279834	-0.053746	4.815644
260.192469	8000.408190	13.284839	-0.053746	4.815665
259.993678	8000.368632	13.289843	-0.053709	4.815655
260.099968	8000.403482	13.294848	-0.053729	4.815664
260.190311	8000.391078	13.299853	-0.053746	4.815660
260.123074	8000.400663	13.304858	-0.053733	4.815663
260.194297	8000.401831	13.309863	-0.053747	4.815663
260.102191	8000.420622	13.314867	-0.053730	4.815669
260.099308	8000.397082	13.319872	-0.053729	4.815662
260.217304	8000.358430	13.324877	-0.053751	4.815651
260.217373	8000.381931	13.329882	-0.053751	4.815657
260.119130	8000.387806	13.334887	-0.053733	4.815660
260.097766	8000.382121	13.339891	-0.053729	4.815658
260.277860	8000.401088	13.344896	-0.053763	4.815663
260.098369	8000.378934	13.349901	-0.053729	4.815657
260.035330	8000.371500	13.354906	-0.053717	4.815655
260.210316	8000.390384	13.359911	-0.053750	4.815660
260.319877	8000.351593	13.364915	-0.053771	4.815648
260.141183	8000.430915	13.369920	-0.053737	4.815672
260.233394	8000.386501	13.374925	-0.053755	4.815659
260.324643	8000.369840	13.379930	-0.053772	4.815653
260.468163	8000.396754	13.384935	-0.053798	4.815660
260.068764	8000.381686	13.389939	-0.053724	4.815658
260.151548	8000.433240	13.394944	-0.053739	4.815673
260.156711	8000.378859	13.399949	-0.053740	4.815657
259.899602	8000.331940	13.404954	-0.053693	4.815644
260.020300	8000.352073	13.409959	-0.053715	4.815650
260.077287	8000.288927	13.414963	-0.053726	4.815631
260.081107	8000.386184	13.419968	-0.053727	4.815659
259.884356	8000.400061	13.424973	-0.053690	4.815664
260.073656	8000.371117	13.429978	-0.053725	4.815655
260.119630	8000.385757	13.434983	-0.053734	4.815659
259.904773	8000.370501	13.439987	-0.053694	4.815656
260.166212	8000.374778	13.444992	-0.053743	4.815656
260.105164	8000.322519	13.449997	-0.053731	4.815641
260.072173	8000.345480	13.455002	-0.053725	4.815647
260.042868	8000.348209	13.460007	-0.053720	4.815648
260.173293	8000.358889	13.465011	-0.053744	4.815651
260.271271	8000.358358	13.470016	-0.053762	4.815650
260.129204	8000.317591	13.475021	-0.053736	4.815639
260.218690	8000.325466	13.480026	-0.053753	4.815641
260.340807	8000.411840	13.485031	-0.053776	4.815665
260.102845	8000.366301	13.490035	-0.053731	4.815653
260.015529	8000.378763	13.495040	-0.053715	4.815657
260.082647	8000.340347	13.500045	-0.053728	4.815646
260.042467	8000.388823	13.505050	-0.053720	4.815660
260.088620	8000.389581	13.510055	-0.053729	4.815660
260.201302	8000.342297	13.515059	-0.053750	4.815646
260.361352	8000.399387	13.520064	-0.053780	4.815662
260.191576	8000.378459	13.525069	-0.053748	4.815656
260.083909	8000.367092	13.530074	-0.053728	4.815654
260.046562	8000.384642	13.535079	-0.053721	4.815659
259.906373	8000.346042	13.540083	-0.053695	4.815648
260.076651	8000.340284	13.545088	-0.053727	4.815646
260.201548	8000.328445	13.550093	-0.053750	4.815642
260.227320	8000.298965	13.555098	-0.053755	4.815633
260.133960	8000.316668	13.560103	-0.053738	4.815639
260.219416	8000.315932	13.565107	-0.053754	4.815638
260.132991	8000.305980	13.570112	-0.053738	4.815636
259.839941	8000.340712	13.575117	-0.053683	4.815647
260.105103	8000.314076	13.580122	-0.053732	4.815638
260.435051	8000.348309	13.585127	-0.053794	4.815646
260.144021	8000.322196	13.590131	-0.053740	4.815640
260.289247	8000.377975	13.595136	-0.053767	4.815656
260.218386	8000.314875	13.600141	-0.053754	4.815638
260.247489	8000.284382	13.605146	-0.053759	4.815629
260.216055	8000.363974	13.610151	-0.053753	4.815652
260.130925	8000.313458	13.615155	-0.053738	4.815638
260.340401	8000.403395	13.620160	-0.053777	4.815663
260.214272	8000.374637	13.625165	-0.053753	4.815655
260.145205	8000.398077	13.630170	-0.053740	4.815662
260.170064	8000.382467	13.635175	-0.053745	4.815658
260.072452	8000.334950	13.640179	-0.053727	4.815644
260.061444	8000.387108	13.645184	-0.053725	4.815660
260.088178	8000.344827	13.650189	-0.053730	4.815647
260.076945	8000.319015	13.655194	-0.053728	4.815640
259.938441	8000.353069	13.660199	-0.053702	4.815650
260.222652	8000.325676	13.665203	-0.053755	4.815641
260.246812	8000.367728	13.670208	-0.053760	4.815653
260.075479	8000.327551	13.675213	-0.053728	4.815642
259.946465	8000.344671	13.680218	-0.053704	4.815648
260.086897	8000.348038	13.685223	-0.053730	4.815648
260.162013	8000.322569	13.690227	-0.053744	4.815640
260.011900	8000.372453	13.695232	-0.053716	4.815656
260.132025	8000.339175	13.700237	-0.053739	4.815645
260.250018	8000.368876	13.705242	-0.053761	4.815653
260.155992	8000.427153	13.710247	-0.053743	4.815671
260.259378	8000.386126	13.715251	-0.053762	4.815658
260.307485	8000.375167	13.720256	-0.053771	4.815655
260.187311	8000.366799	13.725261	-0.053749	4.815653
260.297328	8000.339764	13.730266	-0.053770	4.815645
260.508050	8000.380593	13.735271	-0.053809	4.815656
260.172702	8000.299286	13.740275	-0.053746	4.815633
260.313434	8000.396645	13.745280	-0.053773	4.815661
260.178765	8000.390176	13.750285	-0.053748	4.815660
260.237175	8000.309964	13.755290	-0.053759	4.815636
260.132865	8000.379821	13.760295	-0.053739	4.815657
259.886710	8000.376871	13.765299	-0.053693	4.815657
260.238240	8000.397572	13.770304	-0.053759	4.815662
260.039779	8000.383652	13.775309	-0.053722	4.815659
260.012517	8000.371462	13.780314	-0.053717	4.815655
260.148451	8000.387572	13.785319	-0.053742	4.815659
260.167060	8000.316322	13.790323	-0.053746	4.815638
260.066055	8000.370213	13.795328	-0.053727	4.815655
260.021114	8000.341714	13.800333	-0.053719	4.815646
260.310946	8000.310141	13.805338	-0.053773	4.815636
260.297985	8000.351586	13.810343	-0.053770	4.815648
260.127655	8000.264433	13.815347	-0.053739	4.815623
260.267702	8000.362848	13.820352	-0.053765	4.815651
260.197930	8000.332875	13.825357	-0.053752	4.815643
260.251774	8000.366867	13.830362	-0.053762	4.815653
260.124995	8000.411793	13.835367	-0.053738	4.815666
260.268293	8000.352193	13.840371	-0.053765	4.815648
260.160944	8000.347238	13.845376	-0.053745	4.815647
260.212064	8000.336329	13.850381	-0.053755	4.815644
260.492638	8000.382572	13.855386	-0.053807	4.815656
260.328363	8000.436497	13.860391	-0.053777	4.815673
259.963335	8000.354705	13.865395	-0.053709	4.815651
260.308180	8000.338984	13.870400	-0.053773	4.815644
260.290511	8000.348311	13.875405	-0.053770	4.815647
260.103819	8000.310019	13.880410	-0.053735	4.815637
260.245988	8000.386041	13.885415	-0.053761	4.815658
260.338824	8000.327752	13.890419	-0.053779	4.815641
260.062064	8000.371294	13.895424	-0.053727	4.815655
260.021165	8000.370630	13.900429	-0.053720	4.815655
260.090660	8000.356817	13.905434	-0.053733	4.815651
260.014265	8000.422859	13.910439	-0.053719	4.815670
260.070069	8000.338332	13.915443	-0.053729	4.815645
260.176449	8000.362503	13.920448	-0.053749	4.815652
260.217782	8000.408040	13.925453	-0.053757	4.815665
260.139516	8000.409969	13.930458	-0.053742	4.815666
260.191534	8000.434320	13.935463	-0.053752	4.815673
260.342822	8000.382327	13.940467	-0.053780	4.815657
260.374200	8000.367891	13.945472	-0.053786	4.815652
260.309466	8000.343340	13.950477	-0.053774	4.815646
260.318001	8000.358436	13.955482	-0.053775	4.815650
260.364712	8000.409401	13.960487	-0.053784	4.815665
260.251749	8000.376586	13.965491	-0.053763	4.815656
260.380629	8000.409669	13.970496	-0.053787	4.815665
260.205059	8000.397191	13.975501	-0.053755	4.815662
260.190429	8000.414045	13.980506	-0.053752	4.815667
260.364295	8000.415822	13.985511	-0.053784	4.815666
260.251190	8000.341351	13.990515	-0.053763	4.815645
260.349052	8000.366451	13.995520	-0.053782	4.815652
260.186222	8000.352046	14.000525	-0.053751	4.815649
260.249901	8000.368043	14.005530	-0.053763	4.815653
260.187083	8000.387313	14.010535	-0.053752	4.815659
260.126245	8000.350009	14.015539	-0.053740	4.815648
260.208685	8000.365245	14.020544	-0.053756	4.815652
260.299897	8000.366740	14.025549	-0.053773	4.815652
260.200351	8000.333076	14.030554	-0.053754	4.815643
260.290582	8000.419997	14.035559	-0.053771	4.815668
260.362951	8000.363510	14.040563	-0.053785	4.815651
260.312243	8000.380842	14.045568	-0.053775	4.815656
260.147059	8000.380282	14.050573	-0.053744	4.815657
260.173999	8000.339073	14.055578	-0.053750	4.815645
260.386237	8000.373519	14.060583	-0.053789	4.815654
260.300549	8000.317652	14.065587	-0.053773	4.815638
260.211938	8000.370678	14.070592	-0.053757	4.815654
260.325328	8000.368263	14.075597	-0.053778	4.815653
260.287767	8000.342020	14.080602	-0.053771	4.815645
260.330807	8000.423898	14.085607	-0.053779	4.815669
260.305289	8000.370083	14.090611	-0.053774	4.815653
260.162713	8000.407274	14.095616	-0.053748	4.815665
260.149216	8000.414534	14.100621	-0.053745	4.815667
260.088105	8000.372954	14.105626	-0.053734	4.815655
260.348634	8000.419937	14.110631	-0.053783	4.815668
260.198629	8000.393992	14.115635	-0.053755	4.815661
260.136545	8000.435703	14.120640	-0.053743	4.815673
260.267396	8000.391920	14.125645	-0.053768	4.815660
260.178430	8000.344545	14.130650	-0.053751	4.815646
260.190741	8000.358634	14.135655	-0.053753	4.815651
260.211913	8000.303447	14.140659	-0.053757	4.815634
260.459951	8000.416444	14.145664	-0.053804	4.815666
260.224754	8000.374154	14.150669	-0.053760	4.815655
260.202627	8000.399429	14.155674	-0.053756	4.815662
260.335286	8000.408010	14.160679	-0.053781	4.815664
260.159526	8000.382712	14.165683	-0.053748	4.815658
260.281572	8000.444521	14.170688	-0.053771	4.815675
260.348144	8000.390075	14.175693	-0.053783	4.815659
260.174577	8000.359474	14.180698	-0.053751	4.815651
260.127664	8000.392888	14.185703	-0.053742	4.815661
260.196444	8000.373723	14.190707	-0.053755	4.815655
260.414909	8000.365549	14.195712	-0.053796	4.815651
260.254006	8000.376808	14.200717	-0.053766	4.815656
260.160526	8000.376352	14.205722	-0.053748	4.815656
260.404649	8000.402775	14.210727	-0.053794	4.815662
260.387050	8000.302096	14.215731	-0.053791	4.815633
260.274043	8000.401716	14.220736	-0.053770	4.815663
260.175167	8000.393696	14.225741	-0.053751	4.815661
260.435386	8000.319986	14.230746	-0.053800	4.815638
260.513032	8000.380001	14.235751	-0.053814	4.815655
260.228424	8000.345448	14.240755	-0.053761	4.815646
260.284618	8000.389092	14.245760	-0.053772	4.815659
260.165930	8000.367932	14.250765	-0.053750	4.815653
260.186373	8000.363998	14.255770	-0.053754	4.815652
260.217414	8000.415774	14.260775	-0.053760	4.815667
260.309820	8000.338254	14.265779	-0.053777	4.815644
260.467336	8000.370738	14.270784	-0.053806	4.815653
260.468079	8000.388910	14.275789	-0.053806	4.815658
260.451580	7999.352679	14.280794	-0.053803	4.815355

260.566178	7996.115706	14.285799	-0.053822	4.814408
260.425707	7990.603642	14.290803	-0.053792	4.812797
260.526943	7983.946024	14.295808	-0.053807	4.810849
260.186282	7976.624999	14.300813	-0.053739	4.808708
260.226004	7969.016943	14.305818	-0.053741	4.806480
260.408784	7961.224953	14.310823	-0.053770	4.804197
260.188177	7953.346340	14.315827	-0.053724	4.801888
260.291207	7945.382794	14.320832	-0.053738	4.799553
260.179851	7937.473113	14.325837	-0.053712	4.797233
260.201667	7929.396985	14.330842	-0.053711	4.794862
260.128342	7921.422325	14.335847	-0.053692	4.792521
259.856507	7913.352098	14.340851	-0.053636	4.790151
259.988967	7905.408457	14.345856	-0.053656	4.787815
260.092190	7897.411996	14.350861	-0.053670	4.785463
260.035908	7889.403467	14.355866	-0.053654	4.783107
260.060900	7881.445599	14.360871	-0.053654	4.780764
259.866601	7873.385926	14.365875	-0.053612	4.778391
259.749129	7865.479634	14.370880	-0.053585	4.776062
259.824953	7857.407176	14.375885	-0.053594	4.773682
259.860780	7849.384776	14.380890	-0.053596	4.771315
259.948556	7841.408247	14.385895	-0.053607	4.768961
259.743760	7833.361207	14.390899	-0.053564	4.766586
259.815874	7825.353315	14.395904	-0.053572	4.764220
259.773064	7817.402927	14.400909	-0.053559	4.761870
259.682668	7809.335600	14.405914	-0.053537	4.759485
259.772738	7801.422141	14.410919	-0.053548	4.757144
259.590402	7793.357619	14.415923	-0.053509	4.754757
259.510600	7785.309960	14.420928	-0.053489	4.752374
259.646688	7777.287702	14.425933	-0.053509	4.749997
259.445264	7769.302638	14.430938	-0.053467	4.747630
259.266502	7761.339771	14.435943	-0.053428	4.745269
259.179160	7753.335611	14.440947	-0.053407	4.742894
259.322659	7745.329439	14.445952	-0.053428	4.740517
259.203303	7737.362442	14.450957	-0.053401	4.738151
259.102932	7729.315646	14.455962	-0.053377	4.735759
259.326487	7721.348497	14.460967	-0.053414	4.733390
259.228410	7713.282567	14.465971	-0.053390	4.730991
259.173617	7705.297724	14.470976	-0.053375	4.728614
259.218614	7697.297909	14.475981	-0.053378	4.726232
259.220684	7689.294407	14.480986	-0.053373	4.723847
259.128251	7681.360105	14.485991	-0.053351	4.721482
258.996006	7673.288205	14.490995	-0.053321	4.719075
259.057306	7665.375837	14.496000	-0.053327	4.716714
259.207708	7657.306085	14.501005	-0.053350	4.714304
258.971363	7649.245734	14.506010	-0.053301	4.711897
258.859074	7641.265748	14.511015	-0.053275	4.709513
258.933321	7633.254710	14.516019	-0.053283	4.707117
258.861790	7625.291535	14.521024	-0.053265	4.704735
258.865436	7617.369459	14.526029	-0.053261	4.702364
258.931778	7609.258997	14.531034	-0.053268	4.699935
258.981022	7601.318231	14.536039	-0.053272	4.697556
258.872779	7593.289871	14.541043	-0.053246	4.695149
259.045078	7585.303867	14.546048	-0.053273	4.692754
258.815201	7577.251820	14.551053	-0.053225	4.690338
258.673532	7569.319934	14.556058	-0.053194	4.687957
258.555400	7561.265510	14.561063	-0.053167	4.685538
258.605695	7553.271272	14.566067	-0.053171	4.683135
258.702673	7545.292792	14.571072	-0.053184	4.680736
258.654326	7537.292729	14.576077	-0.053169	4.678329
258.703924	7529.280703	14.581082	-0.053174	4.675917
258.609960	7521.259682	14.586087	-0.053151	4.673502
258.526377	7513.169355	14.591091	-0.053130	4.671064
258.477303	7505.227349	14.596096	-0.053116	4.668670
258.658292	7497.228318	14.601101	-0.053144	4.666257
258.373024	7489.245989	14.606106	-0.053086	4.663848
258.419812	7481.273292	14.611111	-0.053090	4.661441
258.522985	7473.201590	14.616115	-0.053104	4.659002
258.547774	7465.263927	14.621120	-0.053103	4.656603
258.225938	7457.235326	14.626125	-0.053038	4.654175
258.286203	7449.177122	14.631130	-0.053044	4.651737
258.367950	7441.231443	14.636135	-0.053054	4.649331
258.012164	7433.209363	14.641139	-0.052983	4.646902
258.042073	7425.216247	14.646144	-0.052983	4.644480
257.925238	7417.247558	14.651149	-0.052956	4.642063
257.852850	7409.169990	14.656154	-0.052937	4.639613
258.050705	7401.269976	14.661159	-0.052969	4.637215
258.103971	7393.197996	14.666163	-0.052974	4.634764
258.115736	7385.216500	14.671168	-0.052971	4.632338
258.000436	7377.183587	14.676173	-0.052944	4.629896
258.155281	7369.206560	14.681178	-0.052968	4.627470
258.220346	7361.161796	14.686183	-0.052975	4.625022
257.923379	7353.206106	14.691187	-0.052914	4.622599
257.798942	7345.186153	14.696192	-0.052886	4.620156
257.937472	7337.184911	14.701197	-0.052907	4.617717
258.015828	7329.160213	14.706202	-0.052916	4.615270
257.874268	7321.219554	14.711207	-0.052885	4.612847
257.687919	7313.149218	14.716211	-0.052845	4.610383
257.906591	7305.147454	14.721216	-0.052880	4.607939
257.870745	7297.145946	14.726221	-0.052868	4.605493
257.696111	7289.164141	14.731226	-0.052831	4.603052
257.796657	7281.191454	14.736231	-0.052844	4.600613
257.463929	7273.168450	14.741235	-0.052777	4.598157
257.423846	7265.180018	14.746240	-0.052765	4.595710
257.427600	7257.151996	14.751245	-0.052760	4.593250
257.449617	7249.116033	14.756250	-0.052759	4.590786
257.235333	7241.144891	14.761255	-0.052714	4.588341
257.297886	7233.099176	14.766259	-0.052720	4.585871
257.317561	7225.133090	14.771264	-0.052719	4.583425
257.440370	7217.132388	14.776269	-0.052737	4.580967
257.284515	7209.151953	14.781274	-0.052702	4.578513
257.312613	7201.144871	14.786279	-0.052702	4.576050
257.222258	7193.118137	14.791283	-0.052680	4.573580
257.194761	7185.111788	14.796288	-0.052670	4.571114
257.110354	7177.122138	14.801293	-0.052649	4.568653
257.046984	7169.110431	14.806298	-0.052632	4.566183
257.162708	7161.142859	14.811303	-0.052649	4.563725
257.030178	7153.114833	14.816307	-0.052619	4.561248
257.153787	7145.132570	14.821312	-0.052637	4.558783
257.094377	7137.164508	14.826317	-0.052620	4.556322
256.947286	7129.105274	14.831322	-0.052588	4.553830
256.913796	7121.104452	14.836327	-0.052576	4.551356
256.947608	7113.096562	14.841331	-0.052578	4.548878
256.909595	7105.100469	14.846336	-0.052565	4.546402
256.918573	7097.114541	14.851341	-0.052562	4.543928
256.846574	7089.120339	14.856346	-0.052543	4.541450
257.013775	7081.116040	14.861351	-0.052569	4.538968
256.841035	7073.154347	14.866355	-0.052532	4.536498
256.926313	7065.128086	14.871360	-0.052543	4.534006
256.754500	7057.110894	14.876365	-0.052505	4.531515
256.738094	7049.056979	14.881370	-0.052497	4.529012
256.712835	7041.152120	14.886375	-0.052487	4.526554
256.797308	7033.071240	14.891379	-0.052498	4.524040
256.726944	7025.126283	14.896384	-0.052480	4.521566
256.537592	7017.120464	14.901389	-0.052439	4.519072
256.521063	7009.138857	14.906394	-0.052431	4.516584
256.514371	7001.101530	14.911399	-0.052425	4.514078
256.444621	6993.011166	14.916403	-0.052406	4.511553
256.575091	6984.999701	14.921408	-0.052425	4.509053
256.365997	6977.065442	14.926413	-0.052381	4.506574
256.272533	6969.028785	14.931418	-0.052359	4.504062
256.508089	6961.098558	14.936423	-0.052398	4.501583
256.218166	6953.038686	14.941427	-0.052338	4.499060
256.067667	6945.129730	14.946432	-0.052305	4.496584
256.343680	6937.092652	14.951437	-0.052351	4.494067
256.296767	6929.042157	14.956442	-0.052338	4.491544
256.190579	6921.055515	14.961447	-0.052313	4.489039
256.081216	6913.040586	14.966451	-0.052287	4.486524
256.123829	6905.040588	14.971456	-0.052290	4.484013
255.987030	6897.079712	14.976461	-0.052259	4.481512
256.012026	6889.038216	14.981466	-0.052259	4.478984
255.990801	6881.110930	14.986471	-0.052250	4.476491
255.863840	6873.026552	14.991475	-0.052221	4.473947
255.817244	6865.035161	14.996480	-0.052207	4.471431
255.808275	6857.027061	15.001485	-0.052200	4.468909
255.833696	6849.021117	15.006490	-0.052200	4.466385
256.058368	6841.004496	15.011495	-0.052236	4.463858
255.940307	6833.056753	15.016499	-0.052209	4.461350
255.885438	6825.033683	15.021504	-0.052194	4.458817
255.727065	6817.054019	15.026509	-0.052159	4.456295
255.863046	6809.010093	15.031514	-0.052179	4.453754
255.821878	6800.994673	15.036519	-0.052166	4.451218
255.769068	6793.004706	15.041523	-0.052151	4.448690
255.533204	6784.994101	15.046528	-0.052102	4.446153
255.702675	6777.044862	15.051533	-0.052129	4.443635
255.741488	6769.023056	15.056538	-0.052131	4.441093
255.619382	6761.048381	15.061543	-0.052103	4.438563
255.406109	6753.057932	15.066547	-0.052058	4.436026
255.426661	6744.991211	15.071552	-0.052057	4.433465
255.534236	6736.978998	15.076557	-0.052071	4.430920
255.422831	6728.955857	15.081562	-0.052046	4.428369
255.570799	6720.982663	15.086567	-0.052068	4.425833
255.492931	6712.966336	15.091571	-0.052048	4.423282
255.351589	6704.948765	15.096576	-0.052017	4.420728
255.591211	6696.986916	15.101581	-0.052056	4.418192
255.446545	6688.953230	15.106586	-0.052024	4.415630
255.487087	6680.998681	15.111591	-0.052026	4.413093
255.150896	6672.924588	15.116595	-0.051959	4.410514
255.247888	6665.001873	15.121600	-0.051972	4.407985
255.268251	6657.011660	15.126605	-0.051970	4.405432
255.011681	6649.011087	15.131610	-0.051917	4.402872
255.018188	6641.027505	15.136615	-0.051913	4.400318
255.034821	6633.024995	15.141619	-0.051911	4.397756
255.174937	6624.982182	15.146624	-0.051932	4.395181
255.075343	6616.975410	15.151629	-0.051908	4.392614
255.024434	6608.906339	15.156634	-0.051894	4.390027
254.950894	6600.993222	15.161639	-0.051875	4.387487
254.848915	6592.956902	15.166643	-0.051851	4.384907
254.879156	6584.981289	15.171648	-0.051851	4.382345
254.938342	6576.976798	15.176653	-0.051857	4.379772
254.733117	6569.037146	15.181658	-0.051814	4.377217
255.050102	6561.008186	15.186663	-0.051868	4.374635
254.992740	6553.023796	15.191667	-0.051852	4.372064
255.037378	6544.939526	15.196672	-0.051855	4.369460
254.873531	6536.996676	15.201677	-0.051819	4.366898
254.812240	6528.959828	15.206682	-0.051803	4.364305
254.702934	6521.033158	15.211687	-0.051777	4.361746
254.571075	6513.008226	15.216691	-0.051747	4.359154
254.685351	6505.057616	15.221696	-0.051764	4.356585
254.731055	6496.990441	15.226701	-0.051767	4.353977
254.442677	6488.841274	15.231706	-0.051708	4.351339
254.403072	6480.910943	15.236711	-0.051695	4.348771
254.382096	6472.904962	15.241715	-0.051686	4.346178
254.295737	6464.911877	15.246720	-0.051665	4.343587
254.270398	6456.955043	15.251725	-0.051655	4.341006
254.208560	6448.946986	15.256730	-0.051639	4.338407
254.360101	6441.008404	15.261735	-0.051662	4.335830
254.157741	6432.968771	15.266739	-0.051619	4.333217
254.239517	6424.917328	15.271744	-0.051629	4.330600
254.398663	6416.946745	15.276749	-0.051653	4.328008
254.232739	6408.916168	15.281754	-0.051617	4.325393
254.079142	6400.971704	15.286759	-0.051583	4.322805
254.107467	6392.989654	15.291763	-0.051584	4.320204
254.059277	6384.967247	15.296768	-0.051569	4.317588
253.995183	6376.974966	15.301773	-0.051552	4.314980
253.996209	6368.918168	15.306778	-0.051547	4.312349
254.054094	6360.918470	15.311783	-0.051553	4.309736
253.877348	6352.926262	15.316787	-0.051515	4.307123
253.600809	6344.897456	15.321792	-0.051458	4.304495
253.916597	6336.963460	15.326797	-0.051512	4.301901
253.764677	6328.929126	15.331802	-0.051478	4.299268
253.719820	6320.957188	15.336807	-0.051465	4.296656
253.814484	6312.936255	15.341811	-0.051477	4.294027
253.723190	6304.908622	15.346816	-0.051455	4.291393
253.632589	6296.929680	15.351821	-0.051433	4.288773
253.538030	6288.921551	15.356826	-0.051410	4.286141
253.856290	6280.917452	15.361831	-0.051464	4.283513
253.691200	6272.933296	15.366835	-0.051428	4.280886
253.654592	6264.925214	15.371840	-0.051416	4.278250
253.678947	6256.939469	15.376845	-0.051416	4.275621
253.448647	6248.896117	15.381850	-0.051368	4.272969
253.322443	6240.887315	15.386855	-0.051339	4.270327
253.244036	6232.904970	15.391859	-0.051319	4.267693
253.217401	6224.854358	15.396864	-0.051309	4.265036
253.247111	6216.963178	15.401869	-0.051310	4.262429
253.259570	6208.858207	15.406874	-0.051307	4.259751
253.468691	6200.980422	15.411879	-0.051341	4.257147
253.292797	6192.894404	15.416883	-0.051303	4.254470
253.200752	6184.894185	15.421888	-0.051280	4.251820
253.381971	6176.874451	15.426893	-0.051309	4.249164
253.228983	6168.898197	15.431898	-0.051275	4.246518
253.027821	6160.875658	15.436903	-0.051233	4.243855
252.953832	6152.941134	15.441907	-0.051214	4.241220
253.196469	6144.888846	15.446912	-0.051254	4.238548
253.081109	6137.007711	15.451917	-0.051227	4.235927
252.903536	6128.929673	15.456922	-0.051189	4.233239
252.932730	6120.946478	15.461927	-0.051189	4.230582
253.003172	6112.899604	15.466931	-0.051197	4.227903
252.930065	6104.885463	15.471936	-0.051178	4.225232
252.747150	6096.948957	15.476941	-0.051139	4.222584
252.848853	6088.915454	15.481946	-0.051153	4.219905
252.833655	6080.980284	15.486951	-0.051145	4.217256
252.752164	6072.936275	15.491955	-0.051124	4.214568
252.693230	6064.936897	15.496960	-0.051108	4.211893
252.712200	6056.925314	15.501965	-0.051107	4.209213
252.625468	6048.956597	15.506970	-0.051085	4.206545
252.619799	6040.948525	15.511975	-0.051079	4.203863
252.615660	6032.975328	15.516979	-0.051073	4.201191
252.614779	6024.954061	15.521984	-0.051068	4.198501
252.618431	6016.985233	15.526989	-0.051063	4.195827
252.345187	6008.876015	15.531994	-0.051007	4.193101
252.539051	6000.813885	15.536999	-0.051038	4.190395
252.418110	5992.843159	15.542003	-0.051010	4.187713
252.437972	5984.831283	15.547008	-0.051009	4.185018
252.603545	5976.918085	15.552013	-0.051035	4.182356
252.311855	5968.884043	15.557018	-0.050975	4.179646
252.355643	5960.937779	15.562023	-0.050978	4.176968
252.191802	5952.910966	15.567027	-0.050943	4.174259
252.171127	5944.886506	15.572032	-0.050933	4.171550
252.278534	5936.892544	15.577037	-0.050948	4.168852
252.257666	5928.900666	15.582042	-0.050939	4.166151
252.088503	5920.919949	15.587047	-0.050903	4.163450
252.005142	5912.893597	15.592051	-0.050882	4.160733
252.195333	5904.923039	15.597056	-0.050912	4.158036
252.193520	5896.913557	15.602061	-0.050907	4.155322
252.026375	5888.872719	15.607066	-0.050870	4.152594
252.194366	5880.897281	15.612071	-0.050896	4.149890
252.056328	5872.878899	15.617075	-0.050866	4.147166
252.008489	5864.853477	15.622080	-0.050851	4.144439
251.960745	5856.927919	15.627085	-0.050837	4.141744
252.080126	5848.888732	15.632090	-0.050855	4.139010
252.028114	5840.925147	15.637095	-0.050840	4.136299
251.908215	5832.881305	15.642099	-0.050812	4.133558
252.013518	5824.844753	15.647104	-0.050827	4.130820
252.084959	5816.887017	15.652109	-0.050835	4.128106
251.619713	5808.858164	15.657114	-0.050743	4.125360
251.672969	5800.916254	15.662119	-0.050748	4.122648
251.750752	5792.868148	15.667123	-0.050757	4.119899
251.623126	5784.936167	15.672128	-0.050728	4.117184
251.578755	5776.877769	15.677133	-0.050715	4.114426
251.635911	5768.824623	15.682138	-0.050720	4.111669
251.764352	5760.861597	15.687143	-0.050739	4.108942
251.495096	5752.922581	15.692147	-0.050684	4.106216
251.536039	5744.883412	15.697152	-0.050686	4.103458
251.526190	5736.917033	15.702157	-0.050679	4.100723
251.422163	5728.896943	15.707162	-0.050654	4.097966
251.446161	5720.900933	15.712167	-0.050654	4.095217
251.271452	5712.888106	15.717171	-0.050616	4.092458
251.353429	5704.861636	15.722176	-0.050626	4.089695
251.329694	5696.918102	15.727181	-0.050617	4.086958
251.311897	5688.894576	15.732186	-0.050608	4.084192
251.300524	5680.982090	15.737191	-0.050601	4.081462
251.137905	5672.958006	15.742195	-0.050565	4.078690
250.950101	5664.928719	15.747200	-0.050525	4.075913
251.160255	5656.913302	15.752205	-0.050559	4.073145
251.016823	5648.901354	15.757210	-0.050527	4.070372
250.974748	5640.943095	15.762215	-0.050514	4.067616
250.960794	5632.929639	15.767219	-0.050507	4.064840
250.903181	5624.949576	15.772224	-0.050491	4.062073
251.017149	5616.937300	15.777229	-0.050507	4.059295
250.914852	5608.969118	15.782234	-0.050483	4.056528
251.025312	5600.956217	15.787239	-0.050498	4.053746
250.748494	5592.917421	15.792243	-0.050441	4.050948
250.814790	5584.939842	15.797248	-0.050448	4.048174
250.936979	5576.936654	15.802253	-0.050466	4.045390
250.588103	5568.968802	15.807258	-0.050396	4.042610
250.582452	5560.940898	15.812263	-0.050390	4.039812
250.879654	5552.972688	15.817267	-0.050440	4.037037
250.824700	5544.914133	15.822272	-0.050424	4.034223
250.637532	5536.845504	15.827277	-0.050384	4.031402
250.533641	5528.876316	15.832282	-0.050360	4.028615
250.780104	5520.891155	15.837287	-0.050401	4.025826
250.416083	5512.908772	15.842291	-0.050328	4.023026
250.355584	5504.900027	15.847296	-0.050311	4.020220
250.440489	5496.950132	15.852301	-0.050322	4.017435
250.328966	5488.908563	15.857306	-0.050296	4.014613
250.411591	5480.891604	15.862311	-0.050306	4.011800
250.407383	5472.908122	15.867315	-0.050300	4.008996
250.337415	5464.910107	15.872320	-0.050282	4.006184
250.150406	5456.953203	15.877325	-0.050242	4.003382
250.099273	5448.925741	15.882330	-0.050227	4.000556
250.287837	5440.947988	15.887335	-0.050257	3.997749
250.173124	5432.919702	15.892339	-0.050231	3.994917
250.055459	5424.896414	15.897344	-0.050204	3.992085
250.156219	5416.892665	15.902349	-0.050217	3.989262
250.129492	5408.920778	15.907354	-0.050207	3.986445
250.040504	5400.915062	15.912359	-0.050185	3.983614
250.079369	5392.938221	15.917363	-0.050187	3.980793
250.178758	5384.951841	15.922368	-0.050201	3.977967
249.931353	5376.945156	15.927373	-0.050149	3.975127
249.955273	5368.934107	15.932378	-0.050149	3.972288
250.028599	5360.901801	15.937383	-0.050157	3.969439
249.780981	5352.993407	15.942387	-0.050106	3.966628
249.581647	5344.927654	15.947392	-0.050064	3.963759
249.851577	5336.989228	15.952397	-0.050109	3.960941
249.976208	5328.969498	15.957402	-0.050127	3.958090
249.684357	5321.011634	15.962407	-0.050067	3.955252
249.448084	5312.945660	15.967411	-0.050018	3.952374
249.620852	5304.892812	15.972416	-0.050045	3.949506
249.619761	5296.976733	15.977421	-0.050040	3.946682
249.322623	5288.949804	15.982426	-0.049979	3.943810
249.410271	5280.979697	15.987431	-0.049990	3.940964
249.400237	5273.014058	15.992435	-0.049983	3.938115
249.277325	5264.977838	15.997440	-0.049955	3.935238
249.440820	5256.961985	16.002445	-0.049981	3.932370
249.305309	5248.925134	16.007450	-0.049950	3.929487
249.371920	5240.999793	16.012455	-0.049957	3.926646
249.186427	5233.021619	16.017459	-0.049918	3.923780
249.215527	5224.997618	16.022464	-0.049918	3.920899
249.159913	5217.022904	16.027469	-0.049903	3.918031
249.059971	5209.003399	16.032474	-0.049879	3.915145
249.262064	5200.977805	16.037479	-0.049911	3.912260
249.264694	5192.964008	16.042483	-0.049906	3.909373
249.100549	5184.994206	16.047488	-0.049871	3.906497
249.234619	5177.009661	16.052493	-0.049891	3.903619
249.231154	5168.978480	16.057498	-0.049885	3.900720
249.091864	5161.040725	16.062503	-0.049854	3.897850
248.883008	5152.993419	16.067507	-0.049810	3.894936
248.936355	5144.950477	16.072512	-0.049814	3.892027
248.859531	5136.987650	16.077517	-0.049795	3.889142
248.761051	5128.984552	16.082522	-0.049771	3.886241
248.760214	5121.010675	16.087527	-0.049766	3.883349
248.740649	5112.983548	16.092531	-0.049757	3.880436
248.900412	5105.031032	16.097536	-0.049782	3.877550
248.811830	5097.014468	16.102541	-0.049760	3.874635
248.649111	5088.764316	16.107546	-0.049725	3.871631
248.546555	5080.862891	16.112551	-0.049700	3.868753
248.557062	5072.889271	16.117555	-0.049697	3.865849
248.556369	5064.904280	16.122560	-0.049692	3.862938
248.475146	5056.970794	16.127565	-0.049672	3.860042
248.311998	5049.015333	16.132570	-0.049636	3.857134
248.619557	5040.940004	16.137575	-0.049688	3.854189
248.456062	5032.986456	16.142579	-0.049653	3.851278
248.297446	5025.008879	16.147584	-0.049618	3.848355
248.535514	5016.989721	16.152589	-0.049657	3.845423
248.442588	5009.016418	16.157594	-0.049635	3.842499
248.350601	5001.029607	16.162599	-0.049612	3.839568
248.269171	4993.057698	16.167603	-0.049592	3.836640
248.257394	4985.020857	16.172608	-0.049585	3.833688
248.291034	4977.017351	16.177613	-0.049586	3.830746
248.070653	4969.021739	16.182618	-0.049539	3.827800
248.195192	4961.035544	16.187623	-0.049558	3.824862
248.162038	4953.058558	16.192627	-0.049546	3.821922
248.065914	4945.063428	16.197632	-0.049523	3.818972
247.941419	4937.120137	16.202637	-0.049495	3.816038
248.030622	4929.072610	16.207642	-0.049506	3.813068
248.014263	4921.050125	16.212647	-0.049498	3.810102
247.964592	4913.083933	16.217651	-0.049484	3.807154
248.012614	4905.035604	16.222656	-0.049487	3.804176
248.058565	4897.114985	16.227661	-0.049491	3.801242
247.928174	4889.089653	16.232666	-0.049461	3.798264
247.988980	4881.108995	16.237671	-0.049467	3.795304
247.774159	4873.066855	16.242675	-0.049422	3.792313
247.616991	4865.057119	16.247680	-0.049388	3.789333
247.830106	4857.101293	16.252685	-0.049422	3.786378
247.769069	4849.074111	16.257690	-0.049406	3.783389
247.656287	4841.115056	16.262695	-0.049380	3.780422
247.405000	4833.139684	16.267699	-0.049328	3.777443
247.585872	4825.061779	16.272704	-0.049356	3.774433
247.683384	4817.095591	16.277709	-0.049369	3.771460
247.475209	4809.040683	16.282714	-0.049325	3.768445
247.625544	4801.079735	16.287719	-0.049348	3.765471
247.474285	4793.148493	16.292723	-0.049315	3.762499
247.296189	4785.107774	16.297728	-0.049276	3.759483
247.252900	4777.174329	16.302733	-0.049263	3.756508
247.199571	4769.100595	16.307738	-0.049248	3.753477
247.290962	4761.086766	16.312743	-0.049260	3.750470
247.063968	4753.124052	16.317747	-0.049213	3.747472
247.301296	4745.046734	16.322752	-0.049252	3.744440
247.323663	4737.135237	16.327757	-0.049251	3.741462
247.182699	4729.114372	16.332762	-0.049219	3.738437
246.932051	4721.173194	16.337767	-0.049167	3.735438
247.038324	4713.129118	16.342771	-0.049182	3.732405
247.181293	4705.064422	16.347776	-0.049203	3.729363
247.213434	4697.137154	16.352781	-0.049204	3.726367
247.134737	4689.140813	16.357786	-0.049184	3.723341
247.088652	4681.175309	16.362791	-0.049171	3.720325
246.969721	4673.214375	16.367795	-0.049143	3.717306
247.053219	4665.202497	16.372800	-0.049154	3.714270
246.952101	4657.107081	16.377805	-0.049130	3.711195
246.865125	4649.088173	16.382810	-0.049108	3.708147
247.032076	4641.148085	16.387815	-0.049134	3.705133
246.774558	4633.178865	16.392819	-0.049081	3.702095
246.525034	4625.186276	16.397824	-0.049030	3.699046
246.555843	4617.220522	16.402829	-0.049030	3.696012
246.556781	4609.203529	16.407834	-0.049025	3.692954
246.634013	4601.193060	16.412839	-0.049034	3.689899
246.508188	4593.218138	16.417843	-0.049006	3.686849
246.610199	4585.201310	16.422848	-0.049020	3.683787
246.529460	4577.234248	16.427853	-0.048999	3.680736
246.400450	4569.248529	16.432858	-0.048970	3.677675
246.362486	4561.253665	16.437863	-0.048958	3.674610
246.537316	4553.210549	16.442867	-0.048985	3.671529
246.277702	4545.211456	16.447872	-0.048932	3.668451
246.198572	4537.241136	16.452877	-0.048912	3.665387
246.187050	4529.236433	16.457882	-0.048905	3.662308
246.189119	4521.240793	16.462887	-0.048900	3.659231
246.241749	4513.290572	16.467891	-0.048904	3.656170
245.897155	4505.251862	16.472896	-0.048835	3.653061
246.179177	4497.212064	16.477901	-0.048882	3.649966
245.950769	4489.256809	16.482906	-0.048835	3.646888
246.077481	4481.263764	16.487911	-0.048853	3.643802
246.195200	4473.265153	16.492915	-0.048870	3.640711
246.073355	4465.283413	16.497920	-0.048842	3.637617
245.944004	4457.320319	16.502925	-0.048813	3.634528
245.658924	4449.276727	16.507930	-0.048755	3.631401
245.761789	4441.262978	16.512935	-0.048769	3.628293
245.939844	4433.256419	16.517939	-0.048797	3.625187
245.884207	4425.288288	16.522944	-0.048781	3.622087
245.881354	4417.276788	16.527949	-0.048775	3.618969
245.780842	4409.315141	16.532954	-0.048751	3.615865
245.560258	4401.340054	16.537959	-0.048705	3.612750
245.548246	4393.310772	16.542963	-0.048698	3.609617
245.737637	4385.321297	16.547968	-0.048728	3.606502
245.556416	4377.365071	16.552973	-0.048689	3.603387
245.442426	4369.369524	16.557978	-0.048663	3.600256
245.449732	4361.412144	16.562983	-0.048659	3.597141
245.485066	4353.373643	16.567987	-0.048660	3.593992
245.444604	4345.321385	16.572992	-0.048648	3.590832
245.505986	4337.355524	16.577997	-0.048654	3.587707
245.500193	4329.330764	16.583002	-0.048648	3.584554
245.299495	4321.415315	16.588007	-0.048605	3.581435
245.253754	4313.411529	16.593011	-0.048591	3.578283
245.137129	4305.412868	16.598016	-0.048565	3.575129
245.348525	4297.409173	16.603021	-0.048599	3.571979
245.312196	4289.373707	16.608026	-0.048587	3.568807
245.364884	4281.391785	16.613031	-0.048591	3.565656
245.101709	4273.452056	16.618035	-0.048537	3.562509
244.890709	4265.418606	16.623040	-0.048493	3.559324
245.125076	4257.461040	16.628045	-0.048531	3.556179
245.103143	4249.361804	16.633050	-0.048522	3.552968
244.984531	4241.332173	16.638055	-0.048495	3.549778
244.956661	4233.372181	16.643059	-0.048484	3.546616
245.011250	4225.401347	16.648064	-0.048489	3.543450
245.088063	4217.428104	16.653069	-0.048499	3.540280
244.787764	4209.451209	16.658074	-0.048437	3.537094
244.851511	4201.461182	16.663079	-0.048444	3.533912
244.882194	4193.419035	16.668083	-0.048445	3.530705
244.608665	4185.428392	16.673088	-0.048389	3.527506
244.573528	4177.456648	16.678093	-0.048377	3.524319
244.592327	4169.471637	16.683098	-0.048375	3.521125
244.671385	4161.470549	16.688103	-0.048385	3.517924
244.646823	4153.494006	16.693107	-0.048375	3.514727
244.539291	4145.479772	16.698112	-0.048350	3.511509
244.676560	4137.471940	16.703117	-0.048370	3.508299
244.614867	4129.467347	16.708122	-0.048354	3.505080
244.623626	4121.521317	16.713127	-0.048350	3.501885
244.635292	4113.523405	16.718131	-0.048347	3.498665
244.335656	4105.551675	16.723136	-0.048286	3.495444
244.342382	4097.550368	16.728141	-0.048282	3.492217
244.448627	4089.521614	16.733146	-0.048297	3.488979
244.399403	4081.554943	16.738151	-0.048283	3.485758
244.386603	4073.593569	16.743155	-0.048275	3.482538
244.400699	4065.567302	16.748160	-0.048272	3.479289
244.270301	4057.633883	16.753165	-0.048243	3.476070
244.036312	4049.611445	16.758170	-0.048194	3.472809
244.129514	4041.566826	16.763175	-0.048206	3.469546
244.150206	4033.594642	16.768179	-0.048205	3.466307
243.964004	4025.601917	16.773184	-0.048165	3.463051
243.903830	4017.605187	16.778189	-0.048149	3.459793
243.948366	4009.632128	16.783194	-0.048152	3.456546
243.998717	4001.629357	16.788199	-0.048156	3.453283
243.850177	3993.617290	16.793203	-0.048123	3.450007
243.779028	3985.634909	16.798208	-0.048105	3.446743
243.885634	3977.652602	16.803213	-0.048120	3.443481
243.809698	3969.660617	16.808218	-0.048100	3.440207
243.909269	3961.674949	16.813223	-0.048114	3.436937
243.902566	3953.670511	16.818227	-0.048107	3.433653
243.723513	3945.618668	16.823232	-0.048069	3.430341
243.648006	3937.676297	16.828237	-0.048050	3.427074
243.720041	3929.653569	16.833242	-0.048058	3.423776
243.723688	3921.701007	16.838247	-0.048053	3.420502
243.617562	3913.741653	16.843251	-0.048029	3.417217
243.591656	3905.722107	16.848256	-0.048019	3.413908
243.626903	3897.723420	16.853261	-0.048020	3.410606
243.353738	3889.726391	16.858266	-0.047964	3.407290
243.445137	3881.725012	16.863271	-0.047976	3.403983
243.532685	3873.761077	16.868275	-0.047987	3.400687
243.380556	3865.778968	16.873280	-0.047953	3.397372
243.433809	3857.807802	16.878285	-0.047958	3.394066
243.124899	3849.701305	16.883290	-0.047895	3.390688
243.452394	3841.723516	16.888295	-0.047951	3.387382
243.281858	3833.738446	16.893299	-0.047914	3.384052
243.029987	3825.780188	16.898304	-0.047862	3.380728
243.189924	3817.837594	16.903309	-0.047887	3.377421
243.066851	3809.810164	16.908314	-0.047859	3.374065
243.052748	3801.809126	16.913319	-0.047851	3.370721
243.112611	3793.828370	16.918323	-0.047857	3.367385
242.983952	3785.817235	16.923328	-0.047828	3.364026
243.092470	3777.880180	16.928333	-0.047843	3.360704
242.995564	3769.891241	16.933338	-0.047820	3.357348
243.173950	3761.865064	16.938343	-0.047848	3.353984
242.862725	3753.866142	16.943347	-0.047785	3.350610
242.980607	3745.843470	16.948352	-0.047801	3.347238
242.999568	3737.894454	16.953357	-0.047800	3.343891
242.777579	3729.924023	16.958362	-0.047753	3.340522
242.727363	3721.948990	16.963367	-0.047739	3.337154
242.766622	3713.934341	16.968371	-0.047741	3.333769
242.715352	3705.901066	16.973376	-0.047726	3.330369
242.819950	3697.923521	16.978381	-0.047741	3.326996
242.635493	3689.941150	16.983386	-0.047701	3.323606
242.624434	3681.968653	16.988391	-0.047694	3.320223
242.551898	3674.008249	16.993395	-0.047675	3.316840
242.397134	3665.985478	16.998400	-0.047641	3.313423
242.377890	3657.978838	17.003405	-0.047632	3.310015
242.173957	3649.977096	17.008410	-0.047589	3.306599
242.298234	3641.998392	17.013415	-0.047607	3.303201
242.434482	3634.005576	17.018419	-0.047627	3.299794
242.349551	3626.045852	17.023424	-0.047607	3.296390
242.284643	3618.069257	17.028429	-0.047589	3.292975
242.149604	3610.032216	17.033434	-0.047559	3.289529
242.164759	3602.070216	17.038439	-0.047557	3.286116
242.059068	3594.099028	17.043443	-0.047532	3.282692
241.958817	3586.092861	17.048448	-0.047508	3.279249
242.055015	3578.142661	17.053453	-0.047521	3.275834
241.892446	3570.089378	17.058458	-0.047485	3.272361
241.957471	3562.100770	17.063463	-0.047492	3.268921
242.146775	3554.099081	17.068467	-0.047522	3.265477
241.968902	3546.129190	17.073472	-0.047484	3.262029
241.871601	3538.163324	17.078477	-0.047461	3.258581
241.796284	3530.159214	17.083482	-0.047442	3.255115
241.941989	3522.151265	17.088487	-0.047464	3.251651
241.855642	3514.162377	17.093491	-0.047442	3.248183
241.680664	3506.151439	17.098496	-0.047405	3.244699
241.659167	3498.241970	17.103501	-0.047395	3.241260
241.657743	3490.226442	17.108506	-0.047390	3.237773
241.674724	3482.229307	17.113511	-0.047388	3.234291
241.682926	3474.172892	17.118515	-0.047384	3.230779
241.433670	3466.178578	17.123520	-0.047333	3.227279
241.489732	3458.220920	17.128525	-0.047338	3.223804
241.413281	3450.256416	17.133530	-0.047319	3.220317
241.621461	3442.258173	17.138535	-0.047352	3.216824
241.489418	3434.293419	17.143539	-0.047322	3.213327
241.355581	3426.272160	17.148544	-0.047292	3.209801
241.602121	3418.294864	17.153549	-0.047333	3.206306
241.369128	3410.309828	17.158554	-0.047285	3.202785
241.146908	3402.353222	17.163559	-0.047238	3.199272
241.218316	3394.374720	17.168563	-0.047246	3.195758
241.264048	3386.344474	17.173568	-0.047250	3.192217
241.305903	3378.343975	17.178573	-0.047252	3.188684
241.143021	3370.357795	17.183578	-0.047217	3.185145
241.229166	3362.405336	17.188583	-0.047228	3.181628
241.187045	3354.415519	17.193587	-0.047215	3.178085
241.034488	3346.405884	17.198592	-0.047181	3.174524
240.979700	3338.434520	17.203597	-0.047166	3.170981
240.845034	3330.418072	17.208602	-0.047135	3.167410
240.743154	3322.443301	17.213607	-0.047111	3.163855
240.868148	3314.491942	17.218611	-0.047129	3.160316
240.820450	3306.493494	17.223616	-0.047115	3.156745
240.892959	3298.492418	17.228621	-0.047124	3.153174
240.796351	3290.448506	17.233626	-0.047101	3.149572
240.963728	3282.468871	17.238631	-0.047127	3.146006
240.752790	3274.529694	17.243635	-0.047082	3.142438
240.286910	3266.577390	17.248640	-0.046990	3.138849
240.494438	3258.578603	17.253645	-0.047024	3.135264
240.539911	3250.547259	17.258650	-0.047027	3.131653
240.460687	3242.574192	17.263655	-0.047007	3.128059
240.288955	3234.593875	17.268659	-0.046970	3.124454
240.357542	3226.628071	17.273664	-0.046978	3.120861
240.474054	3218.667338	17.278669	-0.046994	3.117269
240.098954	3210.654299	17.283674	-0.046919	3.113627
240.373661	3202.608772	17.288679	-0.046965	3.109995
240.590914	3194.638108	17.293683	-0.047000	3.106390
240.296087	3186.692104	17.298688	-0.046940	3.102770
240.282506	3178.699179	17.303693	-0.046933	3.099136
240.133793	3170.714130	17.308698	-0.046900	3.095495
240.106688	3162.722887	17.313703	-0.046890	3.091853
240.115664	3154.752486	17.318707	-0.046886	3.088218
239.958883	3146.744678	17.323712	-0.046852	3.084554
239.817158	3138.828879	17.328717	-0.046820	3.080928
239.827441	3130.806858	17.333722	-0.046817	3.077256
239.918195	3122.765127	17.338727	-0.046829	3.073574
240.028872	3114.705120	17.343731	-0.046844	3.069881
239.732444	3106.752659	17.348736	-0.046784	3.066214
239.905731	3098.776100	17.353741	-0.046811	3.062553
239.960247	3090.788634	17.358746	-0.046816	3.058877
239.743515	3082.850754	17.363751	-0.046770	3.055207
239.579149	3074.884024	17.368755	-0.046735	3.051521
239.646621	3066.862625	17.373760	-0.046742	3.047817
239.810347	3058.878098	17.378765	-0.046767	3.044130
239.708651	3050.940701	17.383770	-0.046743	3.040448
239.707763	3042.951416	17.388775	-0.046738	3.036741
239.650535	3034.966311	17.393779	-0.046722	3.033030
239.331524	3026.953812	17.398784	-0.046658	3.029289
239.303349	3019.006196	17.403789	-0.046647	3.025587
239.471559	3010.998304	17.408794	-0.046673	3.021862
239.357303	3003.026384	17.413799	-0.046647	3.018135
239.432412	2995.038531	17.418803	-0.046656	3.014406
239.373886	2987.019868	17.423808	-0.046640	3.010651
239.457610	2979.055561	17.428813	-0.046650	3.006924
239.207840	2971.080995	17.433818	-0.046598	3.003171
239.428170	2963.092181	17.438823	-0.046634	2.999430
239.448417	2955.142329	17.443827	-0.046633	2.995693
239.285970	2947.121670	17.448832	-0.046597	2.991908
239.179492	2939.143033	17.453837	-0.046572	2.988142
239.035903	2931.146068	17.458842	-0.046541	2.984360
239.070059	2923.197167	17.463847	-0.046542	2.980605
238.894159	2915.217375	17.468851	-0.046504	2.976820
238.714960	2907.222498	17.473856	-0.046465	2.973022
239.041399	2899.194331	17.478861	-0.046521	2.969230
238.657031	2891.269546	17.483866	-0.046444	2.965446
238.555290	2883.299793	17.488871	-0.046420	2.961650
238.607118	2875.331647	17.493875	-0.046425	2.957857
238.590901	2867.328690	17.498880	-0.046416	2.954040
238.559324	2859.305076	17.503885	-0.046405	2.950207
238.601002	2851.302905	17.508890	-0.046408	2.946383
238.621355	2843.330356	17.513895	-0.046407	2.942568
238.556656	2835.368913	17.518899	-0.046389	2.938748
238.343913	2827.406659	17.523904	-0.046345	2.934915
238.459796	2819.408724	17.528909	-0.046361	2.931077
238.617214	2811.407594	17.533914	-0.046385	2.927235
238.470800	2803.461764	17.538919	-0.046353	2.923398
238.410395	2795.485985	17.543923	-0.046336	2.919547
238.388454	2787.531395	17.548928	-0.046327	2.915702
238.242736	2779.461620	17.553933	-0.046295	2.911790
238.294999	2771.444080	17.558938	-0.046299	2.907909
238.096304	2763.495129	17.563943	-0.046257	2.904043
238.113630	2755.549056	17.568947	-0.046255	2.900184
238.026116	2747.586670	17.573952	-0.046234	2.896306
238.206966	2739.567440	17.578957	-0.046262	2.892410
238.181108	2731.579321	17.583962	-0.046252	2.888513
237.988391	2723.606510	17.588967	-0.046211	2.884609
238.047732	2715.670090	17.593971	-0.046217	2.880731
237.907214	2707.694010	17.598976	-0.046186	2.876818
238.077041	2699.695417	17.603981	-0.046213	2.872905
237.898561	2691.689473	17.608986	-0.046174	2.868964
237.820125	2683.708142	17.613991	-0.046154	2.865035
237.773156	2675.763411	17.618995	-0.046140	2.861121
237.599701	2667.803959	17.624000	-0.046103	2.857187
237.745877	2659.803704	17.629005	-0.046125	2.853245
237.582061	2651.799610	17.634010	-0.046089	2.849279
237.550317	2643.823935	17.639015	-0.046078	2.845328
237.635012	2635.866915	17.644019	-0.046089	2.841388
237.574180	2627.893431	17.649024	-0.046072	2.837426
237.464901	2619.929099	17.654029	-0.046047	2.833460
237.324623	2611.899303	17.659034	-0.046016	2.829454
237.354762	2603.907802	17.664039	-0.046016	2.825471
237.200537	2595.985503	17.669043	-0.045982	2.821507
237.119909	2587.994234	17.674048	-0.045962	2.817507
237.306292	2579.996180	17.679053	-0.045992	2.813513
237.222769	2571.993740	17.684058	-0.045971	2.809495
237.139280	2564.041308	17.689063	-0.045950	2.805497
237.163981	2556.091502	17.694067	-0.045950	2.801501
237.196232	2548.110644	17.699072	-0.045951	2.797484
237.164660	2540.152947	17.704077	-0.045940	2.793469
236.981145	2532.133511	17.709082	-0.045900	2.789408
237.177363	2524.132347	17.714087	-0.045932	2.785373
237.173552	2516.185024	17.719091	-0.045926	2.781348
236.732315	2508.250342	17.724096	-0.045838	2.777297
237.045144	2500.248710	17.729101	-0.045892	2.773251
236.946158	2492.240479	17.734106	-0.045868	2.769171
236.745533	2484.296416	17.739111	-0.045825	2.765112
236.786061	2476.330961	17.744115	-0.045828	2.761050
236.730945	2468.356078	17.749120	-0.045812	2.756972
236.626084	2460.349496	17.754125	-0.045788	2.752868
236.537627	2452.312194	17.759130	-0.045766	2.748743
236.595061	2444.329348	17.764135	-0.045772	2.744650
236.572529	2436.401212	17.769139	-0.045762	2.740573
236.409210	2428.434895	17.774144	-0.045727	2.736462
236.556760	2420.438929	17.779149	-0.045749	2.732348
236.603615	2412.446944	17.784154	-0.045753	2.728224
236.439537	2404.502972	17.789159	-0.045717	2.724106
236.444551	2396.549144	17.794163	-0.045713	2.719987
236.403930	2388.579729	17.799168	-0.045700	2.715851
236.326484	2380.599857	17.804173	-0.045680	2.711700
236.334626	2372.620795	17.809178	-0.045677	2.707549
236.331088	2364.640397	17.814183	-0.045671	2.703390
236.154518	2356.694861	17.819187	-0.045633	2.699233
236.238805	2348.704612	17.824192	-0.045643	2.695061
236.246867	2340.710844	17.829197	-0.045640	2.690877
236.088666	2332.749575	17.834202	-0.045605	2.686692
235.890374	2324.805050	17.839207	-0.045563	2.682508
235.939461	2316.841888	17.844211	-0.045567	2.678322
236.067540	2308.847214	17.849216	-0.045586	2.674119
236.049216	2300.839662	17.854221	-0.045577	2.669893
235.892128	2292.874669	17.859226	-0.045543	2.665673
236.074823	2284.897464	17.864231	-0.045572	2.661463
235.922742	2276.961285	17.869235	-0.045538	2.657245
235.933851	2268.950276	17.874240	-0.045535	2.652992
235.907729	2260.985111	17.879245	-0.045525	2.648754
235.988930	2252.993190	17.884250	-0.045535	2.644502
235.644583	2245.086225	17.889255	-0.045466	2.640261
235.768897	2237.134502	17.894259	-0.045484	2.636020
235.474993	2229.134271	17.899264	-0.045424	2.631718
235.644786	2221.130497	17.904269	-0.045450	2.627438
235.393189	2213.191169	17.909274	-0.045398	2.623157
235.477738	2205.216079	17.914279	-0.045409	2.618873
235.614809	2197.242262	17.919283	-0.045429	2.614586
235.004850	2189.294160	17.924288	-0.045311	2.610255
235.197614	2181.291784	17.929293	-0.045341	2.605942
235.321851	2173.332102	17.934298	-0.045359	2.601641
235.121619	2165.395509	17.939303	-0.045317	2.597322
235.107570	2157.334418	17.944307	-0.045309	2.592942
235.216966	2149.213612	17.949312	-0.045324	2.588530
235.205539	2141.301400	17.954317	-0.045317	2.584216
235.157945	2133.385521	17.959322	-0.045303	2.579890
235.275003	2125.418612	17.964327	-0.045320	2.575541
235.152262	2117.490728	17.969331	-0.045292	2.571189
234.796013	2109.525930	17.974336	-0.045220	2.566793
235.132855	2101.557230	17.979341	-0.045278	2.562435
234.978677	2093.629159	17.984346	-0.045244	2.558058
235.007860	2085.641470	17.989351	-0.045244	2.553654
234.763315	2077.700860	17.994355	-0.045194	2.549249
234.726340	2069.700125	17.999360	-0.045182	2.544817
234.838957	2061.759556	18.004365	-0.045197	2.540422
234.805689	2053.799870	18.009370	-0.045186	2.535998
234.656274	2045.820707	18.014375	-0.045153	2.531547
234.787544	2037.850273	18.019379	-0.045172	2.527114
234.543809	2029.902656	18.024384	-0.045122	2.522658
234.503165	2021.969945	18.029389	-0.045109	2.518218
234.438506	2013.989486	18.034394	-0.045092	2.513741
234.400204	2005.971272	18.039399	-0.045080	2.509236
234.392325	1998.010972	18.044403	-0.045073	2.504759
234.287636	1990.060232	18.049408	-0.045048	2.500272
234.299394	1982.110713	18.054413	-0.045045	2.495785
234.338223	1974.121497	18.059418	-0.045048	2.491271
234.212811	1966.155903	18.064423	-0.045019	2.486749
234.159586	1958.216934	18.069427	-0.045004	2.482240
234.112129	1950.262043	18.074432	-0.044990	2.477713
233.998327	1942.317478	18.079437	-0.044964	2.473180
234.117279	1934.311017	18.084442	-0.044981	2.468620
234.034383	1926.346436	18.089447	-0.044960	2.464060
234.132399	1918.385788	18.094451	-0.044973	2.459508
233.949620	1910.440426	18.099456	-0.044934	2.454935
234.009219	1902.475211	18.104461	-0.044940	2.450360
233.928993	1894.503655	18.109466	-0.044920	2.445763
233.722192	1886.580261	18.114471	-0.044876	2.441175
233.832629	1878.626330	18.119475	-0.044892	2.436585
233.652356	1870.616342	18.124480	-0.044853	2.431931
233.656479	1862.610066	18.129485	-0.044849	2.427285
233.870835	1854.621339	18.134490	-0.044883	2.422657
233.497880	1846.729281	18.139495	-0.044809	2.418030
233.464069	1838.782719	18.144499	-0.044797	2.413389
233.446592	1830.787422	18.149504	-0.044789	2.408712
233.457773	1822.845893	18.154509	-0.044786	2.404059
233.447527	1814.903187	18.159514	-0.044779	2.399395
233.228609	1806.983616	18.164519	-0.044733	2.394719
233.349278	1798.965477	18.169523	-0.044750	2.390003
233.113643	1791.016565	18.174528	-0.044701	2.385290
232.990091	1783.095896	18.179533	-0.044673	2.380593
233.011934	1775.139329	18.184538	-0.044672	2.375878
232.917468	1767.164292	18.189543	-0.044649	2.371132
233.064986	1759.192353	18.194547	-0.044672	2.366398
233.057086	1751.230538	18.199552	-0.044665	2.361649
233.086834	1743.298441	18.204557	-0.044665	2.356910
233.128843	1735.306397	18.209562	-0.044668	2.352127
232.857290	1727.357681	18.214567	-0.044612	2.347335
232.984301	1719.398831	18.219571	-0.044631	2.342560
232.775176	1711.465770	18.224576	-0.044587	2.337762
232.857936	1703.507637	18.229581	-0.044597	2.332964
232.669338	1695.555584	18.234586	-0.044557	2.328137
232.624581	1687.592556	18.239591	-0.044543	2.323305
232.506230	1679.675408	18.244595	-0.044516	2.318485
232.450363	1671.712977	18.249600	-0.044501	2.313633
232.514063	1663.728930	18.254605	-0.044507	2.308767
232.470307	1655.786847	18.259610	-0.044494	2.303907
232.497057	1647.828190	18.264615	-0.044494	2.299033
232.436547	1639.897361	18.269619	-0.044478	2.294158
232.416913	1631.912154	18.274624	-0.044469	2.289243
232.406169	1623.969676	18.279629	-0.044462	2.284345
232.164586	1616.073320	18.284634	-0.044412	2.279444
232.129955	1608.106570	18.289639	-0.044400	2.274508
232.215902	1600.076121	18.294643	-0.044411	2.269531
232.034512	1592.123334	18.299648	-0.044372	2.264568
232.137789	1584.193850	18.304653	-0.044386	2.259634
232.130307	1576.247329	18.309658	-0.044379	2.254669
232.084214	1568.269390	18.314663	-0.044366	2.249670
231.990753	1560.351835	18.319667	-0.044343	2.244693
231.731991	1552.446202	18.324672	-0.044290	2.239698
231.718793	1544.516131	18.329677	-0.044282	2.234699
231.775599	1536.517985	18.334682	-0.044288	2.229651
231.635376	1528.577332	18.339687	-0.044256	2.224611
231.658249	1520.640959	18.344691	-0.044256	2.219576
231.408156	1512.728566	18.349696	-0.044204	2.214521
231.544374	1504.743839	18.354701	-0.044224	2.209443
231.456251	1496.805555	18.359706	-0.044203	2.204362
231.446996	1488.879359	18.364711	-0.044196	2.199285
231.434041	1480.939433	18.369715	-0.044188	2.194187
231.292141	1472.961567	18.374720	-0.044157	2.189040
231.199449	1465.026276	18.379725	-0.044134	2.183914
231.255213	1457.078956	18.384730	-0.044139	2.178781
231.261279	1449.138841	18.389735	-0.044135	2.173636
231.212084	1441.186480	18.394739	-0.044121	2.168466
231.062225	1433.259302	18.399744	-0.044088	2.163291
231.095580	1425.336992	18.404749	-0.044089	2.158123
231.021285	1417.392752	18.409754	-0.044070	2.152919
230.995253	1409.431851	18.414759	-0.044060	2.147696
231.126815	1401.475097	18.419763	-0.044080	2.142477
231.099743	1393.549247	18.424768	-0.044069	2.137251
230.962198	1385.644253	18.429773	-0.044039	2.132016
230.712154	1377.717966	18.434778	-0.043987	2.126742
230.904446	1369.745697	18.439783	-0.044018	2.121468
230.865838	1361.837394	18.444787	-0.044005	2.116201
230.659128	1353.842916	18.449792	-0.043962	2.110846
230.734368	1345.892418	18.454797	-0.043971	2.105535
230.595519	1337.985921	18.459802	-0.043940	2.100219
230.595181	1330.049304	18.464807	-0.043935	2.094883
230.554249	1322.108944	18.469811	-0.043922	2.089527
230.467743	1314.180121	18.474816	-0.043901	2.084160
230.324058	1306.292970	18.479821	-0.043869	2.078802
230.096525	1298.379707	18.484826	-0.043821	2.073404
230.264075	1290.380343	18.489831	-0.043847	2.067973
230.223116	1282.470205	18.494835	-0.043834	2.062567
230.000203	1274.569178	18.499840	-0.043788	2.057135
230.062287	1266.619941	18.504845	-0.043794	2.051685
230.300051	1258.642662	18.509850	-0.043833	2.046218
230.184906	1250.737646	18.514855	-0.043807	2.040751
230.055388	1242.859597	18.519859	-0.043778	2.035286
230.038451	1234.874996	18.524864	-0.043769	2.029744
230.001425	1226.948760	18.529869	-0.043757	2.024225
229.745900	1219.076401	18.534874	-0.043705	2.018707
229.726363	1211.130919	18.539879	-0.043696	2.013146
229.896961	1203.174126	18.544883	-0.043723	2.007582
229.570069	1195.287702	18.549888	-0.043657	2.002000
229.576984	1187.374632	18.554893	-0.043653	1.996418
229.646636	1179.419030	18.559898	-0.043661	1.990798
229.455262	1171.511464	18.564903	-0.043620	1.985168
229.439491	1163.613005	18.569907	-0.043612	1.979547
229.691686	1155.636695	18.574912	-0.043654	1.973883
229.726776	1147.705234	18.579917	-0.043655	1.968211
229.395506	1139.842023	18.584922	-0.043588	1.962533
229.247874	1131.944857	18.589927	-0.043556	1.956834
229.255033	1123.984525	18.594931	-0.043552	1.951089
229.108709	1116.042868	18.599936	-0.043519	1.945324
229.196984	1108.125644	18.604941	-0.043531	1.939585
229.138356	1100.226034	18.609946	-0.043515	1.933825
229.155053	1092.272897	18.614951	-0.043513	1.928018
229.084687	1084.388511	18.619955	-0.043495	1.922234
229.087794	1076.478180	18.624960	-0.043490	1.916422
229.206733	1068.534957	18.629965	-0.043507	1.910580
229.032649	1060.642987	18.634970	-0.043470	1.904726
228.677702	1052.792733	18.639975	-0.043398	1.898865
229.022350	1044.824306	18.644979	-0.043457	1.892976
228.734586	1036.926366	18.649984	-0.043399	1.887049
228.666550	1029.042486	18.654989	-0.043381	1.881140
228.712003	1021.136842	18.659994	-0.043384	1.875208
228.497244	1013.211644	18.664999	-0.043339	1.869213
228.442600	1005.311477	18.670003	-0.043324	1.863236
228.412271	997.395540	18.675008	-0.043313	1.857231
228.439522	989.488178	18.680013	-0.043313	1.851219
228.439927	981.571347	18.685018	-0.043308	1.845178
228.422240	973.681148	18.690023	-0.043300	1.839135
228.559923	965.779580	18.695027	-0.043320	1.833081
228.369779	957.880207	18.700032	-0.043280	1.826971
228.207801	950.009701	18.705037	-0.043244	1.820865
228.123996	942.117883	18.710042	-0.043224	1.814732
228.134860	934.199319	18.715047	-0.043221	1.808568
228.116038	926.318870	18.720051	-0.043212	1.802410
227.811418	918.461490	18.725056	-0.043150	1.796214
228.006234	910.479118	18.730061	-0.043181	1.789958
228.068657	902.575184	18.735066	-0.043188	1.783727
227.703008	894.728926	18.740071	-0.043115	1.777467
227.735408	886.840018	18.745075	-0.043116	1.771200
227.495329	878.955596	18.750080	-0.043066	1.764880
227.381181	871.110107	18.755085	-0.043040	1.758584
227.492137	863.202335	18.760090	-0.043055	1.752244
227.399995	855.304754	18.765095	-0.043033	1.745864
227.421447	847.429841	18.770099	-0.043032	1.739493
227.446881	839.532640	18.775104	-0.043031	1.733081
227.588203	831.616776	18.780109	-0.043053	1.726644
227.391745	823.784855	18.785114	-0.043011	1.720209
227.112464	815.948185	18.790119	-0.042954	1.713735
227.185553	808.028389	18.795123	-0.042962	1.707214
227.128325	800.147992	18.800128	-0.042947	1.700683
227.184239	792.277369	18.805133	-0.042952	1.694150
226.910937	784.424247	18.810138	-0.042896	1.687563
227.010431	776.535166	18.815143	-0.042909	1.680969
227.016095	768.687676	18.820147	-0.042905	1.674372
226.777068	760.824799	18.825152	-0.042856	1.667703
226.956018	752.929346	18.830157	-0.042884	1.661036
226.746691	745.106246	18.835162	-0.042840	1.654351
226.698726	737.221571	18.840167	-0.042826	1.647608
226.580027	729.388971	18.845171	-0.042799	1.640873
226.289674	721.557042	18.850176	-0.042740	1.634086
226.185912	713.648102	18.855181	-0.042715	1.627230
226.268390	705.762991	18.860186	-0.042726	1.620392
226.207974	697.925334	18.865191	-0.042709	1.613547
226.156496	690.063668	18.870195	-0.042695	1.606652
225.908327	682.249087	18.875200	-0.042643	1.599741
226.085148	674.374220	18.880205	-0.042671	1.592808
226.053178	666.523116	18.885210	-0.042660	1.585835
226.012514	658.685538	18.890215	-0.042648	1.578842
226.079307	650.831914	18.895219	-0.042655	1.571820
225.761009	643.023673	18.900224	-0.042591	1.564750
225.644437	635.219571	18.905229	-0.042564	1.557682
225.646977	627.354952	18.910234	-0.042559	1.550544
225.721658	619.485561	18.915239	-0.042568	1.543380
225.613568	611.675747	18.920243	-0.042543	1.536209
225.335728	603.865215	18.925248	-0.042486	1.528979
225.333180	596.036127	18.930253	-0.042481	1.521738
225.252630	588.232116	18.935258	-0.042461	1.514474
225.211020	580.391817	18.940263	-0.042448	1.507148
225.204068	572.574647	18.945267	-0.042441	1.499812
225.316714	564.726706	18.950272	-0.042457	1.492430
225.133093	556.935770	18.955277	-0.042418	1.485019
225.035132	549.151009	18.960282	-0.042395	1.477591
225.212434	541.258757	18.965287	-0.042423	1.470065
225.235153	533.448653	18.970291	-0.042422	1.462555
224.917526	525.691813	18.975296	-0.042358	1.455003
225.087812	517.850380	18.980301	-0.042384	1.447408
225.023152	510.079892	18.985306	-0.042367	1.439805
224.935405	502.288777	18.990311	-0.042346	1.432137
224.744978	494.526236	18.995315	-0.042305	1.424439
224.842349	486.712582	19.000320	-0.042319	1.416696
224.538239	478.971216	19.005325	-0.042257	1.408916
224.373103	471.209541	19.010330	-0.042221	1.401096
224.284959	463.438128	19.015335	-0.042200	1.393234
224.290613	455.634744	19.020339	-0.042196	1.385311
223.993095	447.896093	19.025344	-0.042135	1.377358
224.062901	440.098686	19.030349	-0.042143	1.369360
224.010972	432.332240	19.035354	-0.042129	1.361327
223.977228	424.576042	19.040359	-0.042117	1.353260
224.050396	416.794708	19.045363	-0.042126	1.345136
224.044289	409.046758	19.050368	-0.042120	1.336985
223.859396	401.319900	19.055373	-0.042080	1.328774
223.701972	393.596709	19.060378	-0.042046	1.320521
223.557604	385.822540	19.065383	-0.042014	1.312164
223.679092	377.989460	19.070387	-0.042032	1.303737
223.586491	370.275210	19.075392	-0.042009	1.295346
223.585206	362.541790	19.080397	-0.042004	1.286896
223.515580	354.850424	19.085402	-0.041986	1.278424
223.443968	347.134851	19.090407	-0.041968	1.269867
223.355171	339.441661	19.095411	-0.041946	1.261275
223.305618	331.741056	19.100416	-0.041932	1.252623
223.027259	324.082720	19.105421	-0.041876	1.243914
222.852240	316.424115	19.110426	-0.041838	1.235164
222.931377	308.677418	19.115431	-0.041848	1.226300
222.976586	300.995058	19.120435	-0.041851	1.217438
222.705410	293.342838	19.125440	-0.041796	1.208485
222.693607	285.672754	19.130445	-0.041789	1.199495
222.591754	278.023280	19.135450	-0.041765	1.190443
222.455049	270.368724	19.140455	-0.041734	1.181309
222.350690	262.742811	19.145459	-0.041710	1.172145
222.410624	255.071059	19.150464	-0.041716	1.162887
222.305846	247.445089	19.155469	-0.041692	1.153576
222.036377	239.821469	19.160474	-0.041637	1.144158
221.793879	232.224194	19.165479	-0.041587	1.134700
221.695065	224.608432	19.170483	-0.041563	1.125170
221.763541	216.981375	19.175488	-0.041571	1.115580
221.765246	209.374132	19.180493	-0.041566	1.105918
221.720362	201.795485	19.185498	-0.041553	1.096197
221.504674	194.232929	19.190503	-0.041508	1.086372
221.538597	186.668589	19.195507	-0.041510	1.076511
221.432929	179.095026	19.200512	-0.041485	1.066515
221.166529	171.586467	19.205517	-0.041431	1.056474
221.148363	164.035182	19.210522	-0.041422	1.046337
220.935482	156.539078	19.215527	-0.041378	1.036130
221.068228	148.988841	19.220531	-0.041398	1.025829
220.721155	141.531207	19.225536	-0.041328	1.015437
220.729900	134.023571	19.230541	-0.041325	1.004953
220.558026	126.566518	19.235546	-0.041288	0.994387
220.087452	119.128444	19.240551	-0.041196	0.983659
219.897238	111.697874	19.245555	-0.041156	0.972894
219.407826	104.308606	19.250560	-0.041060	0.961993
218.793732	96.973136	19.255565	-0.040941	0.951015
218.342834	89.601910	19.260570	-0.040852	0.939896
217.714126	82.268638	19.265575	-0.040730	0.928655
217.400443	74.915842	19.270579	-0.040667	0.917331
216.698322	67.613924	19.275584	-0.040531	0.905838
216.304932	60.526500	19.280589	-0.040454	0.894620