Fri Mar 12 13:42:59 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.183349	-0.113442	0.000000	-0.000009	0.720919

0.016715	-0.107511	0.005005	0.000022	0.720872
0.126453	-0.123943	0.010010	0.000001	0.720879
0.155062	-0.128227	0.015014	-0.000004	0.720880
0.400443	-0.175041	0.020019	-0.000050	0.720874
0.395844	-0.170477	0.025024	-0.000049	0.720882
0.138165	-0.127549	0.030029	-0.000001	0.720876
0.060709	-0.113025	0.035034	0.000013	0.720877
0.237208	-0.144677	0.040038	-0.000020	0.720877
0.072210	-0.117935	0.045043	0.000011	0.720872
0.261612	-0.145896	0.050048	-0.000024	0.720883
0.390261	-0.173310	0.055053	-0.000048	0.720874
0.435639	-0.179272	0.060058	-0.000057	0.720879
0.088307	-0.117047	0.065062	0.000008	0.720879
-0.021805	-0.100476	0.070067	0.000028	0.720873
0.309323	-0.276378	0.075072	-0.000033	0.720643
0.305658	-0.331177	0.080077	-0.000033	0.720534
0.230689	-0.315035	0.085082	-0.000019	0.720540
0.248215	-0.318139	0.090086	-0.000022	0.720540
0.222580	-0.316967	0.095091	-0.000017	0.720533
0.320260	-0.331333	0.100096	-0.000035	0.720539
0.333547	-0.401590	0.105101	-0.000038	0.720406
0.196948	-0.470109	0.110106	-0.000012	0.720223
-0.136621	-0.410411	0.115110	0.000050	0.720223
-0.172527	-0.406933	0.120115	0.000056	0.720218
0.220642	-0.473169	0.125120	-0.000017	0.720225
0.000211	-0.470671	0.130125	0.000024	0.720153
0.014250	-0.603179	0.135130	0.000022	0.719897
0.181913	-0.631754	0.140134	-0.000010	0.719899
0.209597	-0.641302	0.145139	-0.000015	0.719890
0.087252	-0.613437	0.150144	0.000008	0.719902
0.165575	-0.772118	0.155149	-0.000007	0.719617
0.398352	-0.823575	0.160154	-0.000050	0.719597
0.415871	-0.823709	0.165158	-0.000053	0.719603
0.119927	-0.829621	0.170163	0.000002	0.719488
0.226762	-0.957008	0.175168	-0.000018	0.719274
-0.172949	-0.889366	0.180173	0.000056	0.719267
-0.218945	-0.880129	0.185178	0.000065	0.719269
0.161029	-1.076384	0.190182	-0.000006	0.719016
0.007871	-1.080857	0.195187	0.000023	0.718953
0.087679	-1.089397	0.200192	0.000008	0.718964
-0.046048	-1.184064	0.205197	0.000033	0.718731
0.118817	-1.255565	0.210202	0.000002	0.718648
0.248356	-1.278857	0.215206	-0.000022	0.718647
-0.000804	-1.360817	0.220211	0.000025	0.718398
0.050110	-1.391451	0.225216	0.000015	0.718355
-0.235286	-1.351551	0.230221	0.000068	0.718334
-0.672165	-1.435774	0.235226	0.000150	0.718014
-0.668834	-1.434534	0.240230	0.000149	0.718017
-0.664296	-1.457330	0.245235	0.000148	0.717974
-0.571719	-1.610066	0.250240	0.000131	0.717705
-0.448852	-1.635094	0.255245	0.000108	0.717699
-0.207582	-1.756232	0.260250	0.000063	0.717544
-0.251206	-1.828858	0.265254	0.000071	0.717385
-0.444928	-1.805507	0.270259	0.000107	0.717363
-0.341767	-1.964788	0.275264	0.000088	0.717085
-0.390487	-1.960433	0.280269	0.000097	0.717076
-0.520809	-2.048252	0.285274	0.000122	0.716856
-0.434169	-2.115098	0.290278	0.000105	0.716755
-0.435582	-2.178791	0.295283	0.000106	0.716628
-0.693154	-2.222546	0.300288	0.000154	0.716451
-0.949158	-2.198608	0.305293	0.000201	0.716408
-1.347277	-2.268800	0.310298	0.000275	0.716129
-2.841580	-2.000073	0.315302	0.000553	0.716134
-2.451562	-2.130639	0.320307	0.000481	0.716013
-2.763072	-2.140913	0.325312	0.000539	0.715882
-3.155546	-2.075118	0.330317	0.000612	0.715874
-3.277467	-2.134548	0.335322	0.000635	0.715713
-4.092633	-2.074873	0.340326	0.000786	0.715544
-4.254606	-2.050450	0.345331	0.000816	0.715535
-4.029217	-2.098459	0.350336	0.000774	0.715520
-4.708960	-2.125806	0.355341	0.000901	0.715225
-4.843066	-2.099302	0.360346	0.000926	0.715231
-5.056073	-2.060867	0.365350	0.000966	0.715232
-5.027288	-2.129679	0.370355	0.000960	0.715105
-5.503197	-2.142474	0.375360	0.001049	0.714912
-6.021217	-2.054105	0.380365	0.001145	0.714904
-6.097143	-2.039658	0.385370	0.001159	0.714906
-5.464865	-2.192280	0.390374	0.001042	0.714827
-6.871279	-2.055418	0.395379	0.001303	0.714601
-6.730188	-2.074719	0.400384	0.001277	0.714613
-6.794622	-2.068217	0.405389	0.001289	0.714603
-6.502420	-2.119786	0.410394	0.001235	0.714604
-6.876263	-2.169161	0.415398	0.001304	0.714374
-8.218986	-1.981996	0.420403	0.001554	0.714270
-7.444615	-2.116404	0.425408	0.001410	0.714277
-7.718989	-2.068802	0.430413	0.001461	0.714275
-7.989149	-2.020812	0.435418	0.001511	0.714275
-7.531338	-2.182942	0.440422	0.001426	0.714115
-8.984602	-1.999978	0.445427	0.001697	0.713964
-8.739343	-2.039966	0.450432	0.001651	0.713971
-8.552811	-2.076992	0.455437	0.001616	0.713964
-8.711554	-2.048301	0.460442	0.001646	0.713964
-8.572925	-2.069842	0.465446	0.001620	0.713971
-8.951594	-2.138033	0.470451	0.001690	0.713701
-9.364464	-2.088171	0.475456	0.001767	0.713654
-9.604972	-2.049230	0.480461	0.001812	0.713646
-9.620513	-2.047112	0.485466	0.001815	0.713645
-9.223931	-2.116497	0.490470	0.001741	0.713648
-9.404206	-2.096375	0.495475	0.001775	0.713624
-10.111082	-2.102763	0.500480	0.001906	0.713361
-10.396700	-2.055350	0.505485	0.001959	0.713354
-10.237721	-2.083306	0.510490	0.001930	0.713355
-10.260917	-2.077392	0.515494	0.001934	0.713358
-10.646829	-2.014150	0.520499	0.002006	0.713347
-10.123316	-2.103916	0.525504	0.001908	0.713354
-10.470045	-2.190344	0.530509	0.001973	0.713060
-11.725073	-1.987110	0.535514	0.002206	0.713019
-11.233982	-2.072789	0.540518	0.002115	0.713023
-11.258218	-2.070847	0.545523	0.002120	0.713018
-11.501813	-2.025507	0.550528	0.002165	0.713022
-11.183215	-2.083238	0.555533	0.002106	0.713020
-11.209391	-2.129660	0.560538	0.002110	0.712919
-12.297108	-2.042565	0.565542	0.002313	0.712706
-12.183865	-2.064021	0.570547	0.002292	0.712704
-11.779120	-2.130358	0.575552	0.002216	0.712715
-11.937448	-2.106170	0.580557	0.002246	0.712707
-12.326599	-2.037991	0.585562	0.002318	0.712705
-11.989607	-2.094766	0.590566	0.002256	0.712712
-12.445794	-2.141365	0.595571	0.002340	0.712457
-13.326357	-2.018385	0.600576	0.002504	0.712389
-13.317794	-2.022559	0.605581	0.002503	0.712384
-12.948900	-2.090115	0.610586	0.002434	0.712381
-12.877317	-2.099797	0.615590	0.002421	0.712387
-13.535858	-1.987926	0.620595	0.002543	0.712376
-12.883517	-2.099679	0.625600	0.002422	0.712385
-13.075334	-2.165000	0.630605	0.002458	0.712187
-14.206331	-2.014457	0.635610	0.002668	0.712085
-13.820884	-2.080890	0.640614	0.002596	0.712090
-13.791236	-2.090191	0.645619	0.002591	0.712082
-14.044959	-2.041557	0.650624	0.002638	0.712089
-14.030053	-2.047409	0.655629	0.002635	0.712082
-14.126187	-2.028657	0.660634	0.002653	0.712086
-14.138597	-2.145792	0.665638	0.002655	0.711848
-15.409462	-1.966694	0.670643	0.002892	0.711753
-14.733003	-2.083575	0.675648	0.002766	0.711761
-14.577765	-2.114118	0.680653	0.002737	0.711755
-15.310754	-1.984156	0.685658	0.002873	0.711754
-14.918950	-2.052233	0.690662	0.002800	0.711757
-14.732205	-2.088547	0.695667	0.002766	0.711751
-15.133200	-2.110511	0.700672	0.002840	0.711565
-16.246330	-1.969357	0.705677	0.003048	0.711451
-15.860686	-2.039469	0.710682	0.002976	0.711448
-15.637930	-2.075038	0.715686	0.002934	0.711457
-16.310157	-1.959383	0.720691	0.003059	0.711448
-15.864915	-2.036163	0.725696	0.002976	0.711454
-15.462358	-2.110619	0.730701	0.002902	0.711448
-16.032163	-2.030471	0.735706	0.003008	0.711406
-16.429029	-2.092589	0.740710	0.003081	0.711141
-16.697809	-2.049801	0.745715	0.003131	0.711130
-17.040875	-1.985170	0.750720	0.003195	0.711137
-16.644352	-2.058395	0.755725	0.003121	0.711132
-16.585167	-2.069082	0.760730	0.003110	0.711132
-16.306350	-2.116717	0.765734	0.003058	0.711136
-16.744724	-2.069442	0.770739	0.003140	0.711075
-17.408260	-2.053791	0.775744	0.003264	0.710870
-17.304405	-2.074706	0.780749	0.003244	0.710865
-17.813155	-1.984069	0.785754	0.003339	0.710865
-17.366849	-2.060693	0.790758	0.003256	0.710871
-17.287048	-2.080175	0.795763	0.003241	0.710861
-17.529353	-2.032367	0.800768	0.003286	0.710870
-17.539650	-2.093301	0.805773	0.003288	0.710745
-18.581274	-2.017918	0.810778	0.003482	0.710525
-18.105536	-2.097640	0.815782	0.003393	0.710535
-18.665775	-2.002750	0.820787	0.003497	0.710525
-18.523817	-2.025452	0.825792	0.003471	0.710530
-18.253275	-2.076032	0.830797	0.003421	0.710525
-18.828414	-1.973601	0.835802	0.003528	0.710525
-18.397988	-2.078151	0.840806	0.003448	0.710470
-19.364903	-2.038532	0.845811	0.003628	0.710205
-19.312834	-2.042796	0.850816	0.003618	0.710215
-19.832806	-1.953397	0.855821	0.003715	0.710208
-19.607469	-1.991859	0.860826	0.003673	0.710212
-19.259874	-2.052225	0.865830	0.003608	0.710215
-19.737884	-1.969757	0.870835	0.003697	0.710210
-19.231935	-2.058540	0.875840	0.003603	0.710212
-19.400370	-2.127665	0.880845	0.003634	0.710014
-20.714640	-1.958359	0.885850	0.003879	0.709885
-20.210050	-2.043349	0.890854	0.003785	0.709894
-19.770998	-2.128293	0.895859	0.003703	0.709881
-20.123968	-2.061626	0.900864	0.003769	0.709889
-20.212795	-2.048747	0.905869	0.003785	0.709883
-20.432306	-2.011368	0.910874	0.003826	0.709879
-20.321970	-2.136720	0.915878	0.003805	0.709668
-21.061858	-2.047148	0.920883	0.003943	0.709584
-21.194092	-2.020326	0.925888	0.003968	0.709590
-20.818982	-2.089074	0.930893	0.003898	0.709586
-21.017861	-2.055565	0.935898	0.003935	0.709583
-21.232782	-2.013110	0.940902	0.003975	0.709591
-21.158693	-2.031567	0.945907	0.003961	0.709580
-21.862814	-2.055956	0.950912	0.004092	0.709281
-22.201250	-2.006311	0.955917	0.004155	0.709259
-22.238655	-2.002164	0.960922	0.004162	0.709254
-21.678284	-2.098742	0.965926	0.004058	0.709261
-22.267903	-1.996412	0.970931	0.004167	0.709256
-22.312206	-1.985537	0.975936	0.004176	0.709262
-21.726992	-2.089623	0.980941	0.004067	0.709262
-22.119770	-2.120340	0.985946	0.004140	0.709060
-23.146888	-1.989124	0.990950	0.004331	0.708957
-22.924710	-2.032721	0.995955	0.004290	0.708949
-22.646959	-2.079868	1.000960	0.004238	0.708954
-22.864660	-2.043197	1.005965	0.004278	0.708949
-23.039076	-2.013616	1.010970	0.004311	0.708946
-22.533629	-2.097446	1.015974	0.004217	0.708959
-23.173592	-2.103587	1.020979	0.004336	0.708718
-24.022280	-1.993075	1.025984	0.004494	0.708637
-23.617075	-2.066097	1.030989	0.004418	0.708635
-23.701537	-2.051378	1.035994	0.004434	0.708635
-24.114172	-1.974857	1.040998	0.004511	0.708641
-24.059210	-1.988845	1.046003	0.004501	0.708632
-23.439718	-2.096786	1.051008	0.004385	0.708637
-23.822223	-2.104071	1.056013	0.004457	0.708486
-24.953719	-1.974649	1.061018	0.004667	0.708341
-24.356279	-2.076326	1.066022	0.004556	0.708351
-24.437572	-2.065015	1.071027	0.004571	0.708345
-24.643561	-2.026649	1.076032	0.004609	0.708348
-24.330464	-2.082905	1.081037	0.004551	0.708347
-24.677711	-2.024114	1.086042	0.004616	0.708341
-25.313814	-2.040290	1.091046	0.004734	0.708082
-25.946401	-1.965485	1.096051	0.004852	0.708005
-25.556413	-2.033344	1.101056	0.004779	0.708009
-25.476660	-2.050385	1.106061	0.004764	0.708003
-26.011540	-1.956007	1.111066	0.004864	0.708001
-25.188208	-2.097912	1.116070	0.004711	0.708011
-25.264479	-2.088001	1.121075	0.004725	0.708004
-25.777987	-2.072407	1.126080	0.004820	0.707852
-26.776389	-1.973596	1.131085	0.005006	0.707693
-26.413526	-2.039814	1.136090	0.004939	0.707690
-26.463182	-2.027212	1.141094	0.004948	0.707697
-26.811656	-1.970570	1.146099	0.005013	0.707686
-26.218051	-2.072312	1.151104	0.004902	0.707695
-26.092280	-2.094909	1.156109	0.004879	0.707694
-26.612833	-2.051021	1.161114	0.004976	0.707596
-27.194400	-2.058177	1.166118	0.005084	0.707374
-27.240845	-2.054511	1.171123	0.005093	0.707365
-27.450883	-2.013168	1.176128	0.005132	0.707373
-27.444798	-2.014781	1.181133	0.005130	0.707372
-27.257021	-2.051153	1.186138	0.005095	0.707366
-27.425519	-2.017058	1.191142	0.005127	0.707374
-27.631487	-1.995032	1.196147	0.005165	0.707345
-27.775231	-2.103280	1.201152	0.005192	0.707076
-27.928978	-2.076170	1.206157	0.005220	0.707076
-28.657019	-1.947937	1.211162	0.005356	0.707072
-27.949950	-2.071584	1.216166	0.005224	0.707077
-27.987349	-2.069062	1.221171	0.005231	0.707069
-28.455976	-1.982443	1.226176	0.005318	0.707075
-28.201484	-2.060252	1.231181	0.005271	0.707010
-29.161271	-2.023789	1.236186	0.005450	0.706740
-28.942936	-2.056708	1.241190	0.005409	0.706752
-29.409674	-1.979051	1.246195	0.005496	0.706741
-28.958135	-2.056765	1.251200	0.005412	0.706747
-28.674824	-2.107444	1.256205	0.005359	0.706746
-29.264189	-2.004860	1.261210	0.005469	0.706741
-29.099013	-2.062303	1.266214	0.005438	0.706685
-29.850148	-2.054770	1.271219	0.005578	0.706431
-29.870356	-2.047035	1.276224	0.005582	0.706440
-30.119994	-2.004345	1.281229	0.005628	0.706436
-30.139677	-2.001753	1.286234	0.005632	0.706434
-29.802618	-2.058014	1.291238	0.005569	0.706442
-30.328685	-1.968185	1.296243	0.005667	0.706434
-30.220236	-1.984160	1.301248	0.005647	0.706441
-30.122195	-2.138124	1.306253	0.005628	0.706167
-31.250749	-1.959722	1.311258	0.005838	0.706121
-30.946885	-2.009603	1.316262	0.005782	0.706130
-30.750035	-2.052016	1.321267	0.005745	0.706115
-30.964189	-2.011845	1.326272	0.005785	0.706119
-31.088119	-1.988339	1.331277	0.005808	0.706122
-30.908575	-2.023591	1.336282	0.005775	0.706115
-30.935915	-2.111709	1.341286	0.005780	0.705928
-31.931761	-1.971507	1.346291	0.005965	0.705853
-31.678771	-2.014766	1.351296	0.005918	0.705857
-31.378115	-2.067997	1.356301	0.005862	0.705858
-31.496480	-2.049598	1.361306	0.005884	0.705853
-31.273797	-2.085708	1.366310	0.005843	0.705860
-31.504312	-2.097958	1.371315	0.005885	0.705753
-32.647808	-2.007379	1.376320	0.006098	0.705525
-32.102116	-2.106505	1.381325	0.005997	0.705521
-32.540705	-2.030281	1.386330	0.006078	0.705517
-32.371994	-2.056346	1.391334	0.006047	0.705525
-32.658380	-2.010319	1.396339	0.006100	0.705515
-32.502300	-2.036460	1.401344	0.006071	0.705519
-32.396765	-2.157025	1.406349	0.006051	0.705314
-33.634712	-1.991999	1.411354	0.006282	0.705202
-33.453666	-2.019607	1.416358	0.006248	0.705211
-33.234056	-2.062773	1.421363	0.006207	0.705203
-33.267158	-2.055073	1.426368	0.006213	0.705207
-33.319623	-2.046286	1.431373	0.006223	0.705206
-33.430716	-2.030265	1.436378	0.006244	0.705198
-33.371304	-2.168761	1.441382	0.006233	0.704941
-34.591778	-1.982671	1.446387	0.006460	0.704877
-34.577187	-1.981692	1.451392	0.006457	0.704885
-34.212624	-2.048878	1.456397	0.006389	0.704880
-34.606063	-1.981551	1.461402	0.006462	0.704875
-34.150707	-2.059536	1.466406	0.006378	0.704881
-34.244766	-2.047015	1.471411	0.006395	0.704873
-34.683321	-2.066804	1.476416	0.006477	0.704675
-35.413400	-1.981993	1.481421	0.006613	0.704584
-35.308468	-2.001653	1.486426	0.006593	0.704582
-34.838646	-2.082027	1.491430	0.006506	0.704589
-35.326708	-1.999222	1.496435	0.006596	0.704581
-35.235278	-2.014267	1.501440	0.006579	0.704583
-34.717615	-2.105843	1.506445	0.006483	0.704585
-35.690067	-2.047598	1.511450	0.006664	0.704353
-36.562531	-1.939351	1.516454	0.006826	0.704257
-36.152137	-2.017690	1.521459	0.006750	0.704247
-35.715961	-2.093347	1.526464	0.006669	0.704251
-36.268912	-1.993781	1.531469	0.006772	0.704253
-36.228092	-2.003753	1.536474	0.006764	0.704248
-35.803854	-2.074959	1.541478	0.006685	0.704257
-36.122211	-2.077145	1.546483	0.006744	0.704138
-37.306445	-1.960628	1.551488	0.006965	0.703947
-36.556163	-2.095269	1.556493	0.006825	0.703946
-37.119834	-1.997389	1.561498	0.006930	0.703940
-36.868662	-2.037008	1.566502	0.006883	0.703951
-36.809442	-2.053200	1.571507	0.006872	0.703940
-36.734092	-2.065767	1.576512	0.006858	0.703941
-37.041010	-2.088458	1.581517	0.006915	0.703785
-37.961962	-2.005251	1.586522	0.007087	0.703622
-37.365794	-2.106615	1.591526	0.006976	0.703632
-37.997210	-1.998742	1.596531	0.007093	0.703623
-38.093947	-1.979584	1.601536	0.007111	0.703626
-37.351940	-2.111591	1.606541	0.006973	0.703627
-37.419242	-2.100427	1.611546	0.006986	0.703625
-37.944707	-2.118299	1.616550	0.007083	0.703400
-38.420048	-2.066901	1.621555	0.007172	0.703333
-38.452148	-2.059887	1.626560	0.007178	0.703336
-38.263872	-2.091893	1.631565	0.007143	0.703339
-38.837914	-1.993279	1.636570	0.007250	0.703331
-38.368687	-2.073831	1.641574	0.007162	0.703338
-38.544601	-2.089656	1.646579	0.007195	0.703242
-39.724159	-1.998374	1.651584	0.007415	0.703002
-39.154913	-2.100704	1.656589	0.007309	0.703001
-39.636617	-2.018202	1.661594	0.007398	0.702994
-39.711107	-2.000770	1.666598	0.007412	0.703002
-39.588183	-2.025184	1.671603	0.007389	0.702997
-39.435497	-2.051387	1.676608	0.007361	0.702999
-39.369277	-2.081264	1.681613	0.007348	0.702963
-40.221683	-2.068616	1.686618	0.007507	0.702681
-39.811020	-2.136840	1.691622	0.007431	0.702692
-40.414778	-2.033035	1.696627	0.007543	0.702684
-40.668319	-1.986075	1.701632	0.007590	0.702687
-40.379647	-2.037801	1.706637	0.007536	0.702687
-40.237839	-2.067396	1.711642	0.007510	0.702678
-40.363315	-2.085137	1.716646	0.007533	0.702597
-41.757924	-1.952799	1.721651	0.007793	0.702362
-41.155205	-2.059094	1.726656	0.007681	0.702365
-41.169179	-2.056819	1.731661	0.007683	0.702364
-41.676046	-1.968240	1.736666	0.007778	0.702361
-41.069592	-2.072190	1.741670	0.007665	0.702369
-41.183403	-2.057132	1.746675	0.007686	0.702359
-41.616237	-1.977777	1.751680	0.007766	0.702363
-41.622752	-2.086574	1.756685	0.007768	0.702141
-42.420056	-1.983987	1.761690	0.007916	0.702061
-42.114920	-2.034444	1.766694	0.007859	0.702069
-42.190668	-2.024241	1.771699	0.007873	0.702062
-42.150753	-2.029953	1.776704	0.007866	0.702065
-42.049760	-2.046132	1.781709	0.007847	0.702069
-42.439610	-1.977722	1.786714	0.007919	0.702067
-42.162230	-2.131228	1.791718	0.007868	0.701856
-42.923120	-2.053630	1.796723	0.008010	0.701739
-43.273061	-1.992565	1.801728	0.008075	0.701736
-43.055773	-2.028325	1.806733	0.008034	0.701742
-43.168642	-2.012156	1.811738	0.008055	0.701734
-43.116312	-2.018078	1.816742	0.008045	0.701741
-43.247667	-1.998882	1.821747	0.008070	0.701733
-43.198006	-2.094650	1.826752	0.008061	0.701557
-43.592797	-2.085428	1.831757	0.008134	0.701433
-43.978170	-2.019854	1.836762	0.008206	0.701427
-44.007075	-2.009596	1.841766	0.008211	0.701437
-43.758513	-2.057720	1.846771	0.008165	0.701429
-43.935622	-2.025853	1.851776	0.008198	0.701430
-43.815684	-2.045876	1.856781	0.008175	0.701433
-44.200533	-2.116924	1.861786	0.008247	0.701150
-44.322858	-2.111435	1.866790	0.008270	0.701117
-44.880593	-2.013967	1.871795	0.008374	0.701113
-44.695393	-2.046592	1.876800	0.008339	0.701114
-44.505364	-2.077842	1.881805	0.008304	0.701119
-45.059752	-1.982705	1.886810	0.008407	0.701112
-44.498856	-2.106717	1.891814	0.008302	0.701063
-45.083737	-2.101687	1.896819	0.008411	0.700862
-45.523808	-2.021270	1.901824	0.008493	0.700866
-45.669279	-1.991577	1.906829	0.008520	0.700874
-45.373449	-2.050787	1.911834	0.008465	0.700861
-45.008852	-2.110473	1.916838	0.008397	0.700872
-45.282778	-2.064653	1.921843	0.008448	0.700866
-45.837766	-2.110323	1.926848	0.008552	0.700572
-45.937315	-2.111345	1.931853	0.008570	0.700534
-46.502514	-2.014657	1.936858	0.008675	0.700526
-46.214745	-2.063072	1.941862	0.008622	0.700532
-46.092849	-2.087489	1.946867	0.008599	0.700527
-46.251496	-2.058220	1.951872	0.008629	0.700529
-46.270459	-2.115266	1.956877	0.008632	0.700406
-47.753278	-1.948424	1.961882	0.008908	0.700208
-46.910042	-2.095092	1.966886	0.008751	0.700216
-47.236631	-2.040106	1.971891	0.008812	0.700209
-47.376611	-2.014819	1.976896	0.008838	0.700210
-46.841509	-2.106536	1.981901	0.008738	0.700218
-47.453809	-2.001599	1.986906	0.008852	0.700209
-47.227704	-2.094778	1.991910	0.008810	0.700102
-47.870515	-2.084576	1.996915	0.008930	0.699890
-47.991283	-2.061224	2.001920	0.008952	0.699894

-47.974760	-2.065026	2.011917	0.008949	0.699892
-48.123919	-2.040551	2.021914	0.008977	0.699888
-47.981200	-2.065164	2.031910	0.008950	0.699890
-48.197641	-2.024531	2.041907	0.008990	0.699894
-48.325455	-2.072604	2.051904	0.009014	0.699750
-48.292112	-2.008584	2.061901	0.009008	0.699892
-48.090864	-2.046138	2.071898	0.008970	0.699889
-48.044675	-2.053228	2.081894	0.008962	0.699892
-48.037966	-2.052429	2.091891	0.008960	0.699896
-47.906337	-2.077067	2.101888	0.008936	0.699893
-47.890669	-2.080254	2.111885	0.008933	0.699893
-48.088035	-2.046258	2.121882	0.008970	0.699890
-47.900165	-2.080078	2.131878	0.008935	0.699890
-48.140711	-2.036455	2.141875	0.008979	0.699891
-47.470453	-2.030144	2.151872	0.008855	0.700147
-47.324798	-2.022412	2.161869	0.008827	0.700215
-47.171713	-2.050336	2.171866	0.008799	0.700214
-47.175413	-2.049145	2.181862	0.008799	0.700215
-47.114931	-1.993038	2.191859	0.008788	0.700351
-46.192347	-2.069725	2.201856	0.008616	0.700529
-46.349363	-2.041269	2.211853	0.008645	0.700530
-46.496551	-2.015684	2.221850	0.008673	0.700529
-45.920956	-2.050866	2.231846	0.008566	0.700666
-45.492757	-2.026617	2.241843	0.008486	0.700870
-45.328519	-2.055719	2.251840	0.008455	0.700870
-45.598858	-2.008059	2.261837	0.008505	0.700869
-45.061869	-2.034159	2.271834	0.008405	0.701010
-44.782234	-2.032255	2.281830	0.008353	0.701115
-44.734481	-2.040161	2.291827	0.008344	0.701117
-44.672490	-2.033241	2.301824	0.008333	0.701153
-44.000883	-2.015380	2.311821	0.008208	0.701432
-43.923640	-2.030320	2.321818	0.008193	0.701430
-43.719713	-2.064993	2.331814	0.008155	0.701433
-43.688698	-1.978797	2.341811	0.008149	0.701619
-42.875170	-2.063742	2.351808	0.007998	0.701741
-43.226022	-2.002578	2.361805	0.008063	0.701738
-42.752013	-2.051228	2.371802	0.007975	0.701811
-41.986186	-2.060691	2.381798	0.007832	0.702068
-41.953851	-2.064841	2.391795	0.007826	0.702071
-41.997246	-2.059043	2.401792	0.007834	0.702067
-41.684945	-2.024385	2.411789	0.007776	0.702250
-41.218059	-2.051942	2.421786	0.007689	0.702363
-41.314290	-2.033631	2.431782	0.007707	0.702365
-41.068563	-2.060831	2.441779	0.007661	0.702399
-40.492620	-2.019225	2.451776	0.007554	0.702691
-40.396702	-2.036529	2.461773	0.007536	0.702690
-40.197778	-2.074364	2.471770	0.007499	0.702686
-39.953553	-2.023691	2.481766	0.007453	0.702876
-39.384022	-2.062529	2.491763	0.007347	0.703003
-39.387129	-2.062060	2.501760	0.007348	0.703003
-39.624225	-1.999595	2.511757	0.007392	0.703044
-38.543118	-2.049116	2.521754	0.007190	0.703333
-38.641156	-2.030676	2.531750	0.007209	0.703335
-38.532257	-2.047622	2.541747	0.007188	0.703340
-38.102644	-2.032038	2.551744	0.007108	0.703526
-37.873901	-2.021012	2.561741	0.007066	0.703631
-37.748707	-2.045277	2.571738	0.007042	0.703627
-37.647452	-2.034909	2.581734	0.007023	0.703685
-36.894186	-2.039008	2.591731	0.006883	0.703947
-36.841862	-2.047957	2.601728	0.006873	0.703948
-36.970184	-2.025939	2.611725	0.006897	0.703947
-36.184794	-2.045869	2.621722	0.006751	0.704189
-36.306933	-1.991578	2.631718	0.006774	0.704254
-35.801484	-2.080535	2.641715	0.006679	0.704257
-35.815622	-2.022893	2.651712	0.006682	0.704368
-35.096923	-2.042877	2.661709	0.006548	0.704586
-35.164288	-2.032348	2.671706	0.006561	0.704583
-35.253775	-2.015277	2.681702	0.006577	0.704586
-34.472591	-2.032901	2.691699	0.006432	0.704831
-34.237579	-2.048189	2.701696	0.006388	0.704884
-34.300062	-2.038221	2.711693	0.006399	0.704882
-34.079694	-2.034674	2.721690	0.006358	0.704968
-33.534212	-2.014166	2.731686	0.006257	0.705206
-33.178347	-2.075945	2.741683	0.006190	0.705209
-33.326111	-2.050736	2.751680	0.006218	0.705207
-32.677164	-2.043347	2.761677	0.006097	0.705455
-32.673777	-2.012539	2.771674	0.006096	0.705518
-32.334475	-2.072101	2.781670	0.006033	0.705520
-32.341086	-2.026146	2.791667	0.006034	0.705610
-31.591985	-2.035796	2.801664	0.005895	0.705859
-31.381007	-2.074617	2.811661	0.005855	0.705857
-31.504270	-2.053390	2.821658	0.005878	0.705856
-31.309013	-2.010440	2.831654	0.005842	0.706012
-30.780993	-2.049222	2.841651	0.005744	0.706124
-31.191256	-1.977378	2.851648	0.005820	0.706121
-30.630558	-2.003935	2.861645	0.005715	0.706269
-30.310955	-1.975247	2.871642	0.005656	0.706441
-30.146724	-2.005113	2.881638	0.005625	0.706440
-29.874325	-2.008131	2.891635	0.005575	0.706531
-29.148670	-2.028561	2.901632	0.005439	0.706750
-28.869770	-2.079100	2.911629	0.005387	0.706749
-29.106061	-2.036910	2.921626	0.005431	0.706749
-28.548325	-2.019274	2.931622	0.005327	0.706984
-28.251997	-2.024651	2.941619	0.005272	0.707079
-28.346187	-2.006701	2.951616	0.005290	0.707082
-28.031433	-2.020066	2.961613	0.005231	0.707168
-27.431014	-2.024062	2.971610	0.005119	0.707375
-27.320070	-2.042909	2.981606	0.005099	0.707377
-27.483022	-2.013910	2.991603	0.005129	0.707377
-26.812990	-1.995606	3.001600	0.005004	0.707653
-26.551279	-2.019624	3.011597	0.004955	0.707698
-26.782142	-1.980547	3.021594	0.004998	0.707694
-26.189963	-2.011597	3.031590	0.004888	0.707844
-25.662285	-2.021387	3.041587	0.004790	0.708013
-25.546967	-2.041948	3.051584	0.004768	0.708013
-25.463141	-2.058339	3.061581	0.004752	0.708010
-25.074206	-1.968115	3.071578	0.004680	0.708330
-24.612280	-2.041911	3.081574	0.004594	0.708347
-24.537382	-2.053045	3.091571	0.004580	0.708352
-24.493651	-2.014431	3.101568	0.004572	0.708445
-23.715966	-2.056176	3.111565	0.004427	0.708639
-23.992077	-2.007128	3.121562	0.004478	0.708639
-23.655725	-2.066263	3.131558	0.004415	0.708641
-23.267592	-2.011930	3.141555	0.004343	0.708888
-22.943368	-2.034903	3.151552	0.004283	0.708958
-22.909518	-2.040826	3.161549	0.004276	0.708958
-23.043282	-1.976002	3.171546	0.004301	0.709040
-21.889236	-2.070790	3.181542	0.004086	0.709262
-22.247833	-2.004192	3.191539	0.004153	0.709268
-22.147192	-2.022722	3.201536	0.004134	0.709267
-21.344645	-2.021577	3.211533	0.003985	0.709555
-21.326946	-2.004499	3.221530	0.003981	0.709596
-21.143847	-2.037450	3.231526	0.003947	0.709595
-21.112817	-1.987224	3.241523	0.003941	0.709707
-20.308310	-2.037270	3.251520	0.003792	0.709893
-20.370092	-2.026267	3.261517	0.003803	0.709893
-20.447122	-2.015126	3.271514	0.003817	0.709888
-19.574783	-2.023034	3.281510	0.003655	0.710183
-19.571767	-2.006019	3.291507	0.003654	0.710219
-19.197081	-2.072682	3.301504	0.003584	0.710219
-19.510728	-1.967864	3.311501	0.003643	0.710317
-18.727323	-2.000718	3.321498	0.003497	0.710530
-18.420446	-2.054160	3.331494	0.003440	0.710533
-18.762906	-1.991534	3.341491	0.003503	0.710536
-17.612327	-2.040305	3.351488	0.003289	0.710848
-17.840334	-1.987232	3.361485	0.003332	0.710873
-17.483675	-2.051149	3.371482	0.003265	0.710872
-17.745769	-1.964518	3.381478	0.003314	0.710952
-17.091506	-1.986158	3.391475	0.003192	0.711142
-16.902673	-2.019853	3.401472	0.003157	0.711142
-17.164181	-1.960258	3.411469	0.003205	0.711168
-16.351622	-1.960474	3.421466	0.003054	0.711456
-15.881823	-2.044471	3.431462	0.002967	0.711456
-15.972727	-2.028358	3.441459	0.002983	0.711456
-15.446982	-2.019810	3.451456	0.002885	0.711660
-15.327612	-1.989663	3.461453	0.002863	0.711762
-15.072811	-2.034681	3.471450	0.002816	0.711763
-15.202936	-1.982336	3.481446	0.002840	0.711821
-14.340492	-2.000903	3.491443	0.002679	0.712091
-14.300657	-2.007537	3.501440	0.002672	0.712092
-14.327605	-2.003056	3.511437	0.002677	0.712091
-13.892437	-1.971954	3.521434	0.002596	0.712308
-13.489874	-2.005439	3.531430	0.002521	0.712384
-13.572968	-1.988247	3.541427	0.002536	0.712389
-13.170246	-1.999584	3.551424	0.002461	0.712509
-12.646171	-1.992654	3.561421	0.002363	0.712709
-12.348067	-2.044952	3.571418	0.002308	0.712711
-12.593389	-2.001170	3.581414	0.002353	0.712711
-12.060328	-1.979946	3.591411	0.002254	0.712943
-11.851442	-1.975350	3.601408	0.002215	0.713026
-11.778988	-1.988580	3.611405	0.002202	0.713025
-11.595932	-1.954396	3.621402	0.002168	0.713158
-10.601166	-2.029697	3.631398	0.001982	0.713361
-10.687037	-2.014404	3.641395	0.001998	0.713361
-10.606252	-2.029079	3.651392	0.001983	0.713361
-10.425063	-1.954402	3.661389	0.001949	0.713574
-9.961601	-1.996459	3.671386	0.001863	0.713654
-9.965847	-1.996338	3.681382	0.001864	0.713653
-9.663330	-2.006176	3.691379	0.001807	0.713741
-9.047002	-1.999723	3.701376	0.001693	0.713972
-9.131728	-1.985264	3.711373	0.001708	0.713971
-8.944584	-2.019635	3.721370	0.001673	0.713969
-8.591502	-1.963015	3.731366	0.001608	0.714206
-8.129483	-2.008550	3.741363	0.001522	0.714280
-8.192071	-1.997170	3.751360	0.001533	0.714280
-8.065631	-1.972527	3.761357	0.001510	0.714374
-6.918499	-2.060053	3.771354	0.001296	0.714606
-6.853359	-2.069697	3.781350	0.001284	0.714610
-6.672360	-2.101950	3.791347	0.001250	0.714610
-6.983194	-2.015009	3.801344	0.001308	0.714673
-5.856766	-2.097964	3.811341	0.001098	0.714907
-6.059440	-2.062416	3.821338	0.001136	0.714906
-6.250515	-2.029012	3.831334	0.001171	0.714904
-5.706884	-2.071833	3.841331	0.001070	0.715012
-5.090820	-2.070423	3.851328	0.000955	0.715232
-5.032128	-2.080847	3.861325	0.000944	0.715232
-5.227215	-2.047281	3.871322	0.000981	0.715230
-4.821655	-2.039981	3.881318	0.000905	0.715388
-3.910660	-2.122898	3.891315	0.000735	0.715546
-4.379182	-2.038495	3.901312	0.000822	0.715547
-3.951674	-2.115802	3.911309	0.000743	0.715545
-3.636692	-2.039333	3.921306	0.000684	0.715808
-3.385181	-2.048416	3.931302	0.000637	0.715879
-3.093189	-2.098979	3.941299	0.000583	0.715882
-3.215816	-2.069214	3.951296	0.000606	0.715898
-2.515484	-2.075168	3.961293	0.000475	0.716133
-2.651467	-2.052214	3.971290	0.000500	0.716131
-2.580136	-2.063073	3.981286	0.000487	0.716135
-2.267981	-2.014044	3.991283	0.000429	0.716342
-2.034260	-2.000234	4.001280	0.000385	0.716452
-1.936157	-2.017321	4.011277	0.000367	0.716453
-1.864784	-1.944935	4.021274	0.000354	0.716621
-1.807238	-1.887756	4.031270	0.000343	0.716755
-1.114386	-2.009994	4.041267	0.000214	0.716757
-1.221539	-1.863743	4.051264	0.000234	0.717009
-1.260154	-1.817763	4.061261	0.000241	0.717086
-1.096454	-1.808409	4.071258	0.000210	0.717163
-1.033464	-1.709822	4.081254	0.000198	0.717380
-0.729710	-1.761048	4.091251	0.000142	0.717386
-0.850328	-1.576940	4.101248	0.000164	0.717707
-0.852967	-1.574420	4.111245	0.000165	0.717711
-0.478948	-1.486845	4.121242	0.000095	0.718016
-0.699942	-1.424427	4.131238	0.000136	0.718062
-0.918768	-1.237120	4.141235	0.000176	0.718355
-0.678650	-1.203426	4.151232	0.000132	0.718506
-0.552952	-1.156145	4.161229	0.000108	0.718644
-0.346963	-1.038042	4.171226	0.000070	0.718949
-0.454104	-0.942514	4.181222	0.000090	0.719100
-0.364628	-0.863521	4.191219	0.000073	0.719287
-0.335145	-0.710076	4.201216	0.000067	0.719600
-0.780910	-0.521618	4.211213	0.000150	0.719815
-0.438137	-0.453604	4.221210	0.000086	0.720070
-0.088362	-0.388933	4.231206	0.000021	0.720320
-0.086991	-0.257447	4.241203	0.000020	0.720579
-0.097659	-0.104429	4.251200	0.000022	0.720877
-0.113086	0.020496	4.261197	0.000025	0.721117
0.000000	0.166381	4.271194	0.000004	0.721444

-0.199767	0.848305	4.276198	0.000041	0.722714
0.168155	2.047538	4.281203	-0.000029	0.725192
0.456071	3.847980	4.286208	-0.000084	0.728805
0.635262	6.233064	4.291213	-0.000118	0.733494
1.037122	9.073168	4.296218	-0.000195	0.739103
1.268378	12.433343	4.301222	-0.000240	0.745603
1.653901	16.220795	4.306227	-0.000315	0.752903
2.283378	20.362556	4.311232	-0.000435	0.760874
2.717204	24.953769	4.316237	-0.000518	0.769527
2.950035	29.938213	4.321242	-0.000565	0.778736
3.411606	35.229960	4.326246	-0.000655	0.788463
3.775597	40.859891	4.331251	-0.000726	0.798641
4.199167	46.772925	4.336256	-0.000809	0.809205
4.824595	52.946310	4.341261	-0.000929	0.820146
5.254680	59.417550	4.346266	-0.001014	0.831391
5.762042	66.102756	4.351270	-0.001112	0.842870
6.066920	73.048104	4.356275	-0.001174	0.854566
7.825595	79.933675	4.361280	-0.001506	0.866425
11.419232	86.747953	4.366285	-0.002179	0.878530
11.909680	94.294669	4.371290	-0.002276	0.890765
12.567691	101.966242	4.376294	-0.002403	0.903077
13.446563	109.753949	4.381299	-0.002572	0.915463
13.872433	117.717851	4.386304	-0.002656	0.927831
14.858173	125.721283	4.391309	-0.002845	0.940243
16.217311	133.765200	4.396314	-0.003103	0.952651
17.104467	141.984760	4.401318	-0.003274	0.965035
17.852501	150.312528	4.406323	-0.003419	0.977383
18.813337	158.687067	4.411328	-0.003603	0.989697
19.753063	167.109700	4.416333	-0.003784	1.001922
20.604720	175.568926	4.421338	-0.003948	1.014029
21.395675	184.084424	4.426342	-0.004101	1.026055
22.211583	192.638299	4.431347	-0.004258	1.038000
22.883229	201.233761	4.436352	-0.004389	1.049831
23.641141	209.850507	4.441357	-0.004536	1.061579
23.919905	218.569977	4.446362	-0.004593	1.073223
24.795128	227.174058	4.451366	-0.004762	1.084726
25.466496	235.836733	4.456371	-0.004893	1.096139
25.970668	244.509982	4.461376	-0.004992	1.107410
26.786707	253.146365	4.466381	-0.005150	1.118588
27.347321	261.814021	4.471386	-0.005260	1.129639
28.147827	270.444121	4.476390	-0.005414	1.140588
28.774232	279.126497	4.481395	-0.005537	1.151460
29.312275	287.780419	4.486400	-0.005643	1.162176
30.300300	296.354656	4.491405	-0.005832	1.172791
30.920433	304.972923	4.496410	-0.005953	1.183288
31.190284	313.651908	4.501414	-0.006009	1.193693
32.042821	322.203091	4.506419	-0.006174	1.203975
32.933732	330.744741	4.511424	-0.006345	1.214165
34.106047	339.234741	4.516429	-0.006569	1.224266
34.261213	347.902123	4.521434	-0.006603	1.234289
35.108404	356.402886	4.526438	-0.006767	1.244175
36.024086	364.904279	4.531443	-0.006943	1.253997
36.730756	373.411858	4.536448	-0.007080	1.263709
37.450606	381.936530	4.541453	-0.007220	1.273368
38.159111	390.415569	4.546458	-0.007357	1.282902
38.570778	398.956620	4.551462	-0.007439	1.292378
39.274216	407.416456	4.556467	-0.007576	1.301750
39.974050	415.932757	4.561472	-0.007712	1.311115
40.423497	424.465890	4.566477	-0.007801	1.320386
40.635604	432.934195	4.571482	-0.007846	1.329481
41.105141	441.365568	4.576486	-0.007939	1.338520
41.798457	449.739936	4.581491	-0.008074	1.347478
42.094789	458.178375	4.586496	-0.008134	1.356375
42.661710	466.553860	4.591501	-0.008245	1.365194
43.431509	474.896526	4.596506	-0.008394	1.373958
43.901904	483.282110	4.601510	-0.008487	1.382659
44.640698	491.644113	4.606515	-0.008630	1.391327
44.853042	500.040028	4.611520	-0.008675	1.399886
45.637107	508.336262	4.616525	-0.008827	1.408389
45.882599	516.716282	4.621530	-0.008878	1.416834
46.111262	525.076523	4.626534	-0.008926	1.425208
46.872583	533.370335	4.631539	-0.009073	1.433553
47.489926	541.649664	4.636544	-0.009193	1.441812
47.954844	549.978531	4.641549	-0.009285	1.450048
48.337205	558.301726	4.646554	-0.009362	1.458219
48.656319	566.624914	4.651558	-0.009427	1.466333
49.366325	574.945557	4.656563	-0.009565	1.474462
49.751113	583.222831	4.661568	-0.009642	1.482454
50.326658	591.493289	4.666573	-0.009754	1.490426
50.555758	599.800745	4.671578	-0.009802	1.498337
51.128001	608.037722	4.676582	-0.009914	1.506193
51.745592	616.297596	4.681587	-0.010035	1.514036
52.117505	624.547241	4.686592	-0.010109	1.521791
52.662942	632.798986	4.691597	-0.010216	1.529535
52.987326	641.077024	4.696602	-0.010282	1.537231
53.742436	649.275055	4.701606	-0.010428	1.544880
54.171808	657.555662	4.706611	-0.010513	1.552517
54.742789	665.767038	4.711616	-0.010625	1.560075
55.404207	673.977244	4.716621	-0.010754	1.567608
55.807955	682.236053	4.721626	-0.010834	1.575112
56.294256	690.463048	4.726630	-0.010930	1.582563
56.973190	698.679157	4.731635	-0.011062	1.589997
57.461972	706.901239	4.736640	-0.011158	1.597374
57.904458	715.122343	4.741645	-0.011246	1.604710
58.096291	723.385947	4.746650	-0.011287	1.612014
58.628908	731.580244	4.751654	-0.011392	1.619273
59.077450	739.793684	4.756659	-0.011481	1.626503
59.318210	748.083557	4.761664	-0.011531	1.633739
59.980717	756.232691	4.766669	-0.011660	1.640880
60.227789	764.443637	4.771674	-0.011711	1.647986
60.522947	772.660614	4.776678	-0.011771	1.655072
61.051506	780.831736	4.781683	-0.011875	1.662121
61.523826	788.999261	4.786688	-0.011968	1.669130
61.893335	797.209846	4.791693	-0.012043	1.676131
62.221592	805.392725	4.796698	-0.012109	1.683075
62.550259	813.577685	4.801702	-0.012176	1.689992
62.688620	821.819718	4.806707	-0.012207	1.696902
63.249854	829.944484	4.811712	-0.012317	1.703743
64.097455	838.073799	4.816717	-0.012480	1.710598
64.169937	846.316058	4.821722	-0.012499	1.717417
64.304107	854.495208	4.826726	-0.012529	1.724165
64.796634	862.638103	4.831731	-0.012626	1.730904
65.376435	870.778895	4.836736	-0.012739	1.737625
65.879957	878.918593	4.841741	-0.012838	1.744310
66.306369	887.090733	4.846746	-0.012923	1.750986
66.760570	895.249688	4.851750	-0.013013	1.757629
66.934722	903.439350	4.856755	-0.013051	1.764236
67.444069	911.576457	4.861760	-0.013151	1.770818
67.861422	919.761829	4.866765	-0.013234	1.777403
68.201280	927.913345	4.871770	-0.013303	1.783927
68.511818	936.103764	4.876774	-0.013366	1.790455
69.030864	944.282177	4.881779	-0.013468	1.796974
69.314704	952.411330	4.886784	-0.013526	1.803403
69.769458	960.543364	4.891789	-0.013616	1.809831
70.251292	968.670758	4.896794	-0.013711	1.816237
70.717534	976.784122	4.901798	-0.013803	1.822606
71.005813	984.949315	4.906803	-0.013862	1.828973
71.257233	993.106236	4.911808	-0.013914	1.835306
71.807607	1001.202011	4.916813	-0.014022	1.841606
72.244236	1009.329239	4.921818	-0.014109	1.847895
72.633920	1017.483809	4.926822	-0.014187	1.854178
73.339664	1025.570052	4.931827	-0.014323	1.860424
73.726522	1033.710247	4.936832	-0.014401	1.866653
74.062581	1041.901465	4.941837	-0.014469	1.872894
74.514978	1050.020348	4.946842	-0.014558	1.879074
74.872587	1058.128439	4.951846	-0.014630	1.885213
75.100172	1066.297055	4.956851	-0.014678	1.891363
75.322404	1074.436394	4.961856	-0.014725	1.897471
75.697614	1082.568065	4.966861	-0.014800	1.903571
75.884544	1090.714688	4.971866	-0.014840	1.909641
76.218564	1098.837288	4.976870	-0.014907	1.915690
76.494947	1106.950512	4.981875	-0.014964	1.921707
76.692690	1115.072812	4.986880	-0.015006	1.927703
77.059087	1123.202219	4.991885	-0.015080	1.933704
77.393965	1131.309563	4.996890	-0.015148	1.939667
77.669418	1139.424708	5.001894	-0.015204	1.945611
78.189128	1147.555815	5.006899	-0.015306	1.951574
78.261891	1155.710181	5.011904	-0.015325	1.957488
78.686380	1163.786193	5.016909	-0.015409	1.963365
79.447225	1171.823903	5.021914	-0.015556	1.969234
79.653042	1179.978487	5.026918	-0.015600	1.975109
79.851611	1188.093309	5.031923	-0.015642	1.980937
80.212539	1196.183283	5.036928	-0.015715	1.986748
80.582051	1204.324554	5.041933	-0.015789	1.992578
80.936218	1212.420436	5.046938	-0.015860	1.998359
81.257428	1220.508932	5.051942	-0.015925	2.004113
81.543797	1228.632330	5.056947	-0.015984	2.009872
82.080972	1236.717286	5.061952	-0.016089	2.015614
82.440510	1244.820787	5.066957	-0.016162	2.021333
82.594836	1252.952568	5.071962	-0.016196	2.027035
82.913784	1261.092330	5.076966	-0.016260	2.032744
83.257176	1269.186682	5.081971	-0.016330	2.038407
83.641484	1277.236059	5.086976	-0.016406	2.044028
84.221442	1285.305882	5.091981	-0.016520	2.049667
84.551681	1293.419365	5.096986	-0.016586	2.055295
85.030714	1301.493590	5.101990	-0.016681	2.060896
85.292016	1309.611743	5.106995	-0.016735	2.066489
85.484338	1317.733619	5.112000	-0.016776	2.072063
85.718304	1325.856800	5.117005	-0.016825	2.077628
86.186095	1333.911171	5.122010	-0.016917	2.083153
86.354211	1342.025114	5.127014	-0.016954	2.088675
86.712318	1350.146495	5.132019	-0.017026	2.094206
87.006378	1358.226205	5.137024	-0.017086	2.099688
87.425828	1366.308192	5.142029	-0.017169	2.105169
87.516649	1374.466082	5.147034	-0.017192	2.110654
87.900918	1382.579107	5.152038	-0.017268	2.116124
88.660975	1390.576176	5.157043	-0.017415	2.121539
88.844173	1398.655279	5.162048	-0.017455	2.126939
88.985345	1406.791219	5.167053	-0.017486	2.132358
89.231013	1414.885108	5.172058	-0.017537	2.137747
89.453760	1422.959645	5.177062	-0.017584	2.143106
89.873222	1431.042050	5.182067	-0.017667	2.148476
90.024309	1439.152263	5.187072	-0.017701	2.153825
90.377188	1447.223463	5.192077	-0.017772	2.159155
90.366801	1455.318700	5.197082	-0.017775	2.164453
90.735486	1463.395110	5.202086	-0.017849	2.169761
91.161779	1471.486752	5.207091	-0.017934	2.175071
91.244363	1479.572995	5.212096	-0.017955	2.180333
91.691080	1487.628649	5.217101	-0.018043	2.185596
91.999857	1495.738344	5.222106	-0.018106	2.190868
92.388524	1503.818481	5.227110	-0.018183	2.196116
92.531133	1511.914387	5.232115	-0.018215	2.201339
92.892453	1519.957895	5.237120	-0.018288	2.206536
93.510486	1528.023279	5.242125	-0.018408	2.211758
93.356761	1536.165624	5.247130	-0.018385	2.216947
93.541697	1544.232803	5.252134	-0.018425	2.222107
93.871672	1552.307626	5.257139	-0.018491	2.227272
94.125820	1560.403938	5.262144	-0.018544	2.232432
94.535424	1568.460159	5.267149	-0.018626	2.237568
95.345943	1576.463612	5.272154	-0.018782	2.242695
95.620213	1584.540678	5.277158	-0.018838	2.247809
95.780300	1592.665674	5.282163	-0.018873	2.252931
96.204371	1600.724242	5.287168	-0.018957	2.258023
96.489550	1608.809619	5.292173	-0.019016	2.263109
96.674692	1616.899993	5.297178	-0.019056	2.268177
96.941215	1625.040476	5.302182	-0.019111	2.273272
97.216918	1633.115955	5.307187	-0.019167	2.278316
97.512827	1641.136960	5.312192	-0.019227	2.283317
97.615262	1649.230981	5.317197	-0.019252	2.288335
98.017116	1657.287955	5.322202	-0.019332	2.293346
98.282052	1665.346420	5.327206	-0.019387	2.298334
98.537551	1673.417784	5.332211	-0.019439	2.303318
98.848670	1681.462773	5.337216	-0.019503	2.308281
99.195176	1689.554402	5.342221	-0.019572	2.313264
99.428473	1697.627540	5.347226	-0.019621	2.318215
99.766473	1705.666387	5.352230	-0.019689	2.323144
99.988736	1713.751688	5.357235	-0.019736	2.328081
100.183941	1721.841524	5.362240	-0.019778	2.333008
100.509321	1729.910011	5.367245	-0.019844	2.337922
100.912075	1737.954957	5.372250	-0.019924	2.342818
101.143099	1746.029674	5.377254	-0.019972	2.347707
101.308574	1754.153631	5.382259	-0.020008	2.352611
101.731778	1762.175537	5.387264	-0.020092	2.357464
102.114378	1770.220531	5.392269	-0.020169	2.362317
102.278697	1778.296607	5.397274	-0.020205	2.367162
102.705516	1786.343027	5.402278	-0.020289	2.372000
103.180652	1794.411481	5.407283	-0.020383	2.376844
103.380087	1802.471696	5.412288	-0.020426	2.381652
103.540870	1810.560632	5.417293	-0.020461	2.386465
103.689045	1818.645798	5.422298	-0.020494	2.391264
104.181758	1826.688592	5.427302	-0.020591	2.396056
104.537877	1834.745380	5.432307	-0.020662	2.400835
104.694703	1842.799091	5.437312	-0.020697	2.405588
105.228988	1850.858267	5.442317	-0.020802	2.410364
105.406040	1858.979106	5.447322	-0.020840	2.415139
105.531732	1867.032154	5.452326	-0.020869	2.419860
105.785723	1875.094468	5.457331	-0.020921	2.424588
106.123922	1883.147618	5.462336	-0.020989	2.429307
106.585694	1891.288184	5.467341	-0.021081	2.434078
106.727500	1899.332992	5.472346	-0.021112	2.438759
107.027725	1907.344728	5.477350	-0.021173	2.443424
107.429090	1915.385972	5.482355	-0.021253	2.448105
107.543023	1923.471398	5.487360	-0.021280	2.452780
107.998496	1931.493671	5.492365	-0.021370	2.457436
108.104543	1939.579089	5.497370	-0.021395	2.462094
108.279955	1947.624004	5.502374	-0.021433	2.466724
108.729680	1955.680824	5.507379	-0.021522	2.471373
108.918906	1963.746058	5.512384	-0.021563	2.475998
108.961162	1971.836587	5.517389	-0.021576	2.480618
109.144962	1979.889290	5.522394	-0.021615	2.485219
109.588642	1987.906848	5.527398	-0.021703	2.489810
109.995259	1995.982289	5.532403	-0.021784	2.494423
110.125675	2004.028943	5.537408	-0.021814	2.498990
110.622551	2012.053876	5.542413	-0.021911	2.503564
110.852455	2020.145663	5.547418	-0.021959	2.508148
111.067954	2028.236232	5.552422	-0.022005	2.512721
111.298292	2036.297546	5.557427	-0.022053	2.517271
111.523121	2044.318077	5.562432	-0.022100	2.521789
111.592555	2052.412929	5.567437	-0.022118	2.526330
111.755586	2060.454830	5.572442	-0.022154	2.530839
112.081376	2068.505226	5.577446	-0.022220	2.535357
112.361884	2076.557185	5.582451	-0.022277	2.539864
112.682681	2084.571034	5.587456	-0.022342	2.544345
113.135727	2092.642611	5.592461	-0.022432	2.548859
113.468270	2100.719282	5.597466	-0.022499	2.553359
113.632848	2108.758863	5.602470	-0.022535	2.557820
113.946189	2116.807053	5.607475	-0.022599	2.562287
114.194573	2124.836048	5.612480	-0.022650	2.566732
114.555535	2132.904937	5.617485	-0.022723	2.571199
114.676598	2140.993004	5.622490	-0.022751	2.575651
114.928586	2149.032541	5.627494	-0.022803	2.580079
115.132907	2157.090896	5.632499	-0.022846	2.584506
115.165595	2165.169861	5.637504	-0.022858	2.588924
115.476791	2173.374369	5.642509	-0.022921	2.593423
116.009270	2181.373230	5.647514	-0.023025	2.597817
116.186099	2189.359394	5.652518	-0.023063	2.602172
116.562171	2197.389186	5.657523	-0.023139	2.606557
116.855281	2205.412791	5.662528	-0.023198	2.610926
117.100985	2213.485069	5.667533	-0.023250	2.615311
117.455443	2221.496250	5.672538	-0.023321	2.619662
117.652404	2229.534970	5.677542	-0.023363	2.624011
118.003826	2237.601425	5.682547	-0.023433	2.628377
118.032474	2245.674559	5.687552	-0.023444	2.632718
118.359518	2253.718738	5.692557	-0.023510	2.637057
118.691599	2261.753292	5.697562	-0.023577	2.641383
118.562108	2269.816746	5.702566	-0.023558	2.645687
118.920103	2277.869162	5.707571	-0.023630	2.650011
119.138397	2285.913375	5.712576	-0.023676	2.654314
119.338759	2293.964752	5.717581	-0.023719	2.658612
119.581325	2302.001789	5.722586	-0.023769	2.662898
119.588177	2310.067111	5.727590	-0.023776	2.667178
120.111806	2318.098443	5.732595	-0.023879	2.671465
120.308992	2326.159018	5.737600	-0.023921	2.675741
120.811601	2334.151771	5.742605	-0.024019	2.679993
121.267292	2342.162017	5.747610	-0.024110	2.684244
121.548989	2350.212802	5.752614	-0.024167	2.688499
121.876764	2358.287602	5.757619	-0.024234	2.692763
122.092685	2366.343616	5.762624	-0.024279	2.697003
122.374067	2374.375933	5.767629	-0.024337	2.701228
122.553324	2382.447006	5.772634	-0.024375	2.705460
122.704359	2390.482154	5.777638	-0.024409	2.709665
122.957956	2398.578730	5.782643	-0.024461	2.713902
123.071616	2406.611202	5.787648	-0.024488	2.718090
123.354866	2414.644915	5.792653	-0.024546	2.722283
123.693542	2422.685184	5.797658	-0.024614	2.726476
123.965950	2430.710337	5.802662	-0.024670	2.730651
124.363903	2438.787383	5.807667	-0.024749	2.734854
124.551301	2446.826441	5.812672	-0.024790	2.739018
124.730177	2454.875222	5.817677	-0.024828	2.743180
124.842971	2462.941718	5.822682	-0.024854	2.747340
125.006179	2470.998160	5.827686	-0.024890	2.751493
125.416575	2479.079145	5.832691	-0.024972	2.755666
125.530944	2487.088576	5.837696	-0.024998	2.759779
125.624105	2495.128388	5.842701	-0.025021	2.763900
125.854951	2503.160455	5.847706	-0.025069	2.768018
126.339976	2511.169376	5.852710	-0.025165	2.772134
126.782577	2519.203409	5.857715	-0.025252	2.776255
126.883683	2527.248312	5.862720	-0.025276	2.780354
127.362703	2535.243940	5.867725	-0.025371	2.784444
127.401345	2543.339734	5.872730	-0.025383	2.788553
127.554108	2551.408970	5.877734	-0.025417	2.792650
128.016702	2559.441909	5.882739	-0.025509	2.796740
128.172682	2567.475313	5.887744	-0.025543	2.800806
128.335258	2575.499283	5.892749	-0.025578	2.804862
128.748584	2583.536469	5.897754	-0.025661	2.808934
128.908459	2591.609742	5.902758	-0.025696	2.813003
129.035225	2599.681182	5.907763	-0.025725	2.817063
129.149620	2607.717162	5.912768	-0.025751	2.821099
129.368173	2615.750926	5.917773	-0.025797	2.825134
129.817677	2623.788662	5.922778	-0.025886	2.829178
129.854373	2631.860213	5.927782	-0.025898	2.833210
130.244778	2639.904265	5.932787	-0.025976	2.837242
130.508350	2647.916665	5.937792	-0.026030	2.841246
130.546364	2655.956060	5.942797	-0.026043	2.845244
131.262635	2663.951983	5.947802	-0.026181	2.849254
131.541452	2671.998330	5.952806	-0.026239	2.853258
131.975398	2680.049988	5.957811	-0.026325	2.857268
132.174829	2688.072006	5.962816	-0.026367	2.861245
132.596238	2696.082859	5.967821	-0.026451	2.865222
133.133032	2704.125081	5.972826	-0.026556	2.869216
133.405586	2712.205898	5.977830	-0.026612	2.873209
133.901474	2720.232440	5.982835	-0.026710	2.877182
134.352881	2728.239046	5.987840	-0.026799	2.881137
134.563373	2736.281863	5.992845	-0.026843	2.885091
134.763674	2744.377178	5.997850	-0.026886	2.889064
135.001077	2752.418279	6.002854	-0.026935	2.893008
135.383618	2760.474866	6.007859	-0.027012	2.896962
135.605034	2768.506687	6.012864	-0.027058	2.900889
135.760293	2776.521539	6.017869	-0.027093	2.904800
135.880223	2784.600017	6.022874	-0.027120	2.908734
136.155365	2792.697502	6.027878	-0.027177	2.912680
136.581431	2800.743782	6.032883	-0.027261	2.916604
136.452613	2808.764618	6.037888	-0.027243	2.920481
136.658318	2816.752935	6.042893	-0.027286	2.924355
137.044356	2824.783343	6.047898	-0.027363	2.928253
137.341839	2832.807777	6.052902	-0.027424	2.932139
137.558479	2840.882968	6.057907	-0.027469	2.936039
137.436441	2848.909090	6.062912	-0.027452	2.939893
137.678819	2856.928875	6.067917	-0.027502	2.943758
138.001074	2864.978680	6.072922	-0.027568	2.947637
138.206025	2872.999141	6.077926	-0.027611	2.951490
138.404507	2881.086398	6.082931	-0.027653	2.955370
138.525857	2889.073721	6.087936	-0.027681	2.959193
138.805648	2897.100217	6.092941	-0.027739	2.963037
139.110760	2905.152927	6.097946	-0.027801	2.966891
139.420206	2913.157396	6.102950	-0.027863	2.970717
139.918255	2921.213944	6.107955	-0.027961	2.974572
140.040531	2929.254900	6.112960	-0.027989	2.978395
140.032783	2937.303654	6.117965	-0.027993	2.982211
140.232342	2945.363743	6.122970	-0.028036	2.986038
140.430973	2953.382195	6.127974	-0.028078	2.989840
140.827533	2961.452810	6.132979	-0.028157	2.993671
141.235490	2969.455948	6.137984	-0.028238	2.997467
141.481687	2977.484555	6.142989	-0.028289	3.001261
141.374120	2985.526911	6.147994	-0.028275	3.005040
141.544735	2993.540745	6.152998	-0.028312	3.008814
141.847657	3001.605416	6.158003	-0.028373	3.012614
142.085149	3009.647309	6.163008	-0.028423	3.016395
142.288447	3017.672307	6.168013	-0.028466	3.020161
142.532443	3025.708529	6.173018	-0.028517	3.023931
142.482868	3033.742718	6.178022	-0.028513	3.027680
142.852373	3041.796131	6.183027	-0.028587	3.031454
143.080667	3049.838908	6.188032	-0.028635	3.035211
143.399209	3057.830711	6.193037	-0.028699	3.038944
143.774868	3065.866267	6.198042	-0.028774	3.042696
143.859044	3073.901673	6.203046	-0.028795	3.046429
144.129406	3081.942611	6.208051	-0.028851	3.050169
144.112474	3090.021790	6.213056	-0.028853	3.053908
144.357105	3098.026564	6.218061	-0.028904	3.057621
144.514970	3106.075128	6.223066	-0.028938	3.061345
144.611173	3114.080291	6.228070	-0.028962	3.065042
144.742635	3122.149890	6.233075	-0.028991	3.068765
145.101031	3130.210979	6.238080	-0.029063	3.072491
145.287812	3138.280476	6.243085	-0.029103	3.076208
145.504927	3146.264875	6.248090	-0.029149	3.079883
145.786058	3154.245623	6.253094	-0.029207	3.083555
146.003446	3162.297745	6.258099	-0.029252	3.087252
145.924769	3170.368364	6.263104	-0.029243	3.090939
146.198859	3178.391829	6.268109	-0.029299	3.094617
146.698029	3186.379061	6.273114	-0.029397	3.098284
146.753700	3194.399986	6.278118	-0.029413	3.101942
146.761522	3202.483936	6.283123	-0.029420	3.105622
147.157770	3210.478855	6.288128	-0.029499	3.109275
147.358679	3218.512514	6.293133	-0.029542	3.112932
147.667958	3226.591080	6.298138	-0.029604	3.116610
147.764421	3234.600528	6.303142	-0.029628	3.120242
148.128798	3242.603133	6.308147	-0.029701	3.123880
148.265116	3250.633007	6.313152	-0.029731	3.127515
148.429652	3258.699265	6.318157	-0.029767	3.131164
148.596738	3266.733204	6.323162	-0.029804	3.134794
148.772586	3274.752795	6.328166	-0.029842	3.138413
149.155973	3282.769677	6.333171	-0.029918	3.142037
149.463678	3290.807608	6.338176	-0.029981	3.145662
149.540613	3298.838584	6.343181	-0.030000	3.149270
149.798994	3306.945406	6.348186	-0.030054	3.152915
149.809377	3314.986165	6.353190	-0.030061	3.156516
150.427527	3322.935779	6.358195	-0.030181	3.160099
150.455061	3330.971656	6.363200	-0.030192	3.163690
150.499780	3339.011519	6.368205	-0.030205	3.167280
150.804662	3347.062704	6.373210	-0.030267	3.170882
150.971316	3355.062875	6.378214	-0.030304	3.174451
151.231921	3363.125605	6.383219	-0.030357	3.178048
151.559963	3371.139086	6.388224	-0.030424	3.181621
151.861061	3379.133357	6.393229	-0.030485	3.185181
151.904237	3387.221328	6.398234	-0.030498	3.188768
152.052855	3395.243445	6.403238	-0.030531	3.192326
152.207397	3403.317117	6.408243	-0.030565	3.195903
152.135305	3411.313993	6.413248	-0.030557	3.199432
152.508021	3419.299379	6.418253	-0.030632	3.202971
152.871548	3427.354193	6.423258	-0.030705	3.206537
153.190322	3435.362082	6.428262	-0.030769	3.210075
153.242095	3443.452470	6.433267	-0.030784	3.213635
153.241893	3451.493470	6.438272	-0.030789	3.217168
153.731255	3459.487337	6.443277	-0.030886	3.220695
153.917875	3467.512908	6.448282	-0.030926	3.224221
154.255301	3475.524687	6.453286	-0.030994	3.227742
154.793822	3483.575176	6.458291	-0.031099	3.231285
154.903306	3491.666895	6.463296	-0.031125	3.234825
154.968808	3499.670698	6.468301	-0.031143	3.238320
155.059414	3507.688023	6.473306	-0.031165	3.241819
155.297014	3515.673186	6.478310	-0.031214	3.245305
155.494528	3523.703799	6.483315	-0.031256	3.248806
155.727821	3531.729094	6.488320	-0.031305	3.252303
155.970395	3539.797558	6.493325	-0.031355	3.255814
156.186846	3547.795843	6.498330	-0.031401	3.259291
156.600725	3555.779639	6.503334	-0.031483	3.262765
156.829980	3563.851130	6.508339	-0.031531	3.266266
156.846990	3571.911015	6.513344	-0.031540	3.269750
157.128062	3579.934482	6.518349	-0.031597	3.273224
157.621928	3587.981330	6.523354	-0.031694	3.276714
157.745008	3595.975629	6.528358	-0.031723	3.280162
157.748754	3604.011707	6.533363	-0.031729	3.283621
158.058390	3612.033009	6.538368	-0.031791	3.287081
158.465979	3620.047551	6.543373	-0.031873	3.290538
158.697671	3628.114937	6.548378	-0.031921	3.294008
158.663988	3636.144769	6.553382	-0.031920	3.297447
159.298681	3644.154536	6.558387	-0.032043	3.300900
159.501188	3652.158273	6.563392	-0.032086	3.304330
159.660073	3660.192600	6.568397	-0.032121	3.307768
159.761110	3668.291022	6.573402	-0.032145	3.311228
159.951728	3676.323339	6.578406	-0.032186	3.314659
160.165546	3684.325345	6.583411	-0.032231	3.318074
160.417663	3692.350681	6.588416	-0.032283	3.321497
160.753258	3700.320466	6.593421	-0.032351	3.324897
160.970581	3708.376672	6.598426	-0.032397	3.328325
161.245247	3716.392805	6.603430	-0.032453	3.331734
161.611088	3724.463871	6.608435	-0.032527	3.335167
161.698489	3732.472539	6.613440	-0.032548	3.338559
161.736659	3740.512165	6.618445	-0.032560	3.341959
161.992507	3748.534417	6.623450	-0.032613	3.345357
162.328086	3756.538785	6.628454	-0.032681	3.348746
162.266236	3764.618446	6.633459	-0.032675	3.352149
162.463365	3772.665378	6.638464	-0.032717	3.355544
162.856073	3780.639095	6.643469	-0.032795	3.358912
162.947284	3788.696742	6.648474	-0.032817	3.362301
162.975974	3796.712866	6.653478	-0.032828	3.365667
163.094590	3804.747959	6.658483	-0.032855	3.369041
163.551121	3812.769021	6.663488	-0.032946	3.372417
163.525490	3820.848388	6.668493	-0.032946	3.375797
163.586261	3828.853040	6.673498	-0.032963	3.379146
163.775569	3836.836817	6.678502	-0.033003	3.382487
164.094433	3844.901466	6.683507	-0.033068	3.385863
164.491477	3852.882293	6.688512	-0.033147	3.389204
164.614210	3860.998564	6.693517	-0.033175	3.392588
164.912790	3869.075937	6.698522	-0.033236	3.395958
164.744401	3877.021752	6.703526	-0.033210	3.399254
165.002174	3885.017801	6.708531	-0.033263	3.402583
165.291576	3893.045526	6.713536	-0.033322	3.405923
165.451109	3901.033289	6.718541	-0.033357	3.409238
165.669831	3909.108504	6.723546	-0.033403	3.412588
165.676016	3917.158773	6.728550	-0.033410	3.415917
166.184434	3925.119432	6.733555	-0.033509	3.419224
166.076666	3933.166870	6.738560	-0.033495	3.422541
166.257555	3941.179381	6.743565	-0.033534	3.425851
166.645229	3949.229010	6.748570	-0.033611	3.429180
166.592183	3957.281760	6.753574	-0.033606	3.432492
166.888001	3965.317565	6.758579	-0.033667	3.435806
167.258851	3973.293558	6.763584	-0.033741	3.439095
167.378102	3981.322945	6.768589	-0.033769	3.442393
167.599902	3989.327395	6.773594	-0.033815	3.445682
167.645069	3997.359236	6.778598	-0.033829	3.448973
168.082417	4005.393070	6.783603	-0.033915	3.452274
168.204572	4013.472418	6.788608	-0.033943	3.455581
168.392212	4021.464817	6.793613	-0.033984	3.458851
168.529146	4029.535545	6.798618	-0.034014	3.462148
168.430658	4037.532470	6.803622	-0.034001	3.465404
168.415185	4045.587786	6.808627	-0.034004	3.468684
168.841091	4053.604859	6.813632	-0.034088	3.471959
169.141029	4061.638936	6.818637	-0.034149	3.475234
169.138157	4069.653175	6.823642	-0.034154	3.478488
169.204759	4077.660967	6.828646	-0.034172	3.481739
169.472416	4085.651192	6.833651	-0.034227	3.484986
169.615567	4093.697354	6.838656	-0.034259	3.488248
169.760504	4101.749439	6.843661	-0.034291	3.491510
170.317150	4109.737515	6.848666	-0.034400	3.494756
170.416180	4117.758149	6.853670	-0.034424	3.497998
170.645643	4125.800130	6.858675	-0.034472	3.501249
170.766861	4133.810050	6.863680	-0.034499	3.504481
170.882796	4141.832490	6.868685	-0.034526	3.507715
171.068868	4149.891141	6.873690	-0.034566	3.510962
171.282252	4157.908612	6.878694	-0.034611	3.514191
171.615740	4165.926667	6.883699	-0.034678	3.517421
171.797061	4173.946784	6.888704	-0.034717	3.520643
171.895591	4181.926896	6.893709	-0.034741	3.523845
172.187217	4190.004119	6.898714	-0.034801	3.527088
172.113084	4198.011333	6.903718	-0.034792	3.530289
172.416740	4206.086997	6.908723	-0.034854	3.533526
172.658875	4214.116202	6.913728	-0.034904	3.536739
172.825878	4222.117788	6.918733	-0.034941	3.539936
172.911163	4230.150865	6.923738	-0.034962	3.543141
173.011073	4238.193301	6.928742	-0.034986	3.546347
173.480008	4246.195803	6.933747	-0.035078	3.549544
173.559572	4254.310262	6.938752	-0.035098	3.552772
173.582070	4262.355387	6.943757	-0.035108	3.555968
173.908437	4270.300959	6.948762	-0.035174	3.559130
174.135340	4278.306821	6.953766	-0.035221	3.562311
174.265668	4286.300274	6.958771	-0.035251	3.565480
174.435598	4294.326402	6.963776	-0.035288	3.568661
174.727023	4302.363482	6.968781	-0.035347	3.571847
174.939262	4310.404988	6.973786	-0.035392	3.575030
174.902418	4318.402334	6.978790	-0.035390	3.578185
175.384121	4326.428314	6.983795	-0.035485	3.581364
175.659771	4334.391806	6.988800	-0.035542	3.584509
175.500414	4342.459057	6.993805	-0.035517	3.587679
175.765492	4350.493930	6.998810	-0.035572	3.590847
176.098710	4358.525543	7.003814	-0.035639	3.594012
176.174114	4366.571014	7.008819	-0.035659	3.597172
176.432209	4374.565096	7.013824	-0.035712	3.600315
176.524220	4382.566219	7.018829	-0.035734	3.603453
176.788475	4390.626688	7.023834	-0.035789	3.606616
176.654763	4398.627675	7.028838	-0.035769	3.609742
176.886942	4406.645529	7.033843	-0.035818	3.612882
177.256550	4414.695933	7.038848	-0.035892	3.616036
177.384143	4422.692173	7.043853	-0.035921	3.619159
177.628378	4430.720023	7.048858	-0.035971	3.622295
177.814930	4438.738950	7.053862	-0.036011	3.625423
177.890517	4446.791927	7.058867	-0.036031	3.628559
178.096061	4454.852476	7.063872	-0.036074	3.631699
178.352275	4462.897275	7.068877	-0.036127	3.634831
178.533597	4470.883519	7.073882	-0.036166	3.637935
178.617557	4478.894691	7.078886	-0.036187	3.641044
178.702966	4486.881216	7.083891	-0.036208	3.644141
178.846003	4494.933542	7.088896	-0.036240	3.647262
179.043467	4502.944687	7.093901	-0.036282	3.650366
179.160632	4511.031283	7.098906	-0.036309	3.653494
179.291848	4519.025226	7.103910	-0.036339	3.656584
179.490411	4527.018174	7.108915	-0.036381	3.659673
179.761500	4535.060853	7.113920	-0.036437	3.662780
179.993912	4543.068505	7.118925	-0.036485	3.665871
180.177174	4551.117996	7.123930	-0.036525	3.668973
180.326466	4559.138496	7.128934	-0.036558	3.672061
180.384969	4567.184921	7.133939	-0.036574	3.675153
180.655189	4575.191443	7.138944	-0.036630	3.678233
180.876935	4583.166504	7.143949	-0.036676	3.681298
181.160104	4591.178461	7.148954	-0.036734	3.684375
181.142998	4599.240008	7.153958	-0.036736	3.687461
181.322881	4607.247927	7.158963	-0.036775	3.690529
181.428204	4615.308369	7.163968	-0.036800	3.693613
181.788722	4623.309755	7.168973	-0.036872	3.696678
181.967468	4631.328226	7.173978	-0.036911	3.699742
182.243155	4639.311052	7.178982	-0.036967	3.702792
182.348155	4647.362544	7.183987	-0.036992	3.705862
182.322872	4655.439896	7.188992	-0.036993	3.708936
182.458286	4663.465905	7.193997	-0.037023	3.711992
182.757107	4671.579276	7.199002	-0.037084	3.715082
182.921332	4679.502560	7.204006	-0.037120	3.718095
182.926860	4687.534740	7.209011	-0.037126	3.721142
183.321584	4695.463743	7.214016	-0.037205	3.724157
183.515289	4703.497111	7.219021	-0.037246	3.727205
183.632546	4711.538708	7.224026	-0.037273	3.730251
183.839423	4719.558954	7.229030	-0.037317	3.733289
183.955657	4727.649425	7.234035	-0.037344	3.736348
184.263961	4735.609557	7.239040	-0.037407	3.739361
184.301385	4743.637979	7.244045	-0.037419	3.742390
184.275271	4751.671937	7.249050	-0.037419	3.745417
184.571027	4759.650828	7.254054	-0.037479	3.748429
184.750727	4767.752228	7.259059	-0.037518	3.751482
184.927882	4775.757466	7.264064	-0.037556	3.754496
185.019054	4783.755418	7.269069	-0.037579	3.757503
185.423062	4791.786297	7.274074	-0.037659	3.760527
185.250913	4799.773468	7.279078	-0.037632	3.763518
185.740466	4807.779721	7.284083	-0.037729	3.766530
186.108145	4815.830907	7.289088	-0.037802	3.769554
186.174335	4823.877863	7.294093	-0.037820	3.772566
186.509594	4831.899088	7.299098	-0.037888	3.775572
186.764735	4839.925019	7.304102	-0.037940	3.778576
187.227927	4847.929014	7.309107	-0.038032	3.781574
187.465161	4855.977434	7.314112	-0.038081	3.784582
187.507437	4863.966942	7.319117	-0.038095	3.787560
187.878602	4872.043776	7.324122	-0.038169	3.790576
187.982826	4880.077624	7.329126	-0.038194	3.793567
188.150459	4888.112426	7.334131	-0.038230	3.796558
188.469721	4896.078260	7.339136	-0.038295	3.799524
188.474329	4904.077420	7.344141	-0.038301	3.802494
188.734142	4912.100694	7.349146	-0.038354	3.805475
188.989270	4920.100316	7.354150	-0.038407	3.808446
189.047547	4928.151522	7.359155	-0.038423	3.811428
189.023200	4936.186018	7.364160	-0.038424	3.814401
189.384078	4944.189248	7.369165	-0.038496	3.817368
189.494112	4952.213356	7.374170	-0.038522	3.820334
189.506640	4960.202838	7.379174	-0.038530	3.823284
189.724374	4968.245998	7.384179	-0.038576	3.826256
190.047532	4976.277622	7.389184	-0.038641	3.829223
190.146381	4984.301267	7.394189	-0.038665	3.832180
190.248477	4992.366620	7.399194	-0.038689	3.835150
190.274308	5000.357660	7.404198	-0.038699	3.838089
190.327874	5008.336280	7.409203	-0.038714	3.841022
190.438277	5016.363768	7.414208	-0.038740	3.843972
190.758506	5024.371252	7.419213	-0.038805	3.846916
191.036181	5032.422322	7.424218	-0.038862	3.849873
191.028294	5040.462341	7.429222	-0.038866	3.852818
191.107480	5048.501129	7.434227	-0.038886	3.855762
191.454505	5056.487761	7.439232	-0.038955	3.858690
191.564978	5064.476542	7.444237	-0.038981	3.861612
191.547109	5072.531491	7.449242	-0.038983	3.864554
191.861864	5080.546156	7.454246	-0.039047	3.867484
192.109325	5088.595547	7.459251	-0.039098	3.870424
192.173925	5096.838533	7.464256	-0.039116	3.873429
192.119168	5104.852492	7.469261	-0.039111	3.876346
192.521329	5112.711357	7.474266	-0.039191	3.879213
192.518896	5120.742264	7.479270	-0.039196	3.882132
192.670980	5128.709915	7.484275	-0.039229	3.885029
193.043632	5136.717435	7.489280	-0.039304	3.887943
193.053939	5144.709034	7.494285	-0.039311	3.890842
193.383412	5152.788821	7.499290	-0.039378	3.893776
193.192142	5160.838479	7.504294	-0.039347	3.896688
193.622649	5168.787217	7.509299	-0.039433	3.899573
193.764281	5176.833145	7.514304	-0.039464	3.902485
193.728144	5184.819221	7.519309	-0.039463	3.905370
194.147737	5192.847213	7.524314	-0.039546	3.908277
194.065168	5200.899554	7.529318	-0.039536	3.911180
194.129743	5208.925146	7.534323	-0.039553	3.914075
194.340742	5216.969137	7.539328	-0.039598	3.916977
194.599787	5224.893541	7.544333	-0.039651	3.919835
194.745563	5232.938139	7.549338	-0.039684	3.922731
194.823916	5240.960897	7.554342	-0.039704	3.925617
195.201747	5248.963153	7.559347	-0.039779	3.928498
195.454013	5257.002139	7.564352	-0.039831	3.931388
195.564569	5265.030756	7.569357	-0.039857	3.934269
195.741041	5273.066375	7.574362	-0.039895	3.937153
195.767486	5281.046545	7.579366	-0.039906	3.940011
195.745849	5289.089018	7.584371	-0.039907	3.942889
196.141133	5297.112406	7.589376	-0.039986	3.945765
196.264636	5305.109750	7.594381	-0.040014	3.948625
196.349167	5313.182205	7.599386	-0.040035	3.951509
196.455113	5321.225421	7.604390	-0.040060	3.954381
196.519727	5329.209980	7.609395	-0.040077	3.957230
196.902982	5337.193662	7.614400	-0.040154	3.960081
197.035834	5345.180432	7.619405	-0.040184	3.962927
197.240568	5353.202909	7.624410	-0.040227	3.965785
197.329780	5361.206928	7.629414	-0.040249	3.968632
197.683155	5369.269205	7.634419	-0.040320	3.971502
198.074054	5377.333053	7.639424	-0.040398	3.974372
198.242088	5385.324518	7.644429	-0.040435	3.977210
198.137733	5393.313444	7.649434	-0.040420	3.980040
198.296839	5401.385596	7.654438	-0.040455	3.982902
198.413570	5409.394146	7.659443	-0.040482	3.985739
198.479090	5417.430262	7.664448	-0.040500	3.988583
198.726774	5425.431028	7.669453	-0.040551	3.991416
199.196527	5433.458300	7.674458	-0.040644	3.994259
199.312462	5441.506849	7.679462	-0.040671	3.997102
199.337180	5449.486551	7.684467	-0.040681	3.999917
199.556040	5457.522423	7.689472	-0.040727	4.002753
199.880712	5465.525607	7.694477	-0.040792	4.005577
200.094619	5473.573297	7.699482	-0.040837	4.008413
200.130234	5481.617033	7.704486	-0.040849	4.011243
200.229186	5489.611215	7.709491	-0.040873	4.014054
200.473824	5497.696149	7.714496	-0.040924	4.016898
200.559964	5505.653358	7.719501	-0.040945	4.019692
200.776949	5513.701197	7.724506	-0.040991	4.022518
200.983635	5521.697326	7.729510	-0.041034	4.025324
201.107264	5529.707221	7.734515	-0.041063	4.028131
201.251495	5537.747743	7.739520	-0.041095	4.030947
201.327482	5545.851384	7.744525	-0.041114	4.033783
201.543388	5553.893072	7.749530	-0.041160	4.036597
201.430868	5561.774845	7.754534	-0.041144	4.039348
201.843077	5569.839050	7.759539	-0.041226	4.042168
202.205346	5577.774192	7.764544	-0.041299	4.044941
202.077854	5585.783187	7.769549	-0.041280	4.047731
202.225500	5593.862271	7.774554	-0.041313	4.050547
202.591876	5601.896584	7.779558	-0.041386	4.053349
202.666416	5609.912001	7.784563	-0.041405	4.056137
202.583292	5617.901793	7.789568	-0.041395	4.058913
202.848375	5625.897892	7.794573	-0.041450	4.061694
202.924848	5633.933458	7.799578	-0.041469	4.064484
203.054689	5641.968794	7.804582	-0.041499	4.067273
203.662793	5649.921702	7.809587	-0.041617	4.070038
203.566574	5658.015293	7.814592	-0.041605	4.072840
203.534881	5666.011662	7.819597	-0.041604	4.075608
203.795785	5674.015229	7.824602	-0.041658	4.078380
204.046172	5682.029295	7.829606	-0.041710	4.081153
204.043887	5690.021925	7.834611	-0.041714	4.083914
204.470453	5698.059961	7.839616	-0.041799	4.086695
204.489780	5706.015611	7.844621	-0.041808	4.089439
204.635579	5714.132013	7.849626	-0.041840	4.092239
204.738669	5722.190435	7.854630	-0.041865	4.095016
205.213642	5730.170969	7.859635	-0.041959	4.097770
205.608193	5738.209212	7.864640	-0.042037	4.100540
205.655540	5746.171945	7.869645	-0.042051	4.103278
205.742019	5754.219433	7.874650	-0.042073	4.106044
206.117401	5762.214079	7.879654	-0.042148	4.108794
206.019501	5770.294084	7.884659	-0.042135	4.111565
206.169358	5778.340103	7.889664	-0.042168	4.114325
206.488682	5786.333280	7.894669	-0.042233	4.117068
206.723437	5794.307718	7.899674	-0.042282	4.119801
206.742143	5802.369511	7.904678	-0.042290	4.122560
206.842113	5810.346034	7.909683	-0.042314	4.125288
207.085980	5818.378353	7.914688	-0.042365	4.128036
207.056489	5826.407830	7.919693	-0.042365	4.130777
207.284820	5834.469873	7.924698	-0.042412	4.133531
207.478045	5842.453492	7.929702	-0.042454	4.136256
207.480553	5850.453903	7.934707	-0.042459	4.138983
207.711156	5858.536725	7.939712	-0.042508	4.141738
207.873118	5866.436602	7.944717	-0.042543	4.144429
208.075605	5874.528494	7.949722	-0.042586	4.147183
208.098454	5882.574289	7.954726	-0.042595	4.149918
208.325594	5890.606308	7.959731	-0.042643	4.152649
208.704187	5898.608083	7.964736	-0.042719	4.155369
208.741497	5906.590245	7.969741	-0.042731	4.158077
208.621484	5914.614370	7.974746	-0.042714	4.160796
208.929073	5922.610634	7.979750	-0.042776	4.163508
209.251582	5930.636648	7.984755	-0.042842	4.166229
209.295688	5938.713465	7.989760	-0.042855	4.168962
209.400705	5946.703959	7.994765	-0.042880	4.171665
209.541675	5954.699407	7.999770	-0.042911	4.174368
209.628396	5962.771276	8.004774	-0.042933	4.177094
209.881230	5970.715250	8.009779	-0.042985	4.179778
210.063313	5978.790865	8.014784	-0.043024	4.182503
209.997238	5986.793746	8.019789	-0.043017	4.185199
210.129816	5994.791610	8.024794	-0.043047	4.187894
210.313269	6002.812533	8.029798	-0.043087	4.190596
210.455653	6010.935672	8.034803	-0.043118	4.193329
210.634926	6018.953362	8.039808	-0.043157	4.196026
210.854855	6026.867152	8.044813	-0.043203	4.198687
210.942571	6034.920469	8.049818	-0.043225	4.201391
210.952538	6042.881839	8.054822	-0.043232	4.204062
211.088290	6050.923554	8.059827	-0.043262	4.206759
211.287397	6058.903285	8.064832	-0.043305	4.209435
211.331222	6066.974099	8.069837	-0.043318	4.212137
211.388201	6074.976919	8.074842	-0.043334	4.214816
211.502297	6083.023289	8.079846	-0.043360	4.217508
211.852302	6090.974293	8.084851	-0.043431	4.220168
211.931956	6099.010561	8.089856	-0.043451	4.222853
212.112292	6107.008753	8.094861	-0.043490	4.225524
212.306655	6115.019163	8.099866	-0.043531	4.228198
212.394580	6123.072520	8.104870	-0.043553	4.230883
212.536917	6131.096637	8.109875	-0.043585	4.233557
212.898155	6139.184286	8.114880	-0.043657	4.236253
213.091568	6147.121547	8.119885	-0.043698	4.238895
213.140143	6155.190095	8.124890	-0.043713	4.241578
213.048917	6163.118300	8.129894	-0.043701	4.244212
213.151899	6171.158786	8.134899	-0.043725	4.246883
213.512870	6179.202810	8.139904	-0.043798	4.249556
213.631184	6187.219245	8.144909	-0.043825	4.252215
213.785136	6195.248252	8.149914	-0.043859	4.254878
213.877164	6203.274625	8.154918	-0.043881	4.257537
213.828795	6211.256105	8.159923	-0.043878	4.260178
214.133607	6219.312286	8.164928	-0.043940	4.262846
214.408862	6227.279973	8.169933	-0.043996	4.265483
214.559153	6235.307078	8.174938	-0.044029	4.268136
214.355065	6243.399688	8.179942	-0.043997	4.270806
214.470619	6251.418866	8.184947	-0.044023	4.273454
214.864621	6259.464232	8.189952	-0.044102	4.276110
214.784270	6267.406681	8.194957	-0.044092	4.278727
215.219867	6275.431759	8.199962	-0.044179	4.281374
215.383225	6283.415785	8.204966	-0.044214	4.284003
215.308178	6291.422204	8.209971	-0.044206	4.286636
215.561421	6299.466142	8.214976	-0.044258	4.289283
215.651306	6307.513519	8.219981	-0.044280	4.291927
215.903140	6315.556200	8.224986	-0.044332	4.294570
215.808077	6323.592451	8.229990	-0.044320	4.297206
216.054253	6331.522468	8.234995	-0.044371	4.299809
216.340384	6339.608897	8.240000	-0.044429	4.302461
216.212235	6347.554922	8.245005	-0.044411	4.305063
216.759545	6355.624222	8.250010	-0.044518	4.307708
216.871518	6363.625889	8.255014	-0.044544	4.310327
216.933786	6371.651783	8.260019	-0.044561	4.312951
217.035579	6379.702714	8.265024	-0.044585	4.315582
217.252750	6387.648842	8.270029	-0.044631	4.318179
217.188490	6395.694288	8.275034	-0.044624	4.320804
217.431611	6403.688845	8.280038	-0.044674	4.323413
217.750517	6411.670354	8.285043	-0.044739	4.326016
217.838567	6419.770259	8.290048	-0.044761	4.328656
217.941347	6427.741479	8.295053	-0.044785	4.331251
217.979489	6435.796689	8.300058	-0.044797	4.333872
218.391295	6443.852584	8.305062	-0.044879	4.336494
218.568289	6451.787838	8.310067	-0.044918	4.339074
218.895625	6459.808373	8.315072	-0.044984	4.341681
218.916027	6467.812402	8.320077	-0.044993	4.344279
219.145165	6475.849635	8.325082	-0.045041	4.346887
219.064461	6483.877944	8.330086	-0.045031	4.349489
219.014062	6491.930660	8.335091	-0.045027	4.352097
219.272379	6500.036940	8.340096	-0.045080	4.354724
219.372799	6508.016263	8.345101	-0.045104	4.357306
219.601805	6515.934081	8.350106	-0.045152	4.359868
219.660109	6523.962432	8.355110	-0.045168	4.362463
219.726387	6531.913255	8.360115	-0.045186	4.365032
220.142754	6539.968482	8.365120	-0.045268	4.367634
220.141420	6547.977589	8.370125	-0.045273	4.370218
220.333519	6556.020732	8.375130	-0.045315	4.372813
220.337309	6564.040264	8.380134	-0.045320	4.375397
220.575682	6572.021427	8.385139	-0.045370	4.377968
220.885926	6580.074968	8.390144	-0.045433	4.380562
220.700413	6588.070519	8.395149	-0.045404	4.383133
220.916242	6596.070328	8.400154	-0.045449	4.385705
221.396833	6604.114965	8.405158	-0.045544	4.388293
221.402252	6612.132975	8.410163	-0.045550	4.390867
221.613047	6620.194000	8.415168	-0.045595	4.393455
221.887631	6628.196456	8.420173	-0.045651	4.396023
222.072400	6636.185739	8.425178	-0.045691	4.398584
222.217837	6644.244763	8.430182	-0.045723	4.401167
222.431315	6652.167963	8.435187	-0.045768	4.403704
222.677407	6660.241708	8.440192	-0.045819	4.406288
222.808056	6668.251838	8.445197	-0.045849	4.408850
223.088496	6676.287757	8.450202	-0.045906	4.411420
223.304313	6684.328519	8.455206	-0.045952	4.413989
223.310865	6692.322517	8.460211	-0.045958	4.416541
223.375671	6700.364309	8.465216	-0.045975	4.419106
223.485511	6708.354294	8.470221	-0.046001	4.421654
223.764888	6716.312100	8.475226	-0.046058	4.424191
223.860111	6724.391067	8.480230	-0.046081	4.426764
224.314524	6732.399885	8.485235	-0.046171	4.429315
224.612773	6740.497243	8.490240	-0.046232	4.431892
224.523732	6748.504719	8.495245	-0.046221	4.434437
224.730930	6756.515579	8.500250	-0.046265	4.436983
225.068245	6764.454590	8.505254	-0.046333	4.439505
225.000578	6772.508069	8.510259	-0.046325	4.442061
225.039381	6780.479076	8.515264	-0.046338	4.444589
225.226299	6788.558111	8.520269	-0.046378	4.447151
225.413272	6796.516689	8.525274	-0.046418	4.449672
225.463846	6804.612796	8.530278	-0.046433	4.452236
225.398222	6812.568995	8.535283	-0.046426	4.454753
225.794195	6820.650346	8.540288	-0.046505	4.457310
225.819637	6828.583927	8.545293	-0.046514	4.459818
225.990199	6836.605268	8.550298	-0.046552	4.462352
226.267890	6844.618106	8.555302	-0.046608	4.464883
226.370392	6852.623790	8.560307	-0.046633	4.467410
226.403412	6860.705161	8.565312	-0.046644	4.469958
226.539794	6868.716678	8.570317	-0.046675	4.472483
226.993390	6876.719365	8.575322	-0.046765	4.475006
226.692087	6884.772643	8.580327	-0.046714	4.477540
227.075251	6892.696027	8.585331	-0.046790	4.480034
227.400216	6900.772572	8.590336	-0.046856	4.482575
227.110659	6908.711089	8.595341	-0.046807	4.485068
227.267836	6916.776683	8.600346	-0.046842	4.487602
227.304105	6924.813282	8.605351	-0.046854	4.490125
227.672598	6932.826319	8.610355	-0.046928	4.492640
228.018576	6940.850190	8.615360	-0.046997	4.495157
228.130463	6948.839024	8.620365	-0.047024	4.497661
228.260885	6956.839172	8.625370	-0.047053	4.500167
228.258954	6964.898890	8.630375	-0.047058	4.502690
228.297216	6972.874944	8.635379	-0.047070	4.505185
228.510647	6980.968808	8.640384	-0.047115	4.507717
228.837118	6988.929466	8.645389	-0.047181	4.510205
228.967934	6996.989235	8.650394	-0.047211	4.512723
228.980119	7005.020491	8.655399	-0.047218	4.515230
228.882775	7013.020034	8.660403	-0.047206	4.517725
229.117238	7020.980401	8.665408	-0.047254	4.520208
229.085148	7028.989293	8.670413	-0.047254	4.522704
229.579944	7036.964741	8.675418	-0.047351	4.525189
229.633514	7045.043155	8.680423	-0.047366	4.527703
229.460037	7052.998137	8.685427	-0.047339	4.530178
229.797556	7061.095660	8.690432	-0.047407	4.532697
229.917378	7069.107770	8.695437	-0.047435	4.535187
230.034851	7077.065032	8.700442	-0.047462	4.537658
230.266227	7085.084351	8.705447	-0.047510	4.540148
230.307930	7093.095179	8.710451	-0.047523	4.542634
230.483989	7101.095565	8.715456	-0.047561	4.545115
230.744448	7109.151335	8.720461	-0.047615	4.547612
230.779498	7117.169464	8.725466	-0.047627	4.550095
230.799456	7125.210228	8.730471	-0.047636	4.552584
230.970086	7133.212290	8.735475	-0.047673	4.555060
231.305409	7141.256395	8.740480	-0.047741	4.557548
231.514829	7149.223745	8.745485	-0.047785	4.560011
231.521285	7157.244881	8.750490	-0.047791	4.562489
231.703529	7165.222133	8.755495	-0.047830	4.564951
231.906139	7173.271504	8.760499	-0.047873	4.567435
232.194424	7181.303766	8.765504	-0.047932	4.569913
232.191417	7189.379004	8.770509	-0.047937	4.572402
232.453337	7197.354379	8.775514	-0.047991	4.574859
232.445230	7205.412068	8.780519	-0.047995	4.577339
232.433921	7213.359462	8.785523	-0.047998	4.579785
232.602461	7221.434506	8.790528	-0.048035	4.582268
232.860206	7229.367482	8.795533	-0.048088	4.584707
233.005394	7237.422965	8.800538	-0.048120	4.587182
233.240628	7245.455212	8.805543	-0.048169	4.589648
233.477035	7253.526478	8.810547	-0.048219	4.592125
233.566149	7261.509798	8.815552	-0.048240	4.594574
233.484458	7269.550651	8.820557	-0.048230	4.597039
233.608023	7277.503790	8.825562	-0.048259	4.599475
233.813432	7285.524340	8.830567	-0.048302	4.601931
233.959654	7293.501360	8.835571	-0.048335	4.604373
234.261689	7301.594865	8.840576	-0.048396	4.606848
234.518877	7309.567233	8.845581	-0.048449	4.609286
234.534865	7317.619640	8.850586	-0.048457	4.611746
234.666117	7325.667142	8.855591	-0.048487	4.614204
234.826856	7333.598267	8.860595	-0.048522	4.616625
235.077558	7341.612468	8.865600	-0.048574	4.619070
235.123377	7349.652439	8.870605	-0.048588	4.621521
235.515273	7357.633389	8.875610	-0.048666	4.623953
235.650164	7365.718968	8.880615	-0.048697	4.626416
235.666511	7373.699028	8.885619	-0.048705	4.628845
235.770620	7381.754222	8.890624	-0.048730	4.631296
236.106836	7389.745253	8.895629	-0.048797	4.633725
236.206772	7397.757706	8.900634	-0.048821	4.636161
236.495365	7405.747000	8.905639	-0.048880	4.638587
236.618400	7413.784497	8.910643	-0.048908	4.641028
236.595662	7421.755979	8.915648	-0.048909	4.643446
236.737832	7429.775256	8.920653	-0.048941	4.645878
236.621324	7437.778558	8.925658	-0.048925	4.648305
237.048978	7445.887494	8.930663	-0.049010	4.650761
236.987577	7453.872591	8.935667	-0.049003	4.653179
237.171282	7461.903874	8.940672	-0.049043	4.655609
237.408532	7469.876638	8.945677	-0.049092	4.658021
237.742424	7477.925247	8.950682	-0.049160	4.660454
237.666064	7485.924990	8.955687	-0.049151	4.662871
237.790570	7493.886225	8.960691	-0.049179	4.665275
238.089299	7501.936141	8.965696	-0.049240	4.667705
238.147589	7509.938615	8.970701	-0.049256	4.670119
238.283361	7518.034674	8.975706	-0.049287	4.672560
238.509228	7526.115767	8.980711	-0.049334	4.674996
238.611480	7534.042980	8.985715	-0.049358	4.677383
238.705199	7542.005364	8.990720	-0.049381	4.679780
238.962852	7550.024633	8.995725	-0.049434	4.682193
239.128793	7557.966653	9.000730	-0.049470	4.684581
239.343897	7566.106305	9.005735	-0.049516	4.687028
239.334041	7574.020307	9.010739	-0.049519	4.689405
239.825385	7582.121288	9.015744	-0.049616	4.691837
239.686322	7590.161323	9.020749	-0.049595	4.694250
239.591422	7598.166176	9.025754	-0.049583	4.696652
239.868584	7606.113002	9.030759	-0.049639	4.699034
239.968102	7614.087766	9.035763	-0.049663	4.701424
240.076185	7622.160530	9.040768	-0.049689	4.703841
240.336953	7630.165583	9.045773	-0.049742	4.706237
240.459365	7638.193623	9.050778	-0.049770	4.708639
240.653136	7646.260823	9.055783	-0.049812	4.711051
240.703111	7654.228725	9.060787	-0.049826	4.713432
241.215261	7662.298473	9.065792	-0.049927	4.715842
241.155762	7670.241303	9.070797	-0.049921	4.718214
241.098664	7678.246733	9.075802	-0.049916	4.720603
241.533685	7686.264631	9.080807	-0.050002	4.722994
241.479629	7694.306550	9.085811	-0.049997	4.725391
241.698264	7702.350803	9.090816	-0.050043	4.727788
241.663735	7710.360204	9.095821	-0.050042	4.730173
242.011126	7718.399260	9.100826	-0.050112	4.732565
242.014854	7726.414039	9.105831	-0.050118	4.734950
241.901066	7734.388665	9.110835	-0.050102	4.737322
242.252459	7742.422322	9.115840	-0.050173	4.739708
242.243339	7750.410253	9.120845	-0.050176	4.742081
242.440775	7758.410641	9.125850	-0.050218	4.744456
242.628468	7766.500250	9.130855	-0.050258	4.746857
242.959973	7774.445033	9.135859	-0.050325	4.749212
243.123657	7782.507921	9.140864	-0.050361	4.751602
243.441103	7790.561901	9.145869	-0.050425	4.753988
243.950777	7798.590605	9.150874	-0.050526	4.756364
243.918215	7806.502284	9.155879	-0.050525	4.758706
243.884630	7814.541331	9.160883	-0.050524	4.761084
244.119813	7822.543248	9.165888	-0.050573	4.763450
244.154515	7830.585902	9.170893	-0.050584	4.765827
244.157831	7838.590981	9.175898	-0.050590	4.768192
244.373146	7846.640768	9.180903	-0.050636	4.770568
244.621683	7854.622072	9.185907	-0.050687	4.772923
244.883416	7862.673226	9.190912	-0.050741	4.775297
244.914391	7870.628030	9.195917	-0.050752	4.777642
244.876328	7878.644128	9.200922	-0.050750	4.780004
244.989997	7886.692735	9.205927	-0.050777	4.782375
244.989830	7894.630332	9.210931	-0.050782	4.784711
245.450480	7902.690702	9.215936	-0.050873	4.787081
245.466227	7910.729880	9.220941	-0.050881	4.789446
245.434856	7918.742628	9.225946	-0.050881	4.791801
245.702149	7926.814649	9.230951	-0.050936	4.794172
245.486842	7934.759290	9.235955	-0.050901	4.796506
245.730060	7942.763472	9.240960	-0.050951	4.798854
245.686999	7950.830171	9.245965	-0.050949	4.801221
246.007368	7958.790300	9.250970	-0.051013	4.803554
246.424451	7966.835830	9.255975	-0.051096	4.805910
246.406923	7974.853101	9.260979	-0.051098	4.808259
246.420807	7982.885457	9.265984	-0.051106	4.810610
246.612512	7990.270515	9.270989	-0.051147	4.812771
246.710637	7994.795763	9.275994	-0.051168	4.814094

246.834128	7997.395784	9.280999	-0.051193	4.814854
247.061335	7998.649529	9.286003	-0.051236	4.815220
246.783386	7999.116894	9.291008	-0.051184	4.815358
246.806783	8000.074928	9.296013	-0.051189	4.815638
247.080369	8000.001434	9.301018	-0.051240	4.815615
247.097832	8000.019870	9.306023	-0.051244	4.815620
247.129011	8000.049205	9.311027	-0.051249	4.815629
247.268178	8000.071752	9.316032	-0.051275	4.815635
247.391869	8000.039598	9.321037	-0.051298	4.815625
247.430020	8000.008189	9.326042	-0.051306	4.815615
247.411740	8000.029248	9.331047	-0.051302	4.815621
247.522206	8000.055600	9.336051	-0.051323	4.815629
247.356628	8000.064658	9.341056	-0.051292	4.815632
247.166103	8000.097866	9.346061	-0.051257	4.815643
247.425165	7999.997445	9.351066	-0.051305	4.815612
247.524898	8000.058855	9.356071	-0.051323	4.815630
247.351696	8000.000526	9.361075	-0.051291	4.815613
247.463266	8000.025829	9.366080	-0.051312	4.815620
247.318624	8000.093948	9.371085	-0.051285	4.815641
247.427761	8000.088249	9.376090	-0.051305	4.815639
247.518590	8000.066237	9.381095	-0.051322	4.815632
247.608469	8000.023925	9.386099	-0.051339	4.815619
247.541058	8000.032441	9.391104	-0.051327	4.815622
247.511846	8000.055457	9.396109	-0.051321	4.815629
247.827358	8000.009336	9.401114	-0.051380	4.815614
247.928745	8000.084654	9.406119	-0.051399	4.815635
247.774896	8000.043721	9.411123	-0.051370	4.815624
247.834873	8000.071389	9.416128	-0.051381	4.815632
248.002134	8000.083717	9.421133	-0.051413	4.815635
247.756352	8000.006058	9.426138	-0.051367	4.815613
247.854562	8000.038617	9.431143	-0.051385	4.815622
247.935327	7999.987615	9.436147	-0.051400	4.815607
247.879994	8000.056117	9.441152	-0.051390	4.815627
247.738547	8000.101867	9.446157	-0.051364	4.815641
247.710514	8000.087534	9.451162	-0.051358	4.815637
247.822279	8000.117111	9.456167	-0.051379	4.815645
247.810207	8000.100902	9.461171	-0.051377	4.815641
247.998900	8000.052721	9.466176	-0.051412	4.815626
247.932050	8000.043096	9.471181	-0.051400	4.815623
248.005346	8000.000514	9.476186	-0.051413	4.815610
247.920212	8000.057855	9.481191	-0.051398	4.815627
248.128018	8000.087925	9.486195	-0.051436	4.815635
248.223705	8000.107632	9.491200	-0.051454	4.815641
248.177386	8000.130371	9.496205	-0.051446	4.815647
248.171306	8000.071551	9.501210	-0.051444	4.815630
248.350187	8000.117167	9.506215	-0.051478	4.815643
248.089900	8000.074504	9.511219	-0.051429	4.815631
248.124907	8000.072939	9.516224	-0.051436	4.815631
248.445262	8000.072808	9.521229	-0.051496	4.815629
248.231156	8000.024489	9.526234	-0.051456	4.815616
248.263979	8000.055987	9.531239	-0.051462	4.815625
248.167560	8000.021324	9.536243	-0.051444	4.815616
248.217429	8000.047761	9.541248	-0.051453	4.815623
248.181088	8000.079203	9.546253	-0.051446	4.815632
248.371439	8000.058809	9.551258	-0.051482	4.815626
248.549486	8000.088396	9.556263	-0.051515	4.815633
248.373395	8000.069521	9.561267	-0.051482	4.815629
248.467035	8000.060368	9.566272	-0.051500	4.815626
248.416738	8000.067027	9.571277	-0.051490	4.815628
248.496771	8000.038434	9.576282	-0.051505	4.815619
248.459221	8000.093346	9.581287	-0.051498	4.815635
248.413841	8000.020008	9.586291	-0.051490	4.815614
248.437543	8000.015057	9.591296	-0.051494	4.815612
248.137950	8000.034748	9.596301	-0.051439	4.815620
248.356500	8000.011609	9.601306	-0.051479	4.815612
248.468501	8000.115929	9.606311	-0.051500	4.815642
248.243463	8000.032198	9.611315	-0.051458	4.815618
248.122828	8000.082557	9.616320	-0.051436	4.815634
248.210189	8000.101061	9.621325	-0.051452	4.815639
248.187211	8000.041967	9.626330	-0.051448	4.815621
248.194690	8000.091204	9.631335	-0.051449	4.815636
248.175474	8000.057796	9.636339	-0.051446	4.815626
248.356888	8000.075693	9.641344	-0.051480	4.815631
248.295230	8000.102453	9.646349	-0.051468	4.815639
248.347168	8000.084081	9.651354	-0.051478	4.815633
248.550850	8000.102340	9.656359	-0.051516	4.815637
248.243154	8000.064245	9.661363	-0.051459	4.815628
248.434927	8000.011843	9.666368	-0.051494	4.815611
248.459059	8000.063486	9.671373	-0.051499	4.815626
248.550768	8000.052166	9.676378	-0.051516	4.815623
248.712580	8000.109249	9.681383	-0.051546	4.815639
248.630117	8000.024631	9.686387	-0.051531	4.815614
248.527965	8000.048598	9.691392	-0.051512	4.815622
248.612635	8000.064924	9.696397	-0.051528	4.815626
248.457375	8000.022899	9.701402	-0.051499	4.815615
248.566980	8000.122909	9.706407	-0.051519	4.815643
248.492743	8000.105690	9.711411	-0.051505	4.815639
248.729163	8000.066826	9.716416	-0.051549	4.815626
248.813156	8000.134390	9.721421	-0.051565	4.815646
248.710304	8000.051576	9.726426	-0.051546	4.815622
248.579639	8000.078283	9.731431	-0.051522	4.815630
248.416374	8000.092715	9.736435	-0.051491	4.815635
248.668157	8000.058371	9.741440	-0.051538	4.815624
248.946054	8000.070363	9.746445	-0.051590	4.815626
248.591163	8000.035771	9.751450	-0.051524	4.815618
248.822475	8000.026719	9.756455	-0.051567	4.815614
248.703965	8000.031201	9.761459	-0.051545	4.815616
248.802290	7999.993296	9.766464	-0.051563	4.815604
248.676330	8000.083074	9.771469	-0.051540	4.815631
248.719245	8000.060284	9.776474	-0.051548	4.815624
248.913350	8000.112554	9.781479	-0.051584	4.815639
248.858581	8000.072161	9.786483	-0.051574	4.815627
248.843834	8000.124241	9.791488	-0.051571	4.815642
248.686961	8000.078986	9.796493	-0.051542	4.815630
248.619022	8000.028770	9.801498	-0.051529	4.815616
248.898570	8000.055736	9.806503	-0.051581	4.815622
248.827809	8000.003339	9.811507	-0.051568	4.815607
248.834671	8000.071785	9.816512	-0.051569	4.815627
248.932922	8000.107551	9.821517	-0.051588	4.815637
249.117977	8000.095612	9.826522	-0.051622	4.815633
249.254385	8000.067936	9.831527	-0.051648	4.815624
248.909838	8000.079422	9.836531	-0.051584	4.815629
248.824161	8000.052407	9.841536	-0.051568	4.815621
249.122345	8000.039103	9.846541	-0.051623	4.815616
249.025965	8000.068503	9.851546	-0.051605	4.815625
248.964591	8000.111283	9.856551	-0.051594	4.815638
248.819117	8000.065145	9.861555	-0.051567	4.815625
248.725678	8000.040140	9.866560	-0.051549	4.815618
248.994731	8000.011415	9.871565	-0.051600	4.815609
249.033508	7999.973610	9.876570	-0.051607	4.815597
249.125744	8000.028496	9.881575	-0.051624	4.815613
249.066178	8000.056358	9.886579	-0.051613	4.815621
248.977997	8000.078417	9.891584	-0.051597	4.815628
249.050500	8000.172488	9.896589	-0.051610	4.815656
248.995787	8000.048815	9.901594	-0.051600	4.815620
249.105018	8000.098639	9.906599	-0.051620	4.815634
248.974251	8000.027115	9.911603	-0.051596	4.815613
248.895445	8000.020498	9.916608	-0.051581	4.815612
248.969632	8000.075091	9.921613	-0.051595	4.815627
248.944649	8000.109921	9.926618	-0.051591	4.815638
249.081611	8000.118555	9.931623	-0.051616	4.815640
248.831680	8000.111292	9.936627	-0.051570	4.815639
249.015605	8000.040612	9.941632	-0.051604	4.815617
249.117845	8000.066833	9.946637	-0.051623	4.815624
248.956717	8000.069555	9.951642	-0.051593	4.815626
249.215203	8000.103654	9.956647	-0.051641	4.815635
249.346296	8000.037453	9.961651	-0.051665	4.815615
249.178551	8000.029390	9.966656	-0.051634	4.815613
249.369157	8000.093350	9.971661	-0.051670	4.815631
249.260164	8000.028586	9.976666	-0.051649	4.815612
249.127808	8000.074483	9.981671	-0.051625	4.815626
249.141484	8000.089656	9.986675	-0.051627	4.815631
249.101599	8000.063385	9.991680	-0.051620	4.815623
249.176198	8000.135068	9.996685	-0.051634	4.815644
249.088952	8000.017272	10.001690	-0.051618	4.815610
249.051525	8000.044426	10.006695	-0.051611	4.815618
249.250517	8000.025240	10.011699	-0.051648	4.815611
249.219494	8000.004452	10.016704	-0.051642	4.815606
249.125015	8000.052033	10.021709	-0.051625	4.815620
249.262006	7999.992335	10.026714	-0.051650	4.815602
249.387285	8000.068045	10.031719	-0.051673	4.815623
249.387132	8000.014659	10.036723	-0.051673	4.815608
249.274278	8000.095040	10.041728	-0.051652	4.815632
249.448200	8000.150188	10.046733	-0.051685	4.815647
249.228278	8000.019557	10.051738	-0.051644	4.815610
249.252115	8000.080806	10.056743	-0.051648	4.815628
249.267146	8000.053292	10.061747	-0.051651	4.815620
249.441382	8000.078548	10.066752	-0.051684	4.815626
249.336828	8000.100340	10.071757	-0.051664	4.815633
249.320928	8000.025344	10.076762	-0.051661	4.815611
249.384442	8000.090441	10.081767	-0.051673	4.815630
248.961113	7999.990673	10.086771	-0.051594	4.815603
249.000888	8000.041504	10.091776	-0.051602	4.815617
249.439713	8000.056112	10.096781	-0.051683	4.815620
249.231805	8000.026042	10.101786	-0.051645	4.815612
249.339023	8000.134558	10.106791	-0.051665	4.815643
249.255658	8000.038179	10.111795	-0.051649	4.815615
249.377710	7999.995321	10.116800	-0.051672	4.815602
249.210444	8000.067344	10.121805	-0.051641	4.815624
249.092937	8000.002442	10.126810	-0.051619	4.815606
249.343385	8000.080186	10.131815	-0.051666	4.815627
249.098958	8000.079418	10.136819	-0.051620	4.815628
249.024223	8000.024821	10.141824	-0.051606	4.815612
249.335795	8000.064053	10.146829	-0.051664	4.815622
249.239986	8000.034738	10.151834	-0.051647	4.815614
249.068107	8000.092806	10.156839	-0.051615	4.815632
249.137574	8000.051229	10.161843	-0.051628	4.815620
249.397646	8000.028765	10.166848	-0.051676	4.815612
249.348570	8000.053594	10.171853	-0.051667	4.815619
249.384045	8000.023209	10.176858	-0.051673	4.815610
249.594564	8000.056529	10.181863	-0.051713	4.815619
249.191070	8000.038228	10.186867	-0.051638	4.815616
249.169175	8000.051755	10.191872	-0.051634	4.815620
249.290411	8000.084691	10.196877	-0.051656	4.815629
249.458521	8000.056462	10.201882	-0.051688	4.815620
249.420380	8000.055844	10.206887	-0.051680	4.815620
249.497340	8000.059232	10.211891	-0.051695	4.815620
249.507853	8000.012426	10.216896	-0.051697	4.815606
249.310387	8000.082891	10.221901	-0.051660	4.815628
249.102366	8000.002637	10.226906	-0.051621	4.815606
249.513213	8000.061634	10.231911	-0.051698	4.815621
249.426604	8000.136036	10.236915	-0.051682	4.815643
249.416339	8000.060064	10.241920	-0.051680	4.815621
249.470721	8000.069491	10.246925	-0.051690	4.815623
249.347167	8000.025845	10.251930	-0.051667	4.815611
249.278772	8000.105881	10.256935	-0.051654	4.815635
249.313087	8000.032769	10.261939	-0.051661	4.815613
249.425959	8000.022861	10.266944	-0.051682	4.815610
249.621397	8000.098644	10.271949	-0.051718	4.815631
249.619055	8000.004649	10.276954	-0.051718	4.815604
249.706894	8000.013553	10.281959	-0.051734	4.815606
249.471393	8000.044962	10.286963	-0.051690	4.815616
249.288844	8000.045200	10.291968	-0.051656	4.815617
249.509988	8000.081896	10.296973	-0.051698	4.815627
249.379446	8000.021052	10.301978	-0.051673	4.815610
249.350739	8000.079311	10.306983	-0.051668	4.815627
249.305169	8000.030526	10.311987	-0.051659	4.815613
249.428292	8000.093389	10.316992	-0.051682	4.815631
249.383328	8000.133233	10.321997	-0.051674	4.815642
249.252266	8000.063839	10.327002	-0.051650	4.815623
249.396987	8000.093954	10.332007	-0.051677	4.815631
249.319370	8000.054257	10.337011	-0.051662	4.815620
249.234819	8000.034734	10.342016	-0.051647	4.815614
249.329840	8000.065108	10.347021	-0.051664	4.815623
249.543966	8000.010934	10.352026	-0.051704	4.815606
249.499898	8000.094570	10.357031	-0.051696	4.815631
249.511972	8000.080888	10.362035	-0.051698	4.815626
249.449152	7999.990181	10.367040	-0.051687	4.815600
249.453342	8000.066059	10.372045	-0.051687	4.815622
249.333893	8000.032088	10.377050	-0.051665	4.815613
249.452708	8000.045766	10.382055	-0.051687	4.815616
249.372868	8000.012439	10.387059	-0.051672	4.815607
249.354509	8000.003601	10.392064	-0.051669	4.815605
249.359241	8000.059201	10.397069	-0.051670	4.815621
249.487240	8000.053810	10.402074	-0.051694	4.815619
249.507439	8000.039192	10.407079	-0.051698	4.815614
249.362515	8000.008011	10.412083	-0.051671	4.815606
249.723640	8000.096097	10.417088	-0.051738	4.815630
249.651773	8000.098134	10.422093	-0.051725	4.815631
249.564007	8000.046526	10.427098	-0.051708	4.815616
249.705216	8000.046688	10.432103	-0.051735	4.815616
249.534118	8000.053519	10.437107	-0.051703	4.815618
249.400661	8000.002237	10.442112	-0.051678	4.815604
249.609437	8000.047273	10.447117	-0.051717	4.815616
249.568260	8000.008168	10.452122	-0.051709	4.815605
249.647915	8000.072460	10.457127	-0.051724	4.815623
249.416983	7999.996104	10.462131	-0.051681	4.815602
249.417291	8000.005721	10.467136	-0.051681	4.815605
249.387286	8000.060756	10.472141	-0.051676	4.815621
249.306410	8000.046631	10.477146	-0.051661	4.815617
249.288003	8000.066621	10.482151	-0.051657	4.815623
249.482721	8000.026012	10.487155	-0.051693	4.815611
249.579463	8000.051076	10.492160	-0.051711	4.815617
249.617847	8000.080530	10.497165	-0.051719	4.815626
249.528270	8000.037435	10.502170	-0.051702	4.815614
249.687031	8000.067779	10.507175	-0.051732	4.815622
249.644799	8000.038266	10.512179	-0.051724	4.815613
249.604300	8000.007714	10.517184	-0.051716	4.815605
249.629177	8000.041219	10.522189	-0.051721	4.815614
249.668234	7999.983132	10.527194	-0.051728	4.815597
249.614981	8000.055941	10.532199	-0.051718	4.815619
249.770124	8000.064871	10.537203	-0.051747	4.815621
249.606593	8000.050470	10.542208	-0.051717	4.815617
249.481123	8000.149866	10.547213	-0.051693	4.815647
249.482318	8000.108246	10.552218	-0.051694	4.815635
249.591062	8000.042750	10.557223	-0.051714	4.815615
249.661896	8000.082341	10.562227	-0.051727	4.815626
249.806122	8000.074011	10.567232	-0.051754	4.815623
249.850070	8000.055508	10.572237	-0.051762	4.815617
249.530488	7999.985185	10.577242	-0.051703	4.815598
249.652297	7999.989302	10.582247	-0.051725	4.815599
249.654574	8000.095046	10.587251	-0.051726	4.815630
249.654957	8000.038465	10.592256	-0.051726	4.815613
249.628069	8000.101025	10.597261	-0.051721	4.815632
249.686863	8000.002685	10.602266	-0.051732	4.815603
249.675338	8000.084714	10.607271	-0.051730	4.815627
249.719560	8000.107858	10.612275	-0.051738	4.815633
249.659974	8000.073792	10.617280	-0.051727	4.815624
249.615321	8000.122183	10.622285	-0.051719	4.815638
249.421121	8000.015460	10.627290	-0.051683	4.815608
249.555430	8000.018713	10.632295	-0.051708	4.815608
249.657647	8000.073762	10.637299	-0.051727	4.815624
249.682607	8000.046409	10.642304	-0.051731	4.815616
249.483205	8000.093353	10.647309	-0.051694	4.815630
249.472552	8000.068624	10.652314	-0.051692	4.815623
249.541611	8000.053733	10.657319	-0.051705	4.815618
249.495981	8000.029504	10.662323	-0.051697	4.815611
249.460261	8000.010774	10.667328	-0.051690	4.815606
249.563830	8000.106419	10.672333	-0.051709	4.815634
249.479043	8000.049522	10.677338	-0.051694	4.815617
249.594550	8000.042859	10.682343	-0.051715	4.815615
249.783554	8000.018173	10.687347	-0.051750	4.815607
249.695451	8000.010337	10.692352	-0.051734	4.815605
249.741697	8000.061273	10.697357	-0.051743	4.815620
249.620620	8000.013396	10.702362	-0.051720	4.815606
249.680474	8000.016506	10.707367	-0.051731	4.815607
249.477510	8000.070866	10.712371	-0.051694	4.815624
249.494292	8000.029500	10.717376	-0.051697	4.815611
249.563547	8000.123519	10.722381	-0.051710	4.815639
249.520772	8000.099336	10.727386	-0.051702	4.815632
249.810563	8000.081627	10.732391	-0.051756	4.815625
249.808614	8000.099749	10.737395	-0.051755	4.815631
249.717970	8000.039552	10.742400	-0.051738	4.815613
249.776447	8000.076808	10.747405	-0.051749	4.815624
249.577397	8000.075709	10.752410	-0.051712	4.815625
249.731031	8000.081412	10.757415	-0.051741	4.815626
249.776903	8000.089634	10.762419	-0.051750	4.815628
249.795448	8000.068583	10.767424	-0.051753	4.815621
249.890271	8000.110700	10.772429	-0.051771	4.815633
249.736803	8000.080447	10.777434	-0.051742	4.815625
249.740917	8000.073042	10.782439	-0.051743	4.815623
249.788623	8000.066345	10.787443	-0.051752	4.815621
249.763703	8000.068078	10.792448	-0.051747	4.815621
249.687344	8000.073245	10.797453	-0.051733	4.815623
249.606873	8000.048449	10.802458	-0.051718	4.815616
249.786221	8000.042825	10.807463	-0.051751	4.815614
249.815133	8000.098818	10.812467	-0.051757	4.815630
249.644652	8000.004225	10.817472	-0.051725	4.815603
249.861915	8000.056874	10.822477	-0.051766	4.815618
249.721183	8000.048182	10.827482	-0.051739	4.815616
249.634480	8000.104432	10.832487	-0.051723	4.815633
249.741986	8000.063473	10.837491	-0.051743	4.815620
249.907218	8000.019181	10.842496	-0.051774	4.815606
249.933266	8000.039893	10.847501	-0.051779	4.815612
249.621443	8000.035894	10.852506	-0.051721	4.815613
249.786993	8000.020436	10.857511	-0.051752	4.815607
249.785010	8000.010797	10.862515	-0.051751	4.815605
249.758800	8000.037066	10.867520	-0.051747	4.815612
249.639602	8000.051146	10.872525	-0.051724	4.815617
249.624427	8000.008193	10.877530	-0.051722	4.815605
249.759152	8000.049890	10.882535	-0.051747	4.815616
249.520002	8000.038531	10.887539	-0.051702	4.815614
249.578935	8000.042694	10.892544	-0.051713	4.815615
249.626760	8000.054151	10.897549	-0.051722	4.815618
249.512569	8000.037349	10.902554	-0.051701	4.815614
249.731786	8000.093233	10.907559	-0.051742	4.815629
249.701062	8000.069245	10.912563	-0.051736	4.815622
249.524541	8000.023669	10.917568	-0.051703	4.815610
249.722928	8000.117653	10.922573	-0.051740	4.815636
249.903429	8000.067203	10.927578	-0.051774	4.815621
249.850422	8000.091969	10.932583	-0.051764	4.815628
249.756441	8000.087240	10.937587	-0.051747	4.815627
249.700485	8000.078858	10.942592	-0.051736	4.815625
249.750174	8000.074329	10.947597	-0.051745	4.815623
249.718002	8000.074876	10.952602	-0.051739	4.815624
249.748366	8000.090320	10.957607	-0.051745	4.815628
249.740122	8000.117949	10.962611	-0.051744	4.815636
249.642215	8000.074718	10.967616	-0.051725	4.815624
249.703367	8000.088527	10.972621	-0.051737	4.815628
249.642688	8000.052308	10.977626	-0.051726	4.815617
249.850831	8000.075981	10.982631	-0.051764	4.815623
249.914704	8000.120798	10.987635	-0.051776	4.815636
249.760634	8000.068112	10.992640	-0.051748	4.815621
249.834417	8000.125903	10.997645	-0.051761	4.815638
249.763769	8000.078845	11.002650	-0.051748	4.815625
249.958457	8000.069199	11.007655	-0.051784	4.815621
249.959496	8000.124740	11.012659	-0.051785	4.815637
249.900228	8000.119508	11.017664	-0.051774	4.815636
249.726541	8000.132702	11.022669	-0.051741	4.815641
249.709731	8000.085451	11.027674	-0.051738	4.815627
249.936196	8000.061374	11.032679	-0.051780	4.815619
249.729272	8000.079366	11.037683	-0.051742	4.815625
249.937759	8000.087029	11.042688	-0.051781	4.815626
250.021759	8000.092667	11.047693	-0.051796	4.815627
249.829453	8000.058579	11.052698	-0.051761	4.815618
249.902386	8000.059767	11.057703	-0.051774	4.815618
249.863451	8000.083694	11.062707	-0.051767	4.815626
249.767688	8000.078936	11.067712	-0.051749	4.815625
249.852945	8000.136913	11.072717	-0.051765	4.815641
249.716513	8000.134697	11.077722	-0.051740	4.815641
249.842918	8000.098316	11.082727	-0.051763	4.815630
249.927175	8000.090079	11.087731	-0.051779	4.815627
249.831187	8000.052218	11.092736	-0.051761	4.815616
249.856169	8000.078251	11.097741	-0.051766	4.815624
249.920899	8000.065425	11.102746	-0.051778	4.815620
249.810062	8000.108470	11.107751	-0.051757	4.815633
249.860818	8000.135991	11.112755	-0.051767	4.815641
249.811426	8000.033756	11.117760	-0.051758	4.815611
249.881092	8000.107496	11.122765	-0.051771	4.815632
249.872041	8000.081725	11.127770	-0.051769	4.815625
249.876907	8000.083942	11.132775	-0.051770	4.815626
249.778910	8000.133602	11.137779	-0.051752	4.815641
249.762358	8000.079948	11.142784	-0.051749	4.815625
250.014421	8000.047746	11.147789	-0.051796	4.815614
249.700689	7999.975381	11.152794	-0.051737	4.815595
249.750210	8000.056267	11.157799	-0.051746	4.815618
249.898168	8000.141958	11.162803	-0.051774	4.815642
249.749980	8000.040252	11.167808	-0.051746	4.815613
249.680916	8000.139497	11.172813	-0.051734	4.815643
249.662852	8000.091158	11.177818	-0.051730	4.815629
249.741159	8000.076417	11.182823	-0.051745	4.815624
249.779229	8000.120815	11.187827	-0.051752	4.815637
249.766232	8000.054407	11.192832	-0.051750	4.815617
249.911226	8000.118695	11.197837	-0.051777	4.815636
249.693235	8000.064970	11.202842	-0.051736	4.815621
249.801182	8000.054982	11.207847	-0.051756	4.815617
249.756148	8000.100164	11.212851	-0.051748	4.815631
249.811330	8000.030593	11.217856	-0.051758	4.815610
249.845414	8000.105890	11.222861	-0.051765	4.815632
249.913145	8000.051472	11.227866	-0.051777	4.815616
249.781511	8000.063214	11.232871	-0.051753	4.815620
249.633130	8000.151561	11.237875	-0.051725	4.815646
249.949847	8000.060616	11.242880	-0.051784	4.815618
249.980296	8000.111297	11.247885	-0.051790	4.815633
249.710302	8000.095164	11.252890	-0.051739	4.815630
249.946134	8000.081917	11.257895	-0.051783	4.815625
250.116752	8000.085761	11.262899	-0.051815	4.815625
249.981936	8000.025914	11.267904	-0.051790	4.815608
249.833237	8000.048056	11.272909	-0.051762	4.815615
249.945679	8000.093663	11.277914	-0.051783	4.815628
250.210537	8000.095836	11.282919	-0.051833	4.815627
250.026566	8000.113134	11.287923	-0.051799	4.815633
249.814103	8000.096869	11.292928	-0.051759	4.815630
250.182110	8000.164783	11.297933	-0.051828	4.815648
250.065782	8000.084949	11.302938	-0.051806	4.815625
249.958219	8000.008461	11.307943	-0.051786	4.815603
250.039644	8000.046090	11.312947	-0.051801	4.815614
250.102360	8000.062060	11.317952	-0.051813	4.815618
249.945469	8000.074459	11.322957	-0.051784	4.815622
249.717135	8000.109188	11.327962	-0.051741	4.815634
250.124676	8000.079513	11.332967	-0.051817	4.815623
249.930570	8000.110526	11.337971	-0.051781	4.815633
249.946821	8000.048864	11.342976	-0.051784	4.815615
250.081623	8000.098038	11.347981	-0.051809	4.815629
249.952485	8000.092738	11.352986	-0.051785	4.815628
249.758862	8000.075711	11.357991	-0.051749	4.815624
250.172040	8000.045060	11.362995	-0.051826	4.815613
250.208574	8000.018963	11.368000	-0.051833	4.815605
250.187072	8000.084815	11.373005	-0.051829	4.815624
250.011842	8000.074494	11.378010	-0.051796	4.815622
250.069046	8000.048733	11.383015	-0.051807	4.815614
250.198134	8000.098882	11.388019	-0.051831	4.815628
250.086222	8000.022323	11.393024	-0.051810	4.815606
250.006480	8000.028503	11.398029	-0.051795	4.815609
250.094154	7999.994695	11.403034	-0.051812	4.815598
250.070942	8000.010336	11.408039	-0.051807	4.815603
250.267083	8000.072252	11.413043	-0.051844	4.815620
250.242339	7999.993908	11.418048	-0.051839	4.815597
250.137122	8000.062669	11.423053	-0.051820	4.815618
250.237862	8000.091003	11.428058	-0.051839	4.815626
250.232100	8000.068489	11.433063	-0.051837	4.815619
250.206050	8000.131064	11.438067	-0.051833	4.815638
250.000383	8000.036965	11.443072	-0.051794	4.815611
250.194978	8000.039063	11.448077	-0.051831	4.815611
249.940844	8000.087252	11.453082	-0.051783	4.815626
249.750630	8000.084162	11.458087	-0.051748	4.815626
249.839682	8000.083476	11.463091	-0.051765	4.815626
249.923741	8000.019713	11.468096	-0.051780	4.815606
250.035476	8000.095205	11.473101	-0.051801	4.815628
249.955524	8000.041589	11.478106	-0.051786	4.815613
250.079841	8000.055357	11.483111	-0.051809	4.815616
250.127857	8000.057207	11.488115	-0.051818	4.815616
250.029597	8000.002226	11.493120	-0.051800	4.815601
250.044041	8000.052646	11.498125	-0.051803	4.815616
250.034682	8000.092002	11.503130	-0.051801	4.815627
250.114198	8000.068739	11.508135	-0.051816	4.815620
250.165725	8000.160336	11.513139	-0.051826	4.815646
250.186354	8000.105152	11.518144	-0.051829	4.815630
250.167771	8000.108055	11.523149	-0.051826	4.815631
250.009172	8000.001908	11.528154	-0.051796	4.815601
250.254323	8000.005896	11.533159	-0.051842	4.815601
250.235560	8000.052573	11.538163	-0.051839	4.815615
250.144236	8000.014788	11.543168	-0.051822	4.815604
250.288536	8000.022475	11.548173	-0.051849	4.815606
250.241604	8000.048407	11.553178	-0.051840	4.815613
250.130737	8000.017778	11.558183	-0.051819	4.815605
250.089040	8000.074759	11.563187	-0.051811	4.815622
249.938163	8000.120356	11.568192	-0.051783	4.815636
250.115760	8000.098688	11.573197	-0.051817	4.815629
249.871210	8000.080834	11.578202	-0.051771	4.815625
249.928129	8000.031578	11.583207	-0.051782	4.815610
249.991983	8000.089208	11.588211	-0.051794	4.815626
249.845244	8000.037709	11.593216	-0.051766	4.815612
249.852750	8000.124319	11.598221	-0.051768	4.815637
249.983091	8000.100815	11.603226	-0.051792	4.815630
250.043629	8000.087921	11.608231	-0.051803	4.815626
250.175988	8000.086872	11.613235	-0.051828	4.815625
249.877398	8000.059597	11.618240	-0.051772	4.815618
250.060934	8000.077531	11.623245	-0.051807	4.815623
250.068390	8000.065909	11.628250	-0.051808	4.815619
249.999782	8000.109641	11.633255	-0.051795	4.815632
249.952229	8000.155850	11.638259	-0.051786	4.815646
249.827507	8000.108979	11.643264	-0.051763	4.815633
250.055723	8000.100947	11.648269	-0.051806	4.815630
249.820541	8000.093922	11.653274	-0.051762	4.815629
249.968498	8000.045079	11.658279	-0.051789	4.815614
249.967290	8000.083499	11.663283	-0.051789	4.815625
250.048288	8000.100834	11.668288	-0.051804	4.815630
250.128646	8000.076518	11.673293	-0.051819	4.815622
250.081583	8000.147293	11.678298	-0.051811	4.815643
250.246130	8000.096584	11.683303	-0.051841	4.815627
250.177863	8000.125372	11.688307	-0.051829	4.815636
250.000219	8000.093657	11.693312	-0.051796	4.815628
250.176148	8000.159516	11.698317	-0.051828	4.815646
249.974639	8000.119939	11.703322	-0.051791	4.815636
250.107155	8000.051625	11.708327	-0.051816	4.815615
250.173134	8000.078326	11.713331	-0.051828	4.815622
250.216566	8000.057679	11.718336	-0.051836	4.815616
250.230560	8000.079263	11.723341	-0.051839	4.815622
250.077445	8000.053286	11.728346	-0.051810	4.815616
250.156089	8000.062041	11.733351	-0.051825	4.815618
250.224711	8000.127223	11.738355	-0.051838	4.815636
249.957811	8000.057754	11.743360	-0.051788	4.815617
250.278417	8000.120626	11.748365	-0.051848	4.815634
250.501888	8000.106111	11.753370	-0.051889	4.815629
250.568025	8000.095443	11.758375	-0.051902	4.815626
250.316732	8000.170372	11.763379	-0.051855	4.815649
250.223521	8000.125081	11.768384	-0.051838	4.815636
250.361501	8000.194594	11.773389	-0.051863	4.815656
250.142601	8000.176088	11.778394	-0.051823	4.815651
250.014717	8000.134505	11.783399	-0.051799	4.815640
250.302457	8000.148795	11.788403	-0.051852	4.815642
250.253949	8000.078606	11.793408	-0.051843	4.815622
250.485848	8000.058888	11.798413	-0.051886	4.815615
250.530661	8000.077771	11.803418	-0.051895	4.815621
250.406492	8000.029841	11.808423	-0.051872	4.815607
250.112973	8000.088067	11.813427	-0.051817	4.815626
250.002738	8000.071328	11.818432	-0.051797	4.815621
250.079313	8000.080050	11.823437	-0.051811	4.815623
250.221057	8000.084492	11.828442	-0.051837	4.815624
250.116481	8000.075320	11.833447	-0.051818	4.815622
250.351794	8000.113316	11.838451	-0.051862	4.815632
250.296972	8000.110291	11.843456	-0.051852	4.815631
250.017846	8000.075858	11.848461	-0.051800	4.815622
250.098021	8000.051538	11.853466	-0.051815	4.815615
250.030928	8000.081413	11.858471	-0.051802	4.815624
250.010601	8000.148352	11.863475	-0.051798	4.815644
249.998899	8000.093709	11.868480	-0.051796	4.815628
250.327461	8000.128951	11.873485	-0.051857	4.815636
250.133479	8000.147153	11.878490	-0.051821	4.815643
249.963945	8000.103825	11.883495	-0.051790	4.815631
249.935871	8000.116183	11.888499	-0.051785	4.815635
250.023440	8000.074900	11.893504	-0.051801	4.815622
249.996661	8000.054180	11.898509	-0.051796	4.815616
250.030044	8000.082486	11.903514	-0.051802	4.815624
250.065606	8000.094811	11.908519	-0.051809	4.815628
250.142252	8000.105669	11.913523	-0.051823	4.815631
250.183558	8000.041211	11.918528	-0.051831	4.815611
250.145435	8000.124944	11.923533	-0.051824	4.815636
250.232466	8000.110345	11.928538	-0.051840	4.815631
250.251205	8000.093568	11.933543	-0.051843	4.815626
250.378561	8000.152232	11.938547	-0.051867	4.815643
250.177718	8000.049668	11.943552	-0.051830	4.815614
250.093339	8000.100617	11.948557	-0.051814	4.815629
250.093801	8000.096356	11.953562	-0.051814	4.815628
250.318436	8000.123501	11.958567	-0.051856	4.815635
250.094971	8000.054738	11.963571	-0.051815	4.815616
249.947256	8000.065151	11.968576	-0.051787	4.815620
250.121851	8000.107498	11.973581	-0.051820	4.815631
250.219081	8000.173145	11.978586	-0.051838	4.815650
250.256951	8000.072328	11.983591	-0.051845	4.815620
250.107582	8000.121153	11.988595	-0.051817	4.815635
250.015130	8000.083349	11.993600	-0.051800	4.815625
250.327013	8000.168503	11.998605	-0.051858	4.815648
250.257540	8000.144952	12.003610	-0.051845	4.815641
250.279595	8000.109010	12.008615	-0.051849	4.815631
250.249616	8000.126676	12.013619	-0.051844	4.815636
250.048522	7999.983536	12.018624	-0.051806	4.815595
250.249349	8000.121337	12.023629	-0.051844	4.815635
250.309101	8000.138327	12.028634	-0.051855	4.815639
250.251895	8000.053048	12.033639	-0.051844	4.815615
250.153292	8000.111240	12.038643	-0.051826	4.815632
250.299366	8000.031401	12.043648	-0.051853	4.815608
250.387730	8000.107582	12.048653	-0.051869	4.815630
250.293647	8000.086835	12.053658	-0.051852	4.815624
250.263881	8000.118385	12.058663	-0.051846	4.815634
250.245242	8000.197097	12.063667	-0.051843	4.815657
250.231303	8000.197940	12.068672	-0.051840	4.815657
250.227277	8000.173319	12.073677	-0.051840	4.815650
250.146637	8000.159197	12.078682	-0.051825	4.815646
250.141320	8000.091845	12.083687	-0.051824	4.815626
250.125161	8000.135361	12.088691	-0.051821	4.815639
250.327016	8000.091665	12.093696	-0.051858	4.815626
250.409107	8000.126102	12.098701	-0.051874	4.815635
250.229904	8000.121055	12.103706	-0.051840	4.815635
250.320078	8000.076611	12.108711	-0.051857	4.815621
250.309904	8000.124496	12.113715	-0.051855	4.815635
250.213096	8000.043911	12.118720	-0.051837	4.815612
250.019896	8000.130461	12.123725	-0.051801	4.815638
250.207863	8000.072659	12.128730	-0.051836	4.815621
250.239895	8000.075317	12.133735	-0.051842	4.815621
250.332757	8000.183604	12.138739	-0.051860	4.815652
250.429219	8000.146736	12.143744	-0.051878	4.815641
250.301114	8000.138248	12.148749	-0.051854	4.815639
250.198491	8000.124836	12.153754	-0.051835	4.815636
250.049503	8000.094655	12.158759	-0.051807	4.815628
250.220543	8000.134809	12.163763	-0.051839	4.815639
250.177836	8000.091407	12.168768	-0.051831	4.815626
250.277621	8000.085557	12.173773	-0.051850	4.815624
250.284408	8000.167886	12.178778	-0.051851	4.815648
250.202105	8000.059776	12.183783	-0.051836	4.815617
250.172867	8000.052896	12.188787	-0.051830	4.815615
250.226852	8000.033489	12.193792	-0.051840	4.815609
250.337397	8000.164485	12.198797	-0.051861	4.815647
250.240684	8000.154372	12.203802	-0.051843	4.815644
250.006522	8000.154838	12.208807	-0.051799	4.815646
250.174842	8000.178932	12.213811	-0.051831	4.815652
250.107281	8000.088145	12.218816	-0.051818	4.815626
250.159242	8000.115686	12.223821	-0.051828	4.815633
250.318565	8000.127888	12.228826	-0.051857	4.815636
250.065482	8000.040492	12.233831	-0.051810	4.815612
250.060207	8000.073508	12.238835	-0.051809	4.815621
250.075102	8000.069481	12.243840	-0.051812	4.815620
250.117644	8000.108613	12.248845	-0.051820	4.815631
250.185252	8000.126799	12.253850	-0.051833	4.815636
250.161896	8000.100795	12.258855	-0.051828	4.815629
250.507573	8000.193974	12.263859	-0.051893	4.815655
250.067175	8000.165459	12.268864	-0.051811	4.815648
250.232400	8000.145725	12.273869	-0.051842	4.815642
250.409551	8000.168895	12.278874	-0.051875	4.815648
250.207159	8000.119693	12.283879	-0.051837	4.815634
250.219092	8000.183954	12.288883	-0.051839	4.815653
250.190089	8000.087388	12.293888	-0.051834	4.815625
250.302505	8000.125521	12.298893	-0.051855	4.815636
250.198171	8000.159062	12.303898	-0.051835	4.815646
250.170280	8000.134053	12.308903	-0.051830	4.815639
250.253752	8000.185596	12.313907	-0.051846	4.815653
250.297850	8000.116912	12.318912	-0.051854	4.815633
250.126936	8000.191012	12.323917	-0.051822	4.815656
250.122469	8000.187738	12.328922	-0.051821	4.815655
250.249015	8000.140682	12.333927	-0.051845	4.815640
250.322776	8000.197406	12.338931	-0.051859	4.815656
250.256155	8000.174970	12.343936	-0.051846	4.815650
250.123551	8000.141851	12.348941	-0.051822	4.815641
250.082857	8000.077128	12.353946	-0.051814	4.815622
250.191515	8000.028713	12.358951	-0.051834	4.815608
250.313148	8000.090486	12.363955	-0.051857	4.815625
250.131329	8000.076854	12.368960	-0.051823	4.815622
250.153885	8000.062275	12.373965	-0.051827	4.815618
250.231268	8000.109448	12.378970	-0.051842	4.815631
250.443662	8000.041365	12.383975	-0.051881	4.815610
250.477454	8000.132675	12.388979	-0.051888	4.815637
250.369700	8000.133060	12.393984	-0.051868	4.815637
250.516523	8000.108757	12.398989	-0.051895	4.815630
250.380761	8000.087332	12.403994	-0.051870	4.815624
250.366619	8000.033717	12.408999	-0.051867	4.815608
250.410366	8000.155085	12.414003	-0.051875	4.815644
250.535109	8000.077035	12.419008	-0.051899	4.815620
250.298672	8000.098818	12.424013	-0.051855	4.815628
250.317865	8000.192026	12.429018	-0.051858	4.815655
250.416340	8000.126361	12.434023	-0.051877	4.815635
250.387214	8000.177142	12.439027	-0.051871	4.815650
250.444257	8000.092652	12.444032	-0.051882	4.815625
250.467090	8000.073806	12.449037	-0.051886	4.815620
250.372042	8000.126717	12.454042	-0.051869	4.815636
250.268356	8000.102611	12.459047	-0.051849	4.815629
250.387475	8000.156869	12.464051	-0.051871	4.815644
250.531124	8000.096211	12.469056	-0.051898	4.815626
250.344757	8000.101724	12.474061	-0.051864	4.815628
250.239413	8000.109623	12.479066	-0.051844	4.815631
250.328087	8000.112135	12.484071	-0.051860	4.815631
250.325772	8000.160147	12.489075	-0.051860	4.815646
250.164951	8000.075318	12.494080	-0.051830	4.815621
250.297253	8000.067862	12.499085	-0.051855	4.815619
250.419276	8000.070916	12.504090	-0.051878	4.815619
250.401796	8000.050347	12.509095	-0.051874	4.815613
250.686651	8000.132927	12.514099	-0.051927	4.815636
250.264643	8000.164505	12.519104	-0.051849	4.815647
250.337625	8000.106968	12.524109	-0.051862	4.815630
250.343053	8000.150836	12.529114	-0.051863	4.815643
250.565308	8000.049813	12.534119	-0.051905	4.815612
250.705586	8000.143923	12.539123	-0.051931	4.815639
250.504204	8000.060569	12.544128	-0.051894	4.815616
250.596478	8000.097307	12.549133	-0.051911	4.815626
250.552499	8000.103001	12.554138	-0.051903	4.815628
250.339886	8000.017329	12.559143	-0.051863	4.815604
250.262053	8000.039556	12.564147	-0.051849	4.815611
250.582662	7999.981775	12.569152	-0.051908	4.815592
250.275127	8000.002402	12.574157	-0.051851	4.815600
250.333971	8000.077035	12.579162	-0.051862	4.815621
250.617036	8000.042134	12.584167	-0.051915	4.815610
250.505300	8000.057403	12.589171	-0.051894	4.815615
250.478495	8000.066578	12.594176	-0.051889	4.815617
250.562154	8000.109583	12.599181	-0.051905	4.815630
250.491031	8000.108428	12.604186	-0.051891	4.815630
250.360859	8000.046520	12.609191	-0.051867	4.815612
250.451341	8000.071484	12.614195	-0.051884	4.815619
250.384963	8000.091762	12.619200	-0.051872	4.815625
250.464090	8000.082373	12.624205	-0.051886	4.815622
250.559597	8000.093538	12.629210	-0.051904	4.815625
250.603250	8000.024847	12.634215	-0.051912	4.815605
250.580860	8000.104565	12.639219	-0.051908	4.815628
250.231358	8000.102087	12.644224	-0.051843	4.815629
250.422282	8000.045401	12.649229	-0.051879	4.815611
250.306995	8000.124676	12.654234	-0.051857	4.815635
250.198672	8000.070598	12.659239	-0.051837	4.815620
250.374398	8000.104422	12.664243	-0.051870	4.815629
250.415659	8000.052775	12.669248	-0.051878	4.815614
250.505654	8000.052105	12.674253	-0.051894	4.815613
250.292660	8000.120183	12.679258	-0.051855	4.815634
250.450654	8000.145177	12.684263	-0.051884	4.815641
250.513476	8000.116304	12.689267	-0.051896	4.815632
250.417578	8000.105136	12.694272	-0.051878	4.815629
250.659304	8000.047140	12.699277	-0.051923	4.815611
250.838559	8000.075684	12.704282	-0.051957	4.815618
250.701169	8000.062774	12.709287	-0.051931	4.815615
250.772905	8000.106653	12.714291	-0.051944	4.815628
250.511529	8000.008443	12.719296	-0.051896	4.815600
250.544212	8000.034602	12.724301	-0.051902	4.815608
250.471390	8000.062249	12.729306	-0.051888	4.815616
250.621365	8000.058283	12.734311	-0.051916	4.815614
250.800986	8000.079358	12.739315	-0.051950	4.815620
250.510536	8000.114144	12.744320	-0.051896	4.815631
250.464984	8000.060018	12.749325	-0.051887	4.815616
250.481408	8000.128622	12.754330	-0.051890	4.815636
250.470346	8000.048364	12.759335	-0.051888	4.815612
250.503307	8000.115102	12.764339	-0.051894	4.815631
250.533370	8000.073951	12.769344	-0.051900	4.815619
250.827472	8000.081940	12.774349	-0.051955	4.815620
250.616541	8000.129763	12.779354	-0.051916	4.815635
250.705944	8000.058612	12.784359	-0.051932	4.815614
250.642785	8000.117381	12.789363	-0.051921	4.815631
250.453042	8000.069452	12.794368	-0.051885	4.815618
250.528277	8000.034375	12.799373	-0.051899	4.815608
250.524768	8000.138958	12.804378	-0.051899	4.815638
250.537706	8000.072971	12.809383	-0.051901	4.815619
250.786626	8000.115460	12.814387	-0.051947	4.815630
250.849975	8000.093002	12.819392	-0.051959	4.815623
250.798305	8000.043047	12.824397	-0.051950	4.815609
250.637469	8000.104499	12.829402	-0.051920	4.815628
250.660601	8000.022660	12.834407	-0.051924	4.815604
250.735949	8000.045243	12.839411	-0.051938	4.815610
250.482480	8000.052868	12.844416	-0.051891	4.815613
250.483287	8000.099864	12.849421	-0.051891	4.815627
250.655211	8000.179540	12.854426	-0.051923	4.815650
250.697605	8000.110828	12.859431	-0.051931	4.815629
250.682420	8000.108448	12.864435	-0.051928	4.815629
250.647194	8000.143113	12.869440	-0.051922	4.815639
250.648752	8000.080143	12.874445	-0.051922	4.815621
250.538210	8000.180851	12.879450	-0.051902	4.815651
250.594156	8000.102750	12.884455	-0.051912	4.815627
250.796513	8000.177582	12.889459	-0.051950	4.815648
250.789292	8000.123012	12.894464	-0.051948	4.815632
250.653035	8000.048191	12.899469	-0.051923	4.815611
250.739348	8000.141423	12.904474	-0.051939	4.815638
250.581868	8000.059850	12.909479	-0.051910	4.815615
250.545336	8000.093426	12.914483	-0.051903	4.815625
250.363161	8000.084059	12.919488	-0.051869	4.815623
250.674362	8000.057090	12.924493	-0.051927	4.815614
250.636179	8000.105588	12.929498	-0.051920	4.815628
250.250874	8000.115340	12.934503	-0.051848	4.815633
250.671772	8000.094425	12.939507	-0.051927	4.815625
250.615151	8000.119133	12.944512	-0.051916	4.815632
250.479317	8000.043251	12.949517	-0.051891	4.815611
250.676237	8000.167111	12.954522	-0.051928	4.815646
250.755098	8000.106467	12.959527	-0.051942	4.815628
250.619983	8000.072239	12.964531	-0.051917	4.815618
250.651874	8000.130418	12.969536	-0.051923	4.815635
250.829291	8000.070308	12.974541	-0.051956	4.815617
250.747012	8000.135173	12.979546	-0.051941	4.815636
250.465299	8000.098561	12.984551	-0.051888	4.815627
250.609642	8000.146823	12.989555	-0.051915	4.815640
250.523088	8000.122995	12.994560	-0.051899	4.815634
250.319828	8000.127166	12.999565	-0.051861	4.815636
250.460189	8000.175364	13.004570	-0.051888	4.815649
250.450583	8000.075909	13.009575	-0.051886	4.815620
250.683096	8000.112793	13.014579	-0.051929	4.815630
250.453530	8000.080233	13.019584	-0.051886	4.815621
250.643204	8000.058761	13.024589	-0.051922	4.815614
250.439824	8000.112046	13.029594	-0.051884	4.815631
250.493312	8000.070208	13.034599	-0.051894	4.815618
250.641670	8000.086504	13.039603	-0.051922	4.815622
250.724753	8000.144448	13.044608	-0.051937	4.815639
250.524655	8000.083537	13.049613	-0.051900	4.815622
250.509791	8000.086501	13.054618	-0.051897	4.815623
250.617079	8000.062622	13.059623	-0.051917	4.815616
250.631216	8000.140800	13.064627	-0.051920	4.815638
250.384690	8000.096218	13.069632	-0.051874	4.815626
250.595916	8000.069758	13.074637	-0.051913	4.815618
250.615636	8000.132010	13.079642	-0.051917	4.815636
250.526324	8000.065428	13.084647	-0.051900	4.815617
250.781341	8000.102677	13.089651	-0.051948	4.815626
250.654445	8000.115564	13.094656	-0.051924	4.815631
250.669041	8000.062416	13.099661	-0.051927	4.815615
250.677545	8000.088182	13.104666	-0.051929	4.815623
250.623397	8000.057407	13.109671	-0.051918	4.815614
250.654056	8000.093143	13.114675	-0.051924	4.815624
250.784982	8000.082462	13.119680	-0.051949	4.815621
250.802314	8000.056052	13.124685	-0.051952	4.815613
250.852086	8000.080354	13.129690	-0.051961	4.815620
250.575242	8000.022467	13.134695	-0.051910	4.815604
250.738513	8000.066766	13.139699	-0.051940	4.815616
250.777496	8000.112248	13.144704	-0.051947	4.815629
250.557679	8000.078778	13.149709	-0.051906	4.815621
250.785200	8000.089954	13.154714	-0.051949	4.815623
250.671649	8000.040061	13.159719	-0.051928	4.815609
250.713543	8000.069574	13.164723	-0.051936	4.815617
250.659129	8000.077233	13.169728	-0.051925	4.815620
250.636863	8000.099296	13.174733	-0.051921	4.815626
250.825822	8000.102371	13.179738	-0.051957	4.815626
250.611051	8000.087135	13.184743	-0.051917	4.815623
250.631590	8000.094945	13.189747	-0.051920	4.815625
250.569520	8000.082193	13.194752	-0.051909	4.815621
250.699435	8000.045869	13.199757	-0.051933	4.815610
250.625868	8000.143975	13.204762	-0.051919	4.815639
250.732247	8000.125420	13.209767	-0.051939	4.815633
250.751608	8000.110788	13.214771	-0.051943	4.815629
250.727953	8000.155251	13.219776	-0.051939	4.815642
250.650703	8000.078187	13.224781	-0.051924	4.815620
250.765032	8000.123826	13.229786	-0.051945	4.815633
250.664358	8000.025026	13.234791	-0.051927	4.815604
250.827693	8000.081072	13.239795	-0.051957	4.815620
250.684345	8000.056320	13.244800	-0.051930	4.815613
250.750575	8000.018960	13.249805	-0.051943	4.815602
250.671530	8000.080674	13.254810	-0.051928	4.815621
250.726671	8000.075166	13.259815	-0.051938	4.815619
250.797228	8000.081654	13.264819	-0.051952	4.815620
250.735940	8000.047560	13.269824	-0.051940	4.815611
250.847521	8000.077138	13.274829	-0.051961	4.815619
251.064567	8000.131923	13.279834	-0.052001	4.815634
250.762956	8000.076835	13.284839	-0.051945	4.815619
250.985399	8000.064438	13.289843	-0.051987	4.815614
250.744396	8000.088282	13.294848	-0.051942	4.815622
250.906863	8000.085588	13.299853	-0.051972	4.815621
250.760746	8000.073604	13.304858	-0.051945	4.815618
250.850497	8000.067591	13.309863	-0.051962	4.815616
251.012066	8000.096915	13.314867	-0.051992	4.815624
250.929992	8000.073159	13.319872	-0.051977	4.815617
250.951766	8000.035077	13.324877	-0.051981	4.815606
251.270239	8000.086173	13.329882	-0.052040	4.815619
250.773140	8000.104783	13.334887	-0.051947	4.815627
250.684166	8000.121490	13.339891	-0.051931	4.815632
250.689724	8000.053246	13.344896	-0.051932	4.815612
250.888192	7999.989208	13.349901	-0.051969	4.815593
250.737570	8000.134110	13.354906	-0.051941	4.815636
250.852081	8000.037741	13.359911	-0.051962	4.815607
250.852210	8000.106081	13.364915	-0.051962	4.815627
250.608420	8000.155506	13.369920	-0.051917	4.815643
250.585985	8000.091078	13.374925	-0.051913	4.815624
250.872441	8000.112823	13.379930	-0.051966	4.815629
250.648650	8000.047256	13.384935	-0.051924	4.815611
250.817453	8000.135424	13.389939	-0.051956	4.815636
250.789008	8000.156318	13.394944	-0.051951	4.815642
250.751450	8000.063883	13.399949	-0.051944	4.815615
250.715341	8000.141244	13.404954	-0.051937	4.815638
250.591614	8000.057017	13.409959	-0.051914	4.815614
250.910506	8000.093170	13.414963	-0.051973	4.815623
250.691400	8000.051170	13.419968	-0.051933	4.815612
250.727089	8000.042142	13.424973	-0.051939	4.815609
250.754290	8000.055400	13.429978	-0.051944	4.815613
250.760425	8000.054434	13.434983	-0.051946	4.815612
250.782653	8000.118863	13.439987	-0.051950	4.815631
250.646326	8000.124122	13.444992	-0.051924	4.815633
250.956145	8000.065098	13.449997	-0.051982	4.815615
250.874652	8000.092604	13.455002	-0.051967	4.815623
250.741476	8000.021036	13.460007	-0.051942	4.815603
250.923362	8000.061368	13.465011	-0.051976	4.815614
250.849466	8000.126369	13.470016	-0.051962	4.815633
250.666096	8000.053985	13.475021	-0.051928	4.815613
250.876814	8000.180205	13.480026	-0.051967	4.815649
250.850019	8000.111435	13.485031	-0.051962	4.815629
250.569535	8000.105808	13.490035	-0.051910	4.815628
250.716055	8000.070822	13.495040	-0.051938	4.815617
250.770429	8000.059963	13.500045	-0.051948	4.815614
250.814576	8000.164255	13.505050	-0.051956	4.815644
250.765806	8000.101534	13.510055	-0.051947	4.815626
250.930922	8000.082867	13.515059	-0.051978	4.815620
250.861480	8000.147940	13.520064	-0.051965	4.815639
250.614456	8000.103350	13.525069	-0.051919	4.815627
250.778318	8000.165811	13.530074	-0.051949	4.815645
250.753069	8000.089592	13.535079	-0.051945	4.815623
250.650285	8000.114616	13.540083	-0.051926	4.815631
250.882181	8000.178185	13.545088	-0.051969	4.815648
250.962157	8000.105812	13.550093	-0.051984	4.815626
251.000111	8000.138465	13.555098	-0.051991	4.815636
250.629905	8000.115361	13.560103	-0.051922	4.815631
250.887425	8000.148381	13.565107	-0.051970	4.815639
251.040955	8000.176507	13.570112	-0.051998	4.815647
250.891241	8000.084382	13.575117	-0.051971	4.815621
250.969541	8000.168943	13.580122	-0.051985	4.815645
250.682331	8000.131173	13.585127	-0.051932	4.815635
250.513446	8000.172206	13.590131	-0.051900	4.815648
250.581308	8000.147686	13.595136	-0.051913	4.815641
250.675812	8000.063805	13.600141	-0.051931	4.815616
250.870762	8000.106485	13.605146	-0.051967	4.815627
250.594978	8000.082782	13.610151	-0.051916	4.815621
250.914282	8000.113603	13.615155	-0.051975	4.815629
250.980909	8000.187297	13.620160	-0.051988	4.815650
250.622852	8000.114206	13.625165	-0.051921	4.815631
250.726076	8000.136174	13.630170	-0.051940	4.815636
250.565872	8000.084455	13.635175	-0.051910	4.815622
250.679051	8000.121533	13.640179	-0.051931	4.815632
250.687671	8000.121675	13.645184	-0.051933	4.815632
250.914084	8000.067701	13.650189	-0.051975	4.815616
251.051458	8000.183120	13.655194	-0.052001	4.815649
250.911512	8000.166965	13.660199	-0.051975	4.815645
250.866915	8000.154496	13.665203	-0.051967	4.815641
250.924149	8000.127668	13.670208	-0.051977	4.815633
250.891071	8000.110048	13.675213	-0.051971	4.815628
250.871297	8000.108660	13.680218	-0.051967	4.815628
250.909890	8000.078325	13.685223	-0.051975	4.815619
250.940339	8000.099110	13.690227	-0.051980	4.815625
250.818814	8000.164404	13.695232	-0.051958	4.815644
250.757293	8000.099340	13.700237	-0.051946	4.815626
250.838116	8000.159384	13.705242	-0.051961	4.815643
250.757666	8000.120706	13.710247	-0.051946	4.815632
250.842628	8000.173342	13.715251	-0.051962	4.815647
250.884031	8000.185763	13.720256	-0.051970	4.815650
250.720721	8000.138263	13.725261	-0.051940	4.815637
250.788153	8000.109465	13.730266	-0.051952	4.815628
250.791496	8000.120199	13.735271	-0.051953	4.815631
250.862120	8000.137366	13.740275	-0.051966	4.815636
250.867836	8000.188713	13.745280	-0.051967	4.815651
250.847954	8000.121123	13.750285	-0.051963	4.815631
250.954101	8000.206137	13.755290	-0.051983	4.815656
250.666352	8000.142732	13.760295	-0.051930	4.815639
251.002837	8000.130056	13.765299	-0.051992	4.815633
250.791504	8000.127688	13.770304	-0.051953	4.815634
250.679446	8000.047922	13.775309	-0.051932	4.815611
250.768218	8000.142262	13.780314	-0.051949	4.815638
250.709216	8000.150914	13.785319	-0.051938	4.815641
250.761967	8000.125080	13.790323	-0.051948	4.815633
250.670230	8000.107574	13.795328	-0.051931	4.815628
250.879368	8000.026625	13.800333	-0.051969	4.815604
250.983708	8000.156455	13.805338	-0.051989	4.815641
250.829114	8000.058913	13.810343	-0.051960	4.815613
250.704194	8000.135897	13.815347	-0.051937	4.815636
251.019523	8000.149570	13.820352	-0.051996	4.815639
250.983312	8000.098798	13.825357	-0.051989	4.815624
250.773185	8000.096450	13.830362	-0.051950	4.815625
250.892007	8000.048201	13.835367	-0.051972	4.815610
250.976804	8000.125393	13.840371	-0.051988	4.815632
250.924876	8000.171532	13.845376	-0.051978	4.815646
250.802743	8000.118295	13.850381	-0.051955	4.815631
250.912644	8000.163862	13.855386	-0.051976	4.815644
250.898394	8000.148684	13.860391	-0.051973	4.815639
250.883426	8000.121749	13.865395	-0.051971	4.815631
250.888771	8000.144261	13.870400	-0.051972	4.815638
250.821484	8000.132491	13.875405	-0.051959	4.815635
250.957237	8000.164598	13.880410	-0.051984	4.815644
251.016750	8000.115384	13.885415	-0.051995	4.815629
250.952554	8000.073767	13.890419	-0.051984	4.815617
250.807919	8000.147227	13.895424	-0.051957	4.815639
250.736934	8000.091619	13.900429	-0.051943	4.815623
251.026313	8000.153987	13.905434	-0.051997	4.815640
250.795546	8000.090441	13.910439	-0.051954	4.815623
250.889852	8000.115468	13.915443	-0.051972	4.815630
251.167869	8000.145619	13.920448	-0.052024	4.815637
251.054932	8000.062634	13.925453	-0.052003	4.815613
250.881226	8000.155909	13.930458	-0.051970	4.815641
250.970513	8000.125331	13.935463	-0.051987	4.815632
251.027672	8000.112382	13.940467	-0.051998	4.815628
251.091864	8000.193510	13.945472	-0.052010	4.815651
251.112190	8000.172488	13.950477	-0.052014	4.815645
251.030932	8000.214946	13.955482	-0.051999	4.815658
250.886503	8000.207260	13.960487	-0.051972	4.815656
250.762780	8000.151861	13.965491	-0.051949	4.815641
250.945429	8000.206087	13.970496	-0.051983	4.815656
250.985085	8000.126652	13.975501	-0.051990	4.815632
250.949526	8000.189074	13.980506	-0.051983	4.815651
250.975069	8000.129697	13.985511	-0.051988	4.815633
250.919230	8000.125587	13.990515	-0.051978	4.815632
250.884879	8000.089795	13.995520	-0.051971	4.815622
250.939489	8000.093888	14.000525	-0.051982	4.815623
251.043249	8000.150034	14.005530	-0.052001	4.815639
250.868491	8000.087399	14.010535	-0.051968	4.815621
250.793816	8000.120355	14.015539	-0.051955	4.815631
250.881839	8000.174109	14.020544	-0.051971	4.815647
250.761720	8000.136921	14.025549	-0.051949	4.815636
250.671208	8000.181364	14.030554	-0.051932	4.815650
250.700006	8000.090008	14.035559	-0.051937	4.815623
250.920084	8000.124555	14.040563	-0.051978	4.815632
251.154521	8000.165742	14.045568	-0.052022	4.815643
250.834298	8000.038811	14.050573	-0.051962	4.815607
251.014014	8000.070565	14.055578	-0.051996	4.815616
251.018413	8000.094130	14.060583	-0.051997	4.815623
251.062896	8000.154650	14.065587	-0.052005	4.815640
251.098514	8000.165909	14.070592	-0.052012	4.815643
251.030732	8000.070846	14.075597	-0.051999	4.815616
250.805553	8000.132318	14.080602	-0.051957	4.815635
250.922912	8000.097926	14.085607	-0.051979	4.815624
251.183816	8000.137408	14.090611	-0.052028	4.815635
251.072271	8000.150544	14.095616	-0.052007	4.815639
250.665424	8000.117235	14.100621	-0.051931	4.815631
250.941222	8000.152688	14.105626	-0.051982	4.815640
251.047728	8000.157626	14.110631	-0.052002	4.815641
250.805146	8000.101362	14.115635	-0.051957	4.815626
250.847096	8000.107385	14.120640	-0.051965	4.815627
250.985312	8000.109635	14.125645	-0.051991	4.815627
251.025443	8000.141255	14.130650	-0.051998	4.815636
250.907289	8000.096625	14.135655	-0.051976	4.815624
251.093501	8000.068691	14.140659	-0.052011	4.815615
251.061100	8000.126893	14.145664	-0.052005	4.815632
250.960700	8000.032367	14.150669	-0.051986	4.815605
250.879813	8000.088712	14.155674	-0.051971	4.815622
251.016476	8000.085598	14.160679	-0.051997	4.815620
250.978091	8000.124483	14.165683	-0.051990	4.815632
250.860566	8000.139658	14.170688	-0.051968	4.815637
250.865638	8000.135471	14.175693	-0.051969	4.815636
250.846332	8000.105262	14.180698	-0.051965	4.815627
250.716026	8000.096738	14.185703	-0.051941	4.815625
251.072529	8000.143114	14.190707	-0.052007	4.815637
251.137042	8000.147369	14.195712	-0.052019	4.815638
250.762391	8000.114583	14.200717	-0.051950	4.815630
250.862809	8000.137573	14.205722	-0.051968	4.815636
251.089992	8000.087883	14.210727	-0.052011	4.815621
250.931746	8000.090650	14.215731	-0.051981	4.815622
250.784749	8000.157665	14.220736	-0.051954	4.815642
250.774167	8000.127598	14.225741	-0.051952	4.815634
250.883705	8000.149669	14.230746	-0.051972	4.815640
250.975073	8000.145819	14.235751	-0.051989	4.815638
250.985542	8000.134246	14.240755	-0.051991	4.815635
251.168951	8000.166061	14.245760	-0.052026	4.815643
251.012710	8000.112269	14.250765	-0.051996	4.815628
250.776450	8000.166087	14.255770	-0.051953	4.815645
250.924280	8000.161019	14.260775	-0.051980	4.815643
250.941178	8000.108976	14.265779	-0.051983	4.815627
250.964966	8000.154211	14.270784	-0.051988	4.815641
250.913688	8000.096788	14.275789	-0.051978	4.815624
251.003933	7999.193892	14.280794	-0.051994	4.815360

250.834984	7996.004391	14.285799	-0.051961	4.814428
250.901942	7990.564319	14.290803	-0.051970	4.812836
250.874407	7983.932979	14.295808	-0.051960	4.810896
250.810984	7976.634162	14.300813	-0.051944	4.808759
250.857416	7969.026995	14.305818	-0.051948	4.806531
250.865582	7961.192670	14.310823	-0.051944	4.804236
250.856366	7953.376737	14.315827	-0.051937	4.801944
250.873035	7945.343581	14.320832	-0.051935	4.799588
250.829383	7937.456015	14.325837	-0.051922	4.797274
250.973757	7929.426174	14.330842	-0.051944	4.794916
250.660475	7921.425544	14.335847	-0.051880	4.792567
250.496514	7913.359918	14.340851	-0.051844	4.790197
250.672926	7905.435808	14.345856	-0.051872	4.787867
250.691763	7897.374328	14.350861	-0.051870	4.785495
250.540044	7889.449214	14.355866	-0.051837	4.783164
250.617022	7881.393294	14.360871	-0.051846	4.780791
250.582302	7873.393912	14.365875	-0.051834	4.778435
250.502125	7865.447676	14.370880	-0.051814	4.776093
250.350824	7857.373221	14.375885	-0.051781	4.773712
250.426938	7849.422098	14.380890	-0.051790	4.771366
250.284297	7841.343148	14.385895	-0.051758	4.768982
250.313345	7833.418359	14.390899	-0.051758	4.766641
250.419218	7825.370570	14.395904	-0.051773	4.764263
250.199438	7817.422155	14.400909	-0.051727	4.761914
250.471954	7809.398013	14.405914	-0.051772	4.759540
250.208930	7801.409615	14.410919	-0.051718	4.757177
250.140449	7793.385318	14.415923	-0.051700	4.754801
249.914345	7785.320120	14.420928	-0.051653	4.752413
250.040825	7777.282916	14.425933	-0.051671	4.750030
250.181253	7769.369852	14.430938	-0.051692	4.747684
250.028736	7761.306081	14.435943	-0.051659	4.745292
250.037449	7753.330125	14.440947	-0.051655	4.742924
250.092148	7745.359671	14.445952	-0.051660	4.740557
249.981595	7737.342175	14.450957	-0.051634	4.738176
249.826063	7729.353524	14.455962	-0.051600	4.735801
249.862166	7721.306755	14.460967	-0.051602	4.733408
249.939093	7713.310584	14.465971	-0.051611	4.731028
249.756635	7705.320240	14.470976	-0.051572	4.728650
249.763341	7697.304249	14.475981	-0.051568	4.726262
249.962165	7689.301326	14.480986	-0.051599	4.723877
249.720245	7681.323733	14.485991	-0.051549	4.721499
249.746484	7673.310650	14.490995	-0.051549	4.719108
250.045112	7665.401105	14.496000	-0.051599	4.716747
249.808525	7657.307190	14.501005	-0.051550	4.714330
249.764785	7649.302598	14.506010	-0.051537	4.711939
249.675054	7641.264158	14.511015	-0.051515	4.709536
249.727173	7633.312312	14.516019	-0.051519	4.707158
249.688652	7625.321056	14.521024	-0.051507	4.704767
249.509805	7617.324562	14.526029	-0.051469	4.702373
249.793510	7609.307233	14.531034	-0.051516	4.699971
249.579505	7601.378093	14.536039	-0.051471	4.697595
249.569062	7593.306548	14.541043	-0.051464	4.695175
249.502979	7585.285649	14.546048	-0.051446	4.692769
249.639576	7577.247243	14.551053	-0.051467	4.690356
249.368546	7569.315523	14.556058	-0.051411	4.687974
249.316419	7561.282185	14.561063	-0.051396	4.685561
249.421207	7553.304745	14.566067	-0.051410	4.683162
249.473366	7545.311367	14.571072	-0.051415	4.680758
249.194398	7537.267509	14.576077	-0.051358	4.678338
249.288956	7529.338599	14.581082	-0.051370	4.675951
249.180782	7521.255270	14.586087	-0.051345	4.673516
249.086934	7513.173162	14.591091	-0.051322	4.671080
249.131105	7505.201481	14.596096	-0.051325	4.668676
249.064193	7497.200338	14.601101	-0.051308	4.666262
249.121565	7489.229703	14.606106	-0.051313	4.663856
248.922130	7481.262216	14.611111	-0.051271	4.661450
249.088948	7473.189695	14.616115	-0.051297	4.659010
248.897120	7465.279138	14.621120	-0.051256	4.656619
248.703453	7457.212790	14.626125	-0.051214	4.654179
248.936357	7449.226257	14.631130	-0.051253	4.651762
248.927894	7441.180259	14.636135	-0.051246	4.649325
248.734119	7433.234856	14.641139	-0.051205	4.646918
248.921655	7425.253364	14.646144	-0.051234	4.644499
248.698402	7417.271993	14.651149	-0.051188	4.642078
248.761831	7409.217270	14.656154	-0.051194	4.639634
248.760826	7401.233485	14.661159	-0.051189	4.637210
248.831990	7393.222144	14.666163	-0.051197	4.634776
249.033278	7385.174095	14.671168	-0.051229	4.632330
248.888037	7377.119549	14.676173	-0.051197	4.629881
248.937770	7369.213147	14.681178	-0.051201	4.627476
248.798878	7361.178425	14.686183	-0.051170	4.625030
248.586497	7353.204334	14.691187	-0.051125	4.622601
248.723155	7345.223403	14.696192	-0.051146	4.620169
248.566718	7337.201520	14.701197	-0.051111	4.617723
248.593694	7329.202380	14.706202	-0.051111	4.615283
248.765291	7321.194151	14.711207	-0.051138	4.612839
248.520516	7313.134042	14.716211	-0.051087	4.610378
248.717387	7305.225198	14.721216	-0.051119	4.607961
248.673919	7297.120499	14.726221	-0.051105	4.605484
248.672048	7289.189542	14.731226	-0.051100	4.603058
248.581281	7281.162924	14.736231	-0.051078	4.600601
248.294290	7273.158225	14.741235	-0.051019	4.598150
248.203776	7265.201425	14.746240	-0.050997	4.595713
248.372313	7257.146620	14.751245	-0.051023	4.593244
248.541641	7249.098123	14.756250	-0.051049	4.590775
248.223504	7241.122054	14.761255	-0.050985	4.588328
248.407872	7233.072973	14.766259	-0.051014	4.585857
248.320358	7225.149757	14.771264	-0.050993	4.583423
247.967087	7217.137059	14.776269	-0.050922	4.580960
248.350640	7209.170343	14.781274	-0.050988	4.578510
248.433542	7201.128532	14.786279	-0.050998	4.576036
248.220452	7193.170080	14.791283	-0.050953	4.573586
248.273068	7185.136026	14.796288	-0.050958	4.571112
248.208689	7177.114839	14.801293	-0.050941	4.568640
248.189143	7169.114051	14.806298	-0.050932	4.566173
248.177095	7161.104420	14.811303	-0.050924	4.563701
248.249799	7153.154396	14.816307	-0.050933	4.561248
248.001800	7145.169623	14.821312	-0.050881	4.558781
247.868732	7137.162484	14.826317	-0.050851	4.556307
247.834089	7129.156254	14.831322	-0.050840	4.553831
248.074765	7121.119728	14.836327	-0.050879	4.551345
247.833086	7113.103121	14.841331	-0.050829	4.548864
247.764285	7105.125334	14.846336	-0.050811	4.546393
248.043896	7097.102632	14.851341	-0.050858	4.543908
247.879120	7089.165311	14.856346	-0.050822	4.541447
247.733991	7081.101443	14.861351	-0.050790	4.538945
247.791328	7073.118272	14.866355	-0.050796	4.536467
247.977754	7065.124556	14.871360	-0.050825	4.533985
247.648041	7057.080272	14.876365	-0.050758	4.531485
247.752694	7049.066750	14.881370	-0.050773	4.528994
247.733750	7041.088564	14.886375	-0.050764	4.526512
247.739365	7033.032359	14.891379	-0.050760	4.524005
247.651604	7025.179767	14.896384	-0.050738	4.521560
247.583141	7017.097911	14.901389	-0.050720	4.519042
247.473549	7009.165083	14.906394	-0.050695	4.516568
247.426627	7001.089063	14.911399	-0.050681	4.514049
247.176263	6992.994224	14.916403	-0.050629	4.511522
247.235664	6985.072374	14.921408	-0.050635	4.509049
246.833103	6977.062878	14.926413	-0.050555	4.506545
246.901690	6969.038930	14.931418	-0.050562	4.504037
247.068315	6961.096396	14.936423	-0.050588	4.501553
246.977284	6953.092709	14.941427	-0.050566	4.499048
246.944216	6945.092988	14.946432	-0.050555	4.496543
246.954539	6937.046530	14.951437	-0.050551	4.494022
247.043533	6929.030714	14.956442	-0.050563	4.491509
246.841797	6921.024208	14.961447	-0.050520	4.488997
246.842809	6913.048083	14.966451	-0.050515	4.486494
246.951296	6905.039535	14.971456	-0.050530	4.483980
246.807043	6897.061922	14.976461	-0.050498	4.481473
246.942396	6889.071968	14.981466	-0.050518	4.478961
246.833067	6881.094058	14.986471	-0.050493	4.476451
246.992862	6873.014573	14.991475	-0.050517	4.473909
246.948154	6865.032111	14.996480	-0.050504	4.471395
246.638623	6857.022510	15.001485	-0.050441	4.468871
246.889421	6849.035824	15.006490	-0.050482	4.466354
246.735806	6841.038524	15.011495	-0.050448	4.463830
246.632646	6833.034332	15.016499	-0.050424	4.461304
246.711310	6825.058209	15.021504	-0.050433	4.458785
246.464148	6817.021452	15.026509	-0.050382	4.456245
246.646609	6809.015580	15.031514	-0.050411	4.453715
246.733012	6800.983847	15.036519	-0.050422	4.451174
246.795175	6793.014180	15.041523	-0.050428	4.448652
246.844991	6785.016656	15.046528	-0.050432	4.446119
246.485845	6776.990714	15.051533	-0.050360	4.443575
246.792088	6769.046166	15.056538	-0.050412	4.441057
246.667338	6761.020423	15.061543	-0.050384	4.438510
246.255365	6753.027921	15.066547	-0.050302	4.435972
246.512713	6744.988471	15.071552	-0.050345	4.433419
246.619919	6736.934096	15.076557	-0.050359	4.430860
246.415771	6728.973266	15.081562	-0.050316	4.428328
246.387625	6720.974273	15.086567	-0.050306	4.425783
246.493588	6712.968101	15.091571	-0.050320	4.423235
246.466594	6704.992029	15.096576	-0.050310	4.420694
246.125432	6696.962681	15.101581	-0.050241	4.418133
246.175073	6689.015283	15.106586	-0.050245	4.415599
246.049202	6681.002799	15.111591	-0.050217	4.413042
245.911151	6672.937532	15.116595	-0.050186	4.410466
246.071986	6664.987533	15.121600	-0.050211	4.407928
246.038590	6656.954402	15.126605	-0.050199	4.405360
245.849131	6649.018320	15.131610	-0.050159	4.402821
245.747639	6640.986931	15.136615	-0.050135	4.400250
245.978518	6633.024877	15.141619	-0.050172	4.397702
245.970998	6624.978861	15.146624	-0.050166	4.395124
245.917047	6616.972452	15.151629	-0.050151	4.392557
245.798729	6608.972845	15.156634	-0.050123	4.389990
245.926593	6600.996981	15.161639	-0.050142	4.387431
245.618196	6592.947959	15.166643	-0.050079	4.384845
245.776393	6584.995475	15.171648	-0.050104	4.382290
245.577339	6576.993877	15.176653	-0.050061	4.379717
245.729475	6569.051742	15.181658	-0.050085	4.377162
245.626985	6560.998684	15.186663	-0.050060	4.374570
245.660701	6552.975028	15.191667	-0.050061	4.371985
245.724743	6544.970064	15.196672	-0.050068	4.369406
245.463682	6536.989580	15.201677	-0.050014	4.366831
245.428243	6528.948614	15.206682	-0.050003	4.364236
245.499773	6520.989635	15.211687	-0.050011	4.361667
245.280300	6512.998552	15.216691	-0.049965	4.359084
245.420876	6505.058239	15.221696	-0.049986	4.356519
245.304228	6496.918320	15.226701	-0.049959	4.353885
245.357123	6488.857092	15.231706	-0.049963	4.351277
245.337079	6480.923625	15.236711	-0.049954	4.348708
245.371111	6472.944616	15.241715	-0.049956	4.346123
245.481088	6464.966838	15.246720	-0.049971	4.343537
245.181795	6456.943707	15.251725	-0.049910	4.340932
245.197123	6449.009216	15.256730	-0.049908	4.338357
245.230572	6440.972380	15.261735	-0.049909	4.335747
245.006845	6432.931541	15.266739	-0.049862	4.333132
245.012017	6424.956879	15.271744	-0.049858	4.330539
244.887444	6416.963001	15.276749	-0.049829	4.327937
245.000474	6408.943780	15.281754	-0.049845	4.325327
245.130838	6400.972087	15.286759	-0.049864	4.322732
244.970318	6392.926501	15.291763	-0.049829	4.320108
245.091506	6385.031597	15.296768	-0.049846	4.317534
244.888517	6376.948944	15.301773	-0.049803	4.314894
244.964196	6368.905002	15.306778	-0.049812	4.312268
245.041001	6360.906029	15.311783	-0.049821	4.309655
244.936751	6352.914246	15.316787	-0.049797	4.307041
244.982700	6344.936194	15.321792	-0.049800	4.304432
244.773873	6336.979565	15.326797	-0.049756	4.301825
244.717484	6328.928881	15.331802	-0.049740	4.299188
244.626774	6320.975421	15.336807	-0.049718	4.296580
244.737878	6312.907677	15.341811	-0.049734	4.293935
244.678239	6304.894745	15.346816	-0.049718	4.291305
244.408619	6296.904352	15.351821	-0.049662	4.288680
244.466330	6288.919289	15.356826	-0.049668	4.286056
244.555662	6280.911718	15.361831	-0.049679	4.283425
244.315137	6272.894689	15.366835	-0.049629	4.280785
244.405694	6264.918757	15.371840	-0.049641	4.278161
244.508848	6256.921782	15.376845	-0.049655	4.275527
244.263464	6248.908493	15.381850	-0.049604	4.272884
244.265443	6240.872944	15.386855	-0.049599	4.270234
244.147189	6232.870166	15.391859	-0.049572	4.267593
244.361342	6224.889049	15.396864	-0.049607	4.264959
244.133816	6216.878368	15.401869	-0.049559	4.262310
244.142121	6208.884318	15.406874	-0.049555	4.259668
244.276424	6200.939915	15.411879	-0.049575	4.257041
244.121139	6192.858404	15.416883	-0.049541	4.254364
244.402918	6184.912248	15.421888	-0.049588	4.251735
244.158818	6176.868774	15.426893	-0.049538	4.249067
244.138448	6168.916413	15.431898	-0.049529	4.246429
244.288633	6160.880488	15.436903	-0.049552	4.243764
244.319307	6152.910291	15.441907	-0.049552	4.241118
244.267418	6144.928640	15.446912	-0.049537	4.238466
244.126647	6136.951758	15.451917	-0.049506	4.235812
244.069096	6128.903411	15.456922	-0.049490	4.233134
244.132049	6120.895110	15.461927	-0.049496	4.230469
243.951010	6112.926182	15.466931	-0.049458	4.227813
243.910819	6104.910420	15.471936	-0.049445	4.225141
243.863907	6096.958907	15.476941	-0.049431	4.222488
243.877616	6088.918017	15.481946	-0.049428	4.219805
243.691066	6080.981744	15.486951	-0.049388	4.217153
243.635067	6072.924230	15.491955	-0.049373	4.214460
243.823016	6064.937247	15.496960	-0.049403	4.211791
243.679862	6056.922530	15.501965	-0.049371	4.209108
243.702440	6048.945149	15.506970	-0.049370	4.206437
243.637962	6040.929894	15.511975	-0.049353	4.203751
243.550163	6032.923319	15.516979	-0.049331	4.201066
243.556302	6024.964536	15.521984	-0.049327	4.198397
243.521705	6016.960041	15.526989	-0.049315	4.195710
243.596385	6008.834552	15.531994	-0.049324	4.192981
243.509493	6000.830950	15.536999	-0.049303	4.190291
243.461378	5992.848912	15.542003	-0.049289	4.187606
243.536971	5984.889332	15.547008	-0.049297	4.184928
243.308406	5976.883593	15.552013	-0.049250	4.182230
243.288805	5968.905891	15.557018	-0.049241	4.179541
243.643098	5960.960776	15.562023	-0.049302	4.176866
243.503454	5952.864060	15.567027	-0.049270	4.174133
243.395546	5944.891827	15.572032	-0.049245	4.171440
243.450996	5936.871257	15.577037	-0.049250	4.168731
243.308530	5928.884742	15.582042	-0.049219	4.166030
243.282188	5920.924430	15.587047	-0.049208	4.163337
243.113280	5912.880121	15.592051	-0.049172	4.160612
243.074881	5904.921437	15.597056	-0.049160	4.157916
242.995151	5896.900307	15.602061	-0.049139	4.155196
243.060845	5888.872044	15.607066	-0.049146	4.152474
243.190555	5880.847706	15.612071	-0.049165	4.149752
242.963275	5872.871479	15.617075	-0.049118	4.147041
243.046945	5864.864767	15.622080	-0.049128	4.144321
243.052249	5856.897279	15.627085	-0.049124	4.141612
243.087641	5848.888990	15.632090	-0.049126	4.138887
243.029676	5840.944321	15.637095	-0.049110	4.136181
242.610291	5832.868647	15.642099	-0.049026	4.133425
242.855624	5824.871402	15.647104	-0.049067	4.130701
242.642515	5816.873226	15.652109	-0.049022	4.127969
242.508472	5808.883019	15.657114	-0.048992	4.125240
242.670252	5800.917382	15.662119	-0.049017	4.122521
242.706383	5792.877616	15.667123	-0.049018	4.119773
242.617084	5784.955545	15.672128	-0.048996	4.117061
242.504155	5776.868218	15.677133	-0.048970	4.114292
242.467763	5768.852749	15.682138	-0.048958	4.111546
242.653399	5760.867929	15.687143	-0.048988	4.108811
242.285215	5752.849405	15.692147	-0.048914	4.106056
242.397212	5744.870771	15.697152	-0.048930	4.103319
242.346821	5736.872777	15.702157	-0.048915	4.100571
242.321596	5728.900085	15.707162	-0.048905	4.097831
242.178617	5720.895578	15.712167	-0.048873	4.095076
242.218674	5712.856727	15.717171	-0.048876	4.092310
242.273414	5704.874381	15.722176	-0.048881	4.089561
241.992370	5696.929651	15.727181	-0.048823	4.086820
242.201727	5688.903962	15.732186	-0.048857	4.084055
242.036517	5680.970904	15.737191	-0.048821	4.081315
241.909316	5672.926947	15.742195	-0.048792	4.078535
242.058996	5664.960485	15.747200	-0.048815	4.075785
242.093221	5656.903831	15.752205	-0.048816	4.072999
241.947002	5648.851894	15.757210	-0.048783	4.070211
241.900171	5640.929471	15.762215	-0.048770	4.067467
241.920461	5632.864657	15.767219	-0.048768	4.064673
241.973002	5624.964273	15.772224	-0.048773	4.061934
241.879553	5616.940324	15.777229	-0.048750	4.059149
241.899581	5608.950468	15.782234	-0.048749	4.056375
241.837991	5600.940742	15.787239	-0.048732	4.053591
241.766549	5592.901958	15.792243	-0.048714	4.050795
241.681051	5584.933938	15.797248	-0.048692	4.048021
241.750699	5576.906586	15.802253	-0.048700	4.045227
241.582870	5568.943233	15.807258	-0.048664	4.042450
241.602574	5560.933551	15.812263	-0.048662	4.039658
241.620562	5552.965262	15.817267	-0.048660	4.036878
241.540238	5544.903902	15.822272	-0.048640	4.034062
241.443114	5536.784626	15.827277	-0.048617	4.031224
241.664761	5528.833092	15.832282	-0.048653	4.028447
241.591228	5520.874881	15.837287	-0.048634	4.025662
241.340040	5512.925559	15.842291	-0.048582	4.022875
241.537149	5504.896171	15.847296	-0.048614	4.020065
241.512375	5496.907074	15.852301	-0.048604	4.017264
241.427791	5488.887978	15.857306	-0.048583	4.014449
241.343359	5480.907432	15.862311	-0.048562	4.011645
241.317324	5472.881919	15.867315	-0.048552	4.008825
241.301574	5464.919305	15.872320	-0.048544	4.006026
241.457586	5456.895066	15.877325	-0.048568	4.003205
241.357761	5448.904009	15.882330	-0.048544	4.000390
241.304456	5440.959906	15.887335	-0.048529	3.997590
241.245518	5432.918977	15.892339	-0.048513	3.994754
241.228902	5424.881842	15.897344	-0.048504	3.991918
241.240117	5416.850030	15.902349	-0.048501	3.989082
241.093824	5408.893956	15.907354	-0.048469	3.986269
241.051187	5400.903429	15.912359	-0.048456	3.983443
241.203306	5392.883904	15.917363	-0.048479	3.980607
241.217753	5384.954068	15.922368	-0.048476	3.977800
240.969793	5376.920669	15.927373	-0.048425	3.974949
241.106144	5368.907499	15.932378	-0.048445	3.972110
241.128770	5360.893986	15.937383	-0.048444	3.969267
240.873653	5352.929362	15.942387	-0.048392	3.966434
240.910924	5344.938073	15.947392	-0.048393	3.963595
240.893764	5336.951614	15.952397	-0.048385	3.960755
240.986272	5328.979626	15.957402	-0.048397	3.957919
240.911939	5320.988117	15.962407	-0.048378	3.955072
240.698032	5312.933894	15.967411	-0.048333	3.952198
240.798236	5304.926260	15.972416	-0.048346	3.949344
240.741315	5296.960081	15.977421	-0.048331	3.946500
240.846946	5288.913891	15.982426	-0.048345	3.943628
240.959803	5280.966595	15.987431	-0.048361	3.940789
240.762703	5272.967970	15.992435	-0.048319	3.937925
240.759043	5264.994376	15.997440	-0.048313	3.935071
240.585605	5256.979319	16.002445	-0.048276	3.932196
240.689113	5248.933640	16.007450	-0.048290	3.929314
240.630673	5241.019450	16.012455	-0.048274	3.926474
240.244722	5232.965046	16.017459	-0.048197	3.923576
240.516979	5225.007508	16.022464	-0.048242	3.920722
240.346742	5217.020956	16.027469	-0.048205	3.917847
240.324179	5208.984199	16.032474	-0.048196	3.914955
240.647035	5200.948629	16.037479	-0.048251	3.912068
240.469203	5192.931724	16.042483	-0.048212	3.909176
240.437696	5184.987683	16.047488	-0.048201	3.906311
240.477070	5176.956721	16.052493	-0.048204	3.903414
240.506180	5168.969410	16.057498	-0.048204	3.900530
240.592569	5161.031631	16.062503	-0.048215	3.897663
240.547183	5152.988371	16.067507	-0.048201	3.894754
240.490999	5144.983623	16.072512	-0.048185	3.891855
240.238034	5136.958246	16.077517	-0.048133	3.888944
240.121478	5128.979094	16.082522	-0.048106	3.886049
240.334142	5121.011599	16.087527	-0.048141	3.883164
240.179075	5112.972496	16.092531	-0.048107	3.880242
240.036879	5105.043634	16.097536	-0.048075	3.877359
240.348508	5096.997529	16.102541	-0.048128	3.874440
240.021532	5088.747481	16.107546	-0.048062	3.871432
239.937894	5080.817324	16.112551	-0.048041	3.868543
239.921686	5072.873182	16.117555	-0.048033	3.865648
239.749336	5064.966659	16.122560	-0.047995	3.862761
239.767882	5056.935915	16.127565	-0.047994	3.859831
239.873373	5048.974838	16.132570	-0.048008	3.856926
240.103892	5040.943641	16.137575	-0.048046	3.853995
239.786586	5032.947163	16.142579	-0.047982	3.851064
239.651851	5024.974882	16.147584	-0.047951	3.848143
239.554293	5017.002380	16.152589	-0.047928	3.845220
239.571205	5009.011691	16.157594	-0.047926	3.842291
239.516406	5001.045591	16.162599	-0.047911	3.839367
239.377783	4993.053774	16.167603	-0.047880	3.836430
239.757513	4984.981865	16.172608	-0.047945	3.833472
239.669022	4976.993573	16.177613	-0.047923	3.830533
239.291143	4969.027969	16.182618	-0.047848	3.827593
239.634028	4961.003664	16.187623	-0.047907	3.824645
239.515174	4953.052570	16.192627	-0.047879	3.821712
239.378106	4945.073154	16.197632	-0.047849	3.818766
239.351142	4937.080913	16.202637	-0.047838	3.815815
239.355765	4929.023771	16.207642	-0.047834	3.812839
239.481841	4921.057016	16.212647	-0.047852	3.809896
239.239574	4913.058842	16.217651	-0.047802	3.806931
239.350923	4905.070728	16.222656	-0.047818	3.803975
239.365058	4897.095339	16.227661	-0.047815	3.801020
239.301186	4889.108876	16.232666	-0.047798	3.798057
239.207261	4881.108598	16.237671	-0.047775	3.795085
239.391403	4873.041834	16.242675	-0.047804	3.792093
239.037557	4865.051188	16.247680	-0.047733	3.789114
239.077039	4857.056900	16.252685	-0.047735	3.786141
239.029119	4849.033890	16.257690	-0.047721	3.783153
238.963427	4841.096201	16.262695	-0.047704	3.780193
238.706237	4833.080084	16.267699	-0.047651	3.777198
238.831641	4825.065678	16.272704	-0.047669	3.774210
239.036890	4817.068597	16.277709	-0.047702	3.771227
238.720698	4809.061108	16.282714	-0.047638	3.768227
238.757149	4801.086969	16.287719	-0.047640	3.765244
238.711438	4793.076667	16.292723	-0.047626	3.762244
238.723190	4785.108390	16.297728	-0.047623	3.759258
238.622100	4777.134266	16.302733	-0.047599	3.756266
238.719993	4769.053622	16.307738	-0.047612	3.753235
238.813402	4761.086092	16.312743	-0.047624	3.750245
238.637866	4753.064426	16.317747	-0.047586	3.747225
238.717689	4745.078980	16.322752	-0.047596	3.744223
238.664207	4737.133128	16.327757	-0.047581	3.741229
238.385294	4729.118392	16.332762	-0.047524	3.738203
238.295148	4721.161264	16.337767	-0.047502	3.735200
238.394797	4713.095225	16.342771	-0.047515	3.732158
238.400954	4705.101138	16.347776	-0.047511	3.729138
238.279140	4697.127451	16.352781	-0.047483	3.726121
238.286283	4689.151227	16.357786	-0.047479	3.723103
238.364306	4681.193419	16.362791	-0.047489	3.720091
237.957259	4673.215529	16.367795	-0.047408	3.717058
238.206936	4665.182296	16.372800	-0.047449	3.714017
238.117770	4657.057399	16.377805	-0.047427	3.710931
238.190677	4649.079126	16.382810	-0.047435	3.707901
238.302121	4641.108946	16.387815	-0.047451	3.704874
238.094925	4633.143045	16.392819	-0.047407	3.701837
238.039992	4625.192670	16.397824	-0.047392	3.698808
237.878393	4617.208345	16.402829	-0.047357	3.695761
237.957660	4609.172306	16.407834	-0.047366	3.692697
238.119355	4601.156270	16.412839	-0.047391	3.689641
238.009236	4593.186841	16.417843	-0.047365	3.686593
237.933026	4585.222623	16.422848	-0.047346	3.683545
238.140128	4577.220098	16.427853	-0.047379	3.680487
237.892377	4569.261818	16.432858	-0.047328	3.677432
237.888757	4561.209276	16.437863	-0.047322	3.674345
237.991026	4553.180803	16.442867	-0.047336	3.671267
237.795501	4545.196131	16.447872	-0.047294	3.668196
237.570997	4537.220195	16.452877	-0.047247	3.665124
237.662272	4529.226430	16.457882	-0.047259	3.662051
237.755504	4521.249745	16.462887	-0.047271	3.658983
237.492791	4513.247255	16.467891	-0.047217	3.655892
237.444403	4505.245924	16.472896	-0.047203	3.652805
237.518207	4497.198552	16.477901	-0.047212	3.649701
237.424083	4489.225268	16.482906	-0.047189	3.646618
237.533692	4481.225375	16.487911	-0.047204	3.643528
237.476663	4473.230022	16.492915	-0.047188	3.640433
237.576202	4465.262891	16.497920	-0.047202	3.637350
237.361216	4457.269569	16.502925	-0.047157	3.634246
237.461314	4449.225044	16.507930	-0.047170	3.631127
237.614365	4441.231111	16.512935	-0.047193	3.628028
237.245968	4433.243515	16.517939	-0.047120	3.624913
237.409448	4425.271347	16.522944	-0.047145	3.621817
237.285245	4417.276481	16.527949	-0.047116	3.618701
237.052486	4409.293821	16.532954	-0.047068	3.615584
237.371869	4401.270271	16.537959	-0.047122	3.612464
237.218897	4393.246264	16.542963	-0.047089	3.609328
236.982962	4385.332668	16.547968	-0.047039	3.606230
237.003497	4377.332655	16.552973	-0.047038	3.603103
236.990515	4369.320452	16.557978	-0.047030	3.599967
237.124646	4361.387549	16.562983	-0.047050	3.596864
236.992292	4353.341297	16.567987	-0.047020	3.593706
236.822893	4345.317580	16.572992	-0.046984	3.590553
237.187485	4337.311641	16.577997	-0.047046	3.587420
236.910826	4329.326489	16.583002	-0.046990	3.584273
236.884544	4321.386596	16.588007	-0.046980	3.581149
236.938336	4313.375686	16.593011	-0.046984	3.577996
236.886497	4305.409631	16.598016	-0.046970	3.574856
236.782510	4297.395089	16.603021	-0.046945	3.571692
236.835135	4289.365916	16.608026	-0.046950	3.568523
236.931793	4281.398266	16.613031	-0.046963	3.565378
236.705799	4273.429091	16.618035	-0.046915	3.562220
236.600544	4265.447111	16.623040	-0.046891	3.559057
236.644029	4257.447056	16.628045	-0.046893	3.555889
236.633238	4249.340114	16.633050	-0.046886	3.552674
236.654547	4241.313604	16.638055	-0.046885	3.549489
236.346089	4233.356680	16.643059	-0.046822	3.546319
236.246658	4225.395257	16.648064	-0.046799	3.543150
236.352094	4217.412264	16.653069	-0.046813	3.539976
236.295120	4209.408682	16.658074	-0.046797	3.536787
236.405630	4201.420821	16.663079	-0.046813	3.533605
236.260396	4193.401627	16.668083	-0.046780	3.530401
236.269116	4185.401524	16.673088	-0.046777	3.527206
236.242050	4177.416082	16.678093	-0.046767	3.524013
236.233286	4169.470811	16.683098	-0.046760	3.520833
236.149428	4161.498740	16.688103	-0.046739	3.517638
236.103052	4153.468801	16.693107	-0.046725	3.514418
236.360500	4145.438420	16.698112	-0.046768	3.511203
236.275280	4137.451044	16.703117	-0.046747	3.507993
236.251152	4129.456983	16.708122	-0.046737	3.504779
236.316292	4121.519968	16.713127	-0.046744	3.501588
236.172037	4113.520428	16.718131	-0.046712	3.498362
235.970902	4105.529674	16.723136	-0.046670	3.495134
236.028336	4097.526198	16.728141	-0.046675	3.491907
235.992946	4089.523460	16.733146	-0.046663	3.488674
236.159548	4081.527743	16.738151	-0.046689	3.485448
235.955282	4073.585516	16.743155	-0.046646	3.482228
235.988555	4065.576510	16.748160	-0.046647	3.478986
235.910322	4057.591477	16.753165	-0.046627	3.475747
235.660233	4049.589866	16.758170	-0.046575	3.472492
235.869624	4041.524779	16.763175	-0.046609	3.469224
235.582963	4033.560461	16.768179	-0.046551	3.465977
235.466775	4025.610836	16.773184	-0.046524	3.462739
235.644019	4017.576251	16.778189	-0.046552	3.459473
235.719425	4009.610172	16.783194	-0.046560	3.456228
235.751230	4001.593866	16.788199	-0.046561	3.452959
235.321157	3993.592587	16.793203	-0.046476	3.449677
235.310985	3985.630835	16.798208	-0.046469	3.446422
235.173545	3977.630492	16.803213	-0.046438	3.443144
235.179421	3969.619339	16.808218	-0.046434	3.439863
235.231228	3961.696584	16.813223	-0.046439	3.436617
235.330644	3953.629881	16.818227	-0.046452	3.433310
235.407737	3945.616039	16.823232	-0.046461	3.430021
235.253988	3937.664452	16.828237	-0.046427	3.426746
235.157999	3929.647551	16.833242	-0.046404	3.423444
235.213238	3921.687337	16.838247	-0.046409	3.420167
235.052951	3913.702579	16.843251	-0.046374	3.416869
235.303567	3905.693114	16.848256	-0.046416	3.413572
235.108364	3897.721460	16.853261	-0.046374	3.410272
234.905074	3889.702450	16.858266	-0.046331	3.406949
235.166556	3881.746862	16.863271	-0.046375	3.403665
235.120696	3873.741663	16.868275	-0.046361	3.400346
234.961101	3865.783924	16.873280	-0.046326	3.397040
234.982984	3857.757896	16.878285	-0.046325	3.393709
235.247378	3849.629233	16.883290	-0.046369	3.390341
235.165688	3841.718500	16.888295	-0.046348	3.387047
235.069085	3833.735074	16.893299	-0.046325	3.383720
235.165032	3825.746238	16.898304	-0.046338	3.380394
235.138380	3817.799567	16.903309	-0.046328	3.377077
234.965378	3809.817126	16.908314	-0.046290	3.373738
234.743464	3801.805043	16.913319	-0.046244	3.370381
234.582848	3793.824151	16.918323	-0.046209	3.367036
234.475103	3785.850467	16.923328	-0.046184	3.363692
234.561351	3777.855460	16.928333	-0.046195	3.360343
234.645323	3769.844790	16.933338	-0.046205	3.356984
234.497290	3761.869538	16.938343	-0.046172	3.353628
234.474602	3753.823244	16.943347	-0.046163	3.350244
234.698562	3745.817102	16.948352	-0.046199	3.346881
234.817456	3737.859127	16.953357	-0.046216	3.343532
234.302967	3729.896863	16.958362	-0.046115	3.340155
234.225834	3721.934323	16.963367	-0.046096	3.336790
234.285770	3713.889619	16.968371	-0.046102	3.333392
234.107025	3705.879163	16.973376	-0.046063	3.329996
234.189814	3697.914424	16.978381	-0.046073	3.326626
234.302416	3689.905049	16.983386	-0.046089	3.323235
234.295591	3681.952564	16.988391	-0.046083	3.319860
234.198323	3673.986785	16.993395	-0.046060	3.316472
234.027494	3665.967470	16.998400	-0.046023	3.313055
233.916122	3657.951970	17.003405	-0.045997	3.309639
233.974151	3649.935595	17.008410	-0.046002	3.306225
233.958770	3641.980103	17.013415	-0.045994	3.302831
233.888225	3633.991692	17.018419	-0.045976	3.299417
233.755324	3626.049287	17.023424	-0.045946	3.296017
233.826409	3618.037779	17.028429	-0.045954	3.292591
233.739013	3609.998564	17.033434	-0.045933	3.289144
233.912902	3602.031602	17.038439	-0.045960	3.285735
233.782679	3594.050132	17.043443	-0.045930	3.282303
233.474389	3586.067771	17.048448	-0.045868	3.278861
233.591286	3578.111244	17.053453	-0.045884	3.275443
233.662157	3570.063528	17.058458	-0.045892	3.271981
233.603592	3562.088207	17.063463	-0.045876	3.268541
233.625600	3554.071297	17.068467	-0.045875	3.265082
233.581396	3546.124552	17.073472	-0.045862	3.261648
233.683518	3538.130218	17.078477	-0.045876	3.258195
233.647035	3530.118118	17.083482	-0.045864	3.254725
233.757768	3522.141359	17.088487	-0.045879	3.251273
233.188797	3514.153708	17.093491	-0.045768	3.247785
233.238844	3506.150043	17.098496	-0.045772	3.244311
233.299571	3498.201311	17.103501	-0.045778	3.240858
233.246113	3490.196341	17.108506	-0.045763	3.237372
233.106711	3482.210164	17.113511	-0.045732	3.233887
233.264712	3474.119102	17.118515	-0.045756	3.230364
233.271310	3466.148836	17.123520	-0.045752	3.226884
233.261624	3458.182980	17.128525	-0.045745	3.223402
233.155047	3450.197033	17.133530	-0.045720	3.219903
233.442145	3442.228418	17.138535	-0.045768	3.216424
233.262744	3434.225404	17.143539	-0.045730	3.212907
233.308087	3426.218568	17.148544	-0.045733	3.209394
233.326869	3418.277661	17.153549	-0.045731	3.205905
233.206361	3410.274902	17.158554	-0.045704	3.202379
233.177270	3402.329015	17.163559	-0.045693	3.198878
233.031611	3394.349152	17.168563	-0.045661	3.195353
232.900846	3386.327975	17.173568	-0.045631	3.191807
233.083613	3378.316904	17.178573	-0.045660	3.188274
232.966406	3370.329226	17.183578	-0.045633	3.184736
232.991615	3362.386146	17.188583	-0.045633	3.181219
232.953273	3354.381242	17.193587	-0.045620	3.177668
232.832339	3346.395367	17.198592	-0.045593	3.174118
232.725857	3338.419905	17.203597	-0.045568	3.170569
232.796729	3330.379474	17.208602	-0.045576	3.166995
232.904536	3322.437685	17.213607	-0.045591	3.163462
232.853752	3314.439633	17.218611	-0.045576	3.159894
232.736476	3306.471789	17.223616	-0.045549	3.156332
232.767319	3298.460866	17.228621	-0.045549	3.152753
232.507817	3290.439252	17.233626	-0.045496	3.149153
232.616119	3282.468287	17.238631	-0.045511	3.145587
232.618233	3274.484014	17.243635	-0.045506	3.142007
232.681971	3266.520861	17.248640	-0.045513	3.138435
232.681344	3258.526568	17.253645	-0.045508	3.134842
232.705529	3250.509179	17.258650	-0.045507	3.131235
232.569713	3242.531369	17.263655	-0.045476	3.127635
232.321711	3234.562158	17.268659	-0.045425	3.124030
232.243444	3226.602025	17.273664	-0.045405	3.120432
232.414209	3218.629130	17.278669	-0.045432	3.116835
232.246405	3210.599097	17.283674	-0.045396	3.113194
232.481269	3202.591403	17.288679	-0.045434	3.109576
232.324134	3194.634154	17.293683	-0.045400	3.105959
232.039210	3186.675007	17.298688	-0.045341	3.102331
232.175065	3178.706429	17.303693	-0.045362	3.098714
232.217702	3170.686550	17.308698	-0.045364	3.095065
232.387817	3162.667379	17.313703	-0.045391	3.091418
231.925237	3154.717330	17.318707	-0.045299	3.087769
231.972169	3146.683058	17.323712	-0.045303	3.084101
232.181865	3138.747570	17.328717	-0.045337	3.080481
231.847772	3130.794732	17.333722	-0.045270	3.076823
231.932597	3122.757206	17.338727	-0.045280	3.073142
231.743062	3114.708282	17.343731	-0.045240	3.069438
231.747751	3106.751859	17.348736	-0.045235	3.065782
231.733923	3098.786479	17.353741	-0.045228	3.062116
231.704614	3090.813269	17.358746	-0.045217	3.058441
231.776089	3082.825108	17.363751	-0.045225	3.054760
231.532441	3074.839763	17.368755	-0.045175	3.051061
231.456729	3066.867844	17.373760	-0.045155	3.047371
231.409831	3058.897255	17.378765	-0.045141	3.043679
231.187246	3050.912123	17.383770	-0.045095	3.039968
231.542840	3042.946877	17.388775	-0.045156	3.036288
231.638222	3034.910002	17.393779	-0.045168	3.032559
231.369853	3026.921466	17.398784	-0.045113	3.028830
231.405849	3018.942681	17.403789	-0.045115	3.025115
231.431117	3010.952720	17.408794	-0.045114	3.021390
231.446829	3002.998324	17.413799	-0.045112	3.017677
231.271356	2995.018350	17.418803	-0.045074	3.013938
231.347998	2986.998579	17.423808	-0.045083	3.010188
231.424711	2979.026037	17.428813	-0.045092	3.006455
231.244566	2971.048529	17.433818	-0.045054	3.002703
231.153376	2963.112872	17.438823	-0.045031	2.998970
231.096290	2955.133795	17.443827	-0.045016	2.995213
230.870143	2947.118414	17.448832	-0.044968	2.991426
231.095196	2939.091882	17.453837	-0.045005	2.987652
231.183491	2931.088596	17.458842	-0.045016	2.983877
231.119860	2923.153146	17.463847	-0.044999	2.980122
230.985114	2915.176665	17.468851	-0.044969	2.976339
230.774879	2907.203326	17.473856	-0.044925	2.972549
231.066074	2899.179341	17.478861	-0.044974	2.968756
230.894899	2891.191429	17.483866	-0.044937	2.964951
231.017415	2883.253767	17.488871	-0.044954	2.961180
230.943891	2875.270642	17.493875	-0.044935	2.957373
230.881065	2867.284912	17.498880	-0.044919	2.953560
230.807641	2859.280627	17.503885	-0.044900	2.949733
230.748914	2851.306706	17.508890	-0.044884	2.945916
230.689954	2843.346433	17.513895	-0.044867	2.942100
230.466642	2835.381842	17.518899	-0.044821	2.938269
230.291368	2827.404985	17.523904	-0.044783	2.934430
230.438292	2819.380178	17.528909	-0.044805	2.930579
230.321376	2811.399191	17.533914	-0.044778	2.926731
230.215353	2803.449576	17.538919	-0.044753	2.922893
230.341029	2795.432714	17.543923	-0.044771	2.919030
230.273870	2787.479843	17.548928	-0.044754	2.915182
230.409679	2779.389484	17.553933	-0.044774	2.911274
230.362448	2771.409265	17.558938	-0.044760	2.907404
230.279704	2763.470620	17.563943	-0.044739	2.903547
230.147217	2755.514679	17.568947	-0.044709	2.899674
230.265869	2747.528161	17.573952	-0.044726	2.895794
230.199620	2739.562552	17.578957	-0.044709	2.891909
230.086223	2731.556649	17.583962	-0.044683	2.887997
230.174319	2723.587756	17.588967	-0.044694	2.884109
230.113442	2715.636612	17.593971	-0.044677	2.880215
229.915543	2707.679077	17.598976	-0.044635	2.876306
230.159991	2699.642898	17.603981	-0.044676	2.872378
230.014702	2691.661906	17.608986	-0.044643	2.868449
230.076781	2683.663566	17.613991	-0.044650	2.864518
229.803206	2675.748130	17.618995	-0.044594	2.860604
229.863229	2667.745998	17.624000	-0.044600	2.856661
229.861836	2659.783291	17.629005	-0.044594	2.852727
229.505463	2651.796010	17.634010	-0.044523	2.848757
229.532092	2643.806286	17.639015	-0.044522	2.844801
229.542727	2635.857779	17.644019	-0.044519	2.840859
229.681002	2627.878785	17.649024	-0.044540	2.836904
229.557785	2619.901719	17.654029	-0.044512	2.832929
229.439538	2611.859560	17.659034	-0.044484	2.828917
229.422518	2603.900500	17.664039	-0.044476	2.824946
229.341961	2595.943044	17.669043	-0.044456	2.820967
229.318193	2587.966028	17.674048	-0.044446	2.816975
229.449122	2579.975098	17.679053	-0.044466	2.812980
229.368175	2571.971923	17.684058	-0.044445	2.808961
229.359488	2564.012291	17.689063	-0.044439	2.804962
229.350395	2556.041735	17.694067	-0.044432	2.800951
229.119991	2548.097028	17.699072	-0.044384	2.796936
229.179840	2540.114799	17.704077	-0.044390	2.792912
229.158962	2532.090416	17.709082	-0.044380	2.788857
229.398470	2524.088168	17.714087	-0.044420	2.784822
229.235133	2516.173803	17.719091	-0.044384	2.780802
229.070729	2508.212690	17.724096	-0.044349	2.776752
229.261082	2500.189950	17.729101	-0.044379	2.772686
229.007974	2492.220298	17.734106	-0.044327	2.768615
228.934338	2484.261689	17.739111	-0.044308	2.764555
228.877029	2476.323900	17.744115	-0.044292	2.760499
228.755738	2468.343073	17.749120	-0.044264	2.756412
228.818721	2460.311026	17.754125	-0.044271	2.752304
228.792373	2452.262525	17.759130	-0.044260	2.748176
229.055104	2444.301962	17.764135	-0.044304	2.744104
228.851874	2436.385728	17.769139	-0.044261	2.740021
228.731620	2428.415243	17.774144	-0.044234	2.735909
228.747555	2420.434602	17.779149	-0.044231	2.731793
228.833778	2412.424407	17.784154	-0.044242	2.727661
228.649095	2404.486287	17.789159	-0.044203	2.723542
228.507862	2396.529206	17.794163	-0.044171	2.719411
228.250811	2388.600531	17.799168	-0.044118	2.715280
228.290346	2380.583763	17.804173	-0.044120	2.711116
228.259685	2372.592491	17.809178	-0.044110	2.706955
228.343030	2364.611213	17.814183	-0.044120	2.702799
228.295352	2356.653725	17.819187	-0.044106	2.698641
228.147223	2348.698547	17.824192	-0.044073	2.694472
228.385968	2340.674570	17.829197	-0.044112	2.690284
228.401977	2332.695200	17.834202	-0.044110	2.686099
228.471467	2324.735440	17.839207	-0.044118	2.681922
228.380410	2316.791484	17.844211	-0.044096	2.677736
228.071893	2308.851466	17.849216	-0.044033	2.673531
228.090069	2300.829446	17.854221	-0.044031	2.669298
227.892428	2292.858212	17.859226	-0.043989	2.665071
227.991283	2284.884204	17.864231	-0.044003	2.660854
227.925975	2276.934000	17.869235	-0.043985	2.656633
227.707046	2268.959470	17.874240	-0.043939	2.652383
227.669406	2261.001141	17.879245	-0.043927	2.648146
227.827041	2252.984782	17.884250	-0.043951	2.643884
227.704628	2245.039921	17.889255	-0.043923	2.639635
227.911188	2237.065096	17.894259	-0.043957	2.635385
227.750917	2229.075712	17.899264	-0.043922	2.631095
227.817107	2221.107833	17.904269	-0.043929	2.626826
227.682567	2213.147206	17.909274	-0.043899	2.622540
227.826130	2205.184354	17.914279	-0.043920	2.618264
227.899018	2197.204415	17.919283	-0.043929	2.613967
227.543370	2189.241971	17.924288	-0.043857	2.609644
227.566757	2181.280370	17.929293	-0.043856	2.605340
227.656042	2173.293754	17.934298	-0.043868	2.601019
227.730207	2165.345520	17.939303	-0.043877	2.596711
227.575002	2157.263485	17.944307	-0.043842	2.592308
227.626740	2149.195716	17.949312	-0.043847	2.587919
227.547058	2141.280477	17.954317	-0.043827	2.583597
227.191729	2133.376600	17.959322	-0.043756	2.579254
227.062275	2125.445003	17.964327	-0.043726	2.574905
227.008163	2117.476986	17.969331	-0.043711	2.570534
226.994870	2109.493541	17.974336	-0.043703	2.566149
227.076309	2101.548069	17.979341	-0.043713	2.561785
227.069017	2093.579190	17.984346	-0.043707	2.557394
226.997537	2085.633262	17.989351	-0.043688	2.553003
226.925050	2077.645595	17.994355	-0.043670	2.548582
227.008003	2069.656854	17.999360	-0.043680	2.544163
226.948609	2061.730983	18.004365	-0.043664	2.539762
226.685612	2053.772159	18.009370	-0.043610	2.535320
226.849691	2045.786065	18.014375	-0.043635	2.530886
226.923201	2037.815379	18.019379	-0.043644	2.526445
226.884859	2029.855395	18.024384	-0.043631	2.521996
226.744071	2021.920946	18.029389	-0.043600	2.517545
226.609053	2013.931997	18.034394	-0.043570	2.513056
226.416974	2005.958632	18.039399	-0.043529	2.508563
226.475627	1997.981211	18.044403	-0.043534	2.504079
226.299973	1990.030570	18.049408	-0.043497	2.499584
226.474378	1982.073391	18.054413	-0.043524	2.495103
226.430612	1974.076205	18.059418	-0.043511	2.490576
226.375124	1966.127021	18.064423	-0.043495	2.486066
226.277444	1958.196667	18.069427	-0.043472	2.481556
226.274270	1950.226274	18.074432	-0.043466	2.477022
226.138267	1942.272166	18.079437	-0.043435	2.472479
226.186333	1934.272969	18.084442	-0.043439	2.467916
226.262742	1926.312367	18.089447	-0.043448	2.463368
226.097386	1918.383605	18.094451	-0.043412	2.458812
226.027841	1910.401398	18.099456	-0.043394	2.454224
226.057166	1902.419831	18.104461	-0.043394	2.449635
225.916474	1894.480397	18.109466	-0.043363	2.445050
226.047004	1886.528634	18.114471	-0.043382	2.440468
225.840579	1878.589460	18.119475	-0.043339	2.435860
225.616717	1870.564672	18.124480	-0.043292	2.431193
225.707219	1862.589631	18.129485	-0.043303	2.426569
225.649114	1854.632501	18.134490	-0.043288	2.421935
225.576003	1846.695826	18.139495	-0.043269	2.417303
225.717576	1838.710397	18.144499	-0.043290	2.412651
225.711801	1830.741997	18.149504	-0.043284	2.407988
225.757276	1822.794708	18.154509	-0.043287	2.403332
225.752086	1814.839003	18.159514	-0.043281	2.398658
225.621828	1806.904893	18.164519	-0.043251	2.393978
225.447172	1798.946029	18.169523	-0.043214	2.389271
225.489734	1790.977571	18.174528	-0.043217	2.384566
225.424210	1783.044298	18.179533	-0.043199	2.379864
225.326966	1775.093928	18.184538	-0.043176	2.375140
225.380760	1767.112627	18.189543	-0.043181	2.370400
225.217433	1759.173071	18.194547	-0.043145	2.365658
225.144643	1751.227134	18.199552	-0.043127	2.360910
225.380785	1743.273504	18.204557	-0.043165	2.356173
225.206612	1735.288902	18.209562	-0.043128	2.351375
225.038745	1727.336473	18.214567	-0.043091	2.346586
225.159216	1719.362058	18.219571	-0.043109	2.341798
225.077684	1711.421202	18.224576	-0.043088	2.337004
225.023023	1703.467993	18.229581	-0.043073	2.332195
224.881850	1695.508736	18.234586	-0.043041	2.327365
224.798368	1687.578782	18.239591	-0.043021	2.322547
224.747083	1679.633995	18.244595	-0.043006	2.317713
224.757935	1671.668383	18.249600	-0.043003	2.312862
224.750677	1663.704832	18.254605	-0.042996	2.308000
224.570493	1655.768513	18.259610	-0.042958	2.303129
224.486703	1647.843992	18.264615	-0.042937	2.298264
224.644142	1639.846524	18.269619	-0.042961	2.293364
224.394701	1631.899515	18.274624	-0.042909	2.288450
224.471633	1623.954044	18.279629	-0.042919	2.283555
224.455060	1616.001892	18.284634	-0.042910	2.278636
224.336329	1608.064175	18.289639	-0.042883	2.273707
224.271128	1600.045933	18.294643	-0.042866	2.268722
224.119285	1592.103710	18.299648	-0.042832	2.263766
224.473922	1584.131392	18.304653	-0.042893	2.258824
224.262637	1576.211052	18.309658	-0.042849	2.253855
224.278570	1568.253280	18.314663	-0.042847	2.248871
224.392880	1560.302387	18.319667	-0.042863	2.243888
224.267711	1552.381683	18.324672	-0.042834	2.238893
224.040617	1544.487046	18.329677	-0.042787	2.233894
224.017196	1536.492908	18.334682	-0.042777	2.228839
223.993039	1528.555897	18.339687	-0.042768	2.223808
223.960483	1520.623048	18.344691	-0.042756	2.218768
223.720170	1512.695300	18.349696	-0.042707	2.213701
224.084117	1504.682951	18.354701	-0.042769	2.208622
223.852999	1496.785322	18.359706	-0.042721	2.203552
223.710054	1488.871917	18.364711	-0.042689	2.198468
223.789032	1480.907183	18.369715	-0.042699	2.193359
223.647051	1472.924158	18.374720	-0.042667	2.188206
223.901236	1464.953882	18.379725	-0.042709	2.183086
223.640431	1457.053746	18.384730	-0.042656	2.177952
223.730433	1449.094179	18.389735	-0.042667	2.172799
223.636587	1441.161343	18.394739	-0.042645	2.167634
223.642783	1433.204729	18.399744	-0.042641	2.162451
223.456494	1425.321135	18.404749	-0.042601	2.157285
223.324189	1417.380475	18.409754	-0.042571	2.152075
223.259464	1409.424747	18.414759	-0.042554	2.146848
223.456095	1401.460933	18.419763	-0.042585	2.141628
223.519528	1393.513731	18.424768	-0.042592	2.136393
223.250946	1385.612410	18.429773	-0.042537	2.131144
223.084490	1377.676048	18.434778	-0.042501	2.125869
223.179056	1369.733862	18.439783	-0.042513	2.120602
223.188093	1361.807736	18.444787	-0.042510	2.115324
222.925923	1353.810939	18.449792	-0.042456	2.109959
222.871573	1345.880995	18.454797	-0.042440	2.104646
222.953930	1337.938989	18.459802	-0.042451	2.099324
222.813083	1330.036193	18.464807	-0.042419	2.093994
222.845978	1322.071520	18.469811	-0.042420	2.088625
222.823353	1314.134430	18.474816	-0.042411	2.083255
222.760764	1306.253049	18.479821	-0.042394	2.077906
222.502278	1298.337978	18.484826	-0.042341	2.072500
222.809982	1290.342796	18.489831	-0.042393	2.067082
222.696108	1282.431983	18.494835	-0.042367	2.061665
222.586919	1274.518812	18.499840	-0.042341	2.056233
222.680797	1266.556009	18.504845	-0.042353	2.050772
222.704987	1258.615715	18.509850	-0.042353	2.045306
222.475450	1250.734107	18.514855	-0.042305	2.039840
222.482159	1242.829573	18.519859	-0.042301	2.034367
222.469809	1234.849851	18.524864	-0.042294	2.028825
222.402470	1226.933388	18.529869	-0.042276	2.023306
222.299424	1219.020379	18.534874	-0.042252	2.017771
222.305476	1211.071366	18.539879	-0.042247	2.012207
222.540860	1203.117239	18.544883	-0.042286	2.006648
222.191905	1195.248762	18.549888	-0.042216	2.001072
221.886474	1187.385184	18.554893	-0.042154	1.995489
221.995638	1179.407341	18.559898	-0.042169	1.989853
222.241912	1171.448268	18.564903	-0.042210	1.984229
222.031512	1163.574332	18.569907	-0.042166	1.978601
221.691077	1155.674226	18.574912	-0.042097	1.972924
221.930294	1147.710289	18.579917	-0.042137	1.967247
221.732695	1139.816877	18.584922	-0.042095	1.961557
221.603726	1131.918905	18.589927	-0.042065	1.955855
221.680480	1123.956866	18.594931	-0.042075	1.950113
221.546994	1116.017053	18.599936	-0.042045	1.944346
221.654498	1108.101966	18.604941	-0.042059	1.938607
221.518022	1100.189180	18.609946	-0.042029	1.932825
221.446812	1092.263660	18.614951	-0.042011	1.927024
221.304698	1084.374859	18.619955	-0.041979	1.921225
221.257318	1076.474454	18.624960	-0.041965	1.915410
221.360706	1068.534031	18.629965	-0.041979	1.909564
221.133451	1060.640719	18.634970	-0.041932	1.903699
221.014552	1052.758397	18.639975	-0.041904	1.897835
221.089576	1044.826664	18.644979	-0.041913	1.891939
220.972015	1036.902726	18.649984	-0.041886	1.886008
220.836294	1029.032549	18.654989	-0.041856	1.880096
220.851939	1021.119542	18.659994	-0.041854	1.874151
220.933571	1013.171287	18.664999	-0.041864	1.868168
220.849405	1005.272079	18.670003	-0.041843	1.862184
220.774670	997.376521	18.675008	-0.041824	1.856184
220.853358	989.449640	18.680013	-0.041833	1.850159
220.819391	981.542085	18.685018	-0.041822	1.844116
220.916099	973.650336	18.690023	-0.041835	1.838080
221.067035	965.740364	18.695027	-0.041858	1.832017
220.739282	957.858389	18.700032	-0.041792	1.825899
220.711009	949.978258	18.705037	-0.041781	1.819797
220.556837	942.106247	18.710042	-0.041747	1.813665
220.509845	934.192587	18.715047	-0.041734	1.807494
220.284790	926.336499	18.720051	-0.041687	1.801324
220.316462	918.425601	18.725056	-0.041687	1.795122
220.435944	910.452934	18.730061	-0.041704	1.788860
220.371494	902.564406	18.735066	-0.041687	1.782620
220.285511	894.701555	18.740071	-0.041666	1.776376
220.339413	886.790351	18.745075	-0.041671	1.770088
220.063233	878.937732	18.750080	-0.041615	1.763784
220.022340	871.077842	18.755085	-0.041602	1.757481
219.942949	863.188021	18.760090	-0.041582	1.751126
219.894686	855.292844	18.765095	-0.041568	1.744748
219.834933	847.432373	18.770099	-0.041552	1.738373
219.615635	839.563293	18.775104	-0.041506	1.731947
219.927348	831.620143	18.780109	-0.041559	1.725504
219.576428	823.804209	18.785114	-0.041488	1.719057
219.545651	815.920875	18.790119	-0.041477	1.712571
219.434611	808.031329	18.795123	-0.041451	1.706044
219.453054	800.146141	18.800128	-0.041450	1.699514
219.397519	792.281707	18.805133	-0.041434	1.692965
219.399486	784.388038	18.810138	-0.041430	1.686375
219.266760	776.541852	18.815143	-0.041400	1.679780
219.011431	768.716370	18.820147	-0.041347	1.673160
218.953442	760.819554	18.825152	-0.041331	1.666481
219.133079	752.935362	18.830157	-0.041360	1.659817
219.049042	745.077904	18.835162	-0.041339	1.653113
218.912935	737.217100	18.840167	-0.041308	1.646372
219.003056	729.358107	18.845171	-0.041320	1.639636
219.018023	721.478033	18.850176	-0.041318	1.632843
218.751350	713.603914	18.855181	-0.041263	1.625988
218.657529	705.761340	18.860186	-0.041240	1.619156
218.714314	697.890835	18.865191	-0.041246	1.612291
218.712328	690.030111	18.870195	-0.041240	1.605398
218.572263	682.211115	18.875200	-0.041209	1.598491
218.741522	674.346830	18.880205	-0.041236	1.591559
218.505729	666.516030	18.885210	-0.041187	1.584568
218.416057	658.685591	18.890215	-0.041165	1.577568
218.568716	650.814848	18.895219	-0.041188	1.570535
218.463440	642.984986	18.900224	-0.041164	1.563470
218.476687	635.162252	18.905229	-0.041161	1.556397
218.205745	627.340108	18.910234	-0.041105	1.549250
218.220482	619.488165	18.915239	-0.041103	1.542085
218.143658	611.677119	18.920243	-0.041084	1.534910
217.930109	603.849606	18.925248	-0.041039	1.527666
218.074275	596.006551	18.930253	-0.041061	1.520427
218.042086	588.193499	18.935258	-0.041050	1.513154
217.963133	580.361774	18.940263	-0.041030	1.505822
217.861057	572.564509	18.945267	-0.041006	1.498482
217.917224	564.713612	18.950272	-0.041011	1.491081
217.705386	556.936207	18.955277	-0.040967	1.483670
217.683882	549.131675	18.960282	-0.040958	1.476226
217.752495	541.254154	18.965287	-0.040965	1.468688
217.589497	533.471251	18.970291	-0.040930	1.461167
217.436342	525.690556	18.975296	-0.040896	1.453609
217.415049	517.874625	18.980301	-0.040887	1.446000
217.472829	510.075425	18.985306	-0.040893	1.438379
217.326579	502.297855	18.990311	-0.040861	1.430705
217.395450	494.496164	18.995315	-0.040868	1.423002
217.281545	486.721491	19.000320	-0.040842	1.415253
217.119454	478.956449	19.005325	-0.040807	1.407463
217.292367	471.144738	19.010330	-0.040834	1.399639
217.233627	463.376610	19.015335	-0.040818	1.391776
217.105771	455.605635	19.020339	-0.040789	1.383854
216.911311	447.856026	19.025344	-0.040748	1.375897
216.779358	440.099200	19.030349	-0.040718	1.367896
216.827465	432.320475	19.035354	-0.040722	1.359857
216.494905	424.606799	19.040359	-0.040655	1.351772
216.558794	416.832481	19.045363	-0.040662	1.343643
216.593529	409.068184	19.050368	-0.040664	1.335471
216.513331	401.326483	19.055373	-0.040644	1.327252
216.286466	393.617153	19.060378	-0.040597	1.318990
216.418616	385.767655	19.065383	-0.040616	1.310590
216.409882	377.986104	19.070387	-0.040609	1.302183
216.238379	370.282882	19.075392	-0.040572	1.293778
216.203382	362.561034	19.080397	-0.040561	1.285322
216.212905	354.847911	19.085402	-0.040558	1.276828
216.190621	347.135307	19.090407	-0.040549	1.268272
216.113792	339.445353	19.095411	-0.040529	1.259673
215.943790	331.758552	19.100416	-0.040493	1.251001
216.001318	324.050256	19.105421	-0.040498	1.242287
215.792568	316.397221	19.110426	-0.040454	1.233523
215.773184	308.683454	19.115431	-0.040446	1.224663
215.776296	301.009202	19.120435	-0.040441	1.215790
215.269483	293.391356	19.125440	-0.040342	1.206815
215.332851	285.717165	19.130445	-0.040349	1.197821
215.455348	278.017158	19.135450	-0.040367	1.188740
215.085154	270.415690	19.140455	-0.040293	1.179607
215.186382	262.744356	19.145459	-0.040307	1.170415
215.179290	255.088768	19.150464	-0.040301	1.161147
214.977243	247.478244	19.155469	-0.040258	1.151819
214.715970	239.854059	19.160474	-0.040204	1.142385
214.591688	232.244927	19.165479	-0.040176	1.132921
214.761231	224.591342	19.170483	-0.040203	1.123384
214.464965	217.032199	19.175488	-0.040143	1.113783
214.335413	209.446654	19.180493	-0.040114	1.104103
214.290121	201.863129	19.185498	-0.040100	1.094357
214.023438	194.309884	19.190503	-0.040046	1.084514
213.832546	186.775827	19.195507	-0.040005	1.074623
213.619209	179.213538	19.200512	-0.039961	1.064597
213.311218	171.710767	19.205517	-0.039899	1.054534
212.772405	164.231010	19.210522	-0.039793	1.044350
212.299365	156.762009	19.215527	-0.039701	1.034097
212.139734	149.241001	19.220531	-0.039666	1.023743
211.482417	141.816394	19.225536	-0.039539	1.013298
211.002946	134.369374	19.230541	-0.039445	1.002755
210.692281	126.889712	19.235546	-0.039382	0.992096
210.357071	119.413063	19.240551	-0.039315	0.981318
209.852185	112.007973	19.245555	-0.039216	0.970482
209.627383	104.558934	19.250560	-0.039169	0.959531
209.373861	97.145273	19.255565	-0.039117	0.948498
208.791313	89.795855	19.260570	-0.039004	0.937345
208.214495	82.452044	19.265575	-0.038892	0.926067
208.069810	75.069423	19.270579	-0.038860	0.914708
207.247916	67.786764	19.275584	-0.038702	0.903175
206.801735	60.705175	19.280589	-0.038615	0.891916