Fri Mar 12 13:46:14 2021

Number of Points = 3585
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
6.859171	-0.230903	0.000000	-0.000112	0.722138

6.428279	-0.185529	0.005005	-0.000032	0.722077
6.495172	-0.193546	0.010010	-0.000045	0.722085
6.752101	-0.241997	0.015014	-0.000093	0.722080
6.584526	-0.212913	0.020019	-0.000062	0.722078
6.505174	-0.195923	0.025024	-0.000047	0.722084
6.654624	-0.225474	0.030029	-0.000075	0.722079
6.889816	-0.262624	0.035034	-0.000119	0.722088
6.241953	-0.150126	0.040038	0.000002	0.722083
6.232788	-0.149527	0.045043	0.000003	0.722081
7.059208	-0.293780	0.050048	-0.000150	0.722087
6.581984	-0.213850	0.055053	-0.000062	0.722077
6.673873	-0.228384	0.060058	-0.000079	0.722080
6.779795	-0.380570	0.065062	-0.000099	0.721819
6.848101	-0.427407	0.070067	-0.000111	0.721751
6.459685	-0.356576	0.075072	-0.000039	0.721754
6.240096	-0.321644	0.080077	0.000002	0.721746
6.737499	-0.406402	0.085082	-0.000091	0.721754
6.399053	-0.348519	0.090086	-0.000028	0.721749
6.285441	-0.365421	0.095091	-0.000007	0.721676
7.035874	-0.617571	0.100096	-0.000147	0.721444
6.706629	-0.562079	0.105101	-0.000086	0.721438
6.352946	-0.494256	0.110106	-0.000020	0.721447
6.621712	-0.543941	0.115110	-0.000070	0.721444
6.815871	-0.647030	0.120115	-0.000106	0.721309
6.258746	-0.637316	0.125120	-0.000002	0.721133
5.989786	-0.594659	0.130125	0.000048	0.721123
6.446551	-0.674330	0.135130	-0.000038	0.721127
5.978002	-0.590735	0.140134	0.000050	0.721127
5.883750	-0.673062	0.145139	0.000067	0.720932
6.481790	-0.803400	0.150144	-0.000044	0.720886
6.002865	-0.721923	0.155149	0.000045	0.720878
5.616311	-0.647890	0.160154	0.000117	0.720889
5.934769	-0.803440	0.165158	0.000057	0.720694
6.128408	-0.914256	0.170163	0.000021	0.720544
5.990007	-0.886517	0.175168	0.000047	0.720550
5.893235	-0.873883	0.180173	0.000065	0.720542
6.725856	-1.158844	0.185178	-0.000090	0.720273
5.963257	-1.045272	0.190182	0.000052	0.720229
5.616278	-0.984828	0.195187	0.000116	0.720226
5.456378	-1.047137	0.200192	0.000146	0.720048
5.214633	-1.080823	0.205197	0.000191	0.719897
4.939941	-1.027824	0.210202	0.000242	0.719905
5.002771	-1.040875	0.215206	0.000230	0.719901
5.109184	-1.190408	0.220211	0.000210	0.719644
4.780919	-1.150082	0.225216	0.000271	0.719609
4.603426	-1.123263	0.230221	0.000304	0.719599
4.997813	-1.244220	0.235226	0.000231	0.719500
4.568378	-1.282060	0.240230	0.000311	0.719274
3.705175	-1.131097	0.245235	0.000471	0.719269
3.863762	-1.155305	0.250240	0.000442	0.719277
3.781170	-1.232245	0.255245	0.000457	0.719097
3.094505	-1.175310	0.260250	0.000585	0.718968
2.792228	-1.123611	0.265254	0.000641	0.718964
2.825257	-1.131986	0.270259	0.000635	0.718959
2.659999	-1.111810	0.275264	0.000665	0.718941
1.877479	-1.123481	0.280269	0.000811	0.718643
1.860202	-1.117043	0.285274	0.000814	0.718650
1.864241	-1.121044	0.290278	0.000813	0.718643
1.405009	-1.039253	0.295283	0.000899	0.718644
1.659879	-1.080456	0.300288	0.000851	0.718652
1.564995	-1.170302	0.305293	0.000869	0.718441
1.306915	-1.166432	0.310298	0.000917	0.718358
0.984896	-1.110778	0.315302	0.000977	0.718355
1.160052	-1.145374	0.320307	0.000944	0.718349
1.323021	-1.170527	0.325312	0.000914	0.718356
0.545072	-1.106068	0.330317	0.001058	0.718210
0.276029	-1.154120	0.335322	0.001108	0.718021
0.368286	-1.173752	0.340326	0.001091	0.718015
0.054746	-1.119013	0.345331	0.001149	0.718013
-0.261829	-1.058993	0.350336	0.001208	0.718020
-0.053441	-1.100139	0.355341	0.001169	0.718012
0.151903	-1.208921	0.360346	0.001131	0.717870
-0.239267	-1.224195	0.365350	0.001204	0.717702
-0.100512	-1.249305	0.370355	0.001178	0.717701
-0.150818	-1.238450	0.375360	0.001187	0.717705
-0.916973	-1.107039	0.380365	0.001330	0.717695
-1.202204	-1.051852	0.385370	0.001383	0.717704
-1.395441	-1.134807	0.390374	0.001419	0.717472
-1.631231	-1.141910	0.395379	0.001463	0.717375
-1.695887	-1.125618	0.400384	0.001474	0.717385
-1.827837	-1.108115	0.405389	0.001499	0.717373
-1.760010	-1.114592	0.410394	0.001486	0.717385
-1.926804	-1.087764	0.415398	0.001517	0.717379
-1.856363	-1.099996	0.420403	0.001504	0.717380
-1.698592	-1.253743	0.425408	0.001475	0.717131
-2.192396	-1.191745	0.430413	0.001566	0.717080
-2.260647	-1.173749	0.435418	0.001579	0.717092
-2.048769	-1.214607	0.440422	0.001540	0.717086
-2.137102	-1.200057	0.445427	0.001556	0.717084
-2.526481	-1.129831	0.450432	0.001628	0.717086
-2.643605	-1.278450	0.455437	0.001650	0.716750
-2.825552	-1.242058	0.460442	0.001684	0.716758
-3.254390	-1.166972	0.465446	0.001764	0.716756
-3.558153	-1.114756	0.470451	0.001820	0.716752
-3.362692	-1.145118	0.475456	0.001784	0.716761
-3.727038	-1.082821	0.480461	0.001851	0.716756
-3.823342	-1.114006	0.485466	0.001869	0.716661
-3.705392	-1.241808	0.490470	0.001847	0.716450
-3.769549	-1.231247	0.495475	0.001859	0.716448
-3.860786	-1.213340	0.500480	0.001876	0.716451
-3.630130	-1.258803	0.505485	0.001833	0.716443
-3.639498	-1.252681	0.510490	0.001835	0.716452
-4.162979	-1.216579	0.515494	0.001932	0.716339
-4.323425	-1.292061	0.520499	0.001962	0.716133
-4.251473	-1.302003	0.525504	0.001948	0.716139
-4.400128	-1.279817	0.530509	0.001976	0.716130
-4.859285	-1.195188	0.535514	0.002061	0.716136
-4.914390	-1.188603	0.540518	0.002071	0.716130
-4.899907	-1.232114	0.545523	0.002069	0.716049
-5.503150	-1.205043	0.550528	0.002181	0.715890
-5.457494	-1.216879	0.555533	0.002172	0.715883
-5.402574	-1.223158	0.560538	0.002162	0.715890
-5.539270	-1.200658	0.565542	0.002187	0.715886
-5.438288	-1.221523	0.570547	0.002169	0.715881
-5.332976	-1.242410	0.575552	0.002149	0.715877
-5.862540	-1.315249	0.580557	0.002247	0.715545
-6.482005	-1.201392	0.585562	0.002363	0.715553
-6.646129	-1.173140	0.590566	0.002393	0.715551
-6.608557	-1.180581	0.595571	0.002386	0.715549
-6.767211	-1.149839	0.600576	0.002415	0.715554
-6.904107	-1.128483	0.605581	0.002441	0.715549
-6.721649	-1.157209	0.610586	0.002407	0.715556
-6.957957	-1.261394	0.615590	0.002451	0.715266
-7.360413	-1.206224	0.620595	0.002526	0.715234
-7.075822	-1.254445	0.625600	0.002473	0.715239
-7.491185	-1.184699	0.630605	0.002550	0.715231
-7.691021	-1.145125	0.635610	0.002587	0.715239
-7.682942	-1.147785	0.640614	0.002585	0.715236
-7.246647	-1.232356	0.645619	0.002504	0.715223
-7.572793	-1.329786	0.650624	0.002565	0.714914
-8.258529	-1.212617	0.655629	0.002692	0.714905
-8.417485	-1.181586	0.660634	0.002722	0.714910
-8.423921	-1.180282	0.665638	0.002723	0.714911
-8.570827	-1.157179	0.670643	0.002750	0.714905
-8.358245	-1.191788	0.675648	0.002710	0.714911
-8.411932	-1.185095	0.680653	0.002720	0.714906
-8.717536	-1.276676	0.685658	0.002777	0.714616
-8.515884	-1.314332	0.690662	0.002740	0.714613
-8.594298	-1.303389	0.695667	0.002754	0.714607
-8.681814	-1.284457	0.700672	0.002770	0.714614
-8.898065	-1.248840	0.705677	0.002811	0.714608
-9.053056	-1.218634	0.710682	0.002839	0.714613
-9.043491	-1.378247	0.715686	0.002838	0.714300
-9.722322	-1.268231	0.720691	0.002964	0.714278
-9.730439	-1.262817	0.725696	0.002965	0.714286
-9.768834	-1.261596	0.730701	0.002972	0.714275
-9.769576	-1.257457	0.735706	0.002972	0.714284
-9.888927	-1.237334	0.740710	0.002994	0.714281
-9.705353	-1.358785	0.745715	0.002960	0.714105
-10.100934	-1.352408	0.750720	0.003034	0.713978
-10.502785	-1.284819	0.755725	0.003109	0.713970
-10.330882	-1.313562	0.760730	0.003076	0.713974
-10.393191	-1.303483	0.765734	0.003088	0.713972
-10.489994	-1.288397	0.770739	0.003106	0.713968
-10.702877	-1.317854	0.775744	0.003145	0.713834
-10.966500	-1.363263	0.780749	0.003195	0.713651
-10.896082	-1.372709	0.785754	0.003181	0.713657
-11.343097	-1.295264	0.790758	0.003264	0.713653
-11.575411	-1.253835	0.795763	0.003308	0.713653
-11.393716	-1.284756	0.800768	0.003274	0.713656
-11.575769	-1.258327	0.805773	0.003307	0.713645
-11.504220	-1.414007	0.810778	0.003294	0.713360
-11.490289	-1.415195	0.815782	0.003292	0.713363
-11.738185	-1.373657	0.820787	0.003338	0.713358
-11.468168	-1.419923	0.825792	0.003287	0.713362
-11.639348	-1.393701	0.830797	0.003319	0.713354
-11.607900	-1.491030	0.835802	0.003313	0.713171
-12.083823	-1.480483	0.840806	0.003402	0.713024
-12.118540	-1.476612	0.845811	0.003408	0.713019
-12.141800	-1.466429	0.850816	0.003412	0.713031
-12.707646	-1.370591	0.855821	0.003517	0.713022
-12.890873	-1.339318	0.860826	0.003551	0.713019
-12.919525	-1.487717	0.865830	0.003557	0.712714
-13.098169	-1.459612	0.870835	0.003590	0.712706
-13.306848	-1.417570	0.875840	0.003629	0.712716
-13.219500	-1.438975	0.880845	0.003612	0.712705
-13.122240	-1.452621	0.885850	0.003594	0.712712
-13.251447	-1.459156	0.890854	0.003618	0.712654
-13.380539	-1.573357	0.895859	0.003642	0.712380
-13.626339	-1.524742	0.900864	0.003688	0.712390
-13.986605	-1.465055	0.905869	0.003755	0.712381
-13.977317	-1.464164	0.910874	0.003753	0.712387
-13.985299	-1.463017	0.915878	0.003754	0.712386
-14.078127	-1.528358	0.920883	0.003772	0.712223
-14.380928	-1.540247	0.925888	0.003828	0.712092
-14.570567	-1.509786	0.930893	0.003863	0.712086
-14.776785	-1.469987	0.935898	0.003901	0.712092
-14.920219	-1.445252	0.940902	0.003928	0.712090
-15.048398	-1.425743	0.945907	0.003952	0.712084
-14.907321	-1.526539	0.950912	0.003926	0.711933
-15.278481	-1.550293	0.955917	0.003995	0.711754
-15.524337	-1.503197	0.960922	0.004040	0.711761
-15.480686	-1.510233	0.965926	0.004032	0.711763
-15.718032	-1.471346	0.970931	0.004076	0.711756
-16.032572	-1.409584	0.975936	0.004135	0.711768
-16.347553	-1.359526	0.980941	0.004193	0.711756
-16.394196	-1.492500	0.985946	0.004202	0.711474
-16.525830	-1.478397	0.990950	0.004226	0.711456
-16.572640	-1.473617	0.995955	0.004235	0.711449
-16.185220	-1.539016	1.000960	0.004163	0.711456
-16.298446	-1.522205	1.005965	0.004184	0.711449
-16.413840	-1.499766	1.010970	0.004205	0.711453
-16.289391	-1.613961	1.015974	0.004182	0.711270
-16.463655	-1.652532	1.020979	0.004214	0.711131
-16.588259	-1.624931	1.025984	0.004237	0.711142
-16.933342	-1.567468	1.030989	0.004302	0.711134
-16.634823	-1.616636	1.035994	0.004246	0.711142
-16.764308	-1.645029	1.040998	0.004270	0.711040
-17.135973	-1.665797	1.046003	0.004339	0.710866
-16.890231	-1.703882	1.051008	0.004293	0.710878
-17.481832	-1.602564	1.056013	0.004403	0.710870
-17.710270	-1.559159	1.061018	0.004446	0.710875
-18.138004	-1.482508	1.066022	0.004525	0.710876
-18.175854	-1.628318	1.071027	0.004532	0.710572
-17.902465	-1.693959	1.076032	0.004481	0.710538
-18.245605	-1.635663	1.081037	0.004545	0.710533
-18.216294	-1.639950	1.086042	0.004540	0.710535
-18.242834	-1.633854	1.091046	0.004544	0.710538
-18.133068	-1.712064	1.096051	0.004524	0.710421
-18.295806	-1.782287	1.101056	0.004554	0.710223
-18.634906	-1.726349	1.106061	0.004617	0.710214
-19.005972	-1.657567	1.111066	0.004686	0.710219
-18.836007	-1.686608	1.116070	0.004654	0.710222
-19.063682	-1.648730	1.121075	0.004697	0.710217
-19.106609	-1.796106	1.126080	0.004705	0.709907
-19.794345	-1.679243	1.131085	0.004833	0.709896
-19.869296	-1.664833	1.136090	0.004847	0.709898
-19.760753	-1.683710	1.141094	0.004826	0.709899
-19.895758	-1.663712	1.146099	0.004851	0.709891
-19.797516	-1.686647	1.151104	0.004833	0.709880
-20.226979	-1.751870	1.156109	0.004913	0.709597
-20.205618	-1.753766	1.161114	0.004909	0.709601
-20.112361	-1.769880	1.166118	0.004891	0.709602
-20.733428	-1.662474	1.171123	0.005007	0.709596
-20.833637	-1.639856	1.176128	0.005025	0.709606
-21.010008	-1.623877	1.181133	0.005058	0.709575
-21.488970	-1.691094	1.186138	0.005147	0.709270
-21.471405	-1.693601	1.191142	0.005144	0.709271
-21.642013	-1.666239	1.196147	0.005176	0.709265
-21.308828	-1.721643	1.201152	0.005114	0.709273
-21.622807	-1.670913	1.206157	0.005172	0.709263
-21.452470	-1.699439	1.211162	0.005140	0.709267
-21.806235	-1.703470	1.216166	0.005206	0.709133
-22.270883	-1.709753	1.221171	0.005292	0.708954
-21.965959	-1.759889	1.226176	0.005235	0.708963
-22.214973	-1.720110	1.231181	0.005282	0.708954
-22.186361	-1.722755	1.236186	0.005276	0.708959
-22.253436	-1.709515	1.241190	0.005289	0.708962
-22.426877	-1.726905	1.246195	0.005321	0.708865
-22.365055	-1.848806	1.251200	0.005309	0.708643
-22.711149	-1.791487	1.256205	0.005374	0.708635
-22.725534	-1.787132	1.261210	0.005376	0.708639
-22.646792	-1.800311	1.266214	0.005362	0.708640
-22.831008	-1.770480	1.271219	0.005396	0.708635
-22.639405	-1.889920	1.276224	0.005360	0.708464
-23.152229	-1.857574	1.281229	0.005456	0.708346
-22.743066	-1.928983	1.286234	0.005379	0.708349
-22.974993	-1.885077	1.291238	0.005422	0.708354
-23.064028	-1.872987	1.296243	0.005439	0.708347
-23.616403	-1.884478	1.301248	0.005542	0.708127
-23.971916	-1.879166	1.306253	0.005608	0.708010
-24.156414	-1.845816	1.311258	0.005642	0.708011
-23.965899	-1.878801	1.316262	0.005606	0.708014
-24.379056	-1.808900	1.321267	0.005683	0.708006
-24.218549	-1.832020	1.326272	0.005653	0.708017
-24.545181	-1.911478	1.331277	0.005714	0.707742
-24.735492	-1.898534	1.336282	0.005749	0.707700
-24.705899	-1.904549	1.341286	0.005744	0.707698
-24.933632	-1.865049	1.346291	0.005786	0.707696
-24.833200	-1.878438	1.351296	0.005767	0.707705
-24.906031	-1.880439	1.356301	0.005781	0.707676
-25.137932	-1.988148	1.361306	0.005824	0.707377
-25.151455	-1.983133	1.366310	0.005826	0.707382
-25.650368	-1.898290	1.371315	0.005919	0.707374
-25.522039	-1.918093	1.376320	0.005895	0.707380
-25.814562	-1.869649	1.381325	0.005950	0.707373
-25.869153	-1.915613	1.386330	0.005960	0.707262
-26.209082	-1.942900	1.391334	0.006023	0.707085
-26.331423	-1.923077	1.396339	0.006046	0.707081
-26.189054	-1.944802	1.401344	0.006019	0.707089
-26.548866	-1.883700	1.406349	0.006086	0.707083
-26.394534	-1.909189	1.411354	0.006057	0.707087
-26.085695	-2.038297	1.416358	0.006000	0.706939
-26.688652	-2.023826	1.421363	0.006112	0.706752
-26.822127	-1.996227	1.426368	0.006137	0.706760
-26.898218	-1.984880	1.431373	0.006151	0.706756
-26.700790	-2.020618	1.436378	0.006114	0.706755
-26.667297	-2.053674	1.441382	0.006108	0.706700
-27.168140	-2.093186	1.446387	0.006201	0.706442
-27.248872	-2.075844	1.451392	0.006216	0.706448
-27.715973	-1.995107	1.456397	0.006302	0.706443
-27.862704	-1.967982	1.461402	0.006330	0.706445
-27.777600	-1.983504	1.466406	0.006314	0.706445
-27.992015	-2.040978	1.471411	0.006354	0.706252
-28.142298	-2.072277	1.476416	0.006382	0.706136
-28.445482	-2.021572	1.481421	0.006438	0.706129
-28.664898	-1.981723	1.486426	0.006479	0.706131
-28.446201	-2.019312	1.491430	0.006438	0.706134
-28.582725	-1.998199	1.496435	0.006463	0.706128
-28.531862	-2.088711	1.501440	0.006454	0.705964
-28.964784	-2.062382	1.506445	0.006534	0.705862
-29.050202	-2.045993	1.511450	0.006550	0.705864
-28.858025	-2.077497	1.516454	0.006514	0.705870
-29.047269	-2.048498	1.521459	0.006549	0.705861
-29.138068	-2.045004	1.526464	0.006566	0.705835
-29.346411	-2.161780	1.531469	0.006605	0.705526
-29.733625	-2.092870	1.536474	0.006677	0.705526
-29.802446	-2.078509	1.541478	0.006690	0.705530
-30.136155	-2.023831	1.546483	0.006752	0.705521
-29.854329	-2.071009	1.551488	0.006699	0.705527
-30.016860	-2.084974	1.556493	0.006729	0.705441
-30.852588	-2.052014	1.561498	0.006885	0.705207
-30.468032	-2.116849	1.566502	0.006813	0.705215
-30.779666	-2.066840	1.571507	0.006871	0.705204
-30.851046	-2.048224	1.576512	0.006884	0.705216
-30.809521	-2.058807	1.581517	0.006876	0.705210
-30.708334	-2.093248	1.586522	0.006858	0.705177
-30.833423	-2.213283	1.591526	0.006881	0.704890
-31.278005	-2.137630	1.596531	0.006964	0.704883
-30.956572	-2.189937	1.601536	0.006904	0.704894
-31.024219	-2.180824	1.606541	0.006916	0.704888
-31.216429	-2.146444	1.611546	0.006952	0.704888
-31.421609	-2.206697	1.616550	0.006990	0.704693
-31.665625	-2.216773	1.621555	0.007035	0.704585
-31.654747	-2.213562	1.626560	0.007033	0.704596
-31.995882	-2.156582	1.631565	0.007097	0.704588
-32.133235	-2.132949	1.636570	0.007122	0.704587
-32.225969	-2.131447	1.641574	0.007139	0.704557
-32.718674	-2.193322	1.646579	0.007231	0.704255
-32.815627	-2.171973	1.651584	0.007249	0.704264
-32.700354	-2.194734	1.656589	0.007227	0.704259
-32.741097	-2.186775	1.661594	0.007235	0.704261
-32.573117	-2.213899	1.666598	0.007204	0.704267
-32.580757	-2.256829	1.671603	0.007205	0.704178
-32.896835	-2.309748	1.676608	0.007264	0.703957
-33.527455	-2.199524	1.681613	0.007381	0.703953
-33.536978	-2.198525	1.686618	0.007383	0.703952
-33.606755	-2.184190	1.691622	0.007396	0.703956
-33.794804	-2.154149	1.696627	0.007430	0.703949
-33.138391	-2.340717	1.701632	0.007308	0.703809
-33.703760	-2.326927	1.706637	0.007413	0.703633
-33.977026	-2.276932	1.711642	0.007464	0.703636
-34.065553	-2.259448	1.716646	0.007481	0.703640
-34.092693	-2.259021	1.721651	0.007486	0.703631
-33.740038	-2.339150	1.726656	0.007420	0.703596
-34.420757	-2.343587	1.731661	0.007547	0.703343
-34.700926	-2.292902	1.736666	0.007599	0.703344
-34.826462	-2.268549	1.741670	0.007622	0.703348
-34.952120	-2.249705	1.746675	0.007645	0.703341
-34.683367	-2.293873	1.751680	0.007595	0.703349
-34.625048	-2.401851	1.756685	0.007584	0.703152
-35.737042	-2.273931	1.761690	0.007791	0.703010
-35.783314	-2.264678	1.766694	0.007800	0.703013
-35.464165	-2.325990	1.771699	0.007740	0.703004
-35.362123	-2.340901	1.776704	0.007721	0.703011
-35.603877	-2.300890	1.781709	0.007766	0.703005
-35.693816	-2.407495	1.786714	0.007783	0.702757
-35.978500	-2.384127	1.791718	0.007836	0.702702
-36.438366	-2.307619	1.796723	0.007921	0.702691
-36.331435	-2.322400	1.801728	0.007901	0.702700
-36.078718	-2.368466	1.806733	0.007854	0.702698
-36.275626	-2.356110	1.811738	0.007891	0.702652
-36.743024	-2.408476	1.816742	0.007978	0.702378
-37.056078	-2.358798	1.821747	0.008036	0.702366
-36.887774	-2.383984	1.826752	0.008004	0.702376
-36.967560	-2.371227	1.831757	0.008019	0.702373
-37.341947	-2.305825	1.836762	0.008089	0.702370
-37.168107	-2.356668	1.841766	0.008056	0.702330
-37.994637	-2.337251	1.846771	0.008210	0.702072
-37.744457	-2.378196	1.851776	0.008163	0.702079
-37.765201	-2.376970	1.856781	0.008167	0.702074
-38.028214	-2.331618	1.861786	0.008216	0.702071
-37.992872	-2.334564	1.866790	0.008209	0.702078
-37.860607	-2.362550	1.871795	0.008185	0.702070
-38.177739	-2.457792	1.876800	0.008244	0.701763
-39.099207	-2.302240	1.881805	0.008415	0.701745
-39.355837	-2.257947	1.886810	0.008463	0.701742
-38.888351	-2.338377	1.891814	0.008376	0.701748
-38.838292	-2.351741	1.896819	0.008366	0.701740
-38.935931	-2.329975	1.901824	0.008384	0.701749
-38.841220	-2.376913	1.906829	0.008367	0.701688
-39.420554	-2.397359	1.911834	0.008475	0.701438
-39.557965	-2.368232	1.916838	0.008500	0.701447
-40.112498	-2.275790	1.921843	0.008603	0.701434
-39.504502	-2.379081	1.926848	0.008490	0.701445
-39.676731	-2.351649	1.931853	0.008522	0.701438
-39.728001	-2.345323	1.936858	0.008531	0.701433
-39.650643	-2.465286	1.941862	0.008517	0.701218
-40.814113	-2.305761	1.946867	0.008733	0.701121
-40.876925	-2.290362	1.951872	0.008745	0.701130
-40.263804	-2.402202	1.956877	0.008631	0.701125
-40.681285	-2.328105	1.961882	0.008708	0.701124
-40.712501	-2.319497	1.966886	0.008714	0.701131
-40.530863	-2.357400	1.971891	0.008680	0.701120
-40.720232	-2.436606	1.976896	0.008716	0.700891
-41.609693	-2.284660	1.981901	0.008881	0.700877
-41.840646	-2.245058	1.986906	0.008924	0.700874
-40.837680	-2.419715	1.991910	0.008737	0.700883
-41.182984	-2.362533	1.996915	0.008801	0.700874
-41.245307	-2.372796	2.001920	0.008813	0.700831

-42.232410	-2.341225	2.011917	0.008996	0.700539
-42.200071	-2.348539	2.021914	0.008990	0.700536
-42.258484	-2.338358	2.031910	0.009001	0.700536
-42.074995	-2.370737	2.041907	0.008967	0.700537
-42.326337	-2.324686	2.051904	0.009013	0.700540
-42.316305	-2.327444	2.061901	0.009011	0.700538
-42.272109	-2.336794	2.071898	0.009003	0.700535
-42.419031	-2.310753	2.081894	0.009030	0.700535
-42.025179	-2.379450	2.091891	0.008957	0.700539
-42.260107	-2.337175	2.101888	0.009000	0.700540
-41.628391	-2.362651	2.111885	0.008882	0.700717
-41.395750	-2.325810	2.121882	0.008839	0.700876
-41.325822	-2.338400	2.131878	0.008826	0.700876
-41.303081	-2.340916	2.141875	0.008821	0.700879
-41.291376	-2.341774	2.151872	0.008819	0.700882
-41.205683	-2.358062	2.161869	0.008803	0.700881
-41.356224	-2.293148	2.171866	0.008831	0.700958
-40.574556	-2.351712	2.181862	0.008685	0.701122
-40.525831	-2.360328	2.191859	0.008676	0.701122
-40.714032	-2.324920	2.201856	0.008711	0.701127
-40.687194	-2.297064	2.211853	0.008705	0.701193
-39.968610	-2.303391	2.221850	0.008571	0.701440
-39.829847	-2.329683	2.231846	0.008545	0.701437
-39.853332	-2.323377	2.241843	0.008550	0.701442
-39.407017	-2.324318	2.251840	0.008466	0.701601
-38.820735	-2.355451	2.261837	0.008357	0.701750
-39.317535	-2.268568	2.271834	0.008449	0.701747
-38.868808	-2.349861	2.281830	0.008366	0.701745
-38.470155	-2.274422	2.291827	0.008291	0.702041
-38.018588	-2.337944	2.301824	0.008207	0.702076
-37.839783	-2.369019	2.311821	0.008174	0.702078
-38.060980	-2.296232	2.321818	0.008215	0.702146
-37.127186	-2.349565	2.331814	0.008041	0.702375
-37.651174	-2.256061	2.341811	0.008138	0.702375
-37.516369	-2.278903	2.351808	0.008113	0.702378
-36.671597	-2.272735	2.361805	0.007955	0.702695
-36.644330	-2.275822	2.371802	0.007950	0.702699
-36.494037	-2.304480	2.381798	0.007922	0.702696
-36.620074	-2.177373	2.391795	0.007945	0.702908
-35.736803	-2.282243	2.401792	0.007780	0.703014
-36.147468	-2.210922	2.411789	0.007857	0.703011
-35.489490	-2.207452	2.421786	0.007734	0.703255
-34.871491	-2.273278	2.431782	0.007619	0.703345
-35.098883	-2.232043	2.441779	0.007661	0.703346
-34.565309	-2.286178	2.451776	0.007562	0.703430
-34.480830	-2.197344	2.461773	0.007546	0.703640
-34.890563	-2.124335	2.471770	0.007622	0.703640
-34.307074	-2.167711	2.481766	0.007513	0.703762
-33.786030	-2.166308	2.491763	0.007416	0.703953
-33.345810	-2.244565	2.501760	0.007334	0.703954
-33.461998	-2.173360	2.511757	0.007355	0.704056
-33.011496	-2.152050	2.521754	0.007271	0.704261
-33.029210	-2.148314	2.531750	0.007274	0.704263
-32.990509	-2.090316	2.541747	0.007267	0.704394
-32.380911	-2.101661	2.551744	0.007153	0.704590
-32.271697	-2.120011	2.561741	0.007133	0.704593
-32.084734	-2.071304	2.571738	0.007098	0.704758
-31.824793	-2.053515	2.581734	0.007049	0.704888
-31.783836	-2.060354	2.591731	0.007041	0.704889
-31.275827	-2.016329	2.601728	0.006946	0.705160
-31.009921	-2.037299	2.611725	0.006897	0.705214
-31.167828	-1.995215	2.621722	0.006926	0.705242
-30.581853	-1.957405	2.631718	0.006817	0.705529
-30.407239	-1.989119	2.641715	0.006784	0.705528
-30.105005	-1.980114	2.651712	0.006728	0.705655
-29.763083	-1.937102	2.661709	0.006664	0.705864
-29.808143	-1.928995	2.671706	0.006672	0.705865
-29.618560	-1.869988	2.681702	0.006636	0.706052
-28.854889	-1.965503	2.691699	0.006494	0.706134
-28.906974	-1.955328	2.701696	0.006504	0.706136
-28.553414	-1.875115	2.711693	0.006438	0.706424
-28.447999	-1.881736	2.721690	0.006418	0.706449
-28.511212	-1.827416	2.731686	0.006429	0.706536
-27.980161	-1.810858	2.741683	0.006330	0.706760
-27.720843	-1.857942	2.751680	0.006282	0.706758
-27.558032	-1.778470	2.761677	0.006251	0.706976
-27.086249	-1.808735	2.771674	0.006163	0.707085
-27.058829	-1.809500	2.781670	0.006158	0.707093
-26.550918	-1.758152	2.791667	0.006063	0.707378
-26.375321	-1.786806	2.801664	0.006030	0.707384
-26.299273	-1.743460	2.811661	0.006016	0.707499
-25.860122	-1.719437	2.821658	0.005934	0.707704
-26.000304	-1.695038	2.831654	0.005960	0.707703
-25.333126	-1.690541	2.841651	0.005836	0.707951
-24.760938	-1.759903	2.851648	0.005729	0.708017
-24.987223	-1.719223	2.861645	0.005771	0.708018
-24.496366	-1.652820	2.871642	0.005679	0.708327
-24.457298	-1.649100	2.881638	0.005672	0.708348
-24.389736	-1.627564	2.891635	0.005659	0.708416
-23.766396	-1.623780	2.901632	0.005543	0.708646
-23.952269	-1.591084	2.911629	0.005577	0.708646
-23.580892	-1.554764	2.921626	0.005508	0.708851
-23.192582	-1.571047	2.931622	0.005436	0.708958
-23.056222	-1.587390	2.941619	0.005410	0.708974
-22.856789	-1.476561	2.951616	0.005373	0.709267
-22.632452	-1.515100	2.961613	0.005331	0.709270
-22.237244	-1.492501	2.971610	0.005257	0.709457
-21.898362	-1.481289	2.981606	0.005194	0.709600
-21.646537	-1.527343	2.991603	0.005147	0.709598
-21.631202	-1.401979	3.001600	0.005144	0.709855
-21.405386	-1.419711	3.011597	0.005101	0.709900
-20.910456	-1.449944	3.021594	0.005009	0.710016
-20.490972	-1.421437	3.031590	0.004931	0.710223
-20.495672	-1.421423	3.041587	0.004931	0.710222
-20.199751	-1.374620	3.051584	0.004876	0.710421
-20.048669	-1.342199	3.061581	0.004848	0.710540
-19.961214	-1.343740	3.071578	0.004831	0.710568
-19.658249	-1.244675	3.081574	0.004775	0.710874
-19.283557	-1.311527	3.091571	0.004705	0.710874
-19.069793	-1.276180	3.101568	0.004665	0.711021
-18.783498	-1.265490	3.111565	0.004611	0.711145
-18.871041	-1.229921	3.121562	0.004627	0.711185
-18.141489	-1.224088	3.131558	0.004491	0.711456
-17.917853	-1.264450	3.141555	0.004450	0.711456
-17.964102	-1.182863	3.151552	0.004458	0.711602
-17.364608	-1.208646	3.161549	0.004346	0.711764
-17.080457	-1.260535	3.171546	0.004293	0.711762
-16.932819	-1.145440	3.181542	0.004266	0.712044
-16.633463	-1.175884	3.191539	0.004210	0.712090
-16.556968	-1.155516	3.201536	0.004195	0.712158
-16.144598	-1.112423	3.211533	0.004118	0.712391
-16.115253	-1.119733	3.221530	0.004113	0.712387
-15.770913	-1.074328	3.231526	0.004048	0.712600
-15.412025	-1.082077	3.241523	0.003981	0.712712
-15.004844	-1.153570	3.251520	0.003905	0.712714
-14.692722	-1.063658	3.261517	0.003847	0.713004
-14.567235	-1.076437	3.271514	0.003824	0.713024
-14.611211	-1.035186	3.281510	0.003832	0.713091
-14.453935	-0.929351	3.291507	0.003802	0.713357
-13.816959	-1.042412	3.301504	0.003683	0.713359
-13.550127	-0.996756	3.311501	0.003633	0.713544
-13.258229	-0.995082	3.321498	0.003579	0.713651
-13.280311	-0.991817	3.331494	0.003583	0.713650
-13.107514	-0.873775	3.341491	0.003550	0.713946
-12.746308	-0.926413	3.351488	0.003483	0.713970
-12.575676	-0.892637	3.361485	0.003451	0.714098
-11.876496	-0.925913	3.371482	0.003321	0.714280
-11.715198	-0.955477	3.381478	0.003291	0.714278
-11.577677	-0.886931	3.391475	0.003265	0.714463
-11.413139	-0.840610	3.401472	0.003234	0.714614
-11.397608	-0.844677	3.411469	0.003231	0.714612
-11.146059	-0.743369	3.421466	0.003184	0.714902
-11.095734	-0.748792	3.431462	0.003174	0.714909
-10.724596	-0.720756	3.441459	0.003105	0.715097
-10.164553	-0.749943	3.451456	0.003001	0.715237
-10.082729	-0.755539	3.461453	0.002985	0.715255
-9.816756	-0.654455	3.471450	0.002935	0.715550
-9.782354	-0.661688	3.481446	0.002929	0.715548
-9.149317	-0.673476	3.491443	0.002811	0.715748
-8.780682	-0.666524	3.501440	0.002742	0.715893
-9.045385	-0.617951	3.511437	0.002791	0.715896
-8.275188	-0.633293	3.521434	0.002648	0.716138
-8.185051	-0.650099	3.531430	0.002631	0.716137
-7.738940	-0.689372	3.541427	0.002547	0.716216
-7.509630	-0.610592	3.551424	0.002504	0.716454
-7.277650	-0.652153	3.561421	0.002461	0.716454
-7.159002	-0.591394	3.571418	0.002439	0.716616
-6.951853	-0.556923	3.581414	0.002400	0.716758
-6.751165	-0.591566	3.591411	0.002363	0.716760
-6.483218	-0.485765	3.601408	0.002312	0.717064
-6.358880	-0.495984	3.611405	0.002289	0.717088
-5.783138	-0.540392	3.621402	0.002182	0.717204
-5.549054	-0.491175	3.631398	0.002138	0.717384
-5.174174	-0.558226	3.641395	0.002068	0.717383
-5.070084	-0.488280	3.651392	0.002048	0.717559
-4.981070	-0.429464	3.661389	0.002032	0.717707
-4.813156	-0.460955	3.671386	0.002000	0.717704
-4.758743	-0.320585	3.681382	0.001990	0.718001
-4.306055	-0.392554	3.691379	0.001905	0.718018
-4.083208	-0.344905	3.701376	0.001864	0.718191
-3.893793	-0.295000	3.711373	0.001828	0.718357
-3.472792	-0.370103	3.721370	0.001750	0.718357
-3.454291	-0.227273	3.731366	0.001746	0.718646
-2.923996	-0.320336	3.741363	0.001647	0.718649
-2.997750	-0.221206	3.751360	0.001661	0.718819
-1.788355	-0.360607	3.761357	0.001435	0.718969
-1.468429	-0.419408	3.771354	0.001376	0.718966
-1.454380	-0.365269	3.781350	0.001373	0.719078
-1.447012	-0.267021	3.791347	0.001371	0.719274
-1.389316	-0.276108	3.801344	0.001360	0.719277
-1.181444	-0.212114	3.811341	0.001322	0.719477
-1.103125	-0.160500	3.821338	0.001307	0.719606
-0.756593	-0.211631	3.831334	0.001242	0.719627
-0.386285	-0.137332	3.841331	0.001173	0.719904
0.000000	-0.121140	3.851328	0.001101	0.720072

0.204072	0.470092	3.856333	0.001062	0.721307
2.894173	1.281061	3.861338	0.000561	0.723840
9.844677	1.992843	3.866342	-0.000734	0.727649
21.072613	2.639781	3.871347	-0.002825	0.732786
35.122204	3.471011	3.876352	-0.005442	0.739201
51.589557	4.529563	3.881357	-0.008509	0.746804
71.870934	5.625119	3.886362	-0.012286	0.755665
96.077651	6.723091	3.891366	-0.016794	0.765708
122.645344	8.137041	3.896371	-0.021742	0.776948
155.711666	9.172094	3.901376	-0.027900	0.789398
177.455555	12.935336	3.906381	-0.031951	0.802910
184.186456	19.780694	3.911386	-0.033209	0.816924
188.980896	27.213158	3.916390	-0.034106	0.831113
192.567280	35.015713	3.921395	-0.034779	0.845324
196.955730	42.854731	3.926400	-0.035602	0.859589
202.377935	50.665036	3.931405	-0.036616	0.873866
207.731275	58.644577	3.936410	-0.037618	0.888160
211.002285	67.146687	3.941414	-0.038233	0.902469
212.250397	76.058543	3.946419	-0.038471	0.916637
213.249496	85.040937	3.951424	-0.038663	0.930630
213.803734	94.117033	3.956429	-0.038773	0.944438
214.529207	103.181112	3.961434	-0.038914	0.958074
215.219947	112.250979	3.966438	-0.039048	0.971517
215.961195	121.313948	3.971443	-0.039192	0.984779
216.543533	130.430352	3.976448	-0.039307	0.997901
217.334685	139.449705	3.981453	-0.039460	1.010767
217.930437	148.494845	3.986458	-0.039577	1.023460
218.537191	157.525822	3.991462	-0.039696	1.035980
220.524770	166.290042	3.996467	-0.040072	1.048313
221.537183	175.252149	4.001472	-0.040266	1.060540
222.314520	184.232739	4.006477	-0.040417	1.072598
223.687401	193.069999	4.011482	-0.040678	1.084469
224.387227	202.017591	4.016486	-0.040815	1.096203
224.994078	210.934394	4.021491	-0.040933	1.107754
225.864816	219.794079	4.026496	-0.041101	1.119169
226.641559	228.633502	4.031501	-0.041252	1.130424
227.599621	237.428031	4.036506	-0.041436	1.141550
228.979767	246.161982	4.041510	-0.041699	1.152582
229.697564	254.937922	4.046515	-0.041838	1.163423
230.639419	263.669721	4.051520	-0.042019	1.174156
231.329025	272.401135	4.056525	-0.042154	1.184740
232.056280	281.109298	4.061530	-0.042295	1.195209
232.814745	289.785655	4.066534	-0.042442	1.205557
233.481411	298.461744	4.071539	-0.042572	1.215798
234.623641	307.037375	4.076544	-0.042790	1.225930
235.602828	315.645853	4.081549	-0.042978	1.235984
236.138182	324.263844	4.086554	-0.043083	1.245882
236.899445	332.851655	4.091558	-0.043231	1.255712
237.962196	341.335418	4.096563	-0.043434	1.265405
238.660385	349.905168	4.101568	-0.043570	1.275051
239.269975	358.436182	4.106573	-0.043689	1.284565
239.893945	366.960626	4.111578	-0.043811	1.294005
240.809965	375.420271	4.116582	-0.043987	1.303359
241.393618	384.011402	4.121587	-0.044101	1.312727
241.985916	392.512851	4.126592	-0.044217	1.321935
242.902952	400.899298	4.131597	-0.044394	1.331014
243.529084	409.329868	4.136602	-0.044516	1.340027
244.178978	417.745651	4.141606	-0.044642	1.348967
244.628286	426.179391	4.146611	-0.044732	1.357833
245.129869	434.580784	4.151616	-0.044831	1.366616
245.591194	442.994624	4.156621	-0.044922	1.375349
246.251910	451.349806	4.161626	-0.045051	1.384001
246.980014	459.725900	4.166630	-0.045192	1.392631
247.459772	468.082724	4.171635	-0.045287	1.401147
247.717189	476.483349	4.176640	-0.045340	1.409618
248.507317	484.788225	4.181645	-0.045493	1.418031
249.296348	493.077328	4.186650	-0.045645	1.426378
249.803364	501.446000	4.191654	-0.045745	1.434709
250.235685	509.763304	4.196659	-0.045831	1.442929
250.839258	518.067138	4.201664	-0.045949	1.451117
251.276315	526.393460	4.206669	-0.046036	1.459254
251.672239	534.705446	4.211674	-0.046115	1.467325
252.453352	543.018828	4.216678	-0.046266	1.475414
253.333040	551.214826	4.221683	-0.046435	1.483362
253.834050	559.517894	4.226688	-0.046534	1.491310
254.296025	567.805958	4.231693	-0.046625	1.499196
254.544549	576.112556	4.236698	-0.046677	1.507024
254.883374	584.435457	4.241702	-0.046746	1.514842
255.443253	592.655976	4.246707	-0.046856	1.522557
256.508795	600.828683	4.251712	-0.047059	1.530265
257.032317	609.084741	4.256717	-0.047162	1.537930
257.320886	617.365145	4.261722	-0.047222	1.545544
257.965937	625.622574	4.266726	-0.047347	1.553152
258.507393	633.836975	4.271731	-0.047453	1.560668
258.961596	642.084761	4.276736	-0.047543	1.568166
259.499373	650.325123	4.281741	-0.047649	1.575633
259.736293	658.578686	4.286746	-0.047699	1.583034
260.208623	666.819963	4.291750	-0.047792	1.590423
260.422496	675.078872	4.296755	-0.047837	1.597756
261.104181	683.251563	4.301760	-0.047970	1.605046
261.386649	691.501032	4.306765	-0.048028	1.612314
261.679538	699.737109	4.311770	-0.048088	1.619539
262.152325	707.930069	4.316774	-0.048181	1.626719
262.580492	716.183942	4.321779	-0.048266	1.633914
263.025912	724.359109	4.326784	-0.048355	1.641012
263.538489	732.523377	4.331789	-0.048455	1.648079
263.809909	740.733234	4.336794	-0.048511	1.655122
264.183982	748.925835	4.341798	-0.048586	1.662134
264.414720	757.126862	4.346803	-0.048635	1.669105
264.912527	765.304561	4.351808	-0.048733	1.676062
265.414556	773.451278	4.356813	-0.048832	1.682965
265.640966	781.654051	4.361818	-0.048879	1.689850
265.921333	789.867386	4.366822	-0.048937	1.696723
266.246635	798.027086	4.371827	-0.049003	1.703530
266.555395	806.227330	4.376832	-0.049066	1.710340
266.880030	814.412860	4.381837	-0.049132	1.717114
267.432797	822.531675	4.386842	-0.049240	1.723835
267.884862	830.694548	4.391846	-0.049330	1.730554
267.972273	838.901924	4.396851	-0.049351	1.737235
268.515354	847.034005	4.401856	-0.049458	1.743888
268.841471	855.200208	4.406861	-0.049524	1.750516
269.216554	863.366142	4.411866	-0.049599	1.757125
269.720652	871.497990	4.416870	-0.049699	1.763697
270.083319	879.640949	4.421875	-0.049771	1.770236
270.285683	887.834800	4.426880	-0.049815	1.776772
270.654393	895.972978	4.431885	-0.049889	1.783260
271.102307	904.131482	4.436890	-0.049977	1.789750
271.606866	912.318659	4.441894	-0.050077	1.796246
271.922951	920.431940	4.446899	-0.050141	1.802637
272.411488	928.556131	4.451904	-0.050237	1.809036
272.818920	936.701376	4.456909	-0.050319	1.815418
273.144911	944.836380	4.461914	-0.050385	1.821760
273.638638	952.974666	4.466918	-0.050482	1.828102
273.865638	961.150991	4.471923	-0.050530	1.834420
274.088105	969.297508	4.476928	-0.050576	1.840693
274.374511	977.432377	4.481933	-0.050635	1.846943
274.622031	985.584212	4.486938	-0.050687	1.853180
274.846826	993.731809	4.491942	-0.050734	1.859391
275.073911	1001.846385	4.496947	-0.050782	1.865556
275.801443	1009.951753	4.501952	-0.050922	1.871751
276.398659	1018.051035	4.506957	-0.051039	1.877906
276.518831	1026.194687	4.511962	-0.051067	1.884020
276.913868	1034.325901	4.516966	-0.051146	1.890135
277.125607	1042.476127	4.521971	-0.051191	1.896225
277.375458	1050.605683	4.526976	-0.051242	1.902283
277.685869	1058.731098	4.531981	-0.051306	1.908327
278.096542	1066.855965	4.536986	-0.051387	1.914361
278.366840	1074.982077	4.541990	-0.051443	1.920362
278.389782	1083.120558	4.546995	-0.051453	1.926326
278.897133	1091.221252	4.552000	-0.051553	1.932297
279.352925	1099.314625	4.557005	-0.051643	1.938239
279.701413	1107.429321	4.562010	-0.051713	1.944166
279.897753	1115.592992	4.567014	-0.051755	1.950094
280.312907	1123.710141	4.572019	-0.051838	1.955994
280.695882	1131.799378	4.577024	-0.051914	1.961852
281.065332	1139.883110	4.582029	-0.051989	1.967688
281.335371	1148.015619	4.587034	-0.052044	1.973531
281.723723	1156.103095	4.592038	-0.052122	1.979336
281.757489	1164.233302	4.597043	-0.052134	1.985118
283.558896	1172.142370	4.602048	-0.052474	1.990912
284.618813	1180.223154	4.607053	-0.052677	1.996732
284.891826	1188.351996	4.612058	-0.052733	2.002487
285.222072	1196.506463	4.617062	-0.052800	2.008249
285.698021	1204.641692	4.622067	-0.052894	2.013996
286.098078	1212.760734	4.627072	-0.052974	2.019708
286.135580	1220.923526	4.632077	-0.052986	2.025396
286.411567	1229.063424	4.637082	-0.053043	2.031077
287.009703	1237.154642	4.642086	-0.053160	2.036742
287.322733	1245.227653	4.647091	-0.053223	2.042349
287.556119	1253.345684	4.652096	-0.053272	2.047963
287.675131	1261.491557	4.657101	-0.053300	2.053570
287.948719	1269.576055	4.662106	-0.053356	2.059134
288.442183	1277.632488	4.667110	-0.053453	2.064687
288.529089	1285.774404	4.672115	-0.053475	2.070242
288.916826	1293.873093	4.677120	-0.053552	2.075783
289.081752	1301.977229	4.682125	-0.053589	2.081291
289.230887	1310.072197	4.687130	-0.053622	2.086776
289.664216	1318.161313	4.692134	-0.053708	2.092271
290.005213	1326.237984	4.697139	-0.053777	2.097734
290.207581	1334.348573	4.702144	-0.053820	2.103191
290.652387	1342.422030	4.707149	-0.053908	2.108634
290.940526	1350.585689	4.712154	-0.053967	2.114107
291.462750	1358.636019	4.717158	-0.054069	2.119513
291.646898	1366.697753	4.722163	-0.054109	2.124881
292.126097	1374.772843	4.727168	-0.054204	2.130271
292.482854	1382.874963	4.732173	-0.054275	2.135655
292.846703	1390.927263	4.737178	-0.054348	2.140992
293.529230	1398.971744	4.742182	-0.054481	2.146341
293.745607	1407.091703	4.747187	-0.054527	2.151682
293.708692	1415.243510	4.752192	-0.054525	2.157007
294.385791	1423.259360	4.757197	-0.054656	2.162297
294.617638	1431.345702	4.762202	-0.054705	2.167579
294.717175	1439.494349	4.767206	-0.054729	2.172875
294.924711	1447.565318	4.772211	-0.054773	2.178119
295.188913	1455.644248	4.777216	-0.054827	2.183360
295.636971	1463.724319	4.782221	-0.054916	2.188606
295.558588	1471.874879	4.787226	-0.054907	2.193836
296.064071	1479.917895	4.792230	-0.055006	2.199039
296.308308	1487.959954	4.797235	-0.055057	2.204204
296.551290	1496.053577	4.802240	-0.055108	2.209390
296.705734	1504.173687	4.807245	-0.055142	2.214573
297.186013	1512.202039	4.812250	-0.055237	2.219715
297.681432	1520.261305	4.817254	-0.055334	2.224866
297.975118	1528.337174	4.822259	-0.055394	2.229997
298.450757	1536.426281	4.827264	-0.055488	2.235140
298.747782	1544.506136	4.832269	-0.055549	2.240251
298.963972	1552.574850	4.837274	-0.055594	2.245335
299.327353	1560.670743	4.842278	-0.055667	2.250438
299.629851	1568.751477	4.847283	-0.055729	2.255514
299.793390	1576.832821	4.852288	-0.055765	2.260568
300.258386	1584.871542	4.857293	-0.055857	2.265609
300.781916	1592.960442	4.862298	-0.055960	2.270675
300.886884	1601.129371	4.867302	-0.055985	2.275744
300.966438	1609.178748	4.872307	-0.056005	2.280725
301.485689	1617.188037	4.877312	-0.056107	2.285708
301.994517	1625.233626	4.882317	-0.056207	2.290702
302.131139	1633.325587	4.887322	-0.056238	2.295681
302.470471	1641.383965	4.892326	-0.056306	2.300646
302.648071	1649.452743	4.897331	-0.056345	2.305594
302.953680	1657.542749	4.902336	-0.056407	2.310554
303.124410	1665.650291	4.907341	-0.056444	2.315503
303.499321	1673.685727	4.912346	-0.056519	2.320415
303.861125	1681.753389	4.917350	-0.056592	2.325334
304.121426	1689.801549	4.922355	-0.056646	2.330223
304.688059	1697.858884	4.927360	-0.056756	2.335132
305.146176	1705.916623	4.932365	-0.056847	2.340022
305.345119	1713.987613	4.937370	-0.056889	2.344889
306.054412	1722.041986	4.942374	-0.057027	2.349777
306.426676	1730.137690	4.947379	-0.057102	2.354652
306.662036	1738.208442	4.952384	-0.057151	2.359491
306.873512	1746.261655	4.957389	-0.057195	2.364308
307.097600	1754.334215	4.962394	-0.057243	2.369127
307.421767	1762.428903	4.967398	-0.057308	2.373958
307.597207	1770.493491	4.972403	-0.057346	2.378749
307.746635	1778.571867	4.977408	-0.057379	2.383537
308.139934	1786.623164	4.982413	-0.057458	2.388318
308.369847	1794.700980	4.987418	-0.057506	2.393092
308.546279	1802.781472	4.992422	-0.057544	2.397855
309.080975	1810.786553	4.997427	-0.057649	2.402591
309.197076	1818.880724	5.002432	-0.057676	2.407337
309.662301	1826.943868	5.007437	-0.057768	2.412084
309.827868	1835.007131	5.012442	-0.057804	2.416797
310.187103	1843.075154	5.017446	-0.057877	2.421519
310.598683	1851.120781	5.022451	-0.057958	2.426223
310.708139	1859.242338	5.027456	-0.057984	2.430938
311.281854	1867.319461	5.032461	-0.058096	2.435654
311.452672	1875.349729	5.037466	-0.058134	2.440303
311.596842	1883.418722	5.042470	-0.058166	2.444964
311.797545	1891.450981	5.047475	-0.058208	2.449599
312.115466	1899.526264	5.052480	-0.058273	2.454258
312.321828	1907.565957	5.057485	-0.058317	2.458880
312.697158	1915.593962	5.062490	-0.058392	2.463499
313.032826	1923.673656	5.067494	-0.058460	2.468136
313.488082	1931.710708	5.072499	-0.058550	2.472748
313.595895	1939.792792	5.077504	-0.058575	2.477352
313.854470	1947.847595	5.082509	-0.058629	2.481943
314.053830	1955.889299	5.087514	-0.058671	2.486514
314.574485	1963.946405	5.092518	-0.058773	2.491108
314.770617	1972.027389	5.097523	-0.058815	2.495684
315.157955	1980.060152	5.102528	-0.058893	2.500238
315.457697	1988.127140	5.107533	-0.058954	2.504796
315.791760	1996.163976	5.112538	-0.059021	2.509332
316.254568	2004.273787	5.117542	-0.059113	2.513909
316.602779	2012.280388	5.122547	-0.059183	2.518412
316.916203	2020.330620	5.127552	-0.059247	2.522929
317.234031	2028.380344	5.132557	-0.059311	2.527438
317.271271	2036.483227	5.137562	-0.059324	2.531948
317.552817	2044.546987	5.142566	-0.059381	2.536446
317.735603	2052.585936	5.147571	-0.059421	2.540916
318.049342	2060.636095	5.152576	-0.059484	2.545392
318.283569	2068.701087	5.157581	-0.059533	2.549863
318.671038	2076.741452	5.162586	-0.059611	2.554324
319.181225	2084.772956	5.167590	-0.059711	2.558780
319.264991	2092.839292	5.172595	-0.059732	2.563218
319.535430	2100.895024	5.177600	-0.059788	2.567656
319.774894	2108.975895	5.182605	-0.059838	2.572097
319.968643	2117.034040	5.187610	-0.059879	2.576515
320.385645	2125.072151	5.192614	-0.059962	2.580930
320.587732	2133.113323	5.197619	-0.060005	2.585324
320.958513	2141.161021	5.202624	-0.060079	2.589726
321.264637	2149.410577	5.207629	-0.060142	2.594225
321.493083	2157.390854	5.212634	-0.060190	2.598566
321.774261	2165.402607	5.217638	-0.060247	2.602919
322.106437	2173.402239	5.222643	-0.060315	2.607263
322.644802	2181.406955	5.227648	-0.060420	2.611615
322.940901	2189.489293	5.232653	-0.060481	2.615986
322.985470	2197.534435	5.237658	-0.060494	2.620312
323.251861	2205.579231	5.242662	-0.060549	2.624646
323.837104	2213.596177	5.247667	-0.060663	2.628979
323.985054	2221.685449	5.252672	-0.060696	2.633315
324.170131	2229.736184	5.257677	-0.060736	2.637625
324.369339	2237.761543	5.262682	-0.060779	2.641915
324.710860	2245.823173	5.267686	-0.060847	2.646228
325.101876	2253.853004	5.272691	-0.060926	2.650519
325.355176	2261.910533	5.277696	-0.060978	2.654809
325.931222	2269.920407	5.282701	-0.061091	2.659088
326.131122	2277.965039	5.287706	-0.061133	2.663354
326.198868	2286.072481	5.292710	-0.061151	2.667637
326.438674	2294.145468	5.297715	-0.061201	2.671907
326.980720	2302.146245	5.302720	-0.061307	2.676151
327.040715	2310.230185	5.307725	-0.061324	2.680401
327.355345	2318.227774	5.312730	-0.061388	2.684616
327.724807	2326.278060	5.317734	-0.061462	2.688854
327.889454	2334.334821	5.322739	-0.061498	2.693077
328.131486	2342.408211	5.327744	-0.061548	2.697306
328.343542	2350.445256	5.332749	-0.061593	2.701508
328.512583	2358.474274	5.337754	-0.061630	2.705697
328.907977	2366.518268	5.342758	-0.061709	2.709900
329.247091	2374.586521	5.347763	-0.061777	2.714107
329.524026	2382.612762	5.352768	-0.061834	2.718281
329.850616	2390.658897	5.357773	-0.061900	2.722462
330.036320	2398.702850	5.362778	-0.061940	2.726627
330.423060	2406.756611	5.367782	-0.062018	2.730802
330.511007	2414.810925	5.372787	-0.062039	2.734954
330.632383	2422.857783	5.377792	-0.062067	2.739097
331.102803	2430.881236	5.382797	-0.062160	2.743243
331.192125	2438.939393	5.387802	-0.062182	2.747377
331.243441	2447.047799	5.392806	-0.062197	2.751529
331.626536	2455.125293	5.397811	-0.062274	2.755678
331.918367	2463.102148	5.402816	-0.062333	2.759765
332.303308	2471.116306	5.407821	-0.062410	2.763870
332.117245	2479.178528	5.412826	-0.062381	2.767959
332.542764	2487.231152	5.417830	-0.062466	2.772073
332.835736	2495.278751	5.422835	-0.062525	2.776171
333.065010	2503.306935	5.427840	-0.062573	2.780249
333.324604	2511.332405	5.432845	-0.062627	2.784322
333.484410	2519.372663	5.437850	-0.062662	2.788390
333.696943	2527.475691	5.442854	-0.062707	2.792487
333.992441	2535.505452	5.447859	-0.062767	2.796546
334.330873	2543.521595	5.452864	-0.062836	2.800595
334.322561	2551.570094	5.457869	-0.062840	2.804634
334.370475	2559.617513	5.462874	-0.062854	2.808670
334.727398	2567.672357	5.467878	-0.062926	2.812721
335.061304	2575.694138	5.472883	-0.062993	2.816749
335.197870	2583.727584	5.477888	-0.063024	2.820765
335.361246	2591.773270	5.482893	-0.063060	2.824784
335.645059	2599.818063	5.487898	-0.063118	2.828803
335.925198	2607.894373	5.492902	-0.063175	2.832831
336.087452	2615.931481	5.497907	-0.063211	2.836828
336.398396	2623.941751	5.502912	-0.063274	2.840814
336.872997	2631.938012	5.507917	-0.063368	2.844797
337.136123	2639.957587	5.512922	-0.063422	2.848774
337.364083	2648.046939	5.517926	-0.063470	2.852777
337.541527	2656.092590	5.522931	-0.063508	2.856751
337.614510	2664.140950	5.527936	-0.063527	2.860715
337.754839	2672.161816	5.532941	-0.063558	2.864663
337.889717	2680.213547	5.537946	-0.063589	2.868621
338.094854	2688.281388	5.542950	-0.063632	2.872585
338.190883	2696.331785	5.547955	-0.063656	2.876529
338.534561	2704.331216	5.552960	-0.063725	2.880456
338.710875	2712.370586	5.557965	-0.063763	2.884388
338.856615	2720.402619	5.562970	-0.063796	2.888310
339.306119	2728.451209	5.567974	-0.063885	2.892250
339.247108	2736.531191	5.572979	-0.063879	2.896174
339.503237	2744.536498	5.577984	-0.063932	2.900072
339.757999	2752.572857	5.582989	-0.063985	2.903980
339.949516	2760.617453	5.587994	-0.064026	2.907884
340.159268	2768.706522	5.592998	-0.064070	2.911804
340.411207	2776.808470	5.598003	-0.064122	2.915728
340.627948	2784.749672	5.603008	-0.064168	2.919567
340.943502	2792.782829	5.608013	-0.064232	2.923450
340.986876	2800.794745	5.613018	-0.064245	2.927304
341.320598	2808.861825	5.618022	-0.064313	2.931195
341.607392	2816.900593	5.623027	-0.064372	2.935064
341.802511	2824.918952	5.628032	-0.064413	2.938913
341.907463	2832.942657	5.633037	-0.064438	2.942755
342.050819	2840.989777	5.638042	-0.064470	2.946606
342.192651	2849.052910	5.643046	-0.064502	2.950459
342.367334	2857.094275	5.648051	-0.064540	2.954298
342.618274	2865.122254	5.653056	-0.064592	2.958129
342.922992	2873.130033	5.658061	-0.064654	2.961949
343.014554	2881.161893	5.663066	-0.064676	2.965765
343.282658	2889.203768	5.668070	-0.064731	2.969589
343.568038	2897.242436	5.673075	-0.064790	2.973407
343.733411	2905.293782	5.678080	-0.064826	2.977221
343.783126	2913.350616	5.683085	-0.064841	2.981026
344.016377	2921.335374	5.688090	-0.064889	2.984802
344.160165	2929.416143	5.693094	-0.064921	2.988614
344.476365	2937.466520	5.698099	-0.064986	2.992415
344.505005	2945.511707	5.703104	-0.064996	2.996194
344.975991	2953.493241	5.708109	-0.065089	2.999961
345.091166	2961.500405	5.713114	-0.065116	3.003717
345.346855	2969.556356	5.718118	-0.065169	3.007499
345.464834	2977.622951	5.723123	-0.065196	3.011273
345.428294	2985.697793	5.728128	-0.065195	3.015040
345.870479	2993.696641	5.733133	-0.065282	3.018789
345.759865	3001.729612	5.738138	-0.065267	3.022523
346.120945	3009.757095	5.743142	-0.065340	3.026273
346.218817	3017.812583	5.748147	-0.065363	3.030018
346.489187	3025.858235	5.753152	-0.065419	3.033762
346.917180	3033.862633	5.758157	-0.065504	3.037490
346.854453	3041.904017	5.763162	-0.065498	3.041207
346.950065	3049.938932	5.768166	-0.065521	3.044924
347.287953	3057.953439	5.773171	-0.065589	3.048639
347.441925	3066.013687	5.778176	-0.065623	3.052361
347.757059	3074.061955	5.783181	-0.065687	3.056081
347.699455	3082.084181	5.788186	-0.065682	3.059767
348.051847	3090.101505	5.793190	-0.065752	3.063465
347.983040	3098.166079	5.798195	-0.065745	3.067161
347.999066	3106.229698	5.803200	-0.065753	3.070856
348.343555	3114.326446	5.808205	-0.065823	3.074577
348.479815	3122.305222	5.813210	-0.065853	3.078229
348.659799	3130.328834	5.818214	-0.065892	3.081900
348.859678	3138.327219	5.823219	-0.065935	3.085556
348.903629	3146.339208	5.828224	-0.065948	3.089207
349.084822	3154.406690	5.833229	-0.065987	3.092884
349.469615	3162.410546	5.838234	-0.066064	3.096538
349.669805	3170.432175	5.843238	-0.066107	3.100187
349.574326	3178.474927	5.848243	-0.066094	3.103828
349.761987	3186.520985	5.853248	-0.066135	3.107479
350.169727	3194.555440	5.858253	-0.066216	3.111130
350.311115	3202.580991	5.863258	-0.066248	3.114761
350.551953	3210.606147	5.868262	-0.066298	3.118392
350.771054	3218.629065	5.873267	-0.066344	3.122016
350.895114	3226.649968	5.878272	-0.066372	3.125632
351.173873	3234.686555	5.883277	-0.066430	3.129257
351.189057	3242.736215	5.888282	-0.066438	3.132872
351.572460	3250.785588	5.893286	-0.066514	3.136498
351.768184	3258.795881	5.898291	-0.066556	3.140095
351.865590	3266.812490	5.903296	-0.066580	3.143687
352.015378	3274.877953	5.908301	-0.066613	3.147298
351.925757	3282.945939	5.913306	-0.066601	3.150896
352.263195	3290.976788	5.918310	-0.066670	3.154491
352.269328	3299.007662	5.923315	-0.066676	3.158068
352.542394	3307.001507	5.928320	-0.066732	3.161636
352.779509	3315.019941	5.933325	-0.066782	3.165210
352.769757	3323.060755	5.938330	-0.066785	3.168779
353.202553	3331.085058	5.943334	-0.066871	3.172355
353.440198	3339.154265	5.948339	-0.066921	3.175939
353.566190	3347.139586	5.953344	-0.066949	3.179477
353.774293	3355.191073	5.958349	-0.066993	3.183043
354.024647	3363.214415	5.963354	-0.067045	3.186595
354.432139	3371.222697	5.968358	-0.067127	3.190143
354.587924	3379.311499	5.973363	-0.067161	3.193712
354.884342	3387.310200	5.978368	-0.067221	3.197243
355.085208	3395.363178	5.983373	-0.067264	3.200790
355.220503	3403.333163	5.988378	-0.067295	3.204293
355.184408	3411.422822	5.993382	-0.067293	3.207839
355.512407	3419.448019	5.998387	-0.067360	3.211367
355.615702	3427.466127	6.003392	-0.067384	3.214879
355.823200	3435.518347	6.008397	-0.067428	3.218406
356.015003	3443.525872	6.013402	-0.067469	3.221909
356.226399	3451.534660	6.018406	-0.067514	3.225410
356.342226	3459.587671	6.023411	-0.067541	3.228922
356.465889	3467.669609	6.028416	-0.067569	3.232444
356.748366	3475.759397	6.033421	-0.067627	3.235971
356.814472	3483.698965	6.038426	-0.067645	3.239420
356.880991	3491.722627	6.043430	-0.067662	3.242903
357.106647	3499.721580	6.048435	-0.067710	3.246377
357.212114	3507.755401	6.053440	-0.067735	3.249857
357.537052	3515.816830	6.058445	-0.067800	3.253355
357.556903	3523.850578	6.063450	-0.067809	3.256825
357.763091	3531.880275	6.068454	-0.067853	3.260296
358.005669	3539.887057	6.073459	-0.067904	3.263756
358.340606	3547.913675	6.078464	-0.067971	3.267224
358.295582	3555.979759	6.083469	-0.067968	3.270690
358.480229	3564.018364	6.088474	-0.068008	3.274150
358.816240	3572.022802	6.093478	-0.068076	3.277597
359.122807	3580.033383	6.098483	-0.068138	3.281042
359.124452	3588.044161	6.103488	-0.068144	3.284472
359.211031	3596.100263	6.108493	-0.068165	3.287921
359.431759	3604.114867	6.113498	-0.068212	3.291354
359.648148	3612.163955	6.118502	-0.068257	3.294797
359.606281	3620.196200	6.123507	-0.068255	3.298220
359.836242	3628.200174	6.128512	-0.068303	3.301638
360.157808	3636.222065	6.133517	-0.068368	3.305063
360.387233	3644.229716	6.138522	-0.068416	3.308475
360.509610	3652.327292	6.143526	-0.068444	3.311918
360.732119	3660.394354	6.148531	-0.068491	3.315348
360.969043	3668.355084	6.153536	-0.068540	3.318729
360.963574	3676.392522	6.158541	-0.068545	3.322131
361.139550	3684.393529	6.163546	-0.068583	3.325521
361.323866	3692.422031	6.168550	-0.068622	3.328919
361.490767	3700.493659	6.173555	-0.068659	3.332331
361.692470	3708.509861	6.178560	-0.068702	3.335717
361.964365	3716.516364	6.183565	-0.068758	3.339099
361.987261	3724.533338	6.188570	-0.068767	3.342472
362.051382	3732.598727	6.193574	-0.068785	3.345864
362.244302	3740.609171	6.198579	-0.068826	3.349234
362.334824	3748.668600	6.203584	-0.068848	3.352617
362.374761	3756.749501	6.208589	-0.068861	3.356004
362.612593	3764.690330	6.213594	-0.068910	3.359336
362.935869	3772.717787	6.218598	-0.068976	3.362704
363.077859	3780.728495	6.223603	-0.069008	3.366055
363.202223	3788.737528	6.228608	-0.069036	3.369402
363.338186	3796.823292	6.233613	-0.069067	3.372777
363.535815	3804.865516	6.238618	-0.069109	3.376133
363.719556	3812.863707	6.243622	-0.069148	3.379467
364.061845	3820.878351	6.248627	-0.069217	3.382810
364.214323	3828.901221	6.253632	-0.069251	3.386147
364.326139	3836.932475	6.258637	-0.069277	3.389482
364.518097	3845.038123	6.263642	-0.069318	3.392848
364.718313	3853.082568	6.268646	-0.069361	3.396185
364.929268	3861.029906	6.273651	-0.069405	3.399479
365.130418	3869.031989	6.278656	-0.069448	3.402792
365.521646	3877.061056	6.283661	-0.069526	3.406119
365.514493	3885.070449	6.288666	-0.069530	3.409422
365.663574	3893.128581	6.293670	-0.069563	3.412746
366.057038	3901.185198	6.298675	-0.069642	3.416075
366.041752	3909.175486	6.303680	-0.069644	3.419360
366.123751	3917.214932	6.308685	-0.069665	3.422665
366.418081	3925.218995	6.313690	-0.069725	3.425959
366.655772	3933.230182	6.318694	-0.069775	3.429251
366.745110	3941.335970	6.323699	-0.069797	3.432574
366.870246	3949.356681	6.328704	-0.069825	3.435860
367.015187	3957.339981	6.333709	-0.069858	3.439128
367.258030	3965.353654	6.338714	-0.069908	3.442409
367.502212	3973.358906	6.343718	-0.069959	3.445683
367.609811	3981.427295	6.348723	-0.069984	3.448975
367.659092	3989.458257	6.353728	-0.069999	3.452247
367.801387	3997.553939	6.358733	-0.070031	3.455545
367.996115	4005.511847	6.363738	-0.070072	3.458786
368.345287	4013.535820	6.368742	-0.070142	3.462055
368.375226	4021.568969	6.373747	-0.070153	3.465315
368.612623	4029.559397	6.378752	-0.070203	3.468561
369.801161	4037.568849	6.383757	-0.070429	3.471842
370.052791	4045.624593	6.388762	-0.070482	3.475108
370.232106	4053.637291	6.393766	-0.070520	3.478352
370.601611	4061.675171	6.398771	-0.070594	3.481609
370.818523	4069.649807	6.403776	-0.070640	3.484832
370.966495	4077.717912	6.408781	-0.070673	3.488088
370.905507	4085.764084	6.413786	-0.070667	3.491326
371.420344	4093.769217	6.418790	-0.070768	3.494562
371.682088	4101.809344	6.423795	-0.070822	3.497801
371.713723	4109.829663	6.428800	-0.070833	3.501022
371.936084	4117.841949	6.433805	-0.070880	3.504242
372.263436	4125.872372	6.438810	-0.070946	3.507470
372.096918	4133.919258	6.443814	-0.070921	3.510687
372.357489	4141.950243	6.448819	-0.070975	3.513907
372.604489	4149.966308	6.453824	-0.071026	3.517118
372.720321	4158.002904	6.458829	-0.071053	3.520331
372.884713	4165.997810	6.463834	-0.071089	3.523525
373.035711	4174.039466	6.468838	-0.071122	3.526734
373.247990	4182.072928	6.473843	-0.071167	3.529939
373.187685	4190.133486	6.478848	-0.071161	3.533144
373.585725	4198.170145	6.483853	-0.071240	3.536350
373.927249	4206.148503	6.488858	-0.071309	3.539528
374.041028	4214.180301	6.493862	-0.071336	3.542718
374.187857	4222.215363	6.498867	-0.071368	3.545907
374.104969	4230.253469	6.503872	-0.071358	3.549088
374.453684	4238.348153	6.508877	-0.071429	3.552301
374.481087	4246.380000	6.513882	-0.071439	3.555476
374.912353	4254.317373	6.518886	-0.071525	3.558624
376.345824	4262.288195	6.523891	-0.071797	3.561810
376.708027	4270.279432	6.528896	-0.071870	3.564971
377.199335	4278.315303	6.533901	-0.071966	3.568150
377.445401	4286.358956	6.538906	-0.072018	3.571322
377.466859	4294.382485	6.543910	-0.072027	3.574477
377.697699	4302.427387	6.548915	-0.072075	3.577644
377.952972	4310.430013	6.553920	-0.072128	3.580792
378.195350	4318.456664	6.558925	-0.072178	3.583946
378.412264	4326.475589	6.563930	-0.072224	3.587094
378.783204	4334.493029	6.568934	-0.072298	3.590242
379.116989	4342.564264	6.573939	-0.072366	3.593408
379.073155	4350.574535	6.578944	-0.072363	3.596536
379.391175	4358.591676	6.583949	-0.072428	3.599675
379.602275	4366.602717	6.588954	-0.072472	3.602805
379.717464	4374.635615	6.593958	-0.072499	3.605939
379.883420	4382.647919	6.598963	-0.072535	3.609063
380.069093	4390.700387	6.603968	-0.072575	3.612201
380.285230	4398.761833	6.608973	-0.072621	3.615340
380.349829	4406.750088	6.613978	-0.072638	3.618444
380.604596	4414.777879	6.618982	-0.072691	3.621566
380.856025	4422.778306	6.623987	-0.072743	3.624674
380.845412	4430.825639	6.628992	-0.072746	3.627791
381.009073	4438.909829	6.633997	-0.072782	3.630923
381.141846	4446.956358	6.639002	-0.072812	3.634038
381.263474	4454.938669	6.644006	-0.072840	3.637125
381.367996	4462.958125	6.649011	-0.072865	3.640224
381.534857	4470.943767	6.654016	-0.072901	3.643308
382.040307	4478.981292	6.659021	-0.073001	3.646418
382.164239	4487.001517	6.664026	-0.073029	3.649509
382.388194	4495.037260	6.669030	-0.073076	3.652606
382.574100	4503.090626	6.674035	-0.073116	3.655707
382.518679	4511.058175	6.679040	-0.073111	3.658765
382.797733	4519.107608	6.684045	-0.073168	3.661861
383.036997	4527.081105	6.689050	-0.073218	3.664924
383.172140	4535.146608	6.694054	-0.073249	3.668017
383.291206	4543.194758	6.699059	-0.073276	3.671100
383.425112	4551.209547	6.704064	-0.073306	3.674168
383.732856	4559.228598	6.709069	-0.073369	3.677240
383.976251	4567.196563	6.714074	-0.073419	3.680288
384.032762	4575.213012	6.719078	-0.073435	3.683347
384.356708	4583.273536	6.724083	-0.073501	3.686427
384.453797	4591.253254	6.729088	-0.073524	3.689469
384.820129	4599.336986	6.734093	-0.073598	3.692553
385.206750	4607.320350	6.739098	-0.073675	3.695598
385.195252	4615.351060	6.744102	-0.073678	3.698648
385.418612	4623.399570	6.749107	-0.073725	3.701708
385.568876	4631.359072	6.754112	-0.073759	3.704730
385.775116	4639.426239	6.759117	-0.073802	3.707792
385.983043	4647.453041	6.764122	-0.073846	3.710836
386.190189	4655.575755	6.769126	-0.073890	3.713914
386.411499	4663.573843	6.774131	-0.073937	3.716942
386.675317	4671.515492	6.779136	-0.073991	3.719948
386.874854	4679.528999	6.784141	-0.074034	3.722976
387.055318	4687.550328	6.789146	-0.074072	3.726005
387.344721	4695.532462	6.794150	-0.074132	3.729019
387.674797	4703.638124	6.799155	-0.074198	3.732078
387.695928	4711.635346	6.804160	-0.074208	3.735086
388.111166	4719.676011	6.809165	-0.074290	3.738118
388.169092	4727.729752	6.814170	-0.074306	3.741143
388.370948	4735.687081	6.819174	-0.074349	3.744134
388.637042	4743.719388	6.824179	-0.074404	3.747151
388.657914	4751.753350	6.829184	-0.074413	3.750161
388.847074	4759.827702	6.834189	-0.074454	3.753187
389.019892	4767.840344	6.839194	-0.074491	3.756188
389.163716	4775.806078	6.844198	-0.074524	3.759168
389.429104	4783.860330	6.849203	-0.074578	3.762181
389.588809	4791.847188	6.854208	-0.074613	3.765165
389.845709	4799.886545	6.859213	-0.074666	3.768167
390.006325	4807.927318	6.864218	-0.074702	3.771166
390.148635	4815.936224	6.869222	-0.074733	3.774150
390.494074	4823.978887	6.874227	-0.074803	3.777149
390.514248	4831.980210	6.879232	-0.074812	3.780122
390.496509	4840.005238	6.884237	-0.074814	3.783102
390.759875	4848.030923	6.889242	-0.074869	3.786085
390.947306	4856.015298	6.894246	-0.074909	3.789049
391.290701	4864.087920	6.899251	-0.074978	3.792047
391.321283	4872.117040	6.904256	-0.074989	3.795019
391.658989	4880.123587	6.909261	-0.075057	3.797988
391.647854	4888.125557	6.914266	-0.075060	3.800945
391.763989	4896.105243	6.919270	-0.075087	3.803894
392.393432	4904.114024	6.924275	-0.075210	3.806862
392.433480	4912.118353	6.929280	-0.075223	3.809814
392.677673	4920.210467	6.934285	-0.075273	3.812800
392.680481	4928.240531	6.939290	-0.075279	3.815756
392.991014	4936.218546	6.944294	-0.075342	3.818697
393.121136	4944.266630	6.949299	-0.075372	3.821658
393.197909	4952.250047	6.954304	-0.075391	3.824591
393.787387	4960.277120	6.959309	-0.075507	3.827549
393.945737	4968.344253	6.964314	-0.075541	3.830510
394.015609	4976.368101	6.969318	-0.075560	3.833451
394.473932	4984.396956	6.974323	-0.075650	3.836400
394.645422	4992.355077	6.979328	-0.075688	3.839315
394.700345	5000.398409	6.984333	-0.075703	3.842256
394.792968	5008.441579	6.989338	-0.075726	3.845196
395.268037	5016.431409	6.994342	-0.075819	3.848121
395.304809	5024.526059	6.999347	-0.075832	3.851074
395.411446	5032.539996	7.004352	-0.075857	3.853997
395.759626	5040.577804	7.009357	-0.075927	3.856930
395.945882	5048.583458	7.014362	-0.075967	3.859847
396.016451	5056.595492	7.019366	-0.075985	3.862761
396.517136	5064.617113	7.024371	-0.076084	3.865685
396.520846	5072.644153	7.029376	-0.076090	3.868599
396.745998	5080.719664	7.034381	-0.076137	3.871533
396.883516	5088.930148	7.039386	-0.076168	3.874512
397.237777	5096.794911	7.044390	-0.076239	3.877367
397.445850	5104.750157	7.049395	-0.076283	3.880250
397.498575	5112.717868	7.054400	-0.076299	3.883133
397.851907	5120.773418	7.059405	-0.076370	3.886051
398.036637	5128.758370	7.064410	-0.076409	3.888938
398.108190	5136.795914	7.069414	-0.076428	3.891839
398.324013	5144.842406	7.074419	-0.076473	3.894745
398.497929	5152.840828	7.079424	-0.076511	3.897630
398.823217	5160.847006	7.084429	-0.076577	3.900518
398.996785	5168.840136	7.089434	-0.076615	3.903397
399.102038	5176.882701	7.094438	-0.076640	3.906290
399.256072	5184.925322	7.099443	-0.076674	3.909182
399.308615	5192.907771	7.104448	-0.076689	3.912048
399.624947	5200.942860	7.109453	-0.076753	3.914936
399.875772	5208.966408	7.114458	-0.076805	3.917816
399.988299	5216.959307	7.119462	-0.076831	3.920681
400.338333	5224.968938	7.124467	-0.076902	3.923554
400.616237	5232.995170	7.129472	-0.076959	3.926429
400.948572	5241.016850	7.134477	-0.077026	3.929302
401.012861	5249.063896	7.139482	-0.077043	3.932177
401.221396	5257.081770	7.144486	-0.077087	3.935042
401.531932	5265.096211	7.149491	-0.077150	3.937905
401.312813	5273.126668	7.154496	-0.077115	3.940762
401.761984	5281.090948	7.159501	-0.077204	3.943606
402.071726	5289.175007	7.164506	-0.077267	3.946487
402.084300	5297.199490	7.169510	-0.077274	3.949341
402.250898	5305.230311	7.174515	-0.077311	3.952197
402.470225	5313.248667	7.179520	-0.077357	3.955047
402.716618	5321.243448	7.184525	-0.077408	3.957887
403.057160	5329.270458	7.189530	-0.077477	3.960739
403.353914	5337.218190	7.194534	-0.077537	3.963559
403.595659	5345.298699	7.199539	-0.077588	3.966424
403.578119	5353.326661	7.204544	-0.077590	3.969263
403.965944	5361.414816	7.209549	-0.077667	3.972128
404.291466	5369.436719	7.214554	-0.077733	3.974967
404.458957	5377.407212	7.219558	-0.077770	3.977783
404.518487	5385.444182	7.224563	-0.077786	3.980619
404.596972	5393.424908	7.229568	-0.077806	3.983433
404.926264	5401.469926	7.234573	-0.077873	3.986272
404.913871	5409.479556	7.239578	-0.077876	3.989091
405.305250	5417.525431	7.244582	-0.077954	3.991927
405.686553	5425.575877	7.249587	-0.078030	3.994762
405.590632	5433.587805	7.254592	-0.078018	3.997575
405.777343	5441.575815	7.259597	-0.078058	4.000381
405.836873	5449.590313	7.264602	-0.078074	4.003193
406.003087	5457.611104	7.269606	-0.078110	4.006006
406.409392	5465.659136	7.274611	-0.078191	4.008831
406.514367	5473.676267	7.279616	-0.078216	4.011638
406.587024	5481.682615	7.284621	-0.078235	4.014439
406.783785	5489.703497	7.289626	-0.078277	4.017245
407.200266	5497.681219	7.294630	-0.078360	4.020038
407.534053	5505.744302	7.299635	-0.078427	4.022857
407.483933	5513.716812	7.304640	-0.078423	4.025636
407.720553	5521.779365	7.309645	-0.078473	4.028449
408.140225	5529.803113	7.314650	-0.078556	4.031250
408.343095	5537.875001	7.319654	-0.078599	4.034062
408.507923	5545.910210	7.324659	-0.078635	4.036858
408.628013	5553.792974	7.329664	-0.078663	4.039600
409.082334	5561.842573	7.334669	-0.078753	4.042402
409.260221	5569.836537	7.339674	-0.078791	4.045178
409.422399	5577.850233	7.344678	-0.078827	4.047960
409.870416	5585.882092	7.349683	-0.078915	4.050750
409.842406	5593.914820	7.354688	-0.078915	4.053531
410.162370	5601.960544	7.359693	-0.078980	4.056320
410.346064	5609.949741	7.364698	-0.079020	4.059085
410.357480	5617.953228	7.369702	-0.079027	4.061851
410.622982	5625.989963	7.374707	-0.079082	4.064631
410.663884	5633.982470	7.379712	-0.079095	4.067389
411.081734	5642.017962	7.384717	-0.079178	4.070166
411.326276	5650.085012	7.389722	-0.079229	4.072950
411.474256	5658.090761	7.394726	-0.079262	4.075709
411.777705	5666.086840	7.399731	-0.079324	4.078465
411.845288	5674.105827	7.404736	-0.079342	4.081224
412.131030	5682.063661	7.409741	-0.079400	4.083963
412.283103	5690.127595	7.414746	-0.079434	4.086735
412.659818	5698.096551	7.419750	-0.079509	4.089475
412.866140	5706.207728	7.424755	-0.079553	4.092260
412.917929	5714.218326	7.429760	-0.079568	4.095006
413.168299	5722.259647	7.434765	-0.079620	4.097764
413.208120	5730.268797	7.439770	-0.079632	4.100506
413.255914	5738.238297	7.444774	-0.079647	4.103233
413.772503	5746.304395	7.449779	-0.079748	4.105997
413.871733	5754.293781	7.454784	-0.079772	4.108727
413.925117	5762.372554	7.459789	-0.079787	4.111486
414.290978	5770.418788	7.464794	-0.079861	4.114235
414.271217	5778.407666	7.469798	-0.079862	4.116959
414.671333	5786.352698	7.474803	-0.079942	4.119671
414.659938	5794.391354	7.479808	-0.079945	4.122407
415.008218	5802.423378	7.484813	-0.080015	4.125144
415.144193	5810.483155	7.489818	-0.080046	4.127886
415.119862	5818.452936	7.494822	-0.080047	4.130594
415.494075	5826.538052	7.499827	-0.080122	4.133344
415.478708	5834.536538	7.504832	-0.080124	4.136058
415.902135	5842.520371	7.509837	-0.080208	4.138770
416.107761	5850.598275	7.514842	-0.080252	4.141510
416.408544	5858.532634	7.519846	-0.080313	4.144201
416.478961	5866.595529	7.524851	-0.080332	4.146930
416.470273	5874.601832	7.529856	-0.080335	4.149638
416.598658	5882.652150	7.534861	-0.080365	4.152360
416.812812	5890.658690	7.539866	-0.080410	4.155067
416.853388	5898.639354	7.544870	-0.080423	4.157761
417.043496	5906.667454	7.549875	-0.080463	4.160472
417.399321	5914.676858	7.554880	-0.080535	4.163176
417.540015	5922.720956	7.559885	-0.080566	4.165887
417.921093	5930.730952	7.564890	-0.080643	4.168588
418.241469	5938.711152	7.569894	-0.080708	4.171276
418.388167	5946.806289	7.574899	-0.080740	4.174000
418.329498	5954.826011	7.579904	-0.080735	4.176694
418.662951	5962.782563	7.584909	-0.080802	4.179369
418.726564	5970.843201	7.589914	-0.080819	4.182074
418.806204	5978.785657	7.594918	-0.080839	4.184739
419.092049	5986.863734	7.599923	-0.080898	4.187449
419.219674	5994.846730	7.604928	-0.080927	4.190124
419.182745	6002.957552	7.609933	-0.080925	4.192838
419.418998	6011.035338	7.614938	-0.080975	4.195542
419.721339	6018.951048	7.619942	-0.081036	4.198191
420.101369	6026.946189	7.624947	-0.081112	4.200866
420.028858	6034.901314	7.629952	-0.081104	4.203521
420.264208	6042.959863	7.634957	-0.081153	4.206212
420.452692	6050.950136	7.639962	-0.081194	4.208878
420.659286	6058.990952	7.644966	-0.081237	4.211559
420.884445	6067.042066	7.649971	-0.081285	4.214242
420.885804	6075.029868	7.654976	-0.081290	4.216900
421.118915	6083.046983	7.659981	-0.081339	4.219568
421.398459	6091.046325	7.664986	-0.081396	4.222230
421.446851	6099.047109	7.669990	-0.081411	4.224887
421.767677	6107.093198	7.674995	-0.081476	4.227561
421.848682	6115.132462	7.680000	-0.081496	4.230228
422.243402	6123.152028	7.685005	-0.081575	4.232891
422.320168	6131.219602	7.690010	-0.081595	4.235564
422.515358	6139.157921	7.695014	-0.081636	4.238194
422.782598	6147.244637	7.700019	-0.081691	4.240872
422.980098	6155.174143	7.705024	-0.081733	4.243496
423.159696	6163.278296	7.710029	-0.081772	4.246175
423.268103	6171.227852	7.715034	-0.081798	4.248802
423.456244	6179.301373	7.720038	-0.081838	4.251468
423.727835	6187.327654	7.725043	-0.081894	4.254117
423.854687	6195.381810	7.730048	-0.081923	4.256773
423.972521	6203.310460	7.735053	-0.081950	4.259386
424.235190	6211.400603	7.740058	-0.082004	4.262052
424.094833	6219.345862	7.745062	-0.081983	4.264664
424.435879	6227.438486	7.750067	-0.082052	4.267328
424.889068	6235.422277	7.755072	-0.082142	4.269955
425.148265	6243.494032	7.760077	-0.082195	4.272608
425.273554	6251.545704	7.765082	-0.082224	4.275251
425.591470	6259.465301	7.770086	-0.082289	4.277851
425.921246	6267.506753	7.775091	-0.082355	4.280490
426.059680	6275.477879	7.780096	-0.082386	4.283102
426.162678	6283.491041	7.785101	-0.082411	4.285726
426.538916	6291.574214	7.790106	-0.082486	4.288374
426.679361	6299.509586	7.795110	-0.082518	4.290969
426.954734	6307.645444	7.800115	-0.082574	4.293630
427.188577	6315.618166	7.805120	-0.082623	4.296235
427.275634	6323.597314	7.810125	-0.082645	4.298840
427.352750	6331.669663	7.815130	-0.082664	4.301473
427.647627	6339.584913	7.820134	-0.082724	4.304055
427.954578	6347.703217	7.825139	-0.082787	4.306702
427.887120	6355.681540	7.830144	-0.082780	4.309299
427.970581	6363.715061	7.835149	-0.082801	4.311913
428.479727	6371.729734	7.840154	-0.082901	4.314523
428.383921	6379.768420	7.845158	-0.082888	4.317135
428.541210	6387.726664	7.850163	-0.082923	4.319720
428.650797	6395.743688	7.855168	-0.082948	4.322323
429.005180	6403.745964	7.860173	-0.083020	4.324921
429.127512	6411.796612	7.865178	-0.083048	4.327532
429.367665	6419.785141	7.870182	-0.083098	4.330122
429.545661	6427.883045	7.875187	-0.083136	4.332745
429.814983	6435.853779	7.880192	-0.083192	4.335326
429.755626	6443.875620	7.885197	-0.083186	4.337919
430.098967	6451.903842	7.890202	-0.083255	4.340516
430.130293	6459.877461	7.895206	-0.083266	4.343092
430.478165	6467.891216	7.900211	-0.083336	4.345681
430.847613	6475.953040	7.905216	-0.083411	4.348284
430.899489	6483.938789	7.910221	-0.083426	4.350859
431.132962	6492.077032	7.915226	-0.083474	4.353483
431.355473	6500.083754	7.920230	-0.083521	4.356063
431.464744	6508.018833	7.925235	-0.083547	4.358617
431.648716	6516.018407	7.930240	-0.083586	4.361191
431.927832	6523.975389	7.935245	-0.083644	4.363751
432.315871	6532.040180	7.940250	-0.083721	4.366344
432.459509	6540.006331	7.945254	-0.083753	4.368902
432.613365	6548.107452	7.950259	-0.083787	4.371503
432.717527	6556.124742	7.955264	-0.083812	4.374074
432.897298	6564.126979	7.960269	-0.083851	4.376640
433.114637	6572.129449	7.965274	-0.083896	4.379204
433.486560	6580.142871	7.970278	-0.083971	4.381771
433.646198	6588.118817	7.975283	-0.084006	4.384324
433.999604	6596.152933	7.980288	-0.084077	4.386895
434.219654	6604.189201	7.985293	-0.084123	4.389464
434.345765	6612.267968	7.990298	-0.084152	4.392044
434.336200	6620.248033	7.995302	-0.084156	4.394591
434.607209	6628.305661	8.000307	-0.084212	4.397163
434.829856	6636.288546	8.005312	-0.084258	4.399709
435.254030	6644.298544	8.010317	-0.084343	4.402263
435.363675	6652.306366	8.015322	-0.084368	4.404813
435.508869	6660.322274	8.020326	-0.084401	4.407365
435.757494	6668.353149	8.025331	-0.084452	4.409920
435.875971	6676.412300	8.030336	-0.084480	4.412483
435.920730	6684.410400	8.035341	-0.084493	4.415024
436.250488	6692.434672	8.040346	-0.084560	4.417573
436.363280	6700.411633	8.045350	-0.084586	4.420104
436.470794	6708.459271	8.050355	-0.084612	4.422657
436.476656	6716.462739	8.055360	-0.084618	4.425193
436.661603	6724.483200	8.060365	-0.084658	4.427735
436.877720	6732.550357	8.065370	-0.084703	4.430290
436.882027	6740.534210	8.070374	-0.084709	4.432816
437.407529	6748.576199	8.075379	-0.084813	4.435361
437.677298	6756.554110	8.080384	-0.084868	4.437883
437.824279	6764.523366	8.085389	-0.084901	4.440400
438.191015	6772.566748	8.090394	-0.084974	4.442941
438.447743	6780.557805	8.095398	-0.085027	4.445463
438.617255	6788.616940	8.100403	-0.085064	4.448004
438.673361	6796.606759	8.105408	-0.085080	4.450522
438.972181	6804.697520	8.110413	-0.085141	4.453071
439.154941	6812.684216	8.115418	-0.085180	4.455586
439.085545	6820.647511	8.120422	-0.085173	4.458091
439.617025	6828.703114	8.125427	-0.085277	4.460625
439.739792	6836.689352	8.130432	-0.085305	4.463135
439.854830	6844.668290	8.135437	-0.085332	4.465641
440.186256	6852.755014	8.140442	-0.085399	4.468180
440.314819	6860.746970	8.145446	-0.085428	4.470687
440.535948	6868.819261	8.150451	-0.085475	4.473219
440.527799	6876.798765	8.155456	-0.085478	4.475719
440.764688	6884.784403	8.160461	-0.085528	4.478220
441.114120	6892.816470	8.165466	-0.085598	4.480735
441.346862	6900.774383	8.170470	-0.085647	4.483225
441.232229	6908.802842	8.175475	-0.085631	4.485734
441.388532	6916.863390	8.180480	-0.085665	4.488253
441.461083	6924.870242	8.185485	-0.085684	4.490753
441.831401	6932.938159	8.190490	-0.085758	4.493272
442.034633	6940.944029	8.195494	-0.085801	4.495770
442.100164	6948.935494	8.200499	-0.085819	4.498261
442.257077	6956.911672	8.205504	-0.085853	4.500747
442.596881	6964.910008	8.210509	-0.085922	4.503238
442.784346	6973.004344	8.215514	-0.085962	4.505757
442.598693	6980.994506	8.220518	-0.085933	4.508242
442.961871	6989.006299	8.225523	-0.086006	4.510734
443.366559	6997.074662	8.230528	-0.086087	4.513241
443.545220	7005.094851	8.235533	-0.086125	4.515732
443.776008	7013.087014	8.240538	-0.086173	4.518213
443.787335	7021.070922	8.245542	-0.086181	4.520689
444.026302	7029.061894	8.250547	-0.086231	4.523167
444.052667	7037.075710	8.255552	-0.086241	4.525650
444.698484	7045.084444	8.260557	-0.086366	4.528131
445.134287	7053.140334	8.265562	-0.086453	4.530624
445.610278	7061.151163	8.270566	-0.086547	4.533103
446.058342	7069.191966	8.275571	-0.086636	4.535589
446.030460	7077.165855	8.280576	-0.086636	4.538053
446.282287	7085.165040	8.285581	-0.086688	4.540523
446.624263	7093.201684	8.290586	-0.086757	4.543004
446.642836	7101.241182	8.295590	-0.086766	4.545484
446.955070	7109.302147	8.300595	-0.086829	4.547969
447.023625	7117.253033	8.305600	-0.086847	4.550419
447.331890	7125.265177	8.310605	-0.086910	4.552887
447.472487	7133.321941	8.315610	-0.086941	4.555367
447.534954	7141.335694	8.320614	-0.086958	4.557832
447.701181	7149.345378	8.325619	-0.086995	4.560294
447.859357	7157.379815	8.330624	-0.087029	4.562763
447.844715	7165.313372	8.335629	-0.087032	4.565200
447.998362	7173.384042	8.340634	-0.087066	4.567677
448.163306	7181.385842	8.345638	-0.087102	4.570132
448.458794	7189.455917	8.350643	-0.087162	4.572606
448.428886	7197.499498	8.355648	-0.087162	4.575071
448.602657	7205.464486	8.360653	-0.087200	4.577511
449.004247	7213.459990	8.365658	-0.087280	4.579958
449.264276	7221.450928	8.370662	-0.087333	4.582403
449.402255	7229.492332	8.375667	-0.087364	4.584862
449.611538	7237.536009	8.380672	-0.087409	4.587320
449.725574	7245.561662	8.385677	-0.087435	4.589772
449.676848	7253.622426	8.390682	-0.087431	4.592232
449.948965	7261.588130	8.395686	-0.087487	4.594663
450.127503	7269.643171	8.400691	-0.087526	4.597119
450.132679	7277.558112	8.405696	-0.087532	4.599532
450.535560	7285.589076	8.410701	-0.087613	4.601978
450.831101	7293.598784	8.415706	-0.087673	4.604417
450.714841	7301.627970	8.420710	-0.087657	4.606860
450.924137	7309.667831	8.425715	-0.087701	4.609305
451.370301	7317.727717	8.430720	-0.087789	4.611755
451.581805	7325.705429	8.435725	-0.087834	4.614179
451.701392	7333.746939	8.440730	-0.087861	4.616620
451.728404	7341.666041	8.445734	-0.087872	4.619024
451.939539	7349.749205	8.450739	-0.087916	4.621475
452.061369	7357.733560	8.455744	-0.087944	4.623896
452.182022	7365.814908	8.460749	-0.087972	4.626344
452.664173	7373.802485	8.465754	-0.088067	4.628763
452.584698	7381.771284	8.470758	-0.088058	4.631175
452.882018	7389.856768	8.475763	-0.088118	4.633621
453.087994	7397.901961	8.480768	-0.088162	4.636053
453.131988	7405.804206	8.485773	-0.088176	4.638441
453.473179	7413.885261	8.490778	-0.088244	4.640882
453.394695	7421.855401	8.495782	-0.088235	4.643288
453.683547	7429.890049	8.500787	-0.088294	4.645712
453.884031	7437.872739	8.505792	-0.088337	4.648119
454.017433	7445.859371	8.510797	-0.088367	4.650526
454.302980	7453.970083	8.515802	-0.088425	4.652969
454.313408	7461.986416	8.520806	-0.088433	4.655382
454.684594	7469.985822	8.525811	-0.088507	4.657789
454.695068	7477.974220	8.530816	-0.088514	4.660192
454.763501	7485.989907	8.535821	-0.088532	4.662601
454.961196	7494.020863	8.540826	-0.088575	4.665014
455.058479	7502.027425	8.545830	-0.088598	4.667418
455.344044	7510.043409	8.550835	-0.088656	4.669824
455.537451	7518.131799	8.555840	-0.088698	4.672250
455.633756	7526.163470	8.560845	-0.088721	4.674658
455.729786	7534.183696	8.565850	-0.088744	4.677061
455.877682	7542.056214	8.570855	-0.088777	4.679419
456.001327	7550.136012	8.575859	-0.088805	4.681838
456.603525	7558.091864	8.580864	-0.088923	4.684217
456.734643	7566.162457	8.585869	-0.088953	4.686630
456.752013	7574.141363	8.590874	-0.088961	4.689015
456.894943	7582.175465	8.595879	-0.088993	4.691415
457.043799	7590.237844	8.600883	-0.089026	4.693822
456.976784	7598.224240	8.605888	-0.089019	4.696206
457.180569	7606.177091	8.610893	-0.089062	4.698578
457.434625	7614.258062	8.615898	-0.089115	4.700986
457.430576	7622.203804	8.620903	-0.089119	4.703354
457.735253	7630.283110	8.625907	-0.089181	4.705759
457.891214	7638.306608	8.630912	-0.089216	4.708147
457.968844	7646.254816	8.635917	-0.089235	4.710512
458.091651	7654.409098	8.640922	-0.089264	4.712937
458.215943	7662.363821	8.645927	-0.089292	4.715301
458.467007	7670.401606	8.650931	-0.089344	4.717688
458.805243	7678.353979	8.655936	-0.089412	4.720048
458.857498	7686.336002	8.660941	-0.089427	4.722417
459.227743	7694.394809	8.665946	-0.089502	4.724806
459.196222	7702.405190	8.670951	-0.089501	4.727181
459.286367	7710.430377	8.675955	-0.089523	4.729558
459.527370	7718.512948	8.680960	-0.089573	4.731951
459.650211	7726.478143	8.685965	-0.089602	4.734309
459.798389	7734.524697	8.690970	-0.089634	4.736689
460.006932	7742.450390	8.695975	-0.089679	4.739032
460.192646	7750.536194	8.700979	-0.089718	4.741421
460.390497	7758.537506	8.705984	-0.089761	4.743784
460.285194	7766.535017	8.710989	-0.089746	4.746146
460.673277	7774.572134	8.715994	-0.089824	4.748517
460.991877	7782.580803	8.720999	-0.089889	4.750878
460.953378	7790.653695	8.726003	-0.089887	4.753258
461.068943	7798.676434	8.731008	-0.089914	4.755622
461.265677	7806.607787	8.736013	-0.089955	4.757957
461.289858	7814.632071	8.741018	-0.089965	4.760319
461.422090	7822.623598	8.746023	-0.089995	4.762670
461.533261	7830.614598	8.751027	-0.090021	4.765020
461.940408	7838.654041	8.756032	-0.090102	4.767381
462.156522	7846.647135	8.761037	-0.090148	4.769729
462.290098	7854.703704	8.766042	-0.090178	4.772094
462.483468	7862.757740	8.771047	-0.090219	4.774457
462.373964	7870.788020	8.776051	-0.090204	4.776813
462.502437	7878.760775	8.781056	-0.090233	4.779150
462.687519	7886.727681	8.786061	-0.090273	4.781484
462.924765	7894.776106	8.791066	-0.090323	4.783841
463.111425	7902.786225	8.796071	-0.090363	4.786185
463.291469	7910.830128	8.801075	-0.090402	4.788538
463.586997	7918.843581	8.806080	-0.090462	4.790881
463.675212	7926.866320	8.811085	-0.090484	4.793225
463.845866	7934.913596	8.816090	-0.090521	4.795576
464.050707	7942.893812	8.821095	-0.090564	4.797906
464.162292	7950.886080	8.826099	-0.090590	4.800238
464.330644	7958.962438	8.831104	-0.090627	4.802594
464.619442	7966.832843	8.836109	-0.090686	4.804887
464.705275	7974.967211	8.841114	-0.090707	4.807258
464.607890	7982.873081	8.846119	-0.090694	4.809562
464.875458	7990.416974	8.851123	-0.090749	4.811757
465.259113	7995.048487	8.856128	-0.090824	4.813103

465.203360	7997.556727	8.861133	-0.090815	4.813834
465.355969	7998.977808	8.866138	-0.090845	4.814246
465.384062	7999.417156	8.871143	-0.090850	4.814374
465.499156	8000.553382	8.876147	-0.090872	4.814704
465.538212	8000.525109	8.881152	-0.090880	4.814695
465.791759	8000.532831	8.886157	-0.090927	4.814696
466.010654	8000.560328	8.891162	-0.090968	4.814703
466.065263	8000.519454	8.896167	-0.090978	4.814691
466.344985	8000.489011	8.901171	-0.091030	4.814681
466.545445	8000.544081	8.906176	-0.091068	4.814696
466.397868	8000.514645	8.911181	-0.091040	4.814688
466.481019	8000.552612	8.916186	-0.091056	4.814699
466.513923	8000.515646	8.921191	-0.091062	4.814688
466.519742	8000.507172	8.926195	-0.091063	4.814685
466.444407	8000.526233	8.931200	-0.091049	4.814691
466.494997	8000.526065	8.936205	-0.091059	4.814691
466.717672	8000.536460	8.941210	-0.091100	4.814693
466.598687	8000.511823	8.946215	-0.091078	4.814686
466.714233	8000.531049	8.951219	-0.091100	4.814691
466.801254	8000.571232	8.956224	-0.091116	4.814702
466.786038	8000.509804	8.961229	-0.091113	4.814685
466.997175	8000.568284	8.966234	-0.091153	4.814700
467.110083	8000.517713	8.971239	-0.091174	4.814685
467.166698	8000.562722	8.976243	-0.091185	4.814698
467.146735	8000.569888	8.981248	-0.091181	4.814700
467.048004	8000.537025	8.986253	-0.091163	4.814691
467.124101	8000.554479	8.991258	-0.091177	4.814696
467.113945	8000.529625	8.996263	-0.091175	4.814689
467.219390	8000.545454	9.001267	-0.091195	4.814693
467.178915	8000.574791	9.006272	-0.091187	4.814701
466.976838	8000.532583	9.011277	-0.091150	4.814690
467.220527	8000.572325	9.016282	-0.091195	4.814700
467.239273	8000.523303	9.021287	-0.091199	4.814686
467.293174	8000.534998	9.026291	-0.091209	4.814689
467.218323	8000.535825	9.031296	-0.091195	4.814690
467.280970	8000.503678	9.036301	-0.091207	4.814680
467.373313	8000.535371	9.041306	-0.091224	4.814689
467.284854	8000.531663	9.046311	-0.091208	4.814688
467.252916	8000.562224	9.051315	-0.091202	4.814697
467.584233	8000.565964	9.056320	-0.091264	4.814697
467.324819	8000.543127	9.061325	-0.091215	4.814691
467.286302	8000.567133	9.066330	-0.091208	4.814699
467.254896	8000.535464	9.071335	-0.091203	4.814690
467.494828	8000.510754	9.076339	-0.091247	4.814681
467.428575	8000.569680	9.081344	-0.091235	4.814699
467.340835	8000.570278	9.086349	-0.091219	4.814699
467.736154	8000.596616	9.091354	-0.091293	4.814705
467.713442	8000.566173	9.096359	-0.091288	4.814696
467.706335	8000.538154	9.101363	-0.091287	4.814688
467.717382	8000.578063	9.106368	-0.091289	4.814700
467.608067	8000.545012	9.111373	-0.091269	4.814690
467.683782	8000.596799	9.116378	-0.091283	4.814705
467.579640	8000.568131	9.121383	-0.091264	4.814697
467.702487	8000.552076	9.126387	-0.091287	4.814692
467.517924	8000.565979	9.131392	-0.091253	4.814697
467.746236	8000.492774	9.136397	-0.091295	4.814675
467.921402	8000.514133	9.141402	-0.091328	4.814680
467.704860	8000.517810	9.146407	-0.091288	4.814682
467.598564	8000.520225	9.151411	-0.091268	4.814683
467.774314	8000.539447	9.156416	-0.091301	4.814688
467.910679	8000.538656	9.161421	-0.091326	4.814687
467.998931	8000.586374	9.166426	-0.091343	4.814700
467.778854	8000.507358	9.171431	-0.091302	4.814679
467.770756	8000.448202	9.176435	-0.091300	4.814661
467.813335	8000.550910	9.181440	-0.091308	4.814691
467.712430	8000.495473	9.186445	-0.091290	4.814676
467.895548	8000.535215	9.191450	-0.091324	4.814686
467.916801	8000.488383	9.196455	-0.091328	4.814672
467.853038	8000.524819	9.201459	-0.091316	4.814683
467.904476	8000.551494	9.206464	-0.091326	4.814691
467.899440	8000.485953	9.211469	-0.091325	4.814672
468.007303	8000.499679	9.216474	-0.091345	4.814675
467.956073	8000.533117	9.221479	-0.091336	4.814685
468.057004	8000.566037	9.226483	-0.091354	4.814694
468.154752	8000.550609	9.231488	-0.091373	4.814689
468.114135	8000.560628	9.236493	-0.091365	4.814692
468.243655	8000.584396	9.241498	-0.091390	4.814699
468.058677	8000.537124	9.246503	-0.091355	4.814686
467.997840	8000.545710	9.251507	-0.091344	4.814689
467.983937	8000.558349	9.256512	-0.091341	4.814692
468.158483	8000.502432	9.261517	-0.091374	4.814675
468.198125	8000.576116	9.266522	-0.091381	4.814696
468.100029	8000.556140	9.271527	-0.091363	4.814691
468.202945	8000.561194	9.276531	-0.091382	4.814692
468.300269	8000.561856	9.281536	-0.091401	4.814692
467.923051	8000.573412	9.286541	-0.091331	4.814697
468.202825	8000.527948	9.291546	-0.091383	4.814682
468.124175	8000.506171	9.296551	-0.091368	4.814676
468.046441	8000.536993	9.301555	-0.091354	4.814686
468.218247	8000.530392	9.306560	-0.091386	4.814683
468.139207	8000.560118	9.311565	-0.091371	4.814692
468.319923	8000.582649	9.316570	-0.091405	4.814698
468.344002	8000.551964	9.321575	-0.091409	4.814689
468.373689	8000.580400	9.326579	-0.091415	4.814697
468.466785	8000.576694	9.331584	-0.091433	4.814695
468.352350	8000.554282	9.336589	-0.091411	4.814689
468.523692	8000.545526	9.341594	-0.091443	4.814686
468.376070	8000.528964	9.346599	-0.091416	4.814682
468.244196	8000.474048	9.351603	-0.091391	4.814666
468.138918	8000.560184	9.356608	-0.091372	4.814692
468.191011	8000.579359	9.361613	-0.091382	4.814697
468.543272	8000.467575	9.366618	-0.091447	4.814663
468.338170	8000.511161	9.371623	-0.091409	4.814677
468.366526	8000.500940	9.376627	-0.091415	4.814674
468.270537	8000.567925	9.381632	-0.091397	4.814694
468.320999	8000.529123	9.386637	-0.091406	4.814682
468.279578	8000.544492	9.391642	-0.091399	4.814687
468.415846	8000.556577	9.396647	-0.091424	4.814690
468.468302	8000.561808	9.401651	-0.091434	4.814691
468.455945	8000.581986	9.406656	-0.091432	4.814697
468.279952	8000.542384	9.411661	-0.091399	4.814686
468.284154	8000.576807	9.416666	-0.091400	4.814696
468.178551	8000.560990	9.421671	-0.091380	4.814692
468.186361	8000.567575	9.426675	-0.091382	4.814694
468.356936	8000.568464	9.431680	-0.091414	4.814693
468.380000	8000.558150	9.436685	-0.091418	4.814690
468.257871	8000.563502	9.441690	-0.091395	4.814692
468.315855	8000.546296	9.446695	-0.091406	4.814687
468.309889	8000.566588	9.451699	-0.091405	4.814693
468.352601	8000.586670	9.456704	-0.091413	4.814699
468.308509	8000.526873	9.461709	-0.091405	4.814681
468.537868	8000.558853	9.466714	-0.091448	4.814690
468.420177	8000.538529	9.471719	-0.091426	4.814684
468.346355	8000.514691	9.476723	-0.091412	4.814678
468.350987	8000.590973	9.481728	-0.091413	4.814700
468.474868	8000.534158	9.486733	-0.091437	4.814683
468.517096	8000.602523	9.491738	-0.091445	4.814702
468.403380	8000.584415	9.496743	-0.091423	4.814698
468.576993	8000.600382	9.501747	-0.091456	4.814701
468.482030	8000.598704	9.506752	-0.091438	4.814701
468.354684	8000.582501	9.511757	-0.091415	4.814697
468.465874	8000.588775	9.516762	-0.091435	4.814699
468.449446	8000.484398	9.521767	-0.091432	4.814668
468.586476	8000.532982	9.526771	-0.091458	4.814682
468.630625	8000.576699	9.531776	-0.091466	4.814694
468.389375	8000.573498	9.536781	-0.091422	4.814695
468.346914	8000.571680	9.541786	-0.091414	4.814694
468.715314	8000.579300	9.546791	-0.091482	4.814695
468.696262	8000.566092	9.551795	-0.091479	4.814691
468.675338	8000.578606	9.556800	-0.091475	4.814695
468.555406	8000.570046	9.561805	-0.091453	4.814693
468.763927	8000.597364	9.566810	-0.091492	4.814700
468.644500	8000.579155	9.571815	-0.091470	4.814695
468.591429	8000.584660	9.576819	-0.091460	4.814697
468.629354	8000.625047	9.581824	-0.091467	4.814708
468.473813	8000.565418	9.586829	-0.091438	4.814692
468.616869	8000.599086	9.591834	-0.091465	4.814701
468.621803	8000.469332	9.596839	-0.091466	4.814663
468.470516	8000.571822	9.601843	-0.091438	4.814694
468.445654	8000.616460	9.606848	-0.091433	4.814707
468.534420	8000.592288	9.611853	-0.091450	4.814699
468.815907	8000.626268	9.616858	-0.091502	4.814708
468.572866	8000.551134	9.621863	-0.091457	4.814687
468.555954	8000.540111	9.626867	-0.091454	4.814684
468.609092	8000.560378	9.631872	-0.091464	4.814690
468.651044	8000.512840	9.636877	-0.091472	4.814676
468.689482	8000.541431	9.641882	-0.091479	4.814684
468.639352	8000.574890	9.646887	-0.091470	4.814694
468.808786	8000.482396	9.651891	-0.091501	4.814666
468.830633	8000.595471	9.656896	-0.091506	4.814699
468.652578	8000.546174	9.661901	-0.091473	4.814685
468.830112	8000.594405	9.666906	-0.091506	4.814698
468.690031	8000.564024	9.671911	-0.091480	4.814690
468.410310	8000.579457	9.676915	-0.091428	4.814696
468.577519	8000.583506	9.681920	-0.091459	4.814696
468.499281	8000.533834	9.686925	-0.091444	4.814682
468.652771	8000.595589	9.691930	-0.091473	4.814700
468.550930	8000.537986	9.696935	-0.091454	4.814683
468.752723	8000.511528	9.701939	-0.091492	4.814675
468.612611	8000.594900	9.706944	-0.091466	4.814700
468.533298	8000.582768	9.711949	-0.091451	4.814696
468.799495	8000.554234	9.716954	-0.091501	4.814687
468.844352	8000.470260	9.721959	-0.091509	4.814662
468.668701	8000.572318	9.726963	-0.091477	4.814693
468.810519	8000.585575	9.731968	-0.091503	4.814696
468.744956	8000.552225	9.736973	-0.091491	4.814686
468.630536	8000.600639	9.741978	-0.091470	4.814701
468.662616	8000.559364	9.746983	-0.091476	4.814689
468.771194	8000.563445	9.751987	-0.091496	4.814690
468.746063	8000.610225	9.756992	-0.091492	4.814703
468.573045	8000.588919	9.761997	-0.091459	4.814698
469.024301	8000.606596	9.767002	-0.091544	4.814701
469.094887	8000.597125	9.772007	-0.091557	4.814698
468.876961	8000.471999	9.777011	-0.091516	4.814662
468.812770	8000.600718	9.782016	-0.091504	4.814700
468.819035	8000.584740	9.787021	-0.091506	4.814695
468.781278	8000.601248	9.792026	-0.091499	4.814700
468.787891	8000.560594	9.797031	-0.091500	4.814689
468.753375	8000.549257	9.802035	-0.091494	4.814685
468.893504	8000.580728	9.807040	-0.091520	4.814694
468.631904	8000.523508	9.812045	-0.091471	4.814679
468.783651	8000.529429	9.817050	-0.091500	4.814680
468.842551	8000.564823	9.822055	-0.091511	4.814690
468.682388	8000.583450	9.827059	-0.091481	4.814696
468.827982	8000.595701	9.832064	-0.091508	4.814699
468.852682	8000.522101	9.837069	-0.091513	4.814677
468.838790	8000.546544	9.842074	-0.091510	4.814684
468.808046	8000.550299	9.847079	-0.091505	4.814685
468.799015	8000.563024	9.852083	-0.091503	4.814689
468.982194	8000.570576	9.857088	-0.091537	4.814690
468.775913	8000.591605	9.862093	-0.091499	4.814698
468.818022	8000.604165	9.867098	-0.091507	4.814701
468.788109	8000.580033	9.872103	-0.091501	4.814694
468.743239	8000.473003	9.877107	-0.091493	4.814663
468.939136	8000.604192	9.882112	-0.091530	4.814700
468.894591	8000.584093	9.887117	-0.091521	4.814695
468.965213	8000.623988	9.892122	-0.091535	4.814706
468.914115	8000.589821	9.897127	-0.091525	4.814696
469.002941	8000.518432	9.902131	-0.091542	4.814675
468.827018	8000.578632	9.907136	-0.091509	4.814694
468.711502	8000.565858	9.912141	-0.091488	4.814690
468.859452	8000.608199	9.917146	-0.091515	4.814702
468.896907	8000.498338	9.922151	-0.091522	4.814670
468.945213	8000.596859	9.927155	-0.091532	4.814698
468.834876	8000.616371	9.932160	-0.091511	4.814705
468.894556	8000.593830	9.937165	-0.091522	4.814698
468.849074	8000.616639	9.942170	-0.091514	4.814705
469.032395	8000.583415	9.947175	-0.091548	4.814694
468.969815	8000.536166	9.952179	-0.091536	4.814681
469.016718	8000.571348	9.957184	-0.091545	4.814690
468.718959	8000.530656	9.962189	-0.091490	4.814680
468.906807	8000.596241	9.967194	-0.091525	4.814698
469.094325	8000.486897	9.972199	-0.091560	4.814666
469.003039	8000.602258	9.977203	-0.091543	4.814700
468.851120	8000.600642	9.982208	-0.091515	4.814700
468.830882	8000.567023	9.987213	-0.091511	4.814690
468.905321	8000.579084	9.992218	-0.091525	4.814693
468.920092	8000.557891	9.997223	-0.091528	4.814687
469.025935	8000.520071	10.002227	-0.091548	4.814676
469.153767	8000.547031	10.007232	-0.091572	4.814683
469.004011	8000.541161	10.012237	-0.091544	4.814682
469.092384	8000.554542	10.017242	-0.091560	4.814685
468.852957	8000.569616	10.022247	-0.091516	4.814691
469.026715	8000.588806	10.027251	-0.091548	4.814695
469.047051	8000.624589	10.032256	-0.091552	4.814706
468.897723	8000.541460	10.037261	-0.091524	4.814682
469.056868	8000.514245	10.042266	-0.091554	4.814674
469.014309	8000.570374	10.047271	-0.091546	4.814690
469.101002	8000.539727	10.052275	-0.091563	4.814681
469.211687	8000.510578	10.057280	-0.091583	4.814672
469.204003	8000.527620	10.062285	-0.091582	4.814677
469.217805	8000.558994	10.067290	-0.091585	4.814686
469.291765	8000.588217	10.072295	-0.091598	4.814694
469.187981	8000.546676	10.077299	-0.091579	4.814682
469.158629	8000.586942	10.082304	-0.091574	4.814694
469.042821	8000.612796	10.087309	-0.091552	4.814702
469.297722	8000.637720	10.092314	-0.091600	4.814708
469.180149	8000.493984	10.097319	-0.091578	4.814667
469.167824	8000.594649	10.102323	-0.091576	4.814696
469.125972	8000.613231	10.107328	-0.091568	4.814702
469.190956	8000.557516	10.112333	-0.091580	4.814685
469.145867	8000.557796	10.117338	-0.091572	4.814686
469.205236	8000.594272	10.122343	-0.091583	4.814696
469.102893	8000.575293	10.127347	-0.091564	4.814691
469.376304	8000.566204	10.132352	-0.091615	4.814687
469.136402	8000.582342	10.137357	-0.091571	4.814693
469.302878	8000.556331	10.142362	-0.091602	4.814685
469.279847	8000.557003	10.147367	-0.091597	4.814685
469.345718	8000.517400	10.152371	-0.091610	4.814673
469.339740	8000.570960	10.157376	-0.091609	4.814689
469.219673	8000.540934	10.162381	-0.091586	4.814681
469.279899	8000.572060	10.167386	-0.091598	4.814689
469.347502	8000.501367	10.172391	-0.091610	4.814668
469.222640	8000.568912	10.177395	-0.091587	4.814689
469.218126	8000.638595	10.182400	-0.091587	4.814709
469.154659	8000.590258	10.187405	-0.091575	4.814695
469.239630	8000.557433	10.192410	-0.091591	4.814685
469.157466	8000.566714	10.197415	-0.091575	4.814688
469.076919	8000.563145	10.202419	-0.091561	4.814688
469.299917	8000.496284	10.207424	-0.091602	4.814667
469.140985	8000.522446	10.212429	-0.091573	4.814676
469.226419	8000.536848	10.217434	-0.091589	4.814679
469.386971	8000.586926	10.222439	-0.091619	4.814693
469.220869	8000.580765	10.227443	-0.091588	4.814692
469.188740	8000.605958	10.232448	-0.091582	4.814700
469.411465	8000.527287	10.237453	-0.091623	4.814676
469.458674	8000.594669	10.242458	-0.091632	4.814695
469.359846	8000.544630	10.247463	-0.091614	4.814681
469.166888	8000.561602	10.252467	-0.091578	4.814687
469.289802	8000.601353	10.257472	-0.091601	4.814698
469.136477	8000.567517	10.262477	-0.091573	4.814689
469.231941	8000.560635	10.267482	-0.091591	4.814686
469.235590	8000.588609	10.272487	-0.091591	4.814694
469.180963	8000.529697	10.277491	-0.091581	4.814677
469.236974	8000.597235	10.282496	-0.091592	4.814697
469.192257	8000.551377	10.287501	-0.091583	4.814684
469.329183	8000.539865	10.292506	-0.091609	4.814680
469.456341	8000.594715	10.297511	-0.091633	4.814695
469.326810	8000.514083	10.302515	-0.091609	4.814672
469.315013	8000.583636	10.307520	-0.091607	4.814692
469.232902	8000.517797	10.312525	-0.091591	4.814674
469.412588	8000.595043	10.317530	-0.091625	4.814695
469.307281	8000.599620	10.322535	-0.091605	4.814697
469.402487	8000.591660	10.327539	-0.091623	4.814694
469.607387	8000.545941	10.332544	-0.091661	4.814680
469.249240	8000.572857	10.337549	-0.091595	4.814690
469.353630	8000.620864	10.342554	-0.091614	4.814703
469.336445	8000.598031	10.347559	-0.091611	4.814696
469.218152	8000.585207	10.352563	-0.091589	4.814693
469.402761	8000.513372	10.357568	-0.091624	4.814671
469.355744	8000.540447	10.362573	-0.091615	4.814680
469.386207	8000.587141	10.367578	-0.091621	4.814693
469.394238	8000.605536	10.372583	-0.091623	4.814698
469.365739	8000.581428	10.377587	-0.091617	4.814691
469.443371	8000.594619	10.382592	-0.091632	4.814695
469.242712	8000.566382	10.387597	-0.091595	4.814688
469.395098	8000.614168	10.392602	-0.091623	4.814701
469.549794	8000.525704	10.397607	-0.091652	4.814674
469.256031	8000.555910	10.402611	-0.091597	4.814685
469.404727	8000.595046	10.407616	-0.091625	4.814695
469.362782	8000.610406	10.412621	-0.091617	4.814700
469.462131	8000.601447	10.417626	-0.091636	4.814697
469.337617	8000.614268	10.422631	-0.091613	4.814701
469.363265	8000.524586	10.427635	-0.091618	4.814675
469.448741	8000.542209	10.432640	-0.091634	4.814680
469.365877	8000.526794	10.437645	-0.091618	4.814676
469.508244	8000.592646	10.442650	-0.091645	4.814694
469.566790	8000.579743	10.447655	-0.091656	4.814690
469.572696	8000.516539	10.452659	-0.091657	4.814671
469.633595	8000.564848	10.457664	-0.091668	4.814685
469.408928	8000.539403	10.462669	-0.091627	4.814679
469.545903	8000.528965	10.467674	-0.091652	4.814675
469.362107	8000.578294	10.472679	-0.091618	4.814690
469.502031	8000.533568	10.477683	-0.091644	4.814677
469.653200	8000.599576	10.482688	-0.091673	4.814695
469.524485	8000.570470	10.487693	-0.091649	4.814687
469.510948	8000.583115	10.492698	-0.091646	4.814691
469.576830	8000.510245	10.497703	-0.091659	4.814670
469.439783	8000.541087	10.502707	-0.091633	4.814679
469.504937	8000.601276	10.507712	-0.091645	4.814696
469.478680	8000.610476	10.512717	-0.091641	4.814699
469.411913	8000.592128	10.517722	-0.091628	4.814694
469.404338	8000.593074	10.522727	-0.091627	4.814695
469.488762	8000.581703	10.527731	-0.091643	4.814691
469.718635	8000.571842	10.532736	-0.091686	4.814687
469.340549	8000.561917	10.537741	-0.091615	4.814686
469.333007	8000.613303	10.542746	-0.091614	4.814701
469.547571	8000.486195	10.547751	-0.091654	4.814663
469.335058	8000.581160	10.552755	-0.091614	4.814691
469.415261	8000.608348	10.557760	-0.091629	4.814699
469.485517	8000.573116	10.562765	-0.091643	4.814688
469.537614	8000.591219	10.567770	-0.091652	4.814693
469.598993	8000.577293	10.572775	-0.091664	4.814689
469.472777	8000.597596	10.577779	-0.091641	4.814695
469.577814	8000.595176	10.582784	-0.091660	4.814694
469.601773	8000.568781	10.587789	-0.091665	4.814686
469.554257	8000.484239	10.592794	-0.091656	4.814662
469.557657	8000.598062	10.597799	-0.091657	4.814695
469.636266	8000.586588	10.602803	-0.091671	4.814691
469.600451	8000.587033	10.607808	-0.091665	4.814692
469.285807	8000.565356	10.612813	-0.091606	4.814687
469.506607	8000.602553	10.617818	-0.091647	4.814697
469.494384	8000.599124	10.622823	-0.091645	4.814696
469.308927	8000.569010	10.627827	-0.091611	4.814688
469.607667	8000.523884	10.632832	-0.091667	4.814673
469.421426	8000.582828	10.637837	-0.091632	4.814691
469.443416	8000.580007	10.642842	-0.091636	4.814690
469.479530	8000.598900	10.647847	-0.091643	4.814696
469.570646	8000.606965	10.652851	-0.091660	4.814698
469.756084	8000.642461	10.657856	-0.091695	4.814707
469.617010	8000.608877	10.662861	-0.091669	4.814698
469.623912	8000.485594	10.667866	-0.091670	4.814662
469.701591	8000.590005	10.672871	-0.091685	4.814692
469.539815	8000.575335	10.677875	-0.091655	4.814689
469.712417	8000.625627	10.682880	-0.091687	4.814702
469.531563	8000.582717	10.687885	-0.091653	4.814691
469.549788	8000.622755	10.692890	-0.091657	4.814702
469.620875	8000.544611	10.697895	-0.091670	4.814679
469.648666	8000.591259	10.702899	-0.091675	4.814693
469.491059	8000.523005	10.707904	-0.091646	4.814674
469.603640	8000.610865	10.712909	-0.091667	4.814699
469.589910	8000.589166	10.717914	-0.091665	4.814692
469.606922	8000.616305	10.722919	-0.091668	4.814700
469.632741	8000.612479	10.727923	-0.091673	4.814699
469.837501	8000.621489	10.732928	-0.091711	4.814700
469.709617	8000.594543	10.737933	-0.091687	4.814693
469.410132	8000.582794	10.742938	-0.091632	4.814691
469.539229	8000.607630	10.747943	-0.091656	4.814698
469.574659	8000.567487	10.752947	-0.091662	4.814686
469.713677	8000.542061	10.757952	-0.091688	4.814678
469.499900	8000.609102	10.762957	-0.091649	4.814699
469.800376	8000.606934	10.767962	-0.091705	4.814696
469.664284	8000.589500	10.772967	-0.091679	4.814692
469.549655	8000.547766	10.777971	-0.091658	4.814681
469.556451	8000.604772	10.782976	-0.091660	4.814697
469.699316	8000.588000	10.787981	-0.091686	4.814691
469.612279	8000.597194	10.792986	-0.091670	4.814695
469.652099	8000.500251	10.797991	-0.091678	4.814666
469.758274	8000.547217	10.802995	-0.091697	4.814679
469.623503	8000.556637	10.808000	-0.091672	4.814683
469.453332	8000.575086	10.813005	-0.091641	4.814689
469.550582	8000.582187	10.818010	-0.091659	4.814690
469.659578	8000.601301	10.823015	-0.091679	4.814695
469.452659	8000.535391	10.828019	-0.091641	4.814677
469.591261	8000.584006	10.833024	-0.091667	4.814691
469.453796	8000.554744	10.838029	-0.091641	4.814683
469.455536	8000.574100	10.843034	-0.091642	4.814689
469.569816	8000.610478	10.848039	-0.091663	4.814699
469.547370	8000.563941	10.853043	-0.091659	4.814685
469.523882	8000.605386	10.858048	-0.091655	4.814697
469.515608	8000.536564	10.863053	-0.091653	4.814677
469.635087	8000.569815	10.868058	-0.091676	4.814686
469.566414	8000.601872	10.873063	-0.091663	4.814696
469.344083	8000.552859	10.878067	-0.091622	4.814683
469.709534	8000.564722	10.883072	-0.091690	4.814685
469.747590	8000.567552	10.888077	-0.091697	4.814685
469.649775	8000.587286	10.893082	-0.091679	4.814691
469.599561	8000.510208	10.898087	-0.091669	4.814669
469.602266	8000.568215	10.903091	-0.091670	4.814686
469.706307	8000.610851	10.908096	-0.091689	4.814698
469.571353	8000.552657	10.913101	-0.091664	4.814682
469.663285	8000.582200	10.918106	-0.091682	4.814690
469.806266	8000.592259	10.923111	-0.091708	4.814692
469.583385	8000.550748	10.928115	-0.091667	4.814681
469.647836	8000.557267	10.933120	-0.091679	4.814683
469.695233	8000.570994	10.938125	-0.091688	4.814686
469.730130	8000.578061	10.943130	-0.091694	4.814688
469.737679	8000.569617	10.948135	-0.091696	4.814686
469.717440	8000.535998	10.953139	-0.091692	4.814676
469.722237	8000.580091	10.958144	-0.091693	4.814689
469.628805	8000.560196	10.963149	-0.091676	4.814684
469.663726	8000.515751	10.968154	-0.091682	4.814671
469.709217	8000.564859	10.973159	-0.091691	4.814685
469.617263	8000.526746	10.978163	-0.091674	4.814674
469.724673	8000.565149	10.983168	-0.091694	4.814685
469.880139	8000.556113	10.988173	-0.091723	4.814681
469.765079	8000.562663	10.993178	-0.091702	4.814684
469.817981	8000.590440	10.998183	-0.091712	4.814691
469.693409	8000.545309	11.003187	-0.091689	4.814679
469.918344	8000.598677	11.008192	-0.091731	4.814693
469.740802	8000.567629	11.013197	-0.091698	4.814685
469.691369	8000.521687	11.018202	-0.091688	4.814672
469.869736	8000.466911	11.023207	-0.091722	4.814655
469.499724	8000.590201	11.028211	-0.091653	4.814693
469.502103	8000.636397	11.033216	-0.091654	4.814706
469.610663	8000.600772	11.038221	-0.091674	4.814695
469.623148	8000.559149	11.043226	-0.091676	4.814683
469.673523	8000.605124	11.048231	-0.091686	4.814696
469.652484	8000.575783	11.053235	-0.091682	4.814688
469.878824	8000.527225	11.058240	-0.091724	4.814673
469.743910	8000.607471	11.063245	-0.091699	4.814697
469.628136	8000.578594	11.068250	-0.091678	4.814689
469.855167	8000.631999	11.073255	-0.091720	4.814703
469.648176	8000.571453	11.078259	-0.091681	4.814687
469.683093	8000.543106	11.083264	-0.091688	4.814678
469.762472	8000.550962	11.088269	-0.091703	4.814680
469.753457	8000.514322	11.093274	-0.091701	4.814670
469.783643	8000.520232	11.098279	-0.091707	4.814671
469.740881	8000.589237	11.103283	-0.091699	4.814691
469.752639	8000.635600	11.108288	-0.091701	4.814705
469.611132	8000.593387	11.113293	-0.091675	4.814693
469.481369	8000.609335	11.118298	-0.091651	4.814699
469.641745	8000.544581	11.123303	-0.091681	4.814679
469.630604	8000.531513	11.128307	-0.091679	4.814675
469.651500	8000.631697	11.133312	-0.091683	4.814704
469.804018	8000.611877	11.138317	-0.091712	4.814698
469.708180	8000.545792	11.143322	-0.091694	4.814679
469.727063	8000.607306	11.148327	-0.091697	4.814697
469.692671	8000.575581	11.153331	-0.091691	4.814688
469.765444	8000.629467	11.158336	-0.091705	4.814703
469.635289	8000.487652	11.163341	-0.091680	4.814662
469.686110	8000.586220	11.168346	-0.091690	4.814691
469.922542	8000.618330	11.173351	-0.091734	4.814699
469.781286	8000.549292	11.178355	-0.091708	4.814680
469.757929	8000.598251	11.183360	-0.091704	4.814694
469.873584	8000.571337	11.188365	-0.091725	4.814685
469.941445	8000.546794	11.193370	-0.091738	4.814678
469.915797	8000.606445	11.198375	-0.091733	4.814695
469.808275	8000.585226	11.203379	-0.091713	4.814690
470.026935	8000.590190	11.208384	-0.091754	4.814690
469.830014	8000.586701	11.213389	-0.091718	4.814690
469.667551	8000.484019	11.218394	-0.091687	4.814661
469.783219	8000.603056	11.223399	-0.091709	4.814695
469.693795	8000.560696	11.228403	-0.091692	4.814683
469.693664	8000.560701	11.233408	-0.091692	4.814683
469.819819	8000.587633	11.238413	-0.091716	4.814690
469.799352	8000.589423	11.243418	-0.091712	4.814691
469.856258	8000.640881	11.248423	-0.091723	4.814706
469.795415	8000.576491	11.253427	-0.091712	4.814687
469.854844	8000.580774	11.258432	-0.091723	4.814688
469.694250	8000.572564	11.263437	-0.091693	4.814687
469.930249	8000.578909	11.268442	-0.091737	4.814687
469.855656	8000.535739	11.273447	-0.091723	4.814675
469.937322	8000.594075	11.278451	-0.091739	4.814692
469.879752	8000.597353	11.283456	-0.091728	4.814693
469.909332	8000.581789	11.288461	-0.091734	4.814688
470.019624	8000.545122	11.293466	-0.091754	4.814677
469.884826	8000.622150	11.298471	-0.091729	4.814700
469.678734	8000.499377	11.303475	-0.091691	4.814666
469.800360	8000.622812	11.308480	-0.091714	4.814701
469.855635	8000.631314	11.313485	-0.091724	4.814703
469.713070	8000.502156	11.318490	-0.091697	4.814666
469.843476	8000.602138	11.323495	-0.091722	4.814695
469.719634	8000.528045	11.328499	-0.091699	4.814674
469.893107	8000.628792	11.333504	-0.091731	4.814702
469.675012	8000.582000	11.338509	-0.091691	4.814690
469.731361	8000.598033	11.343514	-0.091701	4.814694
469.802033	8000.518808	11.348519	-0.091715	4.814671
469.608187	8000.609812	11.353523	-0.091679	4.814698
469.919528	8000.602471	11.358528	-0.091737	4.814694
469.709759	8000.601973	11.363533	-0.091698	4.814695
469.551150	8000.565896	11.368538	-0.091668	4.814685
469.697428	8000.592112	11.373543	-0.091696	4.814692
469.773178	8000.589172	11.378547	-0.091710	4.814691
469.777646	8000.592479	11.383552	-0.091711	4.814692
469.797819	8000.480162	11.388557	-0.091714	4.814659
469.796500	8000.594976	11.393562	-0.091714	4.814693
469.962706	8000.646229	11.398567	-0.091745	4.814707
469.732673	8000.612102	11.403571	-0.091703	4.814698
469.892674	8000.624610	11.408576	-0.091732	4.814701
469.864221	8000.587625	11.413581	-0.091727	4.814690
469.691746	8000.560960	11.418586	-0.091695	4.814683
469.870704	8000.531951	11.423591	-0.091729	4.814674
469.930866	8000.536247	11.428595	-0.091740	4.814675
469.781779	8000.623753	11.433600	-0.091712	4.814701
469.669384	8000.602448	11.438605	-0.091691	4.814695
469.652476	8000.590351	11.443610	-0.091688	4.814692
469.682740	8000.618799	11.448615	-0.091694	4.814700
469.666825	8000.562719	11.453619	-0.091691	4.814684
469.725453	8000.526207	11.458624	-0.091702	4.814673
469.916662	8000.574684	11.463629	-0.091738	4.814686
469.848629	8000.573484	11.468634	-0.091725	4.814686
469.835864	8000.515314	11.473639	-0.091723	4.814669
469.862330	8000.581255	11.478643	-0.091728	4.814688
469.897058	8000.621587	11.483648	-0.091735	4.814700
469.850776	8000.588578	11.488653	-0.091726	4.814690
469.917803	8000.577971	11.493658	-0.091739	4.814687
469.927001	8000.607118	11.498663	-0.091740	4.814695
469.625859	8000.574949	11.503667	-0.091684	4.814688
470.231280	8000.558880	11.508672	-0.091797	4.814680
470.201575	8000.624897	11.513677	-0.091792	4.814699
469.986734	8000.516991	11.518682	-0.091752	4.814669
469.917637	8000.625235	11.523687	-0.091739	4.814701
469.947595	8000.591434	11.528691	-0.091745	4.814691
469.952964	8000.621586	11.533696	-0.091746	4.814700
470.068455	8000.596816	11.538701	-0.091767	4.814692
469.961591	8000.597072	11.543706	-0.091748	4.814692
469.794988	8000.539389	11.548711	-0.091717	4.814676
469.844559	8000.575692	11.553715	-0.091726	4.814687
469.880960	8000.602103	11.558720	-0.091733	4.814694
469.936796	8000.614907	11.563725	-0.091743	4.814698
469.841085	8000.572435	11.568730	-0.091726	4.814686
469.955875	8000.613116	11.573735	-0.091747	4.814697
470.026330	8000.505984	11.578739	-0.091760	4.814666
469.854086	8000.578055	11.583744	-0.091728	4.814687
469.948858	8000.589405	11.588749	-0.091746	4.814690
469.936814	8000.609589	11.593754	-0.091744	4.814696
469.994306	8000.553740	11.598759	-0.091755	4.814680
469.925254	8000.604034	11.603763	-0.091742	4.814695
469.970424	8000.610210	11.608768	-0.091750	4.814696
470.043297	8000.500975	11.613773	-0.091764	4.814664
469.896026	8000.593880	11.618778	-0.091737	4.814692
469.974192	8000.633910	11.623783	-0.091751	4.814703
469.783316	8000.610138	11.628787	-0.091716	4.814697
469.885562	8000.551864	11.633792	-0.091735	4.814680
469.833246	8000.626065	11.638797	-0.091725	4.814701
469.771298	8000.607802	11.643802	-0.091714	4.814696
470.026519	8000.541513	11.648807	-0.091761	4.814676
469.825911	8000.603422	11.653811	-0.091724	4.814695
469.822988	8000.607670	11.658816	-0.091724	4.814696
469.849749	8000.618885	11.663821	-0.091729	4.814699
469.983515	8000.492488	11.668826	-0.091754	4.814662
470.042149	8000.634123	11.673831	-0.091765	4.814703
469.804740	8000.551573	11.678835	-0.091721	4.814680
470.079917	8000.606907	11.683840	-0.091772	4.814695
470.057923	8000.610817	11.688845	-0.091768	4.814696
469.923376	8000.615948	11.693850	-0.091743	4.814698
470.116402	8000.549628	11.698855	-0.091779	4.814678
469.872015	8000.619344	11.703859	-0.091734	4.814699
469.997569	8000.563631	11.708864	-0.091757	4.814682
470.041068	8000.508606	11.713869	-0.091765	4.814666
470.028836	8000.627519	11.718874	-0.091763	4.814701
469.984018	8000.535511	11.723879	-0.091755	4.814674
470.013724	8000.618681	11.728883	-0.091760	4.814698
470.190653	8000.555295	11.733888	-0.091793	4.814679
470.161765	8000.627766	11.738893	-0.091788	4.814700
469.995616	8000.500334	11.743898	-0.091757	4.814664
469.960181	8000.601664	11.748903	-0.091751	4.814694
469.885917	8000.599280	11.753907	-0.091737	4.814693
469.804441	8000.636475	11.758912	-0.091722	4.814705
469.858466	8000.612759	11.763917	-0.091732	4.814697
470.127425	8000.558520	11.768922	-0.091782	4.814680
470.060444	8000.541240	11.773927	-0.091770	4.814676
469.978765	8000.591310	11.778931	-0.091755	4.814690
470.083817	8000.614647	11.783936	-0.091774	4.814697
470.142090	8000.619983	11.788941	-0.091785	4.814698
469.947493	8000.596144	11.793946	-0.091749	4.814692
470.258306	8000.574843	11.798951	-0.091807	4.814684
470.155851	8000.558007	11.803955	-0.091788	4.814680
469.943036	8000.604674	11.808960	-0.091748	4.814695
470.233603	8000.514330	11.813965	-0.091803	4.814667
470.207465	8000.594362	11.818970	-0.091798	4.814690
470.065145	8000.619745	11.823975	-0.091771	4.814698
470.180781	8000.598197	11.828979	-0.091793	4.814691
470.309407	8000.592977	11.833984	-0.091817	4.814689
470.117555	8000.488699	11.838989	-0.091781	4.814660
469.951474	8000.596294	11.843994	-0.091751	4.814692
470.087569	8000.597646	11.848999	-0.091776	4.814692
470.083528	8000.577192	11.854003	-0.091775	4.814686
470.008006	8000.559761	11.859008	-0.091761	4.814681
470.104301	8000.600113	11.864013	-0.091779	4.814692
470.136845	8000.576016	11.869018	-0.091786	4.814685
470.147687	8000.539728	11.874023	-0.091788	4.814675
469.858373	8000.616159	11.879027	-0.091734	4.814698
469.903925	8000.633074	11.884032	-0.091742	4.814703
469.980574	8000.522833	11.889037	-0.091757	4.814671
469.952494	8000.603903	11.894042	-0.091752	4.814694
470.165431	8000.627011	11.899047	-0.091791	4.814700
470.175903	8000.606814	11.904051	-0.091793	4.814694
470.017664	8000.539621	11.909056	-0.091764	4.814675
469.912988	8000.633282	11.914061	-0.091745	4.814703
469.984805	8000.631346	11.919066	-0.091758	4.814702
470.091025	8000.590314	11.924071	-0.091778	4.814690
470.078185	8000.598679	11.929075	-0.091776	4.814692
470.228023	8000.505835	11.934080	-0.091804	4.814664
470.206110	8000.636382	11.939085	-0.091800	4.814702
470.026959	8000.585988	11.944090	-0.091766	4.814689
470.225334	8000.637813	11.949095	-0.091803	4.814703
470.312615	8000.573907	11.954099	-0.091820	4.814684
470.203075	8000.560164	11.959104	-0.091799	4.814680
470.227411	8000.635727	11.964109	-0.091804	4.814702
470.106562	8000.604612	11.969114	-0.091782	4.814694
470.114433	8000.548955	11.974119	-0.091783	4.814677
469.968725	8000.644034	11.979123	-0.091756	4.814706
470.037916	8000.493953	11.984128	-0.091769	4.814662
470.098702	8000.619529	11.989133	-0.091780	4.814698
470.025153	8000.577450	11.994138	-0.091767	4.814686
470.202617	8000.616025	11.999143	-0.091800	4.814696
470.209103	8000.581806	12.004147	-0.091801	4.814686
470.147903	8000.574288	12.009152	-0.091790	4.814685
470.248236	8000.628664	12.014157	-0.091809	4.814700
470.232226	8000.599411	12.019162	-0.091806	4.814691
470.075502	8000.623465	12.024167	-0.091777	4.814699
470.041335	8000.512329	12.029171	-0.091770	4.814667
469.930481	8000.574758	12.034176	-0.091750	4.814686
470.069248	8000.621231	12.039181	-0.091776	4.814699
469.974364	8000.597017	12.044186	-0.091758	4.814692
470.001916	8000.547075	12.049191	-0.091763	4.814677
470.094720	8000.506877	12.054195	-0.091781	4.814665
470.074629	8000.655700	12.059200	-0.091777	4.814709
470.220171	8000.547756	12.064205	-0.091804	4.814676
470.127030	8000.624451	12.069210	-0.091787	4.814699
470.141300	8000.551736	12.074215	-0.091790	4.814678
469.980414	8000.597180	12.079219	-0.091760	4.814692
470.088651	8000.638818	12.084224	-0.091780	4.814704
469.996702	8000.524509	12.089229	-0.091763	4.814671
470.079984	8000.585021	12.094234	-0.091779	4.814688
470.241041	8000.580377	12.099239	-0.091809	4.814686
470.251378	8000.538715	12.104243	-0.091811	4.814674
470.132358	8000.598853	12.109248	-0.091789	4.814692
470.224450	8000.612302	12.114253	-0.091806	4.814695
470.205151	8000.594796	12.119258	-0.091802	4.814690
470.317156	8000.637574	12.124263	-0.091823	4.814702
470.235166	8000.507344	12.129267	-0.091808	4.814665
470.265601	8000.606625	12.134272	-0.091814	4.814693
470.310128	8000.617083	12.139277	-0.091822	4.814696
469.980847	8000.570461	12.144282	-0.091761	4.814684
470.163718	8000.605912	12.149287	-0.091795	4.814694
470.160383	8000.592983	12.154291	-0.091795	4.814690
470.110917	8000.541673	12.159296	-0.091786	4.814675
470.256433	8000.501338	12.164301	-0.091813	4.814663
470.140766	8000.561536	12.169306	-0.091791	4.814681
470.278144	8000.630521	12.174311	-0.091817	4.814700
470.298552	8000.600843	12.179315	-0.091821	4.814691
470.305285	8000.555896	12.184320	-0.091822	4.814678
470.408443	8000.611396	12.189325	-0.091841	4.814694
469.913423	8000.552172	12.194330	-0.091749	4.814679
470.104680	8000.601723	12.199335	-0.091785	4.814693
470.102990	8000.463261	12.204339	-0.091785	4.814652
470.185906	8000.538791	12.209344	-0.091800	4.814674
470.016734	8000.601258	12.214349	-0.091769	4.814693
470.319736	8000.565867	12.219354	-0.091825	4.814681
470.365340	8000.612832	12.224359	-0.091834	4.814695
470.177151	8000.599838	12.229363	-0.091799	4.814692
470.111495	8000.578290	12.234368	-0.091787	4.814686
470.426884	8000.611803	12.239373	-0.091846	4.814694
470.210664	8000.553237	12.244378	-0.091806	4.814678
470.400982	8000.631749	12.249383	-0.091841	4.814700
470.457028	8000.599484	12.254387	-0.091852	4.814690
470.320481	8000.472577	12.259392	-0.091826	4.814654
470.412662	8000.595492	12.264397	-0.091843	4.814689
470.394440	8000.584444	12.269402	-0.091840	4.814686
470.327290	8000.615455	12.274407	-0.091828	4.814695
470.139486	8000.597102	12.279411	-0.091793	4.814691
470.125781	8000.597940	12.284416	-0.091790	4.814691
470.180315	8000.638624	12.289421	-0.091801	4.814703
470.134137	8000.635666	12.294426	-0.091792	4.814702
470.263183	8000.555331	12.299431	-0.091816	4.814678
470.189633	8000.618423	12.304435	-0.091803	4.814697
470.086332	8000.603718	12.309440	-0.091783	4.814693
470.155128	8000.596362	12.314445	-0.091796	4.814691
470.144883	8000.477065	12.319450	-0.091794	4.814656
470.343819	8000.623340	12.324455	-0.091832	4.814698
470.188443	8000.591612	12.329459	-0.091803	4.814689
470.103588	8000.576161	12.334464	-0.091787	4.814685
470.247665	8000.617363	12.339469	-0.091814	4.814696
470.435301	8000.593874	12.344474	-0.091849	4.814689
470.409186	8000.622394	12.349479	-0.091844	4.814697
470.285489	8000.611619	12.354483	-0.091821	4.814695
470.589163	8000.504337	12.359488	-0.091878	4.814662
470.578368	8000.631863	12.364493	-0.091876	4.814699
470.564892	8000.612314	12.369498	-0.091874	4.814693
470.602410	8000.529279	12.374503	-0.091881	4.814669
470.474341	8000.599989	12.379507	-0.091857	4.814690
470.460980	8000.607272	12.384512	-0.091854	4.814692
470.689592	8000.523340	12.389517	-0.091897	4.814667
470.570343	8000.618890	12.394522	-0.091875	4.814695
470.545086	8000.612010	12.399527	-0.091870	4.814693
470.436651	8000.582188	12.404531	-0.091850	4.814685
470.406592	8000.584882	12.409536	-0.091845	4.814686
470.244056	8000.592734	12.414541	-0.091815	4.814689
470.118241	8000.543287	12.419546	-0.091791	4.814676
470.436036	8000.577916	12.424551	-0.091850	4.814684
470.538125	8000.519639	12.429555	-0.091870	4.814666
470.375623	8000.562907	12.434560	-0.091839	4.814680
470.337783	8000.633073	12.439565	-0.091832	4.814700
470.380263	8000.599494	12.444570	-0.091840	4.814690
470.533135	8000.597925	12.449575	-0.091869	4.814689
470.256584	8000.560825	12.454579	-0.091818	4.814680
470.407859	8000.596788	12.459584	-0.091846	4.814690
470.348833	8000.611846	12.464589	-0.091835	4.814694
470.322330	8000.571675	12.469594	-0.091830	4.814683
470.553560	8000.607986	12.474599	-0.091873	4.814692
470.596198	8000.514311	12.479603	-0.091881	4.814665
470.416376	8000.595906	12.484608	-0.091848	4.814689
470.533852	8000.617318	12.489613	-0.091870	4.814695
470.469188	8000.551786	12.494618	-0.091858	4.814676
470.478432	8000.583081	12.499623	-0.091860	4.814685
470.497510	8000.588794	12.504627	-0.091863	4.814687
470.281151	8000.599983	12.509632	-0.091823	4.814691
470.315364	8000.593086	12.514637	-0.091830	4.814689
470.055153	8000.528374	12.519642	-0.091781	4.814671
470.382027	8000.603945	12.524647	-0.091842	4.814692
470.304039	8000.572518	12.529651	-0.091828	4.814683
470.186828	8000.550054	12.534656	-0.091806	4.814677
470.470455	8000.571197	12.539661	-0.091859	4.814682
470.369408	8000.541507	12.544666	-0.091840	4.814674
470.488737	8000.587636	12.549671	-0.091862	4.814686
470.387540	8000.495698	12.554675	-0.091844	4.814660
470.410228	8000.637770	12.559680	-0.091848	4.814701
470.277126	8000.634340	12.564685	-0.091823	4.814701
470.119048	8000.566076	12.569690	-0.091794	4.814682
470.316751	8000.570669	12.574695	-0.091831	4.814682
470.434759	8000.574919	12.579699	-0.091853	4.814683
470.217214	8000.625795	12.584704	-0.091812	4.814699
470.272879	8000.552742	12.589709	-0.091823	4.814677
470.351262	8000.620680	12.594714	-0.091838	4.814697
470.346378	8000.631333	12.599719	-0.091837	4.814700
470.411746	8000.615331	12.604723	-0.091849	4.814695
470.268885	8000.585972	12.609728	-0.091822	4.814687
470.322079	8000.590144	12.614733	-0.091832	4.814688
470.364050	8000.507189	12.619738	-0.091840	4.814664
470.447500	8000.624584	12.624743	-0.091856	4.814697
470.568907	8000.616016	12.629747	-0.091879	4.814694
470.260407	8000.575129	12.634752	-0.091821	4.814684
470.218852	8000.538984	12.639757	-0.091814	4.814674
470.475306	8000.599353	12.644762	-0.091861	4.814690
470.400503	8000.616276	12.649767	-0.091848	4.814695
470.349326	8000.604643	12.654771	-0.091838	4.814692
470.338963	8000.578710	12.659776	-0.091836	4.814685
470.440920	8000.618091	12.664781	-0.091855	4.814695
470.214626	8000.578664	12.669786	-0.091813	4.814685
470.397839	8000.486413	12.674791	-0.091847	4.814657
470.413140	8000.598304	12.679795	-0.091850	4.814690
470.555044	8000.556832	12.684800	-0.091877	4.814677
470.521957	8000.586301	12.689805	-0.091871	4.814686
470.436013	8000.597661	12.694810	-0.091855	4.814690
470.678082	8000.561188	12.699815	-0.091900	4.814678
470.369549	8000.560007	12.704819	-0.091843	4.814679
470.408136	8000.545676	12.709824	-0.091850	4.814675
470.385782	8000.622556	12.714829	-0.091846	4.814697
470.199557	8000.587061	12.719834	-0.091811	4.814688
470.288844	8000.518898	12.724839	-0.091828	4.814667
470.455596	8000.593771	12.729843	-0.091859	4.814688
470.594648	8000.573712	12.734848	-0.091885	4.814682
470.527988	8000.644440	12.739853	-0.091873	4.814703
470.606679	8000.624382	12.744858	-0.091888	4.814696
470.435919	8000.541940	12.749863	-0.091856	4.814673
470.288977	8000.615534	12.754867	-0.091829	4.814695
470.417898	8000.585636	12.759872	-0.091853	4.814686
470.638238	8000.619608	12.764877	-0.091894	4.814695
470.324473	8000.571114	12.769882	-0.091835	4.814682
470.307610	8000.546140	12.774887	-0.091832	4.814675
470.390226	8000.632397	12.779891	-0.091848	4.814700
470.404084	8000.632651	12.784896	-0.091851	4.814700
470.429045	8000.649200	12.789901	-0.091855	4.814705
470.235928	8000.577093	12.794906	-0.091819	4.814685
470.230037	8000.530850	12.799911	-0.091818	4.814671
470.245111	8000.618053	12.804915	-0.091821	4.814696
470.319592	8000.603287	12.809920	-0.091835	4.814692
470.563999	8000.587246	12.814925	-0.091881	4.814686
470.276996	8000.587521	12.819930	-0.091827	4.814687
470.299341	8000.587926	12.824935	-0.091832	4.814687
470.567577	8000.605577	12.829939	-0.091882	4.814691
470.476004	8000.563177	12.834944	-0.091865	4.814679
470.332595	8000.615370	12.839949	-0.091838	4.814695
470.285046	8000.480386	12.844954	-0.091829	4.814656
470.373267	8000.641865	12.849959	-0.091846	4.814703
470.471564	8000.633961	12.854963	-0.091864	4.814700
470.396148	8000.601506	12.859968	-0.091850	4.814691
470.420987	8000.533271	12.864973	-0.091855	4.814671
470.277305	8000.573654	12.869978	-0.091828	4.814683
470.544585	8000.639582	12.874983	-0.091878	4.814701
470.222437	8000.605964	12.879987	-0.091818	4.814693
470.326831	8000.592802	12.884992	-0.091838	4.814689
470.325356	8000.617467	12.889997	-0.091838	4.814696
470.380874	8000.601290	12.895002	-0.091848	4.814691
470.394370	8000.540366	12.900007	-0.091851	4.814673
470.442294	8000.628154	12.905011	-0.091860	4.814698
470.353783	8000.579369	12.910016	-0.091843	4.814685
470.536044	8000.609445	12.915021	-0.091877	4.814692
470.472229	8000.585782	12.920026	-0.091865	4.814686
470.223342	8000.534148	12.925031	-0.091819	4.814672
470.397497	8000.619885	12.930035	-0.091852	4.814696
470.393264	8000.594061	12.935040	-0.091851	4.814689
470.389787	8000.651960	12.940045	-0.091850	4.814705
470.186819	8000.594703	12.945050	-0.091813	4.814690
470.506584	8000.515609	12.950055	-0.091872	4.814665
470.405902	8000.606123	12.955059	-0.091854	4.814692
470.224022	8000.586802	12.960064	-0.091820	4.814687
470.391781	8000.613400	12.965069	-0.091851	4.814694
470.262115	8000.586421	12.970074	-0.091827	4.814687
470.319285	8000.502663	12.975079	-0.091838	4.814662
470.288671	8000.589055	12.980083	-0.091832	4.814688
470.285822	8000.631940	12.985088	-0.091832	4.814700
470.516042	8000.642477	12.990093	-0.091875	4.814702
470.352748	8000.582705	12.995098	-0.091844	4.814685
470.667572	8000.597964	13.000103	-0.091903	4.814688
470.445678	8000.618714	13.005107	-0.091862	4.814695
470.303633	8000.520684	13.010112	-0.091835	4.814668
470.419078	8000.523816	13.015117	-0.091857	4.814668
470.361092	8000.616161	13.020122	-0.091846	4.814695
470.504841	8000.601552	13.025127	-0.091873	4.814690
470.388355	8000.626320	13.030131	-0.091852	4.814698
470.396693	8000.616818	13.035136	-0.091853	4.814695
470.489991	8000.615263	13.040141	-0.091871	4.814694
470.102687	8000.604098	13.045146	-0.091799	4.814693
470.383847	8000.492123	13.050151	-0.091851	4.814659
470.445617	8000.620938	13.055155	-0.091863	4.814696
470.131886	8000.547762	13.060160	-0.091804	4.814676
470.440100	8000.625149	13.065165	-0.091862	4.814697
470.553109	8000.575651	13.070170	-0.091883	4.814682
470.627740	8000.563033	13.075175	-0.091897	4.814678
470.830898	8000.610652	13.080179	-0.091935	4.814691
470.792244	8000.554166	13.085184	-0.091928	4.814675
470.783917	8000.530416	13.090189	-0.091926	4.814668
470.438292	8000.572578	13.095194	-0.091862	4.814682
470.598174	8000.604402	13.100199	-0.091892	4.814690
470.560469	8000.605886	13.105203	-0.091885	4.814691
470.569470	8000.556687	13.110208	-0.091887	4.814677
470.859557	8000.618729	13.115213	-0.091941	4.814693
470.673257	8000.604694	13.120218	-0.091906	4.814690
470.449099	8000.598574	13.125223	-0.091865	4.814690
470.448803	8000.630772	13.130227	-0.091865	4.814699
470.402907	8000.517280	13.135232	-0.091856	4.814666
470.469674	8000.640817	13.140237	-0.091869	4.814702
470.252709	8000.585458	13.145242	-0.091828	4.814687
470.485041	8000.546665	13.150247	-0.091872	4.814674
470.635076	8000.607291	13.155251	-0.091900	4.814691
470.568574	8000.587873	13.160256	-0.091887	4.814686
470.347208	8000.592534	13.165261	-0.091846	4.814688
470.408459	8000.585045	13.170266	-0.091858	4.814686
470.495193	8000.587666	13.175271	-0.091874	4.814686
470.544963	8000.537045	13.180275	-0.091883	4.814671
470.438869	8000.616731	13.185280	-0.091864	4.814695
470.457899	8000.606345	13.190285	-0.091867	4.814692
470.400143	8000.588156	13.195290	-0.091857	4.814687
470.454867	8000.604161	13.200295	-0.091867	4.814691
470.566615	8000.630837	13.205299	-0.091888	4.814698
470.402893	8000.603253	13.210304	-0.091857	4.814691
470.426994	8000.596177	13.215309	-0.091862	4.814689
470.527998	8000.548612	13.220314	-0.091881	4.814675
470.684861	8000.469844	13.225319	-0.091910	4.814651
470.608417	8000.611229	13.230323	-0.091896	4.814692
470.601396	8000.558526	13.235328	-0.091895	4.814677
470.821010	8000.620388	13.240333	-0.091936	4.814694
470.547435	8000.571534	13.245338	-0.091885	4.814681
470.464297	8000.589383	13.250343	-0.091869	4.814687
470.673706	8000.587745	13.255347	-0.091909	4.814685
470.501391	8000.575033	13.260352	-0.091877	4.814682
470.524616	8000.623747	13.265357	-0.091881	4.814696
470.444649	8000.604090	13.270362	-0.091866	4.814691
470.571444	8000.597765	13.275367	-0.091890	4.814689
470.504063	8000.575112	13.280371	-0.091877	4.814682
470.623602	8000.546121	13.285376	-0.091900	4.814673
470.597144	8000.508097	13.290381	-0.091895	4.814662
470.396091	8000.562486	13.295386	-0.091857	4.814679
470.537871	8000.601501	13.300391	-0.091884	4.814690
470.786099	8000.616651	13.305395	-0.091930	4.814693
470.618874	8000.601883	13.310400	-0.091899	4.814690
470.611771	8000.632887	13.315405	-0.091898	4.814699
470.763199	8000.594804	13.320410	-0.091926	4.814687
470.700575	8000.515356	13.325415	-0.091915	4.814664
470.651724	8000.632547	13.330419	-0.091906	4.814698
470.651920	8000.554216	13.335424	-0.091906	4.814676
470.851440	8000.623233	13.340429	-0.091943	4.814695
470.447139	8000.603180	13.345434	-0.091868	4.814691
470.334351	8000.574354	13.350439	-0.091847	4.814683
470.530889	8000.612196	13.355443	-0.091884	4.814693
470.611928	8000.565350	13.360448	-0.091899	4.814679
470.613256	8000.552503	13.365453	-0.091899	4.814675
470.676802	8000.503200	13.370458	-0.091911	4.814661
470.767662	8000.599263	13.375463	-0.091928	4.814688
470.563279	8000.632128	13.380467	-0.091890	4.814699
470.472425	8000.609058	13.385472	-0.091873	4.814692
470.486369	8000.644729	13.390477	-0.091876	4.814703
470.434930	8000.572993	13.395482	-0.091866	4.814682
470.606908	8000.547080	13.400487	-0.091898	4.814674
470.455004	8000.616293	13.405491	-0.091870	4.814695
470.517146	8000.593794	13.410496	-0.091882	4.814688
470.679412	8000.633174	13.415501	-0.091912	4.814698
470.452455	8000.618418	13.420506	-0.091870	4.814695
470.390949	8000.578698	13.425511	-0.091859	4.814684
470.604032	8000.605028	13.430515	-0.091898	4.814690
470.620409	8000.574205	13.435520	-0.091902	4.814681
470.883753	8000.627186	13.440525	-0.091951	4.814695
470.997271	8000.597014	13.445530	-0.091972	4.814686
470.904987	8000.593236	13.450535	-0.091955	4.814685
470.682301	8000.510944	13.455539	-0.091913	4.814663
470.555036	8000.576302	13.460544	-0.091890	4.814682
470.432959	8000.626728	13.465549	-0.091867	4.814698
470.577359	8000.590666	13.470554	-0.091894	4.814686
470.728638	8000.550434	13.475559	-0.091922	4.814674
470.711126	8000.635987	13.480563	-0.091919	4.814699
470.742506	8000.615088	13.485568	-0.091925	4.814693
470.739254	8000.638649	13.490573	-0.091925	4.814700
470.570139	8000.624920	13.495578	-0.091893	4.814696
470.697595	8000.504848	13.500583	-0.091917	4.814661
470.916145	8000.631084	13.505587	-0.091958	4.814696
470.553010	8000.616054	13.510592	-0.091890	4.814694
470.546165	8000.648136	13.515597	-0.091889	4.814703
470.465581	8000.535100	13.520602	-0.091874	4.814671
470.666801	8000.597708	13.525607	-0.091912	4.814688
470.644656	8000.644544	13.530611	-0.091908	4.814702
470.511693	8000.601408	13.535616	-0.091883	4.814690
470.856821	8000.551741	13.540621	-0.091947	4.814674
470.901055	8000.615854	13.545626	-0.091956	4.814692
470.574027	8000.554245	13.550631	-0.091895	4.814676
470.801327	8000.605512	13.555635	-0.091937	4.814690
470.647658	8000.580253	13.560640	-0.091909	4.814683
470.648817	8000.630721	13.565645	-0.091909	4.814698
470.564651	8000.598111	13.570650	-0.091893	4.814689
470.874517	8000.607917	13.575655	-0.091951	4.814690
470.915425	8000.529235	13.580659	-0.091959	4.814667
470.621711	8000.560514	13.585664	-0.091904	4.814677
470.720592	8000.580523	13.590669	-0.091923	4.814683
470.691551	8000.591820	13.595674	-0.091917	4.814686
470.506363	8000.574586	13.600679	-0.091883	4.814682
470.683564	8000.613158	13.605683	-0.091916	4.814692
470.664845	8000.579564	13.610688	-0.091913	4.814683
470.787011	8000.623597	13.615693	-0.091936	4.814695
470.683115	8000.599222	13.620698	-0.091916	4.814688
470.654378	8000.493546	13.625703	-0.091911	4.814658
470.773043	8000.639471	13.630707	-0.091933	4.814700
470.532513	8000.580472	13.635712	-0.091889	4.814684
470.624018	8000.642205	13.640717	-0.091906	4.814701
470.823981	8000.614643	13.645722	-0.091943	4.814692
470.525972	8000.540672	13.650727	-0.091888	4.814672
470.536138	8000.652472	13.655731	-0.091890	4.814705
470.620923	8000.538081	13.660736	-0.091905	4.814671
470.671036	8000.644153	13.665741	-0.091915	4.814701
470.464670	8000.629762	13.670746	-0.091877	4.814698
470.632699	8000.609145	13.675751	-0.091908	4.814691
470.836116	8000.627792	13.680755	-0.091946	4.814696
470.584416	8000.526740	13.685760	-0.091899	4.814668
470.626385	8000.609057	13.690765	-0.091907	4.814691
470.647571	8000.596563	13.695770	-0.091911	4.814688
470.644469	8000.592223	13.700775	-0.091910	4.814686
470.626857	8000.601577	13.705779	-0.091907	4.814689
470.563000	8000.574693	13.710784	-0.091895	4.814682
470.549393	8000.607728	13.715789	-0.091893	4.814691
470.597699	8000.586057	13.720794	-0.091902	4.814685
470.779292	8000.507729	13.725799	-0.091936	4.814661
470.812321	8000.644620	13.730803	-0.091942	4.814701
470.502837	8000.570444	13.735808	-0.091885	4.814681
470.575581	8000.647942	13.740813	-0.091898	4.814703
470.736080	8000.637923	13.745818	-0.091928	4.814699
470.787611	8000.518648	13.750823	-0.091938	4.814664
470.604670	8000.622725	13.755827	-0.091904	4.814695
470.846193	8000.577657	13.760832	-0.091949	4.814681
470.909648	8000.614209	13.765837	-0.091961	4.814691
470.703353	8000.624503	13.770842	-0.091923	4.814695
470.521921	8000.641678	13.775847	-0.091889	4.814701
470.711994	8000.550621	13.780851	-0.091924	4.814674
470.688678	8000.647876	13.785856	-0.091920	4.814702
470.822049	8000.634156	13.790861	-0.091945	4.814698
470.846397	8000.616352	13.795866	-0.091950	4.814692
470.687814	8000.557736	13.800871	-0.091920	4.814676
470.986119	8000.652120	13.805875	-0.091976	4.814702
470.778919	8000.546492	13.810880	-0.091937	4.814672
470.918520	8000.624104	13.815885	-0.091963	4.814694
470.755876	8000.602978	13.820890	-0.091933	4.814689
470.768724	8000.547408	13.825895	-0.091936	4.814673
470.890661	8000.656902	13.830899	-0.091958	4.814704
470.830483	8000.626864	13.835904	-0.091947	4.814695
470.853478	8000.516741	13.840909	-0.091952	4.814663
470.940068	8000.590192	13.845914	-0.091968	4.814684
470.816733	8000.640595	13.850919	-0.091945	4.814700
470.753640	8000.650214	13.855923	-0.091933	4.814703
470.576764	7999.425824	13.860928	-0.091900	4.814347

470.844442	7996.279108	13.865933	-0.091948	4.813430
470.675592	7990.665729	13.870938	-0.091913	4.811798
470.515641	7983.931923	13.875943	-0.091879	4.809838
470.725578	7976.698240	13.880947	-0.091913	4.807730
470.727412	7968.966038	13.885952	-0.091908	4.805477
470.606564	7961.239688	13.890957	-0.091881	4.803225
470.549049	7953.278361	13.895962	-0.091865	4.800903
470.690207	7945.350918	13.900967	-0.091886	4.798589
470.591763	7937.391293	13.905971	-0.091863	4.796266
470.498983	7929.370479	13.910976	-0.091840	4.793923
470.447105	7921.370298	13.915981	-0.091826	4.791585
470.589961	7913.347207	13.920986	-0.091847	4.789239
470.371607	7905.365098	13.925991	-0.091801	4.786905
470.366386	7897.358234	13.930995	-0.091795	4.784562
470.201169	7889.374210	13.936000	-0.091759	4.782224
470.202708	7881.351895	13.941005	-0.091754	4.779874
470.369426	7873.457355	13.946010	-0.091780	4.777560
470.262163	7865.367837	13.951015	-0.091755	4.775188
470.147754	7857.343989	13.956019	-0.091729	4.772834
470.117339	7849.274296	13.961024	-0.091718	4.770465
470.150307	7841.344486	13.966029	-0.091719	4.768136
470.061357	7833.337205	13.971034	-0.091697	4.765784
469.897387	7825.341400	13.976039	-0.091662	4.763434
470.009971	7817.404233	13.981043	-0.091678	4.761099
470.118758	7809.339352	13.986048	-0.091693	4.758725
470.029226	7801.423258	13.991053	-0.091671	4.756395
469.980475	7793.322992	13.996058	-0.091657	4.754009
469.916918	7785.276411	14.001063	-0.091640	4.751638
469.934928	7777.233828	14.006067	-0.091638	4.749267
469.642140	7769.305754	14.011072	-0.091578	4.746929
469.792795	7761.254821	14.016077	-0.091601	4.744552
469.581557	7753.335736	14.021082	-0.091557	4.742214
469.569064	7745.265536	14.026087	-0.091549	4.739830
469.696184	7737.351993	14.031091	-0.091568	4.737491
469.559489	7729.317999	14.036096	-0.091537	4.735115
469.357252	7721.267335	14.041101	-0.091494	4.732734
469.491525	7713.256072	14.046106	-0.091514	4.730361
469.551836	7705.223763	14.051111	-0.091520	4.727982
469.611139	7697.299745	14.056115	-0.091526	4.725634
469.389358	7689.264138	14.061120	-0.091480	4.723252
469.493255	7681.293812	14.066125	-0.091494	4.720887
469.446945	7673.319663	14.071130	-0.091480	4.718521
469.456410	7665.293315	14.076135	-0.091477	4.716138
469.462488	7657.321427	14.081139	-0.091473	4.713769
469.319674	7649.209365	14.086144	-0.091441	4.711358
469.243809	7641.206029	14.091149	-0.091422	4.708979
469.112592	7633.238805	14.096154	-0.091392	4.706608
469.410201	7625.208070	14.101159	-0.091443	4.704217
469.294062	7617.274222	14.106163	-0.091416	4.701854
469.054407	7609.255410	14.111168	-0.091366	4.699465
469.198589	7601.302502	14.116173	-0.091388	4.697094
469.261688	7593.267123	14.121178	-0.091394	4.694697
468.972367	7585.261360	14.126183	-0.091335	4.692308
469.083665	7577.212623	14.131187	-0.091351	4.689904
469.046524	7569.208683	14.136192	-0.091339	4.687513
468.916462	7561.240560	14.141197	-0.091310	4.685132
468.834834	7553.282100	14.146202	-0.091289	4.682752
468.817353	7545.244706	14.151207	-0.091281	4.680347
468.887508	7537.289181	14.156211	-0.091289	4.677965
468.850783	7529.210925	14.161216	-0.091277	4.675546
469.033214	7521.168420	14.166221	-0.091306	4.673135
468.904446	7513.130238	14.171226	-0.091277	4.670725
468.738345	7505.129341	14.176231	-0.091241	4.668325
468.857632	7497.163333	14.181235	-0.091258	4.665934
468.758868	7489.205399	14.186240	-0.091234	4.663545
468.718392	7481.181251	14.191245	-0.091221	4.661134
468.623300	7473.192155	14.196250	-0.091199	4.658732
468.576508	7465.190851	14.201255	-0.091185	4.656326
468.698788	7457.207967	14.206259	-0.091202	4.653924
468.586061	7449.182522	14.211264	-0.091176	4.651507
468.661802	7441.157945	14.216269	-0.091185	4.649090
468.584902	7433.195939	14.221274	-0.091166	4.646691
468.521869	7425.149121	14.226279	-0.091149	4.644264
468.668623	7417.269720	14.231283	-0.091171	4.641887
468.599776	7409.177465	14.236288	-0.091153	4.639444
468.612881	7401.248922	14.241293	-0.091151	4.637049
468.338043	7393.132518	14.246298	-0.091094	4.634597
468.339398	7385.132802	14.251303	-0.091089	4.632179
468.284064	7377.161886	14.256307	-0.091074	4.629767
468.129007	7369.149532	14.261312	-0.091040	4.627343
468.370065	7361.108324	14.266317	-0.091080	4.624907
468.575656	7353.170091	14.271322	-0.091113	4.622502
468.271220	7345.126855	14.276327	-0.091051	4.620064
468.122592	7337.208656	14.281331	-0.091018	4.617663
468.081373	7329.127144	14.286336	-0.091005	4.615210
467.984250	7321.119786	14.291341	-0.090982	4.612779
467.980008	7313.102412	14.296346	-0.090976	4.610344
468.050418	7305.103727	14.301351	-0.090984	4.607913
468.016862	7297.153307	14.306355	-0.090973	4.605495
467.813479	7289.115697	14.311360	-0.090930	4.603050
467.832288	7281.114299	14.316365	-0.090928	4.600614
467.913769	7273.126369	14.321370	-0.090938	4.598181
467.797973	7265.094522	14.326375	-0.090911	4.595733
467.875944	7257.121208	14.331379	-0.090921	4.593302
467.730285	7249.073419	14.336384	-0.090889	4.590847
467.895703	7241.056380	14.341389	-0.090914	4.588400
467.858247	7233.067242	14.346394	-0.090902	4.585960
467.770467	7225.070174	14.351399	-0.090881	4.583516
467.768089	7217.103850	14.356403	-0.090875	4.581081
467.536048	7209.065575	14.361408	-0.090827	4.578622
467.335826	7201.082655	14.366413	-0.090784	4.576179
467.541929	7193.103342	14.371418	-0.090818	4.573736
467.472281	7185.045243	14.376423	-0.090799	4.571267
467.465688	7177.070811	14.381427	-0.090793	4.568822
467.214826	7169.050365	14.386432	-0.090741	4.566362
467.260131	7161.053917	14.391437	-0.090745	4.563908
467.254269	7153.080202	14.396442	-0.090738	4.561460
467.409689	7145.045272	14.401447	-0.090762	4.558992
467.559737	7137.108079	14.406451	-0.090785	4.556552
467.369185	7129.027049	14.411456	-0.090744	4.554067
467.091446	7121.020814	14.416461	-0.090688	4.551603
467.110265	7113.001693	14.421466	-0.090686	4.549134
467.060377	7105.031779	14.426471	-0.090671	4.546679
467.000787	7097.004466	14.431475	-0.090655	4.544205
467.012523	7089.032864	14.436480	-0.090652	4.541746
467.246713	7080.992749	14.441485	-0.090691	4.539266
467.107615	7073.106323	14.446490	-0.090660	4.536831
467.166130	7065.033250	14.451495	-0.090666	4.534337
467.249455	7057.057388	14.456499	-0.090676	4.531873
466.871012	7048.990390	14.461504	-0.090600	4.529378
466.872470	7041.066121	14.466509	-0.090595	4.526926
467.099989	7033.015806	14.471514	-0.090633	4.524434
466.926256	7025.069960	14.476519	-0.090595	4.521973
466.607246	7017.043795	14.481523	-0.090531	4.519485
466.707847	7009.086984	14.486528	-0.090544	4.517018
466.721420	7001.054570	14.491533	-0.090542	4.514526
466.700013	6992.971528	14.496538	-0.090533	4.512017
466.419415	6984.913874	14.501543	-0.090475	4.509513
466.522228	6976.998711	14.506547	-0.090489	4.507054
466.418834	6968.911661	14.511552	-0.090465	4.504539
466.344131	6961.010548	14.516557	-0.090446	4.502081
466.452507	6953.018135	14.521562	-0.090461	4.499593
466.586480	6945.017880	14.526567	-0.090481	4.497102
466.631940	6937.021725	14.531571	-0.090484	4.494610
466.418689	6929.019110	14.536576	-0.090439	4.492115
466.304870	6920.991184	14.541581	-0.090413	4.489610
466.316872	6913.018701	14.546586	-0.090410	4.487121
466.266193	6904.960257	14.551591	-0.090395	4.484604
466.230201	6897.047060	14.556595	-0.090384	4.482131
466.153567	6888.993884	14.561600	-0.090364	4.479613
466.065666	6881.016214	14.566605	-0.090343	4.477117
465.974280	6872.986235	14.571610	-0.090320	4.474603
466.210128	6864.951631	14.576615	-0.090359	4.472088
466.177795	6856.951031	14.581619	-0.090348	4.469580
465.943482	6848.962970	14.586624	-0.090299	4.467075
466.086097	6840.948720	14.591629	-0.090321	4.464561
466.138334	6832.977674	14.596634	-0.090325	4.462059
465.994747	6824.951582	14.601639	-0.090293	4.459538
466.001397	6816.995983	14.606643	-0.090290	4.457038
466.017688	6808.950448	14.611648	-0.090287	4.454508
466.050201	6800.941048	14.616653	-0.090288	4.451988
465.898426	6792.949208	14.621658	-0.090255	4.449472
465.879238	6784.950494	14.626663	-0.090246	4.446952
465.834786	6776.984359	14.631667	-0.090233	4.444442
465.808719	6768.989865	14.636672	-0.090223	4.441921
465.809777	6760.940241	14.641677	-0.090218	4.439381
465.805608	6753.021845	14.646682	-0.090212	4.436881
465.664002	6744.923904	14.651687	-0.090181	4.434323
465.832006	6736.916573	14.656691	-0.090207	4.431792
465.637784	6728.866189	14.661696	-0.090165	4.429246
465.814891	6720.892526	14.666701	-0.090193	4.426724
465.777087	6712.913426	14.671706	-0.090181	4.424197
465.543382	6704.915967	14.676711	-0.090132	4.421663
465.548742	6696.924804	14.681715	-0.090128	4.419130
465.518158	6688.948574	14.686720	-0.090117	4.416600
465.606178	6680.888691	14.691725	-0.090129	4.414043
465.518868	6672.892016	14.696730	-0.090107	4.411503
465.463730	6664.879867	14.701735	-0.090092	4.408958
465.506932	6656.900373	14.706739	-0.090095	4.406421
465.317642	6648.863213	14.711744	-0.090054	4.403864
465.243557	6640.920255	14.716749	-0.090036	4.401336
465.180269	6632.901361	14.721754	-0.090019	4.398782
465.207497	6624.920029	14.726759	-0.090019	4.396239
465.281752	6616.885787	14.731763	-0.090027	4.393678
465.297179	6608.892372	14.736768	-0.090025	4.391129
465.140723	6600.845758	14.741773	-0.089991	4.388560
464.993261	6592.879029	14.746778	-0.089958	4.386015
464.967072	6584.844657	14.751783	-0.089948	4.383447
464.969075	6576.899462	14.756787	-0.089943	4.380907
465.006335	6568.895847	14.761792	-0.089945	4.378346
464.991592	6560.944600	14.766797	-0.089937	4.375801
464.829405	6552.933317	14.771802	-0.089902	4.373234
464.681496	6544.884684	14.776807	-0.089869	4.370654
464.660035	6536.906756	14.781811	-0.089860	4.368095
464.582867	6528.901446	14.786816	-0.089841	4.365526
464.822540	6520.911668	14.791821	-0.089880	4.362962
464.855153	6512.918635	14.796826	-0.089881	4.360395
464.666842	6504.915948	14.801831	-0.089841	4.357821
464.653021	6496.941007	14.806835	-0.089833	4.355256
464.610365	6488.790935	14.811840	-0.089820	4.352633
464.699579	6480.734390	14.816845	-0.089832	4.350039
464.482564	6472.863861	14.821850	-0.089786	4.347502
464.535321	6464.833994	14.826855	-0.089791	4.344914
464.600858	6456.880244	14.831859	-0.089798	4.342348
464.541192	6448.844706	14.836864	-0.089782	4.339754
464.618779	6440.891457	14.841869	-0.089791	4.337186
464.552215	6432.925536	14.846874	-0.089773	4.334611
464.556857	6424.854821	14.851879	-0.089769	4.332002
464.582063	6416.852217	14.856883	-0.089769	4.329413
464.521653	6408.879320	14.861888	-0.089752	4.326831
464.525534	6400.861686	14.866893	-0.089748	4.324234
464.141482	6392.930294	14.871898	-0.089671	4.321660
464.103665	6384.879928	14.876903	-0.089659	4.319049
464.410244	6376.921255	14.881907	-0.089711	4.316468
464.295221	6368.863010	14.886912	-0.089684	4.313851
463.919755	6360.874037	14.891917	-0.089609	4.311253
464.090261	6352.899994	14.896922	-0.089636	4.308661
463.928076	6344.813419	14.901927	-0.089601	4.306029
463.786380	6336.831114	14.906931	-0.089569	4.303430
463.795125	6328.860808	14.911936	-0.089566	4.300834
463.845155	6320.846487	14.916941	-0.089570	4.298223
463.748846	6312.875829	14.921946	-0.089547	4.295623
463.596668	6304.849177	14.926951	-0.089513	4.293002
463.713461	6296.817331	14.931955	-0.089530	4.290381
463.657319	6288.852740	14.936960	-0.089514	4.287778
463.738649	6280.818116	14.941965	-0.089524	4.285152
463.916192	6272.899612	14.946970	-0.089552	4.282564
463.631370	6264.851192	14.951975	-0.089494	4.279927
463.640522	6256.869255	14.956979	-0.089491	4.277313
463.528405	6248.834247	14.961984	-0.089465	4.274679
463.590511	6240.797999	14.966989	-0.089471	4.272044
463.497849	6232.773433	14.971994	-0.089449	4.269411
463.244101	6224.814029	14.976999	-0.089396	4.266795
463.456003	6216.779333	14.982003	-0.089431	4.264157
463.347702	6208.836565	14.987008	-0.089405	4.261546
463.342633	6200.801159	14.992013	-0.089399	4.258902
463.490496	6192.829347	14.997018	-0.089422	4.256280
463.430145	6184.794896	15.002023	-0.089405	4.253633
463.229978	6176.796647	15.007027	-0.089363	4.250996
463.181089	6168.795628	15.012032	-0.089349	4.248357
463.332652	6160.769629	15.017037	-0.089372	4.245710
463.286396	6152.839959	15.022042	-0.089358	4.243092
463.373524	6144.795371	15.027047	-0.089369	4.240435
463.330018	6136.843413	15.032051	-0.089356	4.237806
463.249467	6128.876679	15.037056	-0.089336	4.235170
463.121766	6120.788016	15.042061	-0.089307	4.232492
463.269098	6112.788232	15.047066	-0.089329	4.229844
463.272295	6104.786172	15.052071	-0.089325	4.227192
463.167315	6096.778097	15.057075	-0.089300	4.224535
463.163113	6088.823958	15.062080	-0.089294	4.221896
463.014728	6080.806576	15.067085	-0.089261	4.219233
462.977987	6072.838056	15.072090	-0.089249	4.216585
463.004802	6064.794788	15.077095	-0.089249	4.213911
463.119385	6056.810334	15.082099	-0.089265	4.211256
462.861418	6048.813769	15.087104	-0.089212	4.208592
462.979219	6040.823373	15.092109	-0.089229	4.205932
462.990877	6032.858965	15.097114	-0.089226	4.203277
462.749576	6024.846391	15.102119	-0.089176	4.200603
462.865401	6016.851566	15.107123	-0.089192	4.197936
462.731803	6008.860990	15.112128	-0.089162	4.195266
462.823037	6000.706128	15.117133	-0.089174	4.192542
462.696533	5992.739691	15.122138	-0.089146	4.189878
462.510340	5984.730800	15.127143	-0.089106	4.187196
462.709543	5976.761660	15.132147	-0.089138	4.184530
462.538102	5968.804550	15.137152	-0.089101	4.181863
462.286067	5960.804875	15.142157	-0.089049	4.179178
462.403698	5952.862853	15.147162	-0.089065	4.176516
462.438515	5944.778810	15.152167	-0.089067	4.173803
462.296088	5936.795878	15.157171	-0.089035	4.171120
462.286709	5928.824038	15.162176	-0.089028	4.168441
462.441973	5920.803696	15.167181	-0.089052	4.165745
462.285175	5912.854396	15.172186	-0.089018	4.163068
462.120319	5904.797473	15.177191	-0.088982	4.160353
462.500833	5896.837962	15.182195	-0.089048	4.157676
462.392634	5888.806295	15.187200	-0.089022	4.154966
462.236222	5880.776916	15.192205	-0.088988	4.152255
462.140492	5872.805339	15.197210	-0.088965	4.149563
462.228637	5864.784684	15.202215	-0.088976	4.146854
462.180353	5856.790529	15.207219	-0.088962	4.144151
462.053311	5848.843079	15.212224	-0.088934	4.141461
461.960290	5840.786267	15.217229	-0.088911	4.138733
462.014442	5832.821829	15.222234	-0.088916	4.136036
461.808309	5824.791575	15.227239	-0.088872	4.133312
461.994958	5816.771282	15.232243	-0.088902	4.130594
461.938283	5808.794240	15.237248	-0.088886	4.127886
461.713993	5800.756751	15.242253	-0.088840	4.125153
461.910589	5792.843702	15.247258	-0.088871	4.122467
461.913465	5784.738968	15.252263	-0.088866	4.119710
461.781784	5776.844469	15.257267	-0.088837	4.117022
461.725499	5768.815880	15.262272	-0.088821	4.114288
461.774765	5760.750331	15.267277	-0.088825	4.111540
461.859346	5752.730051	15.272282	-0.088836	4.108807
461.613124	5744.761151	15.277287	-0.088785	4.106085
461.736116	5736.769302	15.282291	-0.088803	4.103357
461.659056	5728.778318	15.287296	-0.088783	4.100626
461.585044	5720.784366	15.292301	-0.088764	4.097892
461.593382	5712.780820	15.297306	-0.088761	4.095154
461.672201	5704.759902	15.302311	-0.088770	4.092410
461.565894	5696.741375	15.307315	-0.088745	4.089661
461.321295	5688.802780	15.312320	-0.088695	4.086937
461.271584	5680.767463	15.317325	-0.088680	4.084180
461.490162	5672.846320	15.322330	-0.088716	4.081463
461.217500	5664.796831	15.327335	-0.088660	4.078695
461.198597	5656.836530	15.332339	-0.088651	4.075958
461.345852	5648.798844	15.337344	-0.088674	4.073196
461.246200	5640.765424	15.342349	-0.088650	4.070429
461.236189	5632.824570	15.347354	-0.088643	4.067694
461.232742	5624.804594	15.352359	-0.088637	4.064930
461.046802	5616.828159	15.357363	-0.088597	4.062176
460.824684	5608.828832	15.362368	-0.088551	4.059412
460.929323	5600.856175	15.367373	-0.088565	4.056660
461.195052	5592.847127	15.372378	-0.088610	4.053896
460.898936	5584.777041	15.377383	-0.088549	4.051101
460.989134	5576.828468	15.382387	-0.088561	4.048351
461.122661	5568.805977	15.387392	-0.088581	4.045575
460.874098	5560.847096	15.392397	-0.088529	4.042813
460.786704	5552.829461	15.397402	-0.088508	4.040032
460.781544	5544.849927	15.402407	-0.088502	4.037262
460.931664	5536.817231	15.407411	-0.088525	4.034475
460.638684	5528.689282	15.412416	-0.088465	4.031646
460.757667	5520.720220	15.417421	-0.088482	4.028877
460.816368	5512.773512	15.422426	-0.088488	4.026112
460.341353	5504.812952	15.427431	-0.088394	4.023333
460.522742	5496.813772	15.432435	-0.088423	4.020548
460.786794	5488.849612	15.437440	-0.088467	4.017775
460.612463	5480.790012	15.442445	-0.088429	4.014960
460.668683	5472.803857	15.447450	-0.088435	4.012172
460.526941	5464.759556	15.452455	-0.088403	4.009359
460.535632	5456.819669	15.457459	-0.088400	4.006582
460.424572	5448.812091	15.462464	-0.088374	4.003778
460.325498	5440.823013	15.467469	-0.088350	4.000979
460.354650	5432.860583	15.472474	-0.088350	3.998189
460.013854	5424.816122	15.477479	-0.088282	3.995363
459.996649	5416.804771	15.482483	-0.088274	3.992551
460.005048	5408.768595	15.487488	-0.088270	3.989729
460.015491	5400.792188	15.492493	-0.088267	3.986926
460.035253	5392.803220	15.497498	-0.088265	3.984117
459.934120	5384.833390	15.502503	-0.088241	3.981311
460.049840	5376.793701	15.507507	-0.088258	3.978481
459.874558	5368.826232	15.512512	-0.088220	3.975671
459.765216	5360.806561	15.517517	-0.088194	3.972841
459.856212	5352.779812	15.522522	-0.088206	3.970009
459.813869	5344.795024	15.527527	-0.088193	3.967188
459.840733	5336.782674	15.532531	-0.088193	3.964357
459.700193	5328.903926	15.537536	-0.088162	3.961568
459.709280	5320.865886	15.542541	-0.088158	3.958723
459.753989	5312.860134	15.547546	-0.088162	3.955889
459.763991	5304.770188	15.552551	-0.088158	3.953021
459.820681	5296.739314	15.557555	-0.088164	3.950174
459.606280	5288.795810	15.562560	-0.088119	3.947351
459.568072	5280.767004	15.567565	-0.088106	3.944498
459.864415	5272.843729	15.572570	-0.088157	3.941687
459.634117	5264.831383	15.577575	-0.088109	3.938833
459.631084	5256.872601	15.582579	-0.088103	3.935999
459.726541	5248.828879	15.587584	-0.088115	3.933136
459.634139	5240.789715	15.592589	-0.088093	3.930268
459.466480	5232.859905	15.597594	-0.088057	3.927436
459.374260	5224.843864	15.602599	-0.088035	3.924573
459.344509	5216.883895	15.607603	-0.088024	3.921728
459.550918	5208.891738	15.612608	-0.088057	3.918874
459.188508	5200.885000	15.617613	-0.087985	3.916003
459.263174	5192.898029	15.622618	-0.087993	3.913144
459.030581	5184.822657	15.627623	-0.087945	3.910247
459.114540	5176.845235	15.632627	-0.087955	3.907387
459.067786	5168.848103	15.637632	-0.087942	3.904517
459.164109	5160.886064	15.642637	-0.087954	3.901659
459.158084	5152.928997	15.647642	-0.087948	3.898799
458.951813	5144.908257	15.652647	-0.087905	3.895911
458.947819	5136.864895	15.657651	-0.087899	3.893016
459.072719	5128.852028	15.662656	-0.087917	3.890132
458.728606	5120.872082	15.667661	-0.087848	3.887249
458.781956	5112.882622	15.672666	-0.087852	3.884368
458.777206	5104.905579	15.677671	-0.087846	3.881489
458.686833	5096.870729	15.682675	-0.087824	3.878584
458.717326	5088.899432	15.687680	-0.087825	3.875703
458.686374	5080.713911	15.692685	-0.087814	3.872741
458.625308	5072.644014	15.697690	-0.087797	3.869818
458.585213	5064.750519	15.702695	-0.087785	3.866957
458.727685	5056.791991	15.707699	-0.087806	3.864073
458.877656	5048.846686	15.712704	-0.087829	3.861193
458.505885	5040.834896	15.717709	-0.087755	3.858276
458.496382	5032.853482	15.722714	-0.087748	3.855375
458.492349	5024.851189	15.727719	-0.087742	3.852465
458.455847	5016.829289	15.732723	-0.087730	3.849544
458.406924	5008.868154	15.737728	-0.087716	3.846643
458.381815	5000.824422	15.742733	-0.087706	3.843710
458.262388	4992.916945	15.747738	-0.087679	3.840823
458.169451	4984.866127	15.752743	-0.087656	3.837882
458.208641	4976.879951	15.757747	-0.087658	3.834964
458.204024	4968.909967	15.762752	-0.087652	3.832050
458.188446	4960.823008	15.767757	-0.087644	3.829090
458.316779	4952.907223	15.772762	-0.087663	3.826194
458.114688	4944.874650	15.777767	-0.087620	3.823246
457.955547	4936.906349	15.782771	-0.087586	3.820320
458.014829	4928.928434	15.787776	-0.087592	3.817393
457.802380	4920.876091	15.792781	-0.087547	3.814430
457.801695	4912.950430	15.797786	-0.087542	3.811517
457.556216	4904.933750	15.802791	-0.087491	3.808562
457.843393	4896.904633	15.807795	-0.087539	3.805612
457.900184	4888.949971	15.812800	-0.087545	3.802682
457.542722	4880.936550	15.817805	-0.087473	3.799719
457.660579	4872.989868	15.822810	-0.087490	3.796789
457.738421	4864.918954	15.827815	-0.087499	3.793809
457.690943	4856.919092	15.832819	-0.087485	3.790851
457.509548	4848.916487	15.837824	-0.087446	3.787887
457.501216	4840.915100	15.842829	-0.087440	3.784924
457.541243	4832.974408	15.847834	-0.087442	3.781983
457.492844	4824.953384	15.852839	-0.087428	3.779008
457.424188	4816.971024	15.857843	-0.087410	3.776044
457.531971	4808.968478	15.862848	-0.087425	3.773075
457.376834	4800.934188	15.867853	-0.087391	3.770085
457.403992	4792.957485	15.872858	-0.087391	3.767118
457.513055	4784.948594	15.877863	-0.087406	3.764139
457.205880	4777.013872	15.882867	-0.087344	3.761176
457.431579	4768.989632	15.887872	-0.087380	3.758189
457.240631	4760.991996	15.892877	-0.087340	3.755201
457.288481	4752.972044	15.897882	-0.087344	3.752207
457.156572	4744.947771	15.902887	-0.087314	3.749205
457.080467	4736.968277	15.907891	-0.087295	3.746218
457.165677	4728.977749	15.912896	-0.087305	3.743229
456.939780	4720.995300	15.917901	-0.087258	3.740233
456.955592	4713.011863	15.922906	-0.087256	3.737240
456.907796	4704.983056	15.927911	-0.087242	3.734226
456.914281	4696.984795	15.932915	-0.087238	3.731222
456.917817	4688.990672	15.937920	-0.087233	3.728218
457.043713	4680.977898	15.942925	-0.087252	3.725206
456.995203	4673.018175	15.947930	-0.087238	3.722209
457.022276	4665.006283	15.952935	-0.087238	3.719191
456.829840	4657.074377	15.957939	-0.087197	3.716195
456.974196	4648.982023	15.962944	-0.087218	3.713145
456.667767	4640.924160	15.967949	-0.087156	3.710094
456.825693	4632.951535	15.972954	-0.087180	3.707084
456.840687	4624.947467	15.977959	-0.087178	3.704056
456.672200	4617.014490	15.982963	-0.087142	3.701048
456.602282	4609.063567	15.987968	-0.087123	3.698034
456.418943	4601.017883	15.992973	-0.087084	3.694978
456.628793	4593.030716	15.997978	-0.087118	3.691951
456.402075	4585.028310	16.002983	-0.087071	3.688906
456.547442	4577.036241	16.007987	-0.087093	3.685871
456.481109	4569.094080	16.012992	-0.087075	3.682847
456.454000	4561.082968	16.017997	-0.087065	3.679796
456.315404	4553.157914	16.023002	-0.087034	3.676772
456.499711	4545.073315	16.028007	-0.087063	3.673693
456.439409	4537.054945	16.033011	-0.087047	3.670630
456.498727	4529.096609	16.038016	-0.087053	3.667591
456.323146	4521.079709	16.043021	-0.087015	3.664521
456.310265	4513.135385	16.048026	-0.087008	3.661480
456.099856	4505.099296	16.053031	-0.086963	3.658396
456.149361	4497.115293	16.058035	-0.086967	3.655337
456.263222	4489.112473	16.063040	-0.086983	3.652269
456.285436	4481.066456	16.068045	-0.086982	3.649180
455.947180	4473.149930	16.073050	-0.086914	3.646128
455.836545	4465.140340	16.078055	-0.086889	3.643044
456.204909	4457.134113	16.083059	-0.086952	3.639972
455.927576	4449.161626	16.088064	-0.086895	3.636892
455.791613	4441.098125	16.093069	-0.086865	3.633779
455.919375	4433.076020	16.098074	-0.086883	3.630686
455.934608	4425.093502	16.103079	-0.086881	3.627603
455.680394	4417.102501	16.108083	-0.086829	3.624507
455.873200	4409.149548	16.113088	-0.086859	3.621434
455.784564	4401.112444	16.118093	-0.086838	3.618319
455.787635	4393.131462	16.123098	-0.086833	3.615225
455.718740	4385.127760	16.128103	-0.086815	3.612118
455.776212	4377.113281	16.133107	-0.086821	3.609008
455.686419	4369.152178	16.138112	-0.086799	3.605912
455.423335	4361.165249	16.143117	-0.086745	3.602798
455.605485	4353.173111	16.148122	-0.086774	3.599691
455.760614	4345.191313	16.153127	-0.086797	3.596585
455.610167	4337.194055	16.158131	-0.086764	3.593463
455.525614	4329.203124	16.163136	-0.086743	3.590341
455.479618	4321.154123	16.168141	-0.086730	3.587195
455.471805	4313.198860	16.173146	-0.086723	3.584085
455.325522	4305.224579	16.178151	-0.086691	3.580960
455.537203	4297.208434	16.183155	-0.086725	3.577826
455.383296	4289.256679	16.188160	-0.086691	3.574704
455.122776	4281.240931	16.193165	-0.086638	3.571552
455.346662	4273.225807	16.198170	-0.086674	3.568410
455.196469	4265.245681	16.203175	-0.086641	3.565269
455.020116	4257.284884	16.208179	-0.086603	3.562132
455.180170	4249.273269	16.213184	-0.086628	3.558982
454.935306	4241.305531	16.218189	-0.086577	3.555835
455.011047	4233.220898	16.223194	-0.086586	3.552648
454.744067	4225.179847	16.228199	-0.086531	3.549465
454.735346	4217.214680	16.233203	-0.086525	3.546318
454.822814	4209.252614	16.238208	-0.086536	3.543171
454.714927	4201.251421	16.243213	-0.086510	3.540000
454.848183	4193.291447	16.248218	-0.086530	3.536850
454.649256	4185.298037	16.253223	-0.086488	3.533674
454.642707	4177.251106	16.258227	-0.086482	3.530480
454.654384	4169.281570	16.263232	-0.086479	3.527314
454.667789	4161.267268	16.268237	-0.086476	3.524127
454.495377	4153.333052	16.273242	-0.086439	3.520964
454.603269	4145.329206	16.278247	-0.086454	3.517778
454.635303	4137.307022	16.283251	-0.086455	3.514580
454.626353	4129.302287	16.288256	-0.086448	3.511385
454.489405	4121.295867	16.293261	-0.086417	3.508183
454.294379	4113.325463	16.298266	-0.086376	3.504990
454.390385	4105.349450	16.303271	-0.086389	3.501801
454.280697	4097.338834	16.308275	-0.086363	3.498589
454.314597	4089.367368	16.313280	-0.086364	3.495394
454.142259	4081.367020	16.318285	-0.086327	3.492178
454.129198	4073.384315	16.323290	-0.086319	3.488971
454.063812	4065.381203	16.328295	-0.086302	3.485751
454.228594	4057.411022	16.333299	-0.086328	3.482549
454.054093	4049.414932	16.338304	-0.086290	3.479322
453.917166	4041.462104	16.343309	-0.086259	3.476112
454.118555	4033.407411	16.348314	-0.086292	3.472868
453.962828	4025.406781	16.353319	-0.086258	3.469631
454.001348	4017.387574	16.358323	-0.086260	3.466390
453.898047	4009.408653	16.363328	-0.086235	3.463158
453.843393	4001.438003	16.368333	-0.086220	3.459928
453.883189	3993.473483	16.373338	-0.086222	3.456700
453.736515	3985.461259	16.378343	-0.086190	3.453444
453.652235	3977.437090	16.383347	-0.086169	3.450181
453.733693	3969.455647	16.388352	-0.086179	3.446939
453.502437	3961.462286	16.393357	-0.086131	3.443678
453.646255	3953.478631	16.398362	-0.086153	3.440431
453.673087	3945.520297	16.403367	-0.086152	3.437187
453.580363	3937.483553	16.408371	-0.086130	3.433904
453.487075	3929.488198	16.413376	-0.086108	3.430634
453.551341	3921.463305	16.418381	-0.086114	3.427355
453.676611	3913.464740	16.423386	-0.086133	3.424085
453.432016	3905.554953	16.428391	-0.086082	3.420836
453.420079	3897.520402	16.433395	-0.086075	3.417541
453.629976	3889.534731	16.438400	-0.086109	3.414270
453.391233	3881.509923	16.443405	-0.086059	3.410965
453.442817	3873.545741	16.448410	-0.086063	3.407691
453.503721	3865.538397	16.453415	-0.086070	3.404397
453.317473	3857.605413	16.458419	-0.086030	3.401122
453.205075	3849.635457	16.463424	-0.086004	3.397830
453.163045	3841.606215	16.468429	-0.085991	3.394514
453.425087	3833.512704	16.473434	-0.086034	3.391178
453.249424	3825.504312	16.478439	-0.085997	3.387859
453.199092	3817.526525	16.483443	-0.085982	3.384554
453.107323	3809.621014	16.488448	-0.085960	3.381274
452.999315	3801.624556	16.493453	-0.085935	3.377952
452.897568	3793.650519	16.498458	-0.085911	3.374637
453.133203	3785.616846	16.503463	-0.085949	3.371306
452.876917	3777.634145	16.508467	-0.085897	3.367975
452.589629	3769.676331	16.513472	-0.085838	3.364650
452.774289	3761.655708	16.518477	-0.085867	3.361312
452.751457	3753.695043	16.523482	-0.085858	3.357989
452.679136	3745.712145	16.528487	-0.085839	3.354651
452.771904	3737.658182	16.533491	-0.085851	3.351286
452.799302	3729.687944	16.538496	-0.085851	3.347950
452.581858	3721.700529	16.543501	-0.085806	3.344596
452.380385	3713.760774	16.548506	-0.085763	3.341258
452.518262	3705.738054	16.553511	-0.085784	3.337894
452.406412	3697.746466	16.558515	-0.085758	3.334531
452.511149	3689.730854	16.563520	-0.085772	3.331162
452.300472	3681.741104	16.568525	-0.085728	3.327790
452.448715	3673.735675	16.573530	-0.085750	3.324420
452.206399	3665.803469	16.578535	-0.085700	3.321064
452.212425	3657.786748	16.583539	-0.085696	3.317677
452.203915	3649.791296	16.588544	-0.085689	3.314296
452.147865	3641.740376	16.593549	-0.085674	3.310886
452.176338	3633.777225	16.598554	-0.085674	3.307512
452.106522	3625.782318	16.603559	-0.085656	3.304118
451.992213	3617.804746	16.608563	-0.085629	3.300727
452.031397	3609.850446	16.613568	-0.085632	3.297347
451.937419	3601.827389	16.618573	-0.085609	3.293930
452.278758	3593.817877	16.623578	-0.085667	3.290531
451.769052	3585.873444	16.628583	-0.085567	3.287124
451.769024	3577.864837	16.633587	-0.085562	3.283706
451.870346	3569.911718	16.638592	-0.085576	3.280312
451.952544	3561.928379	16.643597	-0.085586	3.276901
451.854730	3553.923617	16.648602	-0.085563	3.273469
451.687729	3545.925536	16.653607	-0.085527	3.270035
451.746278	3537.917721	16.658611	-0.085532	3.266601
451.695505	3529.960904	16.663616	-0.085518	3.263182
451.611027	3521.963264	16.668621	-0.085497	3.259740
451.535763	3513.997927	16.673626	-0.085478	3.256308
451.522255	3505.978181	16.678631	-0.085470	3.252852
451.458380	3497.947700	16.683635	-0.085453	3.249386
451.628635	3490.000484	16.688640	-0.085480	3.245961
451.368698	3482.013004	16.693645	-0.085426	3.242498
451.345322	3474.013144	16.698650	-0.085417	3.239036
451.521624	3466.014968	16.703655	-0.085444	3.235578
451.551912	3457.967514	16.708659	-0.085445	3.232089
451.501502	3449.982211	16.713664	-0.085430	3.228621
451.432957	3441.938271	16.718669	-0.085412	3.225122
451.412193	3434.030623	16.723674	-0.085403	3.221681
451.066937	3426.077843	16.728679	-0.085334	3.218204
450.909932	3418.083336	16.733683	-0.085300	3.214712
451.015887	3410.093726	16.738688	-0.085314	3.211229
450.954708	3402.056278	16.743693	-0.085298	3.207714
450.939101	3394.067618	16.748698	-0.085290	3.204219
450.883069	3386.131394	16.753703	-0.085274	3.200742
450.902660	3378.146155	16.758707	-0.085273	3.197242
450.988873	3370.153403	16.763712	-0.085284	3.193738
450.653876	3362.158854	16.768717	-0.085216	3.190212
450.719424	3354.157289	16.773722	-0.085223	3.186695
450.594548	3346.189723	16.778727	-0.085195	3.183181
450.733785	3338.182491	16.783731	-0.085216	3.179658
450.810634	3330.215482	16.788736	-0.085225	3.176145
450.795266	3322.203216	16.793741	-0.085217	3.172605
450.635421	3314.226455	16.798746	-0.085182	3.169070
450.644271	3306.241060	16.803751	-0.085179	3.165535
450.613502	3298.257839	16.808755	-0.085168	3.161995
450.537766	3290.307602	16.813760	-0.085148	3.158463
450.316733	3282.297464	16.818765	-0.085102	3.154895
450.418221	3274.282104	16.823770	-0.085116	3.151335
450.418849	3266.280637	16.828775	-0.085111	3.147772
450.190699	3258.283178	16.833779	-0.085063	3.144197
450.311056	3250.340681	16.838784	-0.085081	3.140657
450.302551	3242.328874	16.843789	-0.085074	3.137077
450.237575	3234.328254	16.848794	-0.085057	3.133496
450.098261	3226.353858	16.853799	-0.085026	3.129918
450.020490	3218.356160	16.858803	-0.085006	3.126329
450.128429	3210.398772	16.863808	-0.085021	3.122763
449.985234	3202.410607	16.868813	-0.084989	3.119167
450.080121	3194.454679	16.873818	-0.085002	3.115592
450.139085	3186.417871	16.878823	-0.085008	3.111974
450.048805	3178.416251	16.883827	-0.084986	3.108362
450.013675	3170.436470	16.888832	-0.084974	3.104758
449.880832	3162.484677	16.893837	-0.084944	3.101158
450.081522	3154.464787	16.898842	-0.084976	3.097538
449.928828	3146.510842	16.903847	-0.084943	3.093928
449.896577	3138.501918	16.908851	-0.084932	3.090294
449.773580	3130.551390	16.913856	-0.084904	3.086678
449.502267	3122.580541	16.918861	-0.084848	3.083042
449.581503	3114.590100	16.923866	-0.084858	3.079409
449.648089	3106.606220	16.928871	-0.084865	3.075773
449.444623	3098.532536	16.933875	-0.084822	3.072080
449.461765	3090.543311	16.938880	-0.084820	3.068432
449.582709	3082.508020	16.943885	-0.084837	3.064762
449.631441	3074.595255	16.948890	-0.084841	3.061141
449.544613	3066.640301	16.953895	-0.084820	3.057491
449.299833	3058.633521	16.958899	-0.084769	3.053804
449.456443	3050.632832	16.963904	-0.084793	3.050135
449.217728	3042.674737	16.968909	-0.084744	3.046462
449.291376	3034.694299	16.973914	-0.084752	3.042789
449.267654	3026.703708	16.978919	-0.084743	3.039103
449.032861	3018.762818	16.983923	-0.084694	3.035425
449.119683	3010.745835	16.988928	-0.084705	3.031722
448.884317	3002.759118	16.993933	-0.084656	3.028014
448.795821	2994.786613	16.998938	-0.084635	3.024315
448.690812	2986.831675	17.003943	-0.084610	3.020618
448.815892	2978.812233	17.008947	-0.084628	3.016899
448.808136	2970.825852	17.013952	-0.084622	3.013183
448.622271	2962.812988	17.018957	-0.084582	3.009442
448.858285	2954.820927	17.023962	-0.084621	3.005726
448.884921	2946.858561	17.028967	-0.084620	3.002010
448.651910	2938.902598	17.033971	-0.084572	2.998279
448.666646	2930.927272	17.038976	-0.084570	2.994547
448.761730	2922.870203	17.043981	-0.084582	2.990776
448.672008	2914.903924	17.048986	-0.084560	2.987033
448.456742	2906.937712	17.053991	-0.084515	2.983279
448.425656	2898.940241	17.058995	-0.084504	2.979515
448.698338	2890.965695	17.064000	-0.084550	2.975773
448.389542	2882.985467	17.069005	-0.084487	2.971994
448.338103	2875.009280	17.074010	-0.084473	2.968224
448.523065	2866.992293	17.079015	-0.084502	2.964443
448.355478	2859.056737	17.084019	-0.084466	2.960678
448.371997	2851.095853	17.089024	-0.084464	2.956905
448.218428	2843.092379	17.094029	-0.084430	2.953098
448.358895	2835.078206	17.099034	-0.084451	2.949296
448.431963	2827.098597	17.104039	-0.084459	2.945503
448.340158	2819.128682	17.109043	-0.084437	2.941700
448.332298	2811.171820	17.114048	-0.084431	2.937904
448.188490	2803.179229	17.119053	-0.084399	2.934078
447.956106	2795.208702	17.124058	-0.084350	2.930253
447.975969	2787.235630	17.129063	-0.084349	2.926435
447.937699	2779.224636	17.134067	-0.084337	2.922591
447.895662	2771.257097	17.139072	-0.084324	2.918763
447.920880	2763.281011	17.144077	-0.084323	2.914929
447.854430	2755.192607	17.149082	-0.084306	2.911031
447.827683	2747.227842	17.154087	-0.084296	2.907189
447.580316	2739.256488	17.159091	-0.084244	2.903327
447.905616	2731.293541	17.164096	-0.084300	2.899495
447.793249	2723.329883	17.169101	-0.084274	2.895634
447.506792	2715.359436	17.174106	-0.084215	2.891755
447.733103	2707.339920	17.179111	-0.084252	2.887875
447.512843	2699.378605	17.184115	-0.084206	2.883994
447.678654	2691.428876	17.189120	-0.084232	2.880134
447.608775	2683.466621	17.194125	-0.084214	2.876250
447.619724	2675.450537	17.199130	-0.084211	2.872338
447.434131	2667.494743	17.204135	-0.084171	2.868440
447.394140	2659.466647	17.209139	-0.084159	2.864510
447.211952	2651.571201	17.214144	-0.084120	2.860631
447.090040	2643.579978	17.219149	-0.084092	2.856703
447.112147	2635.564586	17.224154	-0.084091	2.852766
447.253431	2627.556349	17.229159	-0.084112	2.848834
447.081464	2619.584901	17.234163	-0.084075	2.844896
446.977690	2611.666202	17.239168	-0.084050	2.840984
446.753433	2603.679273	17.244173	-0.084004	2.837025
447.115909	2595.648494	17.249178	-0.084066	2.833072
447.120890	2587.645997	17.254183	-0.084062	2.829107
446.836984	2579.680007	17.259187	-0.084004	2.825139
446.930204	2571.736423	17.264192	-0.084016	2.821197
446.769156	2563.773949	17.269197	-0.083981	2.817226
446.695172	2555.772143	17.274202	-0.083962	2.813235
446.742104	2547.774772	17.279207	-0.083966	2.809248
446.804550	2539.791322	17.284211	-0.083972	2.805262
446.711718	2531.860081	17.289216	-0.083950	2.801288
446.516300	2523.897158	17.294221	-0.083908	2.797287
446.702892	2515.863177	17.299226	-0.083938	2.793266
446.626608	2507.874723	17.304231	-0.083918	2.789247
446.415752	2499.921441	17.309235	-0.083874	2.785232
446.659259	2491.943840	17.314240	-0.083914	2.781225
446.544571	2483.969697	17.319245	-0.083888	2.777194
446.411865	2476.008672	17.324250	-0.083858	2.773162
446.370316	2468.021571	17.329255	-0.083845	2.769117
446.457300	2460.018257	17.334259	-0.083856	2.765065
446.383726	2452.093918	17.339264	-0.083837	2.761037
446.353758	2444.106130	17.344269	-0.083827	2.756974
446.429136	2436.080417	17.349274	-0.083836	2.752892
446.424042	2428.052147	17.354279	-0.083830	2.748798
446.051444	2420.096751	17.359283	-0.083755	2.744713
446.188374	2412.164784	17.364288	-0.083775	2.740664
446.251727	2404.191621	17.369293	-0.083782	2.736584
446.029154	2396.217258	17.374298	-0.083736	2.732480
445.911303	2388.248682	17.379303	-0.083709	2.728379
445.910348	2380.250408	17.384307	-0.083703	2.724264
445.823034	2372.329561	17.389312	-0.083682	2.720177
445.650175	2364.358298	17.394317	-0.083645	2.716052
445.589712	2356.355677	17.399322	-0.083628	2.711912
445.588060	2348.376976	17.404327	-0.083623	2.707782
445.465194	2340.403869	17.409331	-0.083595	2.703640
445.479142	2332.444098	17.414336	-0.083592	2.699508
445.481484	2324.461903	17.419341	-0.083588	2.695357
445.494732	2316.447569	17.424346	-0.083585	2.691183
445.471921	2308.496039	17.429351	-0.083576	2.687034
445.327018	2300.531502	17.434355	-0.083543	2.682864
445.306960	2292.587023	17.439360	-0.083535	2.678705
445.161259	2284.626024	17.444365	-0.083502	2.674523
445.441248	2276.554727	17.449370	-0.083549	2.670304
445.357052	2268.611366	17.454375	-0.083529	2.666123
445.071360	2260.661729	17.459379	-0.083470	2.661918
445.242133	2252.686462	17.464384	-0.083497	2.657723
445.134320	2244.723954	17.469389	-0.083472	2.653510
445.187961	2236.711122	17.474394	-0.083477	2.649274
445.136617	2228.782764	17.479399	-0.083462	2.645069
445.014290	2220.820480	17.484403	-0.083434	2.640835
445.127839	2212.847112	17.489408	-0.083450	2.636603
444.892538	2204.871887	17.494413	-0.083401	2.632341
444.673113	2196.896649	17.499418	-0.083355	2.628073
444.840657	2188.915452	17.504423	-0.083381	2.623820
444.665672	2180.953195	17.509427	-0.083344	2.619548
444.685072	2173.007368	17.514432	-0.083342	2.615291
444.624066	2165.010328	17.519437	-0.083326	2.610993
444.530643	2157.038333	17.524442	-0.083303	2.606700
444.465760	2149.086116	17.529447	-0.083286	2.602413
444.633822	2141.092065	17.534451	-0.083312	2.598111
444.694731	2133.083218	17.539456	-0.083318	2.593787
444.709775	2124.930036	17.544461	-0.083316	2.589374
444.479134	2117.008096	17.549466	-0.083268	2.585063
444.547813	2109.107437	17.554471	-0.083276	2.580777
444.373069	2101.165780	17.559475	-0.083238	2.576444
444.463790	2093.202560	17.564480	-0.083250	2.572111
444.477755	2085.222917	17.569485	-0.083247	2.567756
444.359406	2077.276873	17.574490	-0.083220	2.563403
444.319619	2069.354992	17.579495	-0.083208	2.559061
444.106137	2061.388339	17.584499	-0.083163	2.554675
444.110398	2053.411653	17.589504	-0.083158	2.550291
443.998661	2045.432769	17.594509	-0.083133	2.545890
443.938621	2037.488900	17.599514	-0.083116	2.541504
444.112345	2029.523721	17.604519	-0.083144	2.537116
443.855312	2021.559933	17.609523	-0.083091	2.532690
443.818494	2013.590602	17.614528	-0.083079	2.528270
443.835846	2005.608940	17.619533	-0.083077	2.523838
443.909446	1997.649511	17.624538	-0.083085	2.519415
443.608225	1989.735464	17.629543	-0.083024	2.514982
443.560720	1981.691018	17.634547	-0.083010	2.510488
443.766397	1973.705741	17.639552	-0.083043	2.506036
443.710322	1965.767055	17.644557	-0.083028	2.501584
443.476666	1957.808157	17.649562	-0.082979	2.497099
443.652245	1949.837000	17.654567	-0.083007	2.492629
443.572065	1941.854084	17.659571	-0.082987	2.488126
443.492467	1933.914326	17.664576	-0.082967	2.483640
443.435097	1925.971185	17.669581	-0.082951	2.479144
443.638835	1917.986310	17.674586	-0.082984	2.474636
443.517739	1910.038808	17.679591	-0.082956	2.470118
443.196279	1902.068887	17.684595	-0.082891	2.465563
443.380709	1894.106302	17.689600	-0.082920	2.461042
443.270661	1886.146360	17.694605	-0.082895	2.456491
443.003163	1878.208161	17.699610	-0.082840	2.451933
443.285822	1870.212345	17.704615	-0.082887	2.447375
443.092153	1862.266214	17.709619	-0.082846	2.442801
442.943266	1854.332458	17.714624	-0.082813	2.438229
443.028769	1846.333041	17.719629	-0.082824	2.433628
442.957187	1838.311262	17.724634	-0.082806	2.428994
442.888453	1830.366224	17.729639	-0.082788	2.424395
442.584506	1822.430196	17.734643	-0.082726	2.419775
442.788452	1814.460634	17.739648	-0.082759	2.415165
442.736335	1806.498750	17.744653	-0.082744	2.410531
442.543176	1798.548952	17.749658	-0.082703	2.405885
442.676006	1790.590842	17.754663	-0.082723	2.401250
442.549610	1782.638480	17.759667	-0.082694	2.396589
442.482509	1774.676200	17.764672	-0.082677	2.391918
442.295618	1766.731938	17.769677	-0.082637	2.387239
442.324183	1758.750200	17.774682	-0.082637	2.382545
442.397298	1750.802013	17.779687	-0.082645	2.377866
442.252921	1742.837292	17.784691	-0.082613	2.373150
442.214515	1734.887711	17.789696	-0.082601	2.368442
442.379393	1726.912441	17.794701	-0.082627	2.363726
442.247200	1718.991884	17.799706	-0.082597	2.359010
442.411056	1711.031909	17.804711	-0.082623	2.354284
442.086145	1703.067215	17.809715	-0.082557	2.349506
442.075300	1695.102580	17.814720	-0.082550	2.344744
442.051710	1687.149079	17.819725	-0.082540	2.339978
442.289997	1679.158638	17.824730	-0.082580	2.335201
441.964268	1671.240681	17.829735	-0.082514	2.330413
441.643357	1663.300774	17.834739	-0.082449	2.325601
441.713667	1655.353189	17.839744	-0.082457	2.320807
441.683608	1647.414257	17.844749	-0.082446	2.316000
441.801440	1639.407356	17.849754	-0.082463	2.311154
441.922077	1631.444743	17.854759	-0.082480	2.306324
441.773794	1623.502994	17.859763	-0.082448	2.301476
441.693707	1615.583289	17.864768	-0.082428	2.296635
441.508234	1607.638179	17.869773	-0.082388	2.291761
441.588451	1599.636942	17.874778	-0.082398	2.286864
441.739327	1591.702714	17.879783	-0.082421	2.282003
441.417777	1583.780961	17.884787	-0.082356	2.277100
441.421050	1575.794748	17.889792	-0.082351	2.272174
441.325246	1567.821873	17.894797	-0.082328	2.267237
441.327592	1559.860889	17.899802	-0.082324	2.262305
441.218043	1551.945564	17.904807	-0.082298	2.257381
441.052903	1543.991887	17.909811	-0.082262	2.252417
441.209574	1536.018625	17.914816	-0.082287	2.247458
440.969564	1528.101321	17.919821	-0.082237	2.242489
440.941793	1520.152232	17.924826	-0.082227	2.237507
441.043155	1512.195134	17.929831	-0.082240	2.232521
440.924111	1504.245388	17.934835	-0.082213	2.227508
441.051357	1496.288541	17.939840	-0.082232	2.222502
441.072150	1488.349139	17.944845	-0.082230	2.217485
440.921657	1480.409862	17.949850	-0.082197	2.212443
440.891400	1472.467465	17.954855	-0.082187	2.207397
440.631518	1464.546627	17.959859	-0.082133	2.202333
440.764973	1456.589496	17.964864	-0.082153	2.197269
440.650915	1448.637470	17.969869	-0.082127	2.192175
440.876864	1440.638932	17.974874	-0.082163	2.187070
440.777276	1432.729215	17.979879	-0.082140	2.181980
440.320061	1424.832967	17.984883	-0.082050	2.176855
440.239093	1416.880276	17.989888	-0.082029	2.171715
440.474931	1408.885788	17.994893	-0.082068	2.166565
440.235026	1400.983555	17.999898	-0.082019	2.161419
440.234595	1393.059955	18.004903	-0.082013	2.156269
440.366435	1385.077778	18.009907	-0.082033	2.151080
440.341811	1377.127778	18.014912	-0.082023	2.145886
440.370063	1369.190419	18.019917	-0.082023	2.140692
440.324562	1361.261941	18.024922	-0.082010	2.135484
440.281812	1353.325880	18.029927	-0.081997	2.130259
439.915699	1345.426417	18.034931	-0.081923	2.125014
439.843377	1337.496215	18.039936	-0.081905	2.119764
439.972620	1329.552443	18.044941	-0.081924	2.114512
439.905384	1321.531556	18.049946	-0.081906	2.109176
439.835911	1313.610659	18.054951	-0.081888	2.103893
439.955811	1305.656638	18.059955	-0.081905	2.098592
439.833906	1297.745954	18.064960	-0.081878	2.093284
439.544029	1289.839101	18.069965	-0.081819	2.087949
439.665702	1281.880193	18.074970	-0.081836	2.082605
439.730237	1273.965846	18.079975	-0.081843	2.077272
439.560791	1266.037344	18.084979	-0.081806	2.071892
439.630772	1258.079027	18.089984	-0.081814	2.066502
439.446103	1250.181298	18.094989	-0.081775	2.061114
439.351635	1242.253432	18.099994	-0.081752	2.055700
439.379219	1234.312456	18.104999	-0.081752	2.050275
439.269573	1226.379796	18.110003	-0.081727	2.044827
439.413914	1218.448785	18.115008	-0.081749	2.039392
439.313629	1210.543706	18.120013	-0.081725	2.033935
439.217917	1202.582053	18.125018	-0.081702	2.028425
439.477507	1194.620379	18.130023	-0.081745	2.022936
439.154313	1186.741760	18.135027	-0.081680	2.017430
439.088505	1178.821595	18.140032	-0.081663	2.011907
439.132743	1170.875473	18.145037	-0.081666	2.006361
438.880065	1162.976949	18.150042	-0.081614	2.000803
438.892198	1155.071517	18.155047	-0.081611	1.995252
439.055892	1147.083008	18.160051	-0.081636	1.989643
438.926552	1139.185562	18.165056	-0.081607	1.984051
438.683070	1131.302126	18.170061	-0.081557	1.978442
438.543176	1123.373778	18.175066	-0.081525	1.972795
438.860182	1115.407729	18.180071	-0.081579	1.967154
438.657878	1107.510811	18.185075	-0.081537	1.961491
438.484318	1099.635148	18.190080	-0.081499	1.955830
438.686393	1091.638742	18.195085	-0.081532	1.950105
438.619227	1083.710089	18.200090	-0.081514	1.944384
438.560612	1075.808257	18.205095	-0.081498	1.938666
438.453498	1067.885871	18.210099	-0.081473	1.932912
438.509356	1059.958111	18.215104	-0.081479	1.927153
438.308571	1052.083661	18.220109	-0.081436	1.921389
437.998739	1044.204684	18.225114	-0.081373	1.915591
438.032474	1036.265386	18.230119	-0.081375	1.909770
437.909672	1028.356333	18.235123	-0.081347	1.903935
437.796333	1020.468260	18.240128	-0.081320	1.898099
437.855542	1012.533723	18.245133	-0.081326	1.892230
437.542100	1004.638122	18.250138	-0.081263	1.886330
437.713584	996.714238	18.255143	-0.081290	1.880445
437.640961	988.810222	18.260147	-0.081271	1.874529
437.675354	980.869983	18.265152	-0.081273	1.868579
437.674858	972.957391	18.270157	-0.081267	1.862627
437.354714	965.090600	18.275162	-0.081203	1.856653
437.646370	957.136634	18.280167	-0.081252	1.850665
437.603863	949.228318	18.285171	-0.081239	1.844653
437.376804	941.383286	18.290176	-0.081192	1.838648
437.278174	933.484395	18.295181	-0.081168	1.832598
437.294464	925.543992	18.300186	-0.081166	1.826509
437.267637	917.669450	18.305191	-0.081156	1.820445
437.116321	909.793496	18.310195	-0.081123	1.814345
437.129400	901.864853	18.315200	-0.081120	1.808203
437.346984	893.950939	18.320205	-0.081156	1.802077
437.014086	886.105109	18.325210	-0.081089	1.795916
437.038570	878.151480	18.330215	-0.081088	1.789693
437.013443	870.247822	18.335219	-0.081078	1.783481
436.762771	862.397801	18.340224	-0.081027	1.777262
436.763092	854.498798	18.345229	-0.081022	1.771014
436.722617	846.594130	18.350234	-0.081009	1.764733
436.780031	838.723262	18.355239	-0.081015	1.758470
436.554489	830.856277	18.360243	-0.080968	1.752152
436.692250	822.926511	18.365248	-0.080988	1.745806
436.573567	815.075762	18.370253	-0.080961	1.739468
436.356583	807.218965	18.375258	-0.080916	1.733090
436.421182	799.308685	18.380263	-0.080923	1.726680
436.420690	791.432523	18.385267	-0.080917	1.720267
436.368527	783.566165	18.390272	-0.080903	1.713830
436.410725	775.656206	18.395277	-0.080905	1.707346
435.930303	767.840953	18.400282	-0.080811	1.700847
435.974281	759.961577	18.405287	-0.080814	1.694338
435.846363	752.069508	18.410291	-0.080785	1.687771
435.799472	744.201394	18.415296	-0.080771	1.681210
435.796229	736.340127	18.420301	-0.080766	1.674634
435.631428	728.462012	18.425306	-0.080730	1.667996
435.656692	720.592589	18.430311	-0.080730	1.661364
435.653270	712.722617	18.435315	-0.080724	1.654702
435.433086	704.866895	18.440320	-0.080678	1.647996
435.347531	697.027345	18.445325	-0.080657	1.641294
435.595328	689.111779	18.450330	-0.080698	1.634545
435.398698	681.240519	18.455335	-0.080656	1.627745
435.367531	673.370973	18.460339	-0.080646	1.620941
435.408789	665.520149	18.465344	-0.080648	1.614134
435.378651	657.655848	18.470349	-0.080638	1.607277
435.251822	649.819755	18.475354	-0.080609	1.600402
435.313819	641.979096	18.480359	-0.080615	1.593520
435.332193	634.102073	18.485363	-0.080614	1.586569
435.268928	626.271386	18.490368	-0.080597	1.579618
435.140221	618.455103	18.495373	-0.080568	1.572639
435.059345	610.596212	18.500378	-0.080548	1.565597
434.867223	602.814407	18.505383	-0.080507	1.558577
434.773060	594.963948	18.510387	-0.080485	1.551478
434.610575	587.135262	18.515392	-0.080449	1.544355
434.625428	579.290960	18.520397	-0.080447	1.537212
434.688380	571.424675	18.525402	-0.080454	1.530022
434.590171	563.622751	18.530407	-0.080431	1.522833
434.332229	555.828563	18.535411	-0.080377	1.515593
434.204520	547.996765	18.540416	-0.080349	1.508303
434.188849	540.168424	18.545421	-0.080341	1.500998
434.325850	532.321131	18.550426	-0.080361	1.493663
434.097073	524.532742	18.555431	-0.080314	1.486291
433.905416	516.745023	18.560435	-0.080273	1.478888
434.037737	508.880019	18.565440	-0.080293	1.471425
434.098502	501.032202	18.570445	-0.080299	1.463930
433.667610	493.294772	18.575450	-0.080214	1.456424
433.760502	485.467228	18.580455	-0.080226	1.448875
433.572997	477.683770	18.585459	-0.080186	1.441285
433.524726	469.895375	18.590464	-0.080172	1.433672
433.339647	462.107272	18.595469	-0.080133	1.425997
433.433651	454.291311	18.600474	-0.080145	1.418298
433.373659	446.506151	18.605479	-0.080129	1.410562
433.071214	438.761980	18.610483	-0.080068	1.402784
433.012686	430.992681	18.615488	-0.080052	1.394979
432.913696	423.204116	18.620493	-0.080028	1.387103
432.713739	415.437448	18.625498	-0.079986	1.379187
432.838680	407.637535	18.630503	-0.080004	1.371247
432.793554	399.856386	18.635507	-0.079991	1.363251
432.557736	392.133757	18.640512	-0.079942	1.355235
432.298934	384.398063	18.645517	-0.079889	1.347154
432.248983	376.625866	18.650522	-0.079875	1.339022
432.378404	368.848313	18.655527	-0.079894	1.330867
432.355836	361.096554	18.660531	-0.079885	1.322661
432.313044	353.344787	18.665536	-0.079872	1.314401
432.248780	345.500018	18.670541	-0.079855	1.305985
431.844430	337.836608	18.675546	-0.079775	1.297648
431.869917	330.097895	18.680551	-0.079774	1.289254
431.619096	322.402622	18.685555	-0.079723	1.280802
431.607943	314.683006	18.690560	-0.079716	1.272311
431.640002	306.952942	18.695565	-0.079717	1.263760
431.362960	299.279237	18.700570	-0.079660	1.255155
431.298889	291.574003	18.705575	-0.079643	1.246495
431.037528	283.918249	18.710579	-0.079590	1.237794
430.895008	276.223764	18.715584	-0.079558	1.229009
430.787887	268.535163	18.720589	-0.079533	1.220174
430.350190	260.900775	18.725594	-0.079447	1.211273
430.154685	253.239504	18.730599	-0.079406	1.202322
429.905946	245.593093	18.735603	-0.079354	1.193311
429.629296	237.941761	18.740608	-0.079298	1.184220
429.306556	230.322652	18.745613	-0.079233	1.175088
429.312238	222.628497	18.750618	-0.079229	1.165860
429.228449	215.003155	18.755623	-0.079209	1.156625
428.702047	207.390111	18.760627	-0.079106	1.147237
428.440563	199.769671	18.765632	-0.079052	1.137818
428.188625	192.161394	18.770637	-0.079000	1.128338
427.751281	184.590727	18.775642	-0.078914	1.118785
427.335164	177.025662	18.780647	-0.078832	1.109161
426.881811	169.463033	18.785651	-0.078743	1.099447
426.477296	161.906369	18.790656	-0.078662	1.089665
425.853445	154.395751	18.795661	-0.078541	1.079805
425.328039	146.857629	18.800666	-0.078439	1.069840
425.025654	139.298637	18.805671	-0.078378	1.059804
424.294260	131.817733	18.810675	-0.078237	1.049677
423.788789	124.310113	18.815680	-0.078138	1.039468
423.525987	116.774487	18.820685	-0.078084	1.029177
422.912655	109.297414	18.825690	-0.077965	1.018779
422.425770	101.823993	18.830695	-0.077870	1.008308
421.731009	94.393106	18.835699	-0.077735	0.997737
421.064119	86.926280	18.840704	-0.077606	0.987008
420.292204	79.525264	18.845709	-0.077458	0.976228
419.985463	72.043119	18.850714	-0.077396	0.965328
419.370060	64.656323	18.855719	-0.077277	0.954365
418.605273	57.531823	18.860723	-0.077130	0.943625