Fri Mar 12 13:52:26 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.916883	-0.154178	0.000000	-0.000128	0.721773

0.703854	-0.129485	0.005005	-0.000088	0.721747
0.662089	-0.120355	0.010010	-0.000081	0.721751
0.683361	-0.121615	0.015014	-0.000085	0.721756
0.304928	-0.059128	0.020019	-0.000014	0.721746
0.152419	-0.027180	0.025024	0.000014	0.721756
0.199964	-0.039712	0.030029	0.000005	0.721748
0.468879	-0.086737	0.035034	-0.000045	0.721750
0.612701	-0.111686	0.040038	-0.000072	0.721751
0.400190	-0.077751	0.045043	-0.000032	0.721743
0.608542	-0.109147	0.050048	-0.000071	0.721755
0.379960	-0.072827	0.055053	-0.000029	0.721746
0.222186	-0.044072	0.060058	0.000001	0.721748
0.396311	-0.088079	0.065062	-0.000032	0.721722
0.267468	-0.209638	0.070067	-0.000008	0.721438
0.277427	-0.205590	0.075072	-0.000010	0.721450
0.432067	-0.238500	0.080077	-0.000038	0.721439
0.704705	-0.284522	0.085082	-0.000089	0.721444
0.738460	-0.288483	0.090086	-0.000096	0.721449
0.523903	-0.255690	0.095091	-0.000056	0.721438
0.288626	-0.315103	0.100096	-0.000012	0.721239
0.183899	-0.354525	0.105101	0.000008	0.721125
-0.054093	-0.311325	0.110106	0.000052	0.721127
0.166771	-0.350709	0.115110	0.000011	0.721127
0.425423	-0.399759	0.120115	-0.000038	0.721121
0.539833	-0.456254	0.125120	-0.000059	0.721050
0.256449	-0.492447	0.130125	-0.000006	0.720879
0.314694	-0.502318	0.135130	-0.000017	0.720881
0.333585	-0.503515	0.140134	-0.000021	0.720885
0.037124	-0.455179	0.145139	0.000034	0.720876
0.386092	-0.674937	0.150144	-0.000030	0.720566
0.504142	-0.707472	0.155149	-0.000052	0.720544
0.136371	-0.641003	0.160154	0.000016	0.720546
0.331005	-0.702439	0.165158	-0.000020	0.720493
0.223766	-0.820226	0.170163	-0.000000	0.720224
-0.179264	-0.743672	0.175168	0.000075	0.720233
-0.343227	-0.718846	0.180173	0.000105	0.720225
-0.040805	-0.855495	0.185178	0.000049	0.720062
0.261777	-0.987521	0.190182	-0.000008	0.719908
0.260212	-0.993041	0.195187	-0.000007	0.719896
0.602076	-1.105589	0.200192	-0.000071	0.719795
0.491602	-1.183270	0.205197	-0.000050	0.719603
0.203621	-1.130611	0.210202	0.000003	0.719606
-0.126634	-1.153211	0.215206	0.000065	0.719445
-0.023398	-1.259880	0.220211	0.000045	0.719271
0.010072	-1.261027	0.225216	0.000039	0.719281
-0.421339	-1.287097	0.230221	0.000119	0.719078
-0.323519	-1.361347	0.235226	0.000101	0.718966
-0.062854	-1.405294	0.240230	0.000053	0.718971
-0.045000	-1.547124	0.245235	0.000049	0.718698
0.081377	-1.591594	0.250240	0.000026	0.718654
0.114353	-1.648055	0.255245	0.000020	0.718555
0.156834	-1.755378	0.260250	0.000012	0.718358
-0.065378	-1.712811	0.265254	0.000053	0.718364
-0.244258	-1.846905	0.270259	0.000086	0.718036
-0.302782	-1.840881	0.275264	0.000097	0.718028
-0.594590	-1.876897	0.280269	0.000151	0.717854
-0.229434	-2.015965	0.285274	0.000084	0.717708
-0.020241	-2.092335	0.290278	0.000045	0.717631
-0.774203	-2.084551	0.295283	0.000185	0.717381
-1.008431	-2.037831	0.300288	0.000228	0.717391
-0.657727	-2.235920	0.305293	0.000163	0.717122
-0.741673	-2.239132	0.310298	0.000179	0.717087
-1.490934	-2.205694	0.315302	0.000318	0.716889
-2.802027	-2.040598	0.320307	0.000562	0.716753
-2.524848	-2.086279	0.325312	0.000511	0.716761
-3.064582	-2.117826	0.330317	0.000611	0.716508
-3.945447	-1.989984	0.335322	0.000775	0.716451
-3.520786	-2.064304	0.340326	0.000696	0.716454
-3.785374	-2.103860	0.345331	0.000745	0.716282
-4.780653	-1.999363	0.350336	0.000930	0.716138
-4.317096	-2.084239	0.355341	0.000844	0.716133
-4.434270	-2.062947	0.360346	0.000866	0.716134
-4.688785	-2.136870	0.365350	0.000913	0.715898
-4.807979	-2.124120	0.370355	0.000935	0.715882
-5.303148	-2.030884	0.375360	0.001027	0.715892
-5.521997	-2.035906	0.380365	0.001068	0.715804
-5.925722	-2.093110	0.385370	0.001143	0.715549
-5.727586	-2.126886	0.390374	0.001106	0.715552
-6.519817	-1.989943	0.395379	0.001254	0.715544
-5.968512	-2.087894	0.400384	0.001151	0.715544
-6.652316	-2.124745	0.405389	0.001278	0.715230
-7.360081	-1.997965	0.410394	0.001410	0.715231
-7.340482	-1.998402	0.415398	0.001406	0.715237
-6.832037	-2.095566	0.420403	0.001311	0.715224
-7.013451	-2.094150	0.425408	0.001345	0.715163
-8.067408	-2.034526	0.430413	0.001541	0.714909
-7.888552	-2.068016	0.435418	0.001508	0.714906
-7.833720	-2.072804	0.440422	0.001498	0.714916
-8.291023	-1.995519	0.445427	0.001583	0.714908
-7.798920	-2.079506	0.450432	0.001491	0.714915
-8.447534	-2.109462	0.455437	0.001612	0.714626
-9.022412	-2.016180	0.460442	0.001719	0.714608
-9.035566	-2.010431	0.465446	0.001721	0.714615
-8.685231	-2.078757	0.470451	0.001656	0.714604
-8.569904	-2.093853	0.475456	0.001634	0.714615
-8.947938	-2.082890	0.480461	0.001705	0.714503
-9.771018	-2.049688	0.485466	0.001858	0.714278
-9.252558	-2.137748	0.490470	0.001761	0.714286
-10.257143	-1.963464	0.495475	0.001948	0.714277
-9.918431	-2.020208	0.500480	0.001885	0.714284
-9.622446	-2.076924	0.505485	0.001830	0.714276
-10.132554	-2.018435	0.510490	0.001925	0.714212
-10.774434	-2.022412	0.515494	0.002044	0.713977
-10.524561	-2.072561	0.520499	0.001998	0.713966
-10.783048	-2.020632	0.525504	0.002046	0.713978
-10.785889	-2.021751	0.530509	0.002046	0.713975
-10.725737	-2.032679	0.535514	0.002035	0.713974
-10.521160	-2.067335	0.540518	0.001997	0.713978
-11.245018	-2.065735	0.545523	0.002132	0.713725
-11.815381	-1.996284	0.550528	0.002238	0.713661
-11.570599	-2.043209	0.555533	0.002192	0.713655
-11.796185	-2.003935	0.560538	0.002234	0.713653
-11.755929	-2.007903	0.565542	0.002227	0.713660
-11.578779	-2.044230	0.570547	0.002194	0.713650
-11.345559	-2.080261	0.575552	0.002150	0.713661
-12.479395	-2.025293	0.580557	0.002361	0.713369
-12.610867	-2.004551	0.585562	0.002386	0.713364
-12.237160	-2.067343	0.590566	0.002316	0.713371
-12.600636	-2.008719	0.595571	0.002384	0.713359
-12.582325	-2.008033	0.600576	0.002380	0.713367
-12.231805	-2.073051	0.605581	0.002315	0.713362
-12.456096	-2.076345	0.610586	0.002357	0.713276
-13.487697	-2.013657	0.615590	0.002548	0.713035
-13.374355	-2.039867	0.620595	0.002527	0.713024
-13.227786	-2.062741	0.625600	0.002500	0.713030
-13.639440	-1.989567	0.630605	0.002577	0.713030
-13.547683	-2.008245	0.635610	0.002559	0.713025
-13.297169	-2.049718	0.640614	0.002513	0.713032
-13.779225	-1.984865	0.645619	0.002602	0.712990
-14.335147	-2.021852	0.650624	0.002706	0.712719
-14.170534	-2.054098	0.655629	0.002675	0.712714
-14.702306	-1.960931	0.660634	0.002774	0.712711
-14.502708	-1.993099	0.665638	0.002737	0.712717
-14.428887	-2.011678	0.670643	0.002723	0.712707
-14.339313	-2.023223	0.675648	0.002706	0.712716
-14.520261	-1.993976	0.680653	0.002740	0.712710
-14.857024	-2.046285	0.685658	0.002803	0.712486
-15.130179	-2.044498	0.690662	0.002854	0.712393
-15.312261	-2.015008	0.695667	0.002887	0.712387
-15.435359	-1.990855	0.700672	0.002910	0.712392
-15.375484	-2.005261	0.705677	0.002899	0.712384
-15.111200	-2.053151	0.710682	0.002850	0.712383
-15.448631	-1.988496	0.715686	0.002912	0.712392
-15.797075	-2.002238	0.720691	0.002977	0.712241
-16.066709	-2.027068	0.725696	0.003027	0.712096
-16.126429	-2.020672	0.730701	0.003039	0.712088
-16.470054	-1.960358	0.735706	0.003102	0.712086
-16.098341	-2.023004	0.740710	0.003033	0.712093
-15.959721	-2.051127	0.745715	0.003007	0.712086
-16.326481	-1.982617	0.750720	0.003076	0.712093
-15.967416	-2.115424	0.755725	0.003009	0.711956
-16.968855	-2.036054	0.760730	0.003195	0.711758
-17.079838	-2.012300	0.765734	0.003216	0.711766
-17.312797	-1.975423	0.770739	0.003259	0.711757
-16.982828	-2.030673	0.775744	0.003197	0.711765
-16.964546	-2.035629	0.780749	0.003194	0.711761
-17.343090	-1.968622	0.785754	0.003264	0.711760
-17.004462	-2.082841	0.790758	0.003201	0.711653
-17.955526	-2.014473	0.795763	0.003378	0.711452
-17.831302	-2.031537	0.800768	0.003355	0.711462
-17.781846	-2.043221	0.805773	0.003346	0.711456
-17.801327	-2.041448	0.810778	0.003350	0.711453
-17.849846	-2.030039	0.815782	0.003358	0.711459
-18.234886	-1.965277	0.820787	0.003430	0.711451
-17.703818	-2.136417	0.825792	0.003331	0.711298
-18.706553	-2.038017	0.830797	0.003518	0.711138
-19.055867	-1.975277	0.835802	0.003583	0.711140
-18.586697	-2.054594	0.840806	0.003495	0.711148
-18.765897	-2.028113	0.845811	0.003529	0.711137
-18.967964	-1.988600	0.850816	0.003566	0.711145
-18.910825	-2.000713	0.855821	0.003556	0.711141
-18.742936	-2.094160	0.860826	0.003524	0.711014
-19.235293	-2.074591	0.865830	0.003616	0.710878
-19.179673	-2.088545	0.870835	0.003606	0.710870
-19.236223	-2.075706	0.875840	0.003616	0.710876
-19.573861	-2.014420	0.880845	0.003679	0.710878
-19.625236	-2.005710	0.885850	0.003688	0.710877
-19.581002	-2.035736	0.890854	0.003680	0.710833
-20.203399	-2.073094	0.895859	0.003796	0.710537
-20.387490	-2.037489	0.900864	0.003830	0.710543
-20.763444	-1.973164	0.905869	0.003900	0.710538
-20.477161	-2.024626	0.910874	0.003847	0.710537
-20.144975	-2.081650	0.915878	0.003785	0.710541
-20.959981	-1.939318	0.920883	0.003936	0.710536
-20.425304	-2.046183	0.925888	0.003837	0.710513
-20.658654	-2.148542	0.930893	0.003880	0.710225
-21.268920	-2.041052	0.935898	0.003994	0.710223
-21.310840	-2.030472	0.940902	0.004002	0.710229
-21.206344	-2.054734	0.945907	0.003982	0.710218
-21.352719	-2.025070	0.950912	0.004009	0.710225
-21.538572	-1.995011	0.955917	0.004044	0.710219
-21.470263	-2.056489	0.960922	0.004031	0.710121
-22.337148	-2.010841	0.965926	0.004192	0.709903
-22.294995	-2.022780	0.970931	0.004184	0.709895
-22.218837	-2.031604	0.975936	0.004170	0.709904
-22.150834	-2.044948	0.980941	0.004157	0.709902
-22.356744	-2.011625	0.985946	0.004196	0.709895
-21.961320	-2.078440	0.990950	0.004122	0.709903
-22.015559	-2.106579	0.995955	0.004132	0.709827
-22.813969	-2.073905	1.000960	0.004281	0.709608
-22.981697	-2.046564	1.005965	0.004312	0.709603
-23.339054	-1.985663	1.010970	0.004378	0.709598
-22.756322	-2.087111	1.015974	0.004270	0.709603
-23.299826	-1.992411	1.020979	0.004371	0.709598
-23.438829	-1.965546	1.025984	0.004397	0.709603
-22.859152	-2.114798	1.030989	0.004289	0.709511
-24.142291	-2.007655	1.035994	0.004528	0.709268
-23.856572	-2.055042	1.040998	0.004474	0.709275
-24.090806	-2.019825	1.046003	0.004518	0.709262
-24.052967	-2.022177	1.051008	0.004511	0.709271
-23.989921	-2.032882	1.056013	0.004499	0.709272
-24.165126	-2.003505	1.061018	0.004532	0.709268
-23.924876	-2.056011	1.066022	0.004487	0.709249
-24.746933	-2.055048	1.071027	0.004640	0.708958
-24.687207	-2.062276	1.076032	0.004629	0.708965
-24.795505	-2.043887	1.081037	0.004649	0.708963
-25.177489	-1.977577	1.086042	0.004720	0.708960
-24.886497	-2.025205	1.091046	0.004666	0.708968
-24.930254	-2.022996	1.096051	0.004674	0.708957
-24.802037	-2.042237	1.101056	0.004650	0.708965
-25.446059	-2.083502	1.106061	0.004770	0.708652
-25.763486	-2.033216	1.111066	0.004829	0.708640
-25.487227	-2.078182	1.116070	0.004777	0.708648
-25.842404	-2.021792	1.121075	0.004843	0.708635
-26.018035	-1.985711	1.126080	0.004876	0.708644
-25.603465	-2.060706	1.131085	0.004799	0.708642
-25.694334	-2.050098	1.136090	0.004816	0.708631
-26.373056	-2.064181	1.141094	0.004942	0.708361
-26.670877	-2.016529	1.146099	0.004997	0.708350
-26.549188	-2.034338	1.151104	0.004975	0.708358
-26.532129	-2.038874	1.156109	0.004971	0.708355
-26.650325	-2.018446	1.161114	0.004993	0.708354
-26.331001	-2.071908	1.166118	0.004934	0.708361
-26.712522	-2.023555	1.171123	0.005005	0.708322
-27.479906	-2.036644	1.176128	0.005148	0.708021
-27.151607	-2.095758	1.181133	0.005086	0.708020
-27.797522	-1.981737	1.186138	0.005207	0.708018
-27.559697	-2.020638	1.191142	0.005162	0.708025
-27.673734	-2.005778	1.196147	0.005183	0.708014
-27.482603	-2.035733	1.201152	0.005148	0.708023
-27.439351	-2.044352	1.206157	0.005140	0.708021
-28.121886	-2.074169	1.211162	0.005267	0.707717
-28.162106	-2.069233	1.216166	0.005274	0.707713
-28.727132	-1.973635	1.221171	0.005379	0.707703
-28.718186	-1.973922	1.226176	0.005377	0.707706
-28.466651	-2.018070	1.231181	0.005331	0.707707
-28.517535	-2.011156	1.236186	0.005340	0.707703
-28.236308	-2.057990	1.241190	0.005288	0.707710
-28.760907	-2.074301	1.246195	0.005385	0.707489
-29.330480	-2.026046	1.251200	0.005491	0.707383
-29.096889	-2.066881	1.256205	0.005448	0.707384
-29.356614	-2.024024	1.261210	0.005496	0.707378
-29.345479	-2.023029	1.266214	0.005494	0.707384
-29.295086	-2.037006	1.271219	0.005484	0.707374
-28.961661	-2.092329	1.276224	0.005422	0.707382
-29.356636	-2.150276	1.281229	0.005496	0.707125
-30.148803	-2.029929	1.286234	0.005643	0.707083
-30.124562	-2.029872	1.291238	0.005639	0.707092
-30.209601	-2.019589	1.296243	0.005654	0.707082
-29.885335	-2.076121	1.301248	0.005594	0.707085
-29.896462	-2.074308	1.306253	0.005596	0.707084
-30.395455	-2.006645	1.311258	0.005689	0.707042
-30.484505	-2.131919	1.316262	0.005705	0.706759
-30.780295	-2.083795	1.321267	0.005760	0.706749
-31.524882	-1.947393	1.326272	0.005899	0.706757
-31.072008	-2.029573	1.331277	0.005815	0.706754
-30.950542	-2.051745	1.336282	0.005792	0.706753
-31.040857	-2.031853	1.341286	0.005809	0.706761
-31.274600	-1.993894	1.346291	0.005852	0.706754
-31.417878	-2.115462	1.351296	0.005879	0.706458
-31.877148	-2.041067	1.356301	0.005964	0.706443
-32.286129	-1.969034	1.361306	0.006040	0.706442
-31.571826	-2.090241	1.366310	0.005907	0.706454
-31.985898	-2.022077	1.371315	0.005984	0.706443
-32.279974	-1.966758	1.376320	0.006039	0.706449
-31.669450	-2.075448	1.381325	0.005925	0.706449
-32.285860	-2.110048	1.386330	0.006040	0.706159
-32.741523	-2.039863	1.391334	0.006125	0.706137
-32.854182	-2.024649	1.396339	0.006146	0.706127
-32.497319	-2.084047	1.401344	0.006079	0.706136
-32.908415	-2.012100	1.406349	0.006156	0.706133
-33.031499	-1.993707	1.411354	0.006179	0.706126
-32.439732	-2.096027	1.416358	0.006068	0.706133
-32.950033	-2.140740	1.421363	0.006163	0.705860
-33.688794	-2.005530	1.426368	0.006301	0.705867
-33.674345	-2.008276	1.431373	0.006298	0.705867
-33.386975	-2.062158	1.436378	0.006245	0.705862
-33.423996	-2.049093	1.441382	0.006251	0.705875
-33.842309	-1.980204	1.446387	0.006329	0.705863
-33.639732	-2.060842	1.451392	0.006291	0.705774
-34.223129	-2.077555	1.456397	0.006400	0.705531
-34.339419	-2.059710	1.461402	0.006422	0.705525
-34.300785	-2.062539	1.466406	0.006414	0.705534
-34.251053	-2.076734	1.471411	0.006405	0.705523
-34.341883	-2.057493	1.476416	0.006422	0.705529
-34.074847	-2.104686	1.481421	0.006372	0.705530
-34.672491	-2.125793	1.486426	0.006483	0.705274
-35.508839	-2.004047	1.491430	0.006639	0.705219
-35.715935	-1.969624	1.496435	0.006677	0.705214
-35.159448	-2.067217	1.501440	0.006574	0.705217
-35.207609	-2.057910	1.506445	0.006583	0.705219
-35.583724	-1.993395	1.511450	0.006653	0.705214
-35.077992	-2.081707	1.516454	0.006558	0.705217
-35.297349	-2.147401	1.521459	0.006599	0.705006
-36.646132	-1.962423	1.526464	0.006850	0.704895
-36.084535	-2.064185	1.531469	0.006746	0.704892
-36.094785	-2.063962	1.536474	0.006748	0.704889
-36.185813	-2.043447	1.541478	0.006764	0.704897
-36.387622	-2.013957	1.546483	0.006802	0.704884
-36.156266	-2.049831	1.551488	0.006759	0.704895
-35.902301	-2.183933	1.556493	0.006712	0.704716
-37.343594	-1.990258	1.561498	0.006980	0.704589
-36.809667	-2.080310	1.566502	0.006880	0.704600
-36.688706	-2.105415	1.571507	0.006858	0.704593
-36.816739	-2.079274	1.576512	0.006882	0.704599
-36.703600	-2.100079	1.581517	0.006860	0.704598
-36.539526	-2.184037	1.586522	0.006830	0.704488
-37.534623	-2.113794	1.591526	0.007015	0.704272
-37.731993	-2.083152	1.596531	0.007052	0.704263
-37.686964	-2.088601	1.601536	0.007043	0.704268
-37.662156	-2.093233	1.606541	0.007039	0.704268
-38.185432	-2.003132	1.611546	0.007136	0.704262
-37.898450	-2.049355	1.616550	0.007083	0.704272
-37.697350	-2.185023	1.621555	0.007045	0.704071
-38.544513	-2.089230	1.626560	0.007203	0.703959
-38.798407	-2.043089	1.631565	0.007250	0.703961
-38.714088	-2.062472	1.636570	0.007234	0.703953
-38.491535	-2.096360	1.641574	0.007193	0.703964
-38.897968	-2.029796	1.646579	0.007268	0.703953
-38.786727	-2.046200	1.651584	0.007248	0.703960
-38.640102	-2.187276	1.656589	0.007220	0.703728
-39.792967	-2.027509	1.661594	0.007435	0.703636
-39.585609	-2.059543	1.666598	0.007396	0.703646
-39.621350	-2.059104	1.671603	0.007403	0.703634
-39.723554	-2.038925	1.676608	0.007422	0.703638
-39.827368	-2.019077	1.681613	0.007441	0.703641
-39.659994	-2.051332	1.686618	0.007410	0.703636
-39.557250	-2.152278	1.691622	0.007391	0.703469
-40.700923	-2.010329	1.696627	0.007603	0.703344
-40.509490	-2.042466	1.701632	0.007568	0.703348
-39.871253	-2.156121	1.706637	0.007449	0.703349
-40.608687	-2.027749	1.711642	0.007586	0.703343
-40.682128	-2.011345	1.716646	0.007600	0.703349
-40.310855	-2.081191	1.721651	0.007531	0.703342
-40.408095	-2.183436	1.726656	0.007549	0.703101
-41.395059	-2.050763	1.731661	0.007732	0.703014
-41.500823	-2.035360	1.736666	0.007752	0.703007
-40.826945	-2.152165	1.741670	0.007626	0.703014
-41.496996	-2.037155	1.746675	0.007751	0.703005
-41.494860	-2.037165	1.751680	0.007751	0.703006
-40.952757	-2.131325	1.756685	0.007650	0.703011
-41.755944	-2.135337	1.761690	0.007799	0.702713
-42.226559	-2.056887	1.766694	0.007887	0.702702
-42.213744	-2.063359	1.771699	0.007884	0.702694
-41.946306	-2.109592	1.776704	0.007834	0.702697
-42.171590	-2.068589	1.781709	0.007876	0.702699
-42.515486	-2.012076	1.786714	0.007940	0.702689
-41.900757	-2.116022	1.791718	0.007826	0.702701
-42.932718	-2.095618	1.796723	0.008018	0.702370
-43.186400	-2.047427	1.801728	0.008065	0.702376
-43.037395	-2.074050	1.806733	0.008037	0.702376
-43.109087	-2.064989	1.811738	0.008051	0.702369
-43.352066	-2.017162	1.816742	0.008096	0.702378
-43.334765	-2.023737	1.821747	0.008092	0.702371
-42.892868	-2.100114	1.826752	0.008010	0.702376
-43.259044	-2.129916	1.831757	0.008078	0.702184
-44.396249	-1.981536	1.836762	0.008290	0.702074
-43.560062	-2.126909	1.841766	0.008134	0.702082
-43.784579	-2.091676	1.846771	0.008176	0.702072
-44.188852	-2.015824	1.851776	0.008251	0.702080
-43.928249	-2.061729	1.856781	0.008203	0.702081
-43.623130	-2.119546	1.861786	0.008146	0.702074
-44.408500	-2.107194	1.866790	0.008292	0.701816
-45.082948	-2.023013	1.871795	0.008417	0.701743
-44.763446	-2.078033	1.876800	0.008358	0.701747
-44.559361	-2.113321	1.881805	0.008320	0.701750
-45.008980	-2.037290	1.886810	0.008403	0.701742
-44.607282	-2.103072	1.891814	0.008329	0.701753
-44.676292	-2.094408	1.896819	0.008341	0.701746
-45.546724	-2.069906	1.901824	0.008503	0.701482
-45.809547	-2.042989	1.906829	0.008552	0.701441
-45.673729	-2.069845	1.911834	0.008527	0.701436
-45.825144	-2.038889	1.916838	0.008555	0.701444
-45.979417	-2.017024	1.921843	0.008584	0.701433
-45.600054	-2.081641	1.926848	0.008513	0.701439
-45.662752	-2.069474	1.931853	0.008525	0.701441
-46.327810	-2.033586	1.936858	0.008648	0.701274
-46.703428	-2.038036	1.941862	0.008718	0.701130
-46.196009	-2.133199	1.946867	0.008624	0.701120
-46.738845	-2.034604	1.951872	0.008725	0.701124
-46.812579	-2.020507	1.956877	0.008738	0.701126
-46.437671	-2.091539	1.961882	0.008669	0.701118
-46.321153	-2.107246	1.966886	0.008647	0.701128
-46.497934	-2.154458	1.971891	0.008680	0.700969
-47.026463	-2.105144	1.976896	0.008778	0.700878
-46.932098	-2.120485	1.981901	0.008760	0.700881
-47.341417	-2.051092	1.986906	0.008837	0.700874
-46.948780	-2.115924	1.991910	0.008763	0.700884
-47.052716	-2.103299	1.996915	0.008783	0.700872
-47.972424	-2.067576	2.001920	0.008954	0.700612

-48.072128	-2.086222	2.011917	0.008972	0.700539
-48.428635	-2.024451	2.021914	0.009039	0.700535
-48.298279	-2.046726	2.031910	0.009014	0.700538
-48.128520	-2.075565	2.041907	0.008983	0.700541
-48.320623	-2.042379	2.051904	0.009018	0.700539
-48.134642	-2.076116	2.061901	0.008983	0.700538
-48.449194	-2.019282	2.071898	0.009042	0.700540
-48.139383	-2.075949	2.081894	0.008984	0.700537
-48.255646	-2.053396	2.091891	0.009006	0.700541
-48.359907	-2.034912	2.101888	0.009025	0.700541
-48.081087	-2.084664	2.111885	0.008973	0.700541
-47.661327	-2.002453	2.121882	0.008895	0.700860
-47.303767	-2.057567	2.131878	0.008828	0.700877
-47.094928	-2.094068	2.141875	0.008789	0.700879
-47.379786	-2.042607	2.151872	0.008842	0.700881
-47.332001	-2.052008	2.161869	0.008833	0.700879
-47.340026	-2.034523	2.171866	0.008834	0.700912
-46.549378	-2.071073	2.181862	0.008687	0.701123
-46.667069	-2.048920	2.191859	0.008709	0.701126
-46.630855	-2.055641	2.201856	0.008702	0.701126
-46.655489	-2.046185	2.211853	0.008706	0.701136
-46.156660	-1.987389	2.221850	0.008613	0.701436
-45.546410	-2.095428	2.231846	0.008500	0.701437
-45.638757	-2.077988	2.241843	0.008517	0.701440
-45.684334	-2.043640	2.251840	0.008525	0.701493
-44.898801	-2.057515	2.261837	0.008379	0.701749
-44.870958	-2.063321	2.271834	0.008373	0.701747
-44.879670	-2.061451	2.281830	0.008375	0.701748
-44.621598	-2.027389	2.291827	0.008327	0.701910
-43.833830	-2.084976	2.301824	0.008180	0.702078
-44.040477	-2.048739	2.311821	0.008218	0.702077
-44.212460	-2.020267	2.321818	0.008250	0.702073
-43.290667	-2.044060	2.331814	0.008078	0.702357
-43.290845	-2.036173	2.341811	0.008078	0.702373
-43.042259	-2.080915	2.351808	0.008032	0.702373
-42.942016	-2.021341	2.361805	0.008013	0.702529
-42.108952	-2.089049	2.371802	0.007858	0.702693
-42.353026	-2.045986	2.381798	0.007903	0.702692
-42.506650	-2.016730	2.391795	0.007932	0.702696
-41.643985	-2.032821	2.401792	0.007771	0.702975
-41.520192	-2.038557	2.411789	0.007748	0.703008
-41.559702	-2.032588	2.421786	0.007755	0.703006
-41.157193	-2.024125	2.431782	0.007680	0.703168
-40.535852	-2.047380	2.441779	0.007564	0.703345
-40.284906	-2.090836	2.451776	0.007517	0.703348
-40.656656	-2.026677	2.461773	0.007587	0.703344
-39.882975	-2.038846	2.471770	0.007442	0.703598
-40.007476	-1.996424	2.481766	0.007465	0.703639
-39.708862	-2.050624	2.491763	0.007410	0.703637
-39.233649	-2.048536	2.501760	0.007321	0.703813
-38.628959	-2.084737	2.511757	0.007208	0.703957
-38.745551	-2.065569	2.521754	0.007230	0.703954
-38.796716	-2.055277	2.531750	0.007239	0.703957
-38.257461	-2.022197	2.541747	0.007139	0.704218
-37.817069	-2.076902	2.551744	0.007057	0.704266
-37.924846	-2.058997	2.561741	0.007077	0.704263
-37.696269	-2.055660	2.571738	0.007034	0.704353
-37.082098	-2.046562	2.581734	0.006920	0.704592
-36.946415	-2.070239	2.591731	0.006894	0.704593
-37.060145	-2.050149	2.601728	0.006915	0.704593
-36.301445	-2.064562	2.611725	0.006774	0.704837
-36.255772	-2.048600	2.621722	0.006765	0.704885
-36.189687	-2.059791	2.631718	0.006753	0.704887
-36.104123	-2.023892	2.641715	0.006737	0.704990
-35.109054	-2.090694	2.651712	0.006551	0.705213
-35.363111	-2.046326	2.661709	0.006599	0.705211
-35.152854	-2.085237	2.671706	0.006559	0.705209
-34.750787	-2.027141	2.681702	0.006484	0.705470
-34.318938	-2.075999	2.691699	0.006404	0.705527
-34.179464	-2.099961	2.701696	0.006378	0.705529
-34.308089	-2.039813	2.711693	0.006402	0.705604
-33.344925	-2.083139	2.721690	0.006222	0.705862
-33.328744	-2.085587	2.731686	0.006219	0.705863
-33.838076	-1.994434	2.741683	0.006314	0.705864
-32.954513	-2.052711	2.751680	0.006149	0.706064
-33.144859	-1.986857	2.761677	0.006184	0.706129
-32.779397	-2.053162	2.771674	0.006116	0.706126
-32.591354	-2.003357	2.781670	0.006081	0.706294
-31.915464	-2.049050	2.791667	0.005955	0.706445
-31.968334	-2.037789	2.801664	0.005965	0.706449
-31.897983	-2.014149	2.811661	0.005952	0.706521
-31.022863	-2.055759	2.821658	0.005789	0.706751
-31.233638	-2.018608	2.831654	0.005828	0.706751
-31.326247	-1.999601	2.841651	0.005845	0.706756
-30.505428	-1.982832	2.851648	0.005692	0.707084
-30.492110	-1.984107	2.861645	0.005689	0.707086
-30.235669	-2.032417	2.871642	0.005642	0.707081
-30.099275	-1.943653	2.881638	0.005616	0.707308
-29.369734	-2.038905	2.891635	0.005480	0.707378
-29.485124	-2.017549	2.901632	0.005501	0.707380
-29.220673	-1.996009	2.911629	0.005452	0.707518
-28.452165	-2.039673	2.921626	0.005309	0.707706
-28.818601	-1.976143	2.931622	0.005377	0.707702
-28.557816	-2.014668	2.941619	0.005328	0.707718
-27.946270	-1.975949	2.951616	0.005214	0.708015
-27.291942	-2.092682	2.961613	0.005092	0.708015
-27.582413	-2.040511	2.971610	0.005146	0.708016
-27.527276	-1.989160	2.981606	0.005136	0.708139
-26.203304	-2.117304	2.991603	0.004889	0.708355
-26.726608	-2.023284	3.001600	0.004987	0.708357
-26.750829	-2.019778	3.011597	0.004991	0.708355
-26.262155	-2.001934	3.021594	0.004900	0.708566
-25.925484	-2.024630	3.031590	0.004837	0.708641
-25.730079	-2.058433	3.041587	0.004801	0.708643
-25.899874	-1.985355	3.051584	0.004832	0.708729
-24.932780	-2.042491	3.061581	0.004652	0.708960
-25.288077	-1.980720	3.071578	0.004718	0.708957
-25.303052	-1.978784	3.081574	0.004721	0.708956
-24.357563	-1.994811	3.091571	0.004544	0.709261
-24.407915	-1.983485	3.101568	0.004554	0.709266
-24.028699	-2.051177	3.111565	0.004483	0.709266
-23.969733	-1.957190	3.121562	0.004472	0.709475
-23.356529	-2.007039	3.131558	0.004358	0.709594
-23.288494	-2.017279	3.141555	0.004345	0.709598
-23.275684	-1.995248	3.151552	0.004342	0.709647
-22.340641	-2.037591	3.161549	0.004168	0.709896
-22.431481	-2.020924	3.171546	0.004185	0.709897
-22.296801	-2.046676	3.181542	0.004160	0.709894
-21.913790	-2.032353	3.191539	0.004088	0.710059
-21.485746	-2.027170	3.201536	0.004009	0.710222
-21.436995	-2.035223	3.211533	0.003999	0.710224
-21.420252	-2.040857	3.221530	0.003996	0.710219
-20.849846	-2.008990	3.231526	0.003890	0.710486
-20.584143	-2.031721	3.241523	0.003840	0.710535
-20.591873	-2.028181	3.251520	0.003842	0.710540
-20.351465	-2.025114	3.261517	0.003797	0.710631
-19.754921	-2.010505	3.271514	0.003685	0.710873
-19.413355	-2.072381	3.281510	0.003622	0.710871
-19.914186	-1.982575	3.291507	0.003715	0.710873
-19.024876	-2.050011	3.301504	0.003549	0.711055
-18.916569	-2.025207	3.311501	0.003529	0.711143
-18.910542	-2.027054	3.321498	0.003528	0.711141
-18.882661	-1.998371	3.331494	0.003522	0.711209
-18.039299	-2.024659	3.341491	0.003365	0.711456
-17.965814	-2.037117	3.351488	0.003351	0.711458
-18.035354	-2.025147	3.361485	0.003364	0.711457
-17.693241	-1.956033	3.371482	0.003300	0.711717
-17.013941	-2.052217	3.381478	0.003174	0.711767
-17.333584	-1.994702	3.391475	0.003233	0.711768
-16.821500	-2.006004	3.401472	0.003138	0.711928
-16.181779	-2.036892	3.411469	0.003019	0.712093
-16.369009	-2.004030	3.421466	0.003053	0.712093
-16.218161	-2.030743	3.431462	0.003025	0.712093
-15.779093	-1.959986	3.441459	0.002943	0.712390
-15.406259	-2.026409	3.451456	0.002874	0.712390
-15.439334	-2.022154	3.461453	0.002880	0.712387
-15.075982	-1.981604	3.471450	0.002812	0.712597
-14.501502	-2.026453	3.481446	0.002705	0.712712
-14.830933	-1.968099	3.491443	0.002766	0.712712
-14.361112	-2.013880	3.501440	0.002679	0.712787
-13.651729	-2.020075	3.511437	0.002546	0.713027
-13.625053	-2.023954	3.521434	0.002541	0.713029
-13.715748	-2.010770	3.531430	0.002558	0.713023
-13.175851	-1.997449	3.541427	0.002457	0.713241
-12.502705	-2.054828	3.551424	0.002332	0.713366
-12.851810	-1.992854	3.561421	0.002397	0.713366
-12.665744	-2.026270	3.571418	0.002362	0.713365
-12.127125	-1.976895	3.581414	0.002262	0.713654
-12.034333	-1.993575	3.591411	0.002244	0.713654
-11.754666	-2.041309	3.601408	0.002192	0.713659
-11.514748	-1.989259	3.611405	0.002147	0.713847
-10.925583	-2.031890	3.621402	0.002038	0.713972
-11.103034	-2.001602	3.631398	0.002070	0.713969
-11.076540	-1.991997	3.641395	0.002065	0.713998
-10.204361	-2.004783	3.651392	0.001903	0.714281
-10.163512	-2.013152	3.661389	0.001895	0.714279
-9.964671	-2.051243	3.671386	0.001858	0.714274
-9.931018	-1.958933	3.681382	0.001852	0.714470
-9.361507	-1.991900	3.691379	0.001745	0.714606
-9.173366	-2.024779	3.701376	0.001710	0.714607
-9.412930	-1.962801	3.711373	0.001755	0.714646
-8.486404	-1.995876	3.721370	0.001582	0.714908
-8.368694	-2.018136	3.731366	0.001560	0.714906
-8.236228	-2.040583	3.741363	0.001535	0.714908
-7.789179	-2.030612	3.751360	0.001452	0.715086
-7.647976	-1.981340	3.761357	0.001426	0.715234
-7.323352	-2.041721	3.771354	0.001365	0.715229
-7.449327	-2.019151	3.781350	0.001388	0.715230
-6.709118	-2.002872	3.791347	0.001250	0.715524
-6.480035	-2.033266	3.801344	0.001208	0.715545
-6.327981	-2.060737	3.811341	0.001179	0.715544
-6.413458	-2.013610	3.821338	0.001195	0.715608
-5.672375	-2.008326	3.831334	0.001057	0.715880
-5.530658	-2.032298	3.841331	0.001030	0.715883
-5.561780	-2.024693	3.851328	0.001036	0.715887
-5.385637	-1.982858	3.861325	0.001003	0.716032
-4.582231	-2.075193	3.871322	0.000854	0.716133
-4.992603	-2.003620	3.881318	0.000930	0.716130
-4.640420	-2.039123	3.891315	0.000864	0.716184
-4.066986	-2.006972	3.901312	0.000757	0.716451
-3.919212	-2.033600	3.911309	0.000730	0.716450
-4.117803	-1.997859	3.921306	0.000766	0.716451
-3.389279	-2.005046	3.931302	0.000631	0.716694
-3.105428	-2.023930	3.941299	0.000578	0.716757
-3.205812	-2.004894	3.951296	0.000596	0.716759
-3.080654	-1.965097	3.961293	0.000573	0.716883
-2.929635	-1.889208	3.971290	0.000545	0.717086
-2.184781	-2.022625	3.981286	0.000406	0.717085
-2.365969	-1.954151	3.991283	0.000439	0.717157
-1.958058	-1.912516	4.001280	0.000363	0.717383
-1.499179	-1.993885	4.011277	0.000278	0.717384
-2.556219	-1.744449	4.021274	0.000474	0.717505
-0.817910	-1.953601	4.031270	0.000151	0.717704
-1.707025	-1.795660	4.041267	0.000316	0.717703
-1.634405	-1.695797	4.051264	0.000302	0.717926
-0.701646	-1.814534	4.061261	0.000129	0.718020
-1.698894	-1.587134	4.071258	0.000314	0.718119
-0.614949	-1.660799	4.081254	0.000112	0.718355
-1.413561	-1.495554	4.091251	0.000261	0.718400
-0.614269	-1.513719	4.101248	0.000112	0.718646
-0.680181	-1.479558	4.111245	0.000124	0.718690
-1.076870	-1.270482	4.121242	0.000198	0.718964
-0.622069	-1.288325	4.131238	0.000113	0.719088
-1.116106	-1.107768	4.141235	0.000205	0.719271
-0.491641	-1.075054	4.151232	0.000088	0.719555
-0.481976	-1.012059	4.161229	0.000086	0.719683
-0.499866	-0.899687	4.171226	0.000089	0.719898
-0.041909	-0.852582	4.181222	0.000004	0.720152
-0.428012	-0.694726	4.191219	0.000076	0.720328
-0.254015	-0.618055	4.201216	0.000043	0.720540
-0.779114	-0.354944	4.211213	0.000140	0.720874
-0.219027	-0.353022	4.221210	0.000036	0.721074
0.009687	-0.277158	4.231206	-0.000007	0.721304
-0.277192	-0.096047	4.241203	0.000047	0.721559
0.109843	-0.028013	4.251200	-0.000026	0.721829
0.047572	0.129628	4.261197	-0.000014	0.722117
0.000000	0.311001	4.271194	-0.000006	0.722457

0.253151	0.878388	4.276198	-0.000053	0.723658
0.405891	2.104122	4.281203	-0.000083	0.726110
0.917782	3.872419	4.286208	-0.000179	0.729733
1.428997	6.199723	4.291213	-0.000276	0.734419
2.079263	9.001967	4.296218	-0.000399	0.740033
3.202993	12.225159	4.301222	-0.000610	0.746565
4.053473	15.951319	4.306227	-0.000771	0.753895
5.370784	20.015957	4.311232	-0.001019	0.761939
7.081222	24.424676	4.316237	-0.001340	0.770660
8.992445	29.178504	4.321242	-0.001699	0.779976
13.145873	33.933818	4.326246	-0.002476	0.789897
15.436670	39.385626	4.331251	-0.002906	0.800343
17.381101	45.226110	4.336256	-0.003272	0.811225
19.147527	51.365098	4.341261	-0.003605	0.822423
20.768330	57.820367	4.346266	-0.003911	0.833964
21.850281	64.590554	4.351270	-0.004117	0.845715
22.769348	71.606393	4.356275	-0.004293	0.857663
24.012928	78.767012	4.361280	-0.004529	0.869775
25.245642	86.118614	4.366285	-0.004763	0.882024
26.558481	93.622473	4.371290	-0.005013	0.894369
28.072457	101.262994	4.376294	-0.005300	0.906813
28.600488	109.215261	4.381299	-0.005403	0.919302
30.138294	117.103323	4.386304	-0.005695	0.931795
32.013499	125.054539	4.391309	-0.006049	0.944305
32.632085	133.322309	4.396314	-0.006170	0.956794
34.051224	141.532344	4.401318	-0.006440	0.969241
35.533922	149.817973	4.406323	-0.006721	0.981655
36.469483	158.294697	4.411328	-0.006901	0.994049
37.588816	166.760809	4.416333	-0.007115	1.006321
38.601594	175.272906	4.421338	-0.007309	1.018482
39.750977	183.819449	4.426342	-0.007529	1.030579
40.610548	192.432509	4.431347	-0.007694	1.042557
41.440785	201.086874	4.436352	-0.007855	1.054447
42.472448	209.725573	4.441357	-0.008052	1.066230
43.259606	218.418156	4.446362	-0.008205	1.077899
44.473192	227.031098	4.451366	-0.008436	1.089434
45.203655	235.731612	4.456371	-0.008578	1.100853
45.897185	244.443590	4.461376	-0.008713	1.112161
46.531535	253.152945	4.466381	-0.008837	1.123339
47.226914	261.841555	4.471386	-0.008972	1.134393
48.162033	270.492484	4.476390	-0.009152	1.145345
48.541556	279.262408	4.481395	-0.009228	1.156222
49.342302	287.878848	4.486400	-0.009383	1.166898
50.297686	296.486444	4.491405	-0.009567	1.177498
51.081035	305.093139	4.496410	-0.009718	1.187967
51.787574	313.721229	4.501414	-0.009855	1.198354
52.346266	322.339921	4.506419	-0.009965	1.208610
52.875764	330.961394	4.511424	-0.010069	1.218778
53.232502	339.601025	4.516429	-0.010141	1.228849
54.193390	348.112497	4.521434	-0.010326	1.238807
54.849496	356.660455	4.526438	-0.010454	1.248669
55.354587	365.217314	4.531443	-0.010553	1.258435
55.754079	373.779750	4.536448	-0.010633	1.268111
56.306301	382.303508	4.541453	-0.010742	1.277700
56.815351	390.788540	4.546458	-0.010842	1.287166
57.283833	399.301159	4.551462	-0.010935	1.296586
57.900422	407.747255	4.556467	-0.011056	1.305892
58.423764	416.338542	4.561472	-0.011159	1.315272
58.898777	424.773418	4.566477	-0.011253	1.324409
59.250241	433.207659	4.571482	-0.011324	1.333460
59.919439	441.585534	4.576486	-0.011454	1.342447
60.112277	450.036058	4.581491	-0.011495	1.351367
60.560751	458.423309	4.586496	-0.011584	1.360207
61.331701	466.758953	4.591501	-0.011733	1.368991
62.052146	475.109674	4.596506	-0.011873	1.377726
62.488660	483.485803	4.601510	-0.011960	1.386384
62.951130	491.876910	4.606515	-0.012051	1.395007
63.334560	500.226609	4.611520	-0.012128	1.403522
63.976961	508.544493	4.616525	-0.012253	1.411996
64.298877	516.896205	4.621530	-0.012319	1.420401
65.043547	525.194426	4.626534	-0.012463	1.428772
65.373068	533.551510	4.631539	-0.012530	1.437085
65.690515	541.877472	4.636544	-0.012594	1.445317
65.971121	550.235381	4.641549	-0.012652	1.453528
66.356379	558.528921	4.646554	-0.012729	1.461647
66.785058	566.860592	4.651558	-0.012815	1.469764
67.002192	575.212727	4.656563	-0.012861	1.477823
67.429397	583.460468	4.661568	-0.012946	1.485771
67.986891	591.731046	4.666573	-0.013055	1.493719
68.268785	600.001426	4.671578	-0.013113	1.501582
68.697875	608.273613	4.676582	-0.013198	1.509428
69.132492	616.525667	4.681587	-0.013284	1.517216
69.487206	624.765817	4.686592	-0.013356	1.524940
69.992568	633.022426	4.691597	-0.013455	1.532663
70.363227	641.257988	4.696602	-0.013530	1.540308
70.545624	649.546051	4.701606	-0.013569	1.547935
70.859816	657.813983	4.706611	-0.013633	1.555525
71.300131	666.013601	4.711616	-0.013721	1.563035
71.696260	674.241852	4.716621	-0.013800	1.570529
72.065638	682.465359	4.721626	-0.013874	1.577978
72.497094	690.679066	4.726630	-0.013960	1.585393
72.641426	698.951822	4.731635	-0.013992	1.592784
73.057827	707.144353	4.736640	-0.014075	1.600109
73.317630	715.373510	4.741645	-0.014129	1.607410
73.646579	723.587158	4.746650	-0.014195	1.614675
74.287650	731.753555	4.751654	-0.014320	1.621909
74.612809	739.985250	4.756659	-0.014386	1.629124
75.124622	748.212315	4.761664	-0.014487	1.636328
75.580143	756.386112	4.766669	-0.014577	1.643447
75.709791	764.606505	4.771674	-0.014607	1.650531
76.166113	772.787397	4.776678	-0.014697	1.657595
76.433477	780.968965	4.781683	-0.014752	1.664604
76.813311	789.159759	4.786688	-0.014828	1.671606
77.172408	797.345327	4.791693	-0.014901	1.678572
77.553650	805.500672	4.796698	-0.014977	1.685486
77.890134	813.713452	4.801702	-0.015045	1.692415
78.161819	821.893691	4.806707	-0.015101	1.699279
78.692408	830.036584	4.811712	-0.015205	1.706118
78.982732	838.267782	4.816717	-0.015265	1.712972
79.218929	846.431946	4.821722	-0.015314	1.719736
79.667447	854.572517	4.826726	-0.015403	1.726481
79.927119	862.771809	4.831731	-0.015457	1.733224
80.149958	870.934849	4.836736	-0.015503	1.739906
80.393239	879.114780	4.841741	-0.015554	1.746579
80.699683	887.283532	4.846746	-0.015617	1.753226
81.080763	895.431021	4.851750	-0.015693	1.759839
81.500368	903.551942	4.856755	-0.015776	1.766411
82.027389	911.696407	4.861760	-0.015880	1.772991
82.354640	919.861931	4.866765	-0.015946	1.779538
82.509431	928.028141	4.871770	-0.015980	1.786041
83.006581	936.217243	4.876774	-0.016078	1.792580
83.362691	944.358020	4.881779	-0.016150	1.799039
83.375448	952.516652	4.886784	-0.016158	1.805448
83.771448	960.663870	4.891789	-0.016237	1.811872
84.096149	968.792658	4.896794	-0.016303	1.818250
84.392598	976.926103	4.901798	-0.016363	1.824605
84.738797	985.065413	4.906803	-0.016433	1.830949
85.159772	993.185940	4.911808	-0.016517	1.837265
85.452049	1001.330604	4.916813	-0.016577	1.843563
85.431331	1009.508170	4.921818	-0.016578	1.849828
85.864956	1017.629955	4.926822	-0.016664	1.856082
86.115757	1025.755149	4.931827	-0.016716	1.862297
86.546403	1033.882118	4.936832	-0.016802	1.868512
86.831671	1042.057097	4.941837	-0.016860	1.874727
87.068817	1050.165164	4.946842	-0.016910	1.880865
87.465601	1058.273789	4.951846	-0.016989	1.887001
87.770054	1066.407146	4.956851	-0.017051	1.893126
88.047687	1074.527218	4.961856	-0.017108	1.899218
88.332126	1082.650534	4.966861	-0.017166	1.905293
88.254574	1090.819653	4.971866	-0.017157	1.911343
88.492415	1098.965019	4.976870	-0.017207	1.917390
88.822909	1107.040451	4.981875	-0.017274	1.923378
89.312594	1115.120330	4.986880	-0.017370	1.929368
89.513459	1123.278021	4.991885	-0.017413	1.935364
89.559925	1131.407341	4.996890	-0.017427	1.941304
90.241838	1139.486145	5.001894	-0.017559	1.947259
90.232999	1147.693914	5.006899	-0.017563	1.953214
90.483470	1155.780488	5.011904	-0.017615	1.959091
91.128459	1163.813689	5.016909	-0.017740	1.964954
91.401070	1171.933401	5.021914	-0.017797	1.970822
91.677311	1180.071355	5.026918	-0.017853	1.976686
91.836518	1188.169813	5.031923	-0.017888	1.982492
92.180104	1196.273277	5.036928	-0.017958	1.988304
92.437120	1204.430567	5.041933	-0.018011	1.994128
92.626764	1212.502582	5.046938	-0.018052	1.999867
93.062998	1220.584416	5.051942	-0.018138	2.005623
93.025733	1228.745748	5.056947	-0.018137	2.011369
93.366565	1236.839122	5.061952	-0.018205	2.017089
93.855958	1244.910850	5.066957	-0.018302	2.022794
93.971045	1253.034124	5.071962	-0.018329	2.028480
94.016597	1261.216803	5.076966	-0.018342	2.034185
94.354437	1269.266774	5.081971	-0.018411	2.039811
94.515836	1277.356600	5.086976	-0.018446	2.045431
94.940813	1285.436046	5.091981	-0.018530	2.051055
95.113496	1293.539133	5.096986	-0.018568	2.056655
95.623574	1301.597130	5.101990	-0.018668	2.062242
95.770587	1309.717895	5.106995	-0.018701	2.067821
95.966601	1317.843054	5.112000	-0.018743	2.073393
96.369758	1325.906388	5.117005	-0.018823	2.078928
96.371856	1334.015403	5.122010	-0.018829	2.084439
96.539234	1342.133415	5.127014	-0.018865	2.089959
96.963359	1350.207572	5.132019	-0.018950	2.095459
97.342444	1358.285014	5.137024	-0.019026	2.100943
97.549931	1366.388020	5.142029	-0.019070	2.106412
97.664301	1374.544131	5.147034	-0.019096	2.111894
98.273834	1382.611996	5.152038	-0.019215	2.117351
98.420520	1390.687295	5.157043	-0.019248	2.122754
98.289409	1398.804965	5.162048	-0.019229	2.128145
99.164062	1406.829645	5.167053	-0.019397	2.133556
99.454936	1414.894270	5.172058	-0.019456	2.138925
99.608845	1423.003758	5.177062	-0.019490	2.144296
99.600627	1431.129881	5.182067	-0.019494	2.149650
99.893254	1439.219475	5.187072	-0.019554	2.154995
100.423697	1447.254436	5.192077	-0.019658	2.160312
100.447941	1455.347838	5.197082	-0.019668	2.165608
100.754106	1463.439394	5.202086	-0.019730	2.170916
100.812521	1471.558603	5.207091	-0.019746	2.176206
100.741001	1479.671540	5.212096	-0.019738	2.181467
101.412737	1487.692133	5.217101	-0.019869	2.186723
101.797586	1495.763719	5.222106	-0.019946	2.191974
101.929145	1503.888827	5.227110	-0.019976	2.197223
101.979115	1511.976946	5.232115	-0.019990	2.202429
102.211000	1520.036922	5.237120	-0.020039	2.207620
102.553405	1528.126132	5.242125	-0.020108	2.212829
102.505474	1536.224928	5.247130	-0.020104	2.217996
103.032984	1544.252226	5.252134	-0.020208	2.223156
103.295599	1552.338416	5.257139	-0.020262	2.228319
103.621327	1560.418951	5.262144	-0.020328	2.233471
103.753781	1568.514783	5.267149	-0.020358	2.238605
103.993156	1576.568075	5.272154	-0.020408	2.243709
104.394291	1584.631233	5.277158	-0.020488	2.248821
104.447336	1592.759514	5.282163	-0.020503	2.253933
104.719657	1600.816228	5.287168	-0.020559	2.259007
105.200932	1608.866250	5.292173	-0.020654	2.264084
105.456885	1616.932375	5.297178	-0.020707	2.269140
105.846055	1625.110932	5.302182	-0.020785	2.274265
106.074068	1633.139582	5.307187	-0.020833	2.279273
106.446315	1641.168164	5.312192	-0.020907	2.284281
106.714932	1649.229430	5.317197	-0.020962	2.289290
106.884133	1657.318946	5.322202	-0.020999	2.294297
107.209566	1665.369513	5.327206	-0.021065	2.299282
107.395000	1673.440985	5.332211	-0.021105	2.304258
107.607596	1681.514087	5.337216	-0.021150	2.309226
108.168652	1689.590240	5.342221	-0.021260	2.314214
108.296155	1697.650560	5.347226	-0.021289	2.319145
108.722498	1705.682218	5.352230	-0.021373	2.324074
109.169304	1713.735636	5.357235	-0.021462	2.329007
109.234651	1721.861709	5.362240	-0.021479	2.333941
109.365508	1729.961027	5.367245	-0.021509	2.338855
109.640454	1738.012395	5.372250	-0.021566	2.343741
110.153589	1746.054188	5.377254	-0.021666	2.348631
110.373262	1754.175149	5.382259	-0.021713	2.353534
110.411043	1762.250315	5.387264	-0.021725	2.358384
110.795074	1770.291775	5.392269	-0.021802	2.363232
110.839859	1778.349196	5.397274	-0.021816	2.368053
111.216944	1786.425517	5.402278	-0.021891	2.372901
111.535949	1794.476819	5.407283	-0.021956	2.377721
111.710639	1802.532216	5.412288	-0.021994	2.382521
111.968886	1810.612822	5.417293	-0.022047	2.387333
112.093636	1818.694234	5.422298	-0.022076	2.392125
112.527905	1826.750081	5.427302	-0.022162	2.396917
112.654970	1834.810027	5.432307	-0.022191	2.401678
112.721986	1842.874664	5.437312	-0.022209	2.406427
113.225613	1850.930771	5.442317	-0.022308	2.411196
113.202634	1859.015213	5.447322	-0.022309	2.415931
113.445425	1867.076805	5.452326	-0.022359	2.420664
115.437547	1874.935355	5.457331	-0.022735	2.425404
115.847436	1883.051655	5.462336	-0.022817	2.430163
116.202008	1891.246281	5.467341	-0.022888	2.434954
116.662452	1899.233530	5.472346	-0.022979	2.439623
116.833494	1907.311707	5.477350	-0.023017	2.444313
116.927366	1915.408903	5.482355	-0.023039	2.449000
116.993766	1923.507408	5.487360	-0.023057	2.453677
117.099577	1931.580700	5.492365	-0.023082	2.458333
117.364423	1939.613497	5.497370	-0.023137	2.462968
117.663020	1947.685260	5.502374	-0.023198	2.467620
117.702830	1955.775636	5.507379	-0.023210	2.472255
117.914133	1963.810223	5.512384	-0.023255	2.476862
118.077972	1971.876495	5.517389	-0.023291	2.481474
118.203571	1979.910156	5.522394	-0.023319	2.486057
118.443879	1987.984830	5.527398	-0.023370	2.490663
118.589833	1996.063686	5.532403	-0.023402	2.495255
118.950353	2004.082327	5.537408	-0.023474	2.499821
119.476773	2012.093348	5.542413	-0.023578	2.504387
119.611743	2020.159242	5.547418	-0.023608	2.508946
119.857416	2028.291707	5.552422	-0.023659	2.513543
120.148323	2036.315255	5.557427	-0.023719	2.518073
120.411906	2044.341907	5.562432	-0.023773	2.522594
120.646555	2052.409441	5.567437	-0.023822	2.527129
120.645439	2060.489904	5.572442	-0.023827	2.531645
120.934016	2068.538857	5.577446	-0.023886	2.536157
121.064890	2076.599714	5.582451	-0.023916	2.540656
121.211514	2084.625735	5.587456	-0.023948	2.545129
121.713728	2092.670325	5.592461	-0.024047	2.549629
121.646378	2100.789317	5.597466	-0.024040	2.554122
122.083340	2108.797937	5.602470	-0.024127	2.558582
122.551455	2116.809226	5.607475	-0.024219	2.563038
122.712246	2124.866766	5.612480	-0.024254	2.567490
122.926549	2132.965160	5.617485	-0.024300	2.571960
123.182883	2141.023276	5.622490	-0.024353	2.576403
123.460840	2149.067673	5.627494	-0.024410	2.580832
123.585897	2157.121282	5.632499	-0.024438	2.585249
123.838670	2165.153011	5.637504	-0.024491	2.589654
124.453527	2173.394742	5.642509	-0.024611	2.594192
124.845746	2181.353708	5.647514	-0.024689	2.598552
125.009458	2189.381235	5.652518	-0.024725	2.602926
125.100881	2197.433681	5.657523	-0.024747	2.607302
125.367650	2205.433500	5.662528	-0.024802	2.611654
125.758655	2213.492357	5.667533	-0.024880	2.616039
126.022069	2221.507588	5.672538	-0.024934	2.620384
126.181935	2229.559829	5.677542	-0.024969	2.624735
126.247508	2237.640091	5.682547	-0.024987	2.629087
126.555215	2245.680071	5.687552	-0.025050	2.633427
126.963602	2253.716442	5.692557	-0.025131	2.637764
126.961059	2261.770441	5.697562	-0.025136	2.642077
127.371105	2269.796879	5.702566	-0.025217	2.646395
127.689039	2277.856751	5.707571	-0.025282	2.650717
127.729658	2285.929323	5.712576	-0.025295	2.655021
127.811339	2293.991801	5.717581	-0.025315	2.659315
128.150938	2301.999422	5.722586	-0.025384	2.663590
128.531486	2310.059322	5.727590	-0.025460	2.667889
128.737718	2318.131817	5.732595	-0.025504	2.672175
128.875551	2326.195561	5.737600	-0.025535	2.676446
129.186203	2334.228823	5.742605	-0.025598	2.680705
129.579809	2342.218160	5.747610	-0.025676	2.684940
129.726516	2350.287603	5.752614	-0.025709	2.689194
130.125284	2358.351406	5.757619	-0.025789	2.693454
130.410260	2366.392467	5.762624	-0.025847	2.697688
130.770700	2374.430098	5.767629	-0.025919	2.701919
131.029199	2382.449746	5.772634	-0.025973	2.706127
131.477235	2390.501822	5.777638	-0.026061	2.710358
131.812403	2398.562864	5.782643	-0.026129	2.714579
131.945259	2406.596567	5.787648	-0.026159	2.718767
132.305512	2414.631257	5.792653	-0.026232	2.722963
132.359259	2422.677103	5.797658	-0.026247	2.727139
132.732751	2430.750402	5.802662	-0.026322	2.731343
133.026932	2438.807706	5.807667	-0.026382	2.735527
133.134302	2446.851244	5.812672	-0.026407	2.739686
133.192625	2454.932879	5.817677	-0.026423	2.743855
133.219443	2462.977757	5.822682	-0.026434	2.747998
133.633609	2471.054783	5.827686	-0.026516	2.752174
133.892888	2479.117497	5.832691	-0.026570	2.756327
134.033440	2487.133913	5.837696	-0.026601	2.760442
134.345183	2495.128859	5.842701	-0.026664	2.764551
134.556431	2503.160499	5.847706	-0.026709	2.768667
134.759472	2511.224165	5.852710	-0.026752	2.772792
135.048760	2519.272103	5.857715	-0.026811	2.776908
135.197608	2527.298758	5.862720	-0.026844	2.780998
135.336938	2535.342737	5.867725	-0.026876	2.785091
135.453537	2543.387721	5.872730	-0.026903	2.789177
136.064334	2551.427376	5.877734	-0.027022	2.793284
136.593802	2559.432391	5.882739	-0.027125	2.797362
136.874202	2567.452183	5.887744	-0.027183	2.801427
137.125647	2575.515020	5.892749	-0.027235	2.805506
137.390873	2583.551531	5.897754	-0.027290	2.809566
137.548049	2591.638976	5.902758	-0.027324	2.813640
137.778926	2599.679978	5.907763	-0.027373	2.817689
137.955783	2607.709572	5.912768	-0.027411	2.821723
138.323994	2615.750099	5.917773	-0.027485	2.825768
138.391830	2623.808529	5.922778	-0.027503	2.829799
138.600808	2631.901221	5.927782	-0.027547	2.833849
139.107480	2639.892105	5.932787	-0.027646	2.837859
139.323149	2647.918225	5.937792	-0.027692	2.841865
139.512964	2655.965645	5.942797	-0.027733	2.845875
139.881243	2663.975353	5.947802	-0.027806	2.849870
140.411096	2672.038782	5.952806	-0.027910	2.853894
140.449533	2680.094832	5.957811	-0.027923	2.857882
140.572768	2688.133643	5.962816	-0.027951	2.861861
140.988439	2696.173628	5.967821	-0.028034	2.865851
141.215657	2704.189772	5.972826	-0.028081	2.869813
141.485269	2712.290479	5.977830	-0.028137	2.873814
141.850362	2720.308650	5.982835	-0.028210	2.877773
142.153493	2728.316336	5.987840	-0.028272	2.881719
142.269150	2736.383485	5.992845	-0.028299	2.885678
142.588315	2744.375926	5.997850	-0.028363	2.889606
142.678600	2752.472621	6.002854	-0.028386	2.893567
142.855126	2760.506880	6.007859	-0.028424	2.897497
143.046718	2768.537020	6.012864	-0.028465	2.901421
143.372871	2776.569049	6.017869	-0.028531	2.905347
143.520052	2784.596510	6.022874	-0.028563	2.909256
143.587453	2792.753073	6.027878	-0.028581	2.913218
144.089507	2800.746026	6.032883	-0.028680	2.917119
144.271595	2808.748268	6.037888	-0.028719	2.921002
144.734139	2816.738302	6.042893	-0.028811	2.924888
145.157404	2824.760341	6.047898	-0.028895	2.928783
145.450344	2832.820476	6.052902	-0.028955	2.932684
145.534264	2840.901948	6.057907	-0.028976	2.936579
145.629627	2848.921480	6.062912	-0.028999	2.940439
145.934807	2856.927535	6.067917	-0.029061	2.944300
146.197171	2864.961936	6.072922	-0.029115	2.948166
146.285399	2873.059134	6.077926	-0.029137	2.952048
146.680616	2881.104510	6.082931	-0.029216	2.955916
146.764626	2889.103916	6.087936	-0.029236	2.959741
147.067815	2897.128786	6.092941	-0.029298	2.963585
147.254762	2905.149836	6.097946	-0.029338	2.967415
147.482904	2913.227502	6.102950	-0.029386	2.971270
147.540481	2921.286696	6.107955	-0.029402	2.975102
147.802546	2929.271941	6.112960	-0.029456	2.978905
148.261609	2937.317066	6.117965	-0.029547	2.982741
148.328333	2945.371642	6.122970	-0.029565	2.986557
148.553213	2953.400598	6.127974	-0.029612	2.990363
148.776756	2961.475124	6.132979	-0.029659	2.994187
149.189982	2969.461179	6.137984	-0.029741	2.997973
149.476854	2977.484829	6.142989	-0.029800	3.001765
149.665505	2985.486628	6.147994	-0.029840	3.005538
150.088197	2993.489255	6.152998	-0.029924	3.009318
150.323714	3001.604408	6.158003	-0.029973	3.013136
150.479538	3009.647658	6.163008	-0.030008	3.016912
150.989584	3017.670017	6.168013	-0.030108	3.020691
151.129207	3025.682560	6.173018	-0.030139	3.024443
151.413301	3033.728889	6.178022	-0.030197	3.028212
151.794511	3041.794058	6.183027	-0.030274	3.031990
152.165843	3049.833615	6.188032	-0.030348	3.035751
152.470684	3057.846568	6.193037	-0.030410	3.039492
152.887797	3065.845161	6.198042	-0.030493	3.043227
153.240447	3073.892788	6.203046	-0.030564	3.046977
153.307205	3081.978638	6.208051	-0.030582	3.050726
153.615648	3089.995602	6.213056	-0.030644	3.054450
153.942759	3098.038175	6.218061	-0.030711	3.058183
154.149702	3106.061104	6.223066	-0.030754	3.061896
154.128822	3114.129389	6.228070	-0.030756	3.065614
154.640625	3122.147651	6.233075	-0.030856	3.069330
154.726241	3130.272316	6.238080	-0.030878	3.073071
155.000667	3138.299994	6.243085	-0.030934	3.076771
155.141834	3146.279516	6.248090	-0.030966	3.080438
155.384609	3154.270603	6.253094	-0.031016	3.084112
155.737934	3162.297707	6.258099	-0.031087	3.087802
155.629825	3170.355207	6.263104	-0.031072	3.091480
156.079978	3178.374912	6.268109	-0.031161	3.095162
156.234241	3186.396479	6.273114	-0.031195	3.098828
156.342730	3194.464456	6.278118	-0.031221	3.102508
156.658208	3202.492506	6.283123	-0.031285	3.106174
156.860456	3210.498218	6.288128	-0.031328	3.109822
157.160200	3218.567720	6.293133	-0.031389	3.113498
157.365520	3226.579144	6.298138	-0.031433	3.117139
157.622261	3234.599766	6.303142	-0.031486	3.120782
157.699594	3242.613158	6.308147	-0.031505	3.124410
157.813815	3250.664066	6.313152	-0.031532	3.128052
158.171825	3258.718339	6.318157	-0.031604	3.131702
158.450324	3266.746370	6.323162	-0.031661	3.135333
158.604740	3274.776635	6.328166	-0.031695	3.138955
159.048398	3282.792022	6.333171	-0.031783	3.142579
159.356017	3290.819792	6.338176	-0.031846	3.146198
159.425487	3298.864246	6.343181	-0.031864	3.149809
159.440738	3306.961611	6.348186	-0.031872	3.153438
159.916478	3314.927839	6.353190	-0.031966	3.157025
160.195388	3322.980502	6.358195	-0.032023	3.160637
160.420468	3330.952610	6.363200	-0.032070	3.164207
160.712939	3339.004351	6.368205	-0.032130	3.167811
160.959896	3347.028447	6.373210	-0.032181	3.171396
161.102687	3355.109004	6.378214	-0.032213	3.174998
161.390966	3363.119458	6.383219	-0.032272	3.178571
161.878877	3371.122714	6.388224	-0.032368	3.182146
162.219805	3379.158466	6.393229	-0.032437	3.185724
162.220569	3387.207062	6.398234	-0.032442	3.189290
162.422051	3395.263158	6.403238	-0.032485	3.192863
162.684750	3403.325382	6.408243	-0.032539	3.196438
162.851341	3411.308978	6.413248	-0.032576	3.199970
163.126331	3419.347862	6.418253	-0.032632	3.203527
163.421220	3427.371249	6.423258	-0.032692	3.207074
163.551619	3435.425603	6.428262	-0.032722	3.210624
163.717204	3443.472123	6.433267	-0.032758	3.214167
164.213369	3451.459508	6.438272	-0.032856	3.217695
164.577855	3459.508873	6.443277	-0.032929	3.221240
164.454222	3467.533180	6.448282	-0.032911	3.224751
164.812622	3475.562496	6.453286	-0.032983	3.228279
165.296691	3483.622638	6.458291	-0.033079	3.231822
165.325500	3491.689917	6.463296	-0.033089	3.235346
165.905824	3499.671073	6.468301	-0.033203	3.238851
166.101365	3507.673191	6.473306	-0.033244	3.242345
166.240142	3515.706523	6.478310	-0.033276	3.245847
166.491843	3523.737458	6.483315	-0.033328	3.249349
166.497440	3531.786201	6.488320	-0.033334	3.252845
166.800869	3539.832063	6.493325	-0.033396	3.256347
166.828576	3547.839965	6.498330	-0.033406	3.259818
166.983738	3555.855575	6.503334	-0.033440	3.263295
167.319714	3563.865459	6.508339	-0.033508	3.266771
167.325707	3571.924260	6.513344	-0.033515	3.270253
167.754751	3579.968368	6.518349	-0.033600	3.273741
167.975631	3587.995241	6.523354	-0.033646	3.277209
168.520277	3595.982538	6.528358	-0.033753	3.280670
168.639199	3604.007585	6.533363	-0.033780	3.284126
168.887158	3612.022241	6.538368	-0.033832	3.287579
169.240588	3620.097818	6.543373	-0.033903	3.291059
169.246685	3628.134635	6.548378	-0.033909	3.294505
169.499866	3636.143147	6.553382	-0.033962	3.297945
169.645488	3644.189479	6.558387	-0.033994	3.301393
169.743370	3652.196673	6.563392	-0.034018	3.304819
169.902380	3660.265314	6.568397	-0.034053	3.308270
170.169490	3668.287455	6.573402	-0.034108	3.311702
170.543451	3676.320311	6.578406	-0.034183	3.315139
170.643969	3684.349182	6.583411	-0.034207	3.318560
170.873226	3692.347849	6.588416	-0.034255	3.321969
171.258797	3700.360941	6.593421	-0.034332	3.325387
171.366967	3708.392857	6.598426	-0.034357	3.328799
171.416301	3716.441916	6.603430	-0.034372	3.332213
171.696325	3724.498260	6.608435	-0.034429	3.335635
171.722239	3732.490676	6.613440	-0.034439	3.339017
172.091372	3740.510849	6.618445	-0.034513	3.342419
172.410580	3748.551117	6.623450	-0.034578	3.345825
172.772373	3756.564935	6.628454	-0.034650	3.349218
173.101628	3764.627689	6.633459	-0.034717	3.352626
173.086051	3772.681814	6.638464	-0.034720	3.356015
173.519442	3780.643751	6.643469	-0.034805	3.359378
173.507532	3788.690813	6.648474	-0.034809	3.362757
173.804568	3796.691941	6.653478	-0.034869	3.366125
174.281131	3804.714939	6.658483	-0.034963	3.369505
174.103454	3812.790866	6.663488	-0.034935	3.372880
174.591088	3820.816667	6.668493	-0.035031	3.376255
174.831015	3828.832163	6.673498	-0.035081	3.379613
175.178822	3836.852594	6.678502	-0.035151	3.382973
175.394427	3844.889354	6.683507	-0.035197	3.386333
175.600887	3852.915483	6.688512	-0.035241	3.389684
175.815533	3861.050285	6.693517	-0.035286	3.393077
176.078629	3869.063065	6.698522	-0.035340	3.396418
176.022875	3877.012821	6.703526	-0.035335	3.399718
176.223240	3885.032425	6.708531	-0.035378	3.403053
176.471452	3893.019843	6.713536	-0.035429	3.406373
176.788506	3901.065260	6.718541	-0.035493	3.409716
177.107013	3909.103510	6.723546	-0.035558	3.413053
177.585954	3917.116853	6.728550	-0.035653	3.416382
177.800020	3925.151803	6.733555	-0.035698	3.419707
177.868290	3933.153695	6.738560	-0.035716	3.423010
178.172210	3941.209161	6.743565	-0.035778	3.426340
178.347120	3949.226298	6.748570	-0.035815	3.429647
178.466829	3957.284634	6.753574	-0.035843	3.432966
179.014977	3965.296857	6.758579	-0.035950	3.436277
179.239404	3973.279522	6.763584	-0.035997	3.439562
179.619869	3981.310563	6.768589	-0.036074	3.442868
179.645052	3989.366106	6.773594	-0.036084	3.446170
180.148427	3997.333503	6.778598	-0.036183	3.449448
180.176584	4005.448632	6.783603	-0.036193	3.452767
180.264536	4013.485742	6.788608	-0.036215	3.456054
180.595720	4021.502610	6.793613	-0.036282	3.459337
180.929530	4029.502534	6.798618	-0.036349	3.462610
181.128463	4037.530929	6.803622	-0.036391	3.465887
181.391624	4045.551162	6.808627	-0.036446	3.469160
181.751435	4053.603679	6.813632	-0.036518	3.472446
181.794920	4061.684465	6.818637	-0.036531	3.475730
181.904350	4069.640718	6.823642	-0.036557	3.478962
182.010293	4077.654004	6.828646	-0.036582	3.482215
182.376124	4085.678288	6.833651	-0.036656	3.485477
182.439077	4093.698542	6.838656	-0.036673	3.488725
183.000867	4101.742862	6.843661	-0.036782	3.491995
183.122100	4109.773732	6.848666	-0.036810	3.495243
183.134656	4117.776487	6.853670	-0.036818	3.498473
183.529610	4125.807282	6.858675	-0.036897	3.501723
183.755231	4133.796825	6.863680	-0.036944	3.504949
183.860867	4141.875297	6.868685	-0.036969	3.508203
183.846379	4149.940296	6.873690	-0.036972	3.511445
184.092068	4157.929746	6.878694	-0.037023	3.514662
184.267285	4165.956172	6.883699	-0.037061	3.517889
184.410488	4173.952776	6.888704	-0.037092	3.521100
184.944971	4181.943246	6.893709	-0.037197	3.524317
185.100985	4189.995852	6.898714	-0.037232	3.527544
185.278994	4198.037055	6.903718	-0.037270	3.530765
185.588284	4206.099980	6.908723	-0.037333	3.533995
185.533401	4214.122828	6.913728	-0.037328	3.537196
185.934583	4222.125591	6.918733	-0.037408	3.540399
186.005127	4230.159086	6.923738	-0.037426	3.543601
186.034907	4238.195883	6.928742	-0.037437	3.546801
186.382389	4246.234258	6.933747	-0.037507	3.550008
186.549084	4254.326575	6.938752	-0.037544	3.553228
186.743372	4262.387281	6.943757	-0.037585	3.556433
186.909624	4270.288105	6.948762	-0.037621	3.559572
187.024075	4278.318059	6.953766	-0.037648	3.562757
187.489700	4286.322230	6.958771	-0.037740	3.565939
187.692627	4294.332583	6.963776	-0.037783	3.569113
188.007104	4302.380703	6.968781	-0.037847	3.572303
187.861953	4310.441352	6.973786	-0.037825	3.575481
188.103029	4318.438933	6.978790	-0.037875	3.578642
188.461589	4326.459712	6.983795	-0.037947	3.581814
188.458202	4334.459337	6.988800	-0.037952	3.584964
188.661760	4342.498641	6.993805	-0.037995	3.588132
188.723646	4350.550622	6.998810	-0.038012	3.591299
189.099820	4358.531418	7.003814	-0.038087	3.594443
189.217313	4366.564245	7.008819	-0.038114	3.597599
189.392624	4374.549047	7.013824	-0.038152	3.600734
189.640708	4382.591513	7.018829	-0.038204	3.603891
189.845860	4390.605900	7.023834	-0.038247	3.607033
189.977415	4398.640596	7.028838	-0.038277	3.610178
190.185799	4406.712098	7.033843	-0.038321	3.613337
190.301425	4414.724501	7.038848	-0.038348	3.616467
190.842833	4422.705069	7.043853	-0.038454	3.619594
190.730407	4430.761217	7.048858	-0.038438	3.622730
190.790057	4438.763290	7.053862	-0.038455	3.625846
191.026697	4446.800859	7.058867	-0.038504	3.628979
191.081540	4454.858969	7.063872	-0.038520	3.632112
191.545595	4462.907676	7.068877	-0.038611	3.635250
191.727466	4470.874431	7.073882	-0.038650	3.638345
191.937698	4478.896863	7.078886	-0.038695	3.641460
192.346912	4486.880284	7.083891	-0.038776	3.644563
192.520888	4494.913513	7.088896	-0.038814	3.647676
192.600592	4502.986815	7.093901	-0.038834	3.650799
192.903787	4511.013788	7.098906	-0.038896	3.653908
193.200499	4519.051418	7.103910	-0.038956	3.657017
193.244779	4527.084843	7.108915	-0.038970	3.660116
193.573924	4535.062827	7.113920	-0.039037	3.663199
193.832699	4543.101122	7.118925	-0.039090	3.666300
193.926313	4551.103883	7.123930	-0.039113	3.669380
194.105078	4559.171901	7.128934	-0.039151	3.672485
194.503157	4567.185772	7.133939	-0.039231	3.675573
194.477843	4575.162400	7.138944	-0.039231	3.678632
194.624183	4583.220597	7.143949	-0.039264	3.681725
194.847726	4591.220167	7.148954	-0.039311	3.684795
195.036652	4599.241049	7.153958	-0.039351	3.687869
195.187072	4607.290046	7.158963	-0.039385	3.690950
195.257603	4615.323308	7.163968	-0.039403	3.694021
195.934658	4623.332476	7.168973	-0.039534	3.697095
195.898765	4631.333865	7.173978	-0.039533	3.700146
195.966470	4639.340005	7.178982	-0.039551	3.703199
196.121240	4647.403723	7.183987	-0.039585	3.706273
196.178471	4655.408296	7.188992	-0.039601	3.709320
196.498487	4663.494508	7.193997	-0.039666	3.712402
196.686733	4671.559905	7.199002	-0.039706	3.715469
196.789793	4679.498449	7.204006	-0.039731	3.718485
197.081680	4687.545052	7.209011	-0.039790	3.721543
197.200965	4695.484962	7.214016	-0.039818	3.724554
197.398173	4703.538596	7.219021	-0.039860	3.727608
197.578287	4711.535609	7.224026	-0.039898	3.730637
197.700778	4719.611446	7.229030	-0.039927	3.733692
198.059970	4727.664960	7.234035	-0.039999	3.736742
198.040837	4735.619898	7.239040	-0.040000	3.739743
198.122607	4743.649451	7.244045	-0.040021	3.742773
198.309971	4751.689728	7.249050	-0.040061	3.745806
198.454428	4759.706096	7.254054	-0.040093	3.748827
198.777975	4767.737801	7.259059	-0.040159	3.751855
199.031302	4775.768029	7.264064	-0.040211	3.754879
199.269775	4783.768336	7.269069	-0.040261	3.757888
199.267618	4791.805798	7.274074	-0.040266	3.760904
199.454455	4799.828122	7.279078	-0.040306	3.763916
199.795364	4807.858376	7.284083	-0.040375	3.766932
199.858034	4815.862120	7.289088	-0.040392	3.769929
199.980719	4823.916222	7.294093	-0.040420	3.772944
200.079726	4831.942323	7.299098	-0.040444	3.775945
200.192128	4839.951467	7.304102	-0.040470	3.778938
200.459119	4847.977803	7.309107	-0.040525	3.781939
200.420698	4855.975343	7.314112	-0.040523	3.784919
200.847973	4863.993248	7.319117	-0.040608	3.787916
201.084394	4872.055926	7.324122	-0.040657	3.790922
201.112458	4880.119018	7.329126	-0.040668	3.793921
201.370828	4888.100911	7.334131	-0.040721	3.796893
201.543419	4896.065641	7.339136	-0.040758	3.799854
201.706166	4904.084386	7.344141	-0.040794	3.802833
201.716329	4912.123498	7.349146	-0.040801	3.805813
201.901073	4920.111506	7.354150	-0.040841	3.808776
202.036885	4928.165206	7.359155	-0.040871	3.811760
202.171031	4936.178091	7.364160	-0.040902	3.814727
202.338341	4944.225783	7.369165	-0.040938	3.817705
202.683186	4952.212934	7.374170	-0.041008	3.820662
202.648533	4960.223163	7.379174	-0.041006	3.823617
202.929499	4968.264702	7.384179	-0.041064	3.826588
203.113792	4976.273209	7.389184	-0.041104	3.829542
203.290509	4984.342716	7.394189	-0.041142	3.832516
203.408603	4992.376049	7.399194	-0.041169	3.835474
203.884823	5000.298540	7.404198	-0.041263	3.838396
204.164822	5008.365885	7.409203	-0.041320	3.841364
204.193992	5016.303890	7.414208	-0.041331	3.844278
204.475687	5024.399044	7.419213	-0.041389	3.847252
204.836392	5032.462097	7.424218	-0.041461	3.850214
204.755860	5040.485221	7.429222	-0.041452	3.853150
204.929638	5048.563538	7.434227	-0.041489	3.856109
205.012328	5056.468631	7.439232	-0.041510	3.859001
205.117633	5064.552010	7.444237	-0.041535	3.861956
205.334331	5072.572219	7.449242	-0.041580	3.864888
205.506079	5080.583089	7.454246	-0.041618	3.867813
205.725957	5088.626625	7.459251	-0.041664	3.870749
205.836533	5096.858096	7.464256	-0.041690	3.873749
206.076470	5104.844420	7.469261	-0.041740	3.876660
206.284481	5112.738083	7.474266	-0.041784	3.879534
206.258798	5120.749063	7.479270	-0.041784	3.882445
206.560800	5128.723611	7.484275	-0.041846	3.885346
206.616462	5136.719942	7.489280	-0.041861	3.888248
206.823270	5144.747866	7.494285	-0.041905	3.891162
206.880007	5152.792415	7.499290	-0.041921	3.894078
207.135417	5160.792885	7.504294	-0.041974	3.896979
207.572275	5168.812373	7.509299	-0.042061	3.899888
207.552304	5176.819557	7.514304	-0.042062	3.902782
207.767334	5184.855911	7.519309	-0.042107	3.905688
207.953853	5192.860887	7.524314	-0.042147	3.908581
207.969926	5200.917919	7.529318	-0.042156	3.911487
208.257432	5208.954862	7.534323	-0.042215	3.914388
208.527623	5216.916392	7.539328	-0.042270	3.917260
208.774417	5224.911988	7.544333	-0.042321	3.920142
208.932998	5232.942385	7.549338	-0.042356	3.923032
209.153047	5240.940897	7.554342	-0.042402	3.925910
209.505985	5248.984776	7.559347	-0.042473	3.928804
209.549618	5257.023307	7.564352	-0.042487	3.931689
209.927349	5265.057138	7.569357	-0.042562	3.934576
210.023283	5273.085809	7.574362	-0.042586	3.937454
210.118287	5281.050653	7.579366	-0.042609	3.940307
210.248266	5289.105148	7.584371	-0.042638	3.943190
210.529011	5297.101377	7.589376	-0.042696	3.946053
210.711275	5305.105753	7.594381	-0.042735	3.948916
210.800652	5313.203690	7.599386	-0.042757	3.951808
211.030820	5321.211429	7.604390	-0.042805	3.954668
211.415351	5329.241242	7.609395	-0.042882	3.957536
211.383196	5337.226153	7.614400	-0.042881	3.960379
211.523501	5345.234824	7.619405	-0.042912	3.963232
211.810661	5353.269516	7.624410	-0.042971	3.966094
212.013922	5361.240325	7.629414	-0.043014	3.968930
212.237464	5369.352283	7.634419	-0.043061	3.971815
212.152119	5377.324682	7.639424	-0.043051	3.974642
212.503874	5385.392214	7.644429	-0.043121	3.977509
212.512843	5393.379577	7.649434	-0.043128	3.980339
212.710664	5401.354985	7.654438	-0.043170	3.983167
213.102314	5409.439221	7.659443	-0.043249	3.986034
213.027471	5417.427423	7.664448	-0.043240	3.988857
213.286861	5425.499521	7.669453	-0.043294	3.991713
213.272410	5433.523767	7.674458	-0.043296	3.994546
213.487840	5441.543186	7.679462	-0.043342	3.997379
213.411003	5449.562230	7.684467	-0.043333	4.000205
213.684390	5457.512514	7.689472	-0.043389	4.003010
213.779403	5465.557284	7.694477	-0.043412	4.005844
213.918273	5473.564102	7.699482	-0.043443	4.008663
214.134705	5481.589137	7.704486	-0.043489	4.011488
214.371848	5489.662561	7.709491	-0.043538	4.014328
214.558136	5497.639988	7.714496	-0.043578	4.017132
214.842816	5505.672134	7.719501	-0.043636	4.019954
215.063558	5513.670997	7.724506	-0.043683	4.022762
214.977513	5521.656014	7.729510	-0.043672	4.025558
215.293407	5529.707515	7.734515	-0.043736	4.028381
215.406392	5537.752197	7.739520	-0.043762	4.031197
215.679833	5545.896569	7.744525	-0.043819	4.034049
215.866363	5553.886966	7.749530	-0.043859	4.036843
215.948152	5561.780122	7.754534	-0.043879	4.039600
216.319953	5569.839114	7.759539	-0.043954	4.042417
216.380237	5577.783640	7.764544	-0.043970	4.045187
216.565522	5585.837729	7.769549	-0.044010	4.047996
216.698926	5593.871871	7.774554	-0.044040	4.050794
216.779920	5601.872532	7.779558	-0.044060	4.053579
216.995412	5609.934216	7.784563	-0.044106	4.056385
217.080180	5617.882047	7.789568	-0.044127	4.059147
217.385091	5625.919797	7.794573	-0.044189	4.061942
217.508487	5633.939174	7.799578	-0.044217	4.064726
217.443291	5641.933089	7.804582	-0.044210	4.067496
217.944964	5649.997690	7.809587	-0.044309	4.070297
217.786988	5658.039773	7.814592	-0.044285	4.073079
217.953283	5666.048038	7.819597	-0.044321	4.075852
218.110515	5674.026065	7.824602	-0.044356	4.078613
218.330523	5682.054970	7.829606	-0.044402	4.081390
218.505903	5690.019756	7.834611	-0.044440	4.084142
218.616144	5698.055029	7.839616	-0.044466	4.086916
219.009978	5706.076499	7.844621	-0.044544	4.089687
219.157161	5714.155843	7.849626	-0.044577	4.092473
219.059996	5722.189514	7.854630	-0.044564	4.095238
219.273060	5730.211104	7.859635	-0.044609	4.098001
219.334744	5738.182284	7.864640	-0.044626	4.100742
219.607925	5746.191611	7.869645	-0.044682	4.103498
219.654711	5754.235099	7.874650	-0.044696	4.106261
219.917382	5762.223041	7.879654	-0.044750	4.109005
220.225364	5770.296691	7.884659	-0.044813	4.111778
220.195916	5778.346696	7.889664	-0.044813	4.114536
220.572412	5786.336753	7.894669	-0.044888	4.117278
220.686289	5794.313783	7.899674	-0.044914	4.120009
220.635175	5802.356147	7.904678	-0.044910	4.122759
221.062908	5810.370696	7.909683	-0.044995	4.125503
221.251489	5818.381241	7.914688	-0.045036	4.128242
221.486175	5826.408319	7.919693	-0.045084	4.130984
221.671535	5834.433469	7.924698	-0.045124	4.133724
221.803717	5842.502593	7.929702	-0.045154	4.136476
222.122436	5850.495283	7.934707	-0.045219	4.139202
222.012022	5858.496759	7.939712	-0.045204	4.141925
222.527109	5866.478522	7.944717	-0.045305	4.144646
222.628582	5874.578638	7.949722	-0.045329	4.147401
222.690044	5882.545862	7.954726	-0.045346	4.150108
222.936070	5890.603872	7.959731	-0.045397	4.152847
222.961655	5898.641818	7.964736	-0.045407	4.155574
223.171468	5906.596730	7.969741	-0.045451	4.158274
223.391972	5914.641336	7.974746	-0.045497	4.161002
223.512329	5922.608037	7.979750	-0.045525	4.163701
223.680623	5930.711240	7.984755	-0.045562	4.166445
223.839650	5938.685338	7.989760	-0.045597	4.169144
223.884451	5946.704545	7.994765	-0.045610	4.171854
224.052150	5954.768361	7.999770	-0.045647	4.174579
224.070193	5962.730514	8.004774	-0.045655	4.177267
224.306162	5970.735076	8.009779	-0.045705	4.179969
224.580548	5978.774241	8.014784	-0.045761	4.182682
224.656235	5986.764020	8.019789	-0.045780	4.185374
224.811633	5994.801863	8.024794	-0.045815	4.188081
224.833952	6002.837189	8.029798	-0.045824	4.190785
225.203475	6010.970668	8.034803	-0.045898	4.193523
225.219169	6018.945173	8.039808	-0.045906	4.196202
225.352701	6026.882931	8.044813	-0.045937	4.198869
225.641043	6034.916807	8.049818	-0.045995	4.201568
225.564575	6042.860244	8.054822	-0.045986	4.204230
225.845554	6050.924362	8.059827	-0.046044	4.206935
226.004328	6058.918288	8.064832	-0.046079	4.209614
226.132236	6066.950984	8.069837	-0.046108	4.212304
226.258949	6074.965565	8.074842	-0.046137	4.214986
226.374640	6082.970694	8.079846	-0.046164	4.217662
226.759303	6090.985043	8.084851	-0.046241	4.220343
226.622497	6098.996816	8.089856	-0.046220	4.223016
226.938067	6107.028298	8.094861	-0.046284	4.225699
227.170500	6115.077771	8.099866	-0.046333	4.228385
227.456584	6123.053096	8.104870	-0.046392	4.231045
227.567892	6131.127745	8.109875	-0.046418	4.233734
227.930696	6139.144953	8.114880	-0.046490	4.236405
228.100771	6147.098705	8.119885	-0.046527	4.239052
228.020008	6155.168954	8.124890	-0.046518	4.241733
228.314817	6163.084156	8.129894	-0.046578	4.244365
228.341311	6171.214227	8.134899	-0.046588	4.247063
228.297005	6179.182928	8.139904	-0.046585	4.249706
228.617366	6187.252943	8.144909	-0.046650	4.252384
228.986435	6195.224090	8.149914	-0.046724	4.255028
229.077572	6203.275855	8.154918	-0.046746	4.257695
229.166957	6211.274238	8.159923	-0.046768	4.260342
229.269175	6219.296184	8.164928	-0.046793	4.262995
229.585607	6227.306115	8.169933	-0.046857	4.265645
229.617796	6235.388276	8.174938	-0.046868	4.268314
229.630471	6243.371941	8.179942	-0.046876	4.270949
230.042761	6251.479830	8.184947	-0.046958	4.273627
229.905468	6259.466057	8.189952	-0.046937	4.276258
229.939385	6267.413881	8.194957	-0.046949	4.278876
230.495255	6275.465200	8.199962	-0.047058	4.281532
230.389907	6283.418908	8.204966	-0.047043	4.284148
230.570231	6291.490882	8.209971	-0.047082	4.286803
230.794128	6299.449005	8.214976	-0.047129	4.289420
231.049152	6307.518777	8.219981	-0.047182	4.292072
231.195881	6315.563006	8.224986	-0.047215	4.294713
231.278365	6323.587159	8.229990	-0.047235	4.297346
231.665169	6331.566043	8.234995	-0.047313	4.299964
231.564448	6339.574991	8.240000	-0.047299	4.302587
231.584497	6347.607861	8.245005	-0.047308	4.305217
231.743873	6355.624236	8.250010	-0.047343	4.307841
231.890634	6363.637270	8.255014	-0.047376	4.310462
232.037872	6371.693465	8.260019	-0.047408	4.313096
232.237145	6379.680777	8.265024	-0.047451	4.315706
232.547141	6387.673358	8.270029	-0.047514	4.318317
232.620114	6395.704992	8.275034	-0.047533	4.320937
232.618716	6403.667523	8.280038	-0.047538	4.323533
232.883137	6411.746843	8.285043	-0.047592	4.326167
232.819770	6419.697426	8.290048	-0.047586	4.328755
232.971825	6427.792007	8.295053	-0.047619	4.331390
233.220267	6435.818434	8.300058	-0.047671	4.334002
233.393113	6443.818761	8.305062	-0.047708	4.336603
233.467201	6451.816453	8.310067	-0.047727	4.339201
233.644051	6459.825470	8.315072	-0.047766	4.341802
233.950525	6467.791417	8.320077	-0.047828	4.344389
234.015669	6475.874152	8.325082	-0.047845	4.347009
234.163642	6483.892634	8.330086	-0.047878	4.349609
234.620821	6491.982040	8.335091	-0.047969	4.352231
234.742016	6500.038876	8.340096	-0.047996	4.354839
234.837586	6507.984271	8.345101	-0.048020	4.357409
235.077786	6515.970201	8.350106	-0.048069	4.359992
235.050034	6523.932360	8.355110	-0.048070	4.362564
235.228742	6531.987122	8.360115	-0.048108	4.365166
235.382822	6539.974648	8.365120	-0.048142	4.367744
235.618059	6548.001260	8.370125	-0.048191	4.370334
235.750833	6556.043375	8.375130	-0.048221	4.372926
235.846470	6564.044469	8.380134	-0.048244	4.375504
236.137845	6572.087487	8.385139	-0.048304	4.378094
236.165085	6580.079025	8.390144	-0.048314	4.380665
236.107460	6588.058345	8.395149	-0.048309	4.383230
236.330849	6596.131610	8.400154	-0.048356	4.385826
236.561920	6604.090975	8.405158	-0.048404	4.388383
236.775936	6612.170201	8.410163	-0.048449	4.390977
236.712264	6620.170463	8.415168	-0.048442	4.393543
237.072501	6628.232488	8.420173	-0.048515	4.396129
237.027756	6636.206777	8.425178	-0.048512	4.398683
237.031172	6644.193670	8.430182	-0.048518	4.401241
237.602564	6652.181764	8.435187	-0.048629	4.403800
237.522929	6660.229227	8.440192	-0.048620	4.406373
237.511480	6668.249012	8.445197	-0.048623	4.408936
237.854663	6676.325544	8.450202	-0.048692	4.411518
238.075436	6684.353104	8.455206	-0.048739	4.414081
238.223150	6692.408086	8.460211	-0.048771	4.416652
238.306607	6700.311124	8.465216	-0.048792	4.419172
238.429151	6708.364140	8.470221	-0.048820	4.421739
238.773025	6716.370563	8.475226	-0.048890	4.424291
238.827251	6724.369314	8.480230	-0.048905	4.426837
239.152856	6732.408047	8.485235	-0.048971	4.429396
239.086623	6740.488580	8.490240	-0.048964	4.431965
239.076629	6748.512058	8.495245	-0.048967	4.434514
239.614282	6756.551253	8.500250	-0.049073	4.437070
239.614867	6764.441272	8.505254	-0.049078	4.439574
239.680662	6772.532762	8.510259	-0.049096	4.442141
239.741700	6780.471417	8.515264	-0.049112	4.444658
240.106361	6788.541722	8.520269	-0.049185	4.447216
240.205851	6796.542333	8.525274	-0.049209	4.449750
240.383739	6804.569253	8.530278	-0.049248	4.452291
240.531911	6812.613056	8.535283	-0.049280	4.454836
240.544924	6820.627623	8.540288	-0.049288	4.457369
240.805719	6828.605211	8.545293	-0.049342	4.459890
240.839632	6836.636612	8.550298	-0.049354	4.462426
241.130412	6844.625061	8.555302	-0.049413	4.464948
241.142103	6852.687708	8.560307	-0.049420	4.467491
241.104595	6860.675267	8.565312	-0.049419	4.470009
241.404738	6868.735928	8.570317	-0.049480	4.472549
241.737425	6876.772180	8.575322	-0.049547	4.475081
241.675672	6884.703226	8.580327	-0.049541	4.477576
241.966899	6892.751138	8.585331	-0.049600	4.480108
242.114596	6900.728707	8.590336	-0.049633	4.482616
242.207358	6908.750139	8.595341	-0.049656	4.485136
242.241078	6916.806555	8.600346	-0.049667	4.487665
242.504872	6924.765765	8.605351	-0.049722	4.490164
242.587738	6932.852741	8.610355	-0.049742	4.492700
242.584540	6940.850479	8.615360	-0.049747	4.495207
242.784512	6948.847830	8.620365	-0.049790	4.497712
243.192865	6956.882766	8.625370	-0.049871	4.500229
242.931931	6964.857394	8.630375	-0.049828	4.502723
243.227464	6972.902464	8.635379	-0.049888	4.505240
243.341921	6980.930698	8.640384	-0.049915	4.507750
243.642644	6988.937935	8.645389	-0.049976	4.510252
243.852150	6997.040504	8.650394	-0.050020	4.512782
243.845044	7005.017290	8.655399	-0.050024	4.515270
244.181948	7012.993855	8.660403	-0.050092	4.517759
244.094647	7020.956067	8.665408	-0.050081	4.520240
244.305511	7028.992651	8.670413	-0.050126	4.522744
244.630785	7037.013916	8.675418	-0.050192	4.525242
244.586208	7044.985072	8.680423	-0.050188	4.527722
244.756415	7053.043514	8.685427	-0.050225	4.530228
244.860621	7061.103906	8.690432	-0.050250	4.532734
244.950287	7069.111593	8.695437	-0.050272	4.535221
245.169443	7077.121928	8.700442	-0.050318	4.537709
245.445439	7085.083076	8.705447	-0.050375	4.540179
245.761793	7093.145120	8.710451	-0.050439	4.542680
245.677625	7101.072877	8.715456	-0.050429	4.545137
245.876128	7109.145546	8.720461	-0.050471	4.547638
246.209075	7117.182721	8.725466	-0.050538	4.550127
246.072139	7125.216647	8.730471	-0.050518	4.552613
246.097441	7133.275359	8.735475	-0.050528	4.555105
246.105216	7141.244622	8.740480	-0.050535	4.557568
246.519628	7149.217460	8.745485	-0.050617	4.560032
246.682982	7157.310108	8.750490	-0.050653	4.562531
246.778423	7165.254721	8.755495	-0.050676	4.564982
246.814933	7173.300061	8.760499	-0.050688	4.567464
246.856470	7181.301151	8.765504	-0.050701	4.569930
247.076400	7189.337415	8.770509	-0.050747	4.572406
247.217377	7197.393590	8.775514	-0.050779	4.574887
247.334621	7205.351781	8.780519	-0.050806	4.577336
247.675414	7213.399971	8.785523	-0.050875	4.579812
247.899738	7221.408259	8.790528	-0.050922	4.582274
247.942919	7229.388854	8.795533	-0.050935	4.584726
248.038684	7237.495666	8.800538	-0.050958	4.587215
248.136503	7245.442087	8.805543	-0.050982	4.589654
248.382376	7253.528935	8.810547	-0.051033	4.592135
248.290375	7261.546439	8.815552	-0.051021	4.594593
248.423669	7269.537319	8.820557	-0.051051	4.597042
248.664785	7277.516075	8.825562	-0.051101	4.599485
248.757680	7285.514628	8.830567	-0.051124	4.601933
248.973702	7293.507176	8.835571	-0.051169	4.604379
249.129744	7301.570490	8.840576	-0.051203	4.606844
249.237921	7309.521716	8.845581	-0.051229	4.609274
249.587949	7317.611072	8.850586	-0.051299	4.611745
249.604869	7325.609783	8.855591	-0.051308	4.614186
249.769438	7333.684417	8.860595	-0.051344	4.616650
250.135537	7341.628329	8.865600	-0.051417	4.619072
250.013628	7349.665434	8.870605	-0.051400	4.621522
250.295183	7357.654781	8.875610	-0.051457	4.623955
250.182158	7365.691164	8.880615	-0.051442	4.626402
250.269454	7373.695046	8.885619	-0.051463	4.628838
250.456387	7381.712559	8.890624	-0.051503	4.631276
250.812733	7389.763402	8.895629	-0.051575	4.633723
250.938867	7397.786386	8.900634	-0.051604	4.636160
250.949783	7405.741438	8.905639	-0.051611	4.638576
250.998209	7413.795394	8.910643	-0.051625	4.641020
251.073504	7421.807356	8.915648	-0.051645	4.643450
251.191450	7429.796876	8.920653	-0.051672	4.645872
251.602799	7437.843970	8.925658	-0.051754	4.648310
251.727368	7445.857507	8.930663	-0.051782	4.650737
251.839658	7453.906200	8.935667	-0.051808	4.653173
252.083836	7461.900755	8.940672	-0.051859	4.655591
252.264243	7469.859069	8.945677	-0.051898	4.657997
252.392115	7477.931950	8.950682	-0.051927	4.660437
252.478174	7485.877654	8.955687	-0.051948	4.662837
252.776955	7493.938003	8.960691	-0.052009	4.665270
252.885587	7501.931499	8.965696	-0.052035	4.667682
252.954794	7509.961103	8.970701	-0.052053	4.670103
253.170880	7518.070188	8.975706	-0.052099	4.672547
253.342157	7526.054855	8.980711	-0.052136	4.674952
253.539867	7534.077029	8.985715	-0.052178	4.677367
253.590058	7542.000972	8.990720	-0.052192	4.679752
253.951765	7550.077058	8.995725	-0.052265	4.682181
254.218544	7557.991790	9.000730	-0.052320	4.684559
254.021908	7566.076330	9.005735	-0.052289	4.686989
254.333558	7574.082781	9.010739	-0.052352	4.689393
254.376778	7582.127178	9.015744	-0.052365	4.691808
254.426085	7590.116451	9.020749	-0.052380	4.694204
254.576065	7598.175066	9.025754	-0.052413	4.696620
254.702014	7606.063724	9.030759	-0.052442	4.698984
254.965083	7614.162740	9.035763	-0.052496	4.701410
254.972851	7622.141138	9.040768	-0.052503	4.703799
255.341635	7630.156525	9.045773	-0.052577	4.706196
255.555899	7638.202129	9.050778	-0.052622	4.708602
255.545229	7646.231391	9.055783	-0.052625	4.711002
255.792428	7654.321152	9.060787	-0.052676	4.713419
255.752893	7662.266428	9.065792	-0.052674	4.715791
256.079714	7670.272113	9.070797	-0.052740	4.718180
256.176221	7678.264322	9.075802	-0.052764	4.720564
256.381112	7686.278319	9.080807	-0.052807	4.722953
256.336450	7694.348723	9.085811	-0.052804	4.725358
256.451959	7702.346059	9.090816	-0.052831	4.727740
256.509219	7710.338547	9.095821	-0.052847	4.730119
256.755684	7718.420846	9.100826	-0.052898	4.732523
256.979981	7726.369591	9.105831	-0.052945	4.734887
257.240197	7734.475086	9.110835	-0.052999	4.737295
257.425199	7742.430597	9.115840	-0.053039	4.739658
257.328314	7750.398825	9.120845	-0.053026	4.742025
257.440248	7758.459468	9.125850	-0.053052	4.744417
257.528626	7766.446081	9.130855	-0.053074	4.746786
257.750772	7774.485574	9.135859	-0.053120	4.749169
257.685169	7782.505993	9.140864	-0.053113	4.751546
257.904300	7790.568408	9.145869	-0.053159	4.753934
258.283361	7798.611486	9.150874	-0.053235	4.756313
258.101676	7806.481249	9.155879	-0.053207	4.758643
258.264148	7814.631292	9.160883	-0.053242	4.761053
258.591762	7822.582583	9.165888	-0.053309	4.763402
258.693572	7830.548910	9.170893	-0.053333	4.765755
258.809617	7838.617741	9.175898	-0.053360	4.768138
258.780305	7846.598897	9.180903	-0.053359	4.770494
259.062761	7854.645151	9.185907	-0.053417	4.772866
259.212598	7862.610135	9.190912	-0.053450	4.775214
259.207375	7870.685132	9.195917	-0.053455	4.777594
259.591674	7878.668673	9.200922	-0.053532	4.779944
259.368319	7886.700006	9.205927	-0.053495	4.782310
259.658126	7894.652118	9.210931	-0.053555	4.784649
260.100352	7902.732465	9.215936	-0.053642	4.787024
260.285922	7910.660403	9.220941	-0.053682	4.789354
260.251479	7918.775097	9.225946	-0.053681	4.791738
260.179068	7926.757176	9.230951	-0.053673	4.794083
260.414104	7934.826403	9.235955	-0.053722	4.796451
260.183525	7942.803348	9.240960	-0.053684	4.798792
260.438021	7950.746736	9.245965	-0.053737	4.801121
260.729828	7958.793735	9.250970	-0.053796	4.803478
260.661891	7966.799778	9.255975	-0.053789	4.805824
260.843950	7974.855239	9.260979	-0.053828	4.808182
261.020469	7982.846361	9.265984	-0.053866	4.810520
261.055925	7990.332136	9.270989	-0.053878	4.812710
261.257049	7994.953731	9.275994	-0.053918	4.814060

261.412012	7997.449598	9.280999	-0.053949	4.814789
261.579123	7998.869490	9.286003	-0.053981	4.815204
261.689043	7999.294220	9.291008	-0.054002	4.815327
261.754965	8000.245871	9.296013	-0.054015	4.815605
261.864733	8000.242331	9.301018	-0.054035	4.815604
261.843618	8000.192859	9.306023	-0.054031	4.815589
261.959184	8000.269521	9.311027	-0.054053	4.815611
261.974872	8000.303961	9.316032	-0.054056	4.815621
261.923095	8000.189902	9.321037	-0.054046	4.815588
262.084317	8000.253425	9.326042	-0.054076	4.815606
261.976812	8000.215356	9.331047	-0.054056	4.815595
261.905710	8000.233424	9.336051	-0.054043	4.815601
261.908165	8000.238809	9.341056	-0.054044	4.815602
262.018255	8000.240615	9.346061	-0.054064	4.815602
262.259999	8000.277686	9.351066	-0.054109	4.815612
262.263123	8000.233950	9.356071	-0.054110	4.815599
262.364011	8000.245219	9.361075	-0.054129	4.815602
262.369848	8000.227161	9.366080	-0.054130	4.815597
262.233449	8000.248433	9.371085	-0.054105	4.815604
262.249567	8000.294630	9.376090	-0.054108	4.815617
262.107902	8000.248525	9.381095	-0.054081	4.815604
262.405976	8000.246998	9.386099	-0.054137	4.815602
262.106778	8000.283764	9.391104	-0.054081	4.815615
262.096370	8000.236602	9.396109	-0.054079	4.815601
262.237649	8000.227169	9.401114	-0.054106	4.815597
262.300540	8000.248497	9.406119	-0.054118	4.815603
262.212503	8000.232108	9.411123	-0.054101	4.815599
262.464722	8000.233036	9.416128	-0.054148	4.815598
262.586429	8000.231828	9.421133	-0.054171	4.815597
262.540487	8000.351777	9.426138	-0.054163	4.815632
262.469459	8000.258763	9.431143	-0.054149	4.815606
262.577360	8000.257329	9.436147	-0.054169	4.815605
262.598893	8000.230983	9.441152	-0.054174	4.815597
262.651028	8000.219024	9.446157	-0.054183	4.815593
262.790193	8000.252282	9.451162	-0.054209	4.815602
262.736257	8000.231110	9.456167	-0.054199	4.815596
262.871971	8000.217314	9.461171	-0.054225	4.815592
262.562770	8000.275278	9.466176	-0.054167	4.815610
262.754429	8000.250648	9.471181	-0.054203	4.815602
262.803166	8000.258927	9.476186	-0.054212	4.815604
262.557443	8000.242094	9.481191	-0.054166	4.815600
262.746348	8000.270825	9.486195	-0.054202	4.815608
262.685350	8000.253810	9.491200	-0.054190	4.815603
262.779950	8000.257499	9.496205	-0.054208	4.815604
263.039041	8000.278834	9.501210	-0.054256	4.815609
262.908640	8000.255343	9.506215	-0.054232	4.815602
262.788785	8000.287566	9.511219	-0.054210	4.815612
262.859861	8000.253486	9.516224	-0.054223	4.815602
262.959925	8000.252993	9.521229	-0.054242	4.815601
262.809068	8000.272959	9.526234	-0.054214	4.815608
262.760143	8000.227303	9.531239	-0.054205	4.815595
262.871348	8000.247286	9.536243	-0.054225	4.815600
262.808270	8000.270825	9.541248	-0.054214	4.815607
262.701349	8000.223151	9.546253	-0.054194	4.815594
262.992373	8000.237532	9.551258	-0.054248	4.815597
263.071475	8000.207856	9.556263	-0.054263	4.815588
262.915604	8000.223468	9.561267	-0.054234	4.815593
262.927568	8000.214056	9.566272	-0.054236	4.815590
263.041269	8000.194559	9.571277	-0.054257	4.815584
262.969726	8000.271366	9.576282	-0.054244	4.815607
262.950212	8000.250757	9.581287	-0.054241	4.815601
262.910082	8000.222334	9.586291	-0.054233	4.815593
263.021759	8000.257279	9.591296	-0.054254	4.815602
262.984974	8000.208616	9.596301	-0.054247	4.815588
263.133847	8000.275145	9.601306	-0.054275	4.815607
263.107725	8000.234134	9.606311	-0.054270	4.815595
263.146252	8000.217679	9.611315	-0.054277	4.815590
263.209989	8000.266793	9.616320	-0.054289	4.815604
263.228132	8000.236119	9.621325	-0.054293	4.815595
263.105751	8000.293936	9.626330	-0.054270	4.815613
263.110429	8000.292949	9.631335	-0.054271	4.815612
263.113493	8000.266302	9.636339	-0.054272	4.815605
263.164393	8000.262867	9.641344	-0.054281	4.815603
263.136602	8000.219692	9.646349	-0.054276	4.815591
263.095263	8000.282040	9.651354	-0.054268	4.815609
263.078044	8000.264673	9.656359	-0.054265	4.815604
263.084671	8000.267991	9.661363	-0.054267	4.815605
263.037498	8000.223431	9.666368	-0.054258	4.815592
263.250388	8000.233329	9.671373	-0.054297	4.815594
263.371376	8000.265222	9.676378	-0.054320	4.815603
263.106297	8000.254479	9.681383	-0.054271	4.815601
263.327974	8000.268794	9.686387	-0.054312	4.815604
263.267575	8000.245379	9.691392	-0.054301	4.815598
263.243500	8000.240718	9.696397	-0.054296	4.815596
263.345630	8000.278711	9.701402	-0.054316	4.815607
263.209694	8000.287172	9.706407	-0.054290	4.815610
263.210023	8000.241253	9.711411	-0.054290	4.815597
263.115591	8000.233304	9.716416	-0.054273	4.815595
263.429484	8000.210675	9.721421	-0.054331	4.815587
263.597151	8000.229446	9.726426	-0.054363	4.815592
263.365126	8000.243811	9.731431	-0.054319	4.815597
263.395506	8000.257131	9.736435	-0.054325	4.815601
263.358505	8000.270416	9.741440	-0.054318	4.815605
263.215473	8000.225355	9.746445	-0.054292	4.815592
263.221779	8000.253234	9.751450	-0.054293	4.815600
263.331498	8000.203765	9.756455	-0.054313	4.815585
263.351329	8000.259637	9.761459	-0.054317	4.815601
263.378461	8000.250473	9.766464	-0.054322	4.815599
263.257177	8000.234607	9.771469	-0.054300	4.815595
263.385530	8000.273030	9.776474	-0.054324	4.815605
263.402247	8000.267968	9.781479	-0.054327	4.815604
263.500166	8000.281325	9.786483	-0.054345	4.815607
263.494205	8000.333571	9.791488	-0.054344	4.815622
263.120869	8000.249491	9.796493	-0.054275	4.815600
263.291758	8000.305700	9.801498	-0.054307	4.815615
263.192330	8000.310486	9.806503	-0.054288	4.815617
263.476382	8000.295914	9.811507	-0.054341	4.815611
263.488982	8000.291853	9.816512	-0.054344	4.815610
263.386223	8000.275222	9.821517	-0.054324	4.815606
263.357421	8000.273687	9.826522	-0.054319	4.815606
263.263022	8000.203787	9.831527	-0.054302	4.815586
263.059872	8000.246396	9.836531	-0.054264	4.815599
263.165546	8000.267357	9.841536	-0.054284	4.815605
263.254200	8000.248519	9.846541	-0.054300	4.815599
263.187270	8000.286949	9.851546	-0.054288	4.815610
263.230921	8000.206491	9.856551	-0.054296	4.815587
263.292308	8000.268384	9.861555	-0.054307	4.815604
263.278501	8000.248936	9.866560	-0.054305	4.815599
263.242188	8000.215235	9.871565	-0.054298	4.815589
263.512491	8000.274139	9.876570	-0.054349	4.815605
263.588850	8000.242282	9.881575	-0.054363	4.815595
263.622229	8000.244970	9.886579	-0.054369	4.815596
263.679779	8000.250189	9.891584	-0.054380	4.815597
263.496805	8000.194861	9.896589	-0.054346	4.815582
263.555755	8000.286622	9.901594	-0.054357	4.815608
263.598833	8000.227517	9.906599	-0.054365	4.815591
263.630112	8000.238715	9.911603	-0.054371	4.815594
263.446603	8000.246397	9.916608	-0.054337	4.815597
263.240475	8000.219529	9.921613	-0.054298	4.815590
263.529766	8000.279812	9.926618	-0.054352	4.815606
263.473244	8000.271415	9.931623	-0.054342	4.815604
263.442066	8000.297613	9.936627	-0.054336	4.815612
263.548129	8000.312172	9.941632	-0.054356	4.815616
263.511472	8000.287010	9.946637	-0.054349	4.815609
263.601618	8000.313058	9.951642	-0.054366	4.815616
263.402092	8000.293774	9.956647	-0.054329	4.815611
263.629439	8000.252639	9.961651	-0.054371	4.815598
263.656653	8000.272316	9.966656	-0.054376	4.815604
263.696722	8000.219570	9.971661	-0.054384	4.815588
263.791525	8000.262785	9.976666	-0.054402	4.815600
263.593226	8000.289451	9.981671	-0.054365	4.815609
263.656932	8000.317202	9.986675	-0.054377	4.815617
263.771326	8000.316944	9.991680	-0.054398	4.815616
263.629563	8000.253744	9.996685	-0.054372	4.815598
263.624212	8000.348726	10.001690	-0.054371	4.815626
263.620828	8000.225840	10.006695	-0.054370	4.815590
263.740753	8000.291896	10.011699	-0.054393	4.815609
263.510378	8000.298811	10.016704	-0.054350	4.815612
263.596965	8000.263917	10.021709	-0.054366	4.815601
263.643883	8000.297802	10.026714	-0.054375	4.815611
263.581661	8000.218815	10.031719	-0.054363	4.815588
263.552976	8000.243985	10.036723	-0.054358	4.815596
263.676830	8000.295152	10.041728	-0.054381	4.815610
263.803989	8000.270535	10.046733	-0.054405	4.815602
263.824262	8000.290099	10.051738	-0.054409	4.815608
263.619136	8000.216248	10.056743	-0.054370	4.815587
263.928288	8000.268313	10.061747	-0.054428	4.815601
263.864937	8000.310006	10.066752	-0.054416	4.815614
263.743233	8000.249271	10.071757	-0.054394	4.815596
263.851565	8000.326887	10.076762	-0.054414	4.815619
264.005208	8000.227934	10.081767	-0.054443	4.815589
263.998850	8000.303674	10.086771	-0.054442	4.815611
263.977117	8000.355662	10.091776	-0.054438	4.815626
263.899986	8000.240112	10.096781	-0.054423	4.815593
263.913937	8000.299094	10.101786	-0.054426	4.815610
263.596544	8000.302447	10.106791	-0.054367	4.815613
263.757725	8000.288001	10.111795	-0.054397	4.815608
263.713119	8000.265913	10.116800	-0.054389	4.815601
263.599948	8000.252315	10.121805	-0.054368	4.815598
263.818238	8000.298620	10.126810	-0.054408	4.815611
263.750302	8000.257991	10.131815	-0.054396	4.815599
263.641933	8000.249813	10.136819	-0.054376	4.815597
263.635043	8000.290295	10.141824	-0.054374	4.815609
263.827125	8000.234697	10.146829	-0.054410	4.815592
263.986473	8000.384715	10.151834	-0.054440	4.815635
263.727131	8000.276863	10.156839	-0.054392	4.815605
263.856820	8000.285400	10.161843	-0.054416	4.815606
263.955499	8000.321202	10.166848	-0.054434	4.815616
263.784134	8000.250040	10.171853	-0.054402	4.815596
263.761665	8000.295607	10.176858	-0.054398	4.815610
263.751706	8000.269813	10.181863	-0.054397	4.815602
263.741747	8000.258974	10.186867	-0.054395	4.815599
263.835221	8000.314985	10.191872	-0.054412	4.815615
263.910951	8000.223301	10.196877	-0.054426	4.815588
263.906883	8000.206149	10.201882	-0.054426	4.815583
263.776688	8000.191205	10.206887	-0.054401	4.815579
264.122830	8000.199013	10.211891	-0.054466	4.815580
264.121636	8000.326108	10.216896	-0.054466	4.815617
263.925328	8000.240652	10.221901	-0.054429	4.815593
263.978877	8000.243670	10.226906	-0.054439	4.815594
263.919998	8000.205326	10.231911	-0.054428	4.815583
264.050996	8000.213884	10.236915	-0.054453	4.815585
264.089880	8000.223071	10.241920	-0.054460	4.815587
264.049162	8000.205319	10.246925	-0.054453	4.815582
264.134062	8000.263326	10.251930	-0.054469	4.815599
263.952009	8000.259282	10.256935	-0.054435	4.815598
263.872029	8000.253705	10.261939	-0.054420	4.815597
263.997021	8000.279255	10.266944	-0.054443	4.815604
263.973766	8000.257516	10.271949	-0.054439	4.815598
264.138416	8000.299739	10.276954	-0.054470	4.815609
263.979648	8000.244805	10.281959	-0.054440	4.815594
264.058481	8000.262123	10.286963	-0.054455	4.815599
263.969247	8000.310870	10.291968	-0.054438	4.815613
263.683308	8000.227151	10.296973	-0.054385	4.815590
263.963805	8000.225339	10.301978	-0.054437	4.815588
263.942102	8000.223920	10.306983	-0.054433	4.815588
263.924082	8000.233244	10.311987	-0.054430	4.815591
263.986719	8000.230002	10.316992	-0.054442	4.815590
263.859012	8000.222575	10.321997	-0.054418	4.815588
264.102411	8000.243655	10.327002	-0.054464	4.815593
264.100266	8000.193422	10.332007	-0.054463	4.815578
264.072358	8000.258127	10.337011	-0.054458	4.815597
264.218585	8000.257322	10.342016	-0.054485	4.815596
264.116001	8000.220399	10.347021	-0.054466	4.815586
264.185640	8000.304859	10.352026	-0.054479	4.815611
263.989440	8000.233290	10.357031	-0.054443	4.815591
263.977068	8000.283295	10.362035	-0.054441	4.815605
264.215230	8000.213498	10.367040	-0.054485	4.815584
264.050463	8000.195851	10.372045	-0.054454	4.815579
264.191862	8000.241965	10.377050	-0.054481	4.815592
264.191779	8000.238764	10.382055	-0.054481	4.815591
264.175185	8000.237430	10.387059	-0.054478	4.815591
264.103562	8000.269374	10.392064	-0.054464	4.815601
263.993883	8000.268652	10.397069	-0.054444	4.815601
264.399526	8000.267822	10.402074	-0.054520	4.815599
263.962199	8000.217940	10.407079	-0.054438	4.815586
263.927963	8000.249429	10.412083	-0.054432	4.815596
264.224182	8000.239330	10.417088	-0.054487	4.815591
263.999731	8000.230319	10.422093	-0.054445	4.815590
264.054751	8000.277155	10.427098	-0.054456	4.815603
264.167450	8000.244825	10.432103	-0.054477	4.815593
264.215146	8000.243474	10.437107	-0.054486	4.815592
264.033710	8000.272553	10.442112	-0.054452	4.815602
263.989108	8000.256873	10.447117	-0.054444	4.815597
264.279548	8000.265907	10.452122	-0.054498	4.815599
264.195220	8000.260258	10.457127	-0.054482	4.815597
264.093655	8000.269282	10.462131	-0.054463	4.815601
264.386531	8000.308264	10.467136	-0.054518	4.815611
264.246643	8000.240820	10.472141	-0.054492	4.815592
264.109020	8000.289843	10.477146	-0.054466	4.815606
264.042869	8000.218267	10.482151	-0.054454	4.815586
264.054889	8000.230219	10.487155	-0.054456	4.815589
264.040099	8000.274843	10.492160	-0.054454	4.815602
263.924099	8000.231291	10.497165	-0.054432	4.815590
263.939562	8000.247572	10.502170	-0.054435	4.815595
263.927242	8000.252716	10.507175	-0.054433	4.815596
264.072866	8000.266855	10.512179	-0.054460	4.815600
263.960833	8000.235117	10.517184	-0.054439	4.815591
263.909734	8000.249240	10.522189	-0.054430	4.815596
263.943363	8000.255136	10.527194	-0.054436	4.815597
263.927902	8000.244206	10.532199	-0.054433	4.815594
263.952677	8000.257435	10.537203	-0.054438	4.815598
263.885010	8000.296921	10.542208	-0.054425	4.815610
263.968757	8000.227800	10.547213	-0.054441	4.815589
264.153916	8000.271426	10.552218	-0.054476	4.815601
264.296673	8000.258815	10.557223	-0.054502	4.815596
264.179057	8000.272916	10.562227	-0.054480	4.815601
264.164929	8000.307938	10.567232	-0.054478	4.815611
264.070186	8000.254053	10.572237	-0.054460	4.815596
264.003084	8000.326661	10.577242	-0.054448	4.815618
264.070525	8000.260477	10.582247	-0.054460	4.815598
264.310638	8000.277232	10.587251	-0.054505	4.815602
264.141297	8000.233874	10.592256	-0.054474	4.815590
264.086803	8000.184920	10.597261	-0.054464	4.815576
264.283197	8000.274661	10.602266	-0.054500	4.815601
264.210553	8000.261727	10.607271	-0.054487	4.815598
264.096870	8000.259870	10.612275	-0.054466	4.815598
264.078573	8000.295892	10.617280	-0.054462	4.815608
264.069052	8000.219903	10.622285	-0.054461	4.815586
264.113171	8000.305014	10.627290	-0.054469	4.815611
264.171327	8000.256837	10.632295	-0.054480	4.815596
264.288109	8000.292935	10.637299	-0.054502	4.815606
264.149209	8000.294938	10.642304	-0.054476	4.815608
263.908905	8000.264304	10.647309	-0.054431	4.815600
264.105153	8000.298499	10.652314	-0.054468	4.815609
264.027261	8000.257707	10.657319	-0.054453	4.815597
263.981222	8000.263367	10.662323	-0.054445	4.815599
264.214359	8000.274666	10.667328	-0.054488	4.815601
264.395449	8000.230638	10.672333	-0.054522	4.815588
264.216951	8000.281128	10.677338	-0.054489	4.815603
264.151302	8000.245877	10.682343	-0.054477	4.815593
264.110543	8000.262305	10.687347	-0.054469	4.815598
264.300847	8000.198133	10.692352	-0.054505	4.815579
264.145762	8000.221234	10.697357	-0.054476	4.815586
264.363663	8000.258988	10.702362	-0.054516	4.815596
264.441018	8000.227147	10.707367	-0.054531	4.815587
264.321991	8000.262588	10.712371	-0.054509	4.815597
264.175363	8000.264464	10.717376	-0.054482	4.815599
264.196499	8000.224226	10.722381	-0.054485	4.815587
264.315639	8000.260362	10.727386	-0.054508	4.815597
264.189238	8000.254025	10.732391	-0.054484	4.815596
264.210038	8000.272529	10.737395	-0.054488	4.815601
264.257458	8000.260493	10.742400	-0.054497	4.815597
264.109333	8000.263413	10.747405	-0.054470	4.815599
264.202032	8000.293776	10.752410	-0.054487	4.815607
264.254523	8000.202779	10.757415	-0.054497	4.815580
264.341114	8000.204202	10.762419	-0.054513	4.815580
264.267389	8000.245726	10.767424	-0.054499	4.815593
264.433588	8000.234567	10.772429	-0.054530	4.815589
264.500817	8000.266649	10.777434	-0.054543	4.815598
264.233739	8000.235577	10.782439	-0.054493	4.815590
264.323115	8000.242386	10.787443	-0.054510	4.815592
264.449350	8000.264753	10.792448	-0.054533	4.815597
264.257514	8000.226367	10.797453	-0.054498	4.815587
264.377016	8000.278532	10.802458	-0.054520	4.815602
264.481971	8000.242871	10.807463	-0.054540	4.815591
264.509070	8000.265751	10.812467	-0.054545	4.815597
264.449565	8000.241282	10.817472	-0.054534	4.815591
264.292994	8000.232314	10.822477	-0.054505	4.815589
264.376105	8000.292428	10.827482	-0.054520	4.815606
264.461738	8000.275677	10.832487	-0.054536	4.815601
264.352688	8000.267487	10.837491	-0.054516	4.815599
264.335914	8000.235173	10.842496	-0.054513	4.815589
263.993936	8000.233851	10.847501	-0.054449	4.815591
264.217354	8000.259945	10.852506	-0.054491	4.815597
264.416857	8000.232241	10.857511	-0.054528	4.815588
264.348809	8000.275994	10.862515	-0.054515	4.815601
264.317792	8000.316081	10.867520	-0.054510	4.815613
264.196051	8000.266025	10.872525	-0.054487	4.815599
264.449639	8000.272319	10.877530	-0.054534	4.815600
264.353156	8000.251517	10.882535	-0.054516	4.815594
264.195683	8000.260693	10.887539	-0.054487	4.815597
264.328654	8000.267148	10.892544	-0.054512	4.815599
264.130197	8000.211564	10.897549	-0.054475	4.815583
264.354367	8000.247284	10.902554	-0.054517	4.815593
264.427100	8000.263435	10.907559	-0.054531	4.815597
264.379983	8000.255191	10.912563	-0.054522	4.815595
264.363655	8000.267746	10.917568	-0.054519	4.815599
264.304865	8000.233676	10.922573	-0.054508	4.815589
264.390566	8000.279947	10.927578	-0.054524	4.815602
264.405737	8000.274859	10.932583	-0.054527	4.815601
264.388720	8000.274586	10.937587	-0.054524	4.815601
264.503125	8000.330940	10.942592	-0.054545	4.815616
264.273928	8000.278057	10.947597	-0.054502	4.815602
264.261178	8000.323783	10.952602	-0.054500	4.815616
264.226792	8000.315748	10.957607	-0.054494	4.815613
264.388423	8000.300241	10.962611	-0.054524	4.815608
264.222679	8000.322100	10.967616	-0.054493	4.815615
264.259653	8000.232985	10.972621	-0.054500	4.815589
264.482419	8000.317818	10.977626	-0.054542	4.815613
264.432226	8000.335160	10.982631	-0.054532	4.815618
264.191398	8000.259654	10.987635	-0.054488	4.815597
264.209866	8000.278120	10.992640	-0.054491	4.815602
264.291518	8000.283735	10.997645	-0.054506	4.815604
264.322946	8000.282118	11.002650	-0.054512	4.815603
264.268651	8000.251326	11.007655	-0.054502	4.815594
264.393538	8000.261921	11.012659	-0.054525	4.815597
264.498958	8000.273266	11.017664	-0.054545	4.815600
264.398725	8000.253471	11.022669	-0.054527	4.815594
264.499462	8000.322420	11.027674	-0.054545	4.815614
264.418604	8000.351009	11.032679	-0.054530	4.815623
264.418334	8000.244194	11.037683	-0.054530	4.815592
264.304766	8000.306428	11.042688	-0.054509	4.815610
264.260707	8000.248031	11.047693	-0.054501	4.815593
264.350588	8000.245235	11.052698	-0.054518	4.815592
264.264096	8000.213916	11.057703	-0.054502	4.815583
264.446052	8000.237195	11.062707	-0.054536	4.815589
264.529238	8000.298379	11.067712	-0.054551	4.815607
264.397886	8000.232144	11.072717	-0.054527	4.815588
264.619893	8000.309488	11.077722	-0.054568	4.815610
264.420464	8000.322249	11.082727	-0.054531	4.815614
264.347644	8000.284744	11.087731	-0.054518	4.815604
264.449283	8000.335549	11.092736	-0.054537	4.815618
264.535699	8000.275016	11.097741	-0.054553	4.815600
264.413127	8000.349921	11.102746	-0.054530	4.815622
264.425308	8000.248650	11.107751	-0.054532	4.815593
264.494954	8000.241250	11.112755	-0.054545	4.815590
264.575183	8000.293841	11.117760	-0.054560	4.815605
264.594602	8000.257846	11.122765	-0.054564	4.815595
264.683170	8000.293483	11.127770	-0.054581	4.815605
264.647302	8000.334559	11.132775	-0.054574	4.815617
264.556122	8000.295685	11.137779	-0.054557	4.815606
264.563838	8000.339611	11.142784	-0.054559	4.815619
264.469563	8000.301754	11.147789	-0.054541	4.815608
264.449619	8000.284342	11.152794	-0.054538	4.815603
264.452389	8000.342073	11.157799	-0.054538	4.815620
264.162427	8000.352283	11.162803	-0.054484	4.815624
264.306191	8000.351438	11.167808	-0.054511	4.815623
264.154877	8000.292353	11.172813	-0.054483	4.815607
264.401573	8000.329511	11.177818	-0.054529	4.815616
264.416463	8000.254989	11.182823	-0.054532	4.815595
264.438154	8000.273507	11.187827	-0.054536	4.815600
264.478100	8000.338256	11.192832	-0.054543	4.815619
264.459968	8000.274943	11.197837	-0.054540	4.815600
264.682232	8000.301020	11.202842	-0.054581	4.815607
264.468331	8000.309271	11.207847	-0.054542	4.815610
264.676412	8000.285980	11.212851	-0.054580	4.815602
264.587092	8000.314430	11.217856	-0.054564	4.815611
264.507588	8000.292838	11.222861	-0.054549	4.815605
264.486728	8000.387568	11.227866	-0.054545	4.815633
264.376248	8000.353718	11.232871	-0.054525	4.815624
264.510693	8000.298245	11.237875	-0.054550	4.815607
264.675647	8000.336201	11.242880	-0.054581	4.815617
264.523132	8000.261073	11.247885	-0.054552	4.815596
264.494252	8000.334308	11.252890	-0.054547	4.815617
264.458126	8000.366834	11.257895	-0.054540	4.815627
264.563957	8000.327982	11.262899	-0.054560	4.815615
264.405331	8000.307230	11.267904	-0.054531	4.815610
264.422804	8000.310726	11.272909	-0.054534	4.815611
264.498134	8000.333328	11.277914	-0.054548	4.815617
264.518822	8000.331536	11.282919	-0.054552	4.815616
264.580216	8000.264184	11.287923	-0.054563	4.815596
264.697981	8000.281072	11.292928	-0.054585	4.815601
264.443411	8000.254476	11.297933	-0.054538	4.815594
264.418988	8000.296807	11.302938	-0.054534	4.815607
264.547446	8000.380097	11.307943	-0.054558	4.815631
264.723641	8000.282580	11.312947	-0.054590	4.815601
264.548545	8000.259422	11.317952	-0.054558	4.815595
264.396562	8000.234507	11.322957	-0.054530	4.815589
264.458143	8000.323109	11.327962	-0.054541	4.815614
264.579659	8000.309082	11.332967	-0.054564	4.815610
264.441724	8000.274783	11.337971	-0.054538	4.815600
264.501198	8000.321693	11.342976	-0.054549	4.815614
264.504570	8000.229892	11.347981	-0.054550	4.815587
264.552682	8000.252048	11.352986	-0.054559	4.815593
264.349038	8000.271149	11.357991	-0.054521	4.815600
264.488083	8000.278772	11.362995	-0.054547	4.815601
264.619745	8000.352500	11.368000	-0.054572	4.815622
264.367806	8000.322743	11.373005	-0.054525	4.815615
264.310696	8000.302585	11.378010	-0.054514	4.815609
264.531333	8000.292318	11.383015	-0.054555	4.815605
264.799476	8000.272147	11.388019	-0.054605	4.815598
264.590983	8000.337100	11.393024	-0.054567	4.815618
264.679707	8000.305445	11.398029	-0.054583	4.815608
264.744776	8000.303311	11.403034	-0.054595	4.815607
264.537712	8000.311674	11.408039	-0.054557	4.815611
264.791828	8000.264569	11.413043	-0.054604	4.815596
264.824544	8000.284337	11.418048	-0.054610	4.815601
264.490994	8000.240425	11.423053	-0.054548	4.815590
264.347970	8000.245565	11.428058	-0.054522	4.815592
264.478022	8000.262654	11.433063	-0.054546	4.815596
264.553899	8000.256425	11.438067	-0.054560	4.815594
264.425789	8000.282104	11.443072	-0.054536	4.815602
264.423584	8000.248960	11.448077	-0.054536	4.815593
264.394303	8000.286939	11.453082	-0.054531	4.815604
264.439463	8000.284479	11.458087	-0.054539	4.815603
264.568298	8000.327184	11.463091	-0.054563	4.815615
264.532409	8000.352237	11.468096	-0.054557	4.815622
264.617682	8000.295958	11.473101	-0.054572	4.815606
264.486301	8000.275652	11.478106	-0.054548	4.815600
264.448094	8000.259009	11.483111	-0.054541	4.815596
264.639462	8000.287784	11.488115	-0.054577	4.815603
264.552593	8000.312002	11.493120	-0.054561	4.815611
264.596120	8000.274266	11.498125	-0.054569	4.815599
264.798685	8000.270112	11.503130	-0.054606	4.815597
264.549497	8000.277785	11.508135	-0.054560	4.815601
264.447535	8000.250485	11.513139	-0.054541	4.815593
264.547195	8000.290576	11.518144	-0.054560	4.815604
264.542254	8000.290500	11.523149	-0.054559	4.815604
264.524436	8000.309440	11.528154	-0.054556	4.815610
264.434794	8000.280204	11.533159	-0.054539	4.815602
264.382857	8000.249450	11.538163	-0.054529	4.815593
264.387942	8000.266629	11.543168	-0.054530	4.815598
264.282863	8000.269186	11.548173	-0.054511	4.815599
264.499016	8000.282344	11.553178	-0.054551	4.815602
264.247058	8000.235497	11.558183	-0.054504	4.815590
264.302681	8000.252435	11.563187	-0.054515	4.815594
264.403333	8000.330996	11.568192	-0.054534	4.815617
264.305671	8000.265312	11.573197	-0.054515	4.815598
264.453843	8000.307265	11.578202	-0.054543	4.815610
264.399885	8000.382226	11.583207	-0.054533	4.815632
264.572885	8000.307088	11.588211	-0.054565	4.815609
264.443315	8000.330607	11.593216	-0.054541	4.815616
264.090193	8000.287443	11.598221	-0.054476	4.815606
264.551840	8000.281123	11.603226	-0.054562	4.815601
264.542884	8000.298072	11.608231	-0.054560	4.815606
264.404258	8000.229580	11.613235	-0.054534	4.815587
264.539340	8000.314046	11.618240	-0.054559	4.815611
264.370343	8000.247194	11.623245	-0.054528	4.815592
264.424159	8000.264102	11.628250	-0.054538	4.815597
264.560146	8000.269539	11.633255	-0.054564	4.815598
264.556995	8000.259879	11.638259	-0.054563	4.815595
264.630862	8000.311297	11.643264	-0.054577	4.815610
264.572585	8000.287916	11.648269	-0.054566	4.815603
264.615424	8000.267260	11.653274	-0.054574	4.815597
264.454174	8000.269964	11.658279	-0.054544	4.815599
264.578381	8000.258118	11.663283	-0.054567	4.815595
264.588384	8000.284990	11.668288	-0.054569	4.815602
264.598334	8000.229614	11.673293	-0.054571	4.815586
264.457182	8000.261488	11.678298	-0.054545	4.815596
264.459131	8000.291434	11.683303	-0.054545	4.815605
264.584827	8000.243294	11.688307	-0.054569	4.815590
264.734272	8000.251087	11.693312	-0.054597	4.815592
264.556044	8000.314399	11.698317	-0.054564	4.815611
264.638365	8000.323230	11.703322	-0.054579	4.815613
264.684355	8000.300488	11.708327	-0.054587	4.815606
264.585098	8000.241187	11.713331	-0.054569	4.815590
264.544747	8000.298211	11.718336	-0.054562	4.815606
264.590232	8000.232735	11.723341	-0.054570	4.815587
264.582818	8000.273209	11.728346	-0.054569	4.815599
264.638104	8000.289074	11.733351	-0.054579	4.815603
264.476032	8000.265061	11.738355	-0.054549	4.815597
264.562743	8000.284645	11.743360	-0.054565	4.815602
264.472401	8000.245785	11.748365	-0.054548	4.815592
264.495304	8000.254710	11.753370	-0.054553	4.815594
264.593965	8000.378102	11.758375	-0.054571	4.815630
264.585566	8000.295720	11.763379	-0.054570	4.815606
264.626811	8000.296401	11.768384	-0.054577	4.815606
264.729959	8000.245755	11.773389	-0.054597	4.815590
264.551090	8000.267398	11.778394	-0.054563	4.815597
264.489486	8000.266394	11.783399	-0.054552	4.815597
264.541681	8000.237346	11.788403	-0.054562	4.815589
264.552826	8000.297350	11.793408	-0.054564	4.815606
264.572353	8000.222904	11.798413	-0.054568	4.815584
264.757661	8000.253716	11.803418	-0.054602	4.815592
264.540942	8000.288625	11.808423	-0.054562	4.815604
264.631736	8000.264481	11.813427	-0.054579	4.815596
264.688905	8000.273968	11.818432	-0.054590	4.815599
264.635354	8000.247460	11.823437	-0.054580	4.815591
264.691531	8000.293248	11.828442	-0.054590	4.815604
264.563032	8000.295421	11.833447	-0.054566	4.815606
264.618007	8000.235441	11.838451	-0.054577	4.815588
264.655876	8000.242475	11.843456	-0.054584	4.815590
264.533084	8000.208424	11.848461	-0.054561	4.815580
264.545845	8000.263114	11.853466	-0.054563	4.815596
264.811159	8000.235420	11.858471	-0.054613	4.815587
264.817592	8000.226985	11.863475	-0.054614	4.815584
264.701270	8000.320151	11.868480	-0.054592	4.815612
264.732515	8000.273669	11.873485	-0.054598	4.815598
264.798516	8000.282232	11.878490	-0.054611	4.815601
264.715265	8000.245624	11.883495	-0.054595	4.815590
264.910978	8000.245630	11.888499	-0.054632	4.815589
264.772295	8000.350180	11.893504	-0.054606	4.815621
264.755765	8000.270870	11.898509	-0.054603	4.815597
264.862011	8000.307865	11.903514	-0.054623	4.815608
264.753320	8000.339203	11.908519	-0.054603	4.815617
264.533364	8000.273651	11.913523	-0.054562	4.815599
264.729054	8000.302497	11.918528	-0.054598	4.815607
264.497271	8000.225003	11.923533	-0.054555	4.815585
264.630893	8000.277400	11.928538	-0.054580	4.815600
264.683960	8000.253706	11.933543	-0.054590	4.815593
264.730534	8000.258747	11.938547	-0.054599	4.815594
264.909503	8000.296933	11.943552	-0.054632	4.815604
264.677664	8000.265368	11.948557	-0.054589	4.815596
264.790348	8000.312082	11.953562	-0.054610	4.815609
264.810912	8000.293196	11.958567	-0.054614	4.815604
264.714066	8000.293751	11.963571	-0.054596	4.815604
264.749974	8000.299685	11.968576	-0.054603	4.815606
264.865389	8000.262058	11.973581	-0.054624	4.815594
264.813317	8000.269756	11.978586	-0.054615	4.815597
264.660649	8000.275806	11.983591	-0.054586	4.815599
264.638336	8000.254082	11.988595	-0.054582	4.815593
264.869284	8000.321960	11.993600	-0.054625	4.815612
264.638620	8000.284005	11.998605	-0.054582	4.815602
264.666972	8000.300497	12.003610	-0.054588	4.815606
264.716480	8000.380357	12.008615	-0.054597	4.815630
264.631860	8000.263614	12.013619	-0.054581	4.815596
264.669707	8000.336874	12.018624	-0.054588	4.815617
264.529392	8000.279036	12.023629	-0.054562	4.815601
264.677588	8000.299627	12.028634	-0.054590	4.815606
264.557295	8000.277367	12.033639	-0.054567	4.815600
264.478169	8000.275008	12.038643	-0.054553	4.815600
264.738180	8000.287817	12.043648	-0.054601	4.815602
264.632999	8000.251918	12.048653	-0.054582	4.815592
264.680636	8000.305043	12.053658	-0.054591	4.815608
264.698737	8000.271163	12.058663	-0.054594	4.815598
264.649311	8000.271427	12.063667	-0.054585	4.815598
264.646994	8000.262848	12.068672	-0.054585	4.815596
264.604278	8000.247200	12.073677	-0.054577	4.815591
264.853773	8000.300427	12.078682	-0.054623	4.815606
264.798081	8000.249316	12.083687	-0.054613	4.815591
264.814473	8000.239975	12.088691	-0.054616	4.815588
265.039627	8000.301350	12.093696	-0.054658	4.815605
264.565370	8000.263678	12.098701	-0.054570	4.815596
264.505989	8000.286210	12.103706	-0.054559	4.815603
264.912272	8000.312097	12.108711	-0.054634	4.815609
264.685085	8000.276335	12.113715	-0.054592	4.815599
264.715918	8000.272572	12.118720	-0.054598	4.815598
264.876111	8000.285883	12.123725	-0.054628	4.815601
264.931252	8000.261155	12.128730	-0.054638	4.815594
265.034983	8000.275677	12.133735	-0.054658	4.815597
264.696220	8000.261588	12.138739	-0.054595	4.815595
264.762940	8000.304344	12.143744	-0.054607	4.815607
264.650315	8000.232006	12.148749	-0.054586	4.815587
264.672010	8000.271888	12.153754	-0.054590	4.815598
264.770659	8000.338667	12.158759	-0.054609	4.815617
264.833037	8000.311921	12.163763	-0.054620	4.815609
264.766448	8000.327926	12.168768	-0.054608	4.815614
264.631257	8000.265900	12.173773	-0.054583	4.815596
264.908835	8000.297155	12.178778	-0.054635	4.815604
264.664642	8000.239752	12.183783	-0.054589	4.815589
264.478753	8000.238849	12.188787	-0.054555	4.815589
264.955266	8000.281908	12.193792	-0.054643	4.815600
264.847656	8000.236356	12.198797	-0.054623	4.815587
264.774567	8000.283231	12.203802	-0.054610	4.815601
264.820613	8000.311763	12.208807	-0.054619	4.815609
264.928577	8000.269741	12.213811	-0.054639	4.815596
264.923150	8000.296362	12.218816	-0.054638	4.815604
264.725723	8000.283519	12.223821	-0.054601	4.815601
264.864091	8000.297540	12.228826	-0.054627	4.815605
264.884490	8000.288266	12.233831	-0.054631	4.815602
264.819361	8000.276522	12.238835	-0.054619	4.815599
264.810899	8000.279593	12.243840	-0.054617	4.815600
264.870444	8000.283778	12.248845	-0.054628	4.815601
264.899731	8000.279990	12.253850	-0.054634	4.815599
265.059270	8000.293290	12.258855	-0.054664	4.815602
264.875850	8000.267859	12.263859	-0.054629	4.815596
264.929962	8000.282637	12.268864	-0.054640	4.815600
264.789681	8000.260049	12.273869	-0.054613	4.815594
265.064788	8000.270969	12.278874	-0.054665	4.815596
265.040571	8000.336804	12.283879	-0.054660	4.815615
264.725513	8000.324171	12.288883	-0.054602	4.815613
265.122645	8000.292227	12.293888	-0.054676	4.815602
265.162385	8000.243747	12.298893	-0.054683	4.815587
265.054862	8000.270831	12.303898	-0.054663	4.815596
264.999713	8000.274205	12.308903	-0.054653	4.815597
265.027901	8000.240491	12.313907	-0.054658	4.815587
265.036845	8000.270551	12.318912	-0.054660	4.815596
264.853302	8000.257936	12.323917	-0.054626	4.815593
264.856606	8000.282563	12.328922	-0.054627	4.815600
264.906919	8000.312233	12.333927	-0.054636	4.815609
264.856882	8000.247328	12.338931	-0.054627	4.815590
265.054297	8000.292225	12.343936	-0.054664	4.815602
265.047179	8000.263273	12.348941	-0.054662	4.815594
264.905806	8000.290871	12.353946	-0.054636	4.815602
264.825722	8000.315200	12.358951	-0.054621	4.815610
264.828820	8000.256506	12.363955	-0.054622	4.815593
264.989077	8000.304000	12.368960	-0.054652	4.815606
264.808569	8000.307457	12.373965	-0.054618	4.815608
265.036934	8000.304794	12.378970	-0.054661	4.815606
265.006478	8000.341686	12.383975	-0.054655	4.815617
264.946951	8000.256330	12.388979	-0.054644	4.815592
265.039418	8000.285622	12.393984	-0.054661	4.815600
265.097552	8000.266284	12.398989	-0.054672	4.815594
265.083693	8000.276744	12.403994	-0.054670	4.815597
264.912815	8000.320949	12.408999	-0.054638	4.815611
264.919259	8000.264447	12.414003	-0.054639	4.815595
264.967895	8000.294089	12.419008	-0.054648	4.815603
264.771145	8000.229985	12.424013	-0.054612	4.815585
264.785096	8000.281491	12.429018	-0.054614	4.815600
265.134674	8000.250904	12.434023	-0.054680	4.815590
264.991130	8000.254967	12.439027	-0.054653	4.815592
265.106714	8000.296388	12.444032	-0.054674	4.815603
265.162116	8000.234278	12.449037	-0.054685	4.815585
265.115077	8000.248467	12.454042	-0.054676	4.815589
264.997913	8000.275393	12.459047	-0.054654	4.815597
265.276374	8000.263937	12.464051	-0.054706	4.815593
265.240031	8000.261211	12.469056	-0.054700	4.815592
265.172739	8000.253704	12.474061	-0.054687	4.815590
265.279719	8000.268280	12.479066	-0.054707	4.815594
265.205933	8000.311940	12.484071	-0.054693	4.815607
265.164680	8000.259996	12.489075	-0.054686	4.815592
265.067542	8000.261614	12.494080	-0.054668	4.815593
265.058522	8000.244381	12.499085	-0.054666	4.815588
265.085681	8000.280080	12.504090	-0.054671	4.815598
265.094711	8000.278097	12.509095	-0.054673	4.815598
265.097974	8000.262133	12.514099	-0.054674	4.815593
265.183944	8000.298796	12.519104	-0.054690	4.815603
265.190669	8000.296775	12.524109	-0.054691	4.815603
265.071200	8000.308709	12.529114	-0.054669	4.815607
265.078519	8000.286402	12.534119	-0.054670	4.815600
264.952258	8000.262975	12.539123	-0.054647	4.815594
265.039908	8000.291120	12.544128	-0.054663	4.815602
265.207669	8000.313101	12.549133	-0.054694	4.815607
265.276177	8000.286456	12.554138	-0.054707	4.815599
265.257581	8000.333156	12.559143	-0.054704	4.815613
265.005391	8000.292711	12.564147	-0.054657	4.815602
264.984351	8000.326553	12.569152	-0.054653	4.815612
264.897085	8000.292015	12.574157	-0.054637	4.815603
265.042252	8000.309352	12.579162	-0.054664	4.815607
264.960750	8000.364636	12.584167	-0.054649	4.815624
264.841367	8000.299662	12.589171	-0.054627	4.815605
265.153453	8000.366735	12.594176	-0.054685	4.815623
265.165705	8000.290031	12.599181	-0.054687	4.815601
265.149953	8000.310074	12.604186	-0.054684	4.815607
265.099973	8000.356260	12.609191	-0.054675	4.815621
264.818963	8000.293979	12.614195	-0.054623	4.815604
265.057548	8000.335279	12.619200	-0.054667	4.815615
264.911355	8000.317935	12.624205	-0.054640	4.815610
264.730981	8000.267985	12.629210	-0.054607	4.815596
265.089541	8000.276000	12.634215	-0.054673	4.815597
265.205057	8000.276829	12.639219	-0.054695	4.815597
265.169901	8000.271986	12.644224	-0.054688	4.815596
265.020148	8000.358196	12.649229	-0.054661	4.815621
264.872458	8000.304509	12.654234	-0.054633	4.815606
265.002158	8000.309843	12.659239	-0.054657	4.815607
264.813102	8000.240525	12.664243	-0.054622	4.815588
265.026973	8000.269669	12.669248	-0.054662	4.815596
265.090204	8000.246142	12.674253	-0.054674	4.815588
265.044150	8000.278506	12.679258	-0.054665	4.815598
265.142496	8000.327122	12.684263	-0.054684	4.815612
264.952584	8000.293038	12.689267	-0.054649	4.815603
265.208758	8000.294036	12.694272	-0.054696	4.815602
265.106714	8000.275278	12.699277	-0.054677	4.815597
265.202740	8000.283265	12.704282	-0.054695	4.815599
265.286768	8000.283579	12.709287	-0.054711	4.815598
265.018523	8000.256757	12.714291	-0.054661	4.815592
265.091088	8000.298542	12.719296	-0.054675	4.815604
265.070197	8000.282182	12.724301	-0.054671	4.815599
264.995345	8000.293779	12.729306	-0.054657	4.815603
264.909887	8000.341520	12.734311	-0.054641	4.815617
264.928127	8000.283074	12.739315	-0.054645	4.815600
264.965431	8000.309326	12.744320	-0.054652	4.815607
265.156941	8000.297514	12.749325	-0.054687	4.815603
265.258083	8000.288494	12.754330	-0.054706	4.815600
265.205812	8000.248120	12.759335	-0.054696	4.815588
265.042590	8000.230497	12.764339	-0.054666	4.815584
265.100384	8000.300880	12.769344	-0.054677	4.815604
265.097326	8000.324335	12.774349	-0.054676	4.815611
265.203285	8000.308985	12.779354	-0.054696	4.815606
265.115948	8000.332127	12.784359	-0.054680	4.815613
265.049774	8000.259480	12.789363	-0.054668	4.815592
264.943763	8000.288726	12.794368	-0.054648	4.815601
264.883435	8000.289879	12.799373	-0.054637	4.815602
265.082324	8000.287801	12.804378	-0.054674	4.815601
264.994486	8000.304526	12.809383	-0.054658	4.815606
264.992263	8000.261767	12.814387	-0.054657	4.815593
265.326799	8000.261912	12.819392	-0.054720	4.815592
265.143451	8000.276004	12.824397	-0.054686	4.815597
265.066166	8000.256584	12.829402	-0.054671	4.815592
265.230693	8000.266762	12.834407	-0.054702	4.815594
265.153577	8000.266571	12.839411	-0.054688	4.815594
265.144079	8000.311284	12.844416	-0.054686	4.815607
264.994823	8000.225526	12.849421	-0.054658	4.815583
265.037554	8000.243322	12.854426	-0.054666	4.815588
265.204588	8000.263154	12.859431	-0.054697	4.815593
265.101249	8000.232626	12.864435	-0.054678	4.815584
265.237854	8000.286141	12.869440	-0.054704	4.815599
265.204108	8000.237525	12.874445	-0.054697	4.815585
265.094620	8000.242145	12.879450	-0.054677	4.815587
265.124795	8000.276826	12.884455	-0.054683	4.815597
265.134352	8000.266306	12.889459	-0.054685	4.815594
265.095776	8000.310543	12.894464	-0.054678	4.815607
264.941966	8000.283460	12.899469	-0.054649	4.815600
265.055660	8000.273577	12.904474	-0.054670	4.815596
265.232851	8000.295712	12.909479	-0.054703	4.815602
265.088207	8000.239939	12.914483	-0.054676	4.815587
265.147445	8000.286846	12.919488	-0.054687	4.815600
265.131045	8000.244923	12.924493	-0.054684	4.815588
265.119234	8000.284257	12.929498	-0.054682	4.815599
265.062626	8000.307903	12.934503	-0.054672	4.815606
264.949590	8000.248375	12.939507	-0.054651	4.815590
265.301357	8000.288324	12.944512	-0.054716	4.815600
265.131029	8000.250289	12.949517	-0.054685	4.815589
265.000909	8000.266321	12.954522	-0.054660	4.815595
265.168299	8000.319273	12.959527	-0.054692	4.815609
265.005751	8000.273887	12.964531	-0.054662	4.815597
265.091515	8000.294525	12.969536	-0.054678	4.815602
265.201852	8000.255746	12.974541	-0.054698	4.815591
265.106487	8000.252053	12.979546	-0.054680	4.815590
265.214437	8000.289076	12.984551	-0.054701	4.815600
265.202453	8000.280339	12.989555	-0.054698	4.815598
265.169516	8000.292623	12.994560	-0.054692	4.815601
264.994386	8000.271600	12.999565	-0.054660	4.815596
265.157278	8000.277478	13.004570	-0.054690	4.815597
265.263479	8000.297382	13.009575	-0.054710	4.815602
265.127899	8000.279143	13.014579	-0.054685	4.815598
265.092335	8000.323429	13.019584	-0.054678	4.815611
265.325976	8000.272784	13.024589	-0.054722	4.815595
265.161808	8000.323509	13.029594	-0.054691	4.815611
265.178955	8000.352635	13.034599	-0.054695	4.815619
265.110237	8000.295969	13.039603	-0.054682	4.815603
265.421672	8000.332054	13.044608	-0.054740	4.815612
265.104634	8000.308705	13.049613	-0.054681	4.815606
264.839244	8000.274454	13.054618	-0.054632	4.815598
265.060020	8000.262053	13.059623	-0.054673	4.815593
265.192530	8000.287729	13.064627	-0.054697	4.815600
265.210198	8000.340364	13.069632	-0.054701	4.815615
265.309106	8000.311012	13.074637	-0.054719	4.815606
265.249055	8000.270511	13.079642	-0.054708	4.815595
265.396179	8000.304972	13.084647	-0.054736	4.815604
265.149180	8000.285975	13.089651	-0.054690	4.815600
265.177604	8000.356946	13.094656	-0.054695	4.815620
265.018499	8000.338321	13.099661	-0.054665	4.815616
265.113484	8000.306769	13.104666	-0.054683	4.815606
265.248667	8000.354920	13.109671	-0.054708	4.815619
264.892708	8000.298889	13.114675	-0.054642	4.815605
265.099880	8000.325788	13.119680	-0.054681	4.815611
265.040708	8000.325892	13.124685	-0.054670	4.815612
265.080298	8000.282750	13.129690	-0.054677	4.815599
265.108714	8000.281084	13.134695	-0.054683	4.815598
265.188195	8000.263164	13.139699	-0.054697	4.815593
265.213722	8000.293496	13.144704	-0.054702	4.815601
265.303356	8000.301379	13.149709	-0.054719	4.815603
265.231568	8000.283117	13.154714	-0.054706	4.815598
265.115658	8000.296177	13.159719	-0.054684	4.815603
265.047613	8000.279045	13.164723	-0.054672	4.815598
265.099996	8000.368567	13.169728	-0.054681	4.815624
265.008995	8000.360672	13.174733	-0.054665	4.815622
264.990762	8000.288810	13.179738	-0.054661	4.815601
264.993568	8000.350815	13.184743	-0.054662	4.815619
265.161815	8000.316191	13.189747	-0.054693	4.815608
265.186327	8000.329415	13.194752	-0.054698	4.815612
265.189182	8000.310240	13.199757	-0.054698	4.815606
265.199500	8000.329641	13.204762	-0.054700	4.815612
265.148887	8000.346976	13.209767	-0.054691	4.815617
265.150687	8000.277579	13.214771	-0.054691	4.815597
265.152827	8000.320346	13.219776	-0.054692	4.815610
265.235691	8000.346277	13.224781	-0.054707	4.815617
264.977573	8000.315348	13.229786	-0.054659	4.815609
265.109119	8000.377327	13.234791	-0.054684	4.815626
265.062278	8000.282564	13.239795	-0.054675	4.815599
265.207536	8000.334085	13.244800	-0.054702	4.815613
265.115386	8000.355012	13.249805	-0.054685	4.815620
265.028079	8000.257451	13.254810	-0.054669	4.815592
265.221501	8000.335397	13.259815	-0.054705	4.815614
265.207471	8000.335172	13.264819	-0.054703	4.815614
265.286802	8000.315113	13.269824	-0.054717	4.815607
265.130032	8000.347800	13.274829	-0.054688	4.815618
265.080194	8000.271148	13.279834	-0.054679	4.815596
265.138010	8000.327645	13.284839	-0.054690	4.815612
265.037567	8000.352709	13.289843	-0.054671	4.815620
265.210530	8000.295730	13.294848	-0.054703	4.815602
265.041331	8000.323940	13.299853	-0.054672	4.815611
265.135292	8000.315870	13.304858	-0.054690	4.815608
265.349159	8000.346084	13.309863	-0.054729	4.815616
265.356927	8000.285330	13.314867	-0.054731	4.815598
265.395560	8000.291309	13.319872	-0.054738	4.815600
265.185663	8000.338079	13.324877	-0.054699	4.815615
265.206852	8000.282886	13.329882	-0.054703	4.815598
265.385937	8000.347780	13.334887	-0.054737	4.815616
265.016273	8000.270160	13.339891	-0.054668	4.815596
265.196477	8000.307299	13.344896	-0.054701	4.815606
265.154105	8000.335451	13.349901	-0.054694	4.815614
265.074754	8000.270065	13.354906	-0.054679	4.815595
265.190679	8000.289060	13.359911	-0.054700	4.815600
265.190922	8000.252751	13.364915	-0.054700	4.815590
265.241754	8000.268543	13.369920	-0.054710	4.815594
265.225359	8000.292848	13.374925	-0.054707	4.815601
265.267730	8000.301024	13.379930	-0.054715	4.815603
265.416239	8000.321621	13.384935	-0.054743	4.815609
265.243886	8000.255780	13.389939	-0.054711	4.815590
265.385783	8000.301905	13.394944	-0.054737	4.815603
265.231027	8000.298306	13.399949	-0.054708	4.815603
265.223796	8000.249056	13.404954	-0.054707	4.815588
265.235326	8000.281296	13.409959	-0.054709	4.815598
265.315087	8000.265516	13.414963	-0.054724	4.815593
265.192104	8000.285938	13.419968	-0.054701	4.815599
265.269557	8000.338485	13.424973	-0.054716	4.815614
265.345070	8000.263886	13.429978	-0.054730	4.815592
265.459341	8000.358696	13.434983	-0.054751	4.815619
265.255259	8000.285925	13.439987	-0.054713	4.815599
265.279173	8000.313026	13.444992	-0.054718	4.815607
265.349829	8000.301371	13.449997	-0.054731	4.815603
265.433131	8000.284581	13.455002	-0.054747	4.815598
265.312798	8000.371274	13.460007	-0.054724	4.815624
265.198837	8000.313866	13.465011	-0.054703	4.815607
265.277308	8000.307680	13.470016	-0.054718	4.815605
265.356261	8000.328205	13.475021	-0.054733	4.815611
265.164185	8000.283404	13.480026	-0.054697	4.815599
265.370852	8000.297477	13.485031	-0.054735	4.815602
265.204636	8000.304372	13.490035	-0.054704	4.815605
265.169521	8000.295257	13.495040	-0.054698	4.815602
265.201125	8000.303257	13.500045	-0.054704	4.815604
265.056761	8000.257101	13.505050	-0.054677	4.815592
265.146448	8000.362189	13.510055	-0.054694	4.815622
265.292715	8000.297295	13.515059	-0.054721	4.815602
265.211172	8000.297032	13.520064	-0.054706	4.815602
265.172194	8000.298535	13.525069	-0.054699	4.815603
265.211766	8000.290643	13.530074	-0.054706	4.815601
265.261532	8000.334190	13.535079	-0.054716	4.815613
265.164678	8000.269586	13.540083	-0.054698	4.815595
265.224901	8000.357100	13.545088	-0.054709	4.815620
265.331915	8000.324677	13.550093	-0.054729	4.815610
265.220346	8000.324990	13.555098	-0.054708	4.815611
265.290329	8000.385960	13.560103	-0.054721	4.815628
265.273027	8000.317318	13.565107	-0.054718	4.815608
265.153243	8000.321769	13.570112	-0.054696	4.815610
265.236392	8000.348773	13.575117	-0.054711	4.815617
265.267528	8000.303356	13.580122	-0.054717	4.815604
265.166928	8000.328417	13.585127	-0.054699	4.815612
265.070052	8000.285176	13.590131	-0.054681	4.815600
265.166078	8000.323072	13.595136	-0.054699	4.815610
265.344875	8000.350575	13.600141	-0.054732	4.815617
265.233455	8000.315641	13.605146	-0.054711	4.815608
265.218096	8000.313258	13.610151	-0.054708	4.815607
265.220008	8000.301544	13.615155	-0.054709	4.815604
265.365441	8000.302864	13.620160	-0.054736	4.815603
265.212855	8000.240550	13.625165	-0.054708	4.815586
265.263471	8000.236044	13.630170	-0.054717	4.815584
265.507214	8000.293452	13.635175	-0.054762	4.815600
265.337338	8000.275718	13.640179	-0.054731	4.815596
265.493216	8000.309255	13.645184	-0.054760	4.815605
265.350885	8000.296246	13.650189	-0.054734	4.815601
265.371404	8000.282701	13.655194	-0.054737	4.815597
265.529906	8000.322689	13.660199	-0.054767	4.815608
265.360038	8000.332729	13.665203	-0.054735	4.815612
265.633779	8000.314788	13.670208	-0.054786	4.815606
265.458481	8000.326875	13.675213	-0.054754	4.815610
265.355920	8000.283540	13.680218	-0.054735	4.815598
265.348966	8000.342181	13.685223	-0.054734	4.815615
265.139189	8000.294954	13.690227	-0.054695	4.815602
265.201642	8000.276754	13.695232	-0.054706	4.815596
265.108141	8000.301932	13.700237	-0.054689	4.815604
265.030700	8000.297464	13.705242	-0.054675	4.815603
265.434370	8000.328651	13.710247	-0.054750	4.815611
265.441300	8000.252928	13.715251	-0.054751	4.815588
265.413621	8000.259957	13.720256	-0.054746	4.815591
265.189110	8000.327852	13.725261	-0.054704	4.815611
265.172449	8000.270970	13.730266	-0.054701	4.815595
265.239890	8000.339376	13.735271	-0.054714	4.815615
265.199902	8000.285316	13.740275	-0.054706	4.815599
265.138242	8000.300334	13.745280	-0.054695	4.815604
265.047309	8000.295644	13.750285	-0.054678	4.815603
265.409408	8000.295173	13.755290	-0.054746	4.815601
265.451106	8000.323634	13.760295	-0.054753	4.815609
265.176888	8000.244373	13.765299	-0.054702	4.815587
265.184260	8000.251976	13.770304	-0.054704	4.815589
265.298302	8000.262395	13.775309	-0.054725	4.815592
265.156993	8000.256880	13.780314	-0.054699	4.815591
265.435450	8000.291357	13.785319	-0.054751	4.815600
265.435820	8000.263595	13.790323	-0.054751	4.815592
265.410798	8000.259985	13.795328	-0.054746	4.815591
265.451013	8000.270263	13.800333	-0.054754	4.815593
265.470960	8000.255640	13.805338	-0.054758	4.815589
265.430092	8000.280612	13.810343	-0.054750	4.815596
265.268970	8000.254477	13.815347	-0.054720	4.815590
265.320286	8000.289504	13.820352	-0.054730	4.815600
265.382480	8000.285188	13.825357	-0.054741	4.815598
265.363869	8000.298774	13.830362	-0.054738	4.815602
265.480482	8000.315644	13.835367	-0.054760	4.815606
265.458248	8000.264012	13.840371	-0.054756	4.815592
265.241577	8000.262603	13.845376	-0.054715	4.815592
265.326073	8000.256515	13.850381	-0.054731	4.815590
265.358897	8000.222876	13.855386	-0.054737	4.815580
265.449512	8000.257480	13.860391	-0.054754	4.815590
265.203194	8000.245972	13.865395	-0.054708	4.815587
265.332071	8000.299361	13.870400	-0.054733	4.815602
265.279707	8000.300644	13.875405	-0.054723	4.815603
265.247667	8000.258465	13.880410	-0.054717	4.815591
265.388954	8000.314194	13.885415	-0.054743	4.815606
265.266693	8000.300446	13.890419	-0.054721	4.815603
265.261794	8000.288621	13.895424	-0.054720	4.815600
265.210339	8000.262146	13.900429	-0.054710	4.815592
265.307634	8000.259473	13.905434	-0.054728	4.815591
265.356457	8000.332914	13.910439	-0.054738	4.815612
265.348553	8000.281517	13.915443	-0.054736	4.815597
265.522514	8000.320690	13.920448	-0.054769	4.815608
265.379431	8000.275623	13.925453	-0.054742	4.815595
265.343211	8000.267558	13.930458	-0.054735	4.815593
265.319005	8000.337666	13.935463	-0.054731	4.815614
265.195285	8000.314280	13.940467	-0.054708	4.815607
265.251244	8000.287429	13.945472	-0.054718	4.815599
265.325321	8000.308944	13.950477	-0.054732	4.815605
265.457776	8000.283346	13.955482	-0.054757	4.815597
265.600133	8000.310252	13.960487	-0.054783	4.815604
265.417933	8000.295521	13.965491	-0.054750	4.815601
265.366860	8000.279735	13.970496	-0.054740	4.815596
265.563980	8000.311811	13.975501	-0.054777	4.815605
265.443699	8000.331209	13.980506	-0.054755	4.815611
265.427198	8000.333080	13.985511	-0.054752	4.815612
265.401607	8000.282461	13.990515	-0.054747	4.815597
265.403366	8000.299585	13.995520	-0.054747	4.815602
265.313413	8000.291707	14.000525	-0.054731	4.815600
265.270831	8000.274992	14.005530	-0.054723	4.815596
265.273357	8000.319902	14.010535	-0.054723	4.815609
265.141957	8000.252595	14.015539	-0.054699	4.815590
265.462456	8000.266396	14.020544	-0.054758	4.815592
265.312640	8000.325901	14.025549	-0.054731	4.815610
265.228226	8000.285000	14.030554	-0.054715	4.815599
265.294855	8000.286097	14.035559	-0.054727	4.815599
265.383535	8000.237350	14.040563	-0.054744	4.815584
265.294866	8000.274357	14.045568	-0.054728	4.815595
265.308181	8000.320512	14.050573	-0.054730	4.815609
265.323805	8000.275909	14.055578	-0.054733	4.815596
265.598288	8000.315662	14.060583	-0.054784	4.815606
265.496793	8000.259526	14.065587	-0.054765	4.815590
265.445866	8000.284333	14.070592	-0.054756	4.815597
265.481456	8000.253944	14.075597	-0.054763	4.815588
265.176296	8000.235063	14.080602	-0.054706	4.815584
265.489124	8000.262625	14.085607	-0.054764	4.815591
265.341470	8000.235643	14.090611	-0.054737	4.815584
265.314151	8000.289677	14.095616	-0.054732	4.815600
265.248917	8000.315318	14.100621	-0.054720	4.815607
265.090126	8000.304176	14.105626	-0.054690	4.815605
265.185927	8000.286523	14.110631	-0.054708	4.815599
265.009308	8000.301794	14.115635	-0.054675	4.815605
265.028719	8000.297844	14.120640	-0.054679	4.815603
265.370876	8000.306660	14.125645	-0.054743	4.815604
265.341920	8000.289099	14.130650	-0.054737	4.815599
265.243375	8000.296035	14.135655	-0.054719	4.815602
265.433167	8000.228649	14.140659	-0.054754	4.815581
265.462844	8000.233413	14.145664	-0.054760	4.815582
265.463727	8000.253728	14.150669	-0.054760	4.815588
265.370039	8000.317358	14.155674	-0.054743	4.815607
265.370481	8000.373984	14.160679	-0.054743	4.815624
265.375929	8000.302509	14.165683	-0.054744	4.815603
265.449122	8000.269532	14.170688	-0.054758	4.815593
265.575597	8000.298314	14.175693	-0.054781	4.815601
265.414130	8000.288196	14.180698	-0.054751	4.815599
265.202216	8000.297547	14.185703	-0.054712	4.815602
265.294002	8000.274487	14.190707	-0.054729	4.815595
265.423788	8000.285164	14.195712	-0.054753	4.815598
265.392528	8000.260089	14.200717	-0.054747	4.815591
265.273047	8000.245318	14.205722	-0.054725	4.815587
265.606806	8000.258269	14.210727	-0.054787	4.815589
265.374110	8000.232029	14.215731	-0.054744	4.815582
265.371520	8000.249083	14.220736	-0.054744	4.815587
265.270763	8000.251709	14.225741	-0.054725	4.815589
265.274078	8000.235746	14.230746	-0.054726	4.815584
265.427442	8000.239332	14.235751	-0.054754	4.815584
265.500294	8000.228780	14.240755	-0.054768	4.815581
265.312740	8000.247076	14.245760	-0.054733	4.815587
265.249676	8000.273821	14.250765	-0.054721	4.815595
265.088681	8000.241279	14.255770	-0.054692	4.815587
265.488175	8000.260647	14.260775	-0.054766	4.815590
265.332233	8000.259165	14.265779	-0.054737	4.815591
265.359586	8000.276710	14.270784	-0.054742	4.815596
265.432880	8000.267234	14.275789	-0.054756	4.815592
265.506553	7999.341285	14.280794	-0.054769	4.815321

265.335893	7996.082112	14.285799	-0.054735	4.814370
265.246087	7990.582909	14.290803	-0.054715	4.812762
265.302266	7983.943916	14.295808	-0.054721	4.810820
265.483501	7976.657835	14.300813	-0.054750	4.808687
265.294686	7969.004518	14.305818	-0.054710	4.806447
265.504731	7961.226733	14.310823	-0.054744	4.804168
265.386320	7953.324004	14.315827	-0.054717	4.801853
265.311519	7945.356596	14.320832	-0.054698	4.799517
265.073948	7937.464106	14.325837	-0.054649	4.797203
265.068562	7929.387486	14.330842	-0.054642	4.794833
265.204115	7921.403018	14.335847	-0.054663	4.792488
265.133569	7913.380157	14.340851	-0.054644	4.790132
265.321916	7905.416965	14.345856	-0.054674	4.787790
265.009760	7897.374225	14.350861	-0.054611	4.785427
264.870126	7889.412215	14.355866	-0.054580	4.783085
265.200067	7881.428697	14.360871	-0.054636	4.780734
265.249633	7873.408160	14.365875	-0.054640	4.778372
265.218109	7865.433949	14.370880	-0.054629	4.776022
264.930799	7857.388373	14.375885	-0.054570	4.773652
265.026257	7849.369778	14.380890	-0.054583	4.771287
265.030702	7841.403706	14.385895	-0.054579	4.768936
264.791582	7833.362438	14.390899	-0.054529	4.766563
264.952700	7825.341762	14.395904	-0.054554	4.764193
264.879420	7817.441573	14.400909	-0.054535	4.761859
264.808305	7809.326792	14.405914	-0.054517	4.759460
264.816922	7801.411209	14.410919	-0.054513	4.757119
264.753905	7793.340518	14.415923	-0.054496	4.754730
264.853507	7785.357954	14.420928	-0.054510	4.752366
264.805239	7777.325027	14.425933	-0.054495	4.749987
264.786253	7769.301735	14.430938	-0.054487	4.747609
264.716445	7761.277730	14.435943	-0.054469	4.745229
264.411075	7753.324764	14.440947	-0.054407	4.742871
264.450111	7745.318412	14.445952	-0.054409	4.740494
264.527273	7737.377406	14.450957	-0.054418	4.738135
264.500649	7729.313264	14.455962	-0.054408	4.735739
264.464441	7721.300374	14.460967	-0.054396	4.733357
264.418584	7713.334472	14.465971	-0.054382	4.730988
264.166244	7705.275236	14.470976	-0.054330	4.728590
264.150367	7697.329257	14.475981	-0.054322	4.726224
264.141865	7689.252178	14.480986	-0.054315	4.723818
264.095592	7681.352735	14.485991	-0.054301	4.721464
263.884195	7673.317697	14.490995	-0.054257	4.719068
263.820404	7665.370697	14.496000	-0.054240	4.716697
264.036218	7657.284643	14.501005	-0.054275	4.714283
263.988253	7649.299860	14.506010	-0.054261	4.711899
264.124081	7641.296535	14.511015	-0.054281	4.709507
263.980934	7633.275303	14.516019	-0.054249	4.707109
263.971576	7625.270677	14.521024	-0.054242	4.704715
263.805279	7617.344115	14.526029	-0.054206	4.702343
263.680767	7609.283271	14.531034	-0.054178	4.699930
263.809945	7601.346063	14.536039	-0.054197	4.697552
263.717613	7593.305167	14.541043	-0.054174	4.695142
263.664983	7585.275981	14.546048	-0.054159	4.692734
263.633671	7577.286445	14.551053	-0.054148	4.690337
263.383122	7569.314266	14.556058	-0.054096	4.687944
263.421803	7561.252319	14.561063	-0.054098	4.685523
263.735737	7553.268772	14.566067	-0.054152	4.683123
263.679013	7545.309016	14.571072	-0.054136	4.680730
263.506307	7537.312292	14.576077	-0.054099	4.678325
263.577863	7529.296084	14.581082	-0.054107	4.675912
263.641946	7521.274629	14.586087	-0.054114	4.673497
263.494456	7513.169309	14.591091	-0.054081	4.671055
263.334406	7505.201811	14.596096	-0.054046	4.668654
263.345855	7497.225750	14.601101	-0.054043	4.666248
263.271136	7489.204844	14.606106	-0.054024	4.663828
263.350658	7481.255928	14.611111	-0.054034	4.661428
263.269965	7473.220604	14.616115	-0.054013	4.659001
263.263641	7465.254827	14.621120	-0.054007	4.656594
263.278576	7457.270539	14.626125	-0.054005	4.654180
263.163914	7449.202309	14.631130	-0.053978	4.651739
263.037038	7441.217729	14.636135	-0.053949	4.649322
263.136018	7433.241051	14.641139	-0.053963	4.646906
263.099307	7425.191931	14.646144	-0.053951	4.644467
263.233591	7417.248344	14.651149	-0.053971	4.642059
263.055975	7409.202201	14.656154	-0.053932	4.639619
262.853634	7401.251854	14.661159	-0.053890	4.637206
262.954704	7393.194202	14.666163	-0.053903	4.634759
262.736238	7385.164954	14.671168	-0.053857	4.632320
262.867958	7377.197985	14.676173	-0.053877	4.629898
262.919164	7369.217606	14.681178	-0.053881	4.627471
262.618848	7361.175433	14.686183	-0.053820	4.625024
262.509454	7353.218769	14.691187	-0.053795	4.622602
262.717325	7345.193744	14.696192	-0.053828	4.620157
262.702574	7337.262941	14.701197	-0.053820	4.617740
262.497884	7329.182742	14.706202	-0.053777	4.615276
262.640307	7321.159101	14.711207	-0.053798	4.612828
262.594812	7313.157101	14.716211	-0.053785	4.610386
262.538709	7305.169592	14.721216	-0.053769	4.607946
262.495232	7297.175100	14.726221	-0.053756	4.605503
262.534136	7289.154181	14.731226	-0.053758	4.603051
262.480502	7281.194761	14.736231	-0.053743	4.600616
262.502217	7273.189525	14.741235	-0.053742	4.598166
262.221600	7265.177769	14.746240	-0.053684	4.595712
262.256018	7257.158700	14.751245	-0.053685	4.593255
262.095932	7249.066889	14.756250	-0.053650	4.590775
262.056756	7241.130899	14.761255	-0.053638	4.588340
262.091283	7233.110501	14.766259	-0.053639	4.585879
262.220465	7225.112476	14.771264	-0.053658	4.583423
262.175550	7217.139462	14.776269	-0.053645	4.580974
261.976084	7209.123443	14.781274	-0.053602	4.578509
262.154110	7201.152316	14.786279	-0.053630	4.576058
262.029157	7193.127526	14.791283	-0.053602	4.573589
262.159098	7185.084986	14.796288	-0.053621	4.571112
262.258456	7177.104622	14.801293	-0.053634	4.568654
262.124258	7169.131419	14.806298	-0.053604	4.566197
262.035665	7161.167451	14.811303	-0.053582	4.563740
261.877872	7153.198993	14.816307	-0.053548	4.561282
261.802513	7145.114239	14.821312	-0.053529	4.558786
261.982329	7137.163146	14.826317	-0.053557	4.556330
261.716846	7129.116373	14.831322	-0.053502	4.553842
261.879304	7121.102293	14.836327	-0.053528	4.551365
261.658717	7113.117674	14.841331	-0.053481	4.548894
261.564567	7105.124721	14.846336	-0.053459	4.546419
261.766817	7097.111364	14.851341	-0.053491	4.543938
261.833572	7089.142360	14.856346	-0.053498	4.541468
261.587816	7081.118104	14.861351	-0.053447	4.538980
261.540682	7073.150470	14.866355	-0.053434	4.536508
261.736626	7065.090165	14.871360	-0.053465	4.534006
261.583185	7057.090758	14.876365	-0.053431	4.531521
261.330876	7049.045241	14.881370	-0.053379	4.529020
261.423774	7041.099285	14.886375	-0.053391	4.526550
261.261381	7033.090207	14.891379	-0.053356	4.524058
261.281994	7025.175539	14.896384	-0.053354	4.521594
261.254670	7017.124236	14.901389	-0.053344	4.519087
261.329474	7009.145754	14.906394	-0.053353	4.516601
261.203246	7001.111148	14.911399	-0.053324	4.514095
261.245694	6993.005675	14.916403	-0.053327	4.511567
261.362451	6985.002122	14.921408	-0.053344	4.509069
261.299456	6977.067434	14.926413	-0.053327	4.506591
261.102936	6969.003448	14.931418	-0.053285	4.504070
261.164317	6961.087544	14.936423	-0.053291	4.501595
261.190807	6953.095477	14.941427	-0.053291	4.499095
260.883228	6945.084982	14.946432	-0.053229	4.496587
261.121328	6937.046079	14.951437	-0.053268	4.494070
260.915871	6929.012840	14.956442	-0.053224	4.491552
261.091871	6921.029258	14.961447	-0.053252	4.489050
261.060927	6913.054112	14.966451	-0.053241	4.486548
261.063722	6904.990618	14.971456	-0.053236	4.484017
260.843731	6897.112866	14.976461	-0.053190	4.481542
260.739750	6889.016848	14.981466	-0.053166	4.478997
260.782048	6881.096637	14.986471	-0.053169	4.476507
260.859354	6873.039564	14.991475	-0.053178	4.473973
260.713835	6865.007353	14.996480	-0.053145	4.471444
260.748778	6857.025283	15.001485	-0.053147	4.468930
260.695068	6849.042773	15.006490	-0.053132	4.466415
260.759233	6841.005011	15.011495	-0.053138	4.463880
260.281398	6833.052427	15.016499	-0.053044	4.461370
260.651204	6825.004317	15.021504	-0.053108	4.458831
260.553867	6817.053338	15.026509	-0.053085	4.456319
260.544153	6808.993208	15.031514	-0.053078	4.453772
260.588271	6801.039675	15.036519	-0.053081	4.451257
260.366464	6792.984540	15.041523	-0.053034	4.448707
260.402164	6784.995833	15.046528	-0.053036	4.446179
260.292383	6777.022458	15.051533	-0.053010	4.443653
260.290251	6768.989196	15.056538	-0.053005	4.441107
260.370245	6761.054903	15.061543	-0.053014	4.438591
260.188989	6753.008683	15.066547	-0.052976	4.436037
260.391168	6744.993268	15.071552	-0.053008	4.433493
260.256480	6736.942948	15.076557	-0.052978	4.430935
260.127402	6728.951266	15.081562	-0.052949	4.428395
260.106102	6720.975416	15.086567	-0.052939	4.425858
260.101089	6713.001952	15.091571	-0.052933	4.423321
260.144312	6704.997062	15.096576	-0.052936	4.420772
259.955484	6697.003236	15.101581	-0.052896	4.418225
259.942596	6688.951675	15.106586	-0.052888	4.415658
259.759510	6680.956383	15.111591	-0.052849	4.413107
259.521001	6672.935371	15.116595	-0.052800	4.410546
259.658283	6664.943432	15.121600	-0.052820	4.407995
259.887573	6656.974126	15.126605	-0.052857	4.405450
259.539686	6648.960187	15.131610	-0.052788	4.402886
259.566127	6640.989762	15.136615	-0.052787	4.400337
259.636306	6633.015421	15.141619	-0.052795	4.397785
259.380667	6624.955689	15.146624	-0.052742	4.395202
259.484219	6616.982322	15.151629	-0.052757	4.392648
259.382156	6608.907117	15.156634	-0.052732	4.390058
259.514565	6600.937694	15.161639	-0.052752	4.387502
259.544010	6592.939689	15.166643	-0.052752	4.384935
259.319692	6585.003372	15.171648	-0.052705	4.382385
259.466373	6576.975724	15.176653	-0.052727	4.379805
259.263466	6568.999901	15.181658	-0.052685	4.377240
259.160435	6560.954251	15.186663	-0.052660	4.374650
259.232206	6553.026485	15.191667	-0.052668	4.372098
259.241543	6544.964987	15.196672	-0.052665	4.369501
259.333972	6537.003534	15.201677	-0.052677	4.366936
259.292493	6528.932211	15.206682	-0.052664	4.364332
259.373357	6521.041306	15.211687	-0.052674	4.361786
259.195661	6513.017969	15.216691	-0.052636	4.359194
259.075424	6505.008005	15.221696	-0.052608	4.356606
259.077496	6496.971450	15.226701	-0.052604	4.354007
259.070930	6488.857863	15.231706	-0.052597	4.351383
258.876930	6480.904390	15.236711	-0.052556	4.348807
258.898269	6472.924298	15.241715	-0.052555	4.346223
258.800284	6464.904241	15.246720	-0.052531	4.343623
258.702973	6456.983344	15.251725	-0.052508	4.341054
258.806305	6448.923455	15.256730	-0.052522	4.338440
258.849749	6440.967729	15.261735	-0.052525	4.335857
258.732529	6432.941410	15.266739	-0.052498	4.333249
258.551135	6424.882006	15.271744	-0.052459	4.330628
258.741765	6416.970062	15.276749	-0.052489	4.328056
258.416981	6408.935095	15.281754	-0.052424	4.325439
258.723418	6400.975384	15.286759	-0.052476	4.322849
258.584189	6392.949899	15.291763	-0.052445	4.320233
258.633023	6384.966233	15.296768	-0.052449	4.317631
258.547085	6376.977060	15.301773	-0.052427	4.315024
258.454014	6368.915475	15.306778	-0.052405	4.312392
258.494587	6360.889189	15.311783	-0.052407	4.309771
258.506289	6352.922890	15.316787	-0.052404	4.307167
258.317238	6344.887903	15.321792	-0.052364	4.304538
258.511713	6336.947950	15.326797	-0.052395	4.301941
258.228506	6328.912687	15.331802	-0.052337	4.299308
258.183758	6320.944322	15.336807	-0.052324	4.296697
258.291480	6312.932350	15.341811	-0.052339	4.294072
258.213597	6304.917448	15.346816	-0.052319	4.291442
258.078229	6296.911779	15.351821	-0.052288	4.288813
257.953125	6288.892768	15.356826	-0.052260	4.286179
258.132720	6280.922344	15.361831	-0.052288	4.283561
258.100471	6272.938384	15.366835	-0.052277	4.280935
258.006176	6264.941961	15.371840	-0.052254	4.278304
258.175085	6256.948451	15.376845	-0.052281	4.275673
258.117671	6248.901263	15.381850	-0.052265	4.273022
257.909128	6240.844123	15.386855	-0.052221	4.270364
257.741082	6232.878074	15.391859	-0.052184	4.267735
257.692992	6224.854246	15.396864	-0.052170	4.265086
257.816892	6216.928162	15.401869	-0.052188	4.262470
257.743732	6208.896051	15.406874	-0.052169	4.259815
257.799521	6200.916449	15.411879	-0.052175	4.257177
257.699633	6192.923400	15.416883	-0.052151	4.254531
257.402129	6184.886140	15.421888	-0.052090	4.251867
257.559617	6176.884756	15.426893	-0.052115	4.249218
257.366313	6168.897166	15.431898	-0.052073	4.246568
257.402279	6160.922310	15.436903	-0.052075	4.243923
257.387912	6152.926576	15.441907	-0.052067	4.241269
257.391512	6144.909975	15.446912	-0.052063	4.238607
257.404834	6136.967634	15.451917	-0.052060	4.235968
257.236124	6128.899419	15.456922	-0.052023	4.233283
257.253977	6120.890059	15.461927	-0.052022	4.230618
257.206057	6112.922355	15.466931	-0.052007	4.227965
257.174498	6104.890814	15.471936	-0.051996	4.225289
257.311083	6096.940838	15.476941	-0.052017	4.222639
257.280095	6088.896024	15.481946	-0.052006	4.219956
257.308543	6080.965824	15.486951	-0.052006	4.217309
257.208780	6072.937023	15.491955	-0.051982	4.214626
257.270860	6064.881374	15.496960	-0.051989	4.211934
257.152545	6056.943703	15.501965	-0.051961	4.209278
256.864886	6048.945442	15.506970	-0.051903	4.206599
256.935192	6040.919856	15.511975	-0.051911	4.203912
256.699569	6032.957368	15.516979	-0.051862	4.201241
256.681878	6024.960619	15.521984	-0.051853	4.198560
256.856124	6016.961995	15.526989	-0.051880	4.195878
256.874954	6008.815331	15.531994	-0.051879	4.193143
256.762567	6000.800810	15.536999	-0.051853	4.190449
256.649324	5992.858369	15.542003	-0.051826	4.187778
256.733162	5984.866419	15.547008	-0.051837	4.185091
256.819322	5976.922153	15.552013	-0.051848	4.182418
256.671062	5968.872013	15.557018	-0.051815	4.179705
256.683700	5960.922799	15.562023	-0.051812	4.177026
256.606577	5952.892824	15.567027	-0.051793	4.174317
256.536593	5944.881734	15.572032	-0.051774	4.171613
256.620765	5936.861461	15.577037	-0.051785	4.168905
256.502741	5928.892910	15.582042	-0.051758	4.166211
256.367037	5920.878480	15.587047	-0.051727	4.163500
256.091005	5912.941459	15.592051	-0.051671	4.160811
256.171910	5904.904334	15.597056	-0.051681	4.158091
256.598108	5896.904741	15.602061	-0.051755	4.155386
256.401950	5888.879319	15.607066	-0.051713	4.152663
256.422123	5880.858138	15.612071	-0.051712	4.149942
256.369258	5872.865927	15.617075	-0.051697	4.147228
256.172277	5864.836285	15.622080	-0.051655	4.144498
256.154412	5856.926866	15.627085	-0.051647	4.141810
256.122742	5848.859759	15.632090	-0.051636	4.139065
256.278118	5840.900434	15.637095	-0.051659	4.136358
256.118201	5832.909982	15.642099	-0.051624	4.133635
255.968084	5824.836601	15.647104	-0.051591	4.130882
256.054509	5816.876273	15.652109	-0.051602	4.128168
255.805174	5808.879498	15.657114	-0.051551	4.125436
255.856566	5800.920919	15.662119	-0.051555	4.122719
255.853765	5792.869114	15.667123	-0.051549	4.119967
255.648643	5784.912373	15.672128	-0.051506	4.117244
255.769415	5776.906835	15.677133	-0.051523	4.114506
255.843691	5768.847261	15.682138	-0.051532	4.111748
255.635656	5760.869332	15.687143	-0.051488	4.109012
255.578233	5752.847392	15.692147	-0.051472	4.106261
255.621750	5744.870667	15.697152	-0.051475	4.103524
255.721938	5736.877986	15.702157	-0.051489	4.100782
255.406076	5728.898495	15.707162	-0.051425	4.098036
255.305064	5720.912527	15.712167	-0.051401	4.095290
255.357775	5712.891500	15.717171	-0.051405	4.092531
255.300523	5704.843002	15.722176	-0.051390	4.089760
255.287270	5696.940501	15.727181	-0.051382	4.087037
255.302409	5688.875562	15.732186	-0.051380	4.084257
255.306656	5680.928741	15.737191	-0.051375	4.081516
255.272061	5672.903823	15.742195	-0.051364	4.078746
255.296955	5664.933494	15.747200	-0.051363	4.075993
255.378817	5656.937355	15.752205	-0.051373	4.073230
255.207634	5648.894607	15.757210	-0.051336	4.070446
255.009240	5640.931586	15.762215	-0.051294	4.067687
255.256993	5632.904445	15.767219	-0.051335	4.064911
254.985036	5624.918461	15.772224	-0.051279	4.062139
254.964877	5616.938448	15.777229	-0.051270	4.059371
254.824336	5608.966190	15.782234	-0.051239	4.056602
254.869294	5600.929704	15.787239	-0.051242	4.053812
254.806101	5592.916739	15.792243	-0.051225	4.051026
254.786351	5584.902107	15.797248	-0.051217	4.048238
255.050725	5576.901630	15.802253	-0.051261	4.045458
254.876398	5568.941306	15.807258	-0.051223	4.042683
254.717407	5560.948260	15.812263	-0.051188	4.039895
254.791346	5552.977674	15.817267	-0.051197	4.037116
254.904531	5544.901759	15.822272	-0.051213	4.034300
254.733959	5536.826732	15.827277	-0.051176	4.031477
254.632043	5528.807147	15.832282	-0.051152	4.028673
254.555699	5520.883997	15.837287	-0.051132	4.025901
254.491357	5512.899825	15.842291	-0.051115	4.023106
254.451723	5504.892521	15.847296	-0.051103	4.020301
254.598778	5496.937793	15.852301	-0.051125	4.017515
254.461145	5488.913061	15.857306	-0.051094	4.014699
254.351844	5480.899877	15.862311	-0.051069	4.011885
254.431893	5472.852785	15.867315	-0.051078	4.009060
254.361995	5464.876693	15.872320	-0.051060	4.006256
254.189398	5456.946357	15.877325	-0.051023	4.003465
254.281387	5448.930705	15.882330	-0.051035	4.000645
254.272989	5440.943855	15.887335	-0.051028	3.997832
254.158360	5432.955984	15.892339	-0.051002	3.995015
253.918114	5424.876923	15.897344	-0.050952	3.992162
254.100950	5416.893878	15.902349	-0.050981	3.989348
254.093185	5408.875743	15.907354	-0.050974	3.986516
253.920717	5400.901001	15.912359	-0.050937	3.983694
254.055463	5392.929990	15.917363	-0.050957	3.980877
254.128446	5384.948070	15.922368	-0.050965	3.978053
254.085653	5376.952574	15.927373	-0.050952	3.975221
253.889098	5368.920766	15.932378	-0.050910	3.972371
253.914748	5360.884260	15.937383	-0.050910	3.969521
253.842152	5352.953165	15.942387	-0.050891	3.966704
253.644357	5344.923907	15.947392	-0.050849	3.963849
253.943746	5336.979350	15.952397	-0.050900	3.961030
253.787392	5328.958796	15.957402	-0.050866	3.958174
253.532809	5320.986561	15.962407	-0.050813	3.955332
253.510944	5312.962417	15.967411	-0.050804	3.952473
253.715723	5304.892755	15.972416	-0.050837	3.949600
253.628258	5296.935946	15.977421	-0.050815	3.946760
253.413362	5288.927366	15.982426	-0.050770	3.943897
253.542852	5280.960965	15.987431	-0.050789	3.941053
253.399724	5272.986731	15.992435	-0.050757	3.938200
253.340568	5264.973165	15.997440	-0.050741	3.935332
253.401045	5256.986512	16.002445	-0.050747	3.932473
253.308378	5248.928848	16.007450	-0.050725	3.929584
252.976415	5240.976249	16.012455	-0.050658	3.926727
253.141635	5232.951384	16.017459	-0.050683	3.923850
253.305182	5224.985440	16.022464	-0.050709	3.920993
253.334576	5217.024263	16.027469	-0.050709	3.918132
253.222510	5208.992820	16.032474	-0.050683	3.915242
253.167286	5200.963577	16.037479	-0.050668	3.912351
253.301657	5192.942656	16.042483	-0.050687	3.909465
252.858170	5185.004266	16.047488	-0.050600	3.906595
252.890886	5176.984873	16.052493	-0.050601	3.903703
252.912563	5168.983232	16.057498	-0.050600	3.900816
252.852703	5160.998691	16.062503	-0.050583	3.897930
252.807795	5153.023626	16.067507	-0.050570	3.895046
252.889108	5144.952083	16.072512	-0.050580	3.892128
253.028159	5136.941268	16.077517	-0.050600	3.889230
252.747469	5128.987944	16.082522	-0.050543	3.886344
252.943050	5120.971377	16.087527	-0.050574	3.883441
252.913153	5112.989129	16.092531	-0.050564	3.880544
252.819838	5105.011968	16.097536	-0.050541	3.877645
252.710648	5097.027074	16.102541	-0.050516	3.874742
252.574847	5088.763036	16.107546	-0.050485	3.871734
252.559048	5080.824817	16.112551	-0.050477	3.868844
252.462094	5072.869542	16.117555	-0.050454	3.865945
252.342871	5064.921500	16.122560	-0.050426	3.863045
252.343836	5056.961769	16.127565	-0.050421	3.860142
252.343675	5048.979028	16.132570	-0.050416	3.857228
252.401738	5040.970920	16.137575	-0.050422	3.854303
252.634093	5032.956652	16.142579	-0.050460	3.851378
252.469342	5024.955111	16.147584	-0.050424	3.848447
252.557132	5016.986560	16.152589	-0.050435	3.845531
252.499469	5008.995546	16.157594	-0.050419	3.842602
252.186691	5000.996057	16.162599	-0.050356	3.839662
252.272948	4993.061121	16.167603	-0.050367	3.836752
252.150619	4984.997827	16.172608	-0.050339	3.833787
252.311798	4977.012184	16.177613	-0.050364	3.830856
252.111995	4968.987829	16.182618	-0.050322	3.827900
252.311746	4960.985075	16.187623	-0.050354	3.824958
252.279021	4953.077123	16.192627	-0.050342	3.822044
252.026184	4945.017754	16.197632	-0.050290	3.819067
251.839741	4937.128415	16.202637	-0.050250	3.816152
251.915332	4929.037322	16.207642	-0.050259	3.813166
251.809084	4921.057689	16.212647	-0.050234	3.810214
251.644822	4913.088519	16.217651	-0.050199	3.807264
251.626195	4905.030239	16.222656	-0.050190	3.804280
252.008685	4897.108079	16.227661	-0.050256	3.801354
251.952262	4889.069548	16.232666	-0.050240	3.798373
251.951036	4881.084568	16.237671	-0.050235	3.795411
251.933399	4873.072341	16.242675	-0.050226	3.792435
251.710786	4865.015619	16.247680	-0.050180	3.789437
251.456034	4857.099047	16.252685	-0.050127	3.786487
251.467527	4849.073037	16.257690	-0.050124	3.783500
251.504402	4841.085355	16.262695	-0.050126	3.780526
251.283701	4833.088494	16.267699	-0.050080	3.777540
251.390760	4825.041438	16.272704	-0.050094	3.774540
251.584655	4817.049804	16.277709	-0.050125	3.771561
251.330478	4809.051576	16.282714	-0.050073	3.768567
251.231023	4801.077084	16.287719	-0.050049	3.765582
251.300564	4793.127803	16.292723	-0.050057	3.762609
251.133916	4785.076805	16.297728	-0.050021	3.759590
251.130205	4777.165512	16.302733	-0.050015	3.756624
251.052335	4769.116983	16.307738	-0.049995	3.753603
251.320440	4761.046044	16.312743	-0.050040	3.750579
250.942943	4753.123809	16.317747	-0.049965	3.747593
250.991911	4745.064441	16.322752	-0.049969	3.744564
251.167344	4737.130536	16.327757	-0.049996	3.741582
250.848219	4729.140302	16.332762	-0.049932	3.738565
250.758942	4721.139709	16.337767	-0.049910	3.735547
250.803420	4713.128080	16.342771	-0.049913	3.732525
250.828620	4705.077862	16.347776	-0.049912	3.729486
250.733625	4697.154153	16.352781	-0.049890	3.726490
250.662022	4689.133876	16.357786	-0.049871	3.723455
250.836836	4681.144824	16.362791	-0.049899	3.720435
250.739314	4673.209309	16.367795	-0.049875	3.717427
250.729219	4665.175863	16.372800	-0.049868	3.714381
250.839874	4657.089411	16.377805	-0.049884	3.711316
250.557994	4649.094165	16.382810	-0.049826	3.708273
250.534246	4641.076544	16.387815	-0.049816	3.705225
250.600908	4633.141697	16.392819	-0.049824	3.702208
250.598104	4625.143228	16.397824	-0.049818	3.699164
250.347535	4617.214264	16.402829	-0.049766	3.696136
250.455491	4609.165245	16.407834	-0.049781	3.693070
250.443987	4601.167536	16.412839	-0.049774	3.690018
250.389925	4593.195609	16.417843	-0.049759	3.686972
250.251215	4585.201619	16.422848	-0.049728	3.683912
250.347345	4577.230547	16.427853	-0.049740	3.680865
250.085286	4569.238558	16.432858	-0.049686	3.677798
249.995059	4561.210116	16.437863	-0.049665	3.674720
250.275425	4553.214057	16.442867	-0.049712	3.671660
249.998786	4545.203449	16.447872	-0.049655	3.668578
250.006338	4537.225221	16.452877	-0.049651	3.665513
249.834005	4529.234176	16.457882	-0.049614	3.662436
249.842708	4521.211706	16.462887	-0.049610	3.659349
249.965794	4513.286271	16.467891	-0.049628	3.656300
249.900682	4505.207792	16.472896	-0.049611	3.653184
249.861674	4497.208872	16.477901	-0.049598	3.650097
249.848380	4489.235991	16.482906	-0.049591	3.647018
249.796506	4481.237786	16.487911	-0.049576	3.643926
249.865080	4473.265525	16.492915	-0.049584	3.640844
249.640870	4465.260581	16.497920	-0.049537	3.637739
249.605193	4457.290581	16.502925	-0.049525	3.634650
249.381933	4449.216490	16.507930	-0.049478	3.631513
249.511245	4441.226207	16.512935	-0.049497	3.628416
249.527188	4433.223309	16.517939	-0.049495	3.625307
249.550009	4425.254081	16.522944	-0.049494	3.622210
249.536628	4417.268548	16.527949	-0.049486	3.619102
249.461192	4409.303075	16.532954	-0.049467	3.615998
249.144944	4401.291853	16.537959	-0.049403	3.612866
249.197128	4393.279203	16.542963	-0.049408	3.609742
249.269956	4385.288790	16.547968	-0.049416	3.606624
249.262102	4377.326182	16.552973	-0.049409	3.603512
249.194310	4369.369959	16.557978	-0.049392	3.600398
249.282826	4361.395901	16.562983	-0.049403	3.597279
249.133260	4353.359818	16.567987	-0.049370	3.594126
248.983560	4345.339622	16.572992	-0.049337	3.590977
249.068278	4337.342991	16.577997	-0.049348	3.587840
248.826211	4329.342835	16.583002	-0.049297	3.584690
248.783925	4321.397220	16.588007	-0.049284	3.581565
248.956374	4313.395350	16.593011	-0.049311	3.578421
249.060914	4305.379254	16.598016	-0.049326	3.575266
248.965996	4297.395876	16.603021	-0.049303	3.572116
248.838028	4289.349256	16.608026	-0.049274	3.568937
248.913340	4281.390516	16.613031	-0.049283	3.565796
248.689252	4273.448220	16.618035	-0.049236	3.562650
248.594485	4265.414352	16.623040	-0.049213	3.559469
248.683251	4257.466301	16.628045	-0.049224	3.556324
248.727917	4249.356098	16.633050	-0.049228	3.553111
248.586908	4241.307966	16.638055	-0.049196	3.549914
248.458862	4233.365996	16.643059	-0.049167	3.546757
248.329050	4225.351986	16.648064	-0.049138	3.543568
248.463445	4217.399144	16.653069	-0.049158	3.540408
248.396279	4209.413665	16.658074	-0.049140	3.537227
248.368097	4201.427762	16.663079	-0.049130	3.534044
248.164056	4193.446742	16.668083	-0.049086	3.530855
248.229118	4185.407265	16.673088	-0.049093	3.527647
248.337291	4177.408500	16.678093	-0.049108	3.524454
248.102187	4169.477463	16.683098	-0.049060	3.521275
248.017718	4161.472798	16.688103	-0.049039	3.518068
248.074314	4153.502042	16.693107	-0.049044	3.514876
248.060998	4145.438056	16.698112	-0.049036	3.511642
248.064019	4137.459547	16.703117	-0.049032	3.508439
248.013336	4129.473059	16.708122	-0.049017	3.505229
248.090025	4121.472410	16.713127	-0.049026	3.502014
248.182409	4113.508870	16.718131	-0.049038	3.498811
247.963477	4105.538091	16.723136	-0.048992	3.495593
247.989751	4097.540146	16.728141	-0.048992	3.492369
247.805116	4089.501138	16.733146	-0.048953	3.489118
247.947985	4081.529763	16.738151	-0.048974	3.485902
248.005566	4073.569302	16.743155	-0.048980	3.482685
247.773784	4065.557259	16.748160	-0.048931	3.479435
247.803069	4057.619996	16.753165	-0.048932	3.476220
247.838992	4049.574881	16.758170	-0.048933	3.472959
247.611203	4041.537491	16.763175	-0.048886	3.469689
247.565446	4033.595454	16.768179	-0.048872	3.466461
247.549149	4025.567175	16.773184	-0.048864	3.463195
247.489922	4017.618911	16.778189	-0.048848	3.459958
247.395331	4009.609723	16.783194	-0.048825	3.456692
247.221156	4001.598480	16.788199	-0.048787	3.453419
247.329472	3993.581334	16.793203	-0.048802	3.450150
247.349327	3985.598742	16.798208	-0.048801	3.446889
247.347336	3977.630046	16.803213	-0.048795	3.443630
247.354760	3969.636120	16.808218	-0.048792	3.440358
247.377644	3961.663774	16.813223	-0.048791	3.437092
247.476583	3953.631173	16.818227	-0.048804	3.433801
247.135747	3945.631526	16.823232	-0.048735	3.430505
247.176024	3937.644963	16.828237	-0.048738	3.427225
247.334990	3929.640357	16.833242	-0.048762	3.423937
247.151788	3921.678349	16.838247	-0.048723	3.420653
247.118037	3913.719322	16.843251	-0.048711	3.417372
247.026638	3905.696324	16.848256	-0.048689	3.414059
246.936470	3897.710532	16.853261	-0.048667	3.410759
246.813978	3889.723877	16.858266	-0.048639	3.407453
246.836912	3881.707281	16.863271	-0.048638	3.404137
246.829742	3873.788408	16.868275	-0.048632	3.400858
246.730851	3865.780219	16.873280	-0.048608	3.397535
246.551110	3857.787445	16.878285	-0.048570	3.394212
246.698952	3849.675138	16.883290	-0.048592	3.390848
246.713992	3841.683326	16.888295	-0.048590	3.387526
246.728688	3833.737621	16.893299	-0.048587	3.384219
246.531522	3825.775656	16.898304	-0.048546	3.380896
246.722926	3817.784923	16.903309	-0.048576	3.377570
246.353035	3809.807817	16.908314	-0.048502	3.374228
246.317972	3801.789359	16.913319	-0.048490	3.370876
246.400938	3793.799408	16.918323	-0.048501	3.367538
246.220871	3785.795135	16.923328	-0.048462	3.364180
246.402351	3777.847605	16.928333	-0.048491	3.360856
246.480191	3769.847585	16.933338	-0.048500	3.357503
246.609684	3761.828037	16.938343	-0.048519	3.354140
246.317483	3753.855115	16.943347	-0.048459	3.350779
246.266937	3745.836790	16.948352	-0.048445	3.347403
246.314870	3737.848417	16.953357	-0.048448	3.344040
246.121618	3729.913452	16.958362	-0.048407	3.340688
246.160531	3721.897556	16.963367	-0.048409	3.337307
246.091841	3713.913200	16.968371	-0.048392	3.333931
245.949457	3705.891026	16.973376	-0.048360	3.330533
245.933705	3697.909495	16.978381	-0.048352	3.327154
245.976196	3689.926546	16.983386	-0.048355	3.323773
245.691394	3681.950375	16.988391	-0.048296	3.320379
245.689145	3674.017814	16.993395	-0.048291	3.317011
245.472101	3665.994125	16.998400	-0.048245	3.313592
245.662877	3657.950730	17.003405	-0.048276	3.310177
245.693045	3649.948136	17.008410	-0.048276	3.306770
245.622944	3641.978079	17.013415	-0.048258	3.303369
245.475070	3634.012241	17.018419	-0.048225	3.299963
245.449889	3626.022547	17.023424	-0.048215	3.296549
245.244591	3618.018624	17.028429	-0.048172	3.293118
245.402093	3609.983267	17.033434	-0.048196	3.289684
245.372582	3602.032765	17.038439	-0.048185	3.286275
245.308958	3594.090698	17.043443	-0.048169	3.282865
245.130342	3586.068504	17.048448	-0.048130	3.279413
245.364988	3578.111030	17.053453	-0.048169	3.276001
245.402830	3570.071578	17.058458	-0.048171	3.272542
245.298373	3562.066595	17.063463	-0.048146	3.269089
245.253029	3554.096566	17.068467	-0.048132	3.265650
245.295018	3546.107466	17.073472	-0.048135	3.262202
245.183987	3538.116982	17.078477	-0.048109	3.258745
245.106675	3530.148530	17.083482	-0.048090	3.255294
245.249094	3522.103525	17.088487	-0.048111	3.251815
245.073194	3514.151090	17.093491	-0.048073	3.248360
244.952948	3506.128740	17.098496	-0.048046	3.244873
245.174240	3498.184006	17.103501	-0.048082	3.241430
245.041443	3490.207275	17.108506	-0.048052	3.237954
244.880843	3482.217395	17.113511	-0.048017	3.234469
244.862647	3474.162824	17.118515	-0.048008	3.230957
244.916184	3466.145366	17.123520	-0.048013	3.227460
244.796555	3458.186333	17.128525	-0.047985	3.223978
244.632137	3450.224461	17.133530	-0.047950	3.220489
244.722714	3442.223129	17.138535	-0.047961	3.216990
244.680136	3434.263634	17.143539	-0.047948	3.213500
244.334967	3426.251735	17.148544	-0.047879	3.209970
244.321014	3418.280043	17.153549	-0.047871	3.206468
244.405869	3410.289269	17.158554	-0.047882	3.202957
244.159979	3402.310946	17.163559	-0.047831	3.199435
244.313961	3394.367956	17.168563	-0.047854	3.195940
244.376500	3386.308624	17.173568	-0.047861	3.192387
244.245559	3378.325445	17.178573	-0.047831	3.188856
244.119353	3370.336611	17.183578	-0.047803	3.185318
244.262995	3362.354123	17.188583	-0.047824	3.181790
244.137757	3354.395673	17.193587	-0.047796	3.178258
244.026813	3346.410299	17.198592	-0.047770	3.174710
244.082763	3338.422036	17.203597	-0.047775	3.171165
243.938906	3330.401633	17.208602	-0.047743	3.167592
243.933825	3322.409866	17.213607	-0.047737	3.164034
244.070910	3314.451814	17.218611	-0.047758	3.160494
243.935507	3306.471046	17.223616	-0.047727	3.156927
243.841943	3298.490404	17.228621	-0.047705	3.153358
243.719555	3290.451183	17.233626	-0.047677	3.149758
243.663907	3282.468361	17.238631	-0.047661	3.146182
243.656494	3274.492010	17.243635	-0.047655	3.142607
243.678571	3266.510723	17.248640	-0.047654	3.139026
243.723368	3258.534911	17.253645	-0.047657	3.135445
243.666593	3250.537264	17.258650	-0.047641	3.131846
243.493212	3242.531248	17.263655	-0.047604	3.128234
243.354290	3234.567846	17.268659	-0.047573	3.124638
243.306953	3226.598385	17.273664	-0.047559	3.121039
243.320317	3218.636259	17.278669	-0.047556	3.117442
243.311164	3210.625547	17.283674	-0.047549	3.113818
243.362249	3202.589916	17.288679	-0.047554	3.110181
243.248597	3194.644801	17.293683	-0.047527	3.106574
243.084898	3186.664492	17.298688	-0.047492	3.102944
243.128304	3178.659798	17.303693	-0.047495	3.099308
243.076560	3170.684322	17.308698	-0.047480	3.095677
243.023440	3162.682753	17.313703	-0.047465	3.092029
243.159693	3154.707819	17.318707	-0.047485	3.088398
243.075347	3146.690684	17.323712	-0.047464	3.084734
243.164454	3138.742689	17.328717	-0.047476	3.081104
242.983087	3130.787815	17.333722	-0.047437	3.077455
242.925237	3122.775450	17.338727	-0.047421	3.073781
243.098049	3114.684608	17.343731	-0.047448	3.070077
242.763612	3106.727862	17.348736	-0.047380	3.066406
242.774137	3098.783556	17.353741	-0.047377	3.062753
242.774305	3090.796930	17.358746	-0.047372	3.059076
242.836315	3082.806122	17.363751	-0.047379	3.055395
242.750185	3074.842165	17.368755	-0.047357	3.051715
242.739677	3066.851717	17.373760	-0.047350	3.048022
242.575102	3058.882132	17.378765	-0.047314	3.044327
242.632936	3050.902019	17.383770	-0.047320	3.040633
242.289000	3042.964429	17.388775	-0.047251	3.036935
242.505555	3034.943606	17.393779	-0.047286	3.033221
242.503251	3026.906926	17.398784	-0.047280	3.029484
242.594780	3018.940771	17.403789	-0.047292	3.025780
242.600182	3010.970548	17.408794	-0.047288	3.022065
242.171148	3003.034797	17.413799	-0.047203	3.018341
242.094361	2995.043471	17.418803	-0.047184	3.014604
242.200201	2987.000258	17.423808	-0.047198	3.010846
242.165659	2979.027745	17.428813	-0.047187	3.007110
242.066043	2971.069349	17.433818	-0.047163	3.003372
242.091561	2963.070507	17.438823	-0.047163	2.999618
241.968043	2955.137231	17.443827	-0.047135	2.995882
241.981623	2947.076131	17.448832	-0.047132	2.992087
241.893563	2939.102220	17.453837	-0.047110	2.988324
241.881841	2931.099219	17.458842	-0.047103	2.984547
241.734074	2923.147908	17.463847	-0.047070	2.980782
241.663059	2915.199196	17.468851	-0.047052	2.977017
241.769185	2907.156699	17.473856	-0.047067	2.973213
241.731066	2899.180657	17.478861	-0.047054	2.969427
241.422093	2891.246472	17.483866	-0.046992	2.965643
241.511309	2883.252257	17.488871	-0.047003	2.961846
241.632412	2875.287095	17.493875	-0.047021	2.958059
241.543100	2867.281461	17.498880	-0.046999	2.954237
241.545288	2859.278967	17.503885	-0.046994	2.950417
241.581138	2851.292335	17.508890	-0.046996	2.946601
241.590501	2843.305865	17.513895	-0.046992	2.942779
241.534414	2835.351194	17.518899	-0.046977	2.938963
241.235531	2827.385827	17.523904	-0.046916	2.935125
241.491784	2819.362770	17.528909	-0.046958	2.931283
241.274097	2811.418030	17.533914	-0.046913	2.927449
240.986063	2803.452003	17.538919	-0.046854	2.923596
241.351167	2795.452262	17.543923	-0.046917	2.919756
241.237721	2787.470791	17.548928	-0.046890	2.915894
240.993639	2779.440138	17.553933	-0.046840	2.911997
241.099699	2771.431414	17.558938	-0.046854	2.908123
241.235544	2763.415868	17.563943	-0.046875	2.904243
240.998833	2755.517008	17.568947	-0.046825	2.900394
240.916865	2747.539136	17.573952	-0.046805	2.896510
240.878574	2739.552431	17.578957	-0.046793	2.892619
240.759551	2731.584821	17.583962	-0.046765	2.888727
240.468713	2723.596649	17.588967	-0.046706	2.884811
240.709312	2715.652137	17.593971	-0.046746	2.880940
240.704956	2707.648027	17.598976	-0.046740	2.877021
240.455344	2699.685435	17.603981	-0.046688	2.873103
240.552327	2691.665141	17.608986	-0.046701	2.869171
240.517442	2683.685819	17.613991	-0.046689	2.865246
240.434573	2675.740587	17.618995	-0.046669	2.861330
240.268857	2667.752952	17.624000	-0.046633	2.857384
240.482560	2659.753236	17.629005	-0.046668	2.853446
240.426123	2651.748897	17.634010	-0.046652	2.849486
240.247255	2643.798564	17.639015	-0.046613	2.845541
240.296956	2635.851691	17.644019	-0.046618	2.841604
240.251962	2627.863709	17.649024	-0.046604	2.837637
240.182879	2619.887153	17.654029	-0.046586	2.833668
240.188375	2611.875081	17.659034	-0.046582	2.829680
240.157740	2603.879051	17.664039	-0.046571	2.825692
240.033509	2595.947524	17.669043	-0.046543	2.821725
239.935139	2587.969960	17.674048	-0.046519	2.817732
239.934431	2579.986322	17.679053	-0.046514	2.813735
240.059290	2571.973462	17.684058	-0.046532	2.809725
239.892981	2563.998031	17.689063	-0.046496	2.805711
239.953461	2556.047666	17.694067	-0.046502	2.801718
239.939286	2548.064557	17.699072	-0.046494	2.797697
239.777717	2540.096989	17.704077	-0.046459	2.793671
239.699136	2532.101723	17.709082	-0.046439	2.789629
239.597289	2524.122021	17.714087	-0.046415	2.785588
239.625396	2516.184431	17.719091	-0.046415	2.781570
239.527928	2508.211404	17.724096	-0.046392	2.777521
239.467329	2500.243299	17.729101	-0.046376	2.773470
239.400073	2492.245936	17.734106	-0.046358	2.769398
239.402597	2484.244854	17.739111	-0.046353	2.765323
239.457597	2476.303228	17.744115	-0.046358	2.761275
239.270299	2468.329002	17.749120	-0.046318	2.757190
239.299772	2460.322908	17.754125	-0.046319	2.753095
239.015625	2452.294424	17.759130	-0.046261	2.748964
239.197384	2444.282152	17.764135	-0.046289	2.744863
239.173550	2436.356432	17.769139	-0.046280	2.740789
238.746045	2428.447876	17.774144	-0.046195	2.736692
238.904739	2420.438917	17.779149	-0.046219	2.732573
239.000280	2412.426482	17.784154	-0.046232	2.728442
238.942452	2404.460059	17.789159	-0.046216	2.724320
238.779940	2396.559767	17.794163	-0.046181	2.720219
238.695868	2388.576701	17.799168	-0.046160	2.716073
238.643864	2380.570802	17.804173	-0.046145	2.711912
238.628233	2372.584259	17.809178	-0.046137	2.707756
238.695647	2364.591641	17.814183	-0.046145	2.703596
238.727424	2356.638282	17.819187	-0.046145	2.699448
238.434230	2348.717127	17.824192	-0.046086	2.695289
238.468492	2340.705129	17.829197	-0.046087	2.691098
238.460783	2332.723153	17.834202	-0.046080	2.686913
238.410877	2324.753963	17.839207	-0.046066	2.682725
238.238963	2316.830406	17.844211	-0.046029	2.678547
238.282640	2308.823272	17.849216	-0.046032	2.674333
238.318926	2300.816621	17.854221	-0.046033	2.670111
238.391720	2292.821119	17.859226	-0.046042	2.665891
238.289959	2284.869524	17.864231	-0.046018	2.661676
238.315245	2276.914485	17.869235	-0.046017	2.657461
237.908946	2268.980152	17.874240	-0.045936	2.653223
237.947771	2260.974312	17.879245	-0.045939	2.648968
238.055713	2252.996554	17.884250	-0.045953	2.644726
238.028414	2245.020656	17.889255	-0.045943	2.640469
237.867702	2237.107613	17.894259	-0.045908	2.636231
237.844912	2229.085771	17.899264	-0.045899	2.631936
237.997927	2221.089960	17.904269	-0.045922	2.627660
237.786720	2213.142502	17.909274	-0.045878	2.623378
237.703944	2205.178320	17.914279	-0.045857	2.619089
237.775841	2197.222238	17.919283	-0.045865	2.614808
237.525134	2189.227859	17.924288	-0.045814	2.610478
237.583675	2181.262680	17.929293	-0.045819	2.606176
237.571992	2173.308700	17.934298	-0.045812	2.601869
237.435267	2165.361058	17.939303	-0.045781	2.597550
237.514152	2157.317078	17.944307	-0.045791	2.593186
237.445891	2149.210408	17.949312	-0.045773	2.588771
237.479024	2141.266291	17.954317	-0.045774	2.584443
237.276685	2133.367869	17.959322	-0.045731	2.580117
237.124584	2125.427155	17.964327	-0.045698	2.575764
237.326769	2117.439968	17.969331	-0.045730	2.571403
237.086414	2109.489608	17.974336	-0.045680	2.567023
237.213790	2101.543400	17.979341	-0.045699	2.562664
237.136735	2093.598814	17.984346	-0.045680	2.558285
237.022863	2085.626728	17.989351	-0.045653	2.553880
236.898041	2077.646702	17.994355	-0.045625	2.549462
236.959575	2069.657463	17.999360	-0.045631	2.545045
236.966967	2061.724949	18.004365	-0.045627	2.540647
236.910716	2053.764566	18.009370	-0.045612	2.536222
236.569671	2045.802035	18.014375	-0.045543	2.531768
236.693381	2037.818094	18.019379	-0.045561	2.527327
236.641608	2029.850739	18.024384	-0.045546	2.522874
236.510636	2021.914041	18.029389	-0.045517	2.518426
236.607228	2013.945519	18.034394	-0.045530	2.513968
236.516585	2005.931233	18.039399	-0.045508	2.509463
236.481608	1997.978025	18.044403	-0.045496	2.504988
236.499229	1990.004851	18.049408	-0.045494	2.500498
236.534818	1982.055266	18.054413	-0.045496	2.496014
236.209124	1974.123092	18.059418	-0.045430	2.491506
236.109371	1966.136545	18.064423	-0.045406	2.486975
236.084789	1958.199929	18.069427	-0.045396	2.482470
236.303455	1950.212099	18.074432	-0.045432	2.477945
235.962226	1942.279815	18.079437	-0.045363	2.473403
235.990085	1934.285776	18.084442	-0.045363	2.468844
235.898205	1926.302737	18.089447	-0.045341	2.464274
236.020238	1918.378762	18.094451	-0.045359	2.459745
235.845145	1910.420120	18.099456	-0.045321	2.455166
235.681540	1902.450504	18.104461	-0.045285	2.450573
235.653507	1894.482188	18.109466	-0.045275	2.445982
235.779147	1886.500527	18.114471	-0.045293	2.441386
235.835688	1878.560443	18.119475	-0.045299	2.436801
235.618384	1870.573624	18.124480	-0.045253	2.432159
235.536045	1862.589198	18.129485	-0.045233	2.427519
235.690710	1854.623337	18.134490	-0.045256	2.422900
235.589826	1846.675618	18.139495	-0.045232	2.418263
235.496947	1838.745879	18.144499	-0.045210	2.413628
235.297845	1830.768188	18.149504	-0.045168	2.408948
235.364680	1822.798693	18.154509	-0.045175	2.404284
235.412751	1814.868362	18.159514	-0.045179	2.399633
235.154226	1806.936998	18.164519	-0.045126	2.394948
235.346903	1798.934301	18.169523	-0.045156	2.390247
235.271172	1790.978108	18.174528	-0.045137	2.385543
235.135762	1783.029300	18.179533	-0.045107	2.380830
235.097682	1775.094564	18.184538	-0.045095	2.376123
235.050615	1767.115075	18.189543	-0.045081	2.371380
234.925835	1759.183253	18.194547	-0.045052	2.366649
234.793871	1751.222831	18.199552	-0.045023	2.361891
235.015291	1743.256672	18.204557	-0.045059	2.357148
234.920545	1735.299114	18.209562	-0.045036	2.352376
234.789360	1727.318245	18.214567	-0.045006	2.347577
234.731470	1719.369516	18.219571	-0.044991	2.342793
234.656227	1711.431380	18.224576	-0.044971	2.338005
234.521300	1703.494152	18.229581	-0.044941	2.333202
234.455789	1695.522396	18.234586	-0.044924	2.328374
234.373492	1687.563578	18.239591	-0.044903	2.323543
234.336591	1679.636210	18.244595	-0.044891	2.318724
234.293312	1671.682146	18.249600	-0.044878	2.313878
234.296161	1663.692946	18.254605	-0.044874	2.309005
234.355039	1655.743784	18.259610	-0.044879	2.304151
234.067180	1647.817678	18.264615	-0.044821	2.299271
234.124900	1639.877591	18.269619	-0.044826	2.294402
234.175407	1631.880023	18.274624	-0.044831	2.289486
234.005303	1623.948203	18.279629	-0.044794	2.284581
233.959894	1616.033974	18.284634	-0.044780	2.279687
233.909615	1608.081524	18.289639	-0.044766	2.274759
234.109685	1600.024987	18.294643	-0.044798	2.269777
233.899134	1592.092295	18.299648	-0.044753	2.264825
233.694288	1584.168784	18.304653	-0.044710	2.259869
233.786884	1576.226935	18.309658	-0.044722	2.254916
233.651939	1568.272603	18.314663	-0.044692	2.249925
233.640742	1560.321736	18.319667	-0.044685	2.244935
233.836988	1552.362068	18.324672	-0.044716	2.239948
233.622376	1544.459584	18.329677	-0.044671	2.234948
233.622119	1536.497027	18.334682	-0.044666	2.229919
233.474089	1528.531010	18.339687	-0.044633	2.224863
233.417201	1520.618074	18.344691	-0.044618	2.219837
233.431583	1512.657166	18.349696	-0.044615	2.214776
233.351286	1504.703046	18.354701	-0.044595	2.209699
233.409719	1496.768690	18.359706	-0.044601	2.204635
233.204427	1488.845645	18.364711	-0.044558	2.199543
233.188843	1480.913058	18.369715	-0.044550	2.194450
233.096140	1472.925692	18.374720	-0.044527	2.189303
233.006488	1464.979939	18.379725	-0.044505	2.184171
232.895026	1457.067821	18.384730	-0.044479	2.179047
232.868417	1449.111788	18.389735	-0.044469	2.173890
232.859932	1441.164615	18.394739	-0.044463	2.168728
232.708498	1433.227973	18.399744	-0.044429	2.163547
232.894062	1425.273834	18.404749	-0.044459	2.158374
232.913257	1417.345213	18.409754	-0.044457	2.153190
232.651241	1409.393126	18.414759	-0.044403	2.147951
232.715367	1401.471545	18.419763	-0.044410	2.142750
232.606965	1393.538503	18.424768	-0.044385	2.137513
232.431412	1385.614071	18.429773	-0.044347	2.132262
232.368320	1377.669790	18.434778	-0.044330	2.126996
232.436062	1369.710638	18.439783	-0.044338	2.121719
232.443045	1361.790050	18.444787	-0.044334	2.116449
232.252888	1353.816667	18.449792	-0.044293	2.111111
232.342105	1345.844633	18.454797	-0.044305	2.105788
232.296634	1337.933323	18.459802	-0.044291	2.100479
232.180070	1330.011745	18.464807	-0.044264	2.095143
232.162993	1322.064284	18.469811	-0.044256	2.089785
232.182201	1314.124309	18.474816	-0.044255	2.084422
232.176722	1306.223973	18.479821	-0.044249	2.079070
232.003888	1298.316240	18.484826	-0.044211	2.073682
231.818653	1290.358630	18.489831	-0.044172	2.068246
231.961169	1282.420766	18.494835	-0.044193	2.062840
231.793006	1274.510759	18.499840	-0.044157	2.057409
231.841153	1266.558718	18.504845	-0.044160	2.051956
231.944353	1258.618546	18.509850	-0.044175	2.046502
231.591677	1250.737917	18.514855	-0.044104	2.041029
231.577403	1242.835450	18.519859	-0.044096	2.035560
231.462436	1234.869261	18.524864	-0.044070	2.030022
231.321017	1226.930792	18.529869	-0.044038	2.024485
231.037360	1219.061718	18.534874	-0.043980	2.018967
231.224271	1211.074596	18.539879	-0.044010	2.013400
231.498817	1203.109311	18.544883	-0.044056	2.007842
231.098823	1195.244969	18.549888	-0.043976	2.002269
231.096714	1187.324986	18.554893	-0.043971	1.996683
231.129688	1179.381377	18.559898	-0.043972	1.991068
230.913155	1171.458782	18.564903	-0.043926	1.985425
230.767355	1163.574177	18.569907	-0.043894	1.979802
230.788544	1155.652195	18.574912	-0.043893	1.974153
230.798201	1147.701398	18.579917	-0.043890	1.968466
230.850597	1139.785183	18.584922	-0.043894	1.962792
230.526036	1131.910965	18.589927	-0.043829	1.957091
230.724688	1123.922522	18.594931	-0.043861	1.951348
230.573286	1115.984323	18.599936	-0.043827	1.945586
230.326926	1108.117931	18.604941	-0.043776	1.939849
230.462347	1100.186060	18.609946	-0.043796	1.934088
230.104541	1092.289245	18.614951	-0.043725	1.928282
230.181185	1084.369021	18.619955	-0.043734	1.922489
230.087136	1076.466749	18.624960	-0.043711	1.916673
230.176101	1068.507105	18.629965	-0.043723	1.910817
230.195947	1060.594239	18.634970	-0.043721	1.904971
230.089002	1052.708866	18.639975	-0.043696	1.899112
230.195277	1044.788478	18.644979	-0.043711	1.893233
229.916941	1036.896094	18.649984	-0.043654	1.887313
229.871456	1028.996149	18.654989	-0.043641	1.881395
229.927814	1021.100767	18.659994	-0.043646	1.875474
229.877324	1013.156113	18.664999	-0.043631	1.869484
229.904881	1005.248310	18.670003	-0.043631	1.863512
229.734845	997.364564	18.675008	-0.043595	1.857517
229.717732	989.449967	18.680013	-0.043586	1.851496
229.517686	981.569742	18.685018	-0.043544	1.845460
229.284457	973.701798	18.690023	-0.043496	1.839410
229.421481	965.783505	18.695027	-0.043516	1.833345
229.393036	957.842905	18.700032	-0.043506	1.827223
229.238385	949.964679	18.705037	-0.043472	1.821113
229.109810	942.106553	18.710042	-0.043443	1.815002
229.034661	934.178823	18.715047	-0.043424	1.808822
229.080221	926.292059	18.720051	-0.043427	1.802668
229.234878	918.380848	18.725056	-0.043451	1.796486
229.074035	910.445542	18.730061	-0.043416	1.790226
229.050499	902.554490	18.735066	-0.043406	1.783995
228.747863	894.703477	18.740071	-0.043345	1.777740
228.801917	886.800303	18.745075	-0.043350	1.771466
228.635736	878.915396	18.750080	-0.043314	1.765156
228.586462	871.050088	18.755085	-0.043300	1.758855
228.615668	863.157839	18.760090	-0.043300	1.752518
228.654593	855.235719	18.765095	-0.043302	1.746136
228.369386	847.405172	18.770099	-0.043244	1.739763
228.347238	839.521621	18.775104	-0.043235	1.733357
228.383115	831.609717	18.780109	-0.043236	1.726912
228.387203	823.753015	18.785114	-0.043232	1.720484
228.028084	815.924345	18.790119	-0.043160	1.714008
227.848100	808.030816	18.795123	-0.043121	1.707477
227.917205	800.131330	18.800128	-0.043129	1.700948
227.800913	792.266762	18.805133	-0.043102	1.694399
227.726014	784.387260	18.810138	-0.043083	1.687817
227.658978	776.514564	18.815143	-0.043066	1.681216
227.754509	768.647212	18.820147	-0.043079	1.674616
227.626607	760.776215	18.825152	-0.043050	1.667956
227.515093	752.916285	18.830157	-0.043024	1.661281
227.443389	745.067195	18.835162	-0.043005	1.654594
227.125334	737.220510	18.840167	-0.042941	1.647848
227.203882	729.347520	18.845171	-0.042951	1.641106
227.060226	721.501513	18.850176	-0.042919	1.634329
226.974644	713.575645	18.855181	-0.042898	1.627463
227.131836	705.703583	18.860186	-0.042922	1.620648
226.979754	697.862335	18.865191	-0.042889	1.613787
226.875101	690.018458	18.870195	-0.042864	1.606902
226.659044	682.199215	18.875200	-0.042819	1.599993
226.733723	674.338951	18.880205	-0.042828	1.593060
226.787330	666.473491	18.885210	-0.042833	1.586088
226.631227	658.643249	18.890215	-0.042799	1.579087
226.586438	650.806553	18.895219	-0.042785	1.572065
226.706843	642.928451	18.900224	-0.042802	1.564998
226.616206	635.129334	18.905229	-0.042781	1.557939
226.581129	627.287077	18.910234	-0.042769	1.550818
226.409537	619.451167	18.915239	-0.042732	1.543649
226.385386	611.623587	18.920243	-0.042722	1.536476
226.296707	603.796444	18.925248	-0.042701	1.529260
226.229211	595.972494	18.930253	-0.042683	1.522016
226.248151	588.161644	18.935258	-0.042682	1.514763
226.051465	580.346846	18.940263	-0.042640	1.507438
225.905438	572.542309	18.945267	-0.042608	1.500095
226.070798	564.694282	18.950272	-0.042634	1.492723
225.801844	556.898431	18.955277	-0.042579	1.485296
225.898495	549.092862	18.960282	-0.042592	1.477880
225.772280	541.249067	18.965287	-0.042563	1.470354
225.631744	533.447344	18.970291	-0.042532	1.462829
225.381767	525.671133	18.975296	-0.042480	1.455271
225.245168	517.867518	18.980301	-0.042450	1.447665
225.311927	510.065573	18.985306	-0.042457	1.440054
225.092544	502.294814	18.990311	-0.042411	1.432386
225.016852	494.503315	18.995315	-0.042392	1.424680
225.017260	486.706405	19.000320	-0.042387	1.416939
225.035262	478.901198	19.005325	-0.042386	1.409151
224.966578	471.128706	19.010330	-0.042368	1.401337
224.805200	463.372346	19.015335	-0.042333	1.393480
224.804114	455.571711	19.020339	-0.042327	1.385561
224.607611	447.832028	19.025344	-0.042286	1.377625
224.527489	440.052679	19.030349	-0.042266	1.369623
224.678962	432.265110	19.035354	-0.042289	1.361605
224.465796	424.533273	19.040359	-0.042244	1.353534
224.499703	416.761032	19.045363	-0.042246	1.345415
224.354355	409.028192	19.050368	-0.042214	1.337257
224.119528	401.298596	19.055373	-0.042165	1.329036
223.987897	393.572379	19.060378	-0.042136	1.320787
224.003167	385.769321	19.065383	-0.042133	1.312429
224.062216	377.939744	19.070387	-0.042139	1.303997
223.693266	370.266495	19.075392	-0.042066	1.295602
223.526914	362.553988	19.080397	-0.042030	1.287146
223.737926	354.806928	19.085402	-0.042064	1.278667
223.548894	347.114516	19.090407	-0.042024	1.270116
223.449005	339.417564	19.095411	-0.042000	1.261520
223.297342	331.737297	19.100416	-0.041967	1.252873
223.201221	324.030550	19.105421	-0.041944	1.244146
223.038801	316.369513	19.110426	-0.041909	1.235398
222.941463	308.658517	19.115431	-0.041886	1.226542
222.886920	300.985048	19.120435	-0.041871	1.217673
222.687854	293.319099	19.125440	-0.041829	1.208720
222.636358	285.646844	19.130445	-0.041814	1.199722
222.672845	277.975917	19.135450	-0.041816	1.190675
222.520932	270.322180	19.140455	-0.041783	1.181541
222.452373	262.682347	19.145459	-0.041765	1.172369
222.556649	255.007509	19.150464	-0.041780	1.163119
222.277153	247.409042	19.155469	-0.041723	1.153808
222.261624	239.745318	19.160474	-0.041715	1.144395
222.111134	232.130310	19.165479	-0.041682	1.134937
222.218263	224.489914	19.170483	-0.041697	1.125423
222.097414	216.909304	19.175488	-0.041670	1.115853
221.692728	209.359924	19.180493	-0.041589	1.106179
221.724285	201.768983	19.185498	-0.041590	1.096462
221.581653	194.188123	19.190503	-0.041559	1.086632
221.439085	186.649116	19.195507	-0.041528	1.076767
221.228858	179.095339	19.200512	-0.041484	1.066776
221.256845	171.524963	19.205517	-0.041484	1.056724
221.290386	163.969786	19.210522	-0.041485	1.046596
220.989635	156.486009	19.215527	-0.041424	1.036388
221.100751	148.937718	19.220531	-0.041440	1.026087
220.936561	141.457171	19.225536	-0.041405	1.015710
220.615497	134.002043	19.230541	-0.041340	1.005224
220.467911	126.541642	19.235546	-0.041308	0.994661
220.439326	119.019070	19.240551	-0.041298	0.983926
220.152515	111.605843	19.245555	-0.041240	0.973166
219.986546	104.173152	19.250560	-0.041204	0.962287
219.811918	96.766554	19.255565	-0.041167	0.951321
219.866509	89.334949	19.260570	-0.041172	0.940249
219.213002	82.029403	19.265575	-0.041046	0.929048
218.805482	74.709787	19.270579	-0.040965	0.917755
217.931765	67.456520	19.275584	-0.040798	0.906297
217.227147	60.423756	19.280589	-0.040662	0.895086