Fri Mar 12 13:55:22 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.556885	0.050896	0.000000	0.000036	0.721446

0.652185	0.031148	0.005005	0.000019	0.721441
0.657907	-0.086043	0.010010	0.000018	0.721212
0.588017	-0.114944	0.015014	0.000031	0.721131
0.610069	-0.123910	0.020019	0.000026	0.721121
0.654131	-0.127589	0.025024	0.000018	0.721129
0.450263	-0.093983	0.030029	0.000056	0.721124
0.366209	-0.079729	0.035034	0.000072	0.721123
0.518114	-0.103207	0.040038	0.000043	0.721130
0.404178	-0.087362	0.045043	0.000065	0.721121
0.627316	-0.123723	0.050048	0.000023	0.721128
0.668597	-0.134605	0.055053	0.000015	0.721121
0.797792	-0.156301	0.060058	-0.000009	0.721124
0.540989	-0.109182	0.065062	0.000039	0.721127
0.708336	-0.142552	0.070067	0.000008	0.721120
0.733047	-0.144135	0.075072	0.000003	0.721125
0.509832	-0.107639	0.080077	0.000045	0.721119
0.760434	-0.261523	0.085082	-0.000002	0.720904
0.868968	-0.292670	0.090086	-0.000022	0.720881
0.738713	-0.272806	0.095091	0.000002	0.720874
0.657402	-0.254637	0.100096	0.000017	0.720882
0.522947	-0.231446	0.105101	0.000042	0.720880
0.763013	-0.276496	0.110106	-0.000003	0.720876
0.779215	-0.393639	0.115110	-0.000006	0.720651
0.604464	-0.421279	0.120115	0.000027	0.720536
0.811947	-0.454382	0.125120	-0.000012	0.720543
0.629602	-0.424922	0.130125	0.000022	0.720537
0.608160	-0.420349	0.135130	0.000026	0.720539
0.700238	-0.564664	0.140134	0.000009	0.720287
0.619497	-0.584842	0.145139	0.000024	0.720219
0.775112	-0.607125	0.150144	-0.000005	0.720230
0.747310	-0.605264	0.155149	0.000000	0.720224
0.579886	-0.691107	0.160154	0.000031	0.719996
0.584028	-0.739500	0.165158	0.000030	0.719902
0.563492	-0.739487	0.170163	0.000034	0.719895
0.695148	-0.758734	0.175168	0.000010	0.719904
0.614706	-0.894465	0.180173	0.000025	0.719608
0.567887	-0.891669	0.185178	0.000033	0.719597
0.484606	-0.874738	0.190182	0.000049	0.719601
0.549140	-0.986353	0.195187	0.000037	0.719404
0.382268	-1.023880	0.200192	0.000068	0.719271
0.435138	-1.034562	0.205197	0.000058	0.719269
0.342783	-1.078501	0.210202	0.000075	0.719150
0.540405	-1.206081	0.215206	0.000038	0.718968
0.217715	-1.153199	0.220211	0.000098	0.718959
0.134934	-1.194862	0.225216	0.000114	0.718848
0.320780	-1.331654	0.230221	0.000079	0.718643
0.388090	-1.344828	0.235226	0.000067	0.718641
0.231827	-1.392276	0.240230	0.000096	0.718492
0.356019	-1.487209	0.245235	0.000073	0.718349
0.336830	-1.481103	0.250240	0.000076	0.718354
0.320413	-1.632337	0.255245	0.000079	0.718050
0.450786	-1.671479	0.260250	0.000055	0.718018
0.370897	-1.721720	0.265254	0.000070	0.717891
0.110372	-1.771567	0.270259	0.000118	0.717701
0.138700	-1.771794	0.275264	0.000113	0.717710
0.226366	-1.947310	0.280269	0.000097	0.717394
0.192177	-1.949153	0.285274	0.000103	0.717379
0.215651	-2.045332	0.290278	0.000099	0.717197
0.010257	-2.068053	0.295283	0.000137	0.717080
-0.248674	-2.078111	0.300288	0.000185	0.716969
-0.518657	-2.138055	0.305293	0.000236	0.716755
-0.772707	-2.093748	0.310298	0.000283	0.716753
-2.141041	-1.996759	0.315302	0.000537	0.716463
-2.482581	-1.947114	0.320307	0.000601	0.716441
-2.175746	-1.996844	0.325312	0.000544	0.716450
-2.592978	-2.072202	0.330317	0.000622	0.716154
-3.208726	-1.974099	0.335322	0.000736	0.716131
-3.073923	-1.994408	0.340326	0.000711	0.716139
-3.160804	-2.072653	0.345331	0.000727	0.715953
-3.753129	-2.001287	0.350336	0.000837	0.715885
-3.967888	-1.965393	0.355341	0.000877	0.715881
-4.010510	-1.998641	0.360346	0.000885	0.715800
-4.964600	-1.954872	0.365350	0.001063	0.715550
-4.802048	-1.990521	0.370355	0.001032	0.715537
-4.992459	-1.951719	0.375360	0.001068	0.715546
-5.162446	-1.935766	0.380365	0.001099	0.715518
-5.621702	-1.998666	0.385370	0.001185	0.715231
-5.463062	-2.025274	0.390374	0.001155	0.715235
-6.284662	-1.884732	0.395379	0.001308	0.715223
-5.711584	-1.981629	0.400384	0.001202	0.715233
-5.743574	-2.064139	0.405389	0.001208	0.715059
-7.047268	-1.910908	0.410394	0.001450	0.714902
-6.538596	-1.999207	0.415398	0.001355	0.714907
-7.066860	-1.907967	0.420403	0.001454	0.714901
-6.619525	-1.983255	0.425408	0.001370	0.714910
-6.613739	-2.079412	0.430413	0.001369	0.714721
-8.153348	-1.863666	0.435418	0.001656	0.714605
-7.269877	-2.018151	0.440422	0.001491	0.714611
-7.556011	-1.971420	0.445427	0.001545	0.714602
-8.049418	-1.878328	0.450432	0.001636	0.714613
-7.704681	-1.960658	0.455437	0.001572	0.714571
-8.431278	-1.980124	0.460442	0.001708	0.714276
-8.528291	-1.962093	0.465446	0.001726	0.714277
-8.936685	-1.892517	0.470451	0.001801	0.714271
-8.361554	-1.990226	0.475456	0.001694	0.714280
-8.424812	-1.980253	0.480461	0.001706	0.714278
-8.952365	-1.900292	0.485466	0.001804	0.714250
-8.874684	-2.049936	0.490470	0.001790	0.713980
-9.516311	-1.942063	0.495475	0.001909	0.713968
-9.986193	-1.855323	0.500480	0.001997	0.713974
-9.390187	-1.962884	0.505485	0.001886	0.713971
-9.436504	-1.954749	0.510490	0.001894	0.713971
-9.641194	-1.917574	0.515494	0.001932	0.713972
-10.008554	-1.980021	0.520499	0.002001	0.713718
-10.296182	-1.960064	0.525504	0.002054	0.713656
-10.051577	-2.005136	0.530509	0.002009	0.713653
-10.616273	-1.906528	0.535514	0.002114	0.713649
-10.214947	-1.972024	0.540518	0.002039	0.713661
-10.521330	-1.923208	0.545523	0.002096	0.713650
-10.469941	-1.986181	0.550528	0.002086	0.713543
-11.408077	-1.908239	0.555533	0.002261	0.713366
-11.240486	-1.942847	0.560538	0.002230	0.713356
-11.052186	-1.970785	0.565542	0.002195	0.713368
-11.527887	-1.890620	0.570547	0.002283	0.713359
-11.185276	-1.948170	0.575552	0.002219	0.713366
-11.108006	-1.964331	0.580557	0.002205	0.713361
-11.694360	-1.981287	0.585562	0.002314	0.713119
-11.963608	-1.978069	0.590566	0.002364	0.713031
-12.166328	-1.945714	0.595571	0.002402	0.713023
-12.325191	-1.914114	0.600576	0.002431	0.713030
-12.288173	-1.921376	0.605581	0.002424	0.713028
-12.143190	-1.947797	0.610586	0.002397	0.713027
-11.976262	-1.974479	0.615590	0.002366	0.713034
-12.901213	-1.955744	0.620595	0.002538	0.712743
-12.964710	-1.958661	0.625600	0.002550	0.712715
-12.970969	-1.959389	0.630605	0.002551	0.712711
-13.274549	-1.905807	0.635610	0.002608	0.712710
-13.109188	-1.931154	0.640614	0.002577	0.712718
-13.168539	-1.924695	0.645619	0.002588	0.712710
-13.055145	-1.940900	0.650624	0.002567	0.712718
-13.364159	-2.012287	0.655629	0.002624	0.712467
-14.248127	-1.894319	0.660634	0.002789	0.712388
-13.919074	-1.949933	0.665638	0.002728	0.712394
-13.974000	-1.944731	0.670643	0.002738	0.712385
-14.032905	-1.930003	0.675648	0.002749	0.712393
-13.817835	-1.967854	0.680653	0.002709	0.712394
-14.194293	-1.903675	0.685658	0.002779	0.712389
-14.024969	-2.038609	0.690662	0.002747	0.712180
-14.778105	-1.951493	0.695667	0.002887	0.712086
-14.945772	-1.916486	0.700672	0.002919	0.712097
-14.948711	-1.916942	0.705677	0.002919	0.712095
-15.118089	-1.889032	0.710682	0.002950	0.712090
-14.610729	-1.974972	0.715686	0.002856	0.712099
-15.264277	-1.864785	0.720691	0.002978	0.712087
-15.170722	-1.984683	0.725696	0.002960	0.711881
-15.791847	-1.933673	0.730701	0.003076	0.711762
-16.159626	-1.870800	0.735706	0.003144	0.711757
-15.807823	-1.927341	0.740710	0.003079	0.711770
-15.701116	-1.949800	0.745715	0.003059	0.711763
-15.668986	-1.952785	0.750720	0.003053	0.711768
-15.783658	-1.934426	0.755725	0.003074	0.711764
-16.036733	-1.947735	0.760730	0.003121	0.711648
-16.761037	-1.912400	0.765734	0.003256	0.711461
-16.703266	-1.928094	0.770739	0.003245	0.711450
-16.719655	-1.920987	0.775744	0.003248	0.711459
-16.579334	-1.947869	0.780749	0.003222	0.711455
-17.190230	-1.839950	0.785754	0.003336	0.711453
-16.918698	-1.884775	0.790758	0.003285	0.711460
-16.739222	-1.921178	0.795763	0.003252	0.711452
-17.266792	-1.977003	0.800768	0.003350	0.711153
-18.147977	-1.827996	0.805773	0.003514	0.711137
-18.015455	-1.852471	0.810778	0.003489	0.711135
-17.165964	-1.999273	0.815782	0.003331	0.711145
-17.773969	-1.895973	0.820787	0.003444	0.711135
-17.759045	-1.894095	0.825792	0.003441	0.711144
-17.285914	-1.979775	0.830797	0.003353	0.711141
-17.931522	-1.967617	0.835802	0.003473	0.710936
-18.560100	-1.885632	0.840806	0.003590	0.710876
-18.280972	-1.939400	0.845811	0.003538	0.710868
-18.184605	-1.953093	0.850816	0.003520	0.710875
-18.574407	-1.884607	0.855821	0.003593	0.710873
-18.654418	-1.871834	0.860826	0.003608	0.710870
-18.129050	-1.962602	0.865830	0.003510	0.710876
-18.935287	-1.983956	0.870835	0.003660	0.710546
-19.133293	-1.954102	0.875840	0.003697	0.710536
-19.091672	-1.961988	0.880845	0.003689	0.710535
-19.029983	-1.974427	0.885850	0.003678	0.710532
-19.309634	-1.920918	0.890854	0.003730	0.710539
-19.008042	-1.978806	0.895859	0.003673	0.710531
-19.065865	-2.050750	0.900864	0.003684	0.710367
-20.428369	-1.881926	0.905869	0.003938	0.710219
-20.360881	-1.896102	0.910874	0.003925	0.710215
-19.819820	-1.988579	0.915878	0.003824	0.710223
-20.445190	-1.881077	0.920883	0.003941	0.710215
-20.328484	-1.898516	0.925888	0.003919	0.710222
-19.993532	-1.960161	0.930893	0.003857	0.710218
-20.375360	-1.952183	0.935898	0.003928	0.710098
-21.277646	-1.889820	0.940902	0.004096	0.709902
-20.966343	-1.950764	0.945907	0.004038	0.709891
-21.102327	-1.922158	0.950912	0.004063	0.709900
-21.177676	-1.909940	0.955917	0.004077	0.709897
-21.343773	-1.883931	0.960922	0.004108	0.709890
-21.073186	-1.925945	0.965926	0.004057	0.709903
-21.220359	-1.903153	0.970931	0.004085	0.709896
-21.702597	-1.961435	0.975936	0.004174	0.709607
-21.782437	-1.949898	0.980941	0.004189	0.709602
-21.993153	-1.916365	0.985946	0.004228	0.709594
-21.814175	-1.942486	0.990950	0.004195	0.709606
-22.001807	-1.913652	0.995955	0.004230	0.709597
-21.768648	-1.953644	1.000960	0.004187	0.709600
-21.772889	-1.990973	1.005965	0.004187	0.709524
-23.156229	-1.875123	1.010970	0.004445	0.709262
-22.311825	-2.019802	1.015974	0.004288	0.709274
-22.986235	-1.905498	1.020979	0.004413	0.709262
-23.179703	-1.868092	1.025984	0.004449	0.709268
-22.765244	-1.943089	1.030989	0.004372	0.709266
-22.914352	-1.917802	1.035994	0.004400	0.709264
-22.936026	-1.911404	1.040998	0.004404	0.709269
-23.683700	-1.934912	1.046003	0.004543	0.708955
-23.716964	-1.925865	1.051008	0.004549	0.708961
-24.085593	-1.861491	1.056013	0.004617	0.708959
-23.902221	-1.897682	1.061018	0.004583	0.708952
-23.535690	-1.959342	1.066022	0.004515	0.708959
-23.688265	-1.935970	1.071027	0.004543	0.708952
-23.734180	-1.924902	1.076032	0.004552	0.708958
-23.833089	-2.023902	1.081037	0.004570	0.708724
-24.784934	-1.898098	1.086042	0.004747	0.708636
-24.745500	-1.902281	1.091046	0.004740	0.708642
-24.672347	-1.918476	1.096051	0.004726	0.708636
-24.721974	-1.906747	1.101056	0.004736	0.708642
-24.442956	-1.957022	1.106061	0.004684	0.708641
-24.822687	-1.892421	1.111066	0.004754	0.708635
-24.662324	-2.016734	1.116070	0.004724	0.708443
-25.487287	-1.917106	1.121075	0.004878	0.708348
-25.670454	-1.881188	1.126080	0.004912	0.708355
-25.171082	-1.971439	1.131085	0.004819	0.708352
-25.432957	-1.925622	1.136090	0.004868	0.708351
-25.360364	-1.936067	1.141094	0.004854	0.708356
-25.544504	-1.907298	1.146099	0.004888	0.708348
-25.847356	-2.013917	1.151104	0.004945	0.708026
-26.022760	-1.987676	1.156109	0.004977	0.708016
-26.784555	-1.854777	1.161114	0.005119	0.708010
-26.067421	-1.979288	1.166118	0.004986	0.708017
-26.208236	-1.958940	1.171123	0.005012	0.708008
-26.595766	-1.887337	1.176128	0.005084	0.708013
-26.109899	-1.997373	1.181133	0.004993	0.707966
-27.036272	-1.965526	1.186138	0.005166	0.707699
-27.151323	-1.942645	1.191142	0.005187	0.707703
-27.680924	-1.852101	1.196147	0.005286	0.707696
-27.253461	-1.926191	1.201152	0.005206	0.707700
-27.106891	-1.952433	1.206157	0.005179	0.707700
-27.735544	-1.842405	1.211162	0.005296	0.707696
-27.171163	-1.938642	1.216166	0.005191	0.707705
-27.649727	-1.995739	1.221171	0.005280	0.707419
-28.430959	-1.878348	1.226176	0.005425	0.707375
-28.375985	-1.885969	1.231181	0.005415	0.707380
-28.146637	-1.929961	1.236186	0.005372	0.707374
-28.290209	-1.898536	1.241190	0.005399	0.707385
-28.578439	-1.852801	1.246195	0.005452	0.707374
-28.155319	-1.926586	1.251200	0.005374	0.707378
-28.024478	-2.013613	1.256205	0.005349	0.707250
-29.561013	-1.824689	1.261210	0.005635	0.707079
-28.931935	-1.931184	1.266214	0.005518	0.707091
-29.027190	-1.920309	1.271219	0.005536	0.707079
-29.077651	-1.908205	1.276224	0.005545	0.707085
-28.831170	-1.953073	1.281229	0.005499	0.707083
-29.078284	-1.911319	1.286234	0.005545	0.707079
-29.136803	-1.972611	1.291238	0.005556	0.706935
-30.385070	-1.841826	1.296243	0.005788	0.706751
-29.847696	-1.936293	1.301248	0.005688	0.706753
-29.724746	-1.957277	1.306253	0.005665	0.706755
-30.426253	-1.834213	1.311258	0.005796	0.706751
-29.905151	-1.925042	1.316262	0.005699	0.706756
-29.949752	-1.918957	1.321267	0.005707	0.706752
-30.230178	-1.888244	1.326272	0.005759	0.706713
-30.677357	-1.942369	1.331277	0.005843	0.706444
-30.611286	-1.956787	1.336282	0.005830	0.706439
-30.505530	-1.970745	1.341286	0.005811	0.706449
-30.911967	-1.902413	1.346291	0.005886	0.706441
-31.025023	-1.879774	1.351296	0.005907	0.706446
-30.508695	-1.971774	1.356301	0.005811	0.706446
-30.845962	-1.977291	1.361306	0.005874	0.706314
-31.775036	-1.901564	1.366310	0.006047	0.706134
-31.644528	-1.929954	1.371315	0.006022	0.706123
-31.707042	-1.916985	1.376320	0.006034	0.706127
-31.746650	-1.909653	1.381325	0.006041	0.706128
-31.882057	-1.889514	1.386330	0.006066	0.706120
-31.711759	-1.914592	1.391334	0.006035	0.706131
-31.971128	-1.886604	1.396339	0.006083	0.706094
-32.274889	-1.948821	1.401344	0.006140	0.705860
-32.012160	-1.995035	1.406349	0.006091	0.705861
-32.730486	-1.869546	1.411354	0.006224	0.705856
-32.383629	-1.925712	1.416358	0.006160	0.705868
-32.142347	-1.972838	1.421363	0.006115	0.705860
-32.441408	-1.918362	1.426368	0.006170	0.705862
-32.784930	-1.972559	1.431373	0.006234	0.705630
-33.588130	-1.885002	1.436378	0.006384	0.705518
-32.781620	-2.025402	1.441382	0.006234	0.705525
-33.342931	-1.927589	1.446387	0.006338	0.705520
-33.684683	-1.866083	1.451392	0.006402	0.705522
-33.159728	-1.959356	1.456397	0.006304	0.705522
-33.222957	-1.951847	1.461402	0.006316	0.705515
-33.820099	-1.990122	1.466406	0.006427	0.705224
-34.239836	-1.925298	1.471411	0.006505	0.705204
-34.329280	-1.907453	1.476416	0.006521	0.705208
-34.104972	-1.946045	1.481421	0.006480	0.705210
-34.325206	-1.909188	1.486426	0.006521	0.705206
-34.130641	-1.938833	1.491430	0.006484	0.705216
-34.156120	-1.954491	1.496435	0.006489	0.705175
-34.979542	-1.950839	1.501440	0.006642	0.704887
-34.794968	-1.983705	1.506445	0.006608	0.704887
-35.291253	-1.898214	1.511450	0.006700	0.704881
-35.067330	-1.934530	1.516454	0.006659	0.704889
-35.051684	-1.942396	1.521459	0.006656	0.704879
-35.086098	-1.932192	1.526464	0.006662	0.704887
-35.273664	-1.921152	1.531469	0.006697	0.704842
-36.017186	-1.916292	1.536474	0.006835	0.704585
-35.440476	-2.017172	1.541478	0.006728	0.704589
-35.939617	-1.930587	1.546483	0.006821	0.704584
-36.215552	-1.877714	1.551488	0.006872	0.704591
-35.774289	-1.955569	1.556493	0.006790	0.704593
-36.010735	-1.916321	1.561498	0.006834	0.704587
-35.835138	-2.000263	1.566502	0.006801	0.704481
-36.765105	-1.944555	1.571507	0.006974	0.704259
-36.491021	-1.992297	1.576512	0.006923	0.704262
-36.784778	-1.938144	1.581517	0.006978	0.704265
-37.111360	-1.885573	1.586522	0.007039	0.704254
-36.419464	-2.004901	1.591526	0.006910	0.704262
-36.953427	-1.912414	1.596531	0.007009	0.704257
-37.329105	-1.914034	1.601536	0.007079	0.704119
-37.763164	-1.918156	1.606541	0.007160	0.703954
-37.675733	-1.937692	1.611546	0.007143	0.703947
-37.974771	-1.879540	1.616550	0.007199	0.703956
-38.050869	-1.869688	1.621555	0.007213	0.703949
-37.698771	-1.932889	1.626560	0.007148	0.703948
-37.929941	-1.888888	1.631565	0.007191	0.703954
-38.435027	-1.803133	1.636570	0.007285	0.703945
-37.667276	-2.048661	1.641574	0.007142	0.703726
-38.546271	-1.941497	1.646579	0.007305	0.703626
-39.082164	-1.842162	1.651584	0.007405	0.703634
-38.543531	-1.937963	1.656589	0.007305	0.703635
-38.547260	-1.939233	1.661594	0.007305	0.703631
-38.527054	-1.938349	1.666598	0.007301	0.703640
-38.722059	-1.907914	1.671603	0.007338	0.703631
-38.814986	-2.020589	1.676608	0.007355	0.703370
-39.167960	-1.970531	1.681613	0.007421	0.703345
-39.912055	-1.842194	1.686618	0.007559	0.703336
-39.188140	-1.968171	1.691622	0.007424	0.703342
-39.154767	-1.977408	1.696627	0.007418	0.703336
-39.655968	-1.886191	1.701632	0.007511	0.703339
-39.162334	-2.026086	1.706637	0.007420	0.703235
-40.361398	-1.928943	1.711642	0.007643	0.702999
-40.389064	-1.920108	1.716646	0.007648	0.703007
-40.827182	-1.847209	1.721651	0.007729	0.702997
-40.338161	-1.931117	1.726656	0.007638	0.703004
-40.287433	-1.937805	1.731661	0.007629	0.703008
-40.904904	-1.831382	1.736666	0.007744	0.703001
-40.229037	-1.951541	1.741670	0.007618	0.703002
-40.445943	-2.068334	1.746675	0.007658	0.702688
-41.231547	-1.926752	1.751680	0.007804	0.702691
-41.656871	-1.850646	1.756685	0.007883	0.702692
-41.041254	-1.964314	1.761690	0.007769	0.702684
-41.060275	-1.955283	1.766694	0.007772	0.702695
-41.703752	-1.845803	1.771699	0.007892	0.702685
-41.524486	-1.874715	1.776704	0.007859	0.702691
-41.531033	-2.029830	1.781709	0.007860	0.702375
-42.273268	-1.904280	1.786714	0.007998	0.702362
-42.105277	-1.929524	1.791718	0.007967	0.702371
-42.034201	-1.945402	1.796723	0.007953	0.702365
-42.398506	-1.880290	1.801728	0.008021	0.702365
-42.260971	-1.902613	1.806733	0.007996	0.702370
-42.055390	-1.940815	1.811738	0.007957	0.702367
-42.604366	-1.984586	1.816742	0.008059	0.702080
-43.248845	-1.874300	1.821747	0.008179	0.702071
-43.181025	-1.884155	1.826752	0.008167	0.702076
-42.550241	-1.997982	1.831757	0.008049	0.702073
-43.404022	-1.849256	1.836762	0.008208	0.702066
-43.254972	-1.871781	1.841766	0.008180	0.702074
-42.946274	-1.929566	1.846771	0.008123	0.702069
-43.575216	-1.957933	1.851776	0.008240	0.701785
-44.082842	-1.888361	1.856781	0.008334	0.701742
-43.896895	-1.924026	1.861786	0.008300	0.701737
-43.442072	-2.000846	1.866790	0.008215	0.701746
-44.068034	-1.891504	1.871795	0.008332	0.701741
-44.007498	-1.902183	1.876800	0.008320	0.701742
-43.563581	-1.979335	1.881805	0.008238	0.701746
-44.805663	-1.911176	1.886810	0.008469	0.701436
-45.042542	-1.865081	1.891814	0.008513	0.701444
-44.861272	-1.902572	1.896819	0.008479	0.701433
-44.723409	-1.927965	1.901824	0.008453	0.701432
-44.695844	-1.929874	1.906829	0.008448	0.701438
-44.881504	-1.899235	1.911834	0.008483	0.701433
-44.421095	-1.976747	1.916838	0.008397	0.701442
-45.105289	-1.994703	1.921843	0.008524	0.701159
-45.881365	-1.874886	1.926848	0.008669	0.701121
-45.383407	-1.961680	1.931853	0.008576	0.701125
-45.733980	-1.902711	1.936858	0.008641	0.701118
-45.850741	-1.878846	1.941862	0.008663	0.701125
-45.469475	-1.949108	1.946867	0.008592	0.701120
-45.507166	-1.943197	1.951872	0.008599	0.701119
-46.257337	-1.928630	1.956877	0.008739	0.700877
-46.540448	-1.882806	1.961882	0.008791	0.700868
-46.001943	-1.974868	1.966886	0.008691	0.700876
-46.022382	-1.974575	1.971891	0.008695	0.700869
-46.419478	-1.901991	1.976896	0.008769	0.700873
-46.104097	-1.954881	1.981901	0.008710	0.700880
-46.364047	-2.020181	1.986906	0.008758	0.700653
-47.541399	-1.867598	1.991910	0.008977	0.700537
-47.161823	-1.938099	1.996915	0.008907	0.700532
-47.210779	-1.927395	2.001920	0.008916	0.700536

-47.184705	-1.932354	2.011917	0.008911	0.700535
-47.390885	-1.896936	2.021914	0.008949	0.700533
-47.771916	-1.969244	2.031910	0.009020	0.700248
-48.013559	-1.940294	2.041907	0.009065	0.700220
-47.960431	-1.949461	2.051904	0.009055	0.700221
-47.997978	-1.942496	2.061901	0.009062	0.700221
-47.525799	-1.928505	2.071898	0.008974	0.700421
-47.368353	-1.902386	2.081894	0.008944	0.700531
-47.169335	-1.936297	2.091891	0.008907	0.700534
-47.131488	-1.941775	2.101888	0.008900	0.700537
-47.135037	-1.942646	2.111885	0.008901	0.700534
-47.219329	-1.928194	2.121882	0.008916	0.700533
-46.927905	-1.978661	2.131878	0.008862	0.700536
-47.247959	-1.922049	2.141875	0.008921	0.700535
-47.157948	-1.939181	2.151872	0.008905	0.700533
-46.579615	-1.895056	2.161869	0.008797	0.700832
-46.439763	-1.901021	2.171866	0.008771	0.700871
-46.327194	-1.921404	2.181862	0.008750	0.700870
-46.334536	-1.917936	2.191859	0.008751	0.700875
-45.969294	-1.933116	2.201856	0.008683	0.700976
-45.451623	-1.952473	2.211853	0.008586	0.701124
-45.869949	-1.879035	2.221850	0.008664	0.701122
-45.595241	-1.927443	2.231846	0.008613	0.701123
-45.339954	-1.879695	2.241843	0.008565	0.701312
-44.715222	-1.927717	2.251840	0.008449	0.701441
-44.891153	-1.899010	2.261837	0.008482	0.701435
-44.810316	-1.899451	2.271834	0.008466	0.701464
-44.044056	-1.899054	2.281830	0.008324	0.701741
-43.849652	-1.931827	2.291827	0.008287	0.701745
-43.860400	-1.929603	2.301824	0.008289	0.701746
-43.589965	-1.887093	2.311821	0.008239	0.701930
-43.010126	-1.920981	2.321818	0.008131	0.702071
-43.102578	-1.903299	2.331814	0.008148	0.702073
-43.116051	-1.891624	2.341811	0.008150	0.702092
-42.213169	-1.913597	2.351808	0.007982	0.702373
-42.317108	-1.895645	2.361805	0.008002	0.702372
-42.265759	-1.906386	2.371802	0.007992	0.702369
-41.906086	-1.872317	2.381798	0.007925	0.702568
-41.323013	-1.915916	2.391795	0.007816	0.702690
-41.426468	-1.895846	2.401792	0.007835	0.702693
-41.557343	-1.839597	2.411789	0.007860	0.702760
-40.678330	-1.875395	2.421786	0.007696	0.703005
-40.509189	-1.904121	2.431782	0.007664	0.703008
-40.703479	-1.870718	2.441779	0.007700	0.703005
-39.671671	-1.900924	2.451776	0.007508	0.703316
-39.779613	-1.869253	2.461773	0.007528	0.703341
-39.520492	-1.918202	2.471770	0.007480	0.703336
-39.794089	-1.813943	2.481766	0.007531	0.703448
-38.512609	-1.951266	2.491763	0.007292	0.703632
-38.792914	-1.899780	2.501760	0.007344	0.703635
-38.892036	-1.883657	2.511757	0.007363	0.703632
-38.192759	-1.864383	2.521754	0.007232	0.703923
-37.867494	-1.910634	2.531750	0.007172	0.703947
-37.763223	-1.929535	2.541747	0.007152	0.703946
-37.638665	-1.886641	2.551744	0.007129	0.704078
-36.955430	-1.917792	2.561741	0.007002	0.704261
-37.131581	-1.887977	2.571738	0.007034	0.704258
-37.034882	-1.904752	2.581734	0.007016	0.704259
-36.229431	-1.904422	2.591731	0.006866	0.704549
-36.228636	-1.882690	2.601728	0.006866	0.704593
-36.097887	-1.908288	2.611725	0.006841	0.704589
-36.005246	-1.874653	2.621722	0.006824	0.704690
-35.314871	-1.899811	2.631718	0.006695	0.704887
-35.106093	-1.938001	2.641715	0.006657	0.704885
-35.222916	-1.916283	2.651712	0.006678	0.704887
-34.446076	-1.929537	2.661709	0.006534	0.705140
-34.485336	-1.887369	2.671706	0.006541	0.705211
-34.513141	-1.881442	2.681702	0.006546	0.705213
-34.295587	-1.863854	2.691699	0.006505	0.705326
-33.491245	-1.908493	2.701696	0.006355	0.705525
-33.503185	-1.906520	2.711693	0.006358	0.705525
-33.478300	-1.912704	2.721690	0.006353	0.705522
-32.953918	-1.861598	2.731686	0.006255	0.705813
-32.357338	-1.943040	2.741683	0.006144	0.705863
-32.657382	-1.889709	2.751680	0.006200	0.705863
-32.341528	-1.922699	2.761677	0.006141	0.705910
-31.958140	-1.884509	2.771674	0.006069	0.706124
-31.800825	-1.912591	2.781670	0.006040	0.706124
-31.949030	-1.885511	2.791667	0.006067	0.706126
-31.254254	-1.863712	2.801664	0.005938	0.706419
-31.079423	-1.882393	2.811661	0.005905	0.706444
-30.988421	-1.899899	2.821658	0.005888	0.706442
-30.748033	-1.850331	2.831654	0.005843	0.706628
-29.826265	-1.954453	2.841651	0.005672	0.706749
-30.167179	-1.892673	2.851648	0.005735	0.706751
-29.828200	-1.941891	2.861645	0.005672	0.706773
-29.363524	-1.871456	2.871642	0.005585	0.707081
-29.225580	-1.896278	2.881638	0.005560	0.707081
-28.972655	-1.939960	2.891635	0.005512	0.707084
-28.933177	-1.867808	2.901632	0.005505	0.707243
-28.292926	-1.914834	2.911629	0.005386	0.707378
-28.514170	-1.877424	2.921626	0.005427	0.707374
-28.277583	-1.892332	2.931622	0.005383	0.707429
-27.298606	-1.931027	2.941619	0.005200	0.707701
-27.579926	-1.881936	2.951616	0.005253	0.707700
-27.360177	-1.920208	2.961613	0.005212	0.707701
-27.117024	-1.857784	2.971610	0.005166	0.707914
-26.371233	-1.942105	2.981606	0.005027	0.708011
-26.441817	-1.928238	2.991603	0.005040	0.708014
-26.617823	-1.881703	3.001600	0.005073	0.708045
-25.762840	-1.881241	3.011597	0.004914	0.708351
-25.513788	-1.927463	3.021594	0.004867	0.708348
-25.505473	-1.928672	3.031590	0.004866	0.708348
-25.284267	-1.896952	3.041587	0.004824	0.708491
-24.678806	-1.931830	3.051584	0.004712	0.708637
-24.640881	-1.938784	3.061581	0.004705	0.708637
-25.067743	-1.862315	3.071578	0.004784	0.708638
-24.103718	-1.877711	3.081574	0.004604	0.708952
-24.173911	-1.863015	3.091571	0.004617	0.708956
-23.849062	-1.920638	3.101568	0.004557	0.708957
-23.446486	-1.889627	3.111565	0.004482	0.709163
-23.298106	-1.865501	3.121562	0.004454	0.709264
-22.843495	-1.947030	3.131558	0.004369	0.709263
-23.059198	-1.876835	3.141555	0.004409	0.709327
-22.145057	-1.905094	3.151552	0.004239	0.709596
-22.207272	-1.895217	3.161549	0.004251	0.709594
-22.301912	-1.878077	3.171546	0.004268	0.709595
-21.636274	-1.892832	3.181542	0.004144	0.709803
-21.406778	-1.888468	3.191539	0.004101	0.709893
-21.278112	-1.909795	3.201536	0.004077	0.709897
-21.343383	-1.860751	3.211533	0.004089	0.709972
-20.382564	-1.910256	3.221530	0.003910	0.710215
-20.340645	-1.919955	3.231526	0.003902	0.710211
-20.545776	-1.882616	3.241523	0.003941	0.710212
-19.760697	-1.912376	3.251520	0.003794	0.710433
-19.502999	-1.910685	3.261517	0.003746	0.710528
-19.422969	-1.924046	3.271514	0.003731	0.710530
-19.438863	-1.916792	3.281510	0.003734	0.710539
-19.037570	-1.821893	3.291507	0.003659	0.710871
-18.344883	-1.945292	3.301504	0.003530	0.710872
-18.688038	-1.884963	3.311501	0.003594	0.710870
-18.308057	-1.883105	3.321498	0.003523	0.711009
-17.765110	-1.916264	3.331494	0.003422	0.711136
-18.008025	-1.870235	3.341491	0.003467	0.711142
-17.577869	-1.933102	3.351488	0.003387	0.711170
-17.343933	-1.832359	3.361485	0.003343	0.711454
-16.990791	-1.894894	3.371482	0.003278	0.711455
-16.907776	-1.911058	3.381478	0.003262	0.711452
-16.448758	-1.874311	3.391475	0.003176	0.711689
-16.152750	-1.891780	3.401472	0.003121	0.711759
-16.393739	-1.847662	3.411469	0.003166	0.711762
-15.924583	-1.855247	3.421466	0.003079	0.711913
-15.201780	-1.897618	3.431462	0.002944	0.712086
-15.250076	-1.886227	3.441459	0.002953	0.712092
-15.099860	-1.912248	3.451456	0.002925	0.712093
-14.777525	-1.831179	3.461453	0.002865	0.712369
-14.447294	-1.882487	3.471450	0.002803	0.712384
-14.387917	-1.892517	3.481446	0.002792	0.712386
-14.092007	-1.853893	3.491443	0.002737	0.712568
-13.516763	-1.884839	3.501440	0.002630	0.712710
-13.507161	-1.886785	3.511437	0.002628	0.712710
-13.382334	-1.899173	3.521434	0.002604	0.712730
-13.055562	-1.811419	3.531430	0.002543	0.713021
-12.567498	-1.897555	3.541427	0.002453	0.713022
-12.615820	-1.890044	3.551424	0.002461	0.713020
-12.222991	-1.840278	3.561421	0.002388	0.713259
-11.543608	-1.911429	3.571418	0.002262	0.713358
-11.992043	-1.830587	3.581414	0.002345	0.713360
-11.710996	-1.855239	3.591411	0.002293	0.713411
-11.273847	-1.810115	3.601408	0.002211	0.713656
-10.894015	-1.878339	3.611405	0.002140	0.713655
-11.077780	-1.846815	3.621402	0.002174	0.713653
-10.433204	-1.817644	3.631398	0.002054	0.713939
-10.218638	-1.839197	3.641395	0.002014	0.713972
-9.873393	-1.901218	3.651392	0.001950	0.713971
-9.908182	-1.828395	3.661389	0.001956	0.714104
-8.856008	-1.930565	3.671386	0.001760	0.714273
-9.424352	-1.827971	3.681382	0.001866	0.714276
-8.964944	-1.909031	3.691379	0.001781	0.714278
-8.745218	-1.816980	3.701376	0.001739	0.714539
-8.314978	-1.858559	3.711373	0.001659	0.714609
-8.378209	-1.847726	3.721370	0.001671	0.714608
-8.135388	-1.836661	3.731366	0.001626	0.714716
-6.898421	-1.960050	3.741363	0.001395	0.714908
-7.099551	-1.923272	3.751360	0.001433	0.714910
-6.989882	-1.944227	3.761357	0.001412	0.714908
-7.005990	-1.886141	3.771354	0.001415	0.715018
-6.293107	-1.905441	3.781350	0.001282	0.715231
-5.988838	-1.959211	3.791347	0.001226	0.715232
-6.340221	-1.897519	3.801344	0.001291	0.715231
-5.822230	-1.910281	3.811341	0.001194	0.715389
-5.177104	-1.945789	3.821338	0.001074	0.715546
-5.039402	-1.971225	3.831334	0.001048	0.715545
-5.200532	-1.941850	3.841331	0.001078	0.715546
-4.824605	-1.921144	3.851328	0.001008	0.715720
-4.012280	-1.982531	3.861325	0.000857	0.715885
-4.257096	-1.939707	3.871322	0.000902	0.715884
-4.290701	-1.934193	3.881318	0.000909	0.715883
-3.741630	-1.955842	3.891315	0.000806	0.716034
-3.466775	-1.954822	3.901312	0.000755	0.716133
-3.412195	-1.964583	3.911309	0.000745	0.716133
-3.596517	-1.927724	3.921306	0.000779	0.716142
-2.936438	-1.892832	3.931302	0.000656	0.716444
-2.547424	-1.960785	3.941299	0.000584	0.716447
-2.678075	-1.935340	3.951296	0.000608	0.716451
-2.197452	-1.918041	3.961293	0.000518	0.716655
-1.753218	-1.947145	3.971290	0.000435	0.716754
-1.590526	-1.976479	3.981286	0.000405	0.716753
-1.930819	-1.890314	3.991283	0.000468	0.716804
-1.145862	-1.889010	4.001280	0.000322	0.717084
-0.912431	-1.931497	4.011277	0.000279	0.717082
-1.055903	-1.905703	4.021274	0.000305	0.717083
-0.864602	-1.807646	4.031270	0.000269	0.717344
-1.203595	-1.730625	4.041267	0.000332	0.717377
-0.962044	-1.717959	4.051264	0.000287	0.717487
-0.918221	-1.617164	4.061261	0.000279	0.717702
-0.940075	-1.593935	4.071258	0.000283	0.717741
-0.425535	-1.548264	4.081254	0.000187	0.718012
-0.656695	-1.500128	4.091251	0.000230	0.718026
-0.552816	-1.353477	4.101248	0.000210	0.718352
-0.821785	-1.272087	4.111245	0.000260	0.718419
-0.554976	-1.205600	4.121242	0.000211	0.718644
-0.472497	-1.129215	4.131238	0.000195	0.718824
-0.349098	-1.082119	4.141235	0.000172	0.718960
-0.108623	-0.969445	4.151232	0.000127	0.719267
-0.323308	-0.854880	4.161229	0.000167	0.719418
-0.216593	-0.774823	4.171226	0.000147	0.719613
-0.213473	-0.631316	4.181222	0.000146	0.719897
-0.290660	-0.500152	4.191219	0.000160	0.720129
-0.168561	-0.400074	4.201216	0.000137	0.720369
0.002374	-0.305238	4.211213	0.000106	0.720616
0.034958	-0.174640	4.221210	0.000099	0.720884
-0.058345	-0.039333	4.231206	0.000116	0.721118
0.059903	0.088227	4.241203	0.000094	0.721410
0.000000	0.265955	4.251200	0.000105	0.721739

0.072890	0.899544	4.256205	0.000091	0.723009
0.341411	2.115672	4.261210	0.000040	0.725484
0.672302	3.914391	4.266214	-0.000022	0.729107
0.823077	6.292745	4.271219	-0.000052	0.733772
1.280369	9.132569	4.276224	-0.000139	0.739397
1.233193	12.536391	4.281229	-0.000133	0.745883
1.605594	16.320082	4.286234	-0.000204	0.753168
2.032466	20.501712	4.291238	-0.000287	0.761144
2.301888	25.102855	4.296243	-0.000340	0.769759
2.743641	30.049967	4.301248	-0.000425	0.778964
3.236096	35.331208	4.306253	-0.000521	0.788679
3.795692	40.922915	4.311258	-0.000628	0.798848
5.181796	46.675778	4.316262	-0.000890	0.809428
5.962852	52.828288	4.321267	-0.001040	0.820377
6.620453	59.291728	4.326272	-0.001167	0.831674
7.096861	65.997514	4.331277	-0.001260	0.843173
8.097314	72.841637	4.336282	-0.001450	0.854900
8.706635	79.963011	4.341286	-0.001569	0.866809
10.881932	86.997468	4.346291	-0.001978	0.878861
13.659056	94.160062	4.351296	-0.002500	0.891120
13.979337	101.910439	4.356301	-0.002565	0.903457
14.505766	109.767369	4.361306	-0.002668	0.915849
15.373312	117.682602	4.366310	-0.002835	0.928255
15.929676	125.758541	4.371315	-0.002944	0.940657
17.829832	133.742378	4.376320	-0.003303	0.953110
18.413201	142.014205	4.381325	-0.003417	0.965487
19.886240	150.216845	4.386330	-0.003696	0.977831
20.929517	158.591796	4.391334	-0.003896	0.990160
21.437882	167.088760	4.396339	-0.003996	1.002377
22.215726	175.583978	4.401344	-0.004147	1.014510
23.165579	184.079144	4.406349	-0.004329	1.026541
24.026318	192.641541	4.411354	-0.004495	1.038502
24.875422	201.228191	4.416358	-0.004659	1.050356
25.262674	209.906132	4.421363	-0.004737	1.062093
26.201120	218.526818	4.426368	-0.004917	1.073752
26.832412	227.176185	4.431373	-0.005040	1.085253
27.672432	235.818030	4.436378	-0.005202	1.096670
28.720697	244.427839	4.441382	-0.005403	1.107973
29.361863	253.104716	4.446387	-0.005528	1.119158
29.902421	261.806125	4.451392	-0.005635	1.130241
30.814031	270.432165	4.456397	-0.005810	1.141202
31.640724	279.099027	4.461402	-0.005970	1.152090
32.503187	287.721787	4.466406	-0.006136	1.162830
33.295934	296.330416	4.471411	-0.006289	1.173439
34.274607	304.906177	4.476416	-0.006477	1.183952
35.144577	313.505451	4.481421	-0.006645	1.194377
35.718089	322.125487	4.486426	-0.006757	1.204677
36.528894	330.718747	4.491430	-0.006914	1.214905
37.247570	339.287792	4.496435	-0.007053	1.225001
38.041136	347.871758	4.501440	-0.007207	1.235046
38.775759	356.401823	4.506445	-0.007349	1.244937
39.408368	364.955325	4.511450	-0.007472	1.254756
40.125256	373.475362	4.516454	-0.007611	1.264477
40.276891	382.076350	4.521459	-0.007645	1.274108
40.882256	390.572380	4.526464	-0.007764	1.283635
41.524280	399.066868	4.531469	-0.007889	1.293097
41.902187	407.573354	4.536474	-0.007965	1.302454
42.337024	416.149369	4.541478	-0.008051	1.311830
43.198266	424.572036	4.546483	-0.008217	1.321051
43.948827	432.972863	4.551488	-0.008362	1.330165
44.091872	441.457962	4.556493	-0.008395	1.339198
44.365332	449.886846	4.561498	-0.008451	1.348134
45.040681	458.269134	4.566502	-0.008582	1.357033
45.532116	466.625536	4.571507	-0.008679	1.365815
46.309130	474.976027	4.576512	-0.008830	1.374583
47.175476	483.289450	4.581517	-0.008996	1.383273
47.582205	491.699413	4.586522	-0.009078	1.391929
48.032617	500.066000	4.591526	-0.009167	1.400495
48.373479	508.429434	4.596531	-0.009236	1.408986
49.168268	516.734160	4.601536	-0.009389	1.417444
49.814080	525.041892	4.606541	-0.009515	1.425829
50.342666	533.385845	4.611546	-0.009619	1.434181
50.878384	541.702437	4.616550	-0.009724	1.442460
50.926405	550.083329	4.621555	-0.009739	1.450675
51.583669	558.367847	4.626560	-0.009866	1.458848
52.161761	566.647807	4.631565	-0.009979	1.466957
52.686940	574.991897	4.636570	-0.010083	1.475076
53.219411	583.263052	4.641574	-0.010187	1.483081
53.485923	591.561728	4.646579	-0.010242	1.491028
54.271934	599.796105	4.651584	-0.010394	1.498952
54.609328	608.079933	4.656589	-0.010462	1.506811
55.200861	616.344230	4.661594	-0.010578	1.514650
55.882426	624.580293	4.666598	-0.010710	1.522436
56.316306	632.846252	4.671603	-0.010797	1.530173
56.903334	641.099277	4.676608	-0.010911	1.537881
57.338633	649.350635	4.681613	-0.010998	1.545527
57.769243	657.625380	4.686618	-0.011083	1.553155
58.194298	665.865750	4.691622	-0.011168	1.560714
58.647481	674.087308	4.696627	-0.011258	1.568224
59.289795	682.313836	4.701632	-0.011383	1.575729
59.668107	690.548277	4.706637	-0.011458	1.583168
60.030464	698.791034	4.711642	-0.011531	1.590577
60.570526	707.009965	4.716646	-0.011637	1.597955
60.759358	715.240806	4.721651	-0.011678	1.605260
61.154108	723.480299	4.726656	-0.011757	1.612569
61.528083	731.689054	4.731661	-0.011832	1.619815
61.768118	739.919345	4.736666	-0.011882	1.627028
62.285406	748.176049	4.741670	-0.011984	1.634271
62.877959	756.312897	4.746675	-0.012099	1.641388
63.046944	764.542189	4.751680	-0.012136	1.648496
63.680373	772.708121	4.756685	-0.012260	1.655583
63.694546	780.931807	4.761690	-0.012268	1.662604
64.195077	789.114751	4.766694	-0.012366	1.669627
64.350245	797.324667	4.771699	-0.012400	1.676597
64.750614	805.488366	4.776704	-0.012480	1.683531
65.160322	813.656206	4.781709	-0.012562	1.690442
65.710057	821.819356	4.786714	-0.012670	1.697339
66.228777	829.979329	4.791718	-0.012772	1.704201
66.560746	838.175987	4.796723	-0.012839	1.711042
67.303208	846.326262	4.801728	-0.012982	1.717870
67.576101	854.488521	4.806733	-0.013039	1.724620
67.683576	862.711340	4.811738	-0.013064	1.731372
68.304065	870.856075	4.816742	-0.013185	1.738099
68.600570	879.014331	4.821747	-0.013245	1.744771
68.943598	887.204208	4.826752	-0.013315	1.751448
69.311034	895.366863	4.831757	-0.013389	1.758081
69.616207	903.515012	4.836762	-0.013451	1.764669
70.246419	911.656975	4.841766	-0.013573	1.771268
70.593518	919.810116	4.846771	-0.013643	1.777817
71.252268	927.923617	4.851776	-0.013771	1.784348
71.660021	936.105294	4.856781	-0.013853	1.790878
72.059087	944.287894	4.861786	-0.013932	1.797384
72.358281	952.437862	4.866790	-0.013993	1.803829
72.807323	960.554009	4.871795	-0.014082	1.810243
73.289680	968.699060	4.876800	-0.014177	1.816660
73.823543	976.808570	4.881805	-0.014282	1.823033
74.416391	984.933065	4.886810	-0.014398	1.829402
74.695300	993.114916	4.891814	-0.014455	1.835756
74.880923	1001.256056	4.896819	-0.014495	1.842045
75.524465	1009.373102	4.901824	-0.014620	1.848349
75.588249	1017.582371	4.906829	-0.014638	1.854633
76.134582	1025.671447	4.911834	-0.014745	1.860861
76.753487	1033.789410	4.916838	-0.014865	1.867098
77.199264	1041.938608	4.921843	-0.014954	1.873318
77.459117	1050.093304	4.926848	-0.015007	1.879500
77.916368	1058.186420	4.931853	-0.015098	1.885638
78.191860	1066.337942	4.936858	-0.015154	1.891779
78.426713	1074.491002	4.941862	-0.015203	1.897897
78.498488	1082.627309	4.946867	-0.015222	1.903964
78.913318	1090.751811	4.951872	-0.015305	1.910041
79.164195	1098.900124	4.956877	-0.015357	1.916099
79.499306	1106.990309	4.961882	-0.015425	1.922103
80.112672	1115.079866	4.966886	-0.015544	1.928120
80.531155	1123.197734	4.971891	-0.015627	1.934116
80.868734	1131.333244	4.976896	-0.015696	1.940098
80.880076	1139.491911	4.981901	-0.015703	1.946043
81.556400	1147.600949	4.986906	-0.015834	1.952006
81.910855	1155.735258	4.991910	-0.015906	1.957934
82.024761	1163.848033	4.996915	-0.015932	1.963802
82.874129	1171.875472	5.001920	-0.016096	1.969671
83.020261	1180.028652	5.006925	-0.016128	1.975536
82.947758	1188.182645	5.011930	-0.016120	1.981362
83.317970	1196.268821	5.016934	-0.016194	1.987169
83.612784	1204.390192	5.021939	-0.016254	1.992977
84.042989	1212.470883	5.026944	-0.016340	1.998752
84.445758	1220.551535	5.031949	-0.016420	2.004508
84.908265	1228.634281	5.036954	-0.016512	2.010255
85.405061	1236.757722	5.041958	-0.016609	2.016018
85.555338	1244.868162	5.046963	-0.016643	2.021719
85.996578	1252.962295	5.051968	-0.016730	2.027423
86.494536	1261.086942	5.056973	-0.016828	2.033138
86.526636	1269.211209	5.061978	-0.016840	2.038788
86.836478	1277.312744	5.066982	-0.016903	2.044436
87.088313	1285.395034	5.071987	-0.016955	2.050049
87.729571	1293.474150	5.076992	-0.017079	2.055683
87.782970	1301.606054	5.081997	-0.017095	2.061279
88.220553	1309.674564	5.087002	-0.017182	2.066855
88.858257	1317.771912	5.092006	-0.017306	2.072456
89.130321	1325.866124	5.097011	-0.017362	2.078002
89.475993	1333.959070	5.102016	-0.017431	2.083541
89.727291	1342.065664	5.107021	-0.017483	2.089064
89.884872	1350.192511	5.112026	-0.017518	2.094577
90.350161	1358.266424	5.117030	-0.017610	2.100070
90.599901	1366.352178	5.122035	-0.017662	2.105536
90.867765	1374.499380	5.127040	-0.017717	2.111031
91.026246	1382.642265	5.132045	-0.017752	2.116497
91.506291	1390.669394	5.137050	-0.017847	2.121903
91.972209	1398.733960	5.142054	-0.017939	2.127319
92.035645	1406.846262	5.147059	-0.017956	2.132715
92.155496	1414.959277	5.152064	-0.017983	2.138102
92.470870	1423.026284	5.157069	-0.018047	2.143464
92.917383	1431.099707	5.162074	-0.018136	2.148829
93.314239	1439.202425	5.167078	-0.018215	2.154196
93.801791	1447.227420	5.172083	-0.018311	2.159506
94.281198	1455.292576	5.177088	-0.018406	2.164829
94.513055	1463.403630	5.182093	-0.018454	2.170145
94.816895	1471.506045	5.187098	-0.018516	2.175449
95.411135	1479.558366	5.192102	-0.018632	2.180735
95.625532	1487.648369	5.197107	-0.018677	2.185997
95.981987	1495.759679	5.202112	-0.018749	2.191274
96.277517	1503.872776	5.207117	-0.018809	2.196533
96.329775	1511.956341	5.212122	-0.018824	2.201738
96.600544	1520.025837	5.217126	-0.018880	2.206942
96.929523	1528.092237	5.222131	-0.018947	2.212137
97.277711	1536.181266	5.227136	-0.019017	2.217336
97.493888	1544.264192	5.232141	-0.019062	2.222507
97.830063	1552.320034	5.237146	-0.019130	2.227659
98.164327	1560.425845	5.242150	-0.019198	2.232831
98.439727	1568.491276	5.247155	-0.019254	2.237960
98.802509	1576.557525	5.252160	-0.019327	2.243085
99.256356	1584.616401	5.257165	-0.019417	2.248202
99.459345	1592.711505	5.262170	-0.019460	2.253308
99.822171	1600.787700	5.267174	-0.019533	2.258405
100.063291	1608.851106	5.272179	-0.019583	2.263471
100.454378	1616.938750	5.277184	-0.019661	2.268554
100.488710	1625.143900	5.282189	-0.019673	2.273668
100.828390	1633.160140	5.287194	-0.019742	2.278680
101.321034	1641.178445	5.292198	-0.019839	2.283694
101.540634	1649.239501	5.297203	-0.019885	2.288701
101.582896	1657.372154	5.302208	-0.019898	2.293726
101.810577	1665.426163	5.307213	-0.019946	2.298707
102.630729	1673.393329	5.312218	-0.020104	2.303674
103.000337	1681.487172	5.317222	-0.020178	2.308670
103.131204	1689.587332	5.322227	-0.020207	2.313639
103.584645	1697.640694	5.327232	-0.020297	2.318595
103.790982	1705.713039	5.332237	-0.020341	2.323532
103.964370	1713.779189	5.337242	-0.020378	2.328452
104.371423	1721.876556	5.342246	-0.020460	2.333399
104.785866	1729.917368	5.347251	-0.020542	2.338303
105.021763	1737.992862	5.352256	-0.020591	2.343202
105.186522	1746.078487	5.357261	-0.020627	2.348092
105.266450	1754.205814	5.362266	-0.020647	2.352989
105.556572	1762.269949	5.367270	-0.020707	2.357855
105.787254	1770.306562	5.372275	-0.020755	2.362690
106.330579	1778.339880	5.377280	-0.020861	2.367538
106.592241	1786.417730	5.382285	-0.020915	2.372380
106.654218	1794.492139	5.387290	-0.020932	2.377194
107.106075	1802.543277	5.392294	-0.021022	2.382016
107.466908	1810.576872	5.397299	-0.021094	2.386810
107.680021	1818.681736	5.402304	-0.021139	2.391625
107.965045	1826.755924	5.407309	-0.021198	2.396418
108.102075	1834.807382	5.412314	-0.021228	2.401176
108.374345	1842.872832	5.417318	-0.021284	2.405943
108.573237	1850.931501	5.422323	-0.021327	2.410692
109.102432	1858.987929	5.427328	-0.021431	2.415455
109.158632	1867.083003	5.432333	-0.021446	2.420195
109.378234	1875.120971	5.437338	-0.021492	2.424904
109.900518	1883.179752	5.442342	-0.021595	2.429640
110.061212	1891.339961	5.447347	-0.021630	2.434398
110.265832	1899.373160	5.452352	-0.021674	2.439076
110.630895	1907.394062	5.457357	-0.021747	2.443750
110.844454	1915.436966	5.462362	-0.021792	2.448417
111.101492	1923.535416	5.467366	-0.021845	2.453110
111.100676	1931.595443	5.472371	-0.021850	2.457752
111.268299	1939.648952	5.477376	-0.021887	2.462394
111.561194	1947.672817	5.482381	-0.021947	2.467020
111.860599	1955.745738	5.487386	-0.022008	2.471666
112.238947	1963.814474	5.492390	-0.022083	2.476307
112.537221	1971.841644	5.497395	-0.022144	2.480909
112.863947	1979.883790	5.502400	-0.022210	2.485513
113.096402	1987.958512	5.507405	-0.022259	2.490120
113.432144	1996.006883	5.512410	-0.022327	2.494711
113.916136	2004.042309	5.517414	-0.022422	2.499298
114.037989	2012.111087	5.522419	-0.022450	2.503868
114.537289	2020.162935	5.527424	-0.022548	2.508447
114.542649	2028.303375	5.532429	-0.022555	2.513033
114.929488	2036.322691	5.537434	-0.022632	2.517569
115.171563	2044.381142	5.542438	-0.022682	2.522109
115.360845	2052.421429	5.547443	-0.022723	2.526626
115.699725	2060.467996	5.552448	-0.022791	2.531150
115.821206	2068.575697	5.557453	-0.022819	2.535684
116.002591	2076.596977	5.562458	-0.022858	2.540166
116.268352	2084.643152	5.567462	-0.022913	2.544660
116.568218	2092.698544	5.572467	-0.022974	2.549154
117.041434	2100.777350	5.577472	-0.023068	2.553664
117.506150	2108.796133	5.582477	-0.023159	2.558133
117.575151	2116.849036	5.587482	-0.023177	2.562585
117.967842	2124.902871	5.592486	-0.023256	2.567053
118.311332	2132.961011	5.597491	-0.023325	2.571511
118.356429	2141.054444	5.602496	-0.023339	2.575961
118.780001	2149.076707	5.607501	-0.023423	2.580390
119.006092	2157.113275	5.612506	-0.023470	2.584805
119.322657	2165.195552	5.617510	-0.023535	2.589244
119.550782	2173.422096	5.622515	-0.023583	2.593748
119.871817	2181.435764	5.627520	-0.023648	2.598135
120.135730	2189.422609	5.632525	-0.023702	2.602495
120.242001	2197.429705	5.637530	-0.023727	2.606849
120.538982	2205.485924	5.642534	-0.023788	2.611235
120.688771	2213.529684	5.647539	-0.023821	2.615596
121.026612	2221.524889	5.652544	-0.023889	2.619937
121.184275	2229.583396	5.657549	-0.023924	2.624293
121.285533	2237.645825	5.662554	-0.023948	2.628640
121.625367	2245.711410	5.667558	-0.024016	2.632997
121.816776	2253.739262	5.672563	-0.024057	2.637317
122.281890	2261.741766	5.677568	-0.024149	2.641634
122.705889	2269.780225	5.682573	-0.024233	2.645960
122.778317	2277.853561	5.687578	-0.024252	2.650275
123.196839	2285.922644	5.692582	-0.024335	2.654603
123.453728	2293.951221	5.697587	-0.024388	2.658892
123.549833	2302.022543	5.702592	-0.024412	2.663187
123.752515	2310.078067	5.707597	-0.024455	2.667472
124.192681	2318.127222	5.712602	-0.024542	2.671763
124.732402	2326.191085	5.717606	-0.024648	2.676061
124.690317	2334.230468	5.722611	-0.024645	2.680302
125.059391	2342.228046	5.727616	-0.024719	2.684541
125.344757	2350.294327	5.732621	-0.024778	2.688803
125.464474	2358.359673	5.737626	-0.024805	2.693048
125.531742	2366.451290	5.742630	-0.024823	2.697296
126.138497	2374.416238	5.747635	-0.024941	2.701506
126.161012	2382.494608	5.752640	-0.024951	2.705731
126.292588	2390.562377	5.757645	-0.024980	2.709951
126.668128	2398.606409	5.762650	-0.025056	2.714167
127.352691	2406.586618	5.767654	-0.025188	2.718363
127.432679	2414.651694	5.772659	-0.025209	2.722559
127.557444	2422.696831	5.777664	-0.025237	2.726740
127.988381	2430.748144	5.782669	-0.025323	2.730937
128.277745	2438.798704	5.787674	-0.025382	2.735119
128.413101	2446.860653	5.792678	-0.025412	2.739291
128.590847	2454.911177	5.797683	-0.025451	2.743453
128.880733	2462.958359	5.802688	-0.025510	2.747613
129.219357	2471.048024	5.807693	-0.025578	2.751792
129.419876	2479.141493	5.812698	-0.025621	2.755959
129.682435	2487.163226	5.817702	-0.025675	2.760086
129.959799	2495.139214	5.822707	-0.025732	2.764184
129.971163	2503.207286	5.827712	-0.025739	2.768307
130.458910	2511.247599	5.832717	-0.025835	2.772439
130.600036	2519.285471	5.837722	-0.025867	2.776542
130.744448	2527.338623	5.842726	-0.025899	2.780647
130.997987	2535.343701	5.847731	-0.025952	2.784728
131.462939	2543.369989	5.852736	-0.026044	2.788826
131.450299	2551.484726	5.857741	-0.026046	2.792935
131.663180	2559.489536	5.862746	-0.026091	2.796996
132.121890	2567.506147	5.867750	-0.026182	2.801070
132.092837	2575.561246	5.872755	-0.026182	2.805130
132.407118	2583.584726	5.877760	-0.026246	2.809188
132.617805	2591.669814	5.882765	-0.026290	2.813265
132.843079	2599.704092	5.887770	-0.026337	2.817312
133.090974	2607.749955	5.892774	-0.026389	2.821359
133.459990	2615.753088	5.897779	-0.026463	2.825387
133.656779	2623.811904	5.902784	-0.026505	2.829426
134.158990	2631.870055	5.907789	-0.026604	2.833477
134.270663	2639.891091	5.912794	-0.026630	2.837481
134.805063	2647.921932	5.917798	-0.026734	2.841509
134.931329	2655.953574	5.922803	-0.026763	2.845508
135.015836	2664.011392	5.927808	-0.026784	2.849512
135.639236	2672.029753	5.932813	-0.026906	2.853521
135.892700	2680.090134	5.937818	-0.026958	2.857524
136.277629	2688.127556	5.942822	-0.027035	2.861518
136.291628	2696.172569	5.947827	-0.027043	2.865489
136.575402	2704.192127	5.952832	-0.027101	2.869457
137.060124	2712.269617	5.957837	-0.027197	2.873459
137.026486	2720.306034	5.962842	-0.027196	2.877407
137.409836	2728.334271	5.967846	-0.027272	2.881368
137.683958	2736.371929	5.972851	-0.027329	2.885322
137.564025	2744.448674	5.977856	-0.027312	2.889269
138.022901	2752.481678	5.982861	-0.027402	2.893220
138.203539	2760.499176	5.987866	-0.027441	2.897143
138.489883	2768.551835	5.992870	-0.027500	2.901084
138.739240	2776.558080	5.997875	-0.027552	2.904994
139.023384	2784.599052	6.002880	-0.027610	2.908918
139.248078	2792.754124	6.007885	-0.027657	2.912889
139.407299	2800.775566	6.012890	-0.027692	2.916787
139.655952	2808.818019	6.017894	-0.027743	2.920693
139.537406	2816.797886	6.022899	-0.027727	2.924545
139.942517	2824.806650	6.027904	-0.027807	2.928434
140.286079	2832.873819	6.032909	-0.027877	2.932342
140.420930	2840.907864	6.037914	-0.027907	2.936218
140.383203	2848.974626	6.042918	-0.027905	2.940095
140.571028	2856.959886	6.047923	-0.027945	2.943940
141.012949	2864.986770	6.052928	-0.028033	2.947814
141.363415	2873.053914	6.057933	-0.028104	2.951696
141.663913	2881.096782	6.062938	-0.028165	2.955559
141.962102	2889.103510	6.067942	-0.028226	2.959400
142.170445	2897.132437	6.072947	-0.028270	2.963242
142.287971	2905.187555	6.077952	-0.028297	2.967086
142.478218	2913.259180	6.082957	-0.028337	2.970937
142.680706	2921.295379	6.087962	-0.028380	2.974767
142.972121	2929.328600	6.092966	-0.028440	2.978595
143.312460	2937.324923	6.097971	-0.028509	2.982403
143.424308	2945.381706	6.102976	-0.028535	2.986223
143.714099	2953.429967	6.107981	-0.028594	2.990043
143.855637	2961.499771	6.112986	-0.028626	2.993861
144.142043	2969.497061	6.117990	-0.028684	2.997647
144.519668	2977.514215	6.122995	-0.028760	3.001442
144.633401	2985.537675	6.128000	-0.028786	3.005222
144.924218	2993.565962	6.133005	-0.028846	3.009008
145.152860	3001.603730	6.138010	-0.028894	3.012791
145.203109	3009.692433	6.143014	-0.028908	3.016584
145.281083	3017.711695	6.148019	-0.028928	3.020342
145.731130	3025.696100	6.153024	-0.029017	3.024096
146.058982	3033.764300	6.158029	-0.029083	3.027879
146.074878	3041.817628	6.163034	-0.029092	3.031635
146.217882	3049.887875	6.168038	-0.029124	3.035401
146.794886	3057.845982	6.173043	-0.029236	3.039130
147.126167	3065.859106	6.178048	-0.029303	3.042869
147.483251	3073.940192	6.183053	-0.029375	3.046636
147.849138	3081.957761	6.188058	-0.029448	3.050369
148.122122	3090.036081	6.193062	-0.029504	3.054121
148.177603	3098.067086	6.198067	-0.029520	3.057836
148.474243	3106.070989	6.203072	-0.029581	3.061545
148.866433	3114.110883	6.208077	-0.029659	3.065271
148.899424	3122.145235	6.213082	-0.029670	3.068974
149.222182	3130.243296	6.218086	-0.029736	3.072714
149.306040	3138.317916	6.223091	-0.029757	3.076428
149.445286	3146.293931	6.228096	-0.029788	3.080095
149.705249	3154.308865	6.233101	-0.029841	3.083781
149.750114	3162.319125	6.238106	-0.029855	3.087450
150.213003	3170.358219	6.243110	-0.029947	3.091147
150.347846	3178.409463	6.248115	-0.029977	3.094831
150.620050	3186.426428	6.253120	-0.030033	3.098500
151.054619	3194.435371	6.258125	-0.030119	3.102169
150.967122	3202.496722	6.263130	-0.030108	3.105834
151.151602	3210.527988	6.268134	-0.030148	3.109493
151.573147	3218.564422	6.273139	-0.030231	3.113161
151.687533	3226.610839	6.278144	-0.030258	3.116815
152.110660	3234.618139	6.283149	-0.030342	3.120460
152.500805	3242.576153	6.288154	-0.030420	3.124078
152.935856	3250.653214	6.293158	-0.030506	3.127747
153.062356	3258.700577	6.298163	-0.030535	3.131385
153.189387	3266.768404	6.303168	-0.030564	3.135028
153.454791	3274.804315	6.308173	-0.030619	3.138658
153.661453	3282.808214	6.313178	-0.030663	3.142267
153.866296	3290.856370	6.318182	-0.030706	3.145892
154.118837	3298.866091	6.323187	-0.030758	3.149497
154.336743	3306.965867	6.328192	-0.030804	3.153137
154.305675	3315.016352	6.333197	-0.030804	3.156740
154.705828	3322.981690	6.338202	-0.030883	3.160319
154.933770	3331.005852	6.343206	-0.030931	3.163913
154.904441	3339.042479	6.348211	-0.030931	3.167498
155.285473	3347.077966	6.353216	-0.031007	3.171095
155.711094	3355.136017	6.358221	-0.031092	3.174701
155.778137	3363.134703	6.363226	-0.031109	3.178260
155.623634	3371.204479	6.368230	-0.031086	3.181837
155.981070	3379.181362	6.373235	-0.031158	3.185391
156.303769	3387.202383	6.378240	-0.031223	3.188960
156.804393	3395.261433	6.383245	-0.031322	3.192548
156.780817	3403.311948	6.388250	-0.031322	3.196107
157.120057	3411.334089	6.393254	-0.031391	3.199664
157.153722	3419.348315	6.398259	-0.031402	3.203201
157.125375	3427.403525	6.403264	-0.031402	3.206749
157.541757	3435.432703	6.408269	-0.031485	3.210301
157.624037	3443.475509	6.413274	-0.031506	3.213840
157.687011	3451.532604	6.418278	-0.031523	3.217382
157.929009	3459.530529	6.423283	-0.031573	3.220901
158.034846	3467.545816	6.428288	-0.031598	3.224417
158.583466	3475.563449	6.433293	-0.031706	3.227950
158.484459	3483.627037	6.438298	-0.031692	3.231472
158.926218	3491.692618	6.443302	-0.031780	3.235013
159.090662	3499.699974	6.448307	-0.031816	3.238513
159.459513	3507.679198	6.453312	-0.031890	3.242006
159.601773	3515.714741	6.458317	-0.031922	3.245510
159.709369	3523.717715	6.463322	-0.031947	3.248994
159.928707	3531.775124	6.468326	-0.031993	3.252504
160.317391	3539.809931	6.473331	-0.032071	3.256006
160.498273	3547.821504	6.478336	-0.032110	3.259486
160.764207	3555.855582	6.483341	-0.032164	3.262975
160.821163	3563.880673	6.488346	-0.032180	3.266449
161.346100	3571.909241	6.493350	-0.032283	3.269939
161.607844	3579.969160	6.498355	-0.032337	3.273428
161.633941	3588.012129	6.503360	-0.032347	3.276897
161.984765	3596.018250	6.508365	-0.032418	3.280359
162.221410	3603.996143	6.513370	-0.032467	3.283800
162.345430	3612.082085	6.518374	-0.032496	3.287281
162.358789	3620.115329	6.523379	-0.032504	3.290730
162.769646	3628.114012	6.528384	-0.032585	3.294176
162.959719	3636.175342	6.533389	-0.032626	3.297637
162.927306	3644.206029	6.538394	-0.032625	3.301073
163.450095	3652.189661	6.543398	-0.032728	3.304507
163.463409	3660.239674	6.548403	-0.032736	3.307945
163.574176	3668.313576	6.553408	-0.032761	3.311394
163.769640	3676.380382	6.558413	-0.032803	3.314839
164.010397	3684.351160	6.563418	-0.032853	3.318242
164.139577	3692.381223	6.568422	-0.032883	3.321662
164.298592	3700.364070	6.573427	-0.032917	3.325060
164.751260	3708.370560	6.578432	-0.033007	3.328475
165.112840	3716.447268	6.583437	-0.033080	3.331913
164.881157	3724.498141	6.588442	-0.033042	3.335314
165.276465	3732.523043	6.593446	-0.033121	3.338725
165.394588	3740.538377	6.598451	-0.033148	3.342117
165.523071	3748.546963	6.603456	-0.033177	3.345503
166.028111	3756.590306	6.608461	-0.033276	3.348915
166.045372	3764.631688	6.613466	-0.033285	3.352304
166.382275	3772.696657	6.618470	-0.033353	3.355711
166.611079	3780.691660	6.623475	-0.033401	3.359082
166.817239	3788.707908	6.628480	-0.033444	3.362457
167.184761	3796.737082	6.633485	-0.033518	3.365840
167.087569	3804.768839	6.638490	-0.033505	3.369204
167.355472	3812.828123	6.643494	-0.033560	3.372589
167.791044	3820.846270	6.648499	-0.033647	3.375960
167.936412	3828.843506	6.653504	-0.033679	3.379308
168.329520	3836.860653	6.658509	-0.033758	3.382670
168.435048	3844.878103	6.663514	-0.033783	3.386018
168.594338	3852.924491	6.668518	-0.033817	3.389377
168.653582	3861.051890	6.673523	-0.033834	3.392763
168.950990	3869.090832	6.678528	-0.033894	3.396117
169.453161	3877.007192	6.683533	-0.033993	3.399424
169.543766	3885.029129	6.688538	-0.034015	3.402757
169.783493	3893.051059	6.693542	-0.034065	3.406091
170.084267	3901.044976	6.698547	-0.034126	3.409414
170.317708	3909.099978	6.703552	-0.034175	3.412755
170.700197	3917.138556	6.708557	-0.034252	3.416092
170.966693	3925.116881	6.713562	-0.034307	3.419397
171.216901	3933.179335	6.718566	-0.034358	3.422732
171.264151	3941.192980	6.723571	-0.034373	3.426038
171.630958	3949.228364	6.728576	-0.034446	3.429359
171.924331	3957.286081	6.733581	-0.034506	3.432685
172.424126	3965.319699	6.738586	-0.034604	3.436004
173.012840	3973.297035	6.743590	-0.034719	3.439299
173.250834	3981.312336	6.748595	-0.034769	3.442596
173.517234	3989.336943	6.753600	-0.034824	3.445893
173.752719	3997.387890	6.758605	-0.034873	3.449198
173.989398	4005.423671	6.763610	-0.034922	3.452493
174.181122	4013.503731	6.768614	-0.034963	3.455801
174.158960	4021.487166	6.773619	-0.034964	3.459060
174.397254	4029.521584	6.778624	-0.035014	3.462345
174.756870	4037.541790	6.783629	-0.035086	3.465625
174.814011	4045.566263	6.788634	-0.035102	3.468893
175.050161	4053.640931	6.793638	-0.035151	3.472185
175.233515	4061.694514	6.798643	-0.035191	3.475464
175.608449	4069.642148	6.803648	-0.035266	3.478702
175.687763	4077.675385	6.808653	-0.035286	3.481963
175.662868	4085.687401	6.813658	-0.035286	3.485208
176.099550	4093.695311	6.818662	-0.035373	3.488464
176.378161	4101.768093	6.823667	-0.035430	3.491738
176.355300	4109.790210	6.828672	-0.035431	3.494978
176.998355	4117.777133	6.833677	-0.035556	3.498223
177.001313	4125.825430	6.838682	-0.035562	3.501469
177.422254	4133.798389	6.843686	-0.035646	3.504694
177.802561	4141.850320	6.848691	-0.035722	3.507947
177.562892	4149.952327	6.853696	-0.035682	3.511198
177.808112	4157.938896	6.858701	-0.035733	3.514415
177.943539	4165.954560	6.863706	-0.035764	3.517637
178.134424	4173.993644	6.868710	-0.035805	3.520867
178.495971	4181.971038	6.873715	-0.035877	3.524074
178.767861	4189.991576	6.878720	-0.035933	3.527294
179.055118	4198.067604	6.883725	-0.035992	3.530532
179.251225	4206.089312	6.888730	-0.036034	3.533744
179.444897	4214.140506	6.893734	-0.036075	3.536964
179.678516	4222.118591	6.898739	-0.036124	3.540153
179.895068	4230.148378	6.903744	-0.036169	3.543359
180.076322	4238.210945	6.908749	-0.036208	3.546574
180.242916	4246.206632	6.913754	-0.036245	3.549760
180.628480	4254.309559	6.918758	-0.036322	3.552991
180.589156	4262.387177	6.923763	-0.036320	3.556197
180.747155	4270.308605	6.928768	-0.036354	3.559344
180.903373	4278.357041	6.933773	-0.036389	3.562539
181.163287	4286.322296	6.938778	-0.036442	3.565700
181.345194	4294.347863	6.943782	-0.036482	3.568881
181.741751	4302.386240	6.948787	-0.036561	3.572070
181.991228	4310.403222	6.953792	-0.036612	3.575243
182.065092	4318.455324	6.958797	-0.036631	3.578422
182.203287	4326.428329	6.963802	-0.036662	3.581569
182.519228	4334.445452	6.968806	-0.036727	3.584736
182.647541	4342.502470	6.973811	-0.036756	3.587910
182.682152	4350.530565	6.978816	-0.036767	3.591067
182.995992	4358.567873	6.983821	-0.036831	3.594233
183.076376	4366.568725	6.988826	-0.036851	3.597375
183.404933	4374.577930	6.993830	-0.036918	3.600525
183.540126	4382.604152	6.998835	-0.036948	3.603673
183.808495	4390.619979	7.003840	-0.037003	3.606818
183.987486	4398.662868	7.008845	-0.037042	3.609969
184.168690	4406.664753	7.013850	-0.037081	3.613101
184.595546	4414.733091	7.018854	-0.037166	3.616262
184.720544	4422.704273	7.023859	-0.037194	3.619375
184.943328	4430.716372	7.028864	-0.037241	3.622503
185.158289	4438.781776	7.033869	-0.037286	3.625650
185.154131	4446.808609	7.038874	-0.037291	3.628772
185.504188	4454.887550	7.043878	-0.037361	3.631922
185.586490	4462.927963	7.048883	-0.037382	3.635047
185.846681	4470.900209	7.053888	-0.037436	3.638147
185.973506	4478.925667	7.058893	-0.037465	3.641262
186.132806	4486.860676	7.063898	-0.037499	3.644340
186.535501	4494.949543	7.068902	-0.037580	3.647482
186.676588	4502.972252	7.073907	-0.037611	3.650588
186.477318	4511.017877	7.078912	-0.037579	3.653691
186.972282	4519.054448	7.083917	-0.037677	3.656806
187.183343	4527.036439	7.088922	-0.037721	3.659891
187.346574	4535.083620	7.093926	-0.037757	3.662996
187.748452	4543.110212	7.098931	-0.037837	3.666097
187.935744	4551.105490	7.103936	-0.037877	3.669178
188.201614	4559.198986	7.108941	-0.037932	3.672296
188.146073	4567.216946	7.113946	-0.037927	3.675374
188.325126	4575.223482	7.118950	-0.037966	3.678451
188.608023	4583.242920	7.123955	-0.038024	3.681533
188.770699	4591.194043	7.128960	-0.038059	3.684583
188.862246	4599.272415	7.133965	-0.038082	3.687678
189.029666	4607.286458	7.138970	-0.038118	3.690747
189.548232	4615.324167	7.143974	-0.038220	3.693832
189.632260	4623.346661	7.148979	-0.038241	3.696897
189.892415	4631.329117	7.153984	-0.038294	3.699948
190.114885	4639.374826	7.158989	-0.038341	3.703021
190.053202	4647.414662	7.163994	-0.038335	3.706081
190.435609	4655.424088	7.168998	-0.038411	3.709139
190.621104	4663.487543	7.174003	-0.038451	3.712209
190.754628	4671.575094	7.179008	-0.038481	3.715285
191.023274	4679.511794	7.184013	-0.038537	3.718304
191.189329	4687.519293	7.189018	-0.038573	3.721345
191.520785	4695.489880	7.194022	-0.038640	3.724374
191.492805	4703.560132	7.199027	-0.038640	3.727429
191.624928	4711.554181	7.204032	-0.038670	3.730457
192.079685	4719.611183	7.209037	-0.038760	3.733514
192.040211	4727.653294	7.214042	-0.038758	3.736551
192.452515	4735.608942	7.219046	-0.038840	3.739563
192.395516	4743.657799	7.224051	-0.038834	3.742597
192.408443	4751.679782	7.229056	-0.038842	3.745620
192.773120	4759.721157	7.234061	-0.038915	3.748656
193.035071	4767.740738	7.239066	-0.038969	3.751679
193.332233	4775.748940	7.244070	-0.039030	3.754696
193.561149	4783.797875	7.249075	-0.039078	3.757725
193.849103	4791.809826	7.254080	-0.039137	3.760738
194.110136	4799.818328	7.259085	-0.039190	3.763747
194.068443	4807.854393	7.264090	-0.039188	3.766757
194.431611	4815.866330	7.269094	-0.039261	3.769765
194.617767	4823.905619	7.274099	-0.039301	3.772776
194.783876	4831.935087	7.279104	-0.039337	3.775781
194.894540	4839.925877	7.284109	-0.039363	3.778768
195.098920	4847.964270	7.289114	-0.039406	3.781772
195.383066	4856.001010	7.294118	-0.039464	3.784775
195.492854	4864.058893	7.299123	-0.039490	3.787780
195.532169	4872.052766	7.304128	-0.039503	3.790757
195.850874	4880.126173	7.309133	-0.039567	3.793767
195.851982	4888.126648	7.314138	-0.039573	3.796741
196.036120	4896.076340	7.319142	-0.039612	3.799697
196.320036	4904.111437	7.324147	-0.039670	3.802685
196.417477	4912.122657	7.329152	-0.039694	3.805658
196.592498	4920.169370	7.334157	-0.039732	3.808643
196.741725	4928.160714	7.339162	-0.039765	3.811605
197.032621	4936.233696	7.344166	-0.039824	3.814598
197.154206	4944.207202	7.349171	-0.039852	3.817548
197.278108	4952.251910	7.354176	-0.039880	3.820522
197.558824	4960.243155	7.359181	-0.039938	3.823477
197.578604	4968.275993	7.364186	-0.039947	3.826440
197.918110	4976.233242	7.369190	-0.040015	3.829379
198.048813	4984.314673	7.374195	-0.040045	3.832358
198.286694	4992.336103	7.379200	-0.040095	3.835314
198.384792	5000.339454	7.384205	-0.040118	3.838258
198.558884	5008.363422	7.389210	-0.040156	3.841209
198.881233	5016.346179	7.394214	-0.040221	3.844146
198.997541	5024.438680	7.399219	-0.040248	3.847117
199.532632	5032.395690	7.404224	-0.040353	3.850044
199.984053	5040.470247	7.409229	-0.040442	3.853010
200.047254	5048.492496	7.414234	-0.040459	3.855947
200.492844	5056.492965	7.419238	-0.040547	3.858882
201.020963	5064.529379	7.424243	-0.040651	3.861828
200.952351	5072.497923	7.429248	-0.040644	3.864736
201.085248	5080.618972	7.434253	-0.040674	3.867701
201.319761	5088.637121	7.439258	-0.040723	3.870629
201.539037	5096.884352	7.444262	-0.040769	3.873637
201.558948	5104.868262	7.449267	-0.040778	3.876544
201.677878	5112.720606	7.454272	-0.040805	3.879402
202.006964	5120.728234	7.459277	-0.040872	3.882318
202.280697	5128.708868	7.464282	-0.040928	3.885222
202.491479	5136.759194	7.469286	-0.040972	3.888147
202.540910	5144.767389	7.474291	-0.040987	3.891052
202.697848	5152.812119	7.479296	-0.041021	3.893970
202.901614	5160.864807	7.484301	-0.041065	3.896889
202.818911	5168.810024	7.489306	-0.041054	3.899762
203.141288	5176.818521	7.494310	-0.041120	3.902663
203.202190	5184.850193	7.499315	-0.041136	3.905566
203.301856	5192.880671	7.504320	-0.041160	3.908466
203.833969	5200.891358	7.509325	-0.041264	3.911366
204.009893	5208.908361	7.514330	-0.041302	3.914259
204.028864	5216.977580	7.519334	-0.041311	3.917165
204.128244	5224.940227	7.524339	-0.041335	3.920033
204.631268	5232.878658	7.529344	-0.041434	3.922897
204.702300	5240.987542	7.534349	-0.041452	3.925812
204.907998	5249.000890	7.539354	-0.041496	3.928694
205.198352	5257.034235	7.544358	-0.041555	3.931581
205.443042	5265.071551	7.549363	-0.041606	3.934468
205.624879	5273.068333	7.554368	-0.041645	3.937336
205.861705	5281.065680	7.559373	-0.041695	3.940204
205.977903	5289.066206	7.564378	-0.041722	3.943068
206.048865	5297.120264	7.569382	-0.041740	3.945949
206.475589	5305.125173	7.574387	-0.041825	3.948816
206.570927	5313.149682	7.579392	-0.041848	3.951682
206.985028	5321.205677	7.584397	-0.041930	3.954563
206.939190	5329.232233	7.589402	-0.041927	3.957424
207.123693	5337.242049	7.594406	-0.041967	3.960280
207.265552	5345.235218	7.599411	-0.041998	3.963128
207.344686	5353.222286	7.604416	-0.042018	3.965970
207.765058	5361.241877	7.609421	-0.042102	3.968828
208.030096	5369.288894	7.614426	-0.042156	3.971690
208.233779	5377.313065	7.619430	-0.042200	3.974541
208.182313	5385.360415	7.624435	-0.042195	3.977395
208.363231	5393.380577	7.629440	-0.042234	3.980240
208.630017	5401.421946	7.634445	-0.042289	3.983092
208.601362	5409.404424	7.639450	-0.042289	3.985917
208.494131	5417.426233	7.644454	-0.042274	3.988752
208.799089	5425.482384	7.649459	-0.042336	3.991604
208.811477	5433.482725	7.654464	-0.042344	3.994429
209.217553	5441.518492	7.659469	-0.042425	3.997271
209.271255	5449.481472	7.664474	-0.042440	4.000080
209.498713	5457.513086	7.669478	-0.042488	4.002914
209.785788	5465.551345	7.674483	-0.042546	4.005749
210.047685	5473.545084	7.679488	-0.042600	4.008566
210.202000	5481.647089	7.684493	-0.042635	4.011418
210.423454	5489.646164	7.689498	-0.042681	4.014232
210.613981	5497.675453	7.694502	-0.042722	4.017054
210.762562	5505.686521	7.699507	-0.042755	4.019867
210.798555	5513.693981	7.704512	-0.042767	4.022676
211.151687	5521.721666	7.709517	-0.042838	4.025494
211.196906	5529.698119	7.714522	-0.042851	4.028287
211.506369	5537.747190	7.719526	-0.042914	4.031108
211.696253	5545.881352	7.724531	-0.042955	4.033955
211.859551	5553.864282	7.729536	-0.042991	4.036747
212.012016	5561.843440	7.734541	-0.043024	4.039535
212.123759	5569.840661	7.739546	-0.043050	4.042327
212.384707	5577.821000	7.744550	-0.043104	4.045114
212.622999	5585.859903	7.749555	-0.043154	4.047918
212.688316	5593.842709	7.754560	-0.043171	4.050699
213.029564	5601.927176	7.759565	-0.043240	4.053517
213.257080	5609.938631	7.764570	-0.043288	4.056305
213.403603	5617.908732	7.769574	-0.043320	4.059077
213.460258	5625.941131	7.774579	-0.043336	4.061867
213.599421	5633.903682	7.779584	-0.043367	4.064631
213.955558	5641.993435	7.784589	-0.043439	4.067442
213.922394	5650.006563	7.789594	-0.043438	4.070218
214.325592	5658.048943	7.794598	-0.043518	4.073008
214.648520	5666.053322	7.799603	-0.043584	4.075782
214.699752	5674.018214	7.804608	-0.043598	4.078537
214.813322	5682.107136	7.809613	-0.043625	4.081334
214.968511	5690.048968	7.814618	-0.043659	4.084078
215.278332	5698.070639	7.819622	-0.043722	4.086851
215.123371	5706.098997	7.824627	-0.043698	4.089617
215.423030	5714.134849	7.829632	-0.043759	4.092390
215.674344	5722.188147	7.834637	-0.043811	4.095167
215.839865	5730.172307	7.839642	-0.043848	4.097917
216.098673	5738.172833	7.844646	-0.043901	4.100672
216.356941	5746.170695	7.849651	-0.043954	4.103424
216.401632	5754.193119	7.854656	-0.043968	4.106180
216.743032	5762.271551	7.859661	-0.044037	4.108957
216.830220	5770.300565	7.864666	-0.044058	4.111712
217.045964	5778.352037	7.869670	-0.044104	4.114474
217.386128	5786.349649	7.874675	-0.044172	4.117218
217.668814	5794.301963	7.879680	-0.044230	4.119943
217.866467	5802.342253	7.884685	-0.044272	4.122696
217.636636	5810.354428	7.889690	-0.044235	4.125432
217.966069	5818.371439	7.894694	-0.044301	4.128174
218.440234	5826.422498	7.899699	-0.044395	4.130928
218.354624	5834.457329	7.904704	-0.044384	4.133668
218.439878	5842.529774	7.909709	-0.044405	4.136421
218.520353	5850.493221	7.914714	-0.044426	4.139135
218.931164	5858.516192	7.919718	-0.044507	4.141872
218.923193	5866.517287	7.924723	-0.044511	4.144594
219.136142	5874.536054	7.929728	-0.044556	4.147323
219.470941	5882.569708	7.934733	-0.044624	4.150056
219.340551	5890.621367	7.939738	-0.044605	4.152789
219.457353	5898.662337	7.944742	-0.044632	4.155519
219.847292	5906.645804	7.949747	-0.044710	4.158230
219.818674	5914.632431	7.954752	-0.044710	4.160937
220.148459	5922.638761	7.959757	-0.044776	4.163652
220.242010	5930.668630	7.964762	-0.044799	4.166370
220.401357	5938.672944	7.969766	-0.044834	4.169079
220.434843	5946.708012	7.974771	-0.044845	4.171795
220.684158	5954.733741	7.979776	-0.044897	4.174509
221.057702	5962.790290	7.984781	-0.044972	4.177233
220.868110	5970.750467	7.989786	-0.044942	4.179916
220.831694	5978.771812	7.994790	-0.044940	4.182619
221.250161	5986.763124	7.999795	-0.045023	4.185316
221.422691	5994.795563	8.004800	-0.045061	4.188022
221.470328	6002.829871	8.009805	-0.045075	4.190726
221.634425	6010.936259	8.014810	-0.045111	4.193453
221.851684	6018.973813	8.019814	-0.045157	4.196156
222.031339	6026.871819	8.024819	-0.045195	4.198810
222.131402	6034.912343	8.029824	-0.045219	4.201510
222.613542	6042.885629	8.034829	-0.045314	4.204189
222.628955	6050.919685	8.039834	-0.045322	4.206881
222.730817	6058.925467	8.044838	-0.045347	4.209564
222.866745	6066.981080	8.049843	-0.045377	4.212262
223.055916	6075.004822	8.054848	-0.045418	4.214947
223.273293	6083.016097	8.059853	-0.045463	4.217628
223.320128	6091.002165	8.064858	-0.045477	4.220296
223.568986	6098.971380	8.069862	-0.045529	4.222959
223.747472	6107.008663	8.074867	-0.045567	4.225643
223.857998	6115.039088	8.079872	-0.045593	4.228321
224.067035	6123.105516	8.084877	-0.045637	4.231011
224.090432	6131.148805	8.089882	-0.045647	4.233690
224.431155	6139.158951	8.094886	-0.045716	4.236359
224.480974	6147.146017	8.099891	-0.045730	4.239016
224.776242	6155.141464	8.104896	-0.045791	4.241676
224.866764	6163.130929	8.109901	-0.045813	4.244331
224.760919	6171.176116	8.114906	-0.045798	4.247000
225.283461	6179.185257	8.119910	-0.045901	4.249662
225.412641	6187.252932	8.124915	-0.045930	4.252338
225.435970	6195.248542	8.129920	-0.045940	4.254987
225.680758	6203.310066	8.134925	-0.045991	4.257659
225.719432	6211.277594	8.139930	-0.046003	4.260296
225.854195	6219.284323	8.144934	-0.046033	4.262945
226.142346	6227.322231	8.149939	-0.046092	4.265604
226.453432	6235.304155	8.154944	-0.046156	4.268243
226.458908	6243.408012	8.159949	-0.046162	4.270918
226.517520	6251.427524	8.164954	-0.046178	4.273563
226.690177	6259.446234	8.169958	-0.046215	4.276208
227.022614	6267.406151	8.174963	-0.046283	4.278834
226.858251	6275.463477	8.179968	-0.046257	4.281485
227.282407	6283.446265	8.184973	-0.046342	4.284115
227.507847	6291.474281	8.189978	-0.046389	4.286757
227.600716	6299.459346	8.194982	-0.046411	4.289382
227.857594	6307.569844	8.199987	-0.046464	4.292048
228.222837	6315.535355	8.204992	-0.046538	4.294666
228.436132	6323.575280	8.209997	-0.046583	4.297305
228.302011	6331.555298	8.215002	-0.046563	4.299920
228.596066	6339.567974	8.220006	-0.046623	4.302547
228.909659	6347.582348	8.225011	-0.046687	4.305174
228.791891	6355.628165	8.230016	-0.046670	4.307806
228.986587	6363.652442	8.235021	-0.046712	4.310431
228.856480	6371.668222	8.240026	-0.046693	4.313050
229.010970	6379.697571	8.245030	-0.046727	4.315674
229.183229	6387.702768	8.250035	-0.046764	4.318288
229.722612	6395.683517	8.255040	-0.046870	4.320895
229.985877	6403.683174	8.260045	-0.046924	4.323505
230.044453	6411.735468	8.265050	-0.046940	4.326130
230.433167	6419.701958	8.270054	-0.047018	4.328726
230.516507	6427.775080	8.275059	-0.047038	4.331354
230.557075	6435.800300	8.280064	-0.047051	4.333964
230.805908	6443.828791	8.285069	-0.047103	4.336576
230.753549	6451.802304	8.290074	-0.047098	4.339165
230.903580	6459.840750	8.295078	-0.047132	4.341776
231.157494	6467.847279	8.300083	-0.047184	4.344375
231.225712	6475.839441	8.305088	-0.047202	4.346967
231.419522	6483.922496	8.310093	-0.047244	4.349588
231.518973	6491.920818	8.315098	-0.047267	4.352179
231.857988	6500.014659	8.320102	-0.047336	4.354801
231.968138	6508.017673	8.325107	-0.047361	4.357390
231.879333	6515.947309	8.330112	-0.047350	4.359953
232.114413	6523.998017	8.335117	-0.047399	4.362555
232.217168	6531.920785	8.340122	-0.047424	4.365114
232.448264	6539.987088	8.345126	-0.047472	4.367719
232.744856	6548.000900	8.350131	-0.047532	4.370305
233.010483	6555.984315	8.355136	-0.047587	4.372880
233.228630	6564.045175	8.360141	-0.047633	4.375477
233.287414	6572.038180	8.365146	-0.047649	4.378051
233.398204	6580.067977	8.370150	-0.047675	4.380635
233.577002	6588.076093	8.375155	-0.047714	4.383211
233.786188	6596.092345	8.380160	-0.047758	4.385788
233.856306	6604.147938	8.385165	-0.047776	4.388376
233.911327	6612.130747	8.390170	-0.047792	4.390938
234.005455	6620.138021	8.395174	-0.047814	4.393507
234.168053	6628.223869	8.400179	-0.047850	4.396100
234.431368	6636.201756	8.405184	-0.047904	4.398658
234.694633	6644.253644	8.410189	-0.047959	4.401238
234.646793	6652.215941	8.415194	-0.047955	4.403786
234.782393	6660.253092	8.420198	-0.047985	4.406357
235.173643	6668.250845	8.425203	-0.048064	4.408915
235.101245	6676.283233	8.430208	-0.048055	4.411481
235.176431	6684.335573	8.435213	-0.048075	4.414052
235.427605	6692.384057	8.440218	-0.048127	4.416622
235.718337	6700.313344	8.445222	-0.048186	4.419152
235.851122	6708.398611	8.450227	-0.048216	4.421729
235.889748	6716.335150	8.455232	-0.048229	4.424257
236.278791	6724.431994	8.460237	-0.048306	4.426837
236.379115	6732.413243	8.465242	-0.048330	4.429377
236.402259	6740.468970	8.470246	-0.048340	4.431938
236.828201	6748.532549	8.475251	-0.048424	4.434503
236.812692	6756.516641	8.480256	-0.048427	4.437038
236.870630	6764.504295	8.485261	-0.048443	4.439574
236.972057	6772.529430	8.490266	-0.048467	4.442120
237.249274	6780.465276	8.495270	-0.048524	4.444638
237.263260	6788.577716	8.500275	-0.048532	4.447208
237.726685	6796.508602	8.505280	-0.048623	4.449722
237.913493	6804.623309	8.510285	-0.048663	4.452291
237.986733	6812.617840	8.515290	-0.048682	4.454820
237.975422	6820.600212	8.520294	-0.048685	4.457344
238.403357	6828.618351	8.525299	-0.048770	4.459879
238.489287	6836.617622	8.530304	-0.048792	4.462405
238.646815	6844.647343	8.535309	-0.048826	4.464940
238.664674	6852.648658	8.540314	-0.048835	4.467464
239.102069	6860.643805	8.545318	-0.048921	4.469985
239.243172	6868.748058	8.550323	-0.048953	4.472539
239.168449	6876.733417	8.555328	-0.048944	4.475053
239.425352	6884.739520	8.560333	-0.048997	4.477574
239.342216	6892.711145	8.565338	-0.048987	4.480081
239.479652	6900.717704	8.570343	-0.049018	4.482598
239.502804	6908.763786	8.575347	-0.049028	4.485126
239.652941	6916.764421	8.580352	-0.049061	4.487639
239.854148	6924.829811	8.585357	-0.049104	4.490170
239.940264	6932.858129	8.590362	-0.049125	4.492688
240.130242	6940.868099	8.595367	-0.049166	4.495200
240.099466	6948.902607	8.600371	-0.049165	4.497717
240.411679	6956.854737	8.605376	-0.049228	4.500207
240.736257	6964.904104	8.610381	-0.049294	4.502727
240.983983	6972.889880	8.615386	-0.049346	4.505225
240.884545	6980.908100	8.620391	-0.049332	4.507731
241.047712	6988.958576	8.625395	-0.049368	4.510247
241.213126	6996.980593	8.630400	-0.049404	4.512752
241.377953	7005.043173	8.635405	-0.049440	4.515268
241.415463	7013.014170	8.640410	-0.049452	4.517754
241.690937	7020.968768	8.645415	-0.049509	4.520234
241.904222	7028.996468	8.650419	-0.049554	4.522736
241.783696	7036.991948	8.655424	-0.049537	4.525225
242.104145	7045.030907	8.660429	-0.049602	4.527727
242.359870	7053.021661	8.665434	-0.049654	4.530213
242.470471	7061.053018	8.670439	-0.049680	4.532710
242.546428	7069.117218	8.675443	-0.049700	4.535215
242.759626	7077.087518	8.680448	-0.049745	4.537690
242.857044	7085.105210	8.685453	-0.049768	4.540178
242.965658	7093.113186	8.690458	-0.049794	4.542662
243.064889	7101.114565	8.695463	-0.049817	4.545143
243.245897	7109.172342	8.700467	-0.049856	4.547639
243.219964	7117.147944	8.705472	-0.049857	4.550109
243.400458	7125.232813	8.710477	-0.049896	4.552611
243.795990	7133.242437	8.715482	-0.049974	4.555089
243.804003	7141.235111	8.720487	-0.049981	4.557560
244.004991	7149.228261	8.725491	-0.050024	4.560030
244.077768	7157.220295	8.730496	-0.050043	4.562498
244.610874	7165.228025	8.735501	-0.050147	4.564970
244.479630	7173.306596	8.740506	-0.050128	4.567461
244.673393	7181.283024	8.745511	-0.050169	4.569920
244.635056	7189.382186	8.750515	-0.050168	4.572416
244.587061	7197.328611	8.755520	-0.050164	4.574863
244.843562	7205.419406	8.760525	-0.050217	4.577353
245.006780	7213.372849	8.765530	-0.050253	4.579800
245.112359	7221.401867	8.770535	-0.050277	4.582269
245.236546	7229.413877	8.775539	-0.050306	4.584731
245.339870	7237.421145	8.780544	-0.050330	4.587190
245.541196	7245.460030	8.785549	-0.050373	4.589657
245.498455	7253.522095	8.790554	-0.050370	4.592131
245.736716	7261.524894	8.795559	-0.050420	4.594585
246.051829	7269.583935	8.800563	-0.050484	4.597054
245.986263	7277.490892	8.805568	-0.050477	4.599476
246.125410	7285.547665	8.810573	-0.050508	4.601943
246.489302	7293.502481	8.815578	-0.050581	4.604376
246.551076	7301.561932	8.820583	-0.050598	4.606841
246.719550	7309.570507	8.825587	-0.050635	4.609289
246.579926	7317.595759	8.830592	-0.050614	4.611740
246.911295	7325.621113	8.835597	-0.050681	4.614190
246.828776	7333.678449	8.840602	-0.050671	4.616649
247.206629	7341.619376	8.845607	-0.050746	4.619070
247.422559	7349.677238	8.850611	-0.050792	4.621527
247.510956	7357.637905	8.855616	-0.050814	4.623952
247.841801	7365.670704	8.860621	-0.050880	4.626398
247.726604	7373.715608	8.865626	-0.050864	4.628846
247.709505	7381.719686	8.870631	-0.050866	4.631280
247.961282	7389.805422	8.875635	-0.050919	4.633738
248.163174	7397.794750	8.880640	-0.050961	4.636166
248.394502	7405.764754	8.885645	-0.051010	4.638586
248.327563	7413.809391	8.890650	-0.051003	4.641028
248.472661	7421.722844	8.895655	-0.051035	4.643428
248.851336	7429.795526	8.900659	-0.051111	4.645875
248.821814	7437.786001	8.905664	-0.051110	4.648297
248.915553	7445.859351	8.910669	-0.051133	4.650742
248.928357	7453.913021	8.915674	-0.051141	4.653180
249.366905	7461.885609	8.920679	-0.051228	4.655592
249.531951	7469.878091	8.925683	-0.051264	4.658008
249.685171	7477.873719	8.930688	-0.051297	4.660425
249.861309	7485.960489	8.935693	-0.051335	4.662867
249.814909	7493.937939	8.940698	-0.051332	4.665276
249.953110	7501.943048	8.945703	-0.051363	4.667692
250.224448	7509.971588	8.950707	-0.051419	4.670113
250.297106	7518.050110	8.955712	-0.051438	4.672548
250.424671	7526.062666	8.960717	-0.051467	4.674962
250.582738	7534.050536	8.965722	-0.051501	4.677367
250.627105	7541.985969	8.970727	-0.051515	4.679755
250.717588	7550.061718	8.975731	-0.051537	4.682185
250.811505	7557.949577	8.980736	-0.051560	4.684556
251.177329	7566.130894	8.985741	-0.051633	4.687014
251.363222	7574.043177	8.990746	-0.051673	4.689390
251.284743	7582.083792	8.995751	-0.051664	4.691804
251.635877	7590.151033	9.000755	-0.051734	4.694224
251.529561	7598.150855	9.005760	-0.051720	4.696623
251.714679	7606.097315	9.010765	-0.051759	4.699005
252.047479	7614.140640	9.015770	-0.051827	4.701414
252.164859	7622.143930	9.020775	-0.051854	4.703810
252.420109	7630.187843	9.025779	-0.051907	4.706217
252.318433	7638.149772	9.030784	-0.051893	4.708598
252.649116	7646.228717	9.035789	-0.051960	4.711013
252.521507	7654.264420	9.040794	-0.051941	4.713414
252.668824	7662.262495	9.045799	-0.051974	4.715803
252.927927	7670.283402	9.050803	-0.052028	4.718196
252.995135	7678.264992	9.055808	-0.052045	4.720577
253.036424	7686.271364	9.060813	-0.052058	4.722965
253.144266	7694.327455	9.065818	-0.052084	4.725366
253.299330	7702.305308	9.070823	-0.052118	4.727742
253.431134	7710.341564	9.075827	-0.052148	4.730134
253.568786	7718.398793	9.080832	-0.052178	4.732532
253.739731	7726.442642	9.085837	-0.052216	4.734924
253.769977	7734.437774	9.090842	-0.052226	4.737300
253.952369	7742.392230	9.095847	-0.052266	4.739663
254.135590	7750.431705	9.100851	-0.052305	4.742051
254.305408	7758.453077	9.105856	-0.052342	4.744431
254.408909	7766.469425	9.110861	-0.052366	4.746809
254.649531	7774.471318	9.115866	-0.052417	4.749181
254.929722	7782.470373	9.120871	-0.052474	4.751551
254.995149	7790.563891	9.125875	-0.052491	4.753948
254.858902	7798.574849	9.130880	-0.052471	4.756321
255.286058	7806.501339	9.135885	-0.052556	4.758665
255.366004	7814.593559	9.140890	-0.052576	4.761059
255.294338	7822.498997	9.145895	-0.052568	4.763396
255.595940	7830.593563	9.150899	-0.052630	4.765787
255.618833	7838.593704	9.155904	-0.052639	4.768150
255.771822	7846.580426	9.160909	-0.052673	4.770507
256.159496	7854.641901	9.165914	-0.052750	4.772884
256.175210	7862.627541	9.170919	-0.052759	4.775239
256.322039	7870.667599	9.175923	-0.052791	4.777608
256.421542	7878.598722	9.180928	-0.052815	4.779944
256.647591	7886.707288	9.185933	-0.052862	4.782331
256.869501	7894.666093	9.190938	-0.052909	4.784672
256.990784	7902.721963	9.195943	-0.052937	4.787042
257.106917	7910.737199	9.200947	-0.052964	4.789398
257.168640	7918.766280	9.205952	-0.052980	4.791757
257.198351	7926.802074	9.210957	-0.052991	4.794117
257.352539	7934.797943	9.215962	-0.053025	4.796464
257.670144	7942.758731	9.220967	-0.053090	4.798799
257.903091	7950.827651	9.225971	-0.053138	4.801164
257.847078	7958.797154	9.230976	-0.053133	4.803501
258.252996	7966.780886	9.235981	-0.053214	4.805838
258.345859	7974.842657	9.240986	-0.053236	4.808199
258.410134	7982.831168	9.245991	-0.053254	4.810537
258.457814	7990.381455	9.250995	-0.053267	4.812746
258.763011	7994.926325	9.256000	-0.053327	4.814074

258.860613	7997.502148	9.261005	-0.053347	4.814826
258.806779	7998.823251	9.266010	-0.053338	4.815213
259.070597	7999.292087	9.271015	-0.053388	4.815349
259.115830	8000.288153	9.276019	-0.053397	4.815640
258.918641	8000.239014	9.281024	-0.053360	4.815626
259.147217	8000.214982	9.286029	-0.053403	4.815618
259.274300	8000.258711	9.291034	-0.053426	4.815630
259.210090	8000.218151	9.296039	-0.053414	4.815619
259.508590	8000.291380	9.301043	-0.053470	4.815639
259.470861	8000.289699	9.306048	-0.053463	4.815638
259.476821	8000.320772	9.311053	-0.053464	4.815647
259.578639	8000.329914	9.316058	-0.053483	4.815650
259.648750	8000.258439	9.321063	-0.053496	4.815628
259.622181	8000.331700	9.326067	-0.053491	4.815650
259.466847	8000.285380	9.331072	-0.053462	4.815637
259.677116	8000.267457	9.336077	-0.053502	4.815631
259.657115	8000.298106	9.341082	-0.053498	4.815640
259.725909	8000.251173	9.346087	-0.053511	4.815626
259.469242	8000.338833	9.351091	-0.053463	4.815653
259.791828	8000.304589	9.356096	-0.053523	4.815641
259.752872	8000.324248	9.361101	-0.053516	4.815647
259.649243	8000.340715	9.366106	-0.053497	4.815652
259.805374	8000.266373	9.371111	-0.053526	4.815630
259.869038	8000.278096	9.376115	-0.053538	4.815633
259.754215	8000.266613	9.381120	-0.053516	4.815630
259.752211	8000.275127	9.386125	-0.053516	4.815633
259.810460	8000.254722	9.391130	-0.053527	4.815626
259.789987	8000.225556	9.396135	-0.053523	4.815618
259.862655	8000.306846	9.401139	-0.053537	4.815641
259.927475	8000.302568	9.406144	-0.053549	4.815640
260.034341	8000.224217	9.411149	-0.053569	4.815616
259.932673	8000.286640	9.416154	-0.053550	4.815635
260.109822	8000.277789	9.421159	-0.053583	4.815632
260.144875	8000.320018	9.426163	-0.053589	4.815644
259.985383	8000.264016	9.431168	-0.053560	4.815628
260.118117	8000.220264	9.436173	-0.053585	4.815615
260.106622	8000.230759	9.441178	-0.053582	4.815618
259.983529	8000.224481	9.446183	-0.053560	4.815617
260.013968	8000.252749	9.451187	-0.053565	4.815625
260.146155	8000.252776	9.456192	-0.053590	4.815624
260.031392	8000.246633	9.461197	-0.053569	4.815623
260.142001	8000.251647	9.466202	-0.053589	4.815624
260.236184	8000.204061	9.471207	-0.053607	4.815610
260.393180	8000.309158	9.476211	-0.053636	4.815640
260.348202	8000.267842	9.481216	-0.053628	4.815628
260.359955	8000.297942	9.486221	-0.053630	4.815636
260.519294	8000.325113	9.491226	-0.053660	4.815644
260.330644	8000.246206	9.496231	-0.053625	4.815621
260.316755	8000.289771	9.501235	-0.053622	4.815634
260.248951	8000.250219	9.506240	-0.053609	4.815623
260.284839	8000.308481	9.511245	-0.053616	4.815640
260.407981	8000.295544	9.516250	-0.053639	4.815636
260.350114	8000.231590	9.521255	-0.053628	4.815617
260.494524	8000.249972	9.526259	-0.053655	4.815622
260.248482	8000.281201	9.531264	-0.053610	4.815632
260.390317	8000.264297	9.536269	-0.053636	4.815626
260.451642	8000.293071	9.541274	-0.053648	4.815635
260.464312	8000.225997	9.546279	-0.053650	4.815615
260.346903	8000.302047	9.551283	-0.053628	4.815638
260.379423	8000.267338	9.556288	-0.053634	4.815627
260.538533	8000.299845	9.561293	-0.053664	4.815636
260.584395	8000.308074	9.566298	-0.053672	4.815638
260.388526	8000.203417	9.571303	-0.053636	4.815609
260.753993	8000.320464	9.576307	-0.053704	4.815641
260.655599	8000.203515	9.581312	-0.053686	4.815607
260.573152	8000.245960	9.586317	-0.053670	4.815620
260.566358	8000.298185	9.591322	-0.053669	4.815636
260.725344	8000.238841	9.596327	-0.053699	4.815617
260.727042	8000.357422	9.601331	-0.053699	4.815652
260.670260	8000.267853	9.606336	-0.053689	4.815626
260.743033	8000.222053	9.611341	-0.053702	4.815612
260.747795	8000.288351	9.616346	-0.053703	4.815632
260.580994	8000.277085	9.621351	-0.053672	4.815629
260.764861	8000.354854	9.626355	-0.053707	4.815651
260.657302	8000.251639	9.631360	-0.053687	4.815621
260.676510	8000.352350	9.636365	-0.053690	4.815651
260.920281	8000.336044	9.641370	-0.053736	4.815645
261.047423	8000.250547	9.646375	-0.053759	4.815619
260.871622	8000.288263	9.651379	-0.053727	4.815631
260.964398	8000.253470	9.656384	-0.053744	4.815621
260.888133	8000.258636	9.661389	-0.053730	4.815622
260.932153	8000.276447	9.666394	-0.053738	4.815627
260.600642	8000.250742	9.671399	-0.053676	4.815621
260.867335	8000.384333	9.676403	-0.053726	4.815659
260.955691	8000.309951	9.681408	-0.053743	4.815637
260.967276	8000.275967	9.686413	-0.053745	4.815627
260.841533	8000.308093	9.691418	-0.053721	4.815637
260.822546	8000.236229	9.696423	-0.053718	4.815616
261.053608	8000.288069	9.701427	-0.053761	4.815630
261.000247	8000.291472	9.706432	-0.053751	4.815631
260.971746	8000.310235	9.711437	-0.053746	4.815637
261.133787	8000.373764	9.716442	-0.053776	4.815655
261.110676	8000.290084	9.721447	-0.053772	4.815631
261.246718	8000.341440	9.726451	-0.053797	4.815645
261.029562	8000.240704	9.731456	-0.053757	4.815616
261.043591	8000.286862	9.736461	-0.053759	4.815630
260.878018	8000.284160	9.741466	-0.053729	4.815630
261.041476	8000.241978	9.746471	-0.053759	4.815617
261.047972	8000.284808	9.751475	-0.053760	4.815629
260.909890	8000.271875	9.756480	-0.053735	4.815626
261.107427	8000.291127	9.761485	-0.053771	4.815631
261.117174	8000.288086	9.766490	-0.053773	4.815630
260.878556	8000.211565	9.771495	-0.053729	4.815609
260.899456	8000.225794	9.776499	-0.053733	4.815613
260.941896	8000.170954	9.781504	-0.053741	4.815596
261.143041	8000.192401	9.786509	-0.053778	4.815602
261.092891	8000.258870	9.791514	-0.053769	4.815621
261.037637	8000.212046	9.796519	-0.053759	4.815608
261.216218	8000.205355	9.801523	-0.053792	4.815605
261.044178	8000.261289	9.806528	-0.053760	4.815622
261.226057	8000.240768	9.811533	-0.053794	4.815616
261.305877	8000.262369	9.816538	-0.053809	4.815621
261.254690	8000.205998	9.821543	-0.053799	4.815605
261.114820	8000.314791	9.826547	-0.053773	4.815638
261.236192	8000.208907	9.831552	-0.053796	4.815606
261.292056	8000.240797	9.836557	-0.053806	4.815615
261.248999	8000.331947	9.841562	-0.053798	4.815642
261.367099	8000.284751	9.846567	-0.053820	4.815628
261.403930	8000.290697	9.851571	-0.053827	4.815629
260.987930	8000.249726	9.856576	-0.053750	4.815619
261.227408	8000.239758	9.861581	-0.053795	4.815615
261.460618	8000.321539	9.866586	-0.053838	4.815638
261.547115	8000.306936	9.871591	-0.053854	4.815633
261.474993	8000.333530	9.876595	-0.053841	4.815641
261.331312	8000.206225	9.881600	-0.053814	4.815605
261.324855	8000.252049	9.886605	-0.053813	4.815618
261.253949	8000.253030	9.891610	-0.053800	4.815619
261.517663	8000.212485	9.896615	-0.053849	4.815606
261.501880	8000.265633	9.901619	-0.053846	4.815621
261.338604	8000.242675	9.906624	-0.053816	4.815616
261.501154	8000.220771	9.911629	-0.053846	4.815608
261.516736	8000.294723	9.916634	-0.053849	4.815630
261.376921	8000.223020	9.921639	-0.053823	4.815610
261.385459	8000.265884	9.926643	-0.053825	4.815622
261.347966	8000.256731	9.931648	-0.053818	4.815620
261.384827	8000.239180	9.936653	-0.053824	4.815614
261.271535	8000.254421	9.941658	-0.053803	4.815619
261.294594	8000.258005	9.946663	-0.053808	4.815620
261.463730	8000.247956	9.951667	-0.053839	4.815616
261.533774	8000.210656	9.956672	-0.053852	4.815605
261.529806	8000.234091	9.961677	-0.053852	4.815612
261.630797	8000.277399	9.966682	-0.053871	4.815624
261.523945	8000.241479	9.971687	-0.053851	4.815614
261.454331	8000.315107	9.976691	-0.053838	4.815636
261.545995	8000.246118	9.981696	-0.053855	4.815616
261.523082	8000.217979	9.986701	-0.053851	4.815607
261.586691	8000.313009	9.991706	-0.053863	4.815635
261.417667	8000.293161	9.996711	-0.053831	4.815630
261.427717	8000.338187	10.001715	-0.053833	4.815643
261.360430	8000.308254	10.006720	-0.053821	4.815635
261.486390	8000.283615	10.011725	-0.053844	4.815627
261.575607	8000.277600	10.016730	-0.053861	4.815625
261.564711	8000.266746	10.021735	-0.053859	4.815621
261.570345	8000.263637	10.026739	-0.053860	4.815621
261.376221	8000.244448	10.031744	-0.053824	4.815616
261.584802	8000.259608	10.036749	-0.053863	4.815619
261.615978	8000.264394	10.041754	-0.053868	4.815621
261.680125	8000.243017	10.046759	-0.053880	4.815614
261.819438	8000.280543	10.051763	-0.053906	4.815624
261.611426	8000.239765	10.056768	-0.053868	4.815613
261.532713	8000.203237	10.061773	-0.053853	4.815603
261.840884	8000.290517	10.066778	-0.053910	4.815627
261.763796	8000.209157	10.071783	-0.053896	4.815604
261.608028	8000.271765	10.076787	-0.053867	4.815623
261.425138	8000.194017	10.081792	-0.053833	4.815601
261.767708	8000.191075	10.086797	-0.053897	4.815598
261.636947	8000.257296	10.091802	-0.053873	4.815618
261.455626	8000.262880	10.096807	-0.053839	4.815621
261.731484	8000.300502	10.101811	-0.053890	4.815631
261.654984	8000.290711	10.106816	-0.053876	4.815628
261.755877	8000.234689	10.111821	-0.053895	4.815611
261.633244	8000.283954	10.116826	-0.053872	4.815626
261.397886	8000.211757	10.121831	-0.053828	4.815606
261.410182	8000.318765	10.126835	-0.053831	4.815637
261.416605	8000.262268	10.131840	-0.053832	4.815621
261.571730	8000.243446	10.136845	-0.053861	4.815615
261.557193	8000.262436	10.141850	-0.053858	4.815620
261.603346	8000.202316	10.146855	-0.053867	4.815602
261.699276	8000.186799	10.151859	-0.053885	4.815597
261.673130	8000.184239	10.156864	-0.053880	4.815597
261.482101	8000.238795	10.161869	-0.053844	4.815614
261.576191	8000.240336	10.166874	-0.053862	4.815614
261.484347	8000.258063	10.171879	-0.053845	4.815619
261.831801	8000.274426	10.176883	-0.053910	4.815622
261.479328	8000.227015	10.181888	-0.053844	4.815610
261.701883	8000.209295	10.186893	-0.053886	4.815604
261.790711	8000.224635	10.191898	-0.053902	4.815608
261.650406	8000.203121	10.196903	-0.053876	4.815602
261.814734	8000.272029	10.201907	-0.053907	4.815622
261.758925	8000.203834	10.206912	-0.053896	4.815602
261.712004	8000.208411	10.211917	-0.053888	4.815604
261.761997	8000.241273	10.216922	-0.053897	4.815613
261.815590	8000.203703	10.221927	-0.053907	4.815602
261.711243	8000.275695	10.226931	-0.053888	4.815623
261.680059	8000.237808	10.231936	-0.053882	4.815612
261.723308	8000.191525	10.236941	-0.053890	4.815599
261.664861	8000.233295	10.241946	-0.053879	4.815611
261.540413	8000.232332	10.246951	-0.053856	4.815611
261.761157	8000.260509	10.251955	-0.053897	4.815619
261.694211	8000.230581	10.256960	-0.053885	4.815610
261.767497	8000.195469	10.261965	-0.053898	4.815600
261.878180	8000.246411	10.266970	-0.053919	4.815614
261.865155	8000.185324	10.271975	-0.053917	4.815596
261.924702	8000.235431	10.276979	-0.053928	4.815611
261.710908	8000.244756	10.281984	-0.053888	4.815614
261.778864	8000.250143	10.286989	-0.053901	4.815616
261.954161	8000.269032	10.291994	-0.053933	4.815620
261.837859	8000.223345	10.296999	-0.053912	4.815607
261.968909	8000.263940	10.302003	-0.053936	4.815619
262.038161	8000.273620	10.307008	-0.053949	4.815621
261.980372	8000.202188	10.312013	-0.053938	4.815601
261.998446	8000.252685	10.317018	-0.053942	4.815615
261.899143	8000.238249	10.322023	-0.053923	4.815611
261.982859	8000.291955	10.327027	-0.053939	4.815627
261.819348	8000.261517	10.332032	-0.053909	4.815619
261.985752	8000.238608	10.337037	-0.053940	4.815611
261.901041	8000.276744	10.342042	-0.053924	4.815623
261.932901	8000.198233	10.347047	-0.053930	4.815600
262.067705	8000.266659	10.352051	-0.053955	4.815619
262.068897	8000.200463	10.357056	-0.053955	4.815600
261.934797	8000.277310	10.362061	-0.053930	4.815623
261.984322	8000.256762	10.367066	-0.053940	4.815616
261.718744	8000.210771	10.372071	-0.053890	4.815604
261.732114	8000.265464	10.377075	-0.053893	4.815620
261.593538	8000.221549	10.382080	-0.053867	4.815608
261.986238	8000.260012	10.387085	-0.053940	4.815617
261.909929	8000.218183	10.392090	-0.053926	4.815606
261.963189	8000.185948	10.397095	-0.053936	4.815596
261.896269	8000.238259	10.402099	-0.053924	4.815611
261.793841	8000.225908	10.407104	-0.053904	4.815608
262.021898	8000.208279	10.412109	-0.053947	4.815602
261.919904	8000.258949	10.417114	-0.053928	4.815617
262.013316	8000.244459	10.422119	-0.053945	4.815613
262.018026	8000.288330	10.427123	-0.053946	4.815626
262.070837	8000.227250	10.432128	-0.053956	4.815607
262.102526	8000.257677	10.437133	-0.053962	4.815616
262.103142	8000.273711	10.442138	-0.053962	4.815621
261.944728	8000.246560	10.447143	-0.053933	4.815614
262.049494	8000.296338	10.452147	-0.053952	4.815628
262.098993	8000.290743	10.457152	-0.053962	4.815626
261.973348	8000.265195	10.462157	-0.053938	4.815619
261.891301	8000.290559	10.467162	-0.053923	4.815627
261.814928	8000.199599	10.472167	-0.053909	4.815601
261.964416	8000.234087	10.477171	-0.053937	4.815610
261.917081	8000.267494	10.482176	-0.053928	4.815620
261.984898	8000.230157	10.487181	-0.053941	4.815609
262.132812	8000.295593	10.492186	-0.053968	4.815627
262.092343	8000.283186	10.497191	-0.053961	4.815624
262.031568	8000.301421	10.502195	-0.053950	4.815629
262.157042	8000.296000	10.507200	-0.053973	4.815627
262.005001	8000.259340	10.512205	-0.053945	4.815617
262.031054	8000.305696	10.517210	-0.053950	4.815631
262.041998	8000.230047	10.522215	-0.053952	4.815608
262.269059	8000.234830	10.527219	-0.053994	4.815609
262.115813	8000.257962	10.532224	-0.053965	4.815616
262.206333	8000.246629	10.537229	-0.053982	4.815612
262.017400	8000.301218	10.542234	-0.053947	4.815629
262.000384	8000.242201	10.547239	-0.053944	4.815612
262.131337	8000.303088	10.552243	-0.053969	4.815629
262.208275	8000.264832	10.557248	-0.053983	4.815618
262.240593	8000.302746	10.562253	-0.053989	4.815629
262.167352	8000.304756	10.567258	-0.053975	4.815630
262.138717	8000.264773	10.572263	-0.053970	4.815618
262.367900	8000.306974	10.577267	-0.054013	4.815629
262.175741	8000.295291	10.582272	-0.053977	4.815627
261.951194	8000.225405	10.587277	-0.053935	4.815607
262.048020	8000.291074	10.592282	-0.053953	4.815626
262.067781	8000.263632	10.597287	-0.053957	4.815618
261.899016	8000.259808	10.602291	-0.053926	4.815618
262.156192	8000.283241	10.607296	-0.053974	4.815623
262.047368	8000.226995	10.612301	-0.053953	4.815607
262.022828	8000.259707	10.617306	-0.053949	4.815617
261.985132	8000.263366	10.622311	-0.053942	4.815618
262.236126	8000.286698	10.627315	-0.053989	4.815624
262.007950	8000.258406	10.632320	-0.053946	4.815617
262.032012	8000.259871	10.637325	-0.053951	4.815617
262.228479	8000.285516	10.642330	-0.053987	4.815624
262.040391	8000.255743	10.647335	-0.053952	4.815616
262.154435	8000.244795	10.652339	-0.053974	4.815612
262.055907	8000.278433	10.657344	-0.053955	4.815622
262.260914	8000.229454	10.662349	-0.053994	4.815607
262.099150	8000.298372	10.667354	-0.053963	4.815628
262.215466	8000.237262	10.672359	-0.053985	4.815610
262.545683	8000.290727	10.677363	-0.054047	4.815624
262.445721	8000.292301	10.682368	-0.054028	4.815625
262.234236	8000.240784	10.687373	-0.053989	4.815611
262.362419	8000.314443	10.692378	-0.054013	4.815631
262.287517	8000.274772	10.697383	-0.053999	4.815620
262.446919	8000.283790	10.702387	-0.054029	4.815622
262.361526	8000.269581	10.707392	-0.054013	4.815618
262.417241	8000.232045	10.712397	-0.054023	4.815607
262.246530	8000.290137	10.717402	-0.053991	4.815625
262.242385	8000.259099	10.722407	-0.053991	4.815616
262.504804	8000.289027	10.727411	-0.054039	4.815623
262.384679	8000.258229	10.732416	-0.054017	4.815615
262.516114	8000.241156	10.737421	-0.054042	4.815609
262.510480	8000.283790	10.742426	-0.054041	4.815622
262.501795	8000.247337	10.747431	-0.054039	4.815611
262.437050	8000.292209	10.752435	-0.054027	4.815625
262.390991	8000.327774	10.757440	-0.054019	4.815635
262.439419	8000.253805	10.762445	-0.054028	4.815613
262.032008	8000.326184	10.767450	-0.053952	4.815636
262.037848	8000.324146	10.772455	-0.053953	4.815636
262.409972	8000.313145	10.777459	-0.054022	4.815631
262.440370	8000.330735	10.782464	-0.054028	4.815636
262.132922	8000.241335	10.787469	-0.053971	4.815611
262.249836	8000.315878	10.792474	-0.053993	4.815632
262.280900	8000.225605	10.797479	-0.053998	4.815606
262.263870	8000.275529	10.802483	-0.053995	4.815621
262.103068	8000.279312	10.807488	-0.053965	4.815622
262.296350	8000.256842	10.812493	-0.054001	4.815615
262.293478	8000.258934	10.817498	-0.054001	4.815616
262.254230	8000.257228	10.822503	-0.053994	4.815615
262.393498	8000.262713	10.827507	-0.054020	4.815616
262.406815	8000.280023	10.832512	-0.054022	4.815621
262.286383	8000.269513	10.837517	-0.054000	4.815619
262.317652	8000.322363	10.842522	-0.054006	4.815634
262.384812	8000.286083	10.847527	-0.054018	4.815623
262.435347	8000.276232	10.852531	-0.054028	4.815620
262.270257	8000.285285	10.857536	-0.053997	4.815623
262.329673	8000.260626	10.862541	-0.054008	4.815616
262.531151	8000.321600	10.867546	-0.054046	4.815633
262.415486	8000.266309	10.872551	-0.054024	4.815617
262.430551	8000.315690	10.877555	-0.054027	4.815631
262.344010	8000.248059	10.882560	-0.054011	4.815612
262.290372	8000.240777	10.887565	-0.054001	4.815610
262.285060	8000.258851	10.892570	-0.054000	4.815616
262.379722	8000.216611	10.897575	-0.054018	4.815603
262.427368	8000.261184	10.902579	-0.054026	4.815616
262.559870	8000.313553	10.907584	-0.054051	4.815630
262.543798	8000.276980	10.912589	-0.054048	4.815620
262.573601	8000.337283	10.917594	-0.054054	4.815637
262.346087	8000.254529	10.922599	-0.054012	4.815614
262.481493	8000.218297	10.927603	-0.054037	4.815603
262.385334	8000.256246	10.932608	-0.054019	4.815614
262.349124	8000.224684	10.937613	-0.054012	4.815605
262.314434	8000.267911	10.942618	-0.054006	4.815618
262.386570	8000.224236	10.947623	-0.054019	4.815605
262.576380	8000.303175	10.952627	-0.054055	4.815627
262.336104	8000.296046	10.957632	-0.054010	4.815626
262.323733	8000.205062	10.962637	-0.054008	4.815600
262.312171	8000.242259	10.967642	-0.054006	4.815611
262.251875	8000.220983	10.972647	-0.053994	4.815605
262.364786	8000.286916	10.977651	-0.054015	4.815623
262.495544	8000.261288	10.982656	-0.054040	4.815615
262.595045	8000.221264	10.987661	-0.054058	4.815603
262.496906	8000.255977	10.992666	-0.054040	4.815614
262.522142	8000.213671	10.997671	-0.054045	4.815601
262.754634	8000.261267	11.002675	-0.054088	4.815614
262.461972	8000.303480	11.007680	-0.054034	4.815628
262.527773	8000.281062	11.012685	-0.054046	4.815621
262.522435	8000.284182	11.017690	-0.054045	4.815622
262.385131	8000.221062	11.022695	-0.054020	4.815604
262.477885	8000.252487	11.027699	-0.054037	4.815613
262.319621	8000.249903	11.032704	-0.054007	4.815613
262.326243	8000.226518	11.037709	-0.054009	4.815606
262.368998	8000.246445	11.042714	-0.054017	4.815611
262.321389	8000.223242	11.047719	-0.054008	4.815605
262.506494	8000.261517	11.052723	-0.054042	4.815615
262.418792	8000.225909	11.057728	-0.054026	4.815605
262.547948	8000.246181	11.062733	-0.054050	4.815611
262.656746	8000.274666	11.067738	-0.054071	4.815618
262.714770	8000.243576	11.072743	-0.054081	4.815609
262.607829	8000.308051	11.077747	-0.054062	4.815628
262.638907	8000.258364	11.082752	-0.054067	4.815614
262.779871	8000.258536	11.087757	-0.054094	4.815613
262.651557	8000.329070	11.092762	-0.054070	4.815634
262.620845	8000.306142	11.097767	-0.054064	4.815628
262.662960	8000.276928	11.102771	-0.054072	4.815619
262.683934	8000.284751	11.107776	-0.054076	4.815621
262.552989	8000.268729	11.112781	-0.054052	4.815617
262.801304	8000.368919	11.117786	-0.054098	4.815645
262.634499	8000.313860	11.122791	-0.054067	4.815630
262.562811	8000.283853	11.127795	-0.054054	4.815621
262.520580	8000.243648	11.132800	-0.054046	4.815610
262.374583	8000.261558	11.137805	-0.054019	4.815616
262.489728	8000.347821	11.142810	-0.054040	4.815641
262.480995	8000.287870	11.147815	-0.054038	4.815623
262.698509	8000.303179	11.152819	-0.054079	4.815626
262.809162	8000.235568	11.157824	-0.054100	4.815606
262.769659	8000.224245	11.162829	-0.054092	4.815603
262.664728	8000.208648	11.167834	-0.054073	4.815599
262.651148	8000.156094	11.172839	-0.054070	4.815584
262.744711	8000.240937	11.177843	-0.054088	4.815608
262.664041	8000.262050	11.182848	-0.054073	4.815615
262.583147	8000.220145	11.187853	-0.054058	4.815603
262.454268	8000.235130	11.192858	-0.054034	4.815608
262.496245	8000.223003	11.197863	-0.054042	4.815604
262.588639	8000.252287	11.202867	-0.054059	4.815612
262.468645	8000.236444	11.207872	-0.054037	4.815608
262.591933	8000.234191	11.212877	-0.054060	4.815607
262.751110	8000.314767	11.217882	-0.054089	4.815630
262.605237	8000.237620	11.222887	-0.054062	4.815608
262.649904	8000.235150	11.227891	-0.054071	4.815607
262.667783	8000.191655	11.232896	-0.054074	4.815594
262.654444	8000.197849	11.237901	-0.054071	4.815596
262.579710	8000.274599	11.242906	-0.054058	4.815619
262.608023	8000.229139	11.247911	-0.054063	4.815605
262.684916	8000.256034	11.252915	-0.054077	4.815613
262.569181	8000.258417	11.257920	-0.054056	4.815614
262.497901	8000.216669	11.262925	-0.054043	4.815602
262.602398	8000.305962	11.267930	-0.054062	4.815628
262.563981	8000.231641	11.272935	-0.054055	4.815606
262.510754	8000.256408	11.277939	-0.054045	4.815614
262.578699	8000.242570	11.282944	-0.054058	4.815609
262.571621	8000.226436	11.287949	-0.054056	4.815605
262.569433	8000.249902	11.292954	-0.054056	4.815611
262.634317	8000.205039	11.297959	-0.054068	4.815598
262.821634	8000.240148	11.302963	-0.054103	4.815607
262.651207	8000.232024	11.307968	-0.054071	4.815606
262.582221	8000.230900	11.312973	-0.054059	4.815606
262.697343	8000.271236	11.317978	-0.054080	4.815617
262.587621	8000.202158	11.322983	-0.054060	4.815597
262.649552	8000.244828	11.327987	-0.054071	4.815610
262.822424	8000.260475	11.332992	-0.054104	4.815613
262.798530	8000.250476	11.337997	-0.054099	4.815611
262.772908	8000.300260	11.343002	-0.054094	4.815625
262.586021	8000.234191	11.348007	-0.054060	4.815607
262.760951	8000.230647	11.353011	-0.054092	4.815605
262.639729	8000.221192	11.358016	-0.054070	4.815603
262.664008	8000.272859	11.363021	-0.054074	4.815618
262.781454	8000.263035	11.368026	-0.054096	4.815614
262.612243	8000.244250	11.373031	-0.054065	4.815610
262.480302	8000.302976	11.378035	-0.054040	4.815627
262.747793	8000.321239	11.383040	-0.054090	4.815631
262.823421	8000.238102	11.388045	-0.054104	4.815607
262.818640	8000.261525	11.393050	-0.054103	4.815614
262.515612	8000.241620	11.398055	-0.054047	4.815609
262.737018	8000.260197	11.403059	-0.054088	4.815614
262.797456	8000.257985	11.408064	-0.054100	4.815613
262.463755	8000.199129	11.413069	-0.054037	4.815597
262.617177	8000.247568	11.418074	-0.054066	4.815611
262.679467	8000.187710	11.423079	-0.054078	4.815593
262.673410	8000.231405	11.428083	-0.054077	4.815606
262.620921	8000.270069	11.433088	-0.054067	4.815617
262.893063	8000.216847	11.438093	-0.054118	4.815600
262.784266	8000.265271	11.443098	-0.054097	4.815615
262.718210	8000.205450	11.448103	-0.054085	4.815598
262.772705	8000.217026	11.453107	-0.054095	4.815601
262.604748	8000.266618	11.458112	-0.054064	4.815616
262.519191	8000.217160	11.463117	-0.054048	4.815602
262.483446	8000.277459	11.468122	-0.054042	4.815620
262.469799	8000.274035	11.473127	-0.054039	4.815619
262.624235	8000.279768	11.478131	-0.054068	4.815620
262.546747	8000.312682	11.483136	-0.054053	4.815630
262.539462	8000.288001	11.488141	-0.054052	4.815623
262.631011	8000.326884	11.493146	-0.054069	4.815634
262.623943	8000.210353	11.498151	-0.054068	4.815600
262.608545	8000.258168	11.503155	-0.054065	4.815614
262.675831	8000.245387	11.508160	-0.054078	4.815610
262.728964	8000.256940	11.513165	-0.054088	4.815613
262.488573	8000.253013	11.518170	-0.054043	4.815613
262.742014	8000.235799	11.523175	-0.054090	4.815606
262.867068	8000.237848	11.528179	-0.054113	4.815606
262.684340	8000.211366	11.533184	-0.054079	4.815600
262.682205	8000.189973	11.538189	-0.054079	4.815593
262.894079	8000.252185	11.543194	-0.054119	4.815611
262.677673	8000.221948	11.548199	-0.054078	4.815603
262.673071	8000.246442	11.553203	-0.054078	4.815610
262.854292	8000.294268	11.558208	-0.054111	4.815623
262.683730	8000.212445	11.563213	-0.054080	4.815600
262.738846	8000.248596	11.568218	-0.054090	4.815610
262.763761	8000.200944	11.573223	-0.054095	4.815596
262.674106	8000.229388	11.578227	-0.054078	4.815605
262.780845	8000.299493	11.583232	-0.054098	4.815625
262.956175	8000.263913	11.588237	-0.054131	4.815614
262.916953	8000.247255	11.593242	-0.054123	4.815609
262.657800	8000.199230	11.598247	-0.054075	4.815596
262.791185	8000.253750	11.603251	-0.054100	4.815611
262.927100	8000.236750	11.608256	-0.054125	4.815606
262.898050	8000.225598	11.613261	-0.054120	4.815603
262.754950	8000.254236	11.618266	-0.054093	4.815612
262.775725	8000.199040	11.623271	-0.054097	4.815596
262.898298	8000.221341	11.628275	-0.054120	4.815601
262.809284	8000.269020	11.633280	-0.054104	4.815616
262.933806	8000.213384	11.638285	-0.054127	4.815599
262.902638	8000.245988	11.643290	-0.054121	4.815609
262.990507	8000.190821	11.648295	-0.054137	4.815592
262.930695	8000.211208	11.653299	-0.054126	4.815598
262.956897	8000.237274	11.658304	-0.054131	4.815606
262.988141	8000.230312	11.663309	-0.054137	4.815604
262.914507	8000.307080	11.668314	-0.054123	4.815626
262.750711	8000.260614	11.673319	-0.054093	4.815614
262.857233	8000.258088	11.678323	-0.054113	4.815612
262.785501	8000.225944	11.683328	-0.054100	4.815603
262.698050	8000.230926	11.688333	-0.054083	4.815605
262.926268	8000.279521	11.693338	-0.054126	4.815618
262.665966	8000.185550	11.698343	-0.054077	4.815592
262.911642	8000.253655	11.703347	-0.054123	4.815611
262.798743	8000.231519	11.708352	-0.054102	4.815605
262.770295	8000.197947	11.713357	-0.054097	4.815595
262.846530	8000.218423	11.718362	-0.054111	4.815601
262.742133	8000.184677	11.723367	-0.054092	4.815592
263.118662	8000.225016	11.728371	-0.054162	4.815601
262.958807	8000.212793	11.733376	-0.054132	4.815599
262.920831	8000.229265	11.738381	-0.054125	4.815604
263.062132	8000.252940	11.743386	-0.054152	4.815610
262.876955	8000.222146	11.748391	-0.054117	4.815602
263.000988	8000.246607	11.753395	-0.054140	4.815608
263.187725	8000.230439	11.758400	-0.054175	4.815603
263.058471	8000.217648	11.763405	-0.054151	4.815600
263.185809	8000.323338	11.768410	-0.054175	4.815630
262.940844	8000.263795	11.773415	-0.054129	4.815614
262.919885	8000.268796	11.778419	-0.054125	4.815615
262.952082	8000.228740	11.783424	-0.054131	4.815603
262.890245	8000.213847	11.788429	-0.054120	4.815599
262.893911	8000.323922	11.793434	-0.054121	4.815631
262.792070	8000.248563	11.798439	-0.054102	4.815610
262.887309	8000.266145	11.803443	-0.054119	4.815615
263.008078	8000.235014	11.808448	-0.054142	4.815605
263.123627	8000.213409	11.813453	-0.054164	4.815598
262.996952	8000.242315	11.818458	-0.054140	4.815607
262.880816	8000.209446	11.823463	-0.054118	4.815598
262.933922	8000.250905	11.828467	-0.054128	4.815610
262.951615	8000.290716	11.833472	-0.054132	4.815621
262.850470	8000.218573	11.838477	-0.054113	4.815601
263.067146	8000.278728	11.843482	-0.054153	4.815617
262.956493	8000.191476	11.848487	-0.054133	4.815592
262.931825	8000.230595	11.853491	-0.054128	4.815604
262.871166	8000.275533	11.858496	-0.054117	4.815617
262.993746	8000.205981	11.863501	-0.054140	4.815596
262.985829	8000.249646	11.868506	-0.054138	4.815609
262.874794	8000.241425	11.873511	-0.054118	4.815607
263.145967	8000.240523	11.878515	-0.054168	4.815606
263.068553	8000.252078	11.883520	-0.054154	4.815610
262.813870	8000.207330	11.888525	-0.054106	4.815598
262.994106	8000.266888	11.893530	-0.054140	4.815614
263.042939	8000.279439	11.898535	-0.054149	4.815618
262.862811	8000.235910	11.903539	-0.054116	4.815606
263.022329	8000.226774	11.908544	-0.054145	4.815602
263.024486	8000.184090	11.913549	-0.054146	4.815590
263.065325	8000.227484	11.918554	-0.054154	4.815602
262.854686	8000.203750	11.923559	-0.054114	4.815596
262.797018	8000.247669	11.928563	-0.054104	4.815610
263.112186	8000.289142	11.933568	-0.054162	4.815620
263.009773	8000.227658	11.938573	-0.054143	4.815603
262.980536	8000.247477	11.943578	-0.054138	4.815609
263.078285	8000.206356	11.948583	-0.054156	4.815596
263.070121	8000.230792	11.953587	-0.054155	4.815603
263.092032	8000.300579	11.958592	-0.054159	4.815624
263.158143	8000.241851	11.963597	-0.054171	4.815606
262.897430	8000.272837	11.968602	-0.054123	4.815616
262.934149	8000.236059	11.973607	-0.054130	4.815606
263.131952	8000.276680	11.978611	-0.054166	4.815616
262.824466	8000.242817	11.983616	-0.054109	4.815608
262.765200	8000.211946	11.988621	-0.054098	4.815599
262.973111	8000.238847	11.993626	-0.054137	4.815606
262.849774	8000.197315	11.998631	-0.054114	4.815595
262.918936	8000.240104	12.003635	-0.054127	4.815607
262.906370	8000.189703	12.008640	-0.054125	4.815592
262.824709	8000.179827	12.013645	-0.054109	4.815590
263.115896	8000.201681	12.018650	-0.054164	4.815595
263.161283	8000.225924	12.023655	-0.054172	4.815601
263.115492	8000.251881	12.028659	-0.054164	4.815609
263.078849	8000.276919	12.033664	-0.054157	4.815617
262.814072	8000.211713	12.038669	-0.054108	4.815599
262.961326	8000.248302	12.043674	-0.054135	4.815609
263.050756	8000.196365	12.048679	-0.054152	4.815593
263.087662	8000.278146	12.053683	-0.054159	4.815617
263.126196	8000.269167	12.058688	-0.054166	4.815614
263.055702	8000.234907	12.063693	-0.054153	4.815605
262.996286	8000.336474	12.068698	-0.054142	4.815635
262.813905	8000.277955	12.073703	-0.054108	4.815618
263.072215	8000.231984	12.078707	-0.054156	4.815604
263.058419	8000.233898	12.083712	-0.054154	4.815604
263.042070	8000.216545	12.088717	-0.054151	4.815599
262.958747	8000.254704	12.093722	-0.054135	4.815611
263.106106	8000.201578	12.098727	-0.054163	4.815595
263.015486	8000.191555	12.103731	-0.054146	4.815592
263.049678	8000.225228	12.108736	-0.054152	4.815602
263.109023	8000.190956	12.113741	-0.054163	4.815592
263.159140	8000.233434	12.118746	-0.054173	4.815604
263.103181	8000.193004	12.123751	-0.054162	4.815592
263.164623	8000.233531	12.128755	-0.054174	4.815604
263.073804	8000.220300	12.133760	-0.054157	4.815600
263.017404	8000.223654	12.138765	-0.054146	4.815601
263.007009	8000.256598	12.143770	-0.054145	4.815611
263.044817	8000.208088	12.148775	-0.054152	4.815597
263.233776	8000.207978	12.153779	-0.054187	4.815596
263.080830	8000.212957	12.158784	-0.054158	4.815598
263.202104	8000.179697	12.163789	-0.054181	4.815588
263.229392	8000.269865	12.168794	-0.054186	4.815614
263.074369	8000.187228	12.173799	-0.054157	4.815591
263.075108	8000.212877	12.178803	-0.054157	4.815598
263.132343	8000.265085	12.183808	-0.054168	4.815613
263.037418	8000.234698	12.188813	-0.054151	4.815605
263.009008	8000.302593	12.193818	-0.054145	4.815625
263.225306	8000.321088	12.198823	-0.054186	4.815629
263.307131	8000.263685	12.203827	-0.054201	4.815612
262.947878	8000.304809	12.208832	-0.054134	4.815626
262.851393	8000.218857	12.213837	-0.054116	4.815601
263.097465	8000.308330	12.218842	-0.054162	4.815626
262.997137	8000.190273	12.223847	-0.054143	4.815592
263.019537	8000.232298	12.228851	-0.054148	4.815604
263.103028	8000.245415	12.233856	-0.054163	4.815607
263.182339	8000.247784	12.238861	-0.054178	4.815608
263.151223	8000.310296	12.243866	-0.054172	4.815626
263.069737	8000.197887	12.248871	-0.054157	4.815594
263.108941	8000.236982	12.253875	-0.054164	4.815605
263.009994	8000.218278	12.258880	-0.054146	4.815600
262.878951	8000.207594	12.263885	-0.054122	4.815597
263.138542	8000.215047	12.268890	-0.054170	4.815598
263.112904	8000.239197	12.273895	-0.054165	4.815606
263.021756	8000.267616	12.278899	-0.054148	4.815614
263.076858	8000.308040	12.283904	-0.054159	4.815626
262.865470	8000.243706	12.288909	-0.054119	4.815608
262.954081	8000.328469	12.293914	-0.054136	4.815632
263.044712	8000.322478	12.298919	-0.054153	4.815630
263.123432	8000.231914	12.303923	-0.054167	4.815603
262.954258	8000.254785	12.308928	-0.054136	4.815611
262.914257	8000.228501	12.313933	-0.054129	4.815603
263.074068	8000.270637	12.318938	-0.054158	4.815615
263.053995	8000.224385	12.323943	-0.054155	4.815601
262.820564	8000.237660	12.328947	-0.054111	4.815606
263.105753	8000.274370	12.333952	-0.054164	4.815616
263.303454	8000.209250	12.338957	-0.054201	4.815596
263.188924	8000.278941	12.343962	-0.054180	4.815617
262.820774	8000.226997	12.348967	-0.054111	4.815603
263.004633	8000.247096	12.353971	-0.054146	4.815608
263.053495	8000.258580	12.358976	-0.054155	4.815611
263.011964	8000.227998	12.363981	-0.054147	4.815603
263.145054	8000.322033	12.368986	-0.054172	4.815630
263.081423	8000.265456	12.373991	-0.054160	4.815613
262.944782	8000.289927	12.378995	-0.054135	4.815621
263.141811	8000.289948	12.384000	-0.054172	4.815620
262.924480	8000.246879	12.389005	-0.054131	4.815609
263.033386	8000.274297	12.394010	-0.054151	4.815616
262.921201	8000.227607	12.399015	-0.054131	4.815603
263.147166	8000.238783	12.404019	-0.054173	4.815605
263.025196	8000.293399	12.409024	-0.054150	4.815622
263.087998	8000.236754	12.414029	-0.054162	4.815605
263.176407	8000.244612	12.419034	-0.054178	4.815607
263.090719	8000.202627	12.424039	-0.054162	4.815595
263.080609	8000.251597	12.429043	-0.054161	4.815609
263.211382	8000.244127	12.434048	-0.054185	4.815606
263.443588	8000.200933	12.439053	-0.054228	4.815593
263.175152	8000.268107	12.444058	-0.054178	4.815614
263.019372	8000.221772	12.449063	-0.054149	4.815601
263.174081	8000.186923	12.454067	-0.054178	4.815590
263.535820	8000.246247	12.459072	-0.054246	4.815606
263.301559	8000.212513	12.464077	-0.054202	4.815597
263.260349	8000.306901	12.469082	-0.054194	4.815625
263.206206	8000.279317	12.474087	-0.054184	4.815617
263.137786	8000.258976	12.479091	-0.054172	4.815611
263.300728	8000.334275	12.484096	-0.054202	4.815632
263.025633	8000.245400	12.489101	-0.054151	4.815608
263.167356	8000.238109	12.494106	-0.054177	4.815605
263.169188	8000.258436	12.499111	-0.054178	4.815611
263.220158	8000.259273	12.504115	-0.054187	4.815611
263.362420	8000.300055	12.509120	-0.054214	4.815622
263.262379	8000.241814	12.514125	-0.054195	4.815606
263.265630	8000.291002	12.519130	-0.054196	4.815620
263.066959	8000.246101	12.524135	-0.054159	4.815608
263.123448	8000.256641	12.529139	-0.054169	4.815611
263.312112	8000.273616	12.534144	-0.054205	4.815615
263.252404	8000.219239	12.539149	-0.054193	4.815599
263.223803	8000.266838	12.544154	-0.054188	4.815613
263.118299	8000.227734	12.549159	-0.054169	4.815602
263.204297	8000.205646	12.554163	-0.054185	4.815595
263.330100	8000.210911	12.559168	-0.054208	4.815596
263.287899	8000.184591	12.564173	-0.054200	4.815589
263.089183	8000.234748	12.569178	-0.054163	4.815604
263.050260	8000.184984	12.574183	-0.054156	4.815590
263.089841	8000.235834	12.579187	-0.054163	4.815605
263.123989	8000.244941	12.584192	-0.054170	4.815607
262.996708	8000.200140	12.589197	-0.054146	4.815595
263.130729	8000.245058	12.594202	-0.054171	4.815607
262.996790	8000.223646	12.599207	-0.054146	4.815601
263.242694	8000.204174	12.604211	-0.054192	4.815595
263.223385	8000.254061	12.609216	-0.054189	4.815609
263.083971	8000.187700	12.614221	-0.054163	4.815591
263.328685	8000.231225	12.619226	-0.054208	4.815602
263.296529	8000.254200	12.624231	-0.054202	4.815609
263.287545	8000.220946	12.629235	-0.054201	4.815599
263.079911	8000.266685	12.634240	-0.054162	4.815614
263.161235	8000.225296	12.639245	-0.054177	4.815601
263.130130	8000.284603	12.644250	-0.054172	4.815619
263.053327	8000.234219	12.649255	-0.054157	4.815604
263.059077	8000.227908	12.654259	-0.054158	4.815602
263.218195	8000.228378	12.659264	-0.054188	4.815602
263.084877	8000.224065	12.664269	-0.054163	4.815601
263.157934	8000.224195	12.669274	-0.054177	4.815601
263.127248	8000.208744	12.674279	-0.054171	4.815596
263.211402	8000.219737	12.679283	-0.054187	4.815599
263.281413	8000.221953	12.684288	-0.054200	4.815600
263.305886	8000.203132	12.689293	-0.054205	4.815594
263.491108	8000.260637	12.694298	-0.054239	4.815610
263.150659	8000.213417	12.699303	-0.054176	4.815598
263.129677	8000.217350	12.704307	-0.054172	4.815599
263.355197	8000.258425	12.709312	-0.054214	4.815610
263.205090	8000.207910	12.714317	-0.054186	4.815596
263.303563	8000.244770	12.719322	-0.054204	4.815606
263.065637	8000.277197	12.724327	-0.054160	4.815617
263.281628	8000.293551	12.729331	-0.054200	4.815621
263.061293	8000.345490	12.734336	-0.054159	4.815637
262.996416	8000.225876	12.739341	-0.054147	4.815602
263.253338	8000.239694	12.744346	-0.054195	4.815605
263.105129	8000.223389	12.749351	-0.054168	4.815601
263.239101	8000.252286	12.754355	-0.054193	4.815609
263.297949	8000.322677	12.759360	-0.054204	4.815629
263.098488	8000.233972	12.764365	-0.054167	4.815604
263.073768	8000.243184	12.769370	-0.054162	4.815607
263.040129	8000.277884	12.774375	-0.054156	4.815617
263.001610	8000.269781	12.779379	-0.054149	4.815615
263.066244	8000.244140	12.784384	-0.054161	4.815607
263.017077	8000.201684	12.789389	-0.054152	4.815595
263.345049	8000.215596	12.794394	-0.054213	4.815597
263.102098	8000.246873	12.799399	-0.054168	4.815608
262.949982	8000.209142	12.804403	-0.054139	4.815597
263.254904	8000.266469	12.809408	-0.054196	4.815613
263.171951	8000.228801	12.814413	-0.054181	4.815602
263.094530	8000.242491	12.819418	-0.054166	4.815606
263.277457	8000.259372	12.824423	-0.054200	4.815611
263.502823	8000.261994	12.829427	-0.054242	4.815610
263.374741	8000.341077	12.834432	-0.054219	4.815634
263.189153	8000.255802	12.839437	-0.054184	4.815610
263.504157	8000.269503	12.844442	-0.054243	4.815612
263.175266	8000.326075	12.849447	-0.054182	4.815631
263.125737	8000.282546	12.854451	-0.054172	4.815618
263.322948	8000.267617	12.859456	-0.054209	4.815613
263.259179	8000.190744	12.864461	-0.054197	4.815591
263.453536	8000.258012	12.869466	-0.054234	4.815609
263.148314	8000.243410	12.874471	-0.054177	4.815606
263.320141	8000.228067	12.879475	-0.054209	4.815601
263.448519	8000.328434	12.884480	-0.054233	4.815630
263.429910	8000.305703	12.889485	-0.054229	4.815623
263.231366	8000.284302	12.894490	-0.054192	4.815618
263.029772	8000.236149	12.899495	-0.054155	4.815605
263.269033	8000.258223	12.904499	-0.054200	4.815610
263.314408	8000.248288	12.909504	-0.054208	4.815607
263.293849	8000.176394	12.914509	-0.054204	4.815586
263.420247	8000.266048	12.919514	-0.054228	4.815612
263.344817	8000.287247	12.924519	-0.054214	4.815618
263.436208	8000.243886	12.929523	-0.054231	4.815605
263.360801	8000.281107	12.934528	-0.054217	4.815616
263.168971	8000.257680	12.939533	-0.054181	4.815611
263.303733	8000.292998	12.944538	-0.054206	4.815620
263.319707	8000.314625	12.949543	-0.054209	4.815626
263.083492	8000.247748	12.954547	-0.054165	4.815608
263.259058	8000.264508	12.959552	-0.054198	4.815612
263.319058	8000.260152	12.964557	-0.054209	4.815611
263.382617	8000.301783	12.969562	-0.054221	4.815622
263.332280	8000.316984	12.974567	-0.054212	4.815627
263.250791	8000.257978	12.979571	-0.054197	4.815610
263.152581	8000.350367	12.984576	-0.054179	4.815638
263.070508	8000.233675	12.989581	-0.054163	4.815604
263.096287	8000.253326	12.994586	-0.054168	4.815610
263.210178	8000.345979	12.999591	-0.054189	4.815636
263.265478	8000.277462	13.004595	-0.054200	4.815616
263.397841	8000.272154	13.009600	-0.054224	4.815614
263.308444	8000.234381	13.014605	-0.054208	4.815603
263.408915	8000.284091	13.019610	-0.054227	4.815617
263.268812	8000.264714	13.024615	-0.054200	4.815612
263.436054	8000.211913	13.029619	-0.054232	4.815596
263.337605	8000.253029	13.034624	-0.054213	4.815608
263.211132	8000.246692	13.039629	-0.054190	4.815607
263.218698	8000.275657	13.044634	-0.054191	4.815616
263.262355	8000.277443	13.049639	-0.054199	4.815616
263.340008	8000.229585	13.054643	-0.054214	4.815601
263.322147	8000.262407	13.059648	-0.054211	4.815611
263.320528	8000.190823	13.064653	-0.054210	4.815590
263.349478	8000.255385	13.069658	-0.054216	4.815609
263.176427	8000.255762	13.074663	-0.054184	4.815610
263.322499	8000.226112	13.079667	-0.054211	4.815601
263.512286	8000.333893	13.084672	-0.054246	4.815631
263.241618	8000.289950	13.089677	-0.054196	4.815620
263.256189	8000.285919	13.094682	-0.054199	4.815618
263.374702	8000.285725	13.099687	-0.054221	4.815618
263.156637	8000.280026	13.104691	-0.054180	4.815617
263.325470	8000.251816	13.109696	-0.054212	4.815608
263.309148	8000.204558	13.114701	-0.054209	4.815594
263.239073	8000.282453	13.119706	-0.054196	4.815617
263.065764	8000.289235	13.124711	-0.054163	4.815620
263.257400	8000.265671	13.129715	-0.054199	4.815612
263.387862	8000.242174	13.134720	-0.054223	4.815605
263.410846	8000.229737	13.139725	-0.054228	4.815601
263.498761	8000.311285	13.144730	-0.054244	4.815625
263.496648	8000.313390	13.149735	-0.054244	4.815625
263.226089	8000.245951	13.154739	-0.054194	4.815607
263.219309	8000.264001	13.159744	-0.054192	4.815612
263.416263	8000.195664	13.164749	-0.054229	4.815591
263.427398	8000.267412	13.169754	-0.054231	4.815612
263.359494	8000.271645	13.174759	-0.054219	4.815614
263.218351	8000.227685	13.179763	-0.054192	4.815601
263.263925	8000.288246	13.184768	-0.054201	4.815619
263.193988	8000.259336	13.189773	-0.054188	4.815611
263.263528	8000.306405	13.194778	-0.054201	4.815624
263.480806	8000.321711	13.199783	-0.054241	4.815628
263.409834	8000.326962	13.204787	-0.054228	4.815630
263.419270	8000.292942	13.209792	-0.054230	4.815620
263.346313	8000.221258	13.214797	-0.054216	4.815599
263.352992	8000.256618	13.219802	-0.054218	4.815609
263.168590	8000.229039	13.224807	-0.054183	4.815602
263.356113	8000.242791	13.229811	-0.054218	4.815605
263.357174	8000.303693	13.234816	-0.054219	4.815623
263.335376	8000.263821	13.239821	-0.054215	4.815611
263.187441	8000.274221	13.244826	-0.054187	4.815615
263.234766	8000.328403	13.249831	-0.054196	4.815631
263.401750	8000.296960	13.254835	-0.054227	4.815621
263.279113	8000.287480	13.259840	-0.054204	4.815619
263.304780	8000.204593	13.264845	-0.054209	4.815594
263.529143	8000.261671	13.269850	-0.054251	4.815610
263.273527	8000.243608	13.274855	-0.054203	4.815606
263.257268	8000.230529	13.279859	-0.054200	4.815602
263.328806	8000.238111	13.284864	-0.054214	4.815604
263.315646	8000.282759	13.289869	-0.054211	4.815617
263.307954	8000.299726	13.294874	-0.054210	4.815622
263.189426	8000.254000	13.299879	-0.054188	4.815609
263.376668	8000.250657	13.304883	-0.054223	4.815607
263.196604	8000.301120	13.309888	-0.054189	4.815623
263.320169	8000.234787	13.314893	-0.054212	4.815603
263.611281	8000.270527	13.319898	-0.054267	4.815612
263.499569	8000.238797	13.324903	-0.054246	4.815603
263.548203	8000.248141	13.329907	-0.054255	4.815606
263.592676	8000.293732	13.334912	-0.054263	4.815619
263.367407	8000.258008	13.339917	-0.054221	4.815610
263.454768	8000.303232	13.344922	-0.054238	4.815622
263.426927	8000.261124	13.349927	-0.054233	4.815610
263.538609	8000.258683	13.354931	-0.054253	4.815609
263.361947	8000.257933	13.359936	-0.054221	4.815610
263.365800	8000.217412	13.364941	-0.054221	4.815598
263.386322	8000.279700	13.369946	-0.054225	4.815616
263.155073	8000.223585	13.374951	-0.054182	4.815601
263.286526	8000.223603	13.379955	-0.054207	4.815600
263.410713	8000.264089	13.384960	-0.054230	4.815611
263.316166	8000.230503	13.389965	-0.054212	4.815602
263.311445	8000.296651	13.394970	-0.054211	4.815621
263.172885	8000.270890	13.399975	-0.054186	4.815614
263.444828	8000.229414	13.404979	-0.054236	4.815601
263.330301	8000.275608	13.409984	-0.054215	4.815615
263.224569	8000.249316	13.414989	-0.054195	4.815608
263.389611	8000.263768	13.419994	-0.054226	4.815611
263.230385	8000.266508	13.424999	-0.054197	4.815613
263.497381	8000.261266	13.430003	-0.054246	4.815610
263.500369	8000.243161	13.435008	-0.054247	4.815605
263.269514	8000.261818	13.440013	-0.054204	4.815611
263.516514	8000.265862	13.445018	-0.054250	4.815611
263.441215	8000.227251	13.450023	-0.054236	4.815600
263.440947	8000.203752	13.455027	-0.054236	4.815593
263.412713	8000.243881	13.460032	-0.054231	4.815605
263.394624	8000.244657	13.465037	-0.054227	4.815606
263.430864	8000.262343	13.470042	-0.054234	4.815611
263.315772	8000.275417	13.475047	-0.054213	4.815615
263.298570	8000.277275	13.480051	-0.054210	4.815616
263.391746	8000.277735	13.485056	-0.054227	4.815615
263.532436	8000.221295	13.490061	-0.054253	4.815598
263.457987	8000.291643	13.495066	-0.054240	4.815619
263.381056	8000.240188	13.500071	-0.054225	4.815604
263.422935	8000.218447	13.505075	-0.054233	4.815598
263.482452	8000.239718	13.510080	-0.054244	4.815604
263.193716	8000.208296	13.515085	-0.054190	4.815596
263.409236	8000.276978	13.520090	-0.054231	4.815615
263.323387	8000.228582	13.525095	-0.054215	4.815601
263.384132	8000.228511	13.530099	-0.054226	4.815601
263.475228	8000.284477	13.535104	-0.054243	4.815617
263.582947	8000.269153	13.540109	-0.054263	4.815612
263.576598	8000.276530	13.545114	-0.054262	4.815614
263.269308	8000.246941	13.550119	-0.054205	4.815607
263.562849	8000.247473	13.555123	-0.054260	4.815606
263.571548	8000.281798	13.560128	-0.054261	4.815616
263.229580	8000.249506	13.565133	-0.054198	4.815608
263.547769	8000.348706	13.570138	-0.054257	4.815635
263.536562	8000.299394	13.575143	-0.054255	4.815621
263.290590	8000.228085	13.580147	-0.054209	4.815601
263.529209	8000.344141	13.585152	-0.054254	4.815634
263.504480	8000.318106	13.590157	-0.054249	4.815626
263.404047	8000.282287	13.595162	-0.054230	4.815616
263.312091	8000.309625	13.600167	-0.054213	4.815625
263.375983	8000.241248	13.605171	-0.054225	4.815605
263.397844	8000.265107	13.610176	-0.054229	4.815611
263.411528	8000.237565	13.615181	-0.054232	4.815603
263.514895	8000.260621	13.620186	-0.054251	4.815610
263.603020	8000.282360	13.625191	-0.054268	4.815616
263.471004	8000.280204	13.630195	-0.054243	4.815616
263.467500	8000.335691	13.635200	-0.054242	4.815632
263.456274	8000.239382	13.640205	-0.054240	4.815604
263.532374	8000.313261	13.645210	-0.054255	4.815625
263.389959	8000.243645	13.650215	-0.054228	4.815605
263.439963	8000.228446	13.655219	-0.054237	4.815601
263.581275	8000.316208	13.660224	-0.054264	4.815626
263.280301	8000.225841	13.665229	-0.054208	4.815601
263.402960	8000.231055	13.670234	-0.054231	4.815601
263.632233	8000.247626	13.675239	-0.054273	4.815605
263.417843	8000.224897	13.680243	-0.054234	4.815600
263.526042	8000.267258	13.685248	-0.054254	4.815611
263.394360	8000.207431	13.690253	-0.054229	4.815595
263.556288	8000.250671	13.695258	-0.054259	4.815606
263.549722	8000.260180	13.700263	-0.054258	4.815609
263.596897	8000.229980	13.705267	-0.054267	4.815600
263.690504	8000.302009	13.710272	-0.054285	4.815621
263.525447	8000.249112	13.715277	-0.054254	4.815606
263.405748	8000.313379	13.720282	-0.054232	4.815626
263.510253	8000.303344	13.725287	-0.054251	4.815622
263.576735	8000.258507	13.730291	-0.054264	4.815609
263.602716	8000.287774	13.735296	-0.054268	4.815617
263.735173	8000.210906	13.740301	-0.054293	4.815594
263.718802	8000.267250	13.745306	-0.054290	4.815611
263.583216	8000.244742	13.750311	-0.054265	4.815605
263.659268	8000.227832	13.755315	-0.054279	4.815599
263.763919	8000.318200	13.760320	-0.054299	4.815625
263.579012	8000.225458	13.765325	-0.054264	4.815599
263.617897	8000.273094	13.770330	-0.054272	4.815613
263.638149	8000.255271	13.775335	-0.054275	4.815607
263.483092	8000.264487	13.780339	-0.054247	4.815611
263.361672	8000.304160	13.785344	-0.054224	4.815623
263.343938	8000.218427	13.790349	-0.054221	4.815598
263.449614	8000.240453	13.795354	-0.054240	4.815604
263.481487	8000.233501	13.800359	-0.054246	4.815602
263.558234	8000.234760	13.805363	-0.054261	4.815602
263.652470	8000.284369	13.810368	-0.054278	4.815616
263.634122	8000.224259	13.815373	-0.054275	4.815598
263.624214	8000.252939	13.820378	-0.054273	4.815607
263.686295	8000.215507	13.825383	-0.054285	4.815596
263.428258	8000.193133	13.830387	-0.054237	4.815590
263.541023	8000.323151	13.835392	-0.054258	4.815628
263.418120	8000.217540	13.840397	-0.054235	4.815597
263.563822	8000.293625	13.845402	-0.054262	4.815619
263.540171	8000.259063	13.850407	-0.054258	4.815609
263.430423	8000.264748	13.855411	-0.054237	4.815611
263.508702	8000.285257	13.860416	-0.054252	4.815617
263.481189	8000.231406	13.865421	-0.054247	4.815601
263.580529	8000.282167	13.870426	-0.054265	4.815616
263.787176	8000.333616	13.875431	-0.054304	4.815630
263.655093	8000.223581	13.880435	-0.054279	4.815598
263.430397	8000.248747	13.885440	-0.054238	4.815606
263.313883	8000.226552	13.890445	-0.054216	4.815601
263.526386	8000.243916	13.895450	-0.054255	4.815605
263.430545	8000.303233	13.900455	-0.054238	4.815622
263.412059	8000.237781	13.905459	-0.054234	4.815603
263.466352	8000.269647	13.910464	-0.054244	4.815612
263.272902	8000.215218	13.915469	-0.054208	4.815597
263.593781	8000.264262	13.920474	-0.054268	4.815610
263.595254	8000.304877	13.925479	-0.054269	4.815622
263.587689	8000.255625	13.930483	-0.054267	4.815608
263.457234	8000.256699	13.935488	-0.054243	4.815609
263.589448	8000.271682	13.940493	-0.054268	4.815612
263.531480	8000.288895	13.945498	-0.054257	4.815618
263.438853	8000.283111	13.950503	-0.054240	4.815616
263.334180	8000.238679	13.955507	-0.054220	4.815604
263.529438	8000.295281	13.960512	-0.054257	4.815620
263.578585	8000.225595	13.965517	-0.054266	4.815599
263.401305	8000.214154	13.970522	-0.054233	4.815596
263.467425	8000.272915	13.975527	-0.054245	4.815613
263.524004	8000.265300	13.980531	-0.054256	4.815611
263.446213	8000.265099	13.985536	-0.054241	4.815611
263.386665	8000.239563	13.990541	-0.054230	4.815604
263.585456	8000.259907	13.995546	-0.054267	4.815609
263.630064	8000.237143	14.000551	-0.054276	4.815602
263.580033	8000.232055	14.005555	-0.054266	4.815601
263.686515	8000.353428	14.010560	-0.054286	4.815636
263.490164	8000.341674	14.015565	-0.054250	4.815633
263.484447	8000.303133	14.020570	-0.054249	4.815622
263.475635	8000.288039	14.025575	-0.054247	4.815618
263.524438	8000.309135	14.030579	-0.054256	4.815624
263.711497	8000.335697	14.035584	-0.054291	4.815631
263.546949	8000.331940	14.040589	-0.054261	4.815630
263.687762	8000.315022	14.045594	-0.054287	4.815625
263.398664	8000.342338	14.050599	-0.054233	4.815634
263.355848	8000.281828	14.055603	-0.054225	4.815616
263.553221	8000.392938	14.060608	-0.054262	4.815648
263.524167	8000.293134	14.065613	-0.054256	4.815619
263.554041	8000.325669	14.070618	-0.054262	4.815628
263.456620	8000.349713	14.075623	-0.054244	4.815636
263.408386	8000.220757	14.080627	-0.054235	4.815598
263.620433	8000.271225	14.085632	-0.054275	4.815612
263.399281	8000.234500	14.090637	-0.054233	4.815602
263.641027	8000.287590	14.095642	-0.054278	4.815617
263.601565	8000.279472	14.100647	-0.054271	4.815615
263.550588	8000.230577	14.105651	-0.054262	4.815601
263.443595	8000.250193	14.110656	-0.054242	4.815607
263.613015	8000.226265	14.115661	-0.054273	4.815599
263.693153	8000.224376	14.120666	-0.054288	4.815598
263.579333	8000.263105	14.125671	-0.054267	4.815610
263.473260	8000.221854	14.130675	-0.054247	4.815598
263.544795	8000.327700	14.135680	-0.054261	4.815629
263.697453	8000.235141	14.140685	-0.054289	4.815601
263.634118	8000.258675	14.145690	-0.054278	4.815608
263.691188	8000.260680	14.150695	-0.054288	4.815609
263.622674	8000.244609	14.155699	-0.054276	4.815604
263.827869	8000.306715	14.160704	-0.054314	4.815621
263.779904	8000.287776	14.165709	-0.054305	4.815616
263.523603	8000.285723	14.170714	-0.054257	4.815617
263.512195	8000.286608	14.175719	-0.054255	4.815617
263.628791	8000.279974	14.180723	-0.054277	4.815615
263.789799	8000.369128	14.185728	-0.054307	4.815640
263.488619	8000.270212	14.190733	-0.054251	4.815612
263.565969	8000.301387	14.195738	-0.054265	4.815621
263.597991	8000.341434	14.200743	-0.054271	4.815633
263.469673	8000.270981	14.205747	-0.054247	4.815613
263.632186	8000.297141	14.210752	-0.054278	4.815620
263.416674	8000.295755	14.215757	-0.054238	4.815620
263.490053	8000.248895	14.220762	-0.054251	4.815606
263.560120	8000.279951	14.225767	-0.054264	4.815615
263.480132	8000.248740	14.230771	-0.054250	4.815606
263.609067	8000.317075	14.235776	-0.054274	4.815626
263.358567	8000.229669	14.240781	-0.054227	4.815601
263.587219	8000.244094	14.245786	-0.054270	4.815604
263.643981	8000.229005	14.250791	-0.054280	4.815600
263.637876	8000.196866	14.255795	-0.054279	4.815590
263.780583	7999.309507	14.260800	-0.054305	4.815330

263.818907	7996.059359	14.265805	-0.054310	4.814380
263.817554	7990.627152	14.270810	-0.054306	4.812791
263.488950	7983.917431	14.275815	-0.054241	4.810830
263.461085	7976.606297	14.280819	-0.054231	4.808691
263.651332	7969.044916	14.285824	-0.054262	4.806476
263.501490	7961.179097	14.290829	-0.054229	4.804172
263.615229	7953.358404	14.295834	-0.054245	4.801880
263.703475	7945.381350	14.300839	-0.054256	4.799541
263.593692	7937.455230	14.305843	-0.054230	4.797216
263.431618	7929.401428	14.310848	-0.054195	4.794853
263.181244	7921.373776	14.315853	-0.054143	4.792497
263.205082	7913.370021	14.320858	-0.054143	4.790145
263.166891	7905.401181	14.325863	-0.054130	4.787803
263.268263	7897.356473	14.330867	-0.054144	4.785437
263.218096	7889.418666	14.335872	-0.054129	4.783102
263.365693	7881.393059	14.340877	-0.054152	4.780739
263.048690	7873.396994	14.345882	-0.054088	4.778385
263.128428	7865.410193	14.350887	-0.054097	4.776031
263.070714	7857.383184	14.355891	-0.054081	4.773665
262.965668	7849.420961	14.360896	-0.054057	4.771317
263.043127	7841.322200	14.365901	-0.054066	4.768927
262.986249	7833.378056	14.370906	-0.054050	4.766582
263.070837	7825.345526	14.375911	-0.054061	4.764209
263.125110	7817.433842	14.380915	-0.054066	4.761870
263.239690	7809.432792	14.385920	-0.054082	4.759504
262.944340	7801.372923	14.390925	-0.054022	4.757121
262.857001	7793.374413	14.395930	-0.054000	4.754754
262.887072	7785.326429	14.400935	-0.054001	4.752370
262.796299	7777.283261	14.405939	-0.053978	4.749988
262.747676	7769.330969	14.410944	-0.053964	4.747630
262.633046	7761.270398	14.415949	-0.053938	4.745240
262.766930	7753.390083	14.420954	-0.053957	4.742902
262.771952	7745.343028	14.425959	-0.053953	4.740513
262.693703	7737.322323	14.430963	-0.053933	4.738131
262.766696	7729.376493	14.435968	-0.053942	4.735769
262.775677	7721.298569	14.440973	-0.053938	4.733367
262.527493	7713.318860	14.445978	-0.053887	4.730994
262.712055	7705.308446	14.450983	-0.053916	4.728610
262.527376	7697.306015	14.455987	-0.053877	4.726227
262.310117	7689.330459	14.460992	-0.053831	4.723852
262.359257	7681.305811	14.465997	-0.053835	4.721460
262.560634	7673.349300	14.471002	-0.053867	4.719086
262.356019	7665.383958	14.476007	-0.053824	4.716710
262.152298	7657.312944	14.481011	-0.053781	4.714301
262.326733	7649.306590	14.486016	-0.053808	4.711909
262.210772	7641.296793	14.491021	-0.053781	4.709516
262.173967	7633.299020	14.496026	-0.053769	4.707125
262.136932	7625.291768	14.501031	-0.053757	4.704730
262.303762	7617.302576	14.506035	-0.053783	4.702338
262.219717	7609.276054	14.511040	-0.053762	4.699935
262.196266	7601.317635	14.516045	-0.053753	4.697551
262.125199	7593.325477	14.521050	-0.053734	4.695155
262.226104	7585.309380	14.526055	-0.053748	4.692751
261.913489	7577.227217	14.531059	-0.053685	4.690326
262.072836	7569.310187	14.536064	-0.053709	4.687949
262.031045	7561.247371	14.541069	-0.053696	4.685528
262.117230	7553.334860	14.546074	-0.053707	4.683150
262.079622	7545.296962	14.551079	-0.053695	4.680733
262.004004	7537.295205	14.556083	-0.053676	4.678326
261.989684	7529.310352	14.561088	-0.053668	4.675922
261.752207	7521.197962	14.566093	-0.053618	4.673480
261.712202	7513.148827	14.571098	-0.053606	4.671055
261.668252	7505.171178	14.576103	-0.053592	4.668650
261.467579	7497.194939	14.581107	-0.053550	4.666244
261.690568	7489.276304	14.586112	-0.053586	4.663854
261.703302	7481.226463	14.591117	-0.053583	4.661424
261.561545	7473.228829	14.596122	-0.053552	4.659008
261.559685	7465.284419	14.601127	-0.053546	4.656607
261.365293	7457.235121	14.606131	-0.053505	4.654173
261.405521	7449.256849	14.611136	-0.053507	4.651759
261.428393	7441.177494	14.616141	-0.053506	4.649313
261.335500	7433.223687	14.621146	-0.053484	4.646904
261.465763	7425.195283	14.626151	-0.053503	4.644471
261.338854	7417.214733	14.631155	-0.053474	4.642052
261.344897	7409.242790	14.636160	-0.053470	4.639634
261.349899	7401.216391	14.641165	-0.053466	4.637197
261.410466	7393.205614	14.646170	-0.053472	4.634765
261.317989	7385.192639	14.651175	-0.053450	4.632330
261.233761	7377.098713	14.656179	-0.053429	4.629870
261.228927	7369.210350	14.661184	-0.053423	4.627471
260.952832	7361.165844	14.666189	-0.053366	4.625023
261.286257	7353.266577	14.671194	-0.053423	4.622617
261.220058	7345.193848	14.676199	-0.053406	4.620158
261.103654	7337.175614	14.681203	-0.053379	4.617714
260.900820	7329.165761	14.686208	-0.053336	4.615272
260.946536	7321.161239	14.691213	-0.053339	4.612829
261.034054	7313.137422	14.696218	-0.053350	4.610380
260.809296	7305.141490	14.701223	-0.053303	4.607937
260.751396	7297.115060	14.706227	-0.053287	4.605484
260.894216	7289.196882	14.711232	-0.053309	4.603063
260.856814	7281.152424	14.716237	-0.053296	4.600602
260.976021	7273.214067	14.721242	-0.053314	4.598172
260.803415	7265.175315	14.726247	-0.053276	4.595710
260.645930	7257.120551	14.731251	-0.053242	4.593242
260.701772	7249.097284	14.736256	-0.053247	4.590782
260.821748	7241.096490	14.741261	-0.053264	4.588328
260.806291	7233.114474	14.746266	-0.053256	4.585878
260.606655	7225.178852	14.751271	-0.053214	4.583441
260.628691	7217.136234	14.756275	-0.053213	4.580970
260.559757	7209.156081	14.761280	-0.053195	4.578517
260.510312	7201.109150	14.766285	-0.053180	4.576042
260.651373	7193.147131	14.771290	-0.053201	4.573592
260.753493	7185.120535	14.776295	-0.053215	4.571120
260.594469	7177.078917	14.781299	-0.053180	4.568643
260.644644	7169.117899	14.786304	-0.053185	4.566189
260.589569	7161.130193	14.791309	-0.053169	4.563725
260.522601	7153.134742	14.796314	-0.053151	4.561258
260.244188	7145.153666	14.801319	-0.053094	4.558793
260.300132	7137.108825	14.806323	-0.053100	4.556308
260.457269	7129.171891	14.811328	-0.053124	4.553855
260.317063	7121.083199	14.816333	-0.053092	4.551354
260.263675	7113.107513	14.821338	-0.053077	4.548886
260.322547	7105.146678	14.826343	-0.053083	4.546421
260.164765	7097.094607	14.831347	-0.053049	4.543927
260.207538	7089.152633	14.836352	-0.053051	4.541465
260.218984	7081.111470	14.841357	-0.053048	4.538972
260.243216	7073.129980	14.846362	-0.053048	4.536495
260.154297	7065.096249	14.851367	-0.053026	4.534001
260.193790	7057.073185	14.856371	-0.053028	4.531509
260.077938	7049.099751	14.861376	-0.053001	4.529031
259.970066	7041.091534	14.866381	-0.052976	4.526541
259.998336	7033.071767	14.871386	-0.052976	4.524045
259.910988	7025.135464	14.876391	-0.052955	4.521575
259.947138	7017.087385	14.881395	-0.052956	4.519068
260.040483	7009.187547	14.886400	-0.052969	4.516606
259.979215	7001.067980	14.891405	-0.052952	4.514074
259.686605	6993.018882	14.896410	-0.052892	4.511562
259.910653	6985.007141	14.901415	-0.052929	4.509062
259.691964	6977.028467	14.906419	-0.052883	4.506569
259.931643	6969.049362	14.911424	-0.052922	4.504076
259.786181	6961.099935	14.916429	-0.052890	4.501590
259.717238	6953.032567	14.921434	-0.052872	4.499066
259.805577	6945.095941	14.926439	-0.052883	4.496582
259.649998	6937.020471	14.931443	-0.052849	4.494052
259.681136	6929.064357	14.936448	-0.052850	4.491559
259.673497	6921.019469	14.941453	-0.052843	4.489037
259.633281	6913.067977	14.946458	-0.052831	4.486542
259.889281	6905.021483	14.951463	-0.052873	4.484017
259.464648	6897.079874	14.956467	-0.052789	4.481521
259.665406	6889.120387	14.961472	-0.052821	4.479020
259.513993	6881.089644	14.966477	-0.052788	4.476495
259.468579	6873.051431	14.971482	-0.052774	4.473965
259.583676	6865.044758	14.976487	-0.052790	4.471445
259.389832	6856.973720	14.981491	-0.052749	4.468902
259.362824	6849.051021	14.986496	-0.052739	4.466405
259.520234	6841.028667	14.991501	-0.052763	4.463876
259.577983	6833.059473	14.996506	-0.052769	4.461362
259.269372	6825.053704	15.001511	-0.052706	4.458834
259.012290	6817.041105	15.006515	-0.052653	4.456302
259.261047	6809.013035	15.011520	-0.052694	4.453765
259.253914	6800.980846	15.016525	-0.052688	4.451225
259.298201	6793.002899	15.021530	-0.052691	4.448701
259.116624	6785.027488	15.026535	-0.052652	4.446176
258.987592	6777.009685	15.031539	-0.052622	4.443635
259.222825	6769.013294	15.036544	-0.052661	4.441102
258.885583	6761.021312	15.041549	-0.052593	4.438566
258.975426	6753.014365	15.046554	-0.052605	4.436025
259.046129	6744.981771	15.051559	-0.052613	4.433475
259.049468	6736.943929	15.056563	-0.052608	4.430922
259.114385	6729.000175	15.061568	-0.052615	4.428397
258.810631	6720.946594	15.066573	-0.052553	4.425834
258.659141	6712.997551	15.071578	-0.052520	4.423304
258.666928	6704.984086	15.076583	-0.052516	4.420752
258.676833	6696.979138	15.081587	-0.052513	4.418202
258.689754	6689.003247	15.086592	-0.052510	4.415659
258.687497	6680.977393	15.091597	-0.052504	4.413099
258.734509	6672.954451	15.096602	-0.052508	4.410539
258.799231	6664.991584	15.101607	-0.052515	4.407996
258.774702	6656.914590	15.106611	-0.052505	4.405415
258.956647	6648.993215	15.111616	-0.052534	4.402884
258.892232	6640.986743	15.116621	-0.052517	4.400322
258.610540	6633.029554	15.121626	-0.052459	4.397774
258.508037	6625.037034	15.126631	-0.052435	4.395213
258.484203	6616.970933	15.131635	-0.052425	4.392628
258.399235	6608.953484	15.136640	-0.052404	4.390057
258.353767	6600.982884	15.141645	-0.052391	4.387499
258.412306	6592.945118	15.146650	-0.052396	4.384919
258.488051	6585.021556	15.151655	-0.052405	4.382375
258.362352	6576.964439	15.156659	-0.052377	4.379784
258.375257	6569.023163	15.161664	-0.052374	4.377230
258.262550	6560.996700	15.166669	-0.052348	4.374647
258.265655	6552.966084	15.171674	-0.052343	4.372061
258.223963	6544.949790	15.176679	-0.052330	4.369479
258.159093	6536.990984	15.181683	-0.052313	4.366913
258.063996	6528.970706	15.186688	-0.052290	4.364325
257.996579	6521.021418	15.191693	-0.052272	4.361759
258.331986	6512.967454	15.196698	-0.052330	4.359160
258.152554	6505.015306	15.201703	-0.052291	4.356590
258.126853	6496.958666	15.206707	-0.052281	4.353985
258.129634	6488.878313	15.211712	-0.052276	4.351371
257.996413	6480.859591	15.216717	-0.052246	4.348774
257.896948	6472.934639	15.221722	-0.052223	4.346206
258.108811	6464.976164	15.226727	-0.052257	4.343629
257.931504	6456.963132	15.231731	-0.052219	4.341029
258.015752	6448.983105	15.236736	-0.052229	4.338440
257.875814	6440.997226	15.241741	-0.052198	4.335846
257.926434	6432.939066	15.246746	-0.052202	4.333229
257.750245	6424.913741	15.251751	-0.052164	4.330619
257.461608	6416.949537	15.256755	-0.052105	4.328026
257.504076	6408.959878	15.261760	-0.052108	4.325426
257.349926	6400.955448	15.266765	-0.052074	4.322819
257.417347	6392.962417	15.271770	-0.052082	4.320215
257.438573	6384.971408	15.276775	-0.052081	4.317609
257.607102	6376.915836	15.281779	-0.052107	4.314982
257.789788	6368.932664	15.286784	-0.052136	4.312378
257.544578	6360.896383	15.291789	-0.052085	4.309751
257.522493	6352.921934	15.296794	-0.052075	4.307144
257.491762	6344.932492	15.301799	-0.052065	4.304531
257.362467	6336.922618	15.306803	-0.052035	4.301909
257.399587	6328.948946	15.311808	-0.052037	4.299298
257.323798	6320.943796	15.316813	-0.052018	4.296675
257.320841	6312.908472	15.321818	-0.052012	4.294041
257.178409	6304.916729	15.326823	-0.051980	4.291418
257.325161	6296.878060	15.331827	-0.052002	4.288780
257.387200	6288.940481	15.336832	-0.052009	4.286174
257.271640	6280.921029	15.341837	-0.051982	4.283537
257.127050	6272.924391	15.346842	-0.051950	4.280906
257.193509	6264.944397	15.351847	-0.051957	4.278281
257.038648	6256.933291	15.356851	-0.051923	4.275642
257.163151	6248.918985	15.361856	-0.051941	4.273003
256.954868	6240.834054	15.366861	-0.051897	4.270336
256.782703	6232.871578	15.371866	-0.051860	4.267707
256.696408	6224.866414	15.376871	-0.051839	4.265064
256.682599	6216.907780	15.381875	-0.051831	4.262436
256.862446	6208.904456	15.386880	-0.051859	4.259792
256.684402	6200.952572	15.391885	-0.051821	4.257161
256.637761	6192.883244	15.396890	-0.051807	4.254490
256.814140	6184.912776	15.401895	-0.051835	4.251853
256.706287	6176.854286	15.406899	-0.051810	4.249182
256.691991	6168.922566	15.411904	-0.051802	4.246552
256.651757	6160.871371	15.416909	-0.051789	4.243881
256.764042	6152.927194	15.421914	-0.051805	4.241245
256.891795	6144.904786	15.426919	-0.051823	4.238582
256.594312	6136.938096	15.431923	-0.051763	4.235931
256.747908	6128.897780	15.436928	-0.051786	4.233259
256.733384	6120.858941	15.441933	-0.051778	4.230584
256.754085	6112.905713	15.446938	-0.051777	4.227936
256.697980	6104.912897	15.451943	-0.051762	4.225272
256.418624	6096.931782	15.456947	-0.051704	4.222608
256.537218	6088.973865	15.461952	-0.051721	4.219955
256.426051	6080.934334	15.466957	-0.051695	4.217270
256.415386	6072.930568	15.471962	-0.051688	4.214596
256.436868	6064.918775	15.476967	-0.051687	4.211918
256.505727	6056.919021	15.481971	-0.051695	4.209243
256.547871	6048.984839	15.486976	-0.051697	4.206588
256.074925	6040.954226	15.491981	-0.051604	4.203894
256.167842	6032.944808	15.496986	-0.051616	4.201211
256.579561	6024.936970	15.501991	-0.051688	4.198530
256.422476	6016.954869	15.506995	-0.051653	4.195850
256.198774	6008.881527	15.512000	-0.051606	4.193137
256.206032	6000.824693	15.517005	-0.051603	4.190430
256.123295	5992.873445	15.522010	-0.051582	4.187756
256.040642	5984.853094	15.527015	-0.051561	4.185057
255.930637	5976.923221	15.532019	-0.051536	4.182387
256.084297	5968.909207	15.537024	-0.051559	4.179689
256.009394	5960.943039	15.542029	-0.051540	4.177003
255.910230	5952.917137	15.547034	-0.051517	4.174295
255.899808	5944.903701	15.552039	-0.051509	4.171591
255.756697	5936.881446	15.557043	-0.051478	4.168880
255.860203	5928.907867	15.562048	-0.051492	4.166186
255.668268	5920.890373	15.567053	-0.051451	4.163473
255.822336	5912.924483	15.572058	-0.051474	4.160779
255.827106	5904.934719	15.577063	-0.051470	4.158074
255.538380	5896.898579	15.582067	-0.051411	4.155348
255.646336	5888.903772	15.587072	-0.051426	4.152639
255.628256	5880.892788	15.592077	-0.051417	4.149921
255.602046	5872.846903	15.597082	-0.051407	4.147189
255.594418	5864.873667	15.602087	-0.051401	4.144480
255.513783	5856.890801	15.607091	-0.051381	4.141766
255.512668	5848.913124	15.612096	-0.051375	4.139052
255.501040	5840.892467	15.617101	-0.051368	4.136322
255.658933	5832.881997	15.622106	-0.051392	4.133596
255.460034	5824.870468	15.627111	-0.051350	4.130863
255.183090	5816.866262	15.632115	-0.051293	4.128129
255.407937	5808.895719	15.637120	-0.051330	4.125412
255.501548	5800.905022	15.642125	-0.051342	4.122684
255.372492	5792.894041	15.647130	-0.051313	4.119945
255.352009	5784.948291	15.652135	-0.051304	4.117228
255.291752	5776.884340	15.657139	-0.051288	4.114467
255.320729	5768.864400	15.662144	-0.051288	4.111722
255.252909	5760.865316	15.667149	-0.051270	4.108980
255.277857	5752.828939	15.672154	-0.051269	4.106225
255.179282	5744.874533	15.677159	-0.051246	4.103494
254.997969	5736.913194	15.682163	-0.051207	4.100758
255.191046	5728.940073	15.687168	-0.051238	4.098022
255.203276	5720.922031	15.692173	-0.051235	4.095265
255.084857	5712.903597	15.697178	-0.051208	4.092505
255.117197	5704.911012	15.702183	-0.051209	4.089754
254.935486	5696.921356	15.707187	-0.051170	4.086999
254.948788	5688.881471	15.712192	-0.051167	4.084228
254.841066	5680.957709	15.717197	-0.051142	4.081493
254.920775	5672.897108	15.722202	-0.051151	4.078711
254.783094	5664.969969	15.727207	-0.051121	4.075971
254.613571	5656.911369	15.732211	-0.051084	4.073183
254.892216	5648.877189	15.737216	-0.051130	4.070408
254.713845	5640.913880	15.742221	-0.051092	4.067649
254.650144	5632.920727	15.747226	-0.051075	4.064880
254.560464	5624.984547	15.752231	-0.051053	4.062128
254.633613	5616.919291	15.757235	-0.051062	4.059331
254.614680	5608.964999	15.762240	-0.051053	4.056570
254.464961	5600.944314	15.767245	-0.051020	4.053782
254.651604	5592.900759	15.772250	-0.051049	4.050989
254.545066	5584.930653	15.777255	-0.051024	4.048216
254.504544	5576.909468	15.782259	-0.051012	4.045423
254.575683	5568.954517	15.787264	-0.051020	4.042654
254.567190	5560.943918	15.792269	-0.051013	4.039862
254.455150	5552.966571	15.797274	-0.050987	4.037078
254.488239	5544.932197	15.802279	-0.050988	4.034274
254.365727	5536.825238	15.807283	-0.050960	4.031441
254.300236	5528.842111	15.812288	-0.050943	4.028650
254.238770	5520.884007	15.817293	-0.050926	4.025866
254.238842	5512.881482	15.822298	-0.050921	4.023065
254.236235	5504.925646	15.827303	-0.050915	4.020279
254.137193	5496.917263	15.832307	-0.050892	4.017471
254.234225	5488.929848	15.837312	-0.050904	4.014671
254.296378	5480.892615	15.842317	-0.050911	4.011851
254.126209	5472.853648	15.847322	-0.050874	4.009025
253.971654	5464.904973	15.852327	-0.050840	4.006229
253.880652	5456.889833	15.857331	-0.050818	4.003408
254.063365	5448.936245	15.862336	-0.050847	4.000612
253.931807	5440.943986	15.867341	-0.050817	3.997795
254.026848	5432.896581	15.872346	-0.050830	3.994960
253.988869	5424.897246	15.877351	-0.050817	3.992138
253.993938	5416.859161	15.882355	-0.050813	3.989301
254.075640	5408.917794	15.887360	-0.050823	3.986498
254.153218	5400.904475	15.892365	-0.050832	3.983667
253.854377	5392.921475	15.897370	-0.050772	3.980838
253.900969	5384.943944	15.902375	-0.050775	3.978015
253.814955	5376.933375	15.907379	-0.050754	3.975176
253.767479	5368.945239	15.912384	-0.050740	3.972344
253.654325	5360.904358	15.917389	-0.050714	3.969490
253.690649	5352.941314	15.922394	-0.050715	3.966664
253.793476	5344.929795	15.927399	-0.050729	3.963820
253.582663	5336.968919	15.932403	-0.050685	3.960986
253.520838	5328.978569	15.937408	-0.050668	3.958143
253.432474	5320.988268	15.942413	-0.050647	3.955297
253.448005	5312.947896	15.947418	-0.050644	3.952433
253.186368	5304.941775	15.952423	-0.050590	3.949574
253.128078	5296.959588	15.957427	-0.050574	3.946725
253.477845	5288.956983	15.962432	-0.050634	3.943874
253.278012	5280.965355	15.967437	-0.050592	3.941015
253.221745	5272.966383	15.972442	-0.050576	3.938154
253.142136	5265.004946	15.977447	-0.050556	3.935304
253.196240	5256.946754	15.982451	-0.050561	3.932420
253.031867	5248.958556	15.987456	-0.050525	3.929554
253.199406	5240.983901	15.992461	-0.050551	3.926698
253.079979	5232.976454	15.997466	-0.050524	3.923822
252.939743	5225.053335	16.002471	-0.050493	3.920974
252.758739	5217.011331	16.007475	-0.050454	3.918081
253.023281	5209.002012	16.012480	-0.050498	3.915205
252.829865	5200.973439	16.017485	-0.050457	3.912312
252.871858	5192.947421	16.022490	-0.050459	3.909422
252.896133	5184.998375	16.027495	-0.050459	3.906557
252.824986	5176.954561	16.032499	-0.050440	3.903654
252.694920	5169.014939	16.037504	-0.050411	3.900786
252.963234	5160.998168	16.042509	-0.050456	3.897895
252.968032	5153.000217	16.047514	-0.050452	3.895003
252.757080	5144.989392	16.052519	-0.050407	3.892101
252.668606	5136.955747	16.057523	-0.050385	3.889191
252.725364	5129.015193	16.062528	-0.050391	3.886315
252.764492	5121.006558	16.067533	-0.050393	3.883412
252.657033	5112.970463	16.072538	-0.050368	3.880494
252.705355	5105.074761	16.077543	-0.050372	3.877627
252.677002	5097.019839	16.082547	-0.050361	3.874699
252.751189	5088.793002	16.087552	-0.050370	3.871709
252.608516	5080.817488	16.092557	-0.050338	3.868803
252.556176	5072.886810	16.097562	-0.050323	3.865914
252.438372	5064.954539	16.102567	-0.050296	3.863020
252.339996	5056.927964	16.107571	-0.050272	3.860090
252.557146	5049.008134	16.112576	-0.050308	3.857203
252.310959	5040.989046	16.117581	-0.050257	3.854268
252.246401	5032.941357	16.122586	-0.050240	3.851324
252.244423	5024.978253	16.127591	-0.050234	3.848411
252.315175	5016.983890	16.132595	-0.050242	3.845485
252.122857	5009.038425	16.137600	-0.050201	3.842569
251.981066	5001.028163	16.142605	-0.050169	3.839628
252.032073	4993.046394	16.147610	-0.050174	3.836700
252.112022	4985.014688	16.152615	-0.050183	3.833752
252.080818	4977.003086	16.157619	-0.050173	3.830806
252.309580	4968.976915	16.162624	-0.050210	3.827858
252.053150	4961.017634	16.167629	-0.050157	3.824923
252.049399	4953.067026	16.172634	-0.050151	3.821993
252.193423	4945.066618	16.177639	-0.050173	3.819046
252.050368	4937.095675	16.182643	-0.050141	3.816102
252.116965	4929.046127	16.187648	-0.050148	3.813131
251.804269	4921.069637	16.192653	-0.050085	3.810176
251.926267	4913.067369	16.197658	-0.050102	3.807219
251.768230	4905.102837	16.202663	-0.050068	3.804267
251.738215	4897.118509	16.207667	-0.050057	3.801309
251.940228	4889.099811	16.212672	-0.050089	3.798341
251.943547	4881.067922	16.217677	-0.050085	3.795361
251.841070	4873.052823	16.222682	-0.050061	3.792382
251.793468	4865.048364	16.227687	-0.050047	3.789407
251.751087	4857.064173	16.232691	-0.050034	3.786436
251.768458	4849.081856	16.237696	-0.050032	3.783466
251.627140	4841.108637	16.242701	-0.050000	3.780493
251.656271	4833.082094	16.247706	-0.050000	3.777501
251.584725	4825.107304	16.252711	-0.049982	3.774524
251.273272	4817.097393	16.257715	-0.049919	3.771527
251.327883	4809.089258	16.262720	-0.049924	3.768535
251.353853	4801.090046	16.267725	-0.049923	3.765545
251.260024	4793.097016	16.272730	-0.049901	3.762551
251.335187	4785.107513	16.277735	-0.049910	3.759560
251.295115	4777.122284	16.282739	-0.049897	3.756566
251.213901	4769.110220	16.287744	-0.049877	3.753558
251.125510	4761.082623	16.292749	-0.049855	3.750542
251.202677	4753.059537	16.297754	-0.049864	3.747529
251.477521	4745.108545	16.302759	-0.049910	3.744545
251.098995	4737.130044	16.307763	-0.049835	3.741533
251.169855	4729.142354	16.312768	-0.049843	3.738526
251.093668	4721.146319	16.317773	-0.049823	3.735510
250.892163	4713.138229	16.322778	-0.049781	3.732484
250.897360	4705.123632	16.327783	-0.049776	3.729458
250.764272	4697.134242	16.332787	-0.049746	3.726435
251.014695	4689.146753	16.337792	-0.049788	3.723420
251.038508	4681.165280	16.342797	-0.049787	3.720400
251.043856	4673.204650	16.347802	-0.049783	3.717384
251.111829	4665.188835	16.352807	-0.049790	3.714347
250.863245	4657.053584	16.357811	-0.049739	3.711254
250.723950	4649.123596	16.362816	-0.049708	3.708239
250.992721	4641.103847	16.367821	-0.049753	3.705197
250.830737	4633.129277	16.372826	-0.049717	3.702160
250.762568	4625.169960	16.377831	-0.049700	3.699128
250.526007	4617.222497	16.382835	-0.049650	3.696094
250.520144	4609.209231	16.387840	-0.049644	3.693039
250.452311	4601.176433	16.392845	-0.049626	3.689971
250.446288	4593.193655	16.397850	-0.049620	3.686922
250.528998	4585.233651	16.402855	-0.049630	3.683881
250.280955	4577.236099	16.407859	-0.049579	3.680815
250.422685	4569.269880	16.412864	-0.049600	3.677768
250.296157	4561.240189	16.417869	-0.049571	3.674688
250.309039	4553.207949	16.422874	-0.049569	3.671607
250.231624	4545.233232	16.427879	-0.049549	3.668544
250.261852	4537.192979	16.432883	-0.049549	3.665456
250.460370	4529.251998	16.437888	-0.049581	3.662407
250.243986	4521.236207	16.442893	-0.049536	3.659317
250.167147	4513.268844	16.447898	-0.049516	3.656246
250.405778	4505.230035	16.452903	-0.049556	3.653153
250.180918	4497.202938	16.457907	-0.049509	3.650050
249.965964	4489.279880	16.462912	-0.049463	3.646985
250.060856	4481.252646	16.467917	-0.049476	3.643885
249.958798	4473.267573	16.472922	-0.049452	3.640794
249.949513	4465.303875	16.477927	-0.049445	3.637711
249.758186	4457.284661	16.482931	-0.049404	3.634598
249.936589	4449.222553	16.487936	-0.049432	3.631477
249.722850	4441.229225	16.492941	-0.049387	3.628368
249.703279	4433.247744	16.497946	-0.049378	3.625267
249.760483	4425.291803	16.502951	-0.049384	3.622176
249.558173	4417.274273	16.507955	-0.049341	3.619050
249.715544	4409.330547	16.512960	-0.049365	3.615961
249.756897	4401.292872	16.517965	-0.049368	3.612829
249.662010	4393.257416	16.522970	-0.049345	3.609691
249.571404	4385.338977	16.527975	-0.049323	3.606597
249.385410	4377.308019	16.532979	-0.049283	3.603453
249.643677	4369.325002	16.537984	-0.049326	3.600337
249.581866	4361.398029	16.542989	-0.049309	3.597232
249.412680	4353.363005	16.547994	-0.049272	3.594079
249.674010	4345.358199	16.552999	-0.049316	3.590947
249.644041	4337.345537	16.558003	-0.049305	3.587801
249.690826	4329.350248	16.563008	-0.049309	3.584661
249.303735	4321.438699	16.568013	-0.049232	3.581539
249.537584	4313.381169	16.573018	-0.049270	3.578375
249.373787	4305.438133	16.578023	-0.049234	3.575241
249.332914	4297.382328	16.583027	-0.049221	3.572064
249.408154	4289.356032	16.588032	-0.049230	3.568899
249.262276	4281.398140	16.593037	-0.049198	3.565751
249.141167	4273.421834	16.598042	-0.049170	3.562595
249.313420	4265.425431	16.603047	-0.049197	3.559436
249.334189	4257.452808	16.608051	-0.049196	3.556279
249.236274	4249.384290	16.613056	-0.049172	3.553078
249.118228	4241.348980	16.618061	-0.049145	3.549887
249.284320	4233.361008	16.623066	-0.049171	3.546720
249.282436	4225.408397	16.628071	-0.049165	3.543559
249.025981	4217.411416	16.633075	-0.049113	3.540370
248.965910	4209.443802	16.638080	-0.049096	3.537196
248.944898	4201.439703	16.643085	-0.049087	3.534006
248.701612	4193.422910	16.648090	-0.049037	3.530801
248.749181	4185.443016	16.653095	-0.049040	3.527616
248.849388	4177.401489	16.658099	-0.049054	3.524406
248.792133	4169.497858	16.663104	-0.049038	3.521243
248.781615	4161.512036	16.668109	-0.049031	3.518046
248.870994	4153.458068	16.673114	-0.049042	3.514821
248.806394	4145.474647	16.678119	-0.049025	3.511618
248.653486	4137.496803	16.683123	-0.048992	3.508410
248.840743	4129.479849	16.688128	-0.049021	3.505195
248.487267	4121.515165	16.693133	-0.048950	3.501981
248.597142	4113.533603	16.698138	-0.048966	3.498772
248.680656	4105.545881	16.703143	-0.048976	3.495556
248.373751	4097.554164	16.708147	-0.048914	3.492323
248.542110	4089.539763	16.713152	-0.048940	3.489094
248.342340	4081.582440	16.718157	-0.048897	3.485872
248.360973	4073.583758	16.723162	-0.048896	3.482638
248.227588	4065.612195	16.728167	-0.048866	3.479407
248.098662	4057.646209	16.733171	-0.048837	3.476176
248.238782	4049.578663	16.738176	-0.048857	3.472909
248.566930	4041.532933	16.743181	-0.048913	3.469653
248.250985	4033.586580	16.748186	-0.048849	3.466415
248.309368	4025.593383	16.753191	-0.048855	3.463166
248.183345	4017.576417	16.758195	-0.048826	3.459898
248.144117	4009.612209	16.763200	-0.048814	3.456652
248.110925	4001.629770	16.768205	-0.048803	3.453395
248.219275	3993.582324	16.773210	-0.048818	3.450114
248.107523	3985.635107	16.778215	-0.048792	3.446863
247.926211	3977.636221	16.783219	-0.048753	3.443586
248.127915	3969.645975	16.788224	-0.048785	3.440321
247.986889	3961.686531	16.793229	-0.048754	3.437055
247.819543	3953.672201	16.798234	-0.048717	3.433762
247.724858	3945.668824	16.803239	-0.048695	3.430473
247.762138	3937.657047	16.808243	-0.048696	3.427182
247.691423	3929.661820	16.813248	-0.048678	3.423891
247.641348	3921.705209	16.818253	-0.048664	3.420613
247.529688	3913.701518	16.823258	-0.048638	3.417310
247.686522	3905.701574	16.828263	-0.048662	3.414015
247.605121	3897.690490	16.833267	-0.048641	3.410705
247.482600	3889.751039	16.838272	-0.048613	3.407419
247.522572	3881.740916	16.843277	-0.048616	3.404106
247.306490	3873.788578	16.848282	-0.048570	3.400805
247.547297	3865.793803	16.853287	-0.048610	3.397499
247.382869	3857.769239	16.858291	-0.048574	3.394164
247.531520	3849.689522	16.863296	-0.048596	3.390813
247.449754	3841.700179	16.868301	-0.048576	3.387488
247.285910	3833.725652	16.873306	-0.048540	3.384163
247.477320	3825.794896	16.878311	-0.048571	3.380866
247.216463	3817.790421	16.883315	-0.048517	3.377519
247.416379	3809.809411	16.888320	-0.048549	3.374195
247.258952	3801.812851	16.893325	-0.048515	3.370848
246.978658	3793.807944	16.898330	-0.048457	3.367490
247.042987	3785.830111	16.903335	-0.048464	3.364152
246.978734	3777.889813	16.908339	-0.048447	3.360822
246.948596	3769.888284	16.913344	-0.048436	3.357465
247.006540	3761.863409	16.918349	-0.048442	3.354097
247.138589	3753.811220	16.923354	-0.048461	3.350717
247.081187	3745.859879	16.928359	-0.048446	3.347369
246.757322	3737.870739	16.933363	-0.048380	3.343993
246.910107	3729.889833	16.938368	-0.048403	3.340633
246.902680	3721.919017	16.943373	-0.048397	3.337269
246.754772	3713.912378	16.948378	-0.048364	3.333881
246.699424	3705.927988	16.953383	-0.048349	3.330503
246.786996	3697.918556	16.958387	-0.048360	3.327115
246.729729	3689.928503	16.963392	-0.048344	3.323727
246.579954	3681.976110	16.968397	-0.048311	3.320348
246.679482	3673.979013	16.973402	-0.048324	3.316956
246.756145	3665.987672	16.978407	-0.048333	3.313562
246.444229	3657.953142	16.983411	-0.048270	3.310132
246.538183	3649.976736	16.988416	-0.048282	3.306738
246.578603	3641.981047	16.993421	-0.048285	3.303330
246.464246	3633.969392	16.998426	-0.048258	3.299906
246.480961	3626.039833	17.003431	-0.048256	3.296519
246.404154	3618.026125	17.008435	-0.048237	3.293088
246.281008	3610.025699	17.013440	-0.048209	3.289658
246.191097	3602.065635	17.018445	-0.048187	3.286243
246.284786	3594.067509	17.023450	-0.048199	3.282815
246.562514	3586.078494	17.028455	-0.048246	3.279395
246.225847	3578.131579	17.033459	-0.048178	3.275965
246.204295	3570.102191	17.038464	-0.048169	3.272508
246.108502	3562.101092	17.043469	-0.048146	3.269057
246.016171	3554.113965	17.048474	-0.048123	3.265609
246.124793	3546.138640	17.053479	-0.048138	3.262169
246.143744	3538.116359	17.058483	-0.048137	3.258703
246.094796	3530.167255	17.063488	-0.048122	3.255261
246.042127	3522.165692	17.068493	-0.048107	3.251793
245.885501	3514.149891	17.073498	-0.048073	3.248311
246.143702	3506.163403	17.078503	-0.048116	3.244855
245.864391	3498.214219	17.083507	-0.048059	3.241390
245.835977	3490.221717	17.088512	-0.048048	3.237912
245.983732	3482.225748	17.093517	-0.048071	3.234436
245.798415	3474.151221	17.098522	-0.048031	3.230908
245.908648	3466.164560	17.103527	-0.048046	3.227427
245.953082	3458.144767	17.108531	-0.048049	3.223925
245.845842	3450.225644	17.113536	-0.048024	3.220457
245.876762	3442.264365	17.118541	-0.048025	3.216973
245.681879	3434.273145	17.123546	-0.047983	3.213462
245.751203	3426.282914	17.128551	-0.047991	3.209959
245.552379	3418.309660	17.133555	-0.047949	3.206448
245.451478	3410.316102	17.138560	-0.047925	3.202929
245.733253	3402.315638	17.143565	-0.047972	3.199418
245.508953	3394.368381	17.148570	-0.047925	3.195906
245.284788	3386.359947	17.153575	-0.047879	3.192364
245.482379	3378.309671	17.158579	-0.047910	3.188816
245.385945	3370.357060	17.163584	-0.047887	3.185295
245.283797	3362.405382	17.168589	-0.047863	3.181771
245.032593	3354.405065	17.173594	-0.047811	3.178215
245.341730	3346.423918	17.178599	-0.047863	3.174687
245.384642	3338.390049	17.183603	-0.047866	3.171120
245.141160	3330.413915	17.188608	-0.047816	3.167563
245.188495	3322.441146	17.193613	-0.047819	3.164016
245.040973	3314.451388	17.198618	-0.047787	3.160449
245.222663	3306.498178	17.203623	-0.047815	3.156908
245.206023	3298.472525	17.208627	-0.047807	3.153322
245.004867	3290.462152	17.213632	-0.047764	3.149731
244.953197	3282.511916	17.218637	-0.047750	3.146170
245.057010	3274.473337	17.223642	-0.047764	3.142571
245.052624	3266.539368	17.228647	-0.047758	3.139011
244.777367	3258.562554	17.233651	-0.047701	3.135415
244.743579	3250.578178	17.238656	-0.047690	3.131823
244.651981	3242.553947	17.243661	-0.047668	3.128206
244.844717	3234.551066	17.248666	-0.047698	3.124607
244.712629	3226.642738	17.253671	-0.047669	3.121032
244.686459	3218.645321	17.258675	-0.047659	3.117417
244.802692	3210.628543	17.263680	-0.047675	3.113796
244.914337	3202.620115	17.268685	-0.047691	3.110174
244.520091	3194.649466	17.273690	-0.047612	3.106542
244.510933	3186.679360	17.278695	-0.047605	3.102924
244.759687	3178.659746	17.283699	-0.047646	3.099290
244.753063	3170.699067	17.288704	-0.047640	3.095668
244.491762	3162.731564	17.293709	-0.047586	3.092026
244.395013	3154.726886	17.298714	-0.047563	3.088371
244.388925	3146.747860	17.303719	-0.047557	3.084728
244.244454	3138.784766	17.308723	-0.047525	3.081080
244.212582	3130.829301	17.313728	-0.047514	3.077438
244.134055	3122.805628	17.318733	-0.047494	3.073757
243.868507	3114.741963	17.323738	-0.047439	3.070045
244.015579	3106.769041	17.328743	-0.047461	3.066389
243.981010	3098.783411	17.333747	-0.047450	3.062715
244.027056	3090.812005	17.338752	-0.047453	3.059047
244.040806	3082.831118	17.343757	-0.047451	3.055368
244.200457	3074.819833	17.348762	-0.047475	3.051678
244.241648	3066.850610	17.353767	-0.047478	3.047997
244.026129	3058.879714	17.358771	-0.047432	3.044299
243.864976	3050.944652	17.363776	-0.047397	3.040615
243.719477	3042.983361	17.368781	-0.047365	3.036916
243.574746	3034.967269	17.373786	-0.047333	3.033186
243.682898	3026.953620	17.378791	-0.047348	3.029465
243.738802	3018.965255	17.383795	-0.047353	3.025749
243.697764	3010.994113	17.388800	-0.047340	3.022032
243.520755	3003.038320	17.393805	-0.047302	3.018310
243.548474	2995.033603	17.398810	-0.047302	3.014571
243.594685	2987.037532	17.403815	-0.047306	3.010833
243.642059	2979.038592	17.408819	-0.047309	3.007088
243.660647	2971.052624	17.413824	-0.047308	3.003344
243.573438	2963.114343	17.418829	-0.047286	2.999612
243.411856	2955.152039	17.423834	-0.047251	2.995860
243.560462	2947.115265	17.428839	-0.047273	2.992084
243.298047	2939.114278	17.433843	-0.047219	2.988299
243.283646	2931.137540	17.438848	-0.047212	2.984534
243.305254	2923.179590	17.443853	-0.047210	2.980774
243.262231	2915.191743	17.448858	-0.047197	2.976993
243.287191	2907.219321	17.453863	-0.047197	2.973217
243.147906	2899.204214	17.458867	-0.047166	2.969408
243.200156	2891.234110	17.463872	-0.047170	2.965625
243.572359	2883.236506	17.468877	-0.047234	2.961840
243.141311	2875.301285	17.473882	-0.047149	2.958040
243.172268	2867.307060	17.478887	-0.047150	2.954230
243.235904	2859.287584	17.483891	-0.047156	2.950404
243.087722	2851.329452	17.488896	-0.047124	2.946592
242.998295	2843.358384	17.493901	-0.047102	2.942772
242.921659	2835.363126	17.498906	-0.047082	2.938936
243.122804	2827.390397	17.503911	-0.047115	2.935121
242.905440	2819.392367	17.508915	-0.047069	2.931266
242.755712	2811.426769	17.513920	-0.047036	2.927425
242.914113	2803.443198	17.518925	-0.047060	2.923587
242.749050	2795.472473	17.523930	-0.047024	2.919733
242.821456	2787.522474	17.528935	-0.047033	2.915896
242.682472	2779.443597	17.533939	-0.047002	2.911981
242.751990	2771.435151	17.538944	-0.047009	2.908106
242.581241	2763.479925	17.543949	-0.046972	2.904238
242.592866	2755.530013	17.548954	-0.046969	2.900378
242.760358	2747.561238	17.553959	-0.046995	2.896511
242.588163	2739.584937	17.558963	-0.046958	2.892618
242.393446	2731.613651	17.563968	-0.046917	2.888720
242.508660	2723.611077	17.568973	-0.046933	2.884819
242.238700	2715.677510	17.573978	-0.046878	2.880925
242.537685	2707.677913	17.578983	-0.046928	2.877025
242.269373	2699.692630	17.583987	-0.046873	2.873095
242.267835	2691.693615	17.588992	-0.046868	2.869168
242.206830	2683.723648	17.593997	-0.046851	2.865247
242.093782	2675.727382	17.599002	-0.046825	2.861304
242.213941	2667.764036	17.604007	-0.046842	2.857385
242.146499	2659.784047	17.609011	-0.046824	2.853442
242.099481	2651.777476	17.614016	-0.046810	2.849481
242.158587	2643.817317	17.619021	-0.046816	2.845544
242.119027	2635.857932	17.624026	-0.046804	2.841596
242.227324	2627.885294	17.629031	-0.046819	2.837645
241.995462	2619.912819	17.634035	-0.046771	2.833669
241.958098	2611.910068	17.639040	-0.046758	2.829683
241.931708	2603.915482	17.644045	-0.046748	2.825696
241.660637	2595.962671	17.649050	-0.046693	2.821710
241.884423	2587.980790	17.654055	-0.046729	2.817733
241.796070	2579.994767	17.659059	-0.046708	2.813730
241.855203	2571.996984	17.664064	-0.046713	2.809724
241.892193	2564.015609	17.669069	-0.046715	2.805719
241.618665	2556.068383	17.674074	-0.046659	2.801707
241.755744	2548.121202	17.679079	-0.046679	2.797714
241.701061	2540.111572	17.684083	-0.046664	2.793672
241.687045	2532.106997	17.689088	-0.046656	2.789630
241.674045	2524.149080	17.694093	-0.046649	2.785605
241.404667	2516.206605	17.699098	-0.046593	2.781567
241.503648	2508.231066	17.704103	-0.046607	2.777528
241.445616	2500.235020	17.709107	-0.046591	2.773463
241.273655	2492.251773	17.714112	-0.046554	2.769392
241.352710	2484.280375	17.719117	-0.046563	2.765337
241.255953	2476.322892	17.724122	-0.046540	2.761271
241.310219	2468.353339	17.729127	-0.046545	2.757203
241.210066	2460.340512	17.734131	-0.046521	2.753097
241.323061	2452.290836	17.739136	-0.046537	2.748980
240.918581	2444.362247	17.744141	-0.046456	2.744886
240.889185	2436.395913	17.749146	-0.046446	2.740790
241.057653	2428.432623	17.754151	-0.046472	2.736702
240.900573	2420.441673	17.759155	-0.046438	2.732573
240.847827	2412.469832	17.764160	-0.046423	2.728454
240.895290	2404.475207	17.769165	-0.046426	2.724323
240.937918	2396.514942	17.774170	-0.046429	2.720204
240.939119	2388.593910	17.779175	-0.046424	2.716096
240.835039	2380.580327	17.784179	-0.046400	2.711927
240.900905	2372.574965	17.789184	-0.046407	2.707767
240.850206	2364.624587	17.794189	-0.046392	2.703621
240.738527	2356.663862	17.799194	-0.046366	2.699460
240.779556	2348.718588	17.804199	-0.046369	2.695310
240.594032	2340.718065	17.809203	-0.046329	2.691111
240.504279	2332.757847	17.814208	-0.046307	2.686932
240.699545	2324.773227	17.819213	-0.046338	2.682752
240.740199	2316.807795	17.824218	-0.046341	2.678566
240.594629	2308.851908	17.829223	-0.046309	2.674366
240.386934	2300.853463	17.834227	-0.046265	2.670133
240.334500	2292.859556	17.839232	-0.046250	2.665906
240.365860	2284.907637	17.844237	-0.046250	2.661700
240.268723	2276.938635	17.849242	-0.046227	2.657470
240.370768	2268.978591	17.854247	-0.046241	2.653250
240.246663	2260.982572	17.859251	-0.046213	2.648990
240.080034	2253.025200	17.864256	-0.046177	2.644741
240.198653	2245.060292	17.869261	-0.046194	2.640500
240.048162	2237.110564	17.874266	-0.046160	2.636242
240.226819	2229.110768	17.879271	-0.046189	2.631973
240.031269	2221.122888	17.884275	-0.046147	2.627678
240.138170	2213.137522	17.889280	-0.046162	2.623397
240.276804	2205.180335	17.894285	-0.046182	2.619127
239.901862	2197.263232	17.899290	-0.046107	2.614837
239.920994	2189.256640	17.904295	-0.046106	2.610518
240.153080	2181.253826	17.909299	-0.046144	2.606208
239.940665	2173.331574	17.914304	-0.046099	2.601905
239.871060	2165.393229	17.919309	-0.046081	2.597595
239.624275	2157.350682	17.924314	-0.046030	2.593210
239.714817	2149.233807	17.929319	-0.046042	2.588800
239.725685	2141.268033	17.934323	-0.046038	2.584459
239.638722	2133.379048	17.939328	-0.046017	2.580146
239.650050	2125.446452	17.944333	-0.046014	2.575809
239.459911	2117.477120	17.949338	-0.045974	2.571430
239.562720	2109.508122	17.954343	-0.045988	2.567065
239.574250	2101.547968	17.959347	-0.045985	2.562690
239.380106	2093.629958	17.964352	-0.045943	2.558317
239.212117	2085.671950	17.969357	-0.045907	2.553916
239.217194	2077.661762	17.974362	-0.045903	2.549491
239.193314	2069.698459	17.979367	-0.045893	2.545082
239.207492	2061.752562	17.984371	-0.045890	2.540677
239.211644	2053.774528	17.989376	-0.045886	2.536247
239.353096	2045.790661	17.994381	-0.045907	2.531815
239.265162	2037.819780	17.999386	-0.045886	2.527366
239.059192	2029.904631	18.004391	-0.045842	2.522932
239.121918	2021.935883	18.009395	-0.045849	2.518480
238.915487	2013.980392	18.014400	-0.045805	2.514008
239.013026	2005.952852	18.019405	-0.045818	2.509509
238.909764	1997.997398	18.024410	-0.045794	2.505028
238.913107	1990.048300	18.029415	-0.045789	2.500550
238.792056	1982.093021	18.034419	-0.045762	2.496052
239.021465	1974.083914	18.039424	-0.045799	2.491541
238.874475	1966.144540	18.044429	-0.045767	2.487034
238.784631	1958.187765	18.049434	-0.045745	2.482512
238.836033	1950.257909	18.054439	-0.045749	2.478009
238.743782	1942.278146	18.059443	-0.045727	2.473457
238.604935	1934.309899	18.064448	-0.045696	2.468901
238.573752	1926.344844	18.069453	-0.045685	2.464346
238.468272	1918.394435	18.074458	-0.045660	2.459785
238.361940	1910.463019	18.079463	-0.045635	2.455227
238.216864	1902.477941	18.084467	-0.045603	2.450627
238.399654	1894.487373	18.089472	-0.045632	2.446039
238.239344	1886.565975	18.094477	-0.045597	2.441457
238.052650	1878.622817	18.099482	-0.045557	2.436851
238.074623	1870.613142	18.104487	-0.045556	2.432214
238.130018	1862.582859	18.109491	-0.045561	2.427559
238.047578	1854.636598	18.114496	-0.045541	2.422933
237.961078	1846.720017	18.119501	-0.045519	2.418315
237.927912	1838.752738	18.124506	-0.045508	2.413663
238.116198	1830.763948	18.129511	-0.045538	2.409007
237.950185	1822.817641	18.134515	-0.045502	2.404338
237.972371	1814.874280	18.139520	-0.045501	2.399678
238.177763	1806.923214	18.144525	-0.045534	2.395018
237.934658	1798.951599	18.149530	-0.045484	2.390301
237.798425	1791.015111	18.154535	-0.045453	2.385604
237.895065	1783.042306	18.159539	-0.045466	2.380895
237.885953	1775.096497	18.164544	-0.045459	2.376184
237.888025	1767.128707	18.169549	-0.045454	2.371452
237.825432	1759.170839	18.174554	-0.045438	2.366711
237.875785	1751.226279	18.179559	-0.045442	2.361977
237.784589	1743.289040	18.184563	-0.045420	2.357227
237.481096	1735.347836	18.189568	-0.045358	2.352448
237.433415	1727.381063	18.194573	-0.045344	2.347664
237.311013	1719.407475	18.199578	-0.045316	2.342861
237.349255	1711.450251	18.204583	-0.045318	2.338070
237.338415	1703.496596	18.209587	-0.045311	2.333268
237.365691	1695.521128	18.214592	-0.045311	2.328446
237.418925	1687.569162	18.219597	-0.045316	2.323630
237.291721	1679.635414	18.224602	-0.045287	2.318800
237.363713	1671.698730	18.229607	-0.045295	2.313975
237.197195	1663.724521	18.234611	-0.045259	2.309097
237.100809	1655.773211	18.239616	-0.045236	2.304229
237.245384	1647.817651	18.244621	-0.045258	2.299367
237.048478	1639.880523	18.249626	-0.045216	2.294478
236.875383	1631.936625	18.254631	-0.045178	2.289577
236.849419	1623.970341	18.259635	-0.045168	2.284664
236.875710	1616.036701	18.264640	-0.045168	2.279764
236.809696	1608.128059	18.269645	-0.045151	2.274862
236.673114	1600.074125	18.274650	-0.045120	2.269853
236.770371	1592.104683	18.279655	-0.045133	2.264905
236.710651	1584.178865	18.284659	-0.045117	2.259960
236.538354	1576.261603	18.289664	-0.045080	2.255000
236.736286	1568.271231	18.294669	-0.045111	2.250016
236.828911	1560.300415	18.299674	-0.045123	2.245023
236.649217	1552.415759	18.304679	-0.045085	2.240050
236.580556	1544.477286	18.309683	-0.045067	2.235041
236.506876	1536.520807	18.314688	-0.045048	2.230009
236.428803	1528.576779	18.319693	-0.045028	2.224974
236.190748	1520.659463	18.324698	-0.044979	2.219929
236.567821	1512.669934	18.329703	-0.045044	2.214882
236.401268	1504.721009	18.334707	-0.045008	2.209801
236.341525	1496.786890	18.339712	-0.044992	2.204727
236.333700	1488.862520	18.344717	-0.044985	2.199653
236.160262	1480.926862	18.349722	-0.044948	2.194544
236.132410	1472.946050	18.354727	-0.044937	2.189407
236.030332	1465.004159	18.359731	-0.044913	2.184277
236.246533	1457.041137	18.364736	-0.044948	2.179150
235.837108	1449.178095	18.369741	-0.044867	2.174019
235.964103	1441.170437	18.374746	-0.044885	2.168831
236.016731	1433.234818	18.379751	-0.044890	2.163670
236.003310	1425.307426	18.384755	-0.044882	2.158496
235.728438	1417.407530	18.389760	-0.044826	2.153303
235.886594	1409.411438	18.394765	-0.044850	2.148076
235.912908	1401.456405	18.399770	-0.044850	2.142850
235.629460	1393.581724	18.404775	-0.044792	2.137635
235.599868	1385.633580	18.409779	-0.044782	2.132382
235.562372	1377.676017	18.414784	-0.044769	2.127110
235.578753	1369.751809	18.419789	-0.044767	2.121852
235.599918	1361.808331	18.424794	-0.044766	2.116569
235.625509	1353.827687	18.429799	-0.044766	2.111247
235.446749	1345.878245	18.434803	-0.044727	2.105914
235.150079	1337.993561	18.439808	-0.044667	2.100599
235.306130	1330.052751	18.444813	-0.044691	2.095277
235.282245	1322.083365	18.449818	-0.044681	2.089904
235.184651	1314.170332	18.454823	-0.044658	2.084548
235.227583	1306.242970	18.459827	-0.044661	2.079183
235.151824	1298.318875	18.464832	-0.044642	2.073794
235.221805	1290.372855	18.469837	-0.044650	2.068391
234.854760	1282.467518	18.474842	-0.044576	2.062958
234.921990	1274.551630	18.479847	-0.044584	2.057546
234.903792	1266.604263	18.484851	-0.044575	2.052091
234.722539	1258.678601	18.489856	-0.044536	2.046619
234.861918	1250.740272	18.494861	-0.044557	2.041156
234.784374	1242.824989	18.499866	-0.044537	2.035672
234.817768	1234.860576	18.504871	-0.044538	2.030151
234.713946	1226.937783	18.509875	-0.044514	2.024629
234.615308	1219.031200	18.514880	-0.044491	2.019105
234.698868	1211.090181	18.519885	-0.044501	2.013560
234.530305	1203.169138	18.524890	-0.044464	2.007987
234.497104	1195.256561	18.529895	-0.044453	2.002419
234.431418	1187.351581	18.534899	-0.044436	1.996837
234.281844	1179.424326	18.539904	-0.044403	1.991215
234.450529	1171.473964	18.544909	-0.044429	1.985595
234.224381	1163.575395	18.549914	-0.044382	1.979953
234.089232	1155.680893	18.554919	-0.044352	1.974308
233.982854	1147.747662	18.559923	-0.044327	1.968622
234.250512	1139.791258	18.564928	-0.044371	1.962943
234.142423	1131.912589	18.569933	-0.044346	1.957263
234.032716	1123.949730	18.574938	-0.044321	1.951505
233.833258	1116.038117	18.579943	-0.044278	1.945758
233.949938	1108.103144	18.584947	-0.044295	1.940011
233.913585	1100.185467	18.589952	-0.044283	1.934243
234.016053	1092.261738	18.594957	-0.044297	1.928468
233.905348	1084.352072	18.599962	-0.044271	1.922663
233.909554	1076.463425	18.604967	-0.044267	1.916869
233.657877	1068.575740	18.609971	-0.044215	1.911029
233.713234	1060.623881	18.614976	-0.044220	1.905158
233.714118	1052.733515	18.619981	-0.044215	1.899308
233.484491	1044.841010	18.624986	-0.044167	1.893413
233.501706	1036.910863	18.629991	-0.044165	1.887499
233.630048	1028.989854	18.634995	-0.044184	1.881586
233.546373	1021.104317	18.640000	-0.044164	1.875657
233.526433	1013.183114	18.645005	-0.044155	1.869690
233.526933	1005.253114	18.650010	-0.044150	1.863699
233.526211	997.372615	18.655015	-0.044144	1.857726
233.308383	989.484676	18.660019	-0.044099	1.851703
233.283653	981.562504	18.665024	-0.044089	1.845656
233.235383	973.696360	18.670029	-0.044075	1.839630
233.147989	965.788133	18.675034	-0.044054	1.833547
233.112018	957.881282	18.680039	-0.044042	1.827451
233.098569	949.984431	18.685043	-0.044034	1.821345
232.972949	942.106829	18.690048	-0.044006	1.815220
232.845104	934.221589	18.695053	-0.043977	1.809068
232.765504	926.317269	18.700058	-0.043957	1.802886
232.734910	918.445823	18.705063	-0.043946	1.796714
232.647217	910.495912	18.710067	-0.043925	1.790453
232.740363	902.563347	18.715072	-0.043937	1.784205
232.858969	894.684390	18.720077	-0.043954	1.777980
232.704918	886.800982	18.725082	-0.043920	1.771697
232.399135	878.952867	18.730087	-0.043858	1.765401
232.287141	871.096913	18.735091	-0.043832	1.759099
232.213152	863.206386	18.740096	-0.043813	1.752753
232.156351	855.307558	18.745101	-0.043798	1.746378
232.146680	847.416520	18.750106	-0.043791	1.739993
232.151297	839.537585	18.755111	-0.043786	1.733595
232.269326	831.621510	18.760115	-0.043803	1.727158
231.988631	823.783541	18.765120	-0.043746	1.720710
232.045128	815.917560	18.770125	-0.043751	1.714258
231.848520	808.022482	18.775130	-0.043710	1.707724
231.848807	800.153247	18.780135	-0.043705	1.701213
231.877970	792.274823	18.785139	-0.043705	1.694673
231.847049	784.377187	18.790144	-0.043694	1.688083
231.514206	776.572859	18.795149	-0.043627	1.681506
231.492564	768.696443	18.800154	-0.043618	1.674883
231.658480	760.781127	18.805159	-0.043644	1.668227
231.500026	752.935835	18.810163	-0.043609	1.661560
231.179339	745.116800	18.815168	-0.043544	1.654866
231.250851	737.227442	18.820173	-0.043553	1.648138
231.099228	729.383938	18.825178	-0.043519	1.641391
231.117880	721.514656	18.830183	-0.043518	1.634618
231.150402	713.582186	18.835187	-0.043519	1.627763
230.930528	705.754986	18.840192	-0.043473	1.620936
231.138089	697.880299	18.845197	-0.043506	1.614099
230.865343	690.039062	18.850202	-0.043450	1.607194
230.944671	682.184768	18.855207	-0.043460	1.600298
230.739041	674.374718	18.860211	-0.043417	1.593370
230.736014	666.494185	18.865216	-0.043411	1.586379
231.023174	658.624454	18.870221	-0.043459	1.579408
230.809117	650.811997	18.875226	-0.043414	1.572385
230.813659	642.962043	18.880231	-0.043410	1.565328
230.758328	635.144669	18.885235	-0.043395	1.558260
230.824736	627.283807	18.890240	-0.043402	1.551138
230.780654	619.456293	18.895245	-0.043389	1.543998
230.374555	611.676082	18.900250	-0.043308	1.536814
230.516787	603.806125	18.905255	-0.043330	1.529595
230.493350	595.978451	18.910259	-0.043320	1.522356
230.435354	588.166578	18.915264	-0.043304	1.515092
230.433296	580.338470	18.920269	-0.043299	1.507787
230.258607	572.528399	18.925274	-0.043261	1.500436
230.191532	564.728219	18.930279	-0.043244	1.493075
230.142960	556.896048	18.935283	-0.043230	1.485650
230.049964	549.106342	18.940288	-0.043207	1.478222
230.037913	541.266681	18.945293	-0.043200	1.470720
229.869263	533.452479	18.950298	-0.043164	1.463180
229.799051	525.657969	18.955303	-0.043145	1.455636
229.939239	517.825315	18.960307	-0.043167	1.448049
229.742406	510.047028	18.965312	-0.043125	1.440420
229.541310	502.303965	18.970317	-0.043082	1.432785
229.492919	494.487519	18.975322	-0.043068	1.425062
229.496118	486.706906	18.980327	-0.043064	1.417340
229.435897	478.916981	18.985331	-0.043048	1.409556
229.554825	471.110576	18.990336	-0.043065	1.401742
229.258068	463.393077	18.995341	-0.043004	1.393905
229.173079	455.583767	19.000346	-0.042984	1.385966
229.283317	447.805182	19.005351	-0.042999	1.378045
229.136521	440.042256	19.010355	-0.042967	1.370051
228.896033	432.303835	19.015360	-0.042917	1.362019
229.128832	424.516269	19.020365	-0.042955	1.353970
229.060511	416.750217	19.025370	-0.042938	1.345843
228.986088	409.020867	19.030375	-0.042919	1.337705
228.884323	401.274232	19.035379	-0.042895	1.329493
228.730592	393.546506	19.040384	-0.042861	1.321241
228.730530	385.776761	19.045389	-0.042856	1.312920
228.439728	377.974724	19.050394	-0.042797	1.304458
228.577736	370.233731	19.055399	-0.042818	1.296085
228.442662	362.527294	19.060403	-0.042787	1.287646
228.101878	354.858649	19.065408	-0.042719	1.279154
228.184986	347.129404	19.070413	-0.042730	1.270617
228.361668	339.371683	19.075418	-0.042757	1.262009
228.016598	331.733700	19.080423	-0.042688	1.253377
227.831820	324.047998	19.085427	-0.042649	1.244661
227.765754	316.363625	19.090432	-0.042632	1.235909
227.802623	308.644979	19.095437	-0.042633	1.227075
227.434119	301.006943	19.100442	-0.042560	1.218190
227.640331	293.285570	19.105447	-0.042593	1.209257
227.816583	285.579978	19.110451	-0.042621	1.200269
227.500512	277.968725	19.115456	-0.042557	1.191227
227.431516	270.320841	19.120461	-0.042540	1.182122
227.301065	262.682158	19.125466	-0.042510	1.172944
227.048777	255.069979	19.130471	-0.042458	1.163701
226.988291	247.430657	19.135475	-0.042442	1.154390
226.802881	239.783112	19.140480	-0.042403	1.144968
226.677560	232.172196	19.145485	-0.042375	1.135525
226.360989	224.584288	19.150490	-0.042311	1.125991
225.922150	217.048844	19.155495	-0.042224	1.116415
225.989046	209.411607	19.160499	-0.042232	1.106737
225.347644	201.908938	19.165504	-0.042107	1.096990
224.934717	194.369333	19.170509	-0.042026	1.087159
224.792848	186.793102	19.175514	-0.041994	1.077250
224.429390	179.255064	19.180519	-0.041922	1.067250
224.035575	171.734117	19.185523	-0.041844	1.057171
223.736767	164.198160	19.190528	-0.041783	1.046996
223.397432	156.706933	19.195533	-0.041715	1.036773
222.834812	149.237172	19.200538	-0.041605	1.026423
222.276296	141.788587	19.205543	-0.041497	1.015999
221.868907	134.313368	19.210547	-0.041416	1.005466
221.238495	126.889437	19.215552	-0.041294	0.994838
220.867629	119.402257	19.220557	-0.041220	0.984070
220.268053	111.989536	19.225562	-0.041103	0.973232
219.998315	104.538824	19.230567	-0.041048	0.962301
219.484626	97.153704	19.235571	-0.040948	0.951278
218.957789	89.767116	19.240576	-0.040845	0.940120
218.373154	82.419532	19.245581	-0.040731	0.928872
217.548113	75.119729	19.250586	-0.040573	0.917493
217.103700	67.761998	19.255591	-0.040486	0.905986
216.615926	60.667116	19.260595	-0.040390	0.894732