Fri Mar 12 13:58:25 2021

Number of Points = 3628
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.176195	-0.061791	0.000000	-0.000029	0.721468

0.241314	-0.088435	0.005005	-0.000041	0.721438
0.112382	-0.065559	0.010010	-0.000017	0.721438
0.084443	-0.058205	0.015014	-0.000012	0.721443
0.083263	-0.061253	0.020019	-0.000012	0.721437
0.341694	-0.103464	0.025024	-0.000060	0.721444
0.282829	-0.096161	0.030029	-0.000049	0.721438
-0.011586	-0.043976	0.035034	0.000006	0.721438
0.216364	-0.082506	0.040038	-0.000037	0.721442
0.151641	-0.072929	0.045043	-0.000025	0.721438
0.285248	-0.091881	0.050048	-0.000049	0.721448
0.154262	-0.073482	0.055053	-0.000025	0.721438
0.121967	-0.067615	0.060058	-0.000019	0.721438
0.077063	-0.056129	0.065062	-0.000011	0.721445
0.107291	-0.115221	0.070067	-0.000017	0.721340
0.113165	-0.224929	0.075072	-0.000018	0.721126
0.036592	-0.212844	0.080077	-0.000003	0.721123
0.024347	-0.211421	0.085082	-0.000001	0.721122
0.155505	-0.231486	0.090086	-0.000026	0.721128
0.138547	-0.233747	0.095091	-0.000022	0.721118
0.217419	-0.244026	0.100096	-0.000037	0.721125
0.216505	-0.335356	0.105101	-0.000037	0.720946
0.187500	-0.365974	0.110106	-0.000032	0.720875
0.391118	-0.399540	0.115110	-0.000070	0.720881
0.224408	-0.374695	0.120115	-0.000039	0.720871
0.351525	-0.392892	0.125120	-0.000062	0.720880
0.164061	-0.523178	0.130125	-0.000027	0.720558
0.024749	-0.509117	0.135130	-0.000001	0.720537
0.029148	-0.506057	0.140134	-0.000002	0.720545
0.163462	-0.535213	0.145139	-0.000027	0.720534
0.229734	-0.654564	0.150144	-0.000040	0.720323
0.228205	-0.704985	0.155149	-0.000039	0.720223
0.310373	-0.720493	0.160154	-0.000055	0.720221
0.447065	-0.756451	0.165158	-0.000080	0.720198
0.281028	-0.880057	0.170163	-0.000049	0.719897
0.241931	-0.869612	0.175168	-0.000042	0.719904
0.172543	-0.860427	0.180173	-0.000029	0.719898
0.133456	-0.976325	0.185178	-0.000022	0.719656
0.115113	-1.000898	0.190182	-0.000018	0.719601
-0.093233	-0.967796	0.195187	0.000020	0.719593
-0.267178	-1.038921	0.200192	0.000053	0.719392
-0.157188	-1.121011	0.205197	0.000032	0.719269
0.110254	-1.168011	0.210202	-0.000018	0.719270
-0.245720	-1.201251	0.215206	0.000049	0.719079
-0.105324	-1.288452	0.220211	0.000022	0.718957
0.031822	-1.308253	0.225216	-0.000003	0.718966
0.093221	-1.456678	0.230221	-0.000014	0.718695
-0.101365	-1.449270	0.235226	0.000022	0.718641
-0.100423	-1.479611	0.240230	0.000022	0.718582
-0.081922	-1.599571	0.245235	0.000018	0.718351
-0.308655	-1.557057	0.250240	0.000060	0.718356
-0.341409	-1.669234	0.255245	0.000066	0.718123
-0.043841	-1.776565	0.260250	0.000011	0.718015
-0.221559	-1.784184	0.265254	0.000044	0.717938
-0.349825	-1.881491	0.270259	0.000068	0.717701
-0.182066	-1.906913	0.275264	0.000037	0.717709
-0.500041	-2.006788	0.280269	0.000096	0.717400
-0.528421	-2.012750	0.285274	0.000101	0.717378
-0.157187	-2.169772	0.290278	0.000032	0.717199
-0.282844	-2.208832	0.295283	0.000055	0.717077
-0.504611	-2.247251	0.300288	0.000097	0.716923
-0.831330	-2.275003	0.305293	0.000158	0.716753
-0.756936	-2.334792	0.310298	0.000144	0.716661
-2.991564	-2.042088	0.315302	0.000560	0.716453
-2.476821	-2.138356	0.320307	0.000464	0.716444
-2.473682	-2.218064	0.325312	0.000463	0.716287
-4.078642	-2.009798	0.330317	0.000762	0.716133
-3.605769	-2.094470	0.335322	0.000674	0.716133
-3.138756	-2.221871	0.340326	0.000587	0.716045
-4.705258	-2.025150	0.345331	0.000878	0.715882
-4.094530	-2.132254	0.350336	0.000765	0.715886
-4.202306	-2.122748	0.355341	0.000785	0.715866
-5.061966	-2.130504	0.360346	0.000945	0.715548
-4.823965	-2.170977	0.365350	0.000900	0.715552
-5.173166	-2.113576	0.370355	0.000965	0.715542
-5.170230	-2.186806	0.375360	0.000965	0.715398
-6.273915	-2.075552	0.380365	0.001170	0.715229
-6.192719	-2.088407	0.385370	0.001155	0.715232
-5.628197	-2.185555	0.390374	0.001050	0.715239
-6.386357	-2.098970	0.395379	0.001191	0.715143
-7.196492	-2.071323	0.400384	0.001342	0.714911
-6.464587	-2.203722	0.405389	0.001206	0.714908
-7.311104	-2.054491	0.410394	0.001363	0.714904
-7.273195	-2.057158	0.415398	0.001356	0.714913
-7.075934	-2.169934	0.420403	0.001319	0.714759
-7.770686	-2.119690	0.425408	0.001448	0.714613
-7.720448	-2.130413	0.430413	0.001439	0.714609
-8.305482	-2.029296	0.435418	0.001548	0.714603
-7.712085	-2.131202	0.440422	0.001437	0.714611
-7.858785	-2.204992	0.445427	0.001465	0.714413
-9.256831	-2.022729	0.450432	0.001725	0.714280
-8.668227	-2.129838	0.455437	0.001615	0.714276
-8.811585	-2.106973	0.460442	0.001642	0.714270
-9.111990	-2.048191	0.465446	0.001698	0.714281
-8.875306	-2.093977	0.470451	0.001654	0.714274
-9.127370	-2.180840	0.475456	0.001701	0.714012
-10.040971	-2.038224	0.480461	0.001871	0.713972
-10.073670	-2.035112	0.485466	0.001877	0.713967
-9.238723	-2.178727	0.490470	0.001721	0.713977
-9.832963	-2.077298	0.495475	0.001832	0.713968
-9.915761	-2.059800	0.500480	0.001847	0.713974
-9.822835	-2.211014	0.505485	0.001830	0.713706
-10.719696	-2.080633	0.510490	0.001997	0.713648
-10.724441	-2.074727	0.515494	0.001998	0.713658
-10.695119	-2.083724	0.520499	0.001992	0.713651
-10.802164	-2.061201	0.525504	0.002012	0.713658
-10.629912	-2.094917	0.530509	0.001980	0.713652
-11.027088	-2.100230	0.535514	0.002054	0.713501
-11.647020	-2.059559	0.540518	0.002169	0.713362
-11.293221	-2.125699	0.545523	0.002103	0.713356
-11.798337	-2.032802	0.550528	0.002197	0.713362
-11.838956	-2.026354	0.555533	0.002205	0.713360
-11.411121	-2.102938	0.560538	0.002125	0.713360
-11.448827	-2.093045	0.565542	0.002132	0.713366
-12.256869	-2.110323	0.570547	0.002282	0.713045
-12.313610	-2.111278	0.575552	0.002293	0.713023
-12.610109	-2.056884	0.580557	0.002348	0.713027
-12.909864	-2.006852	0.585562	0.002404	0.713020
-12.276056	-2.116411	0.590566	0.002286	0.713027
-12.477842	-2.082462	0.595571	0.002323	0.713023
-12.633122	-2.052524	0.600576	0.002352	0.713027
-13.008800	-2.138013	0.605581	0.002422	0.712724
-13.396034	-2.075959	0.610586	0.002494	0.712710
-13.408065	-2.069429	0.615590	0.002496	0.712719
-13.498507	-2.059002	0.620595	0.002513	0.712708
-13.446268	-2.066079	0.625600	0.002503	0.712712
-13.417263	-2.070310	0.630605	0.002498	0.712714
-13.602314	-2.040439	0.635610	0.002532	0.712708
-13.583809	-2.188488	0.640614	0.002529	0.712420
-14.199142	-2.098365	0.645619	0.002643	0.712381
-14.590607	-2.025129	0.650624	0.002716	0.712388
-14.194656	-2.095802	0.655629	0.002643	0.712388
-14.366508	-2.068085	0.660634	0.002674	0.712383
-14.210169	-2.091243	0.665638	0.002645	0.712392
-14.544641	-2.035451	0.670643	0.002708	0.712384
-14.843667	-2.121564	0.675648	0.002763	0.712107
-15.281286	-2.050562	0.680653	0.002845	0.712093
-15.670029	-1.984862	0.685658	0.002917	0.712086
-15.042029	-2.094064	0.690662	0.002800	0.712091
-15.278811	-2.054971	0.695667	0.002844	0.712085
-15.462099	-2.019613	0.700672	0.002878	0.712091
-15.037351	-2.096280	0.705677	0.002799	0.712089
-15.271272	-2.174631	0.710682	0.002843	0.711850
-16.273713	-2.038294	0.715686	0.003029	0.711766
-16.367729	-2.025773	0.720691	0.003047	0.711757
-15.940543	-2.099157	0.725696	0.002967	0.711763
-15.924016	-2.101401	0.730701	0.002964	0.711764
-16.291547	-2.036971	0.735706	0.003032	0.711762
-15.927503	-2.099065	0.740710	0.002964	0.711768
-16.279823	-2.155282	0.745715	0.003030	0.711531
-17.074134	-2.049943	0.750720	0.003178	0.711459
-16.847639	-2.091872	0.755725	0.003136	0.711456
-16.821325	-2.097308	0.760730	0.003131	0.711454
-16.856763	-2.087241	0.765734	0.003137	0.711462
-16.930452	-2.078575	0.770739	0.003151	0.711453
-16.777428	-2.103303	0.775744	0.003122	0.711458
-17.441550	-2.141141	0.780749	0.003246	0.711147
-18.331247	-1.987765	0.785754	0.003412	0.711136
-17.962742	-2.049055	0.790758	0.003343	0.711145
-17.711519	-2.098481	0.795763	0.003296	0.711136
-18.142995	-2.020775	0.800768	0.003376	0.711138
-17.943124	-2.054205	0.805773	0.003339	0.711142
-17.930778	-2.059499	0.810778	0.003337	0.711136
-17.866993	-2.146584	0.815782	0.003325	0.710985
-18.980877	-2.008073	0.820787	0.003532	0.710865
-18.528891	-2.086120	0.825792	0.003448	0.710870
-18.297997	-2.125353	0.830797	0.003405	0.710874
-19.086602	-1.989479	0.835802	0.003552	0.710865
-18.515188	-2.086305	0.840806	0.003445	0.710875
-18.482569	-2.094976	0.845811	0.003439	0.710870
-19.113849	-2.130475	0.850816	0.003557	0.710574
-19.709371	-2.044675	0.855821	0.003668	0.710534
-19.862828	-2.021084	0.860826	0.003696	0.710526
-19.091575	-2.152668	0.865830	0.003552	0.710538
-19.666507	-2.056780	0.870835	0.003659	0.710525
-19.570743	-2.069356	0.875840	0.003642	0.710534
-19.209546	-2.139394	0.880845	0.003574	0.710523
-20.411082	-2.081588	0.885850	0.003798	0.710211
-20.342161	-2.090281	0.890854	0.003785	0.710218
-20.634966	-2.041581	0.895859	0.003840	0.710211
-20.515256	-2.060809	0.900864	0.003817	0.710215
-20.639631	-2.037671	0.905869	0.003840	0.710217
-20.748266	-2.021284	0.910874	0.003860	0.710211
-20.162389	-2.120150	0.915878	0.003751	0.710223
-21.084775	-2.084649	0.920883	0.003923	0.709965
-21.840831	-1.988489	0.925888	0.004064	0.709888
-20.962603	-2.143677	0.930893	0.003900	0.709891
-21.476552	-2.054431	0.935898	0.003996	0.709886
-21.714186	-2.006893	0.940902	0.004040	0.709897
-21.549659	-2.040708	0.945907	0.004009	0.709888
-21.311572	-2.081268	0.950912	0.003965	0.709892
-21.543727	-2.089906	0.955917	0.004008	0.709792
-22.336100	-2.051695	0.960922	0.004156	0.709586
-21.799320	-2.141977	0.965926	0.004056	0.709597
-22.369904	-2.044937	0.970931	0.004162	0.709587
-22.656795	-1.990495	0.975936	0.004215	0.709594
-21.826502	-2.138706	0.980941	0.004061	0.709594
-22.443223	-2.030946	0.985946	0.004175	0.709590
-22.451717	-2.098150	0.990950	0.004177	0.709452
-23.336914	-2.036554	0.995955	0.004342	0.709260
-23.036534	-2.088727	1.000960	0.004286	0.709263
-23.267544	-2.047091	1.005965	0.004329	0.709264
-23.283935	-2.047490	1.010970	0.004332	0.709257
-22.654604	-2.154271	1.015974	0.004215	0.709268
-23.048391	-2.087643	1.020979	0.004288	0.709261
-23.503998	-2.074466	1.025984	0.004373	0.709125
-24.014948	-2.067434	1.030989	0.004468	0.708957
-23.841822	-2.101139	1.035994	0.004435	0.708951
-24.186442	-2.034187	1.040998	0.004500	0.708962
-24.132631	-2.048616	1.046003	0.004489	0.708953
-23.892022	-2.090333	1.051008	0.004445	0.708955
-24.133470	-2.045862	1.056013	0.004490	0.708958
-24.393594	-2.035099	1.061018	0.004538	0.708887
-24.437379	-2.147502	1.066022	0.004546	0.708646
-24.628468	-2.115982	1.071027	0.004582	0.708641
-25.305903	-1.994468	1.076032	0.004708	0.708643
-24.811830	-2.081556	1.081037	0.004616	0.708645
-24.921687	-2.065877	1.086042	0.004636	0.708637
-25.322054	-1.990549	1.091046	0.004710	0.708645
-24.940410	-2.087526	1.096051	0.004639	0.708587
-25.255702	-2.147395	1.101056	0.004698	0.708355
-25.528221	-2.098243	1.106061	0.004749	0.708356
-25.993918	-2.018789	1.111066	0.004835	0.708349
-25.261451	-2.144201	1.116070	0.004699	0.708360
-25.476173	-2.110882	1.121075	0.004739	0.708350
-26.178662	-1.985913	1.126080	0.004870	0.708349
-25.616276	-2.183715	1.131085	0.004765	0.708154
-26.738124	-2.055526	1.136090	0.004974	0.708010
-26.740781	-2.050968	1.141094	0.004974	0.708018
-26.846953	-2.036643	1.146099	0.004994	0.708009
-26.601629	-2.079244	1.151104	0.004948	0.708012
-26.470810	-2.099683	1.156109	0.004924	0.708017
-26.924562	-2.022627	1.161114	0.005008	0.708010
-26.610544	-2.163036	1.166118	0.004950	0.707841
-27.486845	-2.077759	1.171123	0.005113	0.707699
-27.657728	-2.046176	1.176128	0.005145	0.707701
-27.350519	-2.102182	1.181133	0.005087	0.707698
-27.556003	-2.067974	1.186138	0.005126	0.707694
-27.389155	-2.093903	1.191142	0.005095	0.707701
-27.580544	-2.061740	1.196147	0.005130	0.707698
-27.681951	-2.150356	1.201152	0.005149	0.707484
-28.396052	-2.075162	1.206157	0.005282	0.707379
-28.619442	-2.038110	1.211162	0.005323	0.707374
-28.011847	-2.143536	1.216166	0.005210	0.707380
-28.297181	-2.095093	1.221171	0.005263	0.707375
-28.820466	-2.002252	1.226176	0.005361	0.707374
-28.335860	-2.086884	1.231181	0.005270	0.707378
-28.361059	-2.178380	1.236186	0.005275	0.707185
-29.453041	-2.034948	1.241190	0.005478	0.707082
-29.520471	-2.025538	1.246195	0.005491	0.707077
-29.313922	-2.063098	1.251200	0.005452	0.707076
-29.239916	-2.072678	1.256205	0.005439	0.707083
-29.468228	-2.036029	1.261210	0.005481	0.707075
-29.400270	-2.043014	1.266214	0.005468	0.707086
-29.060154	-2.168644	1.271219	0.005405	0.706955
-30.280991	-2.051890	1.276224	0.005632	0.706753
-29.827015	-2.131651	1.281229	0.005548	0.706755
-30.224082	-2.065113	1.286234	0.005622	0.706747
-30.114989	-2.077957	1.291238	0.005601	0.706760
-29.982452	-2.105511	1.296243	0.005576	0.706752
-30.259636	-2.055990	1.301248	0.005628	0.706752
-30.359035	-2.132343	1.306253	0.005647	0.706564
-31.581386	-1.975095	1.311258	0.005874	0.706442
-30.930369	-2.088428	1.316262	0.005753	0.706447
-30.862582	-2.103623	1.321267	0.005740	0.706441
-31.162127	-2.048134	1.326272	0.005796	0.706446
-30.867618	-2.100403	1.331277	0.005741	0.706446
-30.779269	-2.118370	1.336282	0.005724	0.706442
-30.977358	-2.187107	1.341286	0.005761	0.706233
-32.165957	-2.028580	1.346291	0.005983	0.706125
-31.847791	-2.084524	1.351296	0.005923	0.706127
-31.417955	-2.159055	1.356301	0.005843	0.706131
-32.101553	-2.040151	1.361306	0.005970	0.706126
-31.842699	-2.083387	1.366310	0.005922	0.706132
-31.468760	-2.151331	1.371315	0.005853	0.706129
-32.224945	-2.138113	1.376320	0.005993	0.705885
-32.543155	-2.089542	1.381325	0.006053	0.705868
-32.660333	-2.074246	1.386330	0.006074	0.705857
-32.473449	-2.102442	1.391334	0.006039	0.705868
-32.597453	-2.085192	1.396339	0.006062	0.705858
-32.725722	-2.061671	1.401344	0.006086	0.705859
-32.589798	-2.130765	1.406349	0.006061	0.705769
-33.951327	-2.011117	1.411354	0.006314	0.705522
-33.432089	-2.100504	1.416358	0.006218	0.705528
-33.270060	-2.132612	1.421363	0.006188	0.705522
-33.631187	-2.068045	1.426368	0.006255	0.705522
-33.542616	-2.080115	1.431373	0.006238	0.705530
-33.577878	-2.079186	1.436378	0.006245	0.705519
-33.414755	-2.160670	1.441382	0.006214	0.705414
-34.686019	-2.037077	1.446387	0.006451	0.705206
-34.730812	-2.029096	1.451392	0.006459	0.705206
-34.293320	-2.105387	1.456397	0.006378	0.705210
-34.526117	-2.067108	1.461402	0.006421	0.705204
-34.358972	-2.092605	1.466406	0.006390	0.705212
-34.462460	-2.076177	1.471411	0.006409	0.705208
-34.849106	-2.007175	1.476416	0.006481	0.705209
-35.099558	-2.118394	1.481421	0.006528	0.704895
-35.346744	-2.080066	1.486426	0.006574	0.704883
-35.456737	-2.056469	1.491430	0.006594	0.704891
-35.327195	-2.082668	1.496435	0.006570	0.704885
-35.356182	-2.075373	1.501440	0.006575	0.704890
-35.323494	-2.080275	1.506445	0.006569	0.704892
-35.588905	-2.037303	1.511450	0.006618	0.704883
-36.086227	-2.069881	1.516454	0.006711	0.704639
-36.206306	-2.075438	1.521459	0.006733	0.704585
-36.380533	-2.042987	1.526464	0.006766	0.704587
-36.528944	-2.013318	1.531469	0.006793	0.704594
-36.572662	-2.011144	1.536474	0.006801	0.704583
-36.062935	-2.097568	1.541478	0.006706	0.704592
-36.166828	-2.080328	1.546483	0.006726	0.704589
-36.637315	-2.092815	1.551488	0.006813	0.704395
-37.082904	-2.078971	1.556493	0.006896	0.704263
-37.043627	-2.089772	1.561498	0.006889	0.704255
-37.305494	-2.039179	1.566502	0.006938	0.704263
-36.907674	-2.112470	1.571507	0.006863	0.704259
-36.811675	-2.128505	1.576512	0.006846	0.704261
-37.248220	-2.048048	1.581517	0.006927	0.704266
-37.749287	-2.079108	1.586522	0.007020	0.704024
-38.024301	-2.064680	1.591526	0.007071	0.703954
-38.035758	-2.064653	1.596531	0.007073	0.703950
-37.990203	-2.073515	1.601536	0.007065	0.703949
-37.668199	-2.127562	1.606541	0.007005	0.703956
-37.951732	-2.081892	1.611546	0.007058	0.703946
-38.067115	-2.057610	1.616550	0.007079	0.703953
-38.017250	-2.193762	1.621555	0.007070	0.703697
-38.919498	-2.065977	1.626560	0.007238	0.703630
-38.834093	-2.077225	1.631565	0.007222	0.703638
-38.814883	-2.085373	1.636570	0.007218	0.703629
-38.604830	-2.119115	1.641574	0.007179	0.703636
-38.724352	-2.099472	1.646579	0.007201	0.703633
-39.030629	-2.063978	1.651584	0.007258	0.703595
-39.088123	-2.178099	1.656589	0.007269	0.703344
-39.500377	-2.108660	1.661594	0.007345	0.703336
-39.843159	-2.043682	1.666598	0.007409	0.703343
-39.639838	-2.082334	1.671603	0.007371	0.703339
-39.615391	-2.088785	1.676608	0.007367	0.703335
-39.512822	-2.101277	1.681613	0.007348	0.703346
-39.837196	-2.125444	1.686618	0.007408	0.703181
-40.672818	-2.062377	1.691622	0.007563	0.703007
-40.479659	-2.097363	1.696627	0.007527	0.703006
-40.851977	-2.033070	1.701632	0.007597	0.703002
-40.382573	-2.111088	1.706637	0.007509	0.703014
-40.561415	-2.082760	1.711642	0.007543	0.703007
-40.731569	-2.050107	1.716646	0.007574	0.703011
-40.799198	-2.078242	1.721651	0.007587	0.702930
-41.525060	-2.068239	1.726656	0.007722	0.702689
-41.142642	-2.131910	1.731661	0.007651	0.702698
-41.727356	-2.031290	1.736666	0.007759	0.702691
-41.193012	-2.124599	1.741670	0.007660	0.702695
-41.086053	-2.144138	1.746675	0.007640	0.702694
-41.750508	-2.026750	1.751680	0.007764	0.702692
-41.270413	-2.180217	1.756685	0.007674	0.702555
-42.265172	-2.097955	1.761690	0.007859	0.702363
-42.199748	-2.105069	1.766694	0.007847	0.702372
-42.545169	-2.044023	1.771699	0.007911	0.702371
-42.472039	-2.058109	1.776704	0.007898	0.702369
-41.977799	-2.142534	1.781709	0.007806	0.702377
-42.361116	-2.078707	1.786714	0.007877	0.702368
-42.522950	-2.123897	1.791718	0.007907	0.702218
-43.211500	-2.072412	1.796723	0.008035	0.702074
-43.562323	-2.011867	1.801728	0.008100	0.702070
-43.004974	-2.106815	1.806733	0.007997	0.702079
-43.139175	-2.087598	1.811738	0.008022	0.702070
-43.050801	-2.100543	1.816742	0.008005	0.702075
-43.241843	-2.066445	1.821747	0.008041	0.702076
-43.611015	-2.065757	1.826752	0.008109	0.701944
-44.066690	-2.079988	1.831757	0.008194	0.701751
-44.268963	-2.048206	1.836762	0.008232	0.701742
-44.050911	-2.083351	1.841766	0.008191	0.701750
-43.792465	-2.130597	1.846771	0.008143	0.701748
-44.289053	-2.044444	1.851776	0.008235	0.701743
-44.037024	-2.085840	1.856781	0.008188	0.701750
-44.158547	-2.108993	1.861786	0.008211	0.701660
-45.309705	-2.013393	1.866790	0.008425	0.701438
-45.240508	-2.026199	1.871795	0.008412	0.701437
-45.332495	-2.011574	1.876800	0.008429	0.701433
-44.580521	-2.140195	1.881805	0.008289	0.701444
-44.955573	-2.080029	1.886810	0.008359	0.701431
-44.809988	-2.102254	1.891814	0.008332	0.701439
-44.551196	-2.178246	1.896819	0.008284	0.701378
-45.945744	-2.057924	1.901824	0.008543	0.701118
-45.762415	-2.087422	1.906829	0.008509	0.701125
-46.022337	-2.047358	1.911834	0.008558	0.701112
-45.583518	-2.120951	1.916838	0.008476	0.701122
-45.635957	-2.112028	1.921843	0.008486	0.701121
-45.881400	-2.069652	1.926848	0.008531	0.701118
-45.563664	-2.172903	1.931853	0.008472	0.701024
-46.750103	-2.037387	1.936858	0.008693	0.700870
-46.365001	-2.102290	1.941862	0.008621	0.700878
-46.060674	-2.158374	1.946867	0.008564	0.700874
-46.527906	-2.076253	1.951872	0.008651	0.700872
-46.277869	-2.117109	1.956877	0.008605	0.700880
-46.166770	-2.166740	1.961882	0.008584	0.700819
-47.112621	-2.136636	1.966886	0.008760	0.700538
-47.496507	-2.068414	1.971891	0.008832	0.700538
-47.832701	-2.010736	1.976896	0.008894	0.700534
-46.983706	-2.157983	1.981901	0.008736	0.700542
-47.450796	-2.078927	1.986906	0.008823	0.700534
-47.710930	-2.030694	1.991910	0.008871	0.700537
-47.477016	-2.126273	1.996915	0.008828	0.700428
-48.338663	-2.076116	2.001920	0.008988	0.700218

-48.166940	-2.107519	2.011917	0.008956	0.700217
-48.352398	-2.073144	2.021914	0.008990	0.700220
-48.222258	-2.095861	2.031910	0.008966	0.700221
-48.179130	-2.102944	2.041907	0.008958	0.700222
-48.244439	-2.091306	2.051904	0.008970	0.700223
-48.087334	-2.122723	2.061901	0.008941	0.700216
-48.192445	-2.104680	2.071898	0.008960	0.700215
-48.064717	-2.125888	2.081894	0.008936	0.700218
-48.072908	-2.122740	2.091891	0.008938	0.700222
-48.340558	-2.076906	2.101888	0.008988	0.700218
-48.114994	-2.117719	2.111885	0.008945	0.700217
-48.296127	-2.086273	2.121882	0.008979	0.700215
-48.063547	-2.128722	2.131878	0.008936	0.700214
-47.809701	-2.084667	2.141875	0.008888	0.700395
-47.278017	-2.110722	2.151872	0.008789	0.700534
-47.213852	-2.123214	2.161869	0.008777	0.700532
-47.217706	-2.122960	2.171866	0.008778	0.700532
-47.158188	-2.132426	2.181862	0.008767	0.700534
-46.899527	-2.094547	2.191859	0.008718	0.700705
-46.418175	-2.098092	2.201856	0.008629	0.700872
-46.397408	-2.103964	2.211853	0.008625	0.700867
-46.691608	-2.051626	2.221850	0.008679	0.700867
-46.216912	-2.077806	2.231846	0.008591	0.700986
-45.975567	-2.053758	2.241843	0.008546	0.701122
-45.871155	-2.074161	2.251840	0.008526	0.701119
-45.953943	-2.042969	2.261837	0.008542	0.701152
-45.088801	-2.059388	2.271834	0.008381	0.701431
-44.815505	-2.106934	2.281830	0.008330	0.701434
-44.956589	-2.080704	2.291827	0.008356	0.701436
-44.541864	-2.056752	2.301824	0.008278	0.701635
-44.067120	-2.089512	2.311821	0.008190	0.701740
-44.349352	-2.038770	2.321818	0.008242	0.701741
-43.817204	-2.109452	2.331814	0.008143	0.701790
-43.377858	-2.048648	2.341811	0.008061	0.702072
-42.987483	-2.118535	2.351808	0.007989	0.702071
-43.414214	-2.043149	2.361805	0.008068	0.702070
-42.743876	-2.062554	2.371802	0.007943	0.702273
-42.425646	-2.071064	2.381798	0.007884	0.702370
-42.367104	-2.082864	2.391795	0.007873	0.702368
-42.205849	-2.082283	2.401792	0.007843	0.702427
-41.739174	-2.036119	2.411789	0.007756	0.702689
-41.526413	-2.073870	2.421786	0.007716	0.702689
-41.443485	-2.088432	2.431782	0.007700	0.702690
-40.874436	-2.063332	2.441779	0.007594	0.702946
-40.651792	-2.073902	2.451776	0.007553	0.703005
-40.806091	-2.049224	2.461773	0.007581	0.702999
-40.349352	-2.075409	2.471770	0.007496	0.703111
-39.670045	-2.083473	2.481766	0.007370	0.703340
-39.696698	-2.078459	2.491763	0.007375	0.703340
-39.637883	-2.089418	2.501760	0.007363	0.703339
-39.262248	-2.042641	2.511757	0.007293	0.703569
-38.849505	-2.086921	2.521754	0.007217	0.703629
-38.848274	-2.085406	2.531750	0.007216	0.703632
-38.814490	-2.040310	2.541747	0.007210	0.703736
-37.753359	-2.123391	2.551744	0.007012	0.703950
-38.072639	-2.068452	2.561741	0.007071	0.703946
-37.921013	-2.095300	2.571738	0.007043	0.703946
-37.609652	-2.029050	2.581734	0.006985	0.704192
-37.013071	-2.103672	2.591731	0.006874	0.704256
-37.219662	-2.067546	2.601728	0.006912	0.704255
-37.289055	-1.985940	2.611725	0.006925	0.704395
-36.154466	-2.093912	2.621722	0.006714	0.704585
-36.326666	-2.062678	2.631718	0.006746	0.704586
-36.317402	-2.060847	2.641715	0.006744	0.704593
-35.541150	-2.053767	2.651712	0.006599	0.704887
-35.714290	-2.025624	2.661709	0.006631	0.704881
-35.354394	-2.088668	2.671706	0.006564	0.704884
-35.119919	-2.026200	2.681702	0.006521	0.705094
-34.551689	-2.070601	2.691699	0.006415	0.705209
-34.693946	-2.044511	2.701696	0.006441	0.705210
-34.635912	-2.014256	2.711693	0.006430	0.705292
-33.569847	-2.088629	2.721690	0.006232	0.705525
-33.790531	-2.049530	2.731686	0.006273	0.705525
-33.551234	-2.092508	2.741683	0.006228	0.705524
-33.161719	-2.040326	2.751680	0.006155	0.705769
-33.002349	-2.022078	2.761677	0.006126	0.705863
-32.743464	-2.068353	2.771674	0.006077	0.705863
-32.810661	-2.021446	2.781670	0.006090	0.705934
-31.754346	-2.113128	2.791667	0.005893	0.706128
-32.087739	-2.054172	2.801664	0.005955	0.706127
-32.015641	-2.066138	2.811661	0.005941	0.706129
-31.272396	-2.076433	2.821658	0.005803	0.706375
-31.315014	-2.034115	2.831654	0.005811	0.706445
-31.172641	-2.060047	2.841651	0.005784	0.706444
-31.107229	-2.003530	2.851648	0.005772	0.706581
-30.154783	-2.089436	2.861645	0.005595	0.706750
-30.286763	-2.065607	2.871642	0.005619	0.706751
-30.370212	-2.049884	2.881638	0.005634	0.706752
-29.526727	-2.040948	2.891635	0.005477	0.707072
-29.604881	-2.023405	2.901632	0.005492	0.707080
-29.364436	-2.067362	2.911629	0.005447	0.707078
-29.190189	-2.005922	2.921626	0.005414	0.707264
-28.743484	-2.029009	2.931622	0.005331	0.707377
-28.675704	-2.040242	2.941619	0.005318	0.707379
-28.631365	-1.991521	2.951616	0.005310	0.707493
-27.558824	-2.079928	2.961613	0.005110	0.707699
-27.836684	-2.031345	2.971610	0.005162	0.707698
-27.712012	-2.052367	2.981606	0.005139	0.707700
-27.118769	-2.025765	2.991603	0.005028	0.707966
-26.933774	-2.034344	3.001600	0.004993	0.708015
-26.770455	-2.065020	3.011597	0.004963	0.708012
-26.884711	-1.975190	3.021594	0.004984	0.708151
-25.981618	-2.036369	3.031590	0.004816	0.708351
-25.847160	-2.059483	3.041587	0.004791	0.708353
-26.153331	-2.004375	3.051584	0.004848	0.708354
-25.235100	-2.027018	3.061581	0.004677	0.708637
-25.496846	-1.979751	3.071578	0.004725	0.708639
-25.027247	-2.061855	3.081574	0.004638	0.708642
-24.741263	-2.015116	3.091571	0.004584	0.708838
-24.392339	-2.018098	3.101568	0.004519	0.708956
-24.361375	-2.025576	3.111565	0.004514	0.708953
-24.374652	-1.989840	3.121562	0.004516	0.709020
-23.574960	-2.010348	3.131558	0.004367	0.709264
-23.265889	-2.064657	3.141555	0.004309	0.709266
-23.535769	-2.016879	3.151552	0.004359	0.709265
-22.812013	-2.011734	3.161549	0.004225	0.709534
-22.782025	-1.987587	3.171546	0.004219	0.709593
-22.368906	-2.059618	3.181542	0.004142	0.709596
-22.350552	-2.022414	3.191539	0.004138	0.709677
-21.596177	-2.049066	3.201536	0.003998	0.709893
-21.587222	-2.050787	3.211533	0.003996	0.709893
-21.777202	-2.017446	3.221530	0.004031	0.709892
-21.013752	-2.049317	3.231526	0.003889	0.710101
-20.722710	-2.043353	3.241523	0.003835	0.710216
-20.669279	-2.051709	3.251520	0.003825	0.710219
-20.614881	-2.061880	3.261517	0.003815	0.710218
-20.149621	-1.987230	3.271514	0.003728	0.710533
-19.393842	-2.120748	3.281510	0.003587	0.710536
-19.742103	-2.059750	3.291507	0.003652	0.710534
-19.623543	-2.039603	3.301504	0.003630	0.710616
-19.081031	-2.007791	3.311501	0.003528	0.710873
-18.925681	-2.036187	3.321498	0.003499	0.710872
-18.921264	-2.036081	3.331494	0.003499	0.710874
-18.434958	-2.008927	3.341491	0.003408	0.711101
-18.287737	-2.015667	3.351488	0.003380	0.711140
-18.189100	-2.032820	3.361485	0.003362	0.711141
-17.988145	-1.985367	3.371482	0.003324	0.711307
-17.054262	-2.076999	3.381478	0.003151	0.711457
-17.620462	-1.975369	3.391475	0.003256	0.711458
-17.247902	-2.012181	3.401472	0.003186	0.711518
-16.738298	-1.980052	3.411469	0.003091	0.711763
-16.375958	-2.044429	3.421466	0.003024	0.711763
-16.427883	-2.035027	3.431462	0.003033	0.711764
-15.815244	-2.006113	3.441459	0.002919	0.712039
-15.245854	-2.080597	3.451456	0.002813	0.712093
-15.478013	-2.038609	3.461453	0.002856	0.712095
-15.481011	-2.020042	3.471450	0.002857	0.712131
-14.740897	-2.022200	3.481446	0.002719	0.712389
-14.630526	-2.042188	3.491443	0.002698	0.712389
-14.695121	-2.031235	3.501440	0.002710	0.712388
-14.262373	-1.983560	3.511437	0.002629	0.712637
-13.765276	-2.035754	3.521434	0.002537	0.712709
-13.785074	-2.030271	3.531430	0.002540	0.712713
-13.705011	-1.996219	3.541427	0.002525	0.712810
-12.853590	-2.039399	3.551424	0.002367	0.713026
-12.768202	-2.055131	3.561421	0.002351	0.713025
-12.964815	-2.019792	3.571418	0.002387	0.713026
-12.405463	-1.993022	3.581414	0.002283	0.713277
-11.811691	-2.056548	3.591411	0.002172	0.713362
-11.827040	-2.054095	3.601408	0.002175	0.713361
-11.876588	-2.041660	3.611405	0.002184	0.713369
-11.307501	-2.001070	3.621402	0.002078	0.713651
-11.143250	-2.029241	3.631398	0.002048	0.713653
-11.308120	-1.999166	3.641395	0.002078	0.713655
-10.474681	-2.034555	3.651392	0.001923	0.713880
-10.520659	-1.981581	3.661389	0.001931	0.713969
-10.135590	-2.049879	3.671386	0.001860	0.713970
-10.129416	-2.026170	3.681382	0.001858	0.714019
-9.328470	-2.038749	3.691379	0.001709	0.714278
-9.191665	-2.062696	3.701376	0.001684	0.714279
-9.428475	-2.021300	3.711373	0.001728	0.714278
-8.844512	-2.042909	3.721370	0.001619	0.714442
-8.356941	-2.044057	3.731366	0.001528	0.714612
-8.482187	-2.022065	3.741363	0.001551	0.714611
-8.305335	-2.054800	3.751360	0.001518	0.714609
-7.816715	-2.010358	3.761357	0.001427	0.714870
-7.338643	-2.076238	3.771354	0.001338	0.714909
-7.433932	-2.059466	3.781350	0.001356	0.714909
-6.971857	-2.128363	3.791347	0.001270	0.714935
-6.534207	-2.057793	3.801344	0.001188	0.715230
-6.403693	-2.080696	3.811341	0.001164	0.715231
-6.160591	-2.125469	3.821338	0.001118	0.715228
-6.317806	-2.060668	3.831334	0.001147	0.715302
-5.087994	-2.154827	3.841331	0.000918	0.715549
-5.143908	-2.146174	3.851328	0.000929	0.715547
-5.410775	-2.099113	3.861325	0.000978	0.715546
-5.051953	-2.158272	3.871322	0.000911	0.715556
-4.721098	-2.051936	3.881318	0.000850	0.715884
-4.183962	-2.148220	3.891315	0.000750	0.715883
-4.604802	-2.073535	3.901312	0.000828	0.715882
-4.227629	-2.106024	3.911309	0.000757	0.715951
-3.595622	-2.128085	3.921306	0.000640	0.716131
-3.672020	-2.113654	3.931302	0.000654	0.716132
-3.641873	-2.118716	3.941299	0.000648	0.716133
-3.083076	-2.086351	3.951296	0.000544	0.716395
-2.873923	-2.096974	3.961293	0.000505	0.716448
-2.775189	-2.114371	3.971290	0.000486	0.716448
-2.812329	-2.051474	3.981286	0.000493	0.716560
-1.821157	-2.128305	3.991283	0.000309	0.716757
-2.124461	-2.076220	4.001280	0.000365	0.716754
-2.072627	-2.073732	4.011277	0.000355	0.716777
-1.595554	-2.004007	4.021274	0.000266	0.717083
-1.580862	-2.005011	4.031270	0.000264	0.717087
-1.278591	-2.056647	4.041267	0.000207	0.717091
-1.251592	-1.914033	4.051264	0.000202	0.717383
-1.587096	-1.855070	4.061261	0.000264	0.717381
-1.039350	-1.870780	4.071258	0.000162	0.717543
-1.252828	-1.750645	4.081254	0.000202	0.717706
-0.884942	-1.776517	4.091251	0.000133	0.717784
-0.719205	-1.687111	4.101248	0.000102	0.718020
-0.780930	-1.656581	4.111245	0.000114	0.718058
-0.695441	-1.521928	4.121242	0.000098	0.718355
-0.891222	-1.447367	4.131238	0.000134	0.718433
-0.809080	-1.353377	4.141235	0.000118	0.718648
-0.488890	-1.318463	4.151232	0.000059	0.718829
-0.587673	-1.234455	4.161229	0.000077	0.718961
-0.402842	-1.118176	4.171226	0.000042	0.719255
-0.394464	-1.040373	4.181222	0.000041	0.719412
-0.519613	-0.917562	4.191219	0.000064	0.719610
-0.378705	-0.796021	4.201216	0.000037	0.719899
-0.330160	-0.693403	4.211213	0.000028	0.720118
-0.233950	-0.598842	4.221210	0.000010	0.720339
-0.354259	-0.447943	4.231206	0.000032	0.720594
-0.138293	-0.340717	4.241203	-0.000008	0.720881
-0.029702	-0.239422	4.251200	-0.000028	0.721118
-0.090201	-0.096370	4.261197	-0.000017	0.721378
-0.264170	0.075363	4.271194	0.000015	0.721655
0.000000	0.205685	4.281190	-0.000035	0.722004

0.218854	0.817994	4.286195	-0.000076	0.723282
0.080650	2.107039	4.291200	-0.000051	0.725758
0.491642	3.886457	4.296205	-0.000129	0.729370
0.485846	6.290389	4.301210	-0.000129	0.734028
0.967527	9.123484	4.306214	-0.000221	0.739647
1.204089	12.474046	4.311219	-0.000267	0.746125
1.697786	16.241507	4.316224	-0.000361	0.753418
2.140229	20.421727	4.321229	-0.000447	0.761394
2.367173	25.037308	4.326234	-0.000492	0.770018
2.746230	29.999544	4.331238	-0.000566	0.779227
3.101700	35.299230	4.336243	-0.000635	0.788928
3.480376	40.923260	4.341248	-0.000710	0.799094
4.115649	46.800397	4.346253	-0.000832	0.809656
4.243137	53.051958	4.351258	-0.000860	0.820573
4.935840	59.475732	4.356262	-0.000993	0.831810
5.393439	66.160552	4.361267	-0.001082	0.843267
5.796389	73.088517	4.366272	-0.001162	0.854958
7.841418	79.929217	4.371277	-0.001547	0.866821
9.204338	87.116986	4.376282	-0.001806	0.878889
9.451789	94.673336	4.381286	-0.001857	0.891067
10.542820	102.230767	4.386291	-0.002065	0.903315
11.110238	110.044140	4.391296	-0.002176	0.915653
14.245439	117.532382	4.396301	-0.002765	0.928017
16.451962	125.369563	4.401306	-0.003181	0.940498
17.159713	133.570900	4.406310	-0.003318	0.952966
17.395545	141.904665	4.411315	-0.003367	0.965346
17.789139	150.302550	4.416320	-0.003446	0.977702
18.894756	158.641986	4.421325	-0.003657	0.989998
20.183714	166.997755	4.426330	-0.003903	1.002210
21.106619	175.474226	4.431334	-0.004080	1.014354
21.604080	184.047695	4.436339	-0.004178	1.026386
22.364948	192.624450	4.441344	-0.004326	1.038345
22.846097	201.259835	4.446349	-0.004421	1.050181
23.759638	209.841437	4.451354	-0.004597	1.061913
24.702946	218.464616	4.456358	-0.004778	1.073578
25.555030	227.073145	4.461363	-0.004942	1.085077
26.410082	235.718611	4.466368	-0.005107	1.096504
27.217873	244.366851	4.471373	-0.005263	1.107806
27.918301	253.031638	4.476378	-0.005399	1.118990
28.694174	261.699042	4.481382	-0.005550	1.130083
29.239544	270.384351	4.486387	-0.005657	1.141041
30.092726	279.050471	4.491392	-0.005821	1.151935
30.860217	287.688454	4.496397	-0.005970	1.162675
31.396103	296.337544	4.501402	-0.006075	1.173282
32.387687	304.903830	4.506406	-0.006266	1.183787
33.343529	313.472033	4.511411	-0.006449	1.194195
34.196703	322.048841	4.516416	-0.006614	1.204502
35.145805	330.609878	4.521421	-0.006796	1.214721
35.766436	339.208221	4.526426	-0.006917	1.224833
36.433808	347.815165	4.531430	-0.007047	1.234882
36.553264	356.441828	4.536435	-0.007075	1.244765
37.374058	364.959312	4.541440	-0.007234	1.254581
38.088122	373.463177	4.546445	-0.007372	1.264286
38.534513	382.010411	4.551450	-0.007461	1.273914
39.619404	390.435790	4.556454	-0.007668	1.283453
39.925033	398.982788	4.561459	-0.007731	1.292912
40.896878	407.410998	4.566464	-0.007917	1.302294
41.372367	415.981241	4.571469	-0.008012	1.311672
41.846629	424.488596	4.576474	-0.008106	1.320915
42.611958	432.890125	4.581478	-0.008254	1.330034
42.826832	441.357675	4.586483	-0.008299	1.339062
43.681830	449.721118	4.591488	-0.008464	1.348033
44.198081	458.140455	4.596493	-0.008565	1.356943
44.657107	466.517246	4.601498	-0.008656	1.365741
45.434278	474.876684	4.606502	-0.008807	1.374519
45.673767	483.289386	4.611507	-0.008857	1.383204
46.368351	491.643074	4.616512	-0.008992	1.391852
47.087640	499.962112	4.621517	-0.009131	1.400415
47.620491	508.311307	4.626522	-0.009236	1.408925
48.247413	516.658025	4.631526	-0.009358	1.417397
48.347448	525.038871	4.636531	-0.009382	1.425765
49.042726	533.360079	4.641536	-0.009517	1.434123
49.474473	541.686109	4.646541	-0.009603	1.442394
49.736887	550.030146	4.651546	-0.009657	1.450608
50.398182	558.312950	4.656550	-0.009786	1.458780
50.665817	566.641864	4.661555	-0.009841	1.466888
51.285365	574.972111	4.666560	-0.009962	1.475009
51.675296	583.249991	4.671565	-0.010040	1.482998
52.165545	591.508388	4.676570	-0.010137	1.490942
52.924401	599.745849	4.681574	-0.010283	1.498865
53.153007	608.042747	4.686579	-0.010331	1.506721
53.747621	616.309473	4.691584	-0.010448	1.514564
54.250271	624.552466	4.696589	-0.010547	1.522329
54.545971	632.829742	4.701594	-0.010607	1.530056
55.267321	641.067129	4.706598	-0.010747	1.537771
56.047798	649.256515	4.711603	-0.010897	1.545412
56.412871	657.569285	4.716608	-0.010971	1.553066
56.809542	665.809586	4.721613	-0.011050	1.560621
57.306197	674.018206	4.726618	-0.011148	1.568126
58.200420	682.203160	4.731622	-0.011320	1.575631
58.864597	690.397985	4.736627	-0.011449	1.583076
59.376509	698.639555	4.741632	-0.011550	1.590505
59.950339	706.873375	4.746637	-0.011662	1.597902
60.317638	715.094661	4.751642	-0.011736	1.605224
60.823119	723.337311	4.756646	-0.011835	1.612551
61.468928	731.520615	4.761651	-0.011961	1.619813
61.681539	739.785976	4.766656	-0.012006	1.627053
61.852264	748.102346	4.771661	-0.012043	1.634299
62.022009	756.308747	4.776666	-0.012080	1.641418
62.564867	764.476465	4.781670	-0.012187	1.648524
63.197395	772.635135	4.786675	-0.012310	1.655604
63.759066	780.798759	4.791680	-0.012420	1.662648
64.596304	788.932368	4.796685	-0.012581	1.669674
64.899503	797.155377	4.801690	-0.012643	1.676674
65.129200	805.371683	4.806694	-0.012691	1.683630
65.723607	813.523751	4.811699	-0.012807	1.690551
66.258108	821.713936	4.816704	-0.012912	1.697468
66.777219	829.885132	4.821709	-0.013014	1.704339
66.995414	838.111086	4.826714	-0.013060	1.711188
67.590070	846.283553	4.831718	-0.013176	1.718014
67.874239	854.453558	4.836723	-0.013234	1.724771
68.121925	862.650017	4.841728	-0.013286	1.731519
68.577473	870.815295	4.846733	-0.013376	1.738241
69.069091	878.948553	4.851738	-0.013473	1.744916
69.445161	887.145460	4.856742	-0.013548	1.751603
69.693739	895.319193	4.861747	-0.013600	1.758229
70.394173	903.410552	4.866752	-0.013736	1.764820
71.004114	911.549720	4.871757	-0.013855	1.771414
71.237894	919.733490	4.876762	-0.013904	1.777972
71.617676	927.904589	4.881766	-0.013980	1.784513
71.979020	936.090770	4.886771	-0.014052	1.791041
72.463022	944.257467	4.891776	-0.014148	1.797544
72.841452	952.382466	4.896781	-0.014224	1.803978
73.207304	960.517850	4.901786	-0.014297	1.810395
73.635994	968.673180	4.906790	-0.014382	1.816813
73.964933	976.804616	4.911795	-0.014449	1.823178
74.393857	984.943760	4.916800	-0.014534	1.829538
74.628942	993.117793	4.921805	-0.014583	1.835880
74.938721	1001.242442	4.926810	-0.014646	1.842171
75.689603	1009.327300	4.931814	-0.014791	1.848462
76.207509	1017.459146	4.936819	-0.014893	1.854740
76.642493	1025.586387	4.941824	-0.014980	1.860983
76.933734	1033.753020	4.946829	-0.015039	1.867219
77.367910	1041.909110	4.951834	-0.015125	1.873442
77.873378	1050.018657	4.956838	-0.015225	1.879618
78.531949	1058.089001	4.961843	-0.015353	1.885761
78.925702	1066.243025	4.966848	-0.015431	1.891917
79.093583	1074.422280	4.971853	-0.015468	1.898046
79.396798	1082.532240	4.976858	-0.015530	1.904118
79.903929	1090.671840	4.981862	-0.015630	1.910217
80.353608	1098.792301	4.986867	-0.015719	1.916275
80.745432	1106.898859	4.991872	-0.015797	1.922297
81.246378	1115.009215	4.996877	-0.015896	1.928315
81.735836	1123.128752	5.001882	-0.015992	1.934320
82.128607	1131.254492	5.006886	-0.016070	1.940300
82.403827	1139.380181	5.011891	-0.016127	1.946248
83.180135	1147.492829	5.016896	-0.016277	1.952223
83.639556	1155.620201	5.021901	-0.016368	1.958157
83.571426	1163.764948	5.026906	-0.016361	1.964027
84.006884	1171.861583	5.031910	-0.016447	1.969900
84.352466	1179.977882	5.036915	-0.016517	1.975760
84.693902	1188.083144	5.041920	-0.016586	1.981594
84.979935	1196.197612	5.046925	-0.016644	1.987411
85.425015	1204.307193	5.051930	-0.016732	1.993225
85.844138	1212.409858	5.056934	-0.016816	1.999014
86.201455	1220.496676	5.061939	-0.016888	2.004768
86.578079	1228.608176	5.066944	-0.016963	2.010526
87.106733	1236.710097	5.071949	-0.017067	2.016275
87.082335	1244.850821	5.076954	-0.017068	2.021979
87.658510	1252.936680	5.081958	-0.017180	2.027689
87.966491	1261.071423	5.086963	-0.017243	2.033391
88.041988	1269.200939	5.091968	-0.017262	2.039048
88.550902	1277.254030	5.096973	-0.017362	2.044681
89.154562	1285.303416	5.101978	-0.017480	2.050306
89.732501	1293.399813	5.106982	-0.017593	2.055945
90.218393	1301.469849	5.111987	-0.017689	2.061541
90.739712	1309.560231	5.116992	-0.017791	2.067139
91.028586	1317.710555	5.121997	-0.017850	2.072739
91.152930	1325.824840	5.127002	-0.017879	2.078284
91.637422	1333.905738	5.132006	-0.017974	2.083826
92.038384	1342.000405	5.137011	-0.018054	2.089355
92.170277	1350.139720	5.142016	-0.018084	2.094873
92.360792	1358.244619	5.147021	-0.018125	2.100359
92.868259	1366.310592	5.152026	-0.018225	2.105836
93.387067	1374.435463	5.157030	-0.018327	2.111338
93.312099	1382.617685	5.162035	-0.018318	2.116807
93.600049	1390.668972	5.167040	-0.018377	2.122210
94.220353	1398.708658	5.172045	-0.018498	2.127623
94.487285	1406.788339	5.177050	-0.018553	2.133015
94.901973	1414.868650	5.182054	-0.018635	2.138407
95.167353	1422.942608	5.187059	-0.018690	2.143768
95.426090	1431.039366	5.192064	-0.018744	2.149130
95.997909	1439.117971	5.197069	-0.018855	2.154495
96.302507	1447.177153	5.202074	-0.018917	2.159810
97.002827	1455.215054	5.207078	-0.019053	2.165134
97.128048	1463.348219	5.212083	-0.019082	2.170454
97.468551	1471.444671	5.217088	-0.019150	2.175756
97.822801	1479.528387	5.222093	-0.019222	2.181039
98.177305	1487.599136	5.227098	-0.019293	2.186301
98.481327	1495.733266	5.232102	-0.019355	2.191586
98.991079	1503.801459	5.237107	-0.019455	2.196834
99.457936	1511.845824	5.242112	-0.019547	2.202051
99.692561	1519.948944	5.247117	-0.019596	2.207272
100.150660	1528.016285	5.252122	-0.019687	2.212478
100.534838	1536.100889	5.257126	-0.019764	2.217676
100.865627	1544.158288	5.262131	-0.019831	2.222839
101.262914	1552.245756	5.267136	-0.019910	2.228015
101.704799	1560.336477	5.272141	-0.019998	2.233186
101.672200	1568.453350	5.277146	-0.019997	2.238319
102.121410	1576.500029	5.282150	-0.020086	2.243438
102.498954	1584.567724	5.287155	-0.020161	2.248552
102.678916	1592.689788	5.292160	-0.020200	2.253672
102.973035	1600.771467	5.297165	-0.020260	2.258765
103.501360	1608.785626	5.302170	-0.020364	2.263824
103.895692	1616.886502	5.307174	-0.020443	2.268914
104.036868	1625.064754	5.312179	-0.020474	2.274019
104.139066	1633.121514	5.317184	-0.020499	2.279034
104.650044	1641.142439	5.322189	-0.020599	2.284051
104.893050	1649.201638	5.327194	-0.020650	2.289057
105.209523	1657.298170	5.332198	-0.020714	2.294082
105.462427	1665.356724	5.337203	-0.020766	2.299066
105.853210	1673.399278	5.342208	-0.020844	2.304042
106.109412	1681.486868	5.347213	-0.020897	2.309023
106.379180	1689.575954	5.352218	-0.020953	2.313996
107.082181	1697.577605	5.357222	-0.021089	2.318940
107.226131	1705.655440	5.362227	-0.021121	2.323874
107.449118	1713.737981	5.367232	-0.021168	2.328806
108.164315	1721.791693	5.372237	-0.021306	2.333752
108.260454	1729.884401	5.377242	-0.021330	2.338659
108.632351	1737.950554	5.382246	-0.021404	2.343562
108.866903	1746.018521	5.387251	-0.021453	2.348446
109.233256	1754.122759	5.392256	-0.021527	2.353351
109.609119	1762.191605	5.397261	-0.021602	2.358226
109.708102	1770.235220	5.402266	-0.021626	2.363053
110.236541	1778.273042	5.407270	-0.021729	2.367901
110.310583	1786.382027	5.412275	-0.021749	2.372745
110.415544	1794.455992	5.417280	-0.021773	2.377561
111.017463	1802.484477	5.422285	-0.021891	2.382380
111.150993	1810.566020	5.427290	-0.021921	2.387183
111.652405	1818.636648	5.432294	-0.022020	2.392000
111.750081	1826.718547	5.437299	-0.022043	2.396781
112.266070	1834.735689	5.442304	-0.022144	2.401547
112.494888	1842.827272	5.447309	-0.022192	2.406325
112.847615	1850.874442	5.452314	-0.022263	2.411077
113.223150	1858.954703	5.457318	-0.022339	2.415841
113.419823	1867.017704	5.462323	-0.022381	2.420572
113.486631	1875.095872	5.467328	-0.022398	2.425292
113.822209	1883.188638	5.472333	-0.022466	2.430032
114.159909	1891.296348	5.477338	-0.022534	2.434771
114.612080	1899.288937	5.482342	-0.022624	2.439443
115.078666	1907.320885	5.487347	-0.022716	2.444130
115.390592	1915.363474	5.492352	-0.022779	2.448803
115.725970	1923.453497	5.497357	-0.022847	2.453495
115.890672	1931.511855	5.502362	-0.022883	2.458148
116.425540	1939.537443	5.507366	-0.022988	2.462800
116.729692	1947.611693	5.512371	-0.023050	2.467455
116.983937	1955.681976	5.517376	-0.023102	2.472094
117.318183	1963.766196	5.522381	-0.023170	2.476739
117.742098	1971.796355	5.527386	-0.023254	2.481350
117.849668	1979.871552	5.532390	-0.023280	2.485956
118.229709	1987.917955	5.537395	-0.023356	2.490556
118.546562	1995.990143	5.542400	-0.023420	2.495158
118.594505	2004.068873	5.547405	-0.023434	2.499735
118.655582	2012.111543	5.552410	-0.023451	2.504285
119.166689	2020.170447	5.557414	-0.023551	2.508868
119.581423	2028.252655	5.562419	-0.023634	2.513449
119.813148	2036.293881	5.567424	-0.023682	2.517985
120.114222	2044.326941	5.572429	-0.023744	2.522513
120.503390	2052.351911	5.577434	-0.023821	2.527035
120.805936	2060.424943	5.582438	-0.023883	2.531569
120.909678	2068.511992	5.587443	-0.023908	2.536089
121.167638	2076.546475	5.592448	-0.023961	2.540583
121.531958	2084.597268	5.597453	-0.024034	2.545085
121.664761	2092.652565	5.602458	-0.024064	2.549565
121.984057	2100.733988	5.607462	-0.024129	2.554065
122.224953	2108.778502	5.612467	-0.024179	2.558531
122.308516	2116.811573	5.617472	-0.024200	2.562972
122.727000	2124.866506	5.622477	-0.024283	2.567440
122.865076	2132.945829	5.627482	-0.024314	2.571895
123.050393	2141.023633	5.632486	-0.024354	2.576344
123.417600	2149.043071	5.637491	-0.024427	2.580766
123.756621	2157.072898	5.642496	-0.024496	2.585185
124.037708	2165.146527	5.647501	-0.024554	2.589615
124.127496	2173.403040	5.652506	-0.024576	2.594125
124.621584	2181.376995	5.657510	-0.024673	2.598500
125.142301	2189.351313	5.662515	-0.024775	2.602870
125.345988	2197.371645	5.667520	-0.024818	2.607237
125.559454	2205.427407	5.672525	-0.024863	2.611615
125.710726	2213.479127	5.677530	-0.024897	2.615980
126.122680	2221.502240	5.682534	-0.024979	2.620340
126.376587	2229.523171	5.687539	-0.025031	2.624680
126.885701	2237.549227	5.692544	-0.025131	2.629033
127.128593	2245.651989	5.697549	-0.025182	2.633402
127.012540	2253.717913	5.702554	-0.025166	2.637721
127.398409	2261.734971	5.707558	-0.025243	2.642039
127.576768	2269.791156	5.712563	-0.025281	2.646358
128.040815	2277.818564	5.717568	-0.025373	2.650672
128.298250	2285.905736	5.722573	-0.025426	2.654998
128.508033	2293.924863	5.727578	-0.025471	2.659278
128.753909	2301.987344	5.732582	-0.025522	2.663576
128.815297	2310.068388	5.737587	-0.025538	2.667865
129.175939	2318.110739	5.742592	-0.025611	2.672146
129.841623	2326.152811	5.747597	-0.025740	2.676439
129.926508	2334.186242	5.752602	-0.025761	2.680684
130.356137	2342.196666	5.757606	-0.025846	2.684932
130.693151	2350.246076	5.762611	-0.025914	2.689188
130.789465	2358.314875	5.767616	-0.025938	2.693431
131.138940	2366.362990	5.772621	-0.026008	2.697673
131.360366	2374.397608	5.777626	-0.026055	2.701894
131.622971	2382.448349	5.782630	-0.026109	2.706118
131.858674	2390.516852	5.787635	-0.026158	2.710344
132.277751	2398.525779	5.792640	-0.026241	2.714544
132.633035	2406.587410	5.797645	-0.026313	2.718760
132.647315	2414.635679	5.802650	-0.026321	2.722941
133.065316	2422.663921	5.807654	-0.026404	2.727131
133.547122	2430.726133	5.812659	-0.026499	2.731336
133.654583	2438.783851	5.817664	-0.026524	2.735509
133.972605	2446.821123	5.822669	-0.026589	2.739678
134.185802	2454.856559	5.827674	-0.026633	2.743833
134.617748	2462.908821	5.832678	-0.026719	2.748003
134.605731	2471.049023	5.837683	-0.026722	2.752186
134.876603	2479.125687	5.842688	-0.026778	2.756347
135.417333	2487.078114	5.847693	-0.026884	2.760453
135.460060	2495.079142	5.852698	-0.026897	2.764549
135.956399	2503.087252	5.857702	-0.026995	2.768670
136.324156	2511.170396	5.862707	-0.027069	2.772814
136.350832	2519.251070	5.867712	-0.027079	2.776931
136.707758	2527.277624	5.872717	-0.027151	2.781034
136.842500	2535.295329	5.877722	-0.027181	2.785114
137.264466	2543.335875	5.882726	-0.027265	2.789215
137.545336	2551.411652	5.887731	-0.027323	2.793320
137.684539	2559.449747	5.892736	-0.027354	2.797392
138.027637	2567.478552	5.897741	-0.027423	2.801465
138.281792	2575.488593	5.902746	-0.027475	2.805517
138.501276	2583.565258	5.907750	-0.027522	2.809595
138.995479	2591.607281	5.912755	-0.027619	2.813666
139.366943	2599.619295	5.917760	-0.027693	2.817708
139.834099	2607.671962	5.922765	-0.027786	2.821771
140.008698	2615.716902	5.927770	-0.027823	2.825806
140.262180	2623.780694	5.932774	-0.027876	2.829850
140.481646	2631.877579	5.937779	-0.027922	2.833903
140.369627	2639.928604	5.942784	-0.027907	2.837908
140.911265	2647.943683	5.947789	-0.028013	2.841927
141.243102	2655.914981	5.952794	-0.028080	2.845906
141.460139	2663.979888	5.957798	-0.028125	2.849920
141.735687	2672.064182	5.962803	-0.028182	2.853941
142.080507	2680.049923	5.967808	-0.028252	2.857911
142.410648	2688.097942	5.972813	-0.028318	2.861905
142.631145	2696.132361	5.977818	-0.028365	2.865882
142.842209	2704.196881	5.982822	-0.028409	2.869867
142.999039	2712.277540	5.987827	-0.028444	2.873851
143.198949	2720.303008	5.992832	-0.028486	2.877805
143.646431	2728.313895	5.997837	-0.028575	2.881760
143.905039	2736.327761	6.002842	-0.028628	2.885700
144.128264	2744.383483	6.007846	-0.028675	2.889654
144.631980	2752.413456	6.012851	-0.028774	2.893605
144.981888	2760.442928	6.017856	-0.028845	2.897542
145.131130	2768.505728	6.022861	-0.028878	2.901479
145.476853	2776.521905	6.027866	-0.028947	2.905398
145.605806	2784.591653	6.032870	-0.028977	2.909327
145.867253	2792.722819	6.037875	-0.029031	2.913286
146.063942	2800.725337	6.042880	-0.029073	2.917175
146.215569	2808.765537	6.047885	-0.029106	2.921075
146.600817	2816.731519	6.052890	-0.029183	2.924945
146.605206	2824.806209	6.057894	-0.029189	2.928843
147.033912	2832.818792	6.062899	-0.029274	2.932728
147.421659	2840.864220	6.067904	-0.029352	2.936622
147.506093	2848.917781	6.072909	-0.029373	2.940498
147.561425	2856.921415	6.077914	-0.029388	2.944344
147.878485	2864.971693	6.082918	-0.029453	2.948220
148.195404	2873.028845	6.087923	-0.029517	2.952095
148.220415	2881.079931	6.092928	-0.029527	2.955946
148.658692	2889.089811	6.097933	-0.029614	2.959795
148.839803	2897.100684	6.102938	-0.029653	2.963625
149.152549	2905.137402	6.107942	-0.029716	2.967469
149.452027	2913.199928	6.112947	-0.029777	2.971320
149.755505	2921.238460	6.117952	-0.029839	2.975155
150.109298	2929.254509	6.122957	-0.029910	2.978977
150.402312	2937.273679	6.127962	-0.029970	2.982792
150.655087	2945.326041	6.132966	-0.030022	2.986616
150.934635	2953.360244	6.137971	-0.030080	2.990427
150.947259	2961.447706	6.142976	-0.030087	2.994246
151.199582	2969.479725	6.147981	-0.030140	2.998045
151.584136	2977.486878	6.152986	-0.030217	3.001835
151.822914	2985.515075	6.157990	-0.030266	3.005622
152.041053	2993.541734	6.162995	-0.030312	3.009403
152.260742	3001.589767	6.168000	-0.030358	3.013189
152.554541	3009.646944	6.173005	-0.030418	3.016978
152.762866	3017.670610	6.178010	-0.030462	3.020743
152.968807	3025.675905	6.183014	-0.030506	3.024494
153.268825	3033.733652	6.188019	-0.030567	3.028269
153.582543	3041.773387	6.193024	-0.030631	3.032032
153.748281	3049.857436	6.198029	-0.030667	3.035804
153.869909	3057.841994	6.203034	-0.030695	3.039522
154.344049	3065.856430	6.208038	-0.030789	3.043267
154.733418	3073.895133	6.213043	-0.030866	3.047015
154.865007	3081.960397	6.218048	-0.030896	3.050757
155.222589	3089.994162	6.223053	-0.030968	3.054492
155.431991	3098.013282	6.228058	-0.031012	3.058207
155.535886	3106.067973	6.233062	-0.031037	3.061930
155.886258	3114.095795	6.238067	-0.031107	3.065647
155.966943	3122.116304	6.243072	-0.031128	3.069344
156.249259	3130.254370	6.248077	-0.031186	3.073100
156.383712	3138.283601	6.253082	-0.031216	3.076794
156.798636	3146.247783	6.258086	-0.031298	3.080467
157.156981	3154.235602	6.263091	-0.031370	3.084144
157.206050	3162.280800	6.268096	-0.031385	3.087828
157.507246	3170.338895	6.273101	-0.031446	3.091526
157.448670	3178.371881	6.278106	-0.031441	3.095191
157.979184	3186.368840	6.283110	-0.031545	3.098862
158.279064	3194.413790	6.288115	-0.031606	3.102540
158.303026	3202.446641	6.293120	-0.031616	3.106195
158.654194	3210.489954	6.298125	-0.031686	3.109866
158.881146	3218.540206	6.303130	-0.031734	3.113530
159.157995	3226.589583	6.308134	-0.031791	3.117192
159.238291	3234.631538	6.313139	-0.031811	3.120837
159.576341	3242.571731	6.318144	-0.031879	3.124443
159.671308	3250.677415	6.323149	-0.031902	3.128109
159.667922	3258.739377	6.328154	-0.031907	3.131746
159.763705	3266.772521	6.333158	-0.031930	3.135371
160.099945	3274.769845	6.338163	-0.031998	3.138986
160.261552	3282.780514	6.343168	-0.032033	3.142595
160.442781	3290.843766	6.348173	-0.032072	3.146224
160.968920	3298.814449	6.353178	-0.032175	3.149823
161.432179	3306.902443	6.358182	-0.032267	3.153467
161.684192	3314.936857	6.363187	-0.032319	3.157074
161.769180	3322.955603	6.368192	-0.032340	3.160662
162.146424	3330.948160	6.373197	-0.032416	3.164248
162.526245	3338.960233	6.378202	-0.032492	3.167838
162.651803	3347.038416	6.383206	-0.032520	3.171442
162.881756	3355.095435	6.388211	-0.032568	3.175037
162.913729	3363.122435	6.393216	-0.032580	3.178607
163.153622	3371.165243	6.398221	-0.032630	3.182188
163.277753	3379.171988	6.403226	-0.032658	3.185744
163.569730	3387.206949	6.408230	-0.032718	3.189316
163.582627	3395.279830	6.413235	-0.032725	3.192889
163.994679	3403.289816	6.418240	-0.032807	3.196447
164.299721	3411.312038	6.423245	-0.032869	3.200002
164.386671	3419.327908	6.428250	-0.032891	3.203540
164.681945	3427.367710	6.433254	-0.032951	3.207094
164.888896	3435.428480	6.438259	-0.032995	3.210650
165.177480	3443.425926	6.443264	-0.033054	3.214177
165.430929	3451.480435	6.448269	-0.033106	3.217724
165.611879	3459.503764	6.453274	-0.033145	3.221251
165.734839	3467.500773	6.458278	-0.033174	3.224759
165.956505	3475.560143	6.463283	-0.033220	3.228295
166.191067	3483.621545	6.468288	-0.033269	3.231828
166.664471	3491.681811	6.473293	-0.033363	3.235367
166.676496	3499.674420	6.478298	-0.033370	3.238854
166.664669	3507.674283	6.483302	-0.033373	3.242339
167.180920	3515.685557	6.488307	-0.033474	3.245847
167.268801	3523.705082	6.493312	-0.033496	3.249337
167.600802	3531.775516	6.498317	-0.033563	3.252855
167.778319	3539.806420	6.503322	-0.033602	3.256346
167.933364	3547.820706	6.508326	-0.033636	3.259825
168.083734	3555.860662	6.513331	-0.033669	3.263311
168.183580	3563.863347	6.518336	-0.033693	3.266776
168.596824	3571.914706	6.523341	-0.033775	3.270270
168.678741	3579.968834	6.528346	-0.033796	3.273749
168.880008	3587.988129	6.533350	-0.033838	3.277213
169.152543	3596.008832	6.538355	-0.033894	3.280677
169.456995	3603.974990	6.543360	-0.033956	3.284115
169.320673	3612.075924	6.548365	-0.033936	3.287591
169.704192	3620.083269	6.553370	-0.034013	3.291043
170.138625	3628.113582	6.558374	-0.034099	3.294502
170.355695	3636.150156	6.563379	-0.034145	3.297953
170.565382	3644.174016	6.568384	-0.034189	3.301394
170.815164	3652.161121	6.573389	-0.034241	3.304817
170.914587	3660.228550	6.578394	-0.034265	3.308265
171.074858	3668.302707	6.583398	-0.034300	3.311715
171.180097	3676.336729	6.588403	-0.034325	3.315142
171.190091	3684.333238	6.593408	-0.034332	3.318546
171.573021	3692.343990	6.598413	-0.034408	3.321967
171.791299	3700.342391	6.603418	-0.034454	3.325372
172.064018	3708.359041	6.608422	-0.034510	3.328784
172.280013	3716.429558	6.613427	-0.034556	3.332213
172.716849	3724.450821	6.618432	-0.034642	3.335625
172.867316	3732.478188	6.623437	-0.034676	3.339027
173.214969	3740.492950	6.628442	-0.034746	3.342426
173.469705	3748.524118	6.633446	-0.034798	3.345826
173.783774	3756.553256	6.638451	-0.034862	3.349223
174.062079	3764.579708	6.643456	-0.034919	3.352614
174.128727	3772.669807	6.648461	-0.034937	3.356021
174.412745	3780.632057	6.653466	-0.034995	3.359379
174.604002	3788.652032	6.658470	-0.035036	3.362754
174.770152	3796.726985	6.663475	-0.035072	3.366148
174.799133	3804.733223	6.668480	-0.035083	3.369505
174.963514	3812.804541	6.673485	-0.035119	3.372891
175.210966	3820.809776	6.678490	-0.035170	3.376248
175.322327	3828.845875	6.683494	-0.035196	3.379610
175.629774	3836.858455	6.688499	-0.035259	3.382966
175.858181	3844.878336	6.693504	-0.035307	3.386319
176.067526	3852.913887	6.698509	-0.035351	3.389674
176.244774	3861.029250	6.703514	-0.035389	3.393058
176.608890	3869.037204	6.708518	-0.035462	3.396400
176.819105	3877.018743	6.713523	-0.035507	3.399723
176.840854	3885.006637	6.718528	-0.035516	3.403038
177.492722	3893.010071	6.723533	-0.035643	3.406379
177.592550	3901.032907	6.728538	-0.035666	3.409705
177.736491	3909.098472	6.733542	-0.035698	3.413047
178.066729	3917.137700	6.738547	-0.035765	3.416382
178.280421	3925.121200	6.743552	-0.035810	3.419686
178.410709	3933.150445	6.748557	-0.035840	3.423002
178.593939	3941.184708	6.753562	-0.035879	3.426320
179.029690	3949.186416	6.758566	-0.035966	3.429629
179.256611	3957.271622	6.763571	-0.036013	3.432963
179.425003	3965.289767	6.768576	-0.036050	3.436263
179.471562	3973.311173	6.773581	-0.036064	3.439558
180.035224	3981.280011	6.778586	-0.036174	3.442845
180.088754	3989.360588	6.783590	-0.036189	3.446158
180.234138	3997.388134	6.788595	-0.036222	3.449449
180.404111	4005.429839	6.793600	-0.036259	3.452743
180.885808	4013.467227	6.798605	-0.036353	3.456043
180.912213	4021.471782	6.803610	-0.036364	3.459311
181.437682	4029.480733	6.808614	-0.036467	3.462594
181.653903	4037.535272	6.813619	-0.036512	3.465882
181.709007	4045.532895	6.818624	-0.036528	3.469139
181.973922	4053.631236	6.823629	-0.036583	3.472441
182.109416	4061.662331	6.828634	-0.036613	3.475707
182.192468	4069.646708	6.833638	-0.036634	3.478951
182.636670	4077.677876	6.838643	-0.036722	3.482221
182.974723	4085.628779	6.843648	-0.036790	3.485453
183.193494	4093.680714	6.848653	-0.036836	3.488718
183.177509	4101.723150	6.853658	-0.036838	3.491970
183.543092	4109.768791	6.858662	-0.036912	3.495231
183.991168	4117.778545	6.863667	-0.037000	3.498478
183.856181	4125.804864	6.868672	-0.036980	3.501710
184.279897	4133.779716	6.873677	-0.037065	3.504935
184.665140	4141.833392	6.878682	-0.037142	3.508188
184.918877	4149.873022	6.883686	-0.037194	3.511429
185.122366	4157.931068	6.888691	-0.037237	3.514672
185.231256	4165.932315	6.893696	-0.037263	3.517886
185.462037	4173.977567	6.898701	-0.037311	3.521119
185.455465	4181.954105	6.903706	-0.037315	3.524314
185.681633	4189.999761	6.908710	-0.037363	3.527541
185.820067	4198.055656	6.913715	-0.037394	3.530766
186.060732	4206.079965	6.918720	-0.037444	3.533979
186.263179	4214.117714	6.923725	-0.037487	3.537193
186.504140	4222.128637	6.928730	-0.037537	3.540395
186.593489	4230.140298	6.933734	-0.037559	3.543589
186.674635	4238.216351	6.938739	-0.037579	3.546806
186.775559	4246.210332	6.943744	-0.037603	3.549988
187.136276	4254.314008	6.948749	-0.037676	3.553219
187.128965	4262.366850	6.953754	-0.037680	3.556415
187.321864	4270.284494	6.958758	-0.037721	3.559561
187.657922	4278.296383	6.963763	-0.037789	3.562745
187.793883	4286.313806	6.968768	-0.037819	3.565923
187.987341	4294.341323	6.973773	-0.037860	3.569104
188.104281	4302.381716	6.978778	-0.037887	3.572284
188.396940	4310.386402	6.983782	-0.037947	3.575453
188.580604	4318.438757	6.988787	-0.037987	3.578635
188.572392	4326.475892	6.993792	-0.037990	3.581802
188.987947	4334.443345	6.998797	-0.038073	3.584951
188.980942	4342.487524	7.003802	-0.038077	3.588116
189.140846	4350.513236	7.008806	-0.038112	3.591275
189.632134	4358.546069	7.013811	-0.038209	3.594443
189.725084	4366.539230	7.018816	-0.038231	3.597582
190.077156	4374.579006	7.023821	-0.038302	3.600744
190.183096	4382.584602	7.028826	-0.038327	3.603883
190.346172	4390.572406	7.033830	-0.038363	3.607013
190.627000	4398.633948	7.038835	-0.038420	3.610173
190.718455	4406.664944	7.043840	-0.038443	3.613313
191.053842	4414.696128	7.048845	-0.038511	3.616456
191.145026	4422.718841	7.053850	-0.038533	3.619587
191.550931	4430.699962	7.058854	-0.038614	3.622708
191.754187	4438.760937	7.063859	-0.038657	3.625852
191.607844	4446.790820	7.068864	-0.038635	3.628971
191.806305	4454.859767	7.073869	-0.038677	3.632112
192.190635	4462.867363	7.078874	-0.038754	3.635232
192.471764	4470.835231	7.083878	-0.038811	3.638330
192.659475	4478.906736	7.088883	-0.038852	3.641464
192.708260	4486.860986	7.093888	-0.038866	3.644545
193.111415	4494.942922	7.098893	-0.038946	3.647683
193.166086	4502.996927	7.103898	-0.038962	3.650798
193.301992	4511.015092	7.108902	-0.038992	3.653899
193.917830	4519.028455	7.113907	-0.039112	3.657008
194.023185	4527.032598	7.118912	-0.039137	3.660097
194.310097	4535.058811	7.123917	-0.039196	3.663197
194.282510	4543.111595	7.128922	-0.039196	3.666296
194.367043	4551.106788	7.133926	-0.039217	3.669374
194.665158	4559.161839	7.138931	-0.039278	3.672477
194.692445	4567.172853	7.143936	-0.039288	3.675554
195.030148	4575.186138	7.148941	-0.039356	3.678637
195.132492	4583.216281	7.153946	-0.039381	3.681718
195.206858	4591.208578	7.158950	-0.039400	3.684781
195.775061	4599.245863	7.163955	-0.039511	3.687871
195.786289	4607.256682	7.168960	-0.039518	3.690934
195.958482	4615.304447	7.173965	-0.039556	3.694013
196.125985	4623.337226	7.178970	-0.039592	3.697083
196.477257	4631.298404	7.183974	-0.039663	3.700129
196.787877	4639.347637	7.188979	-0.039726	3.703204
196.896834	4647.385656	7.193984	-0.039751	3.706267
197.162018	4655.388230	7.198989	-0.039806	3.709318
197.503613	4663.491172	7.203994	-0.039875	3.712407
197.708718	4671.536635	7.208998	-0.039918	3.715468
197.907014	4679.495446	7.214003	-0.039961	3.718493
198.035655	4687.504834	7.219008	-0.039990	3.721533
198.288522	4695.474977	7.224013	-0.040042	3.724559
198.455898	4703.528943	7.229018	-0.040079	3.727612
198.557471	4711.513678	7.234022	-0.040103	3.730635
198.624150	4719.594747	7.239027	-0.040121	3.733690
198.797510	4727.645965	7.244032	-0.040158	3.736735
199.147267	4735.598372	7.249037	-0.040228	3.739744
199.271644	4743.658465	7.254042	-0.040257	3.742786
199.287852	4751.664785	7.259046	-0.040265	3.745802
199.525413	4759.700284	7.264051	-0.040315	3.748832
199.569965	4767.711208	7.269056	-0.040328	3.751846
199.543345	4775.787031	7.274061	-0.040329	3.754881
199.707883	4783.798521	7.279066	-0.040365	3.757893
200.100192	4791.760874	7.284070	-0.040443	3.760889
200.104096	4799.831904	7.289075	-0.040449	3.763915
200.159660	4807.855417	7.294080	-0.040464	3.766922
200.456869	4815.884823	7.299085	-0.040525	3.769934
200.731873	4823.926314	7.304090	-0.040582	3.772948
200.664780	4831.929897	7.309094	-0.040574	3.775937
201.131135	4839.934350	7.314099	-0.040666	3.778936
201.269318	4847.938340	7.319104	-0.040697	3.781926
201.491599	4855.990602	7.324109	-0.040744	3.784932
201.610928	4864.014443	7.329114	-0.040772	3.787924
201.812335	4872.023851	7.334118	-0.040814	3.790910
202.111935	4880.118653	7.339123	-0.040875	3.793927
202.249751	4888.066568	7.344128	-0.040906	3.796883
202.534655	4896.082716	7.349133	-0.040965	3.799866
202.822148	4904.077363	7.354138	-0.041023	3.802838
202.910567	4912.100180	7.359142	-0.041045	3.805815
203.113284	4920.113368	7.364147	-0.041088	3.808787
203.260007	4928.136174	7.369152	-0.041121	3.811760
203.358090	4936.174893	7.374157	-0.041144	3.814735
203.589947	4944.215578	7.379162	-0.041193	3.817712
203.898476	4952.166036	7.384166	-0.041255	3.820654
204.234342	4960.210068	7.389171	-0.041323	3.823630
204.324323	4968.243260	7.394176	-0.041345	3.826593
204.613334	4976.290863	7.399181	-0.041404	3.829564
204.938993	4984.328341	7.404186	-0.041470	3.832530
204.822752	4992.313185	7.409190	-0.041454	3.835465
204.964129	5000.362624	7.414195	-0.041486	3.838426
205.399949	5008.363503	7.419200	-0.041572	3.841374
205.377963	5016.361516	7.424205	-0.041573	3.844308
205.465983	5024.393555	7.429210	-0.041595	3.847255
205.632035	5032.436827	7.434214	-0.041631	3.850206
206.050807	5040.465492	7.439219	-0.041714	3.853154
206.118817	5048.477218	7.444224	-0.041732	3.856087
206.216458	5056.484901	7.449229	-0.041756	3.859016
206.534265	5064.516548	7.454234	-0.041820	3.861956
206.629996	5072.527258	7.459238	-0.041843	3.864882
206.711309	5080.611664	7.464243	-0.041864	3.867833
206.805247	5088.621903	7.469248	-0.041886	3.870754
207.208107	5096.844488	7.474253	-0.041967	3.873756
207.107159	5104.853638	7.479258	-0.041953	3.876669
207.302479	5112.700820	7.484262	-0.041995	3.879526
207.765960	5120.710559	7.489267	-0.042086	3.882445
207.965217	5128.683004	7.494272	-0.042129	3.885344
208.080340	5136.707290	7.499277	-0.042155	3.888257
208.529584	5144.750099	7.504282	-0.042244	3.891182
208.668458	5152.769850	7.509286	-0.042275	3.894090
208.669362	5160.814999	7.514291	-0.042281	3.897002
208.924339	5168.773422	7.519296	-0.042334	3.899885
209.234952	5176.817035	7.524301	-0.042397	3.902798
209.361797	5184.841767	7.529306	-0.042426	3.905699
209.527329	5192.835041	7.534310	-0.042462	3.908587
209.819770	5200.916954	7.539315	-0.042522	3.911507
209.972423	5208.918627	7.544320	-0.042555	3.914393
210.048738	5216.918914	7.549325	-0.042575	3.917275
210.158941	5224.930346	7.554330	-0.042600	3.920160
210.369522	5232.923521	7.559334	-0.042645	3.923038
210.610828	5240.970653	7.564339	-0.042695	3.925934
211.001191	5248.953683	7.569344	-0.042773	3.928807
211.123043	5257.027611	7.574349	-0.042801	3.931706
211.235560	5265.074049	7.579354	-0.042827	3.934592
211.320370	5273.065060	7.584358	-0.042848	3.937456
211.741147	5281.063565	7.589363	-0.042932	3.940327
211.762085	5289.092240	7.594368	-0.042941	3.943199
211.860664	5297.108978	7.599373	-0.042965	3.946067
212.158715	5305.126175	7.604378	-0.043026	3.948935
212.460788	5313.192016	7.609382	-0.043087	3.951819
212.638179	5321.251570	7.614387	-0.043125	3.954697
212.753924	5329.243826	7.619392	-0.043152	3.957547
213.125269	5337.219029	7.624397	-0.043227	3.960394
213.435467	5345.231160	7.629402	-0.043290	3.963251
213.618402	5353.241257	7.634406	-0.043329	3.966102
213.844678	5361.256014	7.639411	-0.043376	3.968954
213.907243	5369.285300	7.644416	-0.043393	3.971807
214.358855	5377.321338	7.649421	-0.043483	3.974666
214.408836	5385.383177	7.654426	-0.043497	3.977525
214.455127	5393.346130	7.659430	-0.043511	3.980347
214.517564	5401.381924	7.664435	-0.043528	3.983194
214.642213	5409.405597	7.669440	-0.043556	3.986035
215.026285	5417.419493	7.674445	-0.043633	3.988875
215.146880	5425.470882	7.679450	-0.043661	3.991721
215.103503	5433.476348	7.684454	-0.043658	3.994547
215.405905	5441.522984	7.689459	-0.043720	3.997391
215.650211	5449.506380	7.694464	-0.043771	4.000209
215.718862	5457.525652	7.699469	-0.043789	4.003036
215.795044	5465.519239	7.704474	-0.043808	4.005851
216.071966	5473.510342	7.709478	-0.043865	4.008667
216.040724	5481.611609	7.714483	-0.043864	4.011514
216.221924	5489.630918	7.719488	-0.043903	4.014334
216.499235	5497.645453	7.724493	-0.043960	4.017152
216.611867	5505.651656	7.729498	-0.043986	4.019963
216.746825	5513.671442	7.734502	-0.044017	4.022776
217.104994	5521.690688	7.739507	-0.044089	4.025591
217.219370	5529.707610	7.744512	-0.044115	4.028399
217.340470	5537.749529	7.749517	-0.044143	4.031215
217.648152	5545.866785	7.754522	-0.044206	4.034057
217.915294	5553.837875	7.759526	-0.044261	4.036845
218.012613	5561.787879	7.764531	-0.044284	4.039622
217.840752	5569.825610	7.769536	-0.044257	4.042423
218.274285	5577.794762	7.774541	-0.044343	4.045208
218.472083	5585.854867	7.779546	-0.044386	4.048019
218.500351	5593.839879	7.784550	-0.044396	4.050799
218.873848	5601.888654	7.789555	-0.044471	4.053604
219.058000	5609.917822	7.794560	-0.044510	4.056398
219.186456	5617.893789	7.799565	-0.044540	4.059171
219.370605	5625.961133	7.804570	-0.044579	4.061974
219.668314	5633.911534	7.809574	-0.044640	4.064736
219.871834	5641.953307	7.814579	-0.044683	4.067527
220.207453	5649.978188	7.819584	-0.044751	4.070312
220.158376	5658.017987	7.824589	-0.044747	4.073095
220.508176	5666.070656	7.829594	-0.044817	4.075885
220.502202	5674.018613	7.834598	-0.044822	4.078633
220.792869	5682.042347	7.839603	-0.044881	4.081409
220.946677	5690.028264	7.844608	-0.044915	4.084168
221.057791	5698.063886	7.849613	-0.044941	4.086942
221.186529	5706.094364	7.854618	-0.044970	4.089713
221.257730	5714.103595	7.859622	-0.044989	4.092473
221.560942	5722.180888	7.864627	-0.045050	4.095258
221.477350	5730.171704	7.869632	-0.045040	4.098007
222.089104	5738.150116	7.874637	-0.045159	4.100758
222.167630	5746.162793	7.879642	-0.045179	4.103512
222.199205	5754.213611	7.884646	-0.045190	4.106277
222.655451	5762.228258	7.889651	-0.045280	4.109033
223.013948	5770.295894	7.894656	-0.045353	4.111804
223.062082	5778.368951	7.899661	-0.045367	4.114571
223.065911	5786.375255	7.904666	-0.045373	4.117313
223.135133	5794.321502	7.909670	-0.045391	4.120033
223.613428	5802.353781	7.914675	-0.045485	4.122786
223.604251	5810.333737	7.919680	-0.045489	4.125513
223.698942	5818.353577	7.924685	-0.045512	4.128254
223.887197	5826.422967	7.929690	-0.045552	4.131010
224.023109	5834.439294	7.934694	-0.045583	4.133746
224.198849	5842.491631	7.939699	-0.045621	4.136492
224.303728	5850.482256	7.944704	-0.045645	4.139216
224.537251	5858.507555	7.949709	-0.045694	4.141950
224.612914	5866.507134	7.954714	-0.045713	4.144672
224.776834	5874.560347	7.959718	-0.045749	4.147412
225.096531	5882.568450	7.964723	-0.045814	4.150136
225.255946	5890.621582	7.969728	-0.045849	4.152872
225.461490	5898.624185	7.974733	-0.045893	4.155589
225.537908	5906.647625	7.979738	-0.045912	4.158310
225.569130	5914.641962	7.984742	-0.045923	4.161019
225.752623	5922.619733	7.989747	-0.045963	4.163723
226.143119	5930.662209	7.994752	-0.046041	4.166448
226.232693	5938.691631	7.999757	-0.046063	4.169165
226.589563	5946.730315	8.004762	-0.046134	4.171885
226.724087	5954.731870	8.009766	-0.046165	4.174589
227.051687	5962.742460	8.014771	-0.046231	4.177296
227.152347	5970.726042	8.019776	-0.046255	4.179989
227.192608	5978.750157	8.024781	-0.046268	4.182694
227.743051	5986.783289	8.029786	-0.046375	4.185406
227.670233	5994.794704	8.034790	-0.046367	4.188102
227.813417	6002.844236	8.039795	-0.046399	4.190811
227.941948	6010.941317	8.044800	-0.046428	4.193535
228.089440	6018.950158	8.049805	-0.046461	4.196227
228.053478	6026.895583	8.054810	-0.046460	4.198894
228.208870	6034.907999	8.059814	-0.046494	4.201584
228.630795	6042.885644	8.064819	-0.046578	4.204263
228.524780	6050.912873	8.069824	-0.046563	4.206952
228.588960	6058.922242	8.074829	-0.046580	4.209634
228.969970	6066.995188	8.079834	-0.046657	4.212340
228.898379	6074.977987	8.084838	-0.046648	4.215009
229.102310	6082.984601	8.089843	-0.046692	4.217687
229.336066	6090.965580	8.094848	-0.046740	4.220355
229.721443	6098.988358	8.099853	-0.046817	4.223037
229.839849	6107.021500	8.104858	-0.046845	4.225718
229.761291	6115.018753	8.109862	-0.046835	4.228383
230.021697	6123.087988	8.114867	-0.046889	4.231074
230.148004	6131.109148	8.119872	-0.046918	4.233746
230.323872	6139.139637	8.124877	-0.046956	4.236419
230.585796	6147.126793	8.129882	-0.047010	4.239078
230.668455	6155.141093	8.134886	-0.047031	4.241742
230.851715	6163.103088	8.139891	-0.047070	4.244388
231.032423	6171.187826	8.144896	-0.047109	4.247073
231.331174	6179.154893	8.149901	-0.047170	4.249718
231.517306	6187.254534	8.154906	-0.047210	4.252404
231.537335	6195.235729	8.159910	-0.047219	4.255048
231.910211	6203.304727	8.164915	-0.047294	4.257723
231.928278	6211.247919	8.169920	-0.047302	4.260351
232.015242	6219.304688	8.174925	-0.047324	4.263016
232.165085	6227.308155	8.179930	-0.047357	4.265662
232.214059	6235.358107	8.184934	-0.047371	4.268320
232.463943	6243.379432	8.189939	-0.047423	4.270970
232.600234	6251.452370	8.194944	-0.047454	4.273633
232.653881	6259.439694	8.199949	-0.047469	4.276266
232.888241	6267.405516	8.204954	-0.047518	4.278892
233.088052	6275.421804	8.209958	-0.047560	4.281533
233.306625	6283.429363	8.214963	-0.047606	4.284169
233.357337	6291.476566	8.219968	-0.047621	4.286815
233.351470	6299.446542	8.224973	-0.047625	4.289434
233.468981	6307.578112	8.229978	-0.047652	4.292105
233.549294	6315.529199	8.234982	-0.047673	4.294715
233.947813	6323.562158	8.239987	-0.047752	4.297353
233.895520	6331.562521	8.244992	-0.047748	4.299975
234.199182	6339.548735	8.249997	-0.047809	4.302593
234.371470	6347.584088	8.255002	-0.047847	4.305225
234.570716	6355.597071	8.260006	-0.047889	4.307848
234.896692	6363.667462	8.265011	-0.047955	4.310490
235.141065	6371.698960	8.270016	-0.048006	4.313116
235.027753	6379.685348	8.275021	-0.047990	4.315723
235.304876	6387.679108	8.280026	-0.048047	4.318334
235.492156	6395.675068	8.285030	-0.048087	4.320943
235.560986	6403.695845	8.290035	-0.048105	4.323558
235.596703	6411.730876	8.295040	-0.048117	4.326176
235.905257	6419.726419	8.300045	-0.048180	4.328781
236.026095	6427.798195	8.305050	-0.048208	4.331409
235.787382	6435.811636	8.310054	-0.048168	4.334013
236.214522	6443.833792	8.315059	-0.048253	4.336623
236.400267	6451.796856	8.320064	-0.048293	4.339210
236.203239	6459.839200	8.325069	-0.048262	4.341819
236.409537	6467.813397	8.330074	-0.048305	4.344407
236.696991	6475.871679	8.335078	-0.048364	4.347022
236.865901	6483.884348	8.340083	-0.048401	4.349619
236.702471	6491.990598	8.345088	-0.048376	4.352243
236.811633	6500.015146	8.350093	-0.048401	4.354840
236.976447	6508.037636	8.355098	-0.048437	4.357436
237.130298	6515.958917	8.360102	-0.048471	4.359997
237.373550	6523.944088	8.365107	-0.048522	4.362578
237.492553	6531.971315	8.370112	-0.048549	4.365170
237.507626	6539.946312	8.375117	-0.048557	4.367743
237.724639	6548.010339	8.380122	-0.048603	4.370345
237.894833	6556.022967	8.385126	-0.048640	4.372928
237.909825	6564.081100	8.390131	-0.048648	4.375523
237.951244	6572.051374	8.395136	-0.048661	4.378089
238.366384	6580.043840	8.400141	-0.048743	4.380662
238.556879	6588.064638	8.405146	-0.048784	4.383242
238.536427	6596.092044	8.410150	-0.048786	4.385821
238.734636	6604.101858	8.415155	-0.048828	4.388394
238.915041	6612.153749	8.420160	-0.048867	4.390979
238.904717	6620.154341	8.425165	-0.048870	4.393545
238.964113	6628.243193	8.430170	-0.048886	4.396139
239.233232	6636.165662	8.435174	-0.048942	4.398678
239.425596	6644.228703	8.440179	-0.048983	4.401261
239.500390	6652.192108	8.445184	-0.049002	4.403809
239.580208	6660.224534	8.450189	-0.049022	4.406378
239.790232	6668.242016	8.455194	-0.049066	4.408942
239.831218	6676.291370	8.460198	-0.049079	4.411513
240.109285	6684.322179	8.465203	-0.049136	4.414078
240.179814	6692.396214	8.470208	-0.049155	4.416654
240.240768	6700.324315	8.475213	-0.049171	4.419182
240.292791	6708.423718	8.480218	-0.049186	4.421764
240.339293	6716.341659	8.485222	-0.049200	4.424286
240.537590	6724.401242	8.490227	-0.049243	4.426852
240.668132	6732.417481	8.495232	-0.049272	4.429403
240.728303	6740.457084	8.500237	-0.049289	4.431959
241.063953	6748.495525	8.505242	-0.049356	4.434515
241.054750	6756.527787	8.510246	-0.049360	4.437065
241.275302	6764.478883	8.515251	-0.049406	4.439590
241.324099	6772.519613	8.520256	-0.049421	4.442140
241.577457	6780.476573	8.525261	-0.049473	4.444664
241.560581	6788.530407	8.530266	-0.049475	4.447215
241.817337	6796.541948	8.535270	-0.049528	4.449753
241.846046	6804.603499	8.540275	-0.049539	4.452305
241.831098	6812.637654	8.545280	-0.049541	4.454846
242.006377	6820.634542	8.550285	-0.049579	4.457374
242.282206	6828.630876	8.555290	-0.049636	4.459901
242.278201	6836.630250	8.560295	-0.049640	4.462427
242.402835	6844.635624	8.565299	-0.049669	4.464954
242.753212	6852.695470	8.570304	-0.049739	4.467497
242.732679	6860.641400	8.575309	-0.049741	4.470001
242.735422	6868.741217	8.580314	-0.049747	4.472553
242.987698	6876.752678	8.585319	-0.049799	4.475076
243.206451	6884.731415	8.590323	-0.049845	4.477588
243.300869	6892.731924	8.595328	-0.049868	4.480104
243.203561	6900.704185	8.600333	-0.049855	4.482609
243.385534	6908.794353	8.605338	-0.049894	4.485151
243.593679	6916.802391	8.610343	-0.049938	4.487666
243.703162	6924.795073	8.615347	-0.049964	4.490174
243.707261	6932.844072	8.620352	-0.049970	4.492698
243.805148	6940.833954	8.625357	-0.049993	4.495203
244.137675	6948.874038	8.630362	-0.050060	4.497722
244.153705	6956.837822	8.635367	-0.050069	4.500216
244.475775	6964.871214	8.640371	-0.050134	4.502730
244.616396	6972.904800	8.645376	-0.050165	4.505243
244.678524	6980.916615	8.650381	-0.050182	4.507747
244.853830	6988.957982	8.655386	-0.050220	4.510259
244.891804	6996.992006	8.660391	-0.050232	4.512767
245.049078	7005.050608	8.665395	-0.050267	4.515282
245.353665	7013.004494	8.670400	-0.050329	4.517763
245.412985	7020.972718	8.675405	-0.050345	4.520247
245.379392	7029.012195	8.680410	-0.050344	4.522751
245.658036	7036.997750	8.685415	-0.050401	4.525237
246.002668	7045.037546	8.690419	-0.050471	4.527740
246.059559	7053.018573	8.695424	-0.050487	4.530222
246.030488	7061.075901	8.700429	-0.050487	4.532726
246.579516	7069.139088	8.705434	-0.050594	4.535232
246.483197	7077.113300	8.710439	-0.050581	4.537707
246.490938	7085.117394	8.715443	-0.050588	4.540191
246.675838	7093.134945	8.720448	-0.050628	4.542677
246.957477	7101.118152	8.725453	-0.050686	4.545152
247.272973	7109.181258	8.730458	-0.050750	4.547650
247.062497	7117.181001	8.735463	-0.050716	4.550127
247.351202	7125.241117	8.740467	-0.050775	4.552621
247.609738	7133.253408	8.745472	-0.050828	4.555099
247.472456	7141.261853	8.750477	-0.050808	4.557575
247.828251	7149.248216	8.755482	-0.050879	4.560042
247.837436	7157.273858	8.760487	-0.050886	4.562520
248.010862	7165.253642	8.765491	-0.050924	4.564983
248.211068	7173.321753	8.770496	-0.050966	4.567471
248.534212	7181.295643	8.775501	-0.051032	4.569930
248.438847	7189.318947	8.780506	-0.051019	4.572401
248.568745	7197.377295	8.785511	-0.051049	4.574883
248.797621	7205.382957	8.790515	-0.051097	4.577346
248.998458	7213.405291	8.795520	-0.051139	4.579814
249.010676	7221.387823	8.800525	-0.051147	4.582268
249.299131	7229.414650	8.805530	-0.051206	4.584734
249.603583	7237.429613	8.810535	-0.051268	4.587196
249.728980	7245.478870	8.815539	-0.051296	4.589666
249.848509	7253.520314	8.820544	-0.051324	4.592133
250.121508	7261.539409	8.825549	-0.051380	4.594591
250.399964	7269.541503	8.830554	-0.051437	4.597043
250.309545	7277.506619	8.835559	-0.051426	4.599483
250.549387	7285.537840	8.840563	-0.051476	4.601941
250.667542	7293.470453	8.845568	-0.051503	4.604368
250.652930	7301.536077	8.850573	-0.051505	4.606834
250.949342	7309.565019	8.855578	-0.051566	4.609287
251.077800	7317.645433	8.860583	-0.051595	4.611755
251.165656	7325.649417	8.865587	-0.051617	4.614199
251.330363	7333.680217	8.870592	-0.051653	4.616649
251.323832	7341.585231	8.875597	-0.051657	4.619059
251.502539	7349.695313	8.880602	-0.051695	4.621531
251.457260	7357.623061	8.885607	-0.051692	4.623946
251.845247	7365.723572	8.890611	-0.051770	4.626412
252.091697	7373.738090	8.895616	-0.051821	4.628850
251.903097	7381.692694	8.900621	-0.051791	4.631270
252.079061	7389.755714	8.905626	-0.051829	4.633720
252.245724	7397.789141	8.910631	-0.051865	4.636161
252.495344	7405.743727	8.915635	-0.051917	4.638576
252.526566	7413.790597	8.920640	-0.051928	4.641018
252.717926	7421.788558	8.925645	-0.051969	4.643444
252.811928	7429.795690	8.930650	-0.051992	4.645871
252.681466	7437.816756	8.935655	-0.051973	4.648302
252.876585	7445.833637	8.940659	-0.052014	4.650729
253.108894	7453.913714	8.945664	-0.052063	4.653175
253.402568	7461.894081	8.950669	-0.052123	4.655589
253.571966	7469.931987	8.955674	-0.052160	4.658019
253.518102	7477.894809	8.960679	-0.052155	4.660425
253.694155	7485.917418	8.965683	-0.052193	4.662848
253.744743	7493.887908	8.970688	-0.052208	4.665255
253.917781	7501.933439	8.975693	-0.052245	4.667682
254.106793	7509.951203	8.980698	-0.052285	4.670100
254.123702	7518.053216	8.985703	-0.052294	4.672542
254.268046	7526.078208	8.990707	-0.052326	4.674959
254.584018	7534.080278	8.995712	-0.052390	4.677368
254.638174	7541.997032	9.000717	-0.052405	4.679750
254.994703	7550.073143	9.005722	-0.052477	4.682179
255.058663	7558.010679	9.010727	-0.052494	4.684565
255.046850	7566.077609	9.015731	-0.052497	4.686989
255.356728	7574.084100	9.020736	-0.052560	4.689393
255.465240	7582.107104	9.025741	-0.052586	4.691801
255.581430	7590.114551	9.030746	-0.052613	4.694203
255.591937	7598.136912	9.035751	-0.052620	4.696609
255.637982	7606.110498	9.040755	-0.052634	4.698998
256.022004	7614.168715	9.045760	-0.052711	4.701411
256.124947	7622.143682	9.050765	-0.052735	4.703799
256.151132	7630.222367	9.055770	-0.052745	4.706216
256.368768	7638.183464	9.060775	-0.052791	4.708596
256.593834	7646.259474	9.065779	-0.052838	4.711010
256.454978	7654.328465	9.070784	-0.052818	4.713421
256.437687	7662.268678	9.075789	-0.052820	4.715792
256.732150	7670.285588	9.080794	-0.052880	4.718184
256.789169	7678.237666	9.085799	-0.052896	4.720556
256.954018	7686.250223	9.090803	-0.052932	4.722945
257.222081	7694.354803	9.095808	-0.052987	4.725360
257.159021	7702.325375	9.100813	-0.052980	4.727734
257.249398	7710.380036	9.105818	-0.053002	4.730132
257.399972	7718.421559	9.110823	-0.053036	4.732524
257.670522	7726.384380	9.115827	-0.053091	4.734891
257.848606	7734.455438	9.120832	-0.053130	4.737290
258.080212	7742.407175	9.125837	-0.053178	4.739652
258.158963	7750.467615	9.130842	-0.053198	4.742045
258.217790	7758.412012	9.135847	-0.053214	4.744403
258.292235	7766.490037	9.140851	-0.053233	4.746799
258.733149	7774.521398	9.145856	-0.053321	4.749179
258.859348	7782.513439	9.150861	-0.053350	4.751547
258.902698	7790.583444	9.155866	-0.053363	4.753937
259.059285	7798.591325	9.160871	-0.053397	4.756307
259.016911	7806.504915	9.165875	-0.053395	4.758649
259.234790	7814.613420	9.170880	-0.053441	4.761047
259.389087	7822.511947	9.175885	-0.053474	4.763381
259.572497	7830.573308	9.180890	-0.053514	4.765762
259.733702	7838.586688	9.185895	-0.053549	4.768128
259.686666	7846.604663	9.190899	-0.053546	4.770495
259.816928	7854.671223	9.195904	-0.053575	4.772874
259.756258	7862.625006	9.200909	-0.053569	4.775220
259.847975	7870.723499	9.205914	-0.053592	4.777606
260.196309	7878.633406	9.210919	-0.053662	4.779935
260.640661	7886.678012	9.215923	-0.053750	4.782302
260.469691	7894.655687	9.220928	-0.053723	4.784650
260.560698	7902.695034	9.225933	-0.053745	4.787014
261.122822	7910.766324	9.230938	-0.053855	4.789385
261.208059	7918.762713	9.235943	-0.053876	4.791734
261.066318	7926.772519	9.240947	-0.053855	4.794087
261.392107	7934.851626	9.245952	-0.053921	4.796457
261.596377	7942.791489	9.250957	-0.053965	4.798786
261.759827	7950.814540	9.255962	-0.054000	4.801138
261.710622	7958.793585	9.260967	-0.053996	4.803477
262.145821	7966.765918	9.265971	-0.054083	4.805811
262.311352	7974.875624	9.270976	-0.054119	4.808185
262.258804	7982.829092	9.275981	-0.054114	4.810513
262.600432	7990.342291	9.280986	-0.054183	4.812709
262.554391	7994.894829	9.285991	-0.054177	4.814041

262.708054	7997.465449	9.290995	-0.054208	4.814792
262.982223	7998.825163	9.296000	-0.054260	4.815188
263.039138	7999.224468	9.301005	-0.054270	4.815304
262.917703	8000.167721	9.306010	-0.054248	4.815581
263.118032	8000.213726	9.311015	-0.054286	4.815593
263.267102	8000.167036	9.316019	-0.054314	4.815579
263.267336	8000.173453	9.321024	-0.054314	4.815581
263.276286	8000.159718	9.326029	-0.054315	4.815577
263.355706	8000.191996	9.331034	-0.054330	4.815586
263.543663	8000.180122	9.336039	-0.054365	4.815581
263.461010	8000.185182	9.341043	-0.054350	4.815583
263.471296	8000.163992	9.346048	-0.054352	4.815577
263.498031	8000.181523	9.351053	-0.054357	4.815582
263.781363	8000.210730	9.356058	-0.054410	4.815589
263.786514	8000.189456	9.361063	-0.054411	4.815583
263.701235	8000.219040	9.366067	-0.054395	4.815592
263.732789	8000.221696	9.371072	-0.054401	4.815592
263.695248	8000.220018	9.376077	-0.054394	4.815592
263.677301	8000.211183	9.381082	-0.054391	4.815590
263.932258	8000.233518	9.386087	-0.054438	4.815595
263.774810	8000.178607	9.391091	-0.054409	4.815580
263.864480	8000.208918	9.396096	-0.054426	4.815588
264.074236	8000.203810	9.401101	-0.054465	4.815586
264.063498	8000.216455	9.406106	-0.054463	4.815589
264.036087	8000.187171	9.411111	-0.054458	4.815581
264.134387	8000.199465	9.416115	-0.054476	4.815584
264.286181	8000.190204	9.421120	-0.054504	4.815581
264.163283	8000.166834	9.426125	-0.054481	4.815574
264.158371	8000.228709	9.431130	-0.054481	4.815592
264.265788	8000.196291	9.436135	-0.054501	4.815582
264.223459	8000.192398	9.441139	-0.054493	4.815582
264.303152	8000.199047	9.446144	-0.054508	4.815583
264.122400	8000.192888	9.451149	-0.054474	4.815582
264.233825	8000.212874	9.456154	-0.054495	4.815587
264.231889	8000.233141	9.461159	-0.054495	4.815593
264.298464	8000.207531	9.466163	-0.054507	4.815586
264.202545	8000.252963	9.471168	-0.054489	4.815599
264.089650	8000.208394	9.476173	-0.054468	4.815587
264.471149	8000.266981	9.481178	-0.054539	4.815602
264.356042	8000.218103	9.486183	-0.054518	4.815588
264.188448	8000.217499	9.491187	-0.054487	4.815589
264.200595	8000.226247	9.496192	-0.054489	4.815592
264.227014	8000.176482	9.501197	-0.054494	4.815577
264.212219	8000.202947	9.506202	-0.054491	4.815585
264.342524	8000.210424	9.511207	-0.054516	4.815586
264.476082	8000.239318	9.516211	-0.054541	4.815594
264.475234	8000.232899	9.521216	-0.054540	4.815592
264.389614	8000.210139	9.526221	-0.054525	4.815586
264.469400	8000.219994	9.531226	-0.054539	4.815588
264.423053	8000.204285	9.536231	-0.054531	4.815584
264.592743	8000.209203	9.541235	-0.054562	4.815585
264.578243	8000.248491	9.546240	-0.054560	4.815596
264.626459	8000.214036	9.551245	-0.054569	4.815586
264.609441	8000.224442	9.556250	-0.054566	4.815589
264.735056	8000.231843	9.561255	-0.054589	4.815591
264.617861	8000.233133	9.566259	-0.054567	4.815592
264.688498	8000.259929	9.571264	-0.054581	4.815599
264.489198	8000.253465	9.576269	-0.054544	4.815598
264.610739	8000.265072	9.581274	-0.054566	4.815601
264.666214	8000.237145	9.586279	-0.054577	4.815592
264.624436	8000.203353	9.591283	-0.054569	4.815583
264.849357	8000.289286	9.596288	-0.054611	4.815607
264.560513	8000.267470	9.601293	-0.054557	4.815602
264.747568	8000.251310	9.606298	-0.054592	4.815596
264.695176	8000.263274	9.611303	-0.054582	4.815600
264.726061	8000.232808	9.616307	-0.054588	4.815591
264.768884	8000.257012	9.621312	-0.054596	4.815598
264.684259	8000.211837	9.626317	-0.054580	4.815585
264.636444	8000.233489	9.631322	-0.054571	4.815592
264.751166	8000.217212	9.636327	-0.054593	4.815586
264.904404	8000.199431	9.641331	-0.054621	4.815580
264.897977	8000.245259	9.646336	-0.054620	4.815594
264.848684	8000.210276	9.651341	-0.054611	4.815584
264.977975	8000.245509	9.656346	-0.054635	4.815593
264.978281	8000.276494	9.661351	-0.054635	4.815602
264.998851	8000.288585	9.666355	-0.054639	4.815606
265.117087	8000.293729	9.671360	-0.054661	4.815607
264.881583	8000.219379	9.676365	-0.054617	4.815586
265.061898	8000.250107	9.681370	-0.054651	4.815594
264.908039	8000.314885	9.686375	-0.054623	4.815614
264.859551	8000.297005	9.691379	-0.054614	4.815609
264.971223	8000.261452	9.696384	-0.054634	4.815598
264.862942	8000.260751	9.701389	-0.054614	4.815598
265.107125	8000.262617	9.706394	-0.054660	4.815598
264.894768	8000.244190	9.711399	-0.054620	4.815593
264.986523	8000.225402	9.716403	-0.054637	4.815587
265.105597	8000.275422	9.721408	-0.054660	4.815601
264.916432	8000.202899	9.726413	-0.054624	4.815581
264.934106	8000.264077	9.731418	-0.054628	4.815599
265.167888	8000.258295	9.736423	-0.054671	4.815596
265.150335	8000.249467	9.741427	-0.054668	4.815594
264.969762	8000.251855	9.746432	-0.054635	4.815595
264.965097	8000.213329	9.751437	-0.054634	4.815584
265.147766	8000.252641	9.756442	-0.054668	4.815595
265.166297	8000.330924	9.761447	-0.054671	4.815617
264.961968	8000.301946	9.766451	-0.054633	4.815610
265.304149	8000.284054	9.771456	-0.054697	4.815603
265.116750	8000.260694	9.776461	-0.054662	4.815597
265.141550	8000.262172	9.781466	-0.054667	4.815597
265.476744	8000.279416	9.786471	-0.054729	4.815601
265.295202	8000.244401	9.791475	-0.054696	4.815592
265.139707	8000.267495	9.796480	-0.054667	4.815599
265.272857	8000.225885	9.801485	-0.054691	4.815586
265.399015	8000.265340	9.806490	-0.054715	4.815597
265.323847	8000.242750	9.811495	-0.054701	4.815591
265.216645	8000.233521	9.816499	-0.054681	4.815589
265.465659	8000.269648	9.821504	-0.054728	4.815598
265.308031	8000.213663	9.826509	-0.054698	4.815582
265.336210	8000.304922	9.831514	-0.054704	4.815609
265.314491	8000.288547	9.836519	-0.054700	4.815604
265.318142	8000.231999	9.841523	-0.054700	4.815588
265.387996	8000.257714	9.846528	-0.054713	4.815595
265.500936	8000.218978	9.851533	-0.054734	4.815583
265.656117	8000.252500	9.856538	-0.054763	4.815592
265.698203	8000.225421	9.861543	-0.054771	4.815584
265.628211	8000.228551	9.866547	-0.054758	4.815585
265.482181	8000.279572	9.871552	-0.054731	4.815601
265.260763	8000.207587	9.876557	-0.054690	4.815581
265.383243	8000.257664	9.881562	-0.054713	4.815595
265.357067	8000.279671	9.886567	-0.054708	4.815601
265.496504	8000.230687	9.891571	-0.054734	4.815587
265.665621	8000.234529	9.896576	-0.054765	4.815587
265.281320	8000.210080	9.901581	-0.054694	4.815582
265.489014	8000.270098	9.906586	-0.054733	4.815598
265.561885	8000.234978	9.911591	-0.054746	4.815587
265.453095	8000.222518	9.916595	-0.054726	4.815584
265.777242	8000.319694	9.921600	-0.054787	4.815611
265.618484	8000.257280	9.926605	-0.054757	4.815594
265.505087	8000.221245	9.931610	-0.054736	4.815584
265.539422	8000.230357	9.936615	-0.054742	4.815586
265.567822	8000.266075	9.941619	-0.054748	4.815596
265.660145	8000.241956	9.946624	-0.054765	4.815589
265.675016	8000.213363	9.951629	-0.054768	4.815581
265.729605	8000.274078	9.956634	-0.054778	4.815598
265.655713	8000.208782	9.961639	-0.054764	4.815579
265.705081	8000.241639	9.966643	-0.054773	4.815589
265.724552	8000.246235	9.971648	-0.054777	4.815590
265.561055	8000.227538	9.976653	-0.054747	4.815585
265.752040	8000.256306	9.981658	-0.054782	4.815593
265.801446	8000.218666	9.986663	-0.054792	4.815582
265.614234	8000.216671	9.991667	-0.054757	4.815582
265.812786	8000.284018	9.996672	-0.054794	4.815601
265.619204	8000.200738	10.001677	-0.054758	4.815577
265.847096	8000.216225	10.006682	-0.054800	4.815581
265.755982	8000.251054	10.011687	-0.054783	4.815591
265.778555	8000.222587	10.016691	-0.054788	4.815583
265.935020	8000.263608	10.021696	-0.054817	4.815594
265.783600	8000.222678	10.026701	-0.054789	4.815583
265.819335	8000.228608	10.031706	-0.054795	4.815584
265.349527	8000.202758	10.036711	-0.054708	4.815579
265.531271	8000.199330	10.041715	-0.054742	4.815577
265.777599	8000.239686	10.046720	-0.054788	4.815588
265.501860	8000.208469	10.051725	-0.054736	4.815580
265.655264	8000.270803	10.056730	-0.054765	4.815597
265.653507	8000.254756	10.061735	-0.054765	4.815593
265.656623	8000.223834	10.066739	-0.054765	4.815584
265.829315	8000.306779	10.071744	-0.054798	4.815607
265.568441	8000.250170	10.076749	-0.054749	4.815592
265.551116	8000.273389	10.081754	-0.054746	4.815599
265.641126	8000.213982	10.086759	-0.054763	4.815581
265.850134	8000.228091	10.091763	-0.054802	4.815584
265.906044	8000.233284	10.096768	-0.054812	4.815585
265.533812	8000.188737	10.101773	-0.054743	4.815574
265.685045	8000.235013	10.106778	-0.054771	4.815587
265.799826	8000.268942	10.111783	-0.054792	4.815596
265.717043	8000.244090	10.116787	-0.054777	4.815589
265.740607	8000.246616	10.121792	-0.054781	4.815590
265.867679	8000.234815	10.126797	-0.054805	4.815586
265.943584	8000.275585	10.131802	-0.054819	4.815597
265.821872	8000.280004	10.136807	-0.054797	4.815599
265.829213	8000.247015	10.141811	-0.054798	4.815590
265.895857	8000.269474	10.146816	-0.054811	4.815596
265.672044	8000.245517	10.151821	-0.054769	4.815590
265.696297	8000.245918	10.156826	-0.054774	4.815590
265.964109	8000.240695	10.161831	-0.054823	4.815587
265.763144	8000.238476	10.166835	-0.054786	4.815587
265.711037	8000.273944	10.171840	-0.054776	4.815598
265.886719	8000.236235	10.176845	-0.054809	4.815586
265.992306	8000.270014	10.181850	-0.054829	4.815596
265.730676	8000.272141	10.186855	-0.054780	4.815597
265.789127	8000.239989	10.191859	-0.054791	4.815588
265.847305	8000.315718	10.196864	-0.054802	4.815610
265.609889	8000.241334	10.201869	-0.054758	4.815589
265.850577	8000.238871	10.206874	-0.054803	4.815587
265.980515	8000.253822	10.211879	-0.054827	4.815591
265.701891	8000.238580	10.216883	-0.054775	4.815588
265.741488	8000.271277	10.221888	-0.054783	4.815597
265.859241	8000.257188	10.226893	-0.054804	4.815592
265.844427	8000.274040	10.231898	-0.054802	4.815597
265.701676	8000.324046	10.236903	-0.054775	4.815613
265.647443	8000.255867	10.241907	-0.054765	4.815593
266.054106	8000.273214	10.246912	-0.054841	4.815596
265.874195	8000.258521	10.251917	-0.054808	4.815593
265.945685	8000.273582	10.256922	-0.054821	4.815597
266.118901	8000.289242	10.261927	-0.054853	4.815601
265.902408	8000.269676	10.266931	-0.054813	4.815596
265.890951	8000.300470	10.271936	-0.054811	4.815605
265.866864	8000.272306	10.276941	-0.054806	4.815597
265.846552	8000.265569	10.281946	-0.054803	4.815595
265.852250	8000.260325	10.286951	-0.054804	4.815593
265.767363	8000.252530	10.291955	-0.054788	4.815592
265.885704	8000.257677	10.296960	-0.054810	4.815592
266.002959	8000.236101	10.301965	-0.054832	4.815586
266.079928	8000.265139	10.306970	-0.054846	4.815594
266.038614	8000.270875	10.311975	-0.054839	4.815596
266.018916	8000.245988	10.316979	-0.054835	4.815588
265.846666	8000.265602	10.321984	-0.054803	4.815595
265.798444	8000.224226	10.326989	-0.054794	4.815583
266.115656	8000.236903	10.331994	-0.054853	4.815585
266.010017	8000.237313	10.336999	-0.054834	4.815586
265.904794	8000.253752	10.342003	-0.054814	4.815591
266.113630	8000.294563	10.347008	-0.054853	4.815602
266.121248	8000.272260	10.352013	-0.054854	4.815596
266.080376	8000.249163	10.357018	-0.054847	4.815589
266.141731	8000.240559	10.362023	-0.054858	4.815586
266.119155	8000.244465	10.367027	-0.054854	4.815587
265.985980	8000.320264	10.372032	-0.054829	4.815610
265.904742	8000.265529	10.377037	-0.054814	4.815595
266.092860	8000.289978	10.382042	-0.054849	4.815601
266.266248	8000.286414	10.387047	-0.054882	4.815599
266.190582	8000.256337	10.392051	-0.054868	4.815591
266.201216	8000.255447	10.397056	-0.054870	4.815590
265.872407	8000.274632	10.402061	-0.054809	4.815597
265.876784	8000.280049	10.407066	-0.054809	4.815599
266.113452	8000.265771	10.412071	-0.054853	4.815594
265.937101	8000.244727	10.417075	-0.054821	4.815588
266.070299	8000.286435	10.422080	-0.054846	4.815600
266.028401	8000.271867	10.427085	-0.054838	4.815596
266.052957	8000.282955	10.432090	-0.054842	4.815599
266.109874	8000.284959	10.437095	-0.054853	4.815599
265.876784	8000.246963	10.442099	-0.054810	4.815589
266.127490	8000.316233	10.447104	-0.054856	4.815608
266.079698	8000.309045	10.452109	-0.054848	4.815606
265.999912	8000.295992	10.457114	-0.054833	4.815603
266.102419	8000.281652	10.462119	-0.054852	4.815598
266.364464	8000.240018	10.467123	-0.054901	4.815585
266.356184	8000.283682	10.472128	-0.054899	4.815598
266.256316	8000.237186	10.477133	-0.054881	4.815585
266.231742	8000.265628	10.482138	-0.054876	4.815593
266.368956	8000.260403	10.487143	-0.054902	4.815591
266.283579	8000.265417	10.492147	-0.054886	4.815593
266.147822	8000.293106	10.497152	-0.054861	4.815601
266.114831	8000.263728	10.502157	-0.054855	4.815593
266.208924	8000.265274	10.507162	-0.054872	4.815593
266.187456	8000.267062	10.512167	-0.054868	4.815594
266.111615	8000.257278	10.517171	-0.054854	4.815591
266.116100	8000.231720	10.522176	-0.054855	4.815584
266.219864	8000.217401	10.527181	-0.054874	4.815579
266.265295	8000.229899	10.532186	-0.054883	4.815582
266.199914	8000.270491	10.537191	-0.054871	4.815595
266.164636	8000.213303	10.542195	-0.054864	4.815578
266.327557	8000.325999	10.547200	-0.054895	4.815610
266.407317	8000.268560	10.552205	-0.054909	4.815593
266.114772	8000.211430	10.557210	-0.054855	4.815578
266.000631	8000.245882	10.562215	-0.054834	4.815588
266.204811	8000.247095	10.567219	-0.054872	4.815588
266.310150	8000.284075	10.572224	-0.054892	4.815598
266.116524	8000.243520	10.577229	-0.054856	4.815587
266.262076	8000.266204	10.582234	-0.054883	4.815593
266.289031	8000.280536	10.587239	-0.054888	4.815597
266.119285	8000.251054	10.592243	-0.054856	4.815589
266.449551	8000.314151	10.597248	-0.054918	4.815606
266.388645	8000.273634	10.602253	-0.054906	4.815595
266.477211	8000.282567	10.607258	-0.054923	4.815597
266.431369	8000.249774	10.612263	-0.054914	4.815587
266.455229	8000.227737	10.617267	-0.054919	4.815581
266.168278	8000.248676	10.622272	-0.054866	4.815588
266.299938	8000.243360	10.627277	-0.054890	4.815586
266.440273	8000.267027	10.632282	-0.054916	4.815592
266.474533	8000.282547	10.637287	-0.054923	4.815597
266.165113	8000.241163	10.642291	-0.054865	4.815586
266.163200	8000.255022	10.647296	-0.054865	4.815590
266.416813	8000.257044	10.652301	-0.054912	4.815590
266.259432	8000.257674	10.657306	-0.054883	4.815591
266.216079	8000.254832	10.662311	-0.054875	4.815590
266.308769	8000.253150	10.667315	-0.054892	4.815589
266.368047	8000.261602	10.672320	-0.054903	4.815591
266.497622	8000.268002	10.677325	-0.054927	4.815592
266.275749	8000.273984	10.682330	-0.054886	4.815595
266.244992	8000.279893	10.687335	-0.054880	4.815597
266.188472	8000.236244	10.692339	-0.054870	4.815585
266.371658	8000.292658	10.697344	-0.054904	4.815600
266.399612	8000.268552	10.702349	-0.054909	4.815593
266.229694	8000.250818	10.707354	-0.054878	4.815589
266.266009	8000.270644	10.712359	-0.054885	4.815594
266.355159	8000.247540	10.717363	-0.054901	4.815587
266.362253	8000.285047	10.722368	-0.054903	4.815598
266.274428	8000.270794	10.727373	-0.054886	4.815594
266.222272	8000.275284	10.732378	-0.054877	4.815596
266.504310	8000.315159	10.737383	-0.054929	4.815606
266.247931	8000.269303	10.742387	-0.054881	4.815594
266.285196	8000.279531	10.747392	-0.054888	4.815597
266.505349	8000.268188	10.752397	-0.054930	4.815592
266.450746	8000.260888	10.757402	-0.054919	4.815591
266.231888	8000.243420	10.762407	-0.054879	4.815587
266.290291	8000.255062	10.767411	-0.054890	4.815590
266.525581	8000.282422	10.772416	-0.054933	4.815596
266.278802	8000.278382	10.777421	-0.054888	4.815596
266.175776	8000.273493	10.782426	-0.054868	4.815596
266.302500	8000.301210	10.787431	-0.054892	4.815603
266.210322	8000.220658	10.792435	-0.054875	4.815580
266.266857	8000.249361	10.797440	-0.054886	4.815588
266.343451	8000.220711	10.802445	-0.054900	4.815579
266.348959	8000.254987	10.807450	-0.054901	4.815589
266.371449	8000.257496	10.812455	-0.054905	4.815590
266.315506	8000.243765	10.817459	-0.054895	4.815586
266.492479	8000.286191	10.822464	-0.054928	4.815598
266.247234	8000.270427	10.827469	-0.054882	4.815594
266.384526	8000.257726	10.832474	-0.054908	4.815590
266.512926	8000.263038	10.837479	-0.054932	4.815591
266.533743	8000.219588	10.842483	-0.054936	4.815578
266.353908	8000.250827	10.847488	-0.054902	4.815588
266.341815	8000.246360	10.852493	-0.054900	4.815587
266.602019	8000.236741	10.857498	-0.054948	4.815583
266.613286	8000.257225	10.862503	-0.054951	4.815589
266.411640	8000.277425	10.867507	-0.054913	4.815596
266.619450	8000.274425	10.872512	-0.054952	4.815594
266.580516	8000.273791	10.877517	-0.054945	4.815594
266.267077	8000.272932	10.882522	-0.054886	4.815595
266.438631	8000.299247	10.887527	-0.054918	4.815602
266.387048	8000.230042	10.892531	-0.054909	4.815582
266.498693	8000.269262	10.897536	-0.054930	4.815593
266.581380	8000.243916	10.902541	-0.054945	4.815585
266.704638	8000.251280	10.907546	-0.054968	4.815587
266.636551	8000.271532	10.912551	-0.054955	4.815593
266.505053	8000.257631	10.917555	-0.054931	4.815589
266.663216	8000.247409	10.922560	-0.054960	4.815586
266.352266	8000.239113	10.927565	-0.054903	4.815585
266.336041	8000.224965	10.932570	-0.054900	4.815581
266.537972	8000.284891	10.937575	-0.054937	4.815597
266.648353	8000.236499	10.942579	-0.054958	4.815582
266.535836	8000.270978	10.947584	-0.054937	4.815593
266.708194	8000.239624	10.952589	-0.054969	4.815583
266.619041	8000.260599	10.957594	-0.054953	4.815590
266.911381	8000.246166	10.962599	-0.055007	4.815584
266.699159	8000.241624	10.967603	-0.054968	4.815584
266.528489	8000.259127	10.972608	-0.054936	4.815590
266.708751	8000.259948	10.977613	-0.054969	4.815589
266.585909	8000.242985	10.982618	-0.054947	4.815585
266.474219	8000.243295	10.987623	-0.054926	4.815585
266.501982	8000.258709	10.992627	-0.054931	4.815590
266.473628	8000.266793	10.997632	-0.054926	4.815592
266.428138	8000.298098	11.002637	-0.054917	4.815601
266.470863	8000.260347	11.007642	-0.054925	4.815590
266.675234	8000.274382	11.012647	-0.054963	4.815593
266.548429	8000.207148	11.017651	-0.054940	4.815574
266.624260	8000.246849	11.022656	-0.054954	4.815586
266.700049	8000.231004	11.027661	-0.054968	4.815581
266.600443	8000.236853	11.032666	-0.054950	4.815583
266.566618	8000.258735	11.037671	-0.054943	4.815589
266.634481	8000.209646	11.042675	-0.054956	4.815575
266.677304	8000.256284	11.047680	-0.054964	4.815588
266.542014	8000.232707	11.052685	-0.054939	4.815582
266.664633	8000.265698	11.057690	-0.054962	4.815591
266.686955	8000.286363	11.062695	-0.054966	4.815597
266.514406	8000.234403	11.067699	-0.054934	4.815582
266.404744	8000.246497	11.072704	-0.054914	4.815587
266.603258	8000.242276	11.077709	-0.054951	4.815584
266.573145	8000.236446	11.082714	-0.054945	4.815583
266.782703	8000.250565	11.087719	-0.054984	4.815586
266.829160	8000.239580	11.092723	-0.054993	4.815582
266.774358	8000.251505	11.097728	-0.054983	4.815586
266.826354	8000.267315	11.102733	-0.054992	4.815591
266.646305	8000.254755	11.107738	-0.054959	4.815588
266.834266	8000.271726	11.112743	-0.054994	4.815592
266.826338	8000.229940	11.117747	-0.054993	4.815580
266.763767	8000.260965	11.122752	-0.054981	4.815589
266.590948	8000.233568	11.127757	-0.054949	4.815582
266.519321	8000.232399	11.132762	-0.054936	4.815582
266.795254	8000.257220	11.137767	-0.054987	4.815588
266.769247	8000.223683	11.142771	-0.054982	4.815578
266.828491	8000.271659	11.147776	-0.054993	4.815592
266.713497	8000.272983	11.152781	-0.054972	4.815593
266.681385	8000.254301	11.157786	-0.054966	4.815587
266.905034	8000.277198	11.162791	-0.055008	4.815593
266.624845	8000.222405	11.167795	-0.054955	4.815578
266.886629	8000.240585	11.172800	-0.055004	4.815582
266.832359	8000.242905	11.177805	-0.054994	4.815583
266.925648	8000.227346	11.182810	-0.055012	4.815578
266.770610	8000.254719	11.187815	-0.054983	4.815587
266.600650	8000.248733	11.192819	-0.054951	4.815586
266.680403	8000.260726	11.197824	-0.054966	4.815589
266.783374	8000.256008	11.202829	-0.054985	4.815587
266.874870	8000.273535	11.207834	-0.055002	4.815592
266.884652	8000.314290	11.212839	-0.055004	4.815604
266.674087	8000.322594	11.217843	-0.054965	4.815607
266.653925	8000.332949	11.222848	-0.054961	4.815611
266.645054	8000.283671	11.227853	-0.054960	4.815596
266.717045	8000.282718	11.232858	-0.054973	4.815596
266.726486	8000.271127	11.237863	-0.054975	4.815592
266.688603	8000.254487	11.242867	-0.054968	4.815587
266.616991	8000.293909	11.247872	-0.054955	4.815599
266.587514	8000.256043	11.252877	-0.054949	4.815588
266.568336	8000.262142	11.257882	-0.054946	4.815590
266.894601	8000.293129	11.262887	-0.055007	4.815598
266.800792	8000.214685	11.267891	-0.054989	4.815575
266.776293	8000.259152	11.272896	-0.054985	4.815588
266.935722	8000.231859	11.277901	-0.055014	4.815580
266.842609	8000.231405	11.282906	-0.054997	4.815580
266.947533	8000.252356	11.287911	-0.055017	4.815586
266.887728	8000.279153	11.292915	-0.055006	4.815594
266.905937	8000.292274	11.297920	-0.055009	4.815597
266.911100	8000.252839	11.302925	-0.055010	4.815586
266.827081	8000.243989	11.307930	-0.054994	4.815584
266.925958	8000.323592	11.312935	-0.055013	4.815606
266.901881	8000.254837	11.317939	-0.055008	4.815587
266.968469	8000.300796	11.322944	-0.055021	4.815600
266.758900	8000.264251	11.327949	-0.054982	4.815590
266.673683	8000.253245	11.332954	-0.054966	4.815587
266.737149	8000.292744	11.337959	-0.054978	4.815598
266.757667	8000.237538	11.342963	-0.054982	4.815582
266.956533	8000.245074	11.347968	-0.055019	4.815583
266.767888	8000.248396	11.352973	-0.054984	4.815585
266.748220	8000.267305	11.357978	-0.054980	4.815591
266.887687	8000.284549	11.362983	-0.055006	4.815595
266.771970	8000.245270	11.367987	-0.054985	4.815584
266.817151	8000.262037	11.372992	-0.054993	4.815589
266.895395	8000.263323	11.377997	-0.055008	4.815589
266.856196	8000.241321	11.383002	-0.055000	4.815583
266.749102	8000.283366	11.388007	-0.054981	4.815596
266.664031	8000.230702	11.393011	-0.054965	4.815581
266.732781	8000.272424	11.398016	-0.054978	4.815592
266.809604	8000.216005	11.403021	-0.054992	4.815576
266.800946	8000.240435	11.408026	-0.054990	4.815583
266.739509	8000.269342	11.413031	-0.054979	4.815592
266.739990	8000.265081	11.418035	-0.054979	4.815590
266.720206	8000.279715	11.423040	-0.054976	4.815595
266.716605	8000.296751	11.428045	-0.054975	4.815600
266.803217	8000.250106	11.433050	-0.054991	4.815586
266.854000	8000.290465	11.438055	-0.055001	4.815597
266.684913	8000.267403	11.443059	-0.054969	4.815591
266.746901	8000.295127	11.448064	-0.054981	4.815599
266.707843	8000.292355	11.453069	-0.054974	4.815598
266.587579	8000.257274	11.458074	-0.054951	4.815589
266.890170	8000.263305	11.463079	-0.055008	4.815589
266.795538	8000.255349	11.468083	-0.054990	4.815587
266.760010	8000.269725	11.473088	-0.054983	4.815592
266.942398	8000.269514	11.478093	-0.055017	4.815591
267.018966	8000.270772	11.483098	-0.055032	4.815591
266.774380	8000.313769	11.488103	-0.054986	4.815604
266.626579	8000.256873	11.493107	-0.054959	4.815588
266.890230	8000.295379	11.498112	-0.055008	4.815598
266.768484	8000.272024	11.503117	-0.054985	4.815592
266.694342	8000.255858	11.508122	-0.054971	4.815588
266.829089	8000.304003	11.513127	-0.054997	4.815601
266.917019	8000.262720	11.518131	-0.055013	4.815589
266.812664	8000.285582	11.523136	-0.054994	4.815596
266.865868	8000.262958	11.528141	-0.055004	4.815589
266.877352	8000.243922	11.533146	-0.055006	4.815583
266.902092	8000.269969	11.538151	-0.055010	4.815591
267.062287	8000.240552	11.543155	-0.055040	4.815582
266.934913	8000.268378	11.548160	-0.055017	4.815590
267.064893	8000.256626	11.553165	-0.055041	4.815586
267.007340	8000.246073	11.558170	-0.055030	4.815583
267.122478	8000.298169	11.563175	-0.055052	4.815598
267.029335	8000.246441	11.568179	-0.055034	4.815583
266.937027	8000.285524	11.573184	-0.055017	4.815595
267.041510	8000.275490	11.578189	-0.055037	4.815592
267.103531	8000.256214	11.583194	-0.055048	4.815586
267.221640	8000.290200	11.588199	-0.055070	4.815595
266.900742	8000.264649	11.593203	-0.055011	4.815589
266.987916	8000.282105	11.598208	-0.055027	4.815594
267.025817	8000.312639	11.603213	-0.055034	4.815603
266.910153	8000.250928	11.608218	-0.055013	4.815585
266.912632	8000.237086	11.613223	-0.055013	4.815581
266.898724	8000.242204	11.618227	-0.055011	4.815583
266.866366	8000.279064	11.623232	-0.055005	4.815594
267.034477	8000.286096	11.628237	-0.055036	4.815595
267.105491	8000.242399	11.633242	-0.055049	4.815582
267.031244	8000.256141	11.638247	-0.055035	4.815586
267.024520	8000.221853	11.643251	-0.055034	4.815576
266.814065	8000.281431	11.648256	-0.054995	4.815595
266.843011	8000.250932	11.653261	-0.055000	4.815586
266.680739	8000.241868	11.658266	-0.054970	4.815584
266.998426	8000.260964	11.663271	-0.055029	4.815588
267.071525	8000.242939	11.668275	-0.055043	4.815582
266.867480	8000.289804	11.673280	-0.055005	4.815597
266.836745	8000.244440	11.678285	-0.055000	4.815584
266.750908	8000.238764	11.683290	-0.054984	4.815582
267.021026	8000.270968	11.688295	-0.055034	4.815591
266.872933	8000.245045	11.693299	-0.055006	4.815584
266.899215	8000.257230	11.698304	-0.055011	4.815587
267.014479	8000.280487	11.703309	-0.055033	4.815593
266.952691	8000.252773	11.708314	-0.055021	4.815586
266.976150	8000.292685	11.713319	-0.055026	4.815597
267.000493	8000.259973	11.718323	-0.055030	4.815587
267.002119	8000.310209	11.723328	-0.055031	4.815602
266.922966	8000.288620	11.728333	-0.055016	4.815596
266.811587	8000.297481	11.733338	-0.054995	4.815599
267.034902	8000.303281	11.738343	-0.055037	4.815600
266.979194	8000.267121	11.743347	-0.055027	4.815590
267.113085	8000.260774	11.748352	-0.055052	4.815587
267.048074	8000.307782	11.753357	-0.055040	4.815601
266.785093	8000.246861	11.758362	-0.054991	4.815585
266.919422	8000.287522	11.763367	-0.055016	4.815596
267.027587	8000.280753	11.768371	-0.055036	4.815593
267.033322	8000.309692	11.773376	-0.055037	4.815602
266.856766	8000.332439	11.778381	-0.055004	4.815609
266.914939	8000.259691	11.783386	-0.055015	4.815588
266.878367	8000.243072	11.788391	-0.055008	4.815583
266.739747	8000.227986	11.793395	-0.054982	4.815579
266.856269	8000.266219	11.798400	-0.055004	4.815590
266.904844	8000.293724	11.803405	-0.055013	4.815598
266.887859	8000.279563	11.808410	-0.055010	4.815594
266.942201	8000.268707	11.813415	-0.055020	4.815590
266.959227	8000.223057	11.818419	-0.055024	4.815577
267.005418	8000.250523	11.823424	-0.055032	4.815585
266.944501	8000.243120	11.828429	-0.055021	4.815583
267.024291	8000.236954	11.833434	-0.055036	4.815581
267.316227	8000.270584	11.838439	-0.055090	4.815589
267.100341	8000.272391	11.843443	-0.055050	4.815591
266.967608	8000.281969	11.848448	-0.055025	4.815594
267.007714	8000.259130	11.853453	-0.055033	4.815587
266.998322	8000.223730	11.858458	-0.055031	4.815577
267.115888	8000.248093	11.863463	-0.055053	4.815583
267.077830	8000.266700	11.868467	-0.055046	4.815589
267.073895	8000.289072	11.873472	-0.055045	4.815596
267.017260	8000.330876	11.878477	-0.055035	4.815608
266.966814	8000.243529	11.883482	-0.055026	4.815583
267.113601	8000.242734	11.888487	-0.055053	4.815582
267.002802	8000.287923	11.893491	-0.055032	4.815596
266.783810	8000.256565	11.898496	-0.054992	4.815587
266.929264	8000.254679	11.903501	-0.055019	4.815586
266.994175	8000.270702	11.908506	-0.055031	4.815591
267.093504	8000.288357	11.913511	-0.055049	4.815595
266.785753	8000.271567	11.918515	-0.054992	4.815592
266.891789	8000.281854	11.923520	-0.055012	4.815594
267.027678	8000.265926	11.928525	-0.055037	4.815589
266.667619	8000.246143	11.933530	-0.054970	4.815585
266.941682	8000.266661	11.938535	-0.055021	4.815590
266.917736	8000.250249	11.943539	-0.055017	4.815585
266.728126	8000.282396	11.948544	-0.054982	4.815595
266.860897	8000.318759	11.953549	-0.055007	4.815605
266.923023	8000.292008	11.958554	-0.055018	4.815597
266.993098	8000.262182	11.963559	-0.055031	4.815588
266.929214	8000.294253	11.968563	-0.055019	4.815598
267.125224	8000.286788	11.973568	-0.055056	4.815595
266.988539	8000.317666	11.978573	-0.055031	4.815604
266.939500	8000.247433	11.983578	-0.055021	4.815584
266.964026	8000.267067	11.988583	-0.055026	4.815590
266.891063	8000.228488	11.993587	-0.055012	4.815579
266.814335	8000.277440	11.998592	-0.054998	4.815593
266.932949	8000.301820	12.003597	-0.055020	4.815600
266.870800	8000.234577	12.008602	-0.055009	4.815581
267.135930	8000.277381	12.013607	-0.055058	4.815592
266.949541	8000.264716	12.018611	-0.055024	4.815589
267.032819	8000.287449	12.023616	-0.055039	4.815595
267.056043	8000.327358	12.028621	-0.055044	4.815607
266.879026	8000.302028	12.033626	-0.055011	4.815600
267.044760	8000.276975	12.038631	-0.055042	4.815592
266.956977	8000.243494	12.043635	-0.055025	4.815583
266.811609	8000.247525	12.048640	-0.054998	4.815585
267.140071	8000.287094	12.053645	-0.055059	4.815595
267.085621	8000.243478	12.058650	-0.055049	4.815582
267.121393	8000.238727	12.063655	-0.055056	4.815581
267.055611	8000.236585	12.068659	-0.055044	4.815580
267.013447	8000.245511	12.073664	-0.055036	4.815583
267.107938	8000.275906	12.078669	-0.055054	4.815592
266.813106	8000.235827	12.083674	-0.054999	4.815581
267.120943	8000.254762	12.088679	-0.055056	4.815585
267.172250	8000.265221	12.093683	-0.055066	4.815588
266.983160	8000.261058	12.098688	-0.055031	4.815588
267.253756	8000.276179	12.103693	-0.055081	4.815591
267.230597	8000.282213	12.108698	-0.055077	4.815593
267.279363	8000.277675	12.113703	-0.055086	4.815591
267.060602	8000.239911	12.118707	-0.055045	4.815581
266.943699	8000.262567	12.123712	-0.055023	4.815588
266.999014	8000.310479	12.128717	-0.055034	4.815602
266.775580	8000.283320	12.133722	-0.054992	4.815595
266.868165	8000.281637	12.138727	-0.055010	4.815594
266.948289	8000.277613	12.143731	-0.055024	4.815593
266.914287	8000.267446	12.148736	-0.055018	4.815590
266.948854	8000.247721	12.153741	-0.055025	4.815584
266.992837	8000.292242	12.158746	-0.055033	4.815597
267.008733	8000.299984	12.163751	-0.055036	4.815599
267.063273	8000.262426	12.168755	-0.055046	4.815588
267.222657	8000.247951	12.173760	-0.055076	4.815583
267.144911	8000.303296	12.178765	-0.055061	4.815599
267.043958	8000.245030	12.183770	-0.055043	4.815583
267.223696	8000.290708	12.188775	-0.055076	4.815595
267.165194	8000.259844	12.193779	-0.055065	4.815587
267.131806	8000.253959	12.198784	-0.055059	4.815585
267.133204	8000.317010	12.203789	-0.055059	4.815603
266.986713	8000.252657	12.208794	-0.055032	4.815585
267.282942	8000.250039	12.213799	-0.055087	4.815583
267.113009	8000.259008	12.218803	-0.055056	4.815587
267.111963	8000.264336	12.223808	-0.055056	4.815588
267.225510	8000.411478	12.228813	-0.055077	4.815631
267.063867	8000.335125	12.233818	-0.055047	4.815609
267.046235	8000.386114	12.238823	-0.055044	4.815624
267.042861	8000.345471	12.243827	-0.055043	4.815612
267.125825	8000.293424	12.248832	-0.055058	4.815596
266.956752	8000.288521	12.253837	-0.055027	4.815596
266.901756	8000.266259	12.258842	-0.055017	4.815590
266.953138	8000.292742	12.263847	-0.055026	4.815597
266.809278	8000.225228	12.268851	-0.055000	4.815578
267.062824	8000.216569	12.273856	-0.055047	4.815574
267.082044	8000.240388	12.278861	-0.055051	4.815581
267.006999	8000.242367	12.283866	-0.055037	4.815582
266.915245	8000.265436	12.288871	-0.055020	4.815589
267.051452	8000.248445	12.293875	-0.055045	4.815584
266.922386	8000.258083	12.298880	-0.055021	4.815587
266.892528	8000.269348	12.303885	-0.055016	4.815591
267.147174	8000.238275	12.308890	-0.055063	4.815580
267.084379	8000.281046	12.313895	-0.055051	4.815593
266.933559	8000.256146	12.318899	-0.055023	4.815587
267.034460	8000.288782	12.323904	-0.055042	4.815596
267.052212	8000.282667	12.328909	-0.055045	4.815594
266.986673	8000.263438	12.333914	-0.055033	4.815588
267.101481	8000.267460	12.338919	-0.055055	4.815589
267.045609	8000.233434	12.343923	-0.055044	4.815579
267.156368	8000.264094	12.348928	-0.055065	4.815588
266.989294	8000.234655	12.353933	-0.055034	4.815580
266.986538	8000.204704	12.358938	-0.055033	4.815571
267.046610	8000.255898	12.363943	-0.055045	4.815586
266.848148	8000.249445	12.368947	-0.055008	4.815585
266.949783	8000.252183	12.373952	-0.055027	4.815585
267.425190	8000.239683	12.378957	-0.055115	4.815579
267.022513	8000.233087	12.383962	-0.055040	4.815579
267.142287	8000.277782	12.388967	-0.055063	4.815592
267.010561	8000.254263	12.393971	-0.055038	4.815586
267.098135	8000.254634	12.398976	-0.055055	4.815585
267.075163	8000.296989	12.403981	-0.055050	4.815598
266.952784	8000.259737	12.408986	-0.055028	4.815587
267.294259	8000.286702	12.413991	-0.055091	4.815594
267.170810	8000.270796	12.418995	-0.055068	4.815590
266.951503	8000.254387	12.424000	-0.055028	4.815586
267.127245	8000.259407	12.429005	-0.055060	4.815587
267.124205	8000.235861	12.434010	-0.055060	4.815580
267.158012	8000.283420	12.439015	-0.055066	4.815593
267.113917	8000.275224	12.444019	-0.055058	4.815591
266.880233	8000.272466	12.449024	-0.055015	4.815592
267.188257	8000.305292	12.454029	-0.055072	4.815600
267.095829	8000.229006	12.459034	-0.055055	4.815578
267.007672	8000.257475	12.464039	-0.055038	4.815587
266.908440	8000.268671	12.469043	-0.055020	4.815590
266.849645	8000.253825	12.474048	-0.055009	4.815586
267.059742	8000.218817	12.479053	-0.055048	4.815575
266.961592	8000.205462	12.484058	-0.055030	4.815572
267.143412	8000.262924	12.489063	-0.055064	4.815587
267.112936	8000.256020	12.494067	-0.055058	4.815586
267.161795	8000.262165	12.499072	-0.055067	4.815587
267.144814	8000.276846	12.504077	-0.055064	4.815592
267.090559	8000.230028	12.509082	-0.055054	4.815578
267.228596	8000.258999	12.514087	-0.055080	4.815586
267.115922	8000.256088	12.519091	-0.055059	4.815586
266.962055	8000.270662	12.524096	-0.055030	4.815591
266.918395	8000.295587	12.529101	-0.055022	4.815598
267.047464	8000.229341	12.534106	-0.055046	4.815578
267.001270	8000.237134	12.539111	-0.055038	4.815581
266.966887	8000.246188	12.544115	-0.055032	4.815583
267.049799	8000.261437	12.549120	-0.055047	4.815587
267.079579	8000.291839	12.554125	-0.055053	4.815596
267.081052	8000.273708	12.559130	-0.055053	4.815591
267.347326	8000.281281	12.564135	-0.055103	4.815592
267.327542	8000.266006	12.569139	-0.055099	4.815587
266.986473	8000.240124	12.574144	-0.055035	4.815582
267.099589	8000.263345	12.579149	-0.055057	4.815588
267.026918	8000.223703	12.584154	-0.055043	4.815577
267.122696	8000.297915	12.589159	-0.055061	4.815598
267.070701	8000.271429	12.594163	-0.055051	4.815590
267.259376	8000.226457	12.599168	-0.055086	4.815576
267.320686	8000.260580	12.604173	-0.055098	4.815586
267.122251	8000.246649	12.609178	-0.055061	4.815583
267.218568	8000.271732	12.614183	-0.055079	4.815590
267.336459	8000.255509	12.619187	-0.055101	4.815584
267.167597	8000.235654	12.624192	-0.055070	4.815579
267.127106	8000.283064	12.629197	-0.055062	4.815593
267.216151	8000.259958	12.634202	-0.055079	4.815586
267.198632	8000.271425	12.639207	-0.055076	4.815590
267.262864	8000.234027	12.644211	-0.055088	4.815578
267.229563	8000.255917	12.649216	-0.055081	4.815585
267.256608	8000.274524	12.654221	-0.055086	4.815590
267.043772	8000.243266	12.659226	-0.055047	4.815582
267.307153	8000.253996	12.664231	-0.055096	4.815584
267.369085	8000.275311	12.669235	-0.055108	4.815590
267.146706	8000.231078	12.674240	-0.055066	4.815578
267.173271	8000.199472	12.679245	-0.055071	4.815569
267.188946	8000.180505	12.684250	-0.055074	4.815563
267.401222	8000.219239	12.689255	-0.055114	4.815573
267.391939	8000.235114	12.694259	-0.055112	4.815578
267.484131	8000.240902	12.699264	-0.055129	4.815579
267.424278	8000.296540	12.704269	-0.055118	4.815596
267.328119	8000.238352	12.709274	-0.055100	4.815579
267.252416	8000.286253	12.714279	-0.055086	4.815594
267.384809	8000.258517	12.719283	-0.055111	4.815585
267.223555	8000.235582	12.724288	-0.055081	4.815579
267.432668	8000.272128	12.729293	-0.055120	4.815589
267.453695	8000.258590	12.734298	-0.055124	4.815585
267.704715	8000.290483	12.739303	-0.055171	4.815593
267.569066	8000.264762	12.744307	-0.055145	4.815586
267.619564	8000.229275	12.749312	-0.055155	4.815575
267.593759	8000.302562	12.754317	-0.055150	4.815597
267.332216	8000.265164	12.759322	-0.055101	4.815587
267.432061	8000.299920	12.764327	-0.055120	4.815597
267.534250	8000.309076	12.769331	-0.055139	4.815599
267.430763	8000.271064	12.774336	-0.055120	4.815588
267.325260	8000.300317	12.779341	-0.055100	4.815597
267.412860	8000.270779	12.784346	-0.055117	4.815588
267.368171	8000.297824	12.789351	-0.055108	4.815596
267.293231	8000.277371	12.794355	-0.055095	4.815591
267.298967	8000.268924	12.799360	-0.055096	4.815588
267.328414	8000.289706	12.804365	-0.055101	4.815594
267.529417	8000.240663	12.809370	-0.055139	4.815579
267.369817	8000.373714	12.814375	-0.055109	4.815619
267.466538	8000.380645	12.819379	-0.055127	4.815620
267.435613	8000.322458	12.824384	-0.055121	4.815603
267.531656	8000.298399	12.829389	-0.055139	4.815596
267.426747	8000.262500	12.834394	-0.055120	4.815586
267.384827	8000.261817	12.839399	-0.055112	4.815586
267.357487	8000.279532	12.844403	-0.055107	4.815591
267.320821	8000.282140	12.849408	-0.055100	4.815592
267.444296	8000.272418	12.854413	-0.055123	4.815589
267.290415	8000.246399	12.859418	-0.055095	4.815582
267.402476	8000.271740	12.864423	-0.055116	4.815589
267.577502	8000.256454	12.869427	-0.055148	4.815583
267.385463	8000.226604	12.874432	-0.055112	4.815576
267.238363	8000.306449	12.879437	-0.055085	4.815600
267.353971	8000.261347	12.884442	-0.055107	4.815586
267.499740	8000.281900	12.889447	-0.055134	4.815591
267.305564	8000.263766	12.894451	-0.055098	4.815587
267.181752	8000.239308	12.899456	-0.055075	4.815580
267.389207	8000.248053	12.904461	-0.055113	4.815582
267.470722	8000.235507	12.909466	-0.055129	4.815578
267.515050	8000.249056	12.914471	-0.055137	4.815582
267.377679	8000.243604	12.919475	-0.055111	4.815581
267.366469	8000.226332	12.924480	-0.055109	4.815576
267.377725	8000.264976	12.929485	-0.055111	4.815587
267.264399	8000.216122	12.934490	-0.055090	4.815573
267.323184	8000.245931	12.939495	-0.055101	4.815582
267.355677	8000.234717	12.944499	-0.055107	4.815578
267.360133	8000.225180	12.949504	-0.055108	4.815575
267.430642	8000.273341	12.954509	-0.055122	4.815589
267.202997	8000.229022	12.959514	-0.055079	4.815577
267.244065	8000.230767	12.964519	-0.055087	4.815577
267.318773	8000.239473	12.969523	-0.055101	4.815580
267.276894	8000.234518	12.974528	-0.055093	4.815578
267.378135	8000.259682	12.979533	-0.055112	4.815585
267.208034	8000.212033	12.984538	-0.055080	4.815572
267.447412	8000.239461	12.989543	-0.055125	4.815579
267.198989	8000.240734	12.994547	-0.055079	4.815581
267.219537	8000.266712	12.999552	-0.055083	4.815588
267.470183	8000.278302	13.004557	-0.055129	4.815590
267.307724	8000.262824	13.009562	-0.055099	4.815587
267.284998	8000.287024	13.014567	-0.055095	4.815594
267.424536	8000.283975	13.019571	-0.055121	4.815592
267.283839	8000.293422	13.024576	-0.055095	4.815596
267.287913	8000.318062	13.029581	-0.055096	4.815603
267.106251	8000.257405	13.034586	-0.055062	4.815586
267.449604	8000.256628	13.039591	-0.055126	4.815584
267.453109	8000.279122	13.044595	-0.055127	4.815591
267.302782	8000.240342	13.049600	-0.055099	4.815580
267.595560	8000.302829	13.054605	-0.055153	4.815597
267.490341	8000.258380	13.059610	-0.055134	4.815584
267.330909	8000.253634	13.064615	-0.055104	4.815584
267.455451	8000.246065	13.069619	-0.055127	4.815581
267.551180	8000.251911	13.074624	-0.055145	4.815582
267.530423	8000.275076	13.079629	-0.055141	4.815589
267.495639	8000.211485	13.084634	-0.055135	4.815571
267.493142	8000.242426	13.089639	-0.055134	4.815580
267.596872	8000.282586	13.094643	-0.055154	4.815591
267.464225	8000.245164	13.099648	-0.055129	4.815581
267.210099	8000.274117	13.104653	-0.055082	4.815590
267.208945	8000.243124	13.109658	-0.055082	4.815581
267.475937	8000.262460	13.114663	-0.055131	4.815586
267.422367	8000.244494	13.119667	-0.055121	4.815581
267.443454	8000.251253	13.124672	-0.055125	4.815582
267.298142	8000.239261	13.129677	-0.055098	4.815580
267.279855	8000.215465	13.134682	-0.055095	4.815573
267.424954	8000.255234	13.139687	-0.055122	4.815584
267.397816	8000.267612	13.144691	-0.055117	4.815587
267.143181	8000.239942	13.149696	-0.055070	4.815581
267.490932	8000.240305	13.154701	-0.055135	4.815579
267.346907	8000.242221	13.159706	-0.055108	4.815580
267.168595	8000.257461	13.164711	-0.055075	4.815586
267.454031	8000.277099	13.169715	-0.055128	4.815590
267.351015	8000.239095	13.174720	-0.055109	4.815579
267.371197	8000.257590	13.179725	-0.055113	4.815585
267.236921	8000.213732	13.184730	-0.055088	4.815572
267.456936	8000.234434	13.189735	-0.055129	4.815577
267.483337	8000.242348	13.194739	-0.055134	4.815580
267.482485	8000.214565	13.199744	-0.055133	4.815572
267.431426	8000.279961	13.204749	-0.055124	4.815591
267.331877	8000.254832	13.209754	-0.055105	4.815584
267.333357	8000.249519	13.214759	-0.055106	4.815582
267.353621	8000.259469	13.219763	-0.055110	4.815585
267.351209	8000.250888	13.224768	-0.055109	4.815583
267.464310	8000.270906	13.229773	-0.055130	4.815588
267.320443	8000.242914	13.234778	-0.055104	4.815581
267.390529	8000.247272	13.239783	-0.055117	4.815582
267.607460	8000.235877	13.244787	-0.055157	4.815577
267.510781	8000.243910	13.249792	-0.055139	4.815580
267.419476	8000.258440	13.254797	-0.055122	4.815585
267.340064	8000.258211	13.259802	-0.055107	4.815585
267.654570	8000.213164	13.264807	-0.055166	4.815570
267.330458	8000.230288	13.269811	-0.055106	4.815577
267.335250	8000.221824	13.274816	-0.055107	4.815574
267.411029	8000.261526	13.279821	-0.055121	4.815586
267.363203	8000.241518	13.284826	-0.055112	4.815580
267.480522	8000.254128	13.289831	-0.055134	4.815583
267.625767	8000.259717	13.294835	-0.055161	4.815584
267.545393	8000.234903	13.299840	-0.055146	4.815577
267.482302	8000.242418	13.304845	-0.055134	4.815580
267.464460	8000.211152	13.309850	-0.055131	4.815571
267.554033	8000.239329	13.314855	-0.055148	4.815578
267.363682	8000.281078	13.319859	-0.055112	4.815592
267.281007	8000.270113	13.324864	-0.055097	4.815589
267.383180	8000.253632	13.329869	-0.055116	4.815583
267.489542	8000.245765	13.334874	-0.055136	4.815581
267.407596	8000.280745	13.339879	-0.055121	4.815591
267.437063	8000.296187	13.344883	-0.055126	4.815596
267.456690	8000.255921	13.349888	-0.055130	4.815584
267.415735	8000.278754	13.354893	-0.055122	4.815591
267.358067	8000.278881	13.359898	-0.055112	4.815591
267.361909	8000.272538	13.364903	-0.055112	4.815589
267.598678	8000.266810	13.369907	-0.055157	4.815586
267.493368	8000.247996	13.374912	-0.055137	4.815581
267.512382	8000.270744	13.379917	-0.055141	4.815588
267.482153	8000.223251	13.384922	-0.055135	4.815574
267.627199	8000.225633	13.389927	-0.055162	4.815574
267.741731	8000.271311	13.394931	-0.055183	4.815587
267.509808	8000.221580	13.399936	-0.055140	4.815573
267.607817	8000.234941	13.404941	-0.055159	4.815577
267.519112	8000.217467	13.409946	-0.055142	4.815572
267.631110	8000.246013	13.414951	-0.055163	4.815580
267.421522	8000.244717	13.419955	-0.055124	4.815581
267.368816	8000.226766	13.424960	-0.055114	4.815576
267.567402	8000.269549	13.429965	-0.055151	4.815587
267.331677	8000.228302	13.434970	-0.055107	4.815576
267.557103	8000.237342	13.439975	-0.055149	4.815578
267.591169	8000.248586	13.444979	-0.055156	4.815581
267.278807	8000.269107	13.449984	-0.055098	4.815588
267.378365	8000.258993	13.454989	-0.055116	4.815585
267.513288	8000.212070	13.459994	-0.055141	4.815571
267.601806	8000.234890	13.464999	-0.055158	4.815577
267.781294	8000.299793	13.470003	-0.055191	4.815595
267.785072	8000.251789	13.475008	-0.055192	4.815581
267.665381	8000.285082	13.480013	-0.055170	4.815591
267.484849	8000.230852	13.485018	-0.055136	4.815576
267.473575	8000.246694	13.490023	-0.055134	4.815581
267.693855	8000.236422	13.495027	-0.055175	4.815577
267.595986	8000.210253	13.500032	-0.055157	4.815570
267.545047	8000.256423	13.505037	-0.055148	4.815583
267.589614	8000.246476	13.510042	-0.055156	4.815580
267.426750	8000.256629	13.515047	-0.055126	4.815584
267.336410	8000.242333	13.520051	-0.055109	4.815580
267.402619	8000.209240	13.525056	-0.055121	4.815570
267.484988	8000.267209	13.530061	-0.055137	4.815587
267.553656	8000.250179	13.535066	-0.055150	4.815582
267.595813	8000.232714	13.540071	-0.055158	4.815576
267.752330	8000.243830	13.545075	-0.055187	4.815579
267.651833	8000.219754	13.550080	-0.055168	4.815572
267.567205	8000.242939	13.555085	-0.055152	4.815579
267.491550	8000.224612	13.560090	-0.055138	4.815574
267.538452	8000.243544	13.565095	-0.055147	4.815580
267.391434	8000.232592	13.570099	-0.055120	4.815577
267.496871	8000.249280	13.575104	-0.055139	4.815582
267.576949	8000.258074	13.580109	-0.055154	4.815584
267.521369	8000.163164	13.585114	-0.055144	4.815556
267.430442	8000.226838	13.590119	-0.055127	4.815575
267.649622	8000.246459	13.595123	-0.055168	4.815580
267.609225	8000.214822	13.600128	-0.055161	4.815571
267.626277	8000.273857	13.605133	-0.055164	4.815588
267.710368	8000.251739	13.610138	-0.055180	4.815581
267.889668	8000.265365	13.615143	-0.055213	4.815584
267.896717	8000.255871	13.620147	-0.055214	4.815582
267.705460	8000.234579	13.625152	-0.055179	4.815576
267.766295	8000.254808	13.630157	-0.055190	4.815582
267.738877	8000.242612	13.635162	-0.055185	4.815578
267.820516	8000.254637	13.640167	-0.055200	4.815582
267.672779	8000.261833	13.645171	-0.055173	4.815584
267.698903	8000.229150	13.650176	-0.055178	4.815575
267.764633	8000.243050	13.655181	-0.055190	4.815578
267.561984	8000.242937	13.660186	-0.055152	4.815579
267.643829	8000.248555	13.665191	-0.055168	4.815581
267.694750	8000.234439	13.670195	-0.055177	4.815576
267.496989	8000.230133	13.675200	-0.055140	4.815576
267.683759	8000.250290	13.680205	-0.055175	4.815581
267.694708	8000.249405	13.685210	-0.055177	4.815581
267.563400	8000.263280	13.690215	-0.055153	4.815585
267.740714	8000.245895	13.695219	-0.055186	4.815579
267.642350	8000.211171	13.700224	-0.055168	4.815570
267.695487	8000.275071	13.705229	-0.055178	4.815588
267.594759	8000.279833	13.710234	-0.055159	4.815590
267.581075	8000.258248	13.715239	-0.055156	4.815584
267.664260	8000.270298	13.720243	-0.055172	4.815587
267.509884	8000.235725	13.725248	-0.055143	4.815577
267.783935	8000.289360	13.730253	-0.055194	4.815592
267.572791	8000.268810	13.735258	-0.055155	4.815587
267.702519	8000.268805	13.740263	-0.055179	4.815586
267.811717	8000.258849	13.745267	-0.055200	4.815583
267.732676	8000.212691	13.750272	-0.055185	4.815570
267.601747	8000.253278	13.755277	-0.055161	4.815582
267.581259	8000.221968	13.760282	-0.055157	4.815573
267.655529	8000.228530	13.765287	-0.055171	4.815575
267.753537	8000.249369	13.770291	-0.055189	4.815580
267.740460	8000.226726	13.775296	-0.055187	4.815574
267.801912	8000.265125	13.780301	-0.055198	4.815585
267.658543	8000.222186	13.785306	-0.055171	4.815573
267.652512	8000.259479	13.790311	-0.055170	4.815584
267.879850	8000.261073	13.795315	-0.055213	4.815583
267.860542	8000.237260	13.800320	-0.055209	4.815576
267.863542	8000.261882	13.805325	-0.055210	4.815583
267.669029	8000.272584	13.810330	-0.055174	4.815587
267.948143	8000.264345	13.815335	-0.055226	4.815584
268.020138	8000.262325	13.820339	-0.055239	4.815583
267.854164	8000.232902	13.825344	-0.055208	4.815575
267.879151	8000.285659	13.830349	-0.055213	4.815590
267.895964	8000.278461	13.835354	-0.055216	4.815588
267.810306	8000.258901	13.840359	-0.055200	4.815583
267.904733	8000.262589	13.845363	-0.055218	4.815583
267.754410	8000.230218	13.850368	-0.055190	4.815575
267.767627	8000.277441	13.855373	-0.055192	4.815588
267.629710	8000.278388	13.860378	-0.055167	4.815589
267.588227	8000.264893	13.865383	-0.055159	4.815586
267.711856	8000.278675	13.870387	-0.055182	4.815589
267.623567	8000.254799	13.875392	-0.055166	4.815582
267.861710	8000.283276	13.880397	-0.055210	4.815590
267.802223	8000.249190	13.885402	-0.055199	4.815580
267.769333	8000.250791	13.890407	-0.055193	4.815581
267.868258	8000.294077	13.895411	-0.055212	4.815593
267.951327	8000.249510	13.900416	-0.055227	4.815579
268.031798	8000.265788	13.905421	-0.055242	4.815584
267.776538	8000.266948	13.910426	-0.055195	4.815585
267.850333	8000.252139	13.915431	-0.055208	4.815581
267.839991	8000.263723	13.920435	-0.055206	4.815584
267.752773	8000.255888	13.925440	-0.055190	4.815582
268.010971	8000.250511	13.930445	-0.055238	4.815579
268.070043	8000.265371	13.935450	-0.055249	4.815583
268.028729	8000.248674	13.940455	-0.055242	4.815579
267.864069	8000.255592	13.945459	-0.055211	4.815582
267.932262	8000.232145	13.950464	-0.055224	4.815574
268.045026	8000.266045	13.955469	-0.055245	4.815584
268.135583	8000.237623	13.960474	-0.055262	4.815575
268.008130	8000.250492	13.965479	-0.055238	4.815579
268.101730	8000.243485	13.970483	-0.055256	4.815577
267.942122	8000.244077	13.975488	-0.055226	4.815578
267.927241	8000.280157	13.980493	-0.055223	4.815588
267.843638	8000.302291	13.985498	-0.055208	4.815595
267.928552	8000.269504	13.990503	-0.055224	4.815585
267.842782	8000.296944	13.995507	-0.055208	4.815594
267.765477	8000.271111	14.000512	-0.055193	4.815587
267.927881	8000.269505	14.005517	-0.055224	4.815585
267.792303	8000.260876	14.010522	-0.055198	4.815583
267.935669	8000.264299	14.015527	-0.055225	4.815584
268.065772	8000.284596	14.020531	-0.055249	4.815589
267.774675	8000.270213	14.025536	-0.055195	4.815586
267.653783	8000.272508	14.030541	-0.055173	4.815587
267.723363	8000.241606	14.035546	-0.055186	4.815578
267.525052	8000.267201	14.040551	-0.055149	4.815587
267.515358	8000.265978	14.045555	-0.055147	4.815586
267.694946	8000.234743	14.050560	-0.055181	4.815576
268.023580	8000.292478	14.055565	-0.055242	4.815592
267.860253	8000.263098	14.060570	-0.055211	4.815584
267.664531	8000.259893	14.065575	-0.055175	4.815584
267.994594	8000.275991	14.070579	-0.055237	4.815587
267.944830	8000.263428	14.075584	-0.055227	4.815583
267.776155	8000.294850	14.080589	-0.055196	4.815593
267.801904	8000.271775	14.085594	-0.055201	4.815587
267.767308	8000.259462	14.090599	-0.055194	4.815583
267.982562	8000.255517	14.095603	-0.055235	4.815581
267.783165	8000.239433	14.100608	-0.055197	4.815577
267.884687	8000.244306	14.105613	-0.055216	4.815578
267.764233	8000.256222	14.110618	-0.055194	4.815582
267.775331	8000.242521	14.115623	-0.055196	4.815578
268.046890	8000.282229	14.120627	-0.055247	4.815588
267.776211	8000.250021	14.125632	-0.055196	4.815580
267.924757	8000.293053	14.130637	-0.055224	4.815592
267.876235	8000.269829	14.135642	-0.055215	4.815586
267.817429	8000.235754	14.140647	-0.055204	4.815576
267.764933	8000.262671	14.145651	-0.055194	4.815584
267.760665	8000.252991	14.150656	-0.055194	4.815581
268.033466	8000.304470	14.155661	-0.055245	4.815595
267.820207	8000.296704	14.160666	-0.055205	4.815594
267.684906	8000.268852	14.165671	-0.055180	4.815586
267.891657	8000.283996	14.170675	-0.055218	4.815590
267.825572	8000.241256	14.175680	-0.055206	4.815577
267.704317	8000.249954	14.180685	-0.055184	4.815581
267.765066	8000.257363	14.185690	-0.055195	4.815582
267.814774	8000.252841	14.190695	-0.055204	4.815581
267.788718	8000.278055	14.195699	-0.055199	4.815588
267.849770	8000.236331	14.200704	-0.055211	4.815576
268.046630	8000.248109	14.205709	-0.055247	4.815578
267.796771	8000.240811	14.210714	-0.055201	4.815577
267.722367	8000.254551	14.215719	-0.055187	4.815582
268.026918	8000.299072	14.220723	-0.055244	4.815593
267.995012	8000.251551	14.225728	-0.055238	4.815580
268.046495	8000.286583	14.230733	-0.055248	4.815590
268.018538	8000.286128	14.235738	-0.055243	4.815590
267.857310	8000.255715	14.240743	-0.055213	4.815582
267.944461	8000.279580	14.245747	-0.055229	4.815588
267.799823	8000.239825	14.250752	-0.055202	4.815577
267.754127	8000.285013	14.255757	-0.055193	4.815591
267.861802	8000.261145	14.260762	-0.055214	4.815583
267.767948	8000.255337	14.265767	-0.055196	4.815582
267.963251	8000.277772	14.270771	-0.055233	4.815587
267.824002	8000.270151	14.275776	-0.055207	4.815586
267.949169	8000.301050	14.280781	-0.055230	4.815594
268.027152	8000.294855	14.285786	-0.055245	4.815592
267.903943	7999.312234	14.290791	-0.055221	4.815306

268.044190	7996.097526	14.295795	-0.055245	4.814365
267.815825	7990.622527	14.300800	-0.055199	4.812765
267.970705	7983.945344	14.305805	-0.055224	4.810812
267.753003	7976.644106	14.310810	-0.055178	4.808676
267.612599	7968.979566	14.315815	-0.055147	4.806433
267.653712	7961.228753	14.320819	-0.055150	4.804163
267.664721	7953.366099	14.325824	-0.055147	4.801859
267.792284	7945.376963	14.330829	-0.055165	4.799516
267.686105	7937.470149	14.335834	-0.055141	4.797197
267.813467	7929.411094	14.340839	-0.055159	4.794832
267.936906	7921.439903	14.345843	-0.055177	4.792491
267.509223	7913.382872	14.350848	-0.055092	4.790126
267.572078	7905.385763	14.355853	-0.055099	4.787775
267.734680	7897.355738	14.360858	-0.055124	4.785414
267.388834	7889.427690	14.365863	-0.055054	4.783083
267.430515	7881.469648	14.370867	-0.055057	4.780740
267.618590	7873.407217	14.375872	-0.055087	4.778365
267.555914	7865.414299	14.380877	-0.055070	4.776011
267.538424	7857.393115	14.385882	-0.055061	4.773646
267.383913	7849.380524	14.390887	-0.055027	4.771284
267.490768	7841.386885	14.395891	-0.055042	4.768925
267.255365	7833.371794	14.400896	-0.054993	4.766560
267.308443	7825.353721	14.405901	-0.054998	4.764191
267.392721	7817.410765	14.410906	-0.055008	4.761844
267.137533	7809.367411	14.415911	-0.054956	4.759467
267.176148	7801.431828	14.420915	-0.054958	4.757120
267.427304	7793.370742	14.425920	-0.054999	4.754733
267.219603	7785.345374	14.430925	-0.054955	4.752358
267.111952	7777.305188	14.435930	-0.054930	4.749976
267.196932	7769.349095	14.440935	-0.054941	4.747618
267.107781	7761.307721	14.445939	-0.054919	4.745233
266.900975	7753.333378	14.450944	-0.054875	4.742868
267.232050	7745.290790	14.455949	-0.054932	4.740480
267.122721	7737.355970	14.460954	-0.054906	4.738124
267.007959	7729.318997	14.465959	-0.054880	4.735736
266.839777	7721.327612	14.470963	-0.054843	4.733361
266.829410	7713.299828	14.475968	-0.054836	4.730973
266.807834	7705.270760	14.480973	-0.054827	4.728584
266.965096	7697.374236	14.485978	-0.054851	4.726232
266.839479	7689.287333	14.490983	-0.054823	4.723824
266.823341	7681.336470	14.495987	-0.054814	4.721454
266.733204	7673.300012	14.500992	-0.054792	4.719058
266.722022	7665.347845	14.505997	-0.054785	4.716686
266.890575	7657.301808	14.511002	-0.054811	4.714283
266.670757	7649.310049	14.516007	-0.054765	4.711897
266.605092	7641.302727	14.521011	-0.054748	4.709505
266.646479	7633.256461	14.526016	-0.054750	4.707099
266.611491	7625.279484	14.531021	-0.054739	4.704714
266.419276	7617.343004	14.536026	-0.054698	4.702339
266.516459	7609.283354	14.541031	-0.054711	4.699926
266.647680	7601.371832	14.546035	-0.054730	4.697555
266.638189	7593.295673	14.551040	-0.054723	4.695135
266.439905	7585.274535	14.556045	-0.054681	4.692730
266.567082	7577.290808	14.561050	-0.054700	4.690335
266.267736	7569.296098	14.566055	-0.054639	4.687935
266.178025	7561.272518	14.571059	-0.054617	4.685526
266.142691	7553.289767	14.576064	-0.054605	4.683127
266.127796	7545.290474	14.581069	-0.054597	4.680722
266.222882	7537.306254	14.586074	-0.054610	4.678320
266.267098	7529.312369	14.591079	-0.054613	4.675915
266.235139	7521.255882	14.596083	-0.054602	4.673489
266.116078	7513.152433	14.601088	-0.054574	4.671048
266.104224	7505.167651	14.606093	-0.054567	4.668641
266.052259	7497.228230	14.611098	-0.054552	4.666247
265.983767	7489.227676	14.616103	-0.054534	4.663833
265.983364	7481.264644	14.621107	-0.054529	4.661429
266.080950	7473.217217	14.626112	-0.054542	4.658998
265.985943	7465.254890	14.631117	-0.054519	4.656592
266.121224	7457.268568	14.636122	-0.054539	4.654177
266.028875	7449.197953	14.641127	-0.054517	4.651736
266.068573	7441.222743	14.646131	-0.054519	4.649322
266.015776	7433.221531	14.651136	-0.054504	4.646899
266.035704	7425.183497	14.656141	-0.054502	4.644463
265.987296	7417.260719	14.661146	-0.054488	4.642062
265.832057	7409.186458	14.666151	-0.054454	4.639613
265.738216	7401.280177	14.671155	-0.054431	4.637213
265.698941	7393.210568	14.676160	-0.054419	4.634763
265.877352	7385.207223	14.681165	-0.054447	4.632332
265.701706	7377.155182	14.686170	-0.054409	4.629884
265.464722	7369.157697	14.691175	-0.054360	4.627452
265.571657	7361.163810	14.696179	-0.054375	4.625020
265.681125	7353.217158	14.701184	-0.054390	4.622601
265.610833	7345.132100	14.706189	-0.054371	4.620138
265.637658	7337.219384	14.711194	-0.054371	4.617727
265.563564	7329.172595	14.716199	-0.054352	4.615273
265.460755	7321.216061	14.721203	-0.054328	4.612846
265.211101	7313.141095	14.726208	-0.054276	4.610381
265.543187	7305.138775	14.731213	-0.054333	4.607937
265.681505	7297.213225	14.736218	-0.054354	4.605515
265.471416	7289.173656	14.741223	-0.054309	4.603057
265.529362	7281.149425	14.746227	-0.054315	4.600603
265.522661	7273.174411	14.751232	-0.054309	4.598162
265.253064	7265.190759	14.756237	-0.054253	4.595717
265.226193	7257.155054	14.761242	-0.054243	4.593255
265.212077	7249.038127	14.766247	-0.054235	4.590767
265.286326	7241.101487	14.771251	-0.054244	4.588333
264.988265	7233.113908	14.776256	-0.054183	4.585881
265.166628	7225.086903	14.781261	-0.054211	4.583417
265.283051	7217.151687	14.786266	-0.054228	4.580979
265.139248	7209.163494	14.791271	-0.054196	4.578524
265.127530	7201.192455	14.796275	-0.054188	4.576072
265.123248	7193.147572	14.801280	-0.054182	4.573597
265.015760	7185.098275	14.806285	-0.054157	4.571119
265.170363	7177.108197	14.811290	-0.054181	4.568658
265.265643	7169.113480	14.816295	-0.054193	4.566194
265.205464	7161.110498	14.821299	-0.054177	4.563726
264.923949	7153.141112	14.826304	-0.054120	4.561267
265.100248	7145.112498	14.831309	-0.054147	4.558788
265.092827	7137.238570	14.836314	-0.054141	4.556356
264.692237	7129.150529	14.841319	-0.054061	4.553856
264.947794	7121.082060	14.846323	-0.054103	4.551362
264.811926	7113.072370	14.851328	-0.054073	4.548883
264.733280	7105.106129	14.856333	-0.054053	4.546417
264.930591	7097.129640	14.861338	-0.054085	4.543947
264.620749	7089.147194	14.866343	-0.054022	4.541473
264.700220	7081.125679	14.871347	-0.054031	4.538986
264.676715	7073.146384	14.876352	-0.054022	4.536511
264.705255	7065.117845	14.881357	-0.054022	4.534019
264.737867	7057.130875	14.886362	-0.054023	4.531538
264.565580	7049.077311	14.891367	-0.053986	4.529035
264.626648	7041.119041	14.896371	-0.053992	4.526561
264.588196	7033.046408	14.901376	-0.053979	4.524050
264.502602	7025.149091	14.906381	-0.053958	4.521592
264.505011	7017.101118	14.911386	-0.053954	4.519085
264.538979	7009.153536	14.916391	-0.053955	4.516609
264.480167	7001.096905	14.921395	-0.053939	4.514097
264.359939	6993.057286	14.926400	-0.053911	4.511589
264.196742	6984.996546	14.931405	-0.053875	4.509072
264.379813	6977.061408	14.936410	-0.053904	4.506595
264.170859	6969.012065	14.941415	-0.053860	4.504079
264.288659	6961.050302	14.946419	-0.053877	4.501590
264.169917	6953.035156	14.951424	-0.053850	4.499083
264.155718	6945.069449	14.956429	-0.053842	4.496589
264.156811	6937.068166	14.961434	-0.053837	4.494084
264.173180	6929.021402	14.966439	-0.053835	4.491562
264.200985	6921.060681	14.971443	-0.053835	4.489067
264.190488	6913.099789	14.976448	-0.053828	4.486569
263.988418	6905.015010	14.981453	-0.053785	4.484031
264.176820	6897.083927	14.986458	-0.053815	4.481541
264.195378	6889.032819	14.991463	-0.053813	4.479011
264.019056	6881.091589	14.996467	-0.053775	4.476514
263.829253	6873.034961	15.001472	-0.053735	4.473979
263.747720	6865.002607	15.006477	-0.053714	4.471450
263.788637	6857.045803	15.011482	-0.053717	4.468945
263.539399	6849.031408	15.016487	-0.053665	4.466418
263.545866	6841.021642	15.021491	-0.053661	4.463893
263.567756	6833.066689	15.026496	-0.053660	4.461383
263.564320	6825.057188	15.031501	-0.053654	4.458855
263.743563	6817.070757	15.036506	-0.053683	4.456334
263.570086	6809.005266	15.041511	-0.053645	4.453784
263.669719	6800.994325	15.046515	-0.053658	4.451252
263.723836	6792.993429	15.051520	-0.053663	4.448721
263.924504	6784.978403	15.056525	-0.053696	4.446184
263.568740	6777.032384	15.061530	-0.053624	4.443666
263.526197	6769.020834	15.066535	-0.053611	4.441127
263.597038	6761.054673	15.071539	-0.053619	4.438601
263.470860	6753.016062	15.076544	-0.053590	4.436050
263.317836	6744.990374	15.081549	-0.053557	4.433502
263.185241	6736.943532	15.086554	-0.053527	4.430945
263.286618	6728.965792	15.091559	-0.053541	4.428410
263.220793	6720.974412	15.096563	-0.053523	4.425868
263.260292	6712.995912	15.101568	-0.053525	4.423330
263.250920	6704.953112	15.106573	-0.053518	4.420769
263.161840	6696.996531	15.111578	-0.053497	4.418234
263.268911	6688.956362	15.116583	-0.053511	4.415672
263.092863	6680.996662	15.121587	-0.053474	4.413133
263.055068	6672.930882	15.126592	-0.053461	4.410558
263.116153	6664.937662	15.131597	-0.053468	4.408007
263.009083	6656.971302	15.136602	-0.053442	4.405461
262.874835	6648.970010	15.141607	-0.053412	4.402902
263.025328	6640.971659	15.146611	-0.053435	4.400345
263.232772	6633.004263	15.151616	-0.053469	4.397796
262.893776	6624.998007	15.156621	-0.053400	4.395230
262.738928	6617.021671	15.161626	-0.053366	4.392674
262.680776	6608.918904	15.166631	-0.053350	4.390076
262.816495	6600.994649	15.171635	-0.053370	4.387534
262.897737	6592.931021	15.176640	-0.053380	4.384946
262.986857	6584.989574	15.181645	-0.053392	4.382396
263.079551	6576.977873	15.186650	-0.053404	4.379822
262.952953	6568.999119	15.191655	-0.053375	4.377256
262.906986	6560.970263	15.196659	-0.053361	4.374673
262.797440	6553.007469	15.201664	-0.053336	4.372108
262.792820	6544.902084	15.206669	-0.053330	4.369498
262.906534	6536.999751	15.211674	-0.053346	4.366951
262.760129	6528.931819	15.216679	-0.053313	4.364348
262.872127	6521.040749	15.221683	-0.053329	4.361803
262.678469	6513.007511	15.226688	-0.053288	4.359208
262.451719	6505.020371	15.231693	-0.053240	4.356626
262.646947	6497.002598	15.236698	-0.053272	4.354035
262.592157	6488.867206	15.241703	-0.053256	4.351403
262.517807	6480.878917	15.246707	-0.053237	4.348817
262.527715	6472.896577	15.251712	-0.053234	4.346232
262.304268	6464.916128	15.256717	-0.053187	4.343645
262.630987	6456.965583	15.261722	-0.053243	4.341069
262.275534	6448.915730	15.266727	-0.053171	4.338455
262.537917	6440.977875	15.271731	-0.053215	4.335880
262.427917	6432.957531	15.276736	-0.053189	4.333274
262.246249	6424.874482	15.281741	-0.053150	4.330646
262.211912	6416.936184	15.286746	-0.053139	4.328064
262.241701	6408.947517	15.291751	-0.053139	4.325465
262.381531	6400.956400	15.296755	-0.053160	4.322864
262.291890	6392.957965	15.301760	-0.053138	4.320257
262.398841	6384.981959	15.306765	-0.053153	4.317658
262.302517	6376.954137	15.311770	-0.053130	4.315038
262.004745	6368.921544	15.316775	-0.053069	4.312414
262.326146	6360.895801	15.321779	-0.053124	4.309796
262.175110	6352.923150	15.326784	-0.053091	4.307189
262.067704	6344.865596	15.331789	-0.053065	4.304553
262.069671	6336.951593	15.336794	-0.053061	4.301964
262.042288	6328.920091	15.341799	-0.053050	4.299334
261.887146	6320.960451	15.346803	-0.053016	4.296726
261.785786	6312.904427	15.351808	-0.052992	4.294084
261.952916	6304.890566	15.356813	-0.053018	4.291457
261.960315	6296.914048	15.361818	-0.053015	4.288839
261.704766	6288.906216	15.366823	-0.052962	4.286207
261.907499	6280.937449	15.371827	-0.052994	4.283590
261.783517	6272.907739	15.376832	-0.052966	4.280949
261.629043	6264.929357	15.381837	-0.052932	4.278323
261.550656	6256.926488	15.386842	-0.052912	4.275688
261.704123	6248.894145	15.391847	-0.052936	4.273043
261.573770	6240.865628	15.396851	-0.052906	4.270396
261.570422	6232.890846	15.401856	-0.052901	4.267765
261.453534	6224.870102	15.406861	-0.052874	4.265117
261.605075	6216.931325	15.411866	-0.052897	4.262497
261.536806	6208.859733	15.416871	-0.052879	4.259829
261.338205	6200.921370	15.421875	-0.052837	4.257203
261.474518	6192.864693	15.426880	-0.052857	4.254538
261.338515	6184.841254	15.431885	-0.052826	4.251881
261.361397	6176.887265	15.436890	-0.052825	4.249246
261.294574	6168.873861	15.441895	-0.052808	4.246589
261.272615	6160.916941	15.446899	-0.052799	4.243950
261.038160	6152.923042	15.451904	-0.052750	4.241295
261.297106	6144.911730	15.456909	-0.052793	4.238637
261.428728	6136.945630	15.461914	-0.052812	4.235991
261.057350	6128.894806	15.466919	-0.052738	4.233310
261.253898	6120.881499	15.471923	-0.052769	4.230646
261.397304	6112.916910	15.476928	-0.052791	4.227996
261.121440	6104.882492	15.481933	-0.052734	4.225316
261.046955	6096.954985	15.486938	-0.052715	4.222673
260.987210	6088.887949	15.491943	-0.052699	4.219981
261.204138	6080.950556	15.496947	-0.052734	4.217334
261.091199	6072.939267	15.501952	-0.052708	4.214657
261.026343	6064.925121	15.506957	-0.052691	4.211978
261.044882	6056.909820	15.511962	-0.052689	4.209298
260.992011	6048.929806	15.516967	-0.052674	4.206627
261.044751	6040.895689	15.521971	-0.052679	4.203938
261.065706	6032.953388	15.526976	-0.052677	4.201277
260.701464	6024.936986	15.531981	-0.052604	4.198585
260.687228	6016.981803	15.536986	-0.052597	4.195916
260.611651	6008.842128	15.541991	-0.052577	4.193183
260.650523	6000.833281	15.546995	-0.052579	4.190493
260.775982	5992.831424	15.552000	-0.052598	4.187805
260.681942	5984.847336	15.557005	-0.052575	4.185118
260.527854	5976.923231	15.562010	-0.052541	4.182450
260.464575	5968.870614	15.567015	-0.052524	4.179737
260.521705	5960.914679	15.572019	-0.052530	4.177056
260.485370	5952.880861	15.577024	-0.052518	4.174347
260.527001	5944.899627	15.582029	-0.052520	4.171654
260.542705	5936.878191	15.587034	-0.052518	4.168946
260.141916	5928.891719	15.592039	-0.052438	4.166243
260.323747	5920.884377	15.597043	-0.052467	4.163537
260.157888	5912.932778	15.602048	-0.052431	4.160845
260.323301	5904.892987	15.607053	-0.052456	4.158125
260.396743	5896.879995	15.612058	-0.052465	4.155412
260.095010	5888.871421	15.617063	-0.052404	4.152694
260.306553	5880.810752	15.622067	-0.052438	4.149962
260.246328	5872.873343	15.627072	-0.052421	4.147267
260.288654	5864.835512	15.632077	-0.052424	4.144537
260.363742	5856.913834	15.637082	-0.052433	4.141846
260.197880	5848.903095	15.642087	-0.052397	4.139119
260.273066	5840.915662	15.647091	-0.052406	4.136402
260.116586	5832.904231	15.652096	-0.052371	4.133672
260.071623	5824.828182	15.657101	-0.052358	4.130919
260.086119	5816.897237	15.662106	-0.052355	4.128215
259.804594	5808.863431	15.667111	-0.052298	4.125470
259.911655	5800.915845	15.672115	-0.052313	4.122758
259.941910	5792.853897	15.677120	-0.052313	4.120003
260.115351	5784.893329	15.682125	-0.052340	4.117284
260.070549	5776.913280	15.687130	-0.052327	4.114553
259.928650	5768.852869	15.692135	-0.052295	4.111792
259.873603	5760.835651	15.697139	-0.052280	4.109044
259.846033	5752.850092	15.702144	-0.052269	4.106306
259.733732	5744.858557	15.707149	-0.052243	4.103563
259.856656	5736.922488	15.712154	-0.052261	4.100840
259.563325	5728.885954	15.717159	-0.052201	4.098076
259.511416	5720.885563	15.722163	-0.052186	4.095325
259.630760	5712.886628	15.727168	-0.052203	4.092575
259.647269	5704.829956	15.732173	-0.052201	4.089802
259.547803	5696.906540	15.737178	-0.052178	4.087072
259.529949	5688.862095	15.742183	-0.052169	4.084299
259.535488	5680.945260	15.747187	-0.052165	4.081568
259.588920	5672.923305	15.752192	-0.052170	4.078800
259.242660	5664.971610	15.757197	-0.052100	4.076049
259.496345	5656.929011	15.762202	-0.052142	4.073273
259.350865	5648.851112	15.767207	-0.052110	4.070477
259.216963	5640.908216	15.772211	-0.052080	4.067727
259.408730	5632.898863	15.777216	-0.052110	4.064956
259.339062	5624.920049	15.782221	-0.052092	4.062189
259.308179	5616.915406	15.787226	-0.052081	4.059413
259.179003	5608.969799	15.792231	-0.052052	4.056654
259.138894	5600.928887	15.797235	-0.052039	4.053861
259.102649	5592.929303	15.802240	-0.052028	4.051080
259.039710	5584.906739	15.807245	-0.052011	4.048290
259.104643	5576.922006	15.812250	-0.052018	4.045512
259.078196	5568.922417	15.817255	-0.052008	4.042726
259.020947	5560.935943	15.822259	-0.051992	4.039942
259.175145	5552.979066	15.827264	-0.052015	4.037170
259.055973	5544.884629	15.832269	-0.051988	4.034343
259.003700	5536.793926	15.837274	-0.051973	4.031517
258.876482	5528.805061	15.842279	-0.051944	4.028724
258.890739	5520.860255	15.847283	-0.051942	4.025946
258.970685	5512.875246	15.852288	-0.051951	4.023153
258.764311	5504.882504	15.857293	-0.051908	4.020351
258.992584	5496.914522	15.862298	-0.051945	4.017562
258.828027	5488.905334	15.867303	-0.051909	4.014751
258.724266	5480.899122	15.872307	-0.051885	4.011940
258.717218	5472.880911	15.877312	-0.051878	4.009124
258.946601	5464.887913	15.882317	-0.051916	4.006319
258.787148	5456.909990	15.887322	-0.051881	4.003511
258.577111	5448.923180	15.892327	-0.051837	4.000698
258.824325	5440.910631	15.897331	-0.051878	3.997880
258.802321	5432.914172	15.902336	-0.051868	3.995062
258.404965	5424.875117	15.907341	-0.051789	3.992220
258.431296	5416.879022	15.912346	-0.051789	3.989399
258.546996	5408.880906	15.917351	-0.051805	3.986576
258.525442	5400.890380	15.922355	-0.051796	3.983752
258.385447	5392.914597	15.927360	-0.051765	3.980929
258.349165	5384.910572	15.932365	-0.051753	3.978096
258.449843	5376.945480	15.937370	-0.051766	3.975277
258.341564	5368.905178	15.942375	-0.051741	3.972426
258.200553	5360.852897	15.947379	-0.051710	3.969567
258.341623	5352.926696	15.952384	-0.051731	3.966757
258.205128	5344.901596	15.957389	-0.051700	3.963904
258.270457	5336.968350	15.962394	-0.051707	3.961086
258.284900	5328.955441	15.967399	-0.051705	3.958236
258.296563	5320.980880	15.972403	-0.051702	3.955398
258.202245	5312.948855	15.977408	-0.051679	3.952535
258.106588	5304.887741	15.982413	-0.051656	3.949660
258.242738	5296.952417	15.987418	-0.051676	3.946832
257.923936	5288.940204	15.992423	-0.051612	3.943966
257.945196	5280.940745	15.997427	-0.051610	3.941109
258.022586	5272.989698	16.002432	-0.051620	3.938268
257.789838	5265.002226	16.007437	-0.051571	3.935406
257.962104	5256.980378	16.012442	-0.051598	3.932537
257.806691	5248.896262	16.017447	-0.051564	3.929638
257.837263	5240.968110	16.022451	-0.051565	3.926796
257.714315	5232.964731	16.027456	-0.051536	3.923923
257.747532	5224.984554	16.032461	-0.051538	3.921058
257.988691	5217.017849	16.037466	-0.051577	3.918200
257.734279	5208.977187	16.042471	-0.051525	3.915304
257.739672	5200.952669	16.047475	-0.051521	3.912416
257.663605	5192.938277	16.052480	-0.051501	3.909529
257.586389	5184.960214	16.057485	-0.051482	3.906652
257.740914	5176.984690	16.062490	-0.051505	3.903778
257.536630	5169.000817	16.067495	-0.051462	3.900893
257.524885	5160.999914	16.072499	-0.051455	3.898003
257.426174	5153.018156	16.077504	-0.051431	3.895116
257.256480	5144.949474	16.082509	-0.051394	3.892194
257.463823	5136.943721	16.087514	-0.051428	3.889300
257.319858	5128.964213	16.092519	-0.051396	3.886407
257.335506	5120.981353	16.097523	-0.051394	3.883513
257.509224	5112.986531	16.102528	-0.051421	3.880616
257.183572	5104.992602	16.107533	-0.051355	3.877707
257.346504	5096.995686	16.112538	-0.051380	3.874804
257.301409	5088.777349	16.117543	-0.051366	3.871815
257.160935	5080.826118	16.122547	-0.051335	3.868919
257.098912	5072.863784	16.127552	-0.051318	3.866018
257.019493	5064.916115	16.132557	-0.051299	3.863120
257.195078	5056.949349	16.137562	-0.051326	3.860217
257.023549	5048.978531	16.142567	-0.051289	3.857305
257.103521	5040.948668	16.147571	-0.051299	3.854373
257.037350	5032.958594	16.152576	-0.051281	3.851451
256.899228	5024.934260	16.157581	-0.051250	3.848512
256.869850	5016.993589	16.162586	-0.051240	3.845605
256.878923	5009.025277	16.167591	-0.051236	3.842685
256.789695	5000.991093	16.172595	-0.051214	3.839737
256.788568	4993.062764	16.177600	-0.051209	3.836828
256.738188	4985.014921	16.182605	-0.051195	3.833871
256.661187	4977.005395	16.187610	-0.051175	3.830926
256.541866	4968.998538	16.192615	-0.051148	3.827979
256.525224	4960.989496	16.197619	-0.051139	3.825030
256.623860	4953.068987	16.202624	-0.051153	3.822115
256.432910	4945.025542	16.207629	-0.051112	3.819145
256.533634	4937.114558	16.212634	-0.051126	3.816229
256.579986	4929.026786	16.217639	-0.051129	3.813243
256.332547	4921.022367	16.222643	-0.051078	3.810280
256.266913	4913.066011	16.227648	-0.051060	3.807337
256.348530	4905.007728	16.232653	-0.051070	3.804356
256.549322	4897.107143	16.237658	-0.051103	3.801434
256.249890	4889.084562	16.242663	-0.051042	3.798454
256.484398	4881.064636	16.247667	-0.051080	3.795484
256.486861	4873.046150	16.252672	-0.051075	3.792507
256.452170	4864.999218	16.257677	-0.051064	3.789517
256.347534	4857.048437	16.262682	-0.051039	3.786558
256.446536	4849.045612	16.267687	-0.051052	3.783582
256.221916	4841.055907	16.272691	-0.051005	3.780601
256.152843	4833.109289	16.277696	-0.050987	3.777638
256.137482	4825.071158	16.282701	-0.050979	3.774639
256.081534	4817.087029	16.287706	-0.050964	3.771657
256.000054	4809.054833	16.292711	-0.050943	3.768655
255.788285	4801.076257	16.297715	-0.050899	3.765667
255.951081	4793.110377	16.302720	-0.050924	3.762689
255.814183	4785.050808	16.307725	-0.050893	3.759668
255.783948	4777.137758	16.312730	-0.050883	3.756701
255.721450	4769.101519	16.317735	-0.050866	3.753686
255.773059	4761.038930	16.322739	-0.050870	3.750660
255.842316	4753.083901	16.327744	-0.050878	3.747673
255.695710	4745.043246	16.332749	-0.050845	3.744646
255.925066	4737.087649	16.337754	-0.050883	3.741658
255.874573	4729.109469	16.342759	-0.050868	3.738652
255.741956	4721.099020	16.347763	-0.050839	3.735630
255.730357	4713.108988	16.352768	-0.050831	3.732615
255.688572	4705.075256	16.357773	-0.050818	3.729581
255.683476	4697.120916	16.362778	-0.050812	3.726576
255.681916	4689.114182	16.367783	-0.050807	3.723548
255.748774	4681.155773	16.372787	-0.050814	3.720538
255.647588	4673.199722	16.377792	-0.050790	3.717522
255.537456	4665.165133	16.382797	-0.050764	3.714474
255.635022	4657.085962	16.387802	-0.050777	3.711411
255.694990	4649.052840	16.392807	-0.050783	3.708362
255.541703	4641.079558	16.397811	-0.050750	3.705329
255.499717	4633.148306	16.402816	-0.050737	3.702311
255.543320	4625.135151	16.407821	-0.050740	3.699262
255.546607	4617.203318	16.412826	-0.050735	3.696241
255.194796	4609.190783	16.417831	-0.050664	3.693177
255.433357	4601.142918	16.422835	-0.050704	3.690112
255.515924	4593.179765	16.427840	-0.050714	3.687073
255.226938	4585.174269	16.432845	-0.050655	3.684006
255.330269	4577.222123	16.437850	-0.050669	3.680967
255.360204	4569.229226	16.442855	-0.050669	3.677908
255.027204	4561.224051	16.447859	-0.050602	3.674832
255.146399	4553.200319	16.452864	-0.050619	3.671758
255.230719	4545.185602	16.457869	-0.050630	3.668684
255.196509	4537.203431	16.462874	-0.050618	3.665617
255.131126	4529.213022	16.467879	-0.050601	3.662543
254.954706	4521.224716	16.472883	-0.050563	3.659465
255.027141	4513.274923	16.477888	-0.050571	3.656406
254.845259	4505.215495	16.482893	-0.050532	3.653294
254.900909	4497.203412	16.487898	-0.050537	3.650205
254.948703	4489.227731	16.492903	-0.050541	3.647127
254.964627	4481.210885	16.497907	-0.050539	3.644030
254.812197	4473.262489	16.502912	-0.050505	3.640952
254.886520	4465.244746	16.507917	-0.050514	3.637851
255.067321	4457.254626	16.512922	-0.050542	3.634760
254.718955	4449.208207	16.517927	-0.050472	3.631631
254.679218	4441.210901	16.522931	-0.050460	3.628526
254.822840	4433.229340	16.527936	-0.050481	3.625430
254.663217	4425.254921	16.532941	-0.050447	3.622326
254.592149	4417.257128	16.537946	-0.050428	3.619213
254.559814	4409.300390	16.542951	-0.050417	3.616113
254.463788	4401.277325	16.547955	-0.050394	3.612984
254.505775	4393.269081	16.552960	-0.050397	3.609861
254.488233	4385.270384	16.557965	-0.050388	3.606738
254.483062	4377.284935	16.562970	-0.050382	3.603617
254.133213	4369.340612	16.567975	-0.050312	3.600501
254.271289	4361.349241	16.572979	-0.050332	3.597377
254.343381	4353.355159	16.577984	-0.050341	3.594247
254.242168	4345.354232	16.582989	-0.050317	3.591107
254.329589	4337.322082	16.587994	-0.050328	3.587957
254.510248	4329.342634	16.592999	-0.050356	3.584828
254.113140	4321.389801	16.598003	-0.050277	3.581690
254.157040	4313.389018	16.603008	-0.050280	3.578543
254.198196	4305.348710	16.608013	-0.050282	3.575377
254.335887	4297.355153	16.613018	-0.050303	3.572230
254.126105	4289.355322	16.618023	-0.050259	3.569068
253.947137	4281.399138	16.623027	-0.050220	3.565921
254.004228	4273.401857	16.628032	-0.050226	3.562762
254.155879	4265.379413	16.633037	-0.050249	3.559593
253.938502	4257.453678	16.638042	-0.050203	3.556448
254.182236	4249.342499	16.643047	-0.050243	3.553241
253.972877	4241.281751	16.648051	-0.050199	3.550038
253.898370	4233.375507	16.653056	-0.050180	3.546897
253.796780	4225.362891	16.658061	-0.050156	3.543710
253.965157	4217.396887	16.663066	-0.050182	3.540546
253.839564	4209.438120	16.668071	-0.050154	3.537375
253.625494	4201.398466	16.673075	-0.050109	3.534165
253.789864	4193.424429	16.678080	-0.050134	3.530990
253.527512	4185.407009	16.683085	-0.050080	3.527782
253.628646	4177.431057	16.688090	-0.050094	3.524598
253.600944	4169.453369	16.693095	-0.050083	3.521407
253.530645	4161.452662	16.698099	-0.050065	3.518203
253.510771	4153.491247	16.703104	-0.050056	3.515013
253.520471	4145.433630	16.708109	-0.050053	3.511782
253.605723	4137.429701	16.713114	-0.050064	3.508572
253.512750	4129.447607	16.718119	-0.050041	3.505363
253.406133	4121.486344	16.723123	-0.050016	3.502158
253.474077	4113.517320	16.728128	-0.050024	3.498953
253.327234	4105.521933	16.733133	-0.049991	3.495728
253.281971	4097.546196	16.738138	-0.049978	3.492511
253.371681	4089.496141	16.743143	-0.049989	3.489265
253.155993	4081.514564	16.748147	-0.049944	3.486034
253.263438	4073.539793	16.753152	-0.049959	3.482813
253.146781	4065.557625	16.758157	-0.049932	3.479579
253.270136	4057.595566	16.763162	-0.049950	3.476357
253.146451	4049.578042	16.768167	-0.049921	3.473103
253.174338	4041.519158	16.773171	-0.049921	3.469833
253.179867	4033.560288	16.778176	-0.049917	3.466600
252.922305	4025.573802	16.783181	-0.049864	3.463345
252.917120	4017.592407	16.788186	-0.049858	3.460096
253.059523	4009.599793	16.793191	-0.049879	3.456845
253.063473	4001.568362	16.798195	-0.049875	3.453570
252.741295	3993.607514	16.803200	-0.049810	3.450311
252.739271	3985.591071	16.808205	-0.049804	3.447036
252.842078	3977.579112	16.813210	-0.049818	3.443763
252.670991	3969.646497	16.818215	-0.049781	3.440510
252.644856	3961.640371	16.823219	-0.049771	3.437229
252.786892	3953.640376	16.828224	-0.049792	3.433953
252.981869	3945.589653	16.833229	-0.049824	3.430655
252.767089	3937.662923	16.838234	-0.049778	3.427391
252.723154	3929.629669	16.843239	-0.049765	3.424086
252.524064	3921.688974	16.848243	-0.049723	3.420810
252.580550	3913.684925	16.853248	-0.049728	3.417514
252.521533	3905.649704	16.858253	-0.049712	3.414198
252.480921	3897.692601	16.863258	-0.049699	3.410912
252.477659	3889.693273	16.868263	-0.049694	3.407606
252.256504	3881.701745	16.873267	-0.049647	3.404292
252.369606	3873.764829	16.878272	-0.049663	3.401010
252.229818	3865.759549	16.883277	-0.049632	3.397687
252.114134	3857.776699	16.888282	-0.049605	3.394371
252.263859	3849.645660	16.893287	-0.049628	3.391000
252.532389	3841.650760	16.898291	-0.049673	3.387686
252.345533	3833.702744	16.903296	-0.049633	3.384372
252.184682	3825.772392	16.908301	-0.049598	3.381063
252.068215	3817.803458	16.913306	-0.049571	3.377737
252.186013	3809.782150	16.918311	-0.049588	3.374393
251.814670	3801.796206	16.923315	-0.049513	3.371044
252.077795	3793.796309	16.928320	-0.049557	3.367708
251.832042	3785.751587	16.933325	-0.049506	3.364332
251.790504	3777.842029	16.938330	-0.049493	3.361017
251.928471	3769.859401	16.943335	-0.049514	3.357674
251.992261	3761.827131	16.948339	-0.049521	3.354304
251.836063	3753.839718	16.953344	-0.049486	3.350941
251.775450	3745.826169	16.958349	-0.049470	3.347568
251.897106	3737.833084	16.963354	-0.049487	3.344207
251.853108	3729.885327	16.968359	-0.049474	3.340855
251.781652	3721.871052	16.973363	-0.049456	3.337470
251.916840	3713.903792	16.978368	-0.049476	3.334110
251.673000	3705.889099	16.983373	-0.049425	3.330713
251.547433	3697.907724	16.988378	-0.049396	3.327330
251.565758	3689.915993	16.993383	-0.049395	3.323945
251.532996	3681.924390	16.998387	-0.049383	3.320554
251.557387	3673.973411	17.003392	-0.049383	3.317180
251.351150	3665.963536	17.008397	-0.049339	3.313768
251.499303	3657.915196	17.013402	-0.049362	3.310350
251.432671	3649.952070	17.018407	-0.049344	3.306956
251.256047	3641.962295	17.023411	-0.049306	3.303543
251.257813	3633.993466	17.028416	-0.049301	3.300143
251.407935	3625.973568	17.033421	-0.049324	3.296723
251.479341	3617.995978	17.038426	-0.049332	3.293314
251.357683	3609.990741	17.043431	-0.049304	3.289883
251.346811	3602.024727	17.048435	-0.049297	3.286469
251.232894	3594.068290	17.053440	-0.049271	3.283051
251.184545	3586.061223	17.058445	-0.049257	3.279611
251.323438	3578.098618	17.063450	-0.049277	3.276194
251.226555	3570.080815	17.068455	-0.049254	3.272740
251.140960	3562.041524	17.073459	-0.049233	3.269274
251.205322	3554.092653	17.078464	-0.049240	3.265849
251.174726	3546.088483	17.083469	-0.049229	3.262392
251.082432	3538.091962	17.088474	-0.049207	3.258933
251.116977	3530.129133	17.093479	-0.049208	3.255490
250.956619	3522.117694	17.098483	-0.049173	3.252014
250.933158	3514.148356	17.103488	-0.049163	3.248558
250.874777	3506.148315	17.108493	-0.049147	3.245084
250.873280	3498.176032	17.113498	-0.049142	3.241621
250.885385	3490.187336	17.118503	-0.049139	3.238147
250.772596	3482.223112	17.123507	-0.049113	3.234675
250.828196	3474.143003	17.128512	-0.049118	3.231155
250.781459	3466.131995	17.133517	-0.049104	3.227658
250.744846	3458.155181	17.138522	-0.049092	3.224172
250.607723	3450.227113	17.143527	-0.049061	3.220700
250.532546	3442.227718	17.148531	-0.049042	3.217195
250.573422	3434.237558	17.153536	-0.049045	3.213696
250.564877	3426.213088	17.158541	-0.049038	3.210175
250.512478	3418.255567	17.163546	-0.049023	3.206678
250.522536	3410.275295	17.168551	-0.049020	3.203170
250.484751	3402.289161	17.173555	-0.049008	3.199653
250.587316	3394.331067	17.178560	-0.049022	3.196151
250.426305	3386.311957	17.183565	-0.048986	3.192607
250.278150	3378.324631	17.188570	-0.048954	3.189073
250.229754	3370.345872	17.193575	-0.048939	3.185544
250.330388	3362.333507	17.198579	-0.048953	3.182002
250.366762	3354.372101	17.203584	-0.048955	3.178476
250.169067	3346.369571	17.208589	-0.048913	3.174918
249.991974	3338.379047	17.213594	-0.048875	3.171362
249.977206	3330.395938	17.218599	-0.048867	3.167812
250.079213	3322.357909	17.223603	-0.048880	3.164239
250.197353	3314.456198	17.228608	-0.048897	3.160723
250.056402	3306.476473	17.233613	-0.048866	3.157158
250.076461	3298.430775	17.238618	-0.048864	3.153565
250.016447	3290.433452	17.243623	-0.048848	3.149987
249.976517	3282.446074	17.248627	-0.048836	3.146410
250.048407	3274.479831	17.253632	-0.048844	3.142844
249.789481	3266.493848	17.258637	-0.048790	3.139250
249.898496	3258.534467	17.263642	-0.048806	3.135680
249.912976	3250.518466	17.268647	-0.048803	3.132076
249.889383	3242.504354	17.273651	-0.048793	3.128467
249.644638	3234.576064	17.278656	-0.048743	3.124883
249.769617	3226.598928	17.283661	-0.048761	3.121290
249.589555	3218.618374	17.288666	-0.048722	3.117677
249.610397	3210.640982	17.293671	-0.048721	3.114070
249.447847	3202.589799	17.298675	-0.048685	3.110417
249.796313	3194.593500	17.303680	-0.048745	3.106808
249.622776	3186.604913	17.308685	-0.048708	3.103174
249.524631	3178.655985	17.313690	-0.048684	3.099558
249.706647	3170.693052	17.318695	-0.048713	3.095944
249.568991	3162.655025	17.323699	-0.048682	3.092277
249.468502	3154.687181	17.328704	-0.048658	3.088639
249.492528	3146.675876	17.333709	-0.048658	3.084983
249.571117	3138.711545	17.338714	-0.048667	3.081347
249.458147	3130.776682	17.343719	-0.048641	3.077710
249.358807	3122.757249	17.348723	-0.048617	3.074032
249.316406	3114.682495	17.353728	-0.048604	3.070326
249.185419	3106.730494	17.358733	-0.048575	3.066668
249.164479	3098.744235	17.363738	-0.048566	3.062995
249.261355	3090.779910	17.368743	-0.048579	3.059333
249.060208	3082.820431	17.373747	-0.048536	3.055655
249.114303	3074.818725	17.378752	-0.048541	3.051965
248.977227	3066.832165	17.383757	-0.048510	3.048269
249.032544	3058.832827	17.388762	-0.048515	3.044571
249.086161	3050.885125	17.393767	-0.048520	3.040893
248.767243	3042.920979	17.398771	-0.048456	3.037184
248.822104	3034.924604	17.403776	-0.048461	3.033475
248.769377	3026.903521	17.408781	-0.048446	3.029743
248.706245	3018.951083	17.413786	-0.048429	3.026039
248.984715	3010.937976	17.418791	-0.048475	3.022319
248.873586	3002.948549	17.423795	-0.048450	3.018586
248.805658	2994.996602	17.428800	-0.048432	3.014868
248.674331	2986.991773	17.433805	-0.048402	3.011117
248.604934	2979.025125	17.438810	-0.048384	3.007383
248.654286	2971.038611	17.443815	-0.048388	3.003641
248.514196	2963.060070	17.448819	-0.048357	2.999888
248.617563	2955.105031	17.453824	-0.048371	2.996154
248.445204	2947.071699	17.458829	-0.048334	2.992364
248.384865	2939.069862	17.463834	-0.048317	2.988590
248.365419	2931.098288	17.468839	-0.048309	2.984828
248.370756	2923.112346	17.473843	-0.048304	2.981055
248.321034	2915.168104	17.478848	-0.048290	2.977295
248.294713	2907.170165	17.483853	-0.048280	2.973506
248.648911	2899.130544	17.488858	-0.048341	2.969711
248.375967	2891.212251	17.493863	-0.048285	2.965937
248.172927	2883.232367	17.498867	-0.048242	2.962132
248.333034	2875.241476	17.503872	-0.048266	2.958336
248.302673	2867.274738	17.508877	-0.048256	2.954537
248.181275	2859.262723	17.513882	-0.048228	2.950707
248.201322	2851.280481	17.518887	-0.048226	2.946893
248.186405	2843.287575	17.523891	-0.048218	2.943067
248.212416	2835.322768	17.528896	-0.048218	2.939252
248.228456	2827.340110	17.533901	-0.048216	2.935423
248.228855	2819.350081	17.538906	-0.048211	2.931585
248.056205	2811.377724	17.543911	-0.048174	2.927740
247.818457	2803.411386	17.548915	-0.048124	2.923891
248.029779	2795.436253	17.553920	-0.048158	2.920055
248.033825	2787.452231	17.558925	-0.048154	2.916200
247.999298	2779.410747	17.563930	-0.048142	2.912309
247.762938	2771.444767	17.568935	-0.048093	2.908439
247.502418	2763.442637	17.573939	-0.048040	2.904545
247.732828	2755.492893	17.578944	-0.048077	2.900697
247.569891	2747.514959	17.583949	-0.048042	2.896810
247.507815	2739.522544	17.588954	-0.048025	2.892915
247.730788	2731.519514	17.593959	-0.048061	2.889026
247.514624	2723.554256	17.598963	-0.048016	2.885126
247.433252	2715.633373	17.603968	-0.047996	2.881250
247.461954	2707.640795	17.608973	-0.047996	2.877339
247.247495	2699.674797	17.613978	-0.047951	2.873423
247.230472	2691.647445	17.618983	-0.047943	2.869482
247.298953	2683.652007	17.623987	-0.047950	2.865556
247.595012	2675.673609	17.628992	-0.048000	2.861646
247.365080	2667.727188	17.633997	-0.047952	2.857717
247.088586	2659.767991	17.639002	-0.047895	2.853773
247.069618	2651.757396	17.644007	-0.047887	2.849813
246.910022	2643.797814	17.649011	-0.047852	2.845865
247.095785	2635.819661	17.654016	-0.047881	2.841922
247.146944	2627.833187	17.659021	-0.047886	2.837961
247.097449	2619.854216	17.664026	-0.047871	2.833993
247.030037	2611.859650	17.669031	-0.047854	2.830011
246.834418	2603.870347	17.674035	-0.047812	2.826018
246.819920	2595.907368	17.679040	-0.047804	2.822043
246.674778	2587.949976	17.684045	-0.047772	2.818058
246.925702	2579.947894	17.689050	-0.047814	2.814067
246.954933	2571.953862	17.694055	-0.047814	2.810062
246.609833	2563.999993	17.699059	-0.047744	2.806050
246.637340	2556.042045	17.704064	-0.047744	2.802052
246.622531	2548.063139	17.709069	-0.047737	2.798035
246.646043	2540.078888	17.714074	-0.047736	2.794012
246.807153	2532.063608	17.719079	-0.047761	2.789975
246.790258	2524.074325	17.724083	-0.047752	2.785935
246.768830	2516.130440	17.729088	-0.047743	2.781912
246.476526	2508.189601	17.734093	-0.047684	2.777869
246.314482	2500.210885	17.739098	-0.047648	2.773808
246.428788	2492.199388	17.744103	-0.047664	2.769741
246.409576	2484.228695	17.749107	-0.047656	2.765681
246.527726	2476.264015	17.754112	-0.047673	2.761626
246.463036	2468.292728	17.759117	-0.047655	2.757551
246.377518	2460.283866	17.764122	-0.047634	2.753449
246.252869	2452.264798	17.769127	-0.047606	2.749334
246.110924	2444.307276	17.774131	-0.047574	2.745242
246.281292	2436.341182	17.779136	-0.047601	2.741160
245.980780	2428.395304	17.784141	-0.047540	2.737053
245.972569	2420.417786	17.789146	-0.047533	2.732941
246.115744	2412.421606	17.794151	-0.047555	2.728823
246.066429	2404.436168	17.799155	-0.047540	2.724692
245.924312	2396.527553	17.804160	-0.047509	2.720589
246.073757	2388.536589	17.809165	-0.047531	2.716455
245.878879	2380.552594	17.814170	-0.047490	2.712298
245.921549	2372.566311	17.819175	-0.047493	2.708147
245.878964	2364.566531	17.824179	-0.047480	2.703977
246.041593	2356.611278	17.829184	-0.047505	2.699838
245.865071	2348.667131	17.834189	-0.047467	2.695676
245.609976	2340.686988	17.839194	-0.047414	2.691484
245.821861	2332.700570	17.844199	-0.047448	2.687312
245.889459	2324.710588	17.849203	-0.047456	2.683122
245.665661	2316.785529	17.854208	-0.047409	2.678941
245.717855	2308.810473	17.859213	-0.047414	2.674745
245.603956	2300.796497	17.864218	-0.047387	2.670512
245.479634	2292.848530	17.869223	-0.047359	2.666305
245.519379	2284.844835	17.874227	-0.047361	2.662074
245.403738	2276.916954	17.879232	-0.047334	2.657865
245.102444	2268.947387	17.884237	-0.047273	2.653616
245.144692	2260.939316	17.889242	-0.047276	2.649361
245.449014	2252.957941	17.894247	-0.047327	2.645132
245.547995	2244.983658	17.899251	-0.047341	2.640885
245.296380	2237.079564	17.904256	-0.047289	2.636647
245.293326	2229.073165	17.909261	-0.047283	2.632363
245.480611	2221.056897	17.914266	-0.047313	2.628079
245.214136	2213.124182	17.919271	-0.047258	2.623804
244.925210	2205.176578	17.924275	-0.047199	2.619511
245.190309	2197.188846	17.929280	-0.047243	2.615227
245.080562	2189.208530	17.934285	-0.047218	2.610915
244.822424	2181.252115	17.939290	-0.047164	2.606599
245.097756	2173.267381	17.944295	-0.047210	2.602296
244.858422	2165.327363	17.949299	-0.047161	2.597975
244.822440	2157.327611	17.954304	-0.047149	2.593629
244.807771	2149.181487	17.959309	-0.047141	2.589197
244.840244	2141.241778	17.964314	-0.047142	2.584873
244.895728	2133.337019	17.969319	-0.047147	2.580563
244.749974	2125.397401	17.974323	-0.047115	2.576212
244.820837	2117.417523	17.979328	-0.047123	2.571847
244.665498	2109.454357	17.984333	-0.047089	2.567468
244.714385	2101.495542	17.989338	-0.047093	2.563098
244.544717	2093.577052	17.994343	-0.047056	2.558728
244.505892	2085.603287	17.999347	-0.047044	2.554329
244.474272	2077.629655	18.004352	-0.047033	2.549923
244.282624	2069.665906	18.009357	-0.046992	2.545503
244.457820	2061.675336	18.014362	-0.047019	2.541087
244.542877	2053.727168	18.019367	-0.047030	2.536680
244.055489	2045.797099	18.024371	-0.046934	2.532235
244.321702	2037.782977	18.029376	-0.046978	2.527788
244.383962	2029.821186	18.034381	-0.046985	2.523349
244.079485	2021.900010	18.039386	-0.046923	2.518898
244.206387	2013.935129	18.044391	-0.046942	2.514446
244.097911	2005.913639	18.049395	-0.046916	2.509937
244.057501	1997.951406	18.054400	-0.046904	2.505459
243.947691	1990.011547	18.059405	-0.046878	2.500980
244.049796	1982.020454	18.064410	-0.046892	2.496479
244.110277	1974.057641	18.069415	-0.046898	2.491983
243.807847	1966.106029	18.074419	-0.046836	2.487459
243.961179	1958.156959	18.079424	-0.046860	2.482961
243.742570	1950.216443	18.084429	-0.046814	2.478433
243.816774	1942.225350	18.089434	-0.046823	2.473889
243.810031	1934.247402	18.094439	-0.046816	2.469339
243.809718	1926.266122	18.099443	-0.046811	2.464778
243.782840	1918.337405	18.104448	-0.046801	2.460237
243.697167	1910.387794	18.109453	-0.046780	2.455672
243.755200	1902.391022	18.114458	-0.046785	2.451081
243.481037	1894.462002	18.119463	-0.046729	2.446496
243.398478	1886.505789	18.124467	-0.046709	2.441901
243.517507	1878.567207	18.129472	-0.046726	2.437323
243.393936	1870.569573	18.134477	-0.046698	2.432684
243.404460	1862.538642	18.139482	-0.046694	2.428026
243.209294	1854.614439	18.144487	-0.046653	2.423406
243.311294	1846.638257	18.149491	-0.046667	2.418770
243.431156	1838.678669	18.154496	-0.046684	2.414136
243.137459	1830.731571	18.159501	-0.046624	2.409468
243.281442	1822.751696	18.164506	-0.046646	2.404806
243.276929	1814.832752	18.169511	-0.046640	2.400159
243.028865	1806.917060	18.174515	-0.046589	2.395486
243.061587	1798.913805	18.179520	-0.046589	2.390774
243.190387	1790.937754	18.184525	-0.046608	2.386076
243.010766	1783.010985	18.189530	-0.046570	2.381374
243.113355	1775.061068	18.194535	-0.046584	2.376671
243.092871	1767.071903	18.199539	-0.046575	2.371926
242.910062	1759.135246	18.204544	-0.046536	2.367190
242.973463	1751.176703	18.209549	-0.046542	2.362451
242.937733	1743.224479	18.214554	-0.046530	2.357698
243.018196	1735.264008	18.219559	-0.046540	2.352940
242.544077	1727.322848	18.224563	-0.046447	2.348139
242.715738	1719.339276	18.229568	-0.046474	2.343355
242.858335	1711.388515	18.234573	-0.046495	2.338578
242.709107	1703.438502	18.239578	-0.046462	2.333769
242.540746	1695.490549	18.244583	-0.046426	2.328949
242.474113	1687.527790	18.249587	-0.046408	2.324118
242.586463	1679.588526	18.254592	-0.046424	2.319307
242.604236	1671.627319	18.259597	-0.046422	2.314464
242.428023	1663.669912	18.264602	-0.046384	2.309597
242.553999	1655.714771	18.269607	-0.046402	2.304747
242.500708	1647.772612	18.274611	-0.046387	2.299879
242.329996	1639.845129	18.279616	-0.046351	2.295000
242.368967	1631.867718	18.284621	-0.046353	2.290098
242.156466	1623.926314	18.289626	-0.046308	2.285186
242.201964	1616.000349	18.294631	-0.046311	2.280295
242.175748	1608.039529	18.299635	-0.046301	2.275366
242.137216	1600.019737	18.304640	-0.046289	2.270388
242.104792	1592.051066	18.309645	-0.046278	2.265432
241.990833	1584.121668	18.314650	-0.046251	2.260482
242.182705	1576.164709	18.319655	-0.046282	2.255530
241.791108	1568.246707	18.324659	-0.046204	2.250542
241.785336	1560.298228	18.329664	-0.046198	2.245557
242.032361	1552.332118	18.334669	-0.046239	2.240571
242.049546	1544.396605	18.339674	-0.046237	2.235574
241.892404	1536.462202	18.344679	-0.046202	2.230551
241.771292	1528.502771	18.349683	-0.046175	2.225504
241.745741	1520.576578	18.354688	-0.046165	2.220475
241.769646	1512.622395	18.359693	-0.046164	2.215421
241.400855	1504.700704	18.364698	-0.046090	2.210341
241.617611	1496.729876	18.369703	-0.046125	2.205270
241.263650	1488.837744	18.374707	-0.046054	2.200187
241.338593	1480.889890	18.379712	-0.046063	2.195095
241.452233	1472.881464	18.384717	-0.046079	2.189956
241.230374	1464.941437	18.389722	-0.046033	2.184818
241.125996	1457.036630	18.394727	-0.046008	2.179701
241.019237	1449.086013	18.399731	-0.045983	2.174543
241.136510	1441.109970	18.404736	-0.046000	2.169376
241.144417	1433.175351	18.409741	-0.045996	2.164214
241.088504	1425.248660	18.414746	-0.045981	2.159039
241.147010	1417.311304	18.419751	-0.045986	2.153855
241.113012	1409.343420	18.424755	-0.045975	2.148630
240.826917	1401.440273	18.429760	-0.045917	2.143411
240.820383	1393.514829	18.434765	-0.045910	2.138191
240.806083	1385.562846	18.439770	-0.045902	2.132940
240.805833	1377.615932	18.444775	-0.045897	2.127680
240.817286	1369.671220	18.449779	-0.045894	2.122410
240.843066	1361.757742	18.454784	-0.045894	2.117149
240.938743	1353.746719	18.459789	-0.045907	2.111817
240.483188	1345.838533	18.464794	-0.045817	2.106487
240.569035	1337.896532	18.469799	-0.045828	2.101173
240.508824	1329.970409	18.474803	-0.045811	2.095841
240.430328	1322.051160	18.479808	-0.045791	2.090499
240.432612	1314.106288	18.484813	-0.045787	2.085134
240.473497	1306.173462	18.489818	-0.045789	2.079768
240.291795	1298.287282	18.494823	-0.045750	2.074396
240.356501	1290.300031	18.499827	-0.045757	2.068967
240.442791	1282.358852	18.504832	-0.045768	2.063557
240.178302	1274.487657	18.509837	-0.045714	2.058145
240.026283	1266.556332	18.514842	-0.045680	2.052690
240.242575	1258.591050	18.519847	-0.045716	2.047233
240.222158	1250.672525	18.524851	-0.045707	2.041770
240.222006	1242.757776	18.529856	-0.045701	2.036297
240.034165	1234.828955	18.534861	-0.045661	2.030781
239.952626	1226.881020	18.539866	-0.045641	2.025246
239.988471	1218.965922	18.544871	-0.045643	2.019732
239.834909	1211.048864	18.549875	-0.045609	2.014182
239.922953	1203.093068	18.554880	-0.045620	2.008614
239.919433	1195.174797	18.559885	-0.045614	2.003048
239.593797	1187.303521	18.564890	-0.045549	1.997465
239.784840	1179.343775	18.569895	-0.045579	1.991859
239.656737	1171.420961	18.574899	-0.045550	1.986229
239.419041	1163.529770	18.579904	-0.045501	1.980594
239.484988	1155.599523	18.584909	-0.045508	1.974948
239.689632	1147.623857	18.589914	-0.045541	1.969267
239.606034	1139.740186	18.594919	-0.045520	1.963605
239.513105	1131.842538	18.599923	-0.045498	1.957916
239.320757	1123.914065	18.604928	-0.045457	1.952177
239.258721	1115.962973	18.609933	-0.045440	1.946419
239.009857	1108.081121	18.614938	-0.045389	1.940674
239.078344	1100.158971	18.619943	-0.045396	1.934917
239.159176	1092.205057	18.624947	-0.045406	1.929121
239.028128	1084.300308	18.629952	-0.045377	1.923320
239.037274	1076.408499	18.634957	-0.045373	1.917527
238.995061	1068.482448	18.639962	-0.045360	1.911685
238.857336	1060.583905	18.644967	-0.045330	1.905835
238.678372	1052.693864	18.649971	-0.045291	1.899968
238.803971	1044.764256	18.654976	-0.045310	1.894088
238.941411	1036.819912	18.659981	-0.045330	1.888181
238.862938	1028.924175	18.664986	-0.045310	1.882266
238.897749	1021.042465	18.669991	-0.045312	1.876356
238.807475	1013.112459	18.674995	-0.045290	1.870377
238.818350	1005.190957	18.680000	-0.045287	1.864397
238.672270	997.321914	18.685005	-0.045254	1.858419
238.602118	989.413950	18.690010	-0.045236	1.852401
238.574155	981.510521	18.695015	-0.045226	1.846372
238.232406	973.654782	18.700019	-0.045157	1.840323
238.421282	965.730176	18.705024	-0.045187	1.834263
238.359575	957.812229	18.710029	-0.045171	1.828159
238.258519	949.916317	18.715034	-0.045147	1.822046
238.103685	942.055849	18.720039	-0.045113	1.815934
238.095800	934.134732	18.725043	-0.045106	1.809772
238.035158	926.249316	18.730048	-0.045090	1.803611
237.926462	918.380392	18.735053	-0.045064	1.797435
237.923318	910.422264	18.740058	-0.045059	1.791180
238.144500	902.474258	18.745063	-0.045095	1.784939
237.945968	894.628483	18.750067	-0.045053	1.778706
237.766169	886.760147	18.755072	-0.045014	1.772435
237.974991	878.825602	18.760077	-0.045048	1.766137
237.902832	870.952036	18.765082	-0.045029	1.759831
237.765806	863.108692	18.770087	-0.044999	1.753517
237.697622	855.214635	18.775091	-0.044981	1.747149
237.745662	847.318460	18.780096	-0.044985	1.740771
237.535530	839.486031	18.785101	-0.044941	1.734387
237.457269	831.566821	18.790106	-0.044921	1.727927
237.599231	823.692957	18.795111	-0.044942	1.721507
237.429189	815.843440	18.800115	-0.044906	1.715043
237.368434	807.945322	18.805120	-0.044889	1.708529
237.549047	800.039078	18.810125	-0.044918	1.702015
237.366642	792.188843	18.815130	-0.044879	1.695474
237.411023	784.305316	18.820135	-0.044882	1.688911
237.371857	776.436505	18.825139	-0.044870	1.682323
237.202048	768.603062	18.830144	-0.044833	1.675721
236.997938	760.741743	18.835149	-0.044790	1.669065
237.012090	752.856648	18.840154	-0.044787	1.662392
237.119484	745.001141	18.845159	-0.044802	1.655729
236.910395	737.140218	18.850163	-0.044758	1.648992
236.825809	729.291724	18.855168	-0.044737	1.642255
236.942037	721.419873	18.860173	-0.044754	1.635498
236.839823	713.510347	18.865178	-0.044730	1.628649
236.860778	705.650327	18.870183	-0.044729	1.621832
236.744185	697.814905	18.875187	-0.044702	1.614989
236.602786	689.970800	18.880192	-0.044670	1.608105
236.576783	682.128719	18.885197	-0.044661	1.601209
236.506683	674.288285	18.890202	-0.044642	1.594279
236.647395	666.404618	18.895207	-0.044664	1.587311
236.321657	658.600061	18.900211	-0.044598	1.580315
236.220775	650.781705	18.905216	-0.044574	1.573308
236.296737	642.902036	18.910221	-0.044583	1.566240
236.259581	635.080376	18.915226	-0.044571	1.559176
236.050949	627.268279	18.920231	-0.044527	1.552064
236.018850	619.401456	18.925235	-0.044516	1.544895
236.183564	611.546657	18.930240	-0.044542	1.537732
236.155360	603.719539	18.935245	-0.044531	1.530533
236.030116	595.900460	18.940250	-0.044503	1.523293
236.085057	588.083736	18.945255	-0.044508	1.516047
235.706968	580.295991	18.950259	-0.044433	1.508728
235.596610	572.482915	18.955264	-0.044407	1.501390
235.611083	564.663530	18.960269	-0.044405	1.494030
235.620622	556.816565	18.965274	-0.044402	1.486606
235.327441	549.066614	18.970279	-0.044342	1.479190
235.356581	541.210732	18.975283	-0.044342	1.471685
235.524430	533.335872	18.980288	-0.044368	1.464146
235.451066	525.559766	18.985293	-0.044350	1.456625
235.368223	517.752066	18.990298	-0.044329	1.449033
235.397643	509.958812	18.995303	-0.044330	1.441433
235.324083	502.178582	19.000307	-0.044311	1.433789
235.239670	494.378159	19.005312	-0.044290	1.426082
235.194830	486.611157	19.010317	-0.044277	1.418373
234.871253	478.855313	19.015322	-0.044212	1.410586
234.814053	471.086661	19.020327	-0.044196	1.402788
234.911094	463.284783	19.025331	-0.044209	1.394939
234.874369	455.482145	19.030336	-0.044197	1.387021
234.715276	447.738212	19.035341	-0.044163	1.379098
234.621521	439.964554	19.040346	-0.044140	1.371109
234.722909	432.185730	19.045351	-0.044154	1.363102
234.574589	424.447642	19.050355	-0.044121	1.355046
234.423382	416.688727	19.055360	-0.044088	1.346920
234.520889	408.925717	19.060365	-0.044101	1.338784
234.321659	401.197195	19.065370	-0.044059	1.330582
234.391621	393.444939	19.070375	-0.044067	1.322352
234.143620	385.713226	19.075379	-0.044016	1.314036
234.293180	377.824092	19.080384	-0.044039	1.305568
234.305365	370.112072	19.085389	-0.044036	1.297212
233.914661	362.440398	19.090394	-0.043958	1.288773
234.167707	354.685426	19.095399	-0.044000	1.280305
233.958011	347.005199	19.100403	-0.043956	1.271777
233.958328	339.285729	19.105408	-0.043952	1.263188
233.714366	331.627517	19.110413	-0.043901	1.254561
233.896491	323.873121	19.115418	-0.043930	1.245848
233.716963	316.234100	19.120423	-0.043892	1.237136
233.562365	308.538095	19.125427	-0.043858	1.228300
233.495950	300.857362	19.130432	-0.043841	1.219436
233.327868	293.204168	19.135437	-0.043804	1.210519
233.136133	285.549678	19.140442	-0.043764	1.201529
233.099827	277.889404	19.145447	-0.043752	1.192496
232.995385	270.227243	19.150451	-0.043728	1.183378
232.994541	262.569942	19.155456	-0.043723	1.174216
232.916716	254.930716	19.160461	-0.043703	1.164987
232.964010	247.277421	19.165466	-0.043707	1.155694
232.958827	239.602414	19.170471	-0.043701	1.146288
232.736435	232.016689	19.175475	-0.043655	1.136869
232.479734	224.427977	19.180480	-0.043602	1.127360
232.538605	216.812956	19.185485	-0.043608	1.117805
232.573015	209.187996	19.190490	-0.043610	1.108149
232.357792	201.635090	19.195495	-0.043565	1.098446
232.172718	194.068460	19.200499	-0.043525	1.088646
231.919482	186.537770	19.205504	-0.043473	1.078788
231.778839	178.979034	19.210509	-0.043442	1.068827
231.514382	171.442910	19.215514	-0.043388	1.058774
231.214161	163.930413	19.220519	-0.043327	1.048649
230.678033	156.467642	19.225523	-0.043223	1.038436
230.427267	148.957156	19.230528	-0.043171	1.028124
230.033427	141.492990	19.235533	-0.043093	1.017737
229.320579	134.071172	19.240538	-0.042955	1.007225
229.098181	126.599287	19.245543	-0.042909	0.996651
228.732568	119.109546	19.250547	-0.042836	0.985903
227.941507	111.743276	19.255552	-0.042684	0.975107
227.573154	104.310174	19.260557	-0.042611	0.964200
227.410814	96.865058	19.265562	-0.042576	0.953203
226.710261	89.527143	19.270567	-0.042441	0.942098
226.081156	82.187457	19.275571	-0.042319	0.930876
225.606978	74.835842	19.280576	-0.042226	0.919540
225.204039	67.482408	19.285581	-0.042146	0.908079
224.651705	60.398502	19.290586	-0.042039	0.896853