Fri Mar 12 14:01:21 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.626402	0.025446	0.000000	0.000021	0.721127

0.517905	0.041557	0.005005	0.000042	0.721120
0.557187	0.040081	0.010010	0.000034	0.721131
0.309812	0.078026	0.015014	0.000080	0.721119
0.550626	0.035783	0.020019	0.000035	0.721121
0.558656	0.037254	0.025024	0.000034	0.721127
0.432301	0.055712	0.030029	0.000057	0.721119
0.732694	0.008533	0.035034	0.000001	0.721131
0.840995	-0.014558	0.040038	-0.000019	0.721124
0.734327	0.004323	0.045043	0.000001	0.721124
0.596649	0.030828	0.050048	0.000027	0.721128
0.626820	0.020817	0.055053	0.000021	0.721119
0.674507	0.018837	0.060058	0.000012	0.721131
0.547911	0.034838	0.065062	0.000036	0.721119
0.572822	0.033620	0.070067	0.000031	0.721125
0.547834	0.039027	0.075072	0.000036	0.721127
0.570368	0.032043	0.080077	0.000031	0.721121
0.424294	-0.062184	0.085082	0.000059	0.720885
0.495172	-0.079125	0.090086	0.000045	0.720876
0.527044	-0.083884	0.095091	0.000039	0.720878
0.520184	-0.079842	0.100096	0.000041	0.720884
0.436550	-0.070100	0.105101	0.000056	0.720874
0.747896	-0.120740	0.110106	-0.000002	0.720883
0.458860	-0.135221	0.115110	0.000052	0.720753
0.612656	-0.270933	0.120115	0.000023	0.720540
0.818468	-0.306470	0.125120	-0.000015	0.720543
0.652383	-0.280259	0.130125	0.000016	0.720536
0.517389	-0.251655	0.135130	0.000041	0.720545
0.682879	-0.362110	0.140134	0.000010	0.720386
0.480326	-0.409025	0.145139	0.000048	0.720222
0.415789	-0.395308	0.150144	0.000060	0.720227
0.396446	-0.397011	0.155149	0.000063	0.720217
0.746886	-0.491314	0.160154	-0.000002	0.720154
0.616126	-0.597335	0.165158	0.000023	0.719899
0.543421	-0.586086	0.170163	0.000036	0.719896
0.541944	-0.583679	0.175168	0.000036	0.719900
0.309671	-0.621918	0.180173	0.000080	0.719744
0.506319	-0.728211	0.185178	0.000043	0.719603
0.477947	-0.726955	0.190182	0.000048	0.719596
0.523008	-0.749942	0.195187	0.000040	0.719566
0.401968	-0.876386	0.200192	0.000062	0.719275
0.258653	-0.854340	0.205197	0.000089	0.719268
0.402285	-0.876077	0.210202	0.000062	0.719275
0.190743	-0.983336	0.215206	0.000102	0.718990
0.523086	-1.056961	0.220211	0.000040	0.718961
0.646842	-1.076426	0.225216	0.000017	0.718966
0.583186	-1.230168	0.230221	0.000029	0.718641
0.618703	-1.232179	0.235226	0.000022	0.718649
0.472612	-1.257991	0.240230	0.000049	0.718547
0.409591	-1.343256	0.245235	0.000061	0.718356
0.368787	-1.334404	0.250240	0.000068	0.718360
0.298883	-1.448883	0.255245	0.000082	0.718109
0.246231	-1.483949	0.260250	0.000091	0.718021
-0.439684	-1.383384	0.265254	0.000219	0.717979
-0.166274	-1.571026	0.270259	0.000168	0.717704
-0.155054	-1.570888	0.275264	0.000166	0.717709
-0.225707	-1.651956	0.280269	0.000179	0.717523
-0.050782	-1.751994	0.285274	0.000147	0.717387
0.029047	-1.791549	0.290278	0.000132	0.717337
0.252178	-1.960528	0.295283	0.000090	0.717082
0.167837	-1.941436	0.300288	0.000106	0.717090
-0.008280	-2.070610	0.305293	0.000139	0.716772
-0.255354	-2.032392	0.310298	0.000185	0.716761
-0.490641	-2.103919	0.315302	0.000229	0.716536
-0.442966	-2.156954	0.320307	0.000220	0.716448
-0.281206	-2.260772	0.325312	0.000190	0.716300
-1.126516	-2.195387	0.330317	0.000347	0.716131
-1.133452	-2.211759	0.335322	0.000348	0.716096
-0.721277	-2.391700	0.340326	0.000271	0.715885
-1.792220	-2.200132	0.345331	0.000471	0.715887
-2.142340	-2.284249	0.350336	0.000536	0.715597
-2.620696	-2.225525	0.355341	0.000625	0.715544
-2.558093	-2.267733	0.360346	0.000613	0.715483
-3.763852	-2.178990	0.365350	0.000838	0.715233
-3.285627	-2.264810	0.370355	0.000749	0.715232
-3.471133	-2.263670	0.375360	0.000783	0.715169
-4.520567	-2.209596	0.380365	0.000979	0.714905
-3.906485	-2.314822	0.385370	0.000864	0.714913
-4.410581	-2.227884	0.390374	0.000958	0.714908
-5.274618	-2.220033	0.395379	0.001119	0.714618
-5.021111	-2.267827	0.400384	0.001072	0.714613
-5.413275	-2.202517	0.405389	0.001145	0.714604
-5.415725	-2.245948	0.410394	0.001145	0.714517
-6.239868	-2.219577	0.415398	0.001298	0.714278
-6.124778	-2.241728	0.420403	0.001277	0.714274
-6.184202	-2.227207	0.425408	0.001288	0.714282
-6.575310	-2.173320	0.430413	0.001361	0.714251
-6.818454	-2.269106	0.435418	0.001406	0.713975
-6.863137	-2.262516	0.440422	0.001414	0.713972
-7.558961	-2.139485	0.445427	0.001544	0.713970
-7.055341	-2.225947	0.450432	0.001450	0.713977
-6.957489	-2.326007	0.455437	0.001432	0.713813
-8.092998	-2.201516	0.460442	0.001643	0.713658
-8.153640	-2.192867	0.465446	0.001654	0.713654
-8.241283	-2.178307	0.470451	0.001671	0.713652
-7.866491	-2.241232	0.475456	0.001601	0.713659
-8.322399	-2.242002	0.480461	0.001686	0.713496
-9.133098	-2.163607	0.485466	0.001837	0.713365
-8.736340	-2.236217	0.490470	0.001763	0.713361
-9.175739	-2.158945	0.495475	0.001844	0.713359
-8.748053	-2.230708	0.500480	0.001765	0.713368
-8.913565	-2.206787	0.505485	0.001796	0.713357
-9.660053	-2.239065	0.510490	0.001935	0.713029
-10.314352	-2.124835	0.515494	0.002056	0.713024
-10.344408	-2.118652	0.520499	0.002062	0.713026
-9.806865	-2.211483	0.525504	0.001962	0.713032
-10.509465	-2.091196	0.530509	0.002092	0.713022
-9.853929	-2.204423	0.535514	0.001970	0.713029
-9.759690	-2.307803	0.540518	0.001953	0.712857
-11.588696	-2.055075	0.545523	0.002293	0.712711
-10.806260	-2.191975	0.550528	0.002148	0.712716
-11.092486	-2.144892	0.555533	0.002201	0.712709
-10.880248	-2.179647	0.560538	0.002161	0.712715
-10.966899	-2.166908	0.565542	0.002177	0.712710
-11.127361	-2.139137	0.570547	0.002207	0.712708
-11.207508	-2.268741	0.575552	0.002222	0.712422
-12.348775	-2.084193	0.580557	0.002435	0.712384
-11.982579	-2.146029	0.585562	0.002366	0.712391
-11.642965	-2.208694	0.590566	0.002303	0.712387
-12.389558	-2.077580	0.595571	0.002442	0.712383
-11.968791	-2.147730	0.600576	0.002364	0.712393
-12.109533	-2.125274	0.605581	0.002390	0.712388
-12.251780	-2.218439	0.610586	0.002416	0.712152
-13.190055	-2.082702	0.615590	0.002591	0.712089
-12.731215	-2.165475	0.620595	0.002506	0.712087
-12.359935	-2.226732	0.625600	0.002436	0.712097
-13.415579	-2.043327	0.630605	0.002633	0.712088
-13.141026	-2.089934	0.635610	0.002582	0.712092
-12.713695	-2.168111	0.640614	0.002502	0.712088
-13.222588	-2.197459	0.645619	0.002597	0.711849
-14.154313	-2.072971	0.650624	0.002770	0.711766
-13.980661	-2.108099	0.655629	0.002738	0.711758
-13.664451	-2.160761	0.660634	0.002679	0.711766
-13.986100	-2.106340	0.665638	0.002739	0.711760
-14.285110	-2.055639	0.670643	0.002794	0.711755
-13.692425	-2.155138	0.675648	0.002684	0.711767
-14.094061	-2.094137	0.680653	0.002759	0.711746
-14.522289	-2.163779	0.685658	0.002839	0.711455
-14.635840	-2.144324	0.690662	0.002860	0.711454
-15.085587	-2.064412	0.695667	0.002943	0.711453
-14.822064	-2.108823	0.700672	0.002894	0.711458
-15.002369	-2.081660	0.705677	0.002928	0.711449
-14.973452	-2.083130	0.710682	0.002922	0.711456
-15.250261	-2.033840	0.715686	0.002974	0.711456
-15.426360	-2.037985	0.720691	0.003007	0.711385
-15.463703	-2.154204	0.725696	0.003014	0.711140
-15.754151	-2.105884	0.730701	0.003068	0.711133
-16.232062	-2.015438	0.735706	0.003156	0.711144
-15.664179	-2.119993	0.740710	0.003051	0.711137
-15.813350	-2.094933	0.745715	0.003078	0.711134
-15.865388	-2.082018	0.750720	0.003088	0.711142
-15.766187	-2.104190	0.755725	0.003070	0.711133
-15.720706	-2.221829	0.760730	0.003061	0.710914
-16.680005	-2.073164	0.765734	0.003240	0.710870
-17.006827	-2.017070	0.770739	0.003300	0.710866
-16.173174	-2.162301	0.775744	0.003145	0.710872
-16.592078	-2.091831	0.780749	0.003223	0.710864
-16.626439	-2.082342	0.785754	0.003230	0.710871
-16.472340	-2.115585	0.790758	0.003201	0.710859
-17.596590	-2.081201	0.795763	0.003410	0.710528
-17.740449	-2.051575	0.800768	0.003437	0.710536
-17.943119	-2.020026	0.805773	0.003475	0.710527
-17.211648	-2.148030	0.810778	0.003338	0.710532
-17.685273	-2.063585	0.815782	0.003426	0.710532
-18.090819	-1.993382	0.820787	0.003502	0.710528
-17.252281	-2.139097	0.825792	0.003346	0.710535
-17.614766	-2.141900	0.830797	0.003413	0.710401
-19.085077	-1.972498	0.835802	0.003687	0.710216
-18.295562	-2.114014	0.840806	0.003540	0.710214
-18.457576	-2.087989	0.845811	0.003570	0.710209
-18.597243	-2.058447	0.850816	0.003596	0.710218
-18.828197	-2.023691	0.855821	0.003639	0.710205
-18.804847	-2.023200	0.860826	0.003635	0.710215
-18.572543	-2.064947	0.865830	0.003591	0.710214
-19.115591	-2.093602	0.870835	0.003692	0.709963
-19.551325	-2.049990	0.875840	0.003773	0.709895
-19.614979	-2.044421	0.880845	0.003785	0.709884
-19.452896	-2.068266	0.885850	0.003755	0.709894
-19.406823	-2.080026	0.890854	0.003746	0.709887
-19.292286	-2.101254	0.895859	0.003725	0.709885
-19.282234	-2.099372	0.900864	0.003723	0.709893
-19.755565	-2.083251	0.905869	0.003811	0.709757
-20.249201	-2.075243	0.910874	0.003903	0.709597
-19.829559	-2.151510	0.915878	0.003825	0.709594
-20.773855	-1.985441	0.920883	0.004001	0.709589
-20.116779	-2.098832	0.925888	0.003878	0.709597
-19.955999	-2.132165	0.930893	0.003848	0.709588
-20.529285	-2.026479	0.935898	0.003955	0.709595
-20.218987	-2.169530	0.940902	0.003897	0.709419
-21.270899	-2.062453	0.945907	0.004093	0.709259
-20.977787	-2.112153	0.950912	0.004039	0.709264
-21.492788	-2.024343	0.955917	0.004134	0.709256
-21.161659	-2.081404	0.960922	0.004073	0.709260
-20.844658	-2.137584	0.965926	0.004014	0.709260
-21.482410	-2.024934	0.970931	0.004132	0.709259
-21.243462	-2.146764	0.975936	0.004088	0.709100
-22.125439	-2.064746	0.980941	0.004252	0.708950
-22.129899	-2.059814	0.985946	0.004253	0.708958
-22.053744	-2.074007	0.990950	0.004239	0.708957
-22.210444	-2.048883	0.995955	0.004268	0.708951
-21.776700	-2.120686	1.000960	0.004187	0.708962
-21.995731	-2.085622	1.005965	0.004228	0.708954
-22.177056	-2.134892	1.010970	0.004261	0.708791
-22.800567	-2.100539	1.015974	0.004377	0.708637
-22.909099	-2.084426	1.020979	0.004398	0.708631
-22.528114	-2.148077	1.025984	0.004327	0.708640
-22.885396	-2.087318	1.030989	0.004393	0.708634
-22.858882	-2.088026	1.035994	0.004388	0.708642
-22.918281	-2.080826	1.040998	0.004399	0.708635
-23.117276	-2.159983	1.046003	0.004436	0.708406
-23.568481	-2.104997	1.051008	0.004520	0.708355
-24.015520	-2.030458	1.056013	0.004603	0.708345
-23.697357	-2.084396	1.061018	0.004544	0.708350
-23.380197	-2.140882	1.066022	0.004485	0.708350
-23.861856	-2.057290	1.071027	0.004575	0.708346
-23.808899	-2.062401	1.076032	0.004565	0.708355
-24.210673	-2.151935	1.081037	0.004640	0.708032
-24.790689	-2.058518	1.086042	0.004748	0.708012
-24.915792	-2.036684	1.091046	0.004771	0.708011
-24.860324	-2.048124	1.096051	0.004760	0.708008
-24.666153	-2.079069	1.101056	0.004724	0.708015
-24.899925	-2.040786	1.106061	0.004768	0.708009
-24.522926	-2.105330	1.111066	0.004697	0.708014
-24.801119	-2.135817	1.116070	0.004749	0.707854
-26.183777	-1.968491	1.121075	0.005007	0.707695
-25.299941	-2.121081	1.126080	0.004842	0.707705
-25.442098	-2.100565	1.131085	0.004868	0.707695
-25.795567	-2.035963	1.136090	0.004934	0.707699
-25.716952	-2.050750	1.141094	0.004920	0.707697
-25.792237	-2.039624	1.146099	0.004934	0.707693
-25.340702	-2.165551	1.151104	0.004850	0.707602
-26.771381	-2.027090	1.156109	0.005116	0.707368
-26.586592	-2.055435	1.161114	0.005081	0.707377
-26.420413	-2.086686	1.166118	0.005050	0.707374
-26.861480	-2.011681	1.171123	0.005132	0.707367
-26.472424	-2.075152	1.176128	0.005060	0.707379
-26.654224	-2.047333	1.181133	0.005094	0.707369
-26.712776	-2.033159	1.186138	0.005105	0.707377
-26.886796	-2.109240	1.191142	0.005137	0.707162
-27.877496	-1.975726	1.196147	0.005321	0.707076
-27.197855	-2.091619	1.201152	0.005195	0.707086
-27.481636	-2.046941	1.206157	0.005248	0.707075
-27.427764	-2.053508	1.211162	0.005238	0.707081
-27.100560	-2.113694	1.216166	0.005177	0.707077
-27.608774	-2.024424	1.221171	0.005271	0.707075
-27.773318	-2.090679	1.226176	0.005302	0.706883
-28.534156	-2.022212	1.231181	0.005443	0.706748
-28.274982	-2.067746	1.236186	0.005395	0.706749
-28.419005	-2.039738	1.241190	0.005422	0.706754
-28.370490	-2.051219	1.246195	0.005413	0.706748
-27.894387	-2.132352	1.251200	0.005324	0.706756
-28.666585	-1.999132	1.256205	0.005468	0.706747
-28.642198	-2.062304	1.261210	0.005463	0.706629
-29.079920	-2.077586	1.266214	0.005545	0.706442
-28.867678	-2.117980	1.271219	0.005505	0.706437
-29.210574	-2.052231	1.276224	0.005569	0.706446
-29.313430	-2.038281	1.281229	0.005588	0.706437
-29.067897	-2.079676	1.286234	0.005542	0.706442
-29.244081	-2.047335	1.291238	0.005575	0.706444
-29.504433	-2.072267	1.296243	0.005624	0.706301
-29.969117	-2.073223	1.301248	0.005710	0.706132
-30.023658	-2.067302	1.306253	0.005720	0.706125
-30.206106	-2.034154	1.311258	0.005754	0.706126
-29.946214	-2.079043	1.316262	0.005706	0.706129
-30.194960	-2.038502	1.321267	0.005752	0.706122
-30.131155	-2.046184	1.326272	0.005740	0.706129
-29.973323	-2.126958	1.331277	0.005711	0.706023
-30.844969	-2.051335	1.336282	0.005873	0.705863
-30.943446	-2.033815	1.341286	0.005891	0.705863
-31.223913	-1.985483	1.346291	0.005943	0.705860
-30.491619	-2.112567	1.351296	0.005807	0.705867
-30.772081	-2.067380	1.356301	0.005859	0.705857
-31.143781	-1.999098	1.361306	0.005928	0.705861
-30.719090	-2.160287	1.366310	0.005849	0.705689
-31.812947	-2.050903	1.371315	0.006053	0.705517
-31.627744	-2.078718	1.376320	0.006018	0.705528
-31.802619	-2.051535	1.381325	0.006051	0.705520
-31.705769	-2.068487	1.386330	0.006033	0.705520
-31.587307	-2.087312	1.391334	0.006011	0.705525
-32.027177	-2.012192	1.396339	0.006093	0.705519
-31.933804	-2.154448	1.401344	0.006075	0.705266
-32.415856	-2.098829	1.406349	0.006165	0.705205
-32.758335	-2.035406	1.411354	0.006229	0.705210
-32.284452	-2.116626	1.416358	0.006140	0.705216
-32.725762	-2.041361	1.421363	0.006223	0.705210
-32.770297	-2.030239	1.426368	0.006231	0.705216
-32.570141	-2.078751	1.431373	0.006194	0.705190
-33.060235	-2.145066	1.436378	0.006285	0.704881
-33.537824	-2.057440	1.441382	0.006374	0.704886
-34.034955	-1.972337	1.446387	0.006466	0.704879
-33.279123	-2.104096	1.451392	0.006325	0.704885
-33.200477	-2.120826	1.456397	0.006311	0.704880
-33.895448	-1.996422	1.461402	0.006440	0.704881
-33.567690	-2.053261	1.466406	0.006379	0.704884
-33.794397	-2.155731	1.471411	0.006421	0.704596
-34.104901	-2.103198	1.476416	0.006479	0.704591
-34.807549	-1.979671	1.481421	0.006610	0.704587
-34.395116	-2.054745	1.486426	0.006533	0.704584
-34.150774	-2.096366	1.491430	0.006487	0.704588
-34.420824	-2.051588	1.496435	0.006538	0.704581
-34.114179	-2.127789	1.501440	0.006481	0.704538
-35.318254	-2.054350	1.506445	0.006705	0.704254
-35.534571	-2.013574	1.511450	0.006745	0.704258
-35.404231	-2.035608	1.516454	0.006721	0.704261
-35.188167	-2.077919	1.521459	0.006680	0.704253
-35.312864	-2.051425	1.526464	0.006703	0.704262
-35.568908	-2.009490	1.531469	0.006751	0.704254
-35.212701	-2.072954	1.536474	0.006685	0.704254
-35.134415	-2.206753	1.541478	0.006670	0.704013
-36.583910	-1.982729	1.546483	0.006940	0.703944
-36.297644	-2.029932	1.551488	0.006887	0.703951
-36.053759	-2.074687	1.556493	0.006841	0.703949
-36.276127	-2.036935	1.561498	0.006883	0.703945
-36.272185	-2.035273	1.566502	0.006882	0.703950
-36.226384	-2.047693	1.571507	0.006873	0.703941
-36.172501	-2.168574	1.576512	0.006863	0.703717
-37.339661	-2.003183	1.581517	0.007080	0.703631
-37.232555	-2.021541	1.586522	0.007060	0.703632
-36.612326	-2.132428	1.591526	0.006945	0.703632
-37.348957	-2.005771	1.596531	0.007082	0.703623
-37.196306	-2.027607	1.601536	0.007054	0.703634
-36.857643	-2.092626	1.606541	0.006991	0.703624
-37.227028	-2.135708	1.611546	0.007059	0.703404
-37.845859	-2.057657	1.616550	0.007174	0.703339
-37.738283	-2.079347	1.621555	0.007154	0.703334
-37.513611	-2.113834	1.626560	0.007113	0.703346
-38.056982	-2.022208	1.631565	0.007214	0.703335
-37.877515	-2.053121	1.636570	0.007180	0.703337
-37.645319	-2.112611	1.641574	0.007137	0.703301
-38.988432	-2.023068	1.646579	0.007387	0.702998
-38.626756	-2.082914	1.651584	0.007320	0.703008
-38.530264	-2.102240	1.656589	0.007302	0.703003
-38.599016	-2.090288	1.661594	0.007314	0.703003
-38.727478	-2.066684	1.666598	0.007338	0.703004
-38.735344	-2.068215	1.671603	0.007340	0.702999
-38.346512	-2.185340	1.676608	0.007267	0.702902
-39.744459	-2.043441	1.681613	0.007527	0.702685
-39.542043	-2.078833	1.686618	0.007490	0.702687
-39.113657	-2.152431	1.691622	0.007410	0.702692
-39.696176	-2.050108	1.696627	0.007518	0.702689
-39.616070	-2.061414	1.701632	0.007503	0.702696
-39.773487	-2.037244	1.706637	0.007533	0.702688
-40.192763	-1.998982	1.711642	0.007611	0.702614
-40.462813	-2.072155	1.716646	0.007661	0.702369
-40.416113	-2.085034	1.721651	0.007652	0.702360
-40.436496	-2.076030	1.726656	0.007656	0.702371
-40.805935	-2.014593	1.731661	0.007725	0.702362
-40.717170	-2.029606	1.736666	0.007708	0.702363
-40.305908	-2.101274	1.741670	0.007632	0.702367
-40.623725	-2.047806	1.746675	0.007691	0.702361
-41.368443	-2.056478	1.751680	0.007829	0.702075
-41.406394	-2.053451	1.756685	0.007836	0.702067
-41.502377	-2.036294	1.761690	0.007854	0.702067
-41.373431	-2.055926	1.766694	0.007830	0.702074
-41.591300	-2.023326	1.771699	0.007871	0.702062
-41.224308	-2.083475	1.776704	0.007802	0.702072
-41.512465	-2.035640	1.781709	0.007856	0.702065
-41.950610	-2.089154	1.786714	0.007938	0.701799
-42.137831	-2.083887	1.791718	0.007972	0.701742
-42.425557	-2.035664	1.796723	0.008026	0.701736
-42.075142	-2.092860	1.801728	0.007961	0.701747
-42.278757	-2.061140	1.806733	0.007998	0.701738
-42.293159	-2.058800	1.811738	0.008001	0.701737
-42.066272	-2.097556	1.816742	0.007959	0.701741
-43.016003	-2.080486	1.821747	0.008136	0.701433
-42.712118	-2.132743	1.826752	0.008079	0.701436
-43.325644	-2.027308	1.831757	0.008193	0.701429
-43.342593	-2.024436	1.836762	0.008196	0.701428
-42.785738	-2.119258	1.841766	0.008093	0.701437
-43.304559	-2.032947	1.846771	0.008189	0.701425
-43.228095	-2.048622	1.851776	0.008175	0.701421
-43.626004	-2.128758	1.856781	0.008249	0.701115
-43.760864	-2.103705	1.861786	0.008274	0.701117
-44.011566	-2.055489	1.866790	0.008321	0.701124
-44.083877	-2.047292	1.871795	0.008334	0.701115
-43.554971	-2.136826	1.876800	0.008236	0.701125
-44.196014	-2.025286	1.881805	0.008355	0.701119
-44.304569	-2.030818	1.886810	0.008375	0.701069
-44.368841	-2.113129	1.891814	0.008387	0.700879
-44.430126	-2.106165	1.896819	0.008398	0.700871
-44.840428	-2.028834	1.901824	0.008475	0.700879
-44.805119	-2.038710	1.906829	0.008468	0.700872
-44.492238	-2.095503	1.911834	0.008410	0.700870
-44.801023	-2.038317	1.916838	0.008467	0.700875
-45.045073	-2.121352	1.921843	0.008513	0.700618
-45.311223	-2.113932	1.926848	0.008562	0.700537
-45.278361	-2.120674	1.931853	0.008556	0.700535
-45.626463	-2.060058	1.936858	0.008621	0.700533
-45.390787	-2.100311	1.941862	0.008577	0.700536
-45.562852	-2.072434	1.946867	0.008609	0.700531
-45.807685	-2.077664	1.951872	0.008655	0.700432
-46.593676	-2.043957	1.956877	0.008801	0.700216
-46.146181	-2.123142	1.961882	0.008717	0.700217
-46.579060	-2.043902	1.966886	0.008798	0.700221
-46.843798	-2.000228	1.971891	0.008847	0.700214
-46.198090	-2.110488	1.976896	0.008727	0.700224
-46.121151	-2.128093	1.981901	0.008713	0.700216
-46.803097	-2.075163	1.986906	0.008840	0.700077
-47.324756	-2.072535	1.991910	0.008937	0.699894
-47.168587	-2.103114	1.996915	0.008908	0.699888
-47.523414	-2.037109	2.001920	0.008974	0.699894

-47.205663	-2.093038	2.011917	0.008914	0.699896
-47.384256	-2.063916	2.021914	0.008948	0.699890
-47.634055	-2.087063	2.031910	0.008994	0.699753
-48.245292	-2.044080	2.041907	0.009108	0.699619
-47.993810	-2.023315	2.051904	0.009061	0.699752
-47.420613	-2.120564	2.061901	0.008954	0.699763
-47.528699	-2.080603	2.071898	0.008974	0.699805
-47.449596	-2.053226	2.081894	0.008959	0.699889
-47.188760	-2.098619	2.091891	0.008911	0.699891
-47.347825	-2.070631	2.101888	0.008940	0.699891
-47.358604	-2.068356	2.111885	0.008942	0.699892
-47.462811	-2.051575	2.121882	0.008961	0.699888
-47.173136	-2.103729	2.131878	0.008907	0.699887
-47.348026	-2.071763	2.141875	0.008940	0.699889
-47.038541	-2.046637	2.151872	0.008882	0.700052
-46.415592	-2.077353	2.161869	0.008766	0.700215
-46.735719	-2.021991	2.171866	0.008826	0.700212
-46.118299	-2.131205	2.181862	0.008711	0.700214
-46.403021	-2.078843	2.191859	0.008764	0.700217
-45.810513	-2.044594	2.201856	0.008653	0.700501
-45.408675	-2.100788	2.211853	0.008578	0.700533
-45.455861	-2.091789	2.221850	0.008587	0.700534
-45.734658	-2.044146	2.231846	0.008639	0.700530
-44.787418	-2.074746	2.241843	0.008462	0.700810
-44.613729	-2.075706	2.251840	0.008430	0.700871
-44.300198	-2.130838	2.261837	0.008372	0.700873
-44.697887	-2.060107	2.271834	0.008445	0.700873
-44.038747	-2.086446	2.281830	0.008323	0.701058
-44.092101	-2.046213	2.291827	0.008333	0.701120
-43.809505	-2.097487	2.301824	0.008280	0.701118
-43.878002	-2.042086	2.311821	0.008293	0.701206
-43.095095	-2.069949	2.321818	0.008147	0.701432
-43.063849	-2.074356	2.331814	0.008141	0.701435
-43.023242	-2.081745	2.341811	0.008133	0.701435
-42.355904	-2.082742	2.351808	0.008009	0.701674
-42.161443	-2.085512	2.361805	0.007973	0.701738
-42.379155	-2.045757	2.371802	0.008013	0.701740
-42.062415	-2.045374	2.381798	0.007954	0.701856
-41.500947	-2.039628	2.391795	0.007849	0.702070
-41.146358	-2.101766	2.401792	0.007783	0.702072
-41.426753	-2.052109	2.411789	0.007835	0.702072
-40.698499	-2.040040	2.421786	0.007700	0.702359
-40.580497	-2.058793	2.431782	0.007678	0.702364
-40.485303	-2.075760	2.441779	0.007660	0.702364
-40.047581	-2.058537	2.451776	0.007578	0.702557
-39.635201	-2.067323	2.461773	0.007501	0.702688
-39.707706	-2.054736	2.471770	0.007515	0.702687
-39.501631	-2.071206	2.481766	0.007476	0.702728
-38.866427	-2.049211	2.491763	0.007358	0.703001
-38.540018	-2.106590	2.501760	0.007297	0.703003
-38.667870	-2.083517	2.511757	0.007321	0.703004
-38.242589	-2.060614	2.521754	0.007242	0.703203
-37.664490	-2.097990	2.531750	0.007134	0.703336
-37.855163	-2.063058	2.541747	0.007169	0.703338
-37.616055	-2.105063	2.551744	0.007125	0.703340
-37.202824	-2.046772	2.561741	0.007048	0.703606
-36.820342	-2.103881	2.571738	0.006977	0.703629
-36.821024	-2.103753	2.581734	0.006977	0.703629
-36.758840	-2.066262	2.591731	0.006965	0.703727
-35.834952	-2.121411	2.601728	0.006793	0.703948
-36.286054	-2.039932	2.611725	0.006877	0.703950
-36.219294	-2.053610	2.621722	0.006864	0.703947
-35.342622	-2.060687	2.631718	0.006701	0.704248
-35.221098	-2.079283	2.641715	0.006678	0.704254
-35.268580	-2.069997	2.651712	0.006687	0.704256
-35.023735	-2.011517	2.661709	0.006641	0.704462
-34.358424	-2.069700	2.671706	0.006517	0.704584
-34.614705	-2.022723	2.681702	0.006565	0.704587
-34.443644	-2.009228	2.691699	0.006533	0.704676
-33.437594	-2.086272	2.701696	0.006346	0.704882
-33.499458	-2.074886	2.711693	0.006357	0.704883
-33.527295	-2.070227	2.721690	0.006362	0.704882
-33.041336	-2.021252	2.731686	0.006272	0.705155
-32.723282	-2.052596	2.741683	0.006212	0.705207
-32.464851	-2.098272	2.751680	0.006164	0.705208
-32.656916	-1.993480	2.761677	0.006200	0.705350
-31.465301	-2.121127	2.771674	0.005978	0.705520
-31.813178	-2.059221	2.781670	0.006043	0.705520
-31.505182	-2.114275	2.791667	0.005985	0.705520
-30.935411	-2.093939	2.801664	0.005879	0.705766
-31.011549	-2.034471	2.811661	0.005893	0.705858
-30.690046	-2.090843	2.821658	0.005833	0.705860
-30.927679	-2.026403	2.831654	0.005877	0.705905
-30.131481	-2.060121	2.841651	0.005729	0.706122
-30.174555	-2.051036	2.851648	0.005737	0.706125
-30.080922	-2.067992	2.861645	0.005719	0.706125
-29.249811	-2.076007	2.871642	0.005565	0.706407
-29.399487	-2.032362	2.881638	0.005592	0.706441
-29.112346	-2.083851	2.891635	0.005539	0.706441
-28.962669	-2.036777	2.901632	0.005511	0.706589
-28.084818	-2.112872	2.911629	0.005347	0.706750
-28.215929	-2.090700	2.921626	0.005372	0.706748
-28.534924	-2.035193	2.931622	0.005431	0.706746
-27.442336	-2.070840	2.941619	0.005228	0.707065
-27.460677	-2.060440	2.951616	0.005231	0.707080
-27.318586	-2.086266	2.961613	0.005204	0.707079
-27.166175	-2.053236	2.971610	0.005176	0.707200
-26.764124	-2.039379	2.981606	0.005101	0.707372
-26.326884	-2.115789	2.991603	0.005020	0.707375
-26.702648	-2.046467	3.001600	0.005089	0.707380
-25.941968	-2.023342	3.011597	0.004948	0.707698
-25.701356	-2.066066	3.021594	0.004903	0.707699
-25.741790	-2.060604	3.031590	0.004910	0.707695
-25.275145	-2.046074	3.041587	0.004823	0.707891
-24.815777	-2.067916	3.051584	0.004738	0.708012
-24.821081	-2.067041	3.061581	0.004739	0.708012
-24.788010	-2.048680	3.071578	0.004732	0.708061
-24.108890	-2.027662	3.081574	0.004606	0.708345
-23.778097	-2.085052	3.091571	0.004544	0.708349
-24.191271	-2.011911	3.101568	0.004621	0.708348
-23.471101	-2.033184	3.111565	0.004487	0.708563
-23.286610	-2.028602	3.121562	0.004452	0.708638
-23.077861	-2.069272	3.131558	0.004414	0.708631
-23.110110	-2.005297	3.141555	0.004419	0.708748
-22.230163	-2.059742	3.151552	0.004256	0.708953
-22.217839	-2.061735	3.161549	0.004253	0.708953
-22.459779	-2.019193	3.171546	0.004298	0.708952
-21.665799	-2.010367	3.181542	0.004150	0.709253
-21.485326	-2.038384	3.191539	0.004117	0.709262
-21.710449	-1.996576	3.201536	0.004158	0.709265
-21.058207	-1.993283	3.211533	0.004037	0.709505
-20.892806	-1.978680	3.221530	0.004006	0.709593
-20.603848	-2.030795	3.231526	0.003952	0.709592
-20.592204	-1.974404	3.241523	0.003950	0.709709
-19.769378	-2.027621	3.251520	0.003797	0.709896
-19.791733	-2.024998	3.261517	0.003801	0.709893
-20.041865	-1.968061	3.271514	0.003847	0.709918
-19.031896	-1.999302	3.281510	0.003659	0.710216
-18.665646	-2.063586	3.291507	0.003591	0.710218
-18.889924	-2.022514	3.301504	0.003632	0.710220
-18.462919	-2.010477	3.311501	0.003553	0.710396
-18.150250	-1.998505	3.321498	0.003495	0.710532
-18.158974	-1.995808	3.331494	0.003496	0.710534
-18.006082	-2.006534	3.341491	0.003468	0.710567
-17.226736	-1.992063	3.351488	0.003322	0.710874
-16.948752	-2.042728	3.361485	0.003271	0.710871
-17.448090	-1.954951	3.371482	0.003363	0.710869
-16.680940	-2.009509	3.381478	0.003221	0.711033
-16.473495	-1.995169	3.391475	0.003182	0.711136
-16.419265	-2.003258	3.401472	0.003172	0.711139
-16.296454	-1.983659	3.411469	0.003149	0.711222
-15.631013	-1.986980	3.421466	0.003025	0.711452
-15.480339	-2.013586	3.431462	0.002997	0.711453
-15.647375	-1.982560	3.441459	0.003028	0.711455
-14.988804	-1.957687	3.451456	0.002905	0.711739
-14.663746	-2.005371	3.461453	0.002844	0.711760
-14.825392	-1.976481	3.471450	0.002874	0.711760
-14.066407	-2.010843	3.481446	0.002733	0.711961
-13.909903	-1.975157	3.491443	0.002704	0.712088
-13.531862	-2.040353	3.501440	0.002633	0.712093
-13.875218	-1.974850	3.511437	0.002697	0.712101
-13.220527	-1.949067	3.521434	0.002575	0.712385
-12.947627	-1.997372	3.531430	0.002524	0.712386
-12.812025	-2.020662	3.541427	0.002499	0.712388
-12.234999	-2.030666	3.551424	0.002391	0.712573
-12.092157	-1.987109	3.561421	0.002365	0.712710
-12.181828	-1.971987	3.571418	0.002381	0.712709
-11.832391	-2.027725	3.581414	0.002316	0.712722
-11.403682	-1.953531	3.591411	0.002236	0.713022
-10.965018	-2.029953	3.601408	0.002155	0.713025
-11.299367	-1.970805	3.611405	0.002217	0.713025
-10.629998	-1.987075	3.621402	0.002092	0.713230
-10.288862	-1.984871	3.631398	0.002028	0.713355
-9.514623	-2.122809	3.641395	0.001884	0.713355
-9.437408	-2.135026	3.651392	0.001870	0.713359
-9.364107	-2.100296	3.661389	0.001856	0.713454
-8.339444	-2.185143	3.671386	0.001665	0.713648
-8.586735	-2.140880	3.681382	0.001711	0.713649
-8.483370	-2.158816	3.691379	0.001692	0.713650
-8.235276	-2.204032	3.701376	0.001646	0.713648
-8.299116	-2.117562	3.711373	0.001657	0.713797
-7.175307	-2.233824	3.721370	0.001448	0.713964
-7.751464	-2.131402	3.731366	0.001555	0.713964
-7.348858	-2.202219	3.741363	0.001480	0.713966
-7.463371	-2.147789	3.751360	0.001502	0.714034
-6.720250	-2.159567	3.761357	0.001363	0.714274
-6.573818	-2.186158	3.771354	0.001336	0.714273
-6.706266	-2.162907	3.781350	0.001360	0.714272
-6.428477	-2.175522	3.791347	0.001309	0.714346
-5.685038	-2.177417	3.801344	0.001170	0.714605
-5.552407	-2.200329	3.811341	0.001145	0.714606
-5.540136	-2.203609	3.821338	0.001143	0.714604
-5.810429	-2.104152	3.831334	0.001193	0.714706
-4.696985	-2.203202	3.841331	0.000986	0.714904
-4.816465	-2.180609	3.851328	0.001008	0.714906
-4.631888	-2.212656	3.861325	0.000974	0.714908
-4.151906	-2.197601	3.871322	0.000884	0.715108
-4.050720	-2.154160	3.881318	0.000865	0.715230
-3.658722	-2.224576	3.891315	0.000792	0.715229
-3.758530	-2.206590	3.901312	0.000811	0.715229
-3.154427	-2.187427	3.911309	0.000698	0.715481
-2.722474	-2.232283	3.921306	0.000618	0.715545
-3.130139	-2.160992	3.931302	0.000693	0.715542
-2.851989	-2.198354	3.941299	0.000642	0.715567
-2.426784	-2.114289	3.951296	0.000562	0.715884
-2.465504	-2.108645	3.961293	0.000569	0.715881
-1.952819	-2.200005	3.971290	0.000474	0.715881
-2.491138	-2.009400	3.981286	0.000574	0.716069
-1.626358	-2.131998	3.991283	0.000413	0.716132
-1.730129	-2.111808	4.001280	0.000432	0.716135
-1.681353	-1.974803	4.011277	0.000423	0.716424
-1.060232	-2.074029	4.021274	0.000307	0.716446
-2.539243	-1.752303	4.031270	0.000582	0.716562
-1.520310	-1.838451	4.041267	0.000393	0.716751
-1.001417	-1.891265	4.051264	0.000296	0.716829
-1.113057	-1.744464	4.061261	0.000317	0.717081
-0.814701	-1.785788	4.071258	0.000261	0.717104
-1.427162	-1.541038	4.081254	0.000375	0.717373
-1.034538	-1.552468	4.091251	0.000302	0.717488
-1.067448	-1.438119	4.101248	0.000308	0.717703
-0.999887	-1.350137	4.111245	0.000295	0.717901
-0.779995	-1.326365	4.121242	0.000254	0.718025
-0.292538	-1.250403	4.131238	0.000163	0.718347
-0.706383	-1.114349	4.141235	0.000240	0.718470
-0.585464	-1.050292	4.151232	0.000217	0.718639
-0.341128	-0.935401	4.161229	0.000172	0.718952
-0.521028	-0.810776	4.171226	0.000205	0.719135
-0.413024	-0.720957	4.181222	0.000185	0.719350
-0.160577	-0.640733	4.191219	0.000138	0.719597
-0.108226	-0.503216	4.201216	0.000128	0.719887
-0.145286	-0.371578	4.211213	0.000134	0.720133
-0.374544	-0.198287	4.221210	0.000177	0.720394
-0.358599	-0.051544	4.231206	0.000174	0.720689
-0.347427	0.088604	4.241203	0.000172	0.720969
0.000000	0.187953	4.251200	0.000107	0.721286

0.182776	0.792774	4.256205	0.000072	0.722538
0.083483	2.082038	4.261210	0.000090	0.725031
0.600892	3.851526	4.266214	-0.000008	0.728664
0.704363	6.243404	4.271219	-0.000029	0.733341
0.914913	9.132004	4.276224	-0.000070	0.738979
1.093167	12.495056	4.281229	-0.000105	0.745467
1.426312	16.290497	4.286234	-0.000170	0.752766
1.564639	20.524891	4.291238	-0.000198	0.760749
1.788475	25.130478	4.296243	-0.000243	0.769362
2.233470	30.076029	4.301248	-0.000329	0.778571
2.789032	35.340437	4.306253	-0.000436	0.788280
2.946525	40.998244	4.311258	-0.000469	0.798446
3.189303	46.939818	4.316262	-0.000518	0.809007
3.571886	53.133734	4.321267	-0.000593	0.819912
4.048900	59.591832	4.326272	-0.000686	0.831153
4.264926	66.309940	4.331277	-0.000731	0.842604
4.834084	73.188562	4.336282	-0.000842	0.854271
5.036938	80.342058	4.341286	-0.000884	0.866125
5.203676	87.673973	4.346291	-0.000920	0.878097
5.856100	95.106239	4.351296	-0.001046	0.890203
6.286198	102.728603	4.356301	-0.001131	0.902385
7.052011	110.448168	4.361306	-0.001279	0.914646
8.361115	118.197975	4.366310	-0.001528	0.926936
8.839767	126.219415	4.371315	-0.001622	0.939255
9.309538	134.351921	4.376320	-0.001715	0.951577
10.083450	142.507560	4.381325	-0.001865	0.963854
10.939140	150.749256	4.386330	-0.002029	0.976122
11.582833	159.105047	4.391334	-0.002155	0.988348
12.214653	167.514834	4.396339	-0.002278	1.000498
12.793101	175.976120	4.401344	-0.002391	1.012560
13.337882	184.478720	4.406349	-0.002498	1.024529
13.787771	193.042050	4.411354	-0.002587	1.036421
14.479452	201.589115	4.416358	-0.002722	1.048212
15.109220	210.173528	4.421363	-0.002845	1.059906
15.872734	218.779193	4.426368	-0.002993	1.071532
16.236791	227.429418	4.431373	-0.003066	1.083000
16.691295	236.086979	4.436378	-0.003156	1.094378
17.350976	244.719658	4.441382	-0.003285	1.105652
17.793236	253.383427	4.446387	-0.003373	1.116804
18.266741	262.038903	4.451392	-0.003467	1.127841
18.860950	270.675184	4.456397	-0.003583	1.138773
19.430037	279.318111	4.461402	-0.003695	1.149604
20.050307	287.947822	4.466406	-0.003816	1.160328
20.730008	296.523062	4.471411	-0.003948	1.170899
21.243027	305.132505	4.476416	-0.004049	1.181383
21.607298	313.762706	4.481421	-0.004123	1.191769
22.045008	322.351295	4.486426	-0.004210	1.202030
22.861643	330.885660	4.491430	-0.004367	1.212216
23.465767	339.430728	4.496435	-0.004486	1.222288
23.946394	348.016043	4.501440	-0.004581	1.232299
24.616631	356.527710	4.506445	-0.004711	1.242182
25.047386	365.080424	4.511450	-0.004797	1.251987
26.019519	373.524916	4.516454	-0.004983	1.261696
26.511246	382.041528	4.521459	-0.005081	1.271322
26.900658	390.567610	4.526464	-0.005159	1.280866
27.208764	399.085134	4.531469	-0.005222	1.290315
27.840636	407.529757	4.536474	-0.005345	1.299674
28.495790	416.014889	4.541478	-0.005472	1.309015
29.085351	424.538380	4.546483	-0.005588	1.318319
29.656945	432.938483	4.551488	-0.005700	1.327422
29.890928	441.396752	4.556493	-0.005749	1.336465
30.664310	449.745698	4.561498	-0.005898	1.345426
31.049407	458.181018	4.566502	-0.005976	1.354351
31.374520	466.576704	4.571507	-0.006042	1.363165
31.716735	474.981288	4.576512	-0.006111	1.371935
32.204880	483.336033	4.581517	-0.006207	1.380623
32.586835	491.717199	4.586522	-0.006284	1.389265
33.087128	500.077862	4.591526	-0.006382	1.397852
33.462456	508.403669	4.596531	-0.006458	1.406331
33.897412	516.756161	4.601536	-0.006544	1.414795
34.298631	525.080010	4.606541	-0.006624	1.423175
35.005908	533.364584	4.611546	-0.006762	1.431517
35.342683	541.711434	4.616550	-0.006830	1.439812
35.631226	550.030544	4.621555	-0.006889	1.448023
36.175882	558.331340	4.626560	-0.006996	1.456212
36.685290	566.620630	4.631565	-0.007096	1.464338
37.166334	574.948410	4.636570	-0.007191	1.472451
37.551331	583.247421	4.641574	-0.007268	1.480477
37.915735	591.526235	4.646579	-0.007342	1.488437
38.072160	599.848811	4.651584	-0.007376	1.496364
38.517729	608.094028	4.656589	-0.007464	1.504221
39.063477	616.346005	4.661594	-0.007571	1.512058
39.574965	624.585359	4.666598	-0.007672	1.519838
39.965068	632.831013	4.671603	-0.007750	1.527565
40.318385	641.104657	4.676608	-0.007821	1.535274
40.697692	649.363650	4.681613	-0.007897	1.542935
41.049715	657.616032	4.686618	-0.007968	1.550547
41.654620	665.847931	4.691622	-0.008086	1.558141
41.856820	674.081701	4.696627	-0.008130	1.565640
42.046561	682.368531	4.701632	-0.008170	1.573149
42.575407	690.558894	4.706637	-0.008274	1.580586
43.036100	698.768168	4.711642	-0.008365	1.587994
43.201793	707.050822	4.716646	-0.008402	1.595391
43.572477	715.239114	4.721651	-0.008476	1.602699
44.113213	723.441699	4.726656	-0.008582	1.610011
44.343980	731.684702	4.731661	-0.008630	1.617281
44.676545	739.876868	4.736666	-0.008698	1.624488
45.113999	748.113524	4.741670	-0.008785	1.631717
45.183942	756.365575	4.746675	-0.008803	1.638876
45.611121	764.522517	4.751680	-0.008888	1.645972
45.972287	772.719676	4.756685	-0.008961	1.653062
46.478529	780.857144	4.761690	-0.009060	1.660090
46.722401	789.073212	4.766694	-0.009111	1.667120
46.953324	797.279106	4.771699	-0.009159	1.674110
47.423015	805.431554	4.776704	-0.009252	1.681058
47.848981	813.596550	4.781709	-0.009337	1.687981
48.091518	821.797108	4.786714	-0.009387	1.694882
48.473646	829.977471	4.791718	-0.009464	1.701756
48.638653	838.175323	4.796723	-0.009500	1.708589
49.106729	846.353371	4.801728	-0.009592	1.715417
49.369210	854.511850	4.806733	-0.009647	1.722175
49.771086	862.657166	4.811738	-0.009727	1.728914
50.255111	870.827559	4.816742	-0.009822	1.735658
50.436306	878.998031	4.821747	-0.009861	1.742337
50.690727	887.179173	4.826752	-0.009914	1.749008
51.046157	895.347811	4.831757	-0.009986	1.755657
51.165319	903.510308	4.836762	-0.010013	1.762245
51.685197	911.645715	4.841766	-0.010115	1.768838
52.204920	919.769589	4.846771	-0.010218	1.775396
52.391396	927.946805	4.851776	-0.010258	1.781932
52.876976	936.076074	4.856781	-0.010353	1.788442
53.160325	944.299872	4.861786	-0.010412	1.794978
53.575930	952.415940	4.866790	-0.010494	1.801422
53.715901	960.572664	4.871795	-0.010526	1.807842
54.158685	968.713357	4.876800	-0.010613	1.814262
54.355693	976.857061	4.881805	-0.010655	1.820633
54.677948	984.973558	4.886810	-0.010721	1.826975
55.224970	993.121575	4.891814	-0.010828	1.833346
55.561120	1001.246552	4.896819	-0.010896	1.839653
56.064855	1009.359170	4.901824	-0.010995	1.845948
56.394202	1017.520999	4.906829	-0.011062	1.852238
56.696374	1025.667343	4.911834	-0.011123	1.858492
56.910433	1033.815657	4.916838	-0.011169	1.864717
57.079824	1041.974529	4.921843	-0.011205	1.870923
57.453200	1050.119629	4.926848	-0.011280	1.877122
57.959567	1058.195997	4.931853	-0.011380	1.883264
57.902889	1066.354888	4.936858	-0.011375	1.889383
58.237171	1074.497934	4.941862	-0.011442	1.895515
58.451444	1082.612528	4.946867	-0.011488	1.901593
58.691929	1090.752900	4.951872	-0.011538	1.907673
58.827273	1098.907764	4.956877	-0.011568	1.913733
59.208862	1106.979878	4.961882	-0.011645	1.919740
59.573037	1115.096817	4.966886	-0.011718	1.925759
59.602300	1123.250597	4.971891	-0.011728	1.931750
60.004583	1131.349864	4.976896	-0.011809	1.937723
60.466006	1139.444175	4.981901	-0.011900	1.943680
60.607634	1147.579316	4.986906	-0.011932	1.949614
60.915512	1155.745708	4.991910	-0.011994	1.955570
61.215412	1163.810486	4.996915	-0.012055	1.961434
61.631714	1171.894840	5.001920	-0.012138	1.967308
61.860044	1180.028327	5.006925	-0.012186	1.973178
62.237530	1188.117314	5.011930	-0.012262	1.979015
62.492450	1196.235657	5.016934	-0.012315	1.984843
62.536465	1204.367347	5.021939	-0.012328	1.990641
62.797373	1212.488592	5.026944	-0.012382	1.996438
63.097482	1220.566722	5.031949	-0.012443	2.002191
63.327076	1228.661984	5.036954	-0.012491	2.007932
63.646690	1236.801486	5.041958	-0.012556	2.013698
63.911940	1244.876243	5.046963	-0.012611	2.019395
64.203188	1252.970650	5.051968	-0.012670	2.025094
64.272048	1261.131644	5.056973	-0.012688	2.030799
64.297449	1269.261449	5.061978	-0.012699	2.036463
64.756505	1277.316398	5.066982	-0.012789	2.042103
64.963432	1285.403935	5.071987	-0.012833	2.047724
65.130071	1293.538576	5.076992	-0.012869	2.053358
65.658394	1301.590313	5.081997	-0.012973	2.058956
66.020683	1309.653634	5.087002	-0.013046	2.064531
65.993622	1317.819195	5.092006	-0.013046	2.070121
66.262429	1325.906693	5.097011	-0.013102	2.075672
66.625523	1333.960808	5.102016	-0.013174	2.081195
66.775949	1342.072156	5.107021	-0.013208	2.086721
66.962485	1350.190208	5.112026	-0.013248	2.092241
67.428346	1358.278701	5.117030	-0.013340	2.097753
67.655147	1366.365512	5.122035	-0.013387	2.103226
68.033502	1374.468162	5.127040	-0.013463	2.108711
68.388349	1382.633140	5.132045	-0.013535	2.114220
68.407857	1390.708245	5.137050	-0.013544	2.119623
68.483068	1398.796895	5.142054	-0.013563	2.125026
68.840263	1406.850599	5.147059	-0.013635	2.130420
69.116209	1414.936440	5.152064	-0.013691	2.135813
69.467895	1422.988164	5.157069	-0.013762	2.141177
69.543841	1431.089464	5.162074	-0.013782	2.146535
70.011643	1439.171843	5.167078	-0.013874	2.151903
70.160779	1447.251101	5.172083	-0.013907	2.157226
70.430239	1455.318724	5.177088	-0.013963	2.162540
70.788093	1463.393808	5.182093	-0.014034	2.167853
71.283620	1471.459087	5.187098	-0.014132	2.173160
71.412200	1479.580525	5.192102	-0.014161	2.178456
71.664635	1487.639489	5.197107	-0.014214	2.183711
71.915010	1495.736941	5.202112	-0.014266	2.188977
72.047178	1503.899857	5.207117	-0.014296	2.194262
72.170815	1511.955235	5.212122	-0.014324	2.199464
72.625765	1519.985698	5.217126	-0.014414	2.204668
72.835776	1528.075366	5.222131	-0.014458	2.209876
73.220239	1536.150691	5.227136	-0.014535	2.215078
73.447966	1544.231088	5.232141	-0.014583	2.220256
73.599457	1552.300005	5.237146	-0.014616	2.225409
73.900588	1560.396531	5.242150	-0.014678	2.230580
74.215570	1568.474637	5.247155	-0.014742	2.235729
74.648812	1576.517268	5.252160	-0.014828	2.240854
74.982189	1584.586629	5.257165	-0.014895	2.245975
75.071782	1592.697966	5.262170	-0.014917	2.251089
75.479459	1600.771112	5.267174	-0.014998	2.256196
75.689086	1608.833775	5.272179	-0.015042	2.261267
75.733377	1616.944645	5.277184	-0.015056	2.266343
75.969030	1625.071516	5.282189	-0.015105	2.271434
76.330763	1633.147884	5.287194	-0.015178	2.276492
76.726398	1641.182697	5.292198	-0.015257	2.281517
76.921785	1649.223308	5.297203	-0.015299	2.286517
77.152885	1657.307323	5.302208	-0.015347	2.291536
77.349072	1665.386940	5.307213	-0.015389	2.296538
77.371122	1673.462059	5.312218	-0.015398	2.301511
77.648503	1681.536421	5.317222	-0.015455	2.306495
77.957279	1689.595089	5.322227	-0.015518	2.311461
77.974363	1697.698457	5.327232	-0.015526	2.316420
78.099789	1705.762933	5.332237	-0.015555	2.321353
78.640534	1713.764644	5.337242	-0.015661	2.326272
78.708182	1721.882843	5.342246	-0.015679	2.331212
78.880591	1729.952022	5.347251	-0.015716	2.336120
79.140201	1738.008123	5.352256	-0.015770	2.341017
79.520684	1746.067986	5.357261	-0.015846	2.345917
79.631636	1754.151149	5.362266	-0.015872	2.350798
80.058979	1762.237755	5.367270	-0.015957	2.355696
80.337413	1770.271529	5.372275	-0.016014	2.360541
80.560949	1778.325497	5.377280	-0.016061	2.365383
81.035050	1786.380156	5.382285	-0.016154	2.370236
81.233974	1794.450678	5.387290	-0.016197	2.375066
81.638132	1802.507324	5.392294	-0.016277	2.379894
81.665050	1810.579913	5.397299	-0.016288	2.384693
81.995144	1818.648221	5.402304	-0.016354	2.389502
82.286667	1826.742663	5.407309	-0.016414	2.394315
82.462151	1834.783089	5.412314	-0.016452	2.399077
82.813077	1842.833195	5.417318	-0.016523	2.403849
82.877952	1850.923805	5.422323	-0.016540	2.408612
82.998072	1859.001580	5.427328	-0.016568	2.413363
83.109509	1867.091982	5.432333	-0.016594	2.418112
83.569496	1875.085095	5.437338	-0.016685	2.422821
83.792321	1883.175528	5.442342	-0.016731	2.427559
83.823613	1891.313943	5.447347	-0.016743	2.432302
84.305214	1899.346220	5.452352	-0.016837	2.437008
85.343367	1907.302968	5.457357	-0.017036	2.441703
85.349659	1915.370452	5.462362	-0.017042	2.446375
85.769788	1923.443076	5.467366	-0.017126	2.451072
86.114155	1931.495626	5.472371	-0.017195	2.455743
86.408810	1939.548808	5.477376	-0.017256	2.460402
86.374956	1947.662046	5.482381	-0.017255	2.465061
86.561160	1955.719661	5.487386	-0.017295	2.469696
86.956658	1963.785996	5.492390	-0.017373	2.474343
87.162273	1971.823568	5.497395	-0.017417	2.478951
87.338896	1979.862196	5.502400	-0.017455	2.483549
87.759377	1987.918497	5.507405	-0.017539	2.488166
87.729099	1996.012988	5.512410	-0.017538	2.492763
88.042793	2004.066327	5.517414	-0.017602	2.497353
88.239783	2012.124379	5.522419	-0.017644	2.501929
88.580667	2020.156078	5.527424	-0.017713	2.506493
88.985660	2028.236207	5.532429	-0.017794	2.511079
89.297368	2036.306464	5.537434	-0.017857	2.515646
89.693938	2044.339820	5.542438	-0.017936	2.520189
89.798423	2052.391684	5.547443	-0.017961	2.524713
90.062320	2060.448814	5.552448	-0.018015	2.529243
90.081946	2068.561578	5.557453	-0.018024	2.533779
90.468171	2076.550815	5.562458	-0.018101	2.538264
90.761181	2084.600253	5.567462	-0.018161	2.542768
90.944743	2092.675554	5.572467	-0.018201	2.547271
91.256127	2100.731851	5.577472	-0.018264	2.551764
91.484038	2108.823292	5.582477	-0.018312	2.556263
91.698054	2116.850379	5.587482	-0.018357	2.560717
91.962482	2124.905299	5.592486	-0.018411	2.565182
92.067412	2132.966786	5.597491	-0.018436	2.569632
92.232283	2141.028514	5.602496	-0.018472	2.574079
92.663567	2149.070751	5.607501	-0.018558	2.578525
92.723534	2157.113402	5.612506	-0.018574	2.582938
93.052356	2165.170937	5.617510	-0.018641	2.587371
92.955344	2173.355340	5.622515	-0.018628	2.591836
93.349068	2181.460899	5.627520	-0.018707	2.596284
93.796481	2189.406612	5.632525	-0.018795	2.600640
95.265740	2197.247674	5.637530	-0.019074	2.605002
96.708766	2205.194138	5.642534	-0.019348	2.609412
97.149309	2213.309847	5.647539	-0.019435	2.613838
97.532363	2221.374209	5.652544	-0.019512	2.618224
98.137141	2229.432959	5.657549	-0.019630	2.622615
98.169886	2237.511726	5.662554	-0.019641	2.626972
98.530276	2245.627334	5.667558	-0.019713	2.631362
98.856373	2253.679224	5.672563	-0.019779	2.635709
99.299427	2261.695246	5.677568	-0.019867	2.640037
99.417057	2269.771418	5.682573	-0.019894	2.644369
99.607416	2277.807849	5.687578	-0.019935	2.648677
99.696646	2285.925503	5.692582	-0.019957	2.653014
99.906265	2293.971983	5.697587	-0.020001	2.657315
100.551860	2301.964853	5.702592	-0.020127	2.661608
100.848073	2310.029522	5.707597	-0.020187	2.665910
101.010294	2318.086589	5.712602	-0.020223	2.670192
101.343221	2326.183752	5.717606	-0.020290	2.674500
101.590594	2334.199318	5.722611	-0.020341	2.678752
101.841050	2342.225029	5.727616	-0.020393	2.683002
101.642631	2350.342255	5.732621	-0.020362	2.687266
102.340416	2358.304591	5.737626	-0.020497	2.691498
102.778107	2366.374314	5.742630	-0.020584	2.695763
102.916069	2374.412720	5.747635	-0.020615	2.699986
103.164204	2382.444586	5.752640	-0.020666	2.704206
103.457060	2390.521445	5.757645	-0.020726	2.708446
103.726580	2398.573817	5.762650	-0.020781	2.712665
103.997415	2406.632136	5.767654	-0.020837	2.716880
104.282229	2414.648609	5.772659	-0.020895	2.721068
104.444813	2422.682554	5.777664	-0.020931	2.725251
104.678339	2430.758455	5.782669	-0.020980	2.729453
104.683850	2438.828186	5.787674	-0.020986	2.733632
105.100715	2446.873553	5.792678	-0.021069	2.737817
105.460781	2454.896442	5.797683	-0.021141	2.741981
105.611751	2462.941921	5.802688	-0.021175	2.746137
105.992363	2471.024778	5.807693	-0.021251	2.750319
106.187433	2479.150551	5.812698	-0.021292	2.754507
106.303810	2487.158008	5.817702	-0.021319	2.758622
106.585051	2495.149589	5.822707	-0.021377	2.762733
107.083997	2503.136256	5.827712	-0.021475	2.766849
107.341991	2511.204914	5.832717	-0.021528	2.770985
107.684650	2519.236678	5.837722	-0.021598	2.775102
108.094584	2527.246951	5.842726	-0.021679	2.779205
108.626091	2535.253294	5.847731	-0.021783	2.783308
108.607946	2543.335690	5.852736	-0.021785	2.787411
108.934651	2551.402889	5.857741	-0.021851	2.791520
109.211712	2559.454594	5.862746	-0.021908	2.795612
109.398516	2567.488532	5.867750	-0.021948	2.799684
109.512399	2575.544560	5.872755	-0.021975	2.803757
109.723489	2583.568929	5.877760	-0.022019	2.807814
110.219824	2591.611294	5.882765	-0.022117	2.811890
110.587223	2599.672353	5.887770	-0.022191	2.815963
110.987418	2607.704799	5.892774	-0.022271	2.820017
111.355203	2615.732171	5.897779	-0.022344	2.824060
111.253393	2623.820593	5.902784	-0.022331	2.828102
111.561109	2631.899419	5.907789	-0.022393	2.832156
111.758927	2639.936152	5.912794	-0.022435	2.836177
112.098972	2647.940007	5.917798	-0.022504	2.840184
112.283651	2655.950401	5.922803	-0.022544	2.844180
112.826357	2663.938491	5.927808	-0.022650	2.848179
113.278387	2672.024576	5.932813	-0.022739	2.852216
113.341207	2680.094462	5.937818	-0.022756	2.856218
113.617590	2688.124462	5.942822	-0.022813	2.860206
113.740488	2696.155287	5.947827	-0.022841	2.864180
113.844535	2704.201360	5.952832	-0.022866	2.868155
114.410941	2712.247998	5.957837	-0.022977	2.872151
114.922414	2720.263414	5.962842	-0.023077	2.876122
114.997273	2728.314218	5.967846	-0.023096	2.880082
115.146945	2736.334047	5.972851	-0.023129	2.884025
115.397837	2744.382994	5.977856	-0.023181	2.887982
115.848526	2752.459212	5.982861	-0.023271	2.891958
116.053600	2760.522278	5.987866	-0.023314	2.895908
116.205944	2768.564540	5.992870	-0.023348	2.899840
116.406027	2776.597778	5.997875	-0.023390	2.903765
116.841888	2784.617884	6.002880	-0.023477	2.907691
117.333760	2792.705903	6.007885	-0.023574	2.911648
117.570827	2800.782383	6.012890	-0.023623	2.915580
117.906837	2808.760395	6.017894	-0.023691	2.919464
117.939312	2816.787028	6.022899	-0.023702	2.923350
118.386365	2824.783503	6.027904	-0.023791	2.927238
118.704320	2832.822442	6.032909	-0.023855	2.931135
118.876872	2840.877101	6.037914	-0.023893	2.935027
119.312280	2848.876934	6.042918	-0.023979	2.938901
119.716999	2856.898697	6.047923	-0.024060	2.942778
119.860468	2864.942691	6.052928	-0.024092	2.946648
120.089757	2873.018671	6.057933	-0.024140	2.950532
120.281362	2881.074919	6.062938	-0.024181	2.954399
120.748716	2889.079410	6.067942	-0.024273	2.958251
120.825491	2897.136664	6.072947	-0.024292	2.962103
121.243312	2905.135032	6.077952	-0.024375	2.965939
121.486377	2913.189631	6.082957	-0.024426	2.969788
121.391836	2921.259465	6.087962	-0.024414	2.973623
121.854128	2929.291959	6.092966	-0.024505	2.977462
122.049837	2937.347070	6.097971	-0.024547	2.981294
122.215303	2945.349295	6.102976	-0.024583	2.985095
122.611078	2953.403985	6.107981	-0.024662	2.988927
122.757417	2961.462662	6.112986	-0.024694	2.992743
123.206586	2969.483075	6.117990	-0.024783	2.996552
123.483073	2977.520936	6.122995	-0.024840	3.000355
123.622825	2985.519225	6.128000	-0.024871	3.004128
124.021174	2993.560852	6.133005	-0.024951	3.007929
124.120929	3001.605696	6.138010	-0.024975	3.011712
124.628929	3009.636501	6.143014	-0.025074	3.015504
124.895988	3017.650923	6.148019	-0.025129	3.019272
125.116957	3025.656287	6.153024	-0.025176	3.023028
125.312990	3033.761241	6.158029	-0.025218	3.026825
125.690525	3041.765197	6.163034	-0.025293	3.030579
125.855138	3049.842308	6.168038	-0.025329	3.034352
126.161860	3057.868511	6.173043	-0.025391	3.038104
126.437363	3065.873099	6.178048	-0.025448	3.041839
126.905925	3073.906724	6.183053	-0.025541	3.045592
126.818110	3081.948675	6.188058	-0.025529	3.049318
127.006847	3090.027225	6.193062	-0.025570	3.053069
127.272773	3098.058590	6.198067	-0.025625	3.056798
127.585385	3106.067397	6.203072	-0.025688	3.060514
127.736858	3114.096522	6.208077	-0.025722	3.064227
127.919020	3122.133689	6.213082	-0.025761	3.067940
128.450878	3130.200639	6.218086	-0.025865	3.071679
128.579245	3138.319483	6.223091	-0.025894	3.075419
128.742918	3146.298463	6.228096	-0.025930	3.079091
129.080030	3154.309634	6.233101	-0.025998	3.082782
129.451159	3162.287598	6.238106	-0.026072	3.086455
129.671746	3170.338260	6.243110	-0.026119	3.090149
129.828412	3178.410593	6.248115	-0.026153	3.093847
129.993633	3186.437754	6.253120	-0.026189	3.097519
130.382161	3194.444554	6.258125	-0.026267	3.101188
130.785985	3202.419040	6.263130	-0.026347	3.104839
131.137676	3210.482504	6.268134	-0.026418	3.108523
131.137385	3218.581954	6.273139	-0.026423	3.112203
131.133264	3226.645262	6.278144	-0.026428	3.115862
131.428427	3234.631760	6.283149	-0.026488	3.119496
131.514657	3242.648480	6.288154	-0.026509	3.123130
131.751777	3250.676206	6.293158	-0.026559	3.126771
131.917826	3258.717682	6.298163	-0.026595	3.130411
132.356111	3266.737572	6.303168	-0.026682	3.134049
132.814000	3274.781713	6.308173	-0.026772	3.137694
132.876399	3282.799399	6.313178	-0.026789	3.141306
133.407583	3290.774775	6.318182	-0.026893	3.144916
133.762078	3298.849238	6.323187	-0.026965	3.148557
133.660245	3306.940247	6.328192	-0.026951	3.152182
134.019361	3314.985787	6.333197	-0.027023	3.155803
134.080829	3322.962948	6.338202	-0.027040	3.159376
134.358580	3330.965191	6.343206	-0.027097	3.162965
134.783487	3339.016265	6.348211	-0.027181	3.166579
134.876742	3347.054228	6.353216	-0.027204	3.170168
135.077316	3355.137966	6.358221	-0.027247	3.173778
135.332955	3363.110582	6.363226	-0.027299	3.177336
135.656303	3371.169386	6.368230	-0.027365	3.180932
135.932753	3379.161774	6.373235	-0.027422	3.184493
135.902680	3387.244745	6.378240	-0.027421	3.188076
136.226261	3395.293112	6.383245	-0.027487	3.191655
136.782414	3403.271303	6.388250	-0.027596	3.195209
136.837532	3411.318393	6.393254	-0.027611	3.198768
137.017254	3419.349193	6.398259	-0.027650	3.202321
137.189805	3427.355690	6.403264	-0.027687	3.205859
137.506232	3435.385869	6.408269	-0.027752	3.209410
137.586459	3443.441027	6.413274	-0.027772	3.212958
137.826004	3451.490829	6.418278	-0.027822	3.216506
138.230232	3459.525615	6.423283	-0.027902	3.220050
138.283160	3467.513407	6.428288	-0.027917	3.223556
138.811627	3475.550230	6.433293	-0.028021	3.227098
139.148489	3483.587652	6.438298	-0.028089	3.230629
139.287701	3491.710363	6.443302	-0.028120	3.234186
139.479171	3499.681984	6.448307	-0.028161	3.237674
139.814218	3507.680476	6.453312	-0.028229	3.241176
140.198156	3515.707635	6.458317	-0.028306	3.244689
140.212059	3523.744904	6.463322	-0.028313	3.248188
140.326219	3531.772257	6.468326	-0.028340	3.251682
140.759053	3539.807723	6.473331	-0.028426	3.255189
140.910992	3547.819569	6.478336	-0.028459	3.258671
141.298004	3555.874007	6.483341	-0.028537	3.262177
141.511132	3563.888997	6.488346	-0.028582	3.265654
141.746726	3571.896143	6.493350	-0.028631	3.269126
141.826143	3579.988348	6.498355	-0.028651	3.272625
141.976348	3588.024182	6.503360	-0.028684	3.276098
142.103674	3596.009825	6.508365	-0.028713	3.279545
142.104408	3604.037166	6.513370	-0.028718	3.283001
142.420712	3612.053898	6.518374	-0.028783	3.286462
142.765641	3620.081021	6.523379	-0.028852	3.289924
142.749861	3628.152141	6.528384	-0.028854	3.293388
143.212136	3636.170623	6.533389	-0.028946	3.296843
143.426587	3644.166711	6.538394	-0.028991	3.300276
143.780969	3652.202530	6.543398	-0.029062	3.303728
144.172915	3660.220926	6.548403	-0.029140	3.307170
144.084615	3668.262813	6.553408	-0.029129	3.310600
144.415924	3676.352640	6.558413	-0.029196	3.314063
144.402754	3684.366517	6.563418	-0.029199	3.317477
144.590920	3692.361308	6.568422	-0.029239	3.320887
145.024871	3700.347137	6.573427	-0.029325	3.324298
145.069892	3708.378563	6.578432	-0.029339	3.327711
145.222345	3716.427232	6.583437	-0.029373	3.331132
145.580998	3724.451444	6.588442	-0.029445	3.334547
145.835588	3732.476931	6.593446	-0.029497	3.337954
145.937751	3740.537340	6.598451	-0.029522	3.341368
146.302097	3748.518172	6.603456	-0.029595	3.344754
146.620941	3756.580040	6.608461	-0.029660	3.348168
146.751203	3764.628866	6.613466	-0.029689	3.351567
146.828830	3772.678619	6.618470	-0.029709	3.354961
147.228805	3780.685748	6.623475	-0.029789	3.358345
147.435861	3788.714043	6.628480	-0.029832	3.361728
147.709348	3796.767138	6.633485	-0.029889	3.365120
148.041262	3804.736383	6.638490	-0.029956	3.368476
148.152741	3812.784751	6.643494	-0.029982	3.371853
147.998118	3820.875883	6.648499	-0.029958	3.375235
148.452859	3828.846292	6.653504	-0.030048	3.378586
148.790097	3836.854994	6.658509	-0.030116	3.381944
148.688263	3844.897796	6.663514	-0.030102	3.385298
148.841861	3852.918705	6.668518	-0.030136	3.388649
149.134086	3861.003417	6.673523	-0.030196	3.392027
149.361324	3869.036513	6.678528	-0.030244	3.395379
149.664980	3877.040447	6.683533	-0.030305	3.398718
149.708497	3885.041099	6.688538	-0.030319	3.402043
149.792707	3893.040185	6.693542	-0.030340	3.405365
150.125336	3901.063340	6.698547	-0.030407	3.408703
150.193102	3909.108253	6.703552	-0.030425	3.412037
150.423899	3917.164911	6.708557	-0.030473	3.415379
150.712022	3925.145488	6.713562	-0.030532	3.418687
150.781009	3933.182288	6.718566	-0.030550	3.422008
151.077269	3941.177171	6.723571	-0.030610	3.425317
151.347782	3949.204023	6.728576	-0.030666	3.428634
151.527746	3957.278068	6.733581	-0.030705	3.431965
151.775190	3965.312766	6.738586	-0.030756	3.435278
151.860109	3973.329841	6.743590	-0.030777	3.438576
151.941355	3981.370936	6.748595	-0.030798	3.441880
152.159681	3989.382777	6.753600	-0.030844	3.445173
152.464540	3997.406054	6.758605	-0.030906	3.448471
152.577172	4005.461854	6.763610	-0.030932	3.451772
152.681573	4013.481793	6.768614	-0.030957	3.455056
153.081435	4021.510115	6.773619	-0.031036	3.458349
153.074470	4029.521536	6.778624	-0.031040	3.461619
153.266694	4037.558293	6.783629	-0.031081	3.464903
153.718271	4045.556763	6.788634	-0.031171	3.468176
153.676713	4053.683628	6.793638	-0.031168	3.471483
153.814358	4061.704136	6.798643	-0.031199	3.474749
154.285727	4069.620467	6.803648	-0.031292	3.477980
154.746076	4077.665308	6.808653	-0.031383	3.481260
154.969341	4085.639599	6.813658	-0.031430	3.484501
155.091890	4093.676380	6.818662	-0.031458	3.487760
155.185730	4101.738431	6.823667	-0.031481	3.491026
155.500702	4109.757555	6.828672	-0.031545	3.494279
155.681261	4117.792480	6.833677	-0.031584	3.497530
155.714510	4125.834065	6.838682	-0.031595	3.500777
155.934925	4133.806624	6.843686	-0.031641	3.503998
156.114486	4141.861127	6.848691	-0.031680	3.507249
156.299488	4149.887847	6.853696	-0.031720	3.510485
156.529655	4157.963638	6.858701	-0.031768	3.513739
156.700534	4165.953624	6.863706	-0.031805	3.516954
156.836015	4173.914810	6.868710	-0.031835	3.520154
157.240589	4181.918017	6.873715	-0.031916	3.523375
157.331434	4189.978422	6.878720	-0.031938	3.526607
157.658103	4198.054066	6.883725	-0.032004	3.529850
157.812924	4206.103478	6.888730	-0.032038	3.533073
157.922478	4214.125439	6.893734	-0.032064	3.536281
158.230944	4222.143626	6.898739	-0.032127	3.539491
158.245579	4230.166320	6.903744	-0.032135	3.542691
158.505300	4238.207648	6.908749	-0.032188	3.545902
158.807217	4246.221841	6.913754	-0.032250	3.549101
158.893266	4254.309033	6.918758	-0.032271	3.552320
159.227160	4262.393769	6.923763	-0.032339	3.555542
159.329129	4270.326219	6.928768	-0.032363	3.558694
159.422402	4278.344363	6.933773	-0.032386	3.561877
159.731430	4286.306469	6.938778	-0.032448	3.565041
160.036115	4294.319507	6.943782	-0.032510	3.568223
160.036014	4302.420712	6.948787	-0.032516	3.571427
160.130499	4310.421882	6.953792	-0.032538	3.574592
160.363925	4318.427137	6.958797	-0.032587	3.577760
160.536745	4326.457486	6.963802	-0.032625	3.580932
160.590177	4334.432418	6.968806	-0.032640	3.584077
160.969512	4342.483510	6.973811	-0.032716	3.587259
161.253247	4350.482964	6.978816	-0.032774	3.590414
161.353323	4358.574371	6.983821	-0.032798	3.593597
161.356556	4366.587733	6.988826	-0.032804	3.596745
161.593262	4374.580200	6.993830	-0.032853	3.599888
162.049852	4382.595077	6.998835	-0.032943	3.603043
162.014181	4390.611712	7.003840	-0.032942	3.606182
162.472075	4398.628073	7.008845	-0.033032	3.609332
162.838334	4406.672544	7.013850	-0.033106	3.612488
162.946792	4414.712117	7.018854	-0.033131	3.615632
163.245310	4422.735706	7.023859	-0.033192	3.618772
163.355607	4430.747639	7.028864	-0.033218	3.621899
163.459359	4438.780642	7.033869	-0.033243	3.625032
163.486087	4446.780318	7.038874	-0.033253	3.628147
163.810358	4454.844776	7.043878	-0.033318	3.631293
164.251810	4462.910623	7.048883	-0.033406	3.634440
164.333325	4470.912166	7.053888	-0.033426	3.637549
164.617805	4478.930678	7.058893	-0.033485	3.640668
164.970897	4486.893444	7.063898	-0.033556	3.643764
165.173257	4494.942085	7.068902	-0.033599	3.646886
165.381626	4502.995696	7.073907	-0.033643	3.650008
165.703907	4510.988715	7.078912	-0.033708	3.653107
165.916441	4519.064899	7.083917	-0.033753	3.656233
165.807948	4527.056686	7.088922	-0.033738	3.659314
166.158955	4535.072532	7.093926	-0.033808	3.662415
166.569377	4543.081582	7.098931	-0.033890	3.665512
166.605614	4551.100164	7.103936	-0.033902	3.668599
167.067313	4559.144765	7.108941	-0.033993	3.671706
167.235062	4567.175507	7.113946	-0.034030	3.674797
167.355590	4575.191042	7.118950	-0.034058	3.677878
167.453434	4583.246622	7.123955	-0.034081	3.680971
167.668476	4591.197754	7.128960	-0.034126	3.684025
167.886638	4599.256487	7.133965	-0.034172	3.687117
168.213199	4607.250442	7.138970	-0.034238	3.690185
168.540072	4615.297737	7.143974	-0.034304	3.693270
168.522427	4623.385218	7.148979	-0.034306	3.696360
168.510537	4631.344092	7.153984	-0.034309	3.699398
168.761729	4639.363534	7.158989	-0.034362	3.702463
169.226835	4647.336447	7.163994	-0.034453	3.705513
169.344971	4655.399406	7.168998	-0.034481	3.708586
169.542976	4663.491022	7.174003	-0.034523	3.711670
169.605117	4671.556347	7.179008	-0.034540	3.714738
169.637040	4679.534942	7.184013	-0.034551	3.717769
169.682415	4687.543892	7.189018	-0.034565	3.720810
169.895200	4695.510811	7.194022	-0.034609	3.723836
170.286817	4703.578394	7.199027	-0.034688	3.726903
170.334261	4711.572426	7.204032	-0.034702	3.729931
170.312559	4719.625257	7.209037	-0.034703	3.732976
170.519663	4727.647044	7.214042	-0.034747	3.736014
170.793606	4735.581100	7.219046	-0.034803	3.739017
170.975307	4743.649128	7.224051	-0.034842	3.742066
171.204051	4751.637212	7.229056	-0.034890	3.745083
171.238400	4759.686278	7.234061	-0.034902	3.748116
171.614976	4767.754576	7.239066	-0.034977	3.751162
171.631700	4775.768096	7.244070	-0.034985	3.754177
172.109419	4783.760352	7.249075	-0.035080	3.757192
172.265919	4791.771591	7.254080	-0.035114	3.760204
172.438274	4799.789186	7.259085	-0.035151	3.763216
172.535785	4807.846202	7.264090	-0.035175	3.766240
172.629826	4815.843258	7.269094	-0.035198	3.769238
172.797587	4823.908151	7.274099	-0.035234	3.772260
173.083836	4831.911435	7.279104	-0.035293	3.775260
173.441326	4839.961196	7.284109	-0.035365	3.778277
173.445039	4847.987057	7.289114	-0.035370	3.781274
173.573048	4855.968287	7.294118	-0.035400	3.784255
173.927728	4864.012645	7.299123	-0.035471	3.787262
173.954001	4872.026183	7.304128	-0.035481	3.790248
174.214413	4880.072381	7.309133	-0.035535	3.793249
174.417936	4888.129290	7.314138	-0.035578	3.796250
174.568274	4896.074804	7.319142	-0.035611	3.799206
174.653757	4904.110306	7.324147	-0.035632	3.802192
174.997007	4912.085663	7.329152	-0.035702	3.805159
175.564700	4920.108998	7.334157	-0.035812	3.808146
175.893029	4928.196712	7.339162	-0.035879	3.811149
175.982853	4936.159725	7.344166	-0.035901	3.814099
176.477443	4944.234648	7.349171	-0.035998	3.817096
176.529024	4952.203176	7.354176	-0.036013	3.820043
176.744171	4960.258947	7.359181	-0.036058	3.823022
176.832435	4968.270839	7.364186	-0.036080	3.825981
176.999599	4976.266674	7.369190	-0.036117	3.828932
177.157109	4984.333733	7.374195	-0.036151	3.831908
177.202377	4992.350744	7.379200	-0.036165	3.834861
177.535169	5000.350024	7.384205	-0.036232	3.837810
177.591262	5008.380583	7.389210	-0.036248	3.840763
177.823990	5016.360646	7.394214	-0.036296	3.843699
178.227885	5024.385823	7.399219	-0.036377	3.846653
178.399151	5032.358815	7.404224	-0.036414	3.849580
178.374903	5040.469019	7.409229	-0.036415	3.852552
178.635588	5048.519343	7.414234	-0.036469	3.855505
178.750679	5056.527675	7.419238	-0.036495	3.858438
178.875788	5064.581753	7.424243	-0.036524	3.861385
179.097286	5072.525616	7.429248	-0.036570	3.864291
179.200719	5080.589822	7.434253	-0.036595	3.867237
179.457835	5088.638149	7.439258	-0.036648	3.870178
179.695419	5096.829163	7.444262	-0.036698	3.873168
179.693103	5104.878390	7.449267	-0.036702	3.876100
179.907290	5112.747829	7.454272	-0.036747	3.878968
180.025600	5120.734836	7.459277	-0.036775	3.881875
180.123592	5128.714365	7.464282	-0.036798	3.884777
180.417062	5136.742805	7.469286	-0.036858	3.887698
180.521938	5144.780556	7.474291	-0.036883	3.890616
180.597165	5152.789787	7.479296	-0.036902	3.893521
180.942905	5160.801969	7.484301	-0.036972	3.896431
181.156017	5168.817779	7.489306	-0.037017	3.899337
181.380890	5176.796747	7.494310	-0.037064	3.902227
181.803674	5184.840525	7.499315	-0.037148	3.905143
181.956374	5192.870826	7.504320	-0.037182	3.908046
181.944316	5200.911379	7.509325	-0.037185	3.910948
182.358361	5208.933319	7.514330	-0.037267	3.913849
182.361248	5216.933138	7.519334	-0.037273	3.916733
182.650413	5224.952816	7.524339	-0.037332	3.919626
182.708435	5232.971251	7.529344	-0.037348	3.922513
183.081336	5240.951827	7.534349	-0.037423	3.925389
183.383904	5248.993265	7.539354	-0.037484	3.928284
183.406564	5257.006181	7.544358	-0.037494	3.931162
183.555026	5265.076113	7.549363	-0.037527	3.934060
183.804514	5273.084293	7.554368	-0.037578	3.936936
183.992784	5281.019550	7.559373	-0.037619	3.939782
184.208208	5289.108458	7.564378	-0.037664	3.942682
184.357898	5297.081832	7.569382	-0.037697	3.945537
184.631775	5305.158024	7.574387	-0.037753	3.948429
184.470410	5313.173317	7.579392	-0.037729	3.951289
184.958771	5321.186220	7.584397	-0.037825	3.954158
185.258220	5329.231866	7.589402	-0.037886	3.957033
185.168424	5337.199857	7.594406	-0.037874	3.959871
185.386401	5345.221802	7.599411	-0.037920	3.962732
185.739457	5353.198394	7.604416	-0.037991	3.965578
185.848354	5361.228571	7.609421	-0.038017	3.968435
185.894140	5369.322085	7.614426	-0.038031	3.971313
186.259845	5377.322751	7.619430	-0.038104	3.974160
186.458196	5385.353078	7.624435	-0.038146	3.977013
186.546688	5393.333674	7.629440	-0.038168	3.979845
186.788021	5401.381566	7.634445	-0.038218	3.982701
187.013178	5409.384067	7.639450	-0.038265	3.985539
187.216392	5417.402220	7.644454	-0.038308	3.988379
187.212780	5425.492294	7.649459	-0.038313	3.991240
187.540801	5433.529564	7.654464	-0.038379	3.994085
187.789279	5441.538335	7.659469	-0.038431	3.996917
187.766273	5449.533458	7.664474	-0.038432	3.999738
187.874890	5457.508739	7.669478	-0.038457	4.002552
188.134014	5465.544900	7.674483	-0.038511	4.005388
188.264235	5473.549234	7.679488	-0.038540	4.008208
188.430779	5481.591364	7.684493	-0.038577	4.011040
188.587431	5489.660129	7.689498	-0.038611	4.013880
188.693831	5497.651589	7.694502	-0.038636	4.016689
188.683634	5505.695680	7.699507	-0.038640	4.019514
189.006120	5513.697790	7.704512	-0.038705	4.022326
189.333588	5521.679591	7.709517	-0.038771	4.025130
189.367503	5529.744146	7.714522	-0.038783	4.027956
189.355441	5537.748598	7.719526	-0.038786	4.030758
189.882528	5545.876247	7.724531	-0.038889	4.033610
190.136774	5553.868921	7.729536	-0.038942	4.036408
190.126743	5561.813375	7.734541	-0.038945	4.039183
190.225374	5569.827518	7.739546	-0.038969	4.041983
190.200609	5577.797031	7.744550	-0.038969	4.044763
190.404975	5585.830372	7.749555	-0.039013	4.047567
190.677672	5593.839598	7.754560	-0.039069	4.050361
190.719642	5601.882122	7.759565	-0.039082	4.053162
190.923883	5609.932416	7.764570	-0.039125	4.055966
190.935207	5617.883235	7.769574	-0.039132	4.058731
191.328007	5625.975569	7.774579	-0.039211	4.061548
191.295275	5633.886179	7.779584	-0.039210	4.064294
191.358327	5641.971917	7.784589	-0.039227	4.067100
191.892840	5649.976435	7.789594	-0.039332	4.069883
191.838368	5658.020553	7.794598	-0.039327	4.072670
192.085554	5666.057944	7.799603	-0.039378	4.075456
192.298859	5674.011149	7.804608	-0.039423	4.078211
192.280773	5682.022466	7.809613	-0.039425	4.080981
192.443734	5690.032901	7.814618	-0.039461	4.083751
192.614919	5698.100076	7.819622	-0.039498	4.086539
192.881080	5706.086723	7.824627	-0.039553	4.089298
192.938995	5714.150474	7.829632	-0.039569	4.092080
192.964615	5722.171161	7.834637	-0.039579	4.094844
193.167187	5730.196740	7.839642	-0.039622	4.097610
193.470890	5738.138607	7.844646	-0.039683	4.100348
193.625026	5746.215189	7.849651	-0.039717	4.103127
193.785916	5754.203457	7.854656	-0.039753	4.105874
193.888425	5762.221204	7.859661	-0.039777	4.108629
193.991247	5770.328999	7.864666	-0.039801	4.111413
194.130175	5778.330792	7.869670	-0.039833	4.114159
194.689010	5786.385085	7.874675	-0.039942	4.116927
194.667919	5794.304417	7.879680	-0.039943	4.119639
194.813018	5802.380637	7.884685	-0.039976	4.122405
195.119901	5810.349532	7.889690	-0.040038	4.125135
195.050158	5818.344101	7.894694	-0.040030	4.127866
195.226989	5826.388857	7.899699	-0.040068	4.130617
195.348544	5834.481325	7.904704	-0.040096	4.133380
195.608663	5842.517485	7.909709	-0.040150	4.136125
195.668057	5850.503118	7.914714	-0.040166	4.138848
195.803754	5858.481223	7.919718	-0.040197	4.141568
196.188583	5866.493366	7.924723	-0.040274	4.144300
196.217368	5874.522667	7.929728	-0.040284	4.147032
196.334707	5882.517418	7.934733	-0.040311	4.149752
196.681204	5890.571937	7.939738	-0.040381	4.152492
196.923400	5898.597854	7.944742	-0.040432	4.155220
197.140652	5906.613451	7.949747	-0.040477	4.157943
197.189048	5914.631010	7.954752	-0.040492	4.160662
197.410954	5922.611951	7.959757	-0.040538	4.163369
197.591125	5930.667851	7.964762	-0.040577	4.166099
197.414483	5938.669231	7.969766	-0.040549	4.168805
197.710316	5946.737389	7.974771	-0.040610	4.171537
197.965958	5954.757795	7.979776	-0.040663	4.174251
197.863393	5962.751083	7.984781	-0.040649	4.176950
198.226195	5970.712814	7.989786	-0.040722	4.179641
198.389590	5978.786387	7.994790	-0.040757	4.182366
198.424940	5986.774069	7.999795	-0.040769	4.185059
198.538812	5994.808860	8.004800	-0.040796	4.187767
198.818015	6002.841705	8.009805	-0.040853	4.190475
198.970167	6010.942431	8.014810	-0.040886	4.193202
199.062981	6018.926858	8.019814	-0.040909	4.195887
199.318018	6026.884341	8.024819	-0.040962	4.198564
199.515251	6034.904640	8.029824	-0.041004	4.201259
199.662060	6042.866614	8.034829	-0.041036	4.203932
199.779688	6050.951039	8.039834	-0.041063	4.206645
199.967210	6058.905317	8.044838	-0.041104	4.209313
200.158059	6067.001693	8.049843	-0.041144	4.212026
200.248385	6074.989819	8.054848	-0.041167	4.214701
200.565984	6083.006967	8.059853	-0.041231	4.217386
200.745315	6090.981218	8.064858	-0.041270	4.220053
200.686240	6099.007946	8.069862	-0.041264	4.222734
201.104344	6106.992794	8.074867	-0.041347	4.225404
201.235237	6115.014777	8.079872	-0.041377	4.228082
201.420997	6123.038419	8.084877	-0.041416	4.230759
201.798006	6131.102876	8.089882	-0.041492	4.233450
201.925750	6139.107647	8.094886	-0.041521	4.236117
201.967183	6147.112504	8.099891	-0.041534	4.238781
202.021286	6155.180278	8.104896	-0.041549	4.241465
202.292214	6163.122054	8.109901	-0.041605	4.244107
202.411656	6171.189762	8.114906	-0.041632	4.246788
202.676824	6179.156929	8.119910	-0.041687	4.249435
202.794268	6187.215196	8.124915	-0.041714	4.252109
202.906370	6195.231640	8.129920	-0.041740	4.254768
202.945661	6203.260806	8.134925	-0.041753	4.257428
203.032739	6211.293716	8.139930	-0.041774	4.260089
203.240860	6219.298211	8.144934	-0.041818	4.262739
203.403079	6227.322235	8.149939	-0.041854	4.265394
203.451960	6235.336404	8.154944	-0.041868	4.268043
203.664776	6243.372982	8.159949	-0.041913	4.270700
203.776451	6251.470302	8.164954	-0.041939	4.273373
203.717297	6259.463598	8.169958	-0.041934	4.276010
204.069003	6267.418007	8.174963	-0.042004	4.278635
204.201155	6275.413431	8.179968	-0.042034	4.281270
204.286600	6283.418828	8.184973	-0.042055	4.283907
204.358223	6291.492189	8.189978	-0.042074	4.286564
204.687463	6299.476750	8.194982	-0.042140	4.289192
204.930774	6307.528359	8.199987	-0.042191	4.291840
205.023501	6315.552642	8.204992	-0.042214	4.294476
205.128616	6323.544489	8.209997	-0.042238	4.297101
205.464089	6331.582310	8.215002	-0.042306	4.299740
205.383198	6339.565733	8.220006	-0.042296	4.302356
205.645127	6347.560071	8.225011	-0.042350	4.304978
205.753135	6355.642218	8.230016	-0.042376	4.307625
205.922886	6363.636313	8.235021	-0.042413	4.310242
206.110636	6371.686489	8.240026	-0.042453	4.312876
206.254667	6379.682484	8.245030	-0.042485	4.315490
206.574555	6387.663095	8.250035	-0.042550	4.318099
206.659885	6395.671239	8.255040	-0.042571	4.320714
206.919517	6403.663103	8.260045	-0.042624	4.323323
207.134652	6411.722209	8.265050	-0.042670	4.325952
207.165067	6419.750160	8.270054	-0.042681	4.328568
207.446984	6427.778408	8.275059	-0.042738	4.331184
207.634379	6435.783945	8.280064	-0.042779	4.333791
207.874266	6443.792289	8.285069	-0.042829	4.336397
208.067862	6451.777723	8.290074	-0.042870	4.338994
208.092512	6459.828338	8.295078	-0.042880	4.341609
208.532663	6467.820246	8.300083	-0.042967	4.344207
208.430080	6475.890043	8.305088	-0.042953	4.346824
208.573268	6483.853648	8.310093	-0.042985	4.349407
209.041569	6491.991761	8.315098	-0.043077	4.352048
208.942537	6500.042364	8.320102	-0.043064	4.354654
209.259179	6507.977490	8.325107	-0.043129	4.357225
209.348354	6515.946092	8.330112	-0.043150	4.359803
209.648049	6523.962646	8.335117	-0.043211	4.362396
209.711702	6531.940368	8.340122	-0.043228	4.364974
210.083415	6539.942042	8.345126	-0.043303	4.367560
210.433226	6547.996454	8.350131	-0.043373	4.370161
210.335598	6556.057494	8.355136	-0.043360	4.372760
210.433215	6564.054726	8.360141	-0.043384	4.375339
210.650138	6572.089415	8.365146	-0.043430	4.377928
210.813885	6580.099857	8.370150	-0.043465	4.380508
211.052466	6588.106944	8.375155	-0.043515	4.383085
211.223589	6596.113257	8.380160	-0.043552	4.385660
211.253968	6604.106441	8.385165	-0.043563	4.388229
211.466879	6612.172110	8.390170	-0.043608	4.390821
211.590972	6620.142017	8.395174	-0.043636	4.393380
211.697465	6628.245436	8.400179	-0.043661	4.395980
211.851021	6636.188279	8.405184	-0.043695	4.398527
211.866933	6644.190735	8.410189	-0.043703	4.401091
212.154656	6652.184591	8.415194	-0.043762	4.403652
212.278903	6660.215175	8.420198	-0.043791	4.406223
212.413858	6668.240569	8.425203	-0.043821	4.408790
212.722506	6676.304074	8.430208	-0.043884	4.411370
212.855630	6684.291131	8.435213	-0.043914	4.413922
213.123899	6692.386402	8.440218	-0.043969	4.416508
212.930179	6700.296928	8.445222	-0.043938	4.419031
213.169610	6708.330664	8.450227	-0.043988	4.421594
213.499172	6716.339397	8.455232	-0.044055	4.424148
213.483193	6724.373702	8.460237	-0.044057	4.426707
213.737918	6732.416548	8.465242	-0.044110	4.429269
213.944275	6740.468784	8.470246	-0.044153	4.431832
213.964316	6748.503869	8.475251	-0.044162	4.434387
214.022809	6756.541098	8.480256	-0.044179	4.436941
214.414065	6764.430896	8.485261	-0.044257	4.439449
214.521373	6772.525956	8.490266	-0.044282	4.442019
214.447556	6780.475610	8.495270	-0.044273	4.444541
214.750833	6788.524237	8.500275	-0.044335	4.447094
214.852158	6796.554633	8.505280	-0.044359	4.449639
215.087132	6804.574149	8.510285	-0.044408	4.452179
215.390339	6812.620176	8.515290	-0.044470	4.454727
215.281213	6820.583283	8.520294	-0.044455	4.457246
215.443996	6828.577151	8.525299	-0.044491	4.459774
215.692463	6836.633892	8.530304	-0.044542	4.462320
215.999786	6844.596738	8.535309	-0.044605	4.464836
216.271059	6852.702166	8.540314	-0.044660	4.467395
216.303394	6860.660656	8.545318	-0.044672	4.469906
216.257543	6868.711699	8.550323	-0.044668	4.472443
216.565572	6876.772292	8.555328	-0.044731	4.474984
216.511203	6884.734445	8.560333	-0.044726	4.477491
216.791100	6892.726236	8.565338	-0.044783	4.480007
217.031372	6900.714120	8.570343	-0.044833	4.482520
217.297713	6908.724201	8.575347	-0.044888	4.485039
217.449326	6916.780817	8.580352	-0.044922	4.487571
217.634448	6924.777069	8.585357	-0.044962	4.490082
217.626241	6932.881269	8.590362	-0.044965	4.492625
217.894527	6940.837071	8.595367	-0.045020	4.495121
217.948706	6948.834282	8.600371	-0.045036	4.497628
218.196552	6956.859129	8.605376	-0.045087	4.500143
218.404429	6964.865990	8.610381	-0.045131	4.502651
218.601828	6972.887474	8.615386	-0.045173	4.505161
218.603061	6980.937171	8.620391	-0.045179	4.507679
218.650952	6988.957016	8.625395	-0.045193	4.510186
218.996677	6996.995903	8.630400	-0.045263	4.512698
219.053116	7005.013723	8.635405	-0.045278	4.515202
219.289003	7013.019611	8.640410	-0.045328	4.517701
219.212959	7020.969324	8.645415	-0.045319	4.520180
219.510250	7028.991742	8.650419	-0.045379	4.522681
219.678665	7036.985574	8.655424	-0.045416	4.525172
219.789372	7045.000337	8.660429	-0.045442	4.527668
220.157547	7053.039892	8.665434	-0.045516	4.530170
220.242065	7061.051790	8.670439	-0.045536	4.532662
220.138921	7069.094463	8.675443	-0.045523	4.535162
220.288093	7077.114834	8.680448	-0.045556	4.537654
220.500528	7085.054813	8.685453	-0.045600	4.540120
220.620064	7093.121508	8.690458	-0.045628	4.542623
220.551580	7101.097114	8.695463	-0.045620	4.545097
220.922982	7109.165305	8.700467	-0.045695	4.547598
221.075123	7117.175748	8.705472	-0.045728	4.550080
221.136572	7125.214289	8.710477	-0.045745	4.552570
221.476109	7133.254893	8.715482	-0.045814	4.555058
221.654417	7141.244253	8.720487	-0.045852	4.557530
221.751638	7149.227278	8.725491	-0.045875	4.559998
222.033329	7157.245214	8.730496	-0.045933	4.562475
222.323691	7165.226126	8.735501	-0.045992	4.564940
222.717837	7173.285946	8.740506	-0.046071	4.567428
222.691661	7181.276966	8.745511	-0.046072	4.569893
222.912306	7189.326128	8.750515	-0.046118	4.572375
223.314637	7197.390303	8.755520	-0.046198	4.574860
223.332388	7205.338542	8.760525	-0.046207	4.577307
223.686098	7213.439215	8.765530	-0.046278	4.579801
223.804745	7221.385707	8.770535	-0.046305	4.582246
223.927058	7229.385243	8.775539	-0.046333	4.584705
224.190388	7237.454858	8.780544	-0.046387	4.587185
224.514838	7245.427134	8.785549	-0.046453	4.589633
224.501294	7253.514343	8.790554	-0.046456	4.592116
224.446259	7261.524569	8.795559	-0.046451	4.594573
224.558323	7269.525565	8.800563	-0.046477	4.597026
224.914583	7277.526475	8.805568	-0.046549	4.599478
225.016516	7285.495396	8.810573	-0.046573	4.601919
225.147936	7293.482847	8.815578	-0.046603	4.604364
225.270059	7301.521563	8.820583	-0.046631	4.606824
225.392316	7309.537056	8.825587	-0.046659	4.609275
225.498320	7317.607968	8.830592	-0.046684	4.611742
225.758903	7325.601430	8.835597	-0.046737	4.614183
226.167899	7333.692317	8.840602	-0.046819	4.616653
226.155623	7341.604433	8.845607	-0.046822	4.619068
226.346539	7349.674364	8.850611	-0.046863	4.621529
226.754523	7357.635079	8.855616	-0.046944	4.623955
226.636455	7365.705323	8.860621	-0.046927	4.626414
226.770396	7373.713398	8.865626	-0.046957	4.628852
226.910890	7381.720632	8.870631	-0.046989	4.631289
227.216655	7389.769330	8.875635	-0.047051	4.633737
227.232973	7397.782928	8.880640	-0.047059	4.636173
227.270313	7405.718569	8.885645	-0.047071	4.638584
227.324758	7413.774595	8.890650	-0.047087	4.641030
227.469066	7421.754840	8.895655	-0.047119	4.643452
227.763099	7429.779809	8.900659	-0.047179	4.645887
228.054085	7437.836911	8.905664	-0.047238	4.648329
228.163422	7445.793797	8.910669	-0.047264	4.650740
228.108098	7453.909043	8.915674	-0.047259	4.653198
228.244531	7461.871326	8.920679	-0.047290	4.655609
228.603038	7469.836462	8.925683	-0.047362	4.658018
228.349266	7477.883250	8.930688	-0.047320	4.660452
228.622576	7485.878233	8.935693	-0.047376	4.662868
228.839215	7493.934115	8.940698	-0.047421	4.665301
228.842624	7501.915853	8.945703	-0.047427	4.667711
229.020464	7509.949037	8.950707	-0.047466	4.670135
229.367504	7518.069022	8.955712	-0.047536	4.672583
229.398733	7526.073842	8.960717	-0.047547	4.674996
229.487199	7534.088278	8.965722	-0.047568	4.677411
229.722740	7542.020530	8.970727	-0.047617	4.679799
229.681794	7550.017736	8.975731	-0.047615	4.682206
229.892986	7558.013154	8.980736	-0.047660	4.684611
230.150901	7565.982911	8.985741	-0.047713	4.687007
230.358371	7574.031380	8.990746	-0.047757	4.689425
230.403540	7582.102870	8.995751	-0.047771	4.691850
230.370380	7590.083410	9.000755	-0.047770	4.694245
230.665963	7598.166922	9.005760	-0.047830	4.696670
230.828075	7606.120563	9.010765	-0.047865	4.699055
230.928883	7614.141451	9.015770	-0.047889	4.701459
231.048112	7622.131179	9.020775	-0.047917	4.703853
231.465420	7630.167846	9.025779	-0.048000	4.706258
231.567239	7638.191856	9.030784	-0.048024	4.708659
231.631410	7646.238517	9.035789	-0.048041	4.711066
231.767465	7654.256458	9.040794	-0.048072	4.713463
231.725575	7662.276078	9.045799	-0.048069	4.715859
231.773450	7670.203260	9.050803	-0.048083	4.718227
232.042716	7678.260789	9.055808	-0.048139	4.720631
232.343814	7686.243263	9.060813	-0.048200	4.723012
232.397073	7694.286366	9.065818	-0.048215	4.725410
232.531764	7702.372029	9.070823	-0.048246	4.727820
232.658678	7710.344400	9.075827	-0.048275	4.730194
232.858242	7718.421147	9.080832	-0.048317	4.732599
232.899383	7726.400890	9.085837	-0.048330	4.734973
233.319231	7734.430338	9.090842	-0.048413	4.737360
233.486464	7742.395324	9.095847	-0.048450	4.739728
233.346419	7750.442182	9.100851	-0.048429	4.742119
233.464403	7758.428419	9.105856	-0.048456	4.744491
233.756260	7766.476287	9.110861	-0.048516	4.746879
233.819290	7774.444835	9.115866	-0.048533	4.749243
234.049083	7782.522403	9.120871	-0.048581	4.751637
234.240450	7790.545767	9.125875	-0.048622	4.754015
234.399645	7798.591840	9.130880	-0.048657	4.756398
234.565671	7806.504988	9.135885	-0.048693	4.758740
234.913347	7814.600445	9.140890	-0.048763	4.761135
234.937103	7822.554807	9.145895	-0.048772	4.763487
235.118335	7830.524523	9.150899	-0.048811	4.765843
235.270566	7838.614151	9.155904	-0.048845	4.768233
235.514482	7846.571593	9.160909	-0.048896	4.770582
235.763493	7854.645256	9.165914	-0.048947	4.772965
235.650782	7862.659143	9.170919	-0.048932	4.775330
235.821098	7870.619239	9.175923	-0.048969	4.777676
236.072021	7878.655370	9.180928	-0.049021	4.780044
235.938706	7886.605636	9.185933	-0.049001	4.782387
236.252382	7894.684616	9.190938	-0.049065	4.784765
236.331223	7902.724183	9.195943	-0.049085	4.787130
236.231402	7910.663354	9.200947	-0.049071	4.789466
236.399354	7918.782228	9.205952	-0.049108	4.791853
236.577326	7926.748100	9.210957	-0.049146	4.794193
236.867135	7934.841832	9.215962	-0.049206	4.796569
236.910200	7942.713744	9.220967	-0.049219	4.798880
237.343634	7950.798578	9.225971	-0.049305	4.801251
237.399539	7958.774318	9.230976	-0.049320	4.803590
237.368135	7966.792047	9.235981	-0.049320	4.805940
237.397839	7974.821043	9.240986	-0.049331	4.808293
237.719160	7982.878843	9.245991	-0.049396	4.810651
237.790218	7990.320128	9.250995	-0.049414	4.812829
237.990205	7995.049853	9.256000	-0.049454	4.814212

238.010836	7997.586861	9.261005	-0.049460	4.814954
238.233386	7998.759145	9.266010	-0.049502	4.815296
238.053123	7999.419066	9.271015	-0.049469	4.815490
238.440831	7999.684711	9.276019	-0.049541	4.815566
238.493985	7999.711191	9.281024	-0.049551	4.815573
238.460887	7999.694648	9.286029	-0.049545	4.815568
238.530107	7999.719254	9.291034	-0.049558	4.815575
238.475180	7999.711964	9.296039	-0.049548	4.815573
238.492785	7999.737870	9.301043	-0.049551	4.815581
238.341810	7999.956387	9.306048	-0.049523	4.815646
238.499973	8000.063556	9.311053	-0.049553	4.815676
238.551397	7999.962985	9.316058	-0.049562	4.815646
238.549792	7999.953355	9.321063	-0.049562	4.815644
238.857744	7999.981823	9.326067	-0.049619	4.815651
239.153652	7999.821161	9.331072	-0.049674	4.815602
238.838239	7999.977244	9.336077	-0.049616	4.815649
238.925770	7999.852707	9.341082	-0.049632	4.815612
239.162021	7999.835182	9.346087	-0.049676	4.815606
239.113105	7999.981700	9.351091	-0.049667	4.815649
239.020697	7999.859589	9.356096	-0.049650	4.815614
239.137057	7999.963948	9.361101	-0.049672	4.815644
239.184058	7999.862237	9.366106	-0.049680	4.815614
239.288374	7999.949323	9.371111	-0.049700	4.815639
239.351214	8000.000513	9.376115	-0.049712	4.815654
239.355357	7999.965358	9.381120	-0.049713	4.815643
239.399840	8000.103782	9.386125	-0.049721	4.815684
239.417271	7999.850014	9.391130	-0.049724	4.815609
239.608389	7999.950247	9.396135	-0.049760	4.815638
239.539776	7999.990771	9.401139	-0.049747	4.815650
239.502592	7999.877023	9.406144	-0.049740	4.815617
239.686247	7999.961124	9.411149	-0.049774	4.815641
239.577612	7999.797117	9.416154	-0.049754	4.815593
239.641361	7999.798152	9.421159	-0.049766	4.815593
239.553834	7999.890674	9.426163	-0.049750	4.815621
239.807678	7999.816861	9.431168	-0.049797	4.815598
239.706798	7999.944393	9.436173	-0.049778	4.815636
239.517335	7999.864474	9.441178	-0.049743	4.815613
239.631997	8000.132129	9.446183	-0.049765	4.815691
239.499253	7999.902616	9.451187	-0.049740	4.815624
239.521080	8000.024662	9.456192	-0.049744	4.815660
239.527157	7999.990605	9.461197	-0.049745	4.815650
239.740687	7999.832878	9.466202	-0.049785	4.815603
239.748828	8000.002738	9.471207	-0.049786	4.815652
239.620921	8000.067921	9.476211	-0.049763	4.815672
239.731714	7999.898925	9.481216	-0.049783	4.815622
239.592164	7999.907344	9.486221	-0.049757	4.815625
239.760188	7999.966641	9.491226	-0.049789	4.815642
239.829777	7999.855688	9.496231	-0.049802	4.815609
239.809282	8000.063513	9.501235	-0.049798	4.815670
239.695504	7999.849252	9.506240	-0.049777	4.815608
239.661229	7999.967188	9.511245	-0.049770	4.815642
239.852720	7999.833655	9.516250	-0.049806	4.815602
239.781536	7999.845316	9.521255	-0.049793	4.815606
239.674889	7999.981295	9.526259	-0.049773	4.815646
239.717261	7999.959567	9.531264	-0.049781	4.815640
239.853122	7999.956432	9.536269	-0.049806	4.815638
239.779998	7999.773785	9.541274	-0.049793	4.815585
240.045564	7999.846402	9.546279	-0.049842	4.815605
240.264379	7999.847811	9.551283	-0.049883	4.815605
240.090811	7999.859950	9.556288	-0.049851	4.815609
239.720968	7999.885993	9.561293	-0.049782	4.815618
239.827234	7999.917604	9.566298	-0.049802	4.815627
240.192706	7999.859474	9.571303	-0.049870	4.815608
239.853660	7999.911633	9.576307	-0.049807	4.815625
240.209578	7999.888575	9.581312	-0.049873	4.815617
240.074912	7999.931232	9.586317	-0.049848	4.815630
240.137566	7999.750781	9.591322	-0.049860	4.815577
240.107093	7999.837823	9.596327	-0.049854	4.815602
240.158446	7999.862141	9.601331	-0.049864	4.815609
240.163626	7999.852621	9.606336	-0.049865	4.815606
239.965919	7999.852627	9.611341	-0.049828	4.815607
239.963569	7999.861132	9.616346	-0.049827	4.815610
239.957889	7999.863178	9.621351	-0.049826	4.815611
239.926853	7999.833858	9.626355	-0.049821	4.815602
239.932138	7999.846756	9.631360	-0.049822	4.815606
239.929275	7999.829634	9.636365	-0.049821	4.815601
239.955697	7999.948552	9.641370	-0.049826	4.815636
240.021665	7999.906924	9.646375	-0.049839	4.815623
239.946952	7999.908921	9.651379	-0.049825	4.815624
240.074395	7999.758341	9.656384	-0.049848	4.815579
239.897938	7999.944428	9.661389	-0.049816	4.815635
239.954051	7999.806570	9.666394	-0.049826	4.815594
240.144679	7999.800050	9.671399	-0.049862	4.815591
239.867009	7999.981298	9.676403	-0.049810	4.815646
240.134354	7999.777473	9.681408	-0.049860	4.815585
240.291622	7999.855811	9.686413	-0.049889	4.815607
240.264232	7999.870315	9.691418	-0.049884	4.815611
240.135265	7999.841545	9.696423	-0.049860	4.815603
240.194736	7999.949257	9.701427	-0.049871	4.815635
240.201790	7999.838358	9.706432	-0.049872	4.815602
240.199262	7999.965348	9.711437	-0.049872	4.815639
240.264974	7999.757193	9.716442	-0.049884	4.815578
240.268066	7999.835170	9.721447	-0.049885	4.815601
240.058735	7999.952409	9.726451	-0.049846	4.815636
240.014694	7999.746748	9.731456	-0.049838	4.815576
240.137906	7999.854423	9.736461	-0.049861	4.815607
240.128644	7999.846804	9.741466	-0.049859	4.815605
240.115493	7999.842324	9.746471	-0.049857	4.815604
240.290878	7999.954047	9.751475	-0.049889	4.815636
240.222441	7999.839792	9.756480	-0.049877	4.815602
240.090866	7999.949749	9.761485	-0.049852	4.815635
240.138600	7999.840576	9.766490	-0.049861	4.815603
240.190302	7999.840349	9.771495	-0.049871	4.815603
240.149799	7999.985939	9.776499	-0.049863	4.815646
240.207458	7999.848105	9.781504	-0.049874	4.815605
240.328349	7999.832985	9.786509	-0.049897	4.815600
240.270597	7999.839526	9.791514	-0.049886	4.815602
240.125882	7999.863874	9.796519	-0.049859	4.815610
240.251863	7999.943841	9.801523	-0.049883	4.815633
240.291275	7999.862287	9.806528	-0.049890	4.815609
240.299579	7999.835738	9.811533	-0.049891	4.815601
240.332389	7999.851217	9.816538	-0.049898	4.815605
240.431260	7999.742871	9.821543	-0.049916	4.815573
240.253017	7999.840331	9.826547	-0.049883	4.815602
240.353988	7999.872925	9.831552	-0.049902	4.815611
240.613112	7999.824816	9.836557	-0.049950	4.815596
240.620919	7999.858037	9.841562	-0.049951	4.815606
240.413751	7999.851485	9.846567	-0.049913	4.815605
240.649344	7999.864908	9.851571	-0.049957	4.815608
240.702366	7999.756888	9.856576	-0.049967	4.815576
240.506134	7999.851922	9.861581	-0.049930	4.815605
240.607519	7999.855701	9.866586	-0.049949	4.815605
240.611030	7999.858964	9.871591	-0.049950	4.815606
240.603243	7999.886595	9.876595	-0.049948	4.815614
240.657564	7999.841576	9.881600	-0.049959	4.815601
240.743680	7999.746901	9.886605	-0.049975	4.815573
240.665682	7999.856659	9.891610	-0.049960	4.815605
240.649983	7999.846801	9.896615	-0.049957	4.815602
240.543687	7999.747944	9.901619	-0.049937	4.815574
240.697306	7999.850775	9.906624	-0.049966	4.815603
240.656817	7999.827706	9.911629	-0.049959	4.815597
240.496466	7999.753594	9.916634	-0.049929	4.815576
240.798697	7999.852426	9.921639	-0.049985	4.815603
240.598837	7999.868409	9.926643	-0.049948	4.815609
240.739095	7999.754328	9.931648	-0.049974	4.815575
240.559258	7999.843223	9.936653	-0.049941	4.815602
240.621099	7999.925355	9.941658	-0.049952	4.815626
240.408755	7999.893099	9.946663	-0.049913	4.815617
240.571292	8000.037708	9.951667	-0.049943	4.815659
240.892042	7999.785641	9.956672	-0.050003	4.815583
240.560252	7999.860335	9.961677	-0.049941	4.815607
240.582999	7999.958913	9.966682	-0.049945	4.815636
240.665523	7999.835358	9.971687	-0.049961	4.815599
240.688325	7999.746063	9.976691	-0.049965	4.815573
240.612684	7999.848386	9.981696	-0.049951	4.815603
240.609504	7999.854743	9.986701	-0.049950	4.815605
240.760506	7999.866798	9.991706	-0.049979	4.815608
240.791172	7999.836340	9.996711	-0.049984	4.815599
240.610444	7999.895332	10.001715	-0.049951	4.815617
240.790113	7999.845937	10.006720	-0.049984	4.815601
240.649699	7999.839397	10.011725	-0.049958	4.815600
240.811042	7999.876171	10.016730	-0.049988	4.815610
241.007264	7999.940198	10.021735	-0.050025	4.815628
240.836076	7999.968386	10.026739	-0.049993	4.815637
240.863084	7999.800165	10.031744	-0.049998	4.815588
240.919817	8000.061552	10.036749	-0.050009	4.815664
240.912799	7999.846878	10.041754	-0.050007	4.815601
240.671231	7999.810947	10.046759	-0.049962	4.815592
240.632351	7999.829535	10.051763	-0.049955	4.815597
240.851541	7999.836288	10.056768	-0.049996	4.815598
240.547894	7999.842052	10.061773	-0.049940	4.815601
240.873576	7999.767266	10.066778	-0.050000	4.815578
240.914275	7999.759388	10.071783	-0.050008	4.815576
241.010086	7999.851677	10.076787	-0.050026	4.815602
240.981048	7999.767947	10.081792	-0.050020	4.815578
240.816212	8000.002263	10.086797	-0.049990	4.815647
240.804980	7999.883594	10.091802	-0.049988	4.815612
240.773436	7999.835050	10.096807	-0.049982	4.815598
240.960010	7999.826331	10.101811	-0.050017	4.815595
241.110317	7999.850117	10.106816	-0.050045	4.815601
240.908680	7999.865003	10.111821	-0.050007	4.815606
240.770967	7999.767772	10.116826	-0.049981	4.815579
240.995355	7999.861075	10.121831	-0.050023	4.815605
241.065177	7999.840859	10.126835	-0.050036	4.815599
241.033037	7999.760281	10.131840	-0.050030	4.815575
240.843369	7999.895986	10.136845	-0.049995	4.815616
241.193513	7999.876038	10.141850	-0.050060	4.815608
241.177454	7999.841622	10.146855	-0.050057	4.815598
241.012097	7999.850691	10.151859	-0.050027	4.815602
241.038477	7999.839379	10.156864	-0.050032	4.815598
241.010731	7999.850675	10.161869	-0.050026	4.815602
240.894609	7999.857338	10.166874	-0.050005	4.815604
241.441120	7999.856582	10.171879	-0.050107	4.815601
241.617346	7999.847696	10.176883	-0.050139	4.815598
241.704073	7999.870453	10.181888	-0.050156	4.815604
241.786013	7999.756494	10.186893	-0.050171	4.815571
242.038083	7999.800076	10.191898	-0.050218	4.815582
242.055846	7999.840932	10.196903	-0.050221	4.815594
241.756460	7999.759227	10.201907	-0.050166	4.815572
241.864175	7999.870927	10.206912	-0.050186	4.815604
241.864965	7999.835715	10.211917	-0.050186	4.815593
241.860460	7999.868738	10.216922	-0.050185	4.815603
242.011481	7999.853040	10.221927	-0.050213	4.815598
242.163300	7999.849096	10.226931	-0.050242	4.815596
242.148255	7999.764523	10.231936	-0.050239	4.815571
242.123998	7999.969095	10.236941	-0.050234	4.815631
242.070242	7999.866814	10.241946	-0.050224	4.815601
242.071742	7999.763294	10.246951	-0.050225	4.815571
241.922069	7999.834531	10.251955	-0.050197	4.815593
242.171085	7999.785191	10.256960	-0.050243	4.815577
242.226725	7999.865091	10.261965	-0.050254	4.815600
242.036438	7999.773410	10.266970	-0.050218	4.815574
242.176087	7999.848265	10.271975	-0.050244	4.815596
242.225247	7999.862942	10.276979	-0.050253	4.815600
242.242799	7999.776761	10.281984	-0.050257	4.815574
242.145733	7999.840310	10.286989	-0.050239	4.815593
242.391857	7999.861380	10.291994	-0.050285	4.815598
242.320261	7999.870899	10.296999	-0.050271	4.815601
242.249746	7999.766212	10.302003	-0.050258	4.815571
241.992744	7999.775930	10.307008	-0.050210	4.815575
242.124601	7999.853862	10.312013	-0.050235	4.815597
242.062268	7999.777063	10.317018	-0.050223	4.815575
241.997566	7999.875296	10.322023	-0.050211	4.815604
242.157415	7999.755125	10.327027	-0.050241	4.815568
242.199226	7999.878568	10.332032	-0.050249	4.815604
242.187965	7999.760963	10.337037	-0.050247	4.815570
242.149875	7999.771025	10.342042	-0.050240	4.815573
242.343041	7999.862760	10.347047	-0.050276	4.815599
242.153472	7999.752942	10.352051	-0.050241	4.815568
242.307002	7999.866452	10.357056	-0.050269	4.815600
242.379489	7999.848415	10.362061	-0.050283	4.815595
242.449603	7999.759882	10.367066	-0.050296	4.815568
242.301808	7999.855703	10.372071	-0.050268	4.815597
242.332597	7999.842327	10.377075	-0.050274	4.815593
242.262237	7999.858271	10.382080	-0.050261	4.815598
242.182194	7999.766240	10.387085	-0.050246	4.815572
242.173823	7999.795997	10.392090	-0.050245	4.815580
242.295239	7999.878030	10.397095	-0.050267	4.815604
242.175426	7999.846203	10.402099	-0.050245	4.815595
242.472565	7999.767752	10.407104	-0.050300	4.815571
242.276041	7999.841433	10.412109	-0.050264	4.815593
242.360744	8000.008274	10.417114	-0.050280	4.815641
242.624497	7999.850287	10.422119	-0.050329	4.815594
242.535102	7999.765576	10.427123	-0.050312	4.815570
242.572404	7999.882542	10.432128	-0.050319	4.815604
242.398479	7999.764437	10.437133	-0.050287	4.815570
242.381343	7999.865576	10.442138	-0.050284	4.815600
242.509397	7999.862316	10.447143	-0.050308	4.815598
242.302098	7999.758616	10.452147	-0.050269	4.815569
242.389880	7999.809146	10.457152	-0.050285	4.815583
242.391692	7999.871094	10.462157	-0.050286	4.815601
242.382557	7999.782346	10.467162	-0.050284	4.815575
242.180756	7999.844199	10.472167	-0.050247	4.815594
242.240979	7999.939118	10.477171	-0.050258	4.815622
242.412752	7999.870381	10.482176	-0.050290	4.815601
242.191984	7999.849728	10.487181	-0.050249	4.815596
242.329982	7999.864776	10.492186	-0.050275	4.815600
242.366493	7999.848291	10.497191	-0.050281	4.815595
242.396770	7999.966211	10.502195	-0.050287	4.815629
242.525969	7999.838070	10.507200	-0.050311	4.815591
242.423192	7999.976253	10.512205	-0.050292	4.815632
242.387838	7999.983156	10.517210	-0.050286	4.815634
242.670053	7999.857494	10.522215	-0.050338	4.815596
242.329692	7999.828499	10.527219	-0.050275	4.815589
242.417370	7999.871555	10.532224	-0.050291	4.815601
242.542164	7999.834081	10.537229	-0.050314	4.815590
242.647457	7999.851803	10.542234	-0.050334	4.815594
242.630710	7999.849400	10.547239	-0.050331	4.815594
242.603459	7999.951444	10.552243	-0.050326	4.815624
242.643940	7999.848553	10.557248	-0.050333	4.815593
242.623668	7999.850363	10.562253	-0.050330	4.815594
242.747819	7999.854512	10.567258	-0.050353	4.815595
242.674487	7999.858665	10.572263	-0.050339	4.815596
242.716271	7999.817712	10.577267	-0.050347	4.815584
242.818454	7999.810830	10.582272	-0.050366	4.815582
242.800211	7999.861779	10.587277	-0.050363	4.815596
242.740965	7999.898186	10.592282	-0.050352	4.815607
242.885834	7999.858903	10.597287	-0.050379	4.815595
242.851486	7999.870092	10.602291	-0.050372	4.815599
242.907701	7999.860331	10.607296	-0.050383	4.815596
242.937835	7999.757272	10.612301	-0.050389	4.815565
242.644372	7999.959621	10.617306	-0.050334	4.815626
242.883514	7999.759601	10.622311	-0.050378	4.815566
242.711900	7999.872117	10.627315	-0.050347	4.815600
242.689599	7999.779952	10.632320	-0.050342	4.815573
242.732910	7999.759307	10.637325	-0.050351	4.815567
242.686741	7999.862111	10.642330	-0.050342	4.815597
242.890530	7999.792824	10.647335	-0.050380	4.815576
242.701760	8000.001140	10.652339	-0.050345	4.815638
242.708840	7999.770672	10.657344	-0.050346	4.815570
242.830005	7999.864445	10.662349	-0.050369	4.815597
242.959991	7999.870824	10.667354	-0.050393	4.815598
243.185916	7999.786950	10.672359	-0.050435	4.815573
242.990285	7999.769907	10.677363	-0.050399	4.815569
243.111473	7999.902112	10.682368	-0.050421	4.815607
243.101271	7999.863518	10.687373	-0.050420	4.815596
243.184892	7999.905443	10.692378	-0.050435	4.815607
243.303646	7999.797414	10.697383	-0.050457	4.815575
243.408124	7999.973120	10.702387	-0.050477	4.815626
243.433269	7999.865708	10.707392	-0.050482	4.815595
243.241236	7999.891423	10.712397	-0.050446	4.815603
243.209077	7999.861014	10.717402	-0.050440	4.815594
243.439385	7999.894641	10.722407	-0.050483	4.815603
243.461024	7999.860833	10.727411	-0.050487	4.815593
243.366941	7999.880663	10.732416	-0.050469	4.815599
243.315988	7999.875570	10.737421	-0.050460	4.815598
243.531304	7999.858779	10.742426	-0.050500	4.815592
243.713260	7999.784868	10.747431	-0.050534	4.815570
243.690447	7999.936093	10.752435	-0.050530	4.815614
243.662484	7999.859847	10.757440	-0.050525	4.815592
243.566012	7999.858287	10.762445	-0.050507	4.815592
243.646736	7999.859598	10.767450	-0.050522	4.815592
243.699601	7999.773987	10.772455	-0.050532	4.815567
243.500308	7999.875380	10.777459	-0.050495	4.815597
243.743729	7999.890004	10.782464	-0.050540	4.815600
243.732423	7999.770258	10.787469	-0.050538	4.815565
243.643131	7999.903325	10.792474	-0.050521	4.815605
243.773235	7999.785872	10.797479	-0.050545	4.815570
243.744546	7999.789680	10.802483	-0.050540	4.815571
243.693129	7999.797391	10.807488	-0.050531	4.815573
243.730023	7999.873788	10.812493	-0.050538	4.815596
243.928012	7999.904756	10.817498	-0.050574	4.815604
243.822681	7999.777081	10.822503	-0.050555	4.815567
243.862677	7999.865272	10.827507	-0.050562	4.815592
243.746498	7999.865527	10.832512	-0.050541	4.815593
243.645098	7999.879900	10.837517	-0.050522	4.815598
243.611248	7999.861206	10.842522	-0.050516	4.815592
243.767389	7999.797552	10.847527	-0.050545	4.815573
243.751627	7999.880569	10.852531	-0.050542	4.815597
243.584832	7999.881071	10.857536	-0.050511	4.815598
243.490123	7999.780258	10.862541	-0.050493	4.815569
243.746078	7999.866610	10.867546	-0.050541	4.815593
243.858156	7999.884443	10.872551	-0.050562	4.815598
243.790759	7999.854530	10.877555	-0.050549	4.815590
243.688045	7999.869949	10.882560	-0.050530	4.815595
243.681904	7999.779112	10.887565	-0.050529	4.815568
243.754242	7999.953230	10.892570	-0.050543	4.815619
243.900039	7999.873395	10.897575	-0.050570	4.815595
243.827751	7999.983252	10.902579	-0.050556	4.815627
243.802277	7999.884628	10.907584	-0.050552	4.815598
243.758827	7999.854035	10.912589	-0.050544	4.815590
243.870846	7999.948731	10.917594	-0.050565	4.815617
243.857508	7999.870587	10.922599	-0.050562	4.815594
243.557775	7999.768586	10.927603	-0.050506	4.815566
243.804325	7999.862258	10.932608	-0.050552	4.815592
243.936062	7999.877207	10.937613	-0.050577	4.815596
243.800187	7999.883549	10.942618	-0.050552	4.815598
243.895670	7999.777277	10.947623	-0.050569	4.815567
243.994321	7999.873891	10.952627	-0.050588	4.815594
243.879299	7999.888043	10.957632	-0.050566	4.815599
243.906569	7999.802017	10.962637	-0.050571	4.815574
244.039579	7999.797770	10.967642	-0.050596	4.815572
243.912731	7999.897135	10.972647	-0.050573	4.815601
243.610419	7999.873023	10.977651	-0.050517	4.815596
243.732849	7999.875010	10.982656	-0.050539	4.815596
244.150917	7999.872182	10.987661	-0.050617	4.815593
243.966013	7999.941781	10.992666	-0.050583	4.815614
243.893717	7999.881897	10.997671	-0.050569	4.815597
243.974961	7999.869339	11.002675	-0.050585	4.815593
244.019604	7999.812418	11.007680	-0.050593	4.815576
243.968582	7999.947174	11.012685	-0.050584	4.815616
243.880912	7999.871027	11.017690	-0.050567	4.815594
244.041506	7999.889647	11.022695	-0.050597	4.815599
243.934418	7999.852685	11.027699	-0.050577	4.815588
243.948579	7999.866796	11.032704	-0.050580	4.815592
243.970548	7999.888506	11.037709	-0.050584	4.815599
243.775340	7999.870399	11.042714	-0.050548	4.815594
243.664928	7999.877154	11.047719	-0.050527	4.815597
243.710250	7999.910985	11.052723	-0.050536	4.815606
243.901206	7999.825477	11.057728	-0.050571	4.815581
243.730695	7999.854743	11.062733	-0.050540	4.815590
243.905989	7999.805277	11.067738	-0.050572	4.815575
244.006114	7999.862416	11.072743	-0.050591	4.815591
243.718504	7999.957040	11.077747	-0.050537	4.815620
243.740584	7999.864524	11.082752	-0.050542	4.815593
243.884943	7999.776125	11.087757	-0.050568	4.815566
243.860776	7999.962558	11.092762	-0.050564	4.815621
243.865543	7999.779020	11.097767	-0.050565	4.815567
243.724385	7999.969962	11.102771	-0.050539	4.815624
244.110904	7999.946339	11.107776	-0.050611	4.815615
243.992674	7999.881440	11.112781	-0.050589	4.815596
244.024567	7999.784813	11.117786	-0.050595	4.815568
244.148894	7999.895722	11.122791	-0.050618	4.815600
244.041555	7999.863026	11.127795	-0.050598	4.815591
244.117286	7999.793798	11.132800	-0.050612	4.815570
244.044017	7999.794749	11.137805	-0.050598	4.815571
244.068632	7999.883758	11.142810	-0.050603	4.815597
243.950073	7999.875434	11.147815	-0.050581	4.815595
243.837992	7999.880026	11.152819	-0.050560	4.815597
244.219044	7999.876598	11.157824	-0.050631	4.815594
244.139028	7999.866763	11.162829	-0.050616	4.815592
243.879384	7999.882842	11.167834	-0.050568	4.815597
244.267663	7999.865652	11.172839	-0.050640	4.815591
244.342638	7999.877547	11.177843	-0.050654	4.815594
244.115632	7999.835438	11.182848	-0.050612	4.815582
244.095992	7999.851136	11.187853	-0.050608	4.815587
244.283184	7999.882998	11.192858	-0.050643	4.815596
244.171465	7999.784042	11.197863	-0.050623	4.815567
243.852441	7999.879225	11.202867	-0.050563	4.815596
244.207749	7999.873244	11.207872	-0.050629	4.815593
244.089766	7999.872402	11.212877	-0.050607	4.815593
243.811777	7999.875373	11.217882	-0.050556	4.815596
244.032579	7999.877887	11.222887	-0.050597	4.815595
244.031816	7999.867202	11.227891	-0.050597	4.815592
244.093915	7999.913050	11.232896	-0.050608	4.815605
244.151955	7999.808305	11.237901	-0.050619	4.815574
244.270983	7999.898846	11.242906	-0.050641	4.815600
244.167547	7999.798957	11.247911	-0.050622	4.815572
244.150785	7999.875552	11.252915	-0.050619	4.815594
244.225042	7999.800962	11.257920	-0.050633	4.815572
244.471555	7999.890367	11.262925	-0.050679	4.815597
244.079078	7999.796468	11.267930	-0.050606	4.815571
244.282818	7999.808314	11.272935	-0.050644	4.815574
244.192462	7999.870906	11.277939	-0.050627	4.815592
244.358195	7999.903488	11.282944	-0.050658	4.815601
244.112933	7999.785286	11.287949	-0.050612	4.815568
244.082493	7999.870201	11.292954	-0.050607	4.815593
244.235408	7999.822507	11.297959	-0.050635	4.815578
244.207382	7999.988596	11.302963	-0.050630	4.815627
244.046469	7999.857883	11.307968	-0.050600	4.815589
244.301867	7999.886580	11.312973	-0.050648	4.815596
244.222663	7999.869286	11.317978	-0.050633	4.815592
244.110705	7999.868542	11.322983	-0.050612	4.815592
243.911927	7999.822621	11.327987	-0.050575	4.815580
243.972293	7999.817197	11.332992	-0.050586	4.815578
244.095437	7999.899263	11.337997	-0.050609	4.815601
244.130934	7999.790951	11.343002	-0.050616	4.815569
244.120250	7999.807862	11.348007	-0.050614	4.815574
243.951030	7999.872378	11.353011	-0.050583	4.815594
244.115318	7999.898531	11.358016	-0.050613	4.815601
244.339096	7999.889351	11.363021	-0.050655	4.815597
244.167424	7999.868423	11.368026	-0.050623	4.815592
244.165254	7999.795797	11.373031	-0.050623	4.815571
244.277175	7999.865938	11.378035	-0.050644	4.815591
244.155480	7999.892793	11.383040	-0.050621	4.815599
244.190606	7999.920054	11.388045	-0.050628	4.815607
244.238071	7999.783112	11.393050	-0.050636	4.815567
244.065906	7999.895621	11.398055	-0.050604	4.815600
244.128711	7999.874223	11.403059	-0.050616	4.815594
244.261881	7999.809129	11.408064	-0.050641	4.815574
244.202793	7999.793228	11.413069	-0.050630	4.815570
244.093845	7999.898221	11.418074	-0.050610	4.815601
244.034580	7999.827873	11.423079	-0.050599	4.815581
244.240563	7999.887796	11.428083	-0.050637	4.815597
244.245420	7999.843040	11.433088	-0.050638	4.815584
244.271704	7999.919266	11.438093	-0.050643	4.815606
244.136409	7999.984333	11.443098	-0.050618	4.815626
244.314529	7999.853778	11.448103	-0.050651	4.815587
244.134889	7999.796424	11.453107	-0.050618	4.815571
244.310278	7999.907094	11.458112	-0.050650	4.815602
244.227717	7999.898285	11.463117	-0.050635	4.815600
244.093466	7999.777614	11.468122	-0.050610	4.815566
244.033786	7999.900486	11.473127	-0.050599	4.815602
244.181697	7999.777982	11.478131	-0.050627	4.815565
244.141175	7999.876612	11.483136	-0.050619	4.815594
244.238808	7999.897414	11.488141	-0.050637	4.815600
244.187646	7999.877371	11.493146	-0.050628	4.815594
244.313664	7999.812161	11.498151	-0.050651	4.815575
244.210142	7999.901229	11.503155	-0.050632	4.815601
244.327388	7999.887119	11.508160	-0.050654	4.815596
244.206639	7999.785882	11.513165	-0.050631	4.815567
244.214855	7999.956828	11.518170	-0.050633	4.815617
244.186539	7999.801576	11.523175	-0.050628	4.815572
244.390898	7999.891365	11.528179	-0.050666	4.815597
244.448108	7999.874147	11.533184	-0.050677	4.815592
244.318506	7999.899805	11.538189	-0.050653	4.815600
244.378096	7999.779072	11.543194	-0.050664	4.815565
244.451807	7999.882757	11.548199	-0.050677	4.815595
244.360568	7999.988038	11.553203	-0.050661	4.815626
244.425697	7999.871664	11.558208	-0.050673	4.815592
244.291424	7999.891909	11.563213	-0.050648	4.815598
244.178305	7999.803607	11.568218	-0.050627	4.815573
244.305750	7999.809946	11.573223	-0.050650	4.815574
244.343519	7999.987777	11.578227	-0.050658	4.815626
244.290171	7999.836389	11.583232	-0.050648	4.815582
244.299422	7999.838677	11.588237	-0.050649	4.815582
244.485956	7999.908961	11.593242	-0.050684	4.815602
244.510753	7999.870934	11.598247	-0.050689	4.815591
244.362484	7999.990236	11.603251	-0.050661	4.815626
244.168196	7999.858981	11.608256	-0.050625	4.815589
244.502495	7999.890026	11.613261	-0.050687	4.815596
244.346497	7999.867216	11.618266	-0.050658	4.815591
244.262465	7999.874397	11.623271	-0.050643	4.815593
244.176671	7999.883685	11.628275	-0.050627	4.815596
244.380961	7999.873122	11.633280	-0.050665	4.815592
244.428426	7999.795963	11.638285	-0.050674	4.815569
244.371019	7999.943427	11.643290	-0.050663	4.815613
244.364320	7999.809876	11.648295	-0.050662	4.815574
244.226199	7999.881302	11.653299	-0.050636	4.815595
244.255712	7999.791041	11.658304	-0.050642	4.815569
244.171976	7999.893240	11.663309	-0.050626	4.815599
244.365212	7999.860079	11.668314	-0.050662	4.815588
244.280870	7999.888606	11.673319	-0.050646	4.815597
244.278284	7999.777541	11.678323	-0.050646	4.815565
244.513588	7999.888115	11.683328	-0.050690	4.815596
244.361901	7999.890997	11.688333	-0.050662	4.815597
244.111591	7999.867726	11.693338	-0.050615	4.815592
244.386999	7999.897816	11.698343	-0.050666	4.815599
244.450403	7999.877496	11.703347	-0.050678	4.815593
244.426238	7999.883512	11.708352	-0.050674	4.815595
244.788481	7999.827470	11.713357	-0.050741	4.815577
244.534836	7999.806280	11.718362	-0.050694	4.815572
244.492424	7999.920893	11.723367	-0.050686	4.815606
244.586875	7999.795386	11.728371	-0.050704	4.815568
244.709189	7999.875305	11.733376	-0.050727	4.815591
244.650111	7999.915986	11.738381	-0.050716	4.815603
244.478904	7999.882254	11.743386	-0.050684	4.815594
244.657043	7999.888348	11.748391	-0.050717	4.815595
244.395337	7999.872365	11.753395	-0.050668	4.815592
244.350491	7999.806520	11.758400	-0.050660	4.815573
244.482603	7999.894070	11.763405	-0.050685	4.815598
244.628819	7999.896444	11.768410	-0.050712	4.815598
244.406849	7999.807443	11.773415	-0.050671	4.815573
244.368704	7999.900773	11.778419	-0.050664	4.815600
244.449734	7999.792131	11.783424	-0.050679	4.815568
244.674635	7999.903605	11.788429	-0.050721	4.815600
244.345254	7999.784038	11.793434	-0.050659	4.815566
244.399109	7999.909820	11.798439	-0.050669	4.815603
244.454246	7999.871217	11.803443	-0.050680	4.815591
244.324096	7999.850961	11.808448	-0.050656	4.815586
244.307267	7999.842151	11.813453	-0.050652	4.815583
244.368260	7999.776954	11.818458	-0.050664	4.815564
244.428339	7999.980769	11.823463	-0.050675	4.815623
244.531079	7999.867141	11.828467	-0.050694	4.815590
244.604150	7999.846977	11.833472	-0.050708	4.815583
244.692905	7999.866568	11.838477	-0.050724	4.815589
244.479465	7999.885530	11.843482	-0.050685	4.815595
244.677932	7999.854588	11.848487	-0.050722	4.815585
244.678378	7999.910113	11.853491	-0.050722	4.815601
244.475274	7999.797931	11.858496	-0.050684	4.815570
244.482786	7999.893069	11.863501	-0.050685	4.815597
244.423914	7999.875037	11.868506	-0.050675	4.815592
244.359533	7999.799267	11.873511	-0.050663	4.815571
244.367015	7999.887999	11.878515	-0.050664	4.815596
244.424633	7999.814207	11.883520	-0.050675	4.815575
244.458607	7999.796612	11.888525	-0.050681	4.815569
244.275885	7999.879059	11.893530	-0.050647	4.815594
244.310989	7999.800631	11.898535	-0.050654	4.815571
244.645692	7999.903209	11.903539	-0.050716	4.815600
244.564362	7999.886948	11.908544	-0.050701	4.815595
244.566174	7999.904062	11.913549	-0.050701	4.815600
244.668899	7999.869433	11.918554	-0.050721	4.815590
244.648803	7999.873381	11.923559	-0.050717	4.815591
244.557810	7999.826003	11.928563	-0.050700	4.815577
244.653893	7999.803010	11.933568	-0.050718	4.815570
244.752143	7999.901755	11.938573	-0.050736	4.815599
244.414241	7999.784185	11.943578	-0.050673	4.815566
244.777419	7999.849860	11.948583	-0.050741	4.815583
244.569582	7999.862507	11.953587	-0.050702	4.815588
244.333698	7999.871497	11.958592	-0.050658	4.815592
244.440289	7999.795296	11.963597	-0.050678	4.815569
244.432517	7999.878443	11.968602	-0.050677	4.815593
244.462479	7999.906689	11.973607	-0.050683	4.815601
244.405385	7999.800078	11.978611	-0.050672	4.815571
244.574164	7999.800682	11.983616	-0.050703	4.815570
244.751054	7999.901770	11.988621	-0.050736	4.815599
244.499130	7999.890215	11.993626	-0.050689	4.815596
244.554783	7999.801445	11.998631	-0.050700	4.815570
244.673119	7999.895178	12.003635	-0.050722	4.815597
244.669994	7999.803319	12.008640	-0.050721	4.815570
244.548741	7999.891032	12.013645	-0.050699	4.815596
244.621078	7999.885803	12.018650	-0.050712	4.815595
244.789385	7999.804197	12.023655	-0.050744	4.815570
244.487078	7999.891110	12.028659	-0.050688	4.815597
244.674558	7999.878139	12.033664	-0.050722	4.815592
244.766625	7999.872162	12.038669	-0.050740	4.815590
244.597353	7999.876894	12.043674	-0.050708	4.815592
244.620283	7999.893282	12.048679	-0.050712	4.815597
244.546774	7999.790675	12.053683	-0.050699	4.815567
244.448747	7999.881967	12.058688	-0.050681	4.815594
244.545806	7999.901693	12.063693	-0.050699	4.815600
244.511369	7999.878718	12.068698	-0.050692	4.815593
244.646197	7999.878773	12.073703	-0.050717	4.815592
244.654098	7999.907728	12.078707	-0.050719	4.815601
244.499978	7999.879611	12.083712	-0.050690	4.815593
244.651827	7999.904495	12.088717	-0.050719	4.815600
244.600818	7999.878050	12.093722	-0.050709	4.815592
244.657452	7999.838403	12.098727	-0.050720	4.815581
244.848533	7999.949330	12.103731	-0.050755	4.815612
244.697440	7999.894572	12.108736	-0.050727	4.815597
244.758150	7999.843248	12.113741	-0.050739	4.815582
244.615722	7999.835604	12.118746	-0.050712	4.815580
244.543584	7999.895290	12.123751	-0.050699	4.815598
244.641530	7999.789056	12.128755	-0.050717	4.815566
244.693809	7999.975665	12.133760	-0.050727	4.815621
244.697738	7999.814528	12.138765	-0.050727	4.815573
244.654158	7999.881082	12.143770	-0.050719	4.815593
244.592038	7999.810686	12.148775	-0.050708	4.815573
244.613636	7999.900715	12.153779	-0.050712	4.815599
244.686321	7999.796207	12.158784	-0.050725	4.815568
244.740306	7999.907046	12.163789	-0.050736	4.815600
244.741140	7999.814183	12.168794	-0.050736	4.815573
244.581052	7999.837213	12.173799	-0.050706	4.815581
244.634082	7999.854089	12.178803	-0.050716	4.815585
244.652435	7999.875742	12.183808	-0.050719	4.815592
244.980442	7999.833022	12.188813	-0.050781	4.815577
244.713063	7999.895947	12.193818	-0.050731	4.815597
244.831263	7999.826340	12.198823	-0.050753	4.815576
244.662463	7999.905809	12.203827	-0.050721	4.815600
244.707297	7999.846755	12.208832	-0.050730	4.815583
244.516626	7999.947221	12.213837	-0.050694	4.815613
244.692616	7999.781402	12.218842	-0.050727	4.815564
244.840558	7999.896966	12.223847	-0.050755	4.815597
244.704570	7999.823237	12.228851	-0.050729	4.815576
244.640198	7999.902265	12.233856	-0.050718	4.815599
244.710248	7999.824403	12.238861	-0.050731	4.815576
244.748518	7999.889081	12.243866	-0.050738	4.815595
244.659977	7999.815054	12.248871	-0.050721	4.815574
244.824576	7999.834807	12.253875	-0.050752	4.815579
244.700777	7999.818925	12.258880	-0.050729	4.815575
244.634383	7999.831730	12.263885	-0.050717	4.815579
244.670491	7999.870751	12.268890	-0.050723	4.815590
244.825356	7999.894617	12.273895	-0.050752	4.815596
244.830382	7999.831715	12.278899	-0.050753	4.815578
244.677629	7999.892228	12.283904	-0.050725	4.815596
244.692149	7999.833750	12.288909	-0.050728	4.815579
244.717201	7999.797862	12.293914	-0.050732	4.815568
244.558303	7999.832654	12.298919	-0.050703	4.815579
244.805747	7999.835601	12.303923	-0.050749	4.815579
244.577432	7999.942930	12.308928	-0.050706	4.815611
244.646056	7999.853303	12.313933	-0.050719	4.815585
244.434857	7999.800774	12.318938	-0.050680	4.815571
244.767045	7999.910785	12.323943	-0.050742	4.815601
244.749968	7999.830443	12.328947	-0.050739	4.815578
244.719236	7999.826745	12.333952	-0.050733	4.815577
244.938878	7999.808958	12.338957	-0.050774	4.815571
244.901751	7999.903374	12.343962	-0.050767	4.815598
244.739446	7999.803596	12.348967	-0.050737	4.815570
244.719122	7999.887608	12.353971	-0.050733	4.815595
244.627238	7999.885054	12.358976	-0.050716	4.815594
244.728351	7999.794885	12.363981	-0.050735	4.815567
244.902957	7999.874585	12.368986	-0.050767	4.815590
244.876985	7999.902991	12.373991	-0.050763	4.815598
244.763096	7999.810404	12.378995	-0.050741	4.815572
244.560532	7999.888258	12.384000	-0.050704	4.815596
244.705543	7999.898086	12.389005	-0.050731	4.815598
244.669616	7999.888966	12.394010	-0.050724	4.815595
244.648999	7999.832053	12.399015	-0.050720	4.815579
244.605973	7999.815346	12.404019	-0.050712	4.815574
244.708141	7999.887465	12.409024	-0.050731	4.815595
244.662402	7999.822672	12.414029	-0.050723	4.815576
244.587131	7999.879104	12.419034	-0.050709	4.815593
244.745828	7999.818693	12.424039	-0.050739	4.815574
244.881427	7999.823030	12.429043	-0.050764	4.815575
244.624796	7999.906414	12.434048	-0.050716	4.815601
244.673743	7999.832480	12.439053	-0.050725	4.815579
244.691348	7999.888283	12.444058	-0.050729	4.815595
244.667711	7999.811038	12.449063	-0.050724	4.815572
244.739109	7999.916821	12.454067	-0.050738	4.815603
244.912057	7999.804330	12.459072	-0.050770	4.815569
244.906148	7999.841602	12.464077	-0.050769	4.815580
244.682802	7999.809160	12.469082	-0.050727	4.815572
244.736412	7999.922128	12.474087	-0.050737	4.815605
244.943248	7999.820862	12.479091	-0.050776	4.815574
244.793586	7999.881426	12.484096	-0.050748	4.815592
244.856394	7999.814122	12.489101	-0.050760	4.815572
244.856586	7999.792777	12.494106	-0.050760	4.815566
244.814537	7999.908464	12.499111	-0.050752	4.815600
244.945207	7999.824113	12.504115	-0.050776	4.815575
244.930065	7999.894331	12.509120	-0.050774	4.815596
245.105562	7999.839530	12.514125	-0.050806	4.815579
244.891815	7999.804040	12.519130	-0.050766	4.815569
244.661369	7999.883578	12.524135	-0.050724	4.815594
244.776901	7999.820332	12.529139	-0.050745	4.815575
244.671370	7999.877341	12.534144	-0.050726	4.815592
244.673701	7999.820801	12.539149	-0.050726	4.815575
244.707732	7999.899288	12.544154	-0.050732	4.815598
244.873805	7999.894512	12.549159	-0.050763	4.815596
244.978424	7999.895144	12.554163	-0.050783	4.815596
244.670907	7999.809025	12.559168	-0.050726	4.815572
244.852710	7999.838665	12.564173	-0.050759	4.815580
244.910777	7999.823596	12.569178	-0.050770	4.815575
244.641010	7999.857658	12.574183	-0.050720	4.815586
244.769498	7999.857609	12.579187	-0.050744	4.815586
244.633163	7999.808429	12.584192	-0.050719	4.815572
244.737034	7999.902995	12.589197	-0.050738	4.815599
244.640955	7999.871548	12.594202	-0.050720	4.815590
244.758935	7999.797667	12.599207	-0.050742	4.815568
244.779874	7999.903699	12.604211	-0.050746	4.815599
244.759329	7999.878815	12.609216	-0.050742	4.815592
245.037648	7999.803263	12.614221	-0.050794	4.815568
244.765957	7999.892808	12.619226	-0.050744	4.815596
244.876093	7999.889259	12.624231	-0.050764	4.815594
244.879753	7999.894659	12.629235	-0.050765	4.815596
244.846034	7999.883440	12.634240	-0.050759	4.815593
244.696855	7999.858605	12.639245	-0.050731	4.815586
244.684651	7999.800762	12.644250	-0.050729	4.815569
244.875761	7999.813472	12.649255	-0.050764	4.815572
244.742768	7999.849751	12.654259	-0.050740	4.815583
244.683751	7999.933136	12.659264	-0.050729	4.815608
244.719992	7999.851523	12.664269	-0.050736	4.815584
244.589551	7999.824858	12.669274	-0.050711	4.815577
244.616017	7999.848776	12.674279	-0.050716	4.815584
244.950506	7999.840325	12.679283	-0.050779	4.815580
244.910388	7999.883448	12.684288	-0.050771	4.815592
244.860843	7999.828201	12.689293	-0.050762	4.815577
244.992954	7999.900807	12.694298	-0.050787	4.815597
245.084681	7999.872406	12.699303	-0.050804	4.815588
244.768290	7999.821373	12.704307	-0.050745	4.815575
244.858917	7999.830318	12.709312	-0.050762	4.815577
244.973720	7999.893035	12.714317	-0.050783	4.815595
244.983884	7999.881460	12.719322	-0.050785	4.815592
244.803916	7999.888153	12.724327	-0.050752	4.815594
244.740789	7999.805997	12.729331	-0.050740	4.815571
244.810253	7999.895735	12.734336	-0.050753	4.815596
244.878267	7999.838124	12.739341	-0.050766	4.815579
244.847880	7999.908095	12.744346	-0.050760	4.815600
244.988905	7999.859141	12.749351	-0.050786	4.815585
244.978703	7999.872857	12.754355	-0.050784	4.815589
244.837836	7999.883387	12.759360	-0.050758	4.815593
244.927942	7999.801581	12.764365	-0.050775	4.815568
244.972166	7999.886640	12.769370	-0.050783	4.815593
244.838600	7999.891950	12.774375	-0.050758	4.815595
245.053213	7999.889028	12.779379	-0.050798	4.815593
244.866138	7999.979945	12.784384	-0.050764	4.815621
244.990382	7999.815420	12.789389	-0.050787	4.815572
245.031590	7999.886552	12.794394	-0.050795	4.815593
245.060609	7999.974568	12.799399	-0.050800	4.815618
245.028892	7999.833135	12.804403	-0.050794	4.815577
244.710676	7999.869614	12.809408	-0.050735	4.815589
245.114370	7999.901786	12.814413	-0.050810	4.815597
245.000844	7999.877529	12.819418	-0.050789	4.815590
245.067579	7999.803883	12.824423	-0.050801	4.815568
245.092470	7999.925995	12.829427	-0.050806	4.815604
244.837684	7999.886636	12.834432	-0.050759	4.815594
244.878210	7999.830714	12.839437	-0.050766	4.815577
244.967741	7999.890886	12.844442	-0.050783	4.815594
245.011699	7999.820074	12.849447	-0.050791	4.815573
245.027639	7999.917486	12.854451	-0.050794	4.815602
244.848261	7999.792877	12.859456	-0.050761	4.815566
244.892834	7999.920644	12.864461	-0.050769	4.815603
244.895517	7999.808595	12.869466	-0.050770	4.815571
244.783118	7999.806776	12.874471	-0.050749	4.815571
244.921086	7999.920045	12.879475	-0.050775	4.815603
244.991077	7999.799479	12.884480	-0.050788	4.815567
245.103274	7999.820518	12.889485	-0.050809	4.815573
244.898955	7999.905817	12.894490	-0.050771	4.815599
245.014632	7999.793465	12.899495	-0.050792	4.815566
244.850521	7999.902903	12.904499	-0.050762	4.815598
244.859245	7999.898777	12.909504	-0.050763	4.815597
244.944856	7999.836114	12.914509	-0.050779	4.815578
244.915475	7999.820694	12.919514	-0.050774	4.815574
244.981432	7999.827105	12.924519	-0.050786	4.815576
244.985245	7999.826102	12.929523	-0.050787	4.815575
245.179092	7999.902912	12.934528	-0.050823	4.815597
244.994763	7999.912737	12.939533	-0.050789	4.815601
244.938698	7999.811479	12.944538	-0.050778	4.815571
245.262473	7999.832746	12.949543	-0.050839	4.815576
245.237317	7999.852625	12.954547	-0.050834	4.815582
244.896474	7999.901548	12.959552	-0.050771	4.815598
244.806817	7999.846718	12.964557	-0.050754	4.815582
244.974234	7999.832355	12.969562	-0.050785	4.815577
244.955762	7999.828856	12.974567	-0.050782	4.815576
245.081750	7999.824497	12.979571	-0.050805	4.815574
244.880065	7999.905568	12.984576	-0.050768	4.815599
244.906217	7999.839806	12.989581	-0.050773	4.815580
244.910012	7999.814248	12.994586	-0.050773	4.815572
244.995452	7999.830583	12.999591	-0.050789	4.815577
244.921795	7999.897717	13.004595	-0.050776	4.815596
244.913303	7999.857015	13.009600	-0.050774	4.815585
245.215035	7999.881127	13.014605	-0.050830	4.815590
245.167656	7999.805631	13.019610	-0.050821	4.815568
245.023488	7999.890838	13.024615	-0.050795	4.815594
245.051059	7999.838977	13.029619	-0.050800	4.815579
245.030891	7999.878154	13.034624	-0.050796	4.815590
245.093263	7999.898385	13.039629	-0.050808	4.815596
245.112529	7999.898701	13.044634	-0.050811	4.815596
245.085131	7999.885449	13.049639	-0.050806	4.815592
245.245085	7999.832531	13.054643	-0.050836	4.815576
245.048176	7999.881653	13.059648	-0.050800	4.815591
245.329676	7999.832842	13.064653	-0.050852	4.815576
245.067621	7999.818987	13.069658	-0.050803	4.815573
244.725708	7999.814514	13.074663	-0.050740	4.815573
244.885375	7999.933472	13.079667	-0.050769	4.815607
244.856180	7999.849731	13.084672	-0.050764	4.815583
244.830111	7999.853582	13.089677	-0.050759	4.815584
244.712517	7999.801502	13.094682	-0.050737	4.815569
244.773957	7999.893246	13.099687	-0.050749	4.815596
244.992237	7999.815652	13.104691	-0.050789	4.815572
244.753289	7999.974053	13.109696	-0.050745	4.815620
244.810607	7999.858619	13.114701	-0.050756	4.815586
245.146103	7999.854455	13.119706	-0.050818	4.815583
245.123252	7999.799641	13.124711	-0.050814	4.815567
245.191604	7999.832780	13.129715	-0.050827	4.815576
245.087615	7999.905828	13.134720	-0.050807	4.815598
245.136090	7999.839359	13.139725	-0.050816	4.815578
245.013598	7999.891823	13.144730	-0.050794	4.815594
245.083772	7999.816098	13.149735	-0.050807	4.815572
245.167883	7999.919953	13.154739	-0.050823	4.815602
245.230116	7999.890006	13.159744	-0.050834	4.815593
245.211774	7999.819251	13.164749	-0.050831	4.815572
245.072845	7999.874651	13.169754	-0.050805	4.815589
245.195510	7999.816858	13.174759	-0.050828	4.815572
245.108946	7999.933960	13.179763	-0.050812	4.815606
245.052001	7999.807065	13.184768	-0.050801	4.815569
245.043959	7999.825086	13.189773	-0.050800	4.815575
245.044506	7999.889153	13.194778	-0.050800	4.815593
244.919514	7999.877521	13.199783	-0.050777	4.815591
245.144900	7999.812854	13.204787	-0.050819	4.815571
244.894799	7999.804532	13.209792	-0.050772	4.815569
244.865954	7999.920433	13.214797	-0.050767	4.815603
245.041435	7999.825065	13.219802	-0.050799	4.815575
245.065312	7999.885240	13.224807	-0.050804	4.815592
245.053493	7999.814591	13.229811	-0.050802	4.815572
245.168495	7999.895460	13.234816	-0.050823	4.815595
245.318165	7999.839173	13.239821	-0.050851	4.815577
244.961121	7999.891036	13.244826	-0.050785	4.815594
244.872718	7999.814875	13.249831	-0.050768	4.815572
245.090526	7999.841897	13.254835	-0.050809	4.815579
245.126940	7999.830747	13.259840	-0.050816	4.815576
245.047856	7999.839076	13.264845	-0.050801	4.815579
245.086688	7999.908034	13.269850	-0.050808	4.815599
244.996841	7999.892702	13.274855	-0.050792	4.815595
244.962859	7999.799275	13.279859	-0.050785	4.815567
245.003193	7999.970745	13.284864	-0.050793	4.815617
245.262017	7999.821213	13.289869	-0.050841	4.815572
245.275336	7999.813960	13.294874	-0.050844	4.815570
245.121146	7999.873382	13.299879	-0.050815	4.815588
245.100208	7999.855965	13.304883	-0.050811	4.815583
244.992154	7999.892648	13.309888	-0.050791	4.815595
245.015585	7999.878085	13.314893	-0.050795	4.815590
245.114733	7999.885035	13.319898	-0.050814	4.815592
245.127023	7999.842534	13.324903	-0.050816	4.815579
244.984345	7999.869048	13.329907	-0.050790	4.815588
244.998719	7999.807364	13.334912	-0.050792	4.815570
245.178464	7999.826296	13.339917	-0.050826	4.815574
245.155752	7999.873972	13.344922	-0.050822	4.815588
244.965151	7999.886898	13.349927	-0.050786	4.815593
245.049887	7999.924574	13.354931	-0.050802	4.815604
245.004233	7999.797862	13.359936	-0.050794	4.815567
245.106241	7999.833682	13.364941	-0.050813	4.815577
245.029421	7999.898629	13.369946	-0.050798	4.815596
245.063596	7999.800969	13.374951	-0.050805	4.815567
244.954031	7999.902751	13.379955	-0.050784	4.815598
244.998005	7999.894927	13.384960	-0.050793	4.815595
245.148490	7999.815166	13.389965	-0.050821	4.815571
245.121205	7999.904404	13.394970	-0.050816	4.815597
244.933374	7999.882145	13.399975	-0.050781	4.815592
244.954676	7999.824844	13.404979	-0.050785	4.815575
244.965283	7999.911493	13.409984	-0.050787	4.815600
245.014323	7999.818345	13.414989	-0.050796	4.815573
245.044390	7999.913850	13.419994	-0.050802	4.815601
245.046000	7999.876514	13.424999	-0.050802	4.815590
245.140664	7999.817200	13.430003	-0.050819	4.815572
245.028329	7999.894383	13.435008	-0.050799	4.815595
245.050694	7999.892614	13.440013	-0.050803	4.815594
245.056648	7999.893781	13.445018	-0.050804	4.815595
244.933752	7999.912075	13.450023	-0.050781	4.815601
245.010539	7999.840728	13.455027	-0.050795	4.815579
244.956225	7999.822769	13.460032	-0.050785	4.815574
244.841372	7999.930871	13.465037	-0.050764	4.815606
244.752291	7999.816266	13.470042	-0.050747	4.815573
244.879066	7999.879177	13.475047	-0.050771	4.815591
244.940639	7999.812921	13.480051	-0.050783	4.815572
244.728853	7999.815896	13.485056	-0.050743	4.815573
244.917965	7999.838182	13.490061	-0.050778	4.815579
244.889059	7999.836649	13.495066	-0.050773	4.815579
244.896653	7999.915776	13.500071	-0.050775	4.815602
245.044463	7999.822094	13.505075	-0.050802	4.815574
244.974761	7999.814561	13.510080	-0.050789	4.815572
245.067293	7999.930297	13.515085	-0.050807	4.815605
245.014783	7999.823757	13.520090	-0.050797	4.815574
245.031912	7999.805890	13.525095	-0.050800	4.815569
245.120159	7999.888460	13.530099	-0.050816	4.815593
245.061295	7999.845873	13.535104	-0.050805	4.815581
245.068656	7999.834252	13.540109	-0.050807	4.815577
245.077991	7999.940098	13.545114	-0.050809	4.815608
244.855523	7999.828667	13.550119	-0.050767	4.815577
245.150418	7999.837723	13.555123	-0.050822	4.815578
245.111332	7999.802930	13.560128	-0.050815	4.815568
245.003533	7999.931430	13.565133	-0.050795	4.815606
244.993956	7999.819182	13.570138	-0.050793	4.815573
245.070728	7999.789470	13.575143	-0.050808	4.815564
245.261775	7999.827801	13.580147	-0.050843	4.815574
244.852708	7999.915118	13.585152	-0.050767	4.815602
245.012194	7999.853653	13.590157	-0.050797	4.815583
245.253696	7999.847964	13.595162	-0.050842	4.815580
245.050281	7999.839331	13.600167	-0.050804	4.815579
245.122323	7999.858651	13.605171	-0.050817	4.815584
245.006796	7999.904822	13.610176	-0.050796	4.815598
244.975169	7999.834919	13.615181	-0.050790	4.815578
244.877081	7999.876035	13.620186	-0.050772	4.815590
244.975241	7999.903252	13.625191	-0.050790	4.815598
245.157728	7999.827214	13.630195	-0.050824	4.815575
244.742280	7999.888805	13.635200	-0.050747	4.815595
245.136603	7999.829013	13.640205	-0.050820	4.815575
245.333199	7999.838610	13.645210	-0.050857	4.815577
245.026532	7999.906235	13.650215	-0.050800	4.815598
245.183683	7999.875692	13.655219	-0.050829	4.815589
245.096414	7999.827306	13.660224	-0.050813	4.815575
245.184077	7999.822326	13.665229	-0.050829	4.815573
245.109690	7999.918273	13.670234	-0.050816	4.815601
245.042562	7999.886227	13.675239	-0.050803	4.815592
245.119128	7999.825552	13.680243	-0.050817	4.815574
245.061177	7999.813940	13.685248	-0.050807	4.815571
245.062806	7999.943147	13.690253	-0.050807	4.815609
245.264574	7999.859948	13.695258	-0.050845	4.815584
244.901640	7999.813498	13.700263	-0.050777	4.815572
244.973225	7999.836013	13.705267	-0.050790	4.815578
245.014531	7999.901809	13.710272	-0.050798	4.815597
244.951995	7999.830338	13.715277	-0.050786	4.815577
244.933725	7999.866342	13.720282	-0.050783	4.815587
244.947632	7999.811057	13.725287	-0.050786	4.815571
245.076495	7999.838772	13.730291	-0.050810	4.815578
244.991266	7999.911056	13.735296	-0.050794	4.815600
244.804621	7999.819423	13.740301	-0.050759	4.815574
245.181163	7999.816992	13.745306	-0.050829	4.815572
244.984066	7999.919490	13.750311	-0.050793	4.815602
244.990062	7999.856602	13.755315	-0.050794	4.815584
245.205228	7999.815256	13.760320	-0.050834	4.815571
245.122487	7999.835270	13.765325	-0.050819	4.815577
245.067066	7999.834374	13.770330	-0.050808	4.815577
245.106026	7999.919348	13.775335	-0.050816	4.815602
245.026455	7999.857209	13.780339	-0.050801	4.815584
244.859835	7999.815010	13.785344	-0.050770	4.815572
244.942146	7999.819550	13.790349	-0.050785	4.815573
245.138484	7999.843021	13.795354	-0.050822	4.815579
245.050816	7999.923807	13.800359	-0.050806	4.815603
245.077963	7999.805749	13.805363	-0.050811	4.815569
245.157018	7999.902049	13.810368	-0.050825	4.815596
245.243389	7999.839398	13.815373	-0.050841	4.815578
245.152000	7999.912650	13.820378	-0.050825	4.815600
244.909874	7999.893780	13.825383	-0.050779	4.815595
245.343073	7999.812199	13.830387	-0.050860	4.815569
244.994483	7999.903699	13.835392	-0.050795	4.815598
245.130520	7999.827975	13.840397	-0.050821	4.815575
245.286414	7999.819830	13.845402	-0.050850	4.815572
245.198502	7999.902747	13.850407	-0.050833	4.815596
245.129230	7999.839707	13.855411	-0.050820	4.815578
245.113220	7999.813829	13.860416	-0.050818	4.815571
245.116776	7999.819227	13.865421	-0.050818	4.815572
245.045693	7999.906687	13.870426	-0.050805	4.815598
244.898564	7999.805020	13.875431	-0.050778	4.815569
245.188774	7999.925028	13.880435	-0.050832	4.815603
244.980883	7999.788212	13.885440	-0.050793	4.815564
244.826397	7999.887130	13.890445	-0.050764	4.815594
245.060361	7999.796980	13.895450	-0.050808	4.815566
245.003002	7999.885730	13.900455	-0.050797	4.815592
244.942315	7999.817492	13.905459	-0.050786	4.815573
245.089201	7999.897810	13.910464	-0.050813	4.815596
245.136910	7999.908196	13.915469	-0.050822	4.815598
245.108314	7999.818058	13.920474	-0.050817	4.815572
244.836518	7999.810451	13.925479	-0.050766	4.815571
245.054551	7999.840679	13.930483	-0.050807	4.815579
245.002087	7999.908157	13.935488	-0.050797	4.815599
244.984292	7999.823533	13.940493	-0.050794	4.815574
245.007102	7999.836717	13.945498	-0.050798	4.815578
245.195810	7999.832307	13.950503	-0.050834	4.815576
245.096270	7999.824291	13.955507	-0.050815	4.815574
244.888238	7999.907394	13.960512	-0.050776	4.815599
244.906448	7999.805205	13.965517	-0.050780	4.815569
244.961271	7999.908585	13.970522	-0.050790	4.815599
244.935186	7999.797137	13.975527	-0.050785	4.815567
245.189207	7999.837557	13.980531	-0.050833	4.815577
245.241096	7999.933417	13.985536	-0.050842	4.815605
245.025645	7999.830641	13.990541	-0.050802	4.815576
245.076760	7999.841081	13.995546	-0.050812	4.815579
245.104158	7999.898111	14.000551	-0.050817	4.815596
245.210967	7999.842196	14.005555	-0.050837	4.815579
245.111543	7999.898237	14.010560	-0.050818	4.815596
245.215323	7999.816652	14.015565	-0.050838	4.815571
245.249395	7999.920763	14.020570	-0.050844	4.815601
244.964239	7999.890520	14.025575	-0.050791	4.815594
245.032261	7999.815828	14.030579	-0.050804	4.815572
245.203734	7999.817544	14.035584	-0.050836	4.815572
245.002559	7999.917840	14.040589	-0.050798	4.815602
244.971646	7999.823395	14.045594	-0.050793	4.815574
245.037480	7999.894926	14.050599	-0.050805	4.815595
244.985565	7999.812951	14.055603	-0.050795	4.815571
244.868795	7999.884724	14.060608	-0.050774	4.815593
245.028267	7999.909733	14.065613	-0.050803	4.815599
245.104174	7999.820222	14.070618	-0.050817	4.815573
244.847993	7999.992222	14.075623	-0.050770	4.815624
245.100851	7999.803094	14.080627	-0.050817	4.815568
245.187934	7999.903794	14.085632	-0.050833	4.815597
245.123306	7999.808802	14.090637	-0.050821	4.815569
244.987406	7999.919765	14.095642	-0.050796	4.815602
244.884175	7999.888202	14.100647	-0.050777	4.815594
244.998259	7999.804649	14.105651	-0.050798	4.815569
245.069238	7999.828222	14.110656	-0.050811	4.815575
244.951240	7999.951219	14.115661	-0.050789	4.815612
245.046866	7999.841744	14.120666	-0.050807	4.815579
244.874753	7999.864579	14.125671	-0.050775	4.815587
244.943449	7999.851817	14.130675	-0.050788	4.815583
245.106611	7999.818168	14.135680	-0.050818	4.815572
244.966747	7999.916256	14.140685	-0.050792	4.815601
245.059352	7999.808868	14.145690	-0.050810	4.815570
245.067994	7999.790862	14.150695	-0.050811	4.815564
245.201494	7999.923276	14.155699	-0.050836	4.815602
244.913624	7999.807582	14.160704	-0.050783	4.815570
244.833073	7999.898091	14.165709	-0.050768	4.815597
245.020048	7999.939559	14.170714	-0.050803	4.815608
244.979484	7999.870579	14.175719	-0.050795	4.815588
245.040048	7999.808577	14.180723	-0.050806	4.815570
245.171459	7999.886510	14.185728	-0.050831	4.815592
245.147445	7999.894664	14.190733	-0.050826	4.815594
245.055535	7999.824852	14.195738	-0.050809	4.815574
245.104060	7999.893967	14.200743	-0.050818	4.815594
244.951119	7999.903234	14.205747	-0.050790	4.815598
244.996930	7999.894372	14.210752	-0.050799	4.815595
245.038348	7999.913195	14.215757	-0.050806	4.815600
245.198770	7999.823988	14.220762	-0.050836	4.815573
245.006463	7999.897738	14.225767	-0.050800	4.815596
244.905010	7999.814960	14.230771	-0.050781	4.815572
245.049206	7999.900573	14.235776	-0.050808	4.815596
244.870480	7999.851772	14.240781	-0.050775	4.815583
244.785617	7999.819440	14.245786	-0.050759	4.815574
244.758542	7999.893734	14.250791	-0.050754	4.815596
244.783717	7999.897348	14.255795	-0.050759	4.815597
244.825814	7999.602317	14.260800	-0.050767	4.815510

244.899176	7996.332820	14.265805	-0.050778	4.814554
244.914443	7990.746437	14.270810	-0.050778	4.812919
244.755768	7983.920892	14.275815	-0.050744	4.810923
244.764644	7976.642449	14.280819	-0.050741	4.808791
244.807879	7969.045963	14.285824	-0.050744	4.806566
244.726536	7961.196531	14.290829	-0.050724	4.804266
244.726245	7953.386185	14.295834	-0.050718	4.801976
244.661956	7945.394542	14.300839	-0.050701	4.799632
244.770952	7937.430654	14.305843	-0.050716	4.797294
244.645525	7929.421505	14.310848	-0.050688	4.794943
244.669901	7921.367488	14.315853	-0.050687	4.792577
244.879534	7913.393338	14.320858	-0.050721	4.790232
244.567435	7905.409384	14.325863	-0.050658	4.787886
244.574229	7897.393538	14.330867	-0.050654	4.785528
244.596886	7889.441245	14.335872	-0.050653	4.783187
244.471918	7881.413506	14.340877	-0.050624	4.780823
244.506884	7873.492532	14.345882	-0.050626	4.778489
244.563767	7865.379830	14.350887	-0.050631	4.776097
244.499397	7857.381807	14.355891	-0.050614	4.773739
244.491107	7849.364147	14.360896	-0.050607	4.771373
244.180794	7841.341450	14.365901	-0.050544	4.769005
244.449758	7833.414458	14.370906	-0.050589	4.766663
244.304546	7825.399696	14.375911	-0.050557	4.764295
244.236964	7817.405733	14.380915	-0.050539	4.761931
244.334140	7809.360710	14.385920	-0.050552	4.759551
244.390792	7801.456316	14.390925	-0.050558	4.757212
244.420692	7793.358387	14.395930	-0.050558	4.754814
244.367953	7785.293129	14.400935	-0.050543	4.752424
244.277383	7777.310520	14.405939	-0.050521	4.750058
244.011707	7769.341646	14.410944	-0.050466	4.747696
243.932817	7761.277813	14.415949	-0.050446	4.745304
243.939736	7753.353545	14.420954	-0.050443	4.742951
244.122990	7745.310984	14.425959	-0.050471	4.740562
244.117499	7737.361934	14.430963	-0.050465	4.738200
244.194377	7729.345218	14.435968	-0.050474	4.735816
244.146159	7721.335529	14.440973	-0.050460	4.733434
243.973516	7713.343426	14.445978	-0.050423	4.731056
243.655121	7705.279668	14.450983	-0.050358	4.728656
243.646184	7697.304608	14.455987	-0.050352	4.726280
243.730632	7689.288306	14.460992	-0.050362	4.723890
243.554736	7681.327201	14.465997	-0.050324	4.721517
243.796861	7673.314022	14.471002	-0.050364	4.719125
243.556386	7665.353181	14.476007	-0.050314	4.716749
243.452981	7657.302439	14.481011	-0.050290	4.714345
243.533306	7649.326211	14.486016	-0.050300	4.711961
243.592999	7641.219167	14.491021	-0.050305	4.709537
243.676084	7633.344969	14.496026	-0.050316	4.707182
243.496753	7625.302816	14.501031	-0.050277	4.704775
243.518779	7617.328799	14.506035	-0.050276	4.702388
243.585198	7609.298706	14.511040	-0.050283	4.699982
243.188743	7601.336309	14.516045	-0.050204	4.697596
243.363502	7593.318273	14.521050	-0.050232	4.695191
243.441599	7585.290166	14.526055	-0.050241	4.692782
243.314788	7577.264932	14.531059	-0.050212	4.690373
243.364936	7569.280236	14.536064	-0.050216	4.687975
243.277088	7561.253142	14.541069	-0.050195	4.685563
243.312598	7553.326397	14.546074	-0.050196	4.683180
243.273678	7545.309912	14.551079	-0.050184	4.680768
243.290646	7537.328973	14.556083	-0.050182	4.678366
243.191724	7529.329808	14.561088	-0.050158	4.675957
242.933146	7521.249123	14.566093	-0.050105	4.673523
242.950721	7513.177089	14.571098	-0.050103	4.671090
243.112393	7505.185421	14.576103	-0.050128	4.668679
242.869870	7497.233425	14.581107	-0.050078	4.666280
242.820047	7489.240877	14.586112	-0.050063	4.663867
242.957089	7481.242844	14.591117	-0.050083	4.661451
243.172357	7473.230597	14.596122	-0.050118	4.659029
242.983327	7465.264468	14.601127	-0.050078	4.656621
242.833084	7457.227350	14.606131	-0.050045	4.654189
242.942768	7449.224121	14.611136	-0.050060	4.651767
242.652278	7441.188909	14.616141	-0.050001	4.649333
242.732995	7433.257837	14.621146	-0.050011	4.646930
242.683885	7425.181267	14.626151	-0.049996	4.644481
242.586315	7417.237501	14.631155	-0.049973	4.642072
242.526939	7409.256843	14.636160	-0.049957	4.639650
242.596732	7401.250797	14.641165	-0.049965	4.637219
242.515478	7393.248700	14.646170	-0.049944	4.634788
242.394398	7385.195341	14.651175	-0.049917	4.632340
242.413718	7377.193663	14.656179	-0.049915	4.629906
242.534310	7369.202444	14.661184	-0.049932	4.627474
242.387573	7361.174177	14.666189	-0.049900	4.625030
242.349387	7353.202537	14.671194	-0.049887	4.622602
242.316442	7345.170593	14.676199	-0.049876	4.620154
242.447882	7337.201299	14.681203	-0.049895	4.617724
242.311648	7329.225931	14.686208	-0.049865	4.615290
242.308881	7321.164827	14.691213	-0.049859	4.612830
242.309054	7313.146864	14.696218	-0.049854	4.610381
242.186901	7305.160820	14.701223	-0.049826	4.607940
242.063807	7297.129044	14.706227	-0.049798	4.605484
242.276162	7289.200244	14.711232	-0.049832	4.603059
242.153399	7281.163772	14.716237	-0.049804	4.600599
242.295368	7273.202636	14.721242	-0.049826	4.598161
242.166895	7265.203314	14.726247	-0.049797	4.595710
241.912313	7257.141345	14.731251	-0.049744	4.593238
241.919630	7249.110787	14.736256	-0.049740	4.590775
241.819643	7241.138675	14.741261	-0.049716	4.588328
241.841319	7233.167528	14.746266	-0.049715	4.585881
241.728063	7225.131897	14.751271	-0.049689	4.583412
241.847451	7217.147736	14.756275	-0.049706	4.580958
242.007081	7209.133195	14.761280	-0.049731	4.578493
241.711206	7201.132448	14.766285	-0.049670	4.576031
241.638300	7193.102954	14.771290	-0.049651	4.573558
241.827380	7185.095159	14.776295	-0.049682	4.571092
241.673581	7177.063522	14.781299	-0.049648	4.568616
241.515310	7169.134494	14.786304	-0.049613	4.566170
241.479080	7161.045420	14.791309	-0.049601	4.563674
241.538819	7153.157521	14.796314	-0.049607	4.561239
241.449744	7145.159297	14.801319	-0.049585	4.558768
241.335728	7137.190814	14.806323	-0.049559	4.556305
241.505908	7129.178885	14.811328	-0.049585	4.553828
241.349349	7121.112380	14.816333	-0.049551	4.551332
241.306145	7113.107244	14.821338	-0.049538	4.548854
241.445238	7105.114574	14.826343	-0.049559	4.546378
241.308172	7097.107623	14.831347	-0.049528	4.543897
241.220605	7089.165214	14.836352	-0.049506	4.541434
241.135237	7081.088313	14.841357	-0.049485	4.538928
241.414659	7073.167484	14.846362	-0.049532	4.536469
241.237840	7065.126145	14.851367	-0.049494	4.533972
241.129735	7057.085849	14.856371	-0.049469	4.531473
241.247003	7049.108736	14.861376	-0.049485	4.528993
241.368988	7041.093786	14.866381	-0.049503	4.526499
241.276186	7033.134888	14.871386	-0.049481	4.524022
241.251926	7025.158845	14.876391	-0.049471	4.521538
241.170939	7017.110509	14.881395	-0.049451	4.519029
241.013202	7009.178392	14.886400	-0.049416	4.516556
240.866903	7001.077517	14.891405	-0.049384	4.514028
241.076644	6993.042339	14.896410	-0.049417	4.511521
240.907956	6985.050687	14.901415	-0.049381	4.509024
240.812410	6977.059915	14.906419	-0.049358	4.506527
240.953791	6969.064563	14.911424	-0.049379	4.504027
240.930446	6961.097019	14.916429	-0.049370	4.501535
240.645784	6953.088426	14.921434	-0.049311	4.499027
240.745052	6945.096789	14.926439	-0.049325	4.496525
240.670965	6937.060421	14.931443	-0.049306	4.494006
240.775695	6929.057721	14.936448	-0.049320	4.491497
240.624332	6921.011252	14.941453	-0.049287	4.488973
240.651224	6913.098833	14.946458	-0.049286	4.486489
240.580352	6905.049686	14.951463	-0.049268	4.483961
240.404814	6897.068783	14.956467	-0.049230	4.481452
240.454475	6889.081091	14.961472	-0.049234	4.478941
240.363566	6881.075584	14.966477	-0.049212	4.476422
240.500480	6873.054261	14.971482	-0.049233	4.473898
240.364244	6865.019681	14.976487	-0.049202	4.471367
240.499572	6857.002452	14.981491	-0.049222	4.468841
240.425361	6849.076286	14.986496	-0.049203	4.466341
240.130395	6841.002875	14.991501	-0.049143	4.463793
240.360856	6833.073226	14.996506	-0.049181	4.461291
240.148355	6825.031808	15.001511	-0.049136	4.458750
240.088689	6817.044524	15.006515	-0.049120	4.456226
240.238018	6809.046334	15.011520	-0.049142	4.453697
240.248983	6801.013959	15.016525	-0.049139	4.451156
240.205711	6793.013500	15.021530	-0.049126	4.448623
240.173980	6785.016485	15.026535	-0.049115	4.446090
240.165410	6777.004042	15.031539	-0.049108	4.443550
240.050997	6769.051760	15.036544	-0.049082	4.441028
239.806966	6761.051731	15.041549	-0.049031	4.438489
240.094821	6753.034216	15.046554	-0.049079	4.435944
239.766965	6745.001413	15.051559	-0.049013	4.433391
239.629765	6736.935291	15.056563	-0.048982	4.430827
239.811905	6729.001746	15.061568	-0.049011	4.428305
239.699479	6720.975971	15.066573	-0.048985	4.425750
239.671767	6712.968322	15.071578	-0.048975	4.423200
239.518675	6704.996595	15.076583	-0.048941	4.420660
239.616685	6697.005113	15.081587	-0.048954	4.418113
239.741264	6689.005076	15.086592	-0.048972	4.415562
239.478738	6680.974621	15.091597	-0.048918	4.412998
239.824852	6672.958823	15.096602	-0.048977	4.410440
239.807733	6664.978786	15.101607	-0.048969	4.407890
239.655192	6656.969462	15.106611	-0.048935	4.405329
239.753363	6649.059284	15.111616	-0.048948	4.402799
239.540205	6640.995957	15.116621	-0.048904	4.400217
239.517639	6633.059964	15.121626	-0.048894	4.397676
239.406735	6625.025863	15.126631	-0.048868	4.395101
239.246639	6616.989583	15.131635	-0.048833	4.392523
239.455678	6608.982786	15.136640	-0.048867	4.389956
239.207335	6600.994497	15.141645	-0.048816	4.387390
239.239824	6592.972943	15.146650	-0.048817	4.384814
239.414139	6585.006956	15.151655	-0.048844	4.382255
238.925829	6576.985806	15.156659	-0.048748	4.379672
239.107004	6569.035836	15.161664	-0.048776	4.377116
239.224018	6560.996637	15.166669	-0.048793	4.374528
239.132687	6552.976728	15.171674	-0.048771	4.371944
239.042950	6544.943178	15.176679	-0.048749	4.369354
239.108654	6537.019837	15.181683	-0.048756	4.366799
239.157446	6528.996025	15.186688	-0.048760	4.364210
238.799983	6521.031306	15.191693	-0.048688	4.361636
238.998639	6513.012151	15.196698	-0.048720	4.359046
239.084974	6505.032756	15.201703	-0.048731	4.356467
238.827662	6496.942449	15.206707	-0.048678	4.353848
238.758588	6488.903432	15.211712	-0.048660	4.351246
238.744245	6480.900902	15.216717	-0.048652	4.348654
238.954107	6472.936070	15.221722	-0.048686	4.346074
238.532067	6464.940985	15.226727	-0.048602	4.343479
238.747125	6456.966261	15.231731	-0.048637	4.340893
238.646515	6449.000054	15.236736	-0.048613	4.338306
238.273395	6440.942662	15.241741	-0.048538	4.335686
238.513666	6432.957646	15.246746	-0.048578	4.333092
238.486829	6424.954382	15.251751	-0.048568	4.330489
238.347837	6416.944040	15.256755	-0.048537	4.327881
238.377788	6408.958787	15.261760	-0.048537	4.325281
238.440888	6400.986208	15.266765	-0.048544	4.322684
238.396777	6392.955735	15.271770	-0.048530	4.320066
238.198416	6384.991087	15.276775	-0.048488	4.317466
238.167379	6376.952885	15.281779	-0.048477	4.314842
238.393956	6368.935584	15.286784	-0.048514	4.312225
238.273097	6360.901605	15.291789	-0.048486	4.309599
238.301033	6352.953053	15.296794	-0.048486	4.306999
238.452276	6344.902389	15.301799	-0.048509	4.304366
238.206016	6336.962424	15.306803	-0.048458	4.301765
238.305049	6328.933268	15.311808	-0.048472	4.299135
237.979033	6320.958402	15.316813	-0.048406	4.296518
238.086523	6312.945519	15.321818	-0.048421	4.293891
237.965501	6304.927955	15.326823	-0.048393	4.291258
238.008249	6296.909376	15.331827	-0.048396	4.288625
238.160229	6288.902458	15.336832	-0.048419	4.285995
237.956117	6280.934115	15.341837	-0.048376	4.283373
237.881012	6272.934243	15.346842	-0.048356	4.280741
238.034885	6264.962819	15.351847	-0.048380	4.278117
237.791414	6256.922224	15.356851	-0.048329	4.275467
237.869874	6248.880197	15.361856	-0.048339	4.272816
237.735923	6240.851570	15.366861	-0.048309	4.270167
237.716719	6232.853312	15.371866	-0.048300	4.267527
237.457527	6224.895730	15.376871	-0.048246	4.264897
237.736120	6216.889967	15.381875	-0.048293	4.262254
237.804649	6208.915528	15.386880	-0.048301	4.259617
237.641544	6200.907996	15.391885	-0.048265	4.256967
237.542757	6192.930152	15.396890	-0.048242	4.254324
237.472909	6184.887736	15.401895	-0.048223	4.251659
237.469688	6176.881494	15.406899	-0.048218	4.249005
237.272876	6168.930864	15.411904	-0.048176	4.246366
237.166064	6160.902791	15.416909	-0.048151	4.243701
237.394533	6152.958603	15.421914	-0.048188	4.241065
237.470389	6144.911884	15.426919	-0.048197	4.238391
237.369181	6136.929766	15.431923	-0.048173	4.235736
237.631601	6128.948704	15.436928	-0.048217	4.233083
237.267064	6120.879332	15.441933	-0.048144	4.230393
237.237658	6112.944028	15.446938	-0.048133	4.227749
237.487433	6104.930539	15.451943	-0.048174	4.225080
237.281823	6096.963670	15.456947	-0.048131	4.222420
237.224552	6088.958189	15.461952	-0.048115	4.219747
237.049005	6080.972596	15.466957	-0.048077	4.217078
237.132889	6072.915147	15.471962	-0.048088	4.214386
237.098919	6064.951350	15.476967	-0.048076	4.211722
236.780973	6056.894105	15.481971	-0.048012	4.209023
237.044253	6048.959300	15.486976	-0.048056	4.206369
237.087752	6040.943113	15.491981	-0.048059	4.203683
236.980586	6032.948866	15.496986	-0.048033	4.201002
237.016403	6024.986889	15.501991	-0.048035	4.198331
237.062677	6016.956198	15.506995	-0.048038	4.195635
237.010511	6008.884561	15.512000	-0.048023	4.192923
236.979556	6000.830493	15.517005	-0.048013	4.190215
237.041486	5992.892772	15.522010	-0.048019	4.187546
236.915257	5984.895745	15.527015	-0.047990	4.184853
236.823626	5976.901866	15.532019	-0.047968	4.182160
236.984295	5968.912284	15.537024	-0.047993	4.179469
236.655978	5960.958789	15.542029	-0.047926	4.176783
236.442141	5952.894830	15.547034	-0.047881	4.174059
236.379355	5944.900488	15.552039	-0.047865	4.171359
236.439182	5936.867508	15.557043	-0.047871	4.168645
236.572005	5928.922188	15.562048	-0.047890	4.165960
236.397818	5920.929680	15.567053	-0.047852	4.163254
236.550047	5912.934025	15.572058	-0.047876	4.160549
236.316261	5904.963270	15.577063	-0.047827	4.157846
236.186014	5896.916878	15.582067	-0.047798	4.155117
236.383666	5888.907647	15.587072	-0.047829	4.152402
236.229770	5880.866251	15.592077	-0.047795	4.149671
236.131206	5872.876969	15.597082	-0.047772	4.146956
236.003249	5864.909618	15.602087	-0.047743	4.144246
236.140531	5856.903217	15.607091	-0.047763	4.141525
236.157845	5848.905411	15.612096	-0.047761	4.138803
236.016039	5840.913099	15.617101	-0.047730	4.136079
235.959353	5832.890066	15.622106	-0.047714	4.133345
236.071259	5824.857999	15.627111	-0.047730	4.130607
235.864154	5816.876734	15.632115	-0.047686	4.127881
236.153814	5808.882557	15.637120	-0.047735	4.125155
236.054923	5800.896963	15.642125	-0.047711	4.122425
235.820749	5792.917172	15.647130	-0.047662	4.119693
235.843687	5784.997021	15.652135	-0.047661	4.116984
235.729113	5776.911316	15.657139	-0.047635	4.114214
235.722339	5768.887163	15.662144	-0.047628	4.111465
235.519377	5760.882205	15.667149	-0.047585	4.108718
235.850957	5752.872308	15.672154	-0.047642	4.105974
235.750213	5744.899666	15.677159	-0.047618	4.103236
235.620645	5736.906250	15.682163	-0.047589	4.100488
235.681118	5728.928143	15.687168	-0.047595	4.097746
235.615286	5720.898579	15.692173	-0.047577	4.094983
235.528567	5712.923339	15.697178	-0.047556	4.092237
235.451803	5704.933171	15.702183	-0.047537	4.089484
235.582010	5696.912180	15.707187	-0.047556	4.086721
235.604197	5688.937048	15.712192	-0.047555	4.083970
235.250401	5680.972336	15.717197	-0.047484	4.081216
235.382413	5672.981936	15.722202	-0.047503	4.078458
235.312049	5664.989693	15.727207	-0.047485	4.075695
235.219359	5656.916280	15.732211	-0.047462	4.072901
235.067325	5648.919398	15.737216	-0.047429	4.070132
235.167395	5640.923138	15.742221	-0.047442	4.067364
235.136108	5632.911564	15.747226	-0.047431	4.064587
235.140663	5624.974199	15.752231	-0.047427	4.061834
235.112842	5616.930251	15.757235	-0.047417	4.059042
235.141767	5608.991044	15.762240	-0.047417	4.056285
235.107652	5600.934138	15.767245	-0.047405	4.053485
235.119334	5592.936538	15.772250	-0.047402	4.050704
235.226718	5584.931426	15.777255	-0.047417	4.047919
234.899779	5576.935860	15.782259	-0.047351	4.045130
234.885870	5568.981875	15.787264	-0.047343	4.042358
234.904033	5560.936227	15.792269	-0.047341	4.039553
234.902038	5552.961426	15.797274	-0.047336	4.036770
234.772440	5544.931506	15.802279	-0.047307	4.033964
234.551153	5536.847803	15.807283	-0.047260	4.031136
234.730014	5528.863106	15.812288	-0.047288	4.028346
234.643107	5520.889258	15.817293	-0.047267	4.025554
234.698640	5512.937897	15.822298	-0.047272	4.022771
234.664958	5504.929167	15.827303	-0.047261	4.019964
234.446316	5496.943151	15.832307	-0.047215	4.017160
234.491510	5488.936832	15.837312	-0.047218	4.014351
234.729627	5480.900814	15.842317	-0.047257	4.011533
234.657884	5472.898479	15.847322	-0.047239	4.008720
234.438620	5464.940402	15.852327	-0.047193	4.005918
234.417004	5456.912524	15.857331	-0.047183	4.003092
234.516825	5448.957475	15.862336	-0.047197	4.000292
234.128220	5440.953230	15.867341	-0.047119	3.997465
234.151802	5432.916435	15.872346	-0.047118	3.994631
234.216239	5424.913525	15.877351	-0.047125	3.991808
234.198191	5416.891795	15.882355	-0.047117	3.988975
234.070727	5408.925900	15.887360	-0.047088	3.986158
234.074994	5400.928665	15.892365	-0.047083	3.983330
234.101458	5392.929020	15.897370	-0.047083	3.980499
233.888258	5384.982466	15.902375	-0.047038	3.977681
234.101808	5376.921976	15.907379	-0.047073	3.974828
234.223895	5368.930486	15.912384	-0.047091	3.971995
233.801842	5360.923961	15.917389	-0.047007	3.969147
234.113411	5352.942768	15.922394	-0.047060	3.966317
234.131132	5344.978620	15.927399	-0.047058	3.963487
234.050168	5336.960865	15.932403	-0.047037	3.960634
233.806487	5329.025193	15.937408	-0.046987	3.957805
233.670195	5321.021746	15.942413	-0.046956	3.954951
233.714820	5312.923385	15.947418	-0.046959	3.952065
233.774081	5304.947444	15.952423	-0.046965	3.949221
233.730435	5296.941200	15.957427	-0.046952	3.946363
233.842359	5288.971543	15.962432	-0.046968	3.943517
233.508323	5281.020095	15.967437	-0.046900	3.940669
233.596669	5272.997700	15.972442	-0.046912	3.937800
233.646865	5264.991743	15.977447	-0.046916	3.934935
233.412303	5256.965812	15.982451	-0.046867	3.932055
233.464924	5248.993212	15.987456	-0.046872	3.929198
233.289117	5241.014453	15.992461	-0.046834	3.926332
233.508998	5233.001543	15.997466	-0.046869	3.923459
233.634559	5225.020062	16.002471	-0.046888	3.920593
233.462393	5217.026606	16.007475	-0.046850	3.917715
233.531258	5209.008527	16.012480	-0.046858	3.914831
233.426586	5200.990537	16.017485	-0.046833	3.911942
233.300278	5192.978774	16.022490	-0.046805	3.909052
233.350982	5184.992369	16.027495	-0.046809	3.906173
233.275913	5177.004553	16.032499	-0.046790	3.903288
233.080492	5169.016009	16.037504	-0.046748	3.900399
233.218235	5161.004773	16.042509	-0.046769	3.897506
233.223525	5152.999506	16.047514	-0.046765	3.894610
233.060452	5145.012542	16.052519	-0.046729	3.891716
232.906995	5136.965616	16.057523	-0.046695	3.888798
233.241360	5128.990941	16.062528	-0.046752	3.885913
233.216562	5121.026618	16.067533	-0.046743	3.883023
233.045299	5113.021943	16.072538	-0.046705	3.880113
233.090386	5105.076128	16.077543	-0.046709	3.877227
233.065018	5096.997553	16.082547	-0.046699	3.874289
232.980225	5088.771409	16.087552	-0.046678	3.871294
232.797492	5080.855210	16.092557	-0.046639	3.868407
232.930755	5072.889221	16.097562	-0.046658	3.865506
232.961105	5064.984427	16.102567	-0.046659	3.862624
232.787572	5056.954805	16.107571	-0.046621	3.859689
232.795560	5049.009354	16.112576	-0.046618	3.856787
232.745770	5041.007351	16.117581	-0.046603	3.853861
232.431494	5032.979229	16.122586	-0.046539	3.850918
232.704167	5025.040592	16.127591	-0.046585	3.848017
232.568771	5016.967974	16.132595	-0.046555	3.845056
232.365805	5009.076501	16.137600	-0.046512	3.842158
232.402080	5001.050882	16.142605	-0.046513	3.839214
232.353132	4993.077868	16.147610	-0.046499	3.836285
232.403769	4985.073056	16.152615	-0.046503	3.833344
232.283106	4977.020484	16.157619	-0.046476	3.830379
232.240543	4969.049440	16.162624	-0.046462	3.827444
232.218280	4961.034236	16.167629	-0.046453	3.824491
232.118833	4953.065230	16.172634	-0.046429	3.821551
232.170979	4945.086049	16.177639	-0.046434	3.818609
232.123779	4937.084944	16.182643	-0.046420	3.815653
232.228144	4929.119268	16.187648	-0.046434	3.812712
232.106926	4921.045415	16.192653	-0.046407	3.809724
232.195549	4913.086273	16.197658	-0.046418	3.806780
232.233792	4905.082284	16.202663	-0.046420	3.803816
232.231121	4897.128185	16.207667	-0.046414	3.800868
231.990973	4889.141285	16.212672	-0.046364	3.797900
231.766523	4881.153083	16.217677	-0.046317	3.794929
231.761181	4873.064149	16.222682	-0.046311	3.791924
231.755280	4865.082382	16.227687	-0.046305	3.788956
231.682254	4857.072317	16.232691	-0.046286	3.785973
231.738832	4849.091829	16.237696	-0.046291	3.783002
231.571809	4841.095886	16.242701	-0.046255	3.780018
231.624180	4833.104800	16.247706	-0.046260	3.777039
231.662068	4825.082426	16.252711	-0.046262	3.774045
231.348070	4817.117030	16.257715	-0.046198	3.771061
231.594351	4809.091369	16.262720	-0.046239	3.768066
231.552597	4801.083768	16.267725	-0.046226	3.765069
231.437933	4793.128707	16.272730	-0.046199	3.762087
231.549826	4785.100286	16.277735	-0.046215	3.759080
231.391321	4777.155674	16.282739	-0.046180	3.756097
231.397955	4769.110791	16.287744	-0.046176	3.753077
231.359876	4761.078487	16.292749	-0.046164	3.750058
231.343399	4753.109425	16.297754	-0.046156	3.747061
231.397182	4745.119139	16.302759	-0.046161	3.744056
231.174999	4737.149242	16.307763	-0.046114	3.741049
231.132673	4729.185307	16.312768	-0.046101	3.738046
231.242031	4721.155350	16.317773	-0.046116	3.735020
231.026163	4713.140044	16.322778	-0.046071	3.731989
231.200922	4705.137113	16.327783	-0.046098	3.728969
231.237160	4697.129608	16.332787	-0.046100	3.725942
231.352950	4689.185366	16.337792	-0.046116	3.722938
231.275585	4681.194773	16.342797	-0.046097	3.719910
231.104523	4673.215100	16.347802	-0.046059	3.716881
231.121082	4665.186324	16.352807	-0.046057	3.713835
230.809988	4657.102299	16.357811	-0.045994	3.710758
231.124102	4649.120092	16.362816	-0.046048	3.707733
230.954264	4641.119939	16.367821	-0.046011	3.704686
230.812551	4633.205784	16.372826	-0.045979	3.701670
230.858398	4625.252289	16.377831	-0.045983	3.698642
230.874373	4617.218034	16.382835	-0.045980	3.695579
230.649750	4609.219355	16.387840	-0.045933	3.692521
230.534688	4601.198112	16.392845	-0.045907	3.689455
230.603835	4593.226924	16.397850	-0.045915	3.686410
230.602589	4585.240048	16.402855	-0.045909	3.683355
230.366233	4577.247743	16.407859	-0.045860	3.680289
230.519718	4569.259799	16.412864	-0.045883	3.677232
230.328616	4561.264888	16.417869	-0.045843	3.674162
230.355033	4553.226369	16.422874	-0.045842	3.671077
230.342370	4545.260600	16.427879	-0.045835	3.668017
230.517172	4537.200350	16.432883	-0.045862	3.664923
230.267419	4529.270484	16.437888	-0.045810	3.661865
230.150426	4521.269460	16.442893	-0.045784	3.658781
230.135541	4513.242374	16.447898	-0.045776	3.655687
230.177991	4505.271574	16.452903	-0.045778	3.652613
230.084120	4497.228704	16.457907	-0.045756	3.649505
230.087685	4489.274876	16.462912	-0.045751	3.646432
230.014963	4481.274914	16.467917	-0.045732	3.643336
230.262967	4473.288657	16.472922	-0.045773	3.640252
229.939803	4465.344606	16.477927	-0.045708	3.637166
229.889879	4457.291076	16.482931	-0.045694	3.634042
229.966833	4449.252547	16.487936	-0.045703	3.630924
229.884127	4441.283471	16.492941	-0.045682	3.627827
229.523023	4433.266085	16.497946	-0.045610	3.624701
229.854300	4425.297784	16.502951	-0.045666	3.621610
229.622818	4417.290032	16.507955	-0.045618	3.618485
229.795693	4409.308789	16.512960	-0.045645	3.615379
229.838096	4401.313972	16.517965	-0.045648	3.612262
229.707504	4393.268787	16.522970	-0.045618	3.609118
229.626630	4385.330162	16.527975	-0.045598	3.606013
229.376355	4377.347472	16.532979	-0.045546	3.602884
229.593758	4369.368645	16.537984	-0.045582	3.599767
229.363129	4361.416854	16.542989	-0.045533	3.596646
229.410429	4353.370095	16.547994	-0.045537	3.593492
229.571752	4345.365888	16.552999	-0.045562	3.590355
229.406567	4337.376350	16.558003	-0.045526	3.587212
229.323039	4329.395112	16.563008	-0.045505	3.584072
229.164305	4321.448590	16.568013	-0.045471	3.580941
229.107467	4313.424009	16.573018	-0.045455	3.577779
228.985909	4305.432663	16.578023	-0.045427	3.574625
228.934013	4297.425918	16.583027	-0.045412	3.571465
229.382549	4289.383961	16.588032	-0.045490	3.568302
229.217849	4281.413096	16.593037	-0.045455	3.565147
228.968907	4273.446128	16.598042	-0.045403	3.561988
229.071014	4265.466634	16.603047	-0.045417	3.558832
228.890570	4257.450601	16.608051	-0.045378	3.555650
228.844567	4249.391691	16.613056	-0.045364	3.552452
228.898500	4241.358539	16.618061	-0.045369	3.549265
228.944447	4233.384230	16.623066	-0.045373	3.546097
228.872331	4225.428248	16.628071	-0.045354	3.542931
228.789168	4217.417533	16.633075	-0.045333	3.539740
228.853432	4209.471883	16.638080	-0.045340	3.536576
228.614255	4201.469418	16.643085	-0.045291	3.533377
228.448842	4193.447610	16.648090	-0.045255	3.530171
228.777229	4185.451859	16.653095	-0.045311	3.526986
228.753811	4177.429916	16.658099	-0.045301	3.523778
228.472147	4169.523138	16.663104	-0.045243	3.520604
228.327310	4161.565619	16.668109	-0.045211	3.517412
228.521446	4153.475732	16.673114	-0.045242	3.514174
228.366991	4145.526584	16.678119	-0.045208	3.510979
228.297644	4137.520693	16.683123	-0.045190	3.507761
228.400440	4129.494115	16.688128	-0.045204	3.504537
228.210699	4121.551859	16.693133	-0.045164	3.501335
227.934729	4113.574861	16.698138	-0.045107	3.498113
228.202133	4105.584646	16.703143	-0.045152	3.494900
228.151941	4097.547615	16.708147	-0.045137	3.491655
227.962347	4089.570726	16.713152	-0.045097	3.488427
227.905211	4081.593994	16.718157	-0.045081	3.485200
227.905237	4073.603215	16.723162	-0.045076	3.481966
227.996466	4065.618058	16.728167	-0.045088	3.478734
227.999034	4057.611895	16.733171	-0.045083	3.475488
228.033824	4049.561447	16.738176	-0.045084	3.472222
228.131298	4041.565817	16.743181	-0.045097	3.468978
227.842792	4033.577696	16.748186	-0.045038	3.465721
227.824181	4025.634698	16.753191	-0.045030	3.462487
227.881688	4017.613366	16.758195	-0.045035	3.459222
227.796224	4009.646271	16.763200	-0.045014	3.455970
227.688210	4001.654890	16.768205	-0.044989	3.452705
227.646115	3993.602403	16.773210	-0.044976	3.449415
227.688915	3985.673627	16.778215	-0.044979	3.446174
227.499966	3977.669677	16.783219	-0.044938	3.442892
227.538609	3969.686188	16.788224	-0.044940	3.439622
227.477772	3961.711530	16.793229	-0.044924	3.436350
227.333619	3953.678321	16.798234	-0.044892	3.433048
227.380104	3945.669969	16.803239	-0.044895	3.429759
227.364246	3937.688813	16.808243	-0.044887	3.426477
227.536146	3929.671831	16.813248	-0.044914	3.423182
227.367663	3921.733713	16.818253	-0.044877	3.419906
227.276345	3913.725034	16.823258	-0.044855	3.416600
227.293228	3905.715951	16.828263	-0.044853	3.413294
227.147555	3897.705463	16.833267	-0.044821	3.409978
227.398053	3889.724949	16.838272	-0.044862	3.406686
227.330775	3881.771753	16.843277	-0.044845	3.403391
227.228732	3873.765956	16.848282	-0.044821	3.400069
227.076764	3865.854957	16.853287	-0.044787	3.396782
227.069979	3857.789210	16.858291	-0.044781	3.393432
226.884689	3849.720183	16.863296	-0.044741	3.390072
226.971172	3841.751069	16.868301	-0.044752	3.386759
226.950089	3833.750859	16.873306	-0.044743	3.383426
226.976057	3825.810696	16.878311	-0.044742	3.380117
226.891909	3817.849518	16.883315	-0.044722	3.376792
226.946612	3809.805970	16.888320	-0.044727	3.373434
226.924513	3801.818753	16.893325	-0.044717	3.370093
226.867900	3793.842422	16.898330	-0.044702	3.366753
226.894925	3785.854954	16.903335	-0.044701	3.363407
226.739130	3777.884432	16.908339	-0.044667	3.360059
226.710744	3769.905017	16.913344	-0.044657	3.356708
226.586004	3761.916655	16.918349	-0.044628	3.353347
226.602096	3753.849266	16.923354	-0.044626	3.349954
226.726095	3745.887406	16.928359	-0.044644	3.346605
226.711976	3737.888453	16.933363	-0.044636	3.343233
226.407739	3729.933931	16.938368	-0.044575	3.339866
226.439912	3721.964877	16.943373	-0.044575	3.336501
226.496461	3713.895438	16.948378	-0.044581	3.333092
226.361270	3705.936565	16.953383	-0.044550	3.329719
226.377132	3697.942359	16.958387	-0.044548	3.326332
226.333121	3689.973333	16.963392	-0.044535	3.322951
226.326481	3681.978275	16.968397	-0.044528	3.319557
226.321100	3674.012584	16.973402	-0.044522	3.316172
226.311187	3665.994550	16.978407	-0.044515	3.312761
226.061231	3657.965795	16.983411	-0.044463	3.309333
225.984869	3650.010559	16.988416	-0.044444	3.305939
226.102527	3642.019173	16.993421	-0.044461	3.302533
226.015556	3634.018470	16.998426	-0.044439	3.299112
225.919929	3626.080888	17.003431	-0.044417	3.295715
225.835335	3618.067445	17.008435	-0.044396	3.292281
225.837244	3610.062635	17.013440	-0.044391	3.288852
225.815066	3602.098176	17.018445	-0.044381	3.285435
225.732527	3594.111135	17.023450	-0.044361	3.282002
225.711429	3586.145080	17.028455	-0.044352	3.278577
225.707024	3578.132908	17.033459	-0.044346	3.275129
225.690516	3570.112894	17.038464	-0.044338	3.271674
225.692496	3562.125007	17.043469	-0.044333	3.268230
225.673619	3554.115640	17.048474	-0.044324	3.264772
225.567230	3546.184160	17.053479	-0.044299	3.261341
225.428781	3538.168080	17.058483	-0.044268	3.257868
225.507409	3530.160128	17.063488	-0.044278	3.254403
225.268766	3522.199961	17.068493	-0.044228	3.250943
225.533385	3514.174627	17.073498	-0.044272	3.247471
225.484836	3506.199637	17.078503	-0.044258	3.244005
225.282579	3498.225197	17.083507	-0.044215	3.240529
225.196850	3490.281566	17.088512	-0.044194	3.237067
225.309816	3482.238494	17.093517	-0.044210	3.233566
225.355925	3474.150237	17.098522	-0.044213	3.230040
225.189109	3466.214997	17.103527	-0.044177	3.226567
225.078015	3458.235353	17.108531	-0.044151	3.223073
225.133589	3450.242367	17.113536	-0.044156	3.219577
225.050111	3442.306716	17.118541	-0.044136	3.216096
224.905664	3434.290127	17.123546	-0.044104	3.212574
225.029148	3426.296194	17.128551	-0.044121	3.209068
224.997018	3418.300815	17.133555	-0.044110	3.205552
224.859505	3410.361792	17.138560	-0.044079	3.202052
224.808376	3402.382948	17.143565	-0.044065	3.198535
224.894551	3394.359521	17.148570	-0.044076	3.194999
224.968020	3386.365932	17.153575	-0.044084	3.191473
224.906953	3378.352355	17.158579	-0.044068	3.187928
224.765432	3370.368121	17.163584	-0.044036	3.184388
224.657135	3362.450216	17.168589	-0.044011	3.180876
224.476763	3354.443221	17.173594	-0.043972	3.177317
224.825634	3346.425934	17.178599	-0.044032	3.173772
224.498312	3338.434968	17.183603	-0.043966	3.170205
224.358489	3330.459566	17.188608	-0.043935	3.166650
224.533094	3322.478131	17.193613	-0.043962	3.163102
224.549578	3314.455864	17.198618	-0.043960	3.159524
224.461389	3306.533917	17.203623	-0.043938	3.155983
224.222208	3298.509994	17.208627	-0.043888	3.152385
224.356331	3290.477712	17.213632	-0.043908	3.148796
224.507995	3282.493895	17.218637	-0.043931	3.145226
224.212863	3274.535061	17.223642	-0.043871	3.141643
224.369248	3266.564716	17.228647	-0.043895	3.138070
224.095013	3258.586082	17.233651	-0.043839	3.134471
223.946767	3250.607097	17.238656	-0.043806	3.130873
223.891505	3242.611555	17.243661	-0.043791	3.127267
224.030234	3234.588073	17.248666	-0.043811	3.123653
223.960189	3226.647023	17.253671	-0.043793	3.120063
223.862178	3218.671701	17.258675	-0.043770	3.116452
223.942913	3210.645830	17.263680	-0.043780	3.112822
224.046989	3202.642786	17.268685	-0.043794	3.109200
223.800615	3194.675812	17.273690	-0.043743	3.105573
223.930990	3186.696321	17.278695	-0.043762	3.101954
223.781041	3178.732267	17.283699	-0.043729	3.098324
223.580790	3170.746368	17.288704	-0.043686	3.094679
223.689843	3162.743608	17.293709	-0.043701	3.091035
223.699272	3154.723377	17.298714	-0.043698	3.087374
223.653907	3146.766673	17.303719	-0.043684	3.083736
223.443569	3138.803370	17.308723	-0.043640	3.080083
223.543286	3130.840620	17.313728	-0.043654	3.076440
223.648236	3122.782636	17.318733	-0.043668	3.072749
223.447360	3114.735555	17.323738	-0.043625	3.069044
223.402996	3106.769859	17.328743	-0.043612	3.065380
223.464298	3098.809681	17.333747	-0.043618	3.061719
223.311863	3090.845021	17.338752	-0.043585	3.058041
223.194074	3082.891873	17.343757	-0.043557	3.054366
223.300514	3074.857075	17.348762	-0.043572	3.050659
223.404122	3066.890296	17.353767	-0.043586	3.046979
223.230525	3058.931398	17.358771	-0.043549	3.043285
223.432177	3050.939392	17.363776	-0.043581	3.039589
223.252472	3043.003928	17.368781	-0.043543	3.035897
223.167117	3034.968391	17.373786	-0.043521	3.032158
223.131114	3026.986620	17.378791	-0.043510	3.028442
223.102463	3019.007873	17.383795	-0.043499	3.024723
223.008977	3011.035026	17.388800	-0.043477	3.020999
222.948267	3003.061281	17.393805	-0.043460	3.017272
223.012648	2995.029605	17.398810	-0.043467	3.013519
223.018609	2987.027363	17.403815	-0.043463	3.009772
222.657924	2979.092290	17.408819	-0.043390	3.006034
222.609217	2971.117777	17.413824	-0.043376	3.002288
222.797164	2963.134230	17.418829	-0.043406	2.998545
222.645314	2955.152078	17.423834	-0.043373	2.994781
222.468026	2947.139697	17.428839	-0.043334	2.990997
222.500286	2939.138449	17.433843	-0.043335	2.987224
222.614433	2931.162363	17.438848	-0.043351	2.983462
222.285260	2923.221088	17.443853	-0.043285	2.979689
222.305985	2915.229635	17.448858	-0.043284	2.975906
222.452428	2907.210546	17.453863	-0.043306	2.972111
222.313681	2899.242034	17.458867	-0.043275	2.968320
222.279045	2891.251600	17.463872	-0.043263	2.964520
222.438010	2883.292565	17.468877	-0.043288	2.960739
222.178568	2875.338928	17.473882	-0.043234	2.956935
221.965415	2867.341638	17.478887	-0.043189	2.953108
222.257491	2859.300870	17.483891	-0.043238	2.949280
222.209228	2851.333975	17.488896	-0.043224	2.945466
222.049579	2843.401883	17.493901	-0.043189	2.941657
222.162899	2835.392602	17.498906	-0.043205	2.937821
221.994502	2827.422444	17.503911	-0.043169	2.933984
221.988642	2819.421725	17.508915	-0.043163	2.930135
222.006516	2811.443827	17.513920	-0.043161	2.926294
222.045650	2803.469541	17.518925	-0.043163	2.922450
221.859229	2795.491688	17.523930	-0.043123	2.918588
221.757841	2787.538385	17.528935	-0.043099	2.914737
221.881017	2779.437551	17.533939	-0.043117	2.910822
221.737278	2771.473499	17.538944	-0.043085	2.906953
221.769184	2763.528368	17.543949	-0.043086	2.903097
221.626894	2755.546935	17.548954	-0.043054	2.899210
221.683078	2747.604287	17.553959	-0.043059	2.895347
221.240957	2739.635344	17.558963	-0.042972	2.891439
221.199027	2731.610545	17.563968	-0.042959	2.887520
221.403170	2723.625433	17.568973	-0.042992	2.883628
221.424672	2715.643955	17.573978	-0.042990	2.879723
221.489746	2707.721263	17.578983	-0.042997	2.875844
221.180501	2699.722708	17.583987	-0.042935	2.871902
221.171946	2691.735865	17.588992	-0.042928	2.867977
221.065703	2683.784883	17.593997	-0.042903	2.864058
221.074007	2675.771802	17.599002	-0.042899	2.860110
221.216139	2667.809070	17.604007	-0.042921	2.856189
220.919850	2659.836616	17.609011	-0.042860	2.852233
220.802713	2651.824225	17.614016	-0.042833	2.848262
221.123953	2643.834476	17.619021	-0.042888	2.844321
220.915003	2635.893794	17.624026	-0.042844	2.840369
220.829723	2627.945193	17.629031	-0.042823	2.836415
220.693574	2619.957085	17.634035	-0.042792	2.832432
220.573552	2611.942132	17.639040	-0.042765	2.828432
220.564202	2603.954073	17.644045	-0.042758	2.824445
220.759027	2595.958921	17.649050	-0.042789	2.820461
220.667174	2588.020920	17.654055	-0.042767	2.816484
220.680466	2580.027319	17.659059	-0.042764	2.812479
220.530851	2572.027780	17.664064	-0.042731	2.808456
220.474949	2564.080511	17.669069	-0.042715	2.804459
220.349597	2556.109845	17.674074	-0.042687	2.800440
220.660996	2548.121240	17.679079	-0.042740	2.796432
220.504960	2540.141180	17.684083	-0.042706	2.792395
220.305301	2532.150648	17.689088	-0.042663	2.788345
220.408681	2524.166825	17.694093	-0.042677	2.784310
220.336676	2516.220469	17.699098	-0.042659	2.780277
220.426881	2508.258167	17.704103	-0.042670	2.776241
220.234719	2500.285138	17.709107	-0.042629	2.772176
220.118822	2492.289254	17.714112	-0.042603	2.768098
220.378535	2484.303428	17.719117	-0.042646	2.764041
220.186307	2476.349223	17.724122	-0.042605	2.759968
219.908472	2468.426079	17.729127	-0.042548	2.755899
219.859299	2460.356299	17.734131	-0.042534	2.751763
219.860647	2452.343200	17.739136	-0.042529	2.747653
219.791545	2444.398386	17.744141	-0.042511	2.743568
219.661012	2436.429658	17.749146	-0.042481	2.739460
219.658827	2428.486807	17.754151	-0.042476	2.735368
219.900353	2420.453762	17.759155	-0.042516	2.731237
219.701762	2412.494714	17.764160	-0.042473	2.727112
219.679383	2404.550343	17.769165	-0.042464	2.722999
219.507163	2396.583501	17.774170	-0.042427	2.718858
219.441861	2388.645560	17.779175	-0.042410	2.714733
219.685692	2380.605331	17.784179	-0.042450	2.710568
219.652032	2372.631546	17.789184	-0.042438	2.706413
219.650930	2364.678673	17.794189	-0.042433	2.702265
219.320412	2356.725063	17.799194	-0.042366	2.698090
219.284994	2348.748412	17.804199	-0.042355	2.693915
219.339974	2340.752999	17.809203	-0.042360	2.689729
219.091663	2332.792970	17.814208	-0.042308	2.685535
219.269128	2324.829006	17.819213	-0.042336	2.681361
219.136549	2316.860994	17.824218	-0.042306	2.677158
218.957912	2308.897554	17.829223	-0.042268	2.672947
218.984275	2300.878123	17.834227	-0.042268	2.668714
219.170265	2292.866113	17.839232	-0.042297	2.664488
219.092389	2284.950706	17.844237	-0.042277	2.660289
218.827955	2276.993613	17.849242	-0.042223	2.656050
218.861525	2268.999998	17.854247	-0.042224	2.651804
218.789844	2261.024737	17.859251	-0.042206	2.647554
218.805121	2253.025320	17.864256	-0.042203	2.643289
218.812564	2245.100802	17.869261	-0.042200	2.639058
218.577670	2237.147386	17.874266	-0.042151	2.634788
218.598593	2229.159146	17.879271	-0.042149	2.630509
218.430793	2221.198186	17.884275	-0.042113	2.626226
218.676388	2213.188724	17.889280	-0.042154	2.621937
218.425045	2205.264219	17.894285	-0.042102	2.617654
218.180961	2197.297845	17.899290	-0.042051	2.613341
218.218843	2189.299611	17.904295	-0.042053	2.609023
218.403906	2181.305495	17.909299	-0.042082	2.604710
218.037653	2173.389499	17.914304	-0.042009	2.600395
218.159122	2165.424519	17.919309	-0.042026	2.596079
218.206711	2157.287775	17.924314	-0.042030	2.591658
218.364646	2149.248698	17.929319	-0.042054	2.587289
217.963156	2141.370167	17.934323	-0.041974	2.582963
218.066828	2133.415349	17.939328	-0.041988	2.578622
218.237988	2125.478758	17.944333	-0.042015	2.574289
218.026124	2117.494767	17.949338	-0.041971	2.569896
217.985949	2109.559947	17.954343	-0.041958	2.565534
217.972544	2101.607481	17.959347	-0.041950	2.561157
217.710214	2093.674660	17.964352	-0.041896	2.556766
217.930140	2085.671315	17.969357	-0.041932	2.552362
217.723155	2077.722884	17.974362	-0.041888	2.547951
217.709738	2069.740358	17.979367	-0.041881	2.543527
217.594250	2061.822376	17.984371	-0.041854	2.539124
217.440503	2053.850705	17.989376	-0.041820	2.534680
217.622512	2045.849647	17.994381	-0.041849	2.530237
217.443796	2037.886041	17.999386	-0.041811	2.525780
217.412318	2029.940326	18.004391	-0.041800	2.521337
217.522938	2021.976193	18.009395	-0.041815	2.516885
217.510689	2013.982092	18.014400	-0.041808	2.512400
217.482257	2006.007958	18.019405	-0.041797	2.507917
217.356080	1998.029944	18.024410	-0.041768	2.503416
217.352718	1990.078976	18.029415	-0.041763	2.498932
217.305604	1982.135511	18.034419	-0.041749	2.494440
217.109790	1974.161705	18.039424	-0.041707	2.489912
217.274413	1966.184106	18.044429	-0.041733	2.485401
217.093176	1958.255917	18.049434	-0.041694	2.480884
216.939932	1950.324109	18.054439	-0.041660	2.476358
216.955489	1942.334573	18.059443	-0.041658	2.471804
216.937319	1934.336569	18.064448	-0.041649	2.467234
216.888797	1926.394960	18.069453	-0.041635	2.462685
216.773175	1918.447720	18.074458	-0.041608	2.458120
216.687403	1910.486419	18.079463	-0.041587	2.453541
216.620959	1902.526923	18.084467	-0.041570	2.448955
216.495363	1894.566070	18.089472	-0.041541	2.444356
216.705229	1886.596374	18.094477	-0.041575	2.439768
216.532155	1878.663972	18.099482	-0.041538	2.435164
216.614669	1870.597559	18.104487	-0.041548	2.430493
216.692812	1862.627162	18.109491	-0.041557	2.425868
216.491210	1854.686698	18.114496	-0.041515	2.421231
216.664373	1846.727932	18.119501	-0.041542	2.416603
216.514815	1838.779628	18.124506	-0.041509	2.411947
216.303162	1830.843826	18.129511	-0.041464	2.407285
216.338353	1822.884546	18.134515	-0.041466	2.402619
216.228350	1814.941215	18.139520	-0.041440	2.397942
216.499238	1806.943520	18.144525	-0.041485	2.393253
216.376169	1798.990731	18.149530	-0.041457	2.388551
216.158369	1791.067412	18.154535	-0.041412	2.383850
216.282598	1783.096089	18.159539	-0.041430	2.379138
216.050111	1775.162097	18.164544	-0.041381	2.374410
215.957701	1767.203447	18.169549	-0.041359	2.369670
215.862710	1759.248823	18.174554	-0.041336	2.364922
215.883675	1751.308689	18.179559	-0.041335	2.360182
215.788919	1743.383950	18.184563	-0.041312	2.355433
215.786318	1735.346517	18.189568	-0.041306	2.350614
215.910847	1727.379459	18.194573	-0.041324	2.345838
215.737996	1719.439338	18.199578	-0.041287	2.341044
215.760223	1711.490123	18.204583	-0.041286	2.336250
215.867109	1703.522721	18.209587	-0.041301	2.331443
215.756028	1695.569180	18.214592	-0.041275	2.326616
215.600991	1687.651818	18.219597	-0.041241	2.321798
215.561292	1679.704464	18.224602	-0.041228	2.316961
215.525473	1671.733793	18.229607	-0.041216	2.312099
215.510007	1663.786811	18.234611	-0.041208	2.307244
215.412351	1655.822483	18.239616	-0.041185	2.302361
215.547916	1647.883490	18.244621	-0.041205	2.297503
215.274522	1639.948948	18.249626	-0.041149	2.292602
215.383592	1631.956331	18.254631	-0.041164	2.287688
215.233384	1624.028944	18.259635	-0.041131	2.282781
215.162979	1616.093300	18.264640	-0.041113	2.277866
215.102418	1608.129700	18.269645	-0.041097	2.272923
214.845441	1600.130357	18.274650	-0.041044	2.267930
214.909496	1592.169362	18.279655	-0.041050	2.262978
214.995060	1584.230994	18.284659	-0.041061	2.258031
214.859442	1576.293100	18.289664	-0.041031	2.253054
214.821144	1568.338375	18.294669	-0.041018	2.248064
214.695076	1560.400412	18.299674	-0.040990	2.243066
214.608311	1552.479431	18.304679	-0.040969	2.238071
214.649118	1544.540054	18.309683	-0.040971	2.233064
214.595502	1536.564364	18.314688	-0.040956	2.228015
214.545429	1528.628171	18.319693	-0.040941	2.222979
214.287913	1520.708192	18.324698	-0.040888	2.217924
214.309111	1512.749857	18.329703	-0.040887	2.212858
214.358271	1504.781840	18.334707	-0.040891	2.207776
214.181298	1496.866686	18.339712	-0.040853	2.202697
214.309542	1488.912213	18.344717	-0.040872	2.197607
214.220433	1480.968706	18.349722	-0.040850	2.192494
214.014760	1473.023497	18.354727	-0.040807	2.187356
214.078844	1465.061735	18.359731	-0.040813	2.182221
214.211155	1457.101740	18.364736	-0.040833	2.177081
214.288120	1449.161091	18.369741	-0.040842	2.171936
214.073359	1441.233726	18.374746	-0.040797	2.166760
213.807132	1433.328949	18.379751	-0.040742	2.161582
213.701317	1425.420152	18.384755	-0.040717	2.156404
213.456036	1417.466566	18.389760	-0.040667	2.151171
213.703678	1409.489725	18.394765	-0.040708	2.145956
213.651339	1401.546171	18.399770	-0.040693	2.140722
213.680343	1393.606846	18.404775	-0.040693	2.135486
213.519325	1385.684091	18.409779	-0.040658	2.130230
213.505078	1377.729307	18.414784	-0.040650	2.124953
213.408772	1369.820871	18.419789	-0.040627	2.119687
213.269267	1361.908431	18.424794	-0.040596	2.114400
213.564023	1353.839255	18.429799	-0.040646	2.109037
213.424187	1345.938648	18.434803	-0.040614	2.103732
213.337378	1338.011835	18.439808	-0.040593	2.098400
213.352624	1330.081147	18.444813	-0.040591	2.093062
213.145106	1322.161434	18.449818	-0.040547	2.087697
212.963200	1314.256188	18.454823	-0.040508	2.082329
213.025664	1306.330342	18.459827	-0.040515	2.076958
212.917194	1298.394617	18.464832	-0.040489	2.071550
212.813553	1290.470973	18.469837	-0.040465	2.066135
212.651418	1282.541824	18.474842	-0.040429	2.060697
212.851259	1274.588451	18.479847	-0.040462	2.055265
212.697593	1266.668512	18.484851	-0.040428	2.049805
212.640064	1258.732816	18.489856	-0.040412	2.044329
212.702475	1250.818822	18.494861	-0.040418	2.038866
212.776603	1242.868901	18.499866	-0.040427	2.033365
212.353038	1234.965284	18.504871	-0.040343	2.027830
212.190614	1227.062478	18.509875	-0.040308	2.022307
212.358046	1219.105639	18.514880	-0.040334	2.016765
212.501018	1211.142535	18.519885	-0.040355	2.011201
211.964891	1203.283712	18.524890	-0.040250	2.005624
212.048269	1195.340894	18.529895	-0.040261	2.000037
212.243174	1187.405601	18.534899	-0.040292	1.994451
212.033754	1179.490423	18.539904	-0.040248	1.988822
211.982547	1171.575121	18.544909	-0.040233	1.983193
211.936895	1163.663099	18.549914	-0.040220	1.977551
211.874855	1155.732700	18.554919	-0.040203	1.971878
211.787962	1147.814719	18.559923	-0.040182	1.966194
211.642920	1139.908422	18.564928	-0.040149	1.960497
211.672194	1131.996701	18.569933	-0.040150	1.954797
211.432933	1124.033359	18.574938	-0.040100	1.949015
211.363054	1116.119539	18.579943	-0.040082	1.943269
211.591610	1108.184265	18.584947	-0.040119	1.937524
211.496084	1100.251658	18.589952	-0.040096	1.931728
211.304862	1092.372891	18.594957	-0.040056	1.925943
211.477182	1084.430748	18.599962	-0.040083	1.920134
211.363961	1076.542071	18.604967	-0.040056	1.914316
211.321343	1068.631707	18.609971	-0.040043	1.908472
211.241324	1060.714410	18.614976	-0.040023	1.902600
211.339956	1052.803502	18.619981	-0.040037	1.896735
211.148027	1044.902519	18.624986	-0.039996	1.890826
211.035867	1036.999006	18.629991	-0.039970	1.884906
210.996460	1029.114084	18.634995	-0.039957	1.878990
210.843799	1021.210348	18.640000	-0.039924	1.873027
210.801558	1013.281967	18.645005	-0.039911	1.867040
210.746929	1005.374941	18.650010	-0.039896	1.861048
210.728332	997.465301	18.655015	-0.039887	1.855039
210.668295	989.561232	18.660019	-0.039871	1.849010
210.600178	981.664423	18.665024	-0.039853	1.842965
210.571100	973.777585	18.670029	-0.039842	1.836913
210.592735	965.859100	18.675034	-0.039841	1.830823
210.390598	957.962817	18.680039	-0.039799	1.824703
210.322101	950.103337	18.685043	-0.039781	1.818606
210.284617	942.185642	18.690048	-0.039769	1.812448
210.134248	934.300513	18.695053	-0.039735	1.806280
210.150281	926.410677	18.700058	-0.039733	1.800108
210.046538	918.516598	18.705063	-0.039709	1.793896
209.894168	910.581717	18.710067	-0.039675	1.787625
209.803939	902.685024	18.715072	-0.039654	1.781369
209.920692	894.787640	18.720077	-0.039670	1.775117
209.839184	886.895388	18.725082	-0.039650	1.768822
209.620078	879.038290	18.730087	-0.039604	1.762515
209.899984	871.132533	18.735091	-0.039651	1.756209
209.687077	863.251951	18.740096	-0.039606	1.749838
209.495269	855.398460	18.745101	-0.039565	1.743469
209.475229	847.523057	18.750106	-0.039557	1.737081
209.674345	839.585925	18.755111	-0.039589	1.730646
209.683700	831.721608	18.760115	-0.039585	1.724223
209.323716	823.900726	18.765120	-0.039513	1.717764
209.295781	816.009191	18.770125	-0.039503	1.711265
209.198813	808.121717	18.775130	-0.039480	1.704735
208.909611	800.283761	18.780135	-0.039421	1.698197
209.085239	792.373010	18.785139	-0.039448	1.691633
209.005362	784.490099	18.790144	-0.039428	1.685034
208.881503	776.658240	18.795149	-0.039400	1.678446
208.868741	768.776886	18.800154	-0.039393	1.671804
208.940743	760.873188	18.805159	-0.039401	1.665129
208.831642	753.050020	18.810163	-0.039376	1.658471
208.640259	745.187551	18.815168	-0.039335	1.651741
208.576045	737.332079	18.820173	-0.039318	1.645007
208.429609	729.509570	18.825178	-0.039286	1.638263
208.304464	721.607323	18.830183	-0.039257	1.631424
208.423495	713.702635	18.835187	-0.039274	1.624588
208.415956	705.844668	18.840192	-0.039268	1.617747
208.295988	698.005296	18.845197	-0.039240	1.610877
208.263147	690.153149	18.850202	-0.039229	1.603979
208.388040	682.291733	18.855207	-0.039247	1.597065
208.329910	674.452967	18.860211	-0.039231	1.590115
208.181879	666.614786	18.865216	-0.039199	1.583122
208.180117	658.790524	18.870221	-0.039193	1.576131
208.130512	650.937638	18.875226	-0.039179	1.569077
207.872057	643.136177	18.880231	-0.039126	1.562007
207.805389	635.319258	18.885235	-0.039108	1.554918
207.856040	627.426693	18.890240	-0.039113	1.547746
207.488370	619.657170	18.895245	-0.039039	1.540590
207.745187	611.772457	18.900250	-0.039082	1.533389
207.366001	603.977504	18.905255	-0.039006	1.526141
207.410744	596.152437	18.910259	-0.039010	1.518894
207.093041	588.362277	18.915264	-0.038945	1.511590
207.311587	580.487617	18.920269	-0.038981	1.504254
207.108951	572.711377	18.925274	-0.038938	1.496909
206.874161	564.896659	18.930279	-0.038889	1.489486
207.143106	557.046145	18.935283	-0.038934	1.482071
207.268333	549.208800	18.940288	-0.038953	1.474609
207.019338	541.388065	18.945293	-0.038901	1.467065
206.778807	533.619278	18.950298	-0.038851	1.459535
206.685569	525.814999	18.955303	-0.038829	1.451954
206.788136	517.995921	18.960307	-0.038843	1.444350
206.642052	510.226513	18.965312	-0.038811	1.436714
206.605092	502.432262	18.970317	-0.038799	1.429031
206.629124	494.633625	18.975322	-0.038798	1.421312
206.286079	486.894462	18.980327	-0.038729	1.413550
206.205021	479.105924	18.985331	-0.038709	1.405738
206.181197	471.331071	18.990336	-0.038700	1.397907
206.143163	463.536869	18.995341	-0.038688	1.390009
205.872904	455.788175	19.000346	-0.038632	1.382073
205.818292	448.010956	19.005351	-0.038617	1.374098
205.826451	440.230295	19.010355	-0.038614	1.366085
205.588453	432.501185	19.015360	-0.038564	1.358035
205.577235	424.728577	19.020365	-0.038557	1.349931
205.597112	416.956955	19.025370	-0.038556	1.341784
205.412960	409.229246	19.030375	-0.038517	1.333598
205.462995	401.463844	19.035379	-0.038521	1.325363
205.350559	393.736576	19.040384	-0.038495	1.317088
205.350701	385.881134	19.045389	-0.038490	1.308643
205.120191	378.164459	19.050394	-0.038442	1.300252
205.191761	370.414161	19.055399	-0.038450	1.291825
205.145075	362.711581	19.060403	-0.038437	1.283373
204.900480	355.037030	19.065408	-0.038386	1.274859
204.755253	347.333512	19.070413	-0.038354	1.266274
204.787537	339.624669	19.075418	-0.038355	1.257658
204.692367	331.923395	19.080423	-0.038332	1.248967
204.682579	324.232486	19.085427	-0.038326	1.240244
204.703301	316.522580	19.090432	-0.038325	1.231442
204.545420	308.845272	19.095437	-0.038290	1.222580
204.327768	301.201279	19.100442	-0.038245	1.213680
204.302501	293.505561	19.105447	-0.038235	1.204692
204.320284	285.849321	19.110451	-0.038233	1.195692
204.032583	278.215277	19.115456	-0.038175	1.186587
204.003129	270.563125	19.120461	-0.038164	1.177444
203.943324	262.911004	19.125466	-0.038148	1.168222
204.052213	255.246924	19.130471	-0.038164	1.158948
203.890685	247.623488	19.135475	-0.038129	1.149592
203.770818	239.987031	19.140480	-0.038101	1.140152
203.709232	232.372442	19.145485	-0.038085	1.130673
203.559667	224.777883	19.150490	-0.038052	1.121119
203.317405	217.211557	19.155495	-0.038002	1.111500
203.312074	209.613510	19.160499	-0.037996	1.101807
203.162362	202.038548	19.165504	-0.037964	1.092027
203.009216	194.478996	19.170509	-0.037930	1.082177
202.960115	186.916263	19.175514	-0.037916	1.072256
202.944507	179.335146	19.180519	-0.037908	1.062225
202.862018	171.805768	19.185523	-0.037888	1.052153
202.667430	164.282498	19.190528	-0.037847	1.041966
202.639854	156.767422	19.195533	-0.037837	1.031728
202.507592	149.266730	19.200538	-0.037808	1.021383
202.265697	141.793996	19.205543	-0.037758	1.010944
202.220532	134.311840	19.210547	-0.037744	1.000431
202.183903	126.804664	19.215552	-0.037733	0.989773
201.939701	119.358729	19.220557	-0.037682	0.979035
201.857857	111.914103	19.225562	-0.037662	0.968221
201.581641	104.516702	19.230567	-0.037606	0.957304
201.797985	97.050218	19.235571	-0.037642	0.946287
201.677007	89.656504	19.240576	-0.037614	0.935161
201.553875	82.279088	19.245581	-0.037587	0.923924
201.428977	74.927487	19.250586	-0.037559	0.912589
201.153300	67.600599	19.255591	-0.037503	0.901109
201.312534	60.462749	19.260595	-0.037528	0.889901