Fri Mar 12 14:04:36 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.615536	-0.121795	0.000000	-0.000039	0.721784

0.407280	-0.102168	0.005005	-0.000000	0.721749
0.592359	-0.138282	0.010010	-0.000035	0.721743
0.731939	-0.161767	0.015014	-0.000061	0.721746
0.644702	-0.144705	0.020019	-0.000045	0.721749
0.609376	-0.143916	0.025024	-0.000038	0.721739
0.898482	-0.190731	0.030029	-0.000092	0.721748
0.500840	-0.123638	0.035034	-0.000018	0.721741
0.466458	-0.114876	0.040038	-0.000012	0.721746
0.714728	-0.159581	0.045043	-0.000058	0.721745
0.552704	-0.133015	0.050048	-0.000028	0.721741
0.589415	-0.134608	0.055053	-0.000035	0.721751
0.547532	-0.130825	0.060058	-0.000027	0.721744
0.749062	-0.166612	0.065062	-0.000065	0.721744
0.652991	-0.274288	0.070067	-0.000047	0.721499
0.513779	-0.283184	0.075072	-0.000021	0.721433
0.771216	-0.324601	0.080077	-0.000069	0.721441
0.547477	-0.287043	0.085082	-0.000027	0.721437
0.346759	-0.249456	0.090086	0.000010	0.721441
0.571034	-0.289532	0.095091	-0.000032	0.721441
0.495617	-0.314787	0.100096	-0.000018	0.721365
0.704969	-0.476387	0.105101	-0.000057	0.721120
0.509859	-0.443013	0.110106	-0.000020	0.721118
0.692261	-0.474999	0.115110	-0.000054	0.721119
0.555600	-0.447351	0.120115	-0.000029	0.721125
0.544376	-0.480092	0.125120	-0.000027	0.721057
0.653918	-0.590111	0.130125	-0.000047	0.720879
0.553278	-0.575185	0.135130	-0.000029	0.720874
0.342865	-0.536983	0.140134	0.000010	0.720875
0.397020	-0.545695	0.145139	0.000000	0.720877
0.262675	-0.686689	0.150144	0.000025	0.720553
0.314845	-0.701947	0.155149	0.000015	0.720541
0.426376	-0.725239	0.160154	-0.000005	0.720534
0.456665	-0.740090	0.165158	-0.000011	0.720516
0.379906	-0.874096	0.170163	0.000003	0.720225
0.246410	-0.856010	0.175168	0.000028	0.720214
0.393038	-0.876952	0.180173	0.000001	0.720224
0.330961	-0.962525	0.185178	0.000012	0.720034
0.301413	-1.026850	0.190182	0.000018	0.719897
0.477570	-1.056024	0.195187	-0.000015	0.719902
0.340977	-1.096520	0.200192	0.000010	0.719774
0.383323	-1.192274	0.205197	0.000002	0.719600
0.235461	-1.168932	0.210202	0.000030	0.719595
0.118163	-1.216716	0.215206	0.000052	0.719459
0.202544	-1.328387	0.220211	0.000036	0.719269
0.142171	-1.321772	0.225216	0.000047	0.719261
0.339224	-1.441732	0.230221	0.000010	0.719094
0.209873	-1.487993	0.235226	0.000034	0.718957
0.163863	-1.478554	0.240230	0.000043	0.718960
0.123682	-1.620335	0.245235	0.000051	0.718666
-0.039334	-1.604925	0.250240	0.000081	0.718639
-0.000804	-1.657517	0.255245	0.000074	0.718549
0.102633	-1.776849	0.260250	0.000054	0.718350
-0.103560	-1.740106	0.265254	0.000093	0.718350
-0.195636	-1.866431	0.270259	0.000110	0.718068
-0.598526	-1.824049	0.275264	0.000185	0.718010
-0.283923	-1.933239	0.280269	0.000126	0.717905
-0.404007	-2.017723	0.285274	0.000149	0.717696
-0.350568	-2.025011	0.290278	0.000139	0.717701
-0.070315	-2.233394	0.295283	0.000086	0.717388
-0.149985	-2.225935	0.300288	0.000101	0.717374
-0.150439	-2.340014	0.305293	0.000101	0.717149
-0.550243	-2.301967	0.310298	0.000176	0.717083
-0.750598	-2.365205	0.315302	0.000213	0.716888
-2.291517	-2.155668	0.320307	0.000500	0.716759
-2.186142	-2.178206	0.325312	0.000480	0.716752
-2.823056	-2.211450	0.330317	0.000599	0.716462
-3.375582	-2.121248	0.335322	0.000701	0.716446
-3.317839	-2.132619	0.340326	0.000690	0.716443
-3.177750	-2.284739	0.345331	0.000664	0.716192
-4.576495	-2.069206	0.350336	0.000925	0.716125
-4.040629	-2.159167	0.355341	0.000825	0.716136
-3.858861	-2.246765	0.360346	0.000791	0.716027
-5.364450	-2.053545	0.365350	0.001071	0.715879
-4.757718	-2.159325	0.370355	0.000958	0.715883
-4.646789	-2.183715	0.375360	0.000937	0.715874
-4.987963	-2.242399	0.380365	0.001001	0.715638
-6.160184	-2.081275	0.385370	0.001219	0.715543
-5.782908	-2.149017	0.390374	0.001149	0.715542
-5.438946	-2.206927	0.395379	0.001085	0.715549
-6.307409	-2.148241	0.400384	0.001246	0.715359
-6.912290	-2.103391	0.405389	0.001359	0.715234
-6.498743	-2.179799	0.410394	0.001282	0.715229
-7.027831	-2.084857	0.415398	0.001380	0.715230
-6.783792	-2.125992	0.420403	0.001335	0.715235
-6.750351	-2.268605	0.425408	0.001329	0.714964
-7.549104	-2.153271	0.430413	0.001477	0.714911
-7.870885	-2.097697	0.435418	0.001537	0.714907
-7.352357	-2.192022	0.440422	0.001440	0.714903
-7.214885	-2.214016	0.445427	0.001415	0.714909
-8.385527	-2.159627	0.450432	0.001633	0.714603
-8.451543	-2.144152	0.455437	0.001645	0.714610
-8.435444	-2.147710	0.460442	0.001642	0.714609
-8.478522	-2.142180	0.465446	0.001650	0.714605
-8.508073	-2.133358	0.470451	0.001655	0.714612
-8.636566	-2.185372	0.475456	0.001679	0.714463
-9.362673	-2.149369	0.480461	0.001814	0.714278
-9.466589	-2.132016	0.485466	0.001834	0.714276
-9.847629	-2.063602	0.490470	0.001904	0.714277
-9.338840	-2.151635	0.495475	0.001810	0.714282
-9.606797	-2.108908	0.500480	0.001859	0.714273
-9.672150	-2.130566	0.505485	0.001872	0.714206
-10.255260	-2.146671	0.510490	0.001980	0.713968
-10.160066	-2.166519	0.515494	0.001962	0.713963
-10.536301	-2.094050	0.520499	0.002032	0.713974
-10.432547	-2.118526	0.525504	0.002013	0.713962
-10.056768	-2.180666	0.530509	0.001943	0.713971
-10.612852	-2.083539	0.535514	0.002046	0.713968
-11.076327	-2.145766	0.540518	0.002133	0.713680
-11.022814	-2.168631	0.545523	0.002123	0.713654
-11.641110	-2.063556	0.550528	0.002238	0.713644
-11.324098	-2.115347	0.555533	0.002178	0.713653
-11.042296	-2.167107	0.560538	0.002126	0.713650
-11.209708	-2.138204	0.565542	0.002157	0.713648
-11.047273	-2.216196	0.570547	0.002127	0.713551
-12.232969	-2.104767	0.575552	0.002347	0.713353
-11.677903	-2.199172	0.580557	0.002244	0.713362
-11.988516	-2.144008	0.585562	0.002302	0.713361
-12.266346	-2.095863	0.590566	0.002353	0.713359
-11.934724	-2.151476	0.595571	0.002292	0.713366
-12.086851	-2.128749	0.600576	0.002320	0.713357
-12.360613	-2.225783	0.605581	0.002371	0.713067
-12.588240	-2.208821	0.610586	0.002413	0.713020
-13.054956	-2.126234	0.615590	0.002500	0.713019
-12.724310	-2.180932	0.620595	0.002438	0.713028
-13.125299	-2.114763	0.625600	0.002513	0.713018
-12.881096	-2.156216	0.630605	0.002467	0.713022
-13.012653	-2.182174	0.635610	0.002492	0.712924
-14.502822	-2.026273	0.640614	0.002769	0.712706
-13.594376	-2.185454	0.645619	0.002600	0.712711
-13.963765	-2.123500	0.650624	0.002669	0.712703
-14.283413	-2.062647	0.655629	0.002728	0.712711
-13.626493	-2.181873	0.660634	0.002606	0.712707
-13.860288	-2.139963	0.665638	0.002649	0.712708
-13.918014	-2.151574	0.670643	0.002660	0.712664
-14.998511	-2.102557	0.675648	0.002861	0.712379
-14.542211	-2.180983	0.680653	0.002776	0.712384
-14.538021	-2.182848	0.685658	0.002775	0.712382
-14.910278	-2.117362	0.690662	0.002845	0.712381
-14.715373	-2.148429	0.695667	0.002808	0.712388
-15.074839	-2.088475	0.700672	0.002875	0.712380
-14.702219	-2.157672	0.705677	0.002806	0.712375
-15.269580	-2.200298	0.710682	0.002911	0.712088
-15.486319	-2.163188	0.715686	0.002952	0.712086
-15.798891	-2.103166	0.720691	0.003010	0.712094
-15.784429	-2.111326	0.725696	0.003007	0.712083
-15.457935	-2.166312	0.730701	0.002946	0.712090
-15.570032	-2.146712	0.735706	0.002967	0.712089
-15.961889	-2.090500	0.740710	0.003040	0.712062
-16.226874	-2.192457	0.745715	0.003089	0.711765
-16.418387	-2.163951	0.750720	0.003125	0.711754
-17.035899	-2.051158	0.755725	0.003239	0.711759
-16.423374	-2.159503	0.760730	0.003125	0.711761
-16.568239	-2.134572	0.765734	0.003152	0.711760
-16.535311	-2.136820	0.770739	0.003146	0.711767
-16.837174	-2.088846	0.775744	0.003202	0.711755
-17.056473	-2.179505	0.780749	0.003243	0.711497
-17.317030	-2.155207	0.785754	0.003291	0.711453
-18.023263	-2.030986	0.790758	0.003423	0.711450
-17.440297	-2.131719	0.795763	0.003314	0.711456
-17.332348	-2.155398	0.800768	0.003294	0.711447
-17.675885	-2.089702	0.805773	0.003358	0.711456
-17.331336	-2.152607	0.810778	0.003294	0.711454
-17.748680	-2.187302	0.815782	0.003372	0.711236
-18.690829	-2.067665	0.820787	0.003547	0.711140
-18.368672	-2.130805	0.825792	0.003487	0.711129
-18.307049	-2.138013	0.830797	0.003475	0.711136
-18.167254	-2.163180	0.835802	0.003449	0.711136
-18.600694	-2.087528	0.840806	0.003530	0.711133
-18.098809	-2.173112	0.845811	0.003436	0.711141
-18.356998	-2.216331	0.850816	0.003484	0.710963
-19.371969	-2.080802	0.855821	0.003673	0.710872
-19.219550	-2.108453	0.860826	0.003645	0.710871
-19.035005	-2.142768	0.865830	0.003610	0.710869
-18.972975	-2.149621	0.870835	0.003599	0.710877
-19.443902	-2.071900	0.875840	0.003686	0.710865
-19.485047	-2.061735	0.880845	0.003694	0.710871
-19.011015	-2.253889	0.885850	0.003606	0.710656
-20.482048	-2.055234	0.890854	0.003879	0.710529
-20.320890	-2.078973	0.895859	0.003849	0.710539
-19.948627	-2.150882	0.900864	0.003780	0.710528
-20.098098	-2.121571	0.905869	0.003808	0.710534
-19.893391	-2.160339	0.910874	0.003770	0.710529
-20.377226	-2.076170	0.915878	0.003860	0.710525
-20.217078	-2.201552	0.920883	0.003830	0.710332
-21.335499	-2.064020	0.925888	0.004038	0.710209
-20.947475	-2.127449	0.930893	0.003966	0.710220
-20.596390	-2.192068	0.935898	0.003900	0.710216
-21.359514	-2.057851	0.940902	0.004042	0.710213
-21.052249	-2.109310	0.945907	0.003985	0.710219
-20.880731	-2.143726	0.950912	0.003953	0.710212
-21.223392	-2.180590	0.955917	0.004017	0.710016
-22.061100	-2.094301	0.960922	0.004173	0.709890
-21.650154	-2.169315	0.965926	0.004096	0.709887
-21.354365	-2.220372	0.970931	0.004041	0.709890
-22.060939	-2.097673	0.975936	0.004172	0.709884
-21.984130	-2.107323	0.980941	0.004158	0.709892
-21.612965	-2.174115	0.985946	0.004089	0.709891
-22.279541	-2.169638	0.990950	0.004213	0.709663
-22.727157	-2.121186	0.995955	0.004296	0.709600
-22.565841	-2.156005	1.000960	0.004266	0.709588
-22.499661	-2.165050	1.005965	0.004254	0.709594
-22.718766	-2.124657	1.010970	0.004294	0.709597
-23.075853	-2.065254	1.015974	0.004361	0.709588
-22.652123	-2.136304	1.020979	0.004282	0.709597
-23.141295	-2.165692	1.025984	0.004373	0.709364
-23.934501	-2.074980	1.030989	0.004521	0.709263
-23.334474	-2.182173	1.035994	0.004409	0.709263
-23.780690	-2.105088	1.040998	0.004492	0.709258
-23.852880	-2.086744	1.046003	0.004505	0.709269
-23.369161	-2.178747	1.051008	0.004415	0.709257
-23.510429	-2.150432	1.056013	0.004441	0.709264
-23.968394	-2.167074	1.061018	0.004527	0.709067
-24.721358	-2.089825	1.066022	0.004667	0.708953
-24.210244	-2.177587	1.071027	0.004571	0.708960
-24.700182	-2.094694	1.076032	0.004663	0.708952
-24.866809	-2.064590	1.081037	0.004693	0.708952
-24.397789	-2.147813	1.086042	0.004606	0.708953
-24.584154	-2.117660	1.091046	0.004641	0.708947
-24.744930	-2.142435	1.096051	0.004671	0.708840
-25.487735	-2.113702	1.101056	0.004809	0.708633
-25.010383	-2.196074	1.106061	0.004720	0.708639
-25.294100	-2.145529	1.111066	0.004773	0.708639
-25.524600	-2.108560	1.116070	0.004816	0.708631
-25.004599	-2.195221	1.121075	0.004719	0.708643
-25.366190	-2.135355	1.126080	0.004786	0.708634
-25.602215	-2.178680	1.131085	0.004830	0.708463
-25.988550	-2.165708	1.136090	0.004902	0.708351
-26.113568	-2.147615	1.141094	0.004925	0.708343
-26.095892	-2.145723	1.146099	0.004922	0.708353
-26.178742	-2.133860	1.151104	0.004937	0.708347
-26.105765	-2.146966	1.156109	0.004923	0.708347
-26.223777	-2.124669	1.161114	0.004945	0.708350
-26.891807	-2.160036	1.166118	0.005070	0.708040
-26.835281	-2.182864	1.171123	0.005059	0.708015
-27.079084	-2.144609	1.176128	0.005104	0.708005
-27.228002	-2.115362	1.181133	0.005132	0.708010
-26.977569	-2.158658	1.186138	0.005085	0.708013
-27.164028	-2.129728	1.191142	0.005120	0.708004
-27.082593	-2.138930	1.196147	0.005105	0.708015
-27.727443	-2.165157	1.201152	0.005225	0.707732
-28.038086	-2.126544	1.206157	0.005282	0.707699
-27.905360	-2.149289	1.211162	0.005258	0.707701
-27.908957	-2.153883	1.216166	0.005258	0.707690
-28.038793	-2.126249	1.221171	0.005282	0.707699
-28.005537	-2.135389	1.226176	0.005276	0.707693
-28.220459	-2.095585	1.231181	0.005316	0.707696
-27.802613	-2.283775	1.236186	0.005238	0.707468
-29.139317	-2.094394	1.241190	0.005487	0.707370
-29.152661	-2.087603	1.246195	0.005489	0.707379
-28.879217	-2.142199	1.251200	0.005438	0.707368
-29.100831	-2.101864	1.256205	0.005480	0.707369
-28.907143	-2.135125	1.261210	0.005444	0.707372
-29.055270	-2.110844	1.266214	0.005471	0.707368
-28.684493	-2.253067	1.271219	0.005402	0.707215
-29.606281	-2.158306	1.276224	0.005574	0.707076
-29.949907	-2.095677	1.281229	0.005637	0.707079
-29.777226	-2.125312	1.286234	0.005605	0.707081
-29.579736	-2.166329	1.291238	0.005568	0.707070
-29.608997	-2.156430	1.296243	0.005574	0.707079
-29.729254	-2.138166	1.301248	0.005596	0.707073
-30.050883	-2.208084	1.306253	0.005656	0.706817
-30.558766	-2.149092	1.311258	0.005750	0.706754
-30.910771	-2.089555	1.316262	0.005816	0.706748
-30.554817	-2.149179	1.321267	0.005750	0.706756
-30.654476	-2.135322	1.326272	0.005768	0.706748
-30.811003	-2.106315	1.331277	0.005797	0.706750
-30.591484	-2.144301	1.336282	0.005756	0.706753
-31.058867	-2.159351	1.341286	0.005843	0.706555
-31.869641	-2.067834	1.346291	0.005994	0.706449
-31.452317	-2.148111	1.351296	0.005916	0.706437
-31.340692	-2.166710	1.356301	0.005896	0.706440
-31.480996	-2.136633	1.361306	0.005922	0.706450
-31.991315	-2.051514	1.366310	0.006016	0.706439
-31.636157	-2.111815	1.371315	0.005950	0.706445
-31.321472	-2.220132	1.376320	0.005892	0.706340
-32.426776	-2.130840	1.381325	0.006097	0.706124
-32.186161	-2.171618	1.386330	0.006053	0.706128
-32.379327	-2.141632	1.391334	0.006088	0.706119
-32.388895	-2.133969	1.396339	0.006090	0.706131
-32.675580	-2.086652	1.401344	0.006143	0.706124
-32.675911	-2.086188	1.406349	0.006143	0.706125
-32.212052	-2.214396	1.411354	0.006057	0.706033
-33.367018	-2.094349	1.416358	0.006272	0.705861
-33.001339	-2.156376	1.421363	0.006204	0.705867
-33.208478	-2.123586	1.426368	0.006242	0.705859
-33.254979	-2.115822	1.431373	0.006251	0.705858
-32.927855	-2.170239	1.436378	0.006190	0.705866
-33.136210	-2.137116	1.441382	0.006229	0.705858
-33.360784	-2.220533	1.446387	0.006271	0.705610
-34.268000	-2.103982	1.451392	0.006439	0.705519
-34.193314	-2.117861	1.456397	0.006425	0.705518
-33.783512	-2.186980	1.461402	0.006349	0.705526
-34.597996	-2.045995	1.466406	0.006501	0.705518
-34.305446	-2.095144	1.471411	0.006446	0.705524
-33.958211	-2.159820	1.476416	0.006381	0.705519
-34.504857	-2.170093	1.481421	0.006483	0.705302
-35.171546	-2.095776	1.486426	0.006607	0.705212
-35.026503	-2.126850	1.491430	0.006580	0.705202
-34.631171	-2.192735	1.496435	0.006506	0.705211
-35.134904	-2.104855	1.501440	0.006600	0.705208
-35.388953	-2.061138	1.506445	0.006647	0.705205
-34.750748	-2.172297	1.511450	0.006529	0.705210
-35.312424	-2.172707	1.516454	0.006633	0.705008
-36.310937	-2.053707	1.521459	0.006819	0.704889
-35.979146	-2.116444	1.526464	0.006757	0.704882
-36.035523	-2.107190	1.531469	0.006767	0.704880
-36.022946	-2.107400	1.536474	0.006765	0.704884
-35.937925	-2.126880	1.541478	0.006749	0.704876
-35.886196	-2.132249	1.546483	0.006739	0.704884
-36.051607	-2.135178	1.551488	0.006770	0.704819
-36.571489	-2.161029	1.556493	0.006867	0.704580
-36.083534	-2.246106	1.561498	0.006776	0.704584
-37.041451	-2.079031	1.566502	0.006954	0.704577
-36.968445	-2.087110	1.571507	0.006941	0.704587
-36.446881	-2.181704	1.576512	0.006844	0.704584
-36.861971	-2.109118	1.581517	0.006921	0.704581
-37.108295	-2.158990	1.586522	0.006967	0.704392
-38.133619	-2.046182	1.591526	0.007157	0.704251
-37.443923	-2.166262	1.596531	0.007029	0.704257
-37.489921	-2.160870	1.601536	0.007037	0.704251
-37.850316	-2.095710	1.606541	0.007104	0.704253
-37.592041	-2.137984	1.611546	0.007056	0.704261
-37.671607	-2.130402	1.616550	0.007071	0.704248
-37.630381	-2.202115	1.621555	0.007063	0.704118
-38.806194	-2.078467	1.626560	0.007282	0.703945
-38.545408	-2.125099	1.631565	0.007234	0.703945
-38.569520	-2.116410	1.636570	0.007238	0.703954
-38.546608	-2.125548	1.641574	0.007234	0.703944
-38.142098	-2.192890	1.646579	0.007158	0.703953
-38.704114	-2.097317	1.651584	0.007263	0.703944
-38.922021	-2.138121	1.656589	0.007303	0.703784
-39.288788	-2.145171	1.661594	0.007372	0.703638
-39.475019	-2.116669	1.666598	0.007406	0.703628
-39.560817	-2.096946	1.671603	0.007422	0.703637
-39.378638	-2.131885	1.676608	0.007388	0.703632
-39.434756	-2.122637	1.681613	0.007398	0.703631
-39.603803	-2.089927	1.686618	0.007430	0.703636
-39.700997	-2.102055	1.691622	0.007448	0.703577
-39.998313	-2.164926	1.696627	0.007503	0.703343
-40.259162	-2.120102	1.701632	0.007552	0.703340
-40.739281	-2.036880	1.706637	0.007641	0.703335
-40.111855	-2.146448	1.711642	0.007524	0.703340
-40.330039	-2.111204	1.716646	0.007565	0.703333
-40.399850	-2.095067	1.721651	0.007578	0.703340
-40.042342	-2.206616	1.726656	0.007511	0.703244
-41.152091	-2.127395	1.731661	0.007718	0.703005
-41.037723	-2.146301	1.736666	0.007696	0.703008
-41.129076	-2.134054	1.741670	0.007713	0.703000
-40.928714	-2.166283	1.746675	0.007676	0.703007
-41.186434	-2.121938	1.751680	0.007724	0.703004
-41.358159	-2.092115	1.756685	0.007756	0.703002
-40.925389	-2.251448	1.761690	0.007675	0.702836
-42.213375	-2.094678	1.766694	0.007915	0.702689
-42.264721	-2.082841	1.771699	0.007924	0.702695
-41.850190	-2.157740	1.776704	0.007847	0.702693
-42.292929	-2.081408	1.781709	0.007929	0.702688
-42.112886	-2.108472	1.786714	0.007896	0.702698
-42.147900	-2.109011	1.791718	0.007902	0.702685
-41.868682	-2.228261	1.796723	0.007850	0.702544
-42.851209	-2.140553	1.801728	0.008033	0.702368
-42.845303	-2.143210	1.806733	0.008032	0.702364
-42.605852	-2.182569	1.811738	0.007987	0.702371
-42.710362	-2.168628	1.816742	0.008007	0.702362
-42.957398	-2.120663	1.821747	0.008053	0.702370
-43.125791	-2.093285	1.826752	0.008084	0.702365
-43.335962	-2.159670	1.831757	0.008123	0.702155
-43.890707	-2.099022	1.836762	0.008226	0.702078
-44.040751	-2.076226	1.841766	0.008254	0.702070
-43.627703	-2.145461	1.846771	0.008177	0.702079
-43.922854	-2.094359	1.851776	0.008232	0.702076
-44.163724	-2.053978	1.856781	0.008277	0.702071
-43.729856	-2.128508	1.861786	0.008196	0.702077
-43.868763	-2.169244	1.866790	0.008222	0.701944
-45.168627	-2.034815	1.871795	0.008464	0.701747
-44.497286	-2.156514	1.876800	0.008339	0.701743
-44.676142	-2.126109	1.881805	0.008372	0.701741
-44.561907	-2.142836	1.886810	0.008351	0.701748
-44.952583	-2.078556	1.891814	0.008423	0.701737
-44.753283	-2.109989	1.896819	0.008386	0.701746
-44.494180	-2.201571	1.901824	0.008338	0.701654
-45.762807	-2.086276	1.906829	0.008574	0.701430
-45.271677	-2.169094	1.911834	0.008482	0.701439
-45.679010	-2.101031	1.916838	0.008558	0.701430
-45.529114	-2.122847	1.921843	0.008530	0.701440
-45.531739	-2.124675	1.926848	0.008531	0.701436
-45.744855	-2.087080	1.931853	0.008570	0.701435
-45.732073	-2.134333	1.936858	0.008568	0.701344
-46.802359	-2.054773	1.941862	0.008767	0.701119
-46.161323	-2.167063	1.946867	0.008648	0.701123
-46.229154	-2.156454	1.951872	0.008660	0.701120
-46.846975	-2.049773	1.956877	0.008775	0.701113
-46.415510	-2.121763	1.961882	0.008695	0.701123
-46.487167	-2.112514	1.966886	0.008708	0.701116
-46.613137	-2.105949	1.971891	0.008731	0.701084
-47.069583	-2.129911	1.976896	0.008816	0.700871
-47.026728	-2.137499	1.981901	0.008808	0.700871
-47.022560	-2.135683	1.986906	0.008808	0.700877
-47.343854	-2.081761	1.991910	0.008867	0.700870
-47.235787	-2.098011	1.996915	0.008847	0.700876
-47.032203	-2.178388	2.001920	0.008809	0.700787

-47.935548	-2.141887	2.011917	0.008977	0.700535
-48.046738	-2.121948	2.021914	0.008998	0.700535
-47.821601	-2.162372	2.031910	0.008956	0.700535
-48.142014	-2.105546	2.041907	0.009015	0.700534
-48.066997	-2.119237	2.051904	0.009001	0.700534
-47.769633	-2.172194	2.061901	0.008946	0.700534
-47.994620	-2.132463	2.071898	0.008987	0.700534
-47.815715	-2.164218	2.081894	0.008954	0.700534
-48.428668	-2.056072	2.091891	0.009068	0.700532
-47.865434	-2.154976	2.101888	0.008963	0.700536
-47.943229	-2.140954	2.111885	0.008977	0.700536
-47.527031	-2.090093	2.121882	0.008900	0.700790
-47.186584	-2.110272	2.131878	0.008836	0.700872
-47.206060	-2.107151	2.141875	0.008840	0.700872
-47.043038	-2.137153	2.151872	0.008809	0.700870
-47.125496	-2.121374	2.161869	0.008824	0.700873
-47.122429	-2.109891	2.171866	0.008824	0.700897
-46.611856	-2.090492	2.181862	0.008729	0.701121
-46.510603	-2.109208	2.191859	0.008710	0.701120
-46.186443	-2.167790	2.201856	0.008649	0.701119
-46.465056	-2.117340	2.211853	0.008701	0.701121
-45.592313	-2.117398	2.221850	0.008538	0.701436
-45.689608	-2.100826	2.231846	0.008556	0.701435
-45.618910	-2.113360	2.241843	0.008543	0.701435
-45.625889	-2.083630	2.251840	0.008544	0.701493
-44.471553	-2.167180	2.261837	0.008329	0.701741
-44.480015	-2.165251	2.271834	0.008331	0.701742
-44.794779	-2.109322	2.281830	0.008389	0.701742
-44.526415	-2.101870	2.291827	0.008339	0.701854
-43.463699	-2.183966	2.301824	0.008141	0.702071
-43.720128	-2.137899	2.311821	0.008188	0.702072
-43.631719	-2.153862	2.321818	0.008172	0.702072
-43.424071	-2.105370	2.331814	0.008133	0.702245
-42.835792	-2.150858	2.341811	0.008023	0.702365
-42.837528	-2.148311	2.351808	0.008024	0.702370
-42.835792	-2.148123	2.361805	0.008023	0.702371
-42.075177	-2.128695	2.371802	0.007881	0.702685
-42.261871	-2.092202	2.381798	0.007916	0.702692
-42.161722	-2.112074	2.391795	0.007897	0.702688
-41.603042	-2.117271	2.401792	0.007793	0.702879
-41.460184	-2.080959	2.411789	0.007766	0.703004
-41.075493	-2.148199	2.421786	0.007695	0.703007
-41.375406	-2.067140	2.431782	0.007750	0.703063
-40.407136	-2.102922	2.441779	0.007570	0.703340
-40.082395	-2.160632	2.451776	0.007509	0.703340
-40.425549	-2.097906	2.461773	0.007573	0.703344
-39.789897	-2.113593	2.471770	0.007455	0.703541
-39.574625	-2.105932	2.481766	0.007414	0.703634
-39.576020	-2.107895	2.491763	0.007415	0.703630
-39.583014	-2.052233	2.501760	0.007416	0.703740
-38.732101	-2.100620	2.511757	0.007257	0.703948
-38.517505	-2.136520	2.521754	0.007217	0.703953
-38.972292	-2.053195	2.531750	0.007302	0.703958
-38.002950	-2.076763	2.541747	0.007121	0.704259
-37.756986	-2.122441	2.551744	0.007075	0.704256
-37.797831	-2.114776	2.561741	0.007083	0.704257
-37.323116	-2.100506	2.571738	0.006994	0.704457
-36.979543	-2.098316	2.581734	0.006930	0.704585
-36.933283	-2.106413	2.591731	0.006921	0.704585
-37.223519	-2.026554	2.601728	0.006975	0.704642
-36.079247	-2.110912	2.611725	0.006762	0.704883
-36.153190	-2.095871	2.621722	0.006776	0.704887
-36.200673	-2.087759	2.631718	0.006784	0.704887
-35.539503	-2.072204	2.641715	0.006661	0.705156
-35.355646	-2.079403	2.651712	0.006627	0.705208
-35.223752	-2.102532	2.661709	0.006602	0.705209
-34.995696	-2.078471	2.671706	0.006559	0.705339
-34.479204	-2.079678	2.681702	0.006463	0.705522
-34.386598	-2.097395	2.691699	0.006446	0.705520
-34.736655	-2.023305	2.701696	0.006511	0.705544
-33.577316	-2.071008	2.711693	0.006295	0.705864
-33.593154	-2.068538	2.721690	0.006298	0.705863
-33.559018	-2.076104	2.731686	0.006291	0.705861
-33.219389	-2.053834	2.741683	0.006228	0.706027
-32.886400	-2.065969	2.751680	0.006166	0.706123
-32.867632	-2.068269	2.761677	0.006162	0.706125
-32.791419	-2.018917	2.771674	0.006148	0.706252
-31.680177	-2.122669	2.781670	0.005941	0.706441
-31.925158	-2.079510	2.791667	0.005986	0.706441
-31.993461	-2.067572	2.801664	0.005999	0.706440
-31.015968	-2.099327	2.811661	0.005817	0.706727
-31.095669	-2.075007	2.821658	0.005831	0.706747
-31.042068	-2.084644	2.831654	0.005821	0.706748
-30.967292	-2.012676	2.841651	0.005807	0.706919
-30.195652	-2.073155	2.851648	0.005663	0.707074
-30.343385	-2.044957	2.861645	0.005691	0.707078
-30.176954	-2.042587	2.871642	0.005660	0.707143
-29.450644	-2.056950	2.881638	0.005524	0.707374
-29.315637	-2.081252	2.891635	0.005499	0.707374
-29.391698	-2.069139	2.901632	0.005513	0.707371
-28.789676	-2.046229	2.911629	0.005401	0.707632
-28.678929	-2.032387	2.921626	0.005380	0.707700
-28.588168	-2.051412	2.931622	0.005363	0.707695
-28.264439	-2.035389	2.941619	0.005303	0.707843
-27.656681	-2.060892	2.951616	0.005189	0.708009
-27.511819	-2.085663	2.961613	0.005162	0.708011
-27.469469	-2.093332	2.971610	0.005154	0.708011
-26.831289	-2.054781	2.981606	0.005035	0.708317
-26.648634	-2.070803	2.991603	0.005001	0.708350
-26.828819	-2.038107	3.001600	0.005035	0.708352
-26.573423	-2.025240	3.011597	0.004987	0.708469
-25.860962	-2.066239	3.021594	0.004854	0.708641
-25.840486	-2.070985	3.031590	0.004850	0.708639
-26.112061	-2.021103	3.041587	0.004901	0.708643
-25.135402	-2.039336	3.051584	0.004719	0.708955
-24.983691	-2.065871	3.061581	0.004690	0.708956
-24.935419	-2.074478	3.071578	0.004681	0.708956
-24.715192	-2.032212	3.081574	0.004640	0.709120
-24.335820	-2.027936	3.091571	0.004569	0.709264
-24.182130	-2.055916	3.101568	0.004540	0.709263
-24.103073	-2.046185	3.111565	0.004526	0.709311
-23.471330	-2.016110	3.121562	0.004408	0.709596
-23.092067	-2.083705	3.131558	0.004337	0.709597
-23.439154	-2.022594	3.141555	0.004402	0.709595
-22.809265	-2.030432	3.151552	0.004284	0.709804
-22.483858	-2.045040	3.161549	0.004224	0.709891
-22.504301	-2.039524	3.171546	0.004227	0.709895
-22.303477	-2.035050	3.181542	0.004190	0.709976
-21.646995	-2.033604	3.191539	0.004067	0.710213
-21.306065	-2.092527	3.201536	0.004004	0.710217
-21.694219	-2.024413	3.211533	0.004076	0.710215
-21.079065	-2.013837	3.221530	0.003961	0.710456
-20.733205	-2.037562	3.231526	0.003897	0.710532
-20.950032	-1.999435	3.241523	0.003937	0.710531
-20.490047	-2.011912	3.251520	0.003851	0.710670
-19.660123	-2.059255	3.261517	0.003696	0.710871
-19.747576	-2.043948	3.271514	0.003713	0.710870
-19.589011	-2.070798	3.281510	0.003683	0.710873
-19.081340	-2.065226	3.291507	0.003588	0.711065
-18.713362	-2.094970	3.301504	0.003520	0.711137
-18.820401	-2.075977	3.311501	0.003540	0.711137
-18.780540	-2.078149	3.321498	0.003532	0.711147
-18.373230	-1.996747	3.331494	0.003456	0.711455
-17.918978	-2.080399	3.341491	0.003371	0.711450
-17.897655	-2.083614	3.351488	0.003367	0.711451
-17.611310	-2.044121	3.361485	0.003314	0.711632
-17.121474	-2.066855	3.371482	0.003222	0.711761
-17.183524	-2.055095	3.381478	0.003234	0.711762
-17.438494	-1.980383	3.391475	0.003281	0.711821
-16.211400	-2.064941	3.401472	0.003053	0.712088
-16.520543	-2.010212	3.411469	0.003110	0.712088
-15.932485	-2.112960	3.421466	0.003000	0.712092
-15.830052	-2.024525	3.431462	0.002981	0.712305
-15.387983	-2.062534	3.441459	0.002899	0.712387
-15.418443	-2.057071	3.451456	0.002904	0.712387
-15.420767	-2.013067	3.461453	0.002905	0.712474
-14.430196	-2.070377	3.471450	0.002720	0.712711
-14.500099	-2.059573	3.481446	0.002733	0.712708
-14.677281	-2.030479	3.491443	0.002766	0.712704
-13.798555	-2.060161	3.501440	0.002602	0.712957
-13.724702	-2.039472	3.511437	0.002588	0.713024
-13.330686	-2.111642	3.521434	0.002515	0.713021
-13.577004	-2.050988	3.531430	0.002560	0.713054
-12.780521	-2.039819	3.541427	0.002412	0.713359
-12.631691	-2.066928	3.551424	0.002384	0.713358
-12.358012	-2.115456	3.561421	0.002333	0.713359
-12.273809	-2.083662	3.571418	0.002317	0.713452
-11.873415	-2.055607	3.581414	0.002243	0.713650
-11.630645	-2.098116	3.591411	0.002197	0.713652
-11.711844	-2.083220	3.601408	0.002212	0.713653
-11.125224	-2.074786	3.611405	0.002103	0.713877
-10.535852	-2.134060	3.621402	0.001993	0.713969
-10.820715	-2.082996	3.631398	0.002046	0.713969
-10.476100	-2.146559	3.641395	0.001982	0.713965
-10.110095	-2.075633	3.651392	0.001913	0.714236
-9.580258	-2.150045	3.661389	0.001815	0.714276
-9.595028	-2.147180	3.671386	0.001817	0.714277
-9.774896	-2.106679	3.681382	0.001851	0.714294
-8.863400	-2.111810	3.691379	0.001681	0.714606
-8.792769	-2.125813	3.701376	0.001667	0.714604
-8.710580	-2.140379	3.711373	0.001652	0.714604
-8.775816	-2.074079	3.721370	0.001664	0.714713
-7.912514	-2.130624	3.731366	0.001503	0.714906
-7.868718	-2.138902	3.741363	0.001495	0.714905
-7.972734	-2.120649	3.751360	0.001514	0.714905
-7.315029	-2.133998	3.761357	0.001392	0.715111
-7.069506	-2.117621	3.771354	0.001346	0.715231
-7.190049	-2.095874	3.781350	0.001368	0.715232
-6.800788	-2.164591	3.791347	0.001295	0.715233
-6.381036	-2.083548	3.801344	0.001217	0.715542
-6.094105	-2.133641	3.811341	0.001164	0.715545
-6.196098	-2.114882	3.821338	0.001182	0.715546
-5.974944	-2.076423	3.831334	0.001141	0.715701
-5.292174	-2.107834	3.841331	0.001014	0.715880
-5.257558	-2.114121	3.851328	0.001007	0.715880
-4.989238	-2.161212	3.861325	0.000957	0.715881
-4.736053	-2.098280	3.871322	0.000910	0.716096
-4.533665	-2.116464	3.881318	0.000872	0.716131
-4.415605	-2.138917	3.891315	0.000850	0.716129
-4.392802	-2.073737	3.901312	0.000846	0.716266
-3.641830	-2.117138	3.911309	0.000706	0.716445
-3.535522	-2.135840	3.921306	0.000686	0.716446
-3.412540	-2.152500	3.931302	0.000663	0.716457
-3.056367	-2.067230	3.941299	0.000596	0.716751
-2.697653	-2.130142	3.951296	0.000529	0.716753
-2.824113	-2.107737	3.961293	0.000553	0.716753
-2.296878	-2.089767	3.971290	0.000455	0.716975
-2.425510	-2.011315	3.981286	0.000478	0.717085
-2.036139	-2.081029	3.991283	0.000406	0.717085
-1.850073	-2.042778	4.001280	0.000371	0.717226
-1.733272	-1.985852	4.011277	0.000349	0.717380
-1.304385	-2.061891	4.021274	0.000269	0.717381
-1.909619	-1.854636	4.031270	0.000381	0.717578
-1.341018	-1.893881	4.041267	0.000276	0.717701
-1.395930	-1.851479	4.051264	0.000286	0.717765
-1.379210	-1.727657	4.061261	0.000282	0.718016
-0.713919	-1.845720	4.071258	0.000158	0.718017
-0.895188	-1.658252	4.081254	0.000192	0.718324
-0.911844	-1.641673	4.091251	0.000195	0.718351
-1.069572	-1.488537	4.101248	0.000224	0.718598
-1.217312	-1.418594	4.111245	0.000251	0.718685
-0.753085	-1.359614	4.121242	0.000165	0.718964
-0.577812	-1.327646	4.131238	0.000132	0.719089
-0.438012	-1.261016	4.141235	0.000106	0.719270
-0.342445	-1.155050	4.151232	0.000088	0.719513
-0.525464	-1.048557	4.161229	0.000122	0.719659
-0.468278	-0.934340	4.171226	0.000111	0.719904
-0.424514	-0.817214	4.181222	0.000102	0.720150
-0.244771	-0.748154	4.191219	0.000069	0.720350
-0.147392	-0.657648	4.201216	0.000050	0.720562
-0.243238	-0.480278	4.211213	0.000068	0.720878
-0.072634	-0.409049	4.221210	0.000036	0.721078
-0.196104	-0.267779	4.231206	0.000059	0.721313
-0.243033	-0.123802	4.241203	0.000067	0.721580
0.022656	-0.028123	4.251200	0.000018	0.721861
0.190558	0.091033	4.261197	-0.000014	0.722154
0.000000	0.305434	4.271194	0.000021	0.722509

0.271547	0.893042	4.276198	-0.000030	0.723756
0.166078	2.165428	4.281203	-0.000011	0.726209
0.509295	3.962382	4.286208	-0.000076	0.729829
0.642087	6.337826	4.291213	-0.000102	0.734477
1.090126	9.171859	4.296218	-0.000188	0.740083
1.278857	12.533802	4.301222	-0.000225	0.746562
1.754395	16.296566	4.306227	-0.000316	0.753836
2.402656	20.444056	4.311232	-0.000440	0.761814
2.522454	25.076997	4.316237	-0.000465	0.770431
2.964904	30.026234	4.321242	-0.000551	0.779632
3.394343	35.325479	4.326246	-0.000634	0.789350
3.725878	40.951524	4.331251	-0.000700	0.799500
4.126683	46.877545	4.336256	-0.000778	0.810068
4.697714	53.045953	4.341261	-0.000888	0.820971
5.136113	59.519508	4.346266	-0.000974	0.832212
5.474647	66.232456	4.351270	-0.001042	0.843675
6.587820	73.028751	4.356275	-0.001254	0.855349
8.941704	79.839045	4.361280	-0.001696	0.867245
9.663885	87.137154	4.366285	-0.001836	0.879303
10.889658	94.526733	4.371290	-0.002069	0.891483
12.268880	102.070273	4.376294	-0.002331	0.903783
13.366692	109.816014	4.381299	-0.002540	0.916153
13.972248	117.769009	4.386304	-0.002658	0.928543
14.528020	125.836630	4.391309	-0.002767	0.940928
15.405153	133.959498	4.396314	-0.002936	0.953318
16.118343	142.191179	4.401318	-0.003074	0.965666
16.509805	150.549656	4.406323	-0.003152	0.977961
17.358538	158.921809	4.411328	-0.003316	0.990236
18.157290	167.328945	4.416333	-0.003470	1.002398
18.847941	175.797756	4.421338	-0.003604	1.014473
19.700540	184.280576	4.426342	-0.003769	1.026464
20.409835	192.830623	4.431347	-0.003906	1.038374
21.151601	201.407299	4.436352	-0.004050	1.050191
21.954099	209.989466	4.441357	-0.004205	1.061899
22.580712	218.647088	4.446362	-0.004328	1.073537
23.183485	227.287975	4.451366	-0.004445	1.085024
23.552610	235.980591	4.456371	-0.004520	1.096404
24.095810	244.645862	4.461376	-0.004627	1.107671
24.460569	253.335791	4.466381	-0.004700	1.118816
25.175227	261.954414	4.471386	-0.004839	1.129837
25.715982	270.610018	4.476390	-0.004946	1.140760
26.488001	279.240241	4.481395	-0.005095	1.151597
27.651078	287.792877	4.486400	-0.005317	1.162319
28.223996	296.426520	4.491405	-0.005430	1.172918
28.587357	305.078137	4.496410	-0.005503	1.183401
29.425679	313.659931	4.501414	-0.005665	1.193805
30.085463	322.232204	4.506419	-0.005793	1.204072
30.876822	330.799799	4.511424	-0.005946	1.214272
31.517243	339.353291	4.516429	-0.006071	1.224341
31.920727	347.977573	4.521434	-0.006152	1.234363
32.598407	356.496748	4.526438	-0.006284	1.244236
33.419774	364.989984	4.531443	-0.006442	1.254030
33.963627	373.526725	4.536448	-0.006549	1.263744
34.489682	382.056074	4.541453	-0.006653	1.273372
35.436444	390.483933	4.546458	-0.006835	1.282894
36.173720	398.958826	4.551462	-0.006977	1.292357
36.613766	407.457867	4.556467	-0.007065	1.301724
37.492107	415.958141	4.561472	-0.007234	1.311104
37.718266	424.511552	4.566477	-0.007282	1.320357
38.153319	432.944191	4.571482	-0.007368	1.329454
38.769047	441.350127	4.576486	-0.007489	1.338493
39.334945	449.737548	4.581491	-0.007599	1.347443
39.715869	458.183092	4.586496	-0.007676	1.356362
40.079665	466.571837	4.591501	-0.007749	1.365160
40.946998	474.914912	4.596506	-0.007916	1.373941
41.575521	483.272199	4.601510	-0.008039	1.382640
41.853026	491.686264	4.606515	-0.008096	1.391283
42.414552	500.041760	4.611520	-0.008206	1.399861
42.490317	508.439112	4.616525	-0.008226	1.408347
42.928959	516.785472	4.621530	-0.008313	1.416792
43.574552	525.073728	4.626534	-0.008439	1.425162
43.987247	533.415874	4.631539	-0.008521	1.433499
44.474513	541.713628	4.636544	-0.008617	1.441756
44.902040	550.025611	4.641549	-0.008702	1.449970
45.359040	558.346814	4.646554	-0.008793	1.458151
45.754133	566.649527	4.651558	-0.008872	1.466258
46.050650	575.010753	4.656563	-0.008933	1.474362
46.829139	583.231050	4.661568	-0.009083	1.482361
47.715193	591.441970	4.666573	-0.009253	1.490326
48.131522	599.738308	4.671578	-0.009336	1.498256
48.605189	608.002972	4.676582	-0.009430	1.506123
49.010236	616.292017	4.681587	-0.009511	1.513961
49.497309	624.545015	4.686592	-0.009607	1.521738
49.772364	632.825499	4.691597	-0.009664	1.529468
50.319625	641.078166	4.696602	-0.009771	1.537174
50.792984	649.315690	4.701606	-0.009865	1.544817
50.953450	657.621737	4.706611	-0.009900	1.552439
51.417875	665.849198	4.711616	-0.009992	1.559996
52.052921	674.036917	4.716621	-0.010115	1.567506
52.402429	682.291886	4.721626	-0.010186	1.574999
52.800632	690.531357	4.726630	-0.010266	1.582449
53.273193	698.744249	4.731635	-0.010359	1.589851
53.761092	706.980006	4.736640	-0.010455	1.597242
54.182687	715.181002	4.741645	-0.010539	1.604558
54.391772	723.439842	4.746650	-0.010584	1.611861
55.002858	731.631884	4.751654	-0.010703	1.619129
55.063715	739.874059	4.756659	-0.010719	1.626332
55.470272	748.137800	4.761664	-0.010801	1.633570
55.828060	756.313751	4.766669	-0.010873	1.640692
56.223268	764.487204	4.771674	-0.010952	1.647787
56.631977	772.684368	4.776678	-0.011033	1.654874
56.982266	780.860327	4.781683	-0.011104	1.661904
57.416438	789.052309	4.786688	-0.011190	1.668929
57.769827	797.234320	4.791693	-0.011261	1.675906
58.294556	805.378632	4.796698	-0.011364	1.682844
58.690091	813.566423	4.801702	-0.011443	1.689773
58.935336	821.777436	4.806707	-0.011494	1.696673
59.567917	829.920115	4.811712	-0.011618	1.703540
60.024348	838.098095	4.816717	-0.011708	1.710384
60.171429	846.317352	4.821722	-0.011741	1.717195
60.434034	854.494455	4.826726	-0.011795	1.723960
60.808825	862.654511	4.831731	-0.011870	1.730698
61.374384	870.805764	4.836736	-0.011981	1.737428
61.645881	878.975112	4.841741	-0.012037	1.744108
61.852419	887.163482	4.846746	-0.012081	1.750770
62.492379	895.292714	4.851750	-0.012205	1.757414
63.336348	903.354072	4.856755	-0.012368	1.764003
64.478784	911.437013	4.861760	-0.012586	1.770622
64.528161	919.680728	4.866765	-0.012600	1.777209
64.709828	927.871428	4.871770	-0.012640	1.783746
65.125032	936.062644	4.876774	-0.012722	1.790287
65.631523	944.231678	4.881779	-0.012822	1.796799
65.928605	952.392918	4.886784	-0.012883	1.803255
66.188704	960.533181	4.891789	-0.012936	1.809667
66.700236	968.667368	4.896794	-0.013037	1.816082
67.180837	976.798835	4.901798	-0.013132	1.822468
67.291112	984.977040	4.906803	-0.013158	1.828824
67.559204	993.140734	4.911808	-0.013213	1.835166
67.948820	1001.250933	4.916813	-0.013291	1.841458
68.323633	1009.380331	4.921818	-0.013366	1.847742
68.429348	1017.577795	4.926822	-0.013391	1.854026
68.913619	1025.654394	4.931827	-0.013487	1.860240
69.277488	1033.794777	4.936832	-0.013560	1.866467
69.588046	1041.957014	4.941837	-0.013623	1.872684
69.921178	1050.084411	4.946842	-0.013690	1.878857
70.280221	1058.185454	4.951846	-0.013763	1.884993
70.774602	1066.283276	4.956851	-0.013860	1.891121
71.230840	1074.408607	4.961856	-0.013950	1.897246
71.879387	1082.489276	4.966861	-0.014076	1.903340
72.394232	1090.608904	4.971866	-0.014178	1.909428
72.604905	1098.790802	4.976870	-0.014222	1.915508
72.766294	1106.921816	4.981875	-0.014258	1.921526
73.013323	1115.061102	4.986880	-0.014309	1.927541
73.387773	1123.187448	4.991885	-0.014384	1.933541
73.880073	1131.277594	4.996890	-0.014481	1.939509
74.470127	1139.368978	5.001894	-0.014596	1.945471
74.620002	1147.552212	5.006899	-0.014630	1.951433
74.699383	1155.726512	5.011904	-0.014650	1.957362
75.149448	1163.779921	5.016909	-0.014739	1.963226
75.448742	1171.881874	5.021914	-0.014800	1.969092
75.674097	1180.021477	5.026918	-0.014847	1.974959
75.795477	1188.133288	5.031923	-0.014875	1.980778
76.243580	1196.219544	5.036928	-0.014964	1.986596
76.748694	1204.306700	5.041933	-0.015063	1.992403
76.997303	1212.426904	5.046938	-0.015115	1.998190
77.548034	1220.486062	5.051942	-0.015223	2.003949
77.820422	1228.601242	5.056947	-0.015279	2.009701
78.129486	1236.741383	5.061952	-0.015342	2.015459
78.652608	1244.805243	5.066957	-0.015445	2.021168
79.064465	1252.910331	5.071962	-0.015527	2.026879
79.185636	1261.094913	5.076966	-0.015555	2.032599
79.452453	1269.179407	5.081971	-0.015610	2.038248
79.891759	1277.258287	5.086976	-0.015697	2.043895
79.999198	1285.380331	5.091981	-0.015722	2.049523
81.068695	1293.374289	5.096986	-0.015927	2.055144
81.635565	1301.452068	5.101990	-0.016037	2.060757
81.913177	1309.554962	5.106995	-0.016095	2.066342
82.140301	1317.722580	5.112000	-0.016142	2.071951
82.520478	1325.818272	5.117005	-0.016218	2.077512
82.926801	1333.883917	5.122010	-0.016299	2.083040
83.318858	1341.991134	5.127014	-0.016378	2.088579
83.348189	1350.146298	5.132019	-0.016388	2.094101
83.778761	1358.222476	5.137024	-0.016474	2.099594
83.934047	1366.323327	5.142029	-0.016508	2.105063
83.987692	1374.475906	5.147034	-0.016524	2.110542
84.369310	1382.603541	5.152038	-0.016600	2.116022
84.765506	1390.637901	5.157043	-0.016679	2.121426
84.984513	1398.734770	5.162048	-0.016725	2.126842
85.180585	1406.833180	5.167053	-0.016767	2.132243
85.483207	1414.897609	5.172058	-0.016829	2.137617
85.738332	1422.982300	5.177062	-0.016882	2.142987
86.096807	1431.048979	5.182067	-0.016954	2.148341
86.372478	1439.167390	5.187072	-0.017010	2.153708
86.735037	1447.221943	5.192077	-0.017083	2.159028
86.931883	1455.301422	5.197082	-0.017125	2.164336
87.442894	1463.357824	5.202086	-0.017226	2.169644
88.014836	1471.405054	5.207091	-0.017337	2.174940
88.309354	1479.516790	5.212096	-0.017398	2.180238
88.560343	1487.615609	5.217101	-0.017450	2.185511
89.031067	1495.704032	5.222106	-0.017543	2.190785
89.248961	1503.832807	5.227110	-0.017589	2.196049
89.539198	1511.882164	5.232115	-0.017648	2.201256
90.037161	1519.940977	5.237120	-0.017746	2.206475
90.339609	1528.041666	5.242125	-0.017808	2.211692
90.369733	1536.153551	5.247130	-0.017819	2.216878
90.841110	1544.207290	5.252134	-0.017912	2.222055
90.944401	1552.286830	5.257139	-0.017936	2.227203
91.212552	1560.416735	5.262144	-0.017992	2.232386
91.374168	1568.497947	5.267149	-0.018027	2.237516
91.427695	1576.562711	5.272154	-0.018042	2.242615
91.991434	1584.608685	5.277158	-0.018152	2.247735
92.210500	1592.694587	5.282163	-0.018199	2.252839
92.291533	1600.797268	5.287168	-0.018219	2.257929
92.825369	1608.835188	5.292173	-0.018324	2.263007
93.003507	1616.913361	5.297178	-0.018362	2.268067
93.362609	1625.060892	5.302182	-0.018434	2.273175
93.505135	1633.124756	5.307187	-0.018466	2.278201
93.511244	1641.202205	5.312192	-0.018473	2.283212
93.786568	1649.247665	5.317197	-0.018529	2.288216
94.299774	1657.285262	5.322202	-0.018630	2.293224
94.646907	1665.344113	5.327206	-0.018700	2.298220
94.845599	1673.399208	5.332211	-0.018742	2.303190
95.051647	1681.488161	5.337216	-0.018786	2.308171
95.497196	1689.555564	5.342221	-0.018874	2.313148
95.600231	1697.625857	5.347226	-0.018899	2.318087
95.785495	1705.706062	5.352230	-0.018939	2.323029
96.324976	1713.734764	5.357235	-0.019045	2.327958
96.848582	1721.795122	5.362240	-0.019147	2.332895
96.940850	1729.904483	5.367245	-0.019170	2.337815
97.409150	1737.939107	5.372250	-0.019262	2.342710
97.789573	1746.020653	5.377254	-0.019339	2.347616
97.838909	1754.132007	5.382259	-0.019353	2.352503
98.187240	1762.203988	5.387264	-0.019423	2.357381
98.530070	1770.243889	5.392269	-0.019492	2.362228
98.862162	1778.282925	5.397274	-0.019560	2.367064
99.206350	1786.365275	5.402278	-0.019629	2.371917
99.582853	1794.414179	5.407283	-0.019704	2.376743
99.776834	1802.485013	5.412288	-0.019746	2.381557
99.953102	1810.575219	5.417293	-0.019784	2.386372
100.070826	1818.664922	5.422298	-0.019811	2.391172
100.567982	1826.707317	5.427302	-0.019909	2.395964
100.633584	1834.774453	5.432307	-0.019927	2.400727
100.818612	1842.835914	5.437312	-0.019966	2.405487
101.249460	1850.889553	5.442317	-0.020052	2.410252
101.458708	1858.973400	5.447322	-0.020096	2.415008
101.651231	1867.049112	5.452326	-0.020137	2.419748
102.085135	1875.060402	5.457331	-0.020224	2.424461
102.284548	1883.166029	5.462336	-0.020266	2.429200
102.777414	1891.285143	5.467341	-0.020363	2.433961
102.823677	1899.329463	5.472346	-0.020377	2.438635
103.168665	1907.351547	5.477350	-0.020447	2.443310
103.421787	1915.389146	5.482355	-0.020499	2.447978
103.625439	1923.470137	5.487360	-0.020542	2.452658
103.867491	1931.534282	5.492365	-0.020593	2.457323
104.061905	1939.586184	5.497370	-0.020634	2.461968
104.322576	1947.648853	5.502374	-0.020688	2.466615
104.519706	1955.703284	5.507379	-0.020730	2.471244
104.909402	1963.770271	5.512384	-0.020808	2.475886
104.923921	1971.838223	5.517389	-0.020816	2.480491
105.059592	1979.873363	5.522394	-0.020846	2.485079
105.562083	1987.899774	5.527398	-0.020945	2.489680
105.777987	1995.994442	5.532403	-0.020991	2.494290
106.424967	2003.993055	5.537408	-0.021117	2.498869
106.865863	2012.027560	5.542413	-0.021204	2.503444
107.189215	2020.097465	5.547418	-0.021270	2.508023
107.424968	2028.219119	5.552422	-0.021319	2.512615
107.732036	2036.268832	5.557427	-0.021381	2.517164
108.194947	2044.286033	5.562432	-0.021473	2.521698
108.455225	2052.352568	5.567437	-0.021527	2.526237
108.460262	2060.436827	5.572442	-0.021533	2.530759
108.791406	2068.516567	5.577446	-0.021600	2.535294
108.964717	2076.553746	5.582451	-0.021637	2.539785
109.131874	2084.600997	5.587456	-0.021674	2.544274
109.502488	2092.659490	5.592461	-0.021748	2.548775
109.645123	2100.733229	5.597466	-0.021780	2.553261
109.889830	2108.800702	5.602470	-0.021831	2.557743
109.884144	2116.842339	5.607475	-0.021835	2.562185
110.295943	2124.883708	5.612480	-0.021917	2.566648
110.420858	2132.965885	5.617485	-0.021946	2.571106
110.545805	2141.022085	5.622490	-0.021974	2.575542
110.833837	2149.074308	5.627494	-0.022033	2.579979
111.035056	2157.098133	5.632499	-0.022076	2.584387
111.212010	2165.168551	5.637504	-0.022114	2.588812
111.490251	2173.383630	5.642509	-0.022171	2.593314
111.719700	2181.399607	5.647514	-0.022219	2.597697
112.088345	2189.384320	5.652518	-0.022293	2.602065
112.263164	2197.398490	5.657523	-0.022331	2.606429
112.833331	2205.393152	5.662528	-0.022443	2.610801
113.341103	2213.445116	5.667533	-0.022543	2.615192
113.433555	2221.485231	5.672538	-0.022565	2.619542
113.737320	2229.537516	5.677542	-0.022627	2.623906
114.153820	2237.565954	5.682547	-0.022710	2.628256
114.301403	2245.652194	5.687552	-0.022743	2.632613
114.529042	2253.713529	5.692557	-0.022790	2.636954
114.755072	2261.740962	5.697562	-0.022838	2.641270
115.142626	2269.791029	5.702566	-0.022915	2.645602
115.339858	2277.838671	5.707571	-0.022957	2.649912
115.591972	2285.917436	5.712576	-0.023009	2.654236
115.849497	2293.969541	5.717581	-0.023063	2.658539
116.110837	2301.990876	5.722586	-0.023117	2.662818
116.306839	2310.056797	5.727590	-0.023158	2.667110
116.396384	2318.134043	5.732595	-0.023180	2.671395
116.681076	2326.201200	5.737600	-0.023239	2.675679
117.013884	2334.204023	5.742605	-0.023306	2.679926
117.259472	2342.212526	5.747610	-0.023357	2.684164
117.774001	2350.238717	5.752614	-0.023458	2.688421
117.911964	2358.315071	5.757619	-0.023489	2.692674
117.984757	2366.380573	5.762624	-0.023508	2.696910
118.015306	2374.449575	5.767629	-0.023519	2.701139
118.121197	2382.475004	5.772634	-0.023544	2.705343
118.522471	2390.508673	5.777638	-0.023624	2.709563
118.913563	2398.547338	5.782643	-0.023702	2.713779
119.218288	2406.576050	5.787648	-0.023764	2.717977
119.365323	2414.634978	5.792653	-0.023797	2.722175
119.658536	2422.663133	5.797658	-0.023857	2.726359
119.778254	2430.746144	5.802662	-0.023884	2.730555
120.060886	2438.799368	5.807667	-0.023942	2.734739
120.399915	2446.825142	5.812672	-0.024011	2.738905
120.931749	2454.832642	5.817677	-0.024115	2.743068
120.677246	2462.943116	5.822682	-0.024073	2.747229
120.979070	2471.025634	5.827686	-0.024135	2.751404
121.120559	2479.138885	5.832691	-0.024166	2.755578
121.364466	2487.118404	5.837696	-0.024217	2.759683
121.422488	2495.148862	5.842701	-0.024233	2.763797
121.621992	2503.168633	5.847706	-0.024276	2.767909
121.839565	2511.216699	5.852710	-0.024321	2.772029
122.085053	2519.272384	5.857715	-0.024372	2.776149
122.270596	2527.283930	5.862720	-0.024412	2.780236
122.691988	2535.303287	5.867725	-0.024496	2.784336
122.662051	2543.370536	5.872730	-0.024496	2.788427
122.975335	2551.423986	5.877734	-0.024559	2.792525
123.494510	2559.429160	5.882739	-0.024661	2.796605
123.587002	2567.469067	5.887744	-0.024684	2.800671
123.662956	2575.525725	5.892749	-0.024703	2.804739
123.751827	2583.559763	5.897754	-0.024725	2.808791
124.391639	2591.600467	5.902758	-0.024850	2.812872
124.154005	2599.689292	5.907763	-0.024811	2.816920
124.620600	2607.683335	5.912768	-0.024903	2.820955
125.136395	2615.714656	5.917773	-0.025004	2.825007
125.029694	2623.801442	5.922778	-0.024990	2.829044
125.190573	2631.898614	5.927782	-0.025025	2.833096
125.375616	2639.914490	5.932787	-0.025065	2.837103
125.784012	2647.912022	5.937792	-0.025146	2.841108
126.113093	2655.916877	5.942797	-0.025213	2.845106
126.365862	2663.946861	5.947802	-0.025265	2.849107
126.754935	2672.023278	5.952806	-0.025343	2.853133
126.780377	2680.088011	5.957811	-0.025353	2.857127
126.928237	2688.117392	5.962816	-0.025386	2.861105
127.275610	2696.146977	5.967821	-0.025456	2.865088
127.397372	2704.196166	5.972826	-0.025483	2.869063
127.479501	2712.292766	5.977830	-0.025504	2.873054
127.813327	2720.285441	5.982835	-0.025572	2.877001
128.180630	2728.312906	5.987840	-0.025645	2.880962
128.352017	2736.338432	5.992845	-0.025682	2.884907
128.702579	2744.369767	5.997850	-0.025753	2.888858
128.906636	2752.454780	6.002854	-0.025796	2.892822
129.163752	2760.477927	6.007859	-0.025850	2.896753
129.073755	2768.537752	6.012864	-0.025838	2.900678
129.592852	2776.531483	6.017869	-0.025940	2.904598
129.848539	2784.588503	6.022874	-0.025993	2.908530
129.942255	2792.713019	6.027878	-0.026016	2.912480
130.236958	2800.749211	6.032883	-0.026076	2.916393
130.577489	2808.727466	6.037888	-0.026145	2.920275
130.667243	2816.756283	6.042893	-0.026167	2.924163
130.804490	2824.779002	6.047898	-0.026197	2.928045
131.371043	2832.807020	6.052902	-0.026308	2.931947
131.468527	2840.865398	6.057907	-0.026332	2.935834
131.613310	2848.890404	6.062912	-0.026364	2.939702
131.947573	2856.908085	6.067917	-0.026431	2.943571
132.112229	2864.947728	6.072922	-0.026467	2.947437
132.321976	2873.038781	6.077926	-0.026512	2.951325
132.452596	2881.087151	6.082931	-0.026541	2.955183
132.542726	2889.087074	6.087936	-0.026564	2.959011
132.786519	2897.129306	6.092941	-0.026614	2.962862
132.917569	2905.148375	6.097946	-0.026644	2.966691
133.289608	2913.192721	6.102950	-0.026718	2.970540
133.444315	2921.275571	6.107955	-0.026753	2.974391
133.565842	2929.302130	6.112960	-0.026781	2.978208
134.010335	2937.315807	6.117965	-0.026869	2.982030
134.196232	2945.327304	6.122970	-0.026908	2.985834
134.291538	2953.397718	6.127974	-0.026932	2.989656
134.640814	2961.456205	6.132979	-0.027002	2.993480
135.027715	2969.468230	6.137984	-0.027079	2.997279
135.225949	2977.510571	6.142989	-0.027121	3.001078
135.075088	2985.515731	6.147994	-0.027099	3.004838
135.560886	2993.532267	6.152998	-0.027194	3.008630
135.703804	3001.599876	6.158003	-0.027226	3.012423
135.714060	3009.658337	6.163008	-0.027234	3.016202
136.087461	3017.661530	6.168013	-0.027308	3.019967
136.362634	3025.660463	6.173018	-0.027365	3.023721
136.626399	3033.733552	6.178022	-0.027419	3.027504
136.879746	3041.781804	6.183027	-0.027472	3.031271
137.024734	3049.811905	6.188032	-0.027504	3.035019
137.082603	3057.863737	6.193037	-0.027520	3.038768
137.172495	3065.871818	6.198042	-0.027542	3.042494
137.604625	3073.903530	6.203046	-0.027628	3.046242
137.905794	3081.922485	6.208051	-0.027689	3.049974
138.260728	3089.980975	6.213056	-0.027761	3.053722
138.787543	3098.011626	6.218061	-0.027864	3.057461
138.879771	3106.063143	6.223066	-0.027887	3.061184
139.053034	3114.080328	6.228070	-0.027924	3.064890
139.114312	3122.145879	6.233075	-0.027941	3.068609
139.416030	3130.232711	6.238080	-0.028002	3.072344
139.830006	3138.297731	6.243085	-0.028085	3.076071
139.646423	3146.284428	6.248090	-0.028056	3.079728
139.873498	3154.297485	6.253094	-0.028103	3.083413
140.060505	3162.294972	6.258099	-0.028144	3.087084
140.240580	3170.300734	6.263104	-0.028182	3.090754
140.583668	3178.360531	6.268109	-0.028252	3.094452
140.805828	3186.385499	6.273114	-0.028298	3.098124
140.979354	3194.428420	6.278118	-0.028336	3.101798
141.045929	3202.477969	6.283123	-0.028353	3.105465
141.317059	3210.486380	6.288128	-0.028409	3.109119
141.569279	3218.572278	6.293133	-0.028462	3.112803
141.624082	3226.605612	6.298138	-0.028477	3.116449
141.879447	3234.582247	6.303142	-0.028530	3.120075
142.138142	3242.599719	6.308147	-0.028583	3.123715
142.397109	3250.625272	6.313152	-0.028637	3.127354
142.563108	3258.711709	6.318157	-0.028673	3.131012
142.775786	3266.732433	6.323162	-0.028718	3.134639
143.149829	3274.754297	6.328166	-0.028793	3.138269
143.211284	3282.821922	6.333171	-0.028810	3.141901
143.423745	3290.818768	6.338176	-0.028855	3.145504
143.737891	3298.850435	6.343181	-0.028918	3.149123
143.612331	3306.921229	6.348186	-0.028900	3.152737
143.741864	3314.977049	6.353190	-0.028930	3.156350
143.993110	3322.977954	6.358195	-0.028982	3.159940
144.369217	3330.952893	6.363200	-0.029057	3.163520
144.362720	3339.033637	6.368205	-0.029061	3.167126
144.452094	3347.032338	6.373210	-0.029083	3.170696
144.843794	3355.095802	6.378214	-0.029161	3.174303
144.967408	3363.113704	6.383219	-0.029190	3.177875
145.335346	3371.117204	6.388224	-0.029263	3.181446
145.725208	3379.155236	6.393229	-0.029341	3.185030
145.689324	3387.192553	6.398234	-0.029340	3.188591
145.961311	3395.282089	6.403238	-0.029396	3.192185
146.115635	3403.305938	6.408243	-0.029430	3.195740
146.260415	3411.279614	6.413248	-0.029462	3.199269
146.410801	3419.328178	6.418253	-0.029495	3.202827
146.642585	3427.358216	6.423258	-0.029544	3.206376
146.915295	3435.401916	6.428262	-0.029600	3.209930
147.182631	3443.446656	6.433267	-0.029655	3.213479
147.151549	3451.478059	6.438272	-0.029655	3.217006
147.680220	3459.494833	6.443277	-0.029758	3.220546
147.913098	3467.481461	6.448282	-0.029807	3.224057
148.034602	3475.537277	6.453286	-0.029835	3.227589
148.197110	3483.618151	6.458291	-0.029870	3.231131
148.299094	3491.689312	6.463296	-0.029895	3.234661
148.569422	3499.691422	6.468301	-0.029950	3.238165
148.719838	3507.682661	6.473306	-0.029984	3.241655
149.060209	3515.669299	6.478310	-0.030052	3.245147
148.975747	3523.723373	6.483315	-0.030042	3.248647
149.271464	3531.739528	6.488320	-0.030102	3.252143
149.534151	3539.825066	6.493325	-0.030157	3.255663
149.552092	3547.798621	6.498330	-0.030165	3.259121
149.911980	3555.826476	6.503334	-0.030237	3.262613
149.963381	3563.881225	6.508339	-0.030252	3.266100
150.235821	3571.870961	6.513344	-0.030308	3.269564
150.331071	3579.961412	6.518349	-0.030331	3.273061
150.555773	3587.997382	6.523354	-0.030379	3.276536
150.780195	3595.978950	6.528358	-0.030426	3.279984
151.000802	3604.017278	6.533363	-0.030472	3.283452
150.994835	3612.070148	6.538368	-0.030476	3.286914
151.347061	3620.097781	6.543373	-0.030547	3.290375
151.372308	3628.132139	6.548378	-0.030557	3.293823
151.423741	3636.177686	6.553382	-0.030572	3.297273
151.656309	3644.204533	6.558387	-0.030620	3.300719
151.749616	3652.190975	6.563392	-0.030643	3.304138
151.997561	3660.233373	6.568397	-0.030695	3.307584
152.382262	3668.260409	6.573402	-0.030772	3.311024
152.445477	3676.334043	6.578406	-0.030789	3.314469
152.523373	3684.348806	6.583411	-0.030808	3.317885
152.686078	3692.324734	6.588416	-0.030844	3.321284
152.916201	3700.346336	6.593421	-0.030892	3.324702
153.023830	3708.380465	6.598426	-0.030917	3.328118
153.288917	3716.423814	6.603430	-0.030972	3.331539
153.445424	3724.482863	6.608435	-0.031007	3.334959
153.640315	3732.458357	6.613440	-0.031048	3.338342
153.821846	3740.511908	6.618445	-0.031087	3.341755
153.735995	3748.540105	6.623450	-0.031077	3.345143
154.114652	3756.572359	6.628454	-0.031152	3.348546
154.300071	3764.626744	6.633459	-0.031192	3.351948
154.488007	3772.650619	6.638464	-0.031232	3.355334
154.633809	3780.669252	6.643469	-0.031265	3.358712
154.816207	3788.669846	6.648474	-0.031304	3.362081
155.108911	3796.704803	6.653478	-0.031364	3.365465
155.307778	3804.723260	6.658483	-0.031406	3.368835
155.527175	3812.751822	6.663488	-0.031452	3.372207
155.768793	3820.831411	6.668493	-0.031503	3.375598
155.846945	3828.821846	6.673498	-0.031523	3.378942
156.003836	3836.875621	6.678502	-0.031557	3.382312
156.137268	3844.899077	6.683507	-0.031587	3.385665
156.215823	3852.893985	6.688512	-0.031607	3.389000
156.476824	3861.034435	6.693517	-0.031661	3.392400
156.789346	3869.039966	6.698522	-0.031725	3.395742
156.833128	3877.021972	6.703526	-0.031738	3.399061
157.115721	3885.022664	6.708531	-0.031796	3.402393
157.236560	3893.013973	6.713536	-0.031824	3.405712
157.516414	3901.045118	6.718541	-0.031881	3.409051
157.466047	3909.107189	6.723546	-0.031877	3.412387
157.742080	3917.137235	6.728550	-0.031934	3.415718
157.885576	3925.152202	6.733555	-0.031966	3.419034
158.069486	3933.139913	6.738560	-0.032005	3.422338
158.011458	3941.201553	6.743565	-0.032000	3.425661
158.165677	3949.229308	6.748570	-0.032034	3.428974
158.264966	3957.280790	6.753574	-0.032058	3.432291
158.666659	3965.322233	6.758579	-0.032138	3.435611
158.735243	3973.291608	6.763584	-0.032156	3.438888
158.868052	3981.335697	6.768589	-0.032186	3.442193
159.332752	3989.324849	6.773594	-0.032277	3.445485
159.813146	3997.324406	6.778598	-0.032372	3.448777
159.915050	4005.441026	6.783603	-0.032397	3.452102
159.930324	4013.431930	6.788608	-0.032405	3.455370
160.332772	4021.459705	6.793613	-0.032485	3.458662
160.463592	4029.499498	6.798618	-0.032515	3.461947
160.552545	4037.525060	6.803622	-0.032536	3.465222
160.709213	4045.552859	6.808627	-0.032571	3.468496
160.967309	4053.610189	6.813632	-0.032624	3.471783
161.146566	4061.666175	6.818637	-0.032663	3.475064
161.332584	4069.643189	6.823642	-0.032703	3.478309
161.621784	4077.638840	6.828646	-0.032762	3.481563
162.007874	4085.650656	6.833651	-0.032839	3.484823
162.167346	4093.685663	6.838656	-0.032874	3.488082
162.394637	4101.726808	6.843661	-0.032922	3.491342
162.663992	4109.763791	6.848666	-0.032977	3.494600
162.714179	4117.798437	6.853670	-0.032992	3.497846
162.682482	4125.844630	6.858675	-0.032991	3.501091
163.173048	4133.782563	6.863680	-0.033088	3.504306
163.508485	4141.846292	6.868685	-0.033156	3.507564
163.522790	4149.881936	6.873690	-0.033164	3.510798
163.697767	4157.925831	6.878694	-0.033201	3.514036
163.870486	4165.985963	6.883699	-0.033239	3.517279
163.901091	4173.964091	6.888704	-0.033250	3.520480
164.017216	4181.977246	6.893709	-0.033277	3.523696
164.240600	4190.004418	6.898714	-0.033324	3.526918
164.256304	4198.022056	6.903718	-0.033332	3.530126
164.446194	4206.112698	6.908723	-0.033373	3.533366
164.525159	4214.102730	6.913728	-0.033393	3.536560
164.810448	4222.126718	6.918733	-0.033451	3.539770
165.107041	4230.132206	6.923738	-0.033511	3.542970
165.369805	4238.135852	6.928742	-0.033566	3.546166
165.703490	4246.165080	6.933747	-0.033633	3.549371
165.797031	4254.279378	6.938752	-0.033656	3.552600
165.876478	4262.352619	6.943757	-0.033676	3.555809
166.003674	4270.290339	6.948762	-0.033705	3.558963
166.394420	4278.296763	6.953766	-0.033783	3.562149
166.419215	4286.306851	6.958771	-0.033793	3.565323
166.581981	4294.313919	6.963776	-0.033828	3.568497
166.859160	4302.371912	6.968781	-0.033885	3.571691
166.742203	4310.410038	6.973786	-0.033869	3.574863
167.058536	4318.400605	6.978790	-0.033933	3.578026
167.466323	4326.418647	6.983795	-0.034014	3.581200
167.319729	4334.439953	6.988800	-0.033992	3.584357
167.426493	4342.466541	6.993805	-0.034017	3.587520
167.574256	4350.486182	6.998810	-0.034050	3.590678
167.885728	4358.521804	7.003814	-0.034114	3.593845
167.904527	4366.583349	7.008819	-0.034122	3.597010
168.042464	4374.539949	7.013824	-0.034153	3.600136
168.345708	4382.576165	7.018829	-0.034215	3.603294
168.435540	4390.638806	7.023834	-0.034237	3.606454
168.559745	4398.626287	7.028838	-0.034266	3.609582
168.802347	4406.690653	7.033843	-0.034316	3.612741
169.090714	4414.662188	7.038848	-0.034375	3.615863
169.200486	4422.694185	7.043853	-0.034401	3.619000
169.451073	4430.722487	7.048858	-0.034453	3.622137
169.670730	4438.721556	7.053862	-0.034499	3.625259
169.826199	4446.796323	7.058867	-0.034533	3.628406
169.951904	4454.834474	7.063872	-0.034562	3.631535
170.232376	4462.876075	7.068877	-0.034619	3.634667
170.376704	4470.889148	7.073882	-0.034651	3.637782
170.463425	4478.882549	7.078886	-0.034673	3.640884
170.621410	4486.893205	7.083891	-0.034708	3.643993
170.847433	4494.914965	7.088896	-0.034755	3.647105
170.860731	4502.968794	7.093901	-0.034763	3.650221
171.031159	4510.991281	7.098906	-0.034800	3.653326
171.289880	4519.060745	7.103910	-0.034853	3.656450
171.404818	4527.053941	7.108915	-0.034880	3.659537
171.439569	4535.078834	7.113920	-0.034892	3.662632
171.947761	4543.081717	7.118925	-0.034992	3.665728
171.946718	4551.116250	7.123930	-0.034997	3.668820
171.904301	4559.167665	7.128934	-0.034994	3.671915
172.393496	4567.182853	7.133939	-0.035091	3.675008
172.424240	4575.151098	7.138944	-0.035102	3.678068
172.591197	4583.207288	7.143949	-0.035138	3.681162
172.640333	4591.208911	7.148954	-0.035152	3.684230
173.198906	4599.207894	7.153958	-0.035262	3.687307
173.412411	4607.261953	7.158963	-0.035307	3.690395
173.246669	4615.297223	7.163968	-0.035281	3.693462
173.628641	4623.321888	7.168973	-0.035358	3.696537
173.897533	4631.314999	7.173978	-0.035413	3.699594
174.037647	4639.338012	7.178982	-0.035444	3.702657
174.256675	4647.382266	7.183987	-0.035490	3.705728
174.482159	4655.389396	7.188992	-0.035538	3.708782
174.549157	4663.452915	7.193997	-0.035555	3.711851
174.695419	4671.534458	7.199002	-0.035588	3.714926
174.821490	4679.501527	7.204006	-0.035617	3.717955
175.167753	4687.503816	7.209011	-0.035686	3.720999
175.273860	4695.444992	7.214016	-0.035711	3.724013
175.470759	4703.513002	7.219021	-0.035753	3.727074
175.639985	4711.519362	7.224026	-0.035790	3.730109
175.663991	4719.575396	7.229030	-0.035800	3.733156
175.911179	4727.628048	7.234035	-0.035851	3.736205
176.104853	4735.595642	7.239040	-0.035893	3.739218
176.294774	4743.621318	7.244045	-0.035933	3.742250
176.148417	4751.664724	7.249050	-0.035911	3.745279
176.381386	4759.711617	7.254054	-0.035960	3.748315
176.477889	4767.747088	7.259059	-0.035983	3.751342
176.618735	4775.748141	7.264064	-0.036015	3.754354
176.915779	4783.789244	7.269069	-0.036075	3.757382
177.014501	4791.785984	7.274074	-0.036099	3.760387
177.262961	4799.740831	7.279078	-0.036151	3.763377
177.481959	4807.834742	7.284083	-0.036197	3.766416
177.779257	4815.829608	7.289088	-0.036257	3.769417
178.081865	4823.886576	7.294093	-0.036319	3.772439
178.182460	4831.943199	7.299098	-0.036343	3.775454
178.285040	4839.915079	7.304102	-0.036367	3.778435
178.316157	4847.982948	7.309107	-0.036379	3.781448
178.326451	4855.955543	7.314112	-0.036386	3.784422
178.516101	4864.025058	7.319117	-0.036426	3.787434
178.435284	4872.082026	7.324122	-0.036417	3.790433
178.517328	4880.090330	7.329126	-0.036437	3.793415
178.838586	4888.126056	7.334131	-0.036502	3.796411
179.058104	4896.049050	7.339136	-0.036548	3.799359
179.178123	4904.098574	7.344141	-0.036576	3.802350
179.040058	4912.085477	7.349146	-0.036556	3.805310
179.282005	4920.116105	7.354150	-0.036606	3.808293
179.424500	4928.177497	7.359155	-0.036638	3.811282
179.555435	4936.180982	7.364160	-0.036667	3.814247
179.865698	4944.214139	7.369165	-0.036731	3.817224
180.161169	4952.192022	7.374170	-0.036791	3.820178
180.232249	4960.196753	7.379174	-0.036809	3.823136
180.227257	4968.289121	7.384179	-0.036814	3.826121
180.453058	4976.224660	7.389184	-0.036861	3.829051
180.701966	4984.332087	7.394189	-0.036913	3.832043
180.703826	4992.326791	7.399194	-0.036918	3.834986
180.884710	5000.337035	7.404198	-0.036957	3.837936
181.093466	5008.370650	7.409203	-0.037001	3.840893
181.159753	5016.319063	7.414208	-0.037019	3.843813
181.473414	5024.380548	7.419213	-0.037083	3.846778
181.592804	5032.381736	7.424218	-0.037110	3.849714
181.681350	5040.459854	7.429222	-0.037132	3.852676
181.984704	5048.476015	7.434227	-0.037194	3.855617
182.133206	5056.475406	7.439232	-0.037227	3.858546
182.358899	5064.550173	7.444237	-0.037274	3.861502
182.404998	5072.521382	7.449242	-0.037288	3.864415
182.641756	5080.571208	7.454246	-0.037337	3.867357
182.911203	5088.581819	7.459251	-0.037393	3.870284
182.913806	5096.809364	7.464256	-0.037399	3.873283
183.322889	5104.854055	7.469261	-0.037480	3.876220
183.581559	5112.739756	7.474266	-0.037534	3.879095
183.649123	5120.708688	7.479270	-0.037551	3.881993
183.811245	5128.727549	7.484275	-0.037587	3.884910
183.969674	5136.731204	7.489280	-0.037622	3.887819
184.188844	5144.746310	7.494285	-0.037668	3.890731
184.236601	5152.790380	7.499290	-0.037682	3.893648
184.468034	5160.819615	7.504294	-0.037730	3.896560
184.824389	5168.782823	7.509299	-0.037802	3.899449
184.673128	5176.823571	7.514304	-0.037779	3.902355
184.921332	5184.855470	7.519309	-0.037831	3.905262
185.162231	5192.852337	7.524314	-0.037881	3.908155
185.398046	5200.857233	7.529318	-0.037930	3.911048
185.598252	5208.938422	7.534323	-0.037973	3.913966
185.783460	5216.937231	7.539328	-0.038012	3.916851
186.085165	5224.937797	7.544333	-0.038074	3.919738
186.293046	5232.937028	7.549338	-0.038118	3.922620
186.295216	5240.966584	7.554342	-0.038123	3.925507
186.652709	5248.990166	7.559347	-0.038195	3.928396
186.797402	5257.003572	7.564352	-0.038228	3.931275
186.987150	5265.045037	7.569357	-0.038268	3.934163
187.009790	5273.072105	7.574362	-0.038278	3.937041
187.037544	5281.049009	7.579366	-0.038288	3.939899
187.284515	5289.092391	7.584371	-0.038339	3.942783
187.616565	5297.079940	7.589376	-0.038406	3.945645
187.794335	5305.096763	7.594381	-0.038445	3.948514
187.845294	5313.150202	7.599386	-0.038460	3.951391
187.809191	5321.201541	7.604390	-0.038458	3.954264
188.201086	5329.235278	7.609395	-0.038537	3.957136
188.177131	5337.195271	7.614400	-0.038537	3.959972
188.327340	5345.212198	7.619405	-0.038571	3.962830
188.487445	5353.216076	7.624410	-0.038606	3.965681
188.547170	5361.216542	7.629414	-0.038622	3.968527
188.790178	5369.325665	7.634419	-0.038673	3.971413
188.917887	5377.300269	7.639424	-0.038702	3.974246
189.247993	5385.326505	7.644429	-0.038768	3.977100
189.080175	5393.348631	7.649434	-0.038743	3.979942
189.154898	5401.364171	7.654438	-0.038762	3.982783
189.389214	5409.404481	7.659443	-0.038811	3.985634
189.407999	5417.383884	7.664448	-0.038819	3.988457
189.612166	5425.467253	7.669453	-0.038863	3.991318
189.686533	5433.505930	7.674458	-0.038882	3.994160
189.909170	5441.492253	7.679462	-0.038929	3.996983
189.991872	5449.529673	7.684467	-0.038949	3.999820
190.297568	5457.498019	7.689472	-0.039011	4.002634
190.626295	5465.506524	7.694477	-0.039078	4.005461
190.763248	5473.556991	7.699482	-0.039109	4.008297
190.862868	5481.592710	7.704486	-0.039133	4.011126
191.224780	5489.656170	7.709491	-0.039205	4.013966
191.246018	5497.638446	7.714496	-0.039215	4.016771
191.134763	5505.649099	7.719501	-0.039199	4.019581
191.279175	5513.671830	7.724506	-0.039231	4.022398
191.657243	5521.673939	7.729510	-0.039307	4.025209
191.720160	5529.724137	7.734515	-0.039324	4.028030
191.643577	5537.735242	7.739520	-0.039315	4.030833
191.913101	5545.854723	7.744525	-0.039371	4.033677
192.272441	5553.848420	7.749530	-0.039443	4.036477
192.184617	5561.774079	7.754534	-0.039432	4.039245
192.482052	5569.812108	7.759539	-0.039492	4.042055
192.647163	5577.766605	7.764544	-0.039528	4.044832
192.840041	5585.819535	7.769549	-0.039570	4.047642
193.011365	5593.862923	7.774554	-0.039607	4.050447
193.158577	5601.856459	7.779558	-0.039639	4.053232
193.253379	5609.928677	7.784563	-0.039662	4.056041
193.389504	5617.905098	7.789568	-0.039693	4.058816
193.896997	5625.902212	7.794573	-0.039793	4.061602
194.119936	5633.910478	7.799578	-0.039840	4.064385
194.016618	5641.947635	7.804582	-0.039826	4.067172
194.218980	5649.993090	7.809587	-0.039869	4.069964
194.567000	5657.998571	7.814592	-0.039939	4.072742
194.698518	5666.011219	7.819597	-0.039968	4.075518
194.806564	5674.038461	7.824602	-0.039994	4.078296
194.794903	5682.026345	7.829606	-0.039997	4.081058
195.031414	5690.023299	7.834611	-0.040046	4.083824
195.106983	5698.066546	7.839616	-0.040066	4.086602
195.521523	5706.060273	7.844621	-0.040148	4.089365
195.800364	5714.137388	7.849626	-0.040205	4.092154
195.746918	5722.136145	7.854630	-0.040201	4.094909
195.855322	5730.184770	7.859635	-0.040226	4.097682
196.070867	5738.164858	7.864640	-0.040272	4.100430
196.295158	5746.183667	7.869645	-0.040319	4.103190
196.350551	5754.228085	7.874650	-0.040334	4.105955
196.581181	5762.205787	7.879654	-0.040382	4.108698
196.857610	5770.287298	7.884659	-0.040439	4.111474
196.822423	5778.361569	7.889664	-0.040438	4.114243
197.150601	5786.388435	7.894669	-0.040504	4.116997
197.319472	5794.305479	7.899674	-0.040541	4.119711
197.413428	5802.320038	7.904678	-0.040564	4.122455
197.644224	5810.340402	7.909683	-0.040612	4.125201
197.532646	5818.372409	7.914688	-0.040597	4.127944
197.531339	5826.377340	7.919693	-0.040602	4.130678
197.874461	5834.494916	7.924698	-0.040671	4.133453
198.029563	5842.494880	7.929702	-0.040705	4.136183
198.310892	5850.501155	7.934707	-0.040763	4.138916
198.318316	5858.507982	7.939712	-0.040769	4.141643
198.532094	5866.443020	7.944717	-0.040814	4.144347
198.731691	5874.537157	7.949722	-0.040857	4.147103
198.953229	5882.526671	7.954726	-0.040904	4.149821
199.179162	5890.600428	7.959731	-0.040951	4.152567
199.487766	5898.598558	7.964736	-0.041014	4.155286
199.593667	5906.568578	7.969741	-0.041039	4.157991
199.752648	5914.609254	7.974746	-0.041074	4.160719
200.026590	5922.619082	7.979750	-0.041130	4.163436
200.110316	5930.689625	7.984755	-0.041151	4.166170
200.117823	5938.627804	7.989760	-0.041157	4.168856
200.208351	5946.705002	7.994765	-0.041180	4.171588
200.558524	5954.746505	7.999770	-0.041250	4.174310
200.517130	5962.760199	8.004774	-0.041248	4.177015
200.760642	5970.721535	8.009779	-0.041298	4.179705
200.963084	5978.744090	8.014784	-0.041341	4.182413
200.973871	5986.785613	8.019789	-0.041349	4.185124
201.249230	5994.813564	8.024794	-0.041405	4.187831
201.503316	6002.803911	8.029798	-0.041458	4.190523
201.814497	6010.941577	8.034803	-0.041521	4.193264
201.759931	6018.942161	8.039808	-0.041516	4.195953
201.831286	6026.890881	8.044813	-0.041535	4.198624
202.108333	6034.867051	8.049818	-0.041591	4.201305
202.105875	6042.811585	8.054822	-0.041596	4.203971
202.454571	6050.916019	8.059827	-0.041667	4.206692
202.464589	6058.896533	8.064832	-0.041674	4.209366
202.830019	6066.980318	8.069837	-0.041747	4.212077
202.971684	6074.953123	8.074842	-0.041779	4.214746
202.902803	6082.979461	8.079846	-0.041771	4.217430
203.137374	6090.987722	8.084851	-0.041820	4.220109
203.111574	6098.988408	8.089856	-0.041821	4.222781
203.440011	6107.012614	8.094861	-0.041887	4.225463
203.734767	6115.044928	8.099866	-0.041947	4.228145
203.766772	6123.061152	8.104870	-0.041958	4.230818
203.707434	6131.115129	8.109875	-0.041953	4.233501
203.949951	6139.117608	8.114880	-0.042003	4.236168
204.207349	6147.071310	8.119885	-0.042056	4.238817
204.361948	6155.162643	8.124890	-0.042090	4.241509
204.463709	6163.110329	8.129894	-0.042115	4.244151
204.829736	6171.199432	8.134899	-0.042188	4.246841
204.586619	6179.174453	8.139904	-0.042148	4.249486
204.653623	6187.202213	8.144909	-0.042166	4.252149
205.087304	6195.232444	8.149914	-0.042252	4.254815
205.198729	6203.244687	8.154918	-0.042278	4.257470
205.323811	6211.258782	8.159923	-0.042307	4.260124
205.498574	6219.273757	8.164928	-0.042344	4.262778
205.811853	6227.309920	8.169933	-0.042408	4.265438
205.885973	6235.340599	8.174938	-0.042427	4.268092
205.978989	6243.357846	8.179942	-0.042450	4.270740
206.383328	6251.477921	8.184947	-0.042530	4.273424
206.319719	6259.457344	8.189952	-0.042524	4.276055
206.472575	6267.395322	8.194957	-0.042557	4.278673
206.860261	6275.471560	8.199962	-0.042635	4.281337
207.116275	6283.382749	8.204966	-0.042688	4.283943
207.073442	6291.466845	8.209971	-0.042685	4.286602
207.288430	6299.467795	8.214976	-0.042731	4.289235
207.415935	6307.485438	8.219981	-0.042760	4.291871
207.657769	6315.570862	8.224986	-0.042810	4.294528
207.516611	6323.550890	8.229990	-0.042789	4.297145
208.005278	6331.570880	8.234995	-0.042885	4.299780
207.973800	6339.577103	8.240000	-0.042885	4.302404
207.954155	6347.563138	8.245005	-0.042886	4.305020
208.224176	6355.649224	8.250010	-0.042942	4.307669
208.470461	6363.637876	8.255014	-0.042993	4.310285
208.393912	6371.654307	8.260019	-0.042984	4.312905
208.835549	6379.697996	8.265024	-0.043072	4.315537
209.110540	6387.666456	8.270029	-0.043128	4.318142
209.275515	6395.719855	8.275034	-0.043164	4.320771
209.211955	6403.662755	8.280038	-0.043157	4.323362
209.607642	6411.728499	8.285043	-0.043236	4.325994
209.547483	6419.732745	8.290048	-0.043230	4.328601
209.705870	6427.752342	8.295053	-0.043265	4.331213
210.050597	6435.826538	8.300058	-0.043335	4.333843
210.047475	6443.837429	8.305062	-0.043339	4.336448
210.179509	6451.788751	8.310067	-0.043369	4.339033
210.258508	6459.802730	8.315072	-0.043389	4.341636
210.382458	6467.803295	8.320077	-0.043418	4.344234
210.498359	6475.857971	8.325082	-0.043445	4.346848
210.508379	6483.871570	8.330086	-0.043452	4.349446
210.688553	6491.976133	8.335091	-0.043491	4.352073
210.930143	6500.018850	8.340096	-0.043541	4.354679
210.886977	6507.973766	8.345101	-0.043538	4.357253
211.096035	6515.932233	8.350106	-0.043582	4.359828
211.113815	6523.936935	8.355110	-0.043591	4.362416
211.294957	6531.929692	8.360115	-0.043630	4.364999
211.499458	6539.932617	8.365120	-0.043673	4.367584
211.622170	6547.987423	8.370125	-0.043701	4.370184
211.890340	6556.025935	8.375130	-0.043757	4.372778
211.815094	6564.029238	8.380134	-0.043748	4.375356
212.051343	6572.041177	8.385139	-0.043797	4.377938
212.298375	6580.063572	8.390144	-0.043848	4.380522
212.262960	6588.019231	8.395149	-0.043847	4.383081
212.406684	6596.081230	8.400154	-0.043879	4.385674
212.568153	6604.110818	8.405158	-0.043915	4.388255
212.982685	6612.129104	8.410163	-0.043997	4.390832
212.868381	6620.183814	8.415168	-0.043981	4.393416
213.145319	6628.202451	8.420173	-0.044038	4.395990
213.297799	6636.210477	8.425178	-0.044072	4.398558
213.247461	6644.185704	8.430182	-0.044067	4.401113
213.261224	6652.215210	8.435187	-0.044075	4.403683
213.661203	6660.237253	8.440192	-0.044155	4.406253
213.694302	6668.206598	8.445197	-0.044167	4.408801
214.093843	6676.308588	8.450202	-0.044246	4.411393
214.260299	6684.328262	8.455206	-0.044283	4.413956
214.310672	6692.354477	8.460211	-0.044297	4.416518
214.446653	6700.323380	8.465216	-0.044328	4.419061
214.560073	6708.383462	8.470221	-0.044354	4.421632
214.705514	6716.389011	8.475226	-0.044387	4.424184
214.779342	6724.375794	8.480230	-0.044406	4.426728
214.923989	6732.421115	8.485235	-0.044438	4.429290
215.278651	6740.478934	8.490240	-0.044509	4.431855
215.098717	6748.497106	8.495245	-0.044481	4.434403
215.236696	6756.553701	8.500250	-0.044512	4.436964
215.355816	6764.437286	8.505254	-0.044539	4.439468
215.618813	6772.501505	8.510259	-0.044594	4.442029
215.736571	6780.474976	8.515264	-0.044621	4.444558
215.972373	6788.472167	8.520269	-0.044670	4.447095
216.179893	6796.548317	8.525274	-0.044714	4.449654
216.233079	6804.572017	8.530278	-0.044729	4.452195
216.436781	6812.616188	8.535283	-0.044772	4.454742
216.655276	6820.625373	8.540288	-0.044818	4.457276
216.596620	6828.611983	8.545293	-0.044813	4.459801
216.724916	6836.628524	8.550298	-0.044842	4.462334
216.814208	6844.605636	8.555302	-0.044864	4.464853
217.086735	6852.664324	8.560307	-0.044920	4.467397
217.010515	6860.684198	8.565312	-0.044911	4.469926
217.012465	6868.682941	8.570317	-0.044917	4.472447
217.266538	6876.707200	8.575322	-0.044969	4.474976
217.427675	6884.704389	8.580327	-0.045004	4.477495
217.540450	6892.731479	8.585331	-0.045031	4.480021
217.712917	6900.732737	8.590336	-0.045068	4.482538
217.717552	6908.735331	8.595341	-0.045074	4.485054
218.069075	6916.791603	8.600346	-0.045145	4.487585
218.092205	6924.787200	8.605351	-0.045155	4.490096
218.432634	6932.831971	8.610355	-0.045223	4.492621
218.502290	6940.843167	8.615360	-0.045242	4.495134
218.557919	6948.850043	8.620365	-0.045257	4.497644
219.136115	6956.867608	8.625370	-0.045370	4.500157
219.028683	6964.845157	8.630375	-0.045355	4.502654
219.196168	6972.877589	8.635379	-0.045392	4.505168
219.325682	6980.934878	8.640384	-0.045421	4.507688
219.515841	6988.911299	8.645389	-0.045462	4.510182
219.540154	6997.025535	8.650394	-0.045472	4.512716
219.680859	7005.029390	8.655399	-0.045503	4.515215
220.079498	7013.007711	8.660403	-0.045583	4.517706
220.003757	7021.010222	8.665408	-0.045574	4.520201
220.194180	7028.971079	8.670413	-0.045615	4.522683
220.468900	7037.016986	8.675418	-0.045671	4.525190
220.296234	7045.024465	8.680423	-0.045644	4.527683
220.538835	7053.040493	8.685427	-0.045695	4.530177
220.822756	7061.084870	8.690432	-0.045753	4.532680
220.723438	7069.071970	8.695437	-0.045740	4.535162
220.975437	7077.097417	8.700442	-0.045792	4.537656
221.074671	7085.086061	8.705447	-0.045816	4.540136
221.288373	7093.102606	8.710451	-0.045861	4.542624
221.313016	7101.092482	8.715456	-0.045871	4.545102
221.276901	7109.128374	8.720461	-0.045869	4.547593
221.647001	7117.161491	8.725466	-0.045943	4.550082
221.720314	7125.220834	8.730471	-0.045962	4.552577
221.806245	7133.245216	8.735475	-0.045984	4.555060
222.054825	7141.289416	8.740480	-0.046035	4.557549
222.373971	7149.187267	8.745485	-0.046100	4.559990
222.437340	7157.243215	8.750490	-0.046117	4.562479
222.498058	7165.225728	8.755495	-0.046134	4.564944
222.704115	7173.233272	8.760499	-0.046177	4.567415
222.821256	7181.315433	8.765504	-0.046204	4.569908
222.653881	7189.315935	8.770509	-0.046178	4.572374
223.068808	7197.378574	8.775514	-0.046261	4.574859
223.173319	7205.356474	8.780519	-0.046286	4.577316
223.179690	7213.357259	8.785523	-0.046292	4.579778
223.457461	7221.392078	8.790528	-0.046349	4.582250
223.510923	7229.389256	8.795533	-0.046365	4.584708
223.791772	7237.465434	8.800538	-0.046422	4.587190
223.770370	7245.452178	8.805543	-0.046423	4.589642
224.295121	7253.507249	8.810547	-0.046526	4.592115
224.362719	7261.552404	8.815552	-0.046544	4.594583
224.371258	7269.472653	8.820557	-0.046551	4.597011
224.466679	7277.525390	8.825562	-0.046574	4.599479
224.617201	7285.531450	8.830567	-0.046608	4.601931
224.735056	7293.469443	8.835571	-0.046635	4.604361
224.697825	7301.577165	8.840576	-0.046633	4.606841
224.844502	7309.499181	8.845581	-0.046666	4.609264
224.947788	7317.640033	8.850586	-0.046690	4.611752
225.035746	7325.586987	8.855591	-0.046712	4.614179
225.461530	7333.653760	8.860595	-0.046796	4.616642
225.598141	7341.629773	8.865600	-0.046827	4.619075
225.705829	7349.658171	8.870605	-0.046853	4.621523
225.624175	7357.643636	8.875610	-0.046843	4.623957
225.616049	7365.684597	8.880615	-0.046846	4.626407
225.700728	7373.655041	8.885619	-0.046867	4.628834
225.797029	7381.763129	8.890624	-0.046891	4.631301
226.045887	7389.727941	8.895629	-0.046942	4.633723
226.236208	7397.762682	8.900634	-0.046983	4.636166
226.238579	7405.768521	8.905639	-0.046989	4.638598
226.506314	7413.766746	8.910643	-0.047044	4.641027
226.710365	7421.771194	8.915648	-0.047087	4.643456
226.629397	7429.769990	8.920653	-0.047077	4.645882
227.070444	7437.840186	8.925658	-0.047165	4.648329
226.980749	7445.817524	8.930663	-0.047153	4.650746
227.072189	7453.892314	8.935667	-0.047176	4.653191
227.092285	7461.893799	8.940672	-0.047185	4.655614
227.327598	7469.858891	8.945677	-0.047234	4.658023
227.498536	7477.907501	8.950682	-0.047271	4.660457
227.620534	7485.904414	8.955687	-0.047299	4.662873
227.923875	7493.909338	8.960691	-0.047361	4.665291
228.017695	7501.947680	8.965696	-0.047383	4.667718
228.169611	7509.922195	8.970701	-0.047417	4.670124
228.212339	7518.067107	8.975706	-0.047430	4.672580
228.391212	7526.071927	8.980711	-0.047469	4.674993
228.524131	7534.054823	8.985715	-0.047499	4.677398
228.739614	7542.034007	8.990720	-0.047544	4.679800
228.696944	7550.019139	8.995725	-0.047542	4.682204
229.089478	7558.020079	9.000730	-0.047620	4.684610
228.950120	7565.972435	9.005735	-0.047599	4.687001
229.028580	7574.050625	9.010739	-0.047619	4.689428
229.277394	7582.110152	9.015744	-0.047671	4.691848
229.519766	7590.086521	9.020749	-0.047721	4.694242
229.613818	7598.171233	9.025754	-0.047744	4.696668
229.715416	7606.120676	9.030759	-0.047768	4.699052
230.059952	7614.137329	9.035763	-0.047838	4.701454
230.150062	7622.142888	9.040768	-0.047860	4.703852
230.070579	7630.181601	9.045773	-0.047850	4.706259
230.329305	7638.178906	9.050778	-0.047904	4.708651
230.367284	7646.205856	9.055783	-0.047916	4.711052
230.531454	7654.234772	9.060787	-0.047952	4.713452
230.790435	7662.286375	9.065792	-0.048005	4.715857
230.489764	7670.234103	9.070797	-0.047955	4.718232
230.794394	7678.304824	9.075802	-0.048017	4.720640
230.913429	7686.279811	9.080807	-0.048044	4.723019
231.031684	7694.320654	9.085811	-0.048072	4.725416
231.379770	7702.370835	9.090816	-0.048142	4.727815
231.234895	7710.312760	9.095821	-0.048120	4.730181
231.516371	7718.404190	9.100826	-0.048178	4.732589
231.468992	7726.394932	9.105831	-0.048174	4.734967
231.807400	7734.425982	9.110835	-0.048242	4.737355
231.952335	7742.441444	9.115840	-0.048275	4.739737
231.991054	7750.444163	9.120845	-0.048287	4.742115
232.174096	7758.462924	9.125850	-0.048327	4.744496
232.385896	7766.483990	9.130855	-0.048371	4.746876
232.707631	7774.435614	9.135859	-0.048436	4.749234
232.620448	7782.518505	9.140864	-0.048426	4.751631
232.901931	7790.548430	9.145869	-0.048483	4.754010
233.269010	7798.561321	9.150874	-0.048557	4.756382
233.241182	7806.512653	9.155879	-0.048557	4.758737
233.310111	7814.507039	9.160883	-0.048575	4.761102
233.492769	7822.560629	9.165888	-0.048614	4.763484
233.461082	7830.536519	9.170893	-0.048614	4.765842
233.648546	7838.579281	9.175898	-0.048654	4.768218
233.757734	7846.613528	9.180903	-0.048680	4.770590
233.983868	7854.610988	9.185907	-0.048727	4.772950
234.152476	7862.681618	9.190912	-0.048764	4.775330
233.988259	7870.648230	9.195917	-0.048738	4.777680
234.363573	7878.651277	9.200922	-0.048814	4.780038
234.224516	7886.674840	9.205927	-0.048793	4.782402
234.430669	7894.669912	9.210931	-0.048837	4.784755
234.698253	7902.740946	9.215936	-0.048892	4.787130
234.850006	7910.679654	9.220941	-0.048925	4.789464
234.943008	7918.764851	9.225946	-0.048948	4.791841
235.054893	7926.784243	9.230951	-0.048974	4.794197
235.270156	7934.803825	9.235955	-0.049019	4.796552
235.275072	7942.756250	9.240960	-0.049026	4.798887
235.415654	7950.802920	9.245965	-0.049057	4.801247
235.548226	7958.780022	9.250970	-0.049087	4.803586
235.641169	7966.814791	9.255975	-0.049110	4.805941
235.692234	7974.793208	9.260979	-0.049124	4.808279
236.046010	7982.894402	9.265984	-0.049196	4.810649
236.023826	7990.318433	9.270989	-0.049196	4.812823
236.212941	7994.985159	9.275994	-0.049235	4.814187

236.198858	7997.310351	9.280999	-0.049234	4.814868
236.399027	7998.661603	9.286003	-0.049272	4.815262
236.500923	7999.310089	9.291008	-0.049291	4.815451
236.467272	7999.688484	9.296013	-0.049285	4.815562
236.780831	7999.698898	9.301018	-0.049344	4.815563
236.515117	7999.687134	9.306023	-0.049294	4.815561
236.608842	7999.945908	9.311027	-0.049312	4.815636
236.783262	7999.926319	9.316032	-0.049345	4.815630
236.840366	8000.063884	9.321037	-0.049355	4.815670
236.924331	7999.944625	9.326042	-0.049371	4.815635
236.734140	7999.957565	9.331047	-0.049336	4.815639
236.849419	8000.120622	9.336051	-0.049357	4.815686
236.840288	7999.833334	9.341056	-0.049355	4.815602
236.830796	7999.978359	9.346061	-0.049354	4.815645
236.792590	7999.831506	9.351066	-0.049347	4.815602
237.003103	7999.971552	9.356071	-0.049386	4.815642
236.909390	7999.860093	9.361075	-0.049369	4.815610
237.049548	7999.831410	9.366080	-0.049395	4.815601
237.022013	7999.936648	9.371085	-0.049390	4.815632
237.006764	7999.870224	9.376090	-0.049387	4.815612
236.997197	7999.961876	9.381095	-0.049385	4.815639
237.084115	7999.837328	9.386099	-0.049401	4.815602
237.189214	7999.832630	9.391104	-0.049421	4.815601
237.106135	7999.924160	9.396109	-0.049406	4.815628
237.279035	7999.852241	9.401114	-0.049438	4.815606
237.313332	7999.874151	9.406119	-0.049444	4.815612
237.156467	7999.871618	9.411123	-0.049415	4.815612
237.388685	7999.947969	9.416128	-0.049459	4.815633
237.455256	7999.843373	9.421133	-0.049471	4.815602
237.459554	7999.858392	9.426138	-0.049472	4.815607
237.422191	7999.844984	9.431143	-0.049465	4.815603
237.456799	7999.867966	9.436147	-0.049471	4.815610
237.525784	7999.866953	9.441152	-0.049484	4.815609
237.442244	7999.858134	9.446157	-0.049469	4.815607
237.492405	7999.883503	9.451162	-0.049478	4.815614
237.455791	7999.873309	9.456167	-0.049472	4.815611
237.365241	7999.838758	9.461171	-0.049455	4.815601
237.366709	7999.861204	9.466176	-0.049455	4.815608
237.623242	7999.966771	9.471181	-0.049503	4.815638
237.619302	7999.842886	9.476186	-0.049502	4.815601
237.409471	7999.950512	9.481191	-0.049463	4.815634
237.533346	7999.985614	9.486195	-0.049486	4.815644
237.829360	7999.851640	9.491200	-0.049541	4.815603
237.617056	8000.044624	9.496205	-0.049502	4.815660
237.750548	7999.877062	9.501210	-0.049527	4.815611
237.705117	7999.945718	9.506215	-0.049519	4.815631
237.780580	7999.845535	9.511219	-0.049533	4.815601
237.743629	7999.879101	9.516224	-0.049526	4.815611
237.891912	7999.856955	9.521229	-0.049554	4.815604
237.735724	7999.862972	9.526234	-0.049525	4.815607
237.715520	7999.827424	9.531239	-0.049521	4.815596
237.873991	7999.851344	9.536243	-0.049550	4.815603
237.925188	7999.760375	9.541248	-0.049560	4.815576
237.891777	7999.852710	9.546253	-0.049554	4.815603
237.988396	7999.771017	9.551258	-0.049572	4.815579
237.902709	7999.971388	9.556263	-0.049556	4.815638
237.950205	7999.852605	9.561267	-0.049565	4.815603
237.956228	7999.868720	9.566272	-0.049566	4.815607
238.062591	7999.749823	9.571277	-0.049586	4.815572
237.986757	7999.882035	9.576282	-0.049572	4.815611
237.962156	7999.860293	9.581287	-0.049567	4.815605
238.091754	7999.922175	9.586291	-0.049592	4.815622
238.123120	7999.793523	9.591296	-0.049597	4.815585
237.907604	7999.938420	9.596301	-0.049557	4.815628
238.071238	7999.759603	9.601306	-0.049588	4.815575
238.188688	7999.901349	9.606311	-0.049610	4.815616
238.008320	7999.877085	9.611315	-0.049576	4.815610
237.937904	7999.756394	9.616320	-0.049563	4.815575
237.945144	7999.881411	9.621325	-0.049565	4.815611
238.083181	7999.942363	9.626330	-0.049591	4.815628
237.926038	7999.854426	9.631335	-0.049561	4.815603
237.963300	8000.002347	9.636339	-0.049568	4.815646
238.132621	7999.747830	9.641344	-0.049600	4.815571
238.021103	7999.835699	9.646349	-0.049579	4.815597
238.084647	7999.877297	9.651354	-0.049591	4.815609
238.033528	7999.954401	9.656359	-0.049582	4.815632
238.082989	7999.955208	9.661363	-0.049591	4.815632
238.029649	7999.753664	9.666368	-0.049581	4.815573
238.184860	7999.870402	9.671373	-0.049610	4.815607
238.115657	7999.897041	9.676378	-0.049597	4.815615
238.025339	7999.848616	9.681383	-0.049580	4.815601
238.094299	7999.974633	9.686387	-0.049593	4.815638
238.253415	7999.761583	9.691392	-0.049623	4.815575
238.118514	7999.845870	9.696397	-0.049598	4.815600
238.049341	7999.849026	9.701402	-0.049585	4.815601
238.042052	7999.836104	9.706407	-0.049584	4.815597
238.054921	8000.014588	9.711411	-0.049586	4.815650
238.324756	7999.807599	9.716416	-0.049637	4.815588
238.251045	7999.954792	9.721421	-0.049623	4.815631
238.365013	7999.856299	9.726426	-0.049644	4.815602
238.198586	7999.831193	9.731431	-0.049613	4.815595
238.237052	7999.971662	9.736435	-0.049621	4.815636
238.342895	7999.754546	9.741440	-0.049640	4.815572
238.237220	7999.954596	9.746445	-0.049621	4.815631
238.347345	7999.846433	9.751450	-0.049641	4.815599
238.542693	7999.977701	9.756455	-0.049678	4.815636
238.494474	7999.989735	9.761459	-0.049669	4.815640
238.383370	7999.839560	9.766464	-0.049648	4.815597
238.222837	7999.747298	9.771469	-0.049618	4.815571
238.461825	7999.865394	9.776474	-0.049663	4.815604
238.506087	7999.757232	9.781479	-0.049671	4.815572
238.408053	7999.854927	9.786483	-0.049653	4.815601
238.443166	7999.845893	9.791488	-0.049660	4.815598
238.352178	7999.839088	9.796493	-0.049643	4.815597
238.471993	7999.851708	9.801498	-0.049665	4.815600
238.297471	7999.856361	9.806503	-0.049633	4.815602
238.393802	7999.856858	9.811507	-0.049651	4.815602
238.391550	7999.774631	9.816512	-0.049650	4.815578
238.202373	7999.842028	9.821517	-0.049615	4.815598
238.619048	7999.957664	9.826522	-0.049693	4.815630
238.526514	7999.846219	9.831527	-0.049676	4.815598
238.463617	7999.852679	9.836531	-0.049664	4.815600
238.604216	7999.772764	9.841536	-0.049690	4.815576
238.514209	7999.867386	9.846541	-0.049674	4.815604
238.414864	7999.770777	9.851546	-0.049655	4.815577
238.471672	7999.843224	9.856551	-0.049666	4.815597
238.467168	7999.858101	9.861555	-0.049665	4.815602
238.436777	7999.746596	9.866560	-0.049659	4.815569
238.583639	7999.988098	9.871565	-0.049687	4.815639
238.653088	7999.847251	9.876570	-0.049700	4.815598
238.453600	7999.888861	9.881575	-0.049663	4.815611
238.379457	7999.837494	9.886579	-0.049649	4.815596
238.492685	7999.860682	9.891584	-0.049670	4.815602
238.433332	7999.835174	9.896589	-0.049659	4.815595
238.450571	7999.775680	9.901594	-0.049662	4.815578
238.759912	7999.845811	9.906599	-0.049720	4.815597
238.704628	7999.967684	9.911603	-0.049710	4.815633
238.746143	7999.850936	9.916608	-0.049718	4.815598
238.562128	7999.993142	9.921613	-0.049683	4.815641
238.434124	7999.963319	9.926618	-0.049660	4.815633
238.532000	7999.859228	9.931623	-0.049678	4.815602
238.454725	7999.961529	9.936627	-0.049664	4.815632
238.750107	7999.940698	9.941632	-0.049719	4.815625
238.751617	8000.033601	9.946637	-0.049719	4.815652
238.839355	7999.929344	9.951642	-0.049735	4.815621
238.717589	7999.868665	9.956647	-0.049713	4.815604
238.669741	7999.939418	9.961651	-0.049704	4.815625
238.850650	7999.854818	9.966656	-0.049738	4.815599
238.634834	7999.898299	9.971661	-0.049698	4.815613
238.549869	7999.959911	9.976666	-0.049682	4.815631
238.594176	7999.861357	9.981671	-0.049690	4.815602
238.394258	7999.936052	9.986675	-0.049653	4.815625
238.584085	7999.781143	9.991680	-0.049688	4.815579
238.340808	7999.848731	9.996685	-0.049643	4.815600
238.382458	7999.760810	10.001690	-0.049651	4.815574
238.471668	7999.842321	10.006695	-0.049668	4.815597
238.628421	7999.975099	10.011699	-0.049697	4.815635
238.601786	7999.763309	10.016704	-0.049692	4.815573
238.287060	7999.997337	10.021709	-0.049634	4.815643
238.717771	7999.875150	10.026714	-0.049714	4.815606
238.577002	7999.884619	10.031719	-0.049688	4.815609
238.496018	8000.006075	10.036723	-0.049673	4.815645
238.617243	7999.862864	10.041728	-0.049695	4.815602
238.524358	7999.866703	10.046733	-0.049678	4.815604
238.694512	7999.890813	10.051738	-0.049710	4.815610
238.644623	7999.848379	10.056743	-0.049700	4.815598
238.567026	7999.915447	10.061747	-0.049686	4.815618
238.687233	7999.815987	10.066752	-0.049708	4.815588
238.488043	8000.042279	10.071757	-0.049672	4.815656
238.509103	8000.036221	10.076762	-0.049676	4.815654
238.737144	7999.988679	10.081767	-0.049718	4.815639
238.674983	7999.867051	10.086771	-0.049706	4.815603
238.810381	7999.866046	10.091776	-0.049732	4.815602
238.943814	7999.857537	10.096781	-0.049757	4.815599
238.815866	7999.856538	10.101786	-0.049733	4.815600
238.553720	7999.873649	10.106791	-0.049684	4.815606
238.717651	7999.976654	10.111795	-0.049715	4.815635
238.956461	7999.771297	10.116800	-0.049759	4.815574
238.764130	7999.864263	10.121805	-0.049724	4.815602
238.836566	7999.857969	10.126810	-0.049737	4.815600
238.991353	7999.871156	10.131815	-0.049766	4.815603
238.633840	8000.046847	10.136819	-0.049700	4.815656
238.998679	7999.799763	10.141824	-0.049767	4.815582
238.771525	7999.969025	10.146829	-0.049725	4.815633
238.803149	7999.848915	10.151834	-0.049731	4.815597
238.730740	7999.953430	10.156839	-0.049718	4.815628
238.821363	7999.855626	10.161843	-0.049735	4.815599
239.002808	7999.947173	10.166848	-0.049769	4.815625
238.829180	7999.853628	10.171853	-0.049736	4.815599
238.898206	7999.766149	10.176858	-0.049749	4.815573
238.833902	7999.890011	10.181863	-0.049737	4.815609
238.698223	7999.852592	10.186867	-0.049712	4.815599
238.668041	7999.778452	10.191872	-0.049706	4.815577
238.889863	7999.868516	10.196877	-0.049748	4.815603
238.987710	7999.847689	10.201882	-0.049766	4.815596
238.890020	7999.862125	10.206887	-0.049748	4.815601
238.791847	7999.872283	10.211891	-0.049730	4.815604
238.985641	7999.901047	10.216896	-0.049766	4.815612
238.668836	7999.845749	10.221901	-0.049707	4.815597
238.914059	7999.792081	10.226906	-0.049753	4.815580
238.938678	7999.817037	10.231911	-0.049757	4.815587
238.895411	7999.956185	10.236915	-0.049749	4.815628
238.862026	7999.951380	10.241920	-0.049743	4.815627
238.679768	7999.831009	10.246925	-0.049709	4.815593
238.884274	7999.973102	10.251930	-0.049748	4.815633
238.773533	7999.906196	10.256935	-0.049727	4.815614
238.629636	7999.971123	10.261939	-0.049700	4.815634
238.875180	7999.848073	10.266944	-0.049746	4.815597
238.942608	7999.865183	10.271949	-0.049759	4.815601
238.814175	7999.965589	10.276954	-0.049735	4.815631
238.989956	7999.833935	10.281959	-0.049768	4.815592
238.763029	7999.766216	10.286963	-0.049725	4.815573
238.745577	7999.865216	10.291968	-0.049722	4.815602
238.651266	7999.872235	10.296973	-0.049705	4.815605
238.808550	7999.980470	10.301978	-0.049734	4.815636
238.760932	7999.872954	10.306983	-0.049725	4.815605
238.672820	7999.980418	10.311987	-0.049709	4.815636
238.826622	7999.953024	10.316992	-0.049738	4.815628
238.853989	7999.986566	10.321997	-0.049743	4.815637
238.737781	7999.924909	10.327002	-0.049721	4.815620
239.082413	7999.927293	10.332007	-0.049785	4.815619
238.735654	7999.979328	10.337011	-0.049721	4.815636
238.979054	7999.862647	10.342016	-0.049766	4.815601
238.834068	7999.961718	10.347021	-0.049739	4.815630
238.863009	7999.889601	10.352026	-0.049745	4.815609
238.907137	7999.991735	10.357031	-0.049753	4.815639
238.700128	7999.974510	10.362035	-0.049715	4.815635
238.826378	7999.862337	10.367040	-0.049738	4.815601
239.012697	8000.118361	10.372045	-0.049773	4.815675
238.826969	7999.874100	10.377050	-0.049738	4.815605
238.881389	7999.857907	10.382055	-0.049749	4.815600
238.731758	7999.854422	10.387059	-0.049721	4.815599
238.779748	7999.863745	10.392064	-0.049730	4.815602
238.844328	7999.774058	10.397069	-0.049742	4.815575
238.868809	7999.920708	10.402074	-0.049747	4.815618
238.807510	7999.859941	10.407079	-0.049735	4.815601
238.645496	7999.973680	10.412083	-0.049705	4.815635
239.077946	7999.803483	10.417088	-0.049786	4.815583
238.964853	7999.914813	10.422093	-0.049765	4.815616
238.715865	7999.982309	10.427098	-0.049718	4.815637
238.956473	7999.877325	10.432103	-0.049763	4.815605
238.913612	7999.847814	10.437107	-0.049755	4.815596
238.958362	7999.862422	10.442112	-0.049764	4.815601
238.992329	7999.836290	10.447117	-0.049770	4.815593
239.076887	7999.892108	10.452122	-0.049786	4.815609
239.097203	7999.978911	10.457127	-0.049790	4.815634
239.081523	7999.885789	10.462131	-0.049787	4.815607
239.173318	7999.812555	10.467136	-0.049804	4.815585
239.199026	7999.878095	10.472141	-0.049809	4.815604
238.986859	7999.882137	10.477146	-0.049769	4.815606
239.182008	7999.853278	10.482151	-0.049806	4.815597
239.012902	7999.860152	10.487155	-0.049774	4.815600
238.826011	7999.776001	10.492160	-0.049740	4.815576
238.974717	7999.775212	10.497165	-0.049767	4.815575
238.898830	7999.780394	10.502170	-0.049753	4.815577
238.974761	7999.868096	10.507175	-0.049768	4.815602
238.990365	7999.856612	10.512179	-0.049771	4.815599
238.894991	7999.905246	10.517184	-0.049753	4.815613
239.006565	7999.944421	10.522189	-0.049774	4.815624
239.054185	7999.895025	10.527194	-0.049783	4.815610
238.932585	7999.959246	10.532199	-0.049760	4.815629
239.169264	7999.988706	10.537203	-0.049804	4.815636
239.049526	7999.775405	10.542208	-0.049782	4.815575
239.144698	7999.972306	10.547213	-0.049800	4.815632
239.090460	7999.884965	10.552218	-0.049790	4.815606
239.189294	7999.754200	10.557223	-0.049808	4.815568
238.992195	7999.966650	10.562227	-0.049772	4.815631
239.007185	7999.868687	10.567232	-0.049774	4.815602
239.030587	7999.874410	10.572237	-0.049779	4.815604
238.989497	7999.855602	10.577242	-0.049771	4.815598
239.024156	7999.781444	10.582247	-0.049778	4.815577
239.056287	7999.786239	10.587251	-0.049784	4.815578
238.991908	7999.886615	10.592256	-0.049772	4.815607
239.027672	7999.848770	10.597261	-0.049779	4.815596
239.209745	7999.865602	10.602266	-0.049813	4.815600
239.158235	7999.754820	10.607271	-0.049803	4.815568
238.789555	7999.992245	10.612275	-0.049735	4.815639
239.031809	7999.836049	10.617280	-0.049780	4.815592
239.029412	7999.855230	10.622285	-0.049779	4.815598
239.089276	7999.787885	10.627290	-0.049790	4.815578
239.096786	7999.865940	10.632295	-0.049792	4.815601
239.111080	7999.951578	10.637299	-0.049795	4.815626
239.116073	7999.753108	10.642304	-0.049796	4.815568
239.015790	7999.954315	10.647309	-0.049777	4.815627
238.998288	7999.947632	10.652314	-0.049774	4.815625
239.128398	7999.900640	10.657319	-0.049798	4.815611
239.186736	7999.932548	10.662323	-0.049809	4.815620
239.226234	7999.793349	10.667328	-0.049816	4.815579
239.206465	7999.858153	10.672333	-0.049813	4.815598
239.056561	7999.865338	10.677338	-0.049785	4.815601
239.241553	7999.864070	10.682343	-0.049819	4.815600
239.141063	7999.869920	10.687347	-0.049801	4.815602
238.881319	7999.859314	10.692352	-0.049753	4.815600
238.757769	7999.874399	10.697357	-0.049730	4.815605
239.029558	7999.775258	10.702362	-0.049780	4.815575
239.148580	7999.879671	10.707367	-0.049802	4.815605
238.994136	7999.851555	10.712371	-0.049774	4.815597
239.125380	7999.787501	10.717376	-0.049798	4.815578
239.134240	7999.921089	10.722381	-0.049800	4.815617
239.162257	7999.776367	10.727386	-0.049805	4.815574
239.134898	7999.883747	10.732391	-0.049800	4.815606
239.008451	7999.850747	10.737395	-0.049777	4.815597
239.089445	7999.779474	10.742400	-0.049792	4.815576
238.911698	7999.844921	10.747405	-0.049759	4.815596
238.985938	7999.966757	10.752410	-0.049773	4.815631
239.107384	7999.857709	10.757415	-0.049795	4.815598
239.051784	7999.852544	10.762419	-0.049785	4.815597
239.127168	7999.767302	10.767424	-0.049799	4.815572
239.174459	7999.856677	10.772429	-0.049808	4.815598
239.023642	7999.855307	10.777434	-0.049780	4.815598
239.048593	7999.770316	10.782439	-0.049785	4.815573
239.069321	7999.948931	10.787443	-0.049789	4.815625
239.233453	7999.867262	10.792448	-0.049819	4.815601
239.046163	7999.927217	10.797453	-0.049785	4.815619
239.072182	8000.016247	10.802458	-0.049790	4.815645
239.248083	7999.962524	10.807463	-0.049822	4.815628
239.026755	7999.844721	10.812467	-0.049781	4.815595
239.020188	7999.782705	10.817472	-0.049780	4.815577
239.216539	7999.874493	10.822477	-0.049817	4.815603
239.269619	7999.956490	10.827482	-0.049827	4.815626
239.122098	7999.859097	10.832487	-0.049799	4.815599
239.204717	7999.870048	10.837491	-0.049815	4.815601
239.403238	7999.858324	10.842496	-0.049852	4.815597
239.337867	7999.853001	10.847501	-0.049839	4.815596
239.073393	7999.861533	10.852506	-0.049790	4.815600
239.274470	7999.867997	10.857511	-0.049828	4.815601
239.271556	7999.855146	10.862515	-0.049827	4.815597
239.388335	7999.762034	10.867520	-0.049849	4.815569
239.487425	7999.857586	10.872525	-0.049868	4.815596
239.297687	7999.860923	10.877530	-0.049832	4.815598
239.267307	7999.776103	10.882535	-0.049827	4.815574
239.080311	7999.766675	10.887539	-0.049792	4.815572
239.341249	7999.878725	10.892544	-0.049841	4.815603
239.276825	7999.879822	10.897549	-0.049829	4.815604
239.222647	7999.775402	10.902554	-0.049819	4.815574
239.414009	7999.795587	10.907559	-0.049854	4.815579
239.205148	7999.955539	10.912563	-0.049816	4.815626
239.163267	7999.848115	10.917568	-0.049808	4.815595
239.279037	7999.863873	10.922573	-0.049829	4.815599
239.403170	7999.855214	10.927578	-0.049853	4.815596
239.366638	7999.776699	10.932583	-0.049846	4.815573
239.374162	7999.895321	10.937587	-0.049847	4.815608
239.351136	7999.790337	10.942592	-0.049843	4.815577
239.107260	7999.864321	10.947597	-0.049798	4.815600
239.202524	7999.862666	10.952602	-0.049816	4.815599
239.355811	7999.773349	10.957607	-0.049844	4.815572
239.429505	7999.931473	10.962611	-0.049858	4.815618
239.236731	7999.844022	10.967616	-0.049822	4.815594
239.318377	7999.885915	10.972621	-0.049837	4.815606
239.340316	7999.935382	10.977626	-0.049842	4.815620
239.376117	7999.856971	10.982631	-0.049848	4.815597
239.320626	7999.858213	10.987635	-0.049838	4.815597
239.538634	7999.877762	10.992640	-0.049879	4.815602
239.374183	7999.849484	10.997645	-0.049848	4.815595
239.093931	7999.867368	11.002650	-0.049796	4.815601
239.276035	7999.972804	11.007655	-0.049830	4.815631
239.280800	7999.996372	11.012659	-0.049831	4.815638
239.165808	7999.879223	11.017664	-0.049810	4.815604
239.376881	7999.859162	11.022669	-0.049849	4.815597
239.327547	7999.867976	11.027674	-0.049840	4.815600
239.333479	7999.767732	11.032679	-0.049841	4.815571
239.318224	7999.964981	11.037683	-0.049838	4.815629
239.331693	7999.777322	11.042688	-0.049841	4.815574
239.336894	7999.961024	11.047693	-0.049842	4.815627
239.265116	7999.952394	11.052698	-0.049829	4.815625
239.311931	7999.841069	11.057703	-0.049837	4.815592
239.402825	7999.950366	11.062707	-0.049854	4.815624
239.378871	7999.856042	11.067712	-0.049850	4.815596
239.392337	7999.878683	11.072717	-0.049852	4.815603
239.617643	7999.938917	11.077722	-0.049895	4.815620
239.686542	7999.857839	11.082727	-0.049907	4.815596
239.183504	7999.859304	11.087731	-0.049814	4.815598
239.348224	7999.864113	11.092736	-0.049845	4.815599
239.322916	7999.879721	11.097741	-0.049840	4.815604
239.304015	7999.995780	11.102746	-0.049836	4.815638
239.447563	7999.851861	11.107751	-0.049863	4.815595
239.375475	7999.872049	11.112755	-0.049850	4.815601
239.351816	7999.857793	11.117760	-0.049845	4.815597
239.474969	7999.844848	11.122765	-0.049868	4.815593
239.521478	7999.992925	11.127770	-0.049877	4.815636
239.520068	7999.849860	11.132775	-0.049877	4.815594
239.356000	7999.966770	11.137779	-0.049847	4.815629
239.497935	7999.909294	11.142784	-0.049873	4.815611
239.643438	7999.985316	11.147789	-0.049900	4.815633
239.508863	7999.976736	11.152794	-0.049875	4.815631
239.372527	7999.842160	11.157799	-0.049850	4.815592
239.338504	8000.034835	11.162803	-0.049844	4.815649
239.455690	7999.840315	11.167808	-0.049865	4.815592
239.249631	7999.880751	11.172813	-0.049827	4.815604
239.299666	8000.032088	11.177818	-0.049837	4.815648
239.474968	7999.872670	11.182823	-0.049869	4.815601
239.416360	7999.858916	11.187827	-0.049858	4.815597
239.490577	7999.852651	11.192832	-0.049872	4.815595
239.499998	7999.870957	11.197837	-0.049874	4.815600
239.314290	7999.853009	11.202842	-0.049840	4.815596
239.576260	7999.775059	11.207847	-0.049888	4.815572
239.621320	7999.857993	11.212851	-0.049897	4.815596
239.590368	7999.854295	11.217856	-0.049891	4.815595
239.413417	7999.841826	11.222861	-0.049858	4.815592
239.406103	7999.955938	11.227866	-0.049857	4.815626
239.473302	7999.761676	11.232871	-0.049870	4.815568
239.434097	8000.147490	11.237875	-0.049863	4.815681
239.400905	7999.915304	11.242880	-0.049856	4.815614
239.476055	7999.994456	11.247885	-0.049870	4.815636
239.565458	7999.871010	11.252890	-0.049887	4.815600
239.361169	7999.877314	11.257895	-0.049849	4.815603
239.324675	7999.945049	11.262899	-0.049842	4.815623
239.381164	7999.869109	11.267904	-0.049853	4.815600
239.514439	7999.770926	11.272909	-0.049878	4.815571
239.660597	7999.869376	11.277914	-0.049905	4.815599
239.902889	7999.792175	11.282919	-0.049950	4.815575
239.560793	7999.762086	11.287923	-0.049886	4.815568
239.385228	7999.885215	11.292928	-0.049854	4.815605
239.541905	7999.792749	11.297933	-0.049883	4.815577
239.385462	7999.774208	11.302938	-0.049854	4.815572
239.614424	7999.800340	11.307943	-0.049897	4.815579
239.681943	7999.784359	11.312947	-0.049909	4.815574
239.571918	7999.887199	11.317952	-0.049889	4.815605
239.421062	7999.799359	11.322957	-0.049861	4.815580
239.355950	7999.772690	11.327962	-0.049849	4.815572
239.513279	7999.890535	11.332967	-0.049878	4.815606
239.377580	7999.761309	11.337971	-0.049853	4.815569
239.511583	7999.874506	11.342976	-0.049878	4.815601
239.674371	7999.862203	11.347981	-0.049908	4.815597
239.584682	7999.783895	11.352986	-0.049892	4.815574
239.421709	7999.789801	11.357991	-0.049861	4.815577
239.675117	7999.882515	11.362995	-0.049909	4.815603
239.617372	7999.794048	11.368000	-0.049898	4.815577
239.654716	7999.783984	11.373005	-0.049905	4.815574
239.602986	7999.773543	11.378010	-0.049895	4.815571
239.653207	7999.886452	11.383015	-0.049905	4.815604
239.698910	7999.755893	11.388019	-0.049913	4.815566
239.572943	7999.900108	11.393024	-0.049890	4.815608
239.462038	7999.790498	11.398029	-0.049870	4.815577
239.432807	7999.796435	11.403034	-0.049864	4.815579
239.643128	7999.789172	11.408039	-0.049903	4.815576
239.516394	7999.868256	11.413043	-0.049880	4.815599
239.480243	7999.778004	11.418048	-0.049873	4.815573
239.636206	7999.874478	11.423053	-0.049902	4.815601
239.494018	7999.855100	11.428058	-0.049876	4.815596
239.724114	7999.774498	11.433063	-0.049919	4.815571
239.834906	7999.857430	11.438067	-0.049939	4.815595
239.743892	7999.828206	11.443072	-0.049923	4.815587
239.848729	7999.838450	11.448077	-0.049942	4.815589
239.864797	7999.866471	11.453082	-0.049945	4.815597
239.824062	7999.776145	11.458087	-0.049938	4.815571
239.741978	7999.867695	11.463091	-0.049923	4.815598
239.931200	7999.908130	11.468096	-0.049958	4.815609
239.794592	7999.851478	11.473101	-0.049932	4.815593
239.582608	7999.780796	11.478106	-0.049893	4.815573
239.796454	7999.799211	11.483111	-0.049933	4.815578
239.639709	7999.859661	11.488115	-0.049904	4.815596
239.480554	7999.905126	11.493120	-0.049874	4.815610
239.620323	7999.852952	11.498125	-0.049900	4.815594
239.592997	7999.853583	11.503130	-0.049895	4.815595
239.507410	7999.860742	11.508135	-0.049879	4.815597
239.578341	7999.865099	11.513139	-0.049893	4.815598
239.654156	7999.888751	11.518144	-0.049907	4.815605
239.684916	7999.783570	11.523149	-0.049913	4.815574
239.639309	7999.865036	11.528154	-0.049904	4.815598
239.734382	7999.783315	11.533159	-0.049922	4.815573
239.868830	7999.769485	11.538163	-0.049947	4.815569
239.793187	7999.877153	11.543168	-0.049933	4.815601
239.762601	7999.768843	11.548173	-0.049927	4.815569
239.757483	7999.854167	11.553178	-0.049927	4.815594
239.536559	7999.867674	11.558183	-0.049885	4.815599
239.719190	7999.762819	11.563187	-0.049919	4.815567
239.856613	7999.879276	11.568192	-0.049945	4.815601
239.740873	7999.871001	11.573197	-0.049924	4.815599
239.503909	7999.856492	11.578202	-0.049880	4.815596
239.449230	7999.872692	11.583207	-0.049870	4.815601
239.721301	7999.842944	11.588211	-0.049920	4.815591
239.545709	7999.891346	11.593216	-0.049888	4.815606
239.696102	7999.775293	11.598221	-0.049916	4.815571
239.641023	7999.905712	11.603226	-0.049906	4.815610
239.569799	7999.896023	11.608231	-0.049892	4.815607
239.512829	7999.750991	11.613235	-0.049882	4.815565
239.581259	8000.043539	11.618240	-0.049895	4.815650
239.494510	7999.918306	11.623245	-0.049878	4.815614
239.423631	8000.012172	11.628250	-0.049865	4.815642
239.743364	7999.830541	11.633255	-0.049925	4.815587
239.769945	7999.938797	11.638259	-0.049930	4.815619
239.684716	7999.843480	11.643264	-0.049914	4.815591
239.534216	7999.788739	11.648269	-0.049886	4.815576
239.650008	7999.865346	11.653274	-0.049908	4.815598
239.673617	7999.804886	11.658279	-0.049912	4.815580
239.614698	7999.864785	11.663283	-0.049901	4.815598
239.701209	7999.871530	11.668288	-0.049918	4.815599
239.953695	7999.756063	11.673293	-0.049965	4.815564
239.693244	7999.887425	11.678298	-0.049916	4.815604
239.811445	7999.792201	11.683303	-0.049938	4.815576
239.845736	7999.958228	11.688307	-0.049945	4.815624
239.609067	7999.881807	11.693312	-0.049901	4.815603
239.534886	7999.781332	11.698317	-0.049887	4.815574
239.709292	7999.848214	11.703322	-0.049919	4.815592
239.815450	7999.780550	11.708327	-0.049939	4.815572
239.579519	7999.874946	11.713331	-0.049895	4.815601
239.638239	7999.880173	11.718336	-0.049906	4.815602
239.797775	7999.771740	11.723341	-0.049936	4.815570
239.613333	7999.953439	11.728346	-0.049902	4.815624
239.628779	7999.874698	11.733351	-0.049905	4.815601
239.829051	7999.864070	11.738355	-0.049942	4.815596
239.724879	7999.836768	11.743360	-0.049923	4.815589
239.647843	7999.848335	11.748365	-0.049909	4.815593
239.603925	7999.978935	11.753370	-0.049901	4.815631
239.855505	7999.890142	11.758375	-0.049947	4.815604
239.708138	7999.861071	11.763379	-0.049920	4.815596
239.833642	7999.977336	11.768384	-0.049943	4.815630
240.019584	7999.899222	11.773389	-0.049978	4.815606
239.794760	7999.844343	11.778394	-0.049936	4.815591
239.758782	7999.772242	11.783399	-0.049930	4.815570
239.812813	7999.904428	11.788403	-0.049940	4.815608
239.762483	7999.875863	11.793408	-0.049930	4.815600
239.881713	7999.785992	11.798413	-0.049953	4.815573
239.779204	7999.942331	11.803418	-0.049934	4.815620
239.895096	7999.840664	11.808423	-0.049955	4.815589
239.658745	7999.852853	11.813427	-0.049911	4.815594
239.682294	7999.854308	11.818432	-0.049916	4.815594
239.960915	7999.974121	11.823437	-0.049968	4.815628
239.601215	7999.996054	11.828442	-0.049901	4.815636
239.734434	7999.779375	11.833447	-0.049926	4.815572
239.794075	7999.873221	11.838451	-0.049937	4.815599
239.738134	7999.860578	11.843456	-0.049927	4.815596
239.802303	7999.761276	11.848461	-0.049939	4.815567
239.926467	7999.960786	11.853466	-0.049962	4.815624
240.103585	7999.859043	11.858471	-0.049995	4.815594
239.994364	7999.851941	11.863475	-0.049975	4.815592
239.919053	7999.857131	11.868480	-0.049961	4.815594
240.028314	7999.771369	11.873485	-0.049981	4.815568
239.760061	7999.931428	11.878490	-0.049931	4.815616
239.811860	7999.825520	11.883495	-0.049941	4.815585
239.935470	7999.869162	11.888499	-0.049964	4.815597
239.863576	7999.871205	11.893504	-0.049951	4.815598
239.793710	7999.795352	11.898509	-0.049938	4.815577
239.872209	7999.860681	11.903514	-0.049952	4.815595
239.992921	7999.826346	11.908519	-0.049975	4.815585
239.949025	7999.838451	11.913523	-0.049967	4.815588
239.897142	7999.946504	11.918528	-0.049957	4.815620
239.927988	7999.869079	11.923533	-0.049963	4.815597
239.736678	7999.947117	11.928538	-0.049927	4.815621
239.755200	7999.872696	11.933543	-0.049931	4.815599
239.951787	7999.882292	11.938547	-0.049968	4.815601
240.044098	7999.781310	11.943552	-0.049985	4.815571
240.041323	7999.885888	11.948557	-0.049984	4.815602
239.982134	7999.873192	11.953562	-0.049973	4.815598
239.791502	7999.937363	11.958567	-0.049938	4.815618
239.908438	7999.859199	11.963571	-0.049960	4.815595
239.773639	7999.937085	11.968576	-0.049935	4.815618
239.669126	7999.932194	11.973581	-0.049915	4.815617
239.757572	7999.969929	11.978586	-0.049932	4.815628
239.894717	7999.829107	11.983591	-0.049957	4.815586
239.850629	7999.910598	11.988595	-0.049949	4.815610
239.782250	7999.956467	11.993600	-0.049937	4.815624
239.942236	8000.003902	11.998605	-0.049967	4.815637
239.787447	7999.879700	12.003610	-0.049938	4.815601
239.779727	7999.847555	12.008615	-0.049936	4.815592
239.865820	7999.973857	12.013619	-0.049953	4.815628
239.714467	7999.871062	12.018624	-0.049924	4.815599
239.794754	7999.852085	12.023629	-0.049939	4.815593
239.667282	7999.939698	12.028634	-0.049916	4.815619
239.823244	7999.849355	12.033639	-0.049945	4.815592
239.843990	7999.858237	12.038643	-0.049949	4.815595
239.782548	7999.860449	12.043648	-0.049937	4.815596
239.736697	7999.779648	12.048653	-0.049929	4.815572
239.830635	8000.029910	12.053658	-0.049947	4.815645
239.987453	7999.784789	12.058663	-0.049976	4.815572
239.728357	7999.925780	12.063667	-0.049928	4.815615
239.649580	7999.835905	12.068672	-0.049913	4.815589
239.857439	7999.873439	12.073677	-0.049952	4.815599
239.914199	8000.079331	12.078682	-0.049962	4.815659
239.838535	7999.863536	12.083687	-0.049948	4.815596
239.906256	7999.857166	12.088691	-0.049961	4.815594
239.925265	7999.950354	12.093696	-0.049965	4.815621
239.989172	7999.858520	12.098701	-0.049977	4.815594
239.898794	7999.886952	12.103706	-0.049960	4.815603
239.875147	7999.869494	12.108711	-0.049955	4.815598
239.894306	7999.792948	12.113715	-0.049959	4.815575
239.777201	7999.950118	12.118720	-0.049937	4.815622
239.633531	7999.867731	12.123725	-0.049911	4.815598
239.842837	7999.850844	12.128730	-0.049950	4.815592
239.836362	7999.972444	12.133735	-0.049949	4.815628
239.770818	7999.851824	12.138739	-0.049936	4.815593
239.811668	7999.910137	12.143744	-0.049944	4.815610
239.860156	7999.874633	12.148749	-0.049953	4.815599
239.715068	7999.868017	12.153754	-0.049926	4.815598
239.823774	7999.760896	12.158759	-0.049946	4.815566
239.914025	7999.941709	12.163763	-0.049963	4.815619
239.754039	8000.029863	12.168768	-0.049934	4.815645
239.774324	7999.998171	12.173773	-0.049938	4.815636
239.782517	7999.850990	12.178778	-0.049939	4.815593
239.618507	7999.823785	12.183783	-0.049909	4.815586
239.754026	7999.908185	12.188787	-0.049934	4.815610
239.782922	7999.863823	12.193792	-0.049939	4.815596
240.198548	7999.889778	12.198797	-0.050017	4.815602
239.892993	7999.876293	12.203802	-0.049960	4.815600
239.858299	7999.863993	12.208807	-0.049954	4.815596
239.915750	7999.887348	12.213811	-0.049964	4.815603
239.728040	7999.917405	12.218816	-0.049929	4.815612
239.876730	7999.823742	12.223821	-0.049957	4.815584
239.946860	7999.772575	12.228826	-0.049970	4.815569
239.890203	7999.897631	12.233831	-0.049960	4.815606
239.694656	7999.951047	12.238835	-0.049924	4.815622
239.790085	7999.857589	12.243840	-0.049941	4.815595
239.871443	7999.906951	12.248845	-0.049957	4.815609
239.711449	7999.870204	12.253850	-0.049927	4.815599
239.770082	7999.787892	12.258855	-0.049938	4.815574
239.957350	7999.892347	12.263859	-0.049973	4.815604
239.839997	7999.850952	12.268864	-0.049951	4.815592
239.910221	7999.870243	12.273869	-0.049964	4.815598
240.014550	7999.965883	12.278874	-0.049984	4.815625
240.105974	7999.804036	12.283879	-0.050001	4.815577
240.073799	7999.962584	12.288883	-0.049995	4.815624
240.080533	7999.887970	12.293888	-0.049996	4.815602
239.993448	7999.769136	12.298893	-0.049980	4.815568
239.743154	7999.947634	12.303898	-0.049933	4.815621
239.829533	7999.782505	12.308903	-0.049949	4.815572
239.993494	7999.884447	12.313907	-0.049980	4.815601
239.799616	7999.820462	12.318912	-0.049944	4.815584
239.895079	7999.799596	12.323917	-0.049962	4.815577
240.075831	7999.849501	12.328922	-0.049996	4.815591
239.904884	7999.873425	12.333927	-0.049964	4.815599
239.918399	7999.874717	12.338931	-0.049966	4.815599
239.940713	7999.869747	12.343936	-0.049971	4.815597
239.966543	7999.773026	12.348941	-0.049975	4.815569
239.720865	7999.965476	12.353946	-0.049930	4.815626
239.920620	7999.877978	12.358951	-0.049967	4.815600
240.101384	7999.857427	12.363955	-0.050001	4.815593
239.944649	7999.810056	12.368960	-0.049972	4.815580
240.135042	7999.837700	12.373965	-0.050007	4.815587
240.084903	7999.866784	12.378970	-0.049998	4.815596
239.967763	7999.794434	12.383975	-0.049976	4.815575
239.889125	7999.866825	12.388979	-0.049962	4.815597
239.766960	7999.860581	12.393984	-0.049939	4.815596
239.987482	7999.775555	12.398989	-0.049980	4.815570
239.822665	7999.866833	12.403994	-0.049949	4.815597
240.032563	7999.853158	12.408999	-0.049989	4.815592
240.072107	7999.865548	12.414003	-0.049996	4.815596
240.033266	7999.915098	12.419008	-0.049989	4.815610
239.877676	7999.854936	12.424013	-0.049960	4.815593
239.956519	7999.859421	12.429018	-0.049975	4.815594
240.073590	7999.795136	12.434023	-0.049996	4.815575
240.011898	7999.786670	12.439027	-0.049985	4.815573
240.016922	7999.863619	12.444032	-0.049986	4.815595
240.105229	7999.783923	12.449037	-0.050003	4.815572
239.973975	8000.024132	12.454042	-0.049978	4.815642
239.912656	7999.819245	12.459047	-0.049967	4.815583
239.820055	7999.809210	12.464051	-0.049950	4.815580
240.017548	7999.986423	12.469056	-0.049987	4.815631
240.100514	7999.875682	12.474061	-0.050002	4.815598
240.023564	7999.847752	12.479066	-0.049988	4.815591
240.057566	7999.961467	12.484071	-0.049994	4.815624
239.984459	7999.898371	12.489075	-0.049981	4.815606
239.958364	7999.771985	12.494080	-0.049976	4.815569
239.962295	7999.794472	12.499085	-0.049977	4.815575
239.998441	7999.879398	12.504090	-0.049983	4.815600
239.856796	7999.787436	12.509095	-0.049957	4.815574
239.999712	7999.771609	12.514099	-0.049984	4.815568
239.925754	7999.951897	12.519104	-0.049970	4.815621
239.844080	7999.776572	12.524109	-0.049955	4.815571
239.908837	7999.875839	12.529114	-0.049967	4.815599
240.156414	7999.950314	12.534119	-0.050013	4.815620
240.105173	7999.762670	12.539123	-0.050004	4.815565
240.011896	7999.953320	12.544128	-0.049986	4.815621
240.071544	7999.865687	12.549133	-0.049998	4.815596
239.928784	7999.964795	12.554138	-0.049971	4.815625
240.044265	7999.846040	12.559143	-0.049993	4.815590
240.192749	7999.788670	12.564147	-0.050020	4.815572
240.040709	8000.001854	12.569152	-0.049992	4.815636
240.158716	7999.857519	12.574157	-0.050014	4.815593
239.964187	7999.867183	12.579162	-0.049978	4.815596
240.047450	7999.903766	12.584167	-0.049994	4.815607
239.855027	7999.768280	12.589171	-0.049958	4.815568
239.780458	7999.868493	12.594176	-0.049944	4.815598
239.996066	7999.772711	12.599181	-0.049984	4.815569
240.057384	7999.866585	12.604186	-0.049996	4.815596
239.898307	7999.956889	12.609191	-0.049966	4.815623
239.970840	7999.863059	12.614195	-0.049980	4.815595
240.009601	7999.851950	12.619200	-0.049987	4.815592
239.889150	7999.857476	12.624205	-0.049965	4.815594
239.910468	7999.852489	12.629210	-0.049969	4.815592
240.218440	7999.924740	12.634215	-0.050026	4.815612
240.137583	7999.927705	12.639219	-0.050011	4.815613
240.055761	8000.004316	12.644224	-0.049996	4.815636
240.132762	7999.868924	12.649229	-0.050010	4.815596
240.161966	8000.020994	12.654234	-0.050016	4.815641
240.025930	7999.898162	12.659239	-0.049990	4.815605
240.143387	7999.925692	12.664243	-0.050012	4.815613
240.103191	7999.883412	12.669248	-0.050005	4.815601
240.019389	7999.837223	12.674253	-0.049989	4.815587
239.899446	7999.861974	12.679258	-0.049967	4.815595
240.112911	7999.877181	12.684263	-0.050007	4.815599
240.293356	7999.760546	12.689267	-0.050041	4.815564
240.058395	7999.959576	12.694272	-0.049997	4.815623
239.961314	7999.874741	12.699277	-0.049979	4.815599
240.019414	7999.967496	12.704282	-0.049990	4.815626
240.143390	7999.958835	12.709287	-0.050013	4.815622
240.089642	7999.783961	12.714291	-0.050003	4.815572
240.154864	8000.087138	12.719296	-0.050015	4.815660
240.076351	7999.764541	12.724301	-0.050001	4.815566
239.996649	7999.991708	12.729306	-0.049986	4.815633
240.022993	8000.010289	12.734311	-0.049991	4.815638
240.202884	7999.887239	12.739315	-0.050024	4.815601
240.142191	7999.847830	12.744320	-0.050013	4.815590
240.208530	7999.779521	12.749325	-0.050026	4.815570
240.018976	8000.007043	12.754330	-0.049990	4.815637
240.075097	7999.774167	12.759335	-0.050001	4.815569
240.040523	7999.869691	12.764339	-0.049995	4.815597
240.155836	7999.970846	12.769344	-0.050016	4.815626
240.052674	7999.976652	12.774349	-0.049997	4.815628
239.880124	7999.867108	12.779354	-0.049965	4.815597
240.055974	7999.903056	12.784359	-0.049998	4.815606
240.036990	7999.855783	12.789363	-0.049994	4.815593
239.876671	8000.001578	12.794368	-0.049964	4.815636
240.070543	7999.851000	12.799373	-0.050001	4.815591
240.000245	7999.988646	12.804378	-0.049988	4.815632
240.130896	7999.854124	12.809383	-0.050012	4.815592
239.980745	7999.857034	12.814387	-0.049984	4.815593
240.107996	7999.945572	12.819392	-0.050008	4.815619
240.241084	7999.781198	12.824397	-0.050033	4.815570
240.180228	7999.960632	12.829402	-0.050021	4.815623
239.918979	7999.856055	12.834407	-0.049973	4.815593
240.064560	7999.887243	12.839411	-0.050000	4.815602
239.970347	7999.956179	12.844416	-0.049983	4.815622
239.978698	7999.980874	12.849421	-0.049984	4.815630
239.915482	7999.913667	12.854426	-0.049972	4.815610
240.023639	7999.888737	12.859431	-0.049993	4.815602
240.032794	7999.848324	12.864435	-0.049994	4.815591
240.218019	7999.915384	12.869440	-0.050029	4.815609
240.311240	7999.876333	12.874445	-0.050046	4.815597
240.185437	7999.876435	12.879450	-0.050023	4.815598
239.967596	7999.877181	12.884455	-0.049982	4.815599
240.249289	7999.905237	12.889459	-0.050035	4.815606
239.987644	8000.018432	12.894464	-0.049986	4.815641
240.225655	7999.892054	12.899469	-0.050031	4.815602
240.243212	7999.980951	12.904474	-0.050034	4.815628
240.197766	7999.889478	12.909479	-0.050026	4.815602
240.093581	7999.768232	12.914483	-0.050006	4.815567
240.074838	7999.861877	12.919488	-0.050003	4.815594
240.045529	7999.860340	12.924493	-0.049997	4.815594
240.208864	7999.871532	12.929498	-0.050028	4.815596
240.186444	7999.855161	12.934503	-0.050024	4.815592
240.438591	7999.904090	12.939507	-0.050071	4.815605
240.318349	7999.976875	12.944512	-0.050049	4.815627
240.171774	7999.781280	12.949517	-0.050021	4.815570
240.251288	7999.856234	12.954522	-0.050036	4.815592
240.296109	7999.947707	12.959527	-0.050045	4.815618
240.252828	7999.783677	12.964531	-0.050037	4.815571
240.219037	7999.955009	12.969536	-0.050030	4.815621
240.236926	7999.791971	12.974541	-0.050034	4.815573
240.034250	7999.861285	12.979546	-0.049996	4.815594
240.071582	7999.869368	12.984551	-0.050003	4.815596
240.238084	7999.874207	12.989555	-0.050034	4.815597
240.207367	7999.877985	12.994560	-0.050028	4.815598
240.008531	7999.875836	12.999565	-0.049992	4.815599
240.037431	7999.770624	13.004570	-0.049997	4.815568
240.267867	7999.787173	13.009575	-0.050040	4.815572
240.282008	7999.797016	13.014579	-0.050043	4.815574
240.131067	7999.875708	13.019584	-0.050015	4.815598
240.091642	7999.882547	13.024589	-0.050007	4.815600
240.184553	7999.864843	13.029594	-0.050025	4.815595
240.054479	7999.767730	13.034599	-0.050000	4.815567
240.241025	7999.868972	13.039603	-0.050035	4.815596
240.176829	7999.775061	13.044608	-0.050023	4.815568
240.220272	7999.885727	13.049613	-0.050032	4.815601
240.161323	7999.782294	13.054618	-0.050021	4.815571
240.145786	7999.775642	13.059623	-0.050018	4.815569
240.102807	7999.899853	13.064627	-0.050010	4.815605
239.962460	7999.781223	13.069632	-0.049984	4.815571
240.330254	7999.805336	13.074637	-0.050052	4.815577
240.148464	7999.790653	13.079642	-0.050019	4.815573
240.235930	7999.891357	13.084647	-0.050035	4.815602
240.234546	7999.785654	13.089651	-0.050035	4.815571
240.101311	7999.858228	13.094656	-0.050010	4.815593
240.082596	7999.793878	13.099661	-0.050007	4.815574
240.052595	7999.892678	13.104666	-0.050001	4.815603
240.019274	7999.892144	13.109671	-0.049995	4.815603
240.141899	7999.768167	13.114675	-0.050018	4.815567
239.967094	7999.973509	13.119680	-0.049985	4.815627
240.254672	7999.802031	13.124685	-0.050039	4.815576
240.144878	7999.771434	13.129690	-0.050018	4.815567
239.944138	7999.864265	13.134695	-0.049981	4.815596
240.105482	7999.897844	13.139699	-0.050011	4.815605
240.119135	7999.762493	13.144704	-0.050014	4.815565
240.301636	7999.896763	13.149709	-0.050048	4.815603
240.255975	7999.761519	13.154714	-0.050039	4.815564
240.038678	7999.876500	13.159719	-0.049999	4.815599
240.040409	7999.869061	13.164723	-0.050000	4.815596
240.021703	7999.966977	13.169728	-0.049996	4.815625
240.048851	7999.838250	13.174733	-0.050001	4.815587
240.424386	8000.105891	13.179738	-0.050071	4.815664
240.047368	7999.903357	13.184743	-0.050001	4.815606
240.269395	7999.845043	13.189747	-0.050042	4.815588
240.304512	7999.857360	13.194752	-0.050049	4.815592
240.354575	7999.768504	13.199757	-0.050058	4.815566
240.236261	7999.881886	13.204762	-0.050037	4.815599
240.389076	7999.874760	13.209767	-0.050065	4.815596
240.408863	7999.790751	13.214771	-0.050069	4.815572
240.204100	7999.955042	13.219776	-0.050031	4.815621
240.324460	7999.871594	13.224781	-0.050053	4.815596
240.254280	7999.870463	13.229786	-0.050040	4.815596
240.127638	7999.780878	13.234791	-0.050017	4.815570
240.291603	7999.881754	13.239795	-0.050047	4.815599
240.228926	7999.855123	13.244800	-0.050036	4.815592
240.174894	7999.798741	13.249805	-0.050026	4.815575
240.085217	7999.859210	13.254810	-0.050009	4.815593
240.281402	7999.796207	13.259815	-0.050046	4.815574
240.453559	7999.876933	13.264819	-0.050078	4.815597
240.180144	7999.857562	13.269824	-0.050027	4.815592
240.334362	7999.883553	13.274829	-0.050056	4.815599
240.428613	7999.857330	13.279834	-0.050073	4.815591
240.296466	7999.843451	13.284839	-0.050049	4.815588
240.327301	7999.829010	13.289843	-0.050055	4.815583
240.381778	7999.991098	13.294848	-0.050065	4.815631
240.433289	7999.788037	13.299853	-0.050074	4.815571
240.220116	7999.869991	13.304858	-0.050035	4.815596
240.142129	7999.786533	13.309863	-0.050020	4.815572
240.297455	7999.870188	13.314867	-0.050049	4.815596
240.066854	7999.871795	13.319872	-0.050006	4.815597
240.222505	7999.840161	13.324877	-0.050035	4.815587
240.107663	7999.822293	13.329882	-0.050014	4.815582
240.150565	7999.923342	13.334887	-0.050022	4.815612
240.296650	7999.810420	13.339891	-0.050049	4.815578
240.243484	7999.985709	13.344896	-0.050040	4.815630
240.209354	7999.789801	13.349901	-0.050033	4.815572
240.177781	7999.769012	13.354906	-0.050027	4.815567
240.219211	7999.863632	13.359911	-0.050035	4.815594
240.510956	7999.864095	13.364915	-0.050090	4.815593
240.267754	7999.955171	13.369920	-0.050045	4.815621
240.117141	7999.872670	13.374925	-0.050016	4.815597
240.128669	7999.857917	13.379930	-0.050019	4.815593
240.266608	7999.789700	13.384935	-0.050044	4.815572
240.247539	7999.879070	13.389939	-0.050041	4.815598
240.092593	7999.852011	13.394944	-0.050012	4.815591
240.111119	7999.791467	13.399949	-0.050016	4.815573
240.225972	7999.874466	13.404954	-0.050037	4.815597
240.212336	7999.878521	13.409959	-0.050035	4.815598
240.265959	7999.880463	13.414963	-0.050045	4.815599
240.033924	7999.872438	13.419968	-0.050002	4.815597
240.179217	7999.866258	13.424973	-0.050029	4.815595
240.198357	7999.854831	13.429978	-0.050032	4.815592
240.157693	7999.871258	13.434983	-0.050025	4.815596
240.456406	7999.871834	13.439987	-0.050080	4.815595
240.428216	7999.947179	13.444992	-0.050075	4.815617
240.386168	7999.872842	13.449997	-0.050068	4.815596
240.437070	7999.866199	13.455002	-0.050077	4.815594
240.292798	7999.866002	13.460007	-0.050050	4.815594
240.384020	7999.791690	13.465011	-0.050067	4.815572
240.134864	7999.967005	13.470016	-0.050021	4.815625
240.081487	7999.783597	13.475021	-0.050011	4.815571
240.217588	7999.776199	13.480026	-0.050036	4.815568
240.234169	7999.874687	13.485031	-0.050040	4.815597
240.233556	7999.780739	13.490035	-0.050040	4.815570
240.167920	7999.873625	13.495040	-0.050027	4.815597
240.237467	7999.899311	13.500045	-0.050040	4.815604
240.306502	8000.048824	13.505050	-0.050053	4.815648
240.365333	7999.977190	13.510055	-0.050064	4.815626
240.352405	7999.936419	13.515059	-0.050062	4.815615
240.228503	8000.007010	13.520064	-0.050039	4.815636
240.200611	7999.780244	13.525069	-0.050034	4.815570
240.361410	7999.954730	13.530074	-0.050064	4.815620
240.164130	7999.874675	13.535079	-0.050027	4.815597
240.292267	7999.867149	13.540083	-0.050051	4.815595
240.333080	7999.943611	13.545088	-0.050059	4.815617
240.348519	7999.867004	13.550093	-0.050062	4.815594
240.228677	7999.773259	13.555098	-0.050039	4.815567
240.265490	7999.989505	13.560103	-0.050047	4.815631
240.428045	7999.826675	13.565107	-0.050077	4.815582
240.435827	7999.864171	13.570112	-0.050078	4.815593
240.450424	7999.878291	13.575117	-0.050081	4.815597
240.411976	7999.868065	13.580122	-0.050074	4.815594
240.506051	7999.892014	13.585127	-0.050092	4.815601
240.408790	7999.783689	13.590131	-0.050073	4.815570
240.307586	7999.851444	13.595136	-0.050055	4.815590
240.304605	7999.910116	13.600141	-0.050054	4.815607
240.465309	7999.842268	13.605146	-0.050084	4.815587
240.225651	7999.856538	13.610151	-0.050040	4.815592
240.393900	7999.878486	13.615155	-0.050071	4.815597
240.449431	7999.948782	13.620160	-0.050082	4.815618
240.314702	7999.879349	13.625165	-0.050056	4.815598
240.393934	7999.862490	13.630170	-0.050071	4.815593
240.366837	7999.872732	13.635175	-0.050066	4.815596
240.141062	7999.782608	13.640179	-0.050024	4.815571
240.239689	8000.070314	13.645184	-0.050043	4.815654
240.340079	7999.869112	13.650189	-0.050061	4.815595
240.234664	7999.755318	13.655194	-0.050042	4.815562
240.119969	7999.979783	13.660199	-0.050021	4.815628
240.441207	7999.869700	13.665203	-0.050080	4.815595
240.452369	7999.877359	13.670208	-0.050083	4.815597
240.394905	7999.843339	13.675213	-0.050072	4.815587
240.369107	7999.871751	13.680218	-0.050067	4.815596
240.376443	7999.894293	13.685223	-0.050069	4.815602
240.444101	7999.980800	13.690227	-0.050081	4.815627
240.377674	7999.872973	13.695232	-0.050069	4.815596
240.525302	7999.903128	13.700237	-0.050097	4.815604
240.232677	7999.773489	13.705242	-0.050042	4.815567
240.227383	7999.856676	13.710247	-0.050041	4.815592
240.405677	7999.898003	13.715251	-0.050075	4.815603
240.442462	7999.875118	13.720256	-0.050081	4.815596
240.458889	7999.867917	13.725261	-0.050085	4.815594
240.463186	7999.785792	13.730266	-0.050085	4.815570
240.603839	7999.862805	13.735271	-0.050112	4.815592
240.627990	7999.797014	13.740275	-0.050116	4.815572
240.358318	7999.860972	13.745280	-0.050066	4.815592
240.501691	7999.879314	13.750285	-0.050093	4.815597
240.509510	7999.861298	13.755290	-0.050094	4.815592
240.193065	7999.860445	13.760295	-0.050035	4.815593
240.258835	7999.849774	13.765299	-0.050048	4.815590
240.402055	7999.889464	13.770304	-0.050075	4.815601
240.212646	7999.858644	13.775309	-0.050039	4.815592
240.433738	7999.955109	13.780314	-0.050081	4.815620
240.534750	7999.875618	13.785319	-0.050099	4.815596
240.421114	7999.880187	13.790323	-0.050078	4.815598
240.132983	7999.843497	13.795328	-0.050025	4.815588
240.333769	7999.895863	13.800333	-0.050062	4.815603
240.441577	7999.775916	13.805338	-0.050082	4.815567
240.444244	7999.875246	13.810343	-0.050083	4.815596
240.470390	7999.875675	13.815347	-0.050088	4.815596
240.400479	7999.857467	13.820352	-0.050075	4.815591
240.362937	7999.910242	13.825357	-0.050068	4.815607
240.466284	7999.777411	13.830362	-0.050087	4.815567
240.470067	7999.969637	13.835367	-0.050088	4.815624
240.363020	7999.865422	13.840371	-0.050068	4.815594
240.317345	7999.868958	13.845376	-0.050060	4.815595
240.387146	7999.777218	13.850381	-0.050073	4.815568
240.372991	7999.877344	13.855386	-0.050070	4.815597
240.413600	7999.779793	13.860391	-0.050078	4.815568
240.517005	7999.802825	13.865395	-0.050097	4.815575
240.456151	7999.869100	13.870400	-0.050086	4.815594
240.420068	7999.834359	13.875405	-0.050079	4.815584
240.363960	7999.832388	13.880410	-0.050069	4.815584
240.294595	7999.800311	13.885415	-0.050056	4.815575
240.426981	7999.791786	13.890419	-0.050081	4.815572
240.539895	7999.867282	13.895424	-0.050102	4.815593
240.314854	7999.859370	13.900429	-0.050060	4.815592
240.319313	7999.873326	13.905434	-0.050061	4.815596
240.278466	7999.874805	13.910439	-0.050053	4.815597
240.259059	7999.880901	13.915443	-0.050050	4.815599
240.347468	7999.877001	13.920448	-0.050066	4.815597
240.358153	7999.818465	13.925453	-0.050068	4.815580
240.312445	7999.831608	13.930458	-0.050060	4.815584
240.466515	7999.967554	13.935463	-0.050089	4.815623
240.449229	7999.786864	13.940467	-0.050085	4.815570
240.312816	7999.786794	13.945472	-0.050060	4.815571
240.344841	7999.784116	13.950477	-0.050066	4.815570
240.384861	7999.885119	13.955482	-0.050074	4.815599
240.243575	7999.780351	13.960487	-0.050047	4.815569
240.241956	7999.801681	13.965491	-0.050047	4.815576
240.360125	7999.977611	13.970496	-0.050069	4.815626
240.423586	7999.855877	13.975501	-0.050081	4.815591
240.431517	7999.828255	13.980506	-0.050083	4.815582
240.367381	7999.866720	13.985511	-0.050071	4.815594
240.565424	7999.894489	13.990515	-0.050108	4.815601
240.686424	7999.770485	13.995520	-0.050130	4.815564
240.555506	7999.877258	14.000525	-0.050106	4.815596
240.571075	7999.778234	14.005530	-0.050109	4.815567
240.255996	7999.866010	14.010535	-0.050050	4.815594
240.214015	7999.794878	14.015539	-0.050043	4.815574
240.298921	7999.856041	14.020544	-0.050058	4.815591
240.662590	7999.786145	14.025549	-0.050126	4.815569
240.528771	7999.883263	14.030554	-0.050101	4.815598
240.483886	7999.781124	14.035559	-0.050093	4.815568
240.593753	7999.791451	14.040563	-0.050114	4.815571
240.443217	7999.881893	14.045568	-0.050086	4.815598
240.450033	7999.791268	14.050573	-0.050087	4.815572
240.602534	7999.888757	14.055578	-0.050115	4.815599
240.431227	7999.865702	14.060583	-0.050084	4.815593
240.564697	7999.883884	14.065587	-0.050109	4.815598
240.537667	7999.882384	14.070592	-0.050104	4.815598
240.536127	7999.881297	14.075597	-0.050103	4.815597
240.568631	7999.779345	14.080602	-0.050109	4.815567
240.458258	7999.884316	14.085607	-0.050089	4.815599
240.585366	7999.789235	14.090611	-0.050113	4.815570
240.415122	7999.866547	14.095616	-0.050081	4.815594
240.395606	7999.784035	14.100621	-0.050077	4.815570
240.462249	7999.868389	14.105626	-0.050090	4.815594
240.722457	7999.867275	14.110631	-0.050138	4.815592
240.749938	7999.800470	14.115635	-0.050144	4.815573
240.722209	7999.864079	14.120640	-0.050139	4.815592
240.624181	7999.787767	14.125645	-0.050120	4.815570
240.601725	7999.894164	14.130650	-0.050116	4.815601
240.530467	7999.774516	14.135655	-0.050103	4.815566
240.654781	7999.901440	14.140659	-0.050126	4.815603
240.622474	7999.858220	14.145664	-0.050120	4.815590
240.614021	7999.826062	14.150669	-0.050119	4.815581
240.736736	7999.796029	14.155674	-0.050142	4.815572
240.748938	7999.873097	14.160679	-0.050144	4.815594
240.792254	7999.907966	14.165683	-0.050152	4.815604
240.696494	7999.819947	14.170688	-0.050134	4.815579
240.781655	7999.890724	14.175693	-0.050150	4.815599
240.647622	7999.884287	14.180698	-0.050125	4.815598
240.646101	7999.960064	14.185703	-0.050125	4.815620
240.936823	7999.826000	14.190707	-0.050179	4.815579
240.765568	7999.885148	14.195712	-0.050148	4.815597
240.428734	7999.803898	14.200717	-0.050085	4.815575
240.527711	7999.782021	14.205722	-0.050103	4.815568
240.618459	7999.865699	14.210727	-0.050120	4.815592
240.646423	7999.885374	14.215731	-0.050126	4.815598
240.474514	7999.862309	14.220736	-0.050094	4.815592
240.647994	7999.879005	14.225741	-0.050126	4.815596
240.553713	7999.780335	14.230746	-0.050109	4.815568
240.401174	7999.866475	14.235751	-0.050080	4.815594
240.451470	7999.853417	14.240755	-0.050090	4.815590
240.553515	7999.823050	14.245760	-0.050109	4.815580
240.593280	7999.794876	14.250765	-0.050116	4.815572
240.492206	7999.795379	14.255770	-0.050097	4.815572
240.614817	7999.869965	14.260775	-0.050120	4.815594
240.602390	7999.887917	14.265779	-0.050118	4.815599
240.522888	7999.855675	14.270784	-0.050103	4.815590
240.451338	7999.886548	14.275789	-0.050090	4.815599
240.404876	7999.591160	14.280794	-0.050081	4.815513

240.394105	7996.343890	14.285799	-0.050077	4.814563
240.648812	7990.743374	14.290803	-0.050121	4.812924
240.515358	7983.947211	14.295808	-0.050092	4.810935
240.509003	7976.623936	14.300813	-0.050086	4.808791
240.837078	7969.095998	14.305818	-0.050142	4.806585
240.504544	7961.176831	14.310823	-0.050075	4.804265
240.436264	7953.372059	14.315827	-0.050057	4.801977
240.377445	7945.416900	14.320832	-0.050041	4.799644
240.555540	7937.438282	14.325837	-0.050069	4.797301
240.337175	7929.444996	14.330842	-0.050024	4.794955
240.195937	7921.362261	14.335847	-0.049992	4.792581
240.229937	7913.384824	14.340851	-0.049993	4.790236
240.428158	7905.419944	14.345856	-0.050025	4.787893
240.108996	7897.377532	14.350861	-0.049960	4.785528
240.254332	7889.454728	14.355866	-0.049982	4.783195
240.206427	7881.390088	14.360871	-0.049968	4.780821
240.215716	7873.452053	14.365875	-0.049965	4.778482
240.065397	7865.396201	14.370880	-0.049932	4.776107
239.925084	7857.371004	14.375885	-0.049900	4.773741
240.123536	7849.369972	14.380890	-0.049932	4.771379
240.077995	7841.356072	14.385895	-0.049919	4.769013
240.214359	7833.406507	14.390899	-0.049939	4.766664
240.083836	7825.383687	14.395904	-0.049909	4.764294
239.826817	7817.423597	14.400909	-0.049856	4.761941
239.860483	7809.362245	14.405914	-0.049858	4.759556
240.043955	7801.426858	14.410919	-0.049887	4.757207
239.940491	7793.375114	14.415923	-0.049862	4.754823
239.601528	7785.316435	14.420928	-0.049794	4.752437
239.587231	7777.298097	14.425933	-0.049786	4.750060
239.836510	7769.348682	14.430938	-0.049827	4.747701
239.511558	7761.314036	14.435943	-0.049762	4.745318
239.668522	7753.354732	14.440947	-0.049786	4.742955
239.662678	7745.331504	14.445952	-0.049779	4.740572
239.663246	7737.384857	14.450957	-0.049774	4.738210
239.546517	7729.350763	14.455962	-0.049748	4.735822
239.505573	7721.318346	14.460967	-0.049735	4.733433
239.761693	7713.278081	14.465971	-0.049777	4.731039
239.626865	7705.280174	14.470976	-0.049747	4.728658
239.593727	7697.322880	14.475981	-0.049736	4.726288
239.736434	7689.305158	14.480986	-0.049757	4.723897
239.456560	7681.325533	14.485991	-0.049700	4.721518
239.520186	7673.312103	14.490995	-0.049707	4.719127
239.576752	7665.369576	14.496000	-0.049712	4.716756
239.292969	7657.309201	14.501005	-0.049654	4.714349
239.388282	7649.314480	14.506010	-0.049667	4.711960
239.339882	7641.271550	14.511015	-0.049652	4.709555
239.575127	7633.342309	14.516019	-0.049691	4.707183
239.268331	7625.322378	14.521024	-0.049629	4.704784
239.090850	7617.295057	14.526029	-0.049591	4.702380
239.176895	7609.305992	14.531034	-0.049601	4.699987
239.021661	7601.337091	14.536039	-0.049567	4.697598
238.965006	7593.287597	14.541043	-0.049552	4.695184
239.163749	7585.285459	14.546048	-0.049584	4.692783
238.999930	7577.276863	14.551053	-0.049548	4.690379
238.870758	7569.287192	14.556058	-0.049519	4.687979
238.813661	7561.274032	14.561063	-0.049503	4.685571
238.969012	7553.319110	14.566067	-0.049527	4.683179
238.890373	7545.300580	14.571072	-0.049507	4.680767
238.910140	7537.317825	14.576077	-0.049505	4.678364
239.098078	7529.326509	14.581082	-0.049535	4.675958
238.849179	7521.209802	14.586087	-0.049484	4.673513
238.853995	7513.164837	14.591091	-0.049479	4.671087
238.921899	7505.186416	14.596096	-0.049487	4.668681
238.736165	7497.226579	14.601101	-0.049447	4.666279
238.703383	7489.242563	14.606106	-0.049436	4.663869
238.624629	7481.241862	14.611111	-0.049416	4.661452
238.718672	7473.265570	14.616115	-0.049429	4.659041
238.732677	7465.297245	14.621120	-0.049426	4.656632
238.480363	7457.228033	14.626125	-0.049374	4.654191
238.648669	7449.246861	14.631130	-0.049400	4.651774
238.612563	7441.202242	14.636135	-0.049388	4.649338
238.549560	7433.229777	14.641139	-0.049371	4.646922
238.534507	7425.180272	14.646144	-0.049363	4.644482
238.697426	7417.241368	14.651149	-0.049389	4.642073
238.585854	7409.215504	14.656154	-0.049363	4.639638
238.428172	7401.280166	14.661159	-0.049328	4.637228
238.354319	7393.241283	14.666163	-0.049309	4.634786
238.324900	7385.187224	14.671168	-0.049299	4.632337
238.274890	7377.147682	14.676173	-0.049284	4.629892
238.415458	7369.194650	14.681178	-0.049305	4.627472
238.259797	7361.198352	14.686183	-0.049271	4.625038
238.148619	7353.202260	14.691187	-0.049245	4.622602
238.269853	7345.181846	14.696192	-0.049263	4.620157
238.418095	7337.192254	14.701197	-0.049285	4.617721
238.120714	7329.206838	14.706202	-0.049224	4.615284
238.099527	7321.173560	14.711207	-0.049215	4.612832
238.142626	7313.141478	14.716211	-0.049218	4.610379
238.111867	7305.170903	14.721216	-0.049207	4.607943
238.004418	7297.142355	14.726221	-0.049182	4.605488
238.032764	7289.215947	14.731226	-0.049182	4.603063
237.987700	7281.185711	14.736231	-0.049169	4.600605
237.887680	7273.168021	14.741235	-0.049145	4.598150
237.805475	7265.202508	14.746240	-0.049125	4.595709
237.860044	7257.127002	14.751245	-0.049130	4.593233
237.694950	7249.123423	14.756250	-0.049094	4.590778
237.929487	7241.096898	14.761255	-0.049132	4.588315
237.836154	7233.122124	14.766259	-0.049110	4.585866
237.674107	7225.131511	14.771264	-0.049074	4.583411
237.467859	7217.134203	14.776269	-0.049031	4.580952
237.703145	7209.163325	14.781274	-0.049069	4.578501
237.576920	7201.139949	14.786279	-0.049041	4.576032
237.611538	7193.075826	14.791283	-0.049042	4.573549
237.466433	7185.109916	14.796288	-0.049010	4.571095
237.704271	7177.060861	14.801293	-0.049049	4.568614
237.545314	7169.160337	14.806298	-0.049014	4.566177
237.421593	7161.147633	14.811303	-0.048986	4.563705
237.602384	7153.199693	14.816307	-0.049015	4.561251
237.513059	7145.180385	14.821312	-0.048993	4.558774
237.373844	7137.170761	14.826317	-0.048962	4.556298
237.241937	7129.124137	14.831322	-0.048932	4.553809
237.381126	7121.078584	14.836327	-0.048953	4.551320
237.090991	7113.089040	14.841331	-0.048894	4.548846
237.127774	7105.132414	14.846336	-0.048895	4.546382
237.084012	7097.081856	14.851341	-0.048882	4.543887
237.120104	7089.142978	14.856346	-0.048884	4.541425
237.020975	7081.117669	14.861351	-0.048860	4.538935
237.238232	7073.148132	14.866355	-0.048895	4.536461
237.211010	7065.147251	14.871360	-0.048885	4.533976
237.168137	7057.089615	14.876365	-0.048872	4.531472
237.077941	7049.117082	14.881370	-0.048850	4.528993
236.920305	7041.108297	14.886375	-0.048815	4.526501
236.966301	7033.109548	14.891379	-0.048819	4.524011
236.703263	7025.132504	14.896384	-0.048765	4.521526
236.769754	7017.101375	14.901389	-0.048772	4.519023
236.816583	7009.193948	14.906394	-0.048776	4.516558
236.764369	7001.095529	14.911399	-0.048761	4.514031
236.926930	6992.981924	14.916403	-0.048786	4.511499
236.815337	6985.051988	14.921408	-0.048760	4.509022
236.708693	6977.025543	14.926413	-0.048735	4.506514
236.889483	6969.077969	14.931418	-0.048763	4.504029
236.799318	6961.036372	14.936423	-0.048741	4.501513
236.803191	6953.066260	14.941427	-0.048737	4.499018
236.752261	6945.110055	14.946432	-0.048722	4.496526
236.650707	6937.059171	14.951437	-0.048698	4.494003
236.646973	6929.076610	14.956442	-0.048692	4.491500
236.395826	6921.033305	14.961447	-0.048641	4.488976
236.499627	6913.053692	14.966451	-0.048655	4.486472
236.493353	6905.040877	14.971456	-0.048648	4.483955
236.475619	6897.061494	14.976461	-0.048640	4.481447
236.693482	6889.068197	14.981466	-0.048675	4.478935
236.559303	6881.116862	14.986471	-0.048645	4.476433
236.439349	6873.075682	14.991475	-0.048618	4.473901
236.370809	6865.038530	14.996480	-0.048600	4.471369
236.330518	6856.991777	15.001485	-0.048587	4.468833
236.267461	6849.064700	15.006490	-0.048570	4.466334
236.253325	6841.022803	15.011495	-0.048562	4.463796
236.470933	6833.049937	15.016499	-0.048598	4.461280
236.364210	6825.031106	15.021504	-0.048573	4.458747
236.158715	6817.021071	15.026509	-0.048529	4.456215
236.123021	6809.053018	15.031514	-0.048518	4.453695
236.091664	6800.998687	15.036519	-0.048507	4.451147
236.097802	6792.987938	15.041523	-0.048503	4.448611
235.950918	6785.036003	15.046528	-0.048470	4.446091
236.070319	6776.985617	15.051533	-0.048487	4.443540
236.197591	6769.021397	15.056538	-0.048506	4.441015
235.870314	6761.052183	15.061543	-0.048440	4.438485
235.820380	6753.043473	15.066547	-0.048425	4.435942
235.903152	6744.971677	15.071552	-0.048435	4.433378
235.918600	6736.942805	15.076557	-0.048433	4.430827
235.872828	6728.972444	15.081562	-0.048419	4.428291
236.034869	6720.947706	15.086567	-0.048444	4.425739
235.847128	6713.007262	15.091571	-0.048404	4.423209
235.844885	6705.025530	15.096576	-0.048399	4.420667
235.559872	6697.009649	15.101581	-0.048341	4.418110
235.612378	6689.029501	15.106586	-0.048345	4.415565
235.481221	6680.970764	15.111591	-0.048316	4.412992
235.421551	6672.966475	15.116595	-0.048299	4.410436
235.587962	6664.995455	15.121600	-0.048325	4.407890
235.589887	6656.945750	15.126605	-0.048320	4.405317
235.737872	6648.992016	15.131610	-0.048343	4.402773
235.615422	6641.005405	15.136615	-0.048315	4.400216
235.821960	6633.066674	15.141619	-0.048348	4.397675
235.564846	6624.999135	15.146624	-0.048295	4.395088
235.544732	6616.958651	15.151629	-0.048286	4.392510
235.585437	6608.974375	15.156634	-0.048289	4.389949
235.559580	6600.980369	15.161639	-0.048279	4.387383
235.356752	6592.964091	15.166643	-0.048236	4.384807
235.389192	6585.013438	15.171648	-0.048237	4.382252
235.365756	6576.949055	15.176653	-0.048227	4.379658
235.271167	6569.041124	15.181658	-0.048204	4.377113
235.178903	6560.985596	15.186663	-0.048182	4.374519
235.191056	6552.955212	15.191667	-0.048179	4.371932
235.120446	6544.963108	15.196672	-0.048161	4.369356
234.962676	6536.985168	15.201677	-0.048126	4.366781
235.223324	6528.983585	15.206682	-0.048170	4.364201
235.283225	6521.038896	15.211687	-0.048176	4.361636
235.163347	6513.013547	15.216691	-0.048148	4.359042
235.205119	6505.068968	15.221696	-0.048151	4.356474
235.091991	6496.918960	15.226701	-0.048125	4.353837
235.067502	6488.848314	15.231706	-0.048115	4.351224
234.986321	6480.889700	15.236711	-0.048095	4.348646
234.991024	6472.907098	15.241715	-0.048090	4.346059
234.972783	6464.945136	15.246720	-0.048082	4.343477
234.812898	6456.980333	15.251725	-0.048047	4.340892
234.890581	6449.007592	15.256730	-0.048056	4.338304
234.770909	6440.953517	15.261735	-0.048029	4.335687
234.600347	6432.947713	15.266739	-0.047992	4.333083
234.576291	6424.940711	15.271744	-0.047982	4.330479
234.729112	6416.945186	15.276749	-0.048006	4.327878
234.647041	6408.941436	15.281754	-0.047985	4.325271
234.471206	6400.967649	15.286759	-0.047947	4.322672
234.471171	6392.923912	15.291763	-0.047942	4.320049
234.429977	6385.022818	15.296768	-0.047929	4.317472
234.219063	6376.959231	15.301773	-0.047885	4.314838
234.241855	6368.905737	15.306778	-0.047884	4.312208
234.393164	6360.885657	15.311783	-0.047907	4.309588
234.220424	6352.970636	15.316787	-0.047870	4.306998
234.244427	6344.915554	15.321792	-0.047869	4.304362
234.406398	6336.955505	15.326797	-0.047894	4.301757
234.381426	6328.925678	15.331802	-0.047884	4.299126
234.313459	6320.934204	15.336807	-0.047866	4.296506
234.224659	6312.884404	15.341811	-0.047845	4.293865
234.252780	6304.925134	15.346816	-0.047845	4.291253
234.216545	6296.917197	15.351821	-0.047833	4.288622
234.350419	6288.923207	15.356826	-0.047853	4.285996
234.303313	6280.914935	15.361831	-0.047839	4.283363
233.922965	6272.928673	15.366835	-0.047763	4.280732
233.881255	6264.972883	15.371840	-0.047750	4.278112
233.961877	6256.908919	15.376845	-0.047760	4.275456
234.050173	6248.898027	15.381850	-0.047771	4.272816
233.835150	6240.870717	15.386855	-0.047726	4.270167
233.795417	6232.881656	15.391859	-0.047713	4.267530
233.972844	6224.884191	15.396864	-0.047741	4.264890
234.035005	6216.877718	15.401869	-0.047748	4.262245
233.964005	6208.899630	15.406874	-0.047729	4.259606
234.057741	6200.928626	15.411879	-0.047742	4.256969
233.862945	6192.900707	15.416883	-0.047700	4.254310
233.759618	6184.892319	15.421888	-0.047676	4.251656
233.823346	6176.879614	15.426893	-0.047682	4.249000
233.914255	6168.922887	15.431898	-0.047694	4.246362
233.742750	6160.902330	15.436903	-0.047657	4.243698
233.697547	6152.926518	15.441907	-0.047644	4.241049
233.625628	6144.956481	15.446912	-0.047625	4.238399
233.527907	6136.955605	15.451917	-0.047602	4.235738
233.572858	6128.940653	15.456922	-0.047605	4.233071
233.730444	6120.886202	15.461927	-0.047629	4.230391
233.701657	6112.890999	15.466931	-0.047619	4.227727
233.678600	6104.890386	15.471936	-0.047609	4.225060
233.430032	6096.948349	15.476941	-0.047558	4.222408
233.605767	6088.925742	15.481946	-0.047585	4.219732
233.489256	6080.963710	15.486951	-0.047558	4.217071
233.684586	6072.903895	15.491955	-0.047590	4.214379
233.668312	6064.941488	15.496960	-0.047581	4.211716
233.322097	6056.896367	15.501965	-0.047512	4.209020
233.338925	6048.945024	15.506970	-0.047510	4.206358
233.332762	6040.915605	15.511975	-0.047504	4.203667
233.136827	6032.951279	15.516979	-0.047462	4.200995
233.098735	6024.979684	15.521984	-0.047450	4.198320
233.107295	6016.950354	15.526989	-0.047446	4.195624
233.238661	6008.864663	15.531994	-0.047465	4.192910
233.182798	6000.813394	15.536999	-0.047450	4.190203
233.142764	5992.857774	15.542003	-0.047437	4.187526
233.173878	5984.889186	15.547008	-0.047438	4.184844
232.901506	5976.921734	15.552013	-0.047382	4.182158
232.850493	5968.906856	15.557018	-0.047367	4.179456
232.922737	5960.916244	15.562023	-0.047376	4.176762
232.782702	5952.856450	15.567027	-0.047344	4.174041
232.998360	5944.887105	15.572032	-0.047379	4.171352
233.011473	5936.859446	15.577037	-0.047377	4.168639
233.011116	5928.907621	15.582042	-0.047372	4.165951
233.082108	5920.885633	15.587047	-0.047380	4.163237
232.902714	5912.910622	15.592051	-0.047341	4.160535
232.899599	5904.931111	15.597056	-0.047335	4.157832
232.574897	5896.899819	15.602061	-0.047270	4.155106
232.704307	5888.901350	15.607066	-0.047289	4.152394
232.745810	5880.868849	15.612071	-0.047291	4.149668
232.766760	5872.869906	15.617075	-0.047290	4.146951
232.561386	5864.892488	15.622080	-0.047247	4.144237
232.403101	5856.919628	15.627085	-0.047212	4.141523
232.563873	5848.868191	15.632090	-0.047237	4.138785
232.450589	5840.919869	15.637095	-0.047211	4.136077
232.475752	5832.877467	15.642099	-0.047210	4.133336
232.592767	5824.849865	15.647104	-0.047227	4.130600
232.576943	5816.856182	15.652109	-0.047219	4.127872
232.552911	5808.894604	15.657114	-0.047209	4.125153
232.430865	5800.919997	15.662119	-0.047181	4.122427
232.261935	5792.889486	15.667123	-0.047144	4.119679
232.175582	5784.971694	15.672128	-0.047123	4.116968
232.340078	5776.873807	15.677133	-0.047149	4.114198
232.283311	5768.886227	15.682138	-0.047133	4.111461
232.127599	5760.866789	15.687143	-0.047099	4.108709
232.055786	5752.844136	15.692147	-0.047080	4.105956
232.141621	5744.899947	15.697152	-0.047091	4.103230
232.094685	5736.887996	15.702157	-0.047077	4.100477
232.097000	5728.921307	15.707162	-0.047073	4.097738
231.870354	5720.906261	15.712167	-0.047025	4.094978
231.884703	5712.907239	15.717171	-0.047023	4.092225
231.887197	5704.889605	15.722176	-0.047018	4.089463
231.898710	5696.899672	15.727181	-0.047015	4.086709
232.087061	5688.902680	15.732186	-0.047045	4.083953
231.888985	5680.943608	15.737191	-0.047003	4.081203
231.715473	5672.957380	15.742195	-0.046966	4.078443
231.876164	5664.981238	15.747200	-0.046990	4.075688
231.681696	5656.934565	15.752205	-0.046949	4.072902
231.583877	5648.916607	15.757210	-0.046926	4.070126
231.551271	5640.942055	15.762215	-0.046914	4.067364
231.712337	5632.903756	15.767219	-0.046939	4.064580
231.632623	5624.975324	15.772224	-0.046919	4.061829
231.408076	5616.914419	15.777229	-0.046872	4.059028
231.476642	5608.956612	15.782234	-0.046880	4.056266
231.328742	5600.898309	15.787239	-0.046847	4.053463
231.489680	5592.889209	15.792243	-0.046872	4.050680
231.508193	5584.935509	15.797248	-0.046870	4.047913
231.534317	5576.895514	15.802253	-0.046870	4.045113
231.370142	5568.981133	15.807258	-0.046834	4.042353
231.325722	5560.923917	15.812263	-0.046821	4.039542
231.430319	5552.956256	15.817267	-0.046835	4.036763
231.287044	5544.931463	15.822272	-0.046803	4.033959
231.210666	5536.828146	15.827277	-0.046784	4.031126
231.238058	5528.837600	15.832282	-0.046784	4.028332
231.140029	5520.872351	15.837287	-0.046760	4.025543
230.918025	5512.908315	15.842291	-0.046714	4.022751
230.950172	5504.928893	15.847296	-0.046715	4.019955
231.072769	5496.908286	15.852301	-0.046732	4.017144
231.149618	5488.897065	15.857306	-0.046742	4.014334
230.999361	5480.890921	15.862311	-0.046709	4.011520
231.008673	5472.863759	15.867315	-0.046705	4.008700
230.983548	5464.922789	15.872320	-0.046695	4.005907
230.853066	5456.925633	15.877325	-0.046666	4.003090
230.868570	5448.940819	15.882330	-0.046664	4.000279
230.804344	5440.973231	15.887335	-0.046647	3.997470
230.613577	5432.917084	15.892339	-0.046606	3.994626
230.742291	5424.877685	15.897344	-0.046625	3.991790
230.793852	5416.860777	15.902349	-0.046629	3.988960
230.623160	5408.914622	15.907354	-0.046592	3.986149
230.734975	5400.898315	15.912359	-0.046608	3.983316
230.888967	5392.890104	15.917363	-0.046631	3.980484
230.707844	5384.952648	15.922368	-0.046592	3.977670
230.502140	5376.934876	15.927373	-0.046549	3.974825
230.463186	5368.932628	15.932378	-0.046537	3.971986
230.575653	5360.924516	15.937383	-0.046552	3.969146
230.443597	5352.920609	15.942387	-0.046523	3.966301
230.669465	5344.960639	15.947392	-0.046560	3.963475
230.341943	5336.956598	15.952397	-0.046493	3.960623
230.344458	5328.985458	15.957402	-0.046489	3.957785
230.238616	5320.969232	15.962407	-0.046464	3.954928
230.258034	5312.914217	15.967411	-0.046462	3.952057
230.315701	5304.948918	15.972416	-0.046468	3.949217
230.282830	5296.922971	15.977421	-0.046457	3.946351
230.412980	5288.937633	15.982426	-0.046476	3.943501
230.398573	5280.958201	15.987431	-0.046468	3.940648
230.196925	5273.001727	15.992435	-0.046425	3.937798
230.062617	5264.997183	15.997440	-0.046395	3.934929
230.077600	5256.951856	16.002445	-0.046393	3.932047
229.985889	5248.955227	16.007450	-0.046370	3.929178
230.046783	5241.003742	16.012455	-0.046377	3.926326
230.054461	5232.972061	16.017459	-0.046373	3.923443
230.121708	5225.009263	16.022464	-0.046380	3.920583
230.012176	5216.999669	16.027469	-0.046355	3.917700
229.940077	5208.983695	16.032474	-0.046336	3.914814
230.016359	5200.969495	16.037479	-0.046345	3.911930
229.806385	5192.951731	16.042483	-0.046301	3.909036
229.922078	5184.972426	16.047488	-0.046317	3.906160
229.873407	5176.954769	16.052493	-0.046303	3.903266
229.886675	5168.987371	16.057498	-0.046301	3.900388
229.662792	5161.028797	16.062503	-0.046254	3.897507
229.658671	5152.955070	16.067507	-0.046248	3.894587
229.645789	5144.996496	16.072512	-0.046240	3.891705
229.412204	5136.972834	16.077517	-0.046192	3.888794
229.583867	5128.998274	16.082522	-0.046218	3.885906
229.545824	5120.997772	16.087527	-0.046206	3.883003
229.592146	5112.972967	16.092531	-0.046210	3.880090
229.569366	5105.042923	16.097536	-0.046200	3.877208
229.499629	5096.965987	16.102541	-0.046182	3.874270
229.419218	5088.727712	16.107546	-0.046162	3.871270
229.331064	5080.845045	16.112551	-0.046140	3.868397
229.134251	5072.884300	16.117555	-0.046099	3.865492
229.289172	5064.962555	16.122560	-0.046122	3.862606
229.225179	5056.958673	16.127565	-0.046105	3.859683
229.050294	5049.027663	16.132570	-0.046068	3.856782
229.372186	5040.968488	16.137575	-0.046122	3.853843
229.224981	5032.943950	16.142579	-0.046090	3.850904
229.088330	5025.002587	16.147584	-0.046059	3.847994
228.963178	5016.972110	16.152589	-0.046031	3.845049
229.036857	5009.035410	16.157594	-0.046039	3.842140
228.960675	5001.048504	16.162599	-0.046020	3.839207
228.838499	4993.088184	16.167603	-0.045992	3.836281
228.992579	4985.069929	16.172608	-0.046016	3.833338
228.869460	4977.004821	16.177613	-0.045988	3.830369
228.711477	4969.042972	16.182618	-0.045953	3.827435
228.683195	4961.030736	16.187623	-0.045943	3.824482
228.948269	4953.029851	16.192627	-0.045987	3.821538
228.607588	4945.080114	16.197632	-0.045918	3.818598
228.440253	4937.065766	16.202637	-0.045882	3.815635
228.583635	4929.057415	16.207642	-0.045903	3.812679
228.698819	4921.021419	16.212647	-0.045920	3.809710
228.479280	4913.071924	16.217651	-0.045874	3.806763
228.632659	4905.073954	16.222656	-0.045897	3.803804
228.357638	4897.114933	16.227661	-0.045841	3.800848
228.365053	4889.098445	16.232666	-0.045837	3.797874
228.502713	4881.100699	16.237671	-0.045857	3.794908
228.346448	4873.014908	16.242675	-0.045823	3.791900
228.524082	4865.055859	16.247680	-0.045851	3.788944
228.358453	4857.048004	16.252685	-0.045815	3.785961
228.527775	4849.075881	16.257690	-0.045842	3.782995
228.422210	4841.085462	16.262695	-0.045817	3.780015
228.149658	4833.117338	16.267699	-0.045761	3.777036
228.316668	4825.087195	16.272704	-0.045787	3.774042
228.412242	4817.070207	16.277709	-0.045799	3.771049
228.127831	4809.076872	16.282714	-0.045741	3.768054
228.307132	4801.083346	16.287719	-0.045770	3.765067
228.140987	4793.125619	16.292723	-0.045733	3.762083
228.074657	4785.108190	16.297728	-0.045716	3.759076
227.866409	4777.135925	16.302733	-0.045672	3.756081
228.028236	4769.089835	16.307738	-0.045697	3.753064
227.907220	4761.067723	16.312743	-0.045669	3.750048
227.813041	4753.087801	16.317747	-0.045647	3.747045
227.852189	4745.084427	16.322752	-0.045649	3.744034
227.945114	4737.120567	16.327757	-0.045661	3.741037
227.924273	4729.137920	16.332762	-0.045652	3.738028
227.847316	4721.140438	16.337767	-0.045632	3.735009
227.747883	4713.112034	16.342771	-0.045609	3.731976
227.629765	4705.115345	16.347776	-0.045582	3.728951
227.579362	4697.135745	16.352781	-0.045567	3.725933
227.722472	4689.160175	16.357786	-0.045589	3.722918
227.599915	4681.174247	16.362791	-0.045561	3.719890
227.521430	4673.186286	16.367795	-0.045541	3.716860
227.619119	4665.163912	16.372800	-0.045554	3.713819
227.517259	4657.065631	16.377805	-0.045530	3.710742
227.340336	4649.080818	16.382810	-0.045492	3.707703
227.365452	4641.096880	16.387815	-0.045491	3.704667
227.515763	4633.144931	16.392819	-0.045514	3.701644
227.660631	4625.228447	16.397824	-0.045536	3.698632
227.560711	4617.189533	16.402829	-0.045512	3.695565
227.459660	4609.181953	16.407834	-0.045488	3.692507
227.307918	4601.188489	16.412839	-0.045455	3.689450
227.133638	4593.219543	16.417843	-0.045417	3.686400
227.356460	4585.231731	16.422848	-0.045454	3.683350
227.319486	4577.225351	16.427853	-0.045442	3.680284
227.044714	4569.270049	16.432858	-0.045385	3.677229
227.283890	4561.243128	16.437863	-0.045425	3.674157
227.202050	4553.188274	16.442867	-0.045404	3.671063
227.111982	4545.216360	16.447872	-0.045382	3.667999
226.999644	4537.192591	16.452877	-0.045356	3.664911
227.096294	4529.219878	16.457882	-0.045369	3.661846
227.225475	4521.241870	16.462887	-0.045388	3.658777
227.121206	4513.225681	16.467891	-0.045363	3.655684
227.181872	4505.219622	16.472896	-0.045370	3.652598
227.129822	4497.194083	16.477901	-0.045355	3.649498
226.963258	4489.243829	16.482906	-0.045319	3.646421
226.904093	4481.252619	16.487911	-0.045302	3.643329
226.860726	4473.238915	16.492915	-0.045289	3.640226
226.797056	4465.292281	16.497920	-0.045272	3.637146
226.903464	4457.256086	16.502925	-0.045287	3.634033
226.916200	4449.216373	16.507930	-0.045284	3.630914
226.728118	4441.231345	16.512935	-0.045244	3.627807
226.739045	4433.236896	16.517939	-0.045241	3.624700
226.522401	4425.313416	16.522944	-0.045195	3.621611
226.442415	4417.290199	16.527949	-0.045175	3.618485
226.392857	4409.308642	16.532954	-0.045161	3.615373
226.267312	4401.345768	16.537959	-0.045132	3.612264
226.293568	4393.290304	16.542963	-0.045132	3.609119
226.388356	4385.318435	16.547968	-0.045145	3.606007
226.254403	4377.332242	16.552973	-0.045115	3.602880
226.351172	4369.318191	16.557978	-0.045127	3.599746
226.346026	4361.394868	16.562983	-0.045121	3.596642
226.094401	4353.360839	16.567987	-0.045069	3.593484
226.236789	4345.344513	16.572992	-0.045091	3.590342
226.454003	4337.342443	16.577997	-0.045126	3.587205
226.106852	4329.347751	16.583002	-0.045056	3.584053
225.945579	4321.412556	16.588007	-0.045021	3.580926
226.080842	4313.381123	16.593011	-0.045041	3.577766
226.200229	4305.409349	16.598016	-0.045058	3.574628
225.927114	4297.414781	16.603021	-0.045002	3.571466
226.024871	4289.365379	16.608026	-0.045015	3.568290
226.121717	4281.396602	16.613031	-0.045028	3.565143
225.967948	4273.406014	16.618035	-0.044994	3.561978
226.029987	4265.434196	16.623040	-0.045001	3.558823
225.896746	4257.431962	16.628045	-0.044971	3.555648
225.802714	4249.357704	16.633050	-0.044948	3.552443
225.615930	4241.368454	16.638055	-0.044908	3.549266
225.598976	4233.353312	16.643059	-0.044900	3.546080
225.749743	4225.383008	16.648064	-0.044923	3.542915
225.573280	4217.409119	16.653069	-0.044885	3.539735
225.669218	4209.430539	16.658074	-0.044897	3.536559
225.810491	4201.425922	16.663079	-0.044919	3.533371
225.596714	4193.386601	16.668083	-0.044874	3.530156
225.593399	4185.441808	16.673088	-0.044868	3.526982
225.573685	4177.451577	16.678093	-0.044859	3.523786
225.418768	4169.482061	16.683098	-0.044825	3.520592
225.228196	4161.527260	16.688103	-0.044785	3.517399
225.129471	4153.476214	16.693107	-0.044761	3.514168
225.313795	4145.484692	16.698112	-0.044790	3.510966
225.186382	4137.486382	16.703117	-0.044761	3.507750
225.076435	4129.475496	16.708122	-0.044736	3.504525
225.456495	4121.503803	16.713127	-0.044801	3.501329
225.274454	4113.521742	16.718131	-0.044762	3.498108
225.376689	4105.540435	16.723136	-0.044776	3.494893
225.137597	4097.525837	16.728141	-0.044726	3.491651
225.176438	4089.542598	16.733146	-0.044729	3.488428
225.258657	4081.554055	16.738151	-0.044739	3.485201
225.168162	4073.584167	16.743155	-0.044717	3.481972
225.151358	4065.593558	16.748160	-0.044708	3.478735
224.987223	4057.622828	16.753165	-0.044673	3.475498
224.772053	4049.547542	16.758170	-0.044627	3.472214
224.987174	4041.559478	16.763175	-0.044662	3.468976
224.817287	4033.548070	16.768179	-0.044626	3.465714
224.734345	4025.628588	16.773184	-0.044605	3.462488
224.905057	4017.588963	16.778189	-0.044632	3.459219
224.959545	4009.603698	16.783194	-0.044637	3.455965
224.968766	4001.602815	16.788199	-0.044633	3.452700
224.787550	3993.572158	16.793203	-0.044594	3.449413
224.808033	3985.624509	16.798208	-0.044593	3.446164
224.794986	3977.638274	16.803213	-0.044585	3.442895
224.726304	3969.648921	16.808218	-0.044568	3.439620
224.626585	3961.694855	16.813223	-0.044544	3.436355
224.534568	3953.643617	16.818227	-0.044522	3.433047
224.637389	3945.614620	16.823232	-0.044535	3.429752
224.639696	3937.657693	16.828237	-0.044531	3.426479
224.679620	3929.627197	16.833242	-0.044533	3.423175
224.870582	3921.685145	16.838247	-0.044564	3.419909
224.674352	3913.692544	16.843251	-0.044522	3.416606
224.623065	3905.718444	16.848256	-0.044507	3.413312
224.422065	3897.704084	16.853261	-0.044465	3.409994
224.440024	3889.699023	16.858266	-0.044463	3.406683
224.544788	3881.751027	16.863271	-0.044477	3.403396
224.435651	3873.770567	16.868275	-0.044452	3.400085
224.489803	3865.814345	16.873280	-0.044457	3.396786
224.290291	3857.763889	16.878285	-0.044414	3.393436
224.243960	3849.676310	16.883290	-0.044400	3.390073
224.114742	3841.744769	16.888295	-0.044371	3.386768
224.068255	3833.731624	16.893299	-0.044357	3.383429
224.147818	3825.783099	16.898304	-0.044367	3.380118
223.976220	3817.818794	16.903309	-0.044330	3.376789
224.014736	3809.793747	16.908314	-0.044332	3.373438
223.853848	3801.816060	16.913319	-0.044297	3.370096
223.912592	3793.797763	16.918323	-0.044303	3.366742
223.784587	3785.833975	16.923328	-0.044274	3.363401
223.831351	3777.854969	16.928333	-0.044277	3.360057
223.630940	3769.904424	16.933338	-0.044235	3.356712
223.632809	3761.893214	16.938343	-0.044230	3.353345
223.577517	3753.820815	16.943347	-0.044215	3.349948
223.800306	3745.827389	16.948352	-0.044251	3.346590
223.766057	3737.865693	16.953357	-0.044240	3.343233
223.474373	3729.914456	16.958362	-0.044180	3.339867
223.627369	3721.928885	16.963367	-0.044203	3.336500
223.650735	3713.883668	16.968371	-0.044203	3.333100
223.477146	3705.904467	16.973376	-0.044165	3.329716
223.559025	3697.915445	16.978381	-0.044175	3.326335
223.543606	3689.910699	16.983386	-0.044167	3.322940
223.443190	3681.961338	16.988391	-0.044143	3.319561
223.315017	3674.000545	16.993395	-0.044114	3.316174
223.278113	3665.973846	16.998400	-0.044102	3.312758
223.168625	3657.944305	17.003405	-0.044077	3.309335
223.030778	3649.970307	17.008410	-0.044046	3.305930
222.982964	3641.992175	17.013415	-0.044032	3.302524
223.092371	3633.982682	17.018419	-0.044047	3.299107
223.219971	3626.044758	17.023424	-0.044066	3.295718
223.044275	3618.038645	17.028429	-0.044028	3.292285
223.069664	3610.014146	17.033434	-0.044028	3.288847
223.105447	3602.058928	17.038439	-0.044029	3.285436
222.906259	3594.088126	17.043443	-0.043987	3.282006
222.997824	3586.086368	17.048448	-0.043999	3.278570
222.911546	3578.124321	17.053453	-0.043978	3.275141
222.653313	3570.092115	17.058458	-0.043924	3.271671
222.839470	3562.070767	17.063463	-0.043954	3.268220
222.862860	3554.078450	17.068467	-0.043953	3.264771
222.854616	3546.127073	17.073472	-0.043946	3.261335
222.870026	3538.161716	17.078477	-0.043944	3.257890
222.828355	3530.142287	17.083482	-0.043931	3.254416
222.781493	3522.161437	17.088487	-0.043917	3.250955
222.491763	3514.168378	17.093491	-0.043858	3.247475
222.557429	3506.163382	17.098496	-0.043865	3.244000
222.677505	3498.197052	17.103501	-0.043883	3.240540
222.421468	3490.248292	17.108506	-0.043830	3.237070
222.437224	3482.214163	17.113511	-0.043827	3.233569
222.317218	3474.135589	17.118515	-0.043800	3.230040
222.178752	3466.196227	17.123520	-0.043769	3.226566
222.318402	3458.198770	17.128525	-0.043790	3.223075
222.222007	3450.200690	17.133530	-0.043767	3.219571
222.247737	3442.273235	17.138535	-0.043766	3.216098
222.098092	3434.271979	17.143539	-0.043733	3.212582
222.284244	3426.237205	17.148544	-0.043763	3.209061
222.095692	3418.289187	17.153549	-0.043723	3.205559
221.909994	3410.326283	17.158554	-0.043683	3.202047
221.748534	3402.369908	17.163559	-0.043648	3.198535
221.988898	3394.325400	17.168563	-0.043687	3.194997
221.968034	3386.334383	17.173568	-0.043678	3.191467
221.817959	3378.336332	17.178573	-0.043645	3.187925
221.713574	3370.323130	17.183578	-0.043621	3.184375
221.849924	3362.407806	17.188583	-0.043641	3.180874
221.759704	3354.374473	17.193587	-0.043619	3.177307
221.897842	3346.404808	17.198592	-0.043640	3.173774
221.824710	3338.392044	17.203597	-0.043621	3.170209
221.483474	3330.428985	17.208602	-0.043552	3.166650
221.578922	3322.462847	17.213607	-0.043565	3.163105
221.779262	3314.416361	17.218611	-0.043597	3.159525
221.664536	3306.505982	17.223616	-0.043570	3.155988
221.685226	3298.469183	17.228621	-0.043569	3.152396
221.622369	3290.462247	17.233626	-0.043552	3.148810
221.713795	3282.470259	17.238631	-0.043564	3.145233
221.358459	3274.508870	17.243635	-0.043493	3.141646
221.374260	3266.543911	17.248640	-0.043491	3.138070
221.427471	3258.534376	17.253645	-0.043495	3.134471
221.319262	3250.565881	17.258650	-0.043470	3.130879
221.226192	3242.583626	17.263655	-0.043448	3.127278
221.217604	3234.573202	17.268659	-0.043441	3.123664
221.219606	3226.606236	17.273664	-0.043436	3.120065
220.978428	3218.671258	17.278669	-0.043386	3.116466
220.888825	3210.633984	17.283674	-0.043364	3.112824
221.032116	3202.621474	17.288679	-0.043386	3.109198
220.924745	3194.623363	17.293683	-0.043361	3.105564
221.023987	3186.651058	17.298688	-0.043374	3.101947
221.117413	3178.671440	17.303693	-0.043386	3.098321
220.941484	3170.694632	17.308698	-0.043348	3.094681
220.852612	3162.717845	17.313703	-0.043327	3.091040
220.955900	3154.690091	17.318707	-0.043341	3.087380
220.814764	3146.742956	17.323712	-0.043309	3.083742
220.822063	3138.759543	17.328717	-0.043306	3.080089
220.616647	3130.801747	17.333722	-0.043262	3.076435
220.789562	3122.753801	17.338727	-0.043289	3.072752
220.655444	3114.702544	17.343731	-0.043259	3.069048
220.693232	3106.728355	17.348736	-0.043261	3.065384
220.563381	3098.790325	17.353741	-0.043232	3.061724
220.429165	3090.819647	17.358746	-0.043202	3.058044
220.384316	3082.862305	17.363751	-0.043188	3.054371
220.483897	3074.808521	17.368755	-0.043201	3.050655
220.477618	3066.864458	17.373760	-0.043195	3.046980
220.299668	3058.903917	17.378765	-0.043157	3.043285
220.459851	3050.908057	17.383770	-0.043182	3.039586
220.466329	3042.949884	17.388775	-0.043178	3.035892
220.400432	3034.920969	17.393779	-0.043160	3.032157
220.217853	3026.950329	17.398784	-0.043121	3.028439
220.259272	3018.956848	17.403789	-0.043124	3.024717
220.270793	3010.987011	17.408794	-0.043121	3.020999
220.420932	3003.001790	17.413799	-0.043144	3.017277
220.039309	2995.020703	17.418803	-0.043067	3.013526
220.098478	2987.008131	17.423808	-0.043073	3.009777
220.055021	2979.057570	17.428813	-0.043060	3.006047
219.978225	2971.081197	17.433818	-0.043041	3.002299
220.277778	2963.087039	17.438823	-0.043091	2.998557
219.928339	2955.132238	17.443827	-0.043021	2.994796
219.876504	2947.097803	17.448832	-0.043006	2.991008
219.806677	2939.113843	17.453837	-0.042988	2.987238
219.648026	2931.118404	17.458842	-0.042953	2.983453
219.802249	2923.148672	17.463847	-0.042977	2.979691
219.738996	2915.187763	17.468851	-0.042960	2.975918
219.860912	2907.182310	17.473856	-0.042978	2.972128
219.634613	2899.217738	17.478861	-0.042930	2.968335
219.488116	2891.222743	17.483866	-0.042898	2.964527
219.620833	2883.259860	17.488871	-0.042917	2.960744
219.573198	2875.275452	17.493875	-0.042903	2.956936
219.474651	2867.316002	17.498880	-0.042880	2.953132
219.464803	2859.291325	17.503885	-0.042873	2.949297
219.446255	2851.312595	17.508890	-0.042864	2.945479
219.471729	2843.345958	17.513895	-0.042864	2.941663
219.368453	2835.352907	17.518899	-0.042840	2.937824
219.457030	2827.366363	17.523904	-0.042851	2.933992
219.510053	2819.358405	17.528909	-0.042856	2.930143
219.335831	2811.410386	17.533914	-0.042818	2.926306
219.285198	2803.466475	17.538919	-0.042804	2.922473
219.111321	2795.472222	17.543923	-0.042766	2.918603
218.992329	2787.500704	17.548928	-0.042739	2.914743
218.954953	2779.421928	17.553933	-0.042727	2.910829
219.007147	2771.418815	17.558938	-0.042731	2.906952
219.028531	2763.483095	17.563943	-0.042730	2.903101
218.868484	2755.497092	17.568947	-0.042695	2.899210
218.937591	2747.534322	17.573952	-0.042703	2.895338
219.013225	2739.555840	17.578957	-0.042712	2.891453
218.700299	2731.580741	17.583962	-0.042648	2.887544
218.896967	2723.602626	17.588967	-0.042680	2.883655
218.937328	2715.611805	17.593971	-0.042682	2.879747
218.743561	2707.686624	17.598976	-0.042641	2.875852
218.551193	2699.698378	17.603981	-0.042600	2.871922
218.528623	2691.678639	17.608986	-0.042591	2.867980
218.603513	2683.710345	17.613991	-0.042600	2.864063
218.413025	2675.739087	17.618995	-0.042559	2.860124
218.617620	2667.756507	17.624000	-0.042592	2.856197
218.555719	2659.768794	17.629005	-0.042575	2.852247
218.538842	2651.768803	17.634010	-0.042567	2.848287
218.468591	2643.831326	17.639015	-0.042549	2.844350
218.454915	2635.852555	17.644019	-0.042541	2.840391
218.378371	2627.893948	17.649024	-0.042522	2.836432
218.501116	2619.883670	17.654029	-0.042539	2.832453
218.423265	2611.871771	17.659034	-0.042520	2.828457
218.298961	2603.913436	17.664039	-0.042492	2.824479
218.155404	2595.969207	17.669043	-0.042460	2.820501
218.366798	2587.968136	17.674048	-0.042494	2.816510
218.457715	2579.979052	17.679053	-0.042506	2.812512
218.085585	2572.002942	17.684058	-0.042431	2.808488
218.122122	2564.023038	17.689063	-0.042433	2.804480
218.118160	2556.064776	17.694067	-0.042427	2.800474
218.030282	2548.107173	17.699072	-0.042406	2.796459
217.977303	2540.126099	17.704077	-0.042391	2.792428
217.883282	2532.131094	17.709082	-0.042368	2.788381
217.986381	2524.142099	17.714087	-0.042382	2.784344
217.866286	2516.182610	17.719091	-0.042354	2.780302
217.912818	2508.217794	17.724096	-0.042358	2.776261
217.808692	2500.239182	17.729101	-0.042333	2.772199
217.729004	2492.243115	17.734106	-0.042313	2.768123
217.758954	2484.277839	17.739111	-0.042314	2.764064
217.777426	2476.313375	17.744115	-0.042312	2.759998
217.513428	2468.378585	17.749120	-0.042258	2.755924
217.359044	2460.339216	17.754125	-0.042224	2.751798
217.480663	2452.290999	17.759130	-0.042242	2.747677
217.407969	2444.355472	17.764135	-0.042223	2.743596
217.144499	2436.389478	17.769139	-0.042169	2.739482
217.118389	2428.434109	17.774144	-0.042159	2.735382
217.333780	2420.425138	17.779149	-0.042194	2.731262
217.188627	2412.442619	17.784154	-0.042161	2.727128
217.152798	2404.498445	17.789159	-0.042150	2.723014
217.177144	2396.524812	17.794163	-0.042149	2.718882
217.076069	2388.591487	17.799168	-0.042125	2.714758
217.086979	2380.583075	17.804173	-0.042122	2.710594
217.076235	2372.590153	17.809178	-0.042115	2.706432
217.217590	2364.633144	17.814183	-0.042136	2.702291
216.911077	2356.689542	17.819187	-0.042074	2.698122
217.030317	2348.685053	17.824192	-0.042091	2.693942
217.075606	2340.693501	17.829197	-0.042094	2.689758
217.036227	2332.730531	17.834202	-0.042082	2.685576
216.918588	2324.784110	17.839207	-0.042055	2.681392
217.046475	2316.801436	17.844211	-0.042073	2.677198
216.844761	2308.848723	17.849216	-0.042031	2.672992
216.530646	2300.869142	17.854221	-0.041967	2.668758
216.571604	2292.857393	17.859226	-0.041970	2.664523
216.682736	2284.905148	17.864231	-0.041985	2.660317
216.718860	2276.931068	17.869235	-0.041987	2.656089
216.466826	2268.969115	17.874240	-0.041935	2.651841
216.723455	2260.955676	17.879245	-0.041977	2.647592
216.647639	2252.991071	17.884250	-0.041958	2.643341
216.539030	2245.076941	17.889255	-0.041933	2.639107
216.514477	2237.095818	17.894259	-0.041923	2.634837
216.504060	2229.091841	17.899264	-0.041916	2.630548
216.596363	2221.122238	17.904269	-0.041928	2.626277
216.375295	2213.156716	17.909274	-0.041882	2.621981
216.438607	2205.214047	17.914279	-0.041888	2.617709
216.154638	2197.244387	17.919283	-0.041830	2.613392
216.333600	2189.227637	17.924288	-0.041859	2.609074
216.094666	2181.317578	17.929293	-0.041809	2.604778
216.043429	2173.351835	17.934298	-0.041794	2.600457
216.115723	2165.380484	17.939303	-0.041803	2.596135
215.810450	2157.273676	17.944307	-0.041741	2.591706
216.082370	2149.217704	17.949312	-0.041786	2.587336
215.855025	2141.327561	17.954317	-0.041739	2.583016
215.810658	2133.378677	17.959322	-0.041725	2.578668
215.856168	2125.425074	17.964327	-0.041729	2.574317
215.802385	2117.468104	17.969331	-0.041713	2.569950
215.719878	2109.506733	17.974336	-0.041693	2.565571
215.811410	2101.559110	17.979341	-0.041705	2.561204
215.722870	2093.610993	17.984346	-0.041683	2.556817
215.720094	2085.643095	17.989351	-0.041678	2.552417
215.424179	2077.680755	17.994355	-0.041617	2.547992
215.425944	2069.706387	17.999360	-0.041613	2.543574
215.503742	2061.753326	18.004365	-0.041622	2.539165
215.298071	2053.800812	18.009370	-0.041579	2.534729
215.537727	2045.786410	18.014375	-0.041618	2.530282
215.416187	2037.820697	18.019379	-0.041590	2.525829
215.206702	2029.895156	18.024384	-0.041546	2.521384
215.145429	2021.967201	18.029389	-0.041530	2.516941
215.225552	2013.944743	18.034394	-0.041539	2.512446
215.311708	2005.946355	18.039399	-0.041550	2.507958
215.062207	1998.012695	18.044403	-0.041499	2.503474
215.023890	1990.053137	18.049408	-0.041486	2.498982
215.304123	1982.055129	18.054413	-0.041534	2.494484
215.074823	1974.098213	18.059418	-0.041486	2.489964
215.114943	1966.139100	18.064423	-0.041488	2.485454
215.090126	1958.195970	18.069427	-0.041478	2.480940
214.926311	1950.264829	18.074432	-0.041443	2.476414
214.913380	1942.294163	18.079437	-0.041435	2.471869
214.751383	1934.318831	18.084442	-0.041400	2.467301
214.885877	1926.346066	18.089447	-0.041420	2.462749
214.710077	1918.414944	18.094451	-0.041382	2.458189
214.692249	1910.439660	18.099456	-0.041373	2.453607
214.782336	1902.448587	18.104461	-0.041385	2.449015
214.426194	1894.500235	18.109466	-0.041314	2.444405
214.495597	1886.561582	18.114471	-0.041321	2.439825
214.516296	1878.608092	18.119475	-0.041320	2.435224
214.316071	1870.574508	18.124480	-0.041278	2.430551
214.324503	1862.607839	18.129485	-0.041274	2.425923
214.477071	1854.628437	18.134490	-0.041297	2.421290
214.327708	1846.703956	18.139495	-0.041265	2.416658
214.217246	1838.750357	18.144499	-0.041239	2.412002
214.228834	1830.776505	18.149504	-0.041236	2.407335
214.455636	1822.804337	18.154509	-0.041273	2.402677
214.235905	1814.879412	18.159514	-0.041227	2.398002
214.214314	1806.953945	18.164519	-0.041218	2.393334
213.911407	1798.994601	18.169523	-0.041156	2.388614
213.926348	1791.017057	18.174528	-0.041154	2.383899
214.029578	1783.054495	18.179533	-0.041168	2.379191
213.941455	1775.110717	18.184538	-0.041147	2.374469
214.044642	1767.122972	18.189543	-0.041161	2.369727
213.900757	1759.178915	18.194547	-0.041129	2.364982
213.848789	1751.246064	18.199552	-0.041114	2.360241
213.825675	1743.317981	18.204557	-0.041105	2.355496
213.728492	1735.312889	18.209562	-0.041081	2.350689
213.729874	1727.347217	18.214567	-0.041076	2.345904
213.710097	1719.393920	18.219571	-0.041068	2.341115
213.559594	1711.461729	18.224576	-0.041034	2.336318
213.722235	1703.474947	18.229581	-0.041060	2.331503
213.765776	1695.503772	18.234586	-0.041063	2.326679
213.568065	1687.590218	18.239591	-0.041021	2.321860
213.445971	1679.666477	18.244595	-0.040993	2.317030
213.343506	1671.711100	18.249600	-0.040969	2.312173
213.265653	1663.748446	18.254605	-0.040949	2.307303
213.026064	1655.812345	18.259610	-0.040899	2.302426
213.335053	1647.831839	18.264615	-0.040952	2.297557
213.268924	1639.880306	18.269619	-0.040934	2.292664
213.172825	1631.913963	18.274624	-0.040911	2.287748
212.990153	1624.003510	18.279629	-0.040872	2.282849
212.962541	1616.054451	18.284634	-0.040862	2.277930
213.064836	1608.066875	18.289639	-0.040876	2.272986
212.947028	1600.064090	18.294643	-0.040849	2.268004
212.876788	1592.119437	18.299648	-0.040831	2.263050
213.093471	1584.167851	18.304653	-0.040866	2.258107
212.895098	1576.233654	18.309658	-0.040824	2.253127
213.050295	1568.259168	18.314663	-0.040847	2.248142
212.875122	1560.350808	18.319667	-0.040810	2.243159
212.802351	1552.414624	18.324672	-0.040791	2.238156
212.611321	1544.504607	18.329677	-0.040750	2.233147
212.728926	1536.502911	18.334682	-0.040767	2.228097
212.756526	1528.557955	18.339687	-0.040767	2.223063
212.610874	1520.639584	18.344691	-0.040735	2.218019
212.494056	1512.701955	18.349696	-0.040708	2.212954
212.575538	1504.740228	18.354701	-0.040718	2.207880
212.571919	1496.781189	18.359706	-0.040712	2.202788
212.475410	1488.875541	18.364711	-0.040689	2.197711
212.576406	1480.907646	18.369715	-0.040703	2.192599
212.451276	1472.930717	18.374720	-0.040675	2.187449
212.454182	1465.004720	18.379725	-0.040670	2.182331
212.366629	1457.062922	18.384730	-0.040649	2.177183
212.566849	1449.106735	18.389735	-0.040681	2.172040
212.201843	1441.198145	18.394739	-0.040608	2.166863
212.088118	1433.271208	18.399744	-0.040581	2.161685
212.256658	1425.324471	18.404749	-0.040608	2.156508
212.004180	1417.388059	18.409754	-0.040556	2.151286
211.845536	1409.465253	18.414759	-0.040521	2.146069
212.023716	1401.500038	18.419763	-0.040549	2.140843
211.902050	1393.570213	18.424768	-0.040521	2.135600
211.760851	1385.644593	18.429773	-0.040490	2.130344
211.720592	1377.682240	18.434778	-0.040477	2.125061
211.940128	1369.738858	18.439783	-0.040513	2.119801
211.781737	1361.833499	18.444787	-0.040478	2.114518
211.669631	1353.818325	18.449792	-0.040452	2.109153
211.745565	1345.873690	18.454797	-0.040461	2.103839
211.722227	1337.960873	18.459802	-0.040452	2.098524
211.336503	1330.088468	18.464807	-0.040375	2.093187
211.369559	1322.122694	18.469811	-0.040376	2.087814
211.454439	1314.170763	18.474816	-0.040387	2.082442
211.381740	1306.273931	18.479821	-0.040368	2.077077
211.317987	1298.324714	18.484826	-0.040351	2.071664
211.233515	1290.397038	18.489831	-0.040330	2.066250
211.151821	1282.472677	18.494835	-0.040310	2.060824
211.214021	1274.529971	18.499840	-0.040316	2.055385
211.289880	1266.588070	18.504845	-0.040325	2.049934
210.990153	1258.689082	18.509850	-0.040265	2.044460
211.035431	1250.779483	18.514855	-0.040268	2.038999
211.030586	1242.844845	18.519859	-0.040262	2.033500
210.965464	1234.879048	18.524864	-0.040245	2.027959
210.868822	1226.966550	18.529869	-0.040222	2.022437
210.679298	1219.056632	18.534874	-0.040181	2.016892
210.931083	1211.091079	18.539879	-0.040223	2.011338
210.862958	1203.167386	18.544883	-0.040205	2.005765
210.568805	1195.285097	18.549888	-0.040145	2.000181
210.603084	1187.374272	18.554893	-0.040147	1.994597
210.623138	1179.417905	18.559898	-0.040145	1.988963
210.525496	1171.510555	18.564903	-0.040122	1.983335
210.438204	1163.606433	18.569907	-0.040101	1.977695
210.529881	1155.658482	18.574912	-0.040113	1.972027
210.426635	1147.754143	18.579917	-0.040088	1.966352
210.306553	1139.843308	18.584922	-0.040061	1.960655
210.267167	1131.941933	18.589927	-0.040048	1.954956
210.223013	1123.965977	18.594931	-0.040035	1.949186
210.024057	1116.056246	18.599936	-0.039993	1.943430
210.206402	1108.124739	18.604941	-0.040022	1.937684
210.093197	1100.213851	18.609946	-0.039996	1.931902
210.062427	1092.283806	18.614951	-0.039985	1.926098
209.989904	1084.403929	18.619955	-0.039966	1.920309
210.065243	1076.475717	18.624960	-0.039975	1.914483
210.067642	1068.556397	18.629965	-0.039970	1.908638
209.796444	1060.672660	18.634970	-0.039915	1.902771
209.790475	1052.767526	18.639975	-0.039909	1.896899
209.861528	1044.832669	18.644979	-0.039917	1.890996
209.699812	1036.930791	18.649984	-0.039882	1.885072
209.980488	1029.008096	18.654989	-0.039929	1.879164
209.856368	1021.112912	18.659994	-0.039901	1.873213
209.730334	1013.203520	18.664999	-0.039872	1.867231
209.575226	1005.311019	18.670003	-0.039838	1.861239
209.618447	997.393762	18.675008	-0.039841	1.855233
209.596499	989.495488	18.680013	-0.039832	1.849213
209.223791	981.631875	18.685018	-0.039757	1.843159
209.231764	973.736711	18.690023	-0.039754	1.837106
209.169075	965.831802	18.695027	-0.039737	1.831017
209.014395	957.925582	18.700032	-0.039703	1.824896
208.959240	950.053575	18.705037	-0.039688	1.818792
209.076906	942.124566	18.710042	-0.039705	1.812645
208.992613	934.231746	18.715047	-0.039684	1.806480
208.913656	926.348744	18.720051	-0.039664	1.800303
208.983763	918.437176	18.725056	-0.039672	1.794099
209.044082	910.481594	18.730061	-0.039678	1.787839
208.822705	902.615279	18.735066	-0.039632	1.781592
208.810690	894.742180	18.740071	-0.039624	1.775344
208.669433	886.866985	18.745075	-0.039593	1.769056
208.440407	878.992999	18.750080	-0.039545	1.762736
208.424371	871.123300	18.755085	-0.039537	1.756423
208.423632	863.209773	18.760090	-0.039532	1.750054
208.237442	855.354029	18.765095	-0.039492	1.743685
208.310695	847.464168	18.770099	-0.039501	1.737297
208.384141	839.549367	18.775104	-0.039510	1.730866
208.419149	831.665699	18.780109	-0.039511	1.724432
208.304060	823.810268	18.785114	-0.039485	1.717977
208.291597	815.922821	18.790119	-0.039477	1.711484
208.284302	808.029929	18.795123	-0.039471	1.704963
207.965717	800.200721	18.800128	-0.039406	1.698430
208.001684	792.316488	18.805133	-0.039408	1.691871
207.768587	784.449000	18.810138	-0.039359	1.685266
207.766017	776.594400	18.815143	-0.039354	1.678676
207.697712	768.729777	18.820147	-0.039336	1.672042
207.741119	760.830550	18.825152	-0.039339	1.665368
207.729799	752.983143	18.830157	-0.039332	1.658704
207.574522	745.127819	18.835162	-0.039298	1.651987
207.497197	737.257722	18.840167	-0.039279	1.645240
207.516969	729.412045	18.845171	-0.039277	1.638499
207.435515	721.520153	18.850176	-0.039257	1.631677
207.508485	713.617716	18.855181	-0.039265	1.624838
207.500598	705.762781	18.860186	-0.039259	1.618001
207.380644	697.931327	18.865191	-0.039232	1.611139
207.355899	690.079858	18.870195	-0.039222	1.604244
207.228316	682.253886	18.875200	-0.039193	1.597327
207.268075	674.393789	18.880205	-0.039195	1.590374
207.138509	666.554236	18.885210	-0.039166	1.583384
207.230686	658.710646	18.890215	-0.039178	1.576391
207.195510	650.864086	18.895219	-0.039167	1.569346
206.824750	643.076371	18.900224	-0.039093	1.562274
206.825528	635.249681	18.905229	-0.039088	1.555188
206.813179	627.374571	18.910234	-0.039080	1.548024
206.686971	619.552270	18.915239	-0.039052	1.540858
206.685799	611.721173	18.920243	-0.039047	1.533669
206.552084	603.880381	18.925248	-0.039017	1.526417
206.665355	596.058056	18.930253	-0.039033	1.519185
206.447885	588.265445	18.935258	-0.038987	1.511896
206.438815	580.430476	18.940263	-0.038981	1.504564
206.355952	572.626955	18.945267	-0.038960	1.497214
206.237297	564.794770	18.950272	-0.038933	1.489795
206.198704	556.996571	18.955277	-0.038921	1.482383
206.304749	549.165156	18.960282	-0.038935	1.474926
206.164374	541.322498	18.965287	-0.038904	1.467380
206.314054	533.494394	18.970291	-0.038927	1.459856
206.182314	525.710716	18.975296	-0.038898	1.452291
206.144986	517.917746	18.980301	-0.038886	1.444693
206.055153	510.140510	18.985306	-0.038864	1.437061
205.797181	502.378105	18.990311	-0.038811	1.429376
205.981249	494.549403	18.995315	-0.038840	1.421655
205.858506	486.781248	19.000320	-0.038812	1.413903
205.833837	478.994238	19.005325	-0.038803	1.406105
205.459585	471.275963	19.010330	-0.038728	1.398274
205.490021	463.467531	19.015335	-0.038729	1.390376
205.313956	455.709169	19.020339	-0.038691	1.382449
205.399772	447.908976	19.025344	-0.038702	1.374478
205.502459	440.120444	19.030349	-0.038716	1.366475
205.407940	432.375883	19.035354	-0.038693	1.358436
205.252249	424.634935	19.040359	-0.038659	1.350343
205.276511	416.872690	19.045363	-0.038659	1.342210
205.031942	409.154030	19.050368	-0.038608	1.334027
204.946428	401.404307	19.055373	-0.038587	1.325787
204.878344	393.678528	19.060378	-0.038570	1.317525
204.735326	385.842209	19.065383	-0.038538	1.309079
204.611208	378.100233	19.070387	-0.038510	1.300683
204.604156	370.369559	19.075392	-0.038504	1.292266
204.817930	362.612997	19.080397	-0.038539	1.283806
204.416449	354.964743	19.085402	-0.038459	1.275296
204.151340	347.280220	19.090407	-0.038405	1.266713
204.453166	339.527231	19.095411	-0.038456	1.258102
204.230829	331.849346	19.100416	-0.038409	1.249417
204.244174	324.159293	19.105421	-0.038407	1.240703
204.043171	316.486492	19.110426	-0.038365	1.231905
203.939811	308.790500	19.115431	-0.038340	1.223036
203.856802	301.122055	19.120435	-0.038320	1.214138
203.871193	293.425467	19.125440	-0.038318	1.205161
203.848256	285.775934	19.130445	-0.038309	1.196164
203.654727	278.123429	19.135450	-0.038268	1.187061
203.371632	270.513991	19.140455	-0.038210	1.177921
203.315088	262.859234	19.145459	-0.038195	1.168702
203.096044	255.243341	19.150464	-0.038149	1.159422
202.896110	247.612900	19.155469	-0.038107	1.150054
202.403229	240.022957	19.160474	-0.038010	1.140597
202.512883	232.365748	19.165479	-0.038026	1.131105
202.275107	224.779720	19.170483	-0.037976	1.121548
201.866653	217.226483	19.175488	-0.037895	1.111912
201.379937	209.686580	19.180493	-0.037800	1.102193
200.873454	202.150455	19.185498	-0.037701	1.092386
200.652232	194.576704	19.190503	-0.037655	1.082506
200.442593	187.024474	19.195507	-0.037611	1.072566
199.818520	179.517901	19.200512	-0.037490	1.062498
199.307165	172.022732	19.205517	-0.037390	1.052375
199.031610	164.485753	19.210522	-0.037334	1.042152
198.575759	157.001007	19.215527	-0.037244	1.031856
198.076425	149.529267	19.220531	-0.037146	1.021464
197.465001	142.080249	19.225536	-0.037028	1.010969
197.254462	134.583225	19.230541	-0.036984	1.000395
196.728767	127.120560	19.235546	-0.036881	0.989678
196.109496	119.694281	19.240551	-0.036761	0.978872
195.775766	112.247603	19.245555	-0.036694	0.967989
195.215396	104.852851	19.250560	-0.036585	0.956999
194.604834	97.479152	19.255565	-0.036466	0.945900
193.920393	90.131817	19.260570	-0.036334	0.934689
193.687289	82.719387	19.265575	-0.036286	0.923363
193.367459	75.354688	19.270579	-0.036222	0.911947
192.559770	68.070310	19.275584	-0.036067	0.900377
192.208862	60.965644	19.280589	-0.035997	0.889069