Fri Mar 12 14:07:31 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.350125	0.020767	0.000000	0.000032	0.721294

0.119745	0.138126	0.005005	0.000075	0.721445
0.286860	0.105001	0.010010	0.000043	0.721438
0.195737	0.123338	0.015014	0.000060	0.721442
0.250956	0.039090	0.020019	0.000050	0.721296
0.313933	-0.059897	0.025024	0.000038	0.721123
0.635048	-0.112667	0.030029	-0.000021	0.721132
0.433362	-0.081467	0.035034	0.000016	0.721123
0.381523	-0.070443	0.040038	0.000026	0.721127
0.457643	-0.081849	0.045043	0.000012	0.721131
0.238316	-0.047785	0.050048	0.000052	0.721121
0.359462	-0.066097	0.055053	0.000030	0.721128
0.292679	-0.054833	0.060058	0.000042	0.721126
0.228090	-0.044356	0.065062	0.000054	0.721124
0.288020	-0.051370	0.070067	0.000043	0.721132
0.177235	-0.037547	0.075072	0.000064	0.721120
0.412535	-0.074799	0.080077	0.000020	0.721129
0.316507	-0.128868	0.085082	0.000038	0.720989
0.244065	-0.171536	0.090086	0.000051	0.720880
0.188470	-0.158931	0.095091	0.000061	0.720886
0.321237	-0.187922	0.100096	0.000037	0.720875
0.332781	-0.186202	0.105101	0.000034	0.720883
0.229887	-0.168229	0.110106	0.000054	0.720882
0.310785	-0.183501	0.115110	0.000038	0.720880
0.374367	-0.357962	0.120115	0.000027	0.720559
0.190295	-0.335008	0.125120	0.000061	0.720540
0.442952	-0.376902	0.130125	0.000014	0.720546
0.495009	-0.387592	0.135130	0.000004	0.720543
0.469512	-0.402590	0.140134	0.000009	0.720505
0.491002	-0.545179	0.145139	0.000005	0.720232
0.219848	-0.501560	0.150144	0.000055	0.720223
0.362247	-0.521721	0.155149	0.000029	0.720233
0.216971	-0.499330	0.160154	0.000056	0.720226
0.233018	-0.659275	0.165158	0.000053	0.719917
0.239431	-0.666234	0.170163	0.000052	0.719905
0.199658	-0.663263	0.175168	0.000059	0.719897
0.188051	-0.683489	0.180173	0.000061	0.719854
0.079750	-0.790801	0.185178	0.000081	0.719604
0.253369	-0.821437	0.190182	0.000049	0.719605
0.204402	-0.811363	0.195187	0.000058	0.719607
0.171171	-0.931723	0.200192	0.000064	0.719359
0.323796	-0.999071	0.205197	0.000036	0.719279
0.334104	-1.003393	0.210202	0.000034	0.719275
0.230063	-1.088335	0.215206	0.000053	0.719071
0.145495	-1.123748	0.220211	0.000069	0.718971
0.184048	-1.135671	0.225216	0.000062	0.718961
0.273105	-1.265360	0.230221	0.000045	0.718737
0.187782	-1.294961	0.235226	0.000061	0.718648
0.195407	-1.301729	0.240230	0.000060	0.718638
0.121470	-1.427475	0.245235	0.000074	0.718363
0.009607	-1.413592	0.250240	0.000094	0.718352
0.088605	-1.492116	0.255245	0.000080	0.718224
-0.098881	-1.560186	0.260250	0.000115	0.718024
-0.014299	-1.576152	0.265254	0.000099	0.718022
-0.236719	-1.670040	0.270259	0.000140	0.717759
-0.345006	-1.677520	0.275264	0.000160	0.717706
-0.167619	-1.766918	0.280269	0.000127	0.717592
-0.186894	-1.869041	0.285274	0.000131	0.717383
-0.198161	-1.869435	0.290278	0.000133	0.717378
-0.062205	-2.037571	0.295283	0.000108	0.717094
-0.091812	-2.036906	0.300288	0.000113	0.717085
-0.320715	-2.126228	0.305293	0.000156	0.716827
-0.521861	-2.125611	0.310298	0.000193	0.716758
-0.385722	-2.236764	0.315302	0.000168	0.716586
-0.451765	-2.289018	0.320307	0.000180	0.716459
-0.762182	-2.300371	0.325312	0.000238	0.716327
-0.711213	-2.404260	0.330317	0.000229	0.716139
-0.893273	-2.400112	0.335322	0.000263	0.716083
-2.942137	-2.136052	0.340326	0.000644	0.715884
-2.564606	-2.199675	0.345331	0.000574	0.715891
-3.869149	-2.018950	0.350336	0.000816	0.715788
-4.258216	-2.069686	0.355341	0.000889	0.715551
-3.770259	-2.156881	0.360346	0.000798	0.715550
-4.690997	-1.993757	0.365350	0.000969	0.715548
-4.595962	-2.136160	0.370355	0.000952	0.715300
-5.269276	-2.051778	0.375360	0.001077	0.715229
-5.156220	-2.067702	0.380365	0.001056	0.715238
-4.941460	-2.106583	0.385370	0.001016	0.715236
-5.955042	-2.083882	0.390374	0.001205	0.714923
-5.960845	-2.086696	0.395379	0.001206	0.714916
-6.260399	-2.038121	0.400384	0.001261	0.714906
-6.036972	-2.074103	0.405389	0.001220	0.714914
-5.974839	-2.165785	0.410394	0.001208	0.714754
-7.171499	-2.026780	0.415398	0.001431	0.714607
-6.466511	-2.148518	0.420403	0.001300	0.714615
-6.802008	-2.093852	0.425408	0.001362	0.714604
-6.864097	-2.080071	0.430413	0.001374	0.714610
-7.313997	-2.166560	0.435418	0.001457	0.714279
-7.861063	-2.069285	0.440422	0.001559	0.714279
-7.872019	-2.064105	0.445427	0.001561	0.714285
-8.038385	-2.038820	0.450432	0.001592	0.714277
-7.980867	-2.045171	0.455437	0.001581	0.714284
-8.048675	-2.138848	0.460442	0.001594	0.714074
-9.022197	-2.016578	0.465446	0.001775	0.713973
-8.869045	-2.039851	0.470451	0.001747	0.713981
-8.699454	-2.077011	0.475456	0.001715	0.713967
-8.730994	-2.066633	0.480461	0.001721	0.713977
-8.698995	-2.073466	0.485466	0.001715	0.713974
-9.353830	-2.110485	0.490470	0.001837	0.713669
-9.276564	-2.127385	0.495475	0.001822	0.713663
-10.025379	-1.998951	0.500480	0.001962	0.713653
-9.696525	-2.053060	0.505485	0.001900	0.713662
-9.811449	-2.035679	0.510490	0.001922	0.713656
-9.879691	-2.025634	0.515494	0.001934	0.713652
-9.671223	-2.168318	0.520499	0.001896	0.713442
-10.594235	-2.043377	0.525504	0.002067	0.713363
-10.366289	-2.082649	0.530509	0.002025	0.713366
-10.376303	-2.082821	0.535514	0.002027	0.713362
-10.722576	-2.022100	0.540518	0.002091	0.713361
-10.173186	-2.116878	0.545523	0.001989	0.713367
-11.133773	-2.071193	0.550528	0.002168	0.713117
-11.918966	-1.975139	0.555533	0.002314	0.713030
-11.375139	-2.073872	0.560538	0.002213	0.713026
-11.605515	-2.034230	0.565542	0.002255	0.713024
-11.764759	-2.002124	0.570547	0.002285	0.713031
-11.677111	-2.021186	0.575552	0.002269	0.713024
-11.209612	-2.099730	0.580557	0.002182	0.713034
-11.791214	-2.104724	0.585562	0.002290	0.712818
-12.821530	-1.974342	0.590566	0.002482	0.712712
-12.090301	-2.099842	0.595571	0.002346	0.712722
-12.660179	-2.003666	0.600576	0.002452	0.712711
-12.586141	-2.013637	0.605581	0.002438	0.712717
-12.182980	-2.087856	0.610586	0.002363	0.712713
-12.299480	-2.067406	0.615590	0.002384	0.712712
-12.619426	-2.134214	0.620595	0.002444	0.712466
-13.729853	-1.976751	0.625600	0.002651	0.712385
-13.462388	-2.021424	0.630605	0.002601	0.712391
-13.419230	-2.029656	0.635610	0.002593	0.712390
-13.820813	-1.961895	0.640614	0.002667	0.712383
-13.236022	-2.061543	0.645619	0.002558	0.712392
-13.471404	-2.024141	0.650624	0.002602	0.712383
-13.821175	-2.008124	0.655629	0.002667	0.712291
-14.063952	-2.064045	0.660634	0.002713	0.712093
-14.169116	-2.046123	0.665638	0.002732	0.712092
-14.572204	-1.971119	0.670643	0.002807	0.712098
-14.753201	-1.943992	0.675648	0.002841	0.712088
-14.115012	-2.053785	0.680653	0.002722	0.712096
-14.461706	-1.992512	0.685658	0.002786	0.712095
-14.733671	-1.947413	0.690662	0.002837	0.712088
-14.484093	-2.125179	0.695667	0.002791	0.711823
-15.443592	-1.986342	0.700672	0.002969	0.711759
-15.517479	-1.969059	0.705677	0.002983	0.711767
-15.070413	-2.050672	0.710682	0.002900	0.711763
-15.502673	-1.975756	0.715686	0.002980	0.711759
-15.432302	-1.983747	0.720691	0.002967	0.711768
-15.385315	-1.996929	0.725696	0.002958	0.711759
-15.227156	-2.098931	0.730701	0.002929	0.711611
-16.199243	-2.003155	0.735706	0.003110	0.711457
-16.370874	-1.974247	0.740710	0.003141	0.711454
-15.898623	-2.055654	0.745715	0.003054	0.711459
-16.146420	-2.014505	0.750720	0.003100	0.711453
-16.205088	-2.000366	0.755725	0.003111	0.711461
-16.244826	-1.995156	0.760730	0.003118	0.711457
-16.331587	-2.039359	0.765734	0.003134	0.711338
-17.058260	-2.006602	0.770739	0.003269	0.711145
-17.212398	-1.984096	0.775744	0.003298	0.711135
-17.067757	-2.005757	0.780749	0.003271	0.711144
-17.201923	-1.981843	0.785754	0.003296	0.711144
-17.552101	-1.921586	0.790758	0.003361	0.711140
-17.012139	-2.013537	0.795763	0.003261	0.711148
-16.976292	-2.026098	0.800768	0.003254	0.711136
-17.645477	-2.035968	0.805773	0.003378	0.710878
-17.696174	-2.029625	0.810778	0.003388	0.710873
-17.718290	-2.029158	0.815782	0.003392	0.710866
-17.404178	-2.078753	0.820787	0.003333	0.710879
-17.969342	-1.982452	0.825792	0.003439	0.710870
-17.786554	-2.011031	0.830797	0.003404	0.710878
-17.695937	-2.105437	0.835802	0.003388	0.710722
-19.376393	-1.899649	0.840806	0.003700	0.710535
-18.615038	-2.033132	0.845811	0.003559	0.710539
-18.836709	-1.996357	0.850816	0.003600	0.710534
-19.128541	-1.940672	0.855821	0.003654	0.710541
-18.931429	-1.975714	0.860826	0.003617	0.710542
-18.800268	-2.002637	0.865830	0.003593	0.710535
-18.906715	-1.990617	0.870835	0.003613	0.710521
-19.739406	-1.994272	0.875840	0.003768	0.710217
-19.714193	-1.996298	0.880845	0.003763	0.710222
-19.667711	-2.004614	0.885850	0.003754	0.710222
-19.986875	-1.950386	0.890854	0.003814	0.710217
-19.396054	-2.049341	0.895859	0.003704	0.710230
-19.613808	-2.015607	0.900864	0.003744	0.710220
-19.721103	-1.995191	0.905869	0.003764	0.710222
-20.372174	-2.031650	0.910874	0.003885	0.709918
-20.626075	-1.998771	0.915878	0.003933	0.709893
-20.354198	-2.041947	0.920883	0.003882	0.709904
-20.628075	-1.999066	0.925888	0.003933	0.709892
-20.561235	-2.007731	0.930893	0.003920	0.709898
-20.296594	-2.055239	0.935898	0.003871	0.709898
-20.807653	-1.966809	0.940902	0.003966	0.709892
-21.132913	-2.045023	0.945907	0.004027	0.709620
-21.367403	-2.018172	0.950912	0.004070	0.709590
-21.471974	-1.995744	0.955917	0.004090	0.709598
-21.514480	-1.986368	0.960922	0.004098	0.709602
-21.436234	-2.003818	0.965926	0.004083	0.709595
-21.267081	-2.030719	0.970931	0.004052	0.709601
-21.723950	-1.954090	0.975936	0.004137	0.709592
-22.031495	-2.047764	0.980941	0.004194	0.709295
-22.186585	-2.034043	0.985946	0.004223	0.709267
-22.682619	-1.948636	0.990950	0.004315	0.709261
-22.246977	-2.020615	0.995955	0.004234	0.709272
-22.086957	-2.055290	1.000960	0.004204	0.709260
-22.373017	-2.000908	1.005965	0.004257	0.709267
-22.352438	-2.003711	1.010970	0.004253	0.709269
-22.935942	-2.044349	1.015974	0.004362	0.708979
-23.005586	-2.040820	1.020979	0.004375	0.708962
-23.618432	-1.935683	1.025984	0.004489	0.708954
-23.411234	-1.969836	1.030989	0.004450	0.708959
-22.933880	-2.054127	1.035994	0.004362	0.708961
-23.493891	-1.956184	1.040998	0.004466	0.708957
-23.280117	-1.990690	1.046003	0.004426	0.708964
-23.475518	-2.060523	1.051008	0.004462	0.708755
-24.257758	-1.977142	1.056013	0.004608	0.708643
-24.064610	-2.011014	1.061018	0.004572	0.708644
-24.098465	-2.009066	1.066022	0.004578	0.708636
-23.609829	-2.090771	1.071027	0.004487	0.708647
-24.130122	-2.002554	1.076032	0.004584	0.708638
-23.996390	-2.025681	1.081037	0.004559	0.708639
-24.212346	-2.120237	1.086042	0.004599	0.708373
-25.107234	-1.971756	1.091046	0.004766	0.708351
-25.130780	-1.964242	1.096051	0.004770	0.708357
-24.662559	-2.051467	1.101056	0.004683	0.708350
-24.748608	-2.034566	1.106061	0.004699	0.708353
-25.077846	-1.975567	1.111066	0.004760	0.708354
-25.197776	-1.963105	1.116070	0.004782	0.708336
-25.234908	-2.113846	1.121075	0.004789	0.708021
-25.817038	-2.015650	1.126080	0.004898	0.708010
-26.237017	-1.938140	1.131085	0.004976	0.708015
-25.425569	-2.081401	1.136090	0.004825	0.708018
-25.685274	-2.037131	1.141094	0.004873	0.708014
-26.010265	-1.975111	1.146099	0.004934	0.708022
-25.856545	-2.024033	1.151104	0.004905	0.707979
-26.525140	-2.042526	1.156109	0.005029	0.707703
-26.631968	-2.022623	1.161114	0.005049	0.707705
-27.019237	-1.957520	1.166118	0.005121	0.707697
-26.094181	-2.118154	1.171123	0.004949	0.707706
-26.742556	-2.007212	1.176128	0.005070	0.707696
-27.106939	-1.940546	1.181133	0.005138	0.707700
-26.505093	-2.071978	1.186138	0.005026	0.707652
-27.609012	-2.014987	1.191142	0.005231	0.707371
-27.588385	-2.012823	1.196147	0.005227	0.707383
-27.601457	-2.014027	1.201152	0.005230	0.707376
-27.318350	-2.061954	1.206157	0.005177	0.707381
-27.576961	-2.014958	1.211162	0.005225	0.707383
-27.831766	-1.974824	1.216166	0.005272	0.707373
-27.273644	-2.092503	1.221171	0.005168	0.707336
-28.353378	-2.026146	1.226176	0.005369	0.707083
-28.755029	-1.952991	1.231181	0.005444	0.707086
-28.609027	-1.979476	1.236186	0.005417	0.707085
-28.390756	-2.023508	1.241190	0.005376	0.707075
-28.204557	-2.050704	1.246195	0.005342	0.707087
-28.518920	-1.998551	1.251200	0.005400	0.707080
-28.237551	-2.065688	1.256205	0.005348	0.707045
-29.048648	-2.063830	1.261210	0.005499	0.706759
-29.512564	-1.985287	1.266214	0.005585	0.706751
-29.129196	-2.048293	1.271219	0.005514	0.706761
-29.187691	-2.043534	1.276224	0.005524	0.706750
-29.652306	-1.960942	1.281229	0.005611	0.706750
-29.669525	-1.957167	1.286234	0.005614	0.706751
-29.287681	-2.028218	1.291238	0.005543	0.706745
-29.798199	-2.078279	1.296243	0.005638	0.706462
-30.323320	-1.995660	1.301248	0.005736	0.706440
-30.225036	-2.011853	1.306253	0.005717	0.706443
-30.096107	-2.033431	1.311258	0.005693	0.706446
-30.837614	-1.904275	1.316262	0.005831	0.706440
-30.209055	-2.010721	1.321267	0.005714	0.706451
-30.126492	-2.029006	1.326272	0.005699	0.706444
-30.938459	-2.012492	1.331277	0.005850	0.706186
-31.236607	-1.986943	1.336282	0.005905	0.706131
-30.928042	-2.046018	1.341286	0.005848	0.706123
-31.224410	-1.988251	1.346291	0.005903	0.706133
-31.356045	-1.968157	1.351296	0.005928	0.706126
-31.238888	-1.987327	1.356301	0.005906	0.706129
-30.810637	-2.061953	1.361306	0.005826	0.706133
-31.528307	-2.020232	1.366310	0.005960	0.705960
-32.017404	-1.977787	1.371315	0.006051	0.705870
-31.866610	-2.009630	1.376320	0.006022	0.705860
-32.181492	-1.951396	1.381325	0.006081	0.705864
-32.114299	-1.961893	1.386330	0.006069	0.705867
-32.014136	-1.983235	1.391334	0.006050	0.705860
-31.917345	-1.995904	1.396339	0.006032	0.705869
-32.078313	-2.068984	1.401344	0.006062	0.705665
-33.081000	-1.959129	1.406349	0.006248	0.705526
-32.369588	-2.083384	1.411354	0.006116	0.705532
-33.235369	-1.931404	1.416358	0.006277	0.705527
-33.090912	-1.953775	1.421363	0.006250	0.705534
-32.707877	-2.026512	1.426368	0.006179	0.705525
-32.826833	-2.003244	1.431373	0.006201	0.705529
-32.969328	-2.088484	1.436378	0.006227	0.705306
-33.990556	-1.956557	1.441382	0.006417	0.705206
-33.860907	-1.973383	1.446387	0.006393	0.705218
-33.955299	-1.959418	1.451392	0.006411	0.705213
-33.796328	-1.986395	1.456397	0.006381	0.705215
-33.266933	-2.078633	1.461402	0.006283	0.705220
-34.133714	-1.927128	1.466406	0.006444	0.705214
-33.863389	-2.078158	1.471411	0.006394	0.705007
-34.509526	-2.021562	1.476416	0.006514	0.704889
-34.763126	-1.974678	1.481421	0.006561	0.704892
-34.713501	-1.981775	1.486426	0.006552	0.704896
-35.031005	-1.929390	1.491430	0.006611	0.704887
-34.467181	-2.025792	1.496435	0.006506	0.704896
-34.670913	-1.992760	1.501440	0.006544	0.704889
-34.835630	-2.053980	1.506445	0.006574	0.704707
-35.255497	-2.033743	1.511450	0.006653	0.704597
-35.481993	-1.997734	1.516454	0.006695	0.704588
-35.395529	-2.007642	1.521459	0.006679	0.704599
-35.374165	-2.015822	1.526464	0.006675	0.704591
-35.494189	-1.992753	1.531469	0.006697	0.704594
-35.281050	-2.028769	1.536474	0.006657	0.704598
-35.773661	-2.102779	1.541478	0.006749	0.704272
-35.904571	-2.080170	1.546483	0.006773	0.704271
-36.768730	-1.928228	1.551488	0.006934	0.704266
-36.338868	-2.006059	1.556493	0.006854	0.704264
-35.882671	-2.085140	1.561498	0.006769	0.704269
-36.538249	-1.972514	1.566502	0.006891	0.704260
-36.431921	-2.029288	1.571507	0.006871	0.704184
-37.090285	-2.025545	1.576512	0.006994	0.703955
-37.116968	-2.020046	1.581517	0.006999	0.703956
-37.190597	-2.005210	1.586522	0.007012	0.703960
-37.193694	-2.009218	1.591526	0.007013	0.703951
-36.883690	-2.059529	1.596531	0.006955	0.703961
-37.395413	-1.969489	1.601536	0.007050	0.703959
-37.225894	-2.059026	1.606541	0.007019	0.703839
-37.784577	-2.056246	1.611546	0.007123	0.703644
-38.137057	-1.998733	1.616550	0.007188	0.703633
-38.194126	-1.984066	1.621555	0.007199	0.703642
-38.131495	-1.998321	1.626560	0.007187	0.703636
-38.038571	-2.015579	1.631565	0.007170	0.703635
-37.973187	-2.024638	1.636570	0.007158	0.703640
-38.098756	-2.060145	1.641574	0.007181	0.703523
-38.779747	-2.025959	1.646579	0.007308	0.703347
-38.665173	-2.047193	1.651584	0.007287	0.703346
-39.050049	-1.979881	1.656589	0.007358	0.703343
-38.683435	-2.042765	1.661594	0.007290	0.703348
-38.562611	-2.068439	1.666598	0.007267	0.703340
-38.931271	-1.998914	1.671603	0.007336	0.703348
-38.987442	-2.114450	1.676608	0.007346	0.703094
-39.857885	-2.001139	1.681613	0.007508	0.703010
-39.859666	-1.998381	1.686618	0.007509	0.703015
-39.857939	-2.004247	1.691622	0.007508	0.703003
-39.522987	-2.059442	1.696627	0.007446	0.703013
-39.707181	-2.029454	1.701632	0.007480	0.703007
-39.910403	-1.994489	1.706637	0.007518	0.703004
-39.840229	-2.132295	1.711642	0.007505	0.702751
-40.843744	-1.986039	1.716646	0.007692	0.702685
-40.659742	-2.015519	1.721651	0.007657	0.702692
-40.304907	-2.080481	1.726656	0.007591	0.702689
-40.525343	-2.039355	1.731661	0.007632	0.702693
-40.588879	-2.024853	1.736666	0.007644	0.702699
-40.695062	-2.017850	1.741670	0.007664	0.702675
-40.967358	-2.116075	1.746675	0.007715	0.702378
-41.236623	-2.072343	1.751680	0.007765	0.702370
-41.798885	-1.971349	1.756685	0.007869	0.702371
-41.145479	-2.084413	1.761690	0.007748	0.702378
-41.407156	-2.041879	1.766694	0.007796	0.702370
-41.767639	-1.975165	1.771699	0.007863	0.702375
-41.416087	-2.068728	1.776704	0.007798	0.702313
-42.093960	-2.064841	1.781709	0.007924	0.702076
-41.902878	-2.096823	1.786714	0.007888	0.702081
-42.521725	-1.990291	1.791718	0.008004	0.702073
-41.868614	-2.103230	1.796723	0.007882	0.702080
-41.954485	-2.090266	1.801728	0.007898	0.702075
-42.411855	-2.008243	1.806733	0.007983	0.702076
-42.104003	-2.179771	1.811738	0.007926	0.701841
-43.043151	-2.060907	1.816742	0.008101	0.701742
-43.177353	-2.032612	1.821747	0.008126	0.701751
-42.906610	-2.084047	1.826752	0.008075	0.701745
-42.816426	-2.098772	1.831757	0.008058	0.701748
-42.811739	-2.096207	1.836762	0.008057	0.701755
-43.341823	-2.043760	1.841766	0.008156	0.701670
-43.791964	-2.074349	1.846771	0.008240	0.701445
-43.582140	-2.113956	1.851776	0.008201	0.701441
-44.177096	-2.008514	1.856781	0.008311	0.701440
-43.814866	-2.070864	1.861786	0.008244	0.701444
-43.593231	-2.115007	1.866790	0.008203	0.701435
-44.095840	-2.021251	1.871795	0.008296	0.701443
-44.183962	-2.084790	1.876800	0.008313	0.701283
-44.910771	-2.034534	1.881805	0.008448	0.701122
-44.648391	-2.078542	1.886810	0.008399	0.701128
-45.118529	-1.997513	1.891814	0.008486	0.701122
-45.030202	-2.010368	1.896819	0.008470	0.701128
-44.780538	-2.057079	1.901824	0.008424	0.701124
-45.217786	-1.979063	1.906829	0.008505	0.701124
-44.930436	-2.044711	1.911834	0.008451	0.701095
-45.277923	-2.091697	1.916838	0.008516	0.700874
-45.476439	-2.051129	1.921843	0.008553	0.700885
-45.711134	-2.014472	1.926848	0.008597	0.700875
-45.518854	-2.049371	1.931853	0.008561	0.700873
-45.432039	-2.060532	1.936858	0.008545	0.700882
-45.878783	-1.986446	1.941862	0.008628	0.700871
-45.353215	-2.174643	1.946867	0.008530	0.700680
-46.458357	-2.047718	1.951872	0.008736	0.700537
-46.530344	-2.034605	1.956877	0.008749	0.700538
-46.065912	-2.115304	1.961882	0.008662	0.700542
-46.476717	-2.047353	1.966886	0.008739	0.700532
-46.317138	-2.071146	1.971891	0.008709	0.700541
-46.601172	-2.036159	1.976896	0.008762	0.700510
-47.425499	-2.033226	1.981901	0.008915	0.700217
-47.014109	-2.103583	1.986906	0.008839	0.700224
-47.605839	-2.002247	1.991910	0.008949	0.700215
-47.363893	-2.040770	1.996915	0.008904	0.700225
-47.428974	-2.032772	2.001920	0.008916	0.700217

-47.418224	-2.034755	2.011917	0.008914	0.700217
-48.260999	-2.039044	2.021914	0.009071	0.699904
-48.263743	-2.041547	2.031910	0.009071	0.699898
-48.523021	-1.995759	2.041907	0.009119	0.699897
-48.277459	-2.040079	2.051904	0.009074	0.699896
-48.084997	-2.075045	2.061901	0.009038	0.699895
-48.102928	-2.038711	2.071898	0.009041	0.699962
-47.341951	-2.052397	2.081894	0.008899	0.700210
-47.536447	-2.014618	2.091891	0.008935	0.700217
-47.290264	-2.058432	2.101888	0.008889	0.700217
-47.379024	-2.041743	2.111885	0.008906	0.700219
-47.327595	-2.047512	2.121882	0.008896	0.700226
-47.199216	-2.071551	2.131878	0.008872	0.700224
-47.581813	-2.004195	2.141875	0.008943	0.700222
-47.199844	-2.073457	2.151872	0.008872	0.700220
-46.972573	-1.999319	2.161869	0.008830	0.700452
-46.494068	-2.042929	2.171866	0.008741	0.700537
-46.158278	-2.101333	2.181862	0.008678	0.700540
-46.658314	-2.013731	2.191859	0.008771	0.700537
-46.382932	-2.047175	2.201856	0.008720	0.700569
-45.777498	-2.002345	2.211853	0.008607	0.700879
-45.281840	-2.090181	2.221850	0.008515	0.700880
-45.494244	-2.053103	2.231846	0.008554	0.700879
-45.682706	-2.020949	2.241843	0.008589	0.700876
-44.918349	-2.035680	2.251840	0.008447	0.701122
-45.112340	-1.999764	2.261837	0.008483	0.701125
-44.896229	-2.038598	2.271834	0.008443	0.701125
-44.610730	-2.004019	2.281830	0.008389	0.701298
-43.997326	-2.044180	2.291827	0.008275	0.701438
-43.937634	-2.053809	2.301824	0.008264	0.701440
-44.091474	-2.028024	2.311821	0.008292	0.701437
-43.106879	-2.057281	2.321818	0.008109	0.701733
-43.256355	-2.024088	2.331814	0.008137	0.701747
-43.220081	-2.031703	2.341811	0.008130	0.701745
-43.066485	-1.981326	2.351808	0.008101	0.701902
-42.469801	-2.003679	2.361805	0.007990	0.702072
-42.144238	-2.061100	2.371802	0.007929	0.702074
-42.228948	-2.043936	2.381798	0.007945	0.702078
-41.525128	-2.022671	2.391795	0.007814	0.702375
-41.482783	-2.031601	2.401792	0.007806	0.702372
-41.532540	-2.021635	2.411789	0.007815	0.702374
-40.961856	-2.035228	2.421786	0.007709	0.702553
-40.724461	-2.005808	2.431782	0.007665	0.702698
-40.518377	-2.042967	2.441779	0.007626	0.702697
-40.742100	-1.984074	2.451776	0.007668	0.702736
-39.709855	-2.031937	2.461773	0.007476	0.703011
-39.534520	-2.061872	2.471770	0.007443	0.703014
-39.774110	-2.020843	2.481766	0.007487	0.703011
-39.262621	-2.006610	2.491763	0.007392	0.703224
-38.865109	-2.017704	2.501760	0.007318	0.703344
-38.767017	-2.034562	2.511757	0.007300	0.703346
-38.491131	-2.083623	2.521754	0.007248	0.703346
-38.471169	-1.942660	2.531750	0.007244	0.703638
-38.013840	-2.024379	2.541747	0.007159	0.703638
-38.101299	-2.009665	2.551744	0.007175	0.703636
-37.469222	-1.996178	2.561741	0.007058	0.703891
-36.955490	-2.055831	2.571738	0.006962	0.703955
-36.915900	-2.062877	2.581734	0.006954	0.703955
-37.041129	-2.021163	2.591731	0.006978	0.703995
-36.390504	-2.005447	2.601728	0.006856	0.704260
-36.027809	-2.068896	2.611725	0.006789	0.704263
-36.111070	-2.054078	2.621722	0.006804	0.704263
-35.731219	-2.021134	2.631718	0.006734	0.704466
-35.251061	-2.045023	2.641715	0.006644	0.704591
-35.418203	-2.015949	2.651712	0.006675	0.704589
-35.223767	-2.032178	2.661709	0.006639	0.704627
-34.437012	-2.041920	2.671706	0.006492	0.704890
-34.331182	-2.061435	2.681702	0.006473	0.704888
-34.393246	-2.049077	2.691699	0.006484	0.704891
-34.301275	-1.969838	2.701696	0.006467	0.705084
-33.566753	-2.035985	2.711693	0.006330	0.705214
-33.724804	-2.008340	2.721690	0.006359	0.705214
-33.463756	-2.017712	2.731686	0.006311	0.705288
-32.814794	-2.016815	2.741683	0.006190	0.705523
-32.666669	-2.042782	2.751680	0.006162	0.705524
-32.597870	-2.054529	2.761677	0.006149	0.705525
-32.005662	-2.039315	2.771674	0.006039	0.705769
-31.846735	-2.020774	2.781670	0.006009	0.705863
-31.809902	-2.027871	2.791667	0.006002	0.705862
-32.023122	-1.961793	2.801664	0.006042	0.705919
-31.016999	-2.037240	2.811661	0.005855	0.706128
-31.194419	-2.004629	2.821658	0.005887	0.706130
-30.952871	-2.047170	2.831654	0.005842	0.706131
-30.528607	-1.982889	2.841651	0.005763	0.706412
-30.263215	-2.015522	2.851648	0.005714	0.706442
-30.206907	-2.023991	2.861645	0.005703	0.706445
-29.861155	-1.996303	2.871642	0.005639	0.706625
-29.297834	-2.031070	2.881638	0.005534	0.706757
-29.485411	-1.999061	2.891635	0.005569	0.706754
-29.511971	-1.959255	2.901632	0.005574	0.706825
-28.405568	-2.028680	2.911629	0.005368	0.707081
-28.609804	-1.990667	2.921626	0.005406	0.707085
-28.487937	-2.012844	2.931622	0.005383	0.707084
-28.032413	-1.964214	2.941619	0.005298	0.707345
-27.756629	-1.996223	2.951616	0.005246	0.707379
-27.710598	-2.005506	2.961613	0.005238	0.707377
-27.274187	-1.993187	2.971610	0.005156	0.707558
-26.576006	-2.046128	2.981606	0.005026	0.707702
-27.048870	-1.961130	2.991603	0.005114	0.707703
-26.885958	-1.973751	3.001600	0.005084	0.707736
-26.046427	-1.985406	3.011597	0.004928	0.708013
-26.007818	-1.989390	3.021594	0.004920	0.708019
-25.766235	-2.032359	3.031590	0.004875	0.708019
-25.708406	-1.923696	3.041587	0.004864	0.708258
-25.178634	-1.970879	3.051584	0.004766	0.708353
-25.197495	-1.966646	3.061581	0.004769	0.708355
-25.095721	-1.931064	3.071578	0.004750	0.708462
-24.184504	-2.004780	3.081574	0.004580	0.708640
-24.318538	-1.981269	3.091571	0.004605	0.708639
-24.219189	-2.000407	3.101568	0.004587	0.708637
-23.604937	-1.951263	3.111565	0.004472	0.708955
-23.337040	-1.996186	3.121562	0.004422	0.708960
-23.165975	-2.026974	3.131558	0.004390	0.708960
-23.258051	-1.934225	3.141555	0.004407	0.709113
-22.466144	-1.997521	3.151552	0.004260	0.709269
-22.490494	-1.993364	3.161549	0.004264	0.709268
-22.330156	-2.021692	3.171546	0.004235	0.709269
-21.538914	-2.007415	3.181542	0.004087	0.709580
-21.682520	-1.970674	3.191539	0.004114	0.709602
-21.413203	-2.021119	3.201536	0.004064	0.709598
-21.517284	-1.960863	3.211533	0.004083	0.709681
-20.658767	-2.005782	3.221530	0.003923	0.709897
-20.723591	-1.993669	3.231526	0.003935	0.709899
-20.909128	-1.961685	3.241523	0.003969	0.709897
-20.106552	-1.957336	3.251520	0.003820	0.710191
-19.954925	-1.968310	3.261517	0.003792	0.710223
-19.728523	-2.007744	3.271514	0.003749	0.710225
-19.767661	-1.921159	3.281510	0.003757	0.710385
-19.007774	-1.980390	3.291507	0.003615	0.710537
-18.979986	-1.987050	3.301504	0.003610	0.710534
-19.171559	-1.932160	3.311501	0.003645	0.710575
-17.922322	-2.002711	3.321498	0.003413	0.710879
-17.834397	-2.019110	3.331494	0.003396	0.710878
-18.047533	-1.982486	3.341491	0.003436	0.710875
-17.908058	-1.969979	3.351488	0.003410	0.710950
-17.156118	-2.008965	3.361485	0.003270	0.711140
-17.022566	-2.031890	3.371482	0.003245	0.711141
-17.412329	-1.962382	3.381478	0.003317	0.711142
-16.680199	-1.956911	3.391475	0.003181	0.711413
-16.513997	-1.965749	3.401472	0.003150	0.711455
-16.642816	-1.941958	3.411469	0.003174	0.711456
-16.042389	-1.955909	3.421466	0.003062	0.711642
-15.599554	-1.972877	3.431462	0.002980	0.711766
-15.598035	-1.974663	3.441459	0.002979	0.711763
-15.537682	-1.945812	3.451456	0.002968	0.711842
-14.638235	-1.980478	3.461453	0.002800	0.712092
-14.569328	-1.991645	3.471450	0.002787	0.712095
-14.587951	-1.986588	3.481446	0.002791	0.712098
-14.359160	-1.921202	3.491443	0.002748	0.712310
-13.695817	-1.998034	3.501440	0.002625	0.712392
-14.023441	-1.940429	3.511437	0.002685	0.712391
-13.489672	-1.985613	3.521434	0.002586	0.712491
-12.950942	-1.968245	3.531430	0.002486	0.712716
-13.033667	-1.953610	3.541427	0.002501	0.712716
-13.158771	-1.931973	3.551424	0.002524	0.712715
-12.270294	-1.944919	3.561421	0.002359	0.713005
-11.896946	-1.997328	3.571418	0.002289	0.713033
-12.018327	-1.976120	3.581414	0.002312	0.713032
-11.950668	-1.938008	3.591411	0.002299	0.713132
-11.027391	-1.986687	3.601408	0.002127	0.713363
-11.128733	-1.967124	3.611405	0.002146	0.713366
-11.063186	-1.979654	3.621402	0.002134	0.713364
-10.710165	-1.937261	3.631398	0.002068	0.713574
-10.053796	-2.014847	3.641395	0.001945	0.713652
-10.296589	-1.971615	3.651392	0.001991	0.713652
-10.043892	-1.997716	3.661389	0.001943	0.713690
-9.061100	-2.031374	3.671386	0.001760	0.713971
-8.909502	-2.059549	3.681382	0.001732	0.713969
-9.059669	-2.032192	3.691379	0.001760	0.713970
-9.210771	-1.981307	3.701376	0.001788	0.714018
-8.229926	-2.024776	3.711373	0.001605	0.714279
-8.106310	-2.047022	3.721370	0.001582	0.714279
-8.064637	-2.053724	3.731366	0.001575	0.714280
-8.082769	-1.994529	3.741363	0.001578	0.714392
-7.344825	-2.017871	3.751360	0.001440	0.714606
-7.174147	-2.046533	3.761357	0.001409	0.714610
-7.137954	-2.052652	3.771354	0.001402	0.714611
-6.911120	-2.005141	3.781350	0.001359	0.714785
-6.187032	-2.071712	3.791347	0.001225	0.714909
-6.513362	-2.013287	3.801344	0.001285	0.714910
-6.259624	-2.058280	3.811341	0.001238	0.714911
-5.650217	-2.019989	3.821338	0.001124	0.715202
-5.340160	-2.057797	3.831334	0.001067	0.715237
-5.324950	-2.062345	3.841331	0.001064	0.715233
-5.344930	-2.039663	3.851328	0.001067	0.715271
-4.489449	-2.052144	3.861325	0.000908	0.715549
-4.270051	-2.092634	3.871322	0.000867	0.715546
-4.506490	-2.049121	3.881318	0.000911	0.715549
-4.337926	-2.007940	3.891315	0.000879	0.715691
-3.599266	-2.040578	3.901312	0.000742	0.715887
-3.558323	-2.048174	3.911309	0.000734	0.715886
-3.484307	-2.061700	3.921306	0.000720	0.715886
-2.964888	-2.064562	3.931302	0.000624	0.716064
-2.728679	-2.069069	3.941299	0.000580	0.716138
-2.760570	-2.066215	3.951296	0.000585	0.716133
-2.788824	-2.031106	3.961293	0.000591	0.716192
-2.120407	-2.020171	3.971290	0.000466	0.716450
-1.669396	-2.100023	3.981286	0.000382	0.716451
-1.856724	-2.067824	3.991283	0.000417	0.716449
-1.665174	-1.989662	4.001280	0.000381	0.716671
-1.291680	-2.014956	4.011277	0.000311	0.716753
-1.459578	-1.984916	4.021274	0.000343	0.716753
-1.618137	-1.833755	4.031270	0.000372	0.716997
-1.629740	-1.786089	4.041267	0.000374	0.717087
-1.306482	-1.782653	4.051264	0.000314	0.717208
-0.877072	-1.773493	4.061261	0.000234	0.717377
-0.789973	-1.782591	4.071258	0.000217	0.717390
-0.943885	-1.596840	4.081254	0.000246	0.717703
-0.962298	-1.587893	4.091251	0.000249	0.717715
-1.408717	-1.356776	4.101248	0.000332	0.718014
-0.909133	-1.384782	4.111245	0.000239	0.718135
-0.738247	-1.305518	4.121242	0.000207	0.718352
-0.549629	-1.239314	4.131238	0.000172	0.718549
-0.561161	-1.183206	4.141235	0.000174	0.718656
-0.596908	-1.022026	4.151232	0.000180	0.718961
-0.437642	-0.967624	4.161229	0.000151	0.719125
-0.871850	-0.786463	4.171226	0.000231	0.719330
-0.444802	-0.724211	4.181222	0.000152	0.719603
-0.301561	-0.622385	4.191219	0.000125	0.719854
-0.152480	-0.537144	4.201216	0.000097	0.720074
-0.324448	-0.385647	4.211213	0.000129	0.720312
-0.154473	-0.282818	4.221210	0.000097	0.720574
-0.136605	-0.131882	4.231206	0.000094	0.720878
-0.075690	-0.023232	4.241203	0.000082	0.721113
-0.181758	0.136892	4.251200	0.000102	0.721391
0.000000	0.257351	4.261197	0.000068	0.721692

-0.028032	0.889698	4.266202	0.000073	0.722924
0.242837	2.109571	4.271206	0.000021	0.725408
0.508004	3.912610	4.276211	-0.000029	0.729017
0.722192	6.281636	4.281216	-0.000071	0.733686
1.040053	9.145583	4.286221	-0.000132	0.739311
1.235098	12.501210	4.291226	-0.000170	0.745787
1.658589	16.285731	4.296230	-0.000252	0.753092
2.051220	20.465310	4.301235	-0.000328	0.761054
2.472589	25.048552	4.306240	-0.000409	0.769686
2.919944	29.996699	4.311245	-0.000496	0.778896
3.068347	35.338720	4.316250	-0.000527	0.788612
3.582469	40.937832	4.321254	-0.000626	0.798780
4.349262	46.785427	4.326259	-0.000773	0.809335
5.562392	52.862690	4.331264	-0.001003	0.820287
5.942143	59.356112	4.336269	-0.001078	0.831553
6.374926	66.060284	4.341274	-0.001163	0.843039
7.111147	72.946167	4.346278	-0.001304	0.854760
7.604442	80.063766	4.351283	-0.001401	0.866631
8.468810	87.322493	4.356288	-0.001567	0.878675
9.017670	94.807420	4.361293	-0.001674	0.890828
9.432291	102.464940	4.366298	-0.001756	0.903050
9.827378	110.284289	4.371302	-0.001835	0.915355
12.266327	117.845771	4.376307	-0.002294	0.927649
15.930591	125.410028	4.381312	-0.002981	0.940109
15.957042	133.706290	4.386317	-0.002991	0.952547
16.150700	142.037334	4.391322	-0.003033	0.964918
16.797570	150.378603	4.396326	-0.003159	0.977262
17.119710	158.844900	4.401331	-0.003224	0.989550
17.922150	167.273008	4.406336	-0.003379	1.001751
18.712181	175.743198	4.411341	-0.003532	1.013861
19.503171	184.239787	4.416346	-0.003685	1.025864
20.072363	192.825248	4.421350	-0.003796	1.037796
20.833823	201.381252	4.426355	-0.003944	1.049598
21.633908	209.968558	4.431360	-0.004098	1.061319
22.111836	218.646198	4.436365	-0.004193	1.072957
22.665445	227.287420	4.441370	-0.004302	1.084439
23.416266	235.927337	4.446374	-0.004447	1.095843
23.959448	244.584355	4.451379	-0.004554	1.107105
24.410159	253.276051	4.456384	-0.004644	1.118278
25.373359	261.866735	4.461389	-0.004829	1.129323
26.183353	270.479505	4.466394	-0.004985	1.140256
26.795397	279.167361	4.471398	-0.005105	1.151135
27.172066	287.836441	4.476403	-0.005181	1.161839
28.012428	296.427273	4.481408	-0.005343	1.172448
28.717286	305.025483	4.486413	-0.005480	1.182941
29.485037	313.612248	4.491418	-0.005628	1.193341
30.168948	322.202434	4.496422	-0.005761	1.203638
30.714462	330.803283	4.501427	-0.005868	1.213833
31.420983	339.363483	4.506432	-0.006005	1.223926
32.121099	347.936415	4.511437	-0.006141	1.233951
32.780956	356.457559	4.516442	-0.006270	1.243827
33.305748	365.017636	4.521446	-0.006373	1.253643
33.935764	373.514819	4.526451	-0.006496	1.263332
34.491628	382.048684	4.531456	-0.006605	1.272975
34.945150	390.560537	4.536461	-0.006695	1.282500
35.618477	399.024556	4.541466	-0.006826	1.291944
36.504434	407.457208	4.546470	-0.006997	1.301324
37.242312	415.965559	4.551475	-0.007140	1.310691
37.558597	424.518654	4.556480	-0.007204	1.319963
38.229010	432.909269	4.561485	-0.007334	1.329060
38.896921	441.304676	4.566490	-0.007464	1.338100
39.791552	449.659095	4.571494	-0.007636	1.347076
40.053822	458.115097	4.576499	-0.007691	1.355988
40.579376	466.499637	4.581504	-0.007794	1.364812
41.252062	474.878253	4.586509	-0.007925	1.373599
41.690192	483.261860	4.591514	-0.008012	1.382295
42.100971	491.670163	4.596518	-0.008094	1.390957
42.560188	500.031206	4.601523	-0.008185	1.399526
43.167621	508.366505	4.606528	-0.008304	1.408041
43.575867	516.731099	4.611533	-0.008385	1.416501
43.957218	525.066368	4.616538	-0.008462	1.424877
44.532998	533.405966	4.621542	-0.008574	1.433239
44.918833	541.716892	4.626547	-0.008651	1.441494
45.256718	550.049157	4.631552	-0.008720	1.449715
45.831498	558.338759	4.636557	-0.008832	1.457886
46.347923	566.618440	4.641562	-0.008934	1.465993
46.660372	574.997670	4.646566	-0.008998	1.474118
46.983275	583.287030	4.651571	-0.009063	1.482114
47.431469	591.552891	4.656576	-0.009152	1.490064
48.119258	599.795684	4.661581	-0.009285	1.497987
48.546579	608.051088	4.666586	-0.009370	1.505840
48.849155	616.366706	4.671590	-0.009432	1.513689
49.015458	624.646540	4.676595	-0.009469	1.521444
49.448971	632.895624	4.681600	-0.009555	1.529171
50.012238	641.137685	4.686605	-0.009665	1.536872
50.479813	649.360273	4.691610	-0.009758	1.544502
50.966246	657.626406	4.696614	-0.009854	1.552138
51.755853	665.793747	4.701619	-0.010006	1.559690
51.978355	674.059486	4.706624	-0.010053	1.567212
52.312470	682.330590	4.711629	-0.010120	1.574719
52.606767	690.553717	4.716634	-0.010181	1.582141
53.024704	698.781242	4.721638	-0.010264	1.589550
53.230570	707.034819	4.726643	-0.010308	1.596918
53.801571	715.212120	4.731648	-0.010419	1.604236
54.196937	723.441082	4.736653	-0.010498	1.611541
54.512121	731.659366	4.741658	-0.010562	1.618793
54.928382	739.871143	4.746662	-0.010645	1.626021
55.558495	748.094259	4.751667	-0.010768	1.633256
56.325311	756.226109	4.756672	-0.010916	1.640398
56.896042	764.408126	4.761677	-0.011028	1.647526
57.499610	772.579993	4.766682	-0.011145	1.654619
58.142521	780.746211	4.771686	-0.011270	1.661682
58.567729	788.945709	4.776691	-0.011355	1.668713
58.872882	797.172561	4.781696	-0.011417	1.675722
59.239386	805.363493	4.786701	-0.011491	1.682680
59.443316	813.578916	4.791706	-0.011534	1.689607
59.776499	821.785642	4.796710	-0.011602	1.696517
60.307462	829.928352	4.801715	-0.011706	1.703370
60.714424	838.119851	4.806720	-0.011787	1.710221
61.044332	846.322155	4.811725	-0.011854	1.717042
61.657333	854.430867	4.816730	-0.011973	1.723797
62.157364	862.595319	4.821734	-0.012072	1.730555
62.427815	870.798561	4.826739	-0.012127	1.737290
62.854839	878.948678	4.831744	-0.012212	1.743975
63.122901	887.143245	4.836749	-0.012268	1.750651
63.285422	895.337654	4.841754	-0.012303	1.757287
63.784063	903.469961	4.846758	-0.012401	1.763891
64.243566	911.601510	4.851763	-0.012492	1.770465
64.998494	919.722292	4.856768	-0.012638	1.777042
65.317400	927.895899	4.861773	-0.012703	1.783583
65.493289	936.094235	4.866778	-0.012741	1.790101
66.057905	944.278631	4.871782	-0.012852	1.796633
66.353322	952.400704	4.876787	-0.012912	1.803059
66.708500	960.540631	4.881792	-0.012983	1.809483
67.332576	968.664321	4.886797	-0.013105	1.815904
67.701580	976.800684	4.891802	-0.013179	1.822282
68.080994	984.960698	4.896806	-0.013255	1.828657
68.423836	993.116562	4.901811	-0.013324	1.835002
68.778374	1001.257796	4.906816	-0.013396	1.841315
69.328897	1009.374441	4.911821	-0.013503	1.847611
69.713826	1017.515460	4.916826	-0.013580	1.853884
69.978103	1025.670298	4.921830	-0.013635	1.860133
70.314014	1033.794757	4.926835	-0.013703	1.866345
70.587272	1041.969812	4.931840	-0.013759	1.872569
71.157144	1050.076572	4.936845	-0.013870	1.878754
71.600300	1058.149872	4.941850	-0.013958	1.884878
72.021404	1066.296368	4.946854	-0.014042	1.891036
72.433398	1074.423510	4.951859	-0.014124	1.897157
72.767611	1082.545025	4.956864	-0.014192	1.903246
73.132118	1090.688070	4.961869	-0.014265	1.909335
73.161461	1098.854097	4.966874	-0.014276	1.915384
73.553507	1106.967885	4.971878	-0.014354	1.921415
73.811508	1115.082069	4.976883	-0.014407	1.927413
73.954982	1123.241169	4.981888	-0.014439	1.933413
74.465005	1131.334457	4.986893	-0.014540	1.939386
74.350128	1139.487238	4.991898	-0.014524	1.945315
74.965400	1147.605567	4.996902	-0.014644	1.951282
75.201371	1155.745080	5.001907	-0.014693	1.957204
75.768222	1163.784819	5.006912	-0.014804	1.963071
75.990400	1171.905641	5.011917	-0.014850	1.968943
76.352979	1180.009915	5.016922	-0.014923	1.974800
76.758622	1188.101141	5.021926	-0.015004	1.980635
76.991853	1196.207655	5.026931	-0.015053	1.986445
77.328746	1204.334126	5.031936	-0.015121	1.992263
77.807579	1212.424133	5.036941	-0.015215	1.998054
78.113372	1220.509997	5.041946	-0.015278	2.003806
78.531507	1228.617797	5.046950	-0.015361	2.009569
78.908215	1236.727362	5.051955	-0.015436	2.015312
79.131737	1244.849367	5.056960	-0.015483	2.021032
79.429244	1252.963777	5.061965	-0.015544	2.026738
79.825831	1261.071475	5.066970	-0.015623	2.032433
80.377716	1269.161872	5.071974	-0.015731	2.038117
80.578178	1277.259116	5.076979	-0.015774	2.043753
80.993170	1285.351476	5.081984	-0.015856	2.049392
81.455555	1293.462704	5.086989	-0.015948	2.055033
81.857983	1301.525614	5.091994	-0.016028	2.060619
82.048106	1309.657726	5.096998	-0.016069	2.066217
82.212693	1317.787910	5.102003	-0.016105	2.071795
82.575647	1325.875038	5.107008	-0.016177	2.077348
82.738283	1333.978815	5.112013	-0.016213	2.082879
82.851985	1342.077531	5.117018	-0.016240	2.088386
83.383976	1350.168870	5.122022	-0.016344	2.093914
83.462853	1358.284511	5.127027	-0.016364	2.099401
83.919866	1366.337921	5.132032	-0.016454	2.104867
84.292444	1374.459993	5.137037	-0.016529	2.110358
84.461468	1382.602345	5.142042	-0.016566	2.115828
84.704651	1390.683392	5.147046	-0.016616	2.121250
84.891729	1398.751879	5.152051	-0.016657	2.126644
85.351587	1406.804605	5.157056	-0.016747	2.132040
85.593560	1414.898544	5.162061	-0.016798	2.137429
85.831955	1422.977934	5.167066	-0.016848	2.142795
86.270184	1431.057442	5.172070	-0.016934	2.148166
86.673700	1439.142529	5.177075	-0.017015	2.153523
86.861059	1447.235366	5.182080	-0.017055	2.158853
87.082950	1455.323856	5.187085	-0.017102	2.164169
87.308648	1463.408184	5.192090	-0.017149	2.169470
87.731359	1471.486364	5.197094	-0.017233	2.174772
88.116658	1479.559120	5.202099	-0.017310	2.180055
88.330943	1487.644436	5.207104	-0.017355	2.185317
88.777824	1495.744735	5.212109	-0.017444	2.190597
88.889744	1503.860227	5.217114	-0.017470	2.195843
89.120065	1511.937467	5.222118	-0.017518	2.201063
89.510833	1519.974681	5.227123	-0.017596	2.206260
89.804183	1528.064138	5.232128	-0.017656	2.211469
90.089919	1536.158317	5.237133	-0.017715	2.216668
90.329701	1544.213714	5.242138	-0.017765	2.221826
90.491329	1552.319370	5.247142	-0.017800	2.226996
90.816147	1560.403899	5.252147	-0.017866	2.232156
91.165961	1568.471059	5.257152	-0.017936	2.237295
91.671336	1576.528127	5.262157	-0.018036	2.242430
91.872495	1584.594901	5.267162	-0.018078	2.247532
92.132647	1592.709966	5.272166	-0.018132	2.252658
92.245363	1600.792738	5.277171	-0.018158	2.257739
92.408563	1608.874069	5.282176	-0.018194	2.262813
93.235365	1616.899377	5.287181	-0.018353	2.267897
93.608522	1625.035469	5.292186	-0.018428	2.273000
94.012153	1633.110256	5.297190	-0.018508	2.278055
94.216983	1641.149881	5.302195	-0.018552	2.283061
94.268783	1649.239772	5.307200	-0.018567	2.288073
94.496602	1657.331810	5.312205	-0.018615	2.293091
94.897788	1665.366177	5.317210	-0.018695	2.298077
95.313927	1673.405810	5.322214	-0.018777	2.303057
95.568252	1681.484827	5.327219	-0.018830	2.308036
95.796356	1689.579709	5.332224	-0.018878	2.313012
95.930180	1697.668514	5.337229	-0.018908	2.317966
96.293632	1705.684423	5.342234	-0.018981	2.322883
96.520137	1713.766559	5.347238	-0.019028	2.327820
96.773531	1721.860812	5.352243	-0.019081	2.332755
97.080530	1729.927960	5.357248	-0.019143	2.337668
97.471118	1737.977171	5.362253	-0.019221	2.342566
97.543839	1746.051636	5.367258	-0.019240	2.347443
97.956082	1754.158503	5.372262	-0.019322	2.352358
98.211685	1762.218479	5.377267	-0.019375	2.357221
98.510579	1770.250865	5.382272	-0.019436	2.362061
98.744357	1778.335877	5.387277	-0.019485	2.366917
98.912666	1786.407479	5.392282	-0.019522	2.371750
99.341630	1794.469290	5.397286	-0.019607	2.376588
99.515343	1802.535311	5.402291	-0.019644	2.381399
99.626678	1810.599006	5.407296	-0.019670	2.386193
100.238584	1818.640776	5.412301	-0.019790	2.391004
100.424565	1826.719327	5.417306	-0.019829	2.395794
100.633661	1834.779041	5.422310	-0.019874	2.400565
100.790942	1842.852020	5.427315	-0.019908	2.405330
101.051144	1850.913601	5.432320	-0.019962	2.410087
101.374117	1859.001604	5.437325	-0.020027	2.414854
101.533717	1867.044447	5.442330	-0.020062	2.419574
101.885759	1875.105441	5.447334	-0.020133	2.424309
102.027230	1883.195275	5.452339	-0.020165	2.429036
102.379015	1891.312944	5.457344	-0.020236	2.433786
102.657268	1899.342580	5.462349	-0.020293	2.438469
102.914301	1907.360712	5.467354	-0.020346	2.443136
103.296108	1915.402256	5.472358	-0.020422	2.447816
103.626829	1923.461824	5.477363	-0.020489	2.452494
103.652234	1931.551805	5.482368	-0.020499	2.457158
103.860718	1939.608498	5.487373	-0.020543	2.461807
104.250400	1947.628576	5.492378	-0.020621	2.466440
104.556155	1955.718033	5.497382	-0.020683	2.471098
105.003875	1963.763750	5.502387	-0.020772	2.475732
105.233846	1971.813476	5.507392	-0.020820	2.480344
105.907620	1979.821236	5.512397	-0.020951	2.484956
105.912073	1987.912993	5.517402	-0.020957	2.489558
106.211726	1996.007378	5.522406	-0.021018	2.494175
106.391023	2004.061097	5.527411	-0.021057	2.498751
106.770272	2012.075151	5.532416	-0.021133	2.503311
106.808552	2020.190097	5.537421	-0.021145	2.507894
106.896684	2028.284944	5.542426	-0.021167	2.512462
107.324689	2036.319787	5.547430	-0.021252	2.517012
107.585412	2044.348334	5.552435	-0.021306	2.521538
107.893366	2052.397136	5.557440	-0.021368	2.526070
108.244846	2060.443017	5.562445	-0.021439	2.530596
108.470560	2068.511483	5.567450	-0.021486	2.535118
108.564052	2076.564558	5.572454	-0.021509	2.539613
108.957405	2084.589284	5.577459	-0.021587	2.544106
109.242710	2092.641907	5.582464	-0.021646	2.548599
109.420022	2100.749971	5.587469	-0.021684	2.553107
109.551555	2108.804609	5.592474	-0.021714	2.557574
109.981160	2116.812499	5.597478	-0.021799	2.562028
110.440854	2124.857990	5.602483	-0.021890	2.566497
110.594904	2132.940758	5.607488	-0.021924	2.570958
111.051346	2141.000136	5.612493	-0.022014	2.575419
111.107670	2149.049501	5.617498	-0.022030	2.579839
111.292734	2157.107670	5.622502	-0.022070	2.584265
111.371535	2165.185100	5.627507	-0.022090	2.588687
111.687982	2173.378598	5.632512	-0.022154	2.593181
112.022353	2181.421120	5.637517	-0.022222	2.597586
112.239926	2189.414534	5.642522	-0.022267	2.601949
112.724275	2197.386243	5.647526	-0.022363	2.606311
113.091791	2205.408620	5.652531	-0.022437	2.610685
113.251919	2213.484302	5.657536	-0.022472	2.615066
113.545593	2221.507332	5.662541	-0.022532	2.619421
113.893798	2229.527007	5.667546	-0.022602	2.623770
114.525890	2237.553534	5.672550	-0.022725	2.628134
114.724204	2245.639786	5.677555	-0.022767	2.632494
115.203167	2253.666265	5.682560	-0.022861	2.636834
115.526916	2261.726819	5.687565	-0.022927	2.641174
115.607304	2269.770281	5.692570	-0.022947	2.645482
116.004064	2277.817060	5.697574	-0.023026	2.649806
116.236916	2285.923378	5.702579	-0.023075	2.654143
116.182788	2293.993084	5.707584	-0.023070	2.658435
116.386302	2302.034360	5.712589	-0.023113	2.662722
116.658220	2310.060952	5.717594	-0.023169	2.666999
116.817588	2318.143783	5.722598	-0.023204	2.671291
117.126708	2326.200254	5.727603	-0.023267	2.675572
117.719796	2334.183892	5.732608	-0.023383	2.679826
118.032391	2342.235283	5.737613	-0.023446	2.684090
118.005155	2350.286743	5.742618	-0.023446	2.688326
118.578636	2358.340804	5.747622	-0.023558	2.692596
118.974563	2366.363886	5.752627	-0.023637	2.696830
119.121489	2374.427392	5.757632	-0.023670	2.701064
119.460693	2382.451274	5.762637	-0.023739	2.705282
119.654342	2390.496964	5.767642	-0.023780	2.709496
119.736885	2398.605756	5.772646	-0.023801	2.713729
120.097220	2406.617835	5.777651	-0.023873	2.717922
120.470718	2414.611479	5.782656	-0.023948	2.722100
120.765256	2422.687238	5.787661	-0.024008	2.726310
120.881769	2430.746185	5.792666	-0.024035	2.730493
121.163623	2438.811819	5.797670	-0.024093	2.734683
121.314398	2446.861385	5.802675	-0.024126	2.738851
121.379687	2454.892235	5.807680	-0.024143	2.742997
121.772433	2462.922062	5.812685	-0.024222	2.747157
121.984024	2471.017259	5.817690	-0.024266	2.751332
122.241728	2479.118843	5.822694	-0.024320	2.755508
122.305665	2487.139257	5.827699	-0.024337	2.759623
122.704667	2495.092069	5.832704	-0.024416	2.763718
122.836036	2503.176908	5.837709	-0.024446	2.767859
123.089476	2511.216801	5.842714	-0.024499	2.771977
123.483986	2519.259067	5.847718	-0.024577	2.776099
123.952465	2527.260684	5.852723	-0.024670	2.780199
124.139359	2535.286259	5.857728	-0.024710	2.784288
124.463510	2543.377994	5.862733	-0.024776	2.788412
124.844862	2551.392005	5.867738	-0.024852	2.792495
125.041331	2559.462852	5.872742	-0.024894	2.796589
125.253929	2567.506049	5.877747	-0.024939	2.800664
125.621932	2575.497927	5.882752	-0.025012	2.804716
125.934114	2583.555155	5.887757	-0.025076	2.808792
126.053269	2591.600508	5.892762	-0.025103	2.812845
126.288278	2599.666627	5.897766	-0.025152	2.816910
126.663621	2607.698538	5.902771	-0.025227	2.820959
126.612758	2615.756054	5.907776	-0.025223	2.824991
126.881371	2623.809795	5.912781	-0.025279	2.829033
127.196429	2631.876172	5.917786	-0.025343	2.833078
127.509022	2639.916944	5.922790	-0.025406	2.837105
127.637085	2647.950766	5.927795	-0.025435	2.841112
127.835248	2655.945322	5.932800	-0.025477	2.845098
128.249775	2663.990878	5.937805	-0.025560	2.849116
128.307843	2672.059985	5.942810	-0.025576	2.853120
128.720027	2680.071455	5.947814	-0.025658	2.857109
128.982547	2688.121968	5.952819	-0.025712	2.861103
129.019865	2696.150370	5.957824	-0.025724	2.865069
129.389741	2704.213405	5.962829	-0.025798	2.869065
129.645144	2712.261381	5.967834	-0.025851	2.873041
129.851215	2720.302027	5.972838	-0.025895	2.877005
130.067986	2728.350778	5.977843	-0.025940	2.880968
130.199458	2736.346335	5.982848	-0.025970	2.884896
130.815710	2744.373543	5.987853	-0.026090	2.888859
130.881879	2752.445147	5.992858	-0.026108	2.892809
130.986674	2760.502426	5.997862	-0.026133	2.896749
131.222809	2768.546579	6.002867	-0.026182	2.900684
131.326643	2776.549050	6.007872	-0.026206	2.904586
131.722758	2784.619390	6.012877	-0.026286	2.908532
131.969507	2792.710934	6.017882	-0.026337	2.912474
132.331594	2800.768687	6.022886	-0.026409	2.916401
132.593072	2808.757591	6.027891	-0.026463	2.920284
132.589621	2816.764992	6.032896	-0.026468	2.924156
133.100595	2824.781068	6.037901	-0.026568	2.928055
133.074251	2832.854481	6.042906	-0.026569	2.931948
133.352033	2840.893142	6.047910	-0.026626	2.935835
133.659326	2848.910179	6.052915	-0.026688	2.939708
133.786180	2856.922444	6.057920	-0.026717	2.943564
134.223859	2864.970190	6.062925	-0.026804	2.947448
134.497328	2873.010054	6.067930	-0.026860	2.951314
134.895213	2881.049786	6.072934	-0.026939	2.955182
134.744704	2889.114955	6.077939	-0.026917	2.959029
134.912549	2897.134024	6.082944	-0.026953	2.962865
135.098893	2905.170770	6.087949	-0.026993	2.966705
135.390327	2913.201514	6.092954	-0.027053	2.970543
135.541879	2921.283408	6.097958	-0.027086	2.974393
135.887826	2929.289292	6.102963	-0.027156	2.978212
136.187936	2937.299990	6.107968	-0.027217	2.982026
136.523705	2945.350954	6.112973	-0.027285	2.985856
136.902189	2953.353739	6.117978	-0.027361	2.989660
137.223110	2961.447762	6.122982	-0.027426	2.993499
137.489927	2969.468023	6.127987	-0.027481	2.997296
137.663424	2977.496530	6.132992	-0.027518	3.001087
137.957663	2985.503961	6.137997	-0.027578	3.004870
137.991872	2993.563648	6.143002	-0.027590	3.008660
138.350388	3001.601432	6.148006	-0.027662	3.012450
138.720162	3009.656350	6.153011	-0.027736	3.016244
139.017959	3017.631731	6.158016	-0.027797	3.019993
139.158789	3025.693048	6.163021	-0.027828	3.023769
139.201175	3033.755395	6.168026	-0.027841	3.027536
139.568036	3041.796704	6.173030	-0.027915	3.031305
139.875245	3049.837655	6.178035	-0.027977	3.035066
139.886274	3057.865758	6.183040	-0.027985	3.038802
140.288044	3065.892199	6.188045	-0.028065	3.042551
140.558085	3073.912083	6.193050	-0.028120	3.046286
140.736322	3081.952100	6.198054	-0.028159	3.050021
140.887508	3090.033872	6.203059	-0.028192	3.053770
141.371079	3098.027324	6.208064	-0.028288	3.057490
141.518392	3106.092988	6.213069	-0.028320	3.061222
141.738480	3114.099500	6.218074	-0.028367	3.064925
141.892150	3122.149047	6.223078	-0.028400	3.068641
142.280837	3130.238101	6.228083	-0.028478	3.072382
142.126844	3138.321770	6.233088	-0.028455	3.076090
142.573962	3146.281235	6.238093	-0.028543	3.079764
142.762086	3154.284879	6.243098	-0.028584	3.083442
142.983240	3162.312577	6.248102	-0.028630	3.087129
143.320470	3170.331436	6.253107	-0.028698	3.090812
143.614147	3178.357593	6.258112	-0.028758	3.094493
143.961352	3186.386021	6.263117	-0.028828	3.098172
144.091966	3194.443187	6.268122	-0.028857	3.101850
144.404161	3202.455420	6.273126	-0.028921	3.105511
144.642429	3210.488791	6.278131	-0.028971	3.109175
144.617109	3218.553955	6.283136	-0.028971	3.112836
144.759979	3226.620114	6.288141	-0.029003	3.116501
144.796475	3234.598867	6.293146	-0.029015	3.120118
145.117410	3242.629079	6.298150	-0.029080	3.123766
145.377717	3250.675546	6.303155	-0.029134	3.127415
145.691980	3258.695771	6.308160	-0.029198	3.131050
145.822747	3266.769218	6.313165	-0.029227	3.134696
145.940737	3274.772947	6.318170	-0.029254	3.138307
146.418408	3282.775605	6.323174	-0.029349	3.141928
146.615473	3290.814573	6.328179	-0.029391	3.145549
146.762209	3298.823992	6.333184	-0.029423	3.149151
146.912486	3306.948222	6.338189	-0.029456	3.152800
147.211244	3314.952372	6.343194	-0.029517	3.156397
147.320667	3322.967474	6.348198	-0.029543	3.159987
147.602910	3330.974271	6.353203	-0.029601	3.163577
147.986357	3338.992400	6.358208	-0.029677	3.167172
148.111444	3347.067952	6.363213	-0.029706	3.170777
148.059032	3355.134121	6.368218	-0.029702	3.174367
148.245206	3363.152001	6.373222	-0.029741	3.177941
148.716702	3371.174780	6.378227	-0.029835	3.181525
148.812922	3379.159791	6.383232	-0.029858	3.185073
149.163866	3387.209002	6.388237	-0.029928	3.188656
149.403915	3395.249825	6.393242	-0.029978	3.192226
149.587697	3403.326330	6.398246	-0.030018	3.195806
149.806212	3411.329489	6.403251	-0.030064	3.199350
150.171027	3419.307924	6.408256	-0.030137	3.202886
150.346289	3427.378526	6.413261	-0.030175	3.206451
150.658547	3435.387780	6.418266	-0.030238	3.209990
150.850442	3443.436572	6.423270	-0.030279	3.213538
151.047707	3451.466835	6.428275	-0.030321	3.217074
151.137729	3459.501170	6.433280	-0.030343	3.220604
151.503191	3467.504281	6.438285	-0.030417	3.224127
151.706384	3475.528668	6.443290	-0.030460	3.227649
151.887902	3483.623229	6.448294	-0.030499	3.231197
151.923800	3491.716763	6.453299	-0.030511	3.234734
152.159523	3499.683928	6.458304	-0.030560	3.238221
152.550559	3507.685509	6.463309	-0.030638	3.241725
152.663737	3515.672191	6.468314	-0.030664	3.245208
152.942204	3523.721171	6.473318	-0.030721	3.248720
153.143448	3531.789724	6.478323	-0.030764	3.252234
153.420435	3539.816239	6.483328	-0.030821	3.255729
153.845922	3547.806905	6.488333	-0.030905	3.259211
153.954926	3555.833173	6.493338	-0.030931	3.262692
154.194745	3563.879933	6.498342	-0.030981	3.266183
154.252152	3571.947014	6.503347	-0.030997	3.269672
154.441802	3579.986105	6.508352	-0.031038	3.273150
154.923656	3587.994979	6.513357	-0.031133	3.276623
154.917038	3595.986555	6.518362	-0.031137	3.280065
155.219989	3604.004972	6.523366	-0.031198	3.283528
155.483032	3612.055955	6.528371	-0.031252	3.286999
155.358908	3620.082821	6.533376	-0.031235	3.290442
155.779695	3628.128758	6.538381	-0.031318	3.293910
156.083398	3636.153070	6.543386	-0.031380	3.297360
156.282252	3644.171247	6.548390	-0.031422	3.300800
156.476811	3652.188781	6.553395	-0.031464	3.304236
156.465588	3660.234563	6.558400	-0.031467	3.307673
156.895334	3668.288294	6.563405	-0.031552	3.311126
156.934988	3676.333970	6.568410	-0.031565	3.314557
157.280044	3684.310360	6.573414	-0.031634	3.317967
157.509474	3692.353803	6.578419	-0.031682	3.321398
157.630267	3700.335140	6.583424	-0.031710	3.324794
157.963441	3708.378863	6.588429	-0.031777	3.328222
158.037005	3716.422157	6.593434	-0.031796	3.331635
158.318579	3724.466589	6.598438	-0.031854	3.335054
158.578381	3732.519105	6.603443	-0.031908	3.338472
158.657349	3740.507852	6.608448	-0.031928	3.341852
159.133028	3748.518296	6.613453	-0.032022	3.345253
159.039224	3756.561379	6.618458	-0.032009	3.348643
159.189602	3764.627002	6.623462	-0.032043	3.352048
159.730208	3772.668677	6.628467	-0.032149	3.355454
159.918713	3780.649632	6.633472	-0.032189	3.358818
160.129880	3788.701405	6.638477	-0.032234	3.362209
160.137444	3796.712663	6.643482	-0.032240	3.365573
160.416663	3804.756357	6.648486	-0.032297	3.368956
160.553604	3812.824903	6.653491	-0.032328	3.372341
160.700756	3820.853740	6.658496	-0.032361	3.375707
161.116517	3828.834955	6.663501	-0.032444	3.379058
161.154279	3836.863844	6.668506	-0.032456	3.382413
161.456977	3844.864831	6.673510	-0.032518	3.385763
161.800437	3852.907915	6.678515	-0.032587	3.389127
162.002601	3860.979317	6.683520	-0.032630	3.392496
162.177221	3869.072421	6.688525	-0.032667	3.395869
162.330388	3877.022143	6.693530	-0.032701	3.399178
162.635868	3885.003056	6.698534	-0.032763	3.402502
162.728102	3893.067710	6.703539	-0.032786	3.405851
162.949435	3901.021809	6.708544	-0.032832	3.409154
163.482646	3909.073264	6.713549	-0.032937	3.412506
163.421179	3917.166323	6.718554	-0.032931	3.415851
163.672443	3925.143153	6.723558	-0.032983	3.419155
163.828878	3933.177267	6.728563	-0.033017	3.422477
163.842913	3941.184781	6.733568	-0.033025	3.425779
164.032300	3949.212932	6.738573	-0.033065	3.429093
164.525179	3957.264309	6.743578	-0.033163	3.432423
164.869876	3965.309265	6.748582	-0.033232	3.435742
164.849452	3973.334143	6.753587	-0.033233	3.439038
165.068096	3981.326721	6.758592	-0.033279	3.442325
165.353193	3989.356703	6.763597	-0.033338	3.445627
165.343766	3997.390912	6.768602	-0.033341	3.448917
165.393273	4005.447121	6.773606	-0.033356	3.452215
165.663026	4013.523122	6.778611	-0.033411	3.455525
165.845809	4021.480911	6.783616	-0.033451	3.458781
166.077628	4029.526569	6.788621	-0.033499	3.462072
166.443181	4037.514896	6.793626	-0.033572	3.465340
166.633620	4045.575532	6.798630	-0.033613	3.468628
166.785314	4053.639321	6.803635	-0.033647	3.471914
166.934295	4061.684913	6.808640	-0.033680	3.475189
167.370042	4069.640851	6.813645	-0.033766	3.478434
167.798587	4077.633482	6.818650	-0.033851	3.481690
167.909172	4085.623405	6.823654	-0.033877	3.484932
168.078110	4093.677949	6.828659	-0.033914	3.488199
168.366469	4101.715325	6.833664	-0.033973	3.491459
168.465815	4109.791366	6.838669	-0.033996	3.494726
168.736583	4117.771913	6.843674	-0.034052	3.497957
168.941013	4125.806169	6.848678	-0.034095	3.501205
169.039584	4133.800405	6.853683	-0.034119	3.504430
169.203959	4141.830316	6.858688	-0.034155	3.507668
169.461816	4149.899333	6.863693	-0.034208	3.510922
169.604028	4157.928916	6.868698	-0.034240	3.514154
169.869559	4165.946375	6.873702	-0.034295	3.517382
170.059472	4173.970115	6.878707	-0.034335	3.520606
170.454248	4181.910051	6.883712	-0.034414	3.523801
170.639757	4189.983321	6.888717	-0.034454	3.527039
170.725617	4198.042796	6.893722	-0.034475	3.530266
170.843871	4206.075976	6.898726	-0.034502	3.533480
171.152718	4214.124010	6.903731	-0.034565	3.536704
171.248110	4222.128318	6.908736	-0.034588	3.539900
171.554823	4230.153778	6.913741	-0.034650	3.543108
171.640148	4238.193872	6.918746	-0.034672	3.546313
171.719771	4246.223656	6.923750	-0.034692	3.549510
172.132182	4254.349796	6.928755	-0.034774	3.552752
172.383587	4262.361068	6.933760	-0.034826	3.555941
172.712815	4270.308536	6.938765	-0.034892	3.559105
172.726479	4278.302376	6.943770	-0.034900	3.562274
172.918371	4286.299637	6.948774	-0.034941	3.565447
173.131220	4294.349928	6.953779	-0.034986	3.568639
173.022990	4302.397962	6.958784	-0.034971	3.571818
173.278794	4310.413774	6.963789	-0.035024	3.574992
173.530443	4318.403897	6.968794	-0.035076	3.578153
173.715681	4326.427438	6.973798	-0.035116	3.581322
173.852226	4334.433179	6.978803	-0.035147	3.584480
173.946470	4342.458640	6.983808	-0.035169	3.587641
174.385722	4350.502002	6.988813	-0.035257	3.590817
174.463197	4358.547006	6.993818	-0.035276	3.593980
174.808094	4366.538518	6.998822	-0.035346	3.597127
174.868909	4374.601382	7.003827	-0.035362	3.600291
175.069754	4382.578458	7.008832	-0.035405	3.603423
175.371145	4390.616020	7.013837	-0.035466	3.606578
175.484871	4398.614244	7.018842	-0.035493	3.609710
175.750723	4406.667008	7.023846	-0.035548	3.612865
175.732717	4414.753436	7.028851	-0.035549	3.616022
176.088325	4422.678854	7.033856	-0.035621	3.619124
176.291905	4430.727705	7.038861	-0.035664	3.622268
176.281834	4438.736100	7.043866	-0.035667	3.625387
176.504562	4446.789669	7.048870	-0.035714	3.628527
176.909145	4454.850475	7.053875	-0.035795	3.631672
176.969512	4462.880520	7.058880	-0.035811	3.634793
177.136862	4470.906049	7.063885	-0.035848	3.637912
177.278567	4478.975762	7.068890	-0.035879	3.641046
177.335722	4486.920494	7.073894	-0.035895	3.644125
177.537199	4494.963695	7.078899	-0.035938	3.647245
177.645510	4502.978287	7.083904	-0.035963	3.650348
178.047411	4511.016019	7.088909	-0.036044	3.653465
177.832891	4519.087523	7.093914	-0.036009	3.656576
178.163741	4527.035582	7.098918	-0.036076	3.659651
178.548077	4535.072735	7.103923	-0.036153	3.662759
178.573053	4543.068238	7.108928	-0.036163	3.665839
178.683722	4551.116642	7.113933	-0.036188	3.668939
178.862989	4559.165669	7.118938	-0.036227	3.672039
179.033509	4567.161196	7.123942	-0.036264	3.675115
179.257742	4575.203849	7.128947	-0.036311	3.678208
179.376902	4583.221301	7.133952	-0.036339	3.681286
179.568788	4591.201562	7.138957	-0.036379	3.684349
179.813254	4599.230749	7.143962	-0.036430	3.687430
179.868514	4607.256420	7.148966	-0.036446	3.690501
180.302388	4615.309600	7.153971	-0.036532	3.693590
180.445939	4623.342198	7.158976	-0.036564	3.696662
180.619138	4631.339498	7.163981	-0.036601	3.699718
180.983231	4639.333475	7.168986	-0.036674	3.702775
181.071145	4647.344845	7.173990	-0.036696	3.705829
181.415007	4655.415165	7.178995	-0.036765	3.708910
181.544185	4663.463559	7.184000	-0.036795	3.711974
181.785290	4671.565684	7.189005	-0.036845	3.715059
182.091679	4679.519102	7.194010	-0.036907	3.718086
181.872340	4687.552405	7.199014	-0.036872	3.721129
182.079707	4695.507212	7.204019	-0.036915	3.724149
182.234603	4703.513153	7.209024	-0.036950	3.727185
182.478852	4711.533217	7.214029	-0.037000	3.730227
182.615720	4719.611352	7.219034	-0.037031	3.733285
182.842199	4727.607024	7.224038	-0.037078	3.736311
182.894926	4735.626855	7.229043	-0.037094	3.739340
182.899297	4743.667020	7.234048	-0.037100	3.742373
183.308240	4751.665175	7.239053	-0.037181	3.745397
183.346010	4759.698963	7.244058	-0.037193	3.748424
183.439088	4767.735825	7.249062	-0.037216	3.751450
184.008041	4775.773786	7.254067	-0.037327	3.754486
184.215417	4783.763560	7.259072	-0.037371	3.757492
183.962138	4791.823181	7.264077	-0.037329	3.760512
184.284276	4799.813005	7.269082	-0.037394	3.763516
184.625672	4807.805682	7.274086	-0.037463	3.766520
184.932912	4815.871201	7.279091	-0.037526	3.769547
184.907253	4823.898507	7.284096	-0.037526	3.772550
185.175476	4831.932749	7.289101	-0.037581	3.775560
185.352896	4839.948086	7.294106	-0.037620	3.778558
185.290257	4847.964269	7.299110	-0.037613	3.781549
185.665479	4855.959623	7.304115	-0.037688	3.784540
185.883755	4863.982607	7.309120	-0.037734	3.787535
185.983642	4872.027501	7.314125	-0.037758	3.790533
186.088080	4880.112119	7.319130	-0.037783	3.793543
186.291339	4888.099066	7.324134	-0.037826	3.796517
186.473818	4896.098643	7.329139	-0.037865	3.799493
186.704783	4904.073956	7.334144	-0.037913	3.802459
187.172577	4912.080424	7.339149	-0.038006	3.805439
187.248221	4920.109596	7.344154	-0.038025	3.808416
187.152959	4928.202292	7.349158	-0.038013	3.811411
187.556159	4936.187085	7.354163	-0.038093	3.814375
187.818016	4944.194909	7.359168	-0.038147	3.817341
187.868245	4952.217081	7.364173	-0.038162	3.820306
188.162904	4960.217060	7.369178	-0.038222	3.823266
188.362381	4968.233068	7.374182	-0.038264	3.826227
188.394956	4976.295426	7.379187	-0.038276	3.829199
188.560874	4984.318313	7.384192	-0.038312	3.832158
188.893031	4992.334642	7.389197	-0.038379	3.835115
189.021639	5000.328914	7.394202	-0.038408	3.838057
189.324501	5008.365452	7.399206	-0.038470	3.841017
189.350149	5016.382228	7.404211	-0.038480	3.843961
189.543899	5024.372768	7.409216	-0.038521	3.846896
189.795959	5032.413955	7.414221	-0.038573	3.849850
189.729678	5040.479140	7.419226	-0.038566	3.852803
189.950600	5048.505562	7.424230	-0.038613	3.855745
190.340230	5056.493890	7.429235	-0.038690	3.858675
190.333989	5064.530762	7.434240	-0.038694	3.861612
190.636659	5072.566223	7.439245	-0.038756	3.864553
190.890188	5080.591798	7.444250	-0.038809	3.867486
190.969395	5088.583399	7.449254	-0.038829	3.870402
191.186071	5096.835046	7.454259	-0.038874	3.873413
191.239198	5104.837842	7.459264	-0.038889	3.876328
191.586386	5112.728692	7.464269	-0.038959	3.879205
191.573312	5120.708468	7.469274	-0.038962	3.882106
191.571463	5128.721986	7.474278	-0.038967	3.885017
191.887689	5136.731454	7.479283	-0.039031	3.887930
191.940280	5144.752459	7.484288	-0.039046	3.890841
192.292797	5152.801549	7.489293	-0.039117	3.893765
192.553911	5160.808200	7.494298	-0.039171	3.896669
192.563803	5168.805656	7.499302	-0.039178	3.899564
192.778646	5176.847571	7.504307	-0.039223	3.902476
192.887724	5184.830233	7.509312	-0.039249	3.905363
193.082749	5192.856774	7.514317	-0.039290	3.908264
193.246930	5200.897025	7.519322	-0.039326	3.911168
193.353947	5208.918557	7.524326	-0.039351	3.914063
193.731028	5216.936548	7.529331	-0.039427	3.916958
193.671828	5224.924830	7.534336	-0.039421	3.919833
193.972092	5232.984855	7.539341	-0.039482	3.922738
194.260378	5240.968192	7.544346	-0.039541	3.925613
194.209279	5248.965978	7.549350	-0.039537	3.928485
194.283661	5257.059862	7.554355	-0.039556	3.931392
194.601596	5265.041324	7.559360	-0.039621	3.934260
194.919222	5273.077567	7.564365	-0.039685	3.937146
194.947496	5281.077572	7.569370	-0.039696	3.940012
195.029208	5289.086880	7.574374	-0.039716	3.942880
195.474161	5297.088484	7.579379	-0.039804	3.945749
195.348355	5305.105839	7.584384	-0.039786	3.948612
195.574259	5313.183446	7.589389	-0.039833	3.951500
196.069745	5321.193519	7.594394	-0.039931	3.954367
196.063311	5329.214754	7.599398	-0.039935	3.957227
196.353345	5337.203775	7.604403	-0.039994	3.960079
196.508876	5345.148158	7.609408	-0.040028	3.962910
196.850230	5353.205235	7.614413	-0.040097	3.965783
196.917554	5361.264726	7.619418	-0.040115	3.968650
196.952834	5369.302598	7.624422	-0.040127	3.971506
197.331958	5377.369550	7.629427	-0.040203	3.974376
197.454002	5385.319079	7.634432	-0.040231	3.977199
197.581115	5393.418553	7.639437	-0.040260	3.980072
197.689801	5401.408433	7.644442	-0.040285	3.982904
198.093380	5409.370883	7.649446	-0.040365	3.985730
197.911563	5417.417571	7.654451	-0.040337	3.988573
198.032795	5425.438237	7.659456	-0.040365	3.991411
198.332347	5433.496237	7.664461	-0.040426	3.994262
198.481643	5441.522786	7.669466	-0.040459	3.997098
198.578546	5449.491981	7.674470	-0.040482	3.999910
198.887990	5457.534245	7.679475	-0.040545	4.002750
198.894502	5465.524264	7.684480	-0.040551	4.005564
199.037816	5473.542134	7.689485	-0.040583	4.008389
199.378151	5481.602161	7.694490	-0.040652	4.011229
199.548559	5489.618785	7.699494	-0.040689	4.014050
199.600715	5497.689072	7.704499	-0.040704	4.016885
199.632112	5505.669023	7.709504	-0.040715	4.019687
200.024280	5513.699185	7.714509	-0.040793	4.022509
199.963599	5521.717636	7.719514	-0.040787	4.025319
199.969797	5529.729828	7.724518	-0.040794	4.028125
200.319333	5537.777279	7.729523	-0.040864	4.030947
200.346481	5545.866825	7.734528	-0.040875	4.033777
200.489645	5553.845368	7.739533	-0.040906	4.036567
200.704049	5561.806767	7.744538	-0.040952	4.039351
200.854811	5569.796162	7.749542	-0.040985	4.042142
201.131186	5577.802813	7.754547	-0.041042	4.044939
201.262454	5585.826655	7.759552	-0.041071	4.047737
201.701435	5593.846717	7.764557	-0.041158	4.050537
201.877415	5601.914072	7.769562	-0.041196	4.053348
202.111987	5609.899355	7.774566	-0.041245	4.056128
202.202046	5617.904323	7.779571	-0.041267	4.058912
202.379028	5625.917526	7.784576	-0.041305	4.061698
202.448243	5633.911959	7.789581	-0.041324	4.064474
202.411016	5641.984692	7.794586	-0.041322	4.067273
202.724375	5649.941442	7.799590	-0.041386	4.070035
203.015747	5658.034466	7.804595	-0.041445	4.072843
202.873508	5666.046074	7.809600	-0.041424	4.075614
203.146769	5674.025594	7.814605	-0.041480	4.078378
203.299515	5682.047098	7.819610	-0.041514	4.081153
203.506979	5690.037594	7.824614	-0.041558	4.083915
203.716071	5698.102291	7.829619	-0.041602	4.086702
203.759278	5706.068681	7.834624	-0.041615	4.089451
203.923002	5714.160746	7.839629	-0.041651	4.092242
204.235706	5722.173718	7.844634	-0.041714	4.095007
204.410774	5730.168562	7.849638	-0.041752	4.097762
204.399543	5738.194230	7.854643	-0.041755	4.100522
204.449854	5746.219307	7.859648	-0.041770	4.103282
204.688403	5754.213515	7.864653	-0.041820	4.106031
205.049614	5762.255817	7.869658	-0.041892	4.108797
204.996790	5770.297544	7.874662	-0.041888	4.111556
205.172741	5778.350603	7.879667	-0.041926	4.114319
205.378136	5786.356096	7.884672	-0.041969	4.117064
205.490505	5794.292965	7.889677	-0.041995	4.119783
205.747426	5802.322863	7.894682	-0.042048	4.122534
205.750111	5810.324702	7.899686	-0.042054	4.125270
205.794940	5818.385150	7.904691	-0.042068	4.128025
205.883465	5826.409171	7.909696	-0.042090	4.130766
206.315221	5834.453544	7.914701	-0.042175	4.133517
206.527512	5842.498575	7.919706	-0.042220	4.136263
206.321515	5850.444042	7.924710	-0.042187	4.138968
206.782395	5858.532170	7.929715	-0.042278	4.141728
206.983074	5866.496585	7.934720	-0.042321	4.144441
207.081041	5874.517692	7.939725	-0.042344	4.147170
207.232081	5882.566152	7.944730	-0.042377	4.149908
207.554560	5890.592851	7.949734	-0.042443	4.152638
207.734845	5898.624400	7.954739	-0.042482	4.155366
207.928969	5906.578890	7.959744	-0.042523	4.158067
208.022798	5914.644351	7.964749	-0.042546	4.160802
208.328585	5922.635085	7.969754	-0.042608	4.163512
208.444723	5930.655138	7.974758	-0.042635	4.166229
208.815617	5938.693096	7.979763	-0.042709	4.168953
208.910089	5946.709741	7.984768	-0.042732	4.171664
208.768859	5954.709950	7.989773	-0.042711	4.174366
208.992026	5962.768847	7.994778	-0.042758	4.177089
209.186339	5970.725772	7.999782	-0.042799	4.179776
209.470002	5978.775728	8.004787	-0.042857	4.182494
209.418071	5986.756745	8.009792	-0.042853	4.185183
209.682689	5994.799372	8.014797	-0.042907	4.187894
210.027862	6002.828026	8.019802	-0.042977	4.190600
210.185697	6010.959953	8.024806	-0.043012	4.193337
210.227153	6018.981113	8.029811	-0.043025	4.196033
210.565406	6026.876258	8.034816	-0.043093	4.198689
210.598128	6034.900598	8.039821	-0.043104	4.201383
210.738972	6042.864352	8.044826	-0.043136	4.204056
211.025629	6050.934902	8.049830	-0.043194	4.206765
211.375503	6058.945439	8.054835	-0.043265	4.209452
211.311924	6066.953420	8.059840	-0.043258	4.212133
211.708822	6074.957101	8.064845	-0.043337	4.214815
211.737737	6082.991216	8.069850	-0.043348	4.217502
211.685734	6090.977772	8.074854	-0.043343	4.220170
211.811792	6099.034175	8.079859	-0.043372	4.222862
212.109924	6107.044810	8.084864	-0.043433	4.225538
212.213551	6115.072954	8.089869	-0.043458	4.228217
212.413285	6123.105292	8.094874	-0.043500	4.230896
212.534545	6131.132910	8.099878	-0.043528	4.233571
212.759887	6139.161711	8.104883	-0.043575	4.236246
212.787312	6147.119709	8.109888	-0.043585	4.238894
213.070788	6155.148654	8.114893	-0.043643	4.241566
213.270891	6163.120296	8.119898	-0.043686	4.244217
213.244194	6171.174879	8.124902	-0.043686	4.246891
213.432742	6179.214396	8.129907	-0.043727	4.249561
213.747388	6187.215056	8.134912	-0.043790	4.252217
213.911409	6195.248567	8.139917	-0.043826	4.254881
213.962927	6203.254441	8.144922	-0.043841	4.257533
213.927803	6211.276183	8.149926	-0.043840	4.260188
214.349143	6219.302866	8.154931	-0.043924	4.262847
214.374770	6227.333070	8.159936	-0.043934	4.265502
214.456893	6235.322365	8.164941	-0.043954	4.268142
214.857387	6243.383901	8.169946	-0.044034	4.270808
214.955047	6251.402748	8.174950	-0.044057	4.273454
215.151605	6259.474231	8.179955	-0.044099	4.276118
215.292696	6267.434761	8.184960	-0.044131	4.278743
215.344036	6275.468920	8.189965	-0.044146	4.281389
215.625823	6283.433900	8.194970	-0.044203	4.284013
215.677238	6291.439134	8.199974	-0.044218	4.286647
215.938863	6299.453551	8.204979	-0.044272	4.289284
215.926207	6307.448466	8.209984	-0.044275	4.291910
216.135911	6315.551224	8.214989	-0.044319	4.294572
216.402494	6323.578717	8.219994	-0.044374	4.297209
216.535697	6331.577352	8.224998	-0.044404	4.299833
216.673754	6339.574147	8.230003	-0.044435	4.302454
216.716834	6347.602944	8.235008	-0.044449	4.305084
216.952873	6355.629240	8.240013	-0.044498	4.307713
217.047049	6363.662923	8.245018	-0.044521	4.310342
216.889755	6371.672072	8.250022	-0.044497	4.312959
217.166552	6379.730479	8.255027	-0.044553	4.315594
217.323379	6387.656085	8.260032	-0.044588	4.318183
217.508533	6395.707414	8.265037	-0.044628	4.320812
217.850484	6403.683589	8.270042	-0.044696	4.323416
217.672256	6411.715621	8.275046	-0.044669	4.326032
218.038686	6419.749020	8.280051	-0.044742	4.328652
218.039391	6427.759013	8.285056	-0.044747	4.331259
218.156752	6435.800100	8.290061	-0.044775	4.333876
218.367005	6443.821048	8.295066	-0.044819	4.336486
218.577037	6451.747931	8.300070	-0.044863	4.339063
218.946683	6459.865688	8.305075	-0.044937	4.341701
218.813595	6467.807596	8.310080	-0.044918	4.344278
219.031375	6475.841239	8.315085	-0.044964	4.346885
219.195505	6483.888612	8.320090	-0.044999	4.349495
219.261535	6491.940001	8.325094	-0.045017	4.352104
219.612816	6500.004962	8.330099	-0.045088	4.354717
219.509141	6507.956616	8.335104	-0.045074	4.357289
219.864060	6515.940548	8.340109	-0.045145	4.359873
219.962363	6523.947927	8.345114	-0.045169	4.362462
219.976549	6531.908565	8.350118	-0.045176	4.365033
220.237375	6539.993970	8.355123	-0.045230	4.367645
220.340955	6547.990515	8.360128	-0.045255	4.370225
220.557743	6556.008106	8.365133	-0.045300	4.372811
220.615388	6564.067427	8.370138	-0.045316	4.375408
220.732197	6572.056773	8.375142	-0.045343	4.377982
220.990551	6580.077401	8.380147	-0.045397	4.380565
220.997093	6588.036543	8.385152	-0.045403	4.383125
221.292780	6596.049587	8.390157	-0.045464	4.385702
221.466293	6604.118234	8.395162	-0.045501	4.388295
221.379745	6612.124297	8.400166	-0.045490	4.390865
221.647102	6620.177571	8.405171	-0.045545	4.393451
221.696896	6628.159569	8.410176	-0.045560	4.396011
221.901976	6636.168958	8.415181	-0.045603	4.398579
222.197630	6644.213778	8.420186	-0.045664	4.401158
222.049984	6652.168327	8.425190	-0.045641	4.403703
222.412880	6660.245994	8.430195	-0.045714	4.406290
222.562529	6668.239211	8.435200	-0.045747	4.408846
223.051783	6676.270821	8.440205	-0.045844	4.411415
223.022844	6684.314483	8.445210	-0.045844	4.413984
223.069970	6692.340122	8.450214	-0.045858	4.416546
223.600347	6700.359123	8.455219	-0.045962	4.419107
223.686396	6708.386781	8.460224	-0.045983	4.421667
223.592369	6716.359095	8.465229	-0.045971	4.424206
223.892013	6724.424301	8.470234	-0.046032	4.426776
224.070762	6732.411692	8.475238	-0.046070	4.429319
224.266929	6740.475174	8.480243	-0.046112	4.431885
224.490382	6748.504716	8.485248	-0.046159	4.434438
224.614395	6756.531524	8.490253	-0.046187	4.436989
224.782446	6764.491586	8.495258	-0.046224	4.439517
224.735812	6772.493619	8.500262	-0.046220	4.442056
224.993431	6780.477438	8.505267	-0.046274	4.444589
225.049469	6788.531636	8.510272	-0.046289	4.447142
225.100791	6796.518590	8.515277	-0.046304	4.449673
225.472718	6804.590842	8.520282	-0.046379	4.452230
225.665450	6812.609947	8.525286	-0.046420	4.454768
225.788785	6820.613832	8.530291	-0.046448	4.457300
225.918471	6828.629164	8.535296	-0.046477	4.459834
226.007451	6836.627852	8.540301	-0.046499	4.462361
226.290639	6844.589251	8.545306	-0.046557	4.464875
226.286993	6852.629858	8.550310	-0.046562	4.467412
226.368834	6860.662180	8.555315	-0.046582	4.469945
226.682135	6868.710369	8.560320	-0.046646	4.472483
226.811923	6876.726621	8.565325	-0.046675	4.475008
227.095936	6884.766619	8.570330	-0.046734	4.477540
227.180280	6892.720113	8.575335	-0.046754	4.480043
227.286314	6900.764271	8.580339	-0.046779	4.482572
227.197454	6908.734534	8.585344	-0.046768	4.485077
227.397378	6916.779891	8.590349	-0.046811	4.487604
227.712877	6924.828729	8.595354	-0.046875	4.490132
227.669000	6932.828977	8.600359	-0.046872	4.492642
228.087943	6940.874116	8.605363	-0.046955	4.495166
228.070309	6948.929004	8.610368	-0.046957	4.497690
228.178935	6956.868614	8.615373	-0.046982	4.500177
228.247255	6964.871887	8.620378	-0.047000	4.502682
228.476036	6972.861284	8.625383	-0.047048	4.505182
228.584903	6980.919161	8.630387	-0.047074	4.507702
228.611463	6988.922322	8.635392	-0.047084	4.510203
228.746750	6996.962057	8.640397	-0.047114	4.512714
228.965808	7005.049687	8.645402	-0.047161	4.515240
229.060175	7012.983742	8.650407	-0.047183	4.517715
229.302624	7020.975160	8.655411	-0.047234	4.520207
229.336540	7028.987657	8.660416	-0.047245	4.522704
229.342095	7036.951663	8.665421	-0.047252	4.525185
229.500740	7044.994226	8.670426	-0.047286	4.527689
229.622996	7052.984341	8.675431	-0.047314	4.530175
229.926798	7061.074124	8.680435	-0.047376	4.532691
229.881041	7069.117499	8.685440	-0.047373	4.535190
229.979358	7077.143296	8.690445	-0.047397	4.537683
230.249515	7085.115181	8.695450	-0.047452	4.540158
230.388417	7093.117454	8.700455	-0.047483	4.542641
230.503967	7101.122284	8.705459	-0.047510	4.545123
230.615244	7109.157766	8.710464	-0.047536	4.547614
230.763485	7117.133993	8.715469	-0.047569	4.550085
230.761445	7125.239456	8.720474	-0.047574	4.552594
230.982014	7133.232249	8.725479	-0.047620	4.555067
231.311665	7141.257254	8.730483	-0.047687	4.557549
231.194293	7149.214987	8.735488	-0.047670	4.560008
231.296790	7157.199299	8.740493	-0.047694	4.562474
231.810014	7165.261174	8.745498	-0.047795	4.564964
231.785788	7173.283170	8.750503	-0.047796	4.567439
231.986867	7181.305654	8.755507	-0.047839	4.569913
232.069033	7189.335011	8.760512	-0.047859	4.572388
232.347651	7197.329592	8.765517	-0.047916	4.574851
232.449329	7205.398116	8.770522	-0.047941	4.577335
232.506437	7213.303744	8.775527	-0.047956	4.579768
232.725898	7221.418286	8.780531	-0.048003	4.582264
232.640876	7229.415167	8.785536	-0.047992	4.584722
232.895267	7237.460265	8.790541	-0.048045	4.587193
233.258484	7245.498394	8.795546	-0.048118	4.589662
233.197945	7253.528575	8.800551	-0.048112	4.592126
233.359944	7261.563693	8.805555	-0.048147	4.594590
233.512894	7269.526804	8.810560	-0.048181	4.597031
233.714389	7277.467650	8.815565	-0.048223	4.599464
233.818028	7285.582188	8.820570	-0.048248	4.601949
233.880049	7293.461409	8.825575	-0.048265	4.604361
234.184462	7301.593719	8.830579	-0.048327	4.606848
234.331152	7309.548813	8.835584	-0.048359	4.609280
234.644142	7317.596010	8.840589	-0.048423	4.611739
234.909790	7325.621052	8.845594	-0.048478	4.614190
234.859104	7333.672966	8.850599	-0.048473	4.616647
235.088798	7341.618669	8.855603	-0.048521	4.619071
235.218236	7349.652585	8.860608	-0.048551	4.621521
235.288061	7357.637497	8.865613	-0.048569	4.623954
235.469526	7365.709791	8.870618	-0.048608	4.626413
235.438388	7373.738025	8.875623	-0.048608	4.628857
235.723158	7381.763698	8.880627	-0.048666	4.631298
235.784359	7389.780059	8.885632	-0.048683	4.633736
235.784342	7397.749200	8.890637	-0.048688	4.636158
235.990307	7405.752699	8.895642	-0.048731	4.638589
236.003347	7413.771415	8.900647	-0.048739	4.641024
236.045238	7421.735758	8.905651	-0.048752	4.643441
236.292047	7429.784045	8.910656	-0.048803	4.645881
236.406630	7437.780697	8.915661	-0.048830	4.648305
236.500280	7445.829961	8.920666	-0.048853	4.650744
236.667751	7453.873402	8.925671	-0.048889	4.653179
236.917079	7461.890433	8.930675	-0.048941	4.655605
236.921415	7469.880989	8.935680	-0.048947	4.658022
237.032358	7477.877117	8.940685	-0.048973	4.660440
237.370247	7485.928936	8.945690	-0.049041	4.662872
237.380574	7493.891782	8.950695	-0.049048	4.665277
237.405250	7501.916743	8.955699	-0.049058	4.667700
237.498356	7509.919273	8.960704	-0.049081	4.670114
237.594695	7518.016102	8.965709	-0.049104	4.672555
237.923773	7526.092405	8.970714	-0.049170	4.674989
238.016997	7534.046452	8.975719	-0.049193	4.677385
238.281018	7542.027275	8.980723	-0.049247	4.679787
238.301127	7550.047338	8.985728	-0.049256	4.682200
238.299727	7557.992524	8.990733	-0.049261	4.684590
238.448522	7566.079756	8.995738	-0.049294	4.687021
238.682039	7574.033512	9.000743	-0.049343	4.689410
238.918551	7582.037197	9.005747	-0.049392	4.691813
239.038900	7590.063084	9.010752	-0.049420	4.694222
239.111424	7598.137601	9.015757	-0.049439	4.696644
239.453325	7606.143126	9.020762	-0.049508	4.699043
239.454477	7614.152630	9.025767	-0.049513	4.701444
239.700682	7622.163794	9.030771	-0.049564	4.703843
239.968258	7630.222075	9.035776	-0.049619	4.706254
239.916319	7638.152803	9.040781	-0.049615	4.708627
240.118419	7646.257581	9.045786	-0.049658	4.711051
240.150811	7654.271260	9.050791	-0.049669	4.713446
240.277437	7662.300245	9.055795	-0.049698	4.715844
240.424511	7670.272883	9.060800	-0.049731	4.718224
240.606717	7678.238397	9.065805	-0.049770	4.720601
240.798471	7686.275087	9.070810	-0.049811	4.722998
240.839447	7694.306234	9.075815	-0.049824	4.725392
241.045824	7702.349255	9.080819	-0.049867	4.727788
241.216780	7710.310139	9.085824	-0.049904	4.730159
241.158503	7718.397775	9.090829	-0.049899	4.732567
241.568470	7726.417383	9.095834	-0.049980	4.734951
241.505590	7734.390371	9.100839	-0.049974	4.737323
241.540100	7742.405081	9.105843	-0.049986	4.739705
241.710840	7750.465174	9.110848	-0.050023	4.742099
241.838696	7758.352283	9.115853	-0.050052	4.744440
242.053079	7766.495741	9.120858	-0.050097	4.746856
242.200611	7774.450063	9.125863	-0.050130	4.749215
242.495091	7782.538515	9.130867	-0.050190	4.751612
242.754141	7790.562280	9.135872	-0.050243	4.753989
242.765971	7798.552569	9.140877	-0.050251	4.756356
242.857235	7806.549876	9.145882	-0.050273	4.758723
243.030811	7814.525787	9.150887	-0.050310	4.761082
243.097754	7822.518185	9.155891	-0.050328	4.763445
243.127141	7830.566955	9.160896	-0.050339	4.765824
243.429872	7838.558653	9.165901	-0.050401	4.768184
243.593102	7846.616142	9.170906	-0.050436	4.770563
243.398314	7854.641435	9.175911	-0.050405	4.772932
243.582185	7862.699879	9.180915	-0.050445	4.775309
243.751135	7870.649952	9.185920	-0.050481	4.777652
243.885926	7878.621561	9.190925	-0.050512	4.780001
244.179524	7886.685165	9.195930	-0.050572	4.782375
244.215360	7894.687851	9.200935	-0.050584	4.784731
244.338041	7902.698891	9.205939	-0.050612	4.787087
244.354358	7910.701819	9.210944	-0.050620	4.789441
244.633074	7918.728374	9.215949	-0.050677	4.791799
244.786225	7926.791194	9.220954	-0.050711	4.794168
244.771453	7934.791807	9.225959	-0.050713	4.796517
244.952227	7942.762012	9.230963	-0.050752	4.798856
244.972229	7950.790177	9.235968	-0.050761	4.801211
245.149109	7958.750144	9.240973	-0.050800	4.803545
245.224236	7966.844603	9.245978	-0.050819	4.805917
245.223174	7974.798002	9.250983	-0.050824	4.808247
245.500153	7982.864178	9.255987	-0.050881	4.810607
245.520544	7990.279449	9.260992	-0.050889	4.812777
245.718475	7994.799814	9.265997	-0.050929	4.814099

245.750896	7997.228595	9.271002	-0.050937	4.814809
245.754680	7998.490427	9.276007	-0.050938	4.815178
245.836122	7998.987089	9.281011	-0.050954	4.815323
246.021971	7999.826028	9.286016	-0.050989	4.815567
245.978024	7999.844536	9.291021	-0.050981	4.815573
246.101392	7999.836932	9.296026	-0.051004	4.815570
246.071696	7999.818303	9.301031	-0.050998	4.815565
246.166623	7999.867890	9.306035	-0.051016	4.815579
246.039687	7999.786829	9.311040	-0.050993	4.815556
246.085959	7999.800394	9.316045	-0.051001	4.815560
246.256852	7999.829861	9.321050	-0.051033	4.815567
246.296147	7999.815555	9.326055	-0.051040	4.815563
246.306914	7999.823206	9.331059	-0.051042	4.815565
246.329257	7999.802219	9.336064	-0.051047	4.815559
246.473916	7999.819516	9.341069	-0.051074	4.815563
246.517721	7999.834109	9.346074	-0.051082	4.815567
246.529752	7999.794805	9.351079	-0.051084	4.815556
246.690032	7999.832641	9.356083	-0.051114	4.815566
246.698142	7999.813559	9.361088	-0.051116	4.815561
246.783237	7999.842701	9.366093	-0.051131	4.815569
246.961080	7999.840253	9.371098	-0.051165	4.815567
246.722326	7999.812892	9.376103	-0.051120	4.815560
246.832510	7999.844578	9.381107	-0.051141	4.815569
246.749103	7999.804792	9.386112	-0.051125	4.815558
246.904929	7999.827609	9.391117	-0.051154	4.815564
246.829442	7999.853078	9.396122	-0.051140	4.815572
246.827776	7999.842378	9.401127	-0.051140	4.815568
246.967701	7999.849990	9.406131	-0.051166	4.815570
246.797104	7999.818398	9.411136	-0.051134	4.815562
247.030963	7999.814723	9.416141	-0.051178	4.815559
247.115676	7999.840657	9.421146	-0.051194	4.815567
247.075965	7999.816527	9.426151	-0.051186	4.815560
246.840595	7999.847942	9.431155	-0.051143	4.815570
246.876398	7999.843188	9.436160	-0.051149	4.815568
246.912468	7999.874738	9.441165	-0.051156	4.815577
247.255231	7999.864291	9.446170	-0.051220	4.815573
247.053751	7999.823655	9.451175	-0.051182	4.815562
247.243240	7999.861967	9.456179	-0.051218	4.815572
247.276293	7999.819800	9.461184	-0.051224	4.815560
247.139037	7999.843198	9.466189	-0.051198	4.815567
247.360655	7999.856408	9.471194	-0.051240	4.815570
247.164620	7999.816929	9.476199	-0.051203	4.815559
247.382496	7999.851431	9.481203	-0.051244	4.815568
247.301069	7999.852247	9.486208	-0.051229	4.815569
247.031413	7999.828654	9.491213	-0.051178	4.815563
247.161586	7999.845718	9.496218	-0.051203	4.815568
247.074095	7999.819744	9.501223	-0.051186	4.815561
247.166470	7999.842600	9.506227	-0.051204	4.815567
247.391347	7999.837713	9.511232	-0.051246	4.815564
247.334923	7999.835732	9.516237	-0.051235	4.815564
247.278020	7999.865773	9.521242	-0.051225	4.815573
247.165620	7999.823380	9.526247	-0.051204	4.815561
247.322412	7999.847282	9.531251	-0.051233	4.815567
247.226131	7999.825436	9.536256	-0.051215	4.815562
247.286302	7999.849905	9.541261	-0.051226	4.815568
247.242497	7999.842790	9.546266	-0.051218	4.815567
247.202105	7999.803702	9.551271	-0.051211	4.815555
247.447851	7999.839725	9.556275	-0.051256	4.815565
247.461357	7999.835676	9.561280	-0.051259	4.815563
247.304797	7999.805378	9.566285	-0.051230	4.815555
247.279005	7999.869022	9.571290	-0.051225	4.815574
247.455897	7999.838799	9.576295	-0.051258	4.815564
247.351241	7999.859524	9.581299	-0.051239	4.815571
247.456245	7999.844149	9.586304	-0.051258	4.815566
247.416860	7999.846716	9.591309	-0.051251	4.815567
247.371847	7999.848123	9.596314	-0.051243	4.815567
247.203835	7999.818707	9.601319	-0.051211	4.815560
247.410847	7999.843424	9.606323	-0.051250	4.815566
247.404181	7999.839048	9.611328	-0.051249	4.815565
247.348206	7999.836007	9.616333	-0.051238	4.815564
247.453308	7999.830243	9.621338	-0.051258	4.815562
247.437624	7999.820382	9.626343	-0.051255	4.815559
247.374808	7999.870613	9.631347	-0.051243	4.815574
247.434020	7999.861968	9.636352	-0.051254	4.815571
247.328780	7999.854924	9.641357	-0.051235	4.815570
247.441793	7999.856762	9.646362	-0.051256	4.815570
247.395425	7999.826118	9.651367	-0.051247	4.815561
247.439170	7999.827899	9.656371	-0.051256	4.815561
247.468787	7999.809165	9.661376	-0.051261	4.815556
247.396394	7999.818669	9.666381	-0.051248	4.815559
247.380384	7999.841901	9.671386	-0.051245	4.815566
247.597313	7999.847561	9.676391	-0.051285	4.815566
247.723230	7999.860285	9.681395	-0.051309	4.815569
247.580996	7999.823814	9.686400	-0.051282	4.815559
247.505243	7999.820451	9.691405	-0.051268	4.815559
247.645677	7999.854764	9.696410	-0.051294	4.815568
247.593893	7999.821897	9.701415	-0.051285	4.815559
247.619061	7999.839391	9.706419	-0.051289	4.815564
247.886819	7999.836268	9.711424	-0.051339	4.815562
247.758361	7999.838456	9.716429	-0.051315	4.815563
247.663117	7999.849724	9.721434	-0.051298	4.815567
247.747440	7999.822269	9.726439	-0.051313	4.815558
247.856644	7999.834722	9.731443	-0.051334	4.815561
247.794767	7999.818773	9.736448	-0.051322	4.815557
247.846667	7999.833499	9.741453	-0.051332	4.815561
247.881599	7999.853287	9.746458	-0.051339	4.815567
247.885195	7999.828792	9.751463	-0.051339	4.815559
247.867449	7999.839183	9.756467	-0.051336	4.815562
247.950803	7999.834134	9.761472	-0.051352	4.815561
247.721678	7999.840025	9.766477	-0.051309	4.815563
247.563371	7999.852405	9.771482	-0.051279	4.815568
247.690856	7999.798959	9.776487	-0.051303	4.815552
247.799753	7999.831693	9.781491	-0.051324	4.815561
247.853281	7999.927588	9.786496	-0.051334	4.815588
247.938914	7999.877733	9.791501	-0.051350	4.815573
247.999111	7999.834939	9.796506	-0.051361	4.815561
247.902265	7999.817355	9.801511	-0.051343	4.815556
247.904335	7999.847286	9.806515	-0.051343	4.815565
247.993692	7999.841266	9.811520	-0.051360	4.815562
247.953454	7999.870511	9.816525	-0.051352	4.815571
247.997188	7999.860547	9.821530	-0.051361	4.815568
247.878089	7999.823383	9.826535	-0.051338	4.815558
247.877019	7999.867143	9.831539	-0.051338	4.815571
247.853387	7999.927619	9.836544	-0.051334	4.815588
247.823914	7999.792617	9.841549	-0.051328	4.815549
248.136335	7999.918341	9.846554	-0.051387	4.815584
248.027745	7999.798069	9.851559	-0.051366	4.815550
248.074537	7999.909870	9.856563	-0.051375	4.815582
248.134902	7999.848928	9.861568	-0.051386	4.815564
248.064840	7999.836048	9.866573	-0.051373	4.815561
247.980202	7999.878451	9.871578	-0.051358	4.815573
247.821909	7999.849192	9.876583	-0.051328	4.815566
248.019026	7999.871614	9.881587	-0.051365	4.815571
248.122226	7999.817774	9.886592	-0.051384	4.815555
248.069563	7999.834005	9.891597	-0.051375	4.815560
247.969959	7999.878300	9.896602	-0.051356	4.815573
247.742997	7999.850061	9.901607	-0.051314	4.815566
247.765295	7999.856832	9.906611	-0.051318	4.815568
247.828650	7999.847187	9.911616	-0.051330	4.815565
247.940548	7999.845804	9.916621	-0.051351	4.815564
248.238403	7999.874133	9.921626	-0.051406	4.815571
247.876725	7999.824488	9.926631	-0.051339	4.815558
248.097692	7999.859042	9.931635	-0.051380	4.815567
247.935033	7999.962103	9.936640	-0.051350	4.815598
247.942476	7999.856527	9.941645	-0.051351	4.815567
247.972284	7999.873029	9.946650	-0.051357	4.815572
247.940399	7999.828740	9.951655	-0.051351	4.815559
247.788446	7999.844425	9.956659	-0.051323	4.815564
248.047956	7999.847575	9.961664	-0.051371	4.815564
247.980155	7999.840071	9.966669	-0.051358	4.815562
247.976802	7999.862441	9.971674	-0.051358	4.815569
247.835851	7999.825989	9.976679	-0.051332	4.815559
248.132710	7999.854302	9.981683	-0.051387	4.815566
248.078348	7999.847016	9.986688	-0.051377	4.815564
248.061960	7999.836076	9.991693	-0.051374	4.815561
248.191407	7999.873415	9.996698	-0.051398	4.815571
248.227005	7999.919906	10.001703	-0.051405	4.815584
248.195684	7999.804091	10.006707	-0.051399	4.815551
248.209531	7999.837417	10.011712	-0.051401	4.815560
248.110769	7999.835816	10.016717	-0.051383	4.815560
248.238861	7999.863524	10.021722	-0.051407	4.815568
248.074229	7999.834161	10.026727	-0.051376	4.815560
248.195307	7999.867093	10.031731	-0.051399	4.815569
248.210789	7999.852400	10.036736	-0.051402	4.815565
248.032595	7999.940261	10.041741	-0.051369	4.815591
248.121312	7999.855223	10.046746	-0.051385	4.815566
248.179024	7999.856164	10.051751	-0.051396	4.815566
248.004796	7999.873623	10.056755	-0.051364	4.815572
248.095909	7999.860158	10.061760	-0.051381	4.815567
248.210554	7999.837466	10.066765	-0.051402	4.815560
248.118802	7999.869077	10.071770	-0.051385	4.815570
247.995414	7999.822234	10.076775	-0.051362	4.815557
248.395470	7999.850088	10.081779	-0.051436	4.815563
248.403322	7999.852354	10.086784	-0.051438	4.815564
248.142734	7999.827838	10.091789	-0.051389	4.815558
248.418127	7999.859006	10.096794	-0.051441	4.815566
248.372732	7999.902047	10.101799	-0.051432	4.815578
248.346145	7999.810865	10.106803	-0.051427	4.815552
248.312045	7999.830600	10.111808	-0.051421	4.815558
248.108148	7999.844374	10.116813	-0.051383	4.815563
248.301974	7999.871014	10.121818	-0.051419	4.815570
248.179673	7999.918144	10.126823	-0.051397	4.815584
248.488863	7999.844161	10.131827	-0.051454	4.815561
248.562536	7999.843225	10.136832	-0.051468	4.815560
248.527720	7999.835189	10.141837	-0.051462	4.815558
248.595495	7999.857647	10.146842	-0.051474	4.815564
248.459212	7999.812729	10.151847	-0.051449	4.815552
248.254169	7999.861717	10.156851	-0.051411	4.815567
248.316193	7999.880878	10.161856	-0.051422	4.815572
248.330788	7999.857629	10.166861	-0.051425	4.815566
248.423503	7999.887966	10.171866	-0.051442	4.815574
248.279027	7999.915517	10.176871	-0.051416	4.815583
248.375136	7999.859426	10.181875	-0.051433	4.815566
248.341716	7999.849277	10.186880	-0.051427	4.815563
248.165149	7999.838939	10.191885	-0.051394	4.815561
248.305857	7999.862581	10.196890	-0.051421	4.815567
248.453929	7999.847906	10.201895	-0.051448	4.815562
248.318364	7999.867061	10.206899	-0.051423	4.815568
248.209467	7999.849280	10.211904	-0.051403	4.815564
248.334804	7999.863063	10.216909	-0.051426	4.815567
248.215426	7999.876074	10.221914	-0.051404	4.815572
248.225844	7999.826066	10.226919	-0.051406	4.815557
248.283769	7999.870784	10.231923	-0.051417	4.815570
248.443892	7999.848831	10.236928	-0.051447	4.815562
248.210983	7999.842916	10.241933	-0.051403	4.815562
248.450891	7999.892726	10.246938	-0.051448	4.815575
248.452672	7999.847915	10.251943	-0.051448	4.815562
248.510152	7999.840311	10.256947	-0.051459	4.815560
248.329420	7999.934537	10.261952	-0.051425	4.815588
248.397591	7999.836353	10.266957	-0.051438	4.815559
248.553021	7999.882656	10.271962	-0.051467	4.815572
248.504254	7999.848768	10.276967	-0.051458	4.815562
248.511507	7999.864904	10.281971	-0.051459	4.815567
248.608839	7999.863285	10.286976	-0.051478	4.815566
248.424810	7999.859231	10.291981	-0.051443	4.815566
248.419380	7999.853807	10.296986	-0.051442	4.815564
248.558145	7999.833643	10.301991	-0.051468	4.815557
248.575218	7999.858480	10.306995	-0.051472	4.815565
248.345992	7999.848354	10.312000	-0.051429	4.815563
248.429676	7999.831565	10.317005	-0.051444	4.815557
248.676121	7999.862264	10.322010	-0.051490	4.815565
248.345270	7999.852622	10.327015	-0.051429	4.815564
248.312479	7999.864904	10.332019	-0.051423	4.815568
248.532926	7999.853540	10.337024	-0.051464	4.815563
248.691552	7999.914843	10.342029	-0.051493	4.815581
248.676948	7999.850548	10.347034	-0.051491	4.815562
248.429093	7999.856133	10.352039	-0.051445	4.815565
248.510591	7999.857460	10.357043	-0.051460	4.815565
248.422510	7999.858168	10.362048	-0.051443	4.815565
248.349585	7999.839903	10.367053	-0.051430	4.815560
248.485484	7999.867738	10.372058	-0.051455	4.815568
248.430605	7999.858308	10.377063	-0.051445	4.815565
248.387257	7999.870419	10.382067	-0.051437	4.815569
248.624930	7999.862539	10.387072	-0.051481	4.815566
248.311234	7999.861716	10.392077	-0.051423	4.815567
248.502954	7999.891526	10.397082	-0.051459	4.815575
248.620720	7999.852870	10.402087	-0.051481	4.815563
248.729078	7999.882393	10.407091	-0.051501	4.815571
248.661928	7999.883441	10.412096	-0.051488	4.815572
248.568723	7999.850966	10.417101	-0.051471	4.815562
248.676609	7999.858060	10.422106	-0.051491	4.815564
248.422537	7999.843259	10.427111	-0.051444	4.815561
248.423409	7999.863562	10.432115	-0.051444	4.815567
248.585347	7999.869399	10.437120	-0.051474	4.815568
248.446849	7999.933349	10.442125	-0.051449	4.815587
248.659754	7999.868478	10.447130	-0.051488	4.815567
248.461837	7999.850319	10.452135	-0.051451	4.815563
248.459322	7999.880176	10.457139	-0.051451	4.815572
248.579854	7999.897085	10.462144	-0.051473	4.815576
248.536408	7999.877163	10.467149	-0.051465	4.815570
248.713364	7999.873635	10.472154	-0.051498	4.815568
248.508108	7999.834002	10.477159	-0.051460	4.815558
248.397808	7999.835417	10.482163	-0.051440	4.815559
248.699053	7999.860599	10.487168	-0.051496	4.815565
248.694181	7999.853049	10.492173	-0.051495	4.815562
248.562785	7999.886151	10.497178	-0.051471	4.815573
248.407700	7999.823845	10.502183	-0.051442	4.815555
248.509905	7999.934412	10.507187	-0.051461	4.815587
248.499587	7999.880863	10.512192	-0.051459	4.815572
248.279852	7999.853807	10.517197	-0.051418	4.815565
248.390459	7999.891908	10.522202	-0.051439	4.815575
248.482260	7999.861372	10.527207	-0.051456	4.815566
248.450674	7999.858726	10.532211	-0.051450	4.815565
248.547914	7999.876324	10.537216	-0.051468	4.815570
248.543045	7999.852759	10.542221	-0.051467	4.815563
248.550275	7999.882775	10.547226	-0.051469	4.815572
248.628956	7999.865905	10.552231	-0.051483	4.815567
248.645583	7999.860840	10.557235	-0.051486	4.815565
248.515909	7999.851263	10.562240	-0.051462	4.815563
248.325259	7999.830018	10.567245	-0.051427	4.815557
248.523570	7999.870611	10.572250	-0.051464	4.815568
248.653240	7999.836419	10.577255	-0.051488	4.815558
248.477415	7999.853852	10.582259	-0.051455	4.815564
248.666133	7999.865462	10.587264	-0.051490	4.815566
248.534880	7999.850521	10.592269	-0.051466	4.815562
248.449141	7999.848063	10.597274	-0.051450	4.815562
248.558472	7999.839166	10.602279	-0.051470	4.815559
248.512497	7999.868317	10.607283	-0.051462	4.815568
248.713374	7999.864109	10.612288	-0.051499	4.815566
248.563708	7999.855275	10.617293	-0.051471	4.815564
248.627632	7999.862722	10.622298	-0.051483	4.815566
248.642823	7999.931304	10.627303	-0.051486	4.815586
248.643878	7999.846977	10.632307	-0.051487	4.815561
248.732042	7999.890052	10.637312	-0.051503	4.815573
248.750323	7999.839103	10.642317	-0.051506	4.815558
248.697346	7999.840381	10.647322	-0.051497	4.815559
248.498441	7999.842491	10.652327	-0.051460	4.815560
248.810932	7999.880669	10.657331	-0.051518	4.815570
248.855755	7999.858978	10.662336	-0.051526	4.815563
248.603812	7999.849550	10.667341	-0.051479	4.815562
248.587828	7999.857835	10.672346	-0.051476	4.815564
248.623041	7999.842394	10.677351	-0.051483	4.815560
248.563080	7999.870251	10.682355	-0.051472	4.815568
248.808298	7999.877441	10.687360	-0.051518	4.815569
248.887629	7999.839228	10.692365	-0.051532	4.815557
248.894609	7999.836141	10.697370	-0.051534	4.815557
248.537281	7999.921093	10.702375	-0.051467	4.815583
248.648819	7999.880200	10.707379	-0.051488	4.815571
248.913168	7999.878092	10.712384	-0.051537	4.815569
248.718106	7999.859978	10.717389	-0.051501	4.815564
248.786577	7999.885650	10.722394	-0.051514	4.815572
248.800391	7999.868795	10.727399	-0.051516	4.815567
248.750411	7999.851970	10.732403	-0.051507	4.815562
248.804650	7999.857125	10.737408	-0.051517	4.815563
248.756331	7999.837125	10.742413	-0.051508	4.815557
248.763779	7999.865009	10.747418	-0.051510	4.815566
248.605565	7999.858171	10.752423	-0.051480	4.815564
248.893540	7999.872461	10.757427	-0.051534	4.815567
248.897653	7999.865057	10.762432	-0.051535	4.815565
248.842692	7999.864167	10.767437	-0.051524	4.815565
248.843549	7999.881267	10.772442	-0.051525	4.815570
248.703025	7999.850160	10.777447	-0.051499	4.815562
248.596760	7999.851639	10.782451	-0.051479	4.815562
248.651122	7999.873879	10.787456	-0.051489	4.815569
248.601105	7999.852783	10.792461	-0.051480	4.815563
249.057510	7999.889029	10.797466	-0.051565	4.815571
248.895812	7999.837291	10.802471	-0.051535	4.815557
248.818180	7999.869131	10.807475	-0.051520	4.815567
248.950945	7999.863817	10.812480	-0.051545	4.815564
248.628784	7999.841503	10.817485	-0.051485	4.815559
248.681365	7999.878662	10.822490	-0.051495	4.815570
248.610248	7999.852953	10.827495	-0.051482	4.815563
248.675295	7999.861486	10.832499	-0.051494	4.815565
248.824815	7999.874595	10.837504	-0.051522	4.815568
248.795696	7999.960609	10.842509	-0.051516	4.815593
248.953045	7999.885226	10.847514	-0.051546	4.815571
248.890656	7999.881013	10.852519	-0.051534	4.815570
248.850414	7999.896377	10.857523	-0.051527	4.815574
248.942144	7999.893600	10.862528	-0.051544	4.815573
248.748119	7999.871232	10.867533	-0.051508	4.815567
248.753014	7999.887330	10.872538	-0.051508	4.815572
248.784593	7999.869695	10.877543	-0.051514	4.815567
248.905570	7999.864190	10.882547	-0.051537	4.815565
248.801647	7999.892400	10.887552	-0.051518	4.815573
248.755417	7999.867095	10.892557	-0.051509	4.815566
248.900417	7999.899349	10.897562	-0.051536	4.815575
248.780997	7999.871787	10.902567	-0.051514	4.815567
248.831220	7999.893960	10.907571	-0.051523	4.815574
248.981878	7999.888937	10.912576	-0.051551	4.815572
248.779575	7999.844013	10.917581	-0.051514	4.815559
248.687635	7999.876688	10.922586	-0.051497	4.815569
248.819222	7999.848934	10.927591	-0.051521	4.815561
248.755249	7999.862845	10.932595	-0.051509	4.815565
248.707612	7999.872751	10.937600	-0.051500	4.815568
248.903692	7999.839638	10.942605	-0.051537	4.815557
248.992799	7999.860307	10.947610	-0.051554	4.815563
248.813047	7999.831765	10.952615	-0.051520	4.815556
248.756305	7999.853268	10.957619	-0.051510	4.815562
249.017013	7999.895944	10.962624	-0.051558	4.815573
248.882353	7999.828629	10.967629	-0.051533	4.815554
248.911802	7999.895308	10.972634	-0.051539	4.815574
248.854031	7999.866612	10.977639	-0.051528	4.815566
249.039977	7999.959323	10.982643	-0.051563	4.815592
248.996591	7999.870002	10.987648	-0.051555	4.815566
248.864023	7999.856106	10.992653	-0.051530	4.815562
248.995206	7999.883865	10.997658	-0.051554	4.815570
248.958938	7999.864061	11.002663	-0.051548	4.815564
248.772656	7999.852495	11.007667	-0.051513	4.815562
248.896654	7999.867325	11.012672	-0.051536	4.815566
248.838549	7999.873858	11.017677	-0.051525	4.815568
248.695054	7999.898222	11.022682	-0.051499	4.815576
248.870708	7999.870116	11.027687	-0.051531	4.815567
248.947177	7999.878835	11.032691	-0.051546	4.815569
248.924161	7999.867787	11.037696	-0.051541	4.815566
248.897489	7999.860951	11.042701	-0.051537	4.815564
248.842805	7999.878216	11.047706	-0.051526	4.815569
248.945306	7999.852124	11.052711	-0.051545	4.815561
248.855275	7999.885898	11.057715	-0.051529	4.815571
248.869803	7999.874393	11.062720	-0.051532	4.815568
248.753032	7999.860754	11.067725	-0.051510	4.815564
248.770532	7999.868515	11.072730	-0.051513	4.815567
248.747531	7999.838249	11.077735	-0.051509	4.815558
248.870458	7999.866941	11.082739	-0.051532	4.815566
248.886352	7999.869338	11.087744	-0.051535	4.815566
248.765865	7999.854571	11.092749	-0.051512	4.815562
248.877243	7999.882008	11.097754	-0.051533	4.815570
248.750260	7999.844714	11.102759	-0.051510	4.815560
248.682387	7999.850021	11.107763	-0.051497	4.815562
248.693701	7999.873697	11.112768	-0.051499	4.815568
248.867959	7999.855177	11.117773	-0.051532	4.815562
248.970621	7999.887811	11.122778	-0.051551	4.815571
249.008812	7999.867081	11.127783	-0.051558	4.815565
249.139949	7999.862808	11.132787	-0.051582	4.815563
248.972140	7999.887845	11.137792	-0.051551	4.815571
248.867117	7999.938458	11.142797	-0.051532	4.815587
249.061606	7999.880763	11.147802	-0.051568	4.815569
249.065431	7999.850932	11.152807	-0.051569	4.815560
248.760515	7999.864132	11.157811	-0.051512	4.815565
249.020477	7999.857682	11.162816	-0.051560	4.815562
249.200839	7999.831787	11.167821	-0.051594	4.815554
248.968731	7999.873930	11.172826	-0.051551	4.815567
248.844993	7999.867652	11.177831	-0.051528	4.815566
249.073770	7999.871372	11.182835	-0.051570	4.815566
249.104734	7999.886826	11.187840	-0.051576	4.815570
249.017562	7999.844840	11.192845	-0.051560	4.815558
249.130606	7999.882982	11.197850	-0.051581	4.815569
249.080783	7999.881107	11.202855	-0.051572	4.815569
248.875265	7999.863891	11.207859	-0.051534	4.815565
249.034329	7999.875020	11.212864	-0.051563	4.815567
248.864615	7999.853047	11.217869	-0.051532	4.815562
249.058894	7999.885034	11.222874	-0.051568	4.815570
248.995322	7999.851973	11.227879	-0.051556	4.815561
248.924759	7999.862574	11.232883	-0.051543	4.815564
248.908633	7999.866586	11.237888	-0.051540	4.815565
248.932865	7999.837087	11.242893	-0.051544	4.815557
248.963875	7999.877099	11.247898	-0.051550	4.815568
249.130906	7999.864868	11.252903	-0.051581	4.815564
248.965743	7999.867526	11.257907	-0.051551	4.815565
248.875734	7999.879947	11.262912	-0.051534	4.815569
249.083397	7999.928167	11.267917	-0.051573	4.815582
249.146842	7999.870478	11.272922	-0.051585	4.815565
248.946743	7999.854417	11.277927	-0.051547	4.815562
249.171620	7999.857006	11.282931	-0.051589	4.815561
249.155917	7999.882379	11.287936	-0.051586	4.815569
248.787679	7999.835826	11.292941	-0.051518	4.815557
248.905558	7999.847353	11.297946	-0.051540	4.815560
249.077136	7999.853347	11.302951	-0.051572	4.815561
248.938959	7999.832954	11.307955	-0.051546	4.815555
248.998029	7999.849933	11.312960	-0.051557	4.815560
249.178185	7999.845389	11.317965	-0.051591	4.815558
249.080003	7999.872624	11.322970	-0.051572	4.815566
248.899713	7999.855818	11.327975	-0.051539	4.815562
248.905158	7999.871925	11.332979	-0.051540	4.815567
249.157355	7999.898447	11.337984	-0.051587	4.815573
249.031775	7999.849431	11.342989	-0.051564	4.815560
249.172512	7999.872007	11.347994	-0.051590	4.815566
249.207818	7999.956933	11.352999	-0.051596	4.815590
248.929349	7999.839234	11.358003	-0.051545	4.815557
249.003217	7999.872468	11.363008	-0.051558	4.815567
248.924615	7999.859449	11.368013	-0.051544	4.815563
248.982683	7999.848651	11.373018	-0.051555	4.815560
248.857956	7999.847695	11.378023	-0.051531	4.815560
248.883269	7999.823553	11.383027	-0.051536	4.815553
249.256440	7999.890478	11.388032	-0.051606	4.815571
249.068893	7999.851132	11.393037	-0.051571	4.815560
249.198796	7999.885276	11.398042	-0.051595	4.815569
249.328459	7999.883116	11.403047	-0.051619	4.815568
249.160691	7999.873986	11.408051	-0.051588	4.815566
249.076921	7999.930284	11.413056	-0.051573	4.815583
248.960218	7999.837636	11.418061	-0.051551	4.815557
249.029785	7999.886816	11.423066	-0.051564	4.815571
249.087725	7999.874948	11.428071	-0.051575	4.815567
249.153491	7999.872816	11.433075	-0.051587	4.815566
249.441233	7999.878563	11.438080	-0.051640	4.815566
249.305807	7999.835792	11.443085	-0.051615	4.815554
248.955521	7999.847187	11.448090	-0.051550	4.815559
249.132676	7999.846865	11.453095	-0.051583	4.815558
249.101385	7999.834615	11.458099	-0.051577	4.815555
249.131235	7999.884217	11.463104	-0.051583	4.815569
249.178045	7999.863627	11.468109	-0.051592	4.815563
249.342210	7999.884449	11.473114	-0.051622	4.815568
249.177211	7999.892447	11.478119	-0.051592	4.815572
249.218976	7999.876046	11.483123	-0.051599	4.815567
249.379077	7999.890395	11.488128	-0.051629	4.815570
249.149981	7999.842899	11.493133	-0.051587	4.815557
249.163686	7999.857005	11.498138	-0.051589	4.815561
249.203337	7999.875803	11.503143	-0.051597	4.815567
249.143167	7999.873761	11.508147	-0.051585	4.815566
249.101776	7999.873091	11.513152	-0.051578	4.815566
248.867512	7999.850069	11.518157	-0.051534	4.815561
249.036374	7999.861358	11.523162	-0.051566	4.815563
249.037923	7999.860318	11.528167	-0.051566	4.815563
249.111622	7999.836961	11.533171	-0.051580	4.815556
249.262131	7999.897066	11.538176	-0.051608	4.815572
249.325726	7999.878884	11.543181	-0.051620	4.815567
249.109048	7999.883907	11.548186	-0.051579	4.815569
249.091283	7999.877215	11.553191	-0.051576	4.815567
249.202477	7999.874755	11.558195	-0.051597	4.815566
249.093278	7999.883660	11.563200	-0.051577	4.815569
248.909275	7999.864658	11.568205	-0.051542	4.815565
249.032509	7999.880543	11.573210	-0.051565	4.815569
249.005212	7999.872629	11.578215	-0.051560	4.815567
248.941112	7999.945261	11.583219	-0.051548	4.815588
249.129392	7999.879991	11.588224	-0.051583	4.815568
249.009156	7999.853483	11.593229	-0.051561	4.815561
249.181461	7999.906468	11.598234	-0.051593	4.815576
249.254763	7999.891647	11.603239	-0.051607	4.815571
249.192482	7999.893841	11.608243	-0.051595	4.815572
249.303710	7999.889245	11.613248	-0.051616	4.815570
248.983487	7999.859487	11.618253	-0.051556	4.815563
249.177823	7999.890408	11.623258	-0.051593	4.815571
249.127716	7999.872514	11.628263	-0.051583	4.815566
248.996691	7999.859711	11.633267	-0.051559	4.815563
249.184246	7999.881980	11.638272	-0.051594	4.815568
248.983372	7999.840282	11.643277	-0.051557	4.815557
248.991845	7999.874589	11.648282	-0.051558	4.815567
249.075330	7999.862068	11.653287	-0.051574	4.815563
249.126254	7999.871440	11.658291	-0.051583	4.815566
249.011152	7999.874911	11.663296	-0.051562	4.815567
249.206805	7999.858875	11.668301	-0.051598	4.815562
249.264304	7999.868354	11.673306	-0.051609	4.815564
249.211573	7999.858958	11.678311	-0.051599	4.815562
249.134023	7999.874784	11.683315	-0.051585	4.815567
249.003323	7999.858783	11.688320	-0.051561	4.815562
249.156609	7999.859142	11.693325	-0.051589	4.815562
248.935103	7999.873696	11.698330	-0.051548	4.815567
249.013050	7999.864289	11.703335	-0.051563	4.815564
249.058019	7999.883174	11.708339	-0.051571	4.815569
249.245753	7999.876618	11.713344	-0.051606	4.815567
249.029423	7999.827195	11.718349	-0.051566	4.815553
249.151314	7999.875089	11.723354	-0.051588	4.815567
249.256752	7999.847977	11.728359	-0.051608	4.815558
249.190703	7999.916308	11.733363	-0.051596	4.815578
249.140600	7999.889872	11.738368	-0.051587	4.815571
248.993414	7999.868265	11.743373	-0.051559	4.815565
248.962749	7999.872040	11.748378	-0.051554	4.815567
249.150360	7999.855873	11.753383	-0.051588	4.815561
249.115032	7999.881994	11.758387	-0.051582	4.815569
248.970399	7999.887121	11.763392	-0.051555	4.815571
248.818326	7999.862232	11.768397	-0.051527	4.815564
248.971840	7999.872203	11.773402	-0.051555	4.815567
249.118939	7999.866054	11.778407	-0.051583	4.815564
248.911195	7999.886171	11.783411	-0.051544	4.815571
249.039054	7999.875439	11.788416	-0.051568	4.815567
249.168754	7999.840180	11.793421	-0.051592	4.815556
249.152412	7999.891167	11.798426	-0.051589	4.815571
249.025802	7999.911535	11.803431	-0.051566	4.815578
249.205584	7999.901647	11.808435	-0.051599	4.815574
249.368439	7999.907499	11.813440	-0.051630	4.815575
249.223581	7999.849627	11.818445	-0.051603	4.815559
249.258839	7999.896115	11.823450	-0.051609	4.815572
249.367357	7999.894678	11.828455	-0.051629	4.815571
249.254221	7999.875759	11.833459	-0.051608	4.815566
249.254917	7999.908872	11.838464	-0.051609	4.815576
249.341845	7999.885731	11.843469	-0.051625	4.815569
249.354158	7999.900882	11.848474	-0.051627	4.815573
249.352219	7999.870957	11.853479	-0.051627	4.815564
249.213268	7999.869770	11.858483	-0.051601	4.815565
249.447318	7999.878915	11.863488	-0.051645	4.815566
249.106228	7999.860563	11.868493	-0.051581	4.815562
249.096748	7999.866818	11.873498	-0.051579	4.815564
249.228470	7999.882841	11.878503	-0.051604	4.815568
249.133162	7999.874889	11.883507	-0.051586	4.815567
249.254517	7999.881135	11.888512	-0.051609	4.815568
249.157316	7999.867814	11.893517	-0.051591	4.815564
249.056492	7999.893939	11.898522	-0.051572	4.815572
249.146482	7999.909284	11.903527	-0.051589	4.815577
249.131980	7999.861005	11.908531	-0.051586	4.815562
249.367478	7999.882986	11.913536	-0.051630	4.815568
249.170205	7999.868038	11.918541	-0.051593	4.815564
249.200096	7999.890949	11.923546	-0.051599	4.815571
249.446425	7999.880007	11.928551	-0.051645	4.815567
249.108860	7999.864915	11.933555	-0.051582	4.815564
249.275801	7999.893256	11.938560	-0.051613	4.815571
249.145520	7999.877261	11.943565	-0.051589	4.815567
249.196788	7999.907993	11.948570	-0.051598	4.815576
249.219875	7999.898762	11.953575	-0.051603	4.815573
249.258998	7999.881250	11.958579	-0.051610	4.815568
249.490773	7999.889290	11.963584	-0.051653	4.815569
249.370941	7999.874533	11.968589	-0.051631	4.815565
249.380978	7999.888580	11.973594	-0.051633	4.815569
249.506888	7999.881019	11.978599	-0.051656	4.815567
249.181355	7999.856513	11.983603	-0.051596	4.815561
249.315554	7999.890728	11.988608	-0.051621	4.815570
249.408567	7999.865550	11.993613	-0.051638	4.815562
249.286056	7999.890255	11.998618	-0.051615	4.815570
249.293451	7999.888243	12.003623	-0.051617	4.815570
249.304570	7999.885223	12.008627	-0.051619	4.815569
249.419982	7999.882831	12.013632	-0.051640	4.815567
249.147797	7999.855989	12.018637	-0.051590	4.815561
249.190236	7999.864156	12.023642	-0.051598	4.815563
249.258756	7999.868475	12.028647	-0.051611	4.815564
249.269455	7999.872923	12.033651	-0.051613	4.815565
249.163044	7999.893618	12.038656	-0.051593	4.815572
249.366148	7999.889448	12.043661	-0.051631	4.815570
249.464570	7999.898524	12.048666	-0.051649	4.815572
249.312056	7999.872559	12.053671	-0.051621	4.815565
249.218013	7999.877440	12.058675	-0.051603	4.815567
249.279568	7999.903001	12.063680	-0.051615	4.815574
249.285193	7999.845439	12.068685	-0.051616	4.815557
249.218144	7999.952191	12.073690	-0.051603	4.815589
249.479094	7999.873153	12.078695	-0.051652	4.815564
249.446932	7999.863024	12.083699	-0.051646	4.815562
249.439485	7999.879990	12.088704	-0.051645	4.815567
249.382099	7999.853435	12.093709	-0.051634	4.815559
249.251953	7999.866271	12.098714	-0.051610	4.815563
249.239195	7999.858593	12.103719	-0.051607	4.815561
249.373349	7999.845828	12.108723	-0.051632	4.815557
249.483407	7999.906343	12.113728	-0.051653	4.815574
249.338519	7999.871960	12.118733	-0.051626	4.815565
249.342718	7999.854948	12.123738	-0.051627	4.815560
249.250000	7999.863054	12.128743	-0.051610	4.815562
249.307525	7999.865059	12.133747	-0.051620	4.815563
249.330234	7999.881447	12.138752	-0.051625	4.815567
249.273398	7999.854901	12.143757	-0.051614	4.815560
249.313094	7999.875836	12.148762	-0.051621	4.815566
249.310766	7999.889681	12.153767	-0.051621	4.815570
249.208164	7999.847444	12.158771	-0.051602	4.815558
249.245102	7999.900365	12.163776	-0.051609	4.815573
249.357610	7999.829592	12.168781	-0.051630	4.815552
249.339437	7999.834638	12.173786	-0.051627	4.815554
249.528167	7999.872943	12.178791	-0.051662	4.815564
249.383904	7999.847112	12.183795	-0.051635	4.815557
249.344894	7999.877444	12.188800	-0.051628	4.815566
249.246439	7999.930300	12.193805	-0.051609	4.815582
249.367464	7999.851124	12.198810	-0.051632	4.815558
249.389537	7999.884585	12.203815	-0.051636	4.815568
249.178731	7999.873688	12.208819	-0.051597	4.815566
249.283459	7999.892476	12.213824	-0.051616	4.815571
249.399780	7999.877286	12.218829	-0.051638	4.815566
249.318596	7999.861022	12.223834	-0.051623	4.815562
249.362424	7999.861737	12.228839	-0.051631	4.815562
249.479565	7999.822003	12.233843	-0.051653	4.815549
249.574124	7999.849168	12.238848	-0.051671	4.815557
249.226911	7999.836055	12.243853	-0.051606	4.815555
249.391005	7999.847266	12.248858	-0.051637	4.815557
249.570517	7999.884353	12.253863	-0.051670	4.815567
249.252016	7999.841810	12.258867	-0.051611	4.815556
249.337350	7999.899788	12.263872	-0.051627	4.815573
249.331609	7999.855922	12.268877	-0.051626	4.815560
249.245968	7999.892970	12.273882	-0.051610	4.815571
249.318635	7999.895222	12.278887	-0.051623	4.815572
249.247836	7999.950663	12.283891	-0.051610	4.815588
249.313444	7999.881263	12.288896	-0.051622	4.815567
249.235688	7999.858649	12.293901	-0.051608	4.815561
249.423220	7999.849954	12.298906	-0.051643	4.815558
249.482025	7999.867996	12.303911	-0.051654	4.815563
249.355168	7999.846719	12.308915	-0.051630	4.815557
249.447935	7999.884532	12.313920	-0.051648	4.815568
249.598706	7999.847480	12.318925	-0.051676	4.815556
249.582026	7999.860024	12.323930	-0.051673	4.815560
249.477882	7999.854064	12.328935	-0.051653	4.815559
249.379019	7999.851392	12.333939	-0.051635	4.815558
249.488923	7999.873468	12.338944	-0.051656	4.815564
249.421881	7999.865975	12.343949	-0.051643	4.815562
249.612609	7999.887229	12.348954	-0.051679	4.815568
249.538536	7999.897773	12.353959	-0.051665	4.815571
249.310773	7999.881262	12.358963	-0.051622	4.815567
249.332906	7999.882692	12.363968	-0.051627	4.815568
249.520037	7999.868653	12.368973	-0.051662	4.815563
249.305037	7999.933495	12.373978	-0.051622	4.815583
249.516857	7999.864336	12.378983	-0.051661	4.815562
249.353029	7999.874489	12.383987	-0.051631	4.815565
249.460526	7999.887984	12.388992	-0.051651	4.815569
249.347034	7999.850908	12.393997	-0.051629	4.815558
249.397549	7999.872019	12.399002	-0.051639	4.815564
249.439898	7999.883387	12.404007	-0.051647	4.815567
249.331832	7999.852806	12.409011	-0.051627	4.815559
249.360481	7999.886373	12.414016	-0.051632	4.815569
249.396142	7999.862398	12.419021	-0.051639	4.815562
249.532620	7999.844333	12.424026	-0.051664	4.815556
249.556830	7999.866083	12.429031	-0.051669	4.815562
249.515203	7999.835514	12.434035	-0.051661	4.815553
249.680240	7999.899059	12.439040	-0.051692	4.815571
249.316474	7999.847238	12.444045	-0.051624	4.815557
249.342817	7999.865821	12.449050	-0.051629	4.815563
249.454783	7999.875117	12.454055	-0.051650	4.815565
249.315535	7999.861112	12.459059	-0.051624	4.815562
249.509841	7999.863205	12.464064	-0.051660	4.815561
249.595931	7999.825102	12.469069	-0.051676	4.815550
249.696602	7999.924971	12.474074	-0.051695	4.815578
249.501234	7999.874819	12.479079	-0.051659	4.815565
249.384471	7999.851570	12.484083	-0.051637	4.815558
249.482934	7999.886273	12.489088	-0.051655	4.815568
249.346148	7999.827464	12.494093	-0.051630	4.815552
249.380553	7999.848312	12.499098	-0.051636	4.815557
249.596078	7999.858224	12.504103	-0.051677	4.815559
249.445323	7999.853642	12.509107	-0.051649	4.815559
249.365643	7999.879043	12.514112	-0.051634	4.815567
249.550428	7999.869236	12.519117	-0.051668	4.815563
249.480849	7999.853160	12.524122	-0.051655	4.815558
249.519194	7999.870870	12.529127	-0.051662	4.815563
249.513809	7999.852634	12.534131	-0.051661	4.815558
249.576285	7999.877142	12.539136	-0.051673	4.815565
249.467059	7999.930891	12.544141	-0.051653	4.815581
249.430275	7999.856624	12.549146	-0.051646	4.815560
249.581000	7999.854806	12.554151	-0.051674	4.815558
249.472433	7999.847706	12.559155	-0.051654	4.815557
249.424617	7999.901385	12.564160	-0.051645	4.815573
249.578377	7999.855840	12.569165	-0.051674	4.815559
249.598295	7999.868979	12.574170	-0.051677	4.815562
249.595667	7999.871075	12.579175	-0.051677	4.815563
249.339612	7999.839156	12.584179	-0.051629	4.815555
249.606532	7999.873393	12.589184	-0.051679	4.815564
249.492643	7999.874748	12.594189	-0.051658	4.815565
249.490155	7999.897133	12.599194	-0.051658	4.815571
249.438315	7999.895225	12.604199	-0.051648	4.815571
249.434550	7999.863136	12.609203	-0.051647	4.815562
249.325455	7999.901939	12.614208	-0.051627	4.815573
249.364698	7999.865210	12.619213	-0.051634	4.815562
249.370080	7999.862097	12.624218	-0.051635	4.815562
249.412713	7999.859590	12.629223	-0.051643	4.815561
249.410505	7999.861692	12.634227	-0.051643	4.815561
249.745256	7999.887422	12.639232	-0.051705	4.815567
249.428248	7999.844903	12.644237	-0.051646	4.815556
249.560651	7999.868412	12.649242	-0.051671	4.815562
249.664297	7999.874370	12.654247	-0.051690	4.815564
249.540016	7999.948161	12.659251	-0.051667	4.815586
249.615126	7999.895999	12.664256	-0.051681	4.815570
249.484014	7999.885330	12.669261	-0.051657	4.815568
249.560397	7999.896183	12.674266	-0.051671	4.815571
249.509313	7999.887882	12.679271	-0.051662	4.815568
249.455393	7999.866722	12.684275	-0.051652	4.815562
249.401921	7999.881872	12.689280	-0.051642	4.815567
249.629860	7999.848209	12.694285	-0.051684	4.815556
249.673818	7999.841453	12.699290	-0.051692	4.815554
249.578110	7999.872999	12.704295	-0.051675	4.815564
249.473233	7999.852079	12.709299	-0.051655	4.815558
249.396312	7999.882863	12.714304	-0.051641	4.815567
249.457564	7999.860372	12.719309	-0.051652	4.815561
249.410084	7999.870281	12.724314	-0.051643	4.815564
249.494734	7999.869524	12.729319	-0.051659	4.815563
249.326239	7999.858247	12.734323	-0.051628	4.815561
249.521320	7999.908400	12.739328	-0.051664	4.815574
249.756710	7999.901551	12.744333	-0.051708	4.815571
249.482669	7999.903507	12.749338	-0.051657	4.815573
249.635108	7999.905987	12.754343	-0.051686	4.815573
249.454006	7999.889166	12.759347	-0.051652	4.815569
249.494154	7999.900499	12.764352	-0.051659	4.815572
249.454762	7999.882778	12.769357	-0.051652	4.815567
249.420747	7999.855536	12.774362	-0.051646	4.815559
249.548240	7999.889642	12.779367	-0.051670	4.815569
249.266156	7999.898941	12.784371	-0.051617	4.815573
249.335585	7999.890463	12.789376	-0.051630	4.815570
249.496771	7999.901627	12.794381	-0.051660	4.815572
249.546552	7999.877882	12.799386	-0.051669	4.815565
249.601412	7999.892657	12.804391	-0.051680	4.815569
249.550818	7999.834181	12.809395	-0.051670	4.815552
249.433865	7999.857908	12.814400	-0.051648	4.815560
249.489945	7999.853484	12.819405	-0.051659	4.815558
249.599609	7999.869150	12.824410	-0.051679	4.815562
249.684116	7999.879068	12.829415	-0.051695	4.815565
249.450938	7999.875281	12.834419	-0.051652	4.815565
249.620046	7999.890845	12.839424	-0.051683	4.815569
249.686276	7999.875909	12.844429	-0.051696	4.815564
249.680774	7999.890770	12.849434	-0.051695	4.815568
249.635690	7999.890040	12.854439	-0.051686	4.815568
249.433312	7999.963630	12.859443	-0.051649	4.815591
249.359770	7999.874885	12.864448	-0.051635	4.815565
249.364710	7999.855749	12.869453	-0.051636	4.815560
249.471720	7999.880981	12.874458	-0.051656	4.815567
249.610504	7999.885375	12.879463	-0.051682	4.815567
249.318259	7999.856071	12.884467	-0.051627	4.815560
249.487225	7999.904732	12.889472	-0.051659	4.815573
249.663208	7999.887308	12.894477	-0.051692	4.815567
249.686931	7999.883426	12.899482	-0.051696	4.815566
249.614325	7999.886520	12.904487	-0.051683	4.815567
249.601511	7999.857486	12.909491	-0.051680	4.815559
249.857088	7999.891539	12.914496	-0.051728	4.815568
249.758067	7999.873917	12.919501	-0.051710	4.815563
249.783695	7999.857253	12.924506	-0.051714	4.815558
249.721220	7999.885069	12.929511	-0.051703	4.815567
249.530099	7999.863814	12.934515	-0.051667	4.815561
249.545114	7999.892890	12.939520	-0.051670	4.815570
249.440068	7999.882644	12.944525	-0.051651	4.815567
249.266185	7999.861670	12.949530	-0.051618	4.815562
249.314975	7999.881685	12.954535	-0.051627	4.815567
249.472013	7999.835125	12.959539	-0.051657	4.815553
249.505736	7999.893332	12.964544	-0.051663	4.815570
249.397723	7999.870226	12.969549	-0.051643	4.815564
249.363009	7999.878206	12.974554	-0.051636	4.815566
249.532356	7999.877758	12.979559	-0.051668	4.815565
249.656122	7999.869096	12.984563	-0.051691	4.815562
249.637754	7999.892290	12.989568	-0.051688	4.815569
249.726718	7999.871317	12.994573	-0.051704	4.815562
249.558322	7999.877124	12.999578	-0.051673	4.815565
249.556847	7999.886713	13.004583	-0.051673	4.815568
249.642331	7999.879564	13.009587	-0.051689	4.815565
249.587531	7999.900030	13.014592	-0.051678	4.815572
249.521586	7999.871201	13.019597	-0.051666	4.815563
249.390831	7999.878688	13.024602	-0.051642	4.815566
249.545168	7999.892944	13.029607	-0.051671	4.815570
249.431391	7999.869744	13.034611	-0.051650	4.815563
249.448052	7999.899914	13.039616	-0.051653	4.815572
249.460305	7999.894777	13.044621	-0.051655	4.815571
249.446039	7999.868923	13.049626	-0.051652	4.815563
249.444321	7999.895591	13.054631	-0.051652	4.815571
249.472116	7999.873624	13.059635	-0.051657	4.815564
249.640577	7999.887042	13.064640	-0.051689	4.815567
249.498497	7999.881532	13.069645	-0.051662	4.815567
249.450422	7999.881822	13.074650	-0.051653	4.815567
249.888216	7999.898550	13.079655	-0.051735	4.815570
249.661804	7999.862841	13.084659	-0.051693	4.815560
249.634503	7999.893364	13.089664	-0.051688	4.815569
249.525031	7999.868098	13.094669	-0.051667	4.815562
249.664424	7999.877841	13.099674	-0.051693	4.815565
249.677182	7999.878051	13.104679	-0.051696	4.815565
249.631487	7999.886921	13.109683	-0.051687	4.815567
249.765342	7999.914725	13.114688	-0.051712	4.815575
249.616675	7999.882415	13.119693	-0.051685	4.815566
249.583012	7999.874397	13.124698	-0.051678	4.815564
249.838735	7999.896708	13.129703	-0.051726	4.815569
249.908280	7999.870080	13.134707	-0.051739	4.815561
249.624684	7999.884693	13.139712	-0.051686	4.815567
249.758071	7999.874051	13.144717	-0.051711	4.815563
249.729288	7999.893873	13.149722	-0.051706	4.815569
249.710202	7999.927733	13.154727	-0.051702	4.815579
249.768621	7999.891315	13.159731	-0.051713	4.815568
249.709458	7999.893560	13.164736	-0.051702	4.815569
249.643509	7999.895694	13.169741	-0.051690	4.815570
249.579009	7999.873294	13.174746	-0.051678	4.815564
249.762866	7999.896572	13.179751	-0.051712	4.815570
249.576546	7999.850838	13.184755	-0.051678	4.815557
249.646526	7999.909635	13.189760	-0.051691	4.815574
249.767046	7999.884904	13.194765	-0.051713	4.815566
249.748054	7999.892072	13.199770	-0.051710	4.815568
249.485371	7999.957207	13.204775	-0.051661	4.815589
249.549848	7999.866435	13.209779	-0.051673	4.815562
249.640138	7999.871108	13.214784	-0.051690	4.815563
249.591561	7999.864983	13.219789	-0.051681	4.815561
249.506699	7999.896706	13.224794	-0.051665	4.815571
249.904045	7999.867933	13.229799	-0.051739	4.815561
249.697842	7999.836823	13.234803	-0.051700	4.815552
249.750150	7999.899604	13.239808	-0.051710	4.815571
249.833647	7999.891355	13.244813	-0.051726	4.815568
249.684550	7999.884664	13.249818	-0.051698	4.815567
249.694033	7999.899769	13.254823	-0.051700	4.815571
249.626587	7999.873050	13.259827	-0.051687	4.815563
249.820946	7999.912515	13.264832	-0.051724	4.815574
249.733246	7999.886535	13.269837	-0.051707	4.815567
249.626299	7999.873055	13.274842	-0.051687	4.815563
249.789105	7999.870365	13.279847	-0.051718	4.815562
249.662627	7999.875786	13.284851	-0.051694	4.815564
249.827918	7999.889153	13.289856	-0.051725	4.815567
249.833521	7999.890315	13.294861	-0.051726	4.815567
249.761307	7999.885941	13.299866	-0.051713	4.815567
249.991024	7999.898220	13.304871	-0.051756	4.815569
249.516015	7999.870215	13.309875	-0.051667	4.815563
249.560120	7999.911508	13.314880	-0.051675	4.815575
249.736076	7999.886611	13.319885	-0.051708	4.815567
249.649275	7999.903354	13.324890	-0.051692	4.815572
249.829270	7999.892402	13.329895	-0.051726	4.815568
249.860006	7999.868347	13.334899	-0.051731	4.815561
249.749280	7999.886837	13.339904	-0.051711	4.815567
249.638314	7999.846599	13.344909	-0.051690	4.815556
249.609295	7999.881365	13.349914	-0.051685	4.815566
249.778763	7999.899070	13.354919	-0.051716	4.815570
249.749759	7999.854825	13.359923	-0.051711	4.815557
249.739950	7999.872820	13.364928	-0.051709	4.815563
249.612839	7999.864351	13.369933	-0.051686	4.815561
249.884767	7999.882654	13.374938	-0.051736	4.815565
249.622862	7999.882671	13.379943	-0.051688	4.815566
249.808587	7999.956162	13.384947	-0.051722	4.815587
249.842343	7999.892650	13.389952	-0.051728	4.815568
249.848383	7999.873533	13.394957	-0.051730	4.815562
249.884135	7999.883726	13.399962	-0.051736	4.815565
249.994659	7999.915422	13.404967	-0.051757	4.815574
249.747915	7999.872976	13.409971	-0.051711	4.815563
249.871441	7999.887800	13.414976	-0.051734	4.815567
249.862028	7999.874837	13.419981	-0.051732	4.815563
249.831000	7999.862591	13.424986	-0.051727	4.815559
249.610674	7999.892112	13.429991	-0.051686	4.815569
249.726213	7999.868368	13.434995	-0.051707	4.815562
249.758828	7999.861427	13.440000	-0.051713	4.815559
249.664093	7999.862025	13.445005	-0.051696	4.815560
249.642702	7999.888373	13.450010	-0.051692	4.815568
249.864892	7999.895191	13.455015	-0.051733	4.815569
249.717845	7999.856502	13.460019	-0.051706	4.815558
249.688902	7999.877388	13.465024	-0.051700	4.815564
249.849316	7999.884270	13.470029	-0.051730	4.815566
249.788570	7999.882218	13.475034	-0.051719	4.815565
249.867284	7999.893110	13.480039	-0.051734	4.815568
249.701046	7999.850905	13.485043	-0.051703	4.815557
249.592490	7999.877972	13.490048	-0.051683	4.815565
249.670220	7999.893118	13.495053	-0.051697	4.815569
249.760936	7999.888190	13.500058	-0.051714	4.815567
249.716514	7999.877861	13.505063	-0.051706	4.815564
249.695763	7999.930913	13.510067	-0.051702	4.815580
249.601791	7999.885612	13.515072	-0.051685	4.815567
249.874084	7999.866551	13.520077	-0.051735	4.815560
249.662552	7999.883402	13.525082	-0.051696	4.815566
249.620529	7999.891264	13.530087	-0.051688	4.815569
249.621626	7999.884878	13.535091	-0.051688	4.815567
249.783133	7999.901387	13.540096	-0.051718	4.815571
249.646041	7999.885281	13.545101	-0.051693	4.815567
249.751989	7999.862449	13.550106	-0.051713	4.815560
249.851754	7999.914256	13.555111	-0.051731	4.815574
249.716646	7999.885370	13.560115	-0.051706	4.815567
249.802493	7999.909191	13.565120	-0.051722	4.815573
249.813840	7999.870940	13.570125	-0.051724	4.815562
249.805442	7999.890025	13.575130	-0.051723	4.815567
249.819095	7999.919079	13.580135	-0.051725	4.815576
249.890024	7999.871120	13.585139	-0.051739	4.815562
249.843155	7999.871428	13.590144	-0.051730	4.815562
249.903744	7999.880958	13.595149	-0.051741	4.815564
249.951067	7999.908423	13.600154	-0.051750	4.815572
250.102028	7999.921558	13.605159	-0.051778	4.815575
249.798010	7999.880316	13.610163	-0.051722	4.815565
249.822834	7999.898874	13.615168	-0.051726	4.815570
249.812071	7999.890160	13.620173	-0.051724	4.815567
249.801813	7999.909215	13.625178	-0.051723	4.815573
249.799104	7999.912377	13.630183	-0.051722	4.815574
249.869319	7999.888964	13.635187	-0.051735	4.815567
250.000393	7999.902843	13.640192	-0.051760	4.815570
249.942962	7999.881625	13.645197	-0.051749	4.815564
249.773977	7999.875678	13.650202	-0.051718	4.815563
249.905497	7999.897038	13.655207	-0.051742	4.815569
249.764086	7999.857372	13.660211	-0.051716	4.815558
249.826053	7999.900024	13.665216	-0.051727	4.815570
250.076080	7999.895549	13.670221	-0.051774	4.815568
249.846928	7999.886489	13.675226	-0.051731	4.815566
249.816383	7999.893469	13.680231	-0.051726	4.815568
249.958448	7999.865885	13.685235	-0.051752	4.815560
250.033248	7999.909813	13.690240	-0.051766	4.815572
249.965937	7999.896977	13.695245	-0.051754	4.815569
249.903551	7999.884221	13.700250	-0.051742	4.815565
250.085676	7999.901065	13.705255	-0.051776	4.815569
249.884308	7999.858288	13.710259	-0.051738	4.815558
249.999840	7999.896472	13.715264	-0.051760	4.815568
250.038993	7999.870418	13.720269	-0.051767	4.815561
249.925157	7999.871774	13.725274	-0.051746	4.815562
249.875020	7999.899791	13.730279	-0.051737	4.815570
249.792837	7999.877103	13.735283	-0.051722	4.815564
249.830530	7999.886261	13.740288	-0.051729	4.815566
249.896153	7999.864908	13.745293	-0.051741	4.815560
249.825059	7999.959851	13.750298	-0.051728	4.815588
249.886685	7999.890386	13.755303	-0.051739	4.815567
249.870585	7999.879450	13.760307	-0.051736	4.815564
249.727783	7999.915569	13.765312	-0.051710	4.815575
249.933649	7999.900767	13.770317	-0.051748	4.815570
249.925251	7999.882483	13.775322	-0.051747	4.815565
249.818477	7999.887156	13.780327	-0.051727	4.815567
249.939637	7999.866707	13.785331	-0.051749	4.815560
249.907101	7999.888603	13.790336	-0.051743	4.815567
249.866091	7999.868720	13.795341	-0.051736	4.815561
249.803204	7999.886920	13.800346	-0.051724	4.815567
249.917864	7999.912277	13.805351	-0.051745	4.815573
250.132431	7999.881601	13.810355	-0.051785	4.815563
249.958889	7999.890527	13.815360	-0.051753	4.815567
249.997286	7999.878342	13.820365	-0.051760	4.815563
250.074158	7999.883865	13.825370	-0.051775	4.815564
250.041959	7999.906835	13.830375	-0.051769	4.815571
249.923482	7999.856864	13.835379	-0.051747	4.815557
250.078070	7999.896751	13.840384	-0.051775	4.815568
250.012334	7999.897820	13.845389	-0.051763	4.815569
249.765463	7999.861779	13.850394	-0.051717	4.815559
249.903127	7999.908864	13.855399	-0.051743	4.815572
249.831558	7999.885281	13.860403	-0.051730	4.815566
249.818965	7999.897892	13.865408	-0.051727	4.815570
249.810155	7999.892413	13.870413	-0.051726	4.815568
249.957288	7999.891605	13.875418	-0.051753	4.815567
250.104855	7999.908955	13.880423	-0.051781	4.815572
250.082393	7999.874425	13.885427	-0.051777	4.815562
250.157189	7999.911947	13.890432	-0.051791	4.815572
249.885314	7999.886176	13.895437	-0.051740	4.815566
249.927903	7999.851636	13.900442	-0.051748	4.815556
250.072940	7999.888164	13.905447	-0.051775	4.815566
250.129271	7999.879473	13.910451	-0.051785	4.815563
250.151602	7999.891584	13.915456	-0.051790	4.815566
249.964855	7999.862926	13.920461	-0.051755	4.815559
249.934576	7999.891265	13.925466	-0.051749	4.815567
249.961993	7999.887443	13.930471	-0.051754	4.815566
249.996842	7999.870929	13.935475	-0.051761	4.815561
249.930437	7999.936052	13.940480	-0.051749	4.815580
249.909674	7999.887669	13.945485	-0.051745	4.815566
249.944845	7999.869025	13.950490	-0.051751	4.815561
249.939232	7999.878546	13.955495	-0.051750	4.815563
250.095373	7999.878952	13.960499	-0.051779	4.815563
250.176198	7999.893082	13.965504	-0.051795	4.815567
249.951002	7999.884085	13.970509	-0.051753	4.815565
249.960141	7999.847934	13.975514	-0.051754	4.815554
250.067140	7999.883844	13.980519	-0.051774	4.815564
249.946657	7999.868008	13.985523	-0.051752	4.815560
250.053039	7999.885756	13.990528	-0.051772	4.815565
250.148422	7999.857413	13.995533	-0.051790	4.815556
250.002838	7999.849711	14.000538	-0.051763	4.815555
250.135582	7999.880700	14.005543	-0.051787	4.815563
250.172643	7999.890915	14.010547	-0.051794	4.815566
250.116073	7999.893202	14.015552	-0.051784	4.815567
249.837032	7999.901481	14.020557	-0.051732	4.815571
250.043249	7999.868534	14.025562	-0.051770	4.815560
250.281510	7999.894833	14.030567	-0.051815	4.815567
250.051689	7999.867609	14.035571	-0.051772	4.815560
250.097148	7999.896112	14.040576	-0.051780	4.815568
250.005081	7999.890348	14.045581	-0.051763	4.815567
249.928526	7999.876293	14.050586	-0.051749	4.815563
249.908183	7999.910133	14.055591	-0.051745	4.815573
249.884396	7999.857431	14.060595	-0.051741	4.815557
250.027858	7999.880053	14.065600	-0.051768	4.815563
249.981946	7999.876106	14.070605	-0.051759	4.815562
250.174489	7999.872833	14.075610	-0.051795	4.815561
250.341666	7999.901179	14.080615	-0.051826	4.815568
249.838301	7999.875915	14.085619	-0.051732	4.815563
250.155448	7999.841568	14.090624	-0.051792	4.815552
249.975558	7999.882423	14.095629	-0.051758	4.815564
249.881743	7999.859547	14.100634	-0.051741	4.815558
250.096056	7999.908946	14.105639	-0.051781	4.815572
250.154138	7999.893877	14.110643	-0.051791	4.815567
250.080907	7999.918315	14.115648	-0.051778	4.815574
249.984563	7999.974409	14.120653	-0.051760	4.815591
250.125225	7999.883807	14.125658	-0.051786	4.815564
250.028196	7999.903587	14.130663	-0.051768	4.815570
249.884588	7999.892713	14.135667	-0.051741	4.815568
249.920175	7999.882618	14.140672	-0.051748	4.815565
250.116479	7999.890083	14.145677	-0.051785	4.815566
250.032376	7999.854551	14.150682	-0.051769	4.815556
249.979077	7999.902803	14.155687	-0.051759	4.815570
249.980200	7999.859048	14.160691	-0.051759	4.815557
249.952734	7999.869281	14.165696	-0.051754	4.815561
250.071709	7999.874422	14.170701	-0.051777	4.815562
249.909356	7999.852566	14.175706	-0.051746	4.815556
250.103703	7999.887760	14.180711	-0.051783	4.815565
249.906984	7999.879227	14.185715	-0.051746	4.815564
249.802717	7999.901025	14.190720	-0.051727	4.815571
250.039944	7999.885665	14.195725	-0.051771	4.815565
249.942301	7999.871268	14.200730	-0.051753	4.815561
249.884687	7999.902366	14.205735	-0.051742	4.815571
250.206983	7999.886254	14.210739	-0.051802	4.815564
250.157336	7999.901466	14.215744	-0.051793	4.815569
250.107701	7999.898527	14.220749	-0.051784	4.815568
250.080254	7999.873526	14.225754	-0.051778	4.815561
250.253741	7999.917991	14.230759	-0.051811	4.815573
249.958506	7999.882230	14.235763	-0.051756	4.815564
250.114943	7999.895453	14.240768	-0.051785	4.815567
250.299114	7999.903789	14.245773	-0.051819	4.815569
250.142169	7999.893766	14.250778	-0.051790	4.815567
250.211774	7999.909849	14.255783	-0.051803	4.815571
250.184245	7999.885914	14.260787	-0.051798	4.815564
250.398281	7999.894736	14.265792	-0.051838	4.815566
250.182799	7999.692639	14.270797	-0.051798	4.815508

250.240777	7996.361568	14.275802	-0.051806	4.814533
250.354266	7990.785566	14.280807	-0.051824	4.812902
250.137026	7983.990092	14.285811	-0.051779	4.810914
249.927049	7976.661302	14.290816	-0.051735	4.808770
249.941546	7969.076110	14.295821	-0.051733	4.806548
249.950940	7961.144959	14.300826	-0.051730	4.804224
250.132909	7953.376771	14.305831	-0.051759	4.801946
250.081128	7945.378854	14.310835	-0.051744	4.799601
250.092532	7937.434735	14.315840	-0.051741	4.797269
250.059226	7929.435358	14.320845	-0.051729	4.794921
249.807043	7921.365583	14.325850	-0.051677	4.792552
250.117306	7913.402396	14.330855	-0.051730	4.790210
250.001284	7905.397760	14.335859	-0.051703	4.787857
249.774643	7897.365879	14.340864	-0.051656	4.785495
249.779289	7889.436646	14.345869	-0.051651	4.783162
249.724180	7881.379050	14.350874	-0.051636	4.780789
249.858440	7873.461475	14.355879	-0.051656	4.778456
249.681682	7865.436726	14.360883	-0.051618	4.776092
249.772085	7857.377113	14.365888	-0.051629	4.773715
249.543422	7849.376705	14.370893	-0.051581	4.771355
249.414941	7841.383710	14.375898	-0.051552	4.768996
249.618455	7833.417810	14.380903	-0.051585	4.766643
249.662747	7825.351396	14.385907	-0.051588	4.764259
249.470034	7817.379114	14.390912	-0.051547	4.761903
249.473406	7809.357215	14.395917	-0.051542	4.759530
249.415392	7801.440929	14.400922	-0.051527	4.757188
249.240674	7793.372290	14.405927	-0.051489	4.754799
249.041833	7785.309622	14.410931	-0.051447	4.752412
249.170637	7777.304150	14.415936	-0.051465	4.750038
249.284066	7769.342472	14.420941	-0.051481	4.747677
248.852998	7761.281170	14.425946	-0.051396	4.745287
249.057411	7753.350516	14.430951	-0.051429	4.742933
249.201387	7745.351652	14.435955	-0.051450	4.740557
249.034892	7737.366283	14.440960	-0.051414	4.738185
248.879623	7729.347295	14.445965	-0.051380	4.735801
248.825448	7721.307138	14.450970	-0.051365	4.733410
248.887194	7713.321452	14.455975	-0.051371	4.731034
248.631504	7705.317996	14.460979	-0.051318	4.728652
248.611894	7697.290401	14.465984	-0.051310	4.726260
248.608322	7689.291112	14.470989	-0.051304	4.723876
248.551464	7681.321585	14.475994	-0.051288	4.721500
248.618275	7673.311099	14.480999	-0.051295	4.719110
248.831035	7665.390548	14.486003	-0.051330	4.716746
248.787603	7657.320302	14.491008	-0.051316	4.714336
248.528525	7649.326702	14.496013	-0.051263	4.711948
248.733619	7641.223837	14.501018	-0.051296	4.709526
248.636507	7633.317992	14.506023	-0.051273	4.707161
248.382455	7625.265878	14.511027	-0.051220	4.704752
248.452850	7617.301580	14.516032	-0.051228	4.702368
248.576825	7609.351047	14.521037	-0.051246	4.699986
248.356531	7601.347031	14.526042	-0.051200	4.697588
248.425339	7593.289718	14.531047	-0.051207	4.695171
248.289347	7585.294563	14.536051	-0.051177	4.692773
248.273058	7577.276201	14.541056	-0.051169	4.690366
248.285141	7569.265254	14.546061	-0.051166	4.687961
248.368923	7561.271292	14.551066	-0.051176	4.685559
248.266694	7553.322961	14.556071	-0.051152	4.683169
248.220631	7545.285634	14.561075	-0.051138	4.680752
248.286997	7537.282096	14.566080	-0.051145	4.678343
248.465433	7529.295648	14.571085	-0.051173	4.675938
248.333199	7521.267243	14.576090	-0.051144	4.673520
248.236539	7513.187293	14.581095	-0.051120	4.671085
248.175713	7505.168682	14.586099	-0.051104	4.668667
248.182946	7497.211432	14.591104	-0.051100	4.666266
247.930592	7489.272780	14.596109	-0.051048	4.663870
248.063269	7481.231231	14.601114	-0.051067	4.661441
248.206548	7473.244479	14.606119	-0.051089	4.659027
247.963768	7465.280153	14.611123	-0.051039	4.656620
247.990800	7457.212551	14.616128	-0.051038	4.654179
247.997778	7449.230590	14.621133	-0.051035	4.651763
247.779276	7441.186198	14.626138	-0.050989	4.649328
247.806696	7433.232245	14.631143	-0.050989	4.646918
247.791278	7425.219506	14.636147	-0.050981	4.644489
247.849412	7417.262587	14.641152	-0.050986	4.642076
247.737499	7409.229231	14.646157	-0.050960	4.639638
247.751593	7401.235323	14.651162	-0.050958	4.637211
247.858382	7393.232393	14.656167	-0.050972	4.634780
247.510649	7385.193977	14.661171	-0.050902	4.632337
247.576036	7377.140933	14.666176	-0.050909	4.629888
247.793762	7369.216413	14.671181	-0.050945	4.627477
247.374996	7361.150869	14.676186	-0.050862	4.625022
247.329464	7353.186332	14.681191	-0.050848	4.622596
247.454099	7345.182031	14.686195	-0.050866	4.620157
247.296495	7337.178784	14.691200	-0.050831	4.617716
247.251200	7329.206441	14.696205	-0.050818	4.615284
247.427549	7321.157504	14.701210	-0.050845	4.612828
247.544669	7313.166985	14.706215	-0.050862	4.610388
247.309955	7305.196177	14.711219	-0.050813	4.607952
247.244886	7297.162173	14.716224	-0.050796	4.605496
247.575165	7289.206606	14.721229	-0.050852	4.603063
247.329530	7281.144612	14.726234	-0.050801	4.600595
247.442912	7273.196658	14.731239	-0.050817	4.598162
247.490400	7265.205094	14.736243	-0.050821	4.595714
247.487257	7257.143533	14.741248	-0.050815	4.593242
247.247413	7249.111196	14.746253	-0.050765	4.590779
247.033667	7241.085253	14.751258	-0.050720	4.588316
247.256692	7233.166399	14.756263	-0.050757	4.585885
247.026690	7225.159318	14.761267	-0.050709	4.583425
246.947455	7217.130841	14.766272	-0.050689	4.580957
247.203827	7209.145346	14.771277	-0.050731	4.578502
246.991105	7201.156354	14.776282	-0.050687	4.576044
246.881084	7193.128830	14.781287	-0.050661	4.573572
246.777530	7185.049941	14.786291	-0.050636	4.571084
246.970377	7177.092910	14.791296	-0.050667	4.568632
247.096956	7169.176779	14.796301	-0.050686	4.566191
246.903043	7161.098197	14.801306	-0.050644	4.563698
247.105118	7153.146804	14.806311	-0.050677	4.561244
246.990521	7145.124218	14.811315	-0.050650	4.558766
246.618663	7137.181977	14.816320	-0.050576	4.556311
246.781746	7129.165884	14.821325	-0.050601	4.553833
246.712182	7121.113898	14.826330	-0.050583	4.551342
246.567362	7113.095991	14.831335	-0.050551	4.548860
246.565245	7105.145247	14.836339	-0.050545	4.546398
246.675035	7097.130707	14.841344	-0.050560	4.543914
246.521691	7089.175390	14.846349	-0.050527	4.541448
246.395484	7081.101551	14.851354	-0.050498	4.538943
246.452451	7073.148751	14.856359	-0.050503	4.536475
246.404839	7065.112486	14.861363	-0.050489	4.533979
246.327602	7057.059774	14.866368	-0.050470	4.531477
246.632156	7049.103340	14.871373	-0.050521	4.529004
246.516395	7041.083823	14.876378	-0.050494	4.526509
246.342129	7033.103294	14.881383	-0.050457	4.524025
246.342870	7025.189086	14.886387	-0.050452	4.521560
246.400495	7017.093453	14.891392	-0.050457	4.519038
246.269517	7009.200010	14.896397	-0.050428	4.516577
246.122248	7001.080915	14.901402	-0.050395	4.514044
246.276811	6993.044000	14.906407	-0.050419	4.511536
246.250919	6985.051981	14.911411	-0.050409	4.509040
246.126888	6977.030275	14.916416	-0.050380	4.506534
246.077840	6969.067350	14.921421	-0.050366	4.504044
246.177402	6961.070614	14.926426	-0.050380	4.501543
246.295947	6953.077123	14.931431	-0.050396	4.499042
246.248807	6945.100538	14.936435	-0.050383	4.496544
246.093822	6937.037785	14.941440	-0.050348	4.494017
245.884491	6929.037906	14.946445	-0.050304	4.491509
245.870213	6921.028724	14.951450	-0.050296	4.488997
245.977575	6913.086466	14.956455	-0.050311	4.486504
245.935686	6905.061655	14.961459	-0.050298	4.483984
245.858186	6897.076519	14.966464	-0.050279	4.481475
245.957323	6889.059269	14.971469	-0.050292	4.478955
245.867884	6881.094184	14.976474	-0.050270	4.476449
245.649923	6873.052706	14.981479	-0.050224	4.473918
245.833935	6865.007406	14.986483	-0.050253	4.471385
245.967663	6856.994910	14.991488	-0.050273	4.468861
245.913364	6849.012835	14.996493	-0.050258	4.466344
245.788788	6841.004455	15.001498	-0.050229	4.463817
245.664741	6833.047138	15.006503	-0.050201	4.461305
245.634188	6825.031945	15.011507	-0.050190	4.458774
245.460508	6817.026057	15.016512	-0.050153	4.456244
245.680906	6809.011947	15.021517	-0.050189	4.453711
245.629281	6801.006772	15.026522	-0.050174	4.451178
245.484940	6792.986675	15.031527	-0.050142	4.448639
245.376685	6785.016081	15.036531	-0.050116	4.446114
245.433737	6777.001568	15.041536	-0.050122	4.443575
245.443387	6769.057233	15.046541	-0.050119	4.441056
245.372002	6761.038832	15.051546	-0.050100	4.438512
245.359154	6753.047848	15.056551	-0.050093	4.435975
245.489484	6745.018156	15.061555	-0.050112	4.433426
245.128115	6736.946055	15.066560	-0.050039	4.430859
245.218690	6728.987073	15.071565	-0.050051	4.428328
245.076866	6720.966376	15.076570	-0.050019	4.425776
245.168690	6712.994933	15.081575	-0.050031	4.423238
245.009984	6705.007317	15.086579	-0.049996	4.420693
245.180890	6696.979189	15.091584	-0.050023	4.418136
245.056492	6689.002300	15.096589	-0.049995	4.415591
244.909620	6680.971731	15.101594	-0.049962	4.413028
244.945488	6672.946907	15.106599	-0.049964	4.410466
245.086041	6664.968048	15.111603	-0.049985	4.407918
244.830666	6656.971867	15.116608	-0.049932	4.405361
244.787998	6649.005244	15.121613	-0.049919	4.402812
244.933843	6640.996236	15.126618	-0.049941	4.400250
244.931739	6633.056714	15.131623	-0.049935	4.397708
244.830816	6625.004624	15.136627	-0.049911	4.395128
244.692129	6616.933622	15.141632	-0.049880	4.392540
244.841956	6608.954856	15.146637	-0.049903	4.389981
244.653700	6600.973995	15.151642	-0.049863	4.387418
244.664262	6592.978794	15.156647	-0.049859	4.384851
244.727974	6585.030062	15.161651	-0.049866	4.382297
244.827325	6576.959103	15.166656	-0.049879	4.379703
244.878290	6569.029605	15.171661	-0.049884	4.377152
244.905297	6560.983963	15.176666	-0.049884	4.374562
244.629635	6552.998178	15.181671	-0.049827	4.371989
244.541553	6544.974921	15.186675	-0.049806	4.369402
244.656841	6536.991280	15.191680	-0.049822	4.366829
244.769373	6528.971736	15.196685	-0.049838	4.364242
244.484556	6521.034271	15.201690	-0.049779	4.361677
244.496817	6512.957579	15.206695	-0.049777	4.359068
244.401004	6505.054921	15.211699	-0.049754	4.356513
244.243484	6496.960362	15.216704	-0.049719	4.353894
244.303745	6488.867288	15.221709	-0.049725	4.351275
244.355174	6480.902620	15.226714	-0.049729	4.348697
244.424801	6472.955774	15.231719	-0.049737	4.346122
244.206488	6464.939726	15.236723	-0.049691	4.343522
244.119490	6456.958518	15.241728	-0.049670	4.340932
244.059609	6448.984422	15.246733	-0.049654	4.338343
243.968156	6440.973515	15.251738	-0.049631	4.335741
244.015538	6432.937564	15.256743	-0.049635	4.333130
244.047345	6424.920224	15.261747	-0.049636	4.330523
243.984575	6416.948160	15.266752	-0.049619	4.327928
243.927068	6408.939571	15.271757	-0.049603	4.325321
243.876991	6400.971124	15.276762	-0.049589	4.322724
243.930138	6392.957284	15.281767	-0.049593	4.320112
243.615071	6385.016962	15.286771	-0.049529	4.317520
243.647035	6376.954974	15.291776	-0.049530	4.314889
243.887943	6368.934147	15.296781	-0.049570	4.312272
243.808482	6360.873063	15.301786	-0.049550	4.309637
243.793542	6352.955748	15.306791	-0.049542	4.307048
243.929849	6344.909867	15.311795	-0.049562	4.304417
243.694656	6336.963573	15.316800	-0.049513	4.301814
243.682909	6328.942469	15.321805	-0.049506	4.299187
243.668009	6320.931120	15.326810	-0.049498	4.296561
243.757073	6312.932597	15.331815	-0.049509	4.293938
243.614546	6304.918035	15.336819	-0.049478	4.291307
243.710295	6296.888252	15.341824	-0.049490	4.288671
243.710629	6288.940817	15.346829	-0.049485	4.286060
243.535137	6280.913450	15.351834	-0.049447	4.283419
243.530083	6272.956019	15.356839	-0.049441	4.280801
243.561885	6264.962695	15.361843	-0.049442	4.278171
243.551318	6256.926107	15.366848	-0.049435	4.275523
243.509021	6248.898178	15.371853	-0.049422	4.272877
243.329411	6240.879805	15.376858	-0.049383	4.270231
243.300185	6232.882360	15.381863	-0.049372	4.267592
243.349043	6224.896304	15.386867	-0.049376	4.264955
243.374136	6216.911090	15.391872	-0.049376	4.262317
243.153716	6208.928025	15.396877	-0.049330	4.259676
243.046667	6200.949747	15.401882	-0.049304	4.257036
242.902701	6192.904883	15.406887	-0.049272	4.254372
243.129716	6184.916112	15.411891	-0.049310	4.251727
242.952762	6176.850251	15.416896	-0.049271	4.249053
242.899539	6168.934770	15.421901	-0.049256	4.246427
242.843846	6160.879447	15.426906	-0.049241	4.243753
243.099073	6152.906862	15.431911	-0.049283	4.241108
243.059248	6144.913785	15.436915	-0.049271	4.238452
242.787162	6136.954026	15.441920	-0.049215	4.235803
242.805651	6128.961852	15.446925	-0.049213	4.233144
242.908274	6120.876614	15.451930	-0.049227	4.230454
242.830468	6112.888925	15.456935	-0.049207	4.227792
242.822851	6104.915465	15.461939	-0.049201	4.225135
242.622533	6096.907855	15.466944	-0.049158	4.222462
242.668012	6088.951340	15.471949	-0.049161	4.219807
242.535038	6080.984646	15.476954	-0.049132	4.217145
242.705218	6072.931647	15.481959	-0.049158	4.214456
242.563693	6064.945522	15.486963	-0.049127	4.211784
242.415529	6056.872388	15.491968	-0.049094	4.209081
242.621416	6048.962277	15.496973	-0.049127	4.206435
242.625619	6040.912429	15.501978	-0.049122	4.203738
242.506201	6032.942381	15.506983	-0.049095	4.201065
242.425245	6024.971597	15.511987	-0.049075	4.198391
242.264795	6016.950807	15.516992	-0.049040	4.195697
242.375691	6008.889414	15.521997	-0.049055	4.192990
242.222592	6000.819378	15.527002	-0.049021	4.190276
242.310035	5992.886998	15.532007	-0.049033	4.187609
242.403693	5984.848153	15.537011	-0.049045	4.184905
242.271782	5976.899698	15.542016	-0.049015	4.182227
242.210784	5968.915163	15.547021	-0.048999	4.179536
242.279472	5960.937068	15.552026	-0.049006	4.176847
242.080558	5952.902692	15.557031	-0.048964	4.174134
242.255419	5944.904568	15.562035	-0.048991	4.171435
242.202361	5936.814836	15.567040	-0.048976	4.168702
242.138958	5928.933896	15.572045	-0.048959	4.166037
242.018980	5920.914183	15.577050	-0.048932	4.163322
241.935782	5912.925237	15.582055	-0.048911	4.160617
242.133410	5904.934623	15.587059	-0.048943	4.157913
241.901878	5896.900458	15.592064	-0.048894	4.155187
241.897456	5888.882164	15.597069	-0.048888	4.152467
241.924463	5880.851480	15.602074	-0.048888	4.149742
242.055877	5872.901425	15.607079	-0.048908	4.147044
241.904522	5864.879260	15.612083	-0.048874	4.144316
241.887060	5856.881543	15.617088	-0.048866	4.141596
241.894937	5848.904698	15.622093	-0.048862	4.138882
241.660094	5840.903326	15.627098	-0.048813	4.136154
241.737551	5832.874972	15.632103	-0.048822	4.133420
241.753016	5824.848669	15.637107	-0.048820	4.130683
241.537266	5816.893768	15.642112	-0.048775	4.127967
241.623734	5808.895612	15.647117	-0.048786	4.125237
241.767560	5800.902431	15.652122	-0.048807	4.122508
241.689026	5792.890796	15.657127	-0.048788	4.119768
241.619252	5784.980909	15.662131	-0.048769	4.117061
241.476277	5776.907604	15.667136	-0.048738	4.114296
241.552243	5768.856136	15.672141	-0.048746	4.111539
241.314940	5760.846504	15.677146	-0.048697	4.108790
241.479458	5752.847042	15.682151	-0.048723	4.106049
241.442256	5744.897869	15.687155	-0.048710	4.103320
241.218683	5736.887579	15.692160	-0.048664	4.100565
241.151417	5728.957540	15.697165	-0.048646	4.097839
241.177250	5720.910320	15.702170	-0.048646	4.095072
241.031654	5712.919668	15.707175	-0.048613	4.092320
240.917044	5704.893369	15.712179	-0.048587	4.089554
240.946560	5696.909431	15.717184	-0.048587	4.086803
241.295935	5688.901890	15.722189	-0.048647	4.084046
240.980467	5680.941485	15.727194	-0.048583	4.081295
240.770727	5672.923609	15.732199	-0.048539	4.078523
240.824538	5664.981955	15.737203	-0.048544	4.075779
240.926086	5656.911936	15.742208	-0.048557	4.072990
240.899731	5648.940090	15.747213	-0.048547	4.070231
241.006094	5640.946620	15.752218	-0.048562	4.067465
240.832444	5632.909688	15.757223	-0.048524	4.064677
240.575939	5624.974468	15.762227	-0.048472	4.061922
240.592655	5616.897620	15.767232	-0.048469	4.059120
240.884471	5608.980293	15.772237	-0.048519	4.056375
240.637642	5600.900294	15.777242	-0.048467	4.053564
240.563263	5592.929175	15.782247	-0.048448	4.050791
240.425250	5584.934841	15.787251	-0.048418	4.048008
240.409846	5576.903231	15.792256	-0.048409	4.045211
240.508584	5568.954737	15.797261	-0.048423	4.042443
240.327433	5560.927842	15.802266	-0.048384	4.039642
240.543199	5552.949484	15.807271	-0.048419	4.036861
240.388978	5544.937973	15.812275	-0.048385	4.034062
240.386609	5536.774557	15.817280	-0.048379	4.031210
240.389189	5528.866645	15.822285	-0.048375	4.028445
240.155716	5520.878150	15.827290	-0.048326	4.025646
240.362188	5512.883127	15.832295	-0.048359	4.022850
240.406830	5504.948822	15.837299	-0.048362	4.020071
240.318832	5496.931513	15.842304	-0.048341	4.017259
240.130439	5488.922550	15.847309	-0.048300	4.014446
240.133959	5480.910711	15.852314	-0.048296	4.011633
240.151845	5472.873652	15.857319	-0.048294	4.008809
239.962352	5464.924387	15.862323	-0.048254	4.006011
239.907720	5456.902810	15.867328	-0.048238	4.003188
240.069625	5448.931148	15.872333	-0.048263	4.000384
239.945092	5440.932917	15.877338	-0.048235	3.997564
239.946737	5432.917788	15.882343	-0.048230	3.994738
239.954120	5424.887729	15.887347	-0.048226	3.991904
239.956854	5416.845912	15.892352	-0.048222	3.989065
239.921604	5408.892849	15.897357	-0.048210	3.986254
239.828019	5400.907537	15.902362	-0.048187	3.983429
239.857794	5392.916869	15.907367	-0.048188	3.980602
239.841876	5384.956935	15.912371	-0.048179	3.977783
239.664087	5376.927508	15.917376	-0.048141	3.974935
239.714004	5368.938012	15.922381	-0.048145	3.972103
239.518404	5360.914874	15.927386	-0.048104	3.969252
239.556577	5352.957606	15.932391	-0.048106	3.966427
239.747155	5344.945115	15.937395	-0.048136	3.963583
239.578000	5336.963527	15.942400	-0.048099	3.960742
239.449517	5328.993671	15.947405	-0.048070	3.957903
239.468169	5320.954973	15.952410	-0.048068	3.955041
239.505895	5312.930797	15.957415	-0.048070	3.952182
239.336582	5304.926927	15.962419	-0.048034	3.949324
239.250693	5296.965925	15.967424	-0.048012	3.946481
239.508994	5288.968387	15.972429	-0.048055	3.943629
239.330215	5280.974601	15.977434	-0.048017	3.940769
239.258567	5273.001443	15.982439	-0.047998	3.937916
239.254879	5264.975781	15.987443	-0.047992	3.935043
239.230940	5256.964845	15.992448	-0.047983	3.932173
239.255351	5248.972143	15.997453	-0.047982	3.929308
239.178107	5240.988659	16.002458	-0.047963	3.926443
239.247826	5232.993162	16.007463	-0.047970	3.923573
239.336571	5225.032927	16.012467	-0.047982	3.920715
239.274030	5217.025428	16.017472	-0.047965	3.917835
239.362675	5209.011765	16.022477	-0.047976	3.914954
239.240691	5200.988804	16.027482	-0.047948	3.912063
239.012248	5192.970403	16.032487	-0.047901	3.909169
238.976273	5184.999993	16.037491	-0.047889	3.906294
238.988698	5176.966362	16.042496	-0.047886	3.903396
238.951835	5168.980163	16.047501	-0.047874	3.900511
238.750869	5161.015405	16.052506	-0.047831	3.897629
239.076834	5152.959875	16.057511	-0.047887	3.894721
239.126011	5144.994687	16.062515	-0.047891	3.891840
238.748499	5136.961498	16.067520	-0.047815	3.888923
238.759408	5129.001661	16.072525	-0.047812	3.886038
238.786310	5121.015912	16.077530	-0.047812	3.883141
238.505141	5113.001901	16.082535	-0.047754	3.880227
238.544080	5105.057575	16.087539	-0.047757	3.877341
238.575313	5096.979649	16.092544	-0.047757	3.874405
238.537835	5088.772610	16.097549	-0.047745	3.871418
238.421449	5080.811912	16.102554	-0.047718	3.868517
238.613931	5072.869512	16.107559	-0.047749	3.865627
238.681298	5064.954374	16.112563	-0.047756	3.862742
238.461876	5056.955698	16.117568	-0.047710	3.859818
238.486190	5048.998453	16.122573	-0.047710	3.856913
238.426949	5040.991199	16.127578	-0.047693	3.853985
238.313869	5032.976839	16.132583	-0.047667	3.851051
238.272325	5025.003022	16.137587	-0.047654	3.848132
238.241817	5016.982698	16.142592	-0.047643	3.845193
238.252074	5009.044553	16.147597	-0.047640	3.842283
238.188204	5001.034939	16.152602	-0.047623	3.839343
238.192570	4993.065887	16.157607	-0.047619	3.836417
238.158149	4985.048215	16.162611	-0.047607	3.833470
238.215106	4977.000982	16.167616	-0.047612	3.830512
238.312839	4969.033092	16.172621	-0.047625	3.827582
238.253234	4961.009947	16.177626	-0.047609	3.824625
238.113853	4953.077208	16.182631	-0.047578	3.821698
238.094130	4945.066728	16.187635	-0.047569	3.818743
237.921698	4937.063686	16.192640	-0.047532	3.815785
238.084964	4929.047452	16.197645	-0.047557	3.812827
237.995565	4921.056306	16.202650	-0.047535	3.809870
237.806964	4913.054430	16.207655	-0.047495	3.806905
238.095051	4905.072234	16.212659	-0.047544	3.803956
237.742859	4897.117760	16.217664	-0.047473	3.801000
237.878093	4889.124048	16.222669	-0.047493	3.798038
237.866330	4881.092252	16.227674	-0.047485	3.795057
237.619047	4873.059762	16.232679	-0.047434	3.792068
237.791258	4865.033072	16.237683	-0.047461	3.789087
237.765071	4857.058038	16.242688	-0.047451	3.786119
237.712324	4849.074105	16.247693	-0.047436	3.783145
237.648304	4841.107207	16.252698	-0.047419	3.780175
237.534214	4833.096909	16.257703	-0.047392	3.777185
237.581108	4825.088280	16.262707	-0.047396	3.774197
237.395218	4817.067534	16.267712	-0.047356	3.771197
237.465359	4809.086077	16.272717	-0.047364	3.768215
237.269080	4801.092164	16.277722	-0.047322	3.765220
237.328587	4793.124860	16.282727	-0.047328	3.762238
237.290046	4785.131575	16.287731	-0.047316	3.759242
237.239388	4777.127125	16.292736	-0.047301	3.756238
237.300535	4769.095578	16.297741	-0.047308	3.753225
237.336017	4761.046299	16.302746	-0.047309	3.750203
237.090051	4753.071668	16.307751	-0.047258	3.747199
237.497787	4745.111643	16.312755	-0.047329	3.744214
237.142580	4737.150077	16.317760	-0.047257	3.741208
236.940994	4729.153117	16.322765	-0.047215	3.738189
237.001705	4721.148655	16.327770	-0.047221	3.735172
236.948143	4713.135544	16.332775	-0.047206	3.732146
236.826888	4705.151431	16.337779	-0.047178	3.729127
236.884352	4697.146786	16.342784	-0.047183	3.726102
236.981687	4689.157624	16.347789	-0.047196	3.723082
236.672299	4681.196828	16.352794	-0.047134	3.720059
236.664917	4673.215838	16.357799	-0.047127	3.717035
236.939942	4665.170509	16.362803	-0.047173	3.713990
236.882980	4657.058572	16.367808	-0.047157	3.710909
236.794874	4649.117235	16.372813	-0.047136	3.707890
236.932384	4641.109476	16.377818	-0.047156	3.704848
236.840818	4633.160894	16.382823	-0.047134	3.701821
236.681912	4625.207693	16.387827	-0.047099	3.698788
236.630354	4617.183645	16.392832	-0.047084	3.695728
236.672135	4609.213304	16.397837	-0.047087	3.692689
236.408231	4601.176498	16.402842	-0.047033	3.689613
236.427658	4593.185755	16.407847	-0.047031	3.686560
236.739783	4585.229539	16.412851	-0.047084	3.683525
236.490104	4577.245380	16.417856	-0.047032	3.680463
236.426552	4569.257192	16.422861	-0.047015	3.677401
236.585889	4561.211124	16.427866	-0.047040	3.674321
236.574336	4553.209234	16.432871	-0.047033	3.671250
236.327230	4545.223403	16.437875	-0.046981	3.668176
236.198904	4537.216066	16.442880	-0.046952	3.665095
236.422265	4529.246069	16.447885	-0.046989	3.662035
236.387585	4521.249905	16.452890	-0.046977	3.658956
236.107487	4513.266675	16.457895	-0.046920	3.655872
236.149433	4505.241621	16.462899	-0.046922	3.652778
236.065532	4497.221460	16.467904	-0.046902	3.649680
236.009805	4489.273263	16.472909	-0.046886	3.646608
235.947097	4481.275779	16.477914	-0.046869	3.643514
236.223410	4473.252035	16.482919	-0.046915	3.640417
235.973600	4465.335086	16.487923	-0.046864	3.637344
235.898963	4457.287999	16.492928	-0.046845	3.634222
236.044313	4449.233352	16.497933	-0.046867	3.631101
236.017862	4441.228909	16.502938	-0.046856	3.627992
236.068469	4433.214709	16.507943	-0.046861	3.624879
235.933416	4425.303046	16.512947	-0.046830	3.621798
235.855078	4417.280362	16.517952	-0.046811	3.618672
235.713213	4409.316388	16.522957	-0.046779	3.615565
235.641644	4401.320744	16.527962	-0.046761	3.612445
235.848024	4393.254752	16.532967	-0.046794	3.609303
235.930772	4385.331509	16.537971	-0.046804	3.606210
235.487573	4377.352802	16.542976	-0.046716	3.603078
235.428385	4369.360136	16.547981	-0.046700	3.599948
235.529951	4361.397177	16.552986	-0.046714	3.596832
235.414246	4353.361982	16.557991	-0.046687	3.593679
235.794841	4345.356950	16.562995	-0.046753	3.590549
235.556397	4337.359009	16.568000	-0.046703	3.587401
235.408342	4329.389433	16.573005	-0.046671	3.584265
235.334112	4321.405672	16.578010	-0.046652	3.581122
235.329072	4313.384287	16.583015	-0.046645	3.577963
235.414490	4305.409307	16.588019	-0.046656	3.574823
235.296788	4297.405557	16.593024	-0.046629	3.571662
235.433634	4289.400518	16.598029	-0.046649	3.568506
235.424497	4281.389570	16.603034	-0.046642	3.565340
235.143932	4273.442095	16.608039	-0.046585	3.562189
235.078738	4265.459029	16.613043	-0.046568	3.559027
235.172656	4257.435832	16.618048	-0.046580	3.555851
235.114198	4249.361862	16.623053	-0.046564	3.552647
234.912111	4241.350744	16.628058	-0.046521	3.549462
234.987658	4233.344202	16.633063	-0.046530	3.546283
235.029403	4225.399143	16.638067	-0.046533	3.543125
234.972630	4217.412894	16.643072	-0.046517	3.539945
235.038038	4209.466157	16.648077	-0.046524	3.536782
235.229125	4201.450474	16.653082	-0.046554	3.533592
234.992127	4193.406367	16.658087	-0.046505	3.530374
234.841938	4185.470144	16.663091	-0.046472	3.527200
234.843040	4177.415648	16.668096	-0.046467	3.523980
234.942749	4169.481863	16.673101	-0.046480	3.520808
234.766085	4161.512462	16.678106	-0.046442	3.517611
234.722635	4153.499687	16.683111	-0.046429	3.514398
234.868568	4145.480466	16.688115	-0.046451	3.511184
234.551087	4137.459217	16.693120	-0.046387	3.507953
234.536063	4129.483439	16.698125	-0.046379	3.504746
234.645123	4121.527841	16.703130	-0.046394	3.501549
234.644428	4113.529883	16.708135	-0.046389	3.498328
234.478033	4105.568468	16.713139	-0.046352	3.495114
234.425160	4097.530566	16.718144	-0.046337	3.491869
234.255580	4089.573440	16.723149	-0.046301	3.488650
234.339560	4081.545161	16.728154	-0.046311	3.485408
234.327530	4073.567354	16.733159	-0.046304	3.482179
234.285976	4065.611615	16.738163	-0.046291	3.478956
234.212666	4057.581872	16.743168	-0.046272	3.475699
234.340327	4049.573755	16.748173	-0.046290	3.472454
234.283855	4041.546212	16.753178	-0.046275	3.469192
234.284101	4033.571630	16.758183	-0.046270	3.465951
234.337853	4025.601774	16.763187	-0.046275	3.462710
234.317596	4017.579389	16.768192	-0.046266	3.459442
234.269321	4009.642633	16.773197	-0.046251	3.456205
234.072651	4001.618206	16.778202	-0.046210	3.452924
234.025301	3993.611617	16.783207	-0.046196	3.449653
234.056112	3985.654423	16.788211	-0.046196	3.446401
233.998932	3977.619584	16.793216	-0.046180	3.443111
233.951899	3969.664771	16.798221	-0.046166	3.439852
234.053474	3961.699337	16.803226	-0.046180	3.436589
233.856649	3953.666920	16.808231	-0.046138	3.433287
233.881127	3945.655373	16.813235	-0.046138	3.429997
233.748638	3937.669690	16.818240	-0.046108	3.426709
233.955474	3929.682804	16.823245	-0.046141	3.423429
233.720554	3921.711089	16.828250	-0.046092	3.420137
233.641058	3913.712382	16.833255	-0.046072	3.416836
233.678861	3905.710982	16.838259	-0.046074	3.413535
233.503320	3897.682892	16.843264	-0.046036	3.410212
233.563062	3889.723133	16.848269	-0.046042	3.406923
233.714717	3881.723425	16.853274	-0.046065	3.403616
233.664839	3873.773112	16.858279	-0.046051	3.400320
233.392540	3865.829598	16.863283	-0.045995	3.397016
233.231354	3857.779389	16.868288	-0.045960	3.393669
233.525447	3849.668120	16.873293	-0.046009	3.390308
233.206803	3841.731944	16.878298	-0.045945	3.386996
233.202589	3833.744140	16.883303	-0.045939	3.383670
233.280097	3825.798453	16.888307	-0.045948	3.380361
233.132290	3817.810830	16.893312	-0.045916	3.377023
233.174965	3809.809741	16.898317	-0.045918	3.373683
233.263163	3801.796256	16.903322	-0.045930	3.370336
233.157699	3793.806500	16.908327	-0.045905	3.366989
233.133090	3785.822287	16.913331	-0.045895	3.363644
233.033525	3777.846515	16.918336	-0.045871	3.360296
233.231608	3769.875433	16.923341	-0.045903	3.356958
233.065224	3761.865637	16.928346	-0.045867	3.353587
233.019937	3753.838671	16.933351	-0.045853	3.350209
233.073293	3745.877251	16.938355	-0.045858	3.346860
232.961532	3737.860363	16.943360	-0.045832	3.343477
232.817022	3729.888523	16.948365	-0.045800	3.340109
232.915407	3721.921350	16.953370	-0.045813	3.336749
232.933342	3713.915300	16.958375	-0.045811	3.333365
232.804387	3705.900742	16.963379	-0.045782	3.329970
232.875818	3697.924720	16.968384	-0.045790	3.326594
232.894941	3689.938551	16.973389	-0.045789	3.323209
232.722146	3681.964203	16.978394	-0.045751	3.319818
232.536806	3673.996259	16.983399	-0.045712	3.316426
232.718972	3665.976864	16.988403	-0.045740	3.313022
232.394476	3657.938765	16.993408	-0.045675	3.309588
232.242589	3650.008772	16.998413	-0.045641	3.306203
232.301732	3641.995752	17.003418	-0.045647	3.302787
232.172930	3634.012172	17.008423	-0.045618	3.299373
232.220103	3626.058394	17.013427	-0.045622	3.295974
232.006758	3618.045026	17.018432	-0.045577	3.292537
232.286795	3610.005240	17.023437	-0.045624	3.289104
232.231505	3602.066512	17.028442	-0.045608	3.285697
232.176770	3594.066941	17.033447	-0.045593	3.282261
232.302618	3586.112445	17.038451	-0.045611	3.278848
232.300228	3578.090033	17.043456	-0.045605	3.275397
232.138584	3570.081133	17.048461	-0.045570	3.271942
232.038315	3562.104140	17.053466	-0.045546	3.268499
232.041089	3554.095829	17.058471	-0.045542	3.265043
231.998502	3546.150711	17.063475	-0.045529	3.261610
231.944435	3538.147209	17.068480	-0.045513	3.258146
232.014520	3530.151657	17.073485	-0.045521	3.254688
232.059463	3522.138806	17.078490	-0.045524	3.251217
231.911161	3514.150159	17.083495	-0.045492	3.247745
231.970283	3506.158143	17.088499	-0.045497	3.244277
231.899825	3498.211771	17.093504	-0.045479	3.240819
231.831262	3490.240761	17.098509	-0.045461	3.237347
231.783043	3482.220586	17.103514	-0.045447	3.233851
231.663396	3474.151385	17.108519	-0.045420	3.230326
231.633676	3466.197705	17.113523	-0.045409	3.226852
231.497555	3458.231871	17.118528	-0.045378	3.223365
231.505332	3450.231285	17.123533	-0.045375	3.219864
231.563795	3442.255293	17.128538	-0.045380	3.216372
231.478400	3434.265197	17.133543	-0.045359	3.212865
231.484109	3426.271721	17.138547	-0.045355	3.209356
231.526336	3418.271467	17.143552	-0.045358	3.205841
231.365603	3410.324018	17.148557	-0.045323	3.202338
231.232828	3402.345149	17.153562	-0.045293	3.198818
231.182792	3394.365138	17.158567	-0.045278	3.195297
231.303838	3386.360680	17.163571	-0.045296	3.191768
231.091805	3378.331875	17.168576	-0.045251	3.188211
231.074181	3370.365467	17.173581	-0.045243	3.184686
231.106740	3362.417874	17.178586	-0.045244	3.181167
231.117305	3354.384066	17.183591	-0.045240	3.177605
231.092449	3346.418204	17.188595	-0.045230	3.174068
231.125618	3338.400874	17.193600	-0.045231	3.170506
231.050251	3330.427578	17.198605	-0.045212	3.166955
230.855792	3322.460089	17.203610	-0.045171	3.163398
230.787027	3314.464271	17.208615	-0.045153	3.159830
230.839209	3306.523773	17.213619	-0.045158	3.156287
230.754617	3298.484015	17.218624	-0.045137	3.152690
230.787574	3290.452461	17.223629	-0.045137	3.149098
230.770820	3282.499701	17.228634	-0.045129	3.145535
230.675830	3274.511449	17.233639	-0.045106	3.141949
230.667590	3266.558597	17.238643	-0.045100	3.138378
230.647743	3258.531256	17.243648	-0.045091	3.134769
230.541780	3250.571587	17.248653	-0.045066	3.131182
230.487578	3242.561958	17.253658	-0.045051	3.127571
230.527014	3234.573093	17.258663	-0.045053	3.123970
230.534818	3226.639403	17.263667	-0.045049	3.120387
230.191609	3218.663430	17.268672	-0.044980	3.116766
230.311737	3210.629397	17.273677	-0.044997	3.113135
230.594432	3202.593282	17.278682	-0.045045	3.109507
230.528958	3194.645227	17.283687	-0.045027	3.105898
230.454590	3186.686038	17.288691	-0.045008	3.102279
230.402071	3178.689383	17.293696	-0.044993	3.098641
230.373703	3170.716170	17.298701	-0.044983	3.095010
230.064608	3162.746379	17.303706	-0.044920	3.091363
230.014826	3154.723745	17.308711	-0.044906	3.087699
230.200909	3146.723006	17.313715	-0.044935	3.084053
230.170073	3138.736560	17.318720	-0.044924	3.080398
230.168584	3130.793422	17.323725	-0.044919	3.076760
230.248085	3122.757537	17.328730	-0.044928	3.073079
230.074159	3114.702008	17.333735	-0.044891	3.069373
230.008340	3106.762706	17.338739	-0.044873	3.065721
229.752839	3098.825177	17.343744	-0.044821	3.062056
229.763258	3090.840915	17.348749	-0.044818	3.058378
229.800429	3082.855390	17.353754	-0.044819	3.054697
229.793371	3074.826601	17.358759	-0.044813	3.050988
229.847463	3066.879550	17.363763	-0.044818	3.047316
229.741146	3058.879086	17.368768	-0.044793	3.043607
229.637146	3050.935310	17.373773	-0.044768	3.039920
229.551820	3042.977778	17.378778	-0.044747	3.036223
229.662518	3034.928384	17.383783	-0.044763	3.032488
229.565265	3026.958097	17.388787	-0.044739	3.028776
229.677076	3018.949726	17.393792	-0.044755	3.025051
229.521568	3011.006499	17.398797	-0.044721	3.021339
229.278644	3003.053525	17.403802	-0.044670	3.017613
229.190829	2995.028848	17.408807	-0.044649	3.013857
229.365935	2987.020615	17.413811	-0.044676	3.010117
229.232270	2979.056715	17.418816	-0.044646	3.006378
229.305258	2971.077697	17.423821	-0.044655	3.002637
229.170372	2963.110606	17.428826	-0.044624	2.998887
229.129773	2955.128992	17.433831	-0.044612	2.995130
229.044696	2947.123049	17.438835	-0.044591	2.991354
228.986085	2939.130403	17.443840	-0.044575	2.987582
229.151486	2931.125388	17.448845	-0.044600	2.983810
229.057931	2923.176470	17.453850	-0.044578	2.980046
229.019896	2915.203381	17.458855	-0.044565	2.976270
229.105691	2907.202844	17.463859	-0.044576	2.972482
228.900052	2899.203575	17.468864	-0.044533	2.968674
228.741359	2891.234587	17.473869	-0.044498	2.964879
229.018436	2883.276914	17.478874	-0.044544	2.961106
228.992122	2875.278089	17.483879	-0.044534	2.957294
228.958838	2867.309966	17.488883	-0.044523	2.953490
228.948162	2859.274573	17.493888	-0.044516	2.949651
228.732087	2851.322759	17.498893	-0.044470	2.945836
228.779324	2843.358017	17.503898	-0.044474	2.942024
228.535895	2835.407177	17.508903	-0.044424	2.938198
228.712178	2827.414648	17.513907	-0.044451	2.934370
228.639892	2819.399213	17.518912	-0.044433	2.930512
228.426913	2811.446026	17.523917	-0.044388	2.926671
228.574825	2803.438022	17.528922	-0.044410	2.922819
228.292767	2795.483099	17.533927	-0.044353	2.918964
228.431347	2787.513953	17.538931	-0.044373	2.915119
228.370416	2779.428291	17.543936	-0.044357	2.911202
228.600807	2771.403198	17.548941	-0.044394	2.907325
228.562169	2763.474954	17.553946	-0.044382	2.903475
228.515809	2755.515085	17.558951	-0.044368	2.899604
228.418191	2747.581805	17.563955	-0.044345	2.895739
228.084111	2739.594486	17.568960	-0.044277	2.891829
227.878633	2731.616643	17.573965	-0.044234	2.887925
227.894783	2723.641626	17.578970	-0.044232	2.884029
227.895365	2715.660619	17.583975	-0.044227	2.880125
227.835025	2707.705520	17.588979	-0.044210	2.876224
227.865128	2699.673537	17.593984	-0.044211	2.872285
227.951369	2691.672935	17.598989	-0.044222	2.868360
227.771000	2683.706838	17.603994	-0.044183	2.864431
227.761233	2675.748409	17.608999	-0.044176	2.860510
227.798182	2667.781718	17.614003	-0.044178	2.856582
227.703553	2659.772606	17.619008	-0.044155	2.852621
227.625651	2651.804945	17.624013	-0.044135	2.848675
227.641857	2643.813772	17.629018	-0.044133	2.844718
227.916516	2635.820740	17.634023	-0.044179	2.840768
227.698111	2627.913553	17.639027	-0.044133	2.836828
227.326198	2619.942118	17.644032	-0.044059	2.832842
227.683390	2611.879547	17.649037	-0.044120	2.828846
227.866382	2603.893727	17.654042	-0.044149	2.824873
227.389226	2595.975839	17.659047	-0.044055	2.820891
227.614395	2587.990768	17.664051	-0.044092	2.816909
227.450430	2580.001128	17.669056	-0.044056	2.812898
227.296240	2572.010658	17.674061	-0.044022	2.808880
227.188017	2564.038207	17.679066	-0.043997	2.804869
227.275956	2556.068848	17.684071	-0.044008	2.800864
227.300420	2548.113839	17.689075	-0.044008	2.796858
227.331098	2540.111990	17.694080	-0.044008	2.792822
227.317460	2532.107070	17.699085	-0.044000	2.788777
227.344319	2524.133730	17.704090	-0.044000	2.784744
227.152572	2516.199821	17.709095	-0.043959	2.780712
227.102498	2508.245645	17.714099	-0.043945	2.776673
227.049310	2500.230386	17.719104	-0.043930	2.772596
226.978937	2492.244890	17.724109	-0.043912	2.768527
227.081808	2484.268630	17.729114	-0.043926	2.764468
226.871900	2476.313829	17.734119	-0.043881	2.760394
226.858030	2468.360056	17.739123	-0.043874	2.756327
226.898515	2460.303780	17.744128	-0.043876	2.752205
226.875410	2452.293816	17.749133	-0.043866	2.748097
226.851152	2444.336681	17.754138	-0.043857	2.744009
226.721721	2436.390510	17.759143	-0.043827	2.739914
226.519666	2428.475187	17.764147	-0.043785	2.735825
226.654608	2420.452597	17.769152	-0.043805	2.731695
226.583178	2412.491952	17.774157	-0.043786	2.727578
226.553868	2404.533526	17.779162	-0.043776	2.723459
226.558649	2396.550582	17.784167	-0.043771	2.719322
226.553566	2388.616423	17.789171	-0.043765	2.715204
226.457578	2380.598940	17.794176	-0.043742	2.711031
226.341696	2372.614217	17.799181	-0.043715	2.706867
226.377104	2364.653605	17.804186	-0.043717	2.702719
226.154987	2356.691340	17.809191	-0.043670	2.698548
226.262220	2348.703649	17.814195	-0.043685	2.694377
226.320233	2340.699059	17.819200	-0.043691	2.690188
226.484627	2332.735083	17.824205	-0.043716	2.686020
226.221698	2324.808941	17.829210	-0.043662	2.681839
226.196944	2316.836218	17.834215	-0.043652	2.677642
226.123255	2308.847618	17.839219	-0.043633	2.673426
225.803503	2300.853702	17.844224	-0.043569	2.669186
226.022054	2292.843126	17.849229	-0.043604	2.664964
226.196737	2284.881093	17.854234	-0.043632	2.660759
226.006370	2276.927314	17.859239	-0.043591	2.656528
225.911876	2268.976935	17.864243	-0.043568	2.652298
225.670825	2260.997744	17.869248	-0.043518	2.648036
225.832320	2253.016087	17.874253	-0.043543	2.643792
225.680985	2245.077998	17.879258	-0.043510	2.639545
225.594296	2237.106018	17.884263	-0.043489	2.635276
225.752452	2229.105167	17.889267	-0.043513	2.631002
225.472253	2221.143146	17.894272	-0.043455	2.626712
225.651350	2213.154909	17.899277	-0.043484	2.622431
225.636136	2205.211208	17.904282	-0.043476	2.618155
225.528597	2197.230317	17.909287	-0.043450	2.613845
225.524814	2189.246580	17.914291	-0.043445	2.609534
225.378328	2181.300426	17.919296	-0.043412	2.605226
225.139490	2173.355111	17.924301	-0.043363	2.600906
225.125867	2165.398474	17.929306	-0.043355	2.596587
225.243556	2157.275115	17.934311	-0.043372	2.592179
225.344414	2149.252676	17.939315	-0.043385	2.587818
225.196308	2141.297794	17.944320	-0.043352	2.583469
225.039747	2133.386001	17.949325	-0.043318	2.579135
225.079591	2125.445217	17.954330	-0.043320	2.574792
224.930549	2117.465920	17.959335	-0.043287	2.570408
225.049846	2109.511909	17.964339	-0.043305	2.566048
225.127517	2101.549662	17.969344	-0.043314	2.561674
224.825226	2093.626973	17.974349	-0.043252	2.557287
224.673413	2085.675811	17.979354	-0.043219	2.552888
224.673182	2077.665324	17.984359	-0.043214	2.548459
224.709429	2069.719310	17.989363	-0.043215	2.544060
224.798969	2061.741715	17.994368	-0.043227	2.539640
224.694975	2053.781302	17.999373	-0.043202	2.535208
224.738845	2045.812901	18.004378	-0.043205	2.530775
224.613543	2037.847353	18.009383	-0.043177	2.526323
224.435879	2029.916860	18.014387	-0.043139	2.521879
224.524093	2021.929001	18.019392	-0.043150	2.517414
224.562571	2013.944121	18.024397	-0.043152	2.512940
224.519753	2005.967791	18.029402	-0.043139	2.508456
224.506391	1997.973955	18.034407	-0.043131	2.503957
224.491228	1990.045347	18.039411	-0.043123	2.499486
224.251920	1982.122067	18.044416	-0.043074	2.494993
224.157732	1974.136803	18.049421	-0.043051	2.490469
224.216070	1966.166691	18.054426	-0.043057	2.485955
224.118998	1958.196856	18.059431	-0.043033	2.481422
223.976111	1950.270623	18.064435	-0.043002	2.476903
223.911867	1942.292876	18.069440	-0.042984	2.472351
224.034250	1934.303057	18.074445	-0.043002	2.467798
223.908403	1926.351049	18.079450	-0.042973	2.463240
223.916512	1918.382978	18.084455	-0.042970	2.458674
224.020482	1910.444302	18.089459	-0.042984	2.454124
223.907278	1902.442759	18.094464	-0.042958	2.449512
223.850571	1894.497364	18.099469	-0.042942	2.444929
223.929737	1886.557123	18.104474	-0.042952	2.440350
223.696220	1878.618737	18.109479	-0.042903	2.435740
223.742507	1870.581110	18.114483	-0.042906	2.431085
223.606447	1862.605225	18.119488	-0.042876	2.426443
223.703014	1854.648474	18.124493	-0.042889	2.421821
223.628208	1846.724471	18.129498	-0.042870	2.417196
223.421835	1838.762643	18.134503	-0.042826	2.412530
223.625161	1830.775748	18.139507	-0.042859	2.407872
223.464821	1822.835816	18.144512	-0.042824	2.403204
223.206325	1814.922895	18.149517	-0.042771	2.398535
223.574020	1806.928440	18.154522	-0.042834	2.393858
223.376751	1798.962745	18.159527	-0.042792	2.389145
223.300640	1791.007489	18.164531	-0.042773	2.384438
223.246829	1783.073157	18.169536	-0.042757	2.379736
223.331011	1775.114189	18.174541	-0.042768	2.375021
223.186694	1767.154726	18.179546	-0.042736	2.370277
222.929520	1759.208671	18.184551	-0.042683	2.365524
223.198598	1751.230786	18.189555	-0.042728	2.360784
223.031801	1743.309337	18.194560	-0.042692	2.356033
222.924457	1735.329050	18.199565	-0.042667	2.351242
222.865485	1727.360876	18.204570	-0.042650	2.346452
222.735258	1719.413997	18.209575	-0.042621	2.341660
222.834415	1711.461883	18.214579	-0.042634	2.336873
222.762128	1703.495616	18.219584	-0.042616	2.332054
222.785563	1695.523545	18.224589	-0.042615	2.327229
222.594254	1687.614227	18.229594	-0.042574	2.322415
222.463298	1679.669838	18.234599	-0.042545	2.317574
222.426256	1671.719811	18.239603	-0.042533	2.312727
222.525689	1663.741465	18.244608	-0.042546	2.307865
222.437723	1655.793575	18.249613	-0.042524	2.302995
222.305639	1647.879285	18.254618	-0.042495	2.298131
222.273545	1639.889146	18.259623	-0.042484	2.293219
222.178753	1631.945535	18.264627	-0.042461	2.288320
222.182617	1623.988705	18.269632	-0.042456	2.283411
222.242175	1616.040525	18.274637	-0.042462	2.278501
222.267695	1608.079157	18.279642	-0.042462	2.273569
222.094344	1600.072943	18.284647	-0.042424	2.268581
222.212016	1592.107963	18.289651	-0.042441	2.263634
222.189807	1584.175229	18.294656	-0.042432	2.258683
222.161113	1576.235349	18.299661	-0.042421	2.253717
221.934431	1568.312674	18.304666	-0.042374	2.248733
221.935684	1560.349601	18.309671	-0.042369	2.243733
221.981197	1552.420878	18.314675	-0.042373	2.238747
221.727672	1544.517718	18.319680	-0.042320	2.233740
221.898711	1536.511336	18.324685	-0.042347	2.228693
221.915604	1528.559577	18.329690	-0.042345	2.223656
221.712942	1520.641656	18.334695	-0.042302	2.218610
221.650504	1512.717019	18.339699	-0.042285	2.213560
221.919928	1504.707560	18.344704	-0.042330	2.208475
221.740592	1496.794482	18.349709	-0.042292	2.203399
221.719282	1488.878172	18.354714	-0.042283	2.198323
221.696272	1480.916309	18.359719	-0.042273	2.193206
221.712388	1472.939398	18.364723	-0.042271	2.188071
221.404508	1465.038222	18.369728	-0.042209	2.182944
221.403217	1457.079763	18.374733	-0.042203	2.177795
221.301593	1449.156774	18.379738	-0.042179	2.172647
221.030896	1441.215754	18.384743	-0.042124	2.167461
221.020332	1433.283171	18.389747	-0.042116	2.162291
221.181915	1425.328751	18.394752	-0.042141	2.157111
220.969639	1417.402910	18.399757	-0.042097	2.151901
220.832642	1409.474222	18.404762	-0.042066	2.146685
221.052572	1401.481284	18.409767	-0.042102	2.141447
221.150058	1393.550110	18.414771	-0.042115	2.136225
221.008947	1385.610258	18.419776	-0.042083	2.130963
220.844862	1377.692470	18.424781	-0.042048	2.125699
221.010592	1369.761904	18.429786	-0.042074	2.120446
220.912298	1361.830883	18.434791	-0.042050	2.115154
220.691981	1353.859640	18.439795	-0.042004	2.109810
220.652798	1345.900009	18.444800	-0.041991	2.104477
220.605904	1337.980493	18.449805	-0.041978	2.099158
220.457868	1330.073026	18.454810	-0.041945	2.093823
220.425726	1322.107733	18.459815	-0.041934	2.088446
220.495282	1314.181132	18.464819	-0.041942	2.083092
220.305717	1306.278760	18.469824	-0.041901	2.077715
220.476150	1298.318118	18.474829	-0.041928	2.072320
220.552518	1290.372571	18.479834	-0.041937	2.066912
220.103100	1282.497895	18.484839	-0.041848	2.061486
220.200542	1274.564244	18.489843	-0.041861	2.056059
220.307561	1266.600342	18.494848	-0.041876	2.050599
220.136810	1258.678389	18.499853	-0.041839	2.045124
220.124469	1250.777954	18.504858	-0.041832	2.039666
220.036760	1242.857968	18.509863	-0.041810	2.034172
219.942386	1234.903385	18.514867	-0.041787	2.028639
219.853148	1226.982110	18.519872	-0.041766	2.023114
219.967984	1219.037646	18.524877	-0.041782	2.017579
219.813227	1211.130689	18.529882	-0.041748	2.012026
219.695132	1203.190492	18.534887	-0.041721	2.006439
219.783297	1195.265146	18.539891	-0.041732	2.000868
219.825031	1187.349681	18.544896	-0.041735	1.995284
219.525036	1179.444582	18.549901	-0.041674	1.989656
219.538028	1171.529753	18.554906	-0.041671	1.984037
219.544771	1163.592484	18.559911	-0.041667	1.978386
219.515583	1155.685184	18.564915	-0.041657	1.972737
219.421230	1147.746928	18.569920	-0.041634	1.967042
219.262429	1139.853939	18.574925	-0.041599	1.961356
219.455650	1131.924716	18.579930	-0.041630	1.955665
219.137878	1123.986279	18.584935	-0.041566	1.949896
219.061278	1116.069556	18.589939	-0.041546	1.944152
219.090644	1108.143386	18.594944	-0.041547	1.938395
219.235216	1100.198983	18.599949	-0.041568	1.932620
219.016381	1092.313341	18.604954	-0.041523	1.926831
219.118870	1084.378815	18.609959	-0.041537	1.921024
219.139935	1076.473898	18.614963	-0.041535	1.915213
219.068806	1068.562085	18.619968	-0.041517	1.909368
218.788684	1060.682809	18.624973	-0.041460	1.903506
218.780918	1052.781863	18.629978	-0.041453	1.897640
218.696628	1044.857704	18.634983	-0.041432	1.891731
218.792984	1036.931288	18.639987	-0.041445	1.885821
218.649565	1029.051966	18.644992	-0.041413	1.879901
218.726645	1021.139052	18.649997	-0.041423	1.873962
218.614047	1013.222614	18.655002	-0.041396	1.867980
218.695927	1005.289098	18.660007	-0.041407	1.861988
218.505052	997.416591	18.665011	-0.041366	1.855991
218.491976	989.490624	18.670016	-0.041358	1.849955
218.252893	981.619255	18.675021	-0.041309	1.843915
218.352842	973.725230	18.680026	-0.041322	1.837877
218.341935	965.804548	18.685031	-0.041315	1.831785
218.155495	957.926305	18.690035	-0.041275	1.825685
218.027840	950.038073	18.695040	-0.041246	1.819564
218.076702	942.129345	18.700045	-0.041250	1.813428
218.095768	934.226710	18.705050	-0.041249	1.807271
217.845715	926.364292	18.710055	-0.041197	1.801093
217.849242	918.470283	18.715059	-0.041193	1.794899
217.806908	910.505305	18.720064	-0.041180	1.788622
217.713226	902.618653	18.725069	-0.041157	1.782379
217.615025	894.761950	18.730074	-0.041134	1.776137
217.590292	886.839422	18.735079	-0.041124	1.769830
217.371254	878.993160	18.740083	-0.041078	1.763537
217.469802	871.099048	18.745088	-0.041091	1.757222
217.454108	863.194845	18.750093	-0.041083	1.750863
217.436993	855.315109	18.755098	-0.041075	1.744499
217.201727	847.468265	18.760103	-0.041026	1.738112
217.450326	839.536991	18.765107	-0.041067	1.731693
217.262631	831.680442	18.770112	-0.041027	1.725257
217.014445	823.845928	18.775117	-0.040976	1.718806
217.221372	815.934319	18.780122	-0.041009	1.712326
217.081094	808.040880	18.785127	-0.040978	1.705791
216.996442	800.186476	18.790131	-0.040957	1.699271
217.008617	792.306681	18.795136	-0.040955	1.692718
217.042359	784.402619	18.800141	-0.040956	1.686121
216.871853	776.575308	18.805146	-0.040919	1.679536
216.877774	768.700858	18.810151	-0.040915	1.672909
216.805196	760.828896	18.815155	-0.040896	1.666247
216.785697	752.971362	18.820160	-0.040888	1.659578
216.631140	745.126816	18.825165	-0.040854	1.652874
216.714072	737.241019	18.830170	-0.040864	1.646140
216.848207	729.359038	18.835175	-0.040884	1.639389
216.526124	721.537204	18.840179	-0.040819	1.632599
216.573168	713.616492	18.845184	-0.040823	1.625746
216.372936	705.794076	18.850189	-0.040780	1.618915
216.316422	697.950751	18.855194	-0.040765	1.612057
216.083049	690.105596	18.860199	-0.040716	1.605143
216.049036	682.278305	18.865203	-0.040705	1.598243
216.268893	674.381096	18.870208	-0.040740	1.591287
215.931706	666.578183	18.875213	-0.040673	1.584305
215.933028	658.741598	18.880218	-0.040668	1.577311
215.790151	650.883229	18.885223	-0.040636	1.570245
215.875740	643.038956	18.890227	-0.040647	1.563193
215.538925	635.264504	18.895232	-0.040579	1.556110
215.621186	627.372005	18.900237	-0.040589	1.548950
215.693253	619.524984	18.905242	-0.040598	1.541796
215.348875	611.740574	18.910247	-0.040529	1.534604
215.335607	603.891997	18.915251	-0.040521	1.527368
215.426555	596.047432	18.920256	-0.040533	1.520118
215.155744	588.266235	18.925261	-0.040477	1.512837
215.289112	580.404995	18.930266	-0.040497	1.505507
215.308303	572.586511	18.935271	-0.040496	1.498165
215.223880	564.771722	18.940275	-0.040475	1.490773
215.005075	556.993730	18.945280	-0.040429	1.483359
215.068266	549.171350	18.950285	-0.040436	1.475910
215.133806	541.302942	18.955290	-0.040443	1.468378
215.011401	533.497668	18.960295	-0.040415	1.460839
214.979766	525.705908	18.965299	-0.040404	1.453289
214.691097	517.940590	18.970304	-0.040345	1.445683
214.529120	510.165118	18.975309	-0.040310	1.438048
214.559910	502.363623	18.980314	-0.040311	1.430377
214.377948	494.587028	18.985319	-0.040272	1.422655
214.476124	486.784216	18.990323	-0.040285	1.414911
214.308630	479.009333	18.995328	-0.040249	1.407108
214.291655	471.228109	19.000333	-0.040241	1.399281
214.206337	463.455640	19.005338	-0.040220	1.391407
214.127669	455.665596	19.010343	-0.040200	1.383471
214.114069	447.904380	19.015347	-0.040193	1.375529
214.255539	440.097603	19.020352	-0.040214	1.367522
213.930153	432.388629	19.025357	-0.040148	1.359488
213.847093	424.637099	19.030362	-0.040128	1.351404
213.728945	416.873146	19.035367	-0.040101	1.343252
213.903307	409.107568	19.040371	-0.040128	1.335100
213.809933	401.357453	19.045376	-0.040106	1.326867
213.627562	393.645249	19.050381	-0.040067	1.318607
213.542426	385.831878	19.055386	-0.040046	1.310203
213.451834	378.050502	19.060391	-0.040024	1.301779
213.472351	370.324810	19.065395	-0.040023	1.293381
213.255255	362.634736	19.070400	-0.039978	1.284924
213.235107	354.925251	19.075405	-0.039969	1.276425
213.371878	347.184944	19.080410	-0.039989	1.267865
213.461882	339.456576	19.085415	-0.040001	1.259251
213.391758	331.770286	19.090419	-0.039983	1.250595
213.004581	324.140598	19.095424	-0.039906	1.241881
212.915212	316.454984	19.100429	-0.039884	1.233100
212.918631	308.745340	19.105434	-0.039880	1.224246
212.822524	301.072602	19.110439	-0.039857	1.215351
212.362941	293.455867	19.115443	-0.039767	1.206383
212.524651	285.764773	19.120448	-0.039792	1.197385
212.430122	278.097705	19.125453	-0.039769	1.188296
212.412643	270.445233	19.130458	-0.039761	1.179169
212.113054	262.828669	19.135463	-0.039700	1.169957
212.105786	255.185664	19.140467	-0.039694	1.160700
212.100696	247.526476	19.145472	-0.039688	1.151349
211.792169	239.907356	19.150477	-0.039626	1.141907
211.993221	232.252103	19.155482	-0.039658	1.132450
211.687106	224.673402	19.160487	-0.039596	1.122900
211.604723	217.084108	19.165491	-0.039576	1.113304
211.662235	209.466027	19.170496	-0.039582	1.103617
211.580319	201.889128	19.175501	-0.039562	1.093868
211.375116	194.341711	19.180506	-0.039519	1.084041
211.215450	186.792981	19.185511	-0.039484	1.074133
210.867506	179.271261	19.190515	-0.039414	1.064125
210.788926	171.725607	19.195520	-0.039395	1.054052
210.379690	164.227048	19.200525	-0.039314	1.043868
210.463594	156.684517	19.205530	-0.039324	1.033641
210.129145	149.199603	19.210535	-0.039257	1.023290
209.719717	141.751827	19.215539	-0.039176	1.012867
209.339857	134.303421	19.220544	-0.039101	1.002342
208.959442	126.848793	19.225549	-0.039025	0.991696
208.346417	119.437518	19.230554	-0.038906	0.980939
207.791281	112.036515	19.235559	-0.038798	0.970091
207.428831	104.625030	19.240563	-0.038726	0.959155
206.947370	97.241160	19.245568	-0.038631	0.948102
206.510597	89.859106	19.250573	-0.038545	0.936933
206.189041	82.478155	19.255578	-0.038480	0.925662
205.673876	75.150450	19.260583	-0.038380	0.914281
204.945739	67.854185	19.265587	-0.038240	0.902747
204.548128	60.761598	19.270592	-0.038161	0.891478