Fri Apr 16 18:24:11 2021

Number of Points = 3638
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.719575	-0.172584	0.000000	-0.000182	0.325537

2.585475	-0.150837	0.005005	-0.000157	0.325526
2.565527	-0.145775	0.010010	-0.000154	0.325534
2.222771	-0.081467	0.015014	-0.000090	0.325545
2.184024	-0.075960	0.020019	-0.000084	0.325540
2.045693	-0.048710	0.025024	-0.000058	0.325551
2.124450	-0.065320	0.030029	-0.000073	0.325542
2.064096	-0.052186	0.035034	-0.000062	0.325553
1.713544	0.010779	0.040038	0.000003	0.325551
2.054829	-0.052553	0.045043	-0.000061	0.325547
2.663442	-0.166607	0.050048	-0.000175	0.325532
2.136419	-0.070276	0.055053	-0.000077	0.325537
1.902196	-0.087998	0.060058	-0.000034	0.325270
2.377266	-0.191709	0.065062	-0.000122	0.325194
2.191971	-0.157999	0.070067	-0.000088	0.325196
2.445191	-0.204820	0.075072	-0.000136	0.325194
2.261209	-0.171756	0.080077	-0.000102	0.325194
2.260310	-0.169506	0.085082	-0.000102	0.325205
2.470149	-0.247398	0.090086	-0.000141	0.325029
2.038867	-0.201002	0.095091	-0.000061	0.324888
2.261321	-0.241525	0.100096	-0.000103	0.324889
1.623871	-0.125956	0.105101	0.000015	0.324890
1.981089	-0.192452	0.110106	-0.000052	0.324884
2.267623	-0.266370	0.115110	-0.000105	0.324788
2.524617	-0.369790	0.120115	-0.000154	0.324537
2.536073	-0.370038	0.125120	-0.000156	0.324547
2.515112	-0.369685	0.130125	-0.000152	0.324533
1.807125	-0.252771	0.135130	-0.000021	0.324482
1.699569	-0.277411	0.140134	-0.000001	0.324287
2.006858	-0.336283	0.145139	-0.000059	0.324274
1.924948	-0.319021	0.150144	-0.000044	0.324287
1.544296	-0.269738	0.155149	0.000027	0.324200
1.745451	-0.362636	0.160154	-0.000011	0.323950
1.646677	-0.345775	0.165158	0.000007	0.323946
1.568443	-0.331291	0.170163	0.000021	0.323949
1.415576	-0.333295	0.175168	0.000049	0.323817
1.394648	-0.370027	0.180173	0.000053	0.323638
1.721755	-0.428433	0.185178	-0.000008	0.323644
1.335954	-0.358222	0.190182	0.000063	0.323646
1.679462	-0.495502	0.195187	-0.000001	0.323313
2.611686	-0.671942	0.200192	-0.000175	0.323282
2.415289	-0.649301	0.205197	-0.000139	0.323225
2.487026	-0.712719	0.210202	-0.000152	0.323001
2.836655	-0.780078	0.215206	-0.000218	0.322985
2.533461	-0.781893	0.220211	-0.000162	0.322732
2.114309	-0.720454	0.225216	-0.000084	0.322668
2.504902	-0.818594	0.230221	-0.000157	0.322547
2.634352	-0.889096	0.235226	-0.000181	0.322338
2.809922	-0.930686	0.240230	-0.000214	0.322296
2.300607	-0.902955	0.245235	-0.000120	0.322007
2.709845	-0.978012	0.250240	-0.000196	0.322005
2.279352	-0.956959	0.255245	-0.000117	0.321750
2.351800	-0.976616	0.260250	-0.000130	0.321722
2.179126	-0.998877	0.265254	-0.000099	0.321482
2.483102	-1.076483	0.270259	-0.000155	0.321383
2.282266	-1.082210	0.275264	-0.000118	0.321195
2.166706	-1.086389	0.280269	-0.000097	0.321083
2.605598	-1.211156	0.285274	-0.000179	0.320881
1.932139	-1.110947	0.290278	-0.000054	0.320783
1.586690	-1.083342	0.295283	0.000010	0.320626
1.676090	-1.118502	0.300288	-0.000007	0.320542
1.729578	-1.176059	0.305293	-0.000018	0.320328
1.946534	-1.245620	0.310298	-0.000058	0.320193
1.925016	-1.286082	0.315302	-0.000054	0.319994
2.259494	-1.375297	0.320307	-0.000117	0.319867
1.785587	-1.343703	0.325312	-0.000029	0.319622
1.379091	-1.283301	0.330317	0.000046	0.319563
1.819296	-1.421966	0.335322	-0.000036	0.319299
2.265631	-1.525163	0.340326	-0.000119	0.319200
1.995179	-1.538336	0.345331	-0.000069	0.318919
1.972164	-1.564744	0.350336	-0.000065	0.318782
2.207816	-1.650258	0.355341	-0.000110	0.318590
1.676987	-1.605876	0.360346	-0.000011	0.318355
1.825066	-1.656386	0.365350	-0.000039	0.318249
2.010225	-1.746930	0.370355	-0.000074	0.317992
1.866602	-1.758937	0.375360	-0.000047	0.317820
1.418680	-1.713321	0.380365	0.000036	0.317659
1.273399	-1.745802	0.385370	0.000062	0.317392
1.422567	-1.800610	0.390374	0.000034	0.317267
1.412817	-1.855575	0.395379	0.000036	0.317010
1.337682	-1.880614	0.400384	0.000049	0.316835
1.668275	-1.972962	0.405389	-0.000012	0.316689
1.563208	-2.016701	0.410394	0.000007	0.316404
1.196684	-1.989614	0.415398	0.000075	0.316225
1.271420	-2.036204	0.420403	0.000061	0.316075
1.098820	-2.066557	0.425408	0.000092	0.315794
0.870687	-2.055938	0.430413	0.000135	0.315655
1.208788	-2.145518	0.435418	0.000071	0.315527
1.367870	-2.248217	0.440422	0.000041	0.315190
0.631461	-2.152902	0.445427	0.000178	0.315015
0.643441	-2.186700	0.450432	0.000176	0.314871
0.091119	-2.154364	0.455437	0.000278	0.314560
-0.218632	-2.129642	0.460442	0.000335	0.314417
-0.830799	-2.050095	0.465446	0.000449	0.314273
-1.170245	-2.050075	0.470451	0.000512	0.313990
-0.968545	-2.107832	0.475456	0.000474	0.313895
-1.072657	-2.149118	0.480461	0.000493	0.313619
-1.194218	-2.163986	0.485466	0.000515	0.313450
-1.877130	-2.072200	0.490470	0.000642	0.313302
-1.414014	-2.207673	0.495475	0.000556	0.313067
-1.820710	-2.155235	0.500480	0.000631	0.312969
-2.711704	-2.057483	0.505485	0.000796	0.312674
-2.815768	-2.056505	0.510490	0.000816	0.312593
-2.942288	-2.082205	0.515494	0.000839	0.312369
-3.155554	-2.075277	0.520499	0.000878	0.312223
-3.176829	-2.112235	0.525504	0.000882	0.312036
-3.220497	-2.141672	0.530509	0.000890	0.311864
-3.984691	-2.027192	0.535514	0.001031	0.311753
-4.142962	-2.044041	0.540518	0.001061	0.311542
-3.934629	-2.112337	0.545523	0.001022	0.311403
-3.893967	-2.163594	0.550528	0.001014	0.311200
-4.874403	-2.005937	0.555533	0.001196	0.311107
-4.634637	-2.097296	0.560538	0.001151	0.310886
-4.881750	-2.071866	0.565542	0.001196	0.310797
-5.676428	-1.964278	0.570547	0.001344	0.310627
-5.381608	-2.036369	0.575552	0.001289	0.310542
-5.689112	-2.019472	0.580557	0.001346	0.310362
-5.872689	-2.019785	0.585562	0.001380	0.310207
-6.325489	-1.961548	0.590566	0.001464	0.310096
-6.410869	-1.991706	0.595571	0.001479	0.309885
-6.367991	-2.006131	0.600576	0.001471	0.309856
-7.076020	-1.942743	0.605581	0.001602	0.309552
-6.923651	-1.968861	0.610586	0.001574	0.309561
-6.912651	-2.018608	0.615590	0.001571	0.309340
-7.145721	-1.991568	0.620595	0.001614	0.309269
-7.499467	-1.960732	0.625600	0.001680	0.309115
-7.531700	-1.995654	0.630605	0.001685	0.308925
-7.118296	-2.085693	0.635610	0.001608	0.308857
-8.088977	-1.958542	0.640614	0.001789	0.308628
-8.260554	-1.927549	0.645619	0.001820	0.308629
-8.008296	-2.030783	0.650624	0.001773	0.308361
-8.938050	-1.873331	0.655629	0.001946	0.308309
-8.183674	-2.038353	0.660634	0.001805	0.308179
-7.788751	-2.149717	0.665638	0.001731	0.307995
-8.044267	-2.118830	0.670643	0.001778	0.307923
-8.662573	-2.062964	0.675648	0.001893	0.307659
-8.842145	-2.030626	0.680653	0.001926	0.307660
-9.026233	-2.053656	0.685658	0.001960	0.307395
-9.319849	-2.011144	0.690662	0.002014	0.307346
-9.363094	-2.036063	0.695667	0.002022	0.307193
-9.037360	-2.134436	0.700672	0.001961	0.307010
-9.886485	-1.983687	0.705677	0.002119	0.306995
-10.093075	-1.999592	0.710682	0.002157	0.306745
-10.032365	-2.009717	0.715686	0.002145	0.306751
-10.108645	-2.044167	0.720691	0.002159	0.306524
-10.632105	-1.974001	0.725696	0.002256	0.306408
-10.344023	-2.033567	0.730701	0.002202	0.306376
-10.472798	-2.069878	0.735706	0.002226	0.306095
-10.966488	-1.979512	0.740710	0.002318	0.306100
-11.014170	-2.011216	0.745715	0.002326	0.305910
-11.419030	-1.965082	0.750720	0.002401	0.305782
-11.534326	-1.945510	0.755725	0.002422	0.305777
-11.806001	-1.942233	0.760730	0.002472	0.305561
-11.937144	-1.925419	0.765734	0.002497	0.305529
-11.313368	-2.061950	0.770739	0.002380	0.305421
-11.781688	-2.030593	0.775744	0.002467	0.305168
-12.079541	-1.977237	0.780749	0.002522	0.305166
-12.165872	-2.001281	0.785754	0.002538	0.304979
-12.311214	-2.001351	0.790758	0.002565	0.304855
-12.210778	-2.025104	0.795763	0.002546	0.304830
-12.612182	-2.016046	0.800768	0.002620	0.304529
-12.780725	-1.989217	0.805773	0.002651	0.304512
-12.832888	-1.999842	0.810778	0.002660	0.304418
-13.035941	-2.001138	0.815782	0.002698	0.304238
-13.401740	-1.934280	0.820787	0.002766	0.304242
-13.499513	-1.954582	0.825792	0.002783	0.304062
-14.161724	-1.866051	0.830797	0.002906	0.303912
-13.267682	-2.032053	0.835802	0.002740	0.303897
-13.711736	-2.000806	0.840806	0.002822	0.303663
-14.379553	-1.893519	0.845811	0.002946	0.303598
-13.898690	-1.981354	0.850816	0.002856	0.303597
-14.064140	-2.020551	0.855821	0.002887	0.303268
-14.336733	-1.972054	0.860826	0.002937	0.303265
-14.540364	-1.950391	0.865830	0.002974	0.303193
-14.559857	-1.993094	0.870835	0.002978	0.302974
-14.410367	-2.017909	0.875840	0.002950	0.302987
-14.950915	-1.958781	0.880845	0.003050	0.302802
-14.964167	-1.990077	0.885850	0.003052	0.302642
-15.106285	-1.964533	0.890854	0.003078	0.302643
-15.520924	-1.938816	0.895859	0.003155	0.302407
-15.766783	-1.908775	0.900864	0.003200	0.302338
-15.885053	-1.888857	0.905869	0.003222	0.302332
-15.876734	-1.941656	0.910874	0.003220	0.302089
-16.136983	-1.911579	0.915878	0.003268	0.302008
-15.850960	-1.966478	0.920883	0.003215	0.301995
-15.828158	-2.019757	0.925888	0.003210	0.301761
-16.488482	-1.910935	0.930893	0.003333	0.301709
-16.601163	-1.886272	0.935898	0.003353	0.301731
-16.671414	-1.940571	0.940902	0.003366	0.301411
-17.265017	-1.837373	0.945907	0.003476	0.301390
-16.953103	-1.892570	0.950912	0.003418	0.301399
-17.298718	-1.888762	0.955917	0.003482	0.301117
-17.463464	-1.865180	0.960922	0.003512	0.301088
-17.550623	-1.849302	0.965926	0.003528	0.301090
-17.817685	-1.852405	0.970931	0.003578	0.300843
-17.616092	-1.903745	0.975936	0.003540	0.300774
-18.105636	-1.815341	0.980941	0.003630	0.300773
-17.719058	-1.920869	0.985946	0.003558	0.300605
-17.976898	-1.890338	0.990950	0.003606	0.300528
-18.166801	-1.857365	0.995955	0.003641	0.300522
-18.214157	-1.894077	1.000960	0.003649	0.300305
-19.056480	-1.761053	1.005965	0.003806	0.300210
-18.889829	-1.793986	1.010970	0.003774	0.300199
-19.066916	-1.786554	1.015974	0.003807	0.300081
-18.986980	-1.846284	1.020979	0.003792	0.299865
-18.949112	-1.851374	1.025984	0.003784	0.299875
-18.664090	-1.934939	1.030989	0.003731	0.299723
-18.887578	-1.935906	1.035994	0.003772	0.299524
-19.045770	-1.906065	1.040998	0.003802	0.299531
-19.119977	-1.928576	1.046003	0.003815	0.299359
-19.162731	-1.945852	1.051008	0.003823	0.299239
-19.264715	-1.927107	1.056013	0.003841	0.299242
-19.593720	-1.917895	1.061018	0.003902	0.298999
-19.583444	-1.940324	1.066022	0.003900	0.298901
-19.511462	-1.954229	1.071027	0.003886	0.298899
-19.529458	-2.009186	1.076032	0.003889	0.298618
-20.676848	-1.804898	1.081037	0.004102	0.298599
-20.304739	-1.872640	1.086042	0.004033	0.298600
-19.858078	-2.020181	1.091046	0.003949	0.298280
-20.858064	-1.840062	1.096051	0.004135	0.298274
-20.886199	-1.834953	1.101056	0.004140	0.298275
-20.978281	-1.875825	1.106061	0.004157	0.297997
-21.367836	-1.803290	1.111066	0.004229	0.298008
-21.347424	-1.808259	1.116070	0.004225	0.298003
-21.797080	-1.789325	1.121075	0.004308	0.297700
-21.528890	-1.844862	1.126080	0.004258	0.297668
-22.089980	-1.743762	1.131085	0.004362	0.297666
-21.268709	-1.941831	1.136090	0.004209	0.297430
-21.768118	-1.868139	1.141094	0.004302	0.297348
-21.807604	-1.866734	1.146099	0.004309	0.297322
-21.509578	-1.971569	1.151104	0.004253	0.297077
-21.610394	-1.970356	1.156109	0.004271	0.296995
-22.206915	-1.858653	1.161114	0.004382	0.297013
-21.916944	-1.971563	1.166118	0.004328	0.296721
-22.136407	-1.934347	1.171123	0.004368	0.296709
-21.889990	-1.994619	1.176128	0.004322	0.296635
-22.685435	-1.903746	1.181133	0.004470	0.296375
-22.625092	-1.915392	1.186138	0.004458	0.296373
-22.426330	-1.974149	1.191142	0.004421	0.296264
-23.129448	-1.886100	1.196147	0.004551	0.296072
-22.676684	-1.967781	1.201152	0.004467	0.296076
-23.033354	-1.943616	1.206157	0.004533	0.295879
-23.819494	-1.822076	1.211162	0.004679	0.295776
-23.174918	-1.943647	1.216166	0.004559	0.295757
-23.320283	-1.955703	1.221171	0.004585	0.295570
-23.841824	-1.870391	1.226176	0.004682	0.295525
-23.875036	-1.868801	1.231181	0.004688	0.295505
-24.284353	-1.851674	1.236186	0.004764	0.295226
-24.365549	-1.845976	1.241190	0.004778	0.295183
-24.756727	-1.775776	1.246195	0.004851	0.295180
-24.683564	-1.833061	1.251200	0.004837	0.294966
-25.304787	-1.737260	1.256205	0.004952	0.294884
-24.696126	-1.853848	1.261210	0.004839	0.294856
-24.591841	-1.914477	1.266214	0.004819	0.294653
-25.554562	-1.761865	1.271219	0.004998	0.294545
-24.847212	-1.891333	1.276224	0.004866	0.294542
-25.276639	-1.851194	1.281229	0.004945	0.294358
-26.119592	-1.717831	1.286234	0.005102	0.294262
-25.304886	-1.868516	1.291238	0.004950	0.294250
-25.687790	-1.834396	1.296243	0.005021	0.294077
-25.834288	-1.842737	1.301248	0.005048	0.293907
-25.585858	-1.890847	1.306253	0.005001	0.293894
-25.036992	-2.030729	1.311258	0.004899	0.293698
-26.682998	-1.747108	1.316262	0.005205	0.293623
-26.870653	-1.714363	1.321267	0.005239	0.293618
-26.528730	-1.808532	1.326272	0.005175	0.293462
-27.082217	-1.742932	1.331277	0.005278	0.293291
-26.979751	-1.761011	1.336282	0.005259	0.293295
-26.754580	-1.820001	1.341286	0.005216	0.293207
-27.378272	-1.748543	1.346291	0.005332	0.293002
-27.307434	-1.759064	1.351296	0.005319	0.293015
-27.169128	-1.800036	1.356301	0.005293	0.292939
-27.643128	-1.769972	1.361306	0.005381	0.292663
-28.005598	-1.701961	1.366310	0.005448	0.292675
-28.167244	-1.673344	1.371315	0.005477	0.292673
-27.806459	-1.793332	1.376320	0.005410	0.292406
-28.135485	-1.742745	1.381325	0.005471	0.292362
-28.424147	-1.693321	1.386330	0.005524	0.292348
-27.936223	-1.826172	1.391334	0.005433	0.292131
-28.096157	-1.820681	1.396339	0.005463	0.292016
-28.202826	-1.799441	1.401344	0.005482	0.292027
-28.298766	-1.827135	1.406349	0.005500	0.291805
-28.181830	-1.864662	1.411354	0.005478	0.291726
-28.614818	-1.781897	1.416358	0.005558	0.291747
-28.561932	-1.852690	1.421363	0.005548	0.291445
-28.576825	-1.860227	1.426368	0.005550	0.291396
-29.138739	-1.757810	1.431373	0.005654	0.291399
-29.115512	-1.820320	1.436378	0.005650	0.291111
-29.224180	-1.802315	1.441382	0.005670	0.291104
-29.284793	-1.795870	1.446387	0.005680	0.291083
-29.239027	-1.862599	1.451392	0.005672	0.290794
-29.792994	-1.764535	1.456397	0.005774	0.290783
-29.421558	-1.838427	1.461402	0.005705	0.290753
-29.533984	-1.863879	1.466406	0.005726	0.290526
-30.136357	-1.756914	1.471411	0.005837	0.290515
-29.589246	-1.870580	1.476416	0.005735	0.290446
-30.064578	-1.838159	1.481421	0.005823	0.290178
-30.254457	-1.804478	1.486426	0.005858	0.290176
-30.441953	-1.791167	1.491430	0.005893	0.290074
-31.299370	-1.675892	1.496435	0.006052	0.289873
-30.568801	-1.809339	1.501440	0.005916	0.289871
-30.919772	-1.765023	1.506445	0.005981	0.289776
-31.073426	-1.787204	1.511450	0.006009	0.289527
-30.728400	-1.849316	1.516454	0.005945	0.289532
-31.329313	-1.759013	1.521459	0.006056	0.289439
-31.845069	-1.700325	1.526464	0.006152	0.289265
-31.534267	-1.758010	1.531469	0.006094	0.289261
-31.875351	-1.712807	1.536474	0.006157	0.289178
-31.887248	-1.764397	1.541478	0.006159	0.288911
-31.680358	-1.804235	1.546483	0.006120	0.288901
-31.838850	-1.789649	1.551488	0.006149	0.288831
-32.385915	-1.737868	1.556493	0.006250	0.288594
-32.326976	-1.745256	1.561498	0.006239	0.288612
-32.539409	-1.719940	1.566502	0.006278	0.288547
-32.836928	-1.718762	1.571507	0.006333	0.288284
-32.638496	-1.752360	1.576512	0.006296	0.288298
-33.034355	-1.686460	1.581517	0.006369	0.288269
-32.775917	-1.790652	1.586522	0.006321	0.287983
-33.319994	-1.684999	1.591526	0.006422	0.288019
-33.240389	-1.709889	1.596531	0.006407	0.287968
-33.078526	-1.802492	1.601536	0.006376	0.287652
-33.408684	-1.742572	1.606541	0.006437	0.287653
-33.080620	-1.816259	1.611546	0.006376	0.287584
-33.267860	-1.831256	1.616550	0.006411	0.287339
-34.052940	-1.684949	1.621555	0.006556	0.287359
-33.747403	-1.759562	1.626560	0.006499	0.287264
-34.030370	-1.756114	1.631565	0.006552	0.287024
-33.963757	-1.768528	1.636570	0.006539	0.287024
-34.056708	-1.770724	1.641574	0.006556	0.286929
-34.706590	-1.690578	1.646579	0.006676	0.286739
-33.966200	-1.828716	1.651584	0.006538	0.286723
-33.755476	-1.904854	1.656589	0.006499	0.286534
-34.364556	-1.825861	1.661594	0.006612	0.286375
-34.194640	-1.854006	1.666598	0.006580	0.286391
-34.846889	-1.788063	1.671603	0.006701	0.286126
-35.343329	-1.703582	1.676608	0.006793	0.286099
-35.065743	-1.756369	1.681613	0.006741	0.286089
-35.690340	-1.695919	1.686618	0.006857	0.285822
-35.601813	-1.721079	1.691622	0.006840	0.285777
-35.583676	-1.727185	1.696627	0.006836	0.285765
-35.523940	-1.778945	1.701632	0.006825	0.285559
-35.679263	-1.760222	1.706637	0.006853	0.285513
-35.681214	-1.762550	1.711642	0.006853	0.285501
-35.216569	-1.915316	1.716646	0.006767	0.285156
-36.368487	-1.703098	1.721651	0.006981	0.285172
-36.468603	-1.697827	1.726656	0.006999	0.285108
-35.966999	-1.841204	1.731661	0.006905	0.284844
-36.240907	-1.791540	1.736666	0.006956	0.284845
-36.529505	-1.762240	1.741670	0.007009	0.284729
-36.991497	-1.718357	1.746675	0.007095	0.284527
-36.878407	-1.734711	1.751680	0.007074	0.284550
-37.619785	-1.623089	1.756685	0.007211	0.284434
-37.933718	-1.599170	1.761690	0.007269	0.284267
-37.475708	-1.683022	1.766694	0.007184	0.284266
-38.256647	-1.552223	1.771699	0.007329	0.284210
-38.267721	-1.605012	1.776704	0.007331	0.283933
-38.301347	-1.597400	1.781709	0.007337	0.283942
-38.385838	-1.584023	1.786714	0.007352	0.283934
-38.627326	-1.588235	1.791718	0.007397	0.283690
-39.094923	-1.514669	1.796723	0.007483	0.283633
-38.638839	-1.598263	1.801728	0.007398	0.283631
-38.841547	-1.589248	1.806733	0.007435	0.283491
-38.616737	-1.670582	1.811738	0.007393	0.283286
-38.618105	-1.667121	1.816742	0.007393	0.283304
-38.800983	-1.659599	1.821747	0.007427	0.283174
-39.135996	-1.632957	1.826752	0.007489	0.283001
-38.955109	-1.666814	1.831757	0.007455	0.282998
-38.521132	-1.777756	1.836762	0.007374	0.282835
-39.147414	-1.699990	1.841766	0.007490	0.282652
-39.100003	-1.710679	1.846771	0.007481	0.282643
-38.517344	-1.857380	1.851776	0.007372	0.282436
-39.502807	-1.698266	1.856781	0.007555	0.282335
-39.638886	-1.672809	1.861786	0.007580	0.282340
-39.258434	-1.798094	1.866790	0.007509	0.282054
-40.033582	-1.664029	1.871795	0.007653	0.282021
-40.102576	-1.654548	1.876800	0.007665	0.282007
-40.089884	-1.710340	1.881805	0.007663	0.281734
-40.071634	-1.715091	1.886810	0.007659	0.281728
-40.179910	-1.711899	1.891814	0.007679	0.281645
-40.726034	-1.661350	1.896819	0.007780	0.281396
-40.380358	-1.721917	1.901824	0.007716	0.281409
-41.000748	-1.626447	1.906829	0.007831	0.281322
-41.088022	-1.656344	1.911834	0.007847	0.281088
-40.575149	-1.748244	1.916838	0.007751	0.281097
-41.027808	-1.696697	1.921843	0.007835	0.280940
-41.589034	-1.626043	1.926848	0.007939	0.280780
-41.219053	-1.695781	1.931853	0.007870	0.280769
-41.132999	-1.738520	1.936858	0.007853	0.280631
-41.484644	-1.692661	1.941862	0.007918	0.280539
-41.520396	-1.689429	1.946867	0.007925	0.280524
-41.431134	-1.756207	1.951872	0.007908	0.280265
-42.170457	-1.632883	1.956877	0.008045	0.280209
-42.143919	-1.640223	1.961882	0.008040	0.280198
-41.922275	-1.737563	1.966886	0.007998	0.279905
-41.943623	-1.740546	1.971891	0.008002	0.279871
-42.299122	-1.688061	1.976896	0.008068	0.279810
-42.690122	-1.664854	1.981901	0.008140	0.279564
-42.050338	-1.785062	1.986906	0.008021	0.279545
-42.719220	-1.686049	1.991910	0.008145	0.279430
-43.356736	-1.602168	1.996915	0.008263	0.279265
-42.995897	-1.683360	2.001920	0.008196	0.279186

-44.100850	-1.526826	2.011917	0.008401	0.278960
-43.632231	-1.637657	2.021914	0.008313	0.278830
-43.844252	-1.637351	2.031910	0.008352	0.278635
-43.866403	-1.646666	2.041907	0.008355	0.278569
-44.117792	-1.649131	2.051904	0.008401	0.278322
-44.305989	-1.616585	2.061901	0.008436	0.278317
-44.344268	-1.611300	2.071898	0.008442	0.278311
-44.215542	-1.691069	2.081894	0.008417	0.278021
-44.507579	-1.638754	2.091891	0.008471	0.278021
-44.317344	-1.673239	2.101888	0.008435	0.278025
-44.314902	-1.677942	2.111885	0.008434	0.278006
-44.303141	-1.679043	2.121882	0.008431	0.278015
-44.647467	-1.616397	2.131878	0.008494	0.278019
-44.536120	-1.637179	2.141875	0.008473	0.278019
-44.227106	-1.696298	2.151872	0.008415	0.278007
-44.429956	-1.657533	2.161869	0.008452	0.278021
-44.225607	-1.697105	2.171866	0.008413	0.278011
-44.499763	-1.647662	2.181862	0.008464	0.278013
-44.351332	-1.675555	2.191859	0.008435	0.278012
-44.319914	-1.681123	2.201856	0.008429	0.278016
-44.222132	-1.702638	2.211853	0.008410	0.278000
-43.889926	-1.765381	2.221850	0.008347	0.277991
-44.039333	-1.699194	2.231846	0.008374	0.278198
-43.769513	-1.730273	2.241843	0.008324	0.278295
-43.589085	-1.764798	2.251840	0.008289	0.278289
-43.603155	-1.763198	2.261837	0.008291	0.278288
-43.599594	-1.733507	2.271834	0.008290	0.278449
-43.695824	-1.683561	2.281830	0.008307	0.278621
-43.233663	-1.772281	2.291827	0.008220	0.278600
-43.217390	-1.752803	2.301824	0.008217	0.278720
-43.229714	-1.710630	2.311821	0.008218	0.278931
-43.390601	-1.681565	2.321818	0.008248	0.278933
-43.675845	-1.573740	2.331814	0.008300	0.279227
-42.909702	-1.706651	2.341811	0.008157	0.279264
-42.922630	-1.667064	2.351808	0.008158	0.279460
-42.429943	-1.739214	2.361805	0.008066	0.279554
-42.395370	-1.718821	2.371802	0.008059	0.279695
-42.173533	-1.726740	2.381798	0.008017	0.279866
-41.779190	-1.784856	2.391795	0.007943	0.279940
-41.561858	-1.777956	2.401792	0.007902	0.280183
-41.999444	-1.682031	2.411789	0.007982	0.280271
-41.329207	-1.756143	2.421786	0.007857	0.280521
-41.491370	-1.715217	2.431782	0.007887	0.280584
-41.190817	-1.735579	2.441779	0.007830	0.280764
-41.438291	-1.661906	2.451776	0.007875	0.280915
-41.212141	-1.669423	2.461773	0.007832	0.281092
-41.232851	-1.616303	2.471770	0.007836	0.281349
-41.237811	-1.590718	2.481766	0.007836	0.281480
-40.704761	-1.637399	2.491763	0.007736	0.281741
-40.873546	-1.564740	2.501760	0.007767	0.281960
-40.413286	-1.620021	2.511757	0.007680	0.282109
-39.761894	-1.694858	2.521754	0.007558	0.282336
-39.806200	-1.647167	2.531750	0.007566	0.282543
-39.256041	-1.726694	2.541747	0.007463	0.282651
-39.300707	-1.650283	2.551744	0.007470	0.283004
-39.133627	-1.654849	2.561741	0.007439	0.283140
-38.752294	-1.696603	2.571738	0.007367	0.283284
-38.570958	-1.672840	2.581734	0.007333	0.283577
-38.122539	-1.727034	2.591731	0.007248	0.283720
-37.760754	-1.756939	2.601728	0.007180	0.283906
-37.408392	-1.772689	2.611725	0.007114	0.284156
-37.910591	-1.653287	2.621722	0.007207	0.284302
-37.570946	-1.667175	2.631718	0.007143	0.284549
-36.671333	-1.791311	2.641715	0.006975	0.284753
-36.944313	-1.715138	2.651712	0.007025	0.284891
-36.497182	-1.740463	2.661709	0.006941	0.285179
-36.736126	-1.657078	2.671706	0.006985	0.285385
-36.199250	-1.723281	2.681702	0.006884	0.285548
-35.768108	-1.760480	2.691699	0.006803	0.285760
-35.821070	-1.714077	2.701696	0.006812	0.285949
-35.135781	-1.812190	2.711693	0.006684	0.286087
-35.479004	-1.689924	2.721690	0.006747	0.286393
-34.925813	-1.752334	2.731686	0.006644	0.286589
-34.984682	-1.706344	2.741683	0.006654	0.286770
-34.806279	-1.688629	2.751680	0.006620	0.287027
-34.406730	-1.714765	2.761677	0.006545	0.287264
-34.431792	-1.674614	2.771674	0.006549	0.287447
-34.128019	-1.687279	2.781670	0.006492	0.287664
-33.567350	-1.727697	2.791667	0.006387	0.287977
-33.572825	-1.696302	2.801664	0.006387	0.288133
-32.798141	-1.807512	2.811661	0.006242	0.288285
-32.822774	-1.741825	2.821658	0.006246	0.288596
-32.362194	-1.792784	2.831654	0.006160	0.288763
-31.818508	-1.867321	2.841651	0.006058	0.288888
-31.713706	-1.822328	2.851648	0.006038	0.289212
-31.671977	-1.802399	2.861645	0.006029	0.289353
-31.667799	-1.768115	2.871642	0.006028	0.289532
-31.677588	-1.702432	2.881638	0.006029	0.289854
-31.739912	-1.649180	2.891635	0.006040	0.290067
-31.217008	-1.699417	2.901632	0.005942	0.290294
-31.096089	-1.671704	2.911629	0.005918	0.290545
-30.877273	-1.665426	2.921626	0.005877	0.290777
-30.359296	-1.719579	2.931622	0.005780	0.290980
-30.412127	-1.670304	2.941619	0.005789	0.291180
-30.337944	-1.632937	2.951616	0.005774	0.291436
-30.244019	-1.585018	2.961613	0.005756	0.291762
-29.539415	-1.674197	2.971610	0.005624	0.291958
-29.492611	-1.639741	2.981606	0.005615	0.292174
-29.065065	-1.674533	2.991603	0.005535	0.292390
-29.076761	-1.611122	3.001600	0.005536	0.292697
-28.815035	-1.604133	3.011597	0.005487	0.292970
-28.183279	-1.682446	3.021594	0.005369	0.293153
-27.906813	-1.696284	3.031590	0.005316	0.293336
-27.579735	-1.699038	3.041587	0.005255	0.293619
-27.028690	-1.757041	3.051584	0.005152	0.293830
-27.218408	-1.684635	3.061581	0.005186	0.294020
-26.157156	-1.833436	3.071578	0.004988	0.294240
-26.332456	-1.754357	3.081574	0.005020	0.294475
-26.171621	-1.751129	3.091571	0.004989	0.294638
-25.845503	-1.761850	3.101568	0.004928	0.294880
-26.074026	-1.662565	3.111565	0.004970	0.295166
-25.743977	-1.675986	3.121562	0.004908	0.295398
-25.855535	-1.611318	3.131558	0.004928	0.295618
-25.667404	-1.608664	3.141555	0.004892	0.295802
-25.064271	-1.655766	3.151552	0.004779	0.296111
-24.896360	-1.641279	3.161549	0.004747	0.296334
-24.775664	-1.621088	3.171546	0.004724	0.296543
-24.503931	-1.621245	3.181542	0.004673	0.296786
-24.267418	-1.609509	3.191539	0.004628	0.297056
-23.304762	-1.735835	3.201536	0.004448	0.297296
-23.532796	-1.658186	3.211533	0.004490	0.297476
-22.909536	-1.731828	3.221530	0.004373	0.297671
-22.821182	-1.680966	3.231526	0.004356	0.298000
-22.273288	-1.748431	3.241523	0.004253	0.298159
-22.668918	-1.631188	3.251520	0.004326	0.298382
-22.336288	-1.640118	3.261517	0.004264	0.298635
-21.986251	-1.649334	3.271514	0.004198	0.298902
-21.934485	-1.610460	3.281510	0.004187	0.299138
-21.593500	-1.631515	3.291507	0.004123	0.299340
-21.155870	-1.662799	3.301504	0.004041	0.299576
-20.913161	-1.652373	3.311501	0.003995	0.299842
-19.931541	-1.796884	3.321498	0.003812	0.300009
-19.949256	-1.756530	3.331494	0.003814	0.300191
-19.398689	-1.793866	3.341491	0.003711	0.300497
-19.038321	-1.840602	3.351488	0.003644	0.300590
-18.686005	-1.870511	3.361485	0.003577	0.300757
-18.803810	-1.801126	3.371482	0.003598	0.300991
-19.013837	-1.731827	3.381478	0.003637	0.301144
-18.530841	-1.767086	3.391475	0.003546	0.301399
-17.862589	-1.839163	3.401472	0.003421	0.301639
-18.203444	-1.743546	3.411469	0.003484	0.301804
-17.580132	-1.812958	3.421466	0.003367	0.302017
-17.533387	-1.770105	3.431462	0.003358	0.302266
-17.635921	-1.713250	3.441459	0.003376	0.302453
-17.018959	-1.782436	3.451456	0.003261	0.302661
-16.591976	-1.797661	3.461453	0.003181	0.302962
-16.821351	-1.720221	3.471450	0.003223	0.303136
-16.710776	-1.701976	3.481446	0.003201	0.303322
-16.523533	-1.669438	3.491443	0.003166	0.303643
-16.349166	-1.655825	3.501440	0.003133	0.303861
-15.686719	-1.735786	3.511437	0.003009	0.304057
-15.710913	-1.684323	3.521434	0.003012	0.304284
-15.321904	-1.699458	3.531430	0.002939	0.304551
-14.989066	-1.718136	3.541427	0.002877	0.304753
-14.889165	-1.692041	3.551424	0.002857	0.304966
-14.685677	-1.675908	3.561421	0.002819	0.305221
-14.069946	-1.728577	3.571418	0.002703	0.305504
-13.936054	-1.724411	3.581414	0.002678	0.305643
-13.616146	-1.749291	3.591411	0.002618	0.305803
-13.437881	-1.716685	3.601408	0.002584	0.306113
-12.989025	-1.762687	3.611405	0.002499	0.306285
-12.488006	-1.822952	3.621402	0.002406	0.306433
-12.295714	-1.792148	3.631398	0.002369	0.306746
-12.238152	-1.769632	3.641395	0.002358	0.306905
-11.891879	-1.803422	3.651392	0.002293	0.307045
-11.689905	-1.771503	3.661389	0.002254	0.307371
-11.368284	-1.795700	3.671386	0.002194	0.307536
-11.141738	-1.805737	3.681382	0.002151	0.307685
-11.023672	-1.755173	3.691379	0.002128	0.308027
-10.589150	-1.802484	3.701376	0.002047	0.308178
-9.981940	-1.887592	3.711373	0.001933	0.308300
-9.946777	-1.826645	3.721370	0.001926	0.308619
-9.884928	-1.808379	3.731366	0.001913	0.308760
-9.284318	-1.881339	3.741363	0.001801	0.308932
-9.173712	-1.838323	3.751360	0.001780	0.309231
-9.264267	-1.788466	3.761357	0.001796	0.309390
-8.863794	-1.824463	3.771354	0.001721	0.309565
-8.181163	-1.891777	3.781350	0.001593	0.309833
-8.029617	-1.896159	3.791347	0.001564	0.309944
-7.790554	-1.883993	3.801344	0.001519	0.310207
-7.881869	-1.819181	3.811341	0.001535	0.310435
-7.147493	-1.930295	3.821338	0.001398	0.310542
-7.201285	-1.867025	3.831334	0.001407	0.310794
-7.115410	-1.847205	3.841331	0.001390	0.310962
-6.385642	-1.949586	3.851328	0.001254	0.311105
-5.741922	-2.009797	3.861325	0.001133	0.311372
-5.615692	-2.020023	3.871322	0.001109	0.311434
-5.605674	-1.955889	3.881318	0.001107	0.311743
-5.908987	-1.867960	3.891315	0.001162	0.311898
-5.074152	-1.990917	3.901312	0.001006	0.312035
-4.954674	-1.952332	3.911309	0.000983	0.312317
-4.866420	-1.941387	3.921306	0.000966	0.312445
-4.512942	-1.954767	3.931302	0.000900	0.312683
-4.225592	-1.959715	3.941299	0.000846	0.312905
-3.928984	-1.989313	3.951296	0.000790	0.313020
-4.076704	-1.898255	3.961293	0.000816	0.313320
-4.162776	-1.846329	3.971290	0.000832	0.313490
-3.739760	-1.887260	3.981286	0.000752	0.313659
-3.420757	-1.885632	3.991283	0.000692	0.313937
-3.011288	-1.917692	4.001280	0.000615	0.314135
-2.972656	-1.887788	4.011277	0.000607	0.314308
-3.339900	-1.762194	4.021274	0.000675	0.314582
-2.753461	-1.814766	4.031270	0.000565	0.314833
-2.517298	-1.817993	4.041267	0.000521	0.315018
-2.888551	-1.699232	4.051264	0.000589	0.315256
-1.707994	-1.848834	4.061261	0.000369	0.315557
-1.904130	-1.778969	4.071258	0.000404	0.315717
-1.765668	-1.764162	4.081254	0.000378	0.315903
-1.684800	-1.730525	4.091251	0.000362	0.316127
-1.760397	-1.650102	4.101248	0.000375	0.316435
-1.346078	-1.669903	4.111245	0.000298	0.316691
-1.524464	-1.587213	4.121242	0.000330	0.316924
-1.091744	-1.616982	4.131238	0.000249	0.317150
-1.094379	-1.554959	4.141235	0.000249	0.317433
-0.840171	-1.544402	4.151232	0.000201	0.317694
-0.816754	-1.478722	4.161229	0.000196	0.318016
-0.653282	-1.455945	4.171226	0.000164	0.318257
-0.172889	-1.482247	4.181222	0.000074	0.318537
-0.102423	-1.434090	4.191219	0.000061	0.318817
-0.066138	-1.377994	4.201216	0.000053	0.319104
0.002328	-1.325062	4.211213	0.000040	0.319403
-0.266587	-1.209626	4.221210	0.000089	0.319707
-0.580716	-1.074298	4.231206	0.000147	0.320064
-0.458336	-1.018088	4.241203	0.000123	0.320421
-0.677676	-0.910751	4.251200	0.000163	0.320729
-0.316530	-0.902427	4.261197	0.000095	0.321065
-0.257667	-0.829273	4.271194	0.000084	0.321445
-0.062055	-0.779208	4.281190	0.000046	0.321833
-0.030014	-0.709663	4.291187	0.000040	0.322175
0.450145	-0.716854	4.301184	-0.000050	0.322537
0.450707	-0.629433	4.311181	-0.000051	0.322932
0.191750	-0.494981	4.321178	-0.000004	0.323326
0.263181	-0.416183	4.331174	-0.000018	0.323739
0.430491	-0.356515	4.341171	-0.000050	0.324144
0.495776	-0.277379	4.351168	-0.000062	0.324553
0.869293	-0.247119	4.361165	-0.000133	0.324992
0.021213	0.005549	4.371162	0.000024	0.325434
0.000000	0.098329	4.381158	0.000028	0.325832

0.444798	0.299472	4.386163	-0.000056	0.327082
0.359400	0.907205	4.391168	-0.000041	0.329692
0.155967	1.830555	4.396173	-0.000004	0.333559
0.321852	2.985868	4.401178	-0.000036	0.338661
0.972592	4.346156	4.406182	-0.000158	0.344917
1.464020	6.056538	4.411187	-0.000251	0.352383
2.433392	7.976236	4.416192	-0.000433	0.360881
2.786841	10.328227	4.421197	-0.000501	0.370438
3.146648	13.002615	4.426202	-0.000570	0.380983
3.473501	16.005068	4.431206	-0.000633	0.392434
4.683780	19.167130	4.436211	-0.000861	0.404702
4.763202	22.892495	4.441216	-0.000878	0.417852
4.917943	26.936116	4.446221	-0.000910	0.431713
6.141231	31.123346	4.451226	-0.001141	0.446236
6.652481	35.793090	4.456230	-0.001239	0.461410
7.385514	40.769785	4.461235	-0.001380	0.477152
8.683457	45.988983	4.466240	-0.001625	0.493402
9.287987	51.682214	4.471245	-0.001742	0.510123
10.091793	57.671868	4.476250	-0.001895	0.527224
10.248573	64.102798	4.481254	-0.001929	0.544649
10.446577	70.830895	4.486259	-0.001971	0.562318
10.797844	77.838917	4.491264	-0.002041	0.580215
10.881503	85.174029	4.496269	-0.002062	0.598251
11.610641	92.663239	4.501274	-0.002203	0.616391
12.233660	100.422519	4.506278	-0.002324	0.634584
12.480106	108.499372	4.511283	-0.002376	0.652824
12.759991	116.792620	4.516288	-0.002434	0.671047
13.052709	125.259020	4.521293	-0.002494	0.689156
14.148556	133.778074	4.526298	-0.002704	0.707201
14.111446	142.674294	4.531302	-0.002703	0.725146
14.962576	151.553941	4.536307	-0.002868	0.742933
15.353519	160.646820	4.541312	-0.002947	0.760553
15.664790	169.847594	4.546317	-0.003011	0.777947
16.442319	179.072454	4.551322	-0.003162	0.795155
16.469961	188.508551	4.556326	-0.003174	0.812138
16.835897	197.942545	4.561331	-0.003248	0.828873
17.251948	207.408872	4.566336	-0.003332	0.845347
17.432614	216.942555	4.571341	-0.003373	0.861549
18.191130	226.397542	4.576346	-0.003520	0.877490
18.900215	235.865813	4.581350	-0.003659	0.893153
19.427727	245.386633	4.586355	-0.003764	0.908578
19.534068	254.981918	4.591360	-0.003790	0.923747
21.053359	264.301764	4.596365	-0.004079	0.938627
24.239851	273.363992	4.601370	-0.004679	0.953325
24.826175	282.861164	4.606374	-0.004795	0.967769
24.965946	292.433757	4.611379	-0.004827	0.981997
26.335685	301.747745	4.616384	-0.005089	0.995957
26.827488	311.161619	4.621389	-0.005187	1.009647
27.586377	320.498977	4.626394	-0.005334	1.023112
28.117682	329.830236	4.631398	-0.005440	1.036337
28.338985	339.166419	4.636403	-0.005487	1.049328
28.888878	348.405951	4.641408	-0.005596	1.062106
29.911522	357.515750	4.646413	-0.005793	1.074668
30.482412	366.658245	4.651418	-0.005905	1.087023
31.022822	375.781752	4.656422	-0.006012	1.099207
31.668296	384.850058	4.661427	-0.006139	1.111209
32.396808	393.835485	4.666432	-0.006281	1.122994
33.244480	402.773150	4.671437	-0.006445	1.134622
33.971861	411.711236	4.676442	-0.006586	1.146105
34.309104	420.688213	4.681446	-0.006655	1.157440
35.726584	429.388177	4.686451	-0.006925	1.168550
36.104035	438.288213	4.691456	-0.007002	1.179582
36.157974	447.189093	4.696461	-0.007018	1.190446
37.053774	455.896199	4.701466	-0.007191	1.201151
37.919224	464.585996	4.706470	-0.007358	1.211734
38.115135	473.381115	4.711475	-0.007400	1.222215
38.248817	482.165578	4.716480	-0.007431	1.232582
38.688435	490.809851	4.721485	-0.007519	1.242760
39.669471	499.365396	4.726490	-0.007708	1.252858
40.028706	508.002389	4.731494	-0.007781	1.262848
40.756149	516.559760	4.736499	-0.007922	1.272740
41.327587	525.113386	4.741504	-0.008034	1.282521
42.030794	533.637685	4.746509	-0.008171	1.292219
42.882180	542.133666	4.751514	-0.008335	1.301842
43.851729	550.636334	4.756518	-0.008522	1.311422
44.346543	559.188336	4.761523	-0.008620	1.320900
44.963970	567.652786	4.766528	-0.008741	1.330237
45.695370	576.080666	4.771533	-0.008883	1.339489
46.588909	584.479420	4.776538	-0.009055	1.348676
47.447992	592.875682	4.781542	-0.009221	1.357792
48.270461	601.267110	4.786547	-0.009380	1.366834
48.775636	609.744163	4.791552	-0.009480	1.375852
49.249503	618.156177	4.796557	-0.009574	1.384737
49.969553	626.548530	4.801562	-0.009713	1.393587
50.534214	634.944385	4.806566	-0.009824	1.402358
51.035738	643.330864	4.811571	-0.009924	1.411054
51.905161	651.648967	4.816576	-0.010091	1.419689
53.003885	659.922302	4.821581	-0.010302	1.428265
53.364022	668.348437	4.826586	-0.010374	1.436819
53.375331	676.779254	4.831590	-0.010382	1.445271
53.691005	685.153896	4.836595	-0.010447	1.453667
54.322738	693.464603	4.841600	-0.010570	1.462003
55.056116	701.746427	4.846605	-0.010713	1.470279
56.022457	710.005764	4.851610	-0.010898	1.478524
56.567451	718.298298	4.856614	-0.011006	1.486688
57.234387	726.575551	4.861619	-0.011135	1.494812
58.140104	734.816336	4.866624	-0.011310	1.502895
58.395809	743.176478	4.871629	-0.011363	1.510946
59.210691	751.416941	4.876634	-0.011521	1.518927
59.444949	759.736942	4.881638	-0.011570	1.526852
59.952449	768.043940	4.886643	-0.011670	1.534766
60.677064	776.288335	4.891648	-0.011811	1.542613
61.255054	784.530443	4.896653	-0.011924	1.550396
61.592926	792.839388	4.901658	-0.011993	1.558166
62.251931	801.041587	4.906662	-0.012121	1.565846
62.633154	809.335662	4.911667	-0.012198	1.573532
63.182727	817.566505	4.916672	-0.012306	1.581148
64.428282	825.670769	4.921677	-0.012544	1.588714
64.509124	834.029569	4.926682	-0.012564	1.596304
65.290254	842.193807	4.931686	-0.012716	1.603784
65.924160	850.415059	4.936691	-0.012839	1.611259
66.734579	858.613324	4.941696	-0.012996	1.618704
67.023359	866.894977	4.946701	-0.013055	1.626115
68.494664	875.003065	4.951706	-0.013335	1.633506
69.022535	883.227296	4.956710	-0.013439	1.640832
69.007109	891.542084	4.961715	-0.013442	1.648129
69.661238	899.726377	4.966720	-0.013569	1.655373
70.312383	907.887363	4.971725	-0.013696	1.662565
70.150893	916.251225	4.976730	-0.013672	1.669789
70.535204	924.447058	4.981734	-0.013749	1.676912
71.109956	932.604249	4.986739	-0.013862	1.683997
71.422331	940.843571	4.991744	-0.013926	1.691088
72.229337	948.950424	4.996749	-0.014082	1.698102
72.863308	957.106170	5.001754	-0.014205	1.705106
73.554095	965.269779	5.006758	-0.014340	1.712095
73.828728	973.487837	5.011763	-0.014396	1.719045
74.204220	981.679165	5.016768	-0.014472	1.725959
74.253383	989.949711	5.021773	-0.014487	1.732868
74.648210	998.123937	5.026778	-0.014566	1.739715
75.459418	1006.208945	5.031782	-0.014723	1.746515
75.977680	1014.399770	5.036787	-0.014825	1.753338
76.698349	1022.510073	5.041792	-0.014965	1.760094
76.775065	1030.747501	5.046797	-0.014985	1.766846
77.161363	1038.952073	5.051802	-0.015062	1.773584
77.938046	1047.035892	5.056806	-0.015213	1.780249
77.970011	1055.289093	5.061811	-0.015224	1.786931
78.029952	1063.551251	5.066816	-0.015241	1.793599
78.481947	1071.642141	5.071821	-0.015331	1.800154
79.154526	1079.742232	5.076826	-0.015462	1.806720
79.473902	1087.903310	5.081830	-0.015527	1.813267
79.816693	1096.053199	5.086835	-0.015596	1.819784
81.065397	1104.073597	5.091840	-0.015834	1.826286
82.043060	1112.150001	5.096845	-0.016022	1.832775
82.226932	1120.370879	5.101850	-0.016062	1.839259
82.311365	1128.590771	5.106854	-0.016083	1.845707
82.670666	1136.750348	5.111859	-0.016156	1.852119
83.425972	1144.850777	5.116864	-0.016302	1.858510
83.911655	1152.968947	5.121869	-0.016398	1.864860
84.939604	1161.034588	5.126874	-0.016595	1.871212
85.315395	1169.209545	5.131878	-0.016671	1.877550
85.137494	1177.449249	5.136883	-0.016644	1.883851
85.774945	1185.550215	5.141888	-0.016768	1.890120
85.481861	1193.805382	5.146893	-0.016719	1.896378
85.486660	1201.981502	5.151898	-0.016726	1.902589
85.821247	1210.110062	5.156902	-0.016793	1.908783
86.861354	1218.081747	5.161907	-0.016993	1.914918
86.797682	1226.295590	5.166912	-0.016987	1.921090
86.660886	1234.486639	5.171917	-0.016967	1.927217
86.557650	1242.690846	5.176922	-0.016953	1.933338
87.675187	1250.628481	5.181926	-0.017167	1.939378
88.290556	1258.700468	5.186931	-0.017287	1.945443
89.129173	1266.791588	5.191936	-0.017449	1.951528
89.439771	1274.923159	5.196941	-0.017512	1.957565
89.830515	1283.043647	5.201946	-0.017591	1.963584
90.118026	1291.175287	5.206950	-0.017650	1.969582
90.834514	1299.239675	5.211955	-0.017789	1.975559
91.175598	1307.381248	5.216960	-0.017858	1.981533
91.468778	1315.519168	5.221965	-0.017918	1.987481
91.940692	1323.649013	5.226970	-0.018012	1.993424
92.283705	1331.755917	5.231974	-0.018081	1.999320
92.420461	1339.890220	5.236979	-0.018112	2.005195
92.994748	1347.983667	5.241984	-0.018225	2.011071
93.202163	1356.117362	5.246989	-0.018269	2.016919
93.541674	1364.233160	5.251994	-0.018338	2.022752
93.974069	1372.342024	5.256998	-0.018424	2.028573
94.713684	1380.396966	5.262003	-0.018567	2.034370
94.848184	1388.543275	5.267008	-0.018598	2.040153
95.066207	1396.655119	5.272013	-0.018644	2.045903
95.364246	1404.802617	5.277018	-0.018705	2.051671
96.130617	1412.840494	5.282022	-0.018854	2.057393
95.867498	1421.020743	5.287027	-0.018810	2.063094
96.838805	1429.030633	5.292032	-0.018997	2.068786
97.471156	1437.091729	5.297037	-0.019120	2.074464
97.940909	1445.200806	5.302042	-0.019213	2.080142
98.511527	1453.277741	5.307046	-0.019325	2.085793
98.833607	1461.418308	5.312051	-0.019391	2.091448
98.950145	1469.586177	5.317056	-0.019418	2.097085
99.071121	1477.691290	5.322061	-0.019446	2.102665
99.532660	1485.792952	5.327066	-0.019538	2.108261
99.881638	1493.928516	5.332070	-0.019608	2.113854
100.158769	1501.992195	5.337075	-0.019666	2.119376
100.748910	1510.035962	5.342080	-0.019781	2.124901
101.342800	1518.086069	5.347085	-0.019897	2.130417
101.184751	1526.280878	5.352090	-0.019873	2.135942
101.655792	1534.347689	5.357094	-0.019967	2.141428
102.055077	1542.425216	5.362099	-0.020047	2.146900
102.956477	1550.451005	5.367104	-0.020220	2.152372
103.256295	1558.556048	5.372109	-0.020282	2.157825
104.023527	1566.580155	5.377114	-0.020430	2.163255
104.448547	1574.696327	5.382118	-0.020515	2.168699
104.637699	1582.810249	5.387123	-0.020556	2.174106
104.997506	1590.939505	5.392128	-0.020628	2.179526
105.087091	1599.061125	5.397133	-0.020651	2.184902
105.719924	1607.122620	5.402138	-0.020774	2.190276
106.022799	1615.230175	5.407142	-0.020836	2.195636
106.440145	1623.271242	5.412147	-0.020919	2.200950
107.229332	1631.291032	5.417152	-0.021072	2.206271
107.208415	1639.453179	5.422157	-0.021074	2.211598
107.577374	1647.549865	5.427162	-0.021148	2.216905
107.795125	1655.651513	5.432166	-0.021194	2.222189
107.828933	1663.776861	5.437171	-0.021206	2.227458
108.038621	1671.884392	5.442176	-0.021251	2.232720
107.999889	1679.986317	5.447181	-0.021249	2.237943
108.641523	1687.981243	5.452186	-0.021374	2.243147
109.163006	1696.037620	5.457190	-0.021477	2.248367
109.762652	1704.075082	5.462195	-0.021594	2.253569
110.457969	1712.136523	5.467200	-0.021729	2.258784
110.205928	1720.310204	5.472205	-0.021688	2.263973
111.201981	1728.310471	5.477210	-0.021879	2.269151
111.657836	1736.423192	5.482214	-0.021969	2.274341
111.509434	1744.559848	5.487219	-0.021947	2.279480
111.961069	1752.576040	5.492224	-0.022037	2.284585
112.275890	1760.661198	5.497229	-0.022101	2.289709
112.616636	1768.745959	5.502234	-0.022170	2.294825
113.154171	1776.755812	5.507238	-0.022276	2.299898
113.575859	1784.813714	5.512243	-0.022360	2.304981
113.941674	1792.940435	5.517248	-0.022434	2.310090
114.135505	1801.034903	5.522253	-0.022475	2.315153
114.483530	1809.090868	5.527258	-0.022546	2.320194
115.143357	1817.108451	5.532262	-0.022674	2.325227
115.151477	1825.245343	5.537267	-0.022681	2.330268
115.365836	1833.350648	5.542272	-0.022727	2.335295
115.699369	1841.407875	5.547277	-0.022795	2.340292
116.201480	1849.444821	5.552282	-0.022894	2.345281
116.198826	1857.598586	5.557286	-0.022899	2.350287
116.862182	1865.592376	5.562291	-0.023028	2.355241
117.177896	1873.669628	5.567296	-0.023092	2.360206
117.014096	1881.781827	5.572301	-0.023067	2.365143
117.209625	1889.870384	5.577306	-0.023109	2.370084
117.927786	1897.879768	5.582310	-0.023249	2.375010
118.020203	1905.970490	5.587315	-0.023272	2.379923
118.755873	1913.977251	5.592320	-0.023414	2.384828
118.928626	1922.079708	5.597325	-0.023452	2.389735
119.268033	1930.150332	5.602330	-0.023521	2.394626
119.427491	1938.248623	5.607334	-0.023556	2.399510
119.367454	1946.341167	5.612339	-0.023550	2.404362
120.415679	1954.315638	5.617344	-0.023751	2.409222
120.764398	1962.390305	5.622349	-0.023822	2.414076
120.774535	1970.515958	5.627354	-0.023829	2.418924
121.494570	1978.502871	5.632358	-0.023969	2.423737
121.601620	1986.630656	5.637363	-0.023994	2.428574
121.950943	1994.734866	5.642368	-0.024065	2.433407
122.055553	2002.803960	5.647373	-0.024090	2.438191
122.489827	2010.802406	5.652378	-0.024177	2.442949
122.654019	2018.891999	5.657382	-0.024213	2.447730
122.798228	2026.949705	5.662387	-0.024245	2.452482
123.384206	2034.985048	5.667392	-0.024360	2.457245
123.612452	2043.048603	5.672397	-0.024408	2.461988
123.611163	2051.167696	5.677402	-0.024413	2.466737
124.328510	2059.173736	5.682406	-0.024552	2.471466
124.856205	2067.206794	5.687411	-0.024656	2.476187
125.223220	2075.263959	5.692416	-0.024730	2.480900
125.426562	2083.320689	5.697421	-0.024774	2.485592
125.955333	2091.386680	5.702426	-0.024878	2.490305
126.308404	2099.471764	5.707430	-0.024949	2.495006
126.462128	2107.550650	5.712435	-0.024983	2.499680
127.023618	2115.580071	5.717440	-0.025093	2.504348
127.288427	2123.661464	5.722445	-0.025148	2.509014
127.317714	2131.772284	5.727450	-0.025159	2.513671
127.505450	2139.845474	5.732454	-0.025200	2.518309
127.976996	2147.839058	5.737459	-0.025293	2.522915
128.578573	2155.852397	5.742464	-0.025411	2.527533
128.643839	2163.957306	5.747469	-0.025429	2.532155
128.827192	2172.043744	5.752474	-0.025468	2.536766
129.042905	2180.095445	5.757478	-0.025514	2.541352
129.212388	2188.136328	5.762483	-0.025551	2.545920
129.523554	2196.229149	5.767488	-0.025615	2.550520
129.706414	2204.273210	5.772493	-0.025654	2.555074
129.918702	2212.330206	5.777498	-0.025700	2.559630
130.309043	2220.339553	5.782502	-0.025778	2.564163
130.731314	2228.384303	5.787507	-0.025862	2.568711
130.910350	2236.491783	5.792512	-0.025901	2.573268
131.183844	2244.531958	5.797517	-0.025958	2.577786
131.938041	2252.514868	5.802522	-0.026103	2.582298
132.470932	2260.575526	5.807526	-0.026208	2.586830
132.359171	2268.760172	5.812531	-0.026193	2.591378
132.809800	2276.850234	5.817536	-0.026283	2.595904
133.369187	2284.806917	5.822541	-0.026392	2.600356
133.498717	2292.851955	5.827546	-0.026422	2.604820
134.028636	2300.855806	5.832550	-0.026526	2.609280
133.811795	2309.002691	5.837555	-0.026492	2.613761
133.823257	2317.079265	5.842560	-0.026499	2.618210
134.227069	2325.072264	5.847565	-0.026580	2.622633
134.350789	2333.141564	5.852570	-0.026609	2.627072
134.354095	2341.243016	5.857574	-0.026615	2.631512
134.614723	2349.261333	5.862579	-0.026669	2.635916
135.022797	2357.290364	5.867584	-0.026751	2.640329
135.574414	2365.281188	5.872589	-0.026859	2.644724
135.820627	2373.353872	5.877594	-0.026910	2.649135
136.042998	2381.430467	5.882598	-0.026957	2.653539
136.922528	2389.364655	5.887603	-0.027127	2.657903
137.087810	2397.483487	5.892608	-0.027163	2.662311
137.396734	2405.520785	5.897613	-0.027226	2.666678
137.672039	2413.601046	5.902618	-0.027283	2.671059
137.903155	2421.675234	5.907622	-0.027332	2.675426
137.949299	2429.715725	5.912627	-0.027346	2.679755
138.185735	2437.763445	5.917632	-0.027395	2.684094
138.115666	2445.855332	5.922637	-0.027388	2.688430
138.264712	2453.919550	5.927642	-0.027421	2.692758
138.737668	2461.929383	5.932646	-0.027515	2.697071
139.031921	2469.947685	5.937651	-0.027575	2.701370
138.678921	2478.100226	5.942656	-0.027515	2.705692
138.920510	2486.127851	5.947661	-0.027566	2.709979
139.554804	2494.101464	5.952666	-0.027689	2.714255
139.934586	2502.141128	5.957670	-0.027766	2.718543
140.035564	2510.173611	5.962675	-0.027790	2.722803
140.180123	2518.277326	5.967680	-0.027823	2.727097
140.255915	2526.350075	5.972685	-0.027842	2.731363
140.633793	2534.376163	5.977690	-0.027918	2.735617
141.181421	2542.383965	5.982694	-0.028026	2.739866
141.277513	2550.412689	5.987699	-0.028049	2.744090
141.682753	2558.484270	5.992704	-0.028130	2.748350
141.533864	2566.625669	5.997709	-0.028108	2.752605
141.696387	2574.664293	6.002714	-0.028144	2.756819
142.717276	2582.563154	6.007718	-0.028340	2.761007
142.466252	2590.670893	6.012723	-0.028298	2.765218
142.910109	2598.678625	6.017728	-0.028387	2.769414
143.282067	2606.745730	6.022733	-0.028462	2.773630
143.569609	2614.780502	6.027738	-0.028521	2.777818
143.782193	2622.838807	6.032742	-0.028566	2.782007
144.117689	2630.866559	6.037747	-0.028634	2.786181
144.545147	2638.907854	6.042752	-0.028719	2.790361
144.425887	2646.997041	6.047757	-0.028702	2.794527
144.845969	2655.012110	6.052762	-0.028786	2.798681
145.189766	2663.040950	6.057766	-0.028856	2.802831
144.864984	2671.166520	6.062771	-0.028801	2.806984
145.391558	2679.182943	6.067776	-0.028905	2.811126
145.987495	2687.172318	6.072781	-0.029021	2.815253
145.827713	2695.282184	6.077786	-0.028997	2.819390
146.166967	2703.295304	6.082790	-0.029066	2.823501
146.647776	2711.303327	6.087795	-0.029161	2.827612
146.927282	2719.403592	6.092800	-0.029218	2.831751
146.960673	2727.442192	6.097805	-0.029230	2.835839
147.349075	2735.433124	6.102810	-0.029308	2.839918
147.527012	2743.487672	6.107814	-0.029347	2.844010
147.780508	2751.511316	6.112819	-0.029400	2.848086
147.844081	2759.609754	6.117824	-0.029417	2.852182
148.181003	2767.623030	6.122829	-0.029485	2.856246
148.617973	2775.633403	6.127834	-0.029572	2.860307
148.927042	2783.659417	6.132838	-0.029635	2.864364
148.888371	2791.770080	6.137843	-0.029634	2.868437
149.630661	2799.771910	6.142848	-0.029778	2.872494
149.406690	2807.904874	6.147853	-0.029741	2.876557
149.680392	2815.919277	6.152858	-0.029798	2.880582
150.088939	2823.895439	6.157862	-0.029880	2.884591
150.374471	2831.924338	6.162867	-0.029938	2.888613
150.452486	2840.028063	6.167872	-0.029959	2.892655
150.687140	2848.064679	6.172877	-0.030008	2.896666
151.003098	2856.090885	6.177882	-0.030072	2.900672
150.929368	2864.177003	6.182886	-0.030064	2.904680
151.030924	2872.213065	6.187891	-0.030089	2.908667
151.350887	2880.311006	6.192896	-0.030154	2.912692
151.514157	2888.327120	6.197901	-0.030190	2.916662
151.424936	2896.367110	6.202906	-0.030179	2.920624
152.114604	2904.320816	6.207910	-0.030313	2.924582
152.239188	2912.367918	6.212915	-0.030341	2.928548
152.521271	2920.416865	6.217920	-0.030400	2.932519
152.500160	2928.488051	6.222925	-0.030401	2.936479
152.846251	2936.501642	6.227930	-0.030471	2.940425
153.306517	2944.484279	6.232934	-0.030562	2.944357
153.179148	2952.577482	6.237939	-0.030544	2.948306
153.482473	2960.634937	6.242944	-0.030606	2.952256
153.479268	2968.680473	6.247949	-0.030611	2.956177
153.836293	2976.657593	6.252954	-0.030683	2.960080
153.799444	2984.726909	6.257958	-0.030682	2.964001
154.199246	2992.742678	6.262963	-0.030762	2.967914
154.344957	3000.809077	6.267968	-0.030795	2.971833
154.456129	3008.878340	6.272973	-0.030821	2.975747
154.241494	3016.948966	6.277978	-0.030787	2.979639
154.589041	3024.946692	6.282982	-0.030857	2.983520
154.938261	3032.930879	6.287987	-0.030928	2.987389
155.426932	3040.975460	6.292992	-0.031024	2.991290
155.547838	3049.055371	6.297997	-0.031052	2.995183
155.785930	3057.045527	6.303002	-0.031102	2.999034
156.058699	3065.105528	6.308006	-0.031159	3.002916
156.444062	3073.085204	6.313011	-0.031236	3.006760
156.506968	3081.171692	6.318016	-0.031253	3.010633
156.561029	3089.232977	6.323021	-0.031269	3.014489
156.814171	3097.249443	6.328026	-0.031322	3.018329
156.944345	3105.308955	6.333030	-0.031351	3.022178
156.963280	3113.319733	6.338035	-0.031360	3.025994
157.342471	3121.374843	6.343040	-0.031437	3.029843
157.523167	3129.404768	6.348045	-0.031476	3.033666
157.808021	3137.399057	6.353050	-0.031534	3.037473
157.999938	3145.475279	6.358054	-0.031576	3.041308
157.718693	3153.568508	6.363059	-0.031529	3.045124
158.045380	3161.582995	6.368064	-0.031595	3.048927
157.782364	3169.685164	6.373069	-0.031552	3.052738
158.617742	3177.588016	6.378074	-0.031713	3.056505
158.821408	3185.675634	6.383078	-0.031757	3.060322
159.075452	3193.632694	6.388083	-0.031809	3.064076
159.315936	3201.721461	6.393088	-0.031860	3.067886
159.895642	3209.760000	6.398093	-0.031973	3.071685
159.629838	3217.891473	6.403098	-0.031930	3.075481
159.903819	3225.867040	6.408102	-0.031986	3.079226
159.853293	3233.903242	6.413107	-0.031982	3.082979
160.249069	3241.898019	6.418112	-0.032061	3.086730
160.505296	3249.897605	6.423117	-0.032115	3.090471
160.544712	3257.988926	6.428122	-0.032128	3.094240
161.029692	3265.991563	6.433126	-0.032224	3.097985
161.052092	3274.023047	6.438131	-0.032233	3.101716
161.357840	3282.058288	6.443136	-0.032296	3.105458
161.374388	3290.118595	6.448141	-0.032304	3.109194
161.534341	3298.157877	6.453146	-0.032340	3.112922
162.052568	3306.163885	6.458150	-0.032442	3.116647
161.910891	3314.213215	6.463155	-0.032421	3.120356
162.231148	3322.208573	6.468160	-0.032486	3.124058
162.287979	3330.264498	6.473165	-0.032502	3.127771
162.421572	3338.350169	6.478170	-0.032533	3.131497
163.112049	3346.312246	6.483174	-0.032667	3.135187
163.237864	3354.352096	6.488179	-0.032696	3.138882
163.143972	3362.446591	6.493184	-0.032684	3.142589
163.359187	3370.467958	6.498189	-0.032730	3.146271
163.595089	3378.496101	6.503194	-0.032779	3.149953
163.988014	3386.512031	6.508198	-0.032858	3.153632
164.317920	3394.497893	6.513203	-0.032925	3.157291
164.749993	3402.533823	6.518208	-0.033011	3.160972
164.923371	3410.517701	6.523213	-0.033049	3.164614
165.058408	3418.598472	6.528218	-0.033080	3.168294
165.281950	3426.666261	6.533222	-0.033127	3.171968
164.956305	3434.757422	6.538227	-0.033072	3.175623
165.185345	3442.766244	6.543232	-0.033120	3.179262
165.558009	3450.762745	6.548237	-0.033195	3.182897
165.472021	3458.836779	6.553242	-0.033185	3.186543
165.626618	3466.905619	6.558246	-0.033219	3.190193
166.162629	3474.853253	6.563251	-0.033324	3.193801
166.631874	3482.867932	6.568256	-0.033417	3.197431
166.218625	3490.999497	6.573261	-0.033346	3.201072
166.626847	3498.948963	6.578266	-0.033427	3.204663
166.943571	3507.006822	6.583270	-0.033492	3.208294
167.357555	3515.005418	6.588275	-0.033575	3.211899
167.396564	3523.093110	6.593280	-0.033587	3.215523
167.957261	3531.053451	6.598285	-0.033697	3.219109
167.892579	3539.118330	6.603290	-0.033691	3.222710
167.827062	3547.241969	6.608294	-0.033684	3.226334
168.136848	3555.205215	6.613299	-0.033748	3.229898
168.252428	3563.257569	6.618304	-0.033775	3.233490
168.500391	3571.256550	6.623309	-0.033826	3.237059
168.660514	3579.284744	6.628314	-0.033862	3.240634
168.764781	3587.298309	6.633318	-0.033887	3.244196
168.964840	3595.323696	6.638323	-0.033930	3.247763
169.059967	3603.392555	6.643328	-0.033953	3.251341
169.599833	3611.379947	6.648333	-0.034059	3.254898
169.632254	3619.418879	6.653338	-0.034071	3.258452
170.057135	3627.432800	6.658342	-0.034155	3.262008
169.779485	3635.516887	6.663347	-0.034109	3.265561
170.203507	3643.525268	6.668352	-0.034194	3.269107
170.461847	3651.553672	6.673357	-0.034247	3.272650
170.908461	3659.548608	6.678362	-0.034336	3.276183
171.117312	3667.599266	6.683366	-0.034381	3.279726
170.655986	3675.675662	6.688371	-0.034300	3.283250
171.426531	3683.640052	6.693376	-0.034449	3.286771
171.894538	3691.630436	6.698381	-0.034542	3.290287
171.849514	3699.730189	6.703386	-0.034539	3.293826
172.200444	3707.753091	6.708390	-0.034610	3.297344
172.637751	3715.761109	6.713395	-0.034697	3.300855
172.644297	3723.819951	6.718400	-0.034704	3.304367
172.609231	3731.911249	6.723405	-0.034703	3.307888
172.537748	3739.954122	6.728410	-0.034695	3.311383
173.101274	3747.918551	6.733414	-0.034806	3.314865
173.259421	3755.927500	6.738419	-0.034841	3.318347
173.630334	3763.937313	6.743424	-0.034915	3.321833
173.471500	3772.011988	6.748429	-0.034891	3.325324
174.064283	3779.967027	6.753434	-0.035007	3.328788
174.594352	3788.021558	6.758438	-0.035112	3.332289
174.647491	3796.073128	6.763443	-0.035127	3.335767
174.929255	3804.093209	6.768448	-0.035185	3.339236
175.132959	3812.128713	6.773453	-0.035229	3.342705
175.166437	3820.191397	6.778458	-0.035240	3.346176
175.115997	3828.259002	6.783462	-0.035237	3.349642
175.442591	3836.228914	6.788467	-0.035303	3.353076
175.750540	3844.264146	6.793472	-0.035366	3.356535
176.078596	3852.247011	6.798477	-0.035432	3.359968
175.939342	3860.314949	6.803482	-0.035412	3.363417
176.060685	3868.401170	6.808486	-0.035440	3.366879
175.679711	3876.462142	6.813491	-0.035375	3.370309
175.966284	3884.485430	6.818496	-0.035434	3.373744
176.462485	3892.440934	6.823501	-0.035532	3.377154
176.643829	3900.457704	6.828506	-0.035571	3.380575
176.908096	3908.480652	6.833510	-0.035626	3.383998
176.895292	3916.543867	6.838515	-0.035629	3.387425
177.323395	3924.576527	6.843520	-0.035714	3.390851
177.392716	3932.641737	6.848525	-0.035733	3.394275
177.743609	3940.581884	6.853530	-0.035804	3.397652
177.651253	3948.694213	6.858534	-0.035792	3.401083
178.166818	3956.584785	6.863539	-0.035894	3.404439
178.489371	3964.665453	6.868544	-0.035959	3.407864
178.188864	3972.790341	6.873549	-0.035909	3.411282
178.161031	3980.787514	6.878554	-0.035909	3.414653
178.831733	3988.748320	6.883558	-0.036040	3.418030
178.768861	3996.834915	6.888563	-0.036034	3.421431
179.063480	4004.812491	6.893568	-0.036094	3.424795
178.986238	4012.902935	6.898573	-0.036085	3.428190
179.123394	4020.920858	6.903578	-0.036116	3.431558
179.258060	4028.961846	6.908582	-0.036147	3.434933
179.358663	4036.929357	6.913587	-0.036171	3.438273
179.838534	4044.928358	6.918592	-0.036266	3.441635
180.216255	4052.950626	6.923597	-0.036342	3.445001
180.459402	4060.993571	6.928602	-0.036393	3.448367
180.483355	4069.097814	6.933606	-0.036403	3.451748
180.779381	4077.081133	6.938611	-0.036464	3.455084
181.086279	4085.094684	6.943616	-0.036526	3.458431
181.093006	4093.154302	6.948621	-0.036533	3.461782
181.148994	4101.170342	6.953626	-0.036549	3.465115
181.758444	4109.179783	6.958630	-0.036668	3.468459
181.350922	4117.273334	6.963635	-0.036598	3.471802
181.748965	4125.226828	6.968640	-0.036678	3.475110
182.168970	4133.245185	6.973645	-0.036762	3.478442
182.277072	4141.259647	6.978650	-0.036787	3.481759
182.494327	4149.304764	6.983654	-0.036833	3.485089
182.385089	4157.371102	6.988659	-0.036818	3.488414
182.514045	4165.419144	6.993664	-0.036848	3.491736
182.625278	4173.463446	6.998669	-0.036874	3.495053
183.127652	4181.350583	7.003674	-0.036973	3.498315
183.535400	4189.446623	7.008678	-0.037055	3.501657
183.420212	4197.472777	7.013683	-0.037039	3.504949
184.036657	4205.455998	7.018688	-0.037159	3.508245
184.242231	4213.545071	7.023693	-0.037203	3.511567
184.136362	4221.573442	7.028698	-0.037189	3.514851
184.418432	4229.614612	7.033702	-0.037247	3.518150
184.557198	4237.610537	7.038707	-0.037279	3.521423
184.853890	4245.628367	7.043712	-0.037339	3.524707
184.789445	4253.696595	7.048717	-0.037333	3.527997
184.794434	4261.758488	7.053722	-0.037340	3.531283
184.774627	4269.809120	7.058726	-0.037341	3.534561
184.993278	4277.769647	7.063731	-0.037388	3.537806
185.599566	4285.758309	7.068736	-0.037506	3.541073
185.671456	4293.748200	7.073741	-0.037525	3.544319
185.822407	4301.837144	7.078746	-0.037559	3.547606
186.048065	4309.884005	7.083750	-0.037606	3.550875
186.372755	4317.885300	7.088755	-0.037672	3.554125
186.721357	4325.903828	7.093760	-0.037743	3.557380
186.752196	4333.941726	7.098765	-0.037754	3.560630
187.177466	4341.863417	7.103770	-0.037839	3.563842
186.898421	4350.023919	7.108774	-0.037793	3.567126
186.922792	4358.038696	7.113779	-0.037803	3.570358
187.447024	4365.975733	7.118784	-0.037906	3.573570
187.576736	4374.039892	7.123789	-0.037936	3.576819
187.940583	4381.999088	7.128794	-0.038009	3.580030
188.271687	4390.031822	7.133798	-0.038076	3.583266
188.339362	4398.095539	7.138803	-0.038094	3.586504
188.483513	4406.121153	7.143808	-0.038127	3.589726
188.249268	4414.221925	7.148813	-0.038089	3.592964
188.410746	4422.210834	7.153818	-0.038124	3.596166
188.838508	4430.195082	7.158822	-0.038209	3.599371
188.653327	4438.241200	7.163827	-0.038181	3.602579
189.249132	4446.230755	7.168832	-0.038297	3.605786
189.326231	4454.274338	7.173837	-0.038317	3.608995
189.299495	4462.358587	7.178842	-0.038318	3.612215
188.931032	4470.463977	7.183846	-0.038255	3.615431
189.307658	4478.395010	7.188851	-0.038330	3.618596
189.444013	4486.413476	7.193856	-0.038361	3.621786
189.900716	4494.396241	7.198861	-0.038452	3.624969
189.679256	4502.500515	7.203866	-0.038416	3.628177
189.794599	4510.575817	7.208870	-0.038443	3.631380
189.909597	4518.510031	7.213875	-0.038470	3.634525
190.149122	4526.502269	7.218880	-0.038520	3.637694
190.688987	4534.493594	7.223885	-0.038626	3.640867
191.046122	4542.439500	7.228890	-0.038698	3.644015
190.993183	4550.599663	7.233894	-0.038694	3.647233
190.999369	4558.626554	7.238899	-0.038701	3.650398
191.329144	4566.627272	7.243904	-0.038768	3.653558
191.338793	4574.705229	7.248909	-0.038775	3.656737
191.560033	4582.678460	7.253914	-0.038822	3.659878
192.017938	4590.677066	7.258918	-0.038913	3.663033
191.889712	4598.749157	7.263923	-0.038895	3.666198
192.074209	4606.778531	7.268928	-0.038934	3.669352
192.263567	4614.807392	7.273933	-0.038975	3.672503
192.150524	4622.864172	7.278938	-0.038960	3.675654
192.446360	4630.830930	7.283942	-0.039020	3.678778
192.795436	4638.811324	7.288947	-0.039091	3.681906
192.750737	4646.870489	7.293952	-0.039088	3.685052
192.702339	4654.938383	7.298957	-0.039085	3.688198
192.521435	4663.019791	7.303962	-0.039057	3.691344
193.206584	4670.940022	7.308966	-0.039190	3.694447
193.502426	4678.920127	7.313971	-0.039250	3.697560
193.758823	4686.957161	7.318976	-0.039304	3.700692
194.372035	4694.913539	7.323981	-0.039423	3.703799
194.452224	4703.028607	7.328986	-0.039444	3.706951
194.286831	4711.117166	7.333990	-0.039419	3.710083
194.589887	4719.150537	7.338995	-0.039481	3.713204
194.833435	4727.183484	7.344000	-0.039532	3.716321
194.850682	4735.164055	7.349005	-0.039541	3.719408
195.083402	4743.169311	7.354010	-0.039589	3.722508
195.223942	4751.212516	7.359014	-0.039621	3.725618
194.999937	4759.216927	7.364019	-0.039585	3.728701
195.739640	4767.179126	7.369024	-0.039728	3.731790
195.940696	4775.256518	7.374029	-0.039771	3.734906
195.597782	4783.326788	7.379034	-0.039713	3.738004
195.737187	4791.372196	7.384038	-0.039745	3.741102
195.893142	4799.303786	7.389043	-0.039779	3.744154
196.431036	4807.319694	7.394048	-0.039885	3.747245
196.445647	4815.409622	7.399053	-0.039893	3.750349
196.452821	4823.416299	7.404058	-0.039900	3.753418
197.166072	4831.406262	7.409062	-0.040038	3.756495
197.461246	4839.344958	7.414067	-0.040099	3.759541
197.555762	4847.419831	7.419072	-0.040122	3.762630
197.791257	4855.493248	7.424077	-0.040172	3.765721
197.854269	4863.474701	7.429082	-0.040189	3.768769
198.063016	4871.540244	7.434086	-0.040233	3.771850
198.102860	4879.554279	7.439091	-0.040246	3.774906
198.405531	4887.566532	7.444096	-0.040308	3.777964
198.505623	4895.612874	7.449101	-0.040332	3.781028
198.293708	4903.594896	7.454106	-0.040299	3.784057
198.635892	4911.680312	7.459110	-0.040368	3.787137
198.423468	4919.732802	7.464115	-0.040334	3.790188
198.654202	4927.699243	7.469120	-0.040382	3.793215
198.828586	4935.754750	7.474125	-0.040420	3.796272
198.832420	4943.697809	7.479130	-0.040427	3.799280
198.718128	4951.804648	7.484134	-0.040411	3.802344
199.224764	4959.701629	7.489139	-0.040511	3.805341
200.094991	4967.670585	7.494144	-0.040678	3.808372
200.042999	4975.814752	7.499149	-0.040674	3.811444
199.943932	4983.808484	7.504154	-0.040661	3.814457
200.119236	4991.900543	7.509158	-0.040700	3.817510
200.426592	4999.884229	7.514163	-0.040762	3.820523
200.283106	5007.903842	7.519168	-0.040741	3.823537
199.988916	5016.039250	7.524173	-0.040692	3.826589
200.114362	5023.974811	7.529178	-0.040721	3.829572
200.471794	5032.030182	7.534182	-0.040793	3.832604
200.599007	5040.007432	7.539187	-0.040822	3.835599
200.718540	5048.023101	7.544192	-0.040850	3.838605
201.040294	5056.084958	7.549197	-0.040916	3.841631
201.023146	5064.042092	7.554202	-0.040918	3.844608
201.153518	5072.089520	7.559206	-0.040948	3.847619
201.318114	5080.142164	7.564211	-0.040984	3.850631
201.334484	5088.178820	7.569216	-0.040993	3.853631
201.248890	5096.222617	7.574221	-0.040982	3.856630
201.878366	5104.120882	7.579226	-0.041105	3.859587
202.103275	5112.187065	7.584230	-0.041153	3.862595
201.634202	5120.279998	7.589235	-0.041071	3.865597
202.379291	5128.200676	7.594240	-0.041215	3.868558
202.476855	5136.347764	7.599245	-0.041239	3.871587
202.586079	5144.412288	7.604250	-0.041265	3.874583
202.638470	5152.434111	7.609254	-0.041280	3.877560
202.890025	5160.364998	7.614259	-0.041333	3.880505
203.051765	5168.320544	7.619264	-0.041368	3.883455
203.481338	5176.371074	7.624269	-0.041454	3.886443
203.301423	5184.372355	7.629274	-0.041426	3.889398
203.532606	5192.449848	7.634278	-0.041474	3.892388
203.698414	5200.433231	7.639283	-0.041511	3.895339
203.809989	5208.417265	7.644288	-0.041537	3.898287
204.409492	5216.428094	7.649293	-0.041654	3.901253
204.359324	5224.425662	7.654298	-0.041651	3.904198
204.358977	5232.530052	7.659302	-0.041656	3.907182
204.708090	5240.522353	7.664307	-0.041727	3.910129
205.145688	5248.488018	7.669312	-0.041814	3.913065
205.192838	5256.577826	7.674317	-0.041828	3.916037
205.548288	5264.510896	7.679322	-0.041900	3.918956
205.990800	5272.577393	7.684326	-0.041988	3.921923
205.554598	5280.612613	7.689331	-0.041912	3.924858
205.535921	5288.662222	7.694336	-0.041914	3.927806
206.108616	5296.660153	7.699341	-0.042026	3.930743
206.265471	5304.634116	7.704346	-0.042061	3.933662
206.860416	5312.674863	7.709350	-0.042178	3.936611
206.484345	5320.768390	7.714355	-0.042113	3.939558
207.013627	5328.752178	7.719360	-0.042217	3.942481
206.797000	5336.830523	7.724365	-0.042182	3.945421
206.748404	5344.812665	7.729370	-0.042179	3.948328
207.113803	5352.912354	7.734374	-0.042253	3.951283
206.686885	5360.944714	7.739379	-0.042179	3.954196
206.946107	5368.908224	7.744384	-0.042233	3.957095
207.112447	5376.911660	7.749389	-0.042269	3.960005
207.222206	5384.898113	7.754394	-0.042295	3.962905
207.220319	5392.993434	7.759398	-0.042300	3.965841
207.212497	5400.965778	7.764403	-0.042304	3.968730
207.905987	5408.935506	7.769408	-0.042439	3.971628
207.923648	5416.984820	7.774413	-0.042448	3.974541
208.070812	5425.010290	7.779418	-0.042481	3.977445
208.215801	5433.043533	7.784422	-0.042513	3.980351
208.728274	5440.994504	7.789427	-0.042614	3.983230
208.769896	5449.054249	7.794432	-0.042628	3.986139
209.014988	5457.072690	7.799437	-0.042679	3.989034
209.784048	5465.053305	7.804442	-0.042828	3.991922
209.674390	5473.131310	7.809446	-0.042813	3.994828
209.503598	5481.175573	7.814451	-0.042787	3.997719
209.555442	5489.196619	7.819456	-0.042802	4.000603
209.714543	5497.217465	7.824461	-0.042837	4.003487
209.316538	5505.275153	7.829466	-0.042769	4.006372
209.944140	5513.214775	7.834470	-0.042891	4.009231
209.844066	5521.286335	7.839475	-0.042878	4.012122
209.786570	5529.304120	7.844480	-0.042873	4.014993
210.197297	5537.289899	7.849485	-0.042955	4.017858
210.070975	5545.360855	7.854490	-0.042937	4.020742
210.228974	5553.359632	7.859494	-0.042972	4.023603
210.153163	5561.438003	7.864499	-0.042963	4.026487
210.466494	5569.376373	7.869504	-0.043027	4.029325
210.505251	5577.483756	7.874509	-0.043040	4.032217
210.450820	5585.471552	7.879514	-0.043035	4.035063
211.117712	5593.405721	7.884518	-0.043165	4.037899
211.762815	5601.359913	7.889523	-0.043291	4.040740
211.772017	5609.378634	7.894528	-0.043298	4.043592
212.037659	5617.483751	7.899533	-0.043353	4.046476
212.010333	5625.467198	7.904538	-0.043354	4.049311
211.941638	5633.585704	7.909542	-0.043346	4.052191
212.687855	5641.498433	7.914547	-0.043491	4.055008
212.888345	5649.520486	7.919552	-0.043534	4.057854
212.806585	5657.621571	7.924557	-0.043524	4.060721
212.426505	5665.647897	7.929562	-0.043459	4.063555
212.477559	5673.707638	7.934566	-0.043474	4.066406
212.903913	5681.622383	7.939571	-0.043559	4.069209
212.638844	5689.746089	7.944576	-0.043515	4.072074
213.230838	5697.694170	7.949581	-0.043631	4.074887
213.366746	5705.702127	7.954586	-0.043662	4.077713
213.472525	5713.748015	7.959590	-0.043687	4.080550
213.842054	5721.670364	7.964595	-0.043761	4.083345
214.134292	5729.707199	7.969600	-0.043821	4.086177
214.101180	5737.801651	7.974605	-0.043821	4.089023
214.123392	5745.800755	7.979610	-0.043830	4.091834
214.666487	5753.820086	7.984614	-0.043937	4.094658
214.428041	5761.919514	7.989619	-0.043898	4.097496
214.947850	5769.832769	7.994624	-0.044001	4.100279
215.117071	5777.873908	7.999629	-0.044038	4.103099
215.390999	5785.917257	8.004634	-0.044094	4.105919
214.903257	5794.029465	8.009638	-0.044009	4.108751
215.030744	5802.040818	8.014643	-0.044038	4.111554
215.392552	5809.991032	8.019648	-0.044111	4.114337
215.672115	5818.003756	8.024653	-0.044169	4.117139
215.598933	5825.989642	8.029658	-0.044161	4.119925
215.967300	5833.997357	8.034662	-0.044235	4.122723
216.160438	5842.023891	8.039667	-0.044277	4.125522
216.180946	5850.045734	8.044672	-0.044286	4.128316
216.227843	5858.155452	8.049677	-0.044300	4.131139
216.766555	5866.042302	8.054682	-0.044406	4.133889
216.651525	5874.128077	8.059686	-0.044390	4.136698
216.810647	5882.105296	8.064691	-0.044425	4.139471
216.961455	5890.160246	8.069696	-0.044459	4.142268
217.512517	5898.141462	8.074701	-0.044567	4.145044
217.387440	5906.178336	8.079706	-0.044550	4.147828
217.935637	5914.192359	8.084710	-0.044657	4.150611
217.931857	5922.244525	8.089715	-0.044662	4.153398
217.703365	5930.329492	8.094720	-0.044625	4.156191
218.128302	5938.252689	8.099725	-0.044710	4.158935
218.074950	5946.313868	8.104730	-0.044705	4.161719
218.815137	5954.205486	8.109734	-0.044849	4.164453
218.659584	5962.312023	8.114739	-0.044825	4.167247
218.587016	5970.369277	8.119744	-0.044817	4.170024
219.094935	5978.356403	8.124749	-0.044918	4.172782
219.413142	5986.338650	8.129754	-0.044982	4.175534
220.007103	5994.323657	8.134758	-0.045098	4.178289
219.923016	6002.461044	8.139763	-0.045088	4.181085
219.996606	6010.384643	8.144768	-0.045108	4.183809
219.881257	6018.553877	8.149773	-0.045092	4.186612
220.346827	6026.469664	8.154778	-0.045184	4.189334
220.478332	6034.582809	8.159782	-0.045214	4.192118
220.778724	6042.527843	8.164787	-0.045276	4.194844
220.934378	6050.537899	8.169792	-0.045310	4.197589
221.093621	6058.607902	8.174797	-0.045345	4.200352
221.111507	6066.563018	8.179802	-0.045354	4.203073
221.149754	6074.606679	8.184806	-0.045367	4.205823
220.755626	6082.679381	8.189811	-0.045299	4.208575
221.553909	6090.611936	8.194816	-0.045453	4.211292
221.272827	6098.699528	8.199821	-0.045407	4.214047
221.311135	6106.733145	8.204826	-0.045419	4.216786
221.906408	6114.642694	8.209830	-0.045536	4.219488
221.684086	6122.761445	8.214835	-0.045500	4.222249
221.932493	6130.715853	8.219840	-0.045552	4.224958
222.471688	6138.719324	8.224845	-0.045658	4.227685
221.974561	6146.780896	8.229850	-0.045571	4.230419
222.235825	6154.812153	8.234854	-0.045625	4.233148
222.646037	6162.825560	8.239859	-0.045707	4.235872
222.470467	6170.775350	8.244864	-0.045680	4.238566
222.734627	6178.884943	8.249869	-0.045734	4.241317
223.253393	6186.774336	8.254874	-0.045837	4.243995
223.073889	6194.889930	8.259878	-0.045809	4.246739
222.796203	6202.920485	8.264883	-0.045763	4.249453
223.337799	6210.911533	8.269888	-0.045869	4.252160
223.290859	6218.982236	8.274893	-0.045866	4.254885
223.767793	6226.907173	8.279898	-0.045960	4.257566
223.503037	6235.001255	8.284902	-0.045916	4.260294
223.732306	6242.981912	8.289907	-0.045965	4.262987
223.747222	6251.022281	8.294912	-0.045973	4.265696
224.247350	6258.982043	8.299917	-0.046072	4.268381
224.642750	6266.998358	8.304922	-0.046151	4.271083
224.907325	6275.011656	8.309926	-0.046206	4.273780
225.049682	6283.070837	8.314931	-0.046238	4.276490
225.268505	6291.012119	8.319936	-0.046284	4.279159
225.642453	6299.124301	8.324941	-0.046359	4.281886
225.204430	6307.111203	8.329946	-0.046283	4.284561
225.412540	6315.149023	8.334950	-0.046328	4.287257
225.464924	6323.165586	8.339955	-0.046343	4.289943
225.800191	6331.161629	8.344960	-0.046411	4.292624
226.322681	6339.192190	8.349965	-0.046514	4.295315
226.300610	6347.148580	8.354970	-0.046515	4.297976
226.315462	6355.259357	8.359974	-0.046524	4.300686
225.658039	6363.302692	8.364979	-0.046407	4.303366
226.040634	6371.272401	8.369984	-0.046484	4.306030
225.932243	6379.377299	8.374989	-0.046469	4.308732
226.392936	6387.309212	8.379994	-0.046560	4.311380
226.939756	6395.252377	8.384998	-0.046668	4.314031
226.837991	6403.320708	8.390003	-0.046654	4.316716
226.942936	6411.297647	8.395008	-0.046679	4.319371
227.405545	6419.325797	8.400013	-0.046771	4.322045
227.289364	6427.328715	8.405018	-0.046755	4.324703
227.391309	6435.377095	8.410022	-0.046780	4.327377
227.838361	6443.396458	8.415027	-0.046868	4.330042
228.055423	6451.384293	8.420032	-0.046914	4.332693
228.666674	6459.399437	8.425037	-0.047034	4.335355
228.647233	6467.450263	8.430042	-0.047036	4.338022
229.062127	6475.428537	8.435046	-0.047118	4.340666
228.969103	6483.492029	8.440051	-0.047107	4.343334
229.226574	6491.476528	8.445056	-0.047160	4.345976
229.542687	6499.503357	8.450061	-0.047225	4.348631
229.484881	6507.557243	8.455066	-0.047219	4.351290
229.497136	6515.654151	8.460070	-0.047227	4.353962
229.649715	6523.681799	8.465075	-0.047261	4.356611
229.706998	6531.541317	8.470080	-0.047277	4.359203
229.799953	6539.657836	8.475085	-0.047300	4.361877
229.923216	6547.558640	8.480090	-0.047329	4.364480
229.784247	6555.687411	8.485094	-0.047309	4.367153
230.154110	6563.649368	8.490099	-0.047383	4.369774
230.396049	6571.670380	8.495104	-0.047434	4.372412
230.653415	6579.715024	8.500109	-0.047487	4.375056
230.902720	6587.667774	8.505114	-0.047539	4.377668
230.788687	6595.753083	8.510118	-0.047523	4.380320
231.265923	6603.636433	8.515123	-0.047618	4.382908
231.340005	6611.711320	8.520128	-0.047637	4.385554
231.391949	6619.793490	8.525133	-0.047652	4.388201
231.414828	6627.819137	8.530138	-0.047662	4.390827
231.312269	6635.859799	8.535142	-0.047649	4.393456
231.896508	6643.800630	8.540147	-0.047763	4.396056
232.301379	6651.768148	8.545152	-0.047844	4.398661
232.446099	6659.900675	8.550157	-0.047877	4.401317
232.837457	6667.731839	8.555162	-0.047955	4.403874
232.943909	6675.892172	8.560167	-0.047980	4.406536
233.117847	6683.865486	8.565171	-0.048018	4.409135
233.513817	6691.920874	8.570176	-0.048098	4.411761
233.391861	6699.979448	8.575181	-0.048080	4.414383
233.530294	6707.999529	8.580186	-0.048112	4.416993
233.922491	6716.010140	8.585191	-0.048190	4.419599
233.646862	6724.104128	8.590195	-0.048145	4.422228
234.001023	6732.046257	8.595200	-0.048216	4.424809
234.098019	6740.153654	8.600205	-0.048240	4.427440
233.823787	6748.207949	8.605210	-0.048194	4.430051
234.471965	6756.137127	8.610215	-0.048321	4.432624
234.601968	6764.222789	8.615219	-0.048350	4.435244
234.639981	6772.183671	8.620224	-0.048363	4.437822
234.630028	6780.240741	8.625229	-0.048367	4.440429
234.756441	6788.184388	8.630234	-0.048396	4.442998
235.319979	6796.186377	8.635239	-0.048506	4.445587
235.361180	6804.231731	8.640243	-0.048519	4.448186
235.484094	6812.292111	8.645248	-0.048548	4.450789
235.011236	6820.403508	8.650253	-0.048466	4.453403
235.243643	6828.348617	8.655258	-0.048514	4.455966
235.273321	6836.340305	8.660263	-0.048525	4.458541
235.602122	6844.357273	8.665267	-0.048592	4.461125
235.910441	6852.297833	8.670272	-0.048655	4.463682
235.941845	6860.410306	8.675277	-0.048667	4.466292
235.841161	6868.386689	8.680282	-0.048653	4.468855
236.539957	6876.434749	8.685287	-0.048789	4.471444
236.294126	6884.391386	8.690291	-0.048749	4.473998
236.762834	6892.435807	8.695296	-0.048842	4.476582
236.591296	6900.446277	8.700301	-0.048815	4.479150
236.484533	6908.490597	8.705306	-0.048801	4.481729
237.122585	6916.430978	8.710311	-0.048925	4.484275
237.802506	6924.475062	8.715315	-0.049058	4.486854
237.930240	6932.490322	8.720320	-0.049087	4.489419
237.868374	6940.611308	8.725325	-0.049081	4.492016
237.694945	6948.578162	8.730330	-0.049054	4.494562
238.072201	6956.606100	8.735335	-0.049130	4.497128
237.977368	6964.625056	8.740339	-0.049118	4.499687
238.154216	6972.612943	8.745344	-0.049156	4.502237
238.774604	6980.577600	8.750349	-0.049277	4.504779
238.786461	6988.593374	8.755354	-0.049285	4.507334
239.280085	6996.622833	8.760359	-0.049383	4.509893
239.393722	7004.661386	8.765363	-0.049409	4.512453
239.056053	7012.681145	8.770368	-0.049352	4.515003
239.333930	7020.719164	8.775373	-0.049409	4.517560
239.125818	7028.692427	8.780378	-0.049376	4.520093
239.661313	7036.674977	8.785383	-0.049481	4.522630
239.287148	7044.755329	8.790387	-0.049417	4.525194
240.185516	7052.670603	8.795392	-0.049590	4.527708
240.382006	7060.802537	8.800397	-0.049632	4.530287
240.453558	7068.754168	8.805402	-0.049651	4.532807
240.513203	7076.807005	8.810407	-0.049668	4.535358
240.499957	7084.839444	8.815411	-0.049671	4.537901
240.947095	7092.789215	8.820416	-0.049760	4.540417
241.102583	7100.824248	8.825421	-0.049794	4.542958
240.846588	7108.847730	8.830426	-0.049752	4.545493
241.361147	7116.831347	8.835431	-0.049854	4.548016
241.153282	7124.966215	8.840435	-0.049821	4.550583
240.991194	7132.948820	8.845440	-0.049796	4.553101
241.342203	7140.998001	8.850445	-0.049867	4.555639
241.518784	7148.897607	8.855450	-0.049905	4.558129
241.449945	7156.989910	8.860455	-0.049898	4.560678
242.099641	7164.911681	8.865459	-0.050025	4.563173
242.421153	7172.922839	8.870464	-0.050090	4.565694
242.770118	7180.957236	8.875469	-0.050160	4.568221
243.127131	7188.975303	8.880474	-0.050233	4.570741
243.132526	7197.011244	8.885479	-0.050239	4.573265
243.086482	7205.057939	8.890483	-0.050236	4.575791
243.238584	7212.982392	8.895488	-0.050270	4.578277
243.923183	7221.097193	8.900493	-0.050403	4.580823
244.046495	7229.028780	8.905498	-0.050432	4.583309
244.052896	7237.128925	8.910503	-0.050438	4.585845
243.668060	7245.181863	8.915507	-0.050372	4.588366
243.918255	7253.156830	8.920512	-0.050424	4.590861
244.613859	7261.113970	8.925517	-0.050559	4.593350
244.737591	7269.142499	8.930522	-0.050588	4.595859
244.605844	7277.176692	8.935527	-0.050569	4.598368
244.570924	7285.263806	8.940531	-0.050568	4.600893
244.866202	7293.127698	8.945536	-0.050629	4.603347
244.588368	7301.275718	8.950541	-0.050583	4.605887
244.664428	7309.249364	8.955546	-0.050602	4.608372
245.343193	7317.279203	8.960551	-0.050734	4.610874
245.327738	7325.284077	8.965555	-0.050737	4.613366
245.746287	7333.280764	8.970560	-0.050820	4.615855
245.582396	7341.291842	8.975565	-0.050795	4.618346
245.679626	7349.347597	8.980570	-0.050819	4.620850
245.973106	7357.298640	8.985575	-0.050879	4.623320
246.190257	7365.365910	8.990579	-0.050925	4.625825
246.359702	7373.343159	8.995584	-0.050962	4.628300
246.719524	7381.464294	9.000589	-0.051035	4.630819
246.721306	7389.409380	9.005594	-0.051041	4.633282
247.052199	7397.427649	9.010599	-0.051108	4.635766
246.896217	7405.447127	9.015603	-0.051085	4.638249
246.933479	7413.472586	9.020608	-0.051097	4.640732
247.639822	7421.422767	9.025613	-0.051234	4.643191
247.118462	7429.529282	9.030618	-0.051143	4.645697
247.549503	7437.482476	9.035623	-0.051228	4.648154
248.052112	7445.511810	9.040627	-0.051328	4.650634
247.727491	7453.516690	9.045632	-0.051273	4.653104
247.779558	7461.623800	9.050637	-0.051288	4.655605
248.178193	7469.516470	9.055642	-0.051368	4.658038
248.168357	7477.577571	9.060647	-0.051371	4.660522
248.489955	7485.541673	9.065651	-0.051437	4.662975
248.745285	7493.561812	9.070656	-0.051490	4.665443
248.744099	7501.643992	9.075661	-0.051495	4.667930
248.682819	7509.672545	9.080666	-0.051490	4.670398
248.608457	7517.740882	9.085671	-0.051481	4.672878
248.851810	7525.762035	9.090675	-0.051532	4.675341
248.654232	7533.697358	9.095680	-0.051501	4.677778
249.382217	7541.699348	9.100685	-0.051642	4.680232
249.371253	7549.686134	9.105690	-0.051646	4.682682
249.344794	7557.653639	9.110695	-0.051646	4.685124
249.604077	7565.726861	9.115699	-0.051700	4.687597
250.329381	7573.679115	9.120704	-0.051841	4.690031
250.620535	7581.785684	9.125709	-0.051900	4.692511
250.713828	7589.746010	9.130714	-0.051923	4.694946
250.928289	7597.810994	9.135719	-0.051969	4.697411
251.138739	7605.824077	9.140723	-0.052014	4.699859
250.594633	7613.857260	9.145728	-0.051918	4.702312
251.011643	7621.844697	9.150733	-0.052001	4.704750
251.343582	7629.825885	9.155738	-0.052068	4.707184
251.472711	7637.884279	9.160743	-0.052098	4.709641
251.561089	7645.976487	9.165747	-0.052120	4.712106
251.021917	7653.992299	9.170752	-0.052025	4.714549
251.285104	7662.028052	9.175757	-0.052080	4.716994
251.868321	7669.871517	9.180762	-0.052194	4.719380
251.762500	7677.968386	9.185767	-0.052180	4.721842
252.203251	7685.924315	9.190771	-0.052267	4.724259
252.559280	7694.006377	9.195776	-0.052339	4.726714
252.279245	7702.041940	9.200781	-0.052293	4.729154
252.443519	7710.059410	9.205786	-0.052329	4.731587
252.510925	7718.005340	9.210791	-0.052347	4.733997
252.658277	7726.096974	9.215795	-0.052380	4.736449
253.058813	7734.000703	9.220800	-0.052460	4.738843
253.019088	7742.195488	9.225805	-0.052458	4.741325
252.951499	7750.058022	9.230810	-0.052451	4.743705
253.363293	7758.157998	9.235815	-0.052534	4.746154
253.501006	7766.181884	9.240819	-0.052565	4.748580
253.715941	7774.178465	9.245824	-0.052610	4.750996
253.598357	7782.230475	9.250829	-0.052594	4.753429
253.955345	7790.233332	9.255834	-0.052666	4.755844
254.116298	7798.196425	9.260839	-0.052702	4.758246
254.037446	7806.252794	9.265843	-0.052692	4.760676
254.396201	7814.199813	9.270848	-0.052765	4.763071
254.334922	7822.310152	9.275853	-0.052759	4.765514
254.333569	7830.283082	9.280858	-0.052764	4.767915
254.574672	7838.310953	9.285863	-0.052815	4.770331
255.274019	7846.313928	9.290867	-0.052950	4.772736
255.507216	7854.295091	9.295872	-0.052999	4.775135
255.082783	7862.418597	9.300877	-0.052926	4.777577
255.464184	7870.369850	9.305882	-0.053003	4.779964
255.874259	7878.384807	9.310887	-0.053084	4.782369
256.232079	7886.374299	9.315891	-0.053157	4.784765
256.161312	7894.456232	9.320896	-0.053149	4.787189
256.429443	7902.441594	9.325901	-0.053205	4.789582
256.564369	7910.513035	9.330906	-0.053235	4.792000
256.779612	7918.406975	9.335911	-0.053281	4.794363
257.132214	7926.509878	9.340915	-0.053352	4.796787
257.068307	7934.488127	9.345920	-0.053346	4.799174
256.930844	7942.576028	9.350925	-0.053326	4.801592
256.910742	7950.493766	9.355930	-0.053328	4.803958
256.666484	7958.614549	9.360935	-0.053288	4.806385
256.808162	7966.568242	9.365939	-0.053320	4.808759
257.140672	7974.610928	9.370944	-0.053387	4.811157
257.680231	7982.584937	9.375949	-0.053493	4.813533
257.864024	7990.115496	9.380954	-0.053533	4.815778
258.058538	7994.867374	9.385959	-0.053572	4.817193

258.272592	7997.382125	9.390963	-0.053614	4.817941
258.130070	7998.756496	9.395968	-0.053589	4.818351
257.981274	7999.273461	9.400973	-0.053562	4.818506
258.221320	8000.335255	9.405978	-0.053607	4.818821
258.985655	8000.257014	9.410983	-0.053750	4.818795
258.975343	8000.265291	9.415987	-0.053748	4.818797
258.749831	8000.245654	9.420992	-0.053707	4.818792
258.733029	8000.349240	9.425997	-0.053704	4.818823
258.886786	8000.368006	9.431002	-0.053733	4.818828
259.228275	8000.373453	9.436007	-0.053797	4.818828
259.424501	8000.377039	9.441011	-0.053834	4.818829
259.434254	8000.303807	9.446016	-0.053836	4.818807
259.079240	8000.419834	9.451021	-0.053770	4.818843
258.986075	8000.439629	9.456026	-0.053753	4.818849
259.558494	8000.372560	9.461031	-0.053860	4.818827
259.428084	8000.397119	9.466035	-0.053836	4.818835
259.554155	8000.362068	9.471040	-0.053860	4.818824
259.690184	8000.378511	9.476045	-0.053886	4.818828
259.856838	8000.290517	9.481050	-0.053917	4.818801
259.940401	8000.282177	9.486055	-0.053933	4.818798
259.999228	8000.357383	9.491059	-0.053944	4.818821
260.058195	8000.302603	9.496064	-0.053956	4.818804
260.020427	8000.393344	9.501069	-0.053949	4.818831
259.719280	8000.440873	9.506074	-0.053893	4.818847
260.204292	8000.339139	9.511079	-0.053984	4.818814
260.131803	8000.394842	9.516083	-0.053971	4.818831
259.868868	8000.400929	9.521088	-0.053922	4.818834
260.110260	8000.441786	9.526093	-0.053967	4.818845
259.730388	8000.444277	9.531098	-0.053897	4.818847
259.630828	8000.427300	9.536103	-0.053879	4.818843
260.005141	8000.411156	9.541107	-0.053949	4.818837
260.107346	8000.375799	9.546112	-0.053968	4.818826
259.637552	8000.441084	9.551117	-0.053881	4.818847
259.367527	8000.481675	9.556122	-0.053831	4.818860
259.818512	8000.423533	9.561127	-0.053915	4.818841
259.816801	8000.451839	9.566131	-0.053915	4.818849
259.724238	8000.411888	9.571136	-0.053899	4.818838
259.746614	8000.497111	9.576141	-0.053903	4.818863
259.939666	8000.434614	9.581146	-0.053939	4.818844
260.156353	8000.408063	9.586151	-0.053980	4.818835
260.313269	8000.430017	9.591155	-0.054010	4.818841
260.574428	8000.242596	9.596160	-0.054058	4.818784
260.627577	8000.308296	9.601165	-0.054069	4.818803
260.422493	8000.425197	9.606170	-0.054031	4.818839
260.649711	8000.391443	9.611175	-0.054074	4.818828
260.499108	8000.429372	9.616179	-0.054046	4.818840
260.352978	8000.364622	9.621184	-0.054019	4.818821
260.880246	8000.382939	9.626189	-0.054117	4.818825
260.504213	8000.419024	9.631194	-0.054048	4.818837
260.138304	8000.474109	9.636199	-0.053980	4.818855
259.994227	8000.503734	9.641203	-0.053954	4.818864
260.172247	8000.469349	9.646208	-0.053987	4.818853
260.455051	8000.467758	9.651213	-0.054040	4.818851
260.684451	8000.446612	9.656218	-0.054083	4.818844
261.301452	8000.344475	9.661223	-0.054198	4.818812
261.165509	8000.400413	9.666227	-0.054173	4.818829
260.918556	8000.368964	9.671232	-0.054128	4.818820
261.147414	8000.398131	9.676237	-0.054171	4.818828
260.789934	8000.417680	9.681242	-0.054104	4.818835
260.770532	8000.433180	9.686247	-0.054101	4.818840
261.010962	8000.300004	9.691251	-0.054146	4.818799
260.566187	8000.440040	9.696256	-0.054064	4.818843
260.892356	8000.421184	9.701261	-0.054125	4.818836
260.749161	8000.430902	9.706266	-0.054099	4.818839
260.985981	8000.378402	9.711271	-0.054143	4.818823
261.291311	8000.392825	9.716275	-0.054200	4.818826
261.299413	8000.304893	9.721280	-0.054202	4.818800
261.311198	8000.399417	9.726285	-0.054205	4.818828
261.144862	8000.381582	9.731290	-0.054174	4.818823
261.189680	8000.387422	9.736295	-0.054183	4.818825
261.201563	8000.431628	9.741299	-0.054185	4.818838
261.047703	8000.404517	9.746304	-0.054157	4.818830
261.179051	8000.373727	9.751309	-0.054182	4.818821
261.011152	8000.383128	9.756314	-0.054151	4.818824
261.206589	8000.350015	9.761319	-0.054187	4.818813
261.563712	8000.372442	9.766323	-0.054254	4.818819
261.110235	8000.401243	9.771328	-0.054170	4.818829
261.417657	8000.402065	9.776333	-0.054228	4.818828
261.202676	8000.449651	9.781338	-0.054188	4.818843
260.985492	8000.393423	9.786343	-0.054148	4.818827
260.855473	8000.493466	9.791347	-0.054124	4.818857
260.824863	8000.410279	9.796352	-0.054119	4.818833
261.328512	8000.455552	9.801357	-0.054213	4.818844
261.524903	8000.366889	9.806362	-0.054250	4.818817
261.107465	8000.421313	9.811367	-0.054172	4.818835
261.329829	8000.449349	9.816371	-0.054214	4.818842
260.959015	8000.408972	9.821376	-0.054145	4.818832
261.146504	8000.438657	9.826381	-0.054181	4.818840
261.505446	8000.420222	9.831386	-0.054248	4.818833
261.139564	8000.482645	9.836391	-0.054180	4.818853
261.174257	8000.469485	9.841395	-0.054187	4.818849
260.936530	8000.354287	9.846400	-0.054143	4.818816
261.119098	8000.487694	9.851405	-0.054177	4.818855
261.566829	8000.401208	9.856410	-0.054261	4.818827
261.797574	8000.399999	9.861415	-0.054304	4.818826
261.843066	8000.467701	9.866419	-0.054313	4.818846
261.471028	8000.470288	9.871424	-0.054244	4.818848
261.343897	8000.501179	9.876429	-0.054221	4.818858
261.286557	8000.457484	9.881434	-0.054210	4.818845
260.999355	8000.390923	9.886439	-0.054157	4.818826
261.754959	8000.426850	9.891443	-0.054298	4.818834
261.794020	8000.363425	9.896448	-0.054306	4.818815
261.667839	8000.437310	9.901453	-0.054283	4.818837
261.660948	8000.456115	9.906458	-0.054282	4.818843
261.319979	8000.466440	9.911463	-0.054219	4.818847
261.719774	8000.445385	9.916467	-0.054293	4.818840
261.825526	8000.399590	9.921472	-0.054313	4.818826
262.040333	8000.348904	9.926477	-0.054354	4.818810
261.784226	8000.425315	9.931482	-0.054307	4.818833
261.565016	8000.408897	9.936487	-0.054266	4.818829
262.120891	8000.412910	9.941491	-0.054370	4.818828
261.894440	8000.347125	9.946496	-0.054328	4.818810
262.044897	8000.373192	9.951501	-0.054356	4.818817
261.931181	8000.426270	9.956506	-0.054336	4.818833
261.696716	8000.449493	9.961511	-0.054292	4.818841
261.398488	8000.493913	9.966515	-0.054237	4.818855
261.594169	8000.458707	9.971520	-0.054274	4.818844
261.627735	8000.497950	9.976525	-0.054280	4.818856
261.769188	8000.462049	9.981530	-0.054307	4.818844
261.832828	8000.434583	9.986535	-0.054319	4.818836
261.728177	8000.464714	9.991539	-0.054300	4.818845
261.679160	8000.356128	9.996544	-0.054291	4.818813
261.623291	8000.513736	10.001549	-0.054281	4.818860
262.119197	8000.420530	10.006554	-0.054374	4.818831
261.673820	8000.455723	10.011559	-0.054291	4.818843
262.052503	8000.485768	10.016563	-0.054362	4.818850
261.881822	8000.421747	10.021568	-0.054331	4.818832
261.356226	8000.509377	10.026573	-0.054233	4.818860
262.013843	8000.411956	10.031578	-0.054356	4.818828
261.858810	8000.413135	10.036583	-0.054328	4.818829
261.561033	8000.478528	10.041587	-0.054272	4.818850
261.648400	8000.438787	10.046592	-0.054289	4.818838
262.104201	8000.381759	10.051597	-0.054374	4.818819
261.373862	8000.350395	10.056602	-0.054239	4.818812
261.659832	8000.462067	10.061607	-0.054292	4.818845
261.843996	8000.475986	10.066611	-0.054327	4.818848
262.252952	8000.352311	10.071616	-0.054403	4.818810
262.376325	8000.369643	10.076621	-0.054427	4.818814
262.051382	8000.389608	10.081626	-0.054366	4.818822
261.839921	8000.442480	10.086631	-0.054327	4.818838
261.843948	8000.485538	10.091635	-0.054329	4.818851
261.819041	8000.442259	10.096640	-0.054324	4.818838
261.556909	8000.480852	10.101645	-0.054276	4.818851
261.422965	8000.384805	10.106650	-0.054251	4.818822
261.429117	8000.449905	10.111655	-0.054253	4.818842
261.335492	8000.533643	10.116659	-0.054236	4.818867
261.221308	8000.435753	10.121664	-0.054215	4.818838
261.535149	8000.398918	10.126669	-0.054273	4.818826
261.871598	8000.474548	10.131674	-0.054336	4.818847
262.007190	8000.451151	10.136679	-0.054362	4.818840
262.050548	8000.447538	10.141683	-0.054370	4.818839
261.711951	8000.439021	10.146688	-0.054308	4.818837
261.350115	8000.513027	10.151693	-0.054241	4.818861
261.575678	8000.413207	10.156698	-0.054283	4.818830
261.622602	8000.453670	10.161703	-0.054292	4.818842
261.803890	8000.495858	10.166707	-0.054326	4.818854
261.773465	8000.427348	10.171712	-0.054321	4.818834
261.477466	8000.493812	10.176717	-0.054266	4.818855
261.472441	8000.495867	10.181722	-0.054265	4.818855
262.198884	8000.420298	10.186727	-0.054401	4.818830
262.053521	8000.472970	10.191731	-0.054374	4.818846
261.927436	8000.422102	10.196736	-0.054351	4.818832
262.412486	8000.429401	10.201741	-0.054442	4.818832
262.124758	8000.452988	10.206746	-0.054389	4.818840
261.975749	8000.432228	10.211751	-0.054361	4.818834
262.029928	8000.465446	10.216755	-0.054372	4.818844
262.504481	8000.373015	10.221760	-0.054460	4.818815
262.506925	8000.464278	10.226765	-0.054461	4.818842
262.126105	8000.490863	10.231770	-0.054391	4.818851
262.435429	8000.359618	10.236775	-0.054448	4.818811
262.630761	8000.431342	10.241779	-0.054485	4.818832
262.171234	8000.422320	10.246784	-0.054400	4.818831
262.575281	8000.458982	10.251789	-0.054476	4.818840
262.260691	8000.387871	10.256794	-0.054417	4.818820
262.472378	8000.405289	10.261799	-0.054457	4.818824
262.472742	8000.461929	10.266803	-0.054457	4.818841
262.364791	8000.432261	10.271808	-0.054438	4.818833
262.351350	8000.488724	10.276813	-0.054436	4.818850
262.417287	8000.456046	10.281818	-0.054448	4.818840
262.164375	8000.420323	10.286823	-0.054401	4.818830
262.089529	8000.438256	10.291827	-0.054388	4.818836
262.097859	8000.449918	10.296832	-0.054390	4.818839
262.397924	8000.426536	10.301837	-0.054446	4.818831
262.214556	8000.461947	10.306842	-0.054412	4.818842
261.875302	8000.476485	10.311847	-0.054349	4.818848
262.481109	8000.383643	10.316851	-0.054462	4.818818
262.527899	8000.387412	10.321856	-0.054471	4.818819
262.718303	8000.415041	10.326861	-0.054507	4.818826
262.596018	8000.386236	10.331866	-0.054485	4.818818
262.550109	8000.355268	10.336871	-0.054477	4.818809
262.526737	8000.442006	10.341875	-0.054473	4.818835
262.265695	8000.431339	10.346880	-0.054424	4.818833
261.813642	8000.427656	10.351885	-0.054340	4.818833
261.915122	8000.509706	10.356890	-0.054360	4.818857
262.420341	8000.368396	10.361895	-0.054454	4.818813
262.516950	8000.427320	10.366899	-0.054472	4.818831
262.564077	8000.379723	10.371904	-0.054482	4.818816
262.533154	8000.430720	10.376909	-0.054476	4.818832
262.529749	8000.411829	10.381914	-0.054476	4.818826
262.512278	8000.377032	10.386919	-0.054473	4.818816
262.330113	8000.487940	10.391923	-0.054439	4.818849
261.734508	8000.494994	10.396928	-0.054329	4.818854
261.867358	8000.424386	10.401933	-0.054354	4.818832
262.413303	8000.466014	10.406938	-0.054456	4.818842
262.626133	8000.463529	10.411943	-0.054496	4.818841
262.568274	8000.478535	10.416947	-0.054485	4.818846
262.587646	8000.419050	10.421952	-0.054489	4.818828
262.158858	8000.497437	10.426957	-0.054410	4.818853
262.143544	8000.467910	10.431962	-0.054407	4.818844
262.093953	8000.403346	10.436967	-0.054398	4.818825
262.574510	8000.496554	10.441971	-0.054488	4.818851
262.706341	8000.402868	10.446976	-0.054513	4.818822
262.111263	8000.506378	10.451981	-0.054403	4.818856
262.143565	8000.495284	10.456986	-0.054409	4.818852
262.170676	8000.432754	10.461991	-0.054414	4.818833
262.139305	8000.387295	10.466995	-0.054409	4.818820
261.600157	8000.536603	10.472000	-0.054309	4.818866
261.765135	8000.455924	10.477005	-0.054340	4.818842
262.404765	8000.490368	10.482010	-0.054459	4.818850
262.084181	8000.492566	10.487015	-0.054400	4.818851
262.411844	8000.368894	10.492019	-0.054461	4.818813
261.766920	8000.522087	10.497024	-0.054342	4.818861
262.220599	8000.405276	10.502029	-0.054426	4.818825
262.033477	8000.495153	10.507034	-0.054392	4.818852
262.079819	8000.469562	10.512039	-0.054401	4.818845
262.191399	8000.480454	10.517043	-0.054422	4.818847
261.899082	8000.370840	10.522048	-0.054368	4.818816
262.800249	8000.367755	10.527053	-0.054536	4.818812
262.638877	8000.428609	10.532058	-0.054506	4.818830
262.582148	8000.442581	10.537063	-0.054496	4.818835
262.504863	8000.483547	10.542067	-0.054482	4.818847
262.624706	8000.438981	10.547072	-0.054505	4.818833
262.695107	8000.440957	10.552077	-0.054518	4.818834
262.562676	8000.466537	10.557082	-0.054494	4.818842
262.130086	8000.486167	10.562087	-0.054414	4.818849
262.172331	8000.425927	10.567091	-0.054422	4.818831
262.094169	8000.485753	10.572096	-0.054408	4.818849
262.426183	8000.503668	10.577101	-0.054470	4.818853
262.266065	8000.468087	10.582106	-0.054440	4.818843
261.998660	8000.403872	10.587111	-0.054391	4.818825
262.591349	8000.503763	10.592115	-0.054502	4.818853
262.722617	8000.450956	10.597120	-0.054526	4.818837
262.312814	8000.471926	10.602125	-0.054450	4.818844
262.783652	8000.460174	10.607130	-0.054538	4.818839
262.732381	8000.441716	10.612135	-0.054529	4.818834
262.480339	8000.367213	10.617139	-0.054483	4.818812
262.638522	8000.416445	10.622144	-0.054512	4.818827
263.072674	8000.369624	10.627149	-0.054594	4.818811
263.290860	8000.423821	10.632154	-0.054635	4.818826
263.178242	8000.342720	10.637159	-0.054614	4.818802
263.108758	8000.407900	10.642163	-0.054601	4.818822
263.374119	8000.367299	10.647168	-0.054651	4.818809
263.043962	8000.365179	10.652173	-0.054590	4.818810
263.085532	8000.392994	10.657178	-0.054598	4.818818
263.081522	8000.337402	10.662183	-0.054598	4.818801
263.089605	8000.411964	10.667187	-0.054599	4.818823
262.818983	8000.466173	10.672192	-0.054549	4.818841
263.099021	8000.371245	10.677197	-0.054602	4.818811
263.120402	8000.404043	10.682202	-0.054606	4.818821
262.874392	8000.439697	10.687207	-0.054561	4.818832
263.196335	8000.400872	10.692211	-0.054621	4.818820
262.984745	8000.430677	10.697216	-0.054582	4.818829
262.640496	8000.472408	10.702221	-0.054518	4.818843
262.873339	8000.485906	10.707226	-0.054562	4.818846
262.857502	8000.433307	10.712231	-0.054559	4.818831
262.533042	8000.502550	10.717235	-0.054499	4.818852
262.831398	8000.383744	10.722240	-0.054555	4.818816
263.039910	8000.439913	10.727245	-0.054594	4.818832
263.280637	8000.431497	10.732250	-0.054639	4.818828
263.071179	8000.346007	10.737255	-0.054601	4.818804
263.122479	8000.415883	10.742259	-0.054611	4.818824
263.134661	8000.389853	10.747264	-0.054613	4.818817
263.139603	8000.448650	10.752269	-0.054614	4.818834
263.192201	8000.461930	10.757274	-0.054625	4.818838
262.588523	8000.507667	10.762279	-0.054513	4.818854
262.461267	8000.409605	10.767283	-0.054489	4.818825
262.396620	8000.492668	10.772288	-0.054478	4.818850
262.870700	8000.333135	10.777293	-0.054566	4.818801
263.147482	8000.442601	10.782298	-0.054618	4.818832
263.219879	8000.420490	10.787303	-0.054632	4.818825
263.106052	8000.437922	10.792307	-0.054611	4.818831
263.058922	8000.448872	10.797312	-0.054603	4.818834
263.113468	8000.437016	10.802317	-0.054613	4.818831
262.886911	8000.461387	10.807322	-0.054571	4.818839
263.169763	8000.408430	10.812327	-0.054624	4.818822
263.351939	8000.399262	10.817331	-0.054658	4.818818
262.803808	8000.420551	10.822336	-0.054557	4.818827
263.182976	8000.424396	10.827341	-0.054628	4.818827
263.024586	8000.478998	10.832346	-0.054599	4.818843
262.476895	8000.419568	10.837351	-0.054497	4.818828
262.797773	8000.512825	10.842355	-0.054557	4.818854
262.866864	8000.462365	10.847360	-0.054570	4.818839
262.563469	8000.411315	10.852365	-0.054514	4.818825
262.201434	8000.512575	10.857370	-0.054447	4.818856
262.312993	8000.387178	10.862375	-0.054468	4.818819
262.588957	8000.528083	10.867379	-0.054520	4.818860
262.763974	8000.468499	10.872384	-0.054553	4.818841
262.607497	8000.485384	10.877389	-0.054524	4.818847
263.026132	8000.470865	10.882394	-0.054602	4.818841
263.273180	8000.370271	10.887399	-0.054648	4.818810
262.853864	8000.437247	10.892403	-0.054571	4.818832
262.765369	8000.455005	10.897408	-0.054555	4.818837
262.554301	8000.410382	10.902413	-0.054516	4.818825
262.486299	8000.523806	10.907418	-0.054503	4.818859
262.679557	8000.477038	10.912423	-0.054540	4.818844
263.383906	8000.426350	10.917427	-0.054671	4.818826
262.971825	8000.454629	10.922432	-0.054595	4.818836
262.785905	8000.402990	10.927437	-0.054560	4.818822
262.935546	8000.520258	10.932442	-0.054589	4.818856
262.987721	8000.474822	10.937447	-0.054599	4.818842
263.037449	8000.477581	10.942451	-0.054608	4.818843
262.880318	8000.449377	10.947456	-0.054579	4.818835
263.064384	8000.439184	10.952461	-0.054614	4.818831
262.700547	8000.366389	10.957466	-0.054547	4.818811
262.537747	8000.505853	10.962471	-0.054517	4.818853
263.185558	8000.507908	10.967475	-0.054638	4.818851
262.940258	8000.468086	10.972480	-0.054592	4.818840
262.430848	8000.399713	10.977485	-0.054498	4.818822
262.387057	8000.422238	10.982490	-0.054490	4.818829
263.104364	8000.389538	10.987495	-0.054624	4.818816
263.506705	8000.396827	10.992499	-0.054699	4.818817
263.544111	8000.319749	10.997504	-0.054706	4.818794
263.062062	8000.360758	11.002509	-0.054617	4.818808
263.220422	8000.479188	11.007514	-0.054647	4.818842
263.359323	8000.408656	11.012519	-0.054673	4.818821
263.676207	8000.378153	11.017523	-0.054732	4.818811
263.334430	8000.439835	11.022528	-0.054669	4.818830
263.663578	8000.356021	11.027533	-0.054731	4.818804
263.881392	8000.396586	11.032538	-0.054772	4.818815
263.580885	8000.373877	11.037543	-0.054716	4.818810
263.417801	8000.414790	11.042547	-0.054686	4.818822
263.870019	8000.378687	11.047552	-0.054770	4.818810
263.486651	8000.429350	11.052557	-0.054699	4.818827
263.516430	8000.465402	11.057562	-0.054705	4.818837
263.350324	8000.426597	11.062567	-0.054675	4.818826
263.544866	8000.484686	11.067571	-0.054711	4.818843
263.392346	8000.456539	11.072576	-0.054683	4.818835
262.778780	8000.497955	11.077581	-0.054569	4.818850
262.880932	8000.507678	11.082586	-0.054589	4.818852
263.115609	8000.476119	11.087591	-0.054633	4.818842
263.206812	8000.455297	11.092595	-0.054650	4.818835
263.264689	8000.427758	11.097600	-0.054661	4.818827
263.432960	8000.401636	11.102605	-0.054693	4.818818
263.489639	8000.371984	11.107610	-0.054704	4.818809
263.535131	8000.334849	11.112615	-0.054712	4.818798
263.453392	8000.406162	11.117619	-0.054698	4.818820
263.564716	8000.347857	11.122624	-0.054719	4.818802
263.735238	8000.299748	11.127629	-0.054751	4.818787
263.480278	8000.452708	11.132634	-0.054704	4.818833
263.477635	8000.418100	11.137639	-0.054704	4.818823
263.481156	8000.448572	11.142643	-0.054705	4.818832
263.200471	8000.451280	11.147648	-0.054653	4.818834
263.377843	8000.369710	11.152653	-0.054686	4.818809
263.518106	8000.449117	11.157658	-0.054712	4.818832
263.341930	8000.420667	11.162663	-0.054680	4.818824
263.388522	8000.481048	11.167667	-0.054689	4.818842
263.360298	8000.434579	11.172672	-0.054684	4.818828
263.676699	8000.354795	11.177677	-0.054743	4.818803
263.285248	8000.461968	11.182682	-0.054671	4.818837
263.321175	8000.373339	11.187687	-0.054678	4.818810
262.966803	8000.463166	11.192691	-0.054612	4.818838
262.836731	8000.451035	11.197696	-0.054588	4.818835
263.236593	8000.485550	11.202701	-0.054663	4.818844
263.296412	8000.411905	11.207706	-0.054675	4.818822
263.249965	8000.444881	11.212711	-0.054666	4.818832
263.263813	8000.496454	11.217715	-0.054669	4.818847
262.724101	8000.545109	11.222720	-0.054569	4.818864
263.088797	8000.379977	11.227725	-0.054637	4.818813
263.002205	8000.482679	11.232730	-0.054621	4.818844
263.179772	8000.443048	11.237735	-0.054655	4.818832
262.518659	8000.446112	11.242739	-0.054532	4.818835
262.637336	8000.435078	11.247744	-0.054555	4.818831
263.165213	8000.421963	11.252749	-0.054653	4.818825
263.322450	8000.486911	11.257754	-0.054683	4.818844
263.255072	8000.414777	11.262759	-0.054671	4.818823
263.105447	8000.479976	11.267763	-0.054643	4.818843
262.910076	8000.456521	11.272768	-0.054607	4.818837
262.778938	8000.494699	11.277773	-0.054583	4.818848
262.944359	8000.437089	11.282778	-0.054614	4.818831
263.364362	8000.458234	11.287783	-0.054693	4.818835
262.685661	8000.426474	11.292787	-0.054567	4.818828
262.415371	8000.423026	11.297792	-0.054517	4.818828
262.483065	8000.300210	11.302797	-0.054529	4.818792
262.443814	8000.440212	11.307802	-0.054523	4.818833
262.639956	8000.422836	11.312807	-0.054559	4.818827
262.189889	8000.390870	11.317811	-0.054476	4.818820
262.752210	8000.424324	11.322816	-0.054581	4.818827
263.151036	8000.515439	11.327821	-0.054656	4.818853
263.146220	8000.397980	11.332826	-0.054655	4.818818
263.158618	8000.474696	11.337831	-0.054658	4.818841
263.463272	8000.442988	11.342835	-0.054715	4.818830
263.142739	8000.482926	11.347840	-0.054655	4.818843
263.336455	8000.447696	11.352845	-0.054692	4.818832
262.959510	8000.399892	11.357850	-0.054622	4.818819
263.049089	8000.483890	11.362855	-0.054639	4.818844
263.318876	8000.488428	11.367859	-0.054690	4.818844
262.976947	8000.511316	11.372864	-0.054626	4.818852
263.100197	8000.429051	11.377869	-0.054650	4.818827
263.258759	8000.489822	11.382874	-0.054679	4.818845
263.111113	8000.378915	11.387879	-0.054652	4.818812
263.422248	8000.448985	11.392883	-0.054711	4.818832
262.956200	8000.476570	11.397888	-0.054624	4.818842
263.334326	8000.403869	11.402893	-0.054695	4.818819
263.620472	8000.457893	11.407898	-0.054748	4.818834
263.198515	8000.440962	11.412903	-0.054670	4.818831
263.303425	8000.501044	11.417907	-0.054690	4.818848
263.059156	8000.488493	11.422912	-0.054645	4.818845
263.207657	8000.422279	11.427917	-0.054673	4.818825
262.781260	8000.431502	11.432922	-0.054594	4.818829
263.173214	8000.472206	11.437927	-0.054667	4.818840
263.308915	8000.500183	11.442931	-0.054693	4.818848
263.101212	8000.407375	11.447936	-0.054654	4.818821
262.920073	8000.427088	11.452941	-0.054621	4.818827
263.427032	8000.461932	11.457946	-0.054716	4.818836
263.133199	8000.448744	11.462951	-0.054661	4.818833
263.462640	8000.445662	11.467955	-0.054723	4.818831
263.562002	8000.429139	11.472960	-0.054742	4.818826
263.194690	8000.473718	11.477965	-0.054674	4.818840
263.368771	8000.479123	11.482970	-0.054707	4.818841
262.905167	8000.497303	11.487975	-0.054621	4.818848
263.214212	8000.431054	11.492979	-0.054679	4.818827
263.366081	8000.480207	11.497984	-0.054707	4.818842
263.320760	8000.498520	11.502989	-0.054699	4.818847
262.778884	8000.431822	11.507994	-0.054599	4.818829
262.787339	8000.527358	11.512999	-0.054600	4.818858
262.778907	8000.350095	11.518003	-0.054599	4.818805
262.856340	8000.349016	11.523008	-0.054614	4.818804
262.625209	8000.467684	11.528013	-0.054571	4.818841
262.939986	8000.507397	11.533018	-0.054630	4.818851
262.377054	8000.416318	11.538023	-0.054526	4.818826
263.304420	8000.480674	11.543027	-0.054699	4.818842
262.806736	8000.490029	11.548032	-0.054606	4.818847
262.644794	8000.534101	11.553037	-0.054577	4.818860
263.146360	8000.395889	11.558042	-0.054670	4.818817
263.079120	8000.486260	11.563047	-0.054658	4.818844
262.986719	8000.422192	11.568051	-0.054641	4.818826
262.890169	8000.466056	11.573056	-0.054624	4.818839
263.314382	8000.436933	11.578061	-0.054703	4.818829
263.541009	8000.459788	11.583066	-0.054746	4.818835
263.222571	8000.425316	11.588071	-0.054687	4.818826
263.525658	8000.414556	11.593075	-0.054743	4.818821
263.125420	8000.427260	11.598080	-0.054669	4.818827
263.083204	8000.441418	11.603085	-0.054662	4.818831
263.573942	8000.500168	11.608090	-0.054753	4.818847
263.331967	8000.371273	11.613095	-0.054709	4.818809
263.145565	8000.539791	11.618099	-0.054674	4.818860
263.602623	8000.527866	11.623104	-0.054760	4.818855
263.241012	8000.440417	11.628109	-0.054693	4.818830
263.697571	8000.466228	11.633114	-0.054778	4.818836
263.579929	8000.406028	11.638119	-0.054756	4.818818
263.274676	8000.496486	11.643123	-0.054700	4.818847
263.377456	8000.491539	11.648128	-0.054720	4.818845
262.624081	8000.447287	11.653133	-0.054580	4.818834
262.899110	8000.481246	11.658138	-0.054631	4.818843
262.672717	8000.436426	11.663143	-0.054589	4.818831
263.187135	8000.473461	11.668147	-0.054685	4.818840
263.138755	8000.482299	11.673152	-0.054677	4.818843
263.285321	8000.460092	11.678157	-0.054704	4.818836
263.366113	8000.442282	11.683162	-0.054720	4.818830
263.262018	8000.433629	11.688167	-0.054701	4.818828
263.677068	8000.440034	11.693171	-0.054778	4.818828
263.148842	8000.447948	11.698176	-0.054680	4.818832
263.019026	8000.392835	11.703181	-0.054656	4.818817
263.517785	8000.517737	11.708186	-0.054750	4.818852
263.360043	8000.476942	11.713191	-0.054721	4.818840
263.288618	8000.393224	11.718195	-0.054708	4.818816
263.347573	8000.484168	11.723200	-0.054719	4.818842
262.950988	8000.501112	11.728205	-0.054646	4.818849
263.460874	8000.478331	11.733210	-0.054741	4.818840
263.240430	8000.462941	11.738215	-0.054700	4.818837
263.385036	8000.409257	11.743219	-0.054727	4.818820
263.518582	8000.461320	11.748224	-0.054753	4.818835
263.362485	8000.497081	11.753229	-0.054724	4.818846
263.567846	8000.495550	11.758234	-0.054762	4.818845
263.198354	8000.466711	11.763239	-0.054694	4.818838
263.016619	8000.372140	11.768243	-0.054660	4.818810
262.704900	8000.468806	11.773248	-0.054603	4.818840
262.824521	8000.465124	11.778253	-0.054625	4.818839
263.468421	8000.506970	11.783258	-0.054746	4.818849
263.726658	8000.383454	11.788263	-0.054794	4.818811
263.583532	8000.470753	11.793267	-0.054768	4.818837
263.374864	8000.496402	11.798272	-0.054729	4.818846
263.389175	8000.363461	11.803277	-0.054732	4.818806
263.770892	8000.477425	11.808282	-0.054804	4.818839
263.404660	8000.467499	11.813287	-0.054736	4.818837
263.784355	8000.455628	11.818291	-0.054807	4.818832
263.533245	8000.444037	11.823296	-0.054760	4.818830
263.586293	8000.463613	11.828301	-0.054771	4.818835
263.667453	8000.460486	11.833306	-0.054786	4.818834
263.565656	8000.461298	11.838311	-0.054767	4.818835
263.651730	8000.506461	11.843315	-0.054784	4.818848
263.489890	8000.408999	11.848320	-0.054754	4.818819
263.285980	8000.512292	11.853325	-0.054716	4.818851
263.336724	8000.389255	11.858330	-0.054726	4.818814
263.694251	8000.408550	11.863335	-0.054793	4.818818
263.942071	8000.424340	11.868339	-0.054840	4.818822
264.117414	8000.383631	11.873344	-0.054872	4.818809
263.636127	8000.461343	11.878349	-0.054783	4.818834
263.709942	8000.468605	11.883354	-0.054797	4.818836
263.557837	8000.441512	11.888359	-0.054769	4.818829
263.415197	8000.517285	11.893363	-0.054743	4.818852
263.539822	8000.521007	11.898368	-0.054767	4.818852
263.193097	8000.409636	11.903373	-0.054702	4.818821
263.273453	8000.531260	11.908378	-0.054718	4.818856
263.167096	8000.450237	11.913383	-0.054698	4.818833
263.134484	8000.415244	11.918387	-0.054693	4.818822
263.293374	8000.509569	11.923392	-0.054723	4.818850
263.534671	8000.472854	11.928397	-0.054768	4.818838
263.513856	8000.405511	11.933402	-0.054764	4.818818
263.141283	8000.523411	11.938407	-0.054695	4.818855
263.110312	8000.423438	11.943411	-0.054690	4.818825
263.520627	8000.458089	11.948416	-0.054766	4.818834
263.567008	8000.503790	11.953421	-0.054775	4.818847
263.343215	8000.501986	11.958426	-0.054734	4.818847
263.034073	8000.416261	11.963431	-0.054677	4.818823
263.436264	8000.421452	11.968435	-0.054752	4.818823
263.486312	8000.504944	11.973440	-0.054762	4.818848
263.310531	8000.513192	11.978445	-0.054729	4.818851
263.304339	8000.452328	11.983450	-0.054729	4.818833
263.303924	8000.394684	11.988455	-0.054729	4.818816
263.302754	8000.493243	11.993459	-0.054729	4.818845
263.410943	8000.507237	11.998464	-0.054749	4.818849
263.556243	8000.367592	12.003469	-0.054777	4.818807
263.692306	8000.486787	12.008474	-0.054803	4.818842
263.773029	8000.443814	12.013479	-0.054818	4.818828
263.531845	8000.500498	12.018483	-0.054773	4.818846
263.713638	8000.488180	12.023488	-0.054808	4.818842
263.710326	8000.352914	12.028493	-0.054807	4.818802
263.975297	8000.408764	12.033498	-0.054857	4.818817
264.275728	8000.370712	12.038503	-0.054913	4.818805
264.048815	8000.444354	12.043507	-0.054871	4.818827
264.089717	8000.431274	12.048512	-0.054879	4.818823
264.195855	8000.440001	12.053517	-0.054899	4.818826
263.952234	8000.496653	12.058522	-0.054854	4.818843
264.044031	8000.441241	12.063527	-0.054872	4.818827
263.988932	8000.445798	12.068531	-0.054862	4.818828
263.928036	8000.430361	12.073536	-0.054851	4.818824
263.915210	8000.408203	12.078541	-0.054849	4.818817
264.108127	8000.458934	12.083546	-0.054885	4.818832
263.745197	8000.449050	12.088551	-0.054818	4.818830
263.719470	8000.415193	12.093555	-0.054813	4.818820
263.994957	8000.460694	12.098560	-0.054865	4.818832
263.797380	8000.461323	12.103565	-0.054829	4.818833
263.638977	8000.504393	12.108570	-0.054799	4.818847
263.565897	8000.511864	12.113575	-0.054786	4.818849
263.586362	8000.394728	12.118579	-0.054790	4.818814
263.485890	8000.510883	12.123584	-0.054772	4.818849
263.500656	8000.510047	12.128589	-0.054775	4.818849
264.096431	8000.379337	12.133594	-0.054886	4.818808
263.847958	8000.400280	12.138599	-0.054840	4.818815
263.591790	8000.471449	12.143603	-0.054793	4.818837
263.654266	8000.447113	12.148608	-0.054805	4.818830
263.749250	8000.438922	12.153613	-0.054823	4.818827
263.818088	8000.505881	12.158618	-0.054836	4.818847
263.625709	8000.458349	12.163623	-0.054801	4.818833
263.943951	8000.428913	12.168627	-0.054860	4.818823
263.864611	8000.450982	12.173632	-0.054846	4.818830
263.444118	8000.390035	12.178637	-0.054768	4.818813
263.308813	8000.518323	12.183642	-0.054743	4.818852
263.436122	8000.481192	12.188647	-0.054767	4.818841
263.863189	8000.475172	12.193651	-0.054847	4.818837
263.827856	8000.394012	12.198656	-0.054841	4.818813
263.486401	8000.506022	12.203661	-0.054777	4.818848
263.617855	8000.542333	12.208666	-0.054802	4.818858
263.245200	8000.413853	12.213671	-0.054733	4.818821
263.492371	8000.450602	12.218675	-0.054780	4.818831
263.877257	8000.459766	12.223680	-0.054852	4.818832
264.005101	8000.404818	12.228685	-0.054876	4.818816
264.056398	8000.483085	12.233690	-0.054886	4.818839
263.855676	8000.461656	12.238695	-0.054849	4.818833
263.845675	8000.425904	12.243699	-0.054847	4.818822
264.104540	8000.459660	12.248704	-0.054896	4.818832
264.181737	8000.465918	12.253709	-0.054910	4.818833
263.876113	8000.528064	12.258714	-0.054854	4.818853
263.954106	8000.359244	12.263719	-0.054869	4.818802
263.909634	8000.486604	12.268723	-0.054861	4.818840
263.644508	8000.474832	12.273728	-0.054812	4.818838
263.558278	8000.496812	12.278733	-0.054796	4.818845
263.649070	8000.428807	12.283738	-0.054813	4.818824
263.724439	8000.501092	12.288743	-0.054828	4.818845
264.186415	8000.386485	12.293747	-0.054914	4.818809
263.915406	8000.476334	12.298752	-0.054864	4.818837
263.548750	8000.505194	12.303757	-0.054796	4.818847
264.037138	8000.404556	12.308762	-0.054887	4.818815
263.788365	8000.473723	12.313767	-0.054841	4.818837
263.584315	8000.392492	12.318771	-0.054803	4.818813
263.365308	8000.542770	12.323776	-0.054763	4.818859
263.279823	8000.411691	12.328781	-0.054747	4.818820
263.723208	8000.533788	12.333786	-0.054830	4.818855
263.752571	8000.449266	12.338791	-0.054836	4.818830
264.240254	8000.437736	12.343795	-0.054927	4.818824
264.241748	8000.426245	12.348800	-0.054928	4.818821
264.396631	8000.430357	12.353805	-0.054957	4.818822
264.454878	8000.461534	12.358810	-0.054968	4.818831
264.200760	8000.411111	12.363815	-0.054921	4.818817
264.318855	8000.357085	12.368819	-0.054944	4.818800
264.775295	8000.394431	12.373824	-0.055029	4.818809
264.209483	8000.392421	12.378829	-0.054924	4.818811
264.210858	8000.489967	12.383834	-0.054925	4.818840
263.785152	8000.496050	12.388839	-0.054846	4.818843
264.029714	8000.469861	12.393843	-0.054891	4.818835
263.758705	8000.507289	12.398848	-0.054841	4.818847
263.927595	8000.341736	12.403853	-0.054873	4.818797
263.780194	8000.527533	12.408858	-0.054846	4.818853
263.732394	8000.482908	12.413863	-0.054837	4.818840
264.084267	8000.463341	12.418867	-0.054903	4.818832
264.367112	8000.479582	12.423872	-0.054956	4.818836
264.147102	8000.460002	12.428877	-0.054916	4.818831
264.185853	8000.417537	12.433882	-0.054923	4.818818
264.166978	8000.469740	12.438887	-0.054920	4.818834
264.222115	8000.491441	12.443891	-0.054931	4.818840
263.876176	8000.499598	12.448896	-0.054867	4.818844
263.904175	8000.445463	12.453901	-0.054872	4.818828
264.061390	8000.509365	12.458906	-0.054902	4.818846
263.579656	8000.407789	12.463911	-0.054812	4.818818
263.634757	8000.507072	12.468915	-0.054823	4.818847
263.897446	8000.406678	12.473920	-0.054872	4.818816
263.363804	8000.517266	12.478925	-0.054773	4.818851
263.667034	8000.518042	12.483930	-0.054830	4.818850
264.028194	8000.479722	12.488935	-0.054898	4.818837
263.934917	8000.396769	12.493939	-0.054881	4.818813
263.685224	8000.526733	12.498944	-0.054834	4.818853
263.780161	8000.442006	12.503949	-0.054852	4.818827
263.587845	8000.421734	12.508954	-0.054817	4.818822
263.881435	8000.489486	12.513959	-0.054872	4.818841
263.523984	8000.440880	12.518963	-0.054806	4.818828
264.068910	8000.511863	12.523968	-0.054908	4.818847
264.102171	8000.466183	12.528973	-0.054914	4.818833
264.047573	8000.507442	12.533978	-0.054904	4.818846
263.617224	8000.410720	12.538983	-0.054824	4.818818
264.020049	8000.496650	12.543987	-0.054900	4.818842
264.054410	8000.496067	12.548992	-0.054907	4.818842
264.472660	8000.389285	12.553997	-0.054985	4.818809
264.488957	8000.400003	12.559002	-0.054988	4.818812
264.167802	8000.423156	12.564007	-0.054929	4.818820
263.833088	8000.442991	12.569011	-0.054867	4.818827
264.092328	8000.474654	12.574016	-0.054915	4.818836
264.113528	8000.446643	12.579021	-0.054920	4.818827
264.565625	8000.340296	12.584026	-0.055004	4.818794
264.318679	8000.366501	12.589031	-0.054958	4.818802
264.380886	8000.351597	12.594035	-0.054970	4.818798
264.318241	8000.431545	12.599040	-0.054959	4.818822
264.154942	8000.391725	12.604045	-0.054929	4.818811
264.536733	8000.387221	12.609050	-0.055000	4.818808
264.077983	8000.350942	12.614055	-0.054915	4.818799
264.240390	8000.390797	12.619059	-0.054946	4.818810
264.285659	8000.477374	12.624064	-0.054955	4.818836
263.772484	8000.466606	12.629069	-0.054860	4.818834
264.252775	8000.493774	12.634074	-0.054949	4.818841
263.999695	8000.416104	12.639079	-0.054902	4.818818
263.718260	8000.558241	12.644083	-0.054850	4.818862
264.424391	8000.410078	12.649088	-0.054982	4.818815
264.320837	8000.381511	12.654093	-0.054963	4.818807
264.111509	8000.393521	12.659098	-0.054925	4.818811
264.018629	8000.481467	12.664103	-0.054908	4.818838
264.446914	8000.396832	12.669107	-0.054988	4.818811
264.184045	8000.436461	12.674112	-0.054939	4.818824
264.214395	8000.444214	12.679117	-0.054945	4.818826
264.202858	8000.443041	12.684122	-0.054943	4.818826
264.237929	8000.374318	12.689127	-0.054950	4.818805
264.317714	8000.397385	12.694131	-0.054965	4.818812
264.325193	8000.404843	12.699136	-0.054967	4.818814
264.355522	8000.381142	12.704141	-0.054973	4.818807
264.544874	8000.447556	12.709146	-0.055009	4.818826
264.174158	8000.423940	12.714151	-0.054940	4.818820
263.922600	8000.487829	12.719155	-0.054894	4.818840
264.461399	8000.452843	12.724160	-0.054994	4.818827
264.175855	8000.443953	12.729165	-0.054941	4.818826
263.836882	8000.408165	12.734170	-0.054879	4.818817
264.038852	8000.462158	12.739175	-0.054917	4.818832
263.961561	8000.452801	12.744179	-0.054903	4.818829
264.199549	8000.463223	12.749184	-0.054947	4.818832
264.164907	8000.416670	12.754189	-0.054941	4.818818
264.193805	8000.427549	12.759194	-0.054947	4.818821
264.389956	8000.385012	12.764199	-0.054984	4.818807
263.852884	8000.457811	12.769203	-0.054884	4.818831
264.193736	8000.338501	12.774208	-0.054948	4.818794
263.868199	8000.475878	12.779213	-0.054888	4.818837
263.948150	8000.473784	12.784218	-0.054903	4.818836
264.153801	8000.441853	12.789223	-0.054941	4.818825
264.098567	8000.485201	12.794227	-0.054931	4.818838
263.813852	8000.403980	12.799232	-0.054879	4.818815
263.880072	8000.507601	12.804237	-0.054891	4.818846
263.958660	8000.535894	12.809242	-0.054906	4.818854
263.942467	8000.480142	12.814247	-0.054904	4.818837
263.937997	8000.383652	12.819251	-0.054903	4.818809
264.126884	8000.485705	12.824256	-0.054939	4.818838
264.026532	8000.492826	12.829261	-0.054920	4.818841
264.167232	8000.507240	12.834266	-0.054947	4.818845
263.534870	8000.319853	12.839271	-0.054829	4.818791
263.763531	8000.532501	12.844275	-0.054872	4.818854
264.194073	8000.454185	12.849280	-0.054953	4.818829
264.103374	8000.420541	12.854285	-0.054936	4.818819
264.078614	8000.499927	12.859290	-0.054932	4.818843
263.759144	8000.430840	12.864295	-0.054873	4.818823
263.608584	8000.434170	12.869299	-0.054845	4.818825
263.909342	8000.527177	12.874304	-0.054902	4.818851
263.813302	8000.432655	12.879309	-0.054884	4.818824
263.920805	8000.433012	12.884314	-0.054904	4.818823
263.732433	8000.520779	12.889319	-0.054870	4.818850
263.726566	8000.516533	12.894323	-0.054869	4.818849
263.923995	8000.385944	12.899328	-0.054906	4.818809
263.650620	8000.403422	12.904333	-0.054855	4.818816
263.534609	8000.341146	12.909338	-0.054834	4.818797
263.792342	8000.511182	12.914343	-0.054883	4.818847
263.668582	8000.372270	12.919347	-0.054860	4.818806
263.658741	8000.418298	12.924352	-0.054858	4.818820
263.662773	8000.534749	12.929357	-0.054859	4.818855
263.942643	8000.428285	12.934362	-0.054912	4.818822
263.896435	8000.519976	12.939367	-0.054904	4.818849
263.729314	8000.366877	12.944371	-0.054873	4.818804
263.791490	8000.540691	12.949376	-0.054885	4.818856
263.915685	8000.495132	12.954381	-0.054908	4.818842
264.025311	8000.443094	12.959386	-0.054929	4.818826
263.623381	8000.445289	12.964391	-0.054854	4.818828
263.679167	8000.446030	12.969395	-0.054865	4.818828
264.088431	8000.541481	12.974400	-0.054942	4.818855
264.268039	8000.472520	12.979405	-0.054976	4.818834
264.103578	8000.412764	12.984410	-0.054945	4.818817
263.945693	8000.510359	12.989415	-0.054916	4.818846
263.948921	8000.527199	12.994419	-0.054917	4.818851
263.837437	8000.436672	12.999424	-0.054897	4.818825
264.320865	8000.435572	13.004429	-0.054987	4.818822
263.644449	8000.432141	13.009434	-0.054861	4.818824
263.519458	8000.450478	13.014439	-0.054838	4.818830
263.511045	8000.439909	13.019443	-0.054837	4.818827
263.354284	8000.455741	13.024448	-0.054808	4.818832
263.511661	8000.421092	13.029453	-0.054838	4.818821
263.985022	8000.534142	13.034458	-0.054927	4.818853
263.704964	8000.507498	13.039463	-0.054875	4.818846
263.543249	8000.441489	13.044467	-0.054845	4.818827
263.783414	8000.541055	13.049472	-0.054890	4.818856
263.880750	8000.385065	13.054477	-0.054908	4.818809
264.014623	8000.553511	13.059482	-0.054934	4.818859
264.042355	8000.425982	13.064487	-0.054939	4.818821
263.651476	8000.422028	13.069491	-0.054867	4.818821
263.871335	8000.529722	13.074496	-0.054908	4.818852
263.931532	8000.505357	13.079501	-0.054920	4.818845
264.621792	8000.370619	13.084506	-0.055048	4.818802
264.132462	8000.485970	13.089511	-0.054958	4.818838
264.336581	8000.435147	13.094515	-0.054996	4.818822
264.798540	8000.452645	13.099520	-0.055082	4.818826
264.279213	8000.448086	13.104525	-0.054986	4.818826
263.822709	8000.526115	13.109530	-0.054901	4.818851
264.076192	8000.391004	13.114535	-0.054949	4.818810
264.237570	8000.478026	13.119539	-0.054979	4.818835
263.877898	8000.457698	13.124544	-0.054913	4.818831
263.481365	8000.505045	13.129549	-0.054839	4.818846
263.527072	8000.338957	13.134554	-0.054848	4.818797
263.968682	8000.496679	13.139559	-0.054931	4.818842
264.072227	8000.400529	13.144563	-0.054950	4.818813
264.629662	8000.497888	13.149568	-0.055054	4.818840
263.880532	8000.475696	13.154573	-0.054915	4.818836
263.866572	8000.545785	13.159578	-0.054913	4.818857
263.720472	8000.389810	13.164583	-0.054886	4.818811
263.727630	8000.399362	13.169587	-0.054888	4.818814
264.187167	8000.465054	13.174592	-0.054974	4.818832
264.120137	8000.450586	13.179597	-0.054962	4.818827
264.497291	8000.505785	13.184602	-0.055032	4.818842
264.466068	8000.433064	13.189607	-0.055027	4.818821
264.331133	8000.448127	13.194611	-0.055002	4.818826
264.857178	8000.411930	13.199616	-0.055100	4.818813
264.811399	8000.373620	13.204621	-0.055092	4.818802
264.422492	8000.465099	13.209626	-0.055020	4.818831
264.186685	8000.459993	13.214631	-0.054976	4.818830
264.439549	8000.456978	13.219635	-0.055024	4.818828
264.476618	8000.498367	13.224640	-0.055031	4.818840
264.428332	8000.398167	13.229645	-0.055022	4.818811
265.120398	8000.398704	13.234650	-0.055151	4.818808
264.623449	8000.422741	13.239655	-0.055059	4.818817
264.245808	8000.476620	13.244659	-0.054989	4.818835
264.934341	8000.423641	13.249664	-0.055118	4.818816
264.775611	8000.388072	13.254669	-0.055089	4.818806
265.077338	8000.354232	13.259674	-0.055145	4.818795
264.835393	8000.388888	13.264679	-0.055100	4.818806
264.752888	8000.379462	13.269683	-0.055085	4.818804
264.935925	8000.386034	13.274688	-0.055120	4.818805
265.206204	8000.354935	13.279693	-0.055170	4.818795
264.896127	8000.439040	13.284698	-0.055113	4.818821
264.638272	8000.460910	13.289703	-0.055065	4.818828
264.762334	8000.438414	13.294707	-0.055089	4.818821
264.768640	8000.466827	13.299712	-0.055090	4.818830
265.169953	8000.333616	13.304717	-0.055165	4.818788
264.815778	8000.404573	13.309722	-0.055100	4.818811
264.793648	8000.421087	13.314727	-0.055096	4.818816
264.833994	8000.432114	13.319731	-0.055104	4.818819
264.714119	8000.500842	13.324736	-0.055082	4.818840
264.493201	8000.411003	13.329741	-0.055041	4.818814
265.019090	8000.396821	13.334746	-0.055139	4.818808
265.117244	8000.388671	13.339751	-0.055158	4.818805
265.015928	8000.416748	13.344755	-0.055139	4.818814
264.602429	8000.386290	13.349760	-0.055063	4.818806
264.552226	8000.451720	13.354765	-0.055054	4.818826
264.796475	8000.462224	13.359770	-0.055100	4.818828
264.847100	8000.448220	13.364775	-0.055109	4.818824
264.926128	8000.403128	13.369779	-0.055124	4.818810
264.952474	8000.424460	13.374784	-0.055130	4.818816
264.450507	8000.400203	13.379789	-0.055037	4.818811
264.498008	8000.515119	13.384794	-0.055046	4.818845
264.622459	8000.493677	13.389799	-0.055069	4.818838
264.568223	8000.461549	13.394803	-0.055060	4.818829
264.381444	8000.430862	13.399808	-0.055025	4.818820
263.904267	8000.457251	13.404813	-0.054937	4.818830
264.016445	8000.357019	13.409818	-0.054958	4.818800
264.179810	8000.497537	13.414823	-0.054989	4.818841
264.344203	8000.501772	13.419827	-0.055020	4.818842
264.198194	8000.409751	13.424832	-0.054993	4.818815
264.447966	8000.399356	13.429837	-0.055039	4.818811
264.420406	8000.484998	13.434842	-0.055035	4.818836
264.727093	8000.418720	13.439847	-0.055092	4.818815
264.734558	8000.437711	13.444851	-0.055094	4.818821
264.490742	8000.527911	13.449856	-0.055049	4.818849
264.629028	8000.490921	13.454861	-0.055075	4.818837
264.355635	8000.423472	13.459866	-0.055024	4.818818
264.266717	8000.427594	13.464871	-0.055008	4.818820
264.727547	8000.460804	13.469875	-0.055094	4.818828
264.720422	8000.501626	13.474880	-0.055093	4.818840
264.499928	8000.485183	13.479885	-0.055053	4.818836
265.102600	8000.457312	13.484890	-0.055165	4.818825
264.626561	8000.495247	13.489895	-0.055077	4.818838
264.576711	8000.512453	13.494899	-0.055068	4.818844
264.726189	8000.399069	13.499904	-0.055096	4.818809
264.228418	8000.486002	13.504909	-0.055004	4.818837
264.260617	8000.399419	13.509914	-0.055010	4.818811
264.202019	8000.505630	13.514919	-0.055000	4.818843
264.178638	8000.505353	13.519923	-0.054996	4.818843
264.174674	8000.421450	13.524928	-0.054995	4.818818
264.086794	8000.510509	13.529933	-0.054979	4.818845
264.326323	8000.395138	13.534938	-0.055024	4.818810
264.477309	8000.487270	13.539943	-0.055052	4.818837
264.650515	8000.443390	13.544947	-0.055085	4.818823
264.665299	8000.489735	13.549952	-0.055088	4.818837
264.560711	8000.449621	13.554957	-0.055069	4.818825
264.769461	8000.482735	13.559962	-0.055108	4.818834
264.380396	8000.402265	13.564967	-0.055036	4.818812
264.545318	8000.487237	13.569971	-0.055067	4.818836
264.723517	8000.491650	13.574976	-0.055101	4.818837
264.027042	8000.448117	13.579981	-0.054971	4.818827
263.981084	8000.251492	13.584986	-0.054963	4.818768
264.040357	8000.446238	13.589991	-0.054974	4.818826
263.530956	8000.352692	13.594995	-0.054880	4.818800
263.826393	8000.341835	13.600000	-0.054935	4.818796
263.561153	8000.460067	13.605005	-0.054886	4.818832
263.465491	8000.362406	13.610010	-0.054869	4.818803
263.972478	8000.531455	13.615015	-0.054964	4.818851
264.199444	8000.420116	13.620019	-0.055006	4.818817
264.110724	8000.427386	13.625024	-0.054990	4.818820
263.957771	8000.530287	13.630029	-0.054962	4.818851
263.985900	8000.401714	13.635034	-0.054967	4.818813
264.127868	8000.525182	13.640039	-0.054994	4.818849
264.441284	8000.355194	13.645043	-0.055053	4.818797
264.541151	8000.374325	13.650048	-0.055072	4.818802
264.278286	8000.525091	13.655053	-0.055023	4.818848
263.653009	8000.454167	13.660058	-0.054907	4.818830
263.949745	8000.453811	13.665063	-0.054963	4.818828
263.870685	8000.418220	13.670067	-0.054948	4.818818
264.283104	8000.525246	13.675072	-0.055025	4.818848
264.197798	8000.485380	13.680077	-0.055010	4.818837
264.100138	8000.456888	13.685082	-0.054992	4.818829
264.158171	8000.519516	13.690087	-0.055003	4.818847
264.572382	8000.511237	13.695091	-0.055081	4.818843
264.221668	8000.356821	13.700096	-0.055016	4.818798
264.069405	8000.532074	13.705101	-0.054988	4.818851
264.242191	8000.353987	13.710106	-0.055020	4.818797
264.122885	8000.432158	13.715111	-0.054998	4.818821
264.306174	8000.456556	13.720115	-0.055033	4.818828
264.265092	8000.468632	13.725120	-0.055025	4.818832
264.129401	8000.542399	13.730125	-0.055001	4.818854
263.846111	8000.323849	13.735130	-0.054948	4.818790
264.024015	8000.404793	13.740135	-0.054982	4.818813
264.207081	8000.545565	13.745139	-0.055016	4.818855
264.380263	8000.426196	13.750144	-0.055049	4.818818
263.931693	8000.452952	13.755149	-0.054965	4.818828
264.107046	8000.439504	13.760154	-0.054998	4.818823
264.057132	8000.459855	13.765159	-0.054989	4.818830
264.420132	8000.509630	13.770163	-0.055057	4.818843
264.567279	8000.508401	13.775168	-0.055085	4.818842
264.534101	8000.462914	13.780173	-0.055079	4.818829
264.679799	8000.456424	13.785178	-0.055107	4.818826
264.280355	8000.421953	13.790183	-0.055033	4.818817
264.683478	8000.468051	13.795187	-0.055108	4.818830
264.827466	8000.523399	13.800192	-0.055135	4.818846
264.903616	8000.417458	13.805197	-0.055150	4.818814
264.448189	8000.389606	13.810202	-0.055065	4.818807
264.589832	8000.508879	13.815207	-0.055092	4.818842
264.382034	8000.405577	13.820211	-0.055054	4.818812
264.415036	8000.449012	13.825216	-0.055060	4.818825
264.606242	8000.487142	13.830221	-0.055096	4.818836
264.584881	8000.426080	13.835226	-0.055092	4.818817
264.928684	8000.451496	13.840231	-0.055157	4.818824
265.127982	8000.340849	13.845235	-0.055194	4.818790
265.142157	8000.411302	13.850240	-0.055197	4.818811
264.993912	8000.389497	13.855245	-0.055170	4.818805
264.670988	8000.483922	13.860250	-0.055110	4.818834
264.670195	8000.467160	13.865255	-0.055110	4.818829
264.499706	8000.370629	13.870259	-0.055079	4.818801
264.682213	8000.491476	13.875264	-0.055113	4.818837
264.605429	8000.471639	13.880269	-0.055099	4.818831
264.237088	8000.532977	13.885274	-0.055031	4.818851
264.168246	8000.452433	13.890279	-0.055019	4.818827
264.200128	8000.441333	13.895283	-0.055025	4.818823
264.835021	8000.489365	13.900288	-0.055143	4.818835
264.789356	8000.425893	13.905293	-0.055135	4.818817
265.275094	8000.378694	13.910298	-0.055226	4.818801
265.307815	8000.420029	13.915303	-0.055232	4.818813
264.463661	8000.458470	13.920307	-0.055076	4.818827
264.593716	8000.550334	13.925312	-0.055100	4.818854
264.827992	8000.468446	13.930317	-0.055144	4.818829
265.182987	8000.402789	13.935322	-0.055211	4.818808
265.101615	8000.443704	13.940327	-0.055196	4.818821
264.882975	8000.429382	13.945331	-0.055155	4.818817
265.300432	8000.444213	13.950336	-0.055234	4.818820
265.311887	8000.416075	13.955341	-0.055236	4.818812
265.309589	8000.440183	13.960346	-0.055236	4.818819
265.002254	8000.444640	13.965351	-0.055179	4.818821
265.171707	8000.462571	13.970355	-0.055211	4.818826
264.432003	8000.464611	13.975360	-0.055074	4.818829
264.022754	8000.372350	13.980365	-0.054998	4.818803
264.417071	8000.426721	13.985370	-0.055071	4.818818
264.399586	8000.410793	13.990375	-0.055068	4.818813
264.364265	8000.543516	13.995379	-0.055062	4.818853
264.930720	8000.503647	14.000384	-0.055168	4.818839
264.419310	8000.415311	14.005389	-0.055073	4.818815
264.364975	8000.463913	14.010394	-0.055063	4.818829
264.807329	8000.506323	14.015399	-0.055146	4.818840
265.204051	8000.427573	14.020403	-0.055220	4.818815
264.986659	8000.505532	14.025408	-0.055180	4.818839
265.082381	8000.398794	14.030413	-0.055198	4.818807
265.101323	8000.394868	14.035418	-0.055202	4.818806
264.765357	8000.502755	14.040423	-0.055140	4.818839
264.675652	8000.499527	14.045427	-0.055124	4.818839
265.215897	8000.485533	14.050432	-0.055225	4.818832
265.284978	8000.445554	14.055437	-0.055238	4.818820
265.192970	8000.478994	14.060442	-0.055221	4.818831
265.271302	8000.445425	14.065447	-0.055236	4.818820
264.945317	8000.374152	14.070451	-0.055175	4.818800
264.883709	8000.524363	14.075456	-0.055164	4.818845
265.018964	8000.477897	14.080461	-0.055190	4.818831
264.920601	8000.515448	14.085466	-0.055172	4.818842
265.200126	8000.455111	14.090471	-0.055224	4.818823
265.281820	8000.389083	14.095475	-0.055240	4.818803
264.993800	8000.406371	14.100480	-0.055187	4.818810
264.947572	8000.473950	14.105485	-0.055178	4.818830
265.354948	8000.390095	14.110490	-0.055254	4.818803
265.637581	8000.309877	14.115495	-0.055307	4.818778
265.505640	8000.375305	14.120499	-0.055283	4.818798
265.197930	8000.486701	14.125504	-0.055226	4.818833
265.104010	8000.415268	14.130509	-0.055209	4.818812
264.956852	8000.479452	14.135514	-0.055182	4.818832
265.381851	8000.443005	14.140519	-0.055262	4.818819
265.394589	8000.407545	14.145523	-0.055264	4.818808
265.487891	8000.371023	14.150528	-0.055282	4.818797
265.078345	8000.416104	14.155533	-0.055206	4.818812
265.404138	8000.429756	14.160538	-0.055267	4.818815
265.228856	8000.445348	14.165543	-0.055235	4.818820
265.341717	8000.367139	14.170547	-0.055256	4.818797
265.295326	8000.399068	14.175552	-0.055248	4.818806
265.244756	8000.457156	14.180557	-0.055239	4.818824
265.607430	8000.397889	14.185562	-0.055307	4.818805
265.412440	8000.422664	14.190567	-0.055271	4.818813
265.484431	8000.359656	14.195571	-0.055284	4.818794
265.638808	8000.410945	14.200576	-0.055313	4.818808
265.609731	8000.353976	14.205581	-0.055308	4.818792
265.245904	8000.420615	14.210586	-0.055241	4.818813
265.573933	8000.296945	14.215591	-0.055302	4.818775
265.488382	8000.401764	14.220595	-0.055287	4.818806
264.977515	8000.525224	14.225600	-0.055192	4.818845
265.214324	8000.430787	14.230605	-0.055236	4.818816
265.197118	8000.477770	14.235610	-0.055234	4.818830
265.371276	8000.461162	14.240615	-0.055266	4.818824
264.952626	8000.465235	14.245619	-0.055189	4.818827
265.452209	8000.444427	14.250624	-0.055282	4.818819
265.446058	8000.446468	14.255629	-0.055281	4.818820
265.397966	8000.515072	14.260634	-0.055273	4.818840
265.104290	8000.516558	14.265639	-0.055218	4.818842
265.366155	8000.359535	14.270643	-0.055267	4.818794
265.112786	8000.364686	14.275648	-0.055221	4.818797
264.916258	8000.439767	14.280653	-0.055184	4.818820
265.239015	8000.437653	14.285658	-0.055245	4.818818
265.588585	8000.342569	14.290663	-0.055310	4.818788
265.748629	8000.301665	14.295667	-0.055340	4.818775
265.930557	8000.326048	14.300672	-0.055374	4.818782
265.614457	8000.334585	14.305677	-0.055316	4.818786
265.309672	8000.418758	14.310682	-0.055260	4.818812
265.674334	8000.427669	14.315687	-0.055328	4.818813
264.841606	8000.517630	14.320691	-0.055173	4.818843
265.159855	8000.478761	14.325696	-0.055233	4.818830
264.955543	8000.502367	14.330701	-0.055195	4.818838
265.077247	8000.420079	14.335706	-0.055218	4.818813
265.172013	8000.504151	14.340711	-0.055236	4.818838
265.058505	8000.430369	14.345715	-0.055215	4.818816
264.616546	8000.544232	14.350720	-0.055133	4.818852
264.445482	8000.507455	14.355725	-0.055102	4.818842
264.808095	8000.383182	14.360730	-0.055170	4.818803
264.894200	8000.449318	14.365735	-0.055186	4.818822
264.941898	8000.433180	14.370739	-0.055195	4.818817
265.012096	8000.478142	14.375744	-0.055209	4.818831
265.021195	8000.419568	14.380749	-0.055211	4.818813
265.463163	8000.392776	14.385754	-0.055293	4.818803
264.976166	7999.354873	14.390759	-0.055202	4.818496

264.745980	7996.246891	14.395763	-0.055158	4.817571
265.116065	7990.671967	14.400768	-0.055223	4.815909
264.666266	7984.073666	14.405773	-0.055136	4.813945
264.338245	7976.903884	14.410778	-0.055070	4.811808
264.813012	7969.205073	14.415783	-0.055154	4.809510
264.767198	7961.414664	14.420787	-0.055141	4.807186
264.358337	7953.539111	14.425792	-0.055060	4.804836
264.484224	7945.584926	14.430797	-0.055078	4.802459
264.658057	7937.592363	14.435802	-0.055106	4.800070
264.889468	7929.683698	14.440807	-0.055144	4.797704
264.420069	7921.604237	14.445811	-0.055052	4.795289
264.027523	7913.708183	14.450816	-0.054974	4.792927
264.333884	7905.628659	14.455821	-0.055026	4.790506
264.197122	7897.565180	14.460826	-0.054996	4.788091
264.192030	7889.524872	14.465831	-0.054990	4.785681
264.155263	7881.574686	14.470835	-0.054978	4.783296
264.379276	7873.609197	14.475840	-0.055015	4.780905
264.214125	7865.550308	14.480845	-0.054979	4.778486
264.563740	7857.612641	14.485850	-0.055040	4.776101
264.463700	7849.536534	14.490855	-0.055016	4.773675
264.691319	7841.528783	14.495859	-0.055053	4.771266
264.782172	7833.553878	14.500864	-0.055066	4.768867
263.940674	7825.670316	14.505869	-0.054904	4.766496
264.204204	7817.499745	14.510874	-0.054948	4.764035
264.132317	7809.666193	14.515879	-0.054930	4.761675
264.524190	7801.571074	14.520883	-0.054998	4.759234
264.069810	7793.654428	14.525888	-0.054909	4.756848
263.641286	7785.550771	14.530893	-0.054824	4.754404
263.656288	7777.630523	14.535898	-0.054822	4.752013
263.690853	7769.569739	14.540903	-0.054823	4.749578
263.619288	7761.502003	14.545907	-0.054805	4.747140
263.595990	7753.528588	14.550912	-0.054796	4.744729
263.787839	7745.530762	14.555917	-0.054827	4.742309
264.081319	7737.486051	14.560922	-0.054877	4.739874
263.766506	7729.551818	14.565927	-0.054813	4.737471
263.760438	7721.506187	14.570931	-0.054807	4.735034
263.661721	7713.560946	14.575936	-0.054784	4.732626
263.841699	7705.496869	14.580941	-0.054812	4.730179
263.668743	7697.564550	14.585946	-0.054775	4.727773
264.059539	7689.507764	14.590951	-0.054843	4.725326
263.487433	7681.573355	14.595955	-0.054732	4.722917
264.071122	7673.525709	14.600960	-0.054836	4.720470
263.590943	7665.584732	14.605965	-0.054741	4.718056
263.376302	7657.601006	14.610970	-0.054697	4.715627
263.995818	7649.542074	14.615975	-0.054807	4.713174
263.940730	7641.511960	14.620979	-0.054792	4.710728
263.490618	7633.603292	14.625984	-0.054703	4.708319
262.840171	7625.633595	14.630989	-0.054577	4.705890
262.899518	7617.551103	14.635994	-0.054583	4.703424
263.230143	7609.530006	14.640999	-0.054640	4.700976
263.581264	7601.424104	14.646003	-0.054700	4.698501
263.323047	7593.517688	14.651008	-0.054648	4.696086
262.947618	7585.536489	14.656013	-0.054573	4.693646
263.130122	7577.536563	14.661018	-0.054602	4.691200
263.592331	7569.465946	14.666023	-0.054683	4.688730
263.658440	7561.442362	14.671027	-0.054691	4.686273
263.697764	7553.489147	14.676032	-0.054693	4.683837
263.911255	7545.543441	14.681037	-0.054728	4.681402
263.466693	7537.516211	14.686042	-0.054640	4.678941
263.493734	7529.591748	14.691047	-0.054640	4.676510
263.010282	7521.552795	14.696051	-0.054546	4.674043
263.129565	7513.501657	14.701056	-0.054563	4.671570
263.342966	7505.424354	14.706061	-0.054598	4.669088
263.317207	7497.472933	14.711066	-0.054588	4.666644
263.297154	7489.455685	14.716071	-0.054579	4.664177
262.805831	7481.599743	14.721075	-0.054483	4.661760
262.885248	7473.508922	14.726080	-0.054493	4.659268
262.670067	7465.567300	14.731085	-0.054448	4.656822
262.692382	7457.458757	14.736090	-0.054447	4.654322
262.669944	7449.494246	14.741095	-0.054438	4.651866
262.806221	7441.378088	14.746099	-0.054459	4.649361
262.599565	7433.523326	14.751104	-0.054415	4.646936
262.371683	7425.460592	14.756109	-0.054368	4.644445
262.221318	7417.585974	14.761114	-0.054335	4.642012
262.145550	7409.528723	14.766119	-0.054316	4.639520
262.176313	7401.446410	14.771123	-0.054317	4.637019
262.583192	7393.398011	14.776128	-0.054388	4.634528
262.327323	7385.472020	14.781133	-0.054335	4.632073
262.350163	7377.453035	14.786138	-0.054335	4.629588
262.210553	7369.476997	14.791143	-0.054304	4.627114
262.438185	7361.338331	14.796147	-0.054341	4.624590
262.115789	7353.527328	14.801152	-0.054277	4.622165
261.938545	7345.457825	14.806157	-0.054239	4.619658
262.327745	7337.408049	14.811162	-0.054306	4.617157
261.824527	7329.484967	14.816167	-0.054208	4.614693
261.874503	7321.459997	14.821171	-0.054212	4.612197
261.861852	7313.453635	14.826176	-0.054205	4.609705
261.663413	7305.429299	14.831181	-0.054163	4.607206
261.711138	7297.396359	14.836186	-0.054167	4.604703
261.300681	7289.549975	14.841191	-0.054086	4.602256
261.276782	7281.388983	14.846195	-0.054076	4.599711
261.604274	7273.469873	14.851200	-0.054133	4.597240
261.626717	7265.384489	14.856205	-0.054132	4.594715
261.428629	7257.484491	14.861210	-0.054090	4.592246
261.175080	7249.359483	14.866215	-0.054038	4.589706
261.208609	7241.355247	14.871219	-0.054039	4.587202
261.270395	7233.354216	14.876224	-0.054046	4.584698
261.612376	7225.389778	14.881229	-0.054105	4.582205
261.608337	7217.347973	14.886234	-0.054099	4.579686
261.281152	7209.438089	14.891239	-0.054033	4.577206
261.335112	7201.315209	14.896243	-0.054038	4.574658
261.675265	7193.393848	14.901248	-0.054097	4.572173
261.078325	7185.368786	14.906253	-0.053981	4.569652
261.477938	7177.397988	14.911258	-0.054050	4.567149
261.294210	7169.347270	14.916263	-0.054011	4.564618
261.300947	7161.378078	14.921267	-0.054008	4.562111
261.616772	7153.341480	14.926272	-0.054062	4.559583
261.270104	7145.421472	14.931277	-0.053992	4.557089
261.237654	7137.345893	14.936282	-0.053981	4.554545
261.427512	7129.363127	14.941287	-0.054012	4.552029
261.691309	7121.310851	14.946291	-0.054056	4.549490
261.668680	7113.363360	14.951296	-0.054047	4.546982
261.447738	7105.301412	14.956301	-0.054001	4.544436
261.487272	7097.340533	14.961306	-0.054003	4.541921
261.361001	7089.355954	14.966311	-0.053975	4.539397
261.162453	7081.400238	14.971315	-0.053933	4.536881
261.467965	7073.338657	14.976320	-0.053985	4.534331
261.265372	7065.363353	14.981325	-0.053943	4.531805
261.136273	7057.273622	14.986330	-0.053914	4.529242
261.143684	7049.328935	14.991335	-0.053910	4.526724
261.707799	7041.162470	14.996339	-0.054010	4.524135
261.782809	7033.342984	15.001344	-0.054019	4.521654
261.489080	7025.305627	15.006349	-0.053960	4.519101
261.490645	7017.376798	15.011354	-0.053955	4.516583
261.318438	7009.335519	15.016359	-0.053918	4.514026
260.923783	7001.353400	15.021363	-0.053840	4.511486
261.281559	6993.299605	15.026368	-0.053902	4.508924
261.210273	6985.286642	15.031373	-0.053884	4.506373
261.404153	6977.225134	15.036378	-0.053915	4.503805
261.572821	6969.308476	15.041383	-0.053941	4.501282
261.140828	6961.297887	15.046387	-0.053856	4.498726
261.280779	6953.270224	15.051392	-0.053877	4.496164
260.882959	6945.271496	15.056397	-0.053798	4.493609
261.326706	6937.213905	15.061402	-0.053876	4.491036
261.519619	6929.226523	15.066407	-0.053907	4.488484
261.212413	6921.229752	15.071411	-0.053845	4.485925
261.942268	6913.217881	15.076416	-0.053976	4.483364
261.601555	6905.243424	15.081421	-0.053908	4.480809
261.276126	6897.273446	15.086426	-0.053842	4.478253
261.680849	6889.257024	15.091431	-0.053913	4.475685
262.248914	6881.160025	15.096435	-0.054014	4.473091
261.762761	6873.248983	15.101440	-0.053918	4.470549
261.608832	6865.194921	15.106445	-0.053885	4.467962
261.350170	6857.273413	15.111450	-0.053832	4.465415
261.394023	6849.328701	15.116455	-0.053835	4.462861
261.116191	6841.247882	15.121459	-0.053778	4.460260
260.750712	6833.320626	15.126464	-0.053705	4.457707
261.027978	6825.230097	15.131469	-0.053752	4.455103
261.006069	6817.264164	15.136474	-0.053743	4.452535
261.139862	6809.191949	15.141479	-0.053763	4.449933
261.254821	6801.141158	15.146483	-0.053780	4.447336
260.866951	6793.241505	15.151488	-0.053703	4.444784
260.526404	6785.286826	15.156493	-0.053634	4.442213
260.638256	6777.218272	15.161498	-0.053650	4.439606
260.971652	6769.228843	15.166503	-0.053708	4.437024
260.926612	6761.142391	15.171507	-0.053694	4.434407
260.695297	6753.251938	15.176512	-0.053646	4.431851
260.323417	6745.229866	15.181517	-0.053572	4.429250
260.720967	6737.167265	15.186522	-0.053641	4.426639
260.582704	6729.158314	15.191527	-0.053611	4.424040
260.280433	6721.248460	15.196531	-0.053550	4.421471
260.594530	6713.204228	15.201536	-0.053603	4.418861
260.298181	6705.219137	15.206541	-0.053543	4.416265
260.738848	6697.165585	15.211546	-0.053620	4.413649
260.579403	6689.235418	15.216551	-0.053586	4.411069
260.446324	6681.212613	15.221555	-0.053556	4.408456
260.792938	6673.181555	15.226560	-0.053616	4.405843
260.528446	6665.196705	15.231565	-0.053562	4.403239
260.282379	6657.299602	15.236570	-0.053511	4.400663
260.050905	6649.274929	15.241575	-0.053463	4.398043
260.510709	6641.187755	15.246579	-0.053544	4.395406
260.840828	6633.213938	15.251584	-0.053600	4.392803
260.435824	6625.187154	15.256589	-0.053520	4.390177
260.395194	6617.225591	15.261594	-0.053508	4.387573
260.303493	6609.214523	15.266599	-0.053486	4.384951
260.242418	6601.270557	15.271603	-0.053469	4.382349
260.131137	6593.292395	15.276608	-0.053444	4.379735
260.530187	6585.212934	15.281613	-0.053513	4.377089
260.119428	6577.303153	15.286618	-0.053432	4.374491
260.297268	6569.303652	15.291623	-0.053460	4.371867
260.118804	6561.223584	15.296627	-0.053422	4.369212
260.394107	6553.304659	15.301632	-0.053468	4.366612
259.943768	6545.281271	15.306637	-0.053380	4.363970
260.266403	6537.282502	15.311642	-0.053435	4.361341
260.399076	6529.252937	15.316647	-0.053455	4.358698
260.079257	6521.282151	15.321651	-0.053390	4.356070
260.119735	6513.298512	15.326656	-0.053393	4.353439
260.080923	6505.176756	15.331661	-0.053381	4.350760
259.962122	6497.251049	15.336666	-0.053354	4.348143
259.543347	6489.273952	15.341671	-0.053271	4.345506
259.638771	6481.243303	15.346675	-0.053284	4.342853
260.123179	6473.229871	15.351680	-0.053369	4.340208
260.065544	6465.254111	15.356685	-0.053354	4.337569
260.201086	6457.198367	15.361690	-0.053374	4.334903
259.853995	6449.331869	15.366695	-0.053304	4.332295
259.981674	6441.224914	15.371699	-0.053323	4.329609
259.559866	6433.306110	15.376704	-0.053240	4.326979
259.817229	6425.190807	15.381709	-0.053283	4.324288
259.624311	6417.273322	15.386714	-0.053242	4.321658
259.824099	6409.222922	15.391719	-0.053274	4.318984
260.416026	6401.187018	15.396723	-0.053380	4.316318
260.109827	6393.269287	15.401728	-0.053318	4.313681
260.041409	6385.230278	15.406733	-0.053300	4.311005
259.346071	6377.309368	15.411738	-0.053166	4.308361
259.521672	6369.290839	15.416743	-0.053194	4.305690
259.780073	6361.178608	15.421747	-0.053237	4.302987
259.824301	6353.246445	15.426752	-0.053240	4.300340
259.847413	6345.224388	15.431757	-0.053240	4.297662
259.436095	6337.235103	15.436762	-0.053158	4.294989
259.559446	6329.234356	15.441767	-0.053176	4.292315
259.715395	6321.111698	15.446771	-0.053201	4.289599
259.488047	6313.263111	15.451776	-0.053153	4.286970
259.312870	6305.194338	15.456781	-0.053116	4.284266
259.237834	6297.264785	15.461786	-0.053097	4.281607
259.241287	6289.230933	15.466791	-0.053093	4.278913
259.226595	6281.261260	15.471795	-0.053085	4.276238
259.236388	6273.212228	15.476800	-0.053082	4.273536
259.133775	6265.197573	15.481805	-0.053058	4.270842
259.069228	6257.205472	15.486810	-0.053041	4.268154
259.099817	6249.172959	15.491815	-0.053042	4.265452
258.570772	6241.226122	15.496819	-0.052939	4.262771
258.736477	6233.190541	15.501824	-0.052965	4.260066
258.938010	6225.157999	15.506829	-0.052997	4.257361
258.742319	6217.186934	15.511834	-0.052956	4.254670
259.202885	6209.166782	15.516839	-0.053037	4.251968
259.069588	6201.116161	15.521843	-0.053007	4.249248
259.189324	6193.190398	15.526848	-0.053025	4.246571
258.625091	6185.192076	15.531853	-0.052915	4.243860
258.883214	6177.189080	15.536858	-0.052958	4.241155
258.869018	6169.205187	15.541863	-0.052950	4.238451
258.320901	6161.258031	15.546867	-0.052843	4.235753
259.157267	6153.099947	15.551872	-0.052994	4.232996
259.409255	6145.083318	15.556877	-0.053036	4.230280
259.311013	6137.137273	15.561882	-0.053013	4.227581
258.957359	6129.207382	15.566887	-0.052942	4.224884
258.810133	6121.221800	15.571891	-0.052910	4.222168
258.859553	6113.198267	15.576896	-0.052915	4.219440
259.106250	6105.144057	15.581901	-0.052956	4.216701
259.341878	6097.131094	15.586906	-0.052995	4.213975
259.203775	6089.196149	15.591911	-0.052964	4.211270
259.143966	6081.130108	15.596915	-0.052948	4.208519
259.486377	6073.132624	15.601920	-0.053007	4.205794
259.587208	6065.106346	15.606925	-0.053021	4.203055
259.648105	6057.142353	15.611930	-0.053027	4.200334
259.690645	6049.175915	15.616935	-0.053030	4.197611
259.603764	6041.179876	15.621939	-0.053009	4.194875
259.534851	6033.140153	15.626944	-0.052991	4.192122
259.509474	6025.079626	15.631949	-0.052982	4.189360
259.241434	6017.150408	15.636954	-0.052927	4.186639
259.416583	6009.126191	15.641959	-0.052955	4.183889
259.154670	6001.212723	15.646963	-0.052901	4.181170
258.624043	5993.261404	15.651968	-0.052798	4.178433
258.956585	5985.156497	15.656973	-0.052855	4.175651
258.922351	5977.119101	15.661978	-0.052843	4.172887
258.900840	5969.166398	15.666983	-0.052834	4.170150
259.114434	5961.108850	15.671987	-0.052869	4.167378
259.400222	5953.091070	15.676992	-0.052918	4.164618
259.068087	5945.210786	15.681997	-0.052851	4.161897
258.695813	5937.218795	15.687002	-0.052777	4.159135
258.487589	5929.302995	15.692007	-0.052733	4.156399
258.344281	5921.208507	15.697011	-0.052702	4.153600
258.224506	5913.246836	15.702016	-0.052674	4.150846
258.782697	5905.111505	15.707021	-0.052773	4.148039
258.782504	5897.116274	15.712026	-0.052768	4.145271
258.550795	5889.233432	15.717031	-0.052721	4.142537
258.308928	5881.184334	15.722035	-0.052671	4.139743
258.615728	5873.218560	15.727040	-0.052723	4.136984
258.786802	5865.131083	15.732045	-0.052750	4.134179
258.498795	5857.195409	15.737050	-0.052691	4.131418
258.772414	5849.181207	15.742055	-0.052737	4.128636
258.357474	5841.178776	15.747059	-0.052655	4.125847
258.548349	5833.197415	15.752064	-0.052686	4.123072
258.508269	5825.213515	15.757069	-0.052674	4.120290
259.042762	5817.149394	15.762074	-0.052768	4.117487
258.945828	5809.174062	15.767079	-0.052745	4.114704
258.775521	5801.225911	15.772083	-0.052709	4.111928
258.724006	5793.163116	15.777088	-0.052694	4.109111
258.781909	5785.186254	15.782093	-0.052700	4.106324
258.408359	5777.177119	15.787098	-0.052626	4.103518
258.716700	5769.183043	15.792103	-0.052678	4.100724
258.656442	5761.148028	15.797107	-0.052662	4.097910
258.710084	5753.161038	15.802112	-0.052667	4.095111
258.468537	5745.199808	15.807117	-0.052617	4.092316
258.451429	5737.111998	15.812122	-0.052609	4.089477
258.651635	5729.189526	15.817127	-0.052642	4.086698
258.337578	5721.144018	15.822131	-0.052578	4.083866
258.491961	5713.221893	15.827136	-0.052602	4.081083
258.194339	5705.218861	15.832141	-0.052542	4.078262
258.007001	5697.241586	15.837146	-0.052502	4.075450
257.636746	5689.271576	15.842151	-0.052429	4.072636
257.761138	5681.168138	15.847155	-0.052447	4.069780
257.779569	5673.196107	15.852160	-0.052445	4.066967
257.902286	5665.114568	15.857165	-0.052463	4.064115
258.240045	5657.181137	15.862170	-0.052521	4.061317
258.286698	5649.169655	15.867175	-0.052525	4.058485
258.039798	5641.196132	15.872179	-0.052474	4.055659
258.279733	5633.180219	15.877184	-0.052514	4.052824
258.273397	5625.150860	15.882189	-0.052508	4.049979
258.397592	5617.148589	15.887194	-0.052526	4.047143
258.633507	5609.113435	15.892199	-0.052565	4.044296
258.453004	5601.226579	15.897203	-0.052527	4.041492
258.507237	5593.205526	15.902208	-0.052532	4.038643
258.316606	5585.255686	15.907213	-0.052492	4.035813
258.396363	5577.202667	15.912218	-0.052502	4.032948
258.041357	5569.187589	15.917223	-0.052431	4.030088
258.295212	5561.138877	15.922227	-0.052473	4.027224
258.518388	5553.135718	15.927232	-0.052510	4.024374
258.298243	5545.205118	15.932237	-0.052464	4.021540
258.030495	5537.222132	15.937242	-0.052409	4.018684
257.850062	5529.285379	15.942247	-0.052371	4.015845
258.236972	5521.156557	15.947251	-0.052438	4.012944
258.016429	5513.182527	15.952256	-0.052392	4.010087
258.005851	5505.219992	15.957261	-0.052385	4.007235
258.051075	5497.182978	15.962266	-0.052389	4.004355
257.867865	5489.306243	15.967271	-0.052350	4.001527
257.854690	5481.240039	15.972275	-0.052342	3.998631
258.012216	5473.273109	15.977280	-0.052367	3.995773
257.665813	5465.247680	15.982285	-0.052297	3.992882
257.578283	5457.219957	15.987290	-0.052276	3.989993
257.376522	5449.276500	15.992295	-0.052234	3.987130
257.714757	5441.154677	15.997299	-0.052292	3.984210
257.593680	5433.325337	16.002304	-0.052265	3.981386
257.544875	5425.236770	16.007309	-0.052251	3.978467
257.615251	5417.176779	16.012314	-0.052259	3.975559
257.702483	5409.241035	16.017319	-0.052270	3.972693
257.331330	5401.220828	16.022323	-0.052196	3.969787
257.258070	5393.255532	16.027328	-0.052178	3.966904
257.191780	5385.214691	16.032333	-0.052160	3.963991
257.278512	5377.257321	16.037338	-0.052172	3.961110
257.261420	5369.322174	16.042343	-0.052164	3.958232
256.999463	5361.286604	16.047347	-0.052110	3.955311
256.745785	5353.288463	16.052352	-0.052058	3.952402
256.956001	5345.200357	16.057357	-0.052092	3.949467
257.130110	5337.196418	16.062362	-0.052120	3.946560
256.464839	5329.307780	16.067367	-0.051991	3.943676
256.230147	5321.312002	16.072371	-0.051942	3.940759
256.937748	5313.198623	16.077376	-0.052069	3.937816
257.226263	5305.195087	16.082381	-0.052118	3.934902
257.285317	5297.211127	16.087386	-0.052124	3.931989
257.220077	5289.184939	16.092391	-0.052107	3.929056
256.573220	5281.282633	16.097395	-0.051982	3.926154
256.959320	5273.235193	16.102400	-0.052049	3.923218
256.871846	5265.258927	16.107405	-0.052028	3.920296
257.001793	5257.222506	16.112410	-0.052047	3.917354
257.066242	5249.246657	16.117415	-0.052054	3.914431
257.020670	5241.259709	16.122419	-0.052041	3.911499
257.152033	5233.245410	16.127424	-0.052060	3.908559
256.929336	5225.258004	16.132429	-0.052014	3.905619
257.095109	5217.247920	16.137434	-0.052040	3.902677
257.227126	5209.286358	16.142439	-0.052060	3.899749
257.035202	5201.301889	16.147443	-0.052019	3.896805
257.286691	5193.277971	16.152448	-0.052061	3.893852
256.894326	5185.330286	16.157453	-0.051983	3.890913
257.131560	5177.270193	16.162458	-0.052022	3.887942
256.859936	5169.346679	16.167463	-0.051967	3.885009
256.520981	5161.379007	16.172467	-0.051899	3.882056
257.006197	5153.284514	16.177472	-0.051985	3.879071
257.015441	5145.355119	16.182477	-0.051981	3.876136
256.717684	5137.300825	16.187482	-0.051921	3.873145
256.525043	5129.229268	16.192487	-0.051880	3.870147
256.470313	5121.276464	16.197491	-0.051865	3.867194
256.221964	5113.275259	16.202496	-0.051814	3.864217
255.885132	5105.397052	16.207501	-0.051747	3.861282
256.268354	5097.258855	16.212506	-0.051813	3.858262
256.460855	5089.276995	16.217511	-0.051844	3.855295
256.589538	5081.272223	16.222515	-0.051863	3.852315
256.374188	5073.281811	16.227520	-0.051818	3.849331
256.648832	5065.266699	16.232525	-0.051864	3.846346
256.084188	5057.363475	16.237530	-0.051754	3.843383
256.561438	5049.314607	16.242535	-0.051838	3.840385
256.411075	5041.349557	16.247539	-0.051806	3.837402
256.415787	5033.329944	16.252544	-0.051801	3.834401
256.407804	5025.344857	16.257549	-0.051795	3.831409
256.297409	5017.345451	16.262554	-0.051770	3.828408
256.529539	5009.291240	16.267559	-0.051808	3.825391
256.469976	5001.304744	16.272563	-0.051792	3.822391
256.521996	4993.309565	16.277568	-0.051797	3.819387
256.628003	4985.338990	16.282573	-0.051812	3.816392
256.318552	4977.369818	16.287578	-0.051749	3.813385
256.078664	4969.361443	16.292583	-0.051700	3.810363
256.128600	4961.332848	16.297587	-0.051704	3.807338
255.930469	4953.392710	16.302592	-0.051662	3.804338
255.746247	4945.453120	16.307597	-0.051623	3.801336
255.634976	4937.427057	16.312602	-0.051598	3.798300
256.118256	4929.361868	16.317607	-0.051683	3.795261
255.768571	4921.383116	16.322611	-0.051613	3.792233
255.573816	4913.354360	16.327616	-0.051572	3.789187
255.408808	4905.419209	16.332621	-0.051536	3.786175
255.096564	4897.439564	16.337626	-0.051473	3.783140
255.182522	4889.411211	16.342631	-0.051484	3.780094
255.429487	4881.370187	16.347635	-0.051525	3.777044
255.580981	4873.360423	16.352640	-0.051549	3.774001
255.649691	4865.364729	16.357645	-0.051557	3.770959
255.454663	4857.398675	16.362650	-0.051515	3.767920
255.978815	4849.340369	16.367655	-0.051608	3.764861
255.588222	4841.470022	16.372659	-0.051531	3.761848
255.853428	4833.434414	16.377664	-0.051575	3.758786
255.515944	4825.480521	16.382669	-0.051507	3.755738
255.419020	4817.472121	16.387674	-0.051484	3.752673
255.532821	4809.445347	16.392679	-0.051501	3.749603
255.480473	4801.433376	16.397683	-0.051486	3.746532
255.836159	4793.370672	16.402688	-0.051547	3.743449
255.881645	4785.415913	16.407693	-0.051551	3.740398
255.690789	4777.455388	16.412698	-0.051511	3.737336
255.835390	4769.469021	16.417703	-0.051533	3.734270
255.495290	4761.506292	16.422707	-0.051464	3.731198
255.399249	4753.500204	16.427712	-0.051442	3.728113
255.789900	4745.417711	16.432717	-0.051510	3.725008
255.950592	4737.414433	16.437722	-0.051535	3.721926
255.763763	4729.478745	16.442727	-0.051495	3.718858
255.702165	4721.512289	16.447731	-0.051479	3.715780
255.749524	4713.449152	16.452736	-0.051483	3.712663
255.812121	4705.411106	16.457741	-0.051489	3.709555
255.621054	4697.413701	16.462746	-0.051449	3.706453
255.741155	4689.465771	16.467751	-0.051466	3.703375
255.569679	4681.470044	16.472755	-0.051430	3.700269
255.589551	4673.520422	16.477760	-0.051428	3.697184
255.546584	4665.485318	16.482765	-0.051416	3.694060
255.684363	4657.479249	16.487770	-0.051436	3.690951
255.205717	4649.541949	16.492775	-0.051342	3.687849
255.307863	4641.491721	16.497779	-0.051356	3.684715
255.446102	4633.533870	16.502784	-0.051377	3.681616
255.392404	4625.533482	16.507789	-0.051362	3.678493
255.298906	4617.541863	16.512794	-0.051340	3.675370
255.270267	4609.597309	16.517799	-0.051330	3.672263
255.254974	4601.514984	16.522803	-0.051322	3.669101
254.883796	4593.651684	16.527808	-0.051248	3.666012
255.211292	4585.551359	16.532813	-0.051304	3.662847
254.863606	4577.600585	16.537818	-0.051235	3.659719
255.184632	4569.590004	16.542823	-0.051290	3.656583
255.133739	4561.559091	16.547827	-0.051275	3.653427
255.328245	4553.558318	16.552832	-0.051307	3.650286
255.510509	4545.559664	16.557837	-0.051336	3.647143
255.448310	4537.532872	16.562842	-0.051319	3.643979
255.253766	4529.668133	16.567847	-0.051278	3.640873
255.353241	4521.602599	16.572851	-0.051292	3.637694
255.303437	4513.612428	16.577856	-0.051278	3.634537
255.277627	4505.645665	16.582861	-0.051268	3.631387
255.054357	4497.627452	16.587866	-0.051222	3.628208
254.848519	4489.643485	16.592871	-0.051178	3.625041
254.836523	4481.644716	16.597875	-0.051171	3.621871
255.252955	4473.569216	16.602880	-0.051244	3.618679
255.289146	4465.590371	16.607885	-0.051246	3.615513
254.966544	4457.650916	16.612890	-0.051181	3.612348
255.050884	4449.643344	16.617895	-0.051192	3.609166
255.060638	4441.642775	16.622899	-0.051189	3.605982
255.023381	4433.645675	16.627904	-0.051177	3.602795
254.913032	4425.670444	16.632909	-0.051151	3.599611
254.968357	4417.719025	16.637914	-0.051157	3.596439
254.631827	4409.754379	16.642919	-0.051089	3.593247
254.865398	4401.655559	16.647923	-0.051128	3.590016
254.445059	4393.720949	16.652928	-0.051045	3.586828
254.582000	4385.677243	16.657933	-0.051065	3.583610
254.410868	4377.710438	16.662938	-0.051029	3.580411
254.075091	4369.815280	16.667943	-0.050961	3.577233
254.330124	4361.699534	16.672947	-0.051004	3.573981
254.205763	4353.738413	16.677952	-0.050976	3.570777
254.133398	4345.764285	16.682957	-0.050958	3.567566
254.042212	4337.718213	16.687962	-0.050936	3.564323
254.177507	4329.793148	16.692967	-0.050956	3.561133
253.615357	4321.836171	16.697971	-0.050847	3.557905
253.490492	4313.831670	16.702976	-0.050818	3.554669
253.202659	4305.823827	16.707981	-0.050760	3.551424
253.132477	4297.757384	16.712986	-0.050742	3.548158
253.154531	4289.738318	16.717991	-0.050741	3.544911
253.539885	4281.657014	16.722995	-0.050808	3.541648
253.899770	4273.681874	16.728000	-0.050870	3.538424
253.487767	4265.775946	16.733005	-0.050789	3.535201
253.576629	4257.786313	16.738010	-0.050800	3.531956
253.550500	4249.798362	16.743015	-0.050791	3.528706
253.170154	4241.814779	16.748019	-0.050715	3.525443
253.415279	4233.820454	16.753024	-0.050756	3.522193
254.265201	4225.688815	16.758029	-0.050909	3.518903
253.715235	4217.821198	16.763034	-0.050802	3.515673
253.872134	4209.831290	16.768039	-0.050826	3.512413
253.970209	4201.799218	16.773043	-0.050839	3.509130
253.910256	4193.819147	16.778048	-0.050823	3.505861
253.737656	4185.867678	16.783053	-0.050786	3.502596
253.736318	4177.847698	16.788058	-0.050781	3.499306
253.476305	4169.937981	16.793063	-0.050728	3.496050
253.845363	4161.834352	16.798067	-0.050792	3.492732
253.367880	4153.901702	16.803072	-0.050698	3.489453
253.600478	4145.863588	16.808077	-0.050737	3.486151
253.483831	4137.883835	16.813082	-0.050710	3.482858
253.724016	4129.908590	16.818087	-0.050750	3.479576
253.486785	4121.971849	16.823091	-0.050701	3.476290
253.140653	4113.966250	16.828096	-0.050632	3.472970
253.187021	4105.968983	16.833101	-0.050635	3.469663
253.534548	4097.886956	16.838106	-0.050695	3.466327
253.778088	4089.866215	16.843111	-0.050736	3.463011
253.677776	4081.882717	16.848115	-0.050712	3.459695
253.475680	4073.960361	16.853120	-0.050670	3.456398
253.009081	4066.038906	16.858125	-0.050578	3.453089
253.276635	4057.931224	16.863130	-0.050623	3.449724
253.260908	4049.988105	16.868135	-0.050615	3.446415
253.581524	4041.959636	16.873139	-0.050670	3.443079
253.839634	4033.960445	16.878144	-0.050713	3.439750
253.729705	4026.022683	16.883149	-0.050688	3.436430
253.770306	4018.003963	16.888154	-0.050690	3.433079
253.598418	4010.043637	16.893159	-0.050653	3.429741
253.317870	4002.072695	16.898163	-0.050596	3.426392
252.971645	3994.093623	16.903168	-0.050527	3.423033
253.299920	3986.077631	16.908173	-0.050583	3.419680
253.211991	3978.066614	16.913178	-0.050562	3.416311
253.066676	3970.081755	16.918183	-0.050530	3.412947
252.808870	3962.102521	16.923187	-0.050477	3.409578
253.203077	3954.074396	16.928192	-0.050546	3.406209
252.946144	3946.100629	16.933197	-0.050493	3.402836
252.817829	3938.131300	16.938202	-0.050464	3.399466
252.758527	3930.197250	16.943207	-0.050448	3.396110
252.777729	3922.079973	16.948211	-0.050447	3.392677
252.816103	3914.068718	16.953216	-0.050449	3.389285
253.143056	3906.078875	16.958221	-0.050505	3.385909
252.867308	3898.098897	16.963226	-0.050449	3.382513
253.103186	3890.104091	16.968231	-0.050488	3.379125
252.936678	3882.141089	16.973235	-0.050452	3.375733
253.049063	3874.129677	16.978240	-0.050468	3.372326
252.936921	3866.142941	16.983245	-0.050443	3.368919
252.965284	3858.154999	16.988250	-0.050443	3.365513
252.835111	3850.229934	16.993255	-0.050414	3.362124
253.251669	3842.170794	16.998259	-0.050487	3.358695
252.944419	3834.261347	17.003264	-0.050425	3.355300
252.841494	3826.268469	17.008269	-0.050401	3.351873
252.851165	3818.224385	17.013274	-0.050397	3.348425
252.788698	3810.251682	17.018279	-0.050381	3.345001
252.313113	3802.323079	17.023283	-0.050288	3.341577
252.560515	3794.284168	17.028288	-0.050329	3.338129
252.575798	3786.283541	17.033293	-0.050327	3.334685
252.546362	3778.274891	17.038298	-0.050316	3.331233
252.755849	3770.260424	17.043303	-0.050350	3.327784
252.374966	3762.310700	17.048307	-0.050275	3.324336
252.342960	3754.362612	17.053312	-0.050264	3.320899
252.501534	3746.373166	17.058317	-0.050289	3.317448
252.493817	3738.327006	17.063322	-0.050282	3.313962
252.390165	3730.377144	17.068327	-0.050258	3.310511
252.157677	3722.387637	17.073331	-0.050210	3.307034
252.076843	3714.370618	17.078336	-0.050190	3.303547
251.770292	3706.463699	17.083341	-0.050128	3.300095
251.858648	3698.408815	17.088346	-0.050140	3.296591
252.230480	3690.358742	17.093351	-0.050204	3.293097
252.118208	3682.364226	17.098355	-0.050178	3.289603
251.885432	3674.412173	17.103360	-0.050130	3.286120
252.043344	3666.439877	17.108365	-0.050155	3.282640
251.668501	3658.470884	17.113370	-0.050080	3.279136
251.759473	3650.514571	17.118375	-0.050092	3.275653
251.840552	3642.487939	17.123379	-0.050102	3.272135
251.966905	3634.437997	17.128384	-0.050121	3.268604
251.827993	3626.479536	17.133389	-0.050090	3.265100
251.905298	3618.483327	17.138394	-0.050100	3.261583
252.082968	3610.494841	17.143399	-0.050128	3.258071
251.821405	3602.511387	17.148403	-0.050074	3.254539
251.729778	3594.554021	17.153408	-0.050052	3.251021
251.919128	3586.544348	17.158413	-0.050083	3.247488
251.951612	3578.509408	17.163418	-0.050084	3.243934
252.055549	3570.576538	17.168423	-0.050098	3.240424
251.708810	3562.646945	17.173427	-0.050029	3.236892
251.838104	3554.624897	17.178432	-0.050048	3.233336
251.799902	3546.628203	17.183437	-0.050036	3.229780
251.588739	3538.609093	17.188442	-0.049992	3.226203
251.629103	3530.620557	17.193447	-0.049995	3.222646
251.725437	3522.584407	17.198451	-0.050008	3.219066
251.366698	3514.699908	17.203456	-0.049936	3.215531
251.299130	3506.695133	17.208461	-0.049919	3.211950
251.206088	3498.678057	17.213466	-0.049896	3.208359
251.465477	3490.657694	17.218471	-0.049940	3.204778
251.068175	3482.735912	17.223475	-0.049861	3.201208
251.256326	3474.731867	17.228480	-0.049891	3.197623
251.565352	3466.684052	17.233485	-0.049944	3.194019
251.089871	3458.778107	17.238490	-0.049850	3.190441
251.478033	3450.725315	17.243495	-0.049918	3.186830
251.546583	3442.722955	17.248499	-0.049926	3.183224
251.167198	3434.771945	17.253504	-0.049850	3.179618
251.020718	3426.842587	17.258509	-0.049818	3.176027
250.851447	3418.815561	17.263514	-0.049782	3.172387
251.276718	3410.767038	17.268519	-0.049856	3.168760
251.063827	3402.799901	17.273523	-0.049812	3.165137
251.361406	3394.811630	17.278528	-0.049862	3.161523
250.659088	3386.976346	17.283533	-0.049727	3.157929
250.820924	3378.870853	17.288538	-0.049752	3.154247
251.082170	3370.873768	17.293543	-0.049795	3.150615
250.987536	3362.884861	17.298547	-0.049773	3.146967
250.601438	3354.928116	17.303552	-0.049696	3.143315
251.067052	3346.887729	17.308557	-0.049778	3.139660
251.055355	3338.923225	17.313562	-0.049771	3.136013
251.448536	3330.896165	17.318567	-0.049839	3.132352
251.264452	3322.902166	17.323571	-0.049800	3.128676
251.226152	3314.926107	17.328576	-0.049788	3.125010
251.133360	3307.002224	17.333581	-0.049766	3.121361
250.579303	3299.098252	17.338586	-0.049658	3.117696
250.913355	3291.033596	17.343591	-0.049715	3.113994
250.886889	3283.044598	17.348595	-0.049706	3.110305
250.591247	3275.082262	17.353600	-0.049646	3.106612
250.885157	3267.049413	17.358605	-0.049696	3.102909
250.529629	3259.078646	17.363610	-0.049624	3.099200
250.920258	3251.091957	17.368615	-0.049692	3.095515
250.749790	3243.085237	17.373619	-0.049656	3.091789
250.473196	3235.152141	17.378624	-0.049599	3.088088
250.728373	3227.115164	17.383629	-0.049642	3.084359
250.669972	3219.170885	17.388634	-0.049626	3.080654
250.856078	3211.174910	17.393639	-0.049656	3.076932
250.772783	3203.157528	17.398643	-0.049636	3.073183
250.393554	3195.206572	17.403648	-0.049560	3.069446
250.282490	3187.233733	17.408653	-0.049535	3.065707
250.195287	3179.224948	17.413658	-0.049514	3.061948
249.946521	3171.327908	17.418663	-0.049462	3.058229
249.904365	3163.255791	17.423667	-0.049450	3.054433
249.410895	3155.339595	17.428672	-0.049353	3.050683
250.298675	3147.207593	17.433677	-0.049513	3.046895
249.945578	3139.290556	17.438682	-0.049443	3.043143
249.858583	3131.349610	17.443687	-0.049422	3.039388
250.090824	3123.316368	17.448691	-0.049460	3.035600
249.872141	3115.372129	17.453696	-0.049415	3.031828
249.326729	3107.468403	17.458701	-0.049308	3.028053
249.632789	3099.369832	17.463706	-0.049360	3.024224
249.651149	3091.440469	17.468711	-0.049359	3.020456
249.551475	3083.446970	17.473715	-0.049335	3.016647
249.937507	3075.389103	17.478720	-0.049402	3.012827
249.731155	3067.447463	17.483725	-0.049359	3.009027
249.383806	3059.482666	17.488730	-0.049290	3.005205
249.637183	3051.495978	17.493735	-0.049332	3.001398
249.636166	3043.496354	17.498739	-0.049327	2.997566
249.480401	3035.540464	17.503744	-0.049293	2.993743
249.379481	3027.588278	17.508749	-0.049269	2.989919
249.510554	3019.522071	17.513754	-0.049289	2.986048
249.331164	3011.609246	17.518759	-0.049251	2.982230
249.517575	3003.563591	17.523763	-0.049280	2.978361
249.621817	2995.573379	17.528768	-0.049295	2.974510
249.586582	2987.589851	17.533773	-0.049283	2.970650
249.170732	2979.682536	17.538778	-0.049201	2.966802
249.470176	2971.670567	17.543783	-0.049252	2.962936
249.419711	2963.681938	17.548787	-0.049238	2.959057
249.055868	2955.811220	17.553792	-0.049165	2.955214
249.260762	2947.731620	17.558797	-0.049199	2.951295
249.109298	2939.736899	17.563802	-0.049165	2.947393
249.282221	2931.749880	17.568807	-0.049193	2.943507
249.357954	2923.768667	17.573811	-0.049202	2.939613
249.530753	2915.771991	17.578816	-0.049229	2.935711
248.873054	2907.898471	17.583821	-0.049102	2.931821
249.028702	2899.832001	17.588826	-0.049126	2.927874
248.834672	2891.895087	17.593831	-0.049085	2.923966
248.492780	2883.965606	17.598835	-0.049017	2.920049
248.483440	2876.001143	17.603840	-0.049010	2.916127
248.615058	2867.921601	17.608845	-0.049030	2.912152
248.943787	2859.828525	17.613850	-0.049086	2.908174
249.192890	2851.827810	17.618855	-0.049127	2.904233
248.981335	2843.935348	17.623859	-0.049083	2.900315
249.318975	2835.915982	17.628864	-0.049141	2.896359
249.119696	2827.989642	17.633869	-0.049099	2.892413
248.988142	2819.995052	17.638874	-0.049070	2.888433
249.002409	2812.022715	17.643879	-0.049068	2.884465
248.996707	2804.066719	17.648883	-0.049062	2.880500
248.939881	2796.106830	17.653888	-0.049046	2.876524
248.815724	2788.146869	17.658893	-0.049018	2.872539
248.497574	2780.185730	17.663898	-0.048954	2.868536
248.433951	2772.221285	17.668903	-0.048938	2.864541
248.767636	2764.149437	17.673907	-0.048995	2.860509
249.012117	2756.144265	17.678912	-0.049036	2.856500
249.078356	2748.181081	17.683917	-0.049043	2.852496
248.953581	2740.195790	17.688922	-0.049015	2.848464
248.885784	2732.256141	17.693927	-0.048997	2.844453
248.763978	2724.313555	17.698931	-0.048970	2.840431
248.920275	2716.301014	17.703936	-0.048994	2.836385
248.776440	2708.349755	17.708941	-0.048963	2.832346
248.666122	2700.358110	17.713946	-0.048937	2.828283
248.677538	2692.369472	17.718951	-0.048934	2.824223
248.345629	2684.462061	17.723955	-0.048868	2.820178
247.899100	2676.517651	17.728960	-0.048780	2.816102
248.578440	2668.402366	17.733965	-0.048901	2.811999
248.139426	2660.481658	17.738970	-0.048815	2.807923
247.955409	2652.528372	17.743975	-0.048776	2.803840
247.818772	2644.578811	17.748979	-0.048745	2.799755
247.884409	2636.600280	17.753984	-0.048753	2.795662
247.946315	2628.595010	17.758989	-0.048759	2.791549
247.969596	2620.584831	17.763994	-0.048759	2.787425
247.964340	2612.606172	17.768999	-0.048753	2.783309
248.036371	2604.619958	17.774003	-0.048762	2.779188
248.002879	2596.677275	17.779008	-0.048750	2.775077
247.554757	2588.768811	17.784013	-0.048662	2.770952
247.661201	2580.740693	17.789018	-0.048677	2.766793
247.850816	2572.737548	17.794023	-0.048708	2.762646
247.545384	2564.795424	17.799027	-0.048646	2.758494
247.584546	2556.828689	17.804032	-0.048648	2.754343
247.673910	2548.777727	17.809037	-0.048660	2.750146
247.410201	2540.808521	17.814042	-0.048606	2.745963
247.631795	2532.830621	17.819047	-0.048642	2.741800
247.454388	2524.882665	17.824051	-0.048605	2.737621
247.611814	2516.869432	17.829056	-0.048629	2.733422
247.955551	2508.837179	17.834061	-0.048688	2.729218
247.913647	2500.895401	17.839066	-0.048676	2.725032
247.577621	2493.011286	17.844071	-0.048608	2.720851
247.514902	2485.043380	17.849075	-0.048592	2.716636
247.681018	2477.024889	17.854080	-0.048618	2.712402
247.860482	2469.017793	17.859085	-0.048646	2.708169
247.196628	2461.151073	17.864090	-0.048518	2.703950
247.361585	2453.149565	17.869095	-0.048544	2.699706
247.084332	2445.225385	17.874099	-0.048487	2.695467
247.046538	2437.216858	17.879104	-0.048475	2.691192
247.091209	2429.210441	17.884109	-0.048479	2.686918
247.224883	2421.224527	17.889114	-0.048499	2.682653
247.500768	2413.221625	17.894119	-0.048545	2.678381
246.992054	2405.341913	17.899123	-0.048446	2.674117
247.176671	2397.314624	17.904128	-0.048475	2.669813
247.640464	2389.285574	17.909133	-0.048557	2.665519
247.080348	2381.391088	17.914138	-0.048448	2.661223
247.222663	2373.398885	17.919143	-0.048469	2.656914
247.173609	2365.441444	17.924147	-0.048455	2.652605
247.158346	2357.447612	17.929152	-0.048447	2.648270
247.010274	2349.494227	17.934157	-0.048415	2.643942
246.582695	2341.592327	17.939162	-0.048331	2.639615
246.757466	2333.616241	17.944167	-0.048358	2.635282
246.766185	2325.597216	17.949171	-0.048355	2.630907
246.709106	2317.627108	17.954176	-0.048340	2.626546
247.245733	2309.574836	17.959181	-0.048435	2.622175
246.824517	2301.681220	17.964186	-0.048351	2.617817
247.060712	2293.693462	17.969191	-0.048390	2.613445
246.919126	2285.728002	17.974195	-0.048359	2.609053
246.464273	2277.834313	17.979200	-0.048270	2.604670
246.652566	2269.849598	17.984205	-0.048300	2.600275
246.730972	2261.860514	17.989210	-0.048310	2.595862
246.954584	2253.785009	17.994215	-0.048346	2.591404
246.378198	2245.845928	17.999219	-0.048234	2.586958
246.185801	2237.914075	18.004224	-0.048194	2.582535
246.121876	2229.961159	18.009229	-0.048177	2.578102
246.491683	2221.898430	18.014234	-0.048241	2.573631
246.370089	2213.969693	18.019239	-0.048213	2.569192
246.452669	2205.985838	18.024243	-0.048224	2.564729
246.365054	2198.072559	18.029248	-0.048203	2.560286
246.073391	2190.178282	18.034253	-0.048144	2.555830
245.610080	2182.230911	18.039258	-0.048052	2.551325
246.158088	2174.160362	18.044263	-0.048150	2.546815
245.836142	2166.243199	18.049267	-0.048085	2.542321
246.010840	2158.227931	18.054272	-0.048112	2.537800
246.232319	2150.260447	18.059277	-0.048149	2.533301
245.915559	2142.328492	18.064282	-0.048085	2.528775
245.964034	2134.342977	18.069287	-0.048089	2.524237
245.884024	2126.427525	18.074291	-0.048069	2.519721
246.043753	2118.437637	18.079296	-0.048094	2.515173
245.859642	2110.488916	18.084301	-0.048055	2.510614
246.141446	2102.441470	18.089306	-0.048103	2.506025
246.060380	2094.535900	18.094311	-0.048083	2.501482
245.967962	2086.572430	18.099315	-0.048061	2.496897
245.941925	2078.595493	18.104320	-0.048051	2.492300
245.752110	2070.689789	18.109325	-0.048011	2.487723
245.585661	2062.694803	18.114330	-0.047975	2.483089
245.409808	2054.796845	18.119335	-0.047938	2.478501
245.134721	2046.859972	18.124339	-0.047881	2.473874
245.200707	2038.849075	18.129344	-0.047889	2.469222
245.554016	2030.814108	18.134349	-0.047950	2.464568
245.802657	2022.803055	18.139354	-0.047991	2.459912
245.685680	2014.887756	18.144359	-0.047965	2.455276
245.711855	2006.933962	18.149363	-0.047965	2.450618
245.639842	1998.971580	18.154368	-0.047946	2.445939
245.722082	1991.039843	18.159373	-0.047957	2.441282
245.168046	1983.167339	18.164378	-0.047849	2.436600
245.495391	1975.102626	18.169383	-0.047905	2.431865
245.643066	1967.098655	18.174387	-0.047928	2.427143
245.569812	1959.168796	18.179392	-0.047909	2.422438
245.559421	1951.227873	18.184397	-0.047902	2.417722
245.561510	1943.239436	18.189402	-0.047898	2.412970
245.746961	1935.265737	18.194407	-0.047928	2.408232
245.663979	1927.338604	18.199411	-0.047907	2.403490
245.149444	1919.467600	18.204416	-0.047807	2.398739
245.381338	1911.473475	18.209421	-0.047845	2.393964
245.490601	1903.463365	18.214426	-0.047860	2.389160
245.294218	1895.547765	18.219431	-0.047819	2.384378
244.932690	1887.674323	18.224435	-0.047747	2.379599
244.841159	1879.712077	18.229440	-0.047725	2.374779
244.647267	1871.758274	18.234445	-0.047684	2.369945
244.985233	1863.683224	18.239450	-0.047742	2.365072
244.740574	1855.810563	18.244455	-0.047692	2.360263
244.442441	1847.893559	18.249459	-0.047631	2.355413
244.426149	1839.902090	18.254464	-0.047624	2.350532
244.435658	1831.934153	18.259469	-0.047620	2.345656
244.378608	1823.963370	18.264474	-0.047605	2.340763
244.238231	1816.049338	18.269479	-0.047574	2.335888
243.988616	1808.117993	18.274483	-0.047523	2.330982
244.168614	1800.092821	18.279488	-0.047551	2.326045
244.181598	1792.157650	18.284493	-0.047549	2.321139
244.396798	1784.150304	18.289498	-0.047584	2.316194
244.583052	1776.194259	18.294503	-0.047614	2.311269
244.886477	1768.182266	18.299507	-0.047666	2.306308
244.635919	1760.295749	18.304512	-0.047614	2.301367
244.760843	1752.354723	18.309517	-0.047632	2.296414
244.853735	1744.373683	18.314522	-0.047645	2.291423
244.940955	1736.433841	18.319527	-0.047656	2.286446
244.511252	1728.562383	18.324531	-0.047572	2.281456
243.965753	1720.713392	18.329536	-0.047465	2.276458
243.937962	1712.736177	18.334541	-0.047455	2.271415
243.593978	1704.760683	18.339546	-0.047386	2.266333
243.985206	1696.730174	18.344551	-0.047454	2.261270
244.259406	1688.729797	18.349555	-0.047500	2.256204
243.992992	1680.822588	18.354560	-0.047446	2.251138
244.120123	1672.856974	18.359565	-0.047465	2.246059
243.956558	1664.936434	18.364570	-0.047429	2.240971
244.484086	1656.923759	18.369575	-0.047523	2.235874
244.470717	1648.987869	18.374579	-0.047516	2.230767
244.410201	1641.056724	18.379584	-0.047499	2.225646
244.142621	1633.190437	18.384589	-0.047445	2.220537
244.267642	1625.191669	18.389594	-0.047463	2.215366
243.956610	1617.322374	18.394599	-0.047401	2.210227
243.900480	1609.373201	18.399603	-0.047385	2.205047
243.553663	1601.480859	18.404608	-0.047316	2.199865
243.855914	1593.490114	18.409613	-0.047367	2.194667
243.801714	1585.535709	18.414618	-0.047352	2.189447
243.688147	1577.589295	18.419623	-0.047326	2.184215
243.585556	1569.665393	18.424627	-0.047302	2.178985
243.138551	1561.782366	18.429632	-0.047214	2.173738
243.222258	1553.828182	18.434637	-0.047225	2.168481
243.155200	1545.842429	18.439642	-0.047208	2.163175
243.302085	1537.914292	18.444647	-0.047230	2.157916
243.195741	1529.984899	18.449651	-0.047206	2.152619
243.087319	1522.035732	18.454656	-0.047181	2.147295
243.416068	1514.048985	18.459661	-0.047237	2.141974
243.656692	1506.053212	18.464666	-0.047277	2.136626
243.525867	1498.157266	18.469671	-0.047248	2.131296
243.674600	1490.202640	18.474675	-0.047271	2.125940
243.665001	1482.274951	18.479680	-0.047264	2.120574
243.815721	1474.351434	18.484685	-0.047287	2.115212
243.265033	1466.465326	18.489690	-0.047180	2.109793
243.146613	1458.543233	18.494695	-0.047153	2.104378
242.742165	1450.671815	18.499699	-0.047073	2.098955
243.137532	1442.634008	18.504704	-0.047142	2.093484
242.527042	1434.820549	18.509709	-0.047023	2.088052
242.490522	1426.852185	18.514714	-0.047012	2.082556
242.604688	1418.908310	18.519719	-0.047028	2.077079
242.598187	1410.963801	18.524723	-0.047022	2.071574
242.617006	1403.000772	18.529728	-0.047021	2.066044
242.106772	1395.196016	18.534733	-0.046921	2.060556
242.158119	1387.205755	18.539738	-0.046926	2.054980
242.171946	1379.254433	18.544743	-0.046923	2.049413
242.479624	1371.262491	18.549747	-0.046976	2.043833
242.285648	1363.384973	18.554752	-0.046935	2.038266
242.558570	1355.428083	18.559757	-0.046981	2.032676
242.426829	1347.501866	18.564762	-0.046951	2.027051
242.726350	1339.534923	18.569767	-0.047002	2.021426
242.322875	1331.684999	18.574771	-0.046922	2.015794
242.193607	1323.770938	18.579776	-0.046893	2.010130
242.796298	1315.750782	18.584781	-0.047001	2.004452
242.602912	1307.877273	18.589786	-0.046960	1.998778
242.422991	1299.996313	18.594791	-0.046922	1.993084
242.158128	1292.124989	18.599795	-0.046868	1.987371
241.872762	1284.235427	18.604800	-0.046810	1.981627
241.670746	1276.342517	18.609805	-0.046767	1.975872
241.599965	1268.402353	18.614810	-0.046749	1.970080
241.728638	1260.452855	18.619815	-0.046768	1.964286
241.545975	1252.561977	18.624819	-0.046730	1.958484
241.411100	1244.655599	18.629824	-0.046700	1.952659
241.468829	1236.728229	18.634829	-0.046706	1.946821
241.261747	1228.800631	18.639834	-0.046662	1.940937
241.789816	1220.783224	18.644839	-0.046756	1.935050
241.994585	1212.821872	18.649843	-0.046789	1.929151
241.662575	1204.973052	18.654848	-0.046722	1.923257
241.838962	1197.059166	18.659853	-0.046750	1.917354
241.623441	1189.177274	18.664858	-0.046705	1.911412
241.755657	1181.248348	18.669863	-0.046725	1.905456
241.701192	1173.354941	18.674867	-0.046710	1.899486
241.638865	1165.447042	18.679872	-0.046694	1.893486
241.954997	1157.479832	18.684877	-0.046748	1.887466
241.980933	1149.578997	18.689882	-0.046748	1.881443
241.478646	1141.794178	18.694887	-0.046650	1.875428
241.318486	1133.911074	18.699891	-0.046615	1.869358
241.695652	1125.901467	18.704896	-0.046680	1.863234
241.388637	1118.074696	18.709901	-0.046618	1.857150
241.241863	1110.169561	18.714906	-0.046586	1.851005
241.161615	1102.284335	18.719911	-0.046566	1.844862
241.412311	1094.352634	18.724915	-0.046608	1.838703
241.279791	1086.461991	18.729920	-0.046579	1.832508
241.385038	1078.551256	18.734925	-0.046594	1.826306
241.412600	1070.635190	18.739930	-0.046594	1.820069
241.233992	1062.783438	18.744935	-0.046556	1.813836
241.023175	1054.912156	18.749939	-0.046512	1.807562
240.945115	1047.030917	18.754944	-0.046493	1.801275
241.185922	1039.109915	18.759949	-0.046533	1.794973
241.044887	1031.204401	18.764954	-0.046501	1.788614
240.907509	1023.324386	18.769959	-0.046471	1.782253
241.123984	1015.394038	18.774963	-0.046507	1.775874
240.900300	1007.546660	18.779968	-0.046460	1.769482
240.351127	999.766635	18.784973	-0.046353	1.763082
240.140067	991.897527	18.789978	-0.046309	1.756628
240.365624	983.955015	18.794983	-0.046346	1.750146
240.790723	975.977956	18.799987	-0.046421	1.743637
240.250795	968.213758	18.804992	-0.046315	1.737155
239.663323	960.425593	18.809997	-0.046201	1.730622
239.492718	952.540270	18.815002	-0.046165	1.724038
239.935866	944.571215	18.820007	-0.046242	1.717440
240.067087	936.657209	18.825011	-0.046262	1.710821
239.430347	928.888400	18.830016	-0.046139	1.704197
239.571580	920.988321	18.835021	-0.046160	1.697539
239.559171	913.084807	18.840026	-0.046153	1.690832
239.601139	905.192087	18.845031	-0.046156	1.684115
239.347578	897.384989	18.850035	-0.046104	1.677404
239.503113	889.463161	18.855040	-0.046128	1.670623
239.593217	881.597603	18.860045	-0.046140	1.663854
239.529600	873.743776	18.865050	-0.046123	1.657047
239.348275	865.912339	18.870055	-0.046085	1.650214
239.138957	858.099549	18.875059	-0.046041	1.643365
238.629441	850.321661	18.880064	-0.045942	1.636477
238.674015	842.410187	18.885069	-0.045945	1.629519
238.587725	834.522361	18.890074	-0.045924	1.622534
238.861295	826.604771	18.895079	-0.045970	1.615543
238.664245	818.789929	18.900083	-0.045929	1.608547
238.858119	810.879694	18.905088	-0.045960	1.601490
239.560857	802.928265	18.910093	-0.046086	1.594440
239.440331	795.113993	18.915098	-0.046059	1.587362
239.383747	787.309196	18.920103	-0.046044	1.580270
239.469586	779.479655	18.925107	-0.046055	1.573145
239.020296	771.717799	18.930112	-0.045967	1.565970
239.225916	763.864960	18.935117	-0.046000	1.558776
239.206791	756.031793	18.940122	-0.045992	1.551533
238.878763	748.265202	18.945127	-0.045926	1.544271
239.118603	740.388649	18.950131	-0.045966	1.536958
238.765397	732.615062	18.955136	-0.045895	1.529617
238.979794	724.754669	18.960141	-0.045930	1.522245
238.990827	716.927861	18.965146	-0.045928	1.514838
239.413723	709.033944	18.970151	-0.046002	1.507395
238.723878	701.362583	18.975155	-0.045869	1.499953
238.674101	693.543978	18.980160	-0.045855	1.492434
238.659991	685.730185	18.985165	-0.045847	1.484886
238.384869	677.982678	18.990170	-0.045791	1.477323
238.101012	670.193841	18.995175	-0.045734	1.469680
238.056772	662.365378	19.000179	-0.045721	1.461995
237.841953	654.597115	19.005184	-0.045676	1.454302
238.247210	646.705487	19.010189	-0.045747	1.446547
238.218566	638.904696	19.015194	-0.045737	1.438770
238.001425	631.163643	19.020199	-0.045691	1.430979
238.288434	623.321053	19.025203	-0.045740	1.423126
238.279212	615.524997	19.030208	-0.045734	1.415228
238.045927	607.800801	19.035213	-0.045685	1.407321
238.356875	599.967524	19.040218	-0.045739	1.399350
238.372586	592.203697	19.045223	-0.045737	1.391354
238.280122	584.440611	19.050227	-0.045715	1.383295
238.820397	576.581196	19.055232	-0.045811	1.375197
238.541849	568.899624	19.060237	-0.045754	1.367095
238.431337	561.165526	19.065242	-0.045729	1.358919
238.280052	553.448864	19.070247	-0.045696	1.350705
238.025993	545.754277	19.075251	-0.045644	1.342445
237.769998	538.043760	19.080256	-0.045592	1.334117
237.701310	530.306703	19.085261	-0.045574	1.325741
237.525642	522.610336	19.090266	-0.045537	1.317337
237.269178	514.839253	19.095271	-0.045484	1.308782
237.445397	507.040860	19.100275	-0.045512	1.300221
237.363740	499.318678	19.105280	-0.045492	1.291640
237.317279	491.615700	19.110285	-0.045479	1.283029
237.301305	483.892684	19.115290	-0.045471	1.274344
237.200291	476.199773	19.120295	-0.045448	1.265616
237.242145	468.503982	19.125299	-0.045451	1.256853
236.927209	460.851990	19.130304	-0.045388	1.248008
236.946778	453.153739	19.135309	-0.045387	1.239113
237.195468	445.420871	19.140314	-0.045428	1.230158
237.003224	437.767329	19.145319	-0.045388	1.221143
237.220786	430.057829	19.150323	-0.045424	1.212077
237.315439	422.367196	19.155328	-0.045437	1.202940
237.561634	414.688346	19.160333	-0.045478	1.193779
237.177559	407.111655	19.165338	-0.045402	1.184540
236.765533	399.549110	19.170343	-0.045320	1.175240
236.896687	391.871548	19.175347	-0.045340	1.165839
237.111162	384.213222	19.180352	-0.045376	1.156403
236.932011	376.606292	19.185357	-0.045338	1.146868
236.910904	368.987626	19.190362	-0.045329	1.137274
236.859243	361.385548	19.195367	-0.045315	1.127612
236.936655	353.778102	19.200371	-0.045325	1.117888
236.402045	346.283427	19.205376	-0.045220	1.108089
236.765420	338.636102	19.210381	-0.045283	1.098205
236.132392	331.176248	19.215386	-0.045161	1.088251
236.161521	323.605960	19.220391	-0.045162	1.078211
236.272618	316.029976	19.225395	-0.045178	1.068087
236.410525	308.443814	19.230400	-0.045199	1.057860
235.822179	301.032382	19.235405	-0.045085	1.047599
235.896532	293.482761	19.240410	-0.045094	1.037205
236.227879	285.906681	19.245415	-0.045151	1.026731
235.890365	278.485378	19.250419	-0.045084	1.016203
235.530980	271.055128	19.255424	-0.045013	1.005547
235.730683	263.553095	19.260429	-0.045045	0.994814
236.029491	256.006852	19.265434	-0.045096	0.983924
235.859879	248.593956	19.270439	-0.045060	0.972989
235.582733	241.215251	19.275443	-0.045004	0.961952
235.339973	233.847948	19.280448	-0.044955	0.950813
235.116425	226.492972	19.285453	-0.044908	0.939567
234.861314	219.143762	19.290458	-0.044856	0.928184
235.064853	211.743194	19.295463	-0.044890	0.916705
235.013895	204.396887	19.300467	-0.044876	0.905096
235.125140	197.033231	19.305472	-0.044892	0.893354
235.206419	189.720365	19.310477	-0.044903	0.881530
234.864004	182.501641	19.315482	-0.044835	0.869578
234.561918	175.287591	19.320487	-0.044774	0.857479
235.036769	167.953924	19.325491	-0.044858	0.845235
234.185698	160.896738	19.330496	-0.044695	0.832886
234.031082	153.712680	19.335501	-0.044662	0.820343
234.005363	146.528339	19.340506	-0.044653	0.807645
233.935578	139.404065	19.345511	-0.044636	0.794839
234.008659	132.262721	19.350515	-0.044645	0.781839
234.213036	125.131804	19.355520	-0.044679	0.768682
234.628735	118.021668	19.360525	-0.044752	0.755406
233.929790	111.138813	19.365530	-0.044618	0.741950
233.545663	104.220675	19.370535	-0.044542	0.728286
233.513049	97.284753	19.375539	-0.044532	0.714450
233.541103	90.365907	19.380544	-0.044533	0.700399
233.596977	83.500087	19.385549	-0.044539	0.686181
233.073598	76.950752	19.390554	-0.044438	0.672118