Fri Apr 16 18:27:01 2021

Number of Points = 3641
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.752142	0.203345	0.000000	0.000157	0.311305

1.094981	0.155501	0.005005	0.000093	0.311372
0.892254	0.191855	0.010010	0.000130	0.311370
0.976662	0.178979	0.015014	0.000115	0.311381
1.323428	0.113214	0.020019	0.000050	0.311369
1.238381	0.129797	0.025024	0.000066	0.311374
0.588305	0.249952	0.030029	0.000187	0.311383
0.558609	0.254875	0.035034	0.000192	0.311381
1.169552	0.144466	0.040038	0.000079	0.311384
1.114359	0.143985	0.045043	0.000089	0.311335
0.952676	0.116973	0.050048	0.000119	0.311073
0.825371	0.141119	0.055053	0.000143	0.311078
1.011633	0.103590	0.060058	0.000108	0.311061
0.853989	0.135261	0.065062	0.000137	0.311075
0.706307	0.161507	0.070067	0.000165	0.311073
0.896422	0.127229	0.075072	0.000130	0.311074
0.905683	0.124781	0.080077	0.000128	0.311070
1.152711	0.078053	0.085082	0.000082	0.311062
1.110711	0.087951	0.090086	0.000090	0.311072
0.421326	0.213397	0.095091	0.000218	0.311073
0.597954	0.181289	0.100096	0.000185	0.311073
0.877263	0.131440	0.105101	0.000133	0.311078
0.617691	0.117271	0.110106	0.000181	0.310792
0.636913	0.105919	0.115110	0.000178	0.310756
0.728402	0.089152	0.120115	0.000161	0.310755
0.830682	0.071037	0.125120	0.000142	0.310757
0.829849	0.070713	0.130125	0.000142	0.310755
0.708627	0.091536	0.135130	0.000164	0.310750
1.068645	0.010281	0.140134	0.000097	0.310676
1.019134	-0.019422	0.145139	0.000107	0.310496
0.811835	0.018796	0.150144	0.000145	0.310499
0.911553	0.002942	0.155149	0.000127	0.310509
0.858018	0.011238	0.160154	0.000136	0.310503
0.506998	0.042844	0.165158	0.000202	0.310353
0.441900	0.014759	0.170163	0.000214	0.310167
0.860918	-0.063057	0.175168	0.000136	0.310159
0.853916	-0.061712	0.180173	0.000137	0.310159
0.673439	-0.040619	0.185178	0.000171	0.310105
0.660506	-0.092522	0.190182	0.000173	0.309852
0.398371	-0.046085	0.195187	0.000222	0.309846
0.492421	-0.062978	0.200192	0.000204	0.309847
0.670616	-0.112211	0.205197	0.000171	0.309768
0.337588	-0.105039	0.210202	0.000233	0.309519
0.094013	-0.056161	0.215206	0.000279	0.309541
0.295157	-0.096102	0.220211	0.000241	0.309525
0.567479	-0.180100	0.225216	0.000191	0.309364
0.378727	-0.173226	0.230221	0.000226	0.309236
0.232666	-0.147979	0.235226	0.000253	0.309230
0.563262	-0.226949	0.240230	0.000191	0.309141
0.117113	-0.198140	0.245235	0.000274	0.308897
0.141050	-0.202233	0.250240	0.000270	0.308898
0.446198	-0.269049	0.255245	0.000213	0.308845
0.371937	-0.312194	0.260250	0.000227	0.308579
0.216169	-0.281227	0.265254	0.000256	0.308592
0.260613	-0.313102	0.270259	0.000248	0.308480
0.243097	-0.354193	0.275264	0.000251	0.308273
0.054895	-0.319385	0.280269	0.000286	0.308276
0.092911	-0.363510	0.285274	0.000279	0.308101
0.368479	-0.437432	0.290278	0.000228	0.307989
0.286911	-0.427009	0.295283	0.000243	0.307968
-0.002101	-0.446786	0.300288	0.000297	0.307629
0.020093	-0.448555	0.305293	0.000292	0.307639
0.062575	-0.492478	0.310298	0.000284	0.307469
-0.000911	-0.511503	0.315302	0.000296	0.307325
0.187963	-0.556172	0.320307	0.000261	0.307277
0.241560	-0.626463	0.325312	0.000251	0.306992
0.414419	-0.655845	0.330317	0.000219	0.307001
0.102479	-0.657438	0.335322	0.000277	0.306727
0.294582	-0.694844	0.340326	0.000241	0.306715
0.082915	-0.710936	0.345331	0.000281	0.306457
-0.329497	-0.652317	0.350336	0.000357	0.306380
-0.679793	-0.623673	0.355341	0.000423	0.306215
-0.279051	-0.728708	0.360346	0.000348	0.306063
-0.243409	-0.761029	0.365350	0.000341	0.305941
-0.434972	-0.768905	0.370355	0.000377	0.305739
-0.341379	-0.802813	0.375360	0.000360	0.305659
-0.209523	-0.861585	0.380365	0.000335	0.305494
-0.469549	-0.841245	0.385370	0.000384	0.305367
-0.486329	-0.884714	0.390374	0.000387	0.305147
-0.158411	-0.971535	0.395379	0.000326	0.305017
-0.260291	-0.992256	0.400384	0.000345	0.304831
-0.233374	-1.033715	0.405389	0.000340	0.304658
-0.145550	-1.084932	0.410394	0.000323	0.304490
-0.194769	-1.117530	0.415398	0.000332	0.304293
-0.411990	-1.096509	0.420403	0.000373	0.304205
-0.491029	-1.148133	0.425408	0.000388	0.303891
-0.402179	-1.178124	0.430413	0.000371	0.303826
-0.729205	-1.173546	0.435418	0.000432	0.303564
-0.672024	-1.210609	0.440422	0.000421	0.303437
-0.692210	-1.248380	0.445427	0.000425	0.303240
-0.883022	-1.255734	0.450432	0.000461	0.303039
-1.312244	-1.194141	0.455437	0.000540	0.302961
-1.070063	-1.308037	0.460442	0.000495	0.302627
-0.597469	-1.413981	0.465446	0.000408	0.302531
-0.538148	-1.475005	0.470451	0.000396	0.302291
-0.868906	-1.459493	0.475456	0.000458	0.302077
-0.839833	-1.489872	0.480461	0.000453	0.301957
-0.861831	-1.543383	0.485466	0.000457	0.301682
-0.999328	-1.550898	0.490470	0.000482	0.301526
-1.311381	-1.531603	0.495475	0.000540	0.301346
-1.430644	-1.567265	0.500480	0.000563	0.301071
-1.370788	-1.603126	0.505485	0.000552	0.300951
-1.518510	-1.625426	0.510490	0.000579	0.300715
-1.495538	-1.662480	0.515494	0.000575	0.300556
-1.741094	-1.644550	0.520499	0.000620	0.300428
-1.862759	-1.678756	0.525504	0.000643	0.300157
-1.362362	-1.811107	0.530509	0.000550	0.299957
-1.307307	-1.860034	0.535514	0.000540	0.299769
-2.038070	-1.780448	0.540518	0.000676	0.299512
-2.036007	-1.820066	0.545523	0.000675	0.299323
-1.890878	-1.877998	0.550528	0.000648	0.299170
-1.862824	-1.942628	0.555533	0.000643	0.298882
-2.380655	-1.892378	0.560538	0.000740	0.298670
-2.529859	-1.893677	0.565542	0.000767	0.298532
-2.671975	-1.926950	0.570547	0.000794	0.298246
-2.767175	-1.945758	0.575552	0.000812	0.298071
-2.591052	-2.007520	0.580557	0.000779	0.297926
-2.251057	-2.133557	0.585562	0.000716	0.297614
-2.533079	-2.125594	0.590566	0.000768	0.297404
-2.916148	-2.093366	0.595571	0.000839	0.297222
-3.055845	-2.116054	0.600576	0.000865	0.296988
-2.915951	-2.188215	0.605581	0.000839	0.296760
-3.617488	-2.097874	0.610586	0.000970	0.296579
-4.020784	-2.068738	0.615590	0.001045	0.296363
-4.439846	-2.041220	0.620595	0.001123	0.296126
-4.344546	-2.085804	0.625600	0.001105	0.295993
-4.650637	-2.081888	0.630605	0.001162	0.295740
-4.767179	-2.092301	0.635610	0.001184	0.295585
-4.788968	-2.108230	0.640614	0.001188	0.295488
-5.349879	-2.077544	0.645619	0.001292	0.295139
-5.568247	-2.057991	0.650624	0.001333	0.295040
-5.376520	-2.135695	0.655629	0.001297	0.294830
-5.435815	-2.175295	0.660634	0.001308	0.294583
-6.413185	-2.014310	0.665638	0.001490	0.294501
-6.529676	-2.050431	0.670643	0.001512	0.294219
-6.219887	-2.129709	0.675648	0.001454	0.294106
-6.767718	-2.074837	0.680653	0.001556	0.293886
-7.112061	-2.049647	0.685658	0.001620	0.293702
-7.227350	-2.052894	0.690662	0.001642	0.293583
-7.427475	-2.067930	0.695667	0.001679	0.293330
-7.615921	-2.049257	0.700672	0.001714	0.293253
-7.834773	-2.061813	0.705677	0.001755	0.292994
-7.696850	-2.102166	0.710682	0.001729	0.292919
-8.262694	-2.058211	0.715686	0.001834	0.292628
-8.148959	-2.096648	0.720691	0.001813	0.292540
-8.726224	-2.037853	0.725696	0.001921	0.292312
-8.722392	-2.059154	0.730701	0.001920	0.292210
-9.333149	-1.991993	0.735706	0.002034	0.291993
-9.264535	-2.024453	0.740710	0.002021	0.291894
-10.060926	-1.914476	0.745715	0.002169	0.291721
-9.635587	-2.015061	0.750720	0.002090	0.291606
-9.881604	-2.016952	0.755725	0.002136	0.291375
-9.883857	-2.034442	0.760730	0.002136	0.291286
-10.097769	-2.039856	0.765734	0.002176	0.291066
-9.906931	-2.091984	0.770739	0.002140	0.290979
-10.422720	-2.046679	0.775744	0.002236	0.290738
-10.431056	-2.053460	0.780749	0.002238	0.290697
-11.436827	-1.910828	0.785754	0.002425	0.290497
-11.214946	-1.950730	0.790758	0.002384	0.290499
-11.230588	-2.018207	0.795763	0.002387	0.290148
-11.463630	-1.975440	0.800768	0.002430	0.290150
-11.416358	-2.038853	0.805773	0.002421	0.289877
-11.531763	-2.029777	0.810778	0.002443	0.289818
-11.618867	-2.062003	0.815782	0.002459	0.289578
-12.015019	-2.006309	0.820787	0.002533	0.289496
-11.814578	-2.079053	0.825792	0.002495	0.289315
-11.936868	-2.077171	0.830797	0.002518	0.289213
-12.397549	-2.028090	0.835802	0.002604	0.289039
-12.540697	-2.034277	0.840806	0.002631	0.288878
-12.794258	-2.004681	0.845811	0.002678	0.288796
-13.190977	-1.979809	0.850816	0.002752	0.288559
-12.768634	-2.057061	0.855821	0.002673	0.288556
-13.357616	-2.011667	0.860826	0.002783	0.288247
-13.305928	-2.021234	0.865830	0.002773	0.288246
-13.556380	-2.019203	0.870835	0.002820	0.288028
-13.709165	-2.005832	0.875840	0.002848	0.287956
-13.491461	-2.078262	0.880845	0.002808	0.287790
-14.146563	-1.994657	0.885850	0.002929	0.287612
-13.975293	-2.037916	0.890854	0.002898	0.287551
-14.686013	-1.956515	0.895859	0.003030	0.287310
-14.755520	-1.943313	0.900864	0.003043	0.287313
-14.568851	-2.026176	0.905869	0.003008	0.287067
-14.790736	-2.002948	0.910874	0.003049	0.286981
-15.061600	-1.975463	0.915878	0.003100	0.286871
-15.591783	-1.912275	0.920883	0.003198	0.286703
-15.558708	-1.918499	0.925888	0.003192	0.286702
-15.292977	-2.026139	0.930893	0.003143	0.286403
-15.755105	-1.951006	0.935898	0.003229	0.286358
-15.496677	-2.026818	0.940902	0.003181	0.286212
-15.959083	-1.973618	0.945907	0.003267	0.286056
-16.426598	-1.888213	0.950912	0.003354	0.286058
-16.232616	-1.985248	0.955917	0.003318	0.285746
-16.132619	-2.007652	0.960922	0.003299	0.285724
-16.357066	-1.991477	0.965926	0.003341	0.285600
-16.812934	-1.931158	0.970931	0.003426	0.285485
-16.684107	-1.957154	0.975936	0.003402	0.285472
-16.710182	-2.017256	0.980941	0.003407	0.285144
-17.118760	-1.944145	0.985946	0.003483	0.285138
-17.109738	-1.977488	0.990950	0.003481	0.284977
-17.727422	-1.892249	0.995955	0.003596	0.284839
-17.746121	-1.890949	1.000960	0.003599	0.284829
-17.543333	-1.985252	1.005965	0.003562	0.284537
-18.095749	-1.890869	1.010970	0.003664	0.284506
-18.144280	-1.897487	1.015974	0.003673	0.284428
-18.316706	-1.906884	1.020979	0.003705	0.284220
-17.694440	-2.024674	1.025984	0.003590	0.284197
-17.897302	-2.035974	1.030989	0.003627	0.283951
-18.447546	-1.953888	1.035994	0.003730	0.283860
-18.433847	-1.968790	1.040998	0.003727	0.283797
-18.583750	-1.987474	1.046003	0.003755	0.283562
-19.167689	-1.880104	1.051008	0.003864	0.283568
-18.771595	-1.993442	1.056013	0.003790	0.283358
-19.089435	-1.957890	1.061018	0.003849	0.283244
-18.938494	-1.993908	1.066022	0.003821	0.283200
-19.533123	-1.932959	1.071027	0.003932	0.282959
-19.799766	-1.883936	1.076032	0.003981	0.282962
-19.540164	-1.962286	1.081037	0.003933	0.282803
-20.512670	-1.821116	1.086042	0.004114	0.282620
-19.850778	-1.940992	1.091046	0.003991	0.282623
-19.791627	-1.998206	1.096051	0.003980	0.282385
-21.061631	-1.779620	1.101056	0.004216	0.282322
-21.228015	-1.745185	1.106061	0.004247	0.282343
-20.850473	-1.874245	1.111066	0.004177	0.282033
-21.017290	-1.850710	1.116070	0.004208	0.281998
-21.334666	-1.792608	1.121075	0.004267	0.282001
-21.153296	-1.884438	1.126080	0.004233	0.281698
-20.886265	-1.933108	1.131085	0.004184	0.281698
-21.766159	-1.788919	1.136090	0.004347	0.281617
-22.128064	-1.766642	1.141094	0.004415	0.281393
-21.725016	-1.841826	1.146099	0.004340	0.281383
-22.120586	-1.787990	1.151104	0.004413	0.281290
-22.324505	-1.792879	1.156109	0.004451	0.281074
-22.242700	-1.806916	1.161114	0.004436	0.281079
-21.829835	-1.906231	1.166118	0.004359	0.280954
-22.282120	-1.864662	1.171123	0.004443	0.280744
-22.135199	-1.891701	1.176128	0.004416	0.280743
-22.145118	-1.917715	1.181133	0.004418	0.280599
-22.385744	-1.893683	1.186138	0.004463	0.280498
-22.111424	-1.949679	1.191142	0.004412	0.280466
-22.435444	-1.948568	1.196147	0.004472	0.280168
-22.666291	-1.908073	1.201152	0.004515	0.280160
-22.359867	-1.997045	1.206157	0.004458	0.279988
-22.861775	-1.937545	1.211162	0.004551	0.279824
-23.039791	-1.901249	1.216166	0.004584	0.279845
-23.194038	-1.936304	1.221171	0.004613	0.279518
-23.827139	-1.819278	1.226176	0.004731	0.279528
-23.260234	-1.935851	1.231181	0.004625	0.279458
-23.630024	-1.913796	1.236186	0.004694	0.279224
-23.660659	-1.907848	1.241190	0.004700	0.279226
-23.604796	-1.961545	1.246195	0.004689	0.279000
-23.742477	-1.959628	1.251200	0.004715	0.278880
-23.748172	-1.966699	1.256205	0.004716	0.278838
-24.204773	-1.936345	1.261210	0.004801	0.278565
-23.805329	-2.007590	1.266214	0.004727	0.278572
-24.416426	-1.932907	1.271219	0.004841	0.278383
-24.977028	-1.853884	1.276224	0.004945	0.278264
-24.730873	-1.896251	1.281229	0.004899	0.278276
-25.400863	-1.827413	1.286234	0.005024	0.278000
-25.546227	-1.803108	1.291238	0.005051	0.277989
-25.445572	-1.826393	1.296243	0.005032	0.277964
-25.316272	-1.912483	1.301248	0.005008	0.277638
-25.359344	-1.903299	1.306253	0.005016	0.277645
-25.811886	-1.844237	1.311258	0.005100	0.277524
-25.650559	-1.911544	1.316262	0.005070	0.277326
-25.477399	-1.944759	1.321267	0.005038	0.277317
-25.926429	-1.910380	1.326272	0.005121	0.277070
-25.892852	-1.929181	1.331277	0.005115	0.277004
-25.753103	-1.967271	1.336282	0.005089	0.276937
-26.422494	-1.888063	1.341286	0.005214	0.276715
-26.334476	-1.905128	1.346291	0.005197	0.276710
-26.279630	-1.950463	1.351296	0.005187	0.276525
-26.651172	-1.910549	1.356301	0.005256	0.276380
-26.814284	-1.882869	1.361306	0.005287	0.276370
-26.521528	-1.987142	1.366310	0.005232	0.276102
-27.165421	-1.876256	1.371315	0.005352	0.276070
-27.149235	-1.900121	1.376320	0.005349	0.275960
-27.298124	-1.912618	1.381325	0.005377	0.275752
-27.001433	-1.969697	1.386330	0.005322	0.275736
-27.312875	-1.943413	1.391334	0.005379	0.275577
-27.469527	-1.931187	1.396339	0.005409	0.275491
-27.565213	-1.919563	1.401344	0.005426	0.275461
-27.529506	-1.983420	1.406349	0.005420	0.275159
-27.600001	-1.972421	1.411354	0.005433	0.275150
-27.577317	-2.015002	1.416358	0.005429	0.274948
-28.000233	-1.960332	1.421363	0.005507	0.274831
-28.059184	-1.959689	1.426368	0.005518	0.274778
-28.257582	-1.971995	1.431373	0.005555	0.274523
-28.369671	-1.954138	1.436378	0.005576	0.274509
-28.490263	-1.965685	1.441382	0.005599	0.274333
-28.994857	-1.892783	1.446387	0.005692	0.274233
-28.858176	-1.919104	1.451392	0.005667	0.274226
-29.162169	-1.925125	1.456397	0.005724	0.273902
-29.629779	-1.840761	1.461402	0.005811	0.273898
-29.212231	-1.936603	1.466406	0.005733	0.273793
-29.405073	-1.941866	1.471411	0.005769	0.273580
-29.367628	-1.950497	1.476416	0.005762	0.273570
-29.197902	-2.025701	1.481421	0.005730	0.273336
-29.477986	-1.991604	1.486426	0.005782	0.273247
-29.328362	-2.036594	1.491430	0.005755	0.273152
-29.887391	-1.971193	1.496435	0.005859	0.272960
-30.084482	-1.934010	1.501440	0.005895	0.272967
-29.863196	-2.024918	1.506445	0.005854	0.272699
-30.514387	-1.919312	1.511450	0.005975	0.272631
-30.092456	-2.013438	1.516454	0.005897	0.272538
-30.098443	-2.055216	1.521459	0.005898	0.272310
-30.389364	-2.002938	1.526464	0.005952	0.272307
-30.655393	-2.007659	1.531469	0.006001	0.272025
-30.931982	-1.965384	1.536474	0.006053	0.271982
-31.070972	-1.959810	1.541478	0.006079	0.271877
-31.122819	-1.984696	1.546483	0.006088	0.271695
-31.256665	-1.961196	1.551488	0.006113	0.271690
-31.326182	-1.997559	1.556493	0.006126	0.271429
-31.900239	-1.904894	1.561498	0.006233	0.271366
-31.799318	-1.934968	1.566502	0.006214	0.271304
-31.829935	-1.973729	1.571507	0.006220	0.271067
-32.148934	-1.915734	1.576512	0.006279	0.271067
-32.129719	-1.953456	1.581517	0.006276	0.270884
-32.638957	-1.884232	1.586522	0.006371	0.270759
-32.788776	-1.855893	1.591526	0.006398	0.270765
-33.151764	-1.829160	1.596531	0.006466	0.270555
-33.395192	-1.792473	1.601536	0.006511	0.270515
-33.162725	-1.832992	1.606541	0.006468	0.270524
-33.378881	-1.861822	1.611546	0.006508	0.270159
-33.430637	-1.850785	1.616550	0.006518	0.270168
-33.348725	-1.878562	1.621555	0.006503	0.270099
-33.587425	-1.882773	1.626560	0.006547	0.269844
-33.207940	-1.951346	1.631565	0.006476	0.269846
-34.080306	-1.826229	1.636570	0.006639	0.269666
-34.659450	-1.743285	1.641574	0.006747	0.269546
-34.218038	-1.825342	1.646579	0.006664	0.269537
-34.363843	-1.833867	1.651584	0.006692	0.269348
-34.410500	-1.844415	1.656589	0.006700	0.269246
-34.263835	-1.875052	1.661594	0.006673	0.269225
-33.944585	-1.990892	1.666598	0.006614	0.268914
-34.048985	-1.976701	1.671603	0.006633	0.268888
-34.638081	-1.896766	1.676608	0.006743	0.268742
-34.450303	-1.961442	1.681613	0.006708	0.268577
-34.664069	-1.922413	1.686618	0.006747	0.268578
-34.459826	-2.013046	1.691622	0.006709	0.268290
-35.143879	-1.895470	1.696627	0.006837	0.268253
-35.039253	-1.934261	1.701632	0.006817	0.268146
-34.979431	-1.977232	1.706637	0.006806	0.267973
-35.307352	-1.919094	1.711642	0.006867	0.267965
-35.224214	-1.988157	1.716646	0.006852	0.267673
-35.428682	-1.959901	1.721651	0.006890	0.267625
-36.217141	-1.833064	1.726656	0.007036	0.267536
-35.940559	-1.923306	1.731661	0.006985	0.267319
-36.015600	-1.910168	1.736666	0.006999	0.267317
-36.137538	-1.928340	1.741670	0.007022	0.267098
-36.562054	-1.871398	1.746675	0.007101	0.266988
-36.174632	-1.946964	1.751680	0.007028	0.266961
-36.071887	-2.013739	1.756685	0.007009	0.266700
-36.615533	-1.915792	1.761690	0.007111	0.266695
-36.719809	-1.929275	1.766694	0.007130	0.266519
-36.965516	-1.911394	1.771699	0.007176	0.266373
-36.932329	-1.919574	1.776704	0.007169	0.266361
-37.003169	-1.961395	1.781709	0.007183	0.266064
-37.194086	-1.929357	1.786714	0.007218	0.266049
-37.053326	-1.981209	1.791718	0.007192	0.265907
-38.025579	-1.832048	1.796723	0.007373	0.265756
-38.084557	-1.823673	1.801728	0.007384	0.265743
-37.584985	-1.950273	1.806733	0.007291	0.265548
-37.861008	-1.914311	1.811738	0.007342	0.265471
-37.901990	-1.918270	1.816742	0.007350	0.265409
-37.962862	-1.958131	1.821747	0.007361	0.265131
-38.295118	-1.896469	1.826752	0.007423	0.265137
-38.069148	-1.976422	1.831757	0.007381	0.264925
-38.087819	-1.994229	1.836762	0.007384	0.264809
-38.021120	-2.022348	1.841766	0.007372	0.264722
-38.978086	-1.890159	1.846771	0.007550	0.264493
-38.752662	-1.934023	1.851776	0.007508	0.264477
-38.553769	-2.004429	1.856781	0.007471	0.264290
-39.292250	-1.884534	1.861786	0.007609	0.264211
-39.412107	-1.872187	1.866790	0.007631	0.264159
-38.987212	-2.002964	1.871795	0.007552	0.263866
-39.175229	-1.970533	1.876800	0.007587	0.263856
-39.505163	-1.946943	1.881805	0.007648	0.263656
-40.097817	-1.857416	1.886810	0.007758	0.263556
-39.541763	-1.964724	1.891814	0.007655	0.263522
-39.551078	-2.015642	1.896819	0.007657	0.263233
-40.067638	-1.922357	1.901824	0.007753	0.263229
-40.101791	-1.948142	1.906829	0.007759	0.263053
-40.363166	-1.920510	1.911834	0.007808	0.262944
-40.408107	-1.919800	1.916838	0.007816	0.262902
-40.322674	-1.989559	1.921843	0.007800	0.262604
-40.413652	-1.975946	1.926848	0.007817	0.262588
-40.722865	-1.953847	1.931853	0.007875	0.262399
-41.250324	-1.877375	1.936858	0.007973	0.262292
-40.979983	-1.930572	1.941862	0.007923	0.262270
-41.373456	-1.910508	1.946867	0.007996	0.261985
-41.722483	-1.849514	1.951872	0.008061	0.261971
-41.216901	-1.964124	1.956877	0.007967	0.261846
-41.628305	-1.918253	1.961882	0.008043	0.261686
-41.611750	-1.921935	1.966886	0.008040	0.261683
-41.752486	-1.951199	1.971891	0.008066	0.261379
-41.651802	-1.977132	1.976896	0.008048	0.261337
-41.850002	-1.965552	1.981901	0.008085	0.261201
-42.305915	-1.912879	1.986906	0.008169	0.261033
-42.244508	-1.922281	1.991910	0.008158	0.261043
-42.005292	-2.018128	1.996915	0.008113	0.260753
-42.792004	-1.885739	2.001920	0.008260	0.260693

-42.970259	-1.890845	2.011917	0.008293	0.260485
-42.949061	-1.933789	2.021914	0.008289	0.260268
-42.982678	-1.951704	2.031910	0.008295	0.260134
-43.180362	-1.970344	2.041907	0.008332	0.259830
-43.605307	-1.895092	2.051904	0.008411	0.259819
-43.493459	-1.969629	2.061901	0.008390	0.259517
-43.813279	-1.916113	2.071898	0.008450	0.259491
-43.547019	-1.982773	2.081894	0.008400	0.259389
-43.939827	-1.943140	2.091891	0.008473	0.259211
-44.460175	-1.846749	2.101888	0.008570	0.259221
-44.283413	-1.879314	2.111885	0.008537	0.259219
-44.164465	-1.900937	2.121882	0.008515	0.259219
-43.883740	-1.955926	2.131878	0.008463	0.259198
-43.880583	-2.015697	2.141875	0.008462	0.258867
-44.569626	-1.888181	2.151872	0.008590	0.258879
-44.146281	-1.966772	2.161869	0.008512	0.258870
-44.458558	-1.909734	2.171866	0.008570	0.258872
-44.021492	-1.990786	2.181862	0.008488	0.258863
-43.966059	-1.983836	2.191859	0.008478	0.258959
-43.688380	-1.991962	2.201856	0.008426	0.259196
-43.612849	-2.005145	2.211853	0.008412	0.259199
-43.730516	-1.984485	2.221850	0.008434	0.259195
-43.608680	-2.006718	2.231846	0.008411	0.259195
-43.727798	-1.983765	2.241843	0.008433	0.259202
-43.759793	-1.978663	2.251840	0.008439	0.259199
-43.798410	-1.956112	2.261837	0.008446	0.259286
-43.658244	-1.944891	2.271834	0.008420	0.259491
-43.468575	-1.979359	2.281830	0.008385	0.259491
-43.430963	-1.986850	2.291827	0.008378	0.259488
-43.220393	-1.970949	2.301824	0.008339	0.259790
-43.093988	-1.990031	2.311821	0.008315	0.259812
-42.786128	-2.047214	2.321818	0.008258	0.259806
-42.943827	-1.965968	2.331814	0.008287	0.260099
-42.585783	-2.025638	2.341811	0.008220	0.260129
-42.781101	-1.969841	2.351808	0.008257	0.260242
-42.328875	-2.010801	2.361805	0.008173	0.260472
-42.604173	-1.959971	2.371802	0.008224	0.260477
-42.072966	-2.013999	2.381798	0.008125	0.260714
-42.174450	-1.995605	2.391795	0.008144	0.260713
-41.825728	-2.012295	2.401792	0.008079	0.260973
-41.705013	-2.024451	2.411789	0.008056	0.261028
-41.693566	-1.985218	2.421786	0.008054	0.261257
-41.621744	-1.982278	2.431782	0.008041	0.261346
-41.416526	-1.970111	2.441779	0.008002	0.261620
-41.261419	-1.988431	2.451776	0.007974	0.261675
-40.819172	-2.018733	2.461773	0.007891	0.261953
-41.059792	-1.962016	2.471770	0.007936	0.262024
-40.522348	-2.011648	2.481766	0.007836	0.262290
-40.717742	-1.949212	2.491763	0.007872	0.262439
-40.552101	-1.949231	2.501760	0.007841	0.262605
-40.713240	-1.863107	2.511757	0.007871	0.262919
-40.285992	-1.914822	2.521754	0.007792	0.263062
-39.837308	-1.964872	2.531750	0.007708	0.263236
-39.895983	-1.903944	2.541747	0.007719	0.263512
-39.637365	-1.923078	2.551744	0.007671	0.263666
-39.093307	-1.985594	2.561741	0.007570	0.263866
-39.177647	-1.920935	2.571738	0.007585	0.264137
-38.736210	-1.974448	2.581734	0.007503	0.264284
-38.616856	-1.959449	2.591731	0.007481	0.264485
-38.212969	-1.985202	2.601728	0.007405	0.264746
-38.243334	-1.952011	2.611725	0.007411	0.264898
-37.874470	-1.976093	2.621722	0.007342	0.265133
-37.595507	-1.976127	2.631718	0.007290	0.265410
-37.591177	-1.948899	2.641715	0.007290	0.265563
-37.171702	-1.993353	2.651712	0.007211	0.265737
-36.985575	-1.978060	2.661709	0.007177	0.266005
-36.969968	-1.949670	2.671706	0.007174	0.266175
-36.407589	-2.018530	2.681702	0.007069	0.266357
-36.635708	-1.915548	2.691699	0.007111	0.266691
-36.073962	-1.985857	2.701696	0.007007	0.266864
-35.954022	-1.978079	2.711693	0.006985	0.267025
-35.434672	-2.021644	2.721690	0.006888	0.267301
-35.417701	-1.982366	2.731686	0.006885	0.267530
-35.743208	-1.880485	2.741683	0.006945	0.267762
-35.204362	-1.937155	2.751680	0.006845	0.267985
-35.134446	-1.899179	2.761677	0.006832	0.268259
-34.713342	-1.933139	2.771674	0.006753	0.268489
-34.546222	-1.923149	2.781670	0.006722	0.268707
-34.132232	-1.962237	2.791667	0.006645	0.268902
-33.948817	-1.936506	2.801664	0.006611	0.269221
-33.742839	-1.937316	2.811661	0.006572	0.269418
-33.401764	-1.962141	2.821658	0.006509	0.269618
-33.256471	-1.946889	2.831654	0.006482	0.269842
-32.877123	-1.958798	2.841651	0.006411	0.270148
-32.808324	-1.925971	2.851648	0.006398	0.270391
-32.733610	-1.900755	2.861645	0.006384	0.270599
-32.315035	-1.943719	2.871642	0.006306	0.270777
-31.783534	-1.987234	2.881638	0.006207	0.271061
-31.672572	-1.965057	2.891635	0.006187	0.271287
-31.405439	-1.973850	2.901632	0.006137	0.271500
-31.436781	-1.926721	2.911629	0.006143	0.271721
-30.851866	-1.983192	2.921626	0.006034	0.271987
-30.614121	-1.983061	2.931622	0.005990	0.272217
-30.339282	-1.994686	2.941619	0.005938	0.272422
-30.111303	-1.997910	2.951616	0.005896	0.272625
-29.954948	-1.963356	2.961613	0.005867	0.272959
-29.606141	-1.989410	2.971610	0.005802	0.273158
-29.489765	-1.973008	2.981606	0.005780	0.273357
-29.172580	-1.989897	2.991603	0.005721	0.273573
-28.893066	-1.984219	3.001600	0.005669	0.273872
-28.846802	-1.950943	3.011597	0.005660	0.274093
-28.493772	-1.974957	3.021594	0.005594	0.274305
-28.199918	-1.989589	3.031590	0.005540	0.274510
-27.705170	-2.019086	3.041587	0.005448	0.274829
-27.649417	-1.991404	3.051584	0.005437	0.275028
-27.460973	-1.986986	3.061581	0.005402	0.275232
-27.036347	-2.015478	3.071578	0.005323	0.275488
-26.857502	-2.007913	3.081574	0.005290	0.275699
-26.528861	-2.030998	3.091571	0.005228	0.275892
-26.643916	-1.968861	3.101568	0.005250	0.276108
-26.406099	-1.964840	3.111565	0.005205	0.276356
-26.264680	-1.933072	3.121562	0.005179	0.276657
-25.830753	-1.972393	3.131558	0.005098	0.276864
-25.565672	-1.978370	3.141555	0.005049	0.277085
-25.370824	-1.970392	3.151552	0.005013	0.277312
-24.874505	-2.003174	3.161549	0.004920	0.277612
-24.730416	-1.984660	3.171546	0.004893	0.277845
-24.596706	-1.968596	3.181542	0.004868	0.278056
-23.842916	-2.069316	3.191539	0.004728	0.278245
-23.902305	-2.000020	3.201536	0.004739	0.278549
-23.558877	-2.023646	3.211533	0.004675	0.278751
-23.522356	-1.990119	3.221530	0.004668	0.278960
-23.131246	-2.013488	3.231526	0.004595	0.279208
-22.708715	-2.039223	3.241523	0.004517	0.279473
-22.682513	-2.005375	3.251520	0.004512	0.279673
-22.345268	-2.026735	3.261517	0.004449	0.279880
-22.263082	-1.991564	3.271514	0.004434	0.280139
-21.708378	-2.034463	3.281510	0.004330	0.280438
-21.716781	-2.001048	3.291507	0.004332	0.280603
-21.735491	-1.962901	3.301504	0.004335	0.280782
-21.182418	-2.014419	3.311501	0.004232	0.281035
-21.229879	-1.952504	3.321498	0.004241	0.281310
-20.747678	-1.994884	3.331494	0.004151	0.281543
-20.854035	-1.929599	3.341491	0.004171	0.281779
-20.257460	-2.000800	3.351488	0.004060	0.281971
-20.025758	-1.980062	3.361485	0.004017	0.282294
-19.758740	-1.986804	3.371482	0.003967	0.282508
-19.555002	-1.980929	3.381478	0.003929	0.282728
-18.972392	-2.042962	3.391475	0.003821	0.282953
-18.865671	-2.007376	3.401472	0.003801	0.283234
-18.569032	-2.020491	3.411469	0.003745	0.283443
-18.585443	-1.976746	3.421466	0.003748	0.283651
-18.026942	-2.037088	3.431462	0.003644	0.283861
-17.878698	-1.999287	3.441459	0.003617	0.284191
-17.799709	-1.975531	3.451456	0.003602	0.284386
-17.540765	-1.982957	3.461453	0.003554	0.284588
-17.055201	-2.027796	3.471450	0.003463	0.284809
-16.595459	-2.049985	3.481446	0.003378	0.285121
-16.824944	-1.966262	3.491443	0.003420	0.285334
-16.572217	-1.969019	3.501440	0.003373	0.285553
-16.180153	-2.006213	3.511437	0.003300	0.285726
-15.863281	-2.003849	3.521434	0.003241	0.286030
-15.477035	-2.035317	3.531430	0.003169	0.286226
-15.317869	-2.025328	3.541427	0.003140	0.286423
-15.015165	-2.028614	3.551424	0.003083	0.286684
-14.784017	-2.022102	3.561421	0.003040	0.286929
-14.722927	-1.992829	3.571418	0.003029	0.287133
-14.560826	-1.976425	3.581414	0.002998	0.287364
-14.218232	-1.989525	3.591411	0.002935	0.287612
-13.951256	-1.977917	3.601408	0.002885	0.287915
-13.675159	-1.990213	3.611405	0.002834	0.288105
-13.739400	-1.936296	3.621402	0.002845	0.288318
-13.498798	-1.928970	3.631398	0.002801	0.288574
-13.049214	-1.952220	3.641395	0.002717	0.288867
-12.483523	-2.009610	3.651392	0.002612	0.289095
-12.616521	-1.943630	3.661389	0.002636	0.289304
-12.194791	-1.982042	3.671386	0.002558	0.289496
-11.674649	-2.011162	3.681382	0.002461	0.289823
-11.708448	-1.963724	3.691379	0.002467	0.290029
-11.278651	-2.000867	3.701376	0.002387	0.290234
-11.058184	-1.990866	3.711373	0.002346	0.290484
-10.722150	-2.005322	3.721370	0.002283	0.290716
-10.292626	-2.046735	3.731366	0.002203	0.290898
-10.119758	-2.042081	3.741363	0.002171	0.291078
-9.786373	-2.046106	3.751360	0.002109	0.291359
-9.429812	-2.066201	3.761357	0.002043	0.291582
-9.288877	-2.059080	3.771354	0.002016	0.291744
-9.068092	-2.052089	3.781350	0.001975	0.291978
-8.747282	-2.058033	3.791347	0.001915	0.292238
-8.670402	-2.035144	3.801344	0.001901	0.292420
-8.448385	-2.035480	3.811341	0.001860	0.292618
-8.089657	-2.032943	3.821338	0.001793	0.292953
-8.078272	-1.997475	3.831334	0.001791	0.293139
-7.774977	-2.015214	3.841331	0.001734	0.293323
-7.070898	-2.094571	3.851328	0.001603	0.293563
-7.212370	-2.019841	3.861325	0.001629	0.293805
-6.886703	-2.038241	3.871322	0.001569	0.294006
-6.325765	-2.098780	3.881318	0.001464	0.294210
-6.237953	-2.060826	3.891315	0.001448	0.294475
-5.857741	-2.094018	3.901312	0.001377	0.294652
-5.961708	-2.036867	3.911309	0.001396	0.294840
-5.406593	-2.076042	3.921306	0.001293	0.295143
-5.650616	-1.987042	3.931302	0.001338	0.295362
-5.205821	-2.028519	3.941299	0.001256	0.295555
-4.778642	-2.069941	3.951296	0.001176	0.295732
-5.214153	-1.934331	3.961293	0.001257	0.296008
-4.087234	-2.095854	3.971290	0.001047	0.296220
-4.375966	-2.006618	3.981286	0.001101	0.296400
-4.303477	-1.960110	3.991283	0.001087	0.296691
-3.962309	-1.972392	4.001280	0.001024	0.296933
-4.544016	-1.819023	4.011277	0.001132	0.297166
-3.254148	-2.005805	4.021274	0.000892	0.297398
-3.572448	-1.901393	4.031270	0.000951	0.297624
-3.048204	-1.929577	4.041267	0.000853	0.297951
-2.781454	-1.932971	4.051264	0.000804	0.298170
-3.246001	-1.801851	4.061261	0.000890	0.298396
-3.156094	-1.762053	4.071258	0.000873	0.298668
-2.976669	-1.736401	4.081254	0.000840	0.298951
-2.668774	-1.733209	4.091251	0.000783	0.299237
-2.803718	-1.654640	4.101248	0.000808	0.299498
-2.465004	-1.648609	4.111245	0.000744	0.299825
-1.886907	-1.693331	4.121242	0.000637	0.300116
-2.448971	-1.529456	4.131238	0.000741	0.300414
-2.383121	-1.487990	4.141235	0.000729	0.300671
-2.662915	-1.372513	4.151232	0.000781	0.300982
-2.143287	-1.399070	4.161229	0.000684	0.301308
-1.994295	-1.354540	4.171226	0.000656	0.301652
-1.760745	-1.330742	4.181222	0.000613	0.301970
-1.181200	-1.365691	4.191219	0.000505	0.302307
-1.713462	-1.197065	4.201216	0.000604	0.302651
-1.866265	-1.090829	4.211213	0.000632	0.303026
-1.647105	-1.058701	4.221210	0.000591	0.303369
-1.369321	-1.032243	4.231206	0.000540	0.303736
-0.909326	-1.037902	4.241203	0.000454	0.304107
-1.062995	-0.938684	4.251200	0.000483	0.304447
-0.935183	-0.872563	4.261197	0.000459	0.304871
-1.201311	-0.741862	4.271194	0.000508	0.305262
-1.057451	-0.690615	4.281190	0.000481	0.305628
-0.886845	-0.638551	4.291187	0.000449	0.306022
-0.637201	-0.590521	4.301184	0.000403	0.306463
-0.365800	-0.558702	4.311181	0.000352	0.306846
-0.385631	-0.472782	4.321178	0.000356	0.307234
-0.724950	-0.306014	4.331174	0.000419	0.307729
-0.486564	-0.262377	4.341171	0.000374	0.308137
-0.456558	-0.167978	4.351168	0.000369	0.308606
-0.298763	-0.100814	4.361165	0.000339	0.309055
-0.126573	-0.037299	4.371162	0.000307	0.309499
-0.022919	0.047049	4.381158	0.000288	0.309981
0.143087	0.118969	4.391155	0.000257	0.310457
0.161959	0.209183	4.401152	0.000253	0.310893
0.000000	0.329593	4.411149	0.000283	0.311317

-0.023516	0.616166	4.416154	0.000287	0.312626
0.252178	1.129351	4.421158	0.000236	0.315222
0.883535	1.863453	4.426163	0.000118	0.319094
1.289197	2.933026	4.431168	0.000041	0.324236
1.851882	4.265450	4.436173	-0.000064	0.330576
3.113001	5.772316	4.441178	-0.000300	0.338087
4.034491	7.647778	4.446182	-0.000473	0.346718
5.145151	9.804485	4.451187	-0.000681	0.356422
6.277968	12.267920	4.456192	-0.000894	0.367095
7.155433	15.106781	4.461197	-0.001059	0.378724
8.458244	18.201192	4.466202	-0.001303	0.391239
9.869518	21.618684	4.471206	-0.001568	0.404591
11.301763	25.384651	4.476211	-0.001838	0.418735
13.222824	29.421385	4.481216	-0.002198	0.433615
15.279441	33.784088	4.486221	-0.002584	0.449130
17.887412	38.426470	4.491226	-0.003072	0.465306
20.005354	43.522453	4.496230	-0.003470	0.482032
21.940194	49.009897	4.501235	-0.003834	0.499235
24.751169	54.713361	4.506240	-0.004361	0.516910
28.380502	60.605807	4.511245	-0.005041	0.534908
33.284138	66.644976	4.516250	-0.005958	0.553301
40.428032	72.652813	4.521254	-0.007292	0.572036
49.794521	78.649061	4.526259	-0.009040	0.591119
55.232790	85.729530	4.531264	-0.010057	0.610495
58.334974	93.532401	4.536269	-0.010640	0.629967
68.146073	100.440615	4.541274	-0.012471	0.649534
70.287498	109.042529	4.546278	-0.012876	0.669216
71.409601	118.001201	4.551283	-0.013090	0.688700
73.396744	126.997967	4.556288	-0.013466	0.708039
75.468666	136.138467	4.561293	-0.013858	0.727178
78.100115	145.341785	4.566298	-0.014354	0.746137
80.702911	154.673859	4.571302	-0.014845	0.764859
82.920403	164.187219	4.576307	-0.015264	0.783338
84.882684	173.838807	4.581312	-0.015635	0.801557
87.235679	183.477893	4.586317	-0.016080	0.819470
89.359700	193.238741	4.591322	-0.016482	0.837137
91.270759	203.035826	4.596326	-0.016844	0.854435
93.070556	212.880725	4.601331	-0.017186	0.871435
95.158040	222.676177	4.606336	-0.017581	0.888110
97.548846	232.414306	4.611341	-0.018032	0.904469
99.563207	242.216340	4.616346	-0.018414	0.920533
101.425023	252.016194	4.621350	-0.018767	0.936275
103.553308	261.732039	4.626355	-0.019169	0.951698
106.243417	271.336981	4.631360	-0.019677	0.966855
108.207343	281.025937	4.636365	-0.020049	0.981713
110.381880	290.656083	4.641370	-0.020460	0.996316
112.241976	300.254907	4.646374	-0.020812	1.010584
114.462239	309.739814	4.651379	-0.021232	1.024580
117.590025	319.036035	4.656384	-0.021820	1.038342
119.527146	328.490274	4.661389	-0.022187	1.051856
121.097041	337.966183	4.666394	-0.022486	1.065141
123.057543	347.298863	4.671398	-0.022857	1.078159
125.163560	356.542967	4.676403	-0.023255	1.090937
127.354996	365.738799	4.681408	-0.023669	1.103522
129.225854	374.934918	4.686413	-0.024024	1.115893
132.064606	383.914896	4.691418	-0.024558	1.128063
133.978249	393.035549	4.696422	-0.024920	1.140079
135.838949	402.117390	4.701427	-0.025273	1.151909
137.931925	411.090466	4.706432	-0.025668	1.163531
139.662691	420.075972	4.711437	-0.025996	1.174977
141.679534	428.974242	4.716442	-0.026378	1.186265
144.319433	437.735833	4.721446	-0.026875	1.197409
147.410292	446.390061	4.726451	-0.027456	1.208412
150.001344	455.140513	4.731456	-0.027944	1.219327
151.713735	463.997854	4.736461	-0.028269	1.230094
153.792576	472.739130	4.741466	-0.028662	1.240705
155.399154	481.528660	4.746470	-0.028967	1.251188
156.844902	490.298906	4.751475	-0.029242	1.261530
159.067252	498.918223	4.756480	-0.029661	1.271764
160.676517	507.598714	4.761485	-0.029966	1.281869
162.289501	516.264700	4.766490	-0.030272	1.291878
163.582088	524.942943	4.771494	-0.030519	1.301763
165.064836	533.606237	4.776499	-0.030800	1.311592
166.856855	542.157259	4.781504	-0.031140	1.321281
168.205224	550.714220	4.786509	-0.031396	1.330824
169.679536	559.239250	4.791514	-0.031676	1.340288
171.061166	567.761783	4.796518	-0.031939	1.349665
172.150014	576.288907	4.801523	-0.032148	1.358930
173.375346	584.792386	4.806528	-0.032381	1.368131
174.609234	593.261650	4.811533	-0.032617	1.377235
175.837395	601.716929	4.816538	-0.032851	1.386264
176.742851	610.222476	4.821542	-0.033025	1.395230
177.549089	618.677137	4.826547	-0.033181	1.404069
178.748912	627.084849	4.831552	-0.033409	1.412871
179.737820	635.475328	4.836557	-0.033599	1.421566
180.996294	643.840187	4.841562	-0.033839	1.430226
182.177633	652.199438	4.846566	-0.034064	1.438815
183.067644	660.589603	4.851571	-0.034236	1.447336
184.167147	668.954072	4.856576	-0.034446	1.455815
185.316639	677.265479	4.861581	-0.034665	1.464201
186.468453	685.624858	4.866586	-0.034885	1.472585
187.624274	693.924531	4.871590	-0.035106	1.480865
188.947991	702.196826	4.876595	-0.035358	1.489097
190.160551	710.502157	4.881600	-0.035589	1.497299
191.294698	718.777934	4.886605	-0.035805	1.505414
192.413537	727.097013	4.891610	-0.036019	1.513525
193.947429	735.306301	4.896614	-0.036310	1.521552
195.039262	743.601646	4.901619	-0.036519	1.529549
196.279076	751.889792	4.906624	-0.036755	1.537521
197.410871	760.152679	4.911629	-0.036971	1.545410
198.470160	768.457400	4.916634	-0.037174	1.553288
199.328449	776.745148	4.921638	-0.037339	1.561079
200.229872	785.029486	4.926643	-0.037512	1.568834
201.271414	793.288541	4.931648	-0.037712	1.576549
202.414436	801.509944	4.936653	-0.037930	1.584206
203.544156	809.766932	4.941658	-0.038146	1.591857
204.633659	818.002150	4.946662	-0.038354	1.599444
205.564929	826.243324	4.951667	-0.038533	1.606979
206.702589	834.477334	4.956672	-0.038750	1.614500
207.808567	842.683561	4.961677	-0.038961	1.621958
209.278891	850.865730	4.966682	-0.039240	1.629411
210.083458	859.165248	4.971686	-0.039396	1.636839
211.035597	867.361090	4.976691	-0.039578	1.644163
212.475204	875.516962	4.981696	-0.039852	1.651488
213.196708	883.779495	4.986701	-0.039991	1.658773
214.408210	891.949139	4.991706	-0.040222	1.666012
215.602645	900.152249	4.996710	-0.040450	1.673247
216.828162	908.292319	5.001715	-0.040684	1.680400
217.781026	916.543005	5.006720	-0.040866	1.687580
219.154079	924.683008	5.011725	-0.041127	1.694691
220.475022	932.849616	5.016730	-0.041379	1.701788
221.448402	941.080740	5.021734	-0.041565	1.708863
222.770373	949.234527	5.026739	-0.041817	1.715890
224.035857	957.411518	5.031744	-0.042058	1.722900
224.854757	965.631731	5.036749	-0.042216	1.729858
226.171800	973.789918	5.041754	-0.042466	1.736802
227.449853	981.950065	5.046758	-0.042710	1.743714
228.494339	990.142964	5.051763	-0.042909	1.750595
229.343199	998.381346	5.056768	-0.043073	1.757461
230.879796	1006.453598	5.061773	-0.043364	1.764253
232.169558	1014.614391	5.066778	-0.043610	1.771058
233.362568	1022.812781	5.071782	-0.043837	1.777855
234.820494	1030.914396	5.076787	-0.044114	1.784581
235.999974	1039.138819	5.081792	-0.044339	1.791345
237.174430	1047.308900	5.086797	-0.044563	1.798039
238.242980	1055.460071	5.091802	-0.044767	1.804680
239.378571	1063.633922	5.096806	-0.044984	1.811322
240.301078	1071.819020	5.101811	-0.045161	1.817923
241.379977	1079.977551	5.106816	-0.045367	1.824497
242.336811	1088.152830	5.111821	-0.045551	1.831046
243.355601	1096.321850	5.116826	-0.045746	1.837574
244.530322	1104.446073	5.121830	-0.045970	1.844062
245.814167	1112.553142	5.126835	-0.046214	1.850527
247.092233	1120.709640	5.131840	-0.046458	1.857006
248.201865	1128.830053	5.136845	-0.046670	1.863415
249.128216	1137.017098	5.141850	-0.046847	1.869831
250.560746	1145.106648	5.146854	-0.047119	1.876210
251.818052	1153.206268	5.151859	-0.047359	1.882553
253.119500	1161.344066	5.156864	-0.047606	1.888909
254.732152	1169.415969	5.161869	-0.047912	1.895230
257.250475	1177.384930	5.166874	-0.048386	1.901555
259.284501	1185.471878	5.171878	-0.048770	1.907892
260.727476	1193.631136	5.176883	-0.049044	1.914194
262.197545	1201.773848	5.181888	-0.049323	1.920466
263.313655	1209.959596	5.186893	-0.049536	1.926709
264.479670	1218.153627	5.191898	-0.049759	1.932943
265.704925	1226.316329	5.196902	-0.049992	1.939140
266.910331	1234.453686	5.201907	-0.050222	1.945297
268.436913	1242.572961	5.206912	-0.050512	1.951455
269.834362	1250.677856	5.211917	-0.050777	1.957570
271.243249	1258.770721	5.216922	-0.051045	1.963657
272.494277	1266.927522	5.221926	-0.051283	1.969754
273.782996	1275.049478	5.226931	-0.051528	1.975811
275.651435	1283.102861	5.231936	-0.051881	1.981862
276.922192	1291.251858	5.236941	-0.052123	1.987899
277.959749	1299.433134	5.241946	-0.052322	1.993915
279.080524	1307.573323	5.246950	-0.052536	1.999892
280.003154	1315.723192	5.251955	-0.052713	2.005837
281.306163	1323.834127	5.256960	-0.052961	2.011777
282.343526	1331.966139	5.261965	-0.053159	2.017685
283.710910	1340.045424	5.266970	-0.053419	2.023574
284.643203	1348.226320	5.271974	-0.053598	2.029471
285.816279	1356.304470	5.276979	-0.053822	2.035304
287.036204	1364.425379	5.281984	-0.054054	2.041154
288.554454	1372.455054	5.286989	-0.054342	2.046954
289.553035	1380.619334	5.291994	-0.054534	2.052778
290.868779	1388.714525	5.296998	-0.054784	2.058570
291.683148	1396.859587	5.302003	-0.054941	2.064328
292.981007	1404.974803	5.307008	-0.055188	2.070099
294.117005	1413.055066	5.312013	-0.055405	2.075813
295.492253	1421.125388	5.317018	-0.055666	2.081528
296.162822	1429.299802	5.322022	-0.055796	2.087228
296.928679	1437.442745	5.327027	-0.055944	2.092900
297.616516	1445.616107	5.332032	-0.056078	2.098569
298.355097	1453.730204	5.337037	-0.056220	2.104188
298.913061	1461.890728	5.342042	-0.056330	2.109805
299.491237	1470.055124	5.347046	-0.056443	2.115412
300.397363	1478.099910	5.352051	-0.056617	2.120955
301.423140	1486.128834	5.357056	-0.056813	2.126484
302.104214	1494.250984	5.362061	-0.056945	2.132028
303.018031	1502.321553	5.367066	-0.057120	2.137545
304.014286	1510.394146	5.372070	-0.057311	2.143057
304.486068	1518.544274	5.377075	-0.057404	2.148557
305.419827	1526.621043	5.382080	-0.057583	2.154037
306.305398	1534.677651	5.387085	-0.057754	2.159485
306.907172	1542.784131	5.392090	-0.057871	2.164925
307.790112	1550.889000	5.397094	-0.058041	2.170377
308.538359	1558.980926	5.402099	-0.058185	2.175794
309.366911	1567.078361	5.407104	-0.058345	2.181208
309.887253	1575.201656	5.412109	-0.058447	2.186597
310.446497	1583.318658	5.417114	-0.058557	2.191972
311.467048	1591.358548	5.422118	-0.058752	2.197326
311.882807	1599.459486	5.427123	-0.058835	2.202651
312.798437	1607.520908	5.432128	-0.059010	2.207983
313.395007	1615.632187	5.437133	-0.059127	2.213305
314.170874	1623.714504	5.442138	-0.059276	2.218612
314.851702	1631.787103	5.447142	-0.059408	2.223891
315.373414	1639.908570	5.452147	-0.059511	2.229174
316.341755	1647.962411	5.457152	-0.059696	2.234442
317.022081	1656.028646	5.462157	-0.059828	2.239679
317.538697	1664.124021	5.467162	-0.059930	2.244907
318.256478	1672.230092	5.472166	-0.060069	2.250148
318.845330	1680.315967	5.477171	-0.060184	2.255353
319.393192	1688.413645	5.482176	-0.060291	2.260549
320.156191	1696.467619	5.487181	-0.060438	2.265724
320.703939	1704.597678	5.492186	-0.060546	2.270917
321.519017	1712.652682	5.497190	-0.060703	2.276073
322.001218	1720.715157	5.502195	-0.060798	2.281194
322.665766	1728.790738	5.507200	-0.060927	2.286327
323.353995	1736.844539	5.512205	-0.061060	2.291436
323.878425	1744.945434	5.517210	-0.061163	2.296550
324.710426	1752.993056	5.522214	-0.061323	2.301645
325.307687	1761.064087	5.527219	-0.061440	2.306723
326.231756	1769.117193	5.532224	-0.061617	2.311806
326.900840	1777.191693	5.537229	-0.061747	2.316870
327.628451	1785.251306	5.542234	-0.061888	2.321918
328.239727	1793.337567	5.547238	-0.062007	2.326962
328.543267	1801.456740	5.552243	-0.062069	2.331989
329.389810	1809.511385	5.557248	-0.062232	2.337011
329.711400	1817.623163	5.562253	-0.062297	2.342013
330.263544	1825.695088	5.567258	-0.062405	2.347000
331.095567	1833.766484	5.572262	-0.062565	2.351998
331.527482	1841.817118	5.577267	-0.062651	2.356940
332.054765	1849.896440	5.582272	-0.062754	2.361897
332.713952	1857.946670	5.587277	-0.062882	2.366837
333.260586	1866.028613	5.592282	-0.062989	2.371776
333.834664	1874.106240	5.597286	-0.063101	2.376704
334.518080	1882.135513	5.602291	-0.063234	2.381601
335.095355	1890.243064	5.607296	-0.063347	2.386527
335.459245	1898.335290	5.612301	-0.063420	2.391417
335.912187	1906.403966	5.617306	-0.063509	2.396289
336.484334	1914.472104	5.622310	-0.063621	2.401160
336.798713	1922.540710	5.627315	-0.063685	2.406001
337.442953	1930.617669	5.632320	-0.063810	2.410864
338.168508	1938.651114	5.637325	-0.063951	2.415697
338.565459	1946.751219	5.642330	-0.064030	2.420534
339.274942	1954.795631	5.647334	-0.064167	2.425353
339.614710	1962.893443	5.652339	-0.064236	2.430164
340.129235	1971.002124	5.657344	-0.064337	2.434986
340.816890	1978.995460	5.662349	-0.064470	2.439745
341.383356	1987.017420	5.667354	-0.064581	2.444501
342.105250	1995.078847	5.672358	-0.064720	2.449282
342.355366	2003.191977	5.677363	-0.064772	2.454049
343.433325	2011.170112	5.682368	-0.064978	2.458790
343.800926	2019.249915	5.687373	-0.065052	2.463527
344.620686	2027.291842	5.692378	-0.065210	2.468268
344.960427	2035.412649	5.697382	-0.065278	2.473008
345.214162	2043.487441	5.702387	-0.065331	2.477706
345.878300	2051.515491	5.707392	-0.065460	2.482400
346.162406	2059.610620	5.712397	-0.065518	2.487094
346.783393	2067.654321	5.717402	-0.065639	2.491775
347.190883	2075.752452	5.722406	-0.065720	2.496462
347.577736	2083.803692	5.727411	-0.065797	2.501112
348.002294	2091.875648	5.732416	-0.065882	2.505768
348.460855	2099.933360	5.737421	-0.065972	2.510410
348.774825	2108.014019	5.742426	-0.066036	2.515045
349.513364	2116.027867	5.747430	-0.066179	2.519665
349.759494	2124.067304	5.752435	-0.066230	2.524255
350.400698	2132.143389	5.757440	-0.066355	2.528886
350.773854	2140.208174	5.762445	-0.066429	2.533483
351.524462	2148.216793	5.767450	-0.066574	2.538066
352.075875	2156.295489	5.772454	-0.066682	2.542667
352.313555	2164.391568	5.777459	-0.066732	2.547246
353.172120	2172.402015	5.782464	-0.066897	2.551813
353.631210	2180.473259	5.787469	-0.066988	2.556378
354.106171	2188.523472	5.792474	-0.067081	2.560923
354.659075	2196.580346	5.797478	-0.067190	2.565470
354.968830	2204.660326	5.802483	-0.067253	2.570004
355.297821	2212.753463	5.807488	-0.067319	2.574539
355.877180	2220.781972	5.812493	-0.067432	2.579048
356.558322	2228.787294	5.817498	-0.067564	2.583543
356.996579	2236.904942	5.822502	-0.067651	2.588075
357.406544	2245.029370	5.827507	-0.067733	2.592600
358.060949	2253.061481	5.832512	-0.067860	2.597084
358.307851	2261.119926	5.837517	-0.067911	2.601547
359.103382	2269.070866	5.842522	-0.068065	2.605980
359.403676	2277.159166	5.847526	-0.068126	2.610447
359.544840	2285.270567	5.852531	-0.068157	2.614908
360.142086	2293.263476	5.857536	-0.068274	2.619327
360.159363	2301.350736	5.862541	-0.068282	2.623752
360.644610	2309.374044	5.867546	-0.068378	2.628165
360.997670	2317.461653	5.872550	-0.068449	2.632597
361.075462	2325.542380	5.877555	-0.068469	2.637000
362.087560	2333.460121	5.882560	-0.068662	2.641369
362.121709	2341.577471	5.887565	-0.068674	2.645773
362.854602	2349.580088	5.892570	-0.068816	2.650155
363.513508	2357.643369	5.897574	-0.068944	2.654557
363.829791	2365.669615	5.902579	-0.069008	2.658909
364.300883	2373.725009	5.907584	-0.069101	2.663280
364.815655	2381.785670	5.912589	-0.069202	2.667649
365.530247	2389.807487	5.917594	-0.069340	2.672004
365.881561	2397.907588	5.922598	-0.069411	2.676369
366.369560	2405.930320	5.927603	-0.069507	2.680694
367.114633	2413.918639	5.932608	-0.069651	2.685011
367.626066	2421.960371	5.937613	-0.069751	2.689334
368.158708	2430.050326	5.942618	-0.069856	2.693677
368.496764	2438.143151	5.947622	-0.069924	2.698002
368.701579	2446.212901	5.952627	-0.069968	2.702299
369.049187	2454.278973	5.957632	-0.070038	2.706597
369.820500	2462.285153	5.962637	-0.070186	2.710883
370.393099	2470.328970	5.967642	-0.070298	2.715169
370.741379	2478.382584	5.972646	-0.070368	2.719439
371.374301	2486.362122	5.977651	-0.070491	2.723682
371.946718	2494.435404	5.982656	-0.070603	2.727963
372.349245	2502.492032	5.987661	-0.070684	2.732218
372.788849	2510.554055	5.992666	-0.070771	2.736471
373.546770	2518.576623	5.997670	-0.070917	2.740717
374.405899	2526.568348	6.002675	-0.071082	2.744947
374.965397	2534.664786	6.007680	-0.071192	2.749205
375.591744	2542.756588	6.012685	-0.071314	2.753459
376.479810	2550.729368	6.017690	-0.071484	2.757660
376.982555	2558.790445	6.022694	-0.071583	2.761877
377.394065	2566.847786	6.027699	-0.071665	2.766080
378.234000	2574.859320	6.032704	-0.071827	2.770279
378.482425	2582.961512	6.037709	-0.071878	2.774482
379.120155	2590.974749	6.042714	-0.072002	2.778656
379.978679	2598.996965	6.047718	-0.072167	2.782842
380.359798	2607.062109	6.052723	-0.072243	2.787015
380.750172	2615.147607	6.057728	-0.072321	2.791193
381.359910	2623.171758	6.062733	-0.072440	2.795346
381.855017	2631.214829	6.067738	-0.072538	2.799495
382.242401	2639.278974	6.072742	-0.072615	2.803643
382.822221	2647.310330	6.077747	-0.072728	2.807779
383.476889	2655.349483	6.082752	-0.072855	2.811917
383.957228	2663.397696	6.087757	-0.072950	2.816043
384.534124	2671.441318	6.092762	-0.073063	2.820167
385.019214	2679.494084	6.097766	-0.073158	2.824283
385.615054	2687.529501	6.102771	-0.073275	2.828392
386.000511	2695.620234	6.107776	-0.073352	2.832510
386.686067	2703.614394	6.112781	-0.073485	2.836590
387.270241	2711.651864	6.117786	-0.073599	2.840681
387.883257	2719.660145	6.122790	-0.073718	2.844752
388.495140	2727.685343	6.127795	-0.073837	2.848826
388.996251	2735.764207	6.132800	-0.073936	2.852914
389.449243	2743.826174	6.137805	-0.074025	2.856986
389.789376	2751.879659	6.142810	-0.074094	2.861041
390.386934	2759.925603	6.147814	-0.074210	2.865101
390.968711	2767.936937	6.152819	-0.074324	2.869136
391.629221	2775.983556	6.157824	-0.074452	2.873188
392.128606	2784.039367	6.162829	-0.074550	2.877230
392.532403	2792.069814	6.167834	-0.074631	2.881248
393.167533	2800.122204	6.172838	-0.074754	2.885284
393.540942	2808.167068	6.177843	-0.074829	2.889296
394.071949	2816.215156	6.182848	-0.074933	2.893313
394.528453	2824.269155	6.187853	-0.075024	2.897323
395.133640	2832.276261	6.192858	-0.075142	2.901312
395.703578	2840.339175	6.197862	-0.075253	2.905322
396.153213	2848.402179	6.202867	-0.075342	2.909319
396.847762	2856.476676	6.207872	-0.075477	2.913329
397.482310	2864.470767	6.212877	-0.075600	2.917291
397.885322	2872.493381	6.217882	-0.075680	2.921249
398.547323	2880.525957	6.222886	-0.075809	2.925221
398.990334	2888.535184	6.227891	-0.075896	2.929164
399.546408	2896.592255	6.232896	-0.076005	2.933131
400.200241	2904.622930	6.237901	-0.076132	2.937084
400.483915	2912.669417	6.242906	-0.076190	2.941020
401.107251	2920.700633	6.247910	-0.076312	2.944962
401.367334	2928.780656	6.252915	-0.076365	2.948903
401.810179	2936.837570	6.257920	-0.076453	2.952836
402.262717	2944.849633	6.262925	-0.076543	2.956743
402.661601	2952.876429	6.267930	-0.076622	2.960650
403.102515	2960.901093	6.272934	-0.076709	2.964552
403.297935	2968.975412	6.277939	-0.076751	2.968460
403.783108	2977.034397	6.282944	-0.076847	2.972371
404.121465	2985.086339	6.287949	-0.076915	2.976265
404.479932	2993.089029	6.292954	-0.076987	2.980132
405.054646	3001.127241	6.297958	-0.077099	2.984021
405.509297	3009.164364	6.302963	-0.077189	2.987899
405.897688	3017.225135	6.307968	-0.077267	2.991780
406.530617	3025.232602	6.312973	-0.077390	2.995642
406.912507	3033.242181	6.317978	-0.077466	2.999488
407.357837	3041.284967	6.322982	-0.077554	3.003348
407.652257	3049.330104	6.327987	-0.077614	3.007196
408.362222	3057.379101	6.332992	-0.077752	3.011062
408.501385	3065.455807	6.337997	-0.077783	3.014907
409.141133	3073.416346	6.343002	-0.077907	3.018718
409.896726	3081.430438	6.348006	-0.078053	3.022554
410.263603	3089.492701	6.353011	-0.078127	3.026389
410.786351	3097.557618	6.358016	-0.078229	3.030229
411.285613	3105.588536	6.363021	-0.078328	3.034046
411.589446	3113.639013	6.368026	-0.078389	3.037857
412.228739	3121.662099	6.373030	-0.078514	3.041668
412.362093	3129.714430	6.378035	-0.078544	3.045462
413.064351	3137.719716	6.383040	-0.078680	3.049257
413.603952	3145.774870	6.388045	-0.078786	3.053064
413.865113	3153.823880	6.393050	-0.078839	3.056848
414.682300	3161.844875	6.398054	-0.078997	3.060642
414.991211	3169.866560	6.403059	-0.079060	3.064407
415.615097	3177.942782	6.408064	-0.079181	3.068208
416.165545	3185.998044	6.413069	-0.079289	3.071990
416.449404	3194.051308	6.418074	-0.079347	3.075755
417.188982	3202.037700	6.423078	-0.079490	3.079505
417.563556	3210.056732	6.428083	-0.079565	3.083248
418.050686	3218.088366	6.433088	-0.079661	3.086998
418.784278	3226.100886	6.438093	-0.079803	3.090746
419.152839	3234.123493	6.443098	-0.079877	3.094477
419.710296	3242.204393	6.448102	-0.079986	3.098239
420.355006	3250.199305	6.453107	-0.080111	3.101960
420.810340	3258.258512	6.458112	-0.080201	3.105698
421.528855	3266.267225	6.463117	-0.080340	3.109421
421.838404	3274.316203	6.468122	-0.080403	3.113138
422.092235	3282.400959	6.473126	-0.080455	3.116865
422.635006	3290.396459	6.478131	-0.080562	3.120559
423.258685	3298.382039	6.483136	-0.080683	3.124249
423.648004	3306.439674	6.488141	-0.080761	3.127956
424.044298	3314.517992	6.493146	-0.080840	3.131668
424.575162	3322.584516	6.498150	-0.080944	3.135377
425.382277	3330.526633	6.503155	-0.081099	3.139037
425.975611	3338.566796	6.508160	-0.081215	3.142727
426.330791	3346.640264	6.513165	-0.081287	3.146418
426.777597	3354.665570	6.518170	-0.081375	3.150086
427.249826	3362.733049	6.523174	-0.081468	3.153770
427.661108	3370.735611	6.528179	-0.081550	3.157418
428.296343	3378.758089	6.533184	-0.081674	3.161080
428.963349	3386.722883	6.538189	-0.081803	3.164714
429.355015	3394.791116	6.543194	-0.081881	3.168378
429.739604	3402.875120	6.548198	-0.081958	3.172044
430.255949	3410.920527	6.553203	-0.082059	3.175694
430.777205	3418.902846	6.558208	-0.082162	3.179312
431.223704	3426.955934	6.563213	-0.082250	3.182954
431.726152	3434.974831	6.568218	-0.082349	3.186579
432.117803	3443.054876	6.573222	-0.082427	3.190222
432.531054	3451.086537	6.578227	-0.082509	3.193841
433.280181	3459.054083	6.583232	-0.082654	3.197441
433.702174	3467.110555	6.588237	-0.082738	3.201062
434.246237	3475.088472	6.593242	-0.082844	3.204650
434.850193	3483.155288	6.598246	-0.082962	3.208275
435.184862	3491.213056	6.603251	-0.083030	3.211881
435.712461	3499.261703	6.608256	-0.083133	3.215487
436.195480	3507.285257	6.613261	-0.083228	3.219076
436.906504	3515.263365	6.618266	-0.083366	3.222650
437.493635	3523.324352	6.623270	-0.083481	3.226251
437.921513	3531.361040	6.628275	-0.083566	3.229831
438.398990	3539.418424	6.633280	-0.083660	3.233419
438.919007	3547.425203	6.638285	-0.083762	3.236981
439.329181	3555.452779	6.643290	-0.083843	3.240544
439.839550	3563.461622	6.648294	-0.083944	3.244099
440.439827	3571.486709	6.653299	-0.084061	3.247661
440.898952	3579.555344	6.658304	-0.084151	3.251232
441.350308	3587.613210	6.663309	-0.084241	3.254795
441.620392	3595.620152	6.668314	-0.084296	3.258323
442.342112	3603.663874	6.673318	-0.084436	3.261882
442.694259	3611.668212	6.678323	-0.084507	3.265405
442.891887	3619.732713	6.683328	-0.084549	3.268944
443.691386	3627.739994	6.688333	-0.084703	3.272479
444.277493	3635.771625	6.693338	-0.084817	3.276011
444.716949	3643.771254	6.698342	-0.084904	3.279520
444.630158	3651.853552	6.703347	-0.084893	3.283040
445.258607	3659.868515	6.708352	-0.085016	3.286555
445.655606	3667.902662	6.713357	-0.085095	3.290066
445.881872	3675.928744	6.718362	-0.085142	3.293563
446.523212	3683.973366	6.723366	-0.085267	3.297080
446.787648	3691.992532	6.728371	-0.085321	3.300567
447.173774	3699.989148	6.733376	-0.085399	3.304046
447.848732	3708.039863	6.738381	-0.085529	3.307556
448.130204	3716.116734	6.743386	-0.085587	3.311058
448.621065	3724.130003	6.748390	-0.085684	3.314537
448.933907	3732.121501	6.753395	-0.085747	3.317996
449.252372	3740.168120	6.758400	-0.085812	3.321475
449.690681	3748.195977	6.763405	-0.085899	3.324947
449.690120	3756.252535	6.768410	-0.085904	3.328411
450.276517	3764.306204	6.773414	-0.086018	3.331892
450.647496	3772.319199	6.778419	-0.086093	3.335344
451.026150	3780.310123	6.783424	-0.086168	3.338783
451.671229	3788.319583	6.788429	-0.086294	3.342237
451.777183	3796.378427	6.793434	-0.086319	3.345688
451.848473	3804.460385	6.798438	-0.086337	3.349143
452.242731	3812.454429	6.803443	-0.086416	3.352570
452.882436	3820.472064	6.808448	-0.086540	3.356012
453.063844	3828.500006	6.813453	-0.086579	3.359438
453.182465	3836.502784	6.818458	-0.086607	3.362848
453.752288	3844.545927	6.823462	-0.086718	3.366288
454.349530	3852.540037	6.828467	-0.086834	3.369704
454.598010	3860.611667	6.833472	-0.086886	3.373137
454.708798	3868.711607	6.838477	-0.086912	3.376574
455.056256	3876.693280	6.843482	-0.086982	3.379965
455.527799	3884.702056	6.848486	-0.087075	3.383369
455.854636	3892.707099	6.853491	-0.087141	3.386763
456.192848	3900.770434	6.858496	-0.087209	3.390178
456.945644	3908.812720	6.863501	-0.087355	3.393595
456.731701	3916.890667	6.868506	-0.087320	3.396990
457.199144	3924.888452	6.873510	-0.087412	3.400372
457.519006	3932.865283	6.878515	-0.087477	3.403736
457.850599	3940.918355	6.883520	-0.087544	3.407129
458.282444	3948.951829	6.888525	-0.087630	3.410514
458.855725	3956.905602	6.893530	-0.087742	3.413868
458.976893	3964.988886	6.898534	-0.087769	3.417256
459.201042	3973.020871	6.903539	-0.087816	3.420623
459.925784	3980.964599	6.908544	-0.087957	3.423967
460.152527	3989.064102	6.913549	-0.088004	3.427356
460.161255	3997.131388	6.918554	-0.088011	3.430720
460.385680	4005.159517	6.923558	-0.088058	3.434072
461.018099	4013.118396	6.928563	-0.088181	3.437406
461.280551	4021.150329	6.933568	-0.088235	3.440755
461.381133	4029.141849	6.938573	-0.088259	3.444078
461.788547	4037.194281	6.943578	-0.088340	3.447433
462.045621	4045.295681	6.948582	-0.088393	3.450800
461.899567	4053.333918	6.953587	-0.088371	3.454124
461.917643	4061.395170	6.958592	-0.088380	3.457460
462.783893	4069.328123	6.963597	-0.088547	3.460768
462.875327	4077.328792	6.968602	-0.088569	3.464075
463.187073	4085.423845	6.973606	-0.088632	3.467424
463.352579	4093.459087	6.978611	-0.088668	3.470742
463.771600	4101.443792	6.983616	-0.088751	3.474043
464.223083	4109.450398	6.988621	-0.088841	3.477352
464.272215	4117.516034	6.993626	-0.088855	3.480668
464.533777	4125.517663	6.998630	-0.088909	3.483961
464.852689	4133.541466	7.003635	-0.088974	3.487263
465.044861	4141.593003	7.008640	-0.089015	3.490569
465.756095	4149.548590	7.013645	-0.089152	3.493849
465.966188	4157.599701	7.018650	-0.089197	3.497148
466.329270	4165.653343	7.023654	-0.089270	3.500451
466.776295	4173.616349	7.028659	-0.089358	3.503716
466.996363	4181.706657	7.033664	-0.089404	3.507022
467.084129	4189.811994	7.038669	-0.089426	3.510327
467.316170	4197.790221	7.043674	-0.089474	3.513582
467.546853	4205.856711	7.048678	-0.089523	3.516870
467.955593	4213.784812	7.053683	-0.089604	3.520104
468.373841	4221.795841	7.058688	-0.089687	3.523369
468.888805	4229.854013	7.063693	-0.089788	3.526653
469.004408	4237.880559	7.068698	-0.089815	3.529909
469.546821	4245.925758	7.073702	-0.089921	3.533182
469.672806	4253.965029	7.078707	-0.089950	3.536437
469.727133	4261.998697	7.083712	-0.089965	3.539685
469.960069	4270.050141	7.088717	-0.090014	3.542942
470.434007	4278.033463	7.093722	-0.090107	3.546176
471.562005	4285.973897	7.098726	-0.090323	3.549410
471.689932	4294.072272	7.103731	-0.090352	3.552674
471.921980	4302.122926	7.108736	-0.090400	3.555918
472.567942	4310.059710	7.113741	-0.090526	3.559127
472.568531	4318.116999	7.118746	-0.090531	3.562361
472.802929	4326.185136	7.123750	-0.090580	3.565604
472.906937	4334.201096	7.128755	-0.090605	3.568819
473.158806	4342.247653	7.133760	-0.090657	3.572048
473.811307	4350.217180	7.138765	-0.090783	3.575255
474.011157	4358.245690	7.143770	-0.090826	3.578469
474.142562	4366.323347	7.148774	-0.090856	3.581698
474.416878	4374.303858	7.153779	-0.090912	3.584889
474.525422	4382.371203	7.158784	-0.090937	3.588107
474.712704	4390.457333	7.163789	-0.090978	3.591332
474.994817	4398.426115	7.168794	-0.091035	3.594510
475.236703	4406.465529	7.173798	-0.091086	3.597713
475.645969	4414.437910	7.178803	-0.091167	3.600890
476.070648	4422.392790	7.183808	-0.091251	3.604058
476.560818	4430.439172	7.188813	-0.091348	3.607262
476.570691	4438.523648	7.193818	-0.091355	3.610464
477.227603	4446.520603	7.198822	-0.091482	3.613647
477.701507	4454.528567	7.203827	-0.091576	3.616826
477.992365	4462.558479	7.208832	-0.091635	3.620006
478.832524	4470.535812	7.213837	-0.091797	3.623177
479.257597	4478.542934	7.218842	-0.091881	3.626346
479.167507	4486.699278	7.223846	-0.091870	3.629556
479.648943	4494.696177	7.228851	-0.091965	3.632717
479.892233	4502.738520	7.233856	-0.092015	3.635886
480.514826	4510.675441	7.238861	-0.092136	3.639022
480.750010	4518.713523	7.243866	-0.092186	3.642183
480.941420	4526.788048	7.248870	-0.092226	3.645355
481.322523	4534.752839	7.253875	-0.092303	3.648487
481.346505	4542.833272	7.258880	-0.092312	3.651651
481.984830	4550.826196	7.263885	-0.092436	3.654795
482.409172	4558.802745	7.268890	-0.092521	3.657923
482.617454	4566.922012	7.273894	-0.092565	3.661100
482.863031	4574.864936	7.278899	-0.092616	3.664205
483.335682	4582.946566	7.283904	-0.092709	3.667368
483.680680	4590.957516	7.288909	-0.092778	3.670497
484.071719	4598.912927	7.293914	-0.092856	3.673603
484.704750	4606.951176	7.298918	-0.092980	3.676745
484.929456	4614.988911	7.303923	-0.093027	3.679873
484.953725	4623.047150	7.308928	-0.093036	3.683002
485.440388	4631.092353	7.313933	-0.093132	3.686134
485.710677	4639.085819	7.318938	-0.093188	3.689238
485.973189	4647.175413	7.323942	-0.093242	3.692377
486.228129	4655.182892	7.328947	-0.093295	3.695481
486.703158	4663.168816	7.333952	-0.093388	3.698579
487.147931	4671.221096	7.338957	-0.093476	3.701700
487.110305	4679.208720	7.343962	-0.093475	3.704781
487.705982	4687.260801	7.348966	-0.093591	3.707900
488.004775	4695.328950	7.353971	-0.093652	3.711015
488.250881	4703.360407	7.358976	-0.093703	3.714112
488.587986	4711.410597	7.363981	-0.093771	3.717216
489.016366	4719.341397	7.368986	-0.093856	3.720274
489.475228	4727.335516	7.373990	-0.093946	3.723354
489.601472	4735.390620	7.378995	-0.093975	3.726447
489.886993	4743.388386	7.384000	-0.094034	3.729519
490.102271	4751.470006	7.389005	-0.094079	3.732619
490.009399	4759.493359	7.394010	-0.094067	3.735686
490.610163	4767.454298	7.399014	-0.094184	3.738744
490.751156	4775.502108	7.404019	-0.094216	3.741821
490.876587	4783.519959	7.409024	-0.094244	3.744884
491.335236	4791.560131	7.414029	-0.094335	3.747961
491.587629	4799.591490	7.419034	-0.094387	3.751028
491.768265	4807.585664	7.424038	-0.094426	3.754075
492.196472	4815.580695	7.429043	-0.094511	3.757127
492.452502	4823.575967	7.434048	-0.094564	3.760172
492.632037	4831.630323	7.439053	-0.094602	3.763235
492.787505	4839.629450	7.444058	-0.094637	3.766274
493.155580	4847.693569	7.449062	-0.094710	3.769340
493.161755	4855.786844	7.454067	-0.094717	3.772406
493.594489	4863.715976	7.459072	-0.094803	3.775417
494.036284	4871.750999	7.464077	-0.094890	3.778467
494.115313	4879.792658	7.469082	-0.094910	3.781507
494.187832	4887.808146	7.474086	-0.094929	3.784536
494.472939	4895.864317	7.479091	-0.094987	3.787582
494.878142	4903.889982	7.484096	-0.095068	3.790617
495.341994	4911.910422	7.489101	-0.095160	3.793649
495.534849	4919.886637	7.494106	-0.095201	3.796655
495.807678	4927.947499	7.499110	-0.095257	3.799693
496.397030	4935.920319	7.504115	-0.095372	3.802702
496.313591	4943.988191	7.509120	-0.095361	3.805729
496.548156	4952.038511	7.514125	-0.095410	3.808755
496.601144	4960.080302	7.519130	-0.095425	3.811771
497.371088	4968.028513	7.524134	-0.095574	3.814765
498.144727	4976.013971	7.529139	-0.095723	3.817771
498.169085	4984.061825	7.534144	-0.095733	3.820781
498.602686	4992.072833	7.539149	-0.095819	3.823784
498.543485	5000.146727	7.544154	-0.095813	3.826798
499.133240	5008.154024	7.549158	-0.095928	3.829798
499.425939	5016.196832	7.554163	-0.095988	3.832802
499.760444	5024.196714	7.559168	-0.096056	3.835790
500.276563	5032.194197	7.564173	-0.096157	3.838777
500.712044	5040.191858	7.569178	-0.096243	3.841761
501.064787	5048.190583	7.574182	-0.096314	3.844741
501.107871	5056.292402	7.579187	-0.096327	3.847750
501.274648	5064.353996	7.584192	-0.096364	3.850745
502.058329	5072.329713	7.589197	-0.096515	3.853718
502.207762	5080.316549	7.594202	-0.096548	3.856680
502.665343	5088.362292	7.599206	-0.096638	3.859668
502.973799	5096.349373	7.604211	-0.096701	3.862629
503.354767	5104.382614	7.609216	-0.096777	3.865605
503.452136	5112.454077	7.614221	-0.096801	3.868588
503.802348	5120.487324	7.619226	-0.096871	3.871560
504.281343	5128.582466	7.624230	-0.096966	3.874554
504.067873	5136.615415	7.629235	-0.096931	3.877510
504.489337	5144.545755	7.634240	-0.097015	3.880438
504.979652	5152.505676	7.639245	-0.097111	3.883376
505.201011	5160.541727	7.644250	-0.097158	3.886334
505.570791	5168.507921	7.649254	-0.097232	3.889268
505.346261	5176.646898	7.654259	-0.097195	3.892250
505.445101	5184.657077	7.659264	-0.097219	3.895190
505.556988	5192.697371	7.664269	-0.097245	3.898139
506.102768	5200.648947	7.669274	-0.097352	3.901061
506.652570	5208.574079	7.674278	-0.097459	3.903972
507.130980	5216.656936	7.679283	-0.097554	3.906937
507.485775	5224.668059	7.684288	-0.097625	3.909870
507.885653	5232.718058	7.689293	-0.097705	3.912817
507.979776	5240.758690	7.694298	-0.097728	3.915752
507.916278	5248.787947	7.699302	-0.097721	3.918678
508.200202	5256.837652	7.704307	-0.097779	3.921615
508.789827	5264.732628	7.709312	-0.097894	3.924500
508.750330	5272.865451	7.714317	-0.097892	3.927457
508.898115	5280.889037	7.719322	-0.097925	3.930376
509.323321	5288.888071	7.724326	-0.098009	3.933289
510.010592	5296.923711	7.729331	-0.098142	3.936217
510.392109	5304.845133	7.734336	-0.098219	3.939097
510.859893	5312.925018	7.739341	-0.098311	3.942033
511.035096	5320.929319	7.744346	-0.098349	3.944934
511.054150	5329.040691	7.749350	-0.098358	3.947869
511.458381	5337.059311	7.754355	-0.098438	3.950775
512.007272	5344.990332	7.759360	-0.098546	3.953651
512.009754	5353.120683	7.764365	-0.098551	3.956586
512.141616	5361.037674	7.769370	-0.098581	3.959444
512.360023	5369.108667	7.774374	-0.098627	3.962357
512.563833	5377.113584	7.779379	-0.098670	3.965244
513.196018	5385.079141	7.784384	-0.098793	3.968122
513.398733	5393.172449	7.789389	-0.098836	3.971036
513.578076	5401.161701	7.794394	-0.098875	3.973911
513.841237	5409.215376	7.799398	-0.098929	3.976808
514.120813	5417.220295	7.804403	-0.098986	3.979685
514.264400	5425.245503	7.809408	-0.099018	3.982566
514.708668	5433.247392	7.814413	-0.099106	3.985441
515.209864	5441.212424	7.819418	-0.099205	3.988301
515.238627	5449.334109	7.824422	-0.099216	3.991208
515.947887	5457.254897	7.829427	-0.099353	3.994052
516.251020	5465.325739	7.834432	-0.099414	3.996941
516.253065	5473.341434	7.839437	-0.099420	3.999803
516.569829	5481.349947	7.844442	-0.099484	4.002665
517.076153	5489.316986	7.849446	-0.099584	4.005514
517.235079	5497.391020	7.854451	-0.099619	4.008393
517.686256	5505.410102	7.859456	-0.099708	4.011256
518.134449	5513.398376	7.864461	-0.099797	4.014105
518.100931	5521.484802	7.869466	-0.099796	4.016979
518.339618	5529.510128	7.874470	-0.099845	4.019834
518.431443	5537.533840	7.879475	-0.099868	4.022683
518.478426	5545.524810	7.884480	-0.099882	4.025519
519.393535	5553.495692	7.889485	-0.100057	4.028359
519.336120	5561.598049	7.894490	-0.100052	4.031228
519.440972	5569.672473	7.899494	-0.100077	4.034088
519.974003	5577.673673	7.904499	-0.100181	4.036926
520.332996	5585.623027	7.909504	-0.100253	4.039742
520.957550	5593.613289	7.914509	-0.100375	4.042574
521.133799	5601.603357	7.919514	-0.100413	4.045397
521.477012	5609.644951	7.924518	-0.100482	4.048238
521.661576	5617.759473	7.929523	-0.100522	4.051101
521.675478	5625.725798	7.934528	-0.100529	4.053907
521.835264	5633.793436	7.939533	-0.100564	4.056749
522.541364	5641.704056	7.944538	-0.100701	4.059542
523.077544	5649.763607	7.949542	-0.100806	4.062383
522.974174	5657.807200	7.954547	-0.100792	4.065206
523.435631	5665.793396	7.959552	-0.100883	4.068016
523.569666	5673.928164	7.964557	-0.100914	4.070871
523.815538	5681.846614	7.969562	-0.100965	4.073650
524.446298	5689.890128	7.974566	-0.101087	4.076476
524.425954	5697.910204	7.979571	-0.101089	4.079283
524.676663	5705.929111	7.984576	-0.101141	4.082091
524.906195	5713.950053	7.989581	-0.101189	4.084898
524.767077	5721.967500	7.994586	-0.101168	4.087696
525.294326	5729.974093	7.999590	-0.101271	4.090498
525.764123	5737.987828	8.004595	-0.101364	4.093300
526.122648	5746.026066	8.009600	-0.101436	4.096107
526.794931	5753.987492	8.014605	-0.101566	4.098889
526.823519	5762.084308	8.019610	-0.101577	4.101707
527.096088	5770.025309	8.024614	-0.101633	4.104473
527.333841	5778.092661	8.029619	-0.101683	4.107281
527.558997	5786.106790	8.034624	-0.101730	4.110067
527.646545	5794.169616	8.039629	-0.101751	4.112867
528.079071	5802.128254	8.044634	-0.101837	4.115633
528.296861	5810.135863	8.049638	-0.101883	4.118412
528.300077	5818.221233	8.054643	-0.101889	4.121213
528.703999	5826.103726	8.059648	-0.101969	4.123947
528.945006	5834.259636	8.064653	-0.102019	4.126771
529.216249	5842.205079	8.069658	-0.102075	4.129521
529.611559	5850.242580	8.074662	-0.102154	4.132303
530.034417	5858.283733	8.079667	-0.102238	4.135084
530.244662	5866.291325	8.084672	-0.102282	4.137850
530.438064	5874.335793	8.089677	-0.102323	4.140625
530.787618	5882.287530	8.094682	-0.102394	4.143369
531.165657	5890.334358	8.099686	-0.102469	4.146144
531.233687	5898.359918	8.104691	-0.102487	4.148907
531.644891	5906.377511	8.109696	-0.102569	4.151668
531.914945	5914.392986	8.114701	-0.102625	4.154426
531.996745	5922.451581	8.119706	-0.102645	4.157194
532.054894	5930.470924	8.124710	-0.102661	4.159946
532.477177	5938.481783	8.129715	-0.102745	4.162698
532.623474	5946.451354	8.134720	-0.102777	4.165431
532.897728	5954.464602	8.139725	-0.102834	4.168178
533.047683	5962.526835	8.144730	-0.102867	4.170939
533.288515	5970.552973	8.149734	-0.102917	4.173686
533.686045	5978.569964	8.154739	-0.102996	4.176431
534.065605	5986.541810	8.159744	-0.103072	4.179158
534.262025	5994.636905	8.164749	-0.103114	4.181923
534.478276	6002.635139	8.169754	-0.103160	4.184654
534.379663	6010.696951	8.174758	-0.103146	4.187401
534.976839	6018.694864	8.179763	-0.103263	4.190132
535.215137	6026.741400	8.184768	-0.103313	4.192873
535.526079	6034.781722	8.189773	-0.103376	4.195612
535.715301	6042.702826	8.194778	-0.103416	4.198307
535.829385	6050.774050	8.199782	-0.103443	4.201050
536.078441	6058.756066	8.204787	-0.103494	4.203763
536.269802	6066.784794	8.209792	-0.103535	4.206489
536.450651	6074.822839	8.214797	-0.103574	4.209216
536.977373	6082.785083	8.219802	-0.103677	4.211920
537.308295	6090.820676	8.224806	-0.103744	4.214645
537.694360	6098.834955	8.229811	-0.103821	4.217361
537.621835	6106.853247	8.234816	-0.103813	4.220072
537.507489	6114.889064	8.239821	-0.103797	4.222786
538.229367	6122.887475	8.244826	-0.103937	4.225495
538.511820	6130.908545	8.249830	-0.103994	4.228205
538.364821	6139.022085	8.254835	-0.103972	4.230941
538.444459	6146.934745	8.259840	-0.103992	4.233609
538.901276	6155.004216	8.264845	-0.104083	4.236332
539.274756	6162.916448	8.269850	-0.104157	4.238999
539.630017	6171.004239	8.274854	-0.104229	4.241724
539.720650	6178.949165	8.279859	-0.104251	4.244396
539.919630	6187.031657	8.284864	-0.104293	4.247113
540.390258	6195.047309	8.289869	-0.104386	4.249810
540.589134	6203.084510	8.294874	-0.104428	4.252509
540.786967	6211.090618	8.299878	-0.104470	4.255195
541.136405	6219.060262	8.304883	-0.104541	4.257870
540.873685	6227.137314	8.309888	-0.104497	4.260572
541.188882	6235.144305	8.314893	-0.104561	4.263255
541.415149	6243.170172	8.319898	-0.104608	4.265942
541.796524	6251.162315	8.324902	-0.104685	4.268618
541.756760	6259.281582	8.329907	-0.104683	4.271330
542.179594	6267.180035	8.334912	-0.104766	4.273971
542.386030	6275.257926	8.339917	-0.104810	4.276668
542.446539	6283.231628	8.344922	-0.104827	4.279327
542.976769	6291.224887	8.349926	-0.104931	4.281995
542.889015	6299.282966	8.354931	-0.104920	4.284678
542.901589	6307.299310	8.359936	-0.104927	4.287346
543.364808	6315.306006	8.364941	-0.105019	4.290013
543.638523	6323.323762	8.369946	-0.105075	4.292681
544.092644	6331.294949	8.374950	-0.105165	4.295333
544.358950	6339.378616	8.379955	-0.105219	4.298018
544.452538	6347.347603	8.384960	-0.105242	4.300663
544.710356	6355.356005	8.389965	-0.105295	4.303320
544.910299	6363.402967	8.394970	-0.105338	4.305989
545.448991	6371.433374	8.399974	-0.105443	4.308652
545.824203	6379.464522	8.404979	-0.105518	4.311313
546.357124	6387.422331	8.409984	-0.105623	4.313949
546.517161	6395.478385	8.414989	-0.105658	4.316613
546.919696	6403.427754	8.419994	-0.105738	4.319242
546.994241	6411.493095	8.424998	-0.105757	4.321905
547.354469	6419.479052	8.430003	-0.105830	4.324543
547.536543	6427.526323	8.435008	-0.105869	4.327198
547.933867	6435.542320	8.440013	-0.105948	4.329842
548.091284	6443.538587	8.445018	-0.105982	4.332476
548.395977	6451.567730	8.450022	-0.106044	4.335121
548.545367	6459.596892	8.455027	-0.106078	4.337763
548.740233	6467.567284	8.460032	-0.106119	4.340384
549.192716	6475.602423	8.465037	-0.106209	4.343027
549.505304	6483.651454	8.470042	-0.106272	4.345671
549.718461	6491.650591	8.475046	-0.106317	4.348297
550.035739	6499.721923	8.480051	-0.106381	4.350946
550.099861	6507.756114	8.485056	-0.106398	4.353579
550.197238	6515.840267	8.490061	-0.106422	4.356227
550.431994	6523.701284	8.495066	-0.106471	4.358802
550.667176	6531.784731	8.500070	-0.106520	4.361447
550.925434	6539.727494	8.505075	-0.106573	4.364045
550.977539	6547.751995	8.510080	-0.106588	4.366667
551.186116	6555.802071	8.515085	-0.106632	4.369297
551.310307	6563.830079	8.520090	-0.106660	4.371917
551.694931	6571.761986	8.525094	-0.106737	4.374506
551.978904	6579.857901	8.530099	-0.106795	4.377146
552.286987	6587.831788	8.535104	-0.106858	4.379746
552.227837	6595.951027	8.540109	-0.106852	4.382388
552.367176	6603.947498	8.545114	-0.106883	4.384990
552.738954	6611.986629	8.550118	-0.106958	4.387606
552.894675	6620.048237	8.555123	-0.106992	4.390226
552.952808	6628.027108	8.560128	-0.107008	4.392818
553.212439	6636.041651	8.565133	-0.107062	4.395420
553.387586	6644.047189	8.570138	-0.107100	4.398018
553.658035	6652.084724	8.575143	-0.107155	4.400625
554.047419	6660.048861	8.580147	-0.107233	4.403207
554.104935	6668.114364	8.585152	-0.107249	4.405818
554.217967	6676.186611	8.590157	-0.107275	4.408431
554.103023	6684.213549	8.595162	-0.107259	4.411026
554.223575	6692.203474	8.600167	-0.107287	4.413609
554.573593	6700.291922	8.605171	-0.107357	4.416223
554.515797	6708.218930	8.610176	-0.107352	4.418782
554.943393	6716.283855	8.615181	-0.107437	4.421386
555.263398	6724.189833	8.620186	-0.107501	4.423936
555.436971	6732.300575	8.625191	-0.107539	4.426551
555.480427	6740.296066	8.630195	-0.107552	4.429126
555.804781	6748.351990	8.635200	-0.107618	4.431720
556.284752	6756.288029	8.640205	-0.107712	4.434275
556.207607	6764.353939	8.645210	-0.107703	4.436868
556.511461	6772.323533	8.650215	-0.107765	4.439429
556.478396	6780.400140	8.655219	-0.107764	4.442023
556.826077	6788.318207	8.660224	-0.107834	4.444565
556.798092	6796.425574	8.665229	-0.107834	4.447165
557.396555	6804.400105	8.670234	-0.107951	4.449724
557.645038	6812.396112	8.675239	-0.108002	4.452287
557.897355	6820.449454	8.680243	-0.108055	4.454866
558.148217	6828.439270	8.685248	-0.108107	4.457423
558.229127	6836.497608	8.690253	-0.108127	4.460001
558.231946	6844.516738	8.695258	-0.108133	4.462564
558.645359	6852.456875	8.700263	-0.108215	4.465101
558.798567	6860.502897	8.705267	-0.108249	4.467671
558.987132	6868.507163	8.710272	-0.108289	4.470225
559.100258	6876.582657	8.715277	-0.108315	4.472800
559.156410	6884.558705	8.720282	-0.108331	4.475342
559.467118	6892.546026	8.725287	-0.108394	4.477887
559.474459	6900.605425	8.730291	-0.108401	4.480453
559.883078	6908.538094	8.735296	-0.108482	4.482978
560.141107	6916.636272	8.740301	-0.108535	4.485553
560.070167	6924.635831	8.745306	-0.108527	4.488095
560.320287	6932.657948	8.750311	-0.108579	4.490643
560.588983	6940.687477	8.755315	-0.108634	4.493193
560.605210	6948.738189	8.760320	-0.108643	4.495747
560.708359	6956.699976	8.765325	-0.108667	4.498271
561.192396	6964.747086	8.770330	-0.108763	4.500822
561.148518	6972.724468	8.775335	-0.108760	4.503348
561.167650	6980.813243	8.780339	-0.108768	4.505908
561.245242	6988.786597	8.785344	-0.108788	4.508431
561.728765	6996.830687	8.790349	-0.108883	4.510975
562.057777	7004.768294	8.795354	-0.108950	4.513484
562.272732	7012.807439	8.800359	-0.108995	4.516023
562.383843	7020.784850	8.805363	-0.109021	4.518541
562.730463	7028.781512	8.810368	-0.109091	4.521064
562.754290	7036.816287	8.815373	-0.109100	4.523597
563.121121	7044.831869	8.820378	-0.109174	4.526123
563.233588	7052.826412	8.825383	-0.109200	4.528641
563.054266	7060.937954	8.830387	-0.109172	4.531193
563.436407	7068.875838	8.835392	-0.109248	4.533691
563.722911	7076.981917	8.840397	-0.109307	4.536240
563.687886	7084.930070	8.845402	-0.109306	4.538737
564.036215	7092.977274	8.850407	-0.109376	4.541264
564.169220	7100.956990	8.855411	-0.109406	4.543769
564.386239	7108.945570	8.860416	-0.109451	4.546275
564.379992	7117.024823	8.865421	-0.109456	4.548807
564.450028	7125.046288	8.870426	-0.109474	4.551321
564.666150	7133.036396	8.875431	-0.109519	4.553823
565.079213	7141.106629	8.880435	-0.109602	4.556349
565.081811	7148.994227	8.885440	-0.109607	4.558816
565.099837	7157.114790	8.890445	-0.109616	4.561355
565.485452	7165.017962	8.895450	-0.109693	4.563824
565.422534	7173.120979	8.900455	-0.109686	4.566355
566.111091	7181.103545	8.905459	-0.109820	4.568847
565.873361	7189.166397	8.910464	-0.109781	4.571361
566.185420	7197.141844	8.915469	-0.109844	4.573848
566.170318	7205.206439	8.920474	-0.109847	4.576361
566.671317	7213.122796	8.925479	-0.109945	4.578826
566.871487	7221.239536	8.930483	-0.109988	4.581353
566.727949	7229.172447	8.935488	-0.109966	4.583820
567.279703	7237.243590	8.940493	-0.110074	4.586330
567.416664	7245.260549	8.945498	-0.110105	4.588821
567.627106	7253.301792	8.950503	-0.110149	4.591318
567.857095	7261.297132	8.955507	-0.110197	4.593800
567.907671	7269.324608	8.960512	-0.110212	4.596290
568.073671	7277.278584	8.965517	-0.110248	4.598756
568.277683	7285.330532	8.970522	-0.110291	4.601251
568.519417	7293.248699	8.975527	-0.110342	4.603703
568.503318	7301.373541	8.980531	-0.110344	4.606218
568.478451	7309.353439	8.985536	-0.110344	4.608687
568.387831	7317.451864	8.990541	-0.110333	4.611191
568.634888	7325.361102	8.995546	-0.110384	4.613635
568.772989	7333.397137	9.000551	-0.110415	4.616117
568.893061	7341.404196	9.005555	-0.110443	4.618588
569.114555	7349.416507	9.010560	-0.110489	4.621060
569.471452	7357.410812	9.015565	-0.110561	4.623526
569.621242	7365.475525	9.020570	-0.110594	4.626011
569.527638	7373.513317	9.025575	-0.110582	4.628487
570.099638	7381.563345	9.030579	-0.110693	4.630965
569.962335	7389.511371	9.035584	-0.110673	4.633410
570.356800	7397.550968	9.040589	-0.110752	4.635883
570.414510	7405.530888	9.045594	-0.110768	4.638335
570.472300	7413.562841	9.050599	-0.110784	4.640803
570.654514	7421.540199	9.055603	-0.110823	4.643252
570.872375	7429.557499	9.060608	-0.110869	4.645712
571.170950	7437.628109	9.065613	-0.110930	4.648187
571.350174	7445.576659	9.070618	-0.110968	4.650624
571.516191	7453.645635	9.075623	-0.111004	4.653096
571.529091	7461.718711	9.080627	-0.111012	4.655568
571.459163	7469.683688	9.085632	-0.111004	4.658005
571.714805	7477.685155	9.090637	-0.111057	4.660453
571.657710	7485.741287	9.095642	-0.111052	4.662916
572.250940	7493.683718	9.100647	-0.111167	4.665342
572.318219	7501.774304	9.105651	-0.111185	4.667813
572.073408	7509.779298	9.110656	-0.111145	4.670256
572.367661	7517.887308	9.115661	-0.111205	4.672730
572.617229	7525.872593	9.120666	-0.111257	4.675164
572.723851	7533.845250	9.125671	-0.111282	4.677594
572.886027	7541.843836	9.130675	-0.111317	4.680030
572.921612	7549.797958	9.135680	-0.111329	4.682451
573.214481	7557.792160	9.140685	-0.111389	4.684883
573.630544	7565.813755	9.145690	-0.111471	4.687322
573.292610	7573.882568	9.150695	-0.111414	4.689775
573.972924	7581.944804	9.155699	-0.111546	4.692223
574.014069	7589.897343	9.160704	-0.111559	4.694638
574.088117	7597.984855	9.165709	-0.111578	4.697092
574.194311	7605.915158	9.170714	-0.111603	4.699497
574.306241	7613.973216	9.175719	-0.111629	4.701940
574.394360	7622.007555	9.180723	-0.111650	4.704374
574.871009	7629.934931	9.185728	-0.111744	4.706774
575.249952	7638.022779	9.190733	-0.111820	4.709221
575.205303	7646.100999	9.195738	-0.111817	4.711665
575.834349	7653.960511	9.200743	-0.111939	4.714041
575.891886	7662.079824	9.205747	-0.111955	4.716494
576.285663	7669.956521	9.210752	-0.112034	4.718872
576.628998	7678.083188	9.215757	-0.112103	4.721325
576.553469	7686.046646	9.220762	-0.112094	4.723728
576.767281	7694.098082	9.225767	-0.112139	4.726156
577.054197	7702.131512	9.230771	-0.112198	4.728577
576.966155	7710.211865	9.235776	-0.112187	4.731011
577.142716	7718.187498	9.240781	-0.112225	4.733412
577.663198	7726.256195	9.245786	-0.112327	4.735839
577.598963	7734.241287	9.250791	-0.112320	4.738241
577.757809	7742.308152	9.255795	-0.112355	4.740666
577.692612	7750.239035	9.260800	-0.112348	4.743050
577.878535	7758.309229	9.265805	-0.112388	4.745473
578.078862	7766.321342	9.270810	-0.112431	4.747877
578.459963	7774.271640	9.275815	-0.112507	4.750262
578.502496	7782.411339	9.280819	-0.112520	4.752703
578.468837	7790.373214	9.285824	-0.112519	4.755089
578.626244	7798.372257	9.290829	-0.112554	4.757485
579.141876	7806.344614	9.295834	-0.112655	4.759870
579.168308	7814.353687	9.300839	-0.112665	4.762267
579.140893	7822.343278	9.305843	-0.112665	4.764657
579.350370	7830.390600	9.310848	-0.112709	4.767062
579.396561	7838.458058	9.315853	-0.112723	4.769473
579.668755	7846.461035	9.320858	-0.112779	4.771862
579.790454	7854.422496	9.325863	-0.112807	4.774238
580.122426	7862.547397	9.330867	-0.112874	4.776661
580.101413	7870.444140	9.335872	-0.112875	4.779016
580.326478	7878.528959	9.340877	-0.112923	4.781425
580.519422	7886.509593	9.345882	-0.112964	4.783802
580.589035	7894.502200	9.350887	-0.112982	4.786181
580.947614	7902.554893	9.355891	-0.113054	4.788576
580.823265	7910.559447	9.360896	-0.113036	4.790958
581.213695	7918.584026	9.365901	-0.113114	4.793342
581.135612	7926.603481	9.370906	-0.113105	4.795726
581.296388	7934.568039	9.375911	-0.113140	4.798090
581.649877	7942.638073	9.380915	-0.113211	4.800485
581.306502	7950.584886	9.385920	-0.113152	4.802844
581.527893	7958.626491	9.390925	-0.113199	4.805228
581.695979	7966.688291	9.395930	-0.113235	4.807617
581.960350	7974.665951	9.400935	-0.113290	4.809979
581.911782	7982.681088	9.405939	-0.113286	4.812353
582.106060	7990.145595	9.410944	-0.113327	4.814562
582.421705	7994.851172	9.415949	-0.113389	4.815952

582.690949	7997.394559	9.420954	-0.113441	4.816704
582.797183	7998.801114	9.425959	-0.113461	4.817119
583.077913	7999.245486	9.430963	-0.113514	4.817249
583.148530	8000.319128	9.435968	-0.113528	4.817566
583.070352	8000.296852	9.440973	-0.113513	4.817560
583.402684	8000.294406	9.445978	-0.113575	4.817558
583.356516	8000.318003	9.450983	-0.113566	4.817565
583.138345	8000.382326	9.455987	-0.113526	4.817585
583.439596	8000.278067	9.460992	-0.113582	4.817553
583.798005	8000.280233	9.465997	-0.113649	4.817552
583.893391	8000.295378	9.471002	-0.113666	4.817556
583.739025	8000.303640	9.476007	-0.113638	4.817559
584.005497	8000.345613	9.481011	-0.113687	4.817571
583.834436	8000.333567	9.486016	-0.113656	4.817568
583.575551	8000.398340	9.491021	-0.113607	4.817588
583.528823	8000.372308	9.496026	-0.113599	4.817581
583.864366	8000.365689	9.501031	-0.113661	4.817577
583.698669	8000.467744	9.506035	-0.113630	4.817608
583.759635	8000.376802	9.511040	-0.113642	4.817581
584.107624	8000.347141	9.516045	-0.113707	4.817571
584.345913	8000.342243	9.521050	-0.113751	4.817568
584.169709	8000.317451	9.526055	-0.113718	4.817561
584.342435	8000.406595	9.531059	-0.113750	4.817587
584.144379	8000.382533	9.536064	-0.113713	4.817581
584.070937	8000.414170	9.541069	-0.113700	4.817591
584.509676	8000.370025	9.546074	-0.113781	4.817576
584.577107	8000.347803	9.551079	-0.113794	4.817569
584.714254	8000.347734	9.556083	-0.113820	4.817568
584.798654	8000.342657	9.561088	-0.113835	4.817566
585.054820	8000.395037	9.566093	-0.113883	4.817581
585.138656	8000.326605	9.571098	-0.113899	4.817560
584.931993	8000.306637	9.576103	-0.113860	4.817555
584.666580	8000.439939	9.581107	-0.113811	4.817596
584.558414	8000.422493	9.586112	-0.113791	4.817591
584.805819	8000.402950	9.591117	-0.113837	4.817584
584.895159	8000.393723	9.596122	-0.113853	4.817581
584.942477	8000.339528	9.601127	-0.113862	4.817565
584.947251	8000.434621	9.606131	-0.113863	4.817593
584.985234	8000.338056	9.611136	-0.113870	4.817564
585.458100	8000.303921	9.616141	-0.113958	4.817552
585.294144	8000.417618	9.621146	-0.113928	4.817586
585.221211	8000.363744	9.626151	-0.113914	4.817571
585.065734	8000.450117	9.631155	-0.113885	4.817597
585.149885	8000.396470	9.636160	-0.113901	4.817581
585.098377	8000.418931	9.641165	-0.113891	4.817587
585.376555	8000.379787	9.646170	-0.113943	4.817575
585.498507	8000.379493	9.651175	-0.113966	4.817574
585.449267	8000.412546	9.656179	-0.113957	4.817584
585.554935	8000.304318	9.661184	-0.113976	4.817551
585.455452	8000.306005	9.666189	-0.113958	4.817552
585.314313	8000.322909	9.671194	-0.113932	4.817558
585.419814	8000.337151	9.676199	-0.113951	4.817562
585.722798	8000.336385	9.681203	-0.114008	4.817560
585.472451	8000.356942	9.686208	-0.113961	4.817567
585.415029	8000.437384	9.691213	-0.113951	4.817591
585.476957	8000.355955	9.696218	-0.113962	4.817567
585.706397	8000.319253	9.701223	-0.114005	4.817555
585.932374	8000.403917	9.706227	-0.114047	4.817579
585.760392	8000.310557	9.711232	-0.114015	4.817552
585.636305	8000.365724	9.716237	-0.113992	4.817569
585.773713	8000.350878	9.721242	-0.114017	4.817564
585.985501	8000.327639	9.726247	-0.114057	4.817556
586.143788	8000.335276	9.731251	-0.114086	4.817558
586.245615	8000.291394	9.736256	-0.114105	4.817545
586.296052	8000.334379	9.741261	-0.114115	4.817557
586.185217	8000.315837	9.746266	-0.114094	4.817552
586.130264	8000.289680	9.751271	-0.114084	4.817545
585.959404	8000.339927	9.756275	-0.114052	4.817560
585.873276	8000.313306	9.761280	-0.114036	4.817553
585.805555	8000.402042	9.766285	-0.114023	4.817579
585.984414	8000.385703	9.771290	-0.114057	4.817574
585.927706	8000.381692	9.776295	-0.114046	4.817573
585.782608	8000.406983	9.781299	-0.114019	4.817581
586.109929	8000.324227	9.786304	-0.114080	4.817555
586.110928	8000.360141	9.791309	-0.114080	4.817566
586.144938	8000.380709	9.796314	-0.114087	4.817571
586.278002	8000.319344	9.801319	-0.114111	4.817553
586.558316	8000.343581	9.806323	-0.114164	4.817559
586.141572	8000.404946	9.811328	-0.114086	4.817579
585.986974	8000.404756	9.816333	-0.114057	4.817579
585.881066	8000.415850	9.821338	-0.114038	4.817583
586.205584	8000.325662	9.826343	-0.114098	4.817555
586.146369	8000.334283	9.831347	-0.114087	4.817558
586.335294	8000.286419	9.836352	-0.114122	4.817543
585.939717	8000.437844	9.841357	-0.114049	4.817589
585.737505	8000.448559	9.846362	-0.114011	4.817593
585.947192	8000.396781	9.851367	-0.114050	4.817577
586.198090	8000.412134	9.856371	-0.114097	4.817581
586.017353	8000.350317	9.861376	-0.114063	4.817563
586.185292	8000.354932	9.866381	-0.114094	4.817564
586.757520	8000.345509	9.871386	-0.114201	4.817558
586.606559	8000.309475	9.876391	-0.114173	4.817548
586.503607	8000.329058	9.881395	-0.114154	4.817555
585.899768	8000.476325	9.886400	-0.114041	4.817601
586.320485	8000.476259	9.891405	-0.114120	4.817599
586.570868	8000.429312	9.896410	-0.114166	4.817584
586.367748	8000.399891	9.901415	-0.114129	4.817576
586.519578	8000.441220	9.906419	-0.114157	4.817588
586.587942	8000.347215	9.911424	-0.114170	4.817560
586.444196	8000.330293	9.916429	-0.114143	4.817555
586.629547	8000.375289	9.921434	-0.114177	4.817568
586.527461	8000.327313	9.926439	-0.114158	4.817554
586.593010	8000.393752	9.931443	-0.114171	4.817573
586.068881	8000.447182	9.936448	-0.114073	4.817591
586.198183	8000.442775	9.941453	-0.114097	4.817590
586.063354	8000.468218	9.946458	-0.114072	4.817598
586.393599	8000.418237	9.951463	-0.114134	4.817581
586.547444	8000.482824	9.956467	-0.114162	4.817600
586.471294	8000.479579	9.961472	-0.114148	4.817599
586.207396	8000.404908	9.966477	-0.114099	4.817578
586.357830	8000.530682	9.971482	-0.114127	4.817615
586.596766	8000.445554	9.976487	-0.114171	4.817589
586.850122	8000.447219	9.981491	-0.114219	4.817588
586.700212	8000.410144	9.986496	-0.114191	4.817578
586.994901	8000.354354	9.991501	-0.114246	4.817560
586.790146	8000.342858	9.996506	-0.114207	4.817557
586.772974	8000.256025	10.001511	-0.114204	4.817532
587.117159	8000.340342	10.006515	-0.114268	4.817555
587.255654	8000.284336	10.011520	-0.114294	4.817538
587.078130	8000.292250	10.016525	-0.114261	4.817541
587.094296	8000.306218	10.021530	-0.114264	4.817545
587.205813	8000.278318	10.026535	-0.114285	4.817537
587.256211	8000.302298	10.031539	-0.114294	4.817543
586.931415	8000.291125	10.036544	-0.114234	4.817542
586.883591	8000.353763	10.041549	-0.114225	4.817560
587.027218	8000.313671	10.046554	-0.114252	4.817548
586.834459	8000.332973	10.051559	-0.114216	4.817554
587.073804	8000.340764	10.056563	-0.114260	4.817556
587.254073	8000.310720	10.061568	-0.114294	4.817546
586.985271	8000.379568	10.066573	-0.114244	4.817567
587.114648	8000.368828	10.071578	-0.114268	4.817564
586.929516	8000.379796	10.076583	-0.114234	4.817568
586.768323	8000.452359	10.081587	-0.114204	4.817590
586.761913	8000.344570	10.086592	-0.114202	4.817558
587.092887	8000.341056	10.091597	-0.114264	4.817556
586.954622	8000.360114	10.096602	-0.114238	4.817562
586.904350	8000.313965	10.101607	-0.114229	4.817548
586.993220	8000.424042	10.106611	-0.114246	4.817581
586.937804	8000.425329	10.111616	-0.114235	4.817581
586.680551	8000.413050	10.116621	-0.114187	4.817579
587.110398	8000.379335	10.121626	-0.114267	4.817567
587.170880	8000.351730	10.126631	-0.114279	4.817558
587.276384	8000.350136	10.131635	-0.114298	4.817557
587.054539	8000.356333	10.136640	-0.114257	4.817560
587.155795	8000.355732	10.141645	-0.114276	4.817560
587.180416	8000.394110	10.146650	-0.114281	4.817571
587.168184	8000.317909	10.151655	-0.114278	4.817548
587.205876	8000.394492	10.156659	-0.114285	4.817571
587.011130	8000.337743	10.161664	-0.114249	4.817555
587.414508	8000.321583	10.166669	-0.114324	4.817548
587.343683	8000.383879	10.171674	-0.114311	4.817567
587.212016	8000.389309	10.176679	-0.114287	4.817569
587.046427	8000.400568	10.181683	-0.114256	4.817573
586.947793	8000.384318	10.186688	-0.114237	4.817569
587.326996	8000.328732	10.191693	-0.114308	4.817551
587.251930	8000.360345	10.196698	-0.114294	4.817561
586.920166	8000.349067	10.201703	-0.114232	4.817559
587.232230	8000.373780	10.206707	-0.114290	4.817565
587.374169	8000.336830	10.211712	-0.114317	4.817553
587.502109	8000.332403	10.216717	-0.114341	4.817551
587.211742	8000.379813	10.221722	-0.114287	4.817566
587.451661	8000.343268	10.226727	-0.114331	4.817555
587.627179	8000.353276	10.231731	-0.114364	4.817557
587.596130	8000.368653	10.236736	-0.114358	4.817561
587.278226	8000.394535	10.241741	-0.114299	4.817571
587.099044	8000.472110	10.246746	-0.114266	4.817594
587.340383	8000.389129	10.251751	-0.114311	4.817569
587.600318	8000.397228	10.256755	-0.114359	4.817570
587.597452	8000.369734	10.261760	-0.114359	4.817562
587.542175	8000.376302	10.266765	-0.114348	4.817564
587.409523	8000.393332	10.271770	-0.114324	4.817570
587.429917	8000.396804	10.276775	-0.114327	4.817571
587.884007	8000.338111	10.281779	-0.114412	4.817551
587.493424	8000.350240	10.286784	-0.114339	4.817556
587.214527	8000.384095	10.291789	-0.114287	4.817568
587.721146	8000.362084	10.296794	-0.114382	4.817559
587.646055	8000.326123	10.301799	-0.114368	4.817549
587.578045	8000.407466	10.306803	-0.114355	4.817573
587.702815	8000.320636	10.311808	-0.114378	4.817547
588.024399	8000.305369	10.316813	-0.114438	4.817541
587.923302	8000.378829	10.321818	-0.114419	4.817563
587.703662	8000.309038	10.326823	-0.114378	4.817543
587.956068	8000.327583	10.331827	-0.114426	4.817548
587.878522	8000.304256	10.336832	-0.114411	4.817541
587.742138	8000.280051	10.341837	-0.114386	4.817535
587.444244	8000.397035	10.346842	-0.114330	4.817571
587.371319	8000.355827	10.351847	-0.114317	4.817559
587.590211	8000.428777	10.356851	-0.114358	4.817579
587.486025	8000.381823	10.361856	-0.114338	4.817566
587.658204	8000.372777	10.366861	-0.114370	4.817562
587.563140	8000.369249	10.371866	-0.114353	4.817562
587.449915	8000.374954	10.376871	-0.114331	4.817564
587.591456	8000.391846	10.381875	-0.114358	4.817568
587.610043	8000.402683	10.386880	-0.114361	4.817571
587.898388	8000.347855	10.391885	-0.114415	4.817554
588.034440	8000.316097	10.396890	-0.114440	4.817544
588.078613	8000.292472	10.401895	-0.114449	4.817537
588.214121	8000.326169	10.406899	-0.114474	4.817546
587.891739	8000.313973	10.411904	-0.114414	4.817544
587.922119	8000.338712	10.416909	-0.114419	4.817551
587.833037	8000.362726	10.421914	-0.114403	4.817559
587.647556	8000.338845	10.426919	-0.114368	4.817552
587.440015	8000.435003	10.431923	-0.114330	4.817582
587.443838	8000.367487	10.436928	-0.114330	4.817562
587.456844	8000.431032	10.441933	-0.114333	4.817581
587.460045	8000.421579	10.446938	-0.114334	4.817578
587.236135	8000.448862	10.451943	-0.114292	4.817587
587.126740	8000.408167	10.456947	-0.114272	4.817575
587.237555	8000.505901	10.461952	-0.114292	4.817604
587.387039	8000.483846	10.466957	-0.114320	4.817596
587.737118	8000.396151	10.471962	-0.114385	4.817569
587.395172	8000.419563	10.476967	-0.114322	4.817577
587.799569	8000.426649	10.481971	-0.114397	4.817578
587.407617	8000.380685	10.486976	-0.114324	4.817566
587.417131	8000.453681	10.491981	-0.114326	4.817587
587.863698	8000.388542	10.496986	-0.114409	4.817566
587.930924	8000.365260	10.501991	-0.114421	4.817559
588.188398	8000.388106	10.506995	-0.114469	4.817565
587.689293	8000.417621	10.512000	-0.114376	4.817576
587.671466	8000.427915	10.517005	-0.114373	4.817579
587.905896	8000.417685	10.522010	-0.114417	4.817575
587.560309	8000.373468	10.527015	-0.114352	4.817563
587.537227	8000.433308	10.532019	-0.114348	4.817581
587.495919	8000.430582	10.537024	-0.114341	4.817580
587.579885	8000.400159	10.542029	-0.114356	4.817571
587.805163	8000.444697	10.547034	-0.114398	4.817583
587.630620	8000.394583	10.552039	-0.114366	4.817569
587.824423	8000.404864	10.557043	-0.114402	4.817571
587.623128	8000.408200	10.562048	-0.114364	4.817573
588.000524	8000.434944	10.567053	-0.114435	4.817579
588.034718	8000.402724	10.572058	-0.114441	4.817570
587.649077	8000.365300	10.577063	-0.114369	4.817560
587.375835	8000.415077	10.582067	-0.114318	4.817576
586.959897	8000.515519	10.587072	-0.114241	4.817608
587.561780	8000.402013	10.592077	-0.114353	4.817571
587.218070	8000.555268	10.597082	-0.114289	4.817618
587.097364	8000.392982	10.602087	-0.114266	4.817571
587.775599	8000.441103	10.607091	-0.114393	4.817582
587.555886	8000.421991	10.612096	-0.114352	4.817577
587.737616	8000.423646	10.617101	-0.114386	4.817577
587.761318	8000.500022	10.622106	-0.114390	4.817600
587.463450	8000.519867	10.627111	-0.114335	4.817607
587.751156	8000.393231	10.632115	-0.114388	4.817568
587.813180	8000.388878	10.637120	-0.114400	4.817566
588.023296	8000.379341	10.642125	-0.114439	4.817563
587.950507	8000.463782	10.647130	-0.114426	4.817588
587.635031	8000.394673	10.652135	-0.114367	4.817569
587.911891	8000.417807	10.657139	-0.114418	4.817575
587.798438	8000.443569	10.662144	-0.114397	4.817583
587.502399	8000.509899	10.667149	-0.114342	4.817604
587.623909	8000.426187	10.672154	-0.114365	4.817578
587.652333	8000.395992	10.677159	-0.114370	4.817569
588.209389	8000.440198	10.682163	-0.114474	4.817580
588.084228	8000.412992	10.687168	-0.114451	4.817572
587.681654	8000.437611	10.692173	-0.114376	4.817581
587.476885	8000.415555	10.697178	-0.114337	4.817576
587.742776	8000.383621	10.702183	-0.114387	4.817565
587.888137	8000.386845	10.707187	-0.114414	4.817566
587.809325	8000.411011	10.712192	-0.114399	4.817573
587.530169	8000.443806	10.717197	-0.114347	4.817584
587.820723	8000.476647	10.722202	-0.114402	4.817592
587.838305	8000.445235	10.727207	-0.114405	4.817583
587.738241	8000.508151	10.732211	-0.114386	4.817602
587.872141	8000.387669	10.737216	-0.114411	4.817566
587.869261	8000.468929	10.742221	-0.114411	4.817590
587.667637	8000.491264	10.747226	-0.114373	4.817597
587.248683	8000.510360	10.752231	-0.114295	4.817605
587.846049	8000.504486	10.757235	-0.114406	4.817601
587.983629	8000.485421	10.762240	-0.114432	4.817594
588.011821	8000.371809	10.767245	-0.114437	4.817561
587.683897	8000.460893	10.772250	-0.114376	4.817588
587.725284	8000.424556	10.777255	-0.114384	4.817577
588.220159	8000.464668	10.782259	-0.114476	4.817587
587.796529	8000.517481	10.787264	-0.114397	4.817605
587.783606	8000.384251	10.792269	-0.114395	4.817565
587.572611	8000.508865	10.797274	-0.114356	4.817603
587.373177	8000.534401	10.802279	-0.114319	4.817611
587.735092	8000.418375	10.807283	-0.114386	4.817576
587.699590	8000.448466	10.812288	-0.114379	4.817585
587.923039	8000.402173	10.817293	-0.114421	4.817570
587.978504	8000.520203	10.822298	-0.114431	4.817605
587.796332	8000.509040	10.827303	-0.114397	4.817602
587.508509	8000.458293	10.832307	-0.114344	4.817588
587.857257	8000.481443	10.837312	-0.114409	4.817594
587.858755	8000.479355	10.842317	-0.114409	4.817593
588.067042	8000.498300	10.847322	-0.114448	4.817598
587.879733	8000.427933	10.852327	-0.114413	4.817578
588.125752	8000.385144	10.857331	-0.114459	4.817564
588.190424	8000.417786	10.862336	-0.114471	4.817573
588.380025	8000.445955	10.867341	-0.114506	4.817581
588.057476	8000.541454	10.872346	-0.114446	4.817611
588.033231	8000.469294	10.877351	-0.114442	4.817589
587.979090	8000.465321	10.882355	-0.114432	4.817588
588.102952	8000.488286	10.887360	-0.114455	4.817595
588.246827	8000.392237	10.892365	-0.114481	4.817566
588.240986	8000.451280	10.897370	-0.114480	4.817583
588.158068	8000.480665	10.902375	-0.114465	4.817592
588.299087	8000.377182	10.907379	-0.114491	4.817561
588.107668	8000.477804	10.912384	-0.114456	4.817591
587.911288	8000.528726	10.917389	-0.114419	4.817607
588.047103	8000.549758	10.922394	-0.114444	4.817613
588.126263	8000.350325	10.927399	-0.114459	4.817554
587.976254	8000.446285	10.932403	-0.114431	4.817583
587.861848	8000.475200	10.937408	-0.114410	4.817592
587.857961	8000.484646	10.942413	-0.114409	4.817595
587.742908	8000.533613	10.947418	-0.114388	4.817610
587.877511	8000.302277	10.952423	-0.114413	4.817541
587.698785	8000.548796	10.957427	-0.114380	4.817614
587.735076	8000.531389	10.962432	-0.114386	4.817609
587.905726	8000.390337	10.967437	-0.114418	4.817566
587.960289	8000.406990	10.972442	-0.114428	4.817571
588.019205	8000.512400	10.977447	-0.114439	4.817602
587.619004	8000.443082	10.982451	-0.114365	4.817583
587.561938	8000.451736	10.987456	-0.114354	4.817586
587.973373	8000.513832	10.992461	-0.114431	4.817603
588.139148	8000.493076	10.997466	-0.114462	4.817596
587.574625	8000.530062	11.002471	-0.114357	4.817609
588.186958	8000.364975	11.007475	-0.114471	4.817558
587.678510	8000.504161	11.012480	-0.114376	4.817601
587.385576	8000.401601	11.017485	-0.114321	4.817572
587.659309	8000.554558	11.022490	-0.114372	4.817616
587.577986	8000.517448	11.027495	-0.114357	4.817606
587.266583	8000.467405	11.032499	-0.114299	4.817592
588.175954	8000.451400	11.037504	-0.114469	4.817583
588.136505	8000.486712	11.042509	-0.114461	4.817594
587.399814	8000.476785	11.047514	-0.114324	4.817594
587.148073	8000.356891	11.052519	-0.114277	4.817560
587.366003	8000.360141	11.057523	-0.114318	4.817560
587.808305	8000.495549	11.062528	-0.114400	4.817598
587.461205	8000.419633	11.067533	-0.114336	4.817577
588.183402	8000.527542	11.072538	-0.114470	4.817606
587.977718	8000.497023	11.077543	-0.114432	4.817598
587.872882	8000.456394	11.082547	-0.114412	4.817586
587.576982	8000.467822	11.087552	-0.114357	4.817591
587.897840	8000.465216	11.092557	-0.114417	4.817589
587.782062	8000.451876	11.097562	-0.114395	4.817585
587.814665	8000.485095	11.102567	-0.114402	4.817595
587.638886	8000.428627	11.107571	-0.114369	4.817579
588.176769	8000.456709	11.112576	-0.114469	4.817585
587.790369	8000.441446	11.117581	-0.114397	4.817582
588.238469	8000.432291	11.122586	-0.114481	4.817577
588.346109	8000.419115	11.127591	-0.114501	4.817573
588.268755	8000.430633	11.132595	-0.114486	4.817577
588.291460	8000.462649	11.137600	-0.114490	4.817586
588.408827	8000.454898	11.142605	-0.114512	4.817583
588.508111	8000.448988	11.147610	-0.114531	4.817581
588.218486	8000.434112	11.152615	-0.114477	4.817578
588.430331	8000.334853	11.157619	-0.114516	4.817548
588.645216	8000.369734	11.162624	-0.114556	4.817557
588.147396	8000.496408	11.167629	-0.114464	4.817597
588.085480	8000.438469	11.172634	-0.114452	4.817580
588.737245	8000.489369	11.177639	-0.114574	4.817592
588.674730	8000.497941	11.182643	-0.114562	4.817595
588.808409	8000.440806	11.187648	-0.114587	4.817577
588.581821	8000.424758	11.192653	-0.114545	4.817574
588.858702	8000.351809	11.197658	-0.114596	4.817551
588.793320	8000.356115	11.202663	-0.114584	4.817552
588.866197	8000.335029	11.207667	-0.114598	4.817546
588.799442	8000.357264	11.212672	-0.114585	4.817553
588.819087	8000.335385	11.217677	-0.114589	4.817546
588.715467	8000.396138	11.222682	-0.114570	4.817565
588.784101	8000.389771	11.227687	-0.114582	4.817562
588.637883	8000.405542	11.232691	-0.114555	4.817568
588.483623	8000.413801	11.237696	-0.114527	4.817571
588.855191	8000.339097	11.242701	-0.114596	4.817547
588.647602	8000.448981	11.247706	-0.114557	4.817581
588.654015	8000.389949	11.252711	-0.114558	4.817563
588.567811	8000.415061	11.257715	-0.114542	4.817571
589.029578	8000.393441	11.262720	-0.114628	4.817562
588.955144	8000.334258	11.267725	-0.114614	4.817545
589.031620	8000.362853	11.272730	-0.114629	4.817553
588.816721	8000.375487	11.277735	-0.114589	4.817558
588.729207	8000.400580	11.282739	-0.114572	4.817566
588.609419	8000.439974	11.287744	-0.114550	4.817578
588.624576	8000.397966	11.292749	-0.114553	4.817566
588.526617	8000.338434	11.297754	-0.114535	4.817548
588.438865	8000.386752	11.302759	-0.114518	4.817563
588.850150	8000.356987	11.307763	-0.114595	4.817552
588.695187	8000.401136	11.312768	-0.114566	4.817566
588.741450	8000.349033	11.317773	-0.114575	4.817551
588.624694	8000.390584	11.322778	-0.114553	4.817563
588.713638	8000.389800	11.327783	-0.114570	4.817563
588.908097	8000.422267	11.332787	-0.114606	4.817571
588.640213	8000.423552	11.337792	-0.114556	4.817573
588.948541	8000.347904	11.342797	-0.114613	4.817549
589.092767	8000.391236	11.347802	-0.114640	4.817561
588.919891	8000.313691	11.352807	-0.114608	4.817539
589.002033	8000.340259	11.357811	-0.114623	4.817547
589.071318	8000.357132	11.362816	-0.114636	4.817551
588.932622	8000.349785	11.367821	-0.114610	4.817550
588.946256	8000.413342	11.372826	-0.114613	4.817569
589.049492	8000.311407	11.377831	-0.114632	4.817538
589.023837	8000.357484	11.382835	-0.114628	4.817552
588.899239	8000.349292	11.387840	-0.114604	4.817550
589.104385	8000.352353	11.392845	-0.114643	4.817550
589.107296	8000.395689	11.397850	-0.114643	4.817563
588.916673	8000.373841	11.402855	-0.114608	4.817557
589.037849	8000.340805	11.407859	-0.114630	4.817547
588.926816	8000.483806	11.412864	-0.114610	4.817590
588.845458	8000.411850	11.417869	-0.114594	4.817569
588.993679	8000.436235	11.422874	-0.114622	4.817575
588.998445	8000.353949	11.427879	-0.114623	4.817551
589.131541	8000.418232	11.432883	-0.114648	4.817569
588.855446	8000.429954	11.437888	-0.114596	4.817574
588.853758	8000.380303	11.442893	-0.114596	4.817559
588.808147	8000.469374	11.447898	-0.114588	4.817586
588.822498	8000.403069	11.452903	-0.114590	4.817566
589.185422	8000.357801	11.457907	-0.114658	4.817551
589.193534	8000.352643	11.462912	-0.114659	4.817550
589.016283	8000.357392	11.467917	-0.114626	4.817552
588.879115	8000.467271	11.472922	-0.114601	4.817585
588.688191	8000.426413	11.477927	-0.114565	4.817574
588.776229	8000.400274	11.482931	-0.114582	4.817566
588.736356	8000.421854	11.487936	-0.114574	4.817572
588.871373	8000.356293	11.492941	-0.114599	4.817552
588.794662	8000.423782	11.497946	-0.114585	4.817572
588.610873	8000.410483	11.502951	-0.114551	4.817569
588.554807	8000.432877	11.507955	-0.114541	4.817576
588.437472	8000.430073	11.512960	-0.114519	4.817576
588.915425	8000.409750	11.517965	-0.114608	4.817568
589.181373	8000.391544	11.522970	-0.114657	4.817561
589.043828	8000.354650	11.527975	-0.114632	4.817551
588.989104	8000.427747	11.532979	-0.114622	4.817573
589.058500	8000.398162	11.537984	-0.114634	4.817564
589.074550	8000.340329	11.542989	-0.114637	4.817547
588.925899	8000.422584	11.547994	-0.114610	4.817571
588.598566	8000.432485	11.552999	-0.114549	4.817576
588.734612	8000.417621	11.558003	-0.114574	4.817571
588.120722	8000.502440	11.563008	-0.114460	4.817599
588.790455	8000.404730	11.568013	-0.114585	4.817567
588.740465	8000.472618	11.573018	-0.114575	4.817587
588.796343	8000.428050	11.578023	-0.114586	4.817574
588.892931	8000.398871	11.583027	-0.114604	4.817565
588.775367	8000.461528	11.588032	-0.114582	4.817584
588.855172	8000.377193	11.593037	-0.114597	4.817558
589.167619	8000.412475	11.598042	-0.114655	4.817567
589.049680	8000.372705	11.603047	-0.114633	4.817556
589.155280	8000.403846	11.608051	-0.114653	4.817565
589.327517	8000.377908	11.613056	-0.114685	4.817556
589.155749	8000.373235	11.618061	-0.114653	4.817556
588.909394	8000.450865	11.623066	-0.114607	4.817580
588.683004	8000.408421	11.628071	-0.114565	4.817568
589.142163	8000.398377	11.633075	-0.114650	4.817563
589.199290	8000.430907	11.638080	-0.114661	4.817573
589.186325	8000.369473	11.643085	-0.114659	4.817555
589.011555	8000.339415	11.648090	-0.114626	4.817547
589.125304	8000.347448	11.653095	-0.114647	4.817548
589.012533	8000.388002	11.658099	-0.114626	4.817561
588.864008	8000.434359	11.663104	-0.114599	4.817575
588.927860	8000.371959	11.668109	-0.114611	4.817556
588.503398	8000.497615	11.673114	-0.114532	4.817596
588.399912	8000.445391	11.678119	-0.114512	4.817581
589.038050	8000.392613	11.683123	-0.114631	4.817562
589.067154	8000.437395	11.688128	-0.114637	4.817575
588.770454	8000.363283	11.693133	-0.114581	4.817555
589.271343	8000.406655	11.698138	-0.114675	4.817565
588.624981	8000.442418	11.703143	-0.114554	4.817579
588.848655	8000.406688	11.708147	-0.114596	4.817567
588.919354	8000.408799	11.713152	-0.114609	4.817567
588.899851	8000.419069	11.718157	-0.114605	4.817571
588.921041	8000.464789	11.723162	-0.114609	4.817584
588.830393	8000.382135	11.728167	-0.114593	4.817560
588.857744	8000.449065	11.733171	-0.114598	4.817580
588.962859	8000.378834	11.738176	-0.114617	4.817558
588.965983	8000.481303	11.743181	-0.114618	4.817589
588.860394	8000.520908	11.748186	-0.114598	4.817601
588.684586	8000.487666	11.753191	-0.114566	4.817592
589.081158	8000.424950	11.758195	-0.114639	4.817571
588.988435	8000.441518	11.763200	-0.114622	4.817577
588.963005	8000.408408	11.768205	-0.114617	4.817567
589.333454	8000.413935	11.773210	-0.114686	4.817567
589.078538	8000.437587	11.778215	-0.114639	4.817575
589.057824	8000.404546	11.783219	-0.114635	4.817566
589.063291	8000.436306	11.788224	-0.114636	4.817575
589.060480	8000.392974	11.793229	-0.114636	4.817562
589.329369	8000.418104	11.798234	-0.114686	4.817568
589.395349	8000.331450	11.803239	-0.114698	4.817542
589.125357	8000.396057	11.808243	-0.114648	4.817563
589.140322	8000.438517	11.813248	-0.114651	4.817575
589.058774	8000.390842	11.818253	-0.114635	4.817561
589.417449	8000.377188	11.823258	-0.114702	4.817556
589.105318	8000.370421	11.828263	-0.114644	4.817555
589.077810	8000.406968	11.833267	-0.114639	4.817566
589.028741	8000.406238	11.838272	-0.114630	4.817566
589.085049	8000.433476	11.843277	-0.114640	4.817574
589.025384	8000.406190	11.848282	-0.114629	4.817566
588.894852	8000.461262	11.853287	-0.114605	4.817583
589.033075	8000.423201	11.858291	-0.114631	4.817571
589.084592	8000.441921	11.863296	-0.114640	4.817576
589.039927	8000.335667	11.868301	-0.114632	4.817545
589.457911	8000.397866	11.873306	-0.114710	4.817562
589.273839	8000.345494	11.878311	-0.114676	4.817547
589.441269	8000.345881	11.883315	-0.114707	4.817547
589.346940	8000.371928	11.888320	-0.114689	4.817555
588.931406	8000.372067	11.893325	-0.114612	4.817556
589.193370	8000.369640	11.898330	-0.114661	4.817555
589.244538	8000.368293	11.903335	-0.114670	4.817554
589.076911	8000.422811	11.908339	-0.114639	4.817571
589.254855	8000.443417	11.913344	-0.114672	4.817576
589.228561	8000.417685	11.918349	-0.114667	4.817569
589.212955	8000.467080	11.923354	-0.114664	4.817583
588.947019	8000.450443	11.928359	-0.114615	4.817580
589.072480	8000.330889	11.933363	-0.114638	4.817544
589.108147	8000.416949	11.938368	-0.114645	4.817569
588.973879	8000.431842	11.943373	-0.114620	4.817574
589.327170	8000.444505	11.948378	-0.114686	4.817576
589.266923	8000.373918	11.953383	-0.114674	4.817556
589.159083	8000.382869	11.958387	-0.114654	4.817559
589.069677	8000.439611	11.963392	-0.114638	4.817576
588.738186	8000.425164	11.968397	-0.114576	4.817573
588.959203	8000.489704	11.973402	-0.114617	4.817591
589.146278	8000.446037	11.978407	-0.114652	4.817577
589.089670	8000.488485	11.983411	-0.114642	4.817590
589.218943	8000.402776	11.988416	-0.114666	4.817564
589.023100	8000.405135	11.993421	-0.114629	4.817566
588.926473	8000.518787	11.998426	-0.114611	4.817600
588.985340	8000.353892	12.003431	-0.114622	4.817551
589.113403	8000.433939	12.008435	-0.114646	4.817574
589.218361	8000.363705	12.013440	-0.114666	4.817553
589.213422	8000.329844	12.018445	-0.114665	4.817543
589.209591	8000.413203	12.023450	-0.114664	4.817567
588.995490	8000.452246	12.028455	-0.114624	4.817580
589.021415	8000.432572	12.033459	-0.114629	4.817574
589.523034	8000.387262	12.038464	-0.114722	4.817558
589.035129	8000.390544	12.043469	-0.114632	4.817561
589.063592	8000.483888	12.048474	-0.114637	4.817589
588.744540	8000.478074	12.053479	-0.114578	4.817589
588.999499	8000.411134	12.058483	-0.114625	4.817568
589.143333	8000.416448	12.063488	-0.114652	4.817569
589.199043	8000.375045	12.068493	-0.114662	4.817556
589.257145	8000.443490	12.073498	-0.114673	4.817576
589.552508	8000.404606	12.078503	-0.114728	4.817563
589.296964	8000.443031	12.083507	-0.114681	4.817576
589.555967	8000.358201	12.088512	-0.114729	4.817550
589.494785	8000.375239	12.093517	-0.114717	4.817555
589.637590	8000.375259	12.098522	-0.114744	4.817554
589.556676	8000.370886	12.103527	-0.114729	4.817553
589.654586	8000.353341	12.108531	-0.114747	4.817548
589.646538	8000.354278	12.113536	-0.114746	4.817548
589.682189	8000.325246	12.118541	-0.114752	4.817539
589.718212	8000.354294	12.123546	-0.114759	4.817548
589.569653	8000.320402	12.128551	-0.114731	4.817538
589.528676	8000.343022	12.133555	-0.114724	4.817545
589.551418	8000.364480	12.138560	-0.114728	4.817551
589.471482	8000.380183	12.143565	-0.114713	4.817556
589.126198	8000.489070	12.148570	-0.114649	4.817590
589.091140	8000.482213	12.153575	-0.114642	4.817588
589.639195	8000.433372	12.158579	-0.114744	4.817571
589.599447	8000.329302	12.163584	-0.114737	4.817541
589.643371	8000.346853	12.168589	-0.114745	4.817546
589.665591	8000.337683	12.173594	-0.114749	4.817543
589.800021	8000.365031	12.178599	-0.114774	4.817551
589.616275	8000.384465	12.183603	-0.114740	4.817557
589.910609	8000.355069	12.188608	-0.114795	4.817547
589.877908	8000.318681	12.193613	-0.114789	4.817537
589.464204	8000.409653	12.198618	-0.114712	4.817565
589.650118	8000.323732	12.203623	-0.114747	4.817539
589.750260	8000.356905	12.208627	-0.114765	4.817548
589.454858	8000.450697	12.213632	-0.114710	4.817577
589.122181	8000.445735	12.218637	-0.114648	4.817577
589.745018	8000.438135	12.223642	-0.114764	4.817572
589.476623	8000.480591	12.228647	-0.114714	4.817586
589.173365	8000.483459	12.233651	-0.114658	4.817588
589.318810	8000.432835	12.238656	-0.114685	4.817573
589.530658	8000.422270	12.243661	-0.114725	4.817569
588.928358	8000.504092	12.248666	-0.114612	4.817596
588.621258	8000.526966	12.253671	-0.114555	4.817604
589.076196	8000.450338	12.258675	-0.114640	4.817579
589.228888	8000.514915	12.263680	-0.114668	4.817597
589.116020	8000.388637	12.268685	-0.114647	4.817561
589.355301	8000.489350	12.273690	-0.114692	4.817589
589.047519	8000.497430	12.278695	-0.114635	4.817593
588.957207	8000.453849	12.283699	-0.114618	4.817581
588.921016	8000.561011	12.288704	-0.114611	4.817612
589.018133	8000.366065	12.293709	-0.114629	4.817554
589.137218	8000.451258	12.298714	-0.114651	4.817579
589.047217	8000.513270	12.303719	-0.114635	4.817598
589.102556	8000.547886	12.308723	-0.114645	4.817608
589.189438	8000.462600	12.313728	-0.114661	4.817582
588.975784	8000.373887	12.318733	-0.114621	4.817557
589.230544	8000.468495	12.323738	-0.114669	4.817584
589.321354	8000.503640	12.328743	-0.114686	4.817594
589.088242	8000.465318	12.333747	-0.114642	4.817583
589.346448	8000.548365	12.338752	-0.114691	4.817607
589.171535	8000.514079	12.343757	-0.114658	4.817597
589.108582	8000.438172	12.348762	-0.114646	4.817575
588.737333	8000.555118	12.353767	-0.114577	4.817611
589.138470	8000.385826	12.358771	-0.114652	4.817560
589.202464	8000.492371	12.363776	-0.114664	4.817591
589.120381	8000.447856	12.368781	-0.114649	4.817578
588.692112	8000.373893	12.373786	-0.114569	4.817558
589.348327	8000.515669	12.378791	-0.114691	4.817597
589.224216	8000.443073	12.383795	-0.114668	4.817576
589.249155	8000.480403	12.388800	-0.114673	4.817587
589.262713	8000.430979	12.393805	-0.114675	4.817572
589.487926	8000.434341	12.398810	-0.114717	4.817572
589.317500	8000.480370	12.403815	-0.114685	4.817587
588.926438	8000.404849	12.408819	-0.114612	4.817566
588.794874	8000.485247	12.413824	-0.114588	4.817591
589.058409	8000.393093	12.418829	-0.114637	4.817562
588.907596	8000.494322	12.423834	-0.114609	4.817593
589.040781	8000.458298	12.428839	-0.114634	4.817581
588.920809	8000.385765	12.433843	-0.114612	4.817561
588.817209	8000.470803	12.438848	-0.114592	4.817586
589.441871	8000.495963	12.443853	-0.114709	4.817591
589.632630	8000.477692	12.448858	-0.114744	4.817585
589.136065	8000.485067	12.453863	-0.114652	4.817589
588.957311	8000.515134	12.458867	-0.114618	4.817599
589.037274	8000.355833	12.463872	-0.114633	4.817551
588.810109	8000.579461	12.468877	-0.114591	4.817618
589.087931	8000.432615	12.473882	-0.114643	4.817574
589.126030	8000.437408	12.478887	-0.114650	4.817575
589.383272	8000.466589	12.483891	-0.114698	4.817582
589.323595	8000.502656	12.488896	-0.114687	4.817593
589.222540	8000.414566	12.493901	-0.114668	4.817568
588.973681	8000.488990	12.498906	-0.114622	4.817591
589.314265	8000.479290	12.503911	-0.114685	4.817586
589.275999	8000.356237	12.508915	-0.114678	4.817550
589.536945	8000.524852	12.513920	-0.114727	4.817599
589.540252	8000.455213	12.518925	-0.114727	4.817578
589.518111	8000.500287	12.523930	-0.114723	4.817592
589.216123	8000.439820	12.528935	-0.114667	4.817575
589.293298	8000.538115	12.533939	-0.114681	4.817604
589.413671	8000.450161	12.538944	-0.114704	4.817577
589.435155	8000.486383	12.543949	-0.114708	4.817588
589.605559	8000.535387	12.548954	-0.114739	4.817602
589.660308	8000.439062	12.553959	-0.114750	4.817573
589.438371	8000.396683	12.558963	-0.114708	4.817561
589.591363	8000.570024	12.563968	-0.114737	4.817612
589.485108	8000.455458	12.568973	-0.114717	4.817579
589.558790	8000.429105	12.573978	-0.114731	4.817571
589.629344	8000.532582	12.578983	-0.114744	4.817601
589.673634	8000.535356	12.583987	-0.114752	4.817601
589.833970	8000.481787	12.588992	-0.114782	4.817585
589.718195	8000.467389	12.593997	-0.114761	4.817581
589.387669	8000.446620	12.599002	-0.114699	4.817576
589.029753	8000.526809	12.604007	-0.114632	4.817602
589.190479	8000.421506	12.609011	-0.114662	4.817570
589.548623	8000.499708	12.614016	-0.114729	4.817591
589.377208	8000.453860	12.619021	-0.114697	4.817579
589.250705	8000.540669	12.624026	-0.114674	4.817605
589.217043	8000.434578	12.629031	-0.114667	4.817574
589.398122	8000.442560	12.634035	-0.114701	4.817575
589.432550	8000.538107	12.639040	-0.114708	4.817603
589.522703	8000.446534	12.644045	-0.114724	4.817576
589.634483	8000.523172	12.649050	-0.114745	4.817598
589.605597	8000.534357	12.654055	-0.114740	4.817601
589.398170	8000.418282	12.659059	-0.114701	4.817568
589.794788	8000.551966	12.664064	-0.114775	4.817606
589.716915	8000.427264	12.669069	-0.114760	4.817569
589.686495	8000.502836	12.674074	-0.114755	4.817592
589.819262	8000.406619	12.679079	-0.114780	4.817563
589.797813	8000.433754	12.684083	-0.114776	4.817571
589.681419	8000.446801	12.689088	-0.114754	4.817575
589.613385	8000.400383	12.694093	-0.114741	4.817562
589.776672	8000.401765	12.699098	-0.114772	4.817561
589.846730	8000.542192	12.704103	-0.114785	4.817603
589.890254	8000.494270	12.709107	-0.114793	4.817588
589.735056	8000.545807	12.714112	-0.114764	4.817604
589.908828	8000.425916	12.719117	-0.114796	4.817568
590.007435	8000.418941	12.724122	-0.114815	4.817566
589.859293	8000.430458	12.729127	-0.114787	4.817570
589.832400	8000.396269	12.734131	-0.114782	4.817560
589.927875	8000.400863	12.739136	-0.114800	4.817561
589.669151	8000.389612	12.744141	-0.114752	4.817558
589.839619	8000.435449	12.749146	-0.114784	4.817571
589.937859	8000.443252	12.754151	-0.114802	4.817573
589.668121	8000.345253	12.759155	-0.114752	4.817545
589.748966	8000.502734	12.764160	-0.114767	4.817591
590.078057	8000.408391	12.769165	-0.114828	4.817562
589.837543	8000.463934	12.774170	-0.114783	4.817580
589.614408	8000.494394	12.779175	-0.114742	4.817590
589.845899	8000.440831	12.784179	-0.114785	4.817573
590.023067	8000.458259	12.789184	-0.114818	4.817577
589.892455	8000.386621	12.794189	-0.114794	4.817556
589.693613	8000.512476	12.799194	-0.114757	4.817595
589.633418	8000.427106	12.804199	-0.114745	4.817570
589.347453	8000.504145	12.809203	-0.114692	4.817594
589.801907	8000.490865	12.814208	-0.114777	4.817588
590.108873	8000.385633	12.819213	-0.114834	4.817555
589.904897	8000.451224	12.824218	-0.114796	4.817576
589.752764	8000.435228	12.829223	-0.114768	4.817571
589.936277	8000.391508	12.834227	-0.114802	4.817558
590.265070	8000.412255	12.839232	-0.114863	4.817562
589.932627	8000.355555	12.844237	-0.114801	4.817547
589.931097	8000.335471	12.849242	-0.114801	4.817541
590.281835	8000.433627	12.854247	-0.114866	4.817569
590.153926	8000.383147	12.859251	-0.114842	4.817554
589.792493	8000.494961	12.864256	-0.114775	4.817589
589.862314	8000.418922	12.869261	-0.114788	4.817566
589.839504	8000.475602	12.874266	-0.114784	4.817583
589.800156	8000.437003	12.879271	-0.114777	4.817572
589.765753	8000.422765	12.884275	-0.114770	4.817568
589.738200	8000.517386	12.889280	-0.114765	4.817596
588.973438	8000.443679	12.894285	-0.114623	4.817577
588.991224	8000.368977	12.899290	-0.114626	4.817555
589.040694	8000.568224	12.904295	-0.114635	4.817614
588.601090	8000.349435	12.909299	-0.114553	4.817551
589.052551	8000.517720	12.914304	-0.114638	4.817599
589.306937	8000.434933	12.919309	-0.114685	4.817573
589.471923	8000.444787	12.924314	-0.114716	4.817576
588.655533	8000.331246	12.929319	-0.114564	4.817546
588.967671	8000.395031	12.934323	-0.114622	4.817563
589.181440	8000.569277	12.939328	-0.114662	4.817614
589.261029	8000.426863	12.944333	-0.114676	4.817571
589.236036	8000.448665	12.949338	-0.114672	4.817578
589.390910	8000.443586	12.954343	-0.114701	4.817576
588.912086	8000.487126	12.959347	-0.114612	4.817591
589.037730	8000.449934	12.964352	-0.114635	4.817579
589.325036	8000.422545	12.969357	-0.114688	4.817570
588.990993	8000.433401	12.974362	-0.114626	4.817574
588.629387	8000.265404	12.979367	-0.114559	4.817526
588.873425	8000.444320	12.984371	-0.114604	4.817578
589.065767	8000.243405	12.989376	-0.114640	4.817518
588.942055	8000.475967	12.994381	-0.114617	4.817587
588.753205	8000.441475	12.999386	-0.114582	4.817578
589.048896	8000.473340	13.004391	-0.114637	4.817586
588.715778	8000.489490	13.009395	-0.114575	4.817592
588.883585	8000.367399	13.014400	-0.114606	4.817555
588.597521	8000.397978	13.019405	-0.114553	4.817566
588.937354	8000.333360	13.024410	-0.114616	4.817545
589.348846	8000.423970	13.029415	-0.114693	4.817570
589.189913	8000.554643	13.034419	-0.114664	4.817609
589.395574	8000.440508	13.039424	-0.114702	4.817575
589.643969	8000.467446	13.044429	-0.114748	4.817581
589.592934	8000.519481	13.049434	-0.114739	4.817597
589.103832	8000.460445	13.054439	-0.114647	4.817582
588.896560	8000.464745	13.059443	-0.114609	4.817584
588.446372	8000.231020	13.064448	-0.114525	4.817517
588.960488	8000.477316	13.069453	-0.114621	4.817587
589.479957	8000.481900	13.074458	-0.114718	4.817586
589.804294	8000.458232	13.079463	-0.114778	4.817578
589.129201	8000.544246	13.084467	-0.114652	4.817606
589.557020	8000.446097	13.089472	-0.114732	4.817576
589.539000	8000.481730	13.094477	-0.114729	4.817586
590.063332	8000.444152	13.099482	-0.114826	4.817573
589.573486	8000.403054	13.104487	-0.114735	4.817563
589.442552	8000.408493	13.109491	-0.114711	4.817565
589.280923	8000.515896	13.114496	-0.114681	4.817597
589.078952	8000.472760	13.119501	-0.114643	4.817586
589.387005	8000.416115	13.124506	-0.114700	4.817567
589.273399	8000.440819	13.129511	-0.114679	4.817575
589.161132	8000.546847	13.134515	-0.114658	4.817607
589.426886	8000.434664	13.139520	-0.114708	4.817573
589.875194	8000.395951	13.144525	-0.114791	4.817559
589.727108	8000.481383	13.149530	-0.114764	4.817585
589.608466	8000.433153	13.154535	-0.114742	4.817571
589.767425	8000.473539	13.159539	-0.114771	4.817583
589.581208	8000.420078	13.164544	-0.114737	4.817568
589.394076	8000.553499	13.169549	-0.114702	4.817608
589.184523	8000.341306	13.174554	-0.114663	4.817546
588.964649	8000.487964	13.179559	-0.114622	4.817591
589.382569	8000.463579	13.184563	-0.114700	4.817581
589.585640	8000.415927	13.189568	-0.114738	4.817566
589.597463	8000.473123	13.194573	-0.114740	4.817583
589.103275	8000.579788	13.199578	-0.114648	4.817617
589.069563	8000.368107	13.204583	-0.114642	4.817555
589.405908	8000.566356	13.209587	-0.114704	4.817612
589.467884	8000.471195	13.214592	-0.114716	4.817583
589.421091	8000.478945	13.219597	-0.114707	4.817586
589.619853	8000.404831	13.224602	-0.114744	4.817563
589.379222	8000.508944	13.229607	-0.114699	4.817595
589.481337	8000.382704	13.234611	-0.114718	4.817557
589.774248	8000.505338	13.239616	-0.114773	4.817592
589.707429	8000.501174	13.244621	-0.114760	4.817591
589.594667	8000.494213	13.249626	-0.114739	4.817590
589.993254	8000.454758	13.254631	-0.114814	4.817576
589.820249	8000.414165	13.259635	-0.114781	4.817565
589.601723	8000.400346	13.264640	-0.114741	4.817562
589.506172	8000.476003	13.269645	-0.114723	4.817585
589.780629	8000.496994	13.274650	-0.114774	4.817590
589.582400	8000.522547	13.279655	-0.114737	4.817598
589.211154	8000.458934	13.284659	-0.114668	4.817581
589.337724	8000.456600	13.289664	-0.114692	4.817580
588.919374	8000.497875	13.294669	-0.114614	4.817594
589.117870	8000.349845	13.299674	-0.114651	4.817549
588.894177	8000.449986	13.304679	-0.114609	4.817580
589.328289	8000.545159	13.309683	-0.114690	4.817606
589.308879	8000.468846	13.314688	-0.114686	4.817583
589.284244	8000.552952	13.319693	-0.114682	4.817608
589.080745	8000.407371	13.324698	-0.114644	4.817566
589.060437	8000.422907	13.329703	-0.114640	4.817571
589.016176	8000.395851	13.334707	-0.114632	4.817563
589.538075	8000.514508	13.339712	-0.114729	4.817596
589.966621	8000.418481	13.344717	-0.114809	4.817566
589.888935	8000.450057	13.349722	-0.114795	4.817575
590.080230	8000.443409	13.354727	-0.114830	4.817572
589.929798	8000.465452	13.359731	-0.114802	4.817580
589.802533	8000.410758	13.364736	-0.114778	4.817564
589.907675	8000.437670	13.369741	-0.114798	4.817571
589.796279	8000.504643	13.374746	-0.114777	4.817592
589.916061	8000.435686	13.379751	-0.114800	4.817571
590.060324	8000.483245	13.384755	-0.114827	4.817584
589.942025	8000.426573	13.389760	-0.114805	4.817568
589.669142	8000.523869	13.394765	-0.114754	4.817598
589.297993	8000.462369	13.399770	-0.114685	4.817581
589.566681	8000.350230	13.404775	-0.114735	4.817547
589.368415	8000.565845	13.409779	-0.114698	4.817612
588.854937	8000.375515	13.414784	-0.114602	4.817558
589.210767	8000.441010	13.419789	-0.114668	4.817576
589.368962	8000.460266	13.424794	-0.114698	4.817581
589.798230	8000.532139	13.429799	-0.114778	4.817600
589.716824	8000.488689	13.434803	-0.114763	4.817587
589.980754	8000.448281	13.439808	-0.114812	4.817574
589.808827	8000.563979	13.444813	-0.114780	4.817609
589.995289	8000.426326	13.449818	-0.114815	4.817568
589.742263	8000.538701	13.454823	-0.114768	4.817602
590.169574	8000.451104	13.459827	-0.114847	4.817574
590.008353	8000.382176	13.464832	-0.114817	4.817555
589.772300	8000.435674	13.469837	-0.114773	4.817571
589.586420	8000.540604	13.474842	-0.114739	4.817603
589.675504	8000.499698	13.479847	-0.114755	4.817591
589.155115	8000.427525	13.484851	-0.114658	4.817572
589.362621	8000.474970	13.489856	-0.114697	4.817585
589.665883	8000.484776	13.494861	-0.114753	4.817586
589.791728	8000.495102	13.499866	-0.114777	4.817589
589.769941	8000.409250	13.504871	-0.114773	4.817564
590.135984	8000.461174	13.509875	-0.114841	4.817577
590.328351	8000.492556	13.514880	-0.114877	4.817586
589.942345	8000.514250	13.519885	-0.114805	4.817594
590.103062	8000.366709	13.524890	-0.114835	4.817550
589.934577	8000.561652	13.529895	-0.114804	4.817608
589.607822	8000.421620	13.534899	-0.114743	4.817568
589.822737	8000.433276	13.539904	-0.114783	4.817571
589.929855	8000.464441	13.544909	-0.114803	4.817579
589.553192	8000.436647	13.549914	-0.114733	4.817573
589.756107	8000.508311	13.554919	-0.114770	4.817593
589.020485	8000.462491	13.559923	-0.114633	4.817583
589.726700	8000.375886	13.564928	-0.114765	4.817554
589.369630	8000.543727	13.569933	-0.114699	4.817605
589.632594	8000.405105	13.574938	-0.114747	4.817563
589.716243	8000.420081	13.579943	-0.114763	4.817567
589.501951	8000.528811	13.584947	-0.114723	4.817600
589.674317	8000.421570	13.589952	-0.114755	4.817568
589.687240	8000.478783	13.594957	-0.114758	4.817585
589.581910	8000.459262	13.599962	-0.114738	4.817579
589.505090	8000.527807	13.604967	-0.114724	4.817600
589.430190	8000.407373	13.609971	-0.114710	4.817565
589.953301	8000.448969	13.614976	-0.114807	4.817575
590.039260	8000.402737	13.619981	-0.114823	4.817561
589.926859	8000.502429	13.624986	-0.114802	4.817591
589.959364	8000.429001	13.629991	-0.114808	4.817569
590.132230	8000.478042	13.634995	-0.114841	4.817582
589.821031	8000.474455	13.640000	-0.114783	4.817583
590.228885	8000.377063	13.645005	-0.114859	4.817552
590.381555	8000.387791	13.650010	-0.114887	4.817555
590.082342	8000.447737	13.655015	-0.114831	4.817574
590.216397	8000.462410	13.660019	-0.114856	4.817577
590.395720	8000.448193	13.665024	-0.114890	4.817572
590.019396	8000.473199	13.670029	-0.114820	4.817581
590.027798	8000.444816	13.675034	-0.114821	4.817573
590.298697	8000.404512	13.680039	-0.114872	4.817560
590.305119	8000.372931	13.685043	-0.114873	4.817551
590.277277	8000.370405	13.690048	-0.114868	4.817550
590.420349	8000.384157	13.695053	-0.114895	4.817553
590.811593	8000.361488	13.700058	-0.114967	4.817545
590.613418	8000.356419	13.705063	-0.114930	4.817544
590.458948	8000.349891	13.710067	-0.114902	4.817543
590.570830	8000.382184	13.715072	-0.114923	4.817552
590.739829	8000.308681	13.720077	-0.114954	4.817530
590.575925	8000.347417	13.725082	-0.114924	4.817542
590.347524	8000.370407	13.730087	-0.114881	4.817550
590.364897	8000.413960	13.735091	-0.114884	4.817562
590.324249	8000.432362	13.740096	-0.114877	4.817568
590.049746	8000.483173	13.745101	-0.114826	4.817584
590.155208	8000.448847	13.750106	-0.114845	4.817574
589.727799	8000.548061	13.755111	-0.114766	4.817605
589.809304	8000.472197	13.760115	-0.114781	4.817582
590.230664	8000.453145	13.765120	-0.114859	4.817575
590.009880	8000.500535	13.770125	-0.114818	4.817590
590.029890	8000.449095	13.775130	-0.114822	4.817574
589.918048	8000.418917	13.780135	-0.114801	4.817566
589.523431	8000.445763	13.785139	-0.114728	4.817576
589.904084	8000.500017	13.790144	-0.114799	4.817590
589.495284	8000.537209	13.795149	-0.114723	4.817603
589.400918	8000.469280	13.800154	-0.114705	4.817583
589.575077	8000.403246	13.805159	-0.114737	4.817563
589.381130	8000.522838	13.810163	-0.114701	4.817599
589.645226	8000.420134	13.815168	-0.114751	4.817567
589.073511	8000.476015	13.820173	-0.114644	4.817586
589.946099	8000.460527	13.825178	-0.114807	4.817578
590.090425	8000.415166	13.830183	-0.114833	4.817564
590.078962	8000.388599	13.835187	-0.114831	4.817556
590.082239	8000.402376	13.840192	-0.114832	4.817560
589.893071	8000.458685	13.845197	-0.114797	4.817578
590.406790	8000.429396	13.850202	-0.114892	4.817567
590.337917	8000.443152	13.855207	-0.114880	4.817571
589.767577	8000.525450	13.860211	-0.114774	4.817598
589.509694	8000.393838	13.865216	-0.114725	4.817560
589.615254	8000.466160	13.870221	-0.114745	4.817581
589.730495	8000.527012	13.875226	-0.114767	4.817599
589.916487	8000.523454	13.880231	-0.114801	4.817597
590.138304	8000.494032	13.885235	-0.114843	4.817587
590.037450	8000.378489	13.890240	-0.114824	4.817553
589.965089	8000.475610	13.895245	-0.114810	4.817582
590.121264	8000.443097	13.900250	-0.114839	4.817572
590.228626	8000.479546	13.905255	-0.114859	4.817582
590.253590	8000.494703	13.910259	-0.114864	4.817587
590.188370	8000.437767	13.915264	-0.114852	4.817570
590.188007	8000.473664	13.920269	-0.114852	4.817581
590.185985	8000.504257	13.925274	-0.114852	4.817590
589.984725	8000.467465	13.930279	-0.114814	4.817580
589.854297	8000.492973	13.935283	-0.114790	4.817588
589.732052	8000.485870	13.940288	-0.114767	4.817586
589.596211	8000.381422	13.945293	-0.114742	4.817556
590.006269	8000.462511	13.950298	-0.114818	4.817578
589.775113	8000.554095	13.955303	-0.114775	4.817606
589.659161	8000.410874	13.960307	-0.114754	4.817565
590.098684	8000.501907	13.965312	-0.114835	4.817590
589.851627	8000.540458	13.970317	-0.114790	4.817602
589.919369	8000.429543	13.975322	-0.114802	4.817569
589.959964	8000.410088	13.980327	-0.114810	4.817563
589.950046	8000.436339	13.985331	-0.114808	4.817571
590.103430	8000.512544	13.990336	-0.114836	4.817593
589.572719	8000.515183	13.995341	-0.114738	4.817596
589.361452	8000.388491	14.000346	-0.114698	4.817559
589.758661	8000.503178	14.005351	-0.114772	4.817591
590.242847	8000.453386	14.010355	-0.114862	4.817575
590.104151	8000.535791	14.015360	-0.114837	4.817600
589.641752	8000.497213	14.020365	-0.114751	4.817590
589.124201	8000.362784	14.025370	-0.114654	4.817553
589.940965	8000.487954	14.030375	-0.114806	4.817586
590.314026	8000.405882	14.035379	-0.114876	4.817560
590.301530	8000.435262	14.040384	-0.114873	4.817569
590.127920	8000.417890	14.045389	-0.114841	4.817565
590.159699	8000.446875	14.050394	-0.114847	4.817573
590.214307	8000.450859	14.055399	-0.114857	4.817574
590.228410	8000.455294	14.060403	-0.114860	4.817575
590.115678	8000.439886	14.065408	-0.114839	4.817571
589.876237	8000.383518	14.070413	-0.114794	4.817556
589.848762	8000.470750	14.075418	-0.114789	4.817581
589.950969	8000.543023	14.080423	-0.114808	4.817602
590.093874	8000.454348	14.085427	-0.114835	4.817576
590.045361	8000.489527	14.090432	-0.114826	4.817586
589.666402	8000.414182	14.095437	-0.114755	4.817566
590.072205	8000.483594	14.100442	-0.114831	4.817584
589.712517	8000.545805	14.105447	-0.114764	4.817604
590.152996	8000.319024	14.110451	-0.114846	4.817535
590.433385	8000.441472	14.115456	-0.114898	4.817570
590.331134	8000.470569	14.120461	-0.114879	4.817579
590.343198	8000.413731	14.125466	-0.114881	4.817562
590.484145	8000.450681	14.130471	-0.114908	4.817573
590.106262	8000.427091	14.135475	-0.114837	4.817567
590.046597	8000.564527	14.140480	-0.114826	4.817608
589.716645	8000.424447	14.145485	-0.114765	4.817568
589.997197	8000.500437	14.150490	-0.114817	4.817590
589.825443	8000.461974	14.155495	-0.114785	4.817579
589.665868	8000.386736	14.160499	-0.114755	4.817557
589.221136	8000.480412	14.165504	-0.114673	4.817587
589.990362	8000.489781	14.170509	-0.114816	4.817586
590.132437	8000.488735	14.175514	-0.114842	4.817586
589.974455	8000.377619	14.180519	-0.114813	4.817553
590.197909	8000.374619	14.185523	-0.114855	4.817551
590.615614	8000.381911	14.190528	-0.114932	4.817552
590.321623	8000.476781	14.195533	-0.114878	4.817581
590.115967	8000.468433	14.200538	-0.114839	4.817580
590.236820	8000.422721	14.205543	-0.114862	4.817566
589.737970	8000.529316	14.210547	-0.114769	4.817599
589.970254	8000.413466	14.215552	-0.114812	4.817564
589.935359	8000.524873	14.220557	-0.114806	4.817597
590.209869	8000.470896	14.225562	-0.114857	4.817580
590.017125	8000.485971	14.230567	-0.114821	4.817585
590.261580	8000.291109	14.235571	-0.114867	4.817527
590.457816	8000.459818	14.240576	-0.114903	4.817576
590.230818	8000.471214	14.245581	-0.114861	4.817580
590.061248	8000.511977	14.250586	-0.114829	4.817593
589.997166	8000.534251	14.255591	-0.114817	4.817600
590.229729	8000.443747	14.260595	-0.114861	4.817572
590.103509	8000.434473	14.265600	-0.114837	4.817570
590.234307	8000.481831	14.270605	-0.114862	4.817583
590.044196	8000.448373	14.275610	-0.114826	4.817574
589.773668	8000.426386	14.280615	-0.114776	4.817569
589.829051	8000.448332	14.285619	-0.114786	4.817575
590.167370	8000.501955	14.290624	-0.114849	4.817589
590.015343	8000.500743	14.295629	-0.114821	4.817590
589.817569	8000.411208	14.300634	-0.114784	4.817564
589.902468	8000.428314	14.305639	-0.114800	4.817569
590.151019	8000.515443	14.310643	-0.114846	4.817593
590.136411	8000.459262	14.315648	-0.114844	4.817577
589.822221	8000.441903	14.320653	-0.114785	4.817573
589.912012	8000.468586	14.325658	-0.114802	4.817581
590.124852	8000.459093	14.330663	-0.114841	4.817577
589.979604	8000.482269	14.335667	-0.114814	4.817584
589.665091	8000.437451	14.340672	-0.114756	4.817572
589.749219	8000.540076	14.345677	-0.114772	4.817602
589.446628	8000.382455	14.350682	-0.114715	4.817557
590.096241	8000.434386	14.355687	-0.114836	4.817570
589.538429	8000.470411	14.360691	-0.114732	4.817583
590.056986	8000.421132	14.365696	-0.114829	4.817566
590.088674	8000.416326	14.370701	-0.114835	4.817564
590.246111	8000.397559	14.375706	-0.114864	4.817558
589.861843	8000.431950	14.380711	-0.114793	4.817570
589.332312	8000.471565	14.385715	-0.114694	4.817584
589.768750	8000.441122	14.390720	-0.114775	4.817573
589.306721	8000.566217	14.395725	-0.114689	4.817612
589.478775	8000.428350	14.400730	-0.114721	4.817571
589.599015	8000.482941	14.405735	-0.114744	4.817586
589.789867	8000.438274	14.410739	-0.114779	4.817572
589.792462	8000.437258	14.415744	-0.114780	4.817572
589.585025	7999.350842	14.420749	-0.114740	4.817251

589.376290	7996.210115	14.425754	-0.114700	4.816324
589.657322	7990.669994	14.430759	-0.114748	4.814684
589.527678	7984.019154	14.435763	-0.114720	4.812716
589.439677	7976.758030	14.440768	-0.114699	4.810567
589.752870	7969.094860	14.445773	-0.114752	4.808296
589.345218	7961.318740	14.450778	-0.114671	4.805994
589.359383	7953.445983	14.455783	-0.114669	4.803660
589.426810	7945.535686	14.460787	-0.114676	4.801313
589.235507	7937.534267	14.465792	-0.114635	4.798939
589.458375	7929.509765	14.470797	-0.114672	4.796556
589.134873	7921.538811	14.475802	-0.114606	4.794190
589.640403	7913.579395	14.480807	-0.114695	4.791822
589.086850	7905.482300	14.485811	-0.114587	4.789417
589.223527	7897.547052	14.490816	-0.114607	4.787055
588.657544	7889.483343	14.495821	-0.114496	4.784657
588.500565	7881.570319	14.500826	-0.114462	4.782302
588.986823	7873.503355	14.505831	-0.114547	4.779896
589.202122	7865.515651	14.510835	-0.114582	4.777515
588.934273	7857.512719	14.515840	-0.114527	4.775129
588.673928	7849.521306	14.520845	-0.114473	4.772745
588.493318	7841.503510	14.525850	-0.114435	4.770352
588.789870	7833.520078	14.530855	-0.114485	4.767967
588.634928	7825.474097	14.535859	-0.114451	4.765563
588.539760	7817.491330	14.540864	-0.114428	4.763176
588.727552	7809.533255	14.545869	-0.114457	4.760795
588.904231	7801.426726	14.550874	-0.114485	4.758368
589.025861	7793.509268	14.555879	-0.114503	4.755997
588.697508	7785.442374	14.560883	-0.114436	4.753581
588.762363	7777.458425	14.565888	-0.114443	4.751188
588.857940	7769.424650	14.570893	-0.114456	4.748778
588.858191	7761.455429	14.575898	-0.114451	4.746387
588.820895	7753.390085	14.580903	-0.114438	4.743966
588.416438	7745.509613	14.585907	-0.114358	4.741600
588.866252	7737.405790	14.590912	-0.114436	4.739164
588.597830	7729.476462	14.595917	-0.114381	4.736781
589.042785	7721.383768	14.600922	-0.114459	4.734345
589.075607	7713.464989	14.605927	-0.114460	4.731962
588.936636	7705.362285	14.610931	-0.114429	4.729522
589.052276	7697.464663	14.615936	-0.114445	4.727143
588.588339	7689.407247	14.620941	-0.114353	4.724715
588.516825	7681.492552	14.625946	-0.114335	4.722328
588.703766	7673.448190	14.630951	-0.114365	4.719901
588.524883	7665.431268	14.635955	-0.114326	4.717481
588.784325	7657.451392	14.640960	-0.114369	4.715070
588.630662	7649.459438	14.645965	-0.114335	4.712655
588.630329	7641.432340	14.650970	-0.114330	4.710228
588.603562	7633.427800	14.655975	-0.114320	4.707807
588.583589	7625.428469	14.660979	-0.114311	4.705385
588.737721	7617.476508	14.665984	-0.114335	4.702977
588.319955	7609.446144	14.670989	-0.114252	4.700545
588.372782	7601.425656	14.675994	-0.114256	4.698113
588.592931	7593.429704	14.680999	-0.114292	4.695688
588.676698	7585.356920	14.686003	-0.114302	4.693238
588.114971	7577.499156	14.691008	-0.114193	4.690853
588.489230	7569.394962	14.696013	-0.114257	4.688391
588.225618	7561.393842	14.701018	-0.114203	4.685959
588.620060	7553.361681	14.706023	-0.114271	4.683516
588.588444	7545.425274	14.711027	-0.114260	4.681102
588.448237	7537.465924	14.716032	-0.114229	4.678679
588.105161	7529.488532	14.721037	-0.114160	4.676250
588.018621	7521.375945	14.726042	-0.114138	4.673778
588.576105	7513.348509	14.731047	-0.114237	4.671330
588.165246	7505.305898	14.736051	-0.114155	4.668877
588.138774	7497.366895	14.741056	-0.114145	4.666454
588.024774	7489.315293	14.746061	-0.114119	4.663995
588.341272	7481.396683	14.751066	-0.114172	4.661576
588.632353	7473.389101	14.756071	-0.114221	4.659128
588.439389	7465.413264	14.761075	-0.114180	4.656689
588.129373	7457.436387	14.766080	-0.114117	4.654248
587.858161	7449.465922	14.771085	-0.114062	4.651808
587.879765	7441.339161	14.776090	-0.114060	4.649318
587.860867	7433.436669	14.781095	-0.114052	4.646896
587.866858	7425.369379	14.786099	-0.114048	4.644422
587.700398	7417.455802	14.791104	-0.114011	4.641994
587.812741	7409.347316	14.796109	-0.114027	4.639505
587.374306	7401.488860	14.801114	-0.113940	4.637092
587.630605	7393.389007	14.806119	-0.113983	4.634602
587.466007	7385.377677	14.811123	-0.113947	4.632139
587.244507	7377.380838	14.816128	-0.113901	4.629679
587.221067	7369.428824	14.821133	-0.113891	4.627231
587.417448	7361.277194	14.826138	-0.113922	4.624721
587.754619	7353.395198	14.831143	-0.113980	4.622292
587.878816	7345.312927	14.836147	-0.113998	4.619801
588.042244	7337.384686	14.841152	-0.114023	4.617355
587.754789	7329.384350	14.846157	-0.113964	4.614886
587.399817	7321.407727	14.851162	-0.113893	4.612423
587.922665	7313.320815	14.856167	-0.113985	4.609925
587.095336	7305.389164	14.861171	-0.113826	4.607472
587.230401	7297.330821	14.866176	-0.113846	4.604980
587.189114	7289.373028	14.871181	-0.113833	4.602517
587.296634	7281.295149	14.876186	-0.113848	4.600016
587.353148	7273.404127	14.881191	-0.113853	4.597572
587.095687	7265.352060	14.886195	-0.113800	4.595076
587.067961	7257.352067	14.891200	-0.113790	4.592595
586.865843	7249.326820	14.896205	-0.113747	4.590104
587.078850	7241.275401	14.901210	-0.113781	4.587605
587.217387	7233.317996	14.906215	-0.113802	4.585133
587.009246	7225.291878	14.911219	-0.113758	4.582638
587.088495	7217.327255	14.916224	-0.113767	4.580162
587.482820	7209.283307	14.921229	-0.113836	4.577659
586.905835	7201.294092	14.926234	-0.113723	4.575171
586.528002	7193.381671	14.931239	-0.113648	4.572706
587.471103	7185.195826	14.936243	-0.113818	4.570156
587.520277	7177.275964	14.941248	-0.113822	4.567687
587.268793	7169.297930	14.946253	-0.113770	4.565198
587.231418	7161.360181	14.951258	-0.113758	4.562720
587.110733	7153.362283	14.956263	-0.113730	4.560221
587.028192	7145.304680	14.961267	-0.113709	4.557703
587.094655	7137.295590	14.966272	-0.113717	4.555199
586.993017	7129.334834	14.971277	-0.113693	4.552708
586.783092	7121.294425	14.976282	-0.113648	4.550191
587.061419	7113.293190	14.981287	-0.113695	4.547686
586.843338	7105.247859	14.986291	-0.113649	4.545164
587.010006	7097.262121	14.991296	-0.113675	4.542660
587.090464	7089.236581	14.996301	-0.113685	4.540143
586.823749	7081.283666	15.001306	-0.113630	4.537646
587.058547	7073.278760	15.006311	-0.113668	4.535132
586.947248	7065.249121	15.011315	-0.113642	4.532609
587.200537	7057.260802	15.016320	-0.113684	4.530098
587.278384	7049.262382	15.021325	-0.113694	4.527582
586.865165	7041.250684	15.026330	-0.113611	4.525059
586.906869	7033.309097	15.031335	-0.113614	4.522558
586.709945	7025.281873	15.036339	-0.113572	4.520028
586.800442	7017.307140	15.041344	-0.113584	4.517514
586.291564	7009.335380	15.046349	-0.113484	4.514997
586.833969	7001.244734	15.051354	-0.113580	4.512445
586.958773	6993.213834	15.056359	-0.113598	4.509909
586.940486	6985.211519	15.061363	-0.113589	4.507380
586.815318	6977.192068	15.066368	-0.113561	4.504844
586.900719	6969.236226	15.071373	-0.113571	4.502328
586.818868	6961.161309	15.076378	-0.113551	4.499771
586.765386	6953.244454	15.081383	-0.113536	4.497264
586.590816	6945.177726	15.086387	-0.113498	4.494707
586.667712	6937.241871	15.091392	-0.113507	4.492191
586.573195	6929.177565	15.096397	-0.113484	4.489632
586.363231	6921.223426	15.101402	-0.113440	4.487106
586.368534	6913.187859	15.106407	-0.113436	4.484554
586.090805	6905.223032	15.111411	-0.113379	4.482022
586.340771	6897.166256	15.116416	-0.113420	4.479461
586.495467	6889.187740	15.121421	-0.113444	4.476923
586.279669	6881.193727	15.126426	-0.113398	4.474377
586.239286	6873.261944	15.131431	-0.113386	4.471851
586.175990	6865.140077	15.136435	-0.113369	4.469262
586.354424	6857.191122	15.141440	-0.113397	4.466728
586.346075	6849.118954	15.146445	-0.113390	4.464152
586.439298	6841.188932	15.151450	-0.113402	4.461621
586.584529	6833.160093	15.156455	-0.113424	4.459057
586.143125	6825.221933	15.161459	-0.113337	4.456517
586.096673	6817.167864	15.166464	-0.113323	4.453941
586.533532	6809.157551	15.171469	-0.113399	4.451380
586.520027	6801.106416	15.176474	-0.113391	4.448802
586.546598	6793.177268	15.181479	-0.113391	4.446262
586.248135	6785.148339	15.186483	-0.113330	4.443687
586.038289	6777.264955	15.191488	-0.113286	4.441158
586.084373	6769.180027	15.196493	-0.113289	4.438563
586.110124	6761.140948	15.201498	-0.113289	4.435982
586.318736	6753.177564	15.206503	-0.113323	4.433425
585.772241	6745.159581	15.211507	-0.113216	4.430844
585.635196	6737.165269	15.216512	-0.113185	4.428272
585.611406	6729.118584	15.221517	-0.113175	4.425682
585.323367	6721.165210	15.226522	-0.113116	4.423119
585.726084	6713.119074	15.231527	-0.113186	4.420529
585.771294	6705.089224	15.236531	-0.113189	4.417940
585.930604	6697.065064	15.241536	-0.113214	4.415352
585.537428	6689.165129	15.246541	-0.113135	4.412800
585.311146	6681.112462	15.251546	-0.113088	4.410198
585.799876	6673.102482	15.256551	-0.113174	4.407612
585.670221	6665.062481	15.261555	-0.113145	4.405011
585.850058	6657.161678	15.266560	-0.113173	4.402456
585.724072	6649.091559	15.271565	-0.113144	4.399842
585.559022	6641.149360	15.276570	-0.113108	4.397268
585.765081	6633.106883	15.281575	-0.113141	4.394663
585.311158	6625.182343	15.286579	-0.113052	4.392090
585.411329	6617.093598	15.291584	-0.113065	4.389466
585.286407	6609.168656	15.296589	-0.113037	4.386891
585.163885	6601.096601	15.301594	-0.113009	4.384268
585.022038	6593.171892	15.306599	-0.112977	4.381691
584.726706	6585.116733	15.311603	-0.112917	4.379069
584.853780	6577.185757	15.316608	-0.112935	4.376488
584.517685	6569.219732	15.321613	-0.112868	4.373891
585.019730	6561.118238	15.326618	-0.112956	4.371255
584.388888	6553.186977	15.331623	-0.112833	4.368664
584.283900	6545.195413	15.336627	-0.112808	4.366056
584.428994	6537.175792	15.341632	-0.112830	4.363439
584.614675	6529.177287	15.346637	-0.112860	4.360827
585.065368	6521.121602	15.351642	-0.112938	4.358197
584.840644	6513.237615	15.356647	-0.112891	4.355617
584.868663	6505.119326	15.361651	-0.112891	4.352961
584.240005	6497.177437	15.366656	-0.112769	4.350356
584.177149	6489.184420	15.371661	-0.112752	4.347737
584.440052	6481.069143	15.376666	-0.112796	4.345078
584.655131	6473.144368	15.381671	-0.112831	4.342480
584.615619	6465.083524	15.386675	-0.112818	4.339834
584.677293	6457.184980	15.391680	-0.112825	4.337240
584.453540	6449.188425	15.396685	-0.112778	4.334610
584.354221	6441.178780	15.401690	-0.112754	4.331975
584.229540	6433.229656	15.406695	-0.112726	4.329359
583.941529	6425.208633	15.411699	-0.112667	4.326716
584.006215	6417.168229	15.416704	-0.112674	4.324067
584.385217	6409.220901	15.421709	-0.112739	4.321451
584.165184	6401.194165	15.426714	-0.112693	4.318801
583.945888	6393.226335	15.431719	-0.112647	4.316170
583.819442	6385.197886	15.436723	-0.112618	4.313517
584.166088	6377.168507	15.441728	-0.112677	4.310867
583.893780	6369.181875	15.446733	-0.112621	4.308224
583.668302	6361.153819	15.451738	-0.112574	4.305566
583.981206	6353.154077	15.456743	-0.112627	4.302920
583.950365	6345.100938	15.461747	-0.112616	4.300252
583.529513	6337.219050	15.466752	-0.112533	4.297635
583.650241	6329.140042	15.471757	-0.112550	4.294957
583.659844	6321.133794	15.476762	-0.112547	4.292299
583.653463	6313.128225	15.481767	-0.112540	4.289641
583.747567	6305.095876	15.486771	-0.112553	4.286972
583.712816	6297.082231	15.491776	-0.112541	4.284307
583.622637	6289.185759	15.496781	-0.112519	4.281679
583.537532	6281.127176	15.501786	-0.112498	4.278996
583.659956	6273.207674	15.506791	-0.112516	4.276359
583.509399	6265.151578	15.511795	-0.112482	4.273672
583.940767	6257.078110	15.516800	-0.112557	4.270983
583.981051	6249.048413	15.521805	-0.112560	4.268303
583.743216	6241.123067	15.526810	-0.112510	4.265654
583.910735	6233.133493	15.531815	-0.112536	4.262986
583.752727	6225.125373	15.536819	-0.112502	4.260306
583.889734	6217.141036	15.541824	-0.112522	4.257636
583.833026	6209.113132	15.546829	-0.112506	4.254948
583.407620	6201.184786	15.551834	-0.112422	4.252288
584.040225	6193.027039	15.556839	-0.112534	4.249559
583.934990	6185.120961	15.561843	-0.112510	4.246906
584.040551	6177.063982	15.566848	-0.112524	4.244203
583.879093	6169.188185	15.571853	-0.112489	4.241556
584.004311	6161.084115	15.576858	-0.112507	4.238833
584.177998	6153.188857	15.581863	-0.112534	4.236180
584.190682	6145.095581	15.586867	-0.112531	4.233457
584.421173	6137.078767	15.591872	-0.112569	4.230760
583.813862	6129.175917	15.596877	-0.112451	4.228091
583.789303	6121.109523	15.601882	-0.112441	4.225371
584.061093	6113.134465	15.606887	-0.112486	4.222683
584.170511	6105.083453	15.611891	-0.112501	4.219966
584.121983	6097.128456	15.616896	-0.112487	4.217278
583.817025	6089.158934	15.621901	-0.112425	4.214581
583.550823	6081.149128	15.626906	-0.112370	4.211869
583.741448	6073.115277	15.631911	-0.112401	4.209152
583.551723	6065.142057	15.636915	-0.112360	4.206450
583.162844	6057.151925	15.641920	-0.112283	4.203738
583.943130	6049.106147	15.646925	-0.112423	4.201018
583.757844	6041.092206	15.651930	-0.112383	4.198296
583.838704	6033.146495	15.656935	-0.112393	4.195599
583.537942	6025.115602	15.661939	-0.112332	4.192867
583.548393	6017.061370	15.666944	-0.112328	4.190129
583.561817	6009.071016	15.671949	-0.112326	4.187410
583.536053	6001.049585	15.676954	-0.112316	4.184679
583.534728	5993.111371	15.681959	-0.112310	4.181975
583.221298	5985.122083	15.686963	-0.112247	4.179248
583.257664	5977.118857	15.691968	-0.112248	4.176518
583.348361	5969.117158	15.696973	-0.112260	4.173788
583.265410	5961.071849	15.701978	-0.112239	4.171039
583.106252	5953.092979	15.706983	-0.112204	4.168310
583.301292	5945.054997	15.711987	-0.112236	4.165564
583.347236	5937.084943	15.716992	-0.112239	4.162837
583.101546	5929.113103	15.721997	-0.112188	4.160104
583.086850	5921.102874	15.727002	-0.112180	4.157358
583.330643	5913.103265	15.732007	-0.112220	4.154618
583.390397	5905.124556	15.737011	-0.112226	4.151881
583.494267	5897.056784	15.742016	-0.112240	4.149112
583.321258	5889.097986	15.747021	-0.112203	4.146376
583.053350	5881.111679	15.752026	-0.112148	4.143626
583.199269	5873.140987	15.757031	-0.112170	4.140886
583.212301	5865.127848	15.762035	-0.112167	4.138127
583.332811	5857.096134	15.767040	-0.112184	4.135362
583.342281	5849.112824	15.772045	-0.112181	4.132610
582.904023	5841.099159	15.777050	-0.112094	4.129840
583.021513	5833.137005	15.782055	-0.112111	4.127092
582.794104	5825.121809	15.787059	-0.112063	4.124321
582.982457	5817.153143	15.792064	-0.112093	4.121569
583.058726	5809.171465	15.797069	-0.112102	4.118809
582.704593	5801.239628	15.802074	-0.112031	4.116059
582.984928	5793.113901	15.807079	-0.112078	4.113248
582.495709	5785.183814	15.812083	-0.111982	4.110493
582.810999	5777.145936	15.817088	-0.112035	4.107709
582.865301	5769.108344	15.822093	-0.112040	4.104920
582.485601	5761.160721	15.827098	-0.111964	4.102155
582.660056	5753.135584	15.832103	-0.111991	4.099368
582.519205	5745.195707	15.837107	-0.111960	4.096605
582.263423	5737.158242	15.842112	-0.111907	4.093804
582.237190	5729.180782	15.847117	-0.111897	4.091026
582.445266	5721.071224	15.852122	-0.111931	4.088202
582.451986	5713.080075	15.857127	-0.111927	4.085416
582.081134	5705.149145	15.862131	-0.111852	4.082643
582.258150	5697.126224	15.867136	-0.111880	4.079843
582.246285	5689.175469	15.872141	-0.111873	4.077065
582.187996	5681.090166	15.877146	-0.111857	4.074237
582.150721	5673.198708	15.882151	-0.111845	4.071475
582.140050	5665.116332	15.887155	-0.111837	4.068644
582.107329	5657.181237	15.892160	-0.111826	4.065863
582.158498	5649.155492	15.897165	-0.111830	4.063050
582.404673	5641.088785	15.902170	-0.111871	4.060223
582.251759	5633.152131	15.907175	-0.111837	4.057433
581.958908	5625.151495	15.912179	-0.111778	4.054618
581.871943	5617.175217	15.917184	-0.111756	4.051812
581.707164	5609.155536	15.922189	-0.111720	4.048987
581.601489	5601.165556	15.927194	-0.111696	4.046172
581.545256	5593.166635	15.932199	-0.111680	4.043353
581.544462	5585.166474	15.937203	-0.111675	4.040531
581.381752	5577.199364	15.942208	-0.111639	4.037718
581.399881	5569.167152	15.947213	-0.111637	4.034882
581.501792	5561.105079	15.952218	-0.111651	4.032034
581.970761	5553.037621	15.957223	-0.111733	4.029189
581.450516	5545.094864	15.962227	-0.111631	4.026370
581.278635	5537.113168	15.967232	-0.111594	4.023541
581.466056	5529.156191	15.972237	-0.111624	4.020724
581.666559	5521.114357	15.977242	-0.111656	4.017876
581.735852	5513.165028	15.982247	-0.111663	4.015056
581.546588	5505.089819	15.987251	-0.111623	4.012185
581.377438	5497.121426	15.992256	-0.111586	4.009351
581.478265	5489.144556	15.997261	-0.111600	4.006516
581.681196	5481.082630	16.002266	-0.111632	4.003650
581.824993	5473.149204	16.007271	-0.111654	4.000827
581.427021	5465.197554	16.012275	-0.111575	3.997987
581.576585	5457.203331	16.017280	-0.111597	3.995138
580.966765	5449.283699	16.022285	-0.111479	3.992302
580.731674	5441.217693	16.027290	-0.111430	3.989417
581.302916	5433.151696	16.032295	-0.111531	3.986544
580.852401	5425.196651	16.037299	-0.111442	3.983691
580.746095	5417.207502	16.042304	-0.111417	3.980829
581.244384	5409.161144	16.047309	-0.111504	3.977956
580.946159	5401.198840	16.052314	-0.111444	3.975097
581.161917	5393.214913	16.057319	-0.111479	3.972237
581.090572	5385.147140	16.062323	-0.111460	3.969340
581.252187	5377.152991	16.067328	-0.111485	3.966471
581.088492	5369.197860	16.072333	-0.111449	3.963608
581.065364	5361.216481	16.077338	-0.111440	3.960737
581.067164	5353.238810	16.082343	-0.111435	3.957865
580.451161	5345.259438	16.087347	-0.111315	3.954979
580.784733	5337.193034	16.092352	-0.111372	3.952077
581.070461	5329.158166	16.097357	-0.111420	3.949183
580.463236	5321.245590	16.102362	-0.111302	3.946315
580.499656	5313.227168	16.107367	-0.111303	3.943418
580.393157	5305.233071	16.112371	-0.111278	3.940526
580.399100	5297.224530	16.117376	-0.111274	3.937628
580.877595	5289.129744	16.122381	-0.111358	3.934706
580.713409	5281.195052	16.127386	-0.111322	3.931827
580.705706	5273.178186	16.132391	-0.111316	3.928920
580.168374	5265.266775	16.137395	-0.111210	3.926038
580.154081	5257.231255	16.142400	-0.111203	3.923120
580.352084	5249.230209	16.147405	-0.111234	3.920215
580.301006	5241.210237	16.152410	-0.111220	3.917297
580.190143	5233.265411	16.157415	-0.111194	3.914403
579.901088	5225.243341	16.162419	-0.111135	3.911475
579.790111	5217.241142	16.167424	-0.111109	3.908556
580.292012	5209.210867	16.172429	-0.111197	3.905636
580.112293	5201.237940	16.177434	-0.111158	3.902721
579.919946	5193.310162	16.182439	-0.111117	3.899821
579.758674	5185.276607	16.187443	-0.111082	3.896880
579.617455	5177.247264	16.192448	-0.111051	3.893939
579.885465	5169.244634	16.197453	-0.111095	3.891014
580.028370	5161.191658	16.202458	-0.111117	3.888066
579.799024	5153.250863	16.207463	-0.111069	3.885149
579.499093	5145.297020	16.212467	-0.111008	3.882223
580.154058	5137.173114	16.217472	-0.111125	3.879253
580.319737	5129.275542	16.222477	-0.111150	3.876353
580.205448	5121.156581	16.227482	-0.111124	3.873364
580.183661	5113.106655	16.232487	-0.111114	3.870400
580.293718	5105.157255	16.237491	-0.111130	3.867473
580.357452	5097.134304	16.242496	-0.111136	3.864516
580.338169	5089.237127	16.247501	-0.111128	3.861602
580.074731	5081.246344	16.252506	-0.111073	3.858646
579.970384	5073.311139	16.257511	-0.111049	3.855711
579.597550	5065.317838	16.262515	-0.110974	3.852747
579.312776	5057.314916	16.267520	-0.110916	3.849779
579.399526	5049.303111	16.272525	-0.110927	3.846813
579.509834	5041.222029	16.277530	-0.110942	3.843820
579.574074	5033.339105	16.282535	-0.110949	3.840897
579.790232	5025.240789	16.287539	-0.110984	3.837894
579.707506	5017.280981	16.292544	-0.110963	3.834935
579.746111	5009.311965	16.297549	-0.110965	3.831973
579.563018	5001.299882	16.302554	-0.110926	3.828987
579.819405	4993.309659	16.307559	-0.110969	3.826017
579.449143	4985.300108	16.312563	-0.110895	3.823023
579.315204	4977.316640	16.317568	-0.110864	3.820043
579.635740	4969.321994	16.322573	-0.110919	3.817065
579.779594	4961.222734	16.327578	-0.110940	3.814042
579.915556	4953.297238	16.332583	-0.110961	3.811082
579.930143	4945.289128	16.337587	-0.110958	3.808086
579.789485	4937.294052	16.342592	-0.110927	3.805089
579.867131	4929.338119	16.347597	-0.110936	3.802109
579.576631	4921.324727	16.352602	-0.110877	3.799097
579.709119	4913.403833	16.357607	-0.110896	3.796126
579.374856	4905.378469	16.362611	-0.110829	3.793104
578.588601	4897.418511	16.367616	-0.110677	3.790093
579.046043	4889.335918	16.372621	-0.110757	3.787063
578.747101	4881.323837	16.377626	-0.110696	3.784039
578.893498	4873.366480	16.382631	-0.110718	3.781043
578.682941	4865.371855	16.387635	-0.110674	3.778023
578.352374	4857.428293	16.392640	-0.110607	3.775017
578.651205	4849.347529	16.397645	-0.110658	3.771971
578.374310	4841.354140	16.402650	-0.110601	3.768942
578.126629	4833.442194	16.407655	-0.110550	3.765943
578.507805	4825.337693	16.412659	-0.110615	3.762882
578.635753	4817.351757	16.417664	-0.110634	3.759859
578.962271	4809.369645	16.422669	-0.110690	3.756839
578.588265	4801.381878	16.427674	-0.110615	3.753798
578.835065	4793.391243	16.432679	-0.110656	3.750768
578.566335	4785.400121	16.437683	-0.110600	3.747723
579.113598	4777.313906	16.442688	-0.110697	3.744659
578.942450	4769.377231	16.447693	-0.110660	3.741632
578.866740	4761.418870	16.452698	-0.110641	3.738597
578.797527	4753.475595	16.457703	-0.110623	3.735565
578.707942	4745.484527	16.462707	-0.110601	3.732512
578.772211	4737.413375	16.467712	-0.110607	3.729430
578.843481	4729.438189	16.472717	-0.110616	3.726382
578.685850	4721.441912	16.477722	-0.110581	3.723318
578.917500	4713.438438	16.482727	-0.110619	3.720258
578.694705	4705.482428	16.487731	-0.110572	3.717202
578.773086	4697.421491	16.492736	-0.110582	3.714111
578.568539	4689.461341	16.497741	-0.110538	3.711050
578.355406	4681.409354	16.502746	-0.110493	3.707950
578.733968	4673.407986	16.507751	-0.110559	3.704882
578.470301	4665.467670	16.512755	-0.110504	3.701819
578.216623	4657.472637	16.517760	-0.110452	3.698732
578.010813	4649.528966	16.522765	-0.110409	3.695664
578.489372	4641.446111	16.527770	-0.110492	3.692556
578.533263	4633.433646	16.532775	-0.110495	3.689463
578.348584	4625.440786	16.537779	-0.110456	3.686368
578.120076	4617.485097	16.542784	-0.110408	3.683284
578.077563	4609.533310	16.547789	-0.110395	3.680204
577.942010	4601.501892	16.552794	-0.110365	3.677088
578.457084	4593.465416	16.557799	-0.110455	3.673985
578.243021	4585.529301	16.562803	-0.110410	3.670898
577.950337	4577.496087	16.567808	-0.110351	3.667769
578.312316	4569.457195	16.572813	-0.110413	3.664653
578.234429	4561.507271	16.577818	-0.110393	3.661557
578.058753	4553.546803	16.582823	-0.110355	3.658451
577.808273	4545.566318	16.587827	-0.110303	3.655333
577.938100	4537.537665	16.592832	-0.110322	3.652204
578.203456	4529.484865	16.597837	-0.110366	3.649067
577.954111	4521.539347	16.602842	-0.110315	3.645954
578.031320	4513.558811	16.607847	-0.110324	3.642835
578.002581	4505.563799	16.612851	-0.110313	3.639703
577.932399	4497.612835	16.617856	-0.110295	3.636586
578.156547	4489.597105	16.622861	-0.110332	3.633448
577.676834	4481.630684	16.627866	-0.110237	3.630308
577.915082	4473.598369	16.632871	-0.110276	3.627159
577.687898	4465.563870	16.637875	-0.110229	3.623993
577.668033	4457.638316	16.642880	-0.110220	3.620873
577.446630	4449.658715	16.647885	-0.110174	3.617724
577.471805	4441.604427	16.652890	-0.110173	3.614549
577.217212	4433.691145	16.657895	-0.110121	3.611419
577.384551	4425.588585	16.662899	-0.110146	3.608224
577.528192	4417.580100	16.667904	-0.110168	3.605062
577.265229	4409.663178	16.672909	-0.110114	3.601922
577.246595	4401.625252	16.677914	-0.110105	3.598739
577.185576	4393.676267	16.682919	-0.110089	3.595586
577.098153	4385.651250	16.687923	-0.110067	3.592400
577.155569	4377.622032	16.692928	-0.110073	3.589214
577.175910	4369.676454	16.697933	-0.110071	3.586057
577.147086	4361.615948	16.702938	-0.110061	3.582850
577.239028	4353.662744	16.707943	-0.110073	3.579687
577.290850	4345.674855	16.712947	-0.110077	3.576505
576.717040	4337.751315	16.717952	-0.109965	3.573328
576.893067	4329.696576	16.722957	-0.109993	3.570118
576.867888	4321.672569	16.727962	-0.109983	3.566912
577.174731	4313.652878	16.732967	-0.110035	3.563714
576.941952	4305.704778	16.737971	-0.109986	3.560526
577.103721	4297.726535	16.742976	-0.110011	3.557334
577.181135	4289.717364	16.747981	-0.110020	3.554125
576.830026	4281.684713	16.752986	-0.109950	3.550891
576.677882	4273.722973	16.757991	-0.109916	3.547688
576.733181	4265.714751	16.762995	-0.109921	3.544470
576.697022	4257.758725	16.768000	-0.109909	3.541267
576.756069	4249.712801	16.773005	-0.109915	3.538028
576.543865	4241.754531	16.778010	-0.109870	3.534813
576.782474	4233.738941	16.783015	-0.109910	3.531586
576.244000	4225.809514	16.788019	-0.109804	3.528366
576.346806	4217.746392	16.793024	-0.109818	3.525110
576.432270	4209.802294	16.798029	-0.109829	3.521898
576.364217	4201.797149	16.803034	-0.109811	3.518653
576.459598	4193.804461	16.808039	-0.109824	3.515416
576.415932	4185.837592	16.813043	-0.109810	3.512182
576.104285	4177.832883	16.818048	-0.109747	3.508921
576.409397	4169.813701	16.823053	-0.109799	3.505671
576.073118	4161.840528	16.828058	-0.109731	3.502416
576.644673	4153.760010	16.833063	-0.109832	3.499143
576.409999	4145.844374	16.838067	-0.109783	3.495909
576.347951	4137.830025	16.843072	-0.109766	3.492637
576.486132	4129.839482	16.848077	-0.109787	3.489377
576.360668	4121.829912	16.853082	-0.109758	3.486099
576.432756	4113.860291	16.858087	-0.109767	3.482840
576.347693	4105.879378	16.863091	-0.109746	3.479569
576.583884	4097.865906	16.868096	-0.109784	3.476291
576.411532	4089.884216	16.873101	-0.109747	3.473010
575.980548	4081.917986	16.878106	-0.109662	3.469724
576.473026	4073.870068	16.883111	-0.109748	3.466432
576.012080	4065.931450	16.888115	-0.109657	3.463150
575.743476	4057.934278	16.893120	-0.109602	3.459846
576.188416	4049.935516	16.898125	-0.109680	3.456563
576.146668	4041.899737	16.903130	-0.109667	3.453246
575.880373	4033.961742	16.908135	-0.109612	3.449958
575.926001	4025.947134	16.913139	-0.109615	3.446645
575.821034	4017.964591	16.918144	-0.109590	3.443338
575.662830	4010.042341	16.923149	-0.109556	3.440050
575.559330	4001.984790	16.928154	-0.109531	3.436705
575.312583	3994.060449	16.933159	-0.109480	3.433407
575.643994	3985.997730	16.938163	-0.109537	3.430069
575.203377	3978.044106	16.943168	-0.109449	3.426746
575.302303	3970.041666	16.948173	-0.109463	3.423418
574.674413	3962.120119	16.953178	-0.109341	3.420095
574.814120	3954.097722	16.958183	-0.109361	3.416753
575.547292	3945.949841	16.963187	-0.109493	3.413377
575.179099	3938.022835	16.968192	-0.109419	3.410051
575.392888	3930.032530	16.973197	-0.109454	3.406716
575.238656	3922.038431	16.978202	-0.109420	3.403363
575.140696	3914.119754	16.983207	-0.109396	3.400040
575.077948	3906.110699	16.988211	-0.109379	3.396677
574.764880	3898.122635	16.993216	-0.109316	3.393311
575.196312	3890.046059	16.998221	-0.109391	3.389931
575.134843	3882.031134	17.003226	-0.109374	3.386556
575.181248	3874.063925	17.008231	-0.109378	3.383201
575.268747	3866.062608	17.013235	-0.109389	3.379830
575.193712	3858.106075	17.018240	-0.109370	3.376469
575.452893	3850.111090	17.023245	-0.109413	3.373101
575.278964	3842.100738	17.028250	-0.109375	3.369706
575.016658	3834.205667	17.033255	-0.109321	3.366354
575.307262	3826.125013	17.038259	-0.109370	3.362940
575.196113	3818.157108	17.043264	-0.109344	3.359556
575.292863	3810.207165	17.048269	-0.109357	3.356184
575.079498	3802.191583	17.053274	-0.109312	3.352769
575.022782	3794.225615	17.058279	-0.109296	3.349377
574.861897	3786.246082	17.063283	-0.109261	3.345972
574.645448	3778.258396	17.068288	-0.109216	3.342558
574.789536	3770.256833	17.073293	-0.109237	3.339148
574.789372	3762.256351	17.078298	-0.109232	3.335730
574.806943	3754.263970	17.083303	-0.109230	3.332312
574.880766	3746.247847	17.088307	-0.109239	3.328883
574.972628	3738.257285	17.093312	-0.109251	3.325462
574.620813	3730.336830	17.098317	-0.109180	3.322051
574.859041	3722.295184	17.103322	-0.109219	3.318606
574.715057	3714.337220	17.108327	-0.109187	3.315179
574.609217	3706.349346	17.113331	-0.109162	3.311738
574.491989	3698.336807	17.118336	-0.109135	3.308281
574.692895	3690.329483	17.123341	-0.109167	3.304836
574.226306	3682.386099	17.128346	-0.109075	3.301389
574.200070	3674.379791	17.133351	-0.109065	3.297928
574.427309	3666.348916	17.138355	-0.109102	3.294462
574.519139	3658.337919	17.143360	-0.109114	3.290996
574.454856	3650.363154	17.148365	-0.109097	3.287537
574.311044	3642.370974	17.153370	-0.109065	3.284062
574.424865	3634.439274	17.158375	-0.109081	3.280621
574.077911	3626.476826	17.163379	-0.109011	3.277144
573.529700	3618.544992	17.168384	-0.108904	3.273669
573.753058	3610.515329	17.173389	-0.108941	3.270179
573.225913	3602.538043	17.178394	-0.108837	3.266677
573.976329	3594.418393	17.183399	-0.108972	3.263161
573.805095	3586.476360	17.188403	-0.108935	3.259681
573.280359	3578.574145	17.193408	-0.108832	3.256201
573.430698	3570.538348	17.198413	-0.108855	3.252686
573.359473	3562.511105	17.203418	-0.108836	3.249162
573.730795	3554.497631	17.208423	-0.108900	3.245658
573.291646	3546.573858	17.213427	-0.108813	3.242157
573.437203	3538.541853	17.218432	-0.108835	3.238628
573.584206	3530.575767	17.223437	-0.108857	3.235124
573.487814	3522.568200	17.228442	-0.108834	3.231589
573.320239	3514.583912	17.233447	-0.108798	3.228056
573.462925	3506.563698	17.238451	-0.108819	3.224517
573.332473	3498.616783	17.243456	-0.108790	3.220995
573.149478	3490.651899	17.248461	-0.108750	3.217459
573.118834	3482.632176	17.253466	-0.108739	3.213902
572.982587	3474.664411	17.258471	-0.108709	3.210358
573.212083	3466.602614	17.263475	-0.108746	3.206785
572.868773	3458.691966	17.268480	-0.108677	3.203251
573.305934	3450.655413	17.273485	-0.108753	3.199689
572.969992	3442.720499	17.278490	-0.108686	3.196136
572.970336	3434.709899	17.283495	-0.108681	3.192560
573.799127	3426.578381	17.288499	-0.108830	3.188962
573.497921	3418.659309	17.293504	-0.108768	3.185405
573.336895	3410.735008	17.298509	-0.108733	3.181849
573.247588	3402.754267	17.303514	-0.108711	3.178266
573.117334	3394.810866	17.308519	-0.108682	3.174694
573.282830	3386.770701	17.313523	-0.108708	3.171087
573.075291	3378.782133	17.318528	-0.108664	3.167484
572.869349	3370.846244	17.323533	-0.108620	3.163900
572.833146	3362.857904	17.328538	-0.108608	3.160295
573.195085	3354.830751	17.333543	-0.108671	3.156687
573.271166	3346.828205	17.338547	-0.108680	3.153073
572.856692	3338.875412	17.343552	-0.108597	3.149455
572.930527	3330.870810	17.348557	-0.108606	3.145832
572.757878	3322.899021	17.353562	-0.108568	3.142208
572.710953	3314.935086	17.358567	-0.108555	3.138590
572.619846	3306.914735	17.363571	-0.108532	3.134939
572.128979	3299.006505	17.368576	-0.108436	3.131317
572.015961	3291.018758	17.373581	-0.108410	3.127672
572.168764	3282.937310	17.378586	-0.108433	3.123992
571.990650	3275.000116	17.383591	-0.108394	3.120358
572.118666	3266.994570	17.388595	-0.108413	3.116703
572.114657	3258.985004	17.393600	-0.108407	3.113035
572.046742	3251.015120	17.398605	-0.108389	3.109379
571.724178	3243.075500	17.403610	-0.108324	3.105720
571.630135	3235.100644	17.408615	-0.108301	3.102052
571.667504	3227.095552	17.413619	-0.108303	3.098371
571.109655	3219.177783	17.418624	-0.108194	3.094698
571.189937	3211.172542	17.423629	-0.108204	3.091010
571.641843	3203.039732	17.428634	-0.108283	3.087277
571.432257	3195.126936	17.433639	-0.108239	3.083609
571.203015	3187.186561	17.438643	-0.108191	3.079924
571.166861	3179.184239	17.443648	-0.108179	3.076214
571.012136	3171.196325	17.448653	-0.108145	3.072501
570.801671	3163.175496	17.453658	-0.108100	3.068766
571.225366	3155.153752	17.458663	-0.108174	3.065055
571.207216	3147.172233	17.463667	-0.108165	3.061338
570.872106	3139.224397	17.468672	-0.108098	3.057617
571.228939	3131.188865	17.473677	-0.108159	3.053884
571.446932	3123.149972	17.478682	-0.108195	3.050138
571.374606	3115.212963	17.483687	-0.108176	3.046421
571.254016	3107.262719	17.488691	-0.108148	3.042691
571.367473	3099.240057	17.493696	-0.108164	3.038933
571.334886	3091.341484	17.498701	-0.108153	3.035223
571.363671	3083.318769	17.503706	-0.108153	3.031452
571.544563	3075.296071	17.508711	-0.108182	3.027684
571.912641	3067.236504	17.513715	-0.108245	3.023903
571.465925	3059.363641	17.518720	-0.108157	3.020165
571.754689	3051.374504	17.523725	-0.108205	3.016405
571.664757	3043.392898	17.528730	-0.108183	3.012624
571.205822	3035.478115	17.533735	-0.108093	3.008852
571.503317	3027.419788	17.538739	-0.108143	3.005044
571.563541	3019.471566	17.543744	-0.108149	3.001273
571.547203	3011.511253	17.548749	-0.108141	2.997487
571.513466	3003.507157	17.553754	-0.108129	2.993674
571.607868	2995.524490	17.558759	-0.108142	2.989873
571.208044	2987.577897	17.563763	-0.108062	2.986060
570.711715	2979.628489	17.568768	-0.107964	2.982235
570.865558	2971.624430	17.573773	-0.107988	2.978412
570.897501	2963.582449	17.578778	-0.107989	2.974560
570.476971	2955.683419	17.583783	-0.107905	2.970749
570.799775	2947.609450	17.588787	-0.107960	2.966887
570.574375	2939.664019	17.593792	-0.107913	2.963053
570.792380	2931.651896	17.598797	-0.107948	2.959205
570.665156	2923.695888	17.603802	-0.107919	2.955361
570.588978	2915.721501	17.608807	-0.107900	2.951506
571.072055	2907.665161	17.613811	-0.107985	2.947636
571.040369	2899.673919	17.618816	-0.107974	2.943765
570.482164	2891.827870	17.623821	-0.107865	2.939931
570.492400	2883.820328	17.628826	-0.107861	2.936044
570.287573	2875.850141	17.633831	-0.107818	2.932159
570.552243	2867.798753	17.638835	-0.107862	2.928254
570.320685	2859.816328	17.643840	-0.107814	2.924351
570.643021	2851.846365	17.648845	-0.107869	2.920478
570.339179	2843.902219	17.653850	-0.107807	2.916580
570.156225	2835.925542	17.658855	-0.107768	2.912666
569.856977	2827.926074	17.663859	-0.107707	2.908730
569.801313	2819.899153	17.668864	-0.107691	2.904788
570.233504	2811.905180	17.673869	-0.107766	2.900884
569.928880	2803.989745	17.678874	-0.107704	2.896972
569.627148	2796.026584	17.683879	-0.107643	2.893032
569.675499	2788.012594	17.688883	-0.107647	2.889081
569.358965	2780.071810	17.693888	-0.107583	2.885141
569.458889	2772.083419	17.698893	-0.107596	2.881194
569.447346	2764.055449	17.703898	-0.107589	2.877216
569.746086	2756.030756	17.708903	-0.107639	2.873252
569.476991	2748.114192	17.713907	-0.107584	2.869304
568.832777	2740.215855	17.718912	-0.107459	2.865339
568.953192	2732.226134	17.723917	-0.107476	2.861366
568.747110	2724.240616	17.728922	-0.107433	2.857370
568.991857	2716.192790	17.733927	-0.107473	2.853364
569.015651	2708.188707	17.738931	-0.107472	2.849361
569.060928	2700.199642	17.743936	-0.107475	2.845362
569.473995	2692.220301	17.748941	-0.107547	2.841382
569.209407	2684.258460	17.753946	-0.107493	2.837367
569.362120	2676.262804	17.758951	-0.107516	2.833354
569.588384	2668.256347	17.763955	-0.107553	2.829333
569.178643	2660.343381	17.768960	-0.107471	2.825317
569.084210	2652.405040	17.773965	-0.107449	2.821301
569.432817	2644.354299	17.778970	-0.107508	2.817248
569.000754	2636.441901	17.783975	-0.107423	2.813214
568.724194	2628.487471	17.788979	-0.107366	2.809162
568.410787	2620.536656	17.793984	-0.107303	2.805103
568.320446	2612.596807	17.798989	-0.107281	2.801057
567.979274	2604.614339	17.803994	-0.107212	2.796969
568.101605	2596.601456	17.808999	-0.107229	2.792887
568.472957	2588.519337	17.814003	-0.107293	2.788778
568.418821	2580.535123	17.819008	-0.107278	2.784688
568.760252	2572.558440	17.824013	-0.107336	2.780619
568.462779	2564.635810	17.829018	-0.107276	2.776534
568.246856	2556.692386	17.834023	-0.107231	2.772437
568.154015	2548.703353	17.839027	-0.107208	2.768318
568.316589	2540.659922	17.844032	-0.107233	2.764180
568.684266	2532.684619	17.849037	-0.107296	2.760084
568.366365	2524.760232	17.854042	-0.107232	2.755966
568.115721	2516.796552	17.859047	-0.107180	2.751825
568.328666	2508.763051	17.864051	-0.107215	2.747671
568.399564	2500.759023	17.869056	-0.107223	2.743517
568.420707	2492.808959	17.874061	-0.107221	2.739381
568.078168	2484.887814	17.879066	-0.107152	2.735232
568.101291	2476.895856	17.884071	-0.107152	2.731062
568.178354	2468.882197	17.889075	-0.107161	2.726878
567.927565	2460.959913	17.894080	-0.107109	2.722715
567.894420	2453.026203	17.899085	-0.107098	2.718553
567.934247	2445.022245	17.904090	-0.107100	2.714352
567.675121	2437.086732	17.909095	-0.107046	2.710162
567.919881	2429.050300	17.914099	-0.107087	2.705945
567.594731	2421.131009	17.919104	-0.107021	2.701746
567.684733	2413.148122	17.924109	-0.107033	2.697533
567.230893	2405.229848	17.929114	-0.106943	2.693314
567.467239	2397.157092	17.934119	-0.106982	2.689050
567.481391	2389.213263	17.939123	-0.106979	2.684833
567.653433	2381.204055	17.944128	-0.107006	2.680585
567.628007	2373.265441	17.949133	-0.106996	2.676355
567.639330	2365.261810	17.954138	-0.106993	2.672087
567.818881	2357.248089	17.959143	-0.107021	2.667817
568.010120	2349.263149	17.964147	-0.107052	2.663556
567.880019	2341.305776	17.969152	-0.107022	2.659282
567.548789	2333.431838	17.974157	-0.106956	2.655033
567.309706	2325.458725	17.979162	-0.106906	2.650730
567.344508	2317.468475	17.984167	-0.106907	2.646429
567.328119	2309.492873	17.989171	-0.106899	2.642125
567.429726	2301.502721	17.994176	-0.106913	2.637814
567.494142	2293.554370	17.999181	-0.106919	2.633516
567.235456	2285.583003	18.004186	-0.106866	2.629177
567.107412	2277.621670	18.009191	-0.106837	2.624846
566.947003	2269.685886	18.014195	-0.106802	2.620518
566.946048	2261.701959	18.019200	-0.106797	2.616168
566.560829	2253.788896	18.024205	-0.106720	2.611823
566.550019	2245.761480	18.029210	-0.106713	2.607434
566.485107	2237.801909	18.034215	-0.106695	2.603071
566.621418	2229.821718	18.039219	-0.106716	2.598703
566.835713	2221.806475	18.044224	-0.106750	2.594314
566.496061	2213.794012	18.049229	-0.106682	2.589881
566.325155	2205.803389	18.054234	-0.106645	2.585464
566.218208	2197.892175	18.059239	-0.106620	2.581088
566.395378	2189.900242	18.064243	-0.106647	2.576679
566.057154	2181.973753	18.069248	-0.106579	2.572263
565.808803	2174.043524	18.074253	-0.106528	2.567843
565.346858	2166.105634	18.079258	-0.106437	2.563397
565.831691	2158.056602	18.084263	-0.106522	2.558947
566.152615	2150.040984	18.089267	-0.106576	2.554497
566.117135	2142.070548	18.094272	-0.106565	2.550040
566.199402	2134.126909	18.099277	-0.106575	2.545598
565.994349	2126.206515	18.104282	-0.106531	2.541140
565.789755	2118.259833	18.109287	-0.106488	2.536660
565.760476	2110.284356	18.114291	-0.106478	2.532168
566.114294	2102.242103	18.119296	-0.106538	2.527659
565.787790	2094.350230	18.124301	-0.106472	2.523177
565.562074	2086.420200	18.129306	-0.106425	2.518673
565.656668	2078.442865	18.134311	-0.106438	2.514157
565.600404	2070.482513	18.139315	-0.106422	2.509631
565.269409	2062.511748	18.144320	-0.106355	2.505072
565.933625	2054.469033	18.149325	-0.106473	2.500536
565.434089	2046.582583	18.154330	-0.106375	2.495996
565.065946	2038.671380	18.159335	-0.106302	2.491442
565.081316	2030.678752	18.164339	-0.106299	2.486862
564.772707	2022.749257	18.169344	-0.106237	2.482286
564.984899	2014.750944	18.174349	-0.106271	2.477700
564.971538	2006.763738	18.179354	-0.106263	2.473096
564.933603	1998.806235	18.184359	-0.106251	2.468498
564.994666	1990.812869	18.189363	-0.106257	2.463878
565.082956	1982.840025	18.194368	-0.106269	2.459264
564.747232	1974.947711	18.199373	-0.106201	2.454656
564.626095	1966.974378	18.204378	-0.106173	2.450007
564.126480	1959.080283	18.209383	-0.106075	2.445368
564.345181	1951.078943	18.214387	-0.106111	2.440712
564.072123	1943.141970	18.219392	-0.106055	2.436046
564.490008	1935.073615	18.224397	-0.106127	2.431349
564.318563	1927.102119	18.229402	-0.106090	2.426653
564.409005	1919.142935	18.234407	-0.106102	2.421976
564.100760	1911.244107	18.239411	-0.106039	2.417294
563.833608	1903.296440	18.244416	-0.105984	2.412578
564.329811	1895.232443	18.249421	-0.106071	2.407843
563.913489	1887.358621	18.254426	-0.105989	2.403140
564.107763	1879.359816	18.259431	-0.106020	2.398402
563.870511	1871.462205	18.264435	-0.105970	2.393680
564.022604	1863.449199	18.269440	-0.105994	2.388911
564.366849	1855.432287	18.274445	-0.106052	2.384146
563.835534	1847.583239	18.279450	-0.105948	2.379401
564.402981	1839.523539	18.284455	-0.106049	2.374609
564.331843	1831.591488	18.289459	-0.106030	2.369833
563.908691	1823.692978	18.294464	-0.105946	2.365038
563.867822	1815.780241	18.299469	-0.105934	2.360256
563.544272	1807.867971	18.304474	-0.105868	2.355442
563.709689	1799.850491	18.309479	-0.105894	2.350594
563.670069	1791.880350	18.314483	-0.105881	2.345748
563.529286	1783.935842	18.319488	-0.105850	2.340899
563.466240	1776.012115	18.324493	-0.105833	2.336059
563.350082	1768.038121	18.329498	-0.105806	2.331174
563.522183	1760.027291	18.334503	-0.105833	2.326280
563.328991	1752.131401	18.339507	-0.105792	2.321416
563.322127	1744.158994	18.344512	-0.105786	2.316510
563.442326	1736.201217	18.349517	-0.105803	2.311613
563.495680	1728.224721	18.354522	-0.105808	2.306689
563.077535	1720.347677	18.359527	-0.105725	2.301776
563.038701	1712.392770	18.364531	-0.105712	2.296836
562.864375	1704.450858	18.369536	-0.105675	2.291882
563.212024	1696.419612	18.374541	-0.105734	2.286907
562.838234	1688.534822	18.379546	-0.105659	2.281949
562.369469	1680.674085	18.384551	-0.105567	2.276988
562.898707	1672.602905	18.389555	-0.105660	2.271971
562.339819	1664.682679	18.394560	-0.105551	2.266942
563.124529	1656.585382	18.399565	-0.105692	2.261909
563.110492	1648.656537	18.404570	-0.105684	2.256900
562.500122	1640.849141	18.409575	-0.105565	2.251905
562.449961	1632.866704	18.414579	-0.105551	2.246837
562.766006	1624.852804	18.419584	-0.105605	2.241770
563.111572	1616.877613	18.424589	-0.105664	2.236719
562.681519	1609.019417	18.429594	-0.105578	2.231662
562.417608	1601.103864	18.434599	-0.105524	2.226571
562.360009	1593.165668	18.439603	-0.105508	2.221473
562.362755	1585.202309	18.444608	-0.105504	2.216352
562.499838	1577.226059	18.449613	-0.105524	2.211223
562.152657	1569.328848	18.454618	-0.105454	2.206090
562.204300	1561.377012	18.459623	-0.105459	2.200945
562.289072	1553.421248	18.464627	-0.105469	2.195789
562.414717	1545.434685	18.469632	-0.105487	2.190604
562.608398	1537.470652	18.474637	-0.105518	2.185429
562.179337	1529.598586	18.479642	-0.105433	2.180243
561.996022	1521.680106	18.484647	-0.105394	2.175037
561.878751	1513.739716	18.489651	-0.105367	2.169811
561.760414	1505.789788	18.494656	-0.105340	2.164565
561.655541	1497.884914	18.499661	-0.105315	2.159338
562.082312	1489.852697	18.504666	-0.105389	2.154064
561.926502	1481.935059	18.509671	-0.105355	2.148797
561.581303	1474.040420	18.514675	-0.105286	2.143515
561.466485	1466.117637	18.519680	-0.105259	2.138224
561.836948	1458.125110	18.524685	-0.105323	2.132919
561.588578	1450.215263	18.529690	-0.105272	2.127596
561.707086	1442.246908	18.534695	-0.105289	2.122257
561.613381	1434.354860	18.539699	-0.105266	2.116935
561.724606	1426.371294	18.544704	-0.105282	2.111557
561.620434	1418.430865	18.549709	-0.105257	2.106174
561.419616	1410.513091	18.554714	-0.105215	2.100783
561.426708	1402.580536	18.559719	-0.105211	2.095388
561.252320	1394.671452	18.564723	-0.105173	2.089978
560.803566	1386.767044	18.569728	-0.105084	2.084529
561.218200	1378.804133	18.574733	-0.105156	2.079112
560.951761	1370.892338	18.579738	-0.105102	2.073648
561.089504	1362.937288	18.584743	-0.105122	2.068181
560.891864	1355.024486	18.589747	-0.105080	2.062694
561.109774	1347.039554	18.594752	-0.105116	2.057184
560.849272	1339.182842	18.599757	-0.105062	2.051700
560.723955	1331.250897	18.604762	-0.105033	2.046163
560.645348	1323.341659	18.609767	-0.105014	2.040632
560.621584	1315.422448	18.614771	-0.105004	2.035084
560.082739	1307.553976	18.619776	-0.104899	2.029503
560.070193	1299.603232	18.624781	-0.104891	2.023903
560.268119	1291.624135	18.629786	-0.104923	2.018290
560.287176	1283.671089	18.634791	-0.104921	2.012661
560.191668	1275.770414	18.639795	-0.104898	2.007041
559.474428	1267.957534	18.644800	-0.104760	2.001402
559.586819	1260.015046	18.649805	-0.104775	1.995743
559.654654	1252.033033	18.654810	-0.104783	1.990034
560.060793	1244.012120	18.659815	-0.104853	1.984318
560.092292	1236.127238	18.664819	-0.104854	1.978642
559.512291	1228.281002	18.669824	-0.104741	1.972913
559.434713	1220.377222	18.674829	-0.104721	1.967179
558.771017	1212.566110	18.679834	-0.104593	1.961431
558.731953	1204.631853	18.684839	-0.104580	1.955646
558.447231	1196.733883	18.689843	-0.104522	1.949842
558.639684	1188.716408	18.694848	-0.104553	1.943987
558.309818	1180.857109	18.699853	-0.104486	1.938172
558.400705	1172.875970	18.704858	-0.104498	1.932296
558.680899	1164.880297	18.709863	-0.104545	1.926413
558.535512	1157.008625	18.714867	-0.104513	1.920556
558.465210	1149.092095	18.719872	-0.104495	1.914657
558.480381	1141.186409	18.724877	-0.104492	1.908757
558.275500	1133.291896	18.729882	-0.104449	1.902822
558.317144	1125.367679	18.734887	-0.104452	1.896874
558.767519	1117.372965	18.739891	-0.104530	1.890901
558.575892	1109.479036	18.744896	-0.104489	1.884911
558.497170	1101.632564	18.749901	-0.104470	1.878952
558.651388	1093.686123	18.754906	-0.104493	1.872924
557.968457	1085.921282	18.759911	-0.104361	1.866918
558.243915	1077.931448	18.764915	-0.104407	1.860833
558.230681	1070.012536	18.769920	-0.104399	1.854748
558.317365	1062.109302	18.774925	-0.104411	1.848667
558.214902	1054.219509	18.779930	-0.104386	1.842554
558.266802	1046.299458	18.784935	-0.104391	1.836415
558.112534	1038.450176	18.789939	-0.104357	1.830286
558.086734	1030.528856	18.794944	-0.104347	1.824096
558.389532	1022.601949	18.799949	-0.104398	1.817920
558.267642	1014.723740	18.804954	-0.104370	1.811710
557.558869	1006.946891	18.809959	-0.104233	1.805486
557.478287	999.078037	18.814963	-0.104213	1.799245
557.231832	991.190289	18.819968	-0.104162	1.792947
557.602806	983.171371	18.824973	-0.104226	1.786599
557.251019	975.332353	18.829978	-0.104156	1.780282
557.343269	967.410938	18.834983	-0.104168	1.773931
557.653930	959.468219	18.839987	-0.104220	1.767569
557.193806	951.653714	18.844992	-0.104130	1.761189
556.898460	943.841952	18.849997	-0.104069	1.754810
557.138695	935.885489	18.855002	-0.104109	1.748357
556.804868	928.050193	18.860007	-0.104042	1.741906
556.662723	920.195508	18.865011	-0.104010	1.735440
556.785559	912.247804	18.870016	-0.104028	1.728907
557.270708	904.288224	18.875021	-0.104113	1.722387
557.430308	896.405593	18.880026	-0.104138	1.715864
557.381351	888.543365	18.885031	-0.104123	1.709305
557.528386	880.658013	18.890035	-0.104146	1.702728
557.200859	872.848821	18.895040	-0.104080	1.696126
557.021623	865.007474	18.900045	-0.104041	1.689491
556.346173	857.246235	18.905050	-0.103910	1.682830
556.078949	849.408680	18.910055	-0.103855	1.676134
556.480269	841.462320	18.915059	-0.103925	1.669408
556.390926	833.581721	18.920064	-0.103903	1.662644
556.074669	825.771340	18.925069	-0.103839	1.655882
555.852877	817.917824	18.930074	-0.103793	1.649069
556.106291	809.998457	18.935079	-0.103835	1.642235
555.738386	802.228892	18.940083	-0.103761	1.635417
555.840534	794.278810	18.945088	-0.103775	1.628478
555.594159	786.457808	18.950093	-0.103724	1.621574
555.455786	778.603188	18.955098	-0.103693	1.614626
555.350925	770.754920	18.960103	-0.103669	1.607658
555.640093	762.845167	18.965107	-0.103718	1.600661
555.147496	755.086888	18.970112	-0.103621	1.593657
555.171373	747.223737	18.975117	-0.103620	1.586602
555.287605	739.336680	18.980122	-0.103637	1.579508
554.614939	731.617943	18.985127	-0.103506	1.572419
554.539945	723.754500	18.990131	-0.103487	1.565253
554.555182	715.904961	18.995136	-0.103485	1.558081
554.374186	708.102411	19.000141	-0.103446	1.550889
554.163811	700.265480	19.005146	-0.103402	1.543628
554.164693	692.415127	19.010151	-0.103397	1.536352
553.549635	684.689686	19.015155	-0.103278	1.529064
553.802963	676.765098	19.020160	-0.103320	1.521687
553.868301	668.927582	19.025165	-0.103327	1.514327
553.755776	661.113358	19.030170	-0.103301	1.506926
554.205914	653.201340	19.035175	-0.103379	1.499482
553.843503	645.463685	19.040179	-0.103307	1.492042
553.502409	637.683544	19.045184	-0.103238	1.484526
553.603819	629.869581	19.050189	-0.103252	1.477010
553.395041	622.055303	19.055194	-0.103208	1.469405
553.270423	614.253088	19.060199	-0.103180	1.461786
553.377374	606.427574	19.065203	-0.103195	1.454141
553.254950	598.612264	19.070208	-0.103167	1.446429
553.165513	590.848340	19.075213	-0.103145	1.438732
553.068122	583.066405	19.080218	-0.103122	1.430974
552.550834	575.356559	19.085223	-0.103020	1.423177
552.730759	567.520421	19.090227	-0.103049	1.415325
552.487993	559.760968	19.095232	-0.102999	1.407436
552.805874	551.926199	19.100237	-0.103053	1.399521
552.905623	544.122432	19.105242	-0.103066	1.391555
552.615991	536.384852	19.110247	-0.103007	1.383546
552.771131	528.594091	19.115251	-0.103031	1.375511
552.813297	520.804976	19.120256	-0.103034	1.367411
552.717822	513.089536	19.125261	-0.103011	1.359316
552.393275	505.387379	19.130266	-0.102946	1.351146
552.564302	497.593161	19.135271	-0.102972	1.342916
551.898105	489.972745	19.140275	-0.102843	1.334672
551.711790	482.222760	19.145280	-0.102804	1.326323
551.807174	474.468588	19.150285	-0.102816	1.317968
551.498970	466.707776	19.155290	-0.102754	1.309479
551.275652	458.960898	19.160295	-0.102707	1.300965
551.106029	451.262073	19.165299	-0.102671	1.292457
551.143249	443.494016	19.170304	-0.102673	1.283856
550.893866	435.828992	19.175309	-0.102621	1.275257
551.018297	428.069426	19.180314	-0.102639	1.266565
550.980847	420.362544	19.185319	-0.102627	1.257841
550.837339	412.687747	19.190323	-0.102596	1.249072
550.413608	405.059361	19.195328	-0.102512	1.240240
549.857276	397.471650	19.200333	-0.102403	1.231366
549.782988	389.750801	19.205338	-0.102385	1.222367
550.161365	381.967241	19.210343	-0.102450	1.213318
550.377190	374.248357	19.215347	-0.102485	1.204245
550.099426	366.637900	19.220352	-0.102428	1.195132
549.596690	359.067100	19.225357	-0.102330	1.185951
549.280934	351.457674	19.230362	-0.102266	1.176690
548.908423	343.851335	19.235367	-0.102192	1.167347
548.697870	336.244831	19.240371	-0.102148	1.157962
548.850628	328.520642	19.245376	-0.102171	1.148432
548.667025	320.909114	19.250381	-0.102132	1.138891
548.303077	313.341205	19.255386	-0.102059	1.129285
547.861467	305.791002	19.260391	-0.101972	1.119602
547.729179	298.189171	19.265395	-0.101943	1.109837
546.273708	290.814425	19.270400	-0.101667	1.099983
540.463597	284.145266	19.275405	-0.100581	1.089981
537.586715	276.873686	19.280410	-0.100040	1.079756
536.278782	269.337742	19.285415	-0.099792	1.069441
535.192420	261.775850	19.290419	-0.099585	1.059041
532.752281	254.454677	19.295424	-0.099125	1.048547
531.315650	246.966791	19.300429	-0.098853	1.037955
529.624239	239.531655	19.305434	-0.098533	1.027264
528.363762	232.029984	19.310439	-0.098294	1.016472
526.854846	224.595456	19.315443	-0.098008	1.005598
525.692934	217.106803	19.320448	-0.097787	0.994613
524.588588	209.608073	19.325453	-0.097576	0.983504
522.927598	202.239075	19.330458	-0.097262	0.972316
522.031127	194.750495	19.335463	-0.097090	0.961018
521.217030	187.289890	19.340467	-0.096934	0.949648
519.366345	180.031237	19.345472	-0.096585	0.938171
518.104267	172.672481	19.350477	-0.096345	0.926556
517.351050	165.258199	19.355482	-0.096200	0.914845
516.021625	157.964299	19.360487	-0.095948	0.903013
514.043929	150.810829	19.365491	-0.095575	0.891064
513.271896	143.428186	19.370496	-0.095426	0.878925
512.229288	136.149842	19.375501	-0.095227	0.866708
510.795943	128.965596	19.380506	-0.094956	0.854359
509.921777	121.691189	19.385511	-0.094788	0.841841
508.504848	114.562482	19.390515	-0.094520	0.829221
507.635805	107.336221	19.395520	-0.094353	0.816402
505.888176	100.319201	19.400525	-0.094023	0.803475
505.310705	93.112508	19.405530	-0.093911	0.790367
503.594733	86.152766	19.410535	-0.093587	0.777120
502.220775	79.157004	19.415539	-0.093327	0.763688
500.523085	72.438237	19.420544	-0.093006	0.750433