Fri Apr 16 18:29:52 2021

Number of Points = 3645
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
-0.402439	0.146195	0.000000	0.000145	0.310171

-0.502043	0.163245	0.005005	0.000164	0.310166
-0.252373	0.117219	0.010010	0.000117	0.310163
-0.052266	0.079508	0.015014	0.000080	0.310157
-0.160631	0.099543	0.020019	0.000100	0.310158
0.076210	0.056780	0.025024	0.000056	0.310160
-0.368579	0.137959	0.030029	0.000139	0.310161
-0.021885	0.073908	0.035034	0.000075	0.310156
-0.224185	0.110972	0.040038	0.000112	0.310158
-0.225056	0.109666	0.045043	0.000112	0.310151
-0.098913	0.088567	0.050048	0.000089	0.310160
-0.124552	0.092259	0.055053	0.000094	0.310155
0.002703	0.069649	0.060058	0.000070	0.310158
-0.265071	0.119362	0.065062	0.000120	0.310162
-0.248168	0.116956	0.070067	0.000117	0.310166
0.153559	0.042366	0.075072	0.000042	0.310158
-0.082815	0.084174	0.080077	0.000086	0.310153
0.094060	-0.009802	0.085082	0.000053	0.309864
-0.002731	0.002644	0.090086	0.000071	0.309840
-0.073800	0.014340	0.095091	0.000084	0.309835
0.123390	-0.020772	0.100096	0.000047	0.309838
-0.160584	0.029593	0.105101	0.000100	0.309832
-0.131608	0.028395	0.110106	0.000095	0.309851
-0.281716	0.054651	0.115110	0.000123	0.309847
0.060614	-0.063187	0.120115	0.000059	0.309587
0.031194	-0.073948	0.125120	0.000065	0.309511
0.115745	-0.092699	0.130125	0.000049	0.309496
-0.007250	-0.067548	0.135130	0.000072	0.309509
0.212330	-0.109304	0.140134	0.000031	0.309500
0.047864	-0.121972	0.145139	0.000062	0.309301
0.140823	-0.154945	0.150144	0.000044	0.309226
-0.074461	-0.117248	0.155149	0.000084	0.309219
0.014094	-0.132633	0.160154	0.000068	0.309223
0.128939	-0.185736	0.165158	0.000046	0.309072
-0.083609	-0.188226	0.170163	0.000086	0.308879
0.079558	-0.216718	0.175168	0.000056	0.308885
-0.272527	-0.152568	0.180173	0.000121	0.308886
0.007532	-0.241525	0.185178	0.000069	0.308707
-0.330847	-0.206709	0.190182	0.000132	0.308582
-0.483799	-0.177775	0.195187	0.000161	0.308588
-0.228676	-0.224936	0.200192	0.000113	0.308584
-0.448348	-0.252462	0.205197	0.000154	0.308267
-0.345685	-0.271864	0.210202	0.000135	0.308264
-0.284258	-0.283823	0.215206	0.000123	0.308260
-0.243084	-0.330853	0.220211	0.000116	0.308075
0.031548	-0.403409	0.225216	0.000065	0.307968
-0.117174	-0.378210	0.230221	0.000092	0.307960
-0.002653	-0.450793	0.235226	0.000071	0.307716
-0.059833	-0.460806	0.240230	0.000082	0.307620
0.000359	-0.473511	0.245235	0.000071	0.307612
0.181249	-0.571056	0.250240	0.000037	0.307308
-0.456790	-0.454827	0.255245	0.000156	0.307309
-0.115980	-0.544555	0.260250	0.000092	0.307178
0.134572	-0.633068	0.265254	0.000046	0.306976
-0.116834	-0.587173	0.270259	0.000092	0.306977
0.087290	-0.681882	0.275264	0.000054	0.306705
-0.066608	-0.656173	0.280269	0.000083	0.306694
0.177977	-0.750028	0.285274	0.000038	0.306461
-0.148029	-0.709905	0.290278	0.000098	0.306371
0.146485	-0.798452	0.295283	0.000043	0.306206
0.253388	-0.850435	0.300288	0.000024	0.306052
-0.069933	-0.819455	0.305293	0.000084	0.305920
-0.118397	-0.849465	0.310298	0.000093	0.305737
-0.087712	-0.871243	0.315302	0.000087	0.305660
0.051024	-0.936739	0.320307	0.000061	0.305469
-0.000671	-0.947406	0.325312	0.000071	0.305374
-0.259399	-0.952309	0.330317	0.000119	0.305128
-0.171558	-0.990505	0.335322	0.000103	0.305023
-0.131633	-1.039882	0.340326	0.000095	0.304823
-0.035205	-1.090966	0.345331	0.000077	0.304664
-0.074178	-1.119407	0.350336	0.000085	0.304495
-0.326704	-1.111088	0.355341	0.000132	0.304317
-0.330777	-1.133044	0.360346	0.000133	0.304209
-0.258435	-1.200146	0.365350	0.000119	0.303952
-0.348650	-1.201094	0.370355	0.000136	0.303869
-0.184858	-1.293683	0.375360	0.000105	0.303570
-0.318921	-1.289400	0.380365	0.000130	0.303474
-0.309708	-1.340565	0.385370	0.000129	0.303238
-0.191923	-1.397012	0.390374	0.000107	0.303071
-0.636467	-1.340577	0.395379	0.000190	0.302955
-0.611622	-1.404225	0.400384	0.000185	0.302672
-0.462615	-1.458830	0.405389	0.000157	0.302541
-0.412731	-1.518811	0.410394	0.000148	0.302297
-0.373360	-1.566938	0.415398	0.000141	0.302101
-0.497659	-1.573535	0.420403	0.000164	0.301961
-0.380470	-1.652416	0.425408	0.000142	0.301685
-0.486587	-1.668320	0.430413	0.000162	0.301517
-0.628032	-1.676849	0.435418	0.000188	0.301352
-0.399047	-1.778615	0.440422	0.000146	0.301063
-0.677853	-1.761927	0.445427	0.000197	0.300900
-0.431925	-1.842868	0.450432	0.000152	0.300726
-0.687203	-1.845639	0.455437	0.000199	0.300489
-0.530370	-1.911065	0.460442	0.000170	0.300311
-0.584737	-1.942559	0.465446	0.000180	0.300112
-0.964106	-1.934982	0.470451	0.000251	0.299816
-0.700805	-2.022604	0.475456	0.000202	0.299624
-1.021492	-2.001209	0.480461	0.000262	0.299446
-0.781784	-2.092145	0.485466	0.000217	0.299217
-1.033300	-2.101089	0.490470	0.000264	0.298952
-0.884962	-2.172260	0.495475	0.000236	0.298738
-1.032260	-2.183346	0.500480	0.000264	0.298555
-1.198687	-2.219449	0.505485	0.000295	0.298233
-0.936144	-2.305592	0.510490	0.000246	0.298047
-0.951081	-2.346935	0.515494	0.000249	0.297833
-1.440684	-2.304426	0.520499	0.000340	0.297607
-1.454140	-2.364536	0.525504	0.000342	0.297303
-2.661846	-2.187269	0.530509	0.000567	0.297097
-3.032349	-2.150880	0.535514	0.000636	0.296947
-2.816481	-2.243971	0.540518	0.000596	0.296684
-3.106435	-2.234578	0.545523	0.000650	0.296473
-3.515373	-2.190155	0.550528	0.000726	0.296327
-3.977185	-2.164884	0.555533	0.000812	0.296040
-3.562942	-2.275133	0.560538	0.000735	0.295869
-4.019662	-2.222520	0.565542	0.000820	0.295721
-4.457987	-2.193548	0.570547	0.000902	0.295472
-4.319297	-2.244004	0.575552	0.000876	0.295349
-4.832890	-2.196041	0.580557	0.000971	0.295126
-5.051369	-2.203512	0.585562	0.001012	0.294895
-5.435276	-2.153278	0.590566	0.001083	0.294799
-6.004547	-2.110923	0.595571	0.001189	0.294499
-5.812559	-2.164410	0.600576	0.001154	0.294408
-6.263663	-2.122066	0.605581	0.001238	0.294213
-6.411208	-2.133734	0.610586	0.001265	0.294023
-7.266762	-2.005297	0.615590	0.001424	0.293890
-6.996030	-2.099493	0.620595	0.001374	0.293669
-6.857778	-2.142819	0.625600	0.001348	0.293579
-7.228641	-2.132817	0.630605	0.001417	0.293296
-7.511795	-2.090369	0.635610	0.001470	0.293251
-7.668852	-2.118162	0.640614	0.001499	0.292973
-7.800549	-2.101101	0.645619	0.001524	0.292939
-8.068674	-2.115897	0.650624	0.001574	0.292625
-7.949790	-2.149512	0.655629	0.001552	0.292566
-8.069266	-2.181165	0.660634	0.001574	0.292302
-8.094696	-2.194139	0.665638	0.001579	0.292215
-8.800397	-2.115600	0.670643	0.001710	0.291968
-8.404859	-2.205208	0.675648	0.001636	0.291881
-8.890806	-2.157575	0.680653	0.001727	0.291679
-9.237496	-2.117157	0.685658	0.001791	0.291567
-9.531991	-2.105525	0.690662	0.001846	0.291359
-9.481457	-2.139503	0.695667	0.001837	0.291235
-9.855395	-2.108092	0.700672	0.001906	0.291054
-9.710317	-2.155331	0.705677	0.001879	0.290950
-9.804021	-2.183010	0.710682	0.001897	0.290727
-10.137081	-2.137231	0.715686	0.001959	0.290654
-10.356017	-2.133667	0.720691	0.002000	0.290474
-10.092453	-2.197090	0.725696	0.001951	0.290396
-10.602685	-2.159004	0.730701	0.002045	0.290124
-10.584666	-2.173533	0.735706	0.002042	0.290068
-10.879654	-2.170585	0.740710	0.002097	0.289815
-10.884234	-2.178822	0.745715	0.002098	0.289769
-11.344499	-2.151939	0.750720	0.002184	0.289486
-11.580387	-2.110490	0.755725	0.002227	0.289479
-11.465001	-2.184982	0.760730	0.002206	0.289211
-11.672817	-2.149563	0.765734	0.002245	0.289199
-12.266514	-2.099034	0.770739	0.002355	0.288912
-12.305188	-2.100608	0.775744	0.002362	0.288869
-12.508366	-2.098861	0.780749	0.002400	0.288692
-12.822264	-2.069138	0.785754	0.002459	0.288555
-12.531613	-2.139609	0.790758	0.002405	0.288467
-12.871732	-2.124298	0.795763	0.002468	0.288233
-12.723825	-2.152807	0.800768	0.002440	0.288225
-13.193908	-2.125884	0.805773	0.002528	0.287931
-12.951003	-2.168436	0.810778	0.002483	0.287939
-13.361060	-2.146762	0.815782	0.002559	0.287673
-13.791005	-2.083143	0.820787	0.002639	0.287600
-13.549800	-2.154377	0.825792	0.002594	0.287462
-13.964551	-2.112812	0.830797	0.002671	0.287292
-13.903964	-2.135690	0.835802	0.002660	0.287232
-14.441498	-2.090975	0.840806	0.002760	0.286965
-14.578735	-2.064668	0.845811	0.002786	0.286972
-14.501672	-2.122175	0.850816	0.002771	0.286753
-15.144577	-2.021062	0.855821	0.002891	0.286673
-14.649185	-2.131126	0.860826	0.002799	0.286572
-14.968514	-2.117859	0.865830	0.002858	0.286346
-15.251814	-2.067154	0.870835	0.002911	0.286342
-15.128078	-2.143553	0.875840	0.002888	0.286069
-15.473682	-2.087867	0.880845	0.002952	0.286033
-15.637282	-2.085989	0.885850	0.002983	0.285892
-16.100401	-2.035079	0.890854	0.003069	0.285723
-15.929094	-2.067095	0.895859	0.003037	0.285719
-16.092512	-2.083211	0.900864	0.003068	0.285487
-16.468501	-2.018010	0.905869	0.003137	0.285471
-16.035290	-2.126112	0.910874	0.003057	0.285322
-16.746259	-2.032371	0.915878	0.003189	0.285142
-16.911960	-2.004410	0.920883	0.003220	0.285131
-17.056523	-2.029819	0.925888	0.003247	0.284868
-16.925818	-2.065079	0.930893	0.003223	0.284810
-17.480519	-1.978876	0.935898	0.003326	0.284736
-17.702479	-1.983590	0.940902	0.003367	0.284506
-18.100940	-1.910497	0.945907	0.003441	0.284510
-18.059090	-1.940949	0.950912	0.003434	0.284393
-18.608152	-1.875536	0.955917	0.003536	0.284218
-18.364517	-1.918917	0.960922	0.003490	0.284223
-17.993135	-2.023110	0.965926	0.003421	0.284036
-18.977714	-1.874655	0.970931	0.003605	0.283880
-18.608017	-1.941060	0.975936	0.003536	0.283885
-18.752910	-1.956380	0.980941	0.003563	0.283672
-18.851544	-1.958244	0.985946	0.003581	0.283571
-18.640447	-1.997914	0.990950	0.003542	0.283565
-18.994159	-1.996548	0.995955	0.003608	0.283243
-18.749194	-2.040148	1.000960	0.003562	0.283248
-19.175300	-1.982282	1.005965	0.003641	0.283148
-19.137012	-2.029803	1.010970	0.003634	0.282940
-18.694999	-2.110085	1.015974	0.003552	0.282941
-19.726043	-1.971928	1.020979	0.003744	0.282688
-20.008873	-1.933897	1.025984	0.003797	0.282620
-19.626415	-2.006747	1.030989	0.003725	0.282603
-20.098801	-1.978568	1.035994	0.003813	0.282307
-20.069811	-1.985872	1.040998	0.003808	0.282297
-20.373389	-1.946317	1.046003	0.003864	0.282217
-20.306576	-2.003626	1.051008	0.003852	0.281985
-20.496383	-1.971194	1.056013	0.003887	0.281974
-20.646041	-1.974086	1.061018	0.003915	0.281820
-20.805483	-1.969836	1.066022	0.003945	0.281693
-20.538984	-2.022337	1.071027	0.003895	0.281672
-20.987851	-1.992411	1.076032	0.003979	0.281406
-21.241018	-1.956244	1.081037	0.004026	0.281355
-20.913799	-2.027202	1.086042	0.003965	0.281296
-21.534502	-1.961051	1.091046	0.004081	0.281056
-21.344546	-1.999175	1.096051	0.004045	0.281038
-21.627073	-1.971059	1.101056	0.004098	0.280918
-22.096862	-1.921614	1.106061	0.004185	0.280732
-21.676690	-1.998518	1.111066	0.004107	0.280730
-21.733147	-2.020286	1.116070	0.004118	0.280565
-22.112589	-1.965821	1.121075	0.004188	0.280490
-21.930434	-2.001926	1.126080	0.004154	0.280474
-22.165993	-2.022567	1.131085	0.004198	0.280146
-22.577031	-1.945355	1.136090	0.004275	0.280159
-22.262620	-2.028187	1.141094	0.004216	0.280027
-22.645926	-1.998198	1.146099	0.004287	0.279821
-22.339153	-2.052607	1.151104	0.004230	0.279828
-23.208147	-1.944583	1.156109	0.004392	0.279570
-23.484170	-1.903659	1.161114	0.004443	0.279522
-22.951073	-2.004023	1.166118	0.004344	0.279504
-23.244334	-2.005953	1.171123	0.004399	0.279218
-23.412603	-1.974314	1.176128	0.004430	0.279223
-23.252535	-2.030372	1.181133	0.004400	0.279083
-23.086687	-2.102472	1.186138	0.004370	0.278866
-23.435575	-2.036773	1.191142	0.004434	0.278877
-23.738777	-2.037326	1.196147	0.004491	0.278588
-23.631723	-2.060961	1.201152	0.004471	0.278567
-23.731882	-2.065073	1.206157	0.004490	0.278451
-24.218245	-2.016331	1.211162	0.004580	0.278244
-24.315199	-1.996980	1.216166	0.004598	0.278253
-24.350912	-2.034004	1.221171	0.004605	0.278027
-24.656099	-1.991466	1.226176	0.004662	0.277959
-24.856684	-1.957805	1.231181	0.004699	0.277945
-24.917690	-2.008365	1.236186	0.004710	0.277623
-25.349663	-1.928584	1.241190	0.004791	0.277630
-25.485997	-1.924774	1.246195	0.004816	0.277520
-25.226352	-2.011855	1.251200	0.004768	0.277312
-25.864815	-1.896053	1.256205	0.004887	0.277311
-25.877404	-1.924950	1.261210	0.004889	0.277148
-26.075915	-1.918678	1.266214	0.004926	0.276992
-25.649582	-1.998696	1.271219	0.004847	0.276979
-26.239802	-1.927439	1.276224	0.004956	0.276791
-26.706486	-1.859445	1.281229	0.005043	0.276702
-26.348077	-1.924841	1.286234	0.004977	0.276701
-26.731762	-1.906368	1.291238	0.005048	0.276433
-26.879135	-1.893948	1.296243	0.005076	0.276357
-26.469558	-1.967677	1.301248	0.004999	0.276361
-26.643847	-1.995560	1.306253	0.005032	0.276049
-26.900303	-1.947979	1.311258	0.005079	0.276054
-26.854775	-1.974078	1.316262	0.005071	0.275961
-27.137733	-1.966766	1.321267	0.005124	0.275729
-27.071103	-1.977684	1.326272	0.005111	0.275735
-27.327040	-1.960280	1.331277	0.005159	0.275582
-27.468400	-1.951920	1.336282	0.005185	0.275491
-27.191087	-2.002863	1.341286	0.005134	0.275488
-28.199680	-1.883318	1.346291	0.005321	0.275153
-27.664983	-1.980474	1.351296	0.005222	0.275153
-27.764060	-1.979405	1.356301	0.005240	0.275064
-28.251623	-1.933995	1.361306	0.005331	0.274836
-28.407295	-1.902804	1.366310	0.005360	0.274851
-28.542658	-1.910682	1.371315	0.005385	0.274680
-28.614629	-1.927397	1.376320	0.005399	0.274523
-28.957571	-1.866915	1.381325	0.005462	0.274513
-28.575304	-1.974877	1.386330	0.005391	0.274310
-28.842532	-1.942902	1.391334	0.005441	0.274223
-29.073976	-1.902224	1.396339	0.005484	0.274215
-28.928080	-1.990803	1.401344	0.005457	0.273887
-29.220491	-1.937973	1.406349	0.005511	0.273886
-29.474173	-1.908243	1.411354	0.005559	0.273799
-29.818259	-1.885858	1.416358	0.005623	0.273586
-29.302644	-1.983876	1.421363	0.005527	0.273564
-29.396373	-2.000613	1.426368	0.005544	0.273385
-29.958353	-1.923414	1.431373	0.005649	0.273252
-29.612265	-1.986635	1.436378	0.005584	0.273251
-29.566978	-2.048429	1.441382	0.005576	0.272967
-30.286599	-1.920907	1.446387	0.005710	0.272949
-29.902843	-2.012773	1.451392	0.005638	0.272832
-30.394779	-1.964181	1.456397	0.005730	0.272615
-30.660185	-1.913790	1.461402	0.005779	0.272627
-30.776854	-1.933180	1.466406	0.005801	0.272411
-30.842995	-1.940855	1.471411	0.005813	0.272306
-30.638734	-1.979009	1.476416	0.005775	0.272301
-31.415729	-1.894624	1.481421	0.005920	0.271998
-31.354768	-1.906408	1.486426	0.005909	0.271994
-31.061752	-1.976942	1.491430	0.005854	0.271902
-31.561032	-1.925964	1.496435	0.005947	0.271690
-31.624169	-1.910531	1.501440	0.005959	0.271711
-31.937349	-1.889709	1.506445	0.006017	0.271519
-32.126891	-1.882160	1.511450	0.006052	0.271375
-31.693417	-1.962705	1.516454	0.005972	0.271366
-31.812344	-1.991908	1.521459	0.005994	0.271095
-32.056307	-1.952759	1.526464	0.006039	0.271067
-32.540829	-1.877922	1.531469	0.006129	0.270996
-32.536720	-1.924553	1.536474	0.006129	0.270751
-32.488429	-1.933537	1.541478	0.006120	0.270750
-32.601373	-1.941407	1.546483	0.006141	0.270598
-32.970128	-1.891695	1.551488	0.006209	0.270505
-32.389254	-2.002839	1.556493	0.006101	0.270475
-33.238407	-1.904768	1.561498	0.006259	0.270174
-33.226584	-1.911950	1.566502	0.006257	0.270147
-33.132379	-1.943539	1.571507	0.006240	0.270069
-32.950315	-2.022815	1.576512	0.006206	0.269822
-33.265452	-1.966885	1.581517	0.006264	0.269814
-33.510326	-1.964819	1.586522	0.006310	0.269586
-33.541626	-1.975381	1.591526	0.006316	0.269499
-33.575489	-1.977851	1.596531	0.006322	0.269452
-33.752703	-1.991632	1.601536	0.006355	0.269205
-33.670417	-2.006821	1.606541	0.006340	0.269204
-33.851993	-2.012890	1.611546	0.006374	0.268994
-34.191206	-1.973797	1.616550	0.006437	0.268872
-34.057138	-2.006040	1.621555	0.006412	0.268830
-33.929729	-2.080111	1.626560	0.006388	0.268555
-34.313812	-2.011389	1.631565	0.006460	0.268549
-34.517227	-2.014902	1.636570	0.006497	0.268331
-34.598751	-2.017597	1.641574	0.006513	0.268236
-34.960507	-1.961764	1.646579	0.006580	0.268182
-35.189727	-1.961755	1.651584	0.006623	0.267957
-35.060990	-1.986564	1.656589	0.006599	0.267950
-35.227324	-1.995164	1.661594	0.006630	0.267740
-35.635670	-1.944048	1.666598	0.006706	0.267614
-35.444694	-1.981533	1.671603	0.006670	0.267600
-35.394017	-2.047083	1.676608	0.006661	0.267295
-35.691001	-1.994102	1.681613	0.006716	0.267289
-35.716800	-2.023334	1.686618	0.006721	0.267105
-35.548410	-2.080496	1.691622	0.006689	0.266961
-35.741534	-2.054686	1.696627	0.006725	0.266911
-36.164983	-2.020545	1.701632	0.006804	0.266678
-36.080198	-2.036848	1.706637	0.006788	0.266673
-36.229266	-2.052954	1.711642	0.006816	0.266439
-36.583131	-2.006296	1.716646	0.006882	0.266342
-36.741530	-1.987662	1.721651	0.006912	0.266287
-36.846173	-2.012853	1.726656	0.006931	0.266046
-37.081642	-1.971363	1.731661	0.006975	0.266039
-37.230149	-1.981500	1.736666	0.007003	0.265837
-37.263427	-1.995617	1.741670	0.007009	0.265727
-37.491625	-1.958316	1.746675	0.007051	0.265704
-37.608259	-1.980327	1.751680	0.007073	0.265468
-37.821738	-1.941546	1.756685	0.007113	0.265468
-37.746975	-1.983686	1.761690	0.007099	0.265312
-38.135990	-1.946710	1.766694	0.007171	0.265128
-38.280484	-1.922552	1.771699	0.007198	0.265116
-38.011249	-2.017529	1.776704	0.007148	0.264865
-38.701195	-1.900835	1.781709	0.007276	0.264817
-38.914542	-1.871707	1.786714	0.007316	0.264764
-39.061753	-1.892623	1.791718	0.007343	0.264503
-39.085667	-1.891489	1.796723	0.007348	0.264485
-38.615851	-2.001697	1.801728	0.007261	0.264350
-39.290678	-1.906199	1.806733	0.007386	0.264201
-38.996754	-1.960993	1.811738	0.007331	0.264193
-39.279770	-1.959745	1.816742	0.007384	0.263918
-39.932218	-1.850964	1.821747	0.007505	0.263864
-39.523115	-1.933459	1.826752	0.007429	0.263819
-40.272531	-1.842869	1.831757	0.007569	0.263568
-40.045332	-1.887154	1.836762	0.007527	0.263552
-39.714685	-1.970043	1.841766	0.007465	0.263427
-40.411727	-1.878836	1.846771	0.007595	0.263231
-40.415643	-1.876330	1.851776	0.007596	0.263241
-40.206995	-1.953596	1.856781	0.007557	0.263025
-40.259248	-1.960181	1.861786	0.007566	0.262936
-40.184355	-1.985297	1.866790	0.007552	0.262873
-40.784758	-1.927498	1.871795	0.007664	0.262589
-40.401063	-1.996303	1.876800	0.007593	0.262595
-40.746208	-1.970854	1.881805	0.007657	0.262389
-41.211013	-1.906327	1.886810	0.007744	0.262278
-41.198656	-1.908604	1.891814	0.007741	0.262278
-41.327651	-1.943271	1.896819	0.007765	0.261957
-41.361153	-1.936606	1.901824	0.007772	0.261960
-41.632301	-1.908918	1.906829	0.007822	0.261841
-41.580740	-1.950123	1.911834	0.007812	0.261665
-41.499014	-1.962551	1.916838	0.007797	0.261678
-42.199459	-1.887026	1.921843	0.007928	0.261391
-42.425733	-1.850987	1.926848	0.007970	0.261362
-42.605977	-1.822452	1.931853	0.008003	0.261339
-42.506696	-1.895267	1.936858	0.007985	0.261035
-42.790619	-1.840618	1.941862	0.008038	0.261052
-42.434153	-1.929397	1.946867	0.007971	0.260919
-42.682176	-1.920046	1.951872	0.008017	0.260721
-42.892233	-1.882438	1.956877	0.008057	0.260717
-42.906500	-1.910873	1.961882	0.008059	0.260545
-42.779915	-1.946162	1.966886	0.008036	0.260477
-43.399465	-1.842685	1.971891	0.008151	0.260425
-43.701031	-1.837381	1.976896	0.008207	0.260150
-43.416367	-1.890774	1.981901	0.008154	0.260141
-43.698067	-1.868481	1.986906	0.008207	0.259979
-43.870922	-1.864473	1.991910	0.008239	0.259827
-43.593740	-1.917343	1.996915	0.008187	0.259813
-44.347336	-1.830726	2.001920	0.008327	0.259531

-44.264490	-1.872084	2.011917	0.008312	0.259385
-44.477559	-1.864722	2.021914	0.008352	0.259209
-44.632959	-1.881197	2.031910	0.008381	0.258959
-44.878234	-1.851322	2.041907	0.008426	0.258877
-45.003398	-1.869022	2.051904	0.008450	0.258650
-44.822703	-1.918857	2.061901	0.008416	0.258555
-44.971971	-1.899919	2.071898	0.008444	0.258509
-45.157290	-1.915952	2.081894	0.008478	0.258231
-45.846448	-1.786957	2.091891	0.008606	0.258251
-45.766317	-1.800296	2.101888	0.008592	0.258258
-45.812995	-1.791694	2.111885	0.008600	0.258259
-45.663074	-1.821733	2.121882	0.008572	0.258243
-45.587210	-1.854281	2.131878	0.008558	0.258138
-45.643599	-1.878054	2.141875	0.008569	0.257947
-45.984402	-1.813057	2.151872	0.008632	0.257964
-45.897417	-1.800485	2.161869	0.008616	0.258123
-45.879117	-1.781082	2.171866	0.008612	0.258251
-45.686684	-1.815967	2.181862	0.008577	0.258252
-45.930307	-1.770929	2.191859	0.008622	0.258256
-45.346028	-1.878914	2.201856	0.008513	0.258246
-45.640550	-1.824006	2.211853	0.008568	0.258254
-45.426835	-1.864833	2.221850	0.008528	0.258243
-45.297343	-1.877778	2.231846	0.008504	0.258302
-45.308444	-1.828053	2.241843	0.008506	0.258570
-45.220254	-1.844619	2.251840	0.008490	0.258567
-45.023007	-1.881544	2.261837	0.008453	0.258561
-44.837151	-1.901520	2.271834	0.008418	0.258639
-44.329535	-1.955056	2.281830	0.008324	0.258856
-45.171919	-1.798240	2.291827	0.008481	0.258876
-44.540361	-1.906915	2.301824	0.008363	0.258911
-44.492403	-1.862231	2.311821	0.008354	0.259210
-44.680864	-1.827472	2.321818	0.008389	0.259212
-44.566484	-1.817344	2.331814	0.008368	0.259385
-44.100371	-1.882850	2.341811	0.008281	0.259493
-43.992644	-1.892476	2.351808	0.008261	0.259549
-43.628430	-1.910707	2.361805	0.008193	0.259816
-43.633994	-1.910268	2.371802	0.008194	0.259813
-43.593044	-1.867174	2.381798	0.008187	0.260095
-43.414866	-1.893306	2.391795	0.008153	0.260130
-43.027888	-1.916616	2.401792	0.008081	0.260392
-43.028521	-1.900921	2.411789	0.008082	0.260479
-42.757545	-1.921105	2.421786	0.008031	0.260641
-42.866145	-1.888617	2.431782	0.008051	0.260711
-42.590354	-1.893272	2.441779	0.008000	0.260964
-42.616933	-1.874211	2.451776	0.008005	0.261043
-42.647590	-1.813147	2.461773	0.008011	0.261351
-42.470762	-1.823608	2.471770	0.007978	0.261471
-42.023527	-1.867293	2.481766	0.007894	0.261680
-41.886706	-1.856912	2.491763	0.007869	0.261875
-41.797584	-1.849465	2.501760	0.007852	0.262006
-41.645187	-1.823477	2.511757	0.007824	0.262303
-41.552364	-1.809460	2.521754	0.007807	0.262473
-41.294700	-1.830560	2.531750	0.007759	0.262616
-41.031477	-1.816646	2.541747	0.007710	0.262956
-40.707038	-1.848922	2.551744	0.007649	0.263103
-40.383016	-1.883770	2.561741	0.007589	0.263236
-39.959183	-1.905979	2.571738	0.007510	0.263538
-40.280795	-1.819350	2.581734	0.007570	0.263693
-39.807781	-1.873229	2.591731	0.007482	0.263869
-39.712953	-1.832435	2.601728	0.007464	0.264188
-39.240737	-1.893611	2.611725	0.007376	0.264323
-39.273005	-1.855481	2.621722	0.007382	0.264500
-39.219752	-1.807795	2.631718	0.007372	0.264814
-38.784686	-1.853155	2.641715	0.007291	0.264999
-38.437901	-1.883506	2.651712	0.007227	0.265177
-38.439339	-1.827150	2.661709	0.007227	0.265484
-37.935938	-1.886859	2.671706	0.007133	0.265657
-38.279609	-1.789524	2.681702	0.007197	0.265847
-37.545681	-1.885378	2.691699	0.007060	0.266052
-37.159318	-1.904426	2.701696	0.006988	0.266331
-37.085052	-1.884314	2.711693	0.006975	0.266514
-36.678223	-1.925359	2.721690	0.006899	0.266693
-36.697621	-1.869606	2.731686	0.006902	0.266976
-36.390259	-1.889639	2.741683	0.006845	0.267171
-36.133033	-1.901111	2.751680	0.006797	0.267362
-36.004044	-1.877286	2.761677	0.006773	0.267618
-35.503404	-1.918292	2.771674	0.006680	0.267889
-35.767661	-1.835901	2.781670	0.006729	0.268075
-35.167287	-1.911823	2.791667	0.006617	0.268254
-35.246259	-1.837970	2.801664	0.006632	0.268575
-34.371879	-1.960789	2.811661	0.006469	0.268770
-34.311609	-1.939169	2.821658	0.006458	0.268946
-34.171601	-1.915816	2.831654	0.006432	0.269209
-33.607674	-1.977137	2.841651	0.006327	0.269431
-33.973849	-1.874109	2.851648	0.006395	0.269626
-34.211990	-1.780587	2.861645	0.006439	0.269896
-33.757482	-1.813163	2.871642	0.006355	0.270165
-33.469136	-1.810107	2.881638	0.006301	0.270462
-32.962606	-1.867367	2.891635	0.006207	0.270648
-33.087823	-1.807040	2.901632	0.006230	0.270849
-32.635161	-1.846383	2.911629	0.006146	0.271079
-32.417357	-1.830805	2.921626	0.006105	0.271374
-32.071434	-1.847913	2.931622	0.006041	0.271618
-31.927062	-1.834823	2.941619	0.006014	0.271828
-31.470198	-1.879199	2.951616	0.005929	0.272034
-31.297284	-1.856885	2.961613	0.005897	0.272320
-31.158407	-1.833553	2.971610	0.005871	0.272578
-30.838347	-1.849292	2.981606	0.005811	0.272804
-30.621807	-1.844714	2.991603	0.005771	0.273037
-30.935381	-1.738877	3.001600	0.005829	0.273296
-29.707611	-1.908677	3.011597	0.005601	0.273579
-29.515005	-1.905978	3.021594	0.005565	0.273779
-29.043509	-1.959892	3.031590	0.005477	0.273947
-28.948827	-1.926834	3.041587	0.005459	0.274213
-28.669103	-1.930001	3.051584	0.005407	0.274465
-28.700933	-1.886141	3.061581	0.005413	0.274665
-28.554673	-1.868095	3.071578	0.005386	0.274901
-28.558925	-1.816157	3.081574	0.005387	0.275170
-28.162427	-1.829620	3.091571	0.005313	0.275478
-27.950590	-1.834114	3.101568	0.005273	0.275657
-27.260489	-1.924253	3.111565	0.005145	0.275843
-26.860172	-1.957799	3.121562	0.005070	0.276049
-26.818243	-1.910754	3.131558	0.005063	0.276336
-26.663322	-1.897637	3.141555	0.005034	0.276552
-26.201315	-1.946141	3.151552	0.004948	0.276738
-26.128378	-1.911454	3.161549	0.004934	0.276988
-25.890639	-1.903327	3.171546	0.004890	0.277257
-25.723214	-1.892491	3.181542	0.004859	0.277472
-25.261742	-1.938918	3.191539	0.004773	0.277668
-25.121642	-1.907875	3.201536	0.004747	0.277962
-24.663462	-1.947979	3.211533	0.004661	0.278188
-24.915255	-1.861128	3.221530	0.004708	0.278401
-24.278584	-1.939225	3.231526	0.004590	0.278597
-24.125074	-1.913874	3.241523	0.004561	0.278874
-24.027660	-1.880815	3.251520	0.004543	0.279137
-23.921424	-1.855949	3.261517	0.004523	0.279366
-23.932213	-1.810982	3.271514	0.004525	0.279589
-23.253869	-1.885649	3.281510	0.004399	0.279841
-23.445490	-1.792100	3.291507	0.004434	0.280145
-22.625268	-1.894649	3.301504	0.004282	0.280385
-22.618341	-1.856328	3.311501	0.004280	0.280590
-22.379428	-1.866882	3.321498	0.004236	0.280759
-21.958478	-1.886790	3.331494	0.004157	0.281051
-21.790050	-1.873218	3.341491	0.004126	0.281279
-21.241827	-1.931542	3.351488	0.004024	0.281492
-20.977990	-1.939403	3.361485	0.003975	0.281698
-20.665250	-1.944291	3.371482	0.003917	0.281965
-20.444350	-1.941512	3.381478	0.003876	0.282185
-20.498836	-1.890484	3.391475	0.003886	0.282396
-20.109432	-1.919309	3.401472	0.003813	0.282611
-19.873355	-1.897082	3.411469	0.003769	0.282945
-19.411145	-1.946445	3.421466	0.003683	0.283122
-19.158463	-1.956195	3.431462	0.003636	0.283307
-19.009462	-1.935340	3.441459	0.003608	0.283552
-18.380121	-1.998946	3.451456	0.003491	0.283812
-18.618930	-1.916751	3.461453	0.003536	0.284009
-18.212614	-1.949143	3.471450	0.003460	0.284221
-18.094689	-1.917590	3.481446	0.003438	0.284490
-17.464448	-1.990107	3.491443	0.003321	0.284704
-17.085690	-2.024853	3.501440	0.003250	0.284878
-17.325371	-1.931382	3.511437	0.003295	0.285131
-16.799456	-1.970840	3.521434	0.003197	0.285416
-16.784597	-1.939795	3.531430	0.003194	0.285587
-16.318283	-1.996163	3.541427	0.003107	0.285731
-16.048662	-1.985280	3.551424	0.003057	0.286035
-15.738625	-2.004154	3.561421	0.002999	0.286224
-15.572652	-1.999125	3.571418	0.002968	0.286402
-15.401640	-1.976785	3.581414	0.002936	0.286672
-15.331604	-1.941618	3.591411	0.002923	0.286914
-15.206033	-1.921011	3.601408	0.002900	0.287133
-14.686962	-1.976171	3.611405	0.002803	0.287331
-14.323718	-1.987291	3.621402	0.002736	0.287607
-14.185508	-1.963439	3.631398	0.002710	0.287854
-13.703664	-2.017259	3.641395	0.002620	0.288024
-13.395937	-2.031806	3.651392	0.002563	0.288232
-13.203485	-2.012999	3.661389	0.002527	0.288502
-13.166063	-1.983217	3.671386	0.002520	0.288685
-13.384623	-1.897497	3.681382	0.002561	0.288916
-12.604247	-1.981418	3.691379	0.002415	0.289206
-12.271225	-2.001849	3.701376	0.002353	0.289406
-12.468956	-1.924840	3.711373	0.002390	0.289612
-11.983638	-1.970856	3.721370	0.002300	0.289823
-11.644208	-1.971018	3.731366	0.002237	0.290130
-11.222630	-2.006644	3.741363	0.002158	0.290334
-11.052772	-2.000407	3.751360	0.002127	0.290519
-11.014293	-1.963412	3.761357	0.002119	0.290738
-10.723061	-1.965408	3.771354	0.002065	0.290992
-10.595136	-1.950383	3.781350	0.002041	0.291182
-10.309649	-1.962518	3.791347	0.001988	0.291380
-9.964670	-1.962806	3.801344	0.001924	0.291690
-9.498736	-2.008156	3.811341	0.001837	0.291885
-9.247468	-2.016936	3.821338	0.001790	0.292068
-9.078254	-2.001700	3.831334	0.001759	0.292296
-8.808055	-1.995874	3.841331	0.001709	0.292568
-8.534590	-2.005952	3.851328	0.001658	0.292764
-7.953705	-2.073397	3.861325	0.001549	0.292952
-7.944381	-2.018107	3.871322	0.001548	0.293234
-7.839013	-2.000248	3.881318	0.001528	0.293416
-7.678763	-1.990997	3.891315	0.001498	0.293605
-7.405157	-1.985811	3.901312	0.001447	0.293876
-6.929140	-2.021804	3.911309	0.001359	0.294125
-6.869534	-1.996260	3.921306	0.001347	0.294304
-6.415113	-2.040533	3.931302	0.001263	0.294492
-6.116564	-2.036324	3.941299	0.001207	0.294779
-6.048526	-2.012156	3.951296	0.001195	0.294959
-5.864978	-2.004959	3.961293	0.001160	0.295158
-5.771933	-1.954819	3.971290	0.001143	0.295486
-5.355338	-1.998322	3.981286	0.001065	0.295644
-5.475942	-1.937889	3.991283	0.001088	0.295833
-5.157681	-1.950119	4.001280	0.001029	0.296056
-4.966670	-1.921521	4.011277	0.000993	0.296365
-4.949053	-1.877719	4.021274	0.000990	0.296594
-4.702055	-1.876701	4.031270	0.000944	0.296818
-4.736857	-1.822101	4.041267	0.000950	0.297054
-4.246257	-1.858417	4.051264	0.000859	0.297311
-3.755345	-1.886450	4.061261	0.000767	0.297609
-3.366577	-1.911702	4.071258	0.000695	0.297829
-3.308499	-1.877579	4.081254	0.000684	0.298046
-3.207031	-1.852477	4.091251	0.000665	0.298258
-3.051552	-1.818188	4.101248	0.000636	0.298561
-3.271490	-1.723680	4.111245	0.000677	0.298825
-3.051354	-1.706603	4.121242	0.000636	0.299102
-2.755261	-1.705493	4.131238	0.000581	0.299367
-2.564537	-1.687587	4.141235	0.000545	0.299621
-2.073781	-1.721676	4.151232	0.000454	0.299887
-2.376415	-1.606819	4.161229	0.000510	0.300176
-2.056084	-1.601508	4.171226	0.000451	0.300482
-2.195722	-1.527172	4.181222	0.000477	0.300718
-2.008272	-1.499510	4.191219	0.000442	0.301015
-1.647793	-1.503614	4.201216	0.000375	0.301310
-1.658397	-1.434910	4.211213	0.000377	0.301630
-1.212351	-1.457262	4.221210	0.000293	0.301912
-1.356271	-1.365311	4.231206	0.000320	0.302227
-1.365037	-1.297775	4.241203	0.000322	0.302543
-1.417328	-1.214564	4.251200	0.000331	0.302895
-1.372457	-1.151544	4.261197	0.000323	0.303235
-1.090719	-1.126875	4.271194	0.000271	0.303597
-1.248967	-1.022133	4.281190	0.000300	0.303958
-1.092894	-0.975437	4.291187	0.000271	0.304316
-0.959982	-0.924707	4.301184	0.000246	0.304671
-0.818148	-0.872030	4.311181	0.000220	0.305044
-1.030097	-0.743546	4.321178	0.000259	0.305470
-1.115324	-0.648310	4.331174	0.000275	0.305848
-0.857158	-0.615421	4.341171	0.000227	0.306225
-0.632809	-0.568227	4.351168	0.000185	0.306640
-0.575029	-0.486641	4.361165	0.000174	0.307075
-0.301242	-0.451867	4.371162	0.000123	0.307473
-0.672913	-0.290609	4.381158	0.000192	0.307913
-0.705996	-0.185640	4.391155	0.000198	0.308378
-0.460913	-0.142371	4.401152	0.000153	0.308790
-0.302460	-0.060143	4.411149	0.000123	0.309310
0.063812	-0.040634	4.421146	0.000055	0.309712
0.150729	0.051540	4.431142	0.000039	0.310216
-0.167196	0.200472	4.441139	0.000098	0.310641
0.000000	0.269211	4.451136	0.000066	0.311102

-0.132364	0.568508	4.456141	0.000091	0.312380
-0.052519	1.117842	4.461146	0.000076	0.314980
0.409305	1.878316	4.466150	-0.000011	0.318835
1.167814	2.878017	4.471155	-0.000153	0.323956
1.616571	4.237471	4.476160	-0.000237	0.330328
2.290028	5.842929	4.481165	-0.000364	0.337811
3.781302	7.610513	4.486170	-0.000642	0.346430
5.105773	9.727177	4.491174	-0.000890	0.356136
6.209178	12.191548	4.496179	-0.001098	0.366800
7.511990	14.953829	4.501184	-0.001342	0.378441
8.951520	18.026277	4.506189	-0.001612	0.390975
11.064142	21.323819	4.511194	-0.002007	0.404361
13.534949	24.918619	4.516198	-0.002470	0.418570
16.540052	28.778666	4.521203	-0.003032	0.433520
19.865808	32.953780	4.526208	-0.003654	0.449172
22.032111	37.714649	4.531213	-0.004060	0.465465
24.804235	42.736057	4.536218	-0.004580	0.482314
27.724403	48.098881	4.541222	-0.005127	0.499659
30.593098	53.847255	4.546227	-0.005665	0.517472
33.410603	59.952460	4.551232	-0.006194	0.535628
35.800148	66.474458	4.556237	-0.006643	0.554074
38.171764	73.337518	4.561242	-0.007089	0.572776
40.187391	80.580549	4.566246	-0.007469	0.591657
42.167413	88.111953	4.571251	-0.007842	0.610620
44.474043	95.875580	4.576256	-0.008277	0.629677
46.110255	104.012179	4.581261	-0.008587	0.648736
48.032530	112.344588	4.586266	-0.008950	0.667784
49.772773	120.904887	4.591270	-0.009280	0.686713
51.642423	129.640866	4.596275	-0.009634	0.705540
53.522957	138.557368	4.601280	-0.009990	0.724240
55.571697	147.597052	4.606285	-0.010377	0.742765
57.893430	156.726788	4.611290	-0.010815	0.761101
59.788714	166.050740	4.616294	-0.011174	0.779222
61.583305	175.496365	4.621299	-0.011515	0.797119
63.552389	184.985314	4.626304	-0.011888	0.814752
65.534793	194.559143	4.631309	-0.012263	0.832162
67.563148	204.142434	4.636314	-0.012647	0.849243
69.809089	213.725140	4.641318	-0.013071	0.866049
71.713849	223.390184	4.646323	-0.013432	0.882569
73.646544	233.069848	4.651328	-0.013798	0.898815
75.171602	242.812330	4.656333	-0.014089	0.914758
77.256460	252.431276	4.661338	-0.014483	0.930387
78.669175	262.160227	4.666342	-0.014753	0.945745
79.669853	271.925462	4.671347	-0.014945	0.960802
81.400390	281.518607	4.676352	-0.015274	0.975560
82.919655	291.121812	4.681357	-0.015563	0.990058
84.340495	300.673834	4.686362	-0.015834	1.004247
85.763315	310.172925	4.691366	-0.016105	1.018163
87.278988	319.610351	4.696371	-0.016393	1.031827
88.460807	329.059486	4.701376	-0.016619	1.045247
89.928684	338.397047	4.706381	-0.016899	1.058412
91.262239	347.724140	4.711386	-0.017153	1.071369
92.516215	356.989799	4.716390	-0.017393	1.084070
93.755183	366.211471	4.721395	-0.017630	1.096562
95.408032	375.309904	4.726400	-0.017943	1.108845
96.631251	384.427727	4.731405	-0.018177	1.120922
97.619143	393.568434	4.736410	-0.018367	1.132847
99.199903	402.527590	4.741414	-0.018667	1.144547
100.583033	411.513689	4.746419	-0.018930	1.156118
101.777226	420.459017	4.751424	-0.019159	1.167484
102.767481	429.388618	4.756429	-0.019349	1.178678
103.998630	438.263542	4.761434	-0.019584	1.189750
105.161794	447.082934	4.766438	-0.019806	1.200638
106.262588	455.888418	4.771443	-0.020017	1.211398
107.359757	464.670411	4.776448	-0.020227	1.222035
108.629323	473.381680	4.781453	-0.020469	1.232530
110.005807	482.039979	4.786458	-0.020731	1.242896
111.364579	490.685446	4.791462	-0.020990	1.253158
112.909077	499.271306	4.796467	-0.021283	1.263303
114.471945	507.852225	4.801472	-0.021579	1.273364
115.734547	516.446000	4.806477	-0.021820	1.283303
117.334625	524.977486	4.811482	-0.022124	1.293160
118.828912	533.517337	4.816486	-0.022407	1.302930
120.206791	542.115667	4.821491	-0.022670	1.312670
122.040680	550.569363	4.826496	-0.023017	1.322263
123.576962	559.024911	4.831501	-0.023308	1.331734
126.141521	567.314504	4.836506	-0.023791	1.341144
128.911347	575.606752	4.841510	-0.024312	1.350527
130.907300	584.011457	4.846515	-0.024689	1.359827
132.343188	592.520030	4.851520	-0.024962	1.369073
133.704494	600.993661	4.856525	-0.025221	1.378207
135.183144	609.444481	4.861530	-0.025502	1.387276
136.312987	617.936886	4.866534	-0.025718	1.396270
137.422348	626.383234	4.871539	-0.025930	1.405154
139.237823	634.731154	4.876544	-0.026274	1.414001
141.556541	642.974559	4.881549	-0.026711	1.422771
143.167020	651.369256	4.886554	-0.027016	1.431521
144.294367	659.796478	4.891558	-0.027231	1.440169
145.037752	668.279784	4.896563	-0.027375	1.448758
146.365520	676.649830	4.901568	-0.027628	1.457280
147.283089	685.034337	4.906573	-0.027804	1.465699
148.319768	693.452985	4.911578	-0.028003	1.474122
149.205406	701.817489	4.916582	-0.028173	1.482420
149.987667	710.174117	4.921587	-0.028324	1.490648
150.706857	718.560284	4.926592	-0.028464	1.498848
151.503105	726.876363	4.931597	-0.028617	1.506949
152.550428	735.165639	4.936602	-0.028818	1.515019
153.195408	743.503976	4.941606	-0.028943	1.523031
154.025898	751.797376	4.946611	-0.029103	1.530987
155.302869	760.036070	4.951616	-0.029347	1.538918
156.239625	768.305697	4.956621	-0.029526	1.546785
156.692884	776.666980	4.961626	-0.029616	1.554624
157.816603	784.865804	4.966630	-0.029831	1.562374
158.660049	793.117956	4.971635	-0.029993	1.570093
159.346016	801.418977	4.976640	-0.030126	1.577795
160.187765	809.643216	4.981645	-0.030288	1.585412
161.149860	817.903851	4.986650	-0.030473	1.593043
162.085295	826.101570	4.991654	-0.030653	1.600577
162.652302	834.385790	4.996659	-0.030763	1.608100
163.522203	842.613257	5.001664	-0.030931	1.615580
164.806447	850.757345	5.006669	-0.031175	1.623010
165.339989	859.085489	5.011674	-0.031280	1.630463
166.061176	867.320343	5.016678	-0.031420	1.637825
166.942410	875.479667	5.021683	-0.031589	1.645111
167.776179	883.704544	5.026688	-0.031750	1.652415
168.175221	891.964901	5.031693	-0.031829	1.659657
169.053298	900.150511	5.036698	-0.031998	1.666868
169.757451	908.371769	5.041702	-0.032135	1.674055
170.228688	916.585294	5.046707	-0.032228	1.681173
171.403767	924.717406	5.051712	-0.032452	1.688287
172.164130	932.908214	5.056717	-0.032599	1.695364
172.771806	941.133366	5.061722	-0.032717	1.702420
173.477513	949.337276	5.066726	-0.032854	1.709442
173.890433	957.562032	5.071731	-0.032936	1.716414
174.528870	965.741270	5.076736	-0.033061	1.723349
175.259437	973.886033	5.081741	-0.033202	1.730239
176.030511	982.074256	5.086746	-0.033351	1.737144
176.844924	990.211785	5.091750	-0.033508	1.743984
177.190197	998.452298	5.096755	-0.033577	1.750821
177.624662	1006.666685	5.101760	-0.033664	1.757622
178.074581	1014.829492	5.106765	-0.033753	1.764356
178.670330	1023.004646	5.111770	-0.033869	1.771094
179.123446	1031.204724	5.116774	-0.033959	1.777807
179.423568	1039.388572	5.121779	-0.034020	1.784463
179.944921	1047.583822	5.126784	-0.034122	1.791131
180.399136	1055.746751	5.131789	-0.034212	1.797739
180.905153	1063.869966	5.136794	-0.034312	1.804298
181.220295	1072.051484	5.141798	-0.034376	1.810856
181.630357	1080.205753	5.146803	-0.034458	1.817381
182.247194	1088.340181	5.151808	-0.034578	1.823891
182.413085	1096.528907	5.156813	-0.034614	1.830366
182.908313	1104.658192	5.161818	-0.034711	1.836811
183.264400	1112.810594	5.166822	-0.034783	1.843235
183.724471	1120.935906	5.171827	-0.034874	1.849628
184.186816	1129.092861	5.176832	-0.034965	1.856023
184.136177	1137.296772	5.181837	-0.034961	1.862372
184.372434	1145.478617	5.186842	-0.035011	1.868716
185.047745	1153.538390	5.191846	-0.035142	1.874996
185.275130	1161.676560	5.196851	-0.035189	1.881263
185.554097	1169.830339	5.201856	-0.035247	1.887527
185.931278	1177.947655	5.206861	-0.035322	1.893753
186.338900	1186.061881	5.211866	-0.035403	1.899961
186.333715	1194.258374	5.216870	-0.035408	1.906163
186.898701	1202.330313	5.221875	-0.035518	1.912316
187.280712	1210.478783	5.226880	-0.035595	1.918485
187.300044	1218.616572	5.231885	-0.035604	1.924586
187.879229	1226.699924	5.236890	-0.035717	1.930690
188.197535	1234.841877	5.241894	-0.035781	1.936789
188.466114	1242.969702	5.246899	-0.035837	1.942852
188.924839	1251.097694	5.251904	-0.035927	1.948918
189.080142	1259.223977	5.256909	-0.035961	1.954930
188.757267	1267.437949	5.261914	-0.035907	1.960935
189.127383	1275.515473	5.266918	-0.035981	1.966899
189.727854	1283.565354	5.271923	-0.036098	1.972849
189.835612	1291.738500	5.276928	-0.036123	1.978817
189.842995	1299.843430	5.281933	-0.036130	1.984706
189.818937	1308.020319	5.286938	-0.036131	1.990627
190.207533	1316.106345	5.291942	-0.036208	1.996509
190.665951	1324.146470	5.296947	-0.036299	2.002349
191.046460	1332.252316	5.301952	-0.036375	2.008210
191.875998	1340.264175	5.306957	-0.036535	2.014034
192.010664	1348.421834	5.311962	-0.036565	2.019871
192.488061	1356.510948	5.316966	-0.036659	2.025680
192.809794	1364.635708	5.321971	-0.036725	2.031480
193.408387	1372.716787	5.326976	-0.036841	2.037262
193.494191	1380.845155	5.331981	-0.036863	2.043007
193.546725	1389.017833	5.336986	-0.036878	2.048764
193.596481	1397.161179	5.341990	-0.036892	2.054484
194.291543	1405.157624	5.346995	-0.037027	2.060151
194.806397	1413.233795	5.352000	-0.037128	2.065840
194.571692	1421.444082	5.357005	-0.037090	2.071530
195.091537	1429.490218	5.362010	-0.037192	2.077167
195.108533	1437.640496	5.367014	-0.037200	2.082810
195.446538	1445.712160	5.372019	-0.037269	2.088416
196.100457	1453.757022	5.377024	-0.037396	2.094020
195.709984	1461.980326	5.382029	-0.037328	2.099627
196.440387	1469.984767	5.387034	-0.037469	2.105181
196.534628	1478.150207	5.392038	-0.037492	2.110767
197.106919	1486.193482	5.397043	-0.037604	2.116302
197.607042	1494.241575	5.402048	-0.037702	2.121819
197.933135	1502.325798	5.407053	-0.037768	2.127329
198.339904	1510.414280	5.412058	-0.037849	2.132835
199.162395	1518.425791	5.417062	-0.038008	2.138315
199.508104	1526.504372	5.422067	-0.038077	2.143780
199.820319	1534.657610	5.427072	-0.038141	2.149278
200.064251	1542.746217	5.432077	-0.038192	2.154712
200.027972	1550.911791	5.437082	-0.038190	2.160157
200.091446	1559.012750	5.442086	-0.038207	2.165554
199.975478	1567.165297	5.447091	-0.038191	2.170956
200.550224	1575.199547	5.452096	-0.038303	2.176331
201.007117	1583.226196	5.457101	-0.038394	2.181676
201.464389	1591.297735	5.462106	-0.038484	2.187038
201.778850	1599.393345	5.467110	-0.038548	2.192389
202.237392	1607.446571	5.472115	-0.038638	2.197713
202.449600	1615.549599	5.477120	-0.038683	2.203033
203.197075	1623.564003	5.482125	-0.038828	2.208332
202.970730	1631.773649	5.487130	-0.038791	2.213656
203.253022	1639.864407	5.492134	-0.038849	2.218936
203.777489	1647.866204	5.497139	-0.038952	2.224169
204.140186	1655.982561	5.502144	-0.039024	2.229448
204.113398	1664.082574	5.507149	-0.039025	2.234669
204.470574	1672.155853	5.512154	-0.039096	2.239895
204.429930	1680.295779	5.517158	-0.039094	2.245116
205.011790	1688.303502	5.522163	-0.039208	2.250295
205.744340	1696.326887	5.527168	-0.039349	2.255487
205.974268	1704.423561	5.532173	-0.039398	2.260668
206.243156	1712.519054	5.537178	-0.039453	2.265840
206.505942	1720.658978	5.542182	-0.039507	2.271027
207.004939	1728.692283	5.547187	-0.039605	2.276157
207.269924	1736.765193	5.552192	-0.039660	2.281279
207.343666	1744.844283	5.557197	-0.039679	2.286376
207.733747	1752.928726	5.562202	-0.039757	2.291493
208.058961	1761.005874	5.567206	-0.039823	2.296589
208.047107	1769.101815	5.572211	-0.039826	2.301655
208.582495	1777.138129	5.577216	-0.039931	2.306721
208.384459	1785.279954	5.582221	-0.039899	2.311778
208.421245	1793.378794	5.587226	-0.039911	2.316817
209.010816	1801.361472	5.592230	-0.040026	2.321821
209.269538	1809.438704	5.597235	-0.040080	2.326844
209.644433	1817.513120	5.602240	-0.040155	2.331864
209.572175	1825.636183	5.607245	-0.040147	2.336865
210.402272	1833.615304	5.612250	-0.040306	2.341844
210.274017	1841.760464	5.617254	-0.040288	2.346833
210.335641	1849.865907	5.622259	-0.040304	2.351803
210.492618	1857.951812	5.627264	-0.040339	2.356758
210.792971	1865.957511	5.632269	-0.040400	2.361666
210.857780	1874.047692	5.637274	-0.040417	2.366596
211.520823	1882.056841	5.642278	-0.040546	2.371516
211.712562	1890.132346	5.647283	-0.040587	2.376427
212.303021	1898.160549	5.652288	-0.040702	2.381331
212.450233	1906.236973	5.657293	-0.040735	2.386218
213.232148	1914.239462	5.662298	-0.040886	2.391103
213.535980	1922.340247	5.667302	-0.040948	2.395997
213.617319	1930.419427	5.672307	-0.040968	2.400851
213.992987	1938.497768	5.677312	-0.041043	2.405718
214.440078	1946.547870	5.682317	-0.041132	2.410563
214.761514	1954.622617	5.687322	-0.041197	2.415404
215.077726	1962.707920	5.692326	-0.041261	2.420241
215.441809	1970.754041	5.697331	-0.041334	2.425048
215.573021	1978.888213	5.702336	-0.041364	2.429880
215.913745	1986.950097	5.707341	-0.041433	2.434676
216.325636	1994.985854	5.712346	-0.041514	2.439453
216.659263	2003.020956	5.717350	-0.041582	2.444213
216.735686	2011.116321	5.722355	-0.041601	2.448980
217.265950	2019.160945	5.727360	-0.041705	2.453743
217.342739	2027.248793	5.732365	-0.041725	2.458486
217.633264	2035.277954	5.737370	-0.041784	2.463203
218.383155	2043.290707	5.742374	-0.041929	2.467936
218.638823	2051.368640	5.747379	-0.041982	2.472661
219.014905	2059.444536	5.752384	-0.042057	2.477384
219.220797	2067.488344	5.757389	-0.042101	2.482066
219.391250	2075.567494	5.762394	-0.042138	2.486758
219.826330	2083.628580	5.767398	-0.042224	2.491450
220.083887	2091.690627	5.772403	-0.042277	2.496120
220.304666	2099.803665	5.777408	-0.042324	2.500808
220.268381	2107.881187	5.782413	-0.042322	2.505448
220.297948	2115.983923	5.787418	-0.042333	2.510099
220.879992	2123.969061	5.792422	-0.042447	2.514714
221.470476	2131.960226	5.797427	-0.042562	2.519325
221.825115	2140.017397	5.802432	-0.042633	2.523948
222.208186	2148.057648	5.807437	-0.042710	2.528555
222.347640	2156.164779	5.812442	-0.042741	2.533173
222.930433	2164.194036	5.817446	-0.042855	2.537771
222.917490	2172.271626	5.822451	-0.042858	2.542345
223.106988	2180.380944	5.827456	-0.042898	2.546943
223.534679	2188.408959	5.832461	-0.042983	2.551504
223.556514	2196.512601	5.837466	-0.042992	2.556070
224.059617	2204.502976	5.842470	-0.043091	2.560599
224.442846	2212.513058	5.847475	-0.043168	2.565122
224.779629	2220.604220	5.852480	-0.043236	2.569680
224.944475	2228.672566	5.857485	-0.043272	2.574204
225.362425	2236.725099	5.862490	-0.043355	2.578729
225.411324	2244.821081	5.867494	-0.043369	2.583245
225.697146	2252.869040	5.872499	-0.043428	2.587742
225.936919	2261.027016	5.877504	-0.043478	2.592290
227.013386	2268.946142	5.882509	-0.043683	2.596755
227.150945	2277.010902	5.887514	-0.043714	2.601228
227.301810	2285.061383	5.892518	-0.043747	2.605687
227.727923	2293.086998	5.897523	-0.043832	2.610142
228.071181	2301.162220	5.902528	-0.043901	2.614612
228.212602	2309.193986	5.907533	-0.043933	2.619037
228.355743	2317.258290	5.912538	-0.043965	2.623471
228.524171	2325.336037	5.917542	-0.044001	2.627908
228.363959	2333.445852	5.922547	-0.043977	2.632332
228.923302	2341.430928	5.927552	-0.044086	2.636729
229.351538	2349.456253	5.932557	-0.044171	2.641132
229.357300	2357.526576	5.937562	-0.044177	2.645524
229.891535	2365.559381	5.942566	-0.044282	2.649923
229.901248	2373.646106	5.947571	-0.044289	2.654309
230.220724	2381.689587	5.952576	-0.044354	2.658685
230.711514	2389.679777	5.957581	-0.044451	2.663037
230.741865	2397.783313	5.962586	-0.044461	2.667412
231.421871	2405.792678	5.967590	-0.044593	2.671771
231.783316	2413.813872	5.972595	-0.044666	2.676109
231.873071	2421.906534	5.977600	-0.044688	2.680461
231.652510	2430.005401	5.982605	-0.044652	2.684788
231.985867	2438.035129	5.987610	-0.044719	2.689108
232.516187	2446.041150	5.992614	-0.044823	2.693421
232.490236	2454.137837	5.997619	-0.044824	2.697739
233.140362	2462.128558	6.002624	-0.044950	2.702037
233.269379	2470.201351	6.007629	-0.044979	2.706339
233.117952	2478.316260	6.012634	-0.044956	2.710638
233.810377	2486.287922	6.017638	-0.045091	2.714908
234.409328	2494.259013	6.022643	-0.045207	2.719165
234.262919	2502.392318	6.027648	-0.045185	2.723454
235.085356	2510.344450	6.032653	-0.045344	2.727702
235.304465	2518.448222	6.037658	-0.045390	2.731984
235.134631	2526.612586	6.042662	-0.045363	2.736268
235.267180	2534.641665	6.047667	-0.045393	2.740492
235.585954	2542.646104	6.052672	-0.045458	2.744709
235.338715	2550.792527	6.057677	-0.045417	2.748959
235.525449	2558.849608	6.062682	-0.045457	2.753182
236.120596	2566.837168	6.067686	-0.045573	2.757387
236.409175	2574.801057	6.072691	-0.045632	2.761555
237.288230	2582.759524	6.077696	-0.045801	2.765750
237.414245	2590.866448	6.082701	-0.045830	2.769970
237.703235	2598.907566	6.087706	-0.045889	2.774158
237.890103	2606.986305	6.092710	-0.045929	2.778354
237.488079	2615.111548	6.097715	-0.045859	2.782532
237.934691	2623.126207	6.102720	-0.045948	2.786697
238.520221	2631.107154	6.107725	-0.046062	2.790848
238.655925	2639.170528	6.112730	-0.046093	2.795007
239.083815	2647.167516	6.117734	-0.046177	2.799144
239.315207	2655.204965	6.122739	-0.046226	2.803283
239.557567	2663.275101	6.127744	-0.046276	2.807434
239.730185	2671.330630	6.132749	-0.046314	2.811567
239.626228	2679.446089	6.137754	-0.046299	2.815708
239.942352	2687.459293	6.142758	-0.046364	2.819816
240.204989	2695.469701	6.147763	-0.046418	2.823913
240.843100	2703.479887	6.152768	-0.046542	2.828026
240.998376	2711.550340	6.157773	-0.046576	2.832135
241.226227	2719.596549	6.162778	-0.046624	2.836230
241.507442	2727.650863	6.167782	-0.046681	2.840326
241.754303	2735.632582	6.172787	-0.046732	2.844378
242.138003	2743.687487	6.177792	-0.046809	2.848469
242.132599	2751.767044	6.182797	-0.046813	2.852544
242.026848	2759.870841	6.187802	-0.046799	2.856619
242.290089	2767.918069	6.192806	-0.046853	2.860681
242.553827	2775.898451	6.197811	-0.046908	2.864704
242.969052	2783.935938	6.202816	-0.046990	2.868759
242.881908	2792.038179	6.207821	-0.046979	2.872812
242.923935	2800.099110	6.212826	-0.046992	2.876845
243.596257	2808.058341	6.217830	-0.047123	2.880858
243.799727	2816.071840	6.222835	-0.047166	2.884866
244.160267	2824.119715	6.227840	-0.047238	2.888894
244.557895	2832.117695	6.232845	-0.047317	2.892893
244.909601	2840.189364	6.237850	-0.047388	2.896921
245.465464	2848.218129	6.242854	-0.047497	2.900934
245.413064	2856.266318	6.247859	-0.047492	2.904916
245.772257	2864.354823	6.252864	-0.047564	2.908936
246.059323	2872.451360	6.257869	-0.047623	2.912951
246.277072	2880.449736	6.262874	-0.047669	2.916907
246.418484	2888.521482	6.267878	-0.047701	2.920890
246.638257	2896.495292	6.272883	-0.047747	2.924824
247.070776	2904.532146	6.277888	-0.047832	2.928795
247.499247	2912.535372	6.282893	-0.047917	2.932743
247.593159	2920.615164	6.287898	-0.047940	2.936706
247.707897	2928.688310	6.292902	-0.047967	2.940661
247.826262	2936.705487	6.297907	-0.047994	2.944584
248.190648	2944.732095	6.302912	-0.048067	2.948520
248.690014	2952.727299	6.307917	-0.048165	2.952441
249.100349	2960.762388	6.312922	-0.048247	2.956373
249.159187	2968.833190	6.317926	-0.048263	2.960297
249.566646	2976.814382	6.322931	-0.048344	2.964192
249.759371	2984.903740	6.327936	-0.048385	2.968122
249.556423	2993.008072	6.332941	-0.048353	2.972034
249.814184	3001.011746	6.337946	-0.048406	2.975915
250.262612	3009.024199	6.342950	-0.048495	2.979806
250.139080	3017.096049	6.347955	-0.048477	2.983691
250.222581	3025.193725	6.352960	-0.048498	2.987594
250.435812	3033.247828	6.357965	-0.048543	2.991477
250.508949	3041.282641	6.362970	-0.048562	2.995339
251.074018	3049.233547	6.367974	-0.048672	2.999181
251.387522	3057.209424	6.372979	-0.048736	3.003017
251.451503	3065.292808	6.377984	-0.048753	3.006887
251.238932	3073.421959	6.382989	-0.048719	3.010759
251.713418	3081.362122	6.387994	-0.048812	3.014572
252.574066	3089.325416	6.392998	-0.048978	3.018410
252.411203	3097.414176	6.398003	-0.048953	3.022251
252.433209	3105.544235	6.403008	-0.048962	3.026116
252.468837	3113.562171	6.408013	-0.048974	3.029923
252.511797	3121.618442	6.413018	-0.048987	3.033745
252.785859	3129.635553	6.418022	-0.049043	3.037554
253.205390	3137.610631	6.423027	-0.049127	3.041346
254.011728	3145.566655	6.428032	-0.049282	3.045143
254.168141	3153.641324	6.433037	-0.049316	3.048960
254.153624	3161.742030	6.438042	-0.049319	3.052775
254.513348	3169.776080	6.443046	-0.049391	3.056573
254.594756	3177.827951	6.448051	-0.049412	3.060360
254.917223	3185.840227	6.453056	-0.049477	3.064136
255.096497	3193.888041	6.458061	-0.049516	3.067917
254.943031	3202.001602	6.463066	-0.049492	3.071708
254.961408	3210.090697	6.468070	-0.049501	3.075492
255.322266	3218.002689	6.473075	-0.049573	3.079204
255.686427	3226.041282	6.478080	-0.049646	3.082971
255.262901	3234.127057	6.483085	-0.049573	3.086718
255.843249	3242.091544	6.488090	-0.049686	3.090451
256.208559	3250.101369	6.493094	-0.049759	3.094191
256.241354	3258.157661	6.498099	-0.049771	3.097932
256.855648	3266.138960	6.503104	-0.049890	3.101662
257.062064	3274.171596	6.508109	-0.049934	3.105391
256.936470	3282.286145	6.513114	-0.049916	3.109138
257.281574	3290.305339	6.518118	-0.049985	3.112858
257.486395	3298.322066	6.523123	-0.050029	3.116567
257.651472	3306.384317	6.528128	-0.050065	3.120290
257.922334	3314.342491	6.533133	-0.050120	3.123965
258.405752	3322.358158	6.538138	-0.050216	3.127673
258.524939	3330.454767	6.543142	-0.050243	3.131396
258.701249	3338.473637	6.548147	-0.050281	3.135082
258.786418	3346.536364	6.553152	-0.050302	3.138779
258.472169	3354.628622	6.558157	-0.050249	3.142467
259.023261	3362.598440	6.563162	-0.050357	3.146135
258.825099	3370.727436	6.568166	-0.050325	3.149837
259.212531	3378.681868	6.573171	-0.050403	3.153481
259.602699	3386.715399	6.578176	-0.050480	3.157157
259.641691	3394.752606	6.583181	-0.050493	3.160815
259.630939	3402.773107	6.588186	-0.050496	3.164458
260.432935	3410.727162	6.593190	-0.050651	3.168104
260.504743	3418.797505	6.598195	-0.050669	3.171766
260.464305	3426.893716	6.603200	-0.050667	3.175429
260.735952	3434.874860	6.608205	-0.050723	3.179051
260.711755	3442.934180	6.613210	-0.050724	3.182691
261.240745	3450.946162	6.618214	-0.050827	3.186329
261.302070	3458.957508	6.623219	-0.050844	3.189942
261.660886	3467.003982	6.628224	-0.050916	3.193581
261.941907	3475.031215	6.633229	-0.050974	3.197202
261.935966	3483.084248	6.638234	-0.050978	3.200819
261.867483	3491.146845	6.643238	-0.050970	3.204434
262.369353	3499.100295	6.648243	-0.051069	3.208019
262.507482	3507.196864	6.653248	-0.051100	3.211650
262.495527	3515.254155	6.658253	-0.051103	3.215252
262.543824	3523.260175	6.663258	-0.051117	3.218830
263.004948	3531.268006	6.668262	-0.051208	3.222422
262.959226	3539.317083	6.673267	-0.051205	3.226007
263.373053	3547.334997	6.678272	-0.051287	3.229593
263.008798	3555.477874	6.683277	-0.051225	3.233199
262.651178	3563.521433	6.688282	-0.051163	3.236756
263.711375	3571.380809	6.693286	-0.051366	3.240288
263.448822	3579.433696	6.698291	-0.051322	3.243845
263.850872	3587.463221	6.703296	-0.051402	3.247417
263.589583	3595.566792	6.708301	-0.051359	3.250989
264.062294	3603.527758	6.713306	-0.051452	3.254525
264.521439	3611.547029	6.718310	-0.051543	3.258082
264.391848	3619.606038	6.723315	-0.051524	3.261629
264.550509	3627.644841	6.728320	-0.051559	3.265175
264.858879	3635.665084	6.733325	-0.051621	3.268714
265.382340	3643.655073	6.738330	-0.051724	3.272246
265.336667	3651.764894	6.743334	-0.051721	3.275803
265.217841	3659.771964	6.748339	-0.051704	3.279308
265.683327	3667.723820	6.753344	-0.051796	3.282808
265.834247	3675.811106	6.758349	-0.051829	3.286352
266.311939	3683.778616	6.763354	-0.051923	3.289852
266.153916	3691.921733	6.768358	-0.051899	3.293400
266.489156	3699.892453	6.773363	-0.051967	3.296889
266.476205	3707.987383	6.778368	-0.051970	3.300414
266.602710	3715.969173	6.783373	-0.051999	3.303891
266.648281	3724.035773	6.788378	-0.052012	3.307399
266.643615	3732.121263	6.793382	-0.052017	3.310909
267.133575	3740.026661	6.798387	-0.052113	3.314356
267.573300	3748.025809	6.803392	-0.052200	3.317839
267.656104	3756.098125	6.808397	-0.052221	3.321336
268.084942	3764.048988	6.813402	-0.052306	3.324790
268.158091	3772.170342	6.818406	-0.052325	3.328300
267.699216	3780.273213	6.823411	-0.052245	3.331778
267.666160	3788.341342	6.828416	-0.052244	3.335253
268.623058	3796.192781	6.833421	-0.052427	3.338670
268.668957	3804.255523	6.838426	-0.052441	3.342139
269.152423	3812.257423	6.843430	-0.052536	3.345595
268.665125	3820.404477	6.848435	-0.052451	3.349073
268.952559	3828.418677	6.853440	-0.052509	3.352520
269.400466	3836.392888	6.858445	-0.052598	3.355952
269.812609	3844.360366	6.863450	-0.052680	3.359376
269.755473	3852.444474	6.868454	-0.052675	3.362829
270.068186	3860.466541	6.873459	-0.052738	3.366266
270.236006	3868.523498	6.878464	-0.052775	3.369708
270.529873	3876.525777	6.883469	-0.052835	3.373129
270.372121	3884.606308	6.888474	-0.052810	3.376562
270.696613	3892.609198	6.893478	-0.052876	3.379977
270.664372	3900.661432	6.898483	-0.052875	3.383396
271.042578	3908.676883	6.903488	-0.052951	3.386812
271.043314	3916.716102	6.908493	-0.052956	3.390220
271.175973	3924.773496	6.913498	-0.052986	3.393637
271.690164	3932.762145	6.918502	-0.053087	3.397035
271.790370	3940.780335	6.923507	-0.053111	3.400427
272.213295	3948.721400	6.928512	-0.053195	3.403795
272.347998	3956.786113	6.933517	-0.053225	3.407202
272.264340	3964.880441	6.938522	-0.053215	3.410609
272.536423	3972.886707	6.943526	-0.053271	3.413989
272.709517	3980.881168	6.948531	-0.053308	3.417357
272.653622	3988.977233	6.953536	-0.053303	3.420756
272.976391	3996.933426	6.958541	-0.053369	3.424107
273.118439	4004.987957	6.963546	-0.053400	3.427489
273.026799	4013.087204	6.968550	-0.053389	3.430878
272.779530	4021.107379	6.973555	-0.053348	3.434226
272.876703	4029.153682	6.978560	-0.053371	3.437593
273.338342	4037.134293	6.983565	-0.053462	3.440942
273.586671	4045.048485	6.988570	-0.053514	3.444252
274.056574	4053.107976	6.993574	-0.053606	3.447628
274.522796	4061.118891	6.998579	-0.053698	3.450980
274.354690	4069.216261	7.003584	-0.053672	3.454342
274.452056	4077.244805	7.008589	-0.053696	3.457682
274.937559	4085.226078	7.013594	-0.053791	3.461013
274.968072	4093.290826	7.018598	-0.053802	3.464359
274.801294	4101.353079	7.023603	-0.053777	3.467694
275.102110	4109.391065	7.028608	-0.053838	3.471032
275.392098	4117.378906	7.033613	-0.053897	3.474345
275.186901	4125.429677	7.038618	-0.053864	3.477665
275.639338	4133.449376	7.043622	-0.053953	3.480990
275.727074	4141.385129	7.048627	-0.053975	3.484266
275.628706	4149.497993	7.053632	-0.053962	3.487605
276.624165	4157.455108	7.058637	-0.054153	3.490913
276.621402	4165.461253	7.063642	-0.054157	3.494205
276.350628	4173.624804	7.068646	-0.054112	3.497550
276.579394	4181.611742	7.073651	-0.054160	3.500836
277.302209	4189.508461	7.078656	-0.054300	3.504097
277.725339	4197.563155	7.083661	-0.054384	3.507411
277.562819	4205.688677	7.088666	-0.054359	3.510731
277.687580	4213.697609	7.093670	-0.054387	3.514010
277.696487	4221.730064	7.098675	-0.054394	3.517291
277.674726	4229.796925	7.103680	-0.054395	3.520583
278.047360	4237.727906	7.108685	-0.054470	3.523828
278.352911	4245.775119	7.113690	-0.054532	3.527116
278.785061	4253.790215	7.118694	-0.054618	3.530392
278.970952	4261.811318	7.123699	-0.054658	3.533659
278.872407	4269.907306	7.128704	-0.054644	3.536945
279.474886	4277.843556	7.133709	-0.054762	3.540184
279.491995	4285.875552	7.138714	-0.054770	3.543442
279.676225	4293.936822	7.143718	-0.054810	3.546713
279.466681	4302.009539	7.148723	-0.054776	3.549973
279.771819	4310.085039	7.153728	-0.054838	3.553248
280.186185	4318.053887	7.158733	-0.054921	3.556480
280.103544	4326.044731	7.163738	-0.054910	3.559702
280.611863	4334.026653	7.168742	-0.055010	3.562937
280.687761	4342.036354	7.173747	-0.055030	3.566166
280.402225	4350.128725	7.178752	-0.054982	3.569414
280.852878	4358.111610	7.183757	-0.055071	3.572638
280.515331	4366.228687	7.188762	-0.055013	3.575889
280.390229	4374.262406	7.193766	-0.054995	3.579110
280.915818	4382.145713	7.198771	-0.055098	3.582287
281.516805	4390.163951	7.203776	-0.055215	3.585518
281.716902	4398.228049	7.208781	-0.055258	3.588752
281.798613	4406.268457	7.213786	-0.055278	3.591970
281.873054	4414.342452	7.218790	-0.055297	3.595198
282.285785	4422.276780	7.223795	-0.055379	3.598378
282.508919	4430.345793	7.228800	-0.055426	3.601603
282.493132	4438.390274	7.233805	-0.055429	3.604809
282.691739	4446.378397	7.238810	-0.055471	3.607995
282.638073	4454.496489	7.243814	-0.055466	3.611223
282.806734	4462.447711	7.248819	-0.055503	3.614388
283.468666	4470.433940	7.253824	-0.055631	3.617578
283.588769	4478.523379	7.258829	-0.055659	3.620791
283.976524	4486.452632	7.263834	-0.055736	3.623945
284.097908	4494.572956	7.268838	-0.055764	3.627165
284.054103	4502.620836	7.273843	-0.055761	3.630348
284.421160	4510.617944	7.278848	-0.055835	3.633520
284.705441	4518.649467	7.283853	-0.055893	3.636700
284.700460	4526.630376	7.288858	-0.055897	3.639850
285.023341	4534.606830	7.293862	-0.055962	3.643004
285.016329	4542.689001	7.298867	-0.055966	3.646188
285.177500	4550.691786	7.303872	-0.056002	3.649342
285.352892	4558.778408	7.308877	-0.056040	3.652527
285.432511	4566.817685	7.313882	-0.056060	3.655688
285.821161	4574.768357	7.318886	-0.056137	3.658820
285.981689	4582.797674	7.323891	-0.056172	3.661974
286.183418	4590.792076	7.328896	-0.056215	3.665113
286.604603	4598.803729	7.333901	-0.056299	3.668261
286.898087	4606.848061	7.338906	-0.056359	3.671416
287.088233	4614.903384	7.343910	-0.056399	3.674570
286.712577	4622.950255	7.348915	-0.056335	3.677703
286.865721	4631.008378	7.353920	-0.056368	3.680851
287.382014	4638.927675	7.358925	-0.056470	3.683953
287.291378	4646.994693	7.363930	-0.056458	3.687093
287.668951	4655.026284	7.368934	-0.056534	3.690229
287.967118	4663.027701	7.373939	-0.056594	3.693348
288.006918	4671.118602	7.378944	-0.056607	3.696493
288.298393	4679.086014	7.383949	-0.056666	3.699594
288.292784	4687.111620	7.388954	-0.056671	3.702707
288.389980	4695.211235	7.393958	-0.056694	3.705848
288.114767	4703.243456	7.398963	-0.056648	3.708952
288.614334	4711.271021	7.403968	-0.056746	3.712071
288.787681	4719.298157	7.408973	-0.056784	3.715178
288.777356	4727.271492	7.413978	-0.056787	3.718258
289.130290	4735.284094	7.418982	-0.056858	3.721359
289.538040	4743.227038	7.423987	-0.056939	3.724432
289.668156	4751.277645	7.428992	-0.056969	3.727538
289.574928	4759.373992	7.433997	-0.056957	3.730652
289.841200	4767.348858	7.439002	-0.057011	3.733726
289.825242	4775.449559	7.444006	-0.057014	3.736839
289.637760	4783.438825	7.449011	-0.056984	3.739903
290.169107	4791.398644	7.454016	-0.057088	3.742970
290.445932	4799.427272	7.459021	-0.057145	3.746055
290.235732	4807.477658	7.464026	-0.057111	3.749133
290.347411	4815.518837	7.469030	-0.057137	3.752214
290.602087	4823.520789	7.474035	-0.057190	3.755280
290.980643	4831.503526	7.479040	-0.057265	3.758340
290.712934	4839.614981	7.484045	-0.057221	3.761430
290.694785	4847.570643	7.489050	-0.057223	3.764465
291.334428	4855.562479	7.494054	-0.057347	3.767527
291.114476	4863.644729	7.499059	-0.057311	3.770600
291.611905	4871.624455	7.504064	-0.057409	3.773648
291.607903	4879.692329	7.509069	-0.057414	3.776716
291.718509	4887.665908	7.514074	-0.057439	3.779748
292.008454	4895.673465	7.519078	-0.057499	3.782795
292.221416	4903.707203	7.524083	-0.057543	3.785847
292.124897	4911.770763	7.529088	-0.057531	3.788901
292.416779	4919.771518	7.534093	-0.057590	3.791938
292.294901	4927.842187	7.539098	-0.057573	3.794989
292.904288	4935.825824	7.544102	-0.057692	3.798022
292.639538	4943.885140	7.549107	-0.057648	3.801060
292.840122	4951.817428	7.554112	-0.057690	3.804059
293.344785	4959.863503	7.559117	-0.057789	3.807106
293.492416	4967.842518	7.564122	-0.057822	3.810116
293.645759	4975.911337	7.569126	-0.057856	3.813159
293.633083	4983.994978	7.574131	-0.057859	3.816200
294.082715	4991.940286	7.579136	-0.057948	3.819197
294.315964	5000.008860	7.584141	-0.057996	3.822234
294.238799	5008.029191	7.589146	-0.057987	3.825243
294.232794	5016.108216	7.594150	-0.057991	3.828273
293.945038	5024.168617	7.599155	-0.057943	3.831288
294.046809	5032.121421	7.604160	-0.057967	3.834268
294.487700	5040.146540	7.609165	-0.058054	3.837281
294.489791	5048.165394	7.614170	-0.058060	3.840279
294.471471	5056.177502	7.619174	-0.058062	3.843272
294.945199	5064.169789	7.624179	-0.058155	3.846266
295.055520	5072.217180	7.629184	-0.058181	3.849271
294.975304	5080.263470	7.634189	-0.058171	3.852268
295.147118	5088.257067	7.639194	-0.058209	3.855249
295.603247	5096.247356	7.644198	-0.058299	3.858232
295.588285	5104.333084	7.649203	-0.058301	3.861239
295.436531	5112.301776	7.654208	-0.058278	3.864197
295.732957	5120.389052	7.659213	-0.058339	3.867206
295.798532	5128.391422	7.664218	-0.058356	3.870176
296.211782	5136.514349	7.669222	-0.058438	3.873196
296.269732	5144.501860	7.674227	-0.058454	3.876156
296.482332	5152.421888	7.679232	-0.058499	3.879092
296.589549	5160.465352	7.684237	-0.058524	3.882069
296.662997	5168.418890	7.689242	-0.058543	3.885010
297.014476	5176.428226	7.694246	-0.058614	3.887975
297.001077	5184.479194	7.699251	-0.058617	3.890945
297.335092	5192.455390	7.704256	-0.058684	3.893893
297.357492	5200.532831	7.709261	-0.058693	3.896870
297.669831	5208.497149	7.714266	-0.058757	3.899808
297.508278	5216.585919	7.719270	-0.058732	3.902781
297.601161	5224.593093	7.724275	-0.058754	3.905726
298.016149	5232.578766	7.729280	-0.058837	3.908667
297.816901	5240.688770	7.734285	-0.058805	3.911640
297.901526	5248.652551	7.739290	-0.058826	3.914563
298.344464	5256.713978	7.744294	-0.058914	3.917526
298.708424	5264.660541	7.749299	-0.058987	3.920443
298.650282	5272.657751	7.754304	-0.058981	3.923368
299.023860	5280.738044	7.759309	-0.059056	3.926330
298.863339	5288.741589	7.764314	-0.059031	3.929251
299.032828	5296.860329	7.769318	-0.059068	3.932219
298.905616	5304.875795	7.774323	-0.059050	3.935141
299.060209	5312.849096	7.779328	-0.059084	3.938051
299.491347	5320.868900	7.784333	-0.059169	3.940980
299.487916	5328.818640	7.789338	-0.059174	3.943874
299.668759	5336.934747	7.794342	-0.059213	3.946830
299.909951	5344.926761	7.799347	-0.059263	3.949739
300.400937	5352.928360	7.804352	-0.059359	3.952654
300.597464	5360.949341	7.809357	-0.059401	3.955569
300.515449	5369.000778	7.814362	-0.059391	3.958487
300.842234	5377.021981	7.819366	-0.059457	3.961400
300.808132	5384.984586	7.824371	-0.059456	3.964283
301.146035	5393.040505	7.829376	-0.059524	3.967204
301.173959	5401.073930	7.834381	-0.059535	3.970110
301.049846	5409.087104	7.839386	-0.059517	3.973003
301.448850	5417.126023	7.844390	-0.059596	3.975913
301.666759	5425.078659	7.849395	-0.059642	3.978786
301.673939	5433.125455	7.854400	-0.059649	3.981687
301.877171	5441.132131	7.859405	-0.059692	3.984575
302.155571	5449.152325	7.864410	-0.059749	3.987467
302.252708	5457.231540	7.869414	-0.059772	3.990376
302.165965	5465.226543	7.874419	-0.059761	3.993248
302.346817	5473.272643	7.879424	-0.059800	3.996142
302.397496	5481.271736	7.884429	-0.059815	3.999014
302.765950	5489.244021	7.889434	-0.059889	4.001880
302.765944	5497.248420	7.894438	-0.059894	4.004749
302.867020	5505.279937	7.899443	-0.059918	4.007627
303.187202	5513.308688	7.904448	-0.059983	4.010507
303.250569	5521.395583	7.909453	-0.060000	4.013400
303.391013	5529.406972	7.914458	-0.060031	4.016266
303.607776	5537.372499	7.919462	-0.060077	4.019114
303.721002	5545.413334	7.924467	-0.060103	4.021986
303.923903	5553.402411	7.929472	-0.060146	4.024838
304.086104	5561.425410	7.934477	-0.060182	4.027700
303.909176	5569.505680	7.939482	-0.060154	4.030575
304.302335	5577.575305	7.944486	-0.060232	4.033453
304.544779	5585.554082	7.949491	-0.060283	4.036295
304.740975	5593.512559	7.954496	-0.060325	4.039126
304.260123	5601.644388	7.959501	-0.060240	4.042006
304.424313	5609.585690	7.964506	-0.060276	4.044827
304.825161	5617.576650	7.969510	-0.060356	4.047667
305.072514	5625.574932	7.974515	-0.060407	4.050505
305.208759	5633.581206	7.979520	-0.060438	4.053342
305.591218	5641.653796	7.984525	-0.060514	4.056205
305.128291	5649.657168	7.989530	-0.060433	4.059028
305.721879	5657.738225	7.994534	-0.060549	4.061893
306.188951	5665.648549	7.999539	-0.060641	4.064693
306.018564	5673.739034	8.004544	-0.060615	4.067545
306.272496	5681.766371	8.009549	-0.060667	4.070380
306.389446	5689.760977	8.014554	-0.060694	4.073199
306.372506	5697.865341	8.019558	-0.060696	4.076052
306.467753	5705.825948	8.024563	-0.060719	4.078855
306.595202	5713.859991	8.029568	-0.060748	4.081682
307.190647	5721.784862	8.034573	-0.060864	4.084475
306.926630	5729.889288	8.039578	-0.060820	4.087317
306.965692	5737.921638	8.044582	-0.060833	4.090136
307.464247	5745.879023	8.049587	-0.060931	4.092934
307.539272	5753.958498	8.054592	-0.060950	4.095766
307.771445	5761.952414	8.059597	-0.060999	4.098569
307.946298	5769.990843	8.064602	-0.061036	4.101384
308.050158	5777.968108	8.069606	-0.061061	4.104175
307.886885	5786.024243	8.074611	-0.061036	4.106988
308.247127	5794.007480	8.079616	-0.061108	4.109781
308.428174	5802.087625	8.084621	-0.061147	4.112604
308.445887	5810.051867	8.089626	-0.061156	4.115381
308.602635	5818.060783	8.094630	-0.061190	4.118174
308.582428	5826.118082	8.099635	-0.061192	4.120980
308.965083	5834.060014	8.104640	-0.061268	4.123749
309.138624	5842.151241	8.109645	-0.061306	4.126566
308.788889	5850.165137	8.114650	-0.061246	4.129346
309.498047	5858.131528	8.119654	-0.061383	4.132123
309.448620	5866.198547	8.124659	-0.061379	4.134922
309.440039	5874.212723	8.129664	-0.061383	4.137701
309.704494	5882.242583	8.134669	-0.061437	4.140488
310.040386	5890.161647	8.139674	-0.061505	4.143235
309.880382	5898.287123	8.144678	-0.061480	4.146046
310.003436	5906.304476	8.149683	-0.061508	4.148821
310.038901	5914.308850	8.154688	-0.061520	4.151588
309.973758	5922.360304	8.159693	-0.061513	4.154368
310.018884	5930.321676	8.164698	-0.061527	4.157117
310.698932	5938.319265	8.169702	-0.061659	4.159885
310.582594	5946.341693	8.174707	-0.061642	4.162649
310.882089	5954.345188	8.179712	-0.061703	4.165410
310.936743	5962.406544	8.184717	-0.061719	4.168186
311.037761	5970.417170	8.189722	-0.061743	4.170944
311.065094	5978.492105	8.194726	-0.061753	4.173721
311.050802	5986.491209	8.199731	-0.061756	4.176469
311.279779	5994.485132	8.204736	-0.061804	4.179216
311.533380	6002.524505	8.209741	-0.061856	4.181978
311.783644	6010.454668	8.214746	-0.061908	4.184701
311.605264	6018.605559	8.219750	-0.061880	4.187492
311.592045	6026.634802	8.224755	-0.061883	4.190241
311.939426	6034.632237	8.229760	-0.061953	4.192982
312.224410	6042.672811	8.234765	-0.062011	4.195736
311.747229	6050.668955	8.239770	-0.061927	4.198463
312.123987	6058.701485	8.244774	-0.062003	4.201211
312.040780	6066.592095	8.249779	-0.061992	4.203903
312.336113	6074.647158	8.254784	-0.062053	4.206655
312.419637	6082.700944	8.259789	-0.062073	4.209401
312.220245	6090.754742	8.264794	-0.062041	4.212142
312.913787	6098.736586	8.269798	-0.062176	4.214868
312.727621	6106.776573	8.274803	-0.062146	4.217601
312.556300	6114.819386	8.279808	-0.062120	4.220334
313.054471	6122.759279	8.284813	-0.062218	4.223037
313.099421	6130.800910	8.289818	-0.062231	4.225768
313.280342	6138.812129	8.294822	-0.062270	4.228489
313.510434	6146.862021	8.299827	-0.062318	4.231221
313.445336	6154.870332	8.304832	-0.062311	4.233934
313.614432	6162.906837	8.309837	-0.062348	4.236658
313.792386	6170.822827	8.314842	-0.062386	4.239339
314.119720	6178.926704	8.319846	-0.062453	4.242084
314.156454	6186.890635	8.324851	-0.062465	4.244776
314.280730	6194.917980	8.329856	-0.062493	4.247489
314.610851	6202.951654	8.334861	-0.062560	4.250205
315.004656	6210.941474	8.339866	-0.062638	4.252904
314.640453	6219.091761	8.344870	-0.062576	4.255648
314.683474	6227.078376	8.349875	-0.062589	4.258340
314.550095	6235.081791	8.354880	-0.062569	4.261034
314.796731	6243.045623	8.359885	-0.062621	4.263716
314.747788	6251.056655	8.364890	-0.062617	4.266410
315.003301	6259.096412	8.369894	-0.062669	4.269114
315.075867	6267.159678	8.374899	-0.062688	4.271823
315.263723	6275.098259	8.379904	-0.062728	4.274490
315.081342	6283.217209	8.384909	-0.062700	4.277211
315.773395	6291.048237	8.389914	-0.062834	4.279843
315.624295	6299.164344	8.394918	-0.062811	4.282561
315.562095	6307.168401	8.399923	-0.062805	4.285240
316.210592	6315.130696	8.404928	-0.062931	4.287911
316.298756	6323.228510	8.409933	-0.062953	4.290619
316.447730	6331.213009	8.414938	-0.062985	4.293289
316.605933	6339.278040	8.419942	-0.063020	4.295984
316.883406	6347.271076	8.424947	-0.063077	4.298654
316.873504	6355.288117	8.429952	-0.063080	4.301328
316.765647	6363.305255	8.434957	-0.063066	4.304000
316.755867	6371.369752	8.439962	-0.063069	4.306686
316.671401	6379.440303	8.444966	-0.063059	4.309372
317.185442	6387.367048	8.449971	-0.063159	4.312014
317.267569	6395.348501	8.454976	-0.063180	4.314669
317.703430	6403.343724	8.459981	-0.063266	4.317329
317.952731	6411.331868	8.464986	-0.063318	4.319984
317.870918	6419.415232	8.469990	-0.063308	4.322666
318.216341	6427.395942	8.474995	-0.063378	4.325316
318.142218	6435.423180	8.480000	-0.063369	4.327976
318.263939	6443.484457	8.485005	-0.063397	4.330648
318.410126	6451.449239	8.490010	-0.063429	4.333286
318.771244	6459.489252	8.495014	-0.063502	4.335949
318.661001	6467.491839	8.500019	-0.063486	4.338594
318.665756	6475.557963	8.505024	-0.063493	4.341260
318.768877	6483.506638	8.510029	-0.063517	4.343886
318.972456	6491.571362	8.515034	-0.063560	4.346549
318.657225	6499.652224	8.520038	-0.063507	4.349212
318.971640	6507.644790	8.525043	-0.063571	4.351850
319.397401	6515.591451	8.530048	-0.063655	4.354471
319.644736	6523.624897	8.535053	-0.063706	4.357118
319.864420	6531.571892	8.540058	-0.063752	4.359734
319.812877	6539.644702	8.545062	-0.063748	4.362388
319.906369	6547.665053	8.550067	-0.063771	4.365025
319.921111	6555.699626	8.555072	-0.063779	4.367664
320.240701	6563.710586	8.560077	-0.063843	4.370296
319.952484	6571.708145	8.565082	-0.063795	4.372917
320.162938	6579.792183	8.570087	-0.063839	4.375569
320.642120	6587.730677	8.575091	-0.063934	4.378174
320.570601	6595.784784	8.580096	-0.063926	4.380810
320.829956	6603.767214	8.585101	-0.063979	4.383425
320.917922	6611.757079	8.590106	-0.064001	4.386038
320.735853	6619.869020	8.595111	-0.063972	4.388689
320.776512	6627.894323	8.600115	-0.063985	4.391310
321.132241	6635.811993	8.605120	-0.064056	4.393898
321.442954	6643.919140	8.610125	-0.064120	4.396545
321.482446	6651.866124	8.615130	-0.064132	4.399136
321.862871	6659.951140	8.620135	-0.064208	4.401773
321.836496	6667.899363	8.625139	-0.064208	4.404362
322.377264	6675.906760	8.630144	-0.064314	4.406972
322.484109	6683.974303	8.635149	-0.064340	4.409597
322.893127	6691.981541	8.640154	-0.064421	4.412202
322.539872	6700.065344	8.645159	-0.064360	4.414827
322.465540	6708.144911	8.650163	-0.064352	4.417450
322.821995	6716.102194	8.655168	-0.064423	4.420034
323.003339	6724.134797	8.660173	-0.064462	4.422640
323.036396	6732.093893	8.665178	-0.064474	4.425220
322.963134	6740.189646	8.670183	-0.064465	4.427842
323.322848	6748.143835	8.675187	-0.064538	4.430420
323.390467	6756.258334	8.680192	-0.064555	4.433046
323.637790	6764.227869	8.685197	-0.064607	4.435624
323.399421	6772.257558	8.690202	-0.064568	4.438218
323.993203	6780.260803	8.695207	-0.064683	4.440806
324.152544	6788.240208	8.700211	-0.064718	4.443383
323.879930	6796.300929	8.705216	-0.064673	4.445982
324.114123	6804.286574	8.710221	-0.064722	4.448558
324.539122	6812.331146	8.715226	-0.064806	4.451152
324.837805	6820.327265	8.720231	-0.064867	4.453729
325.227159	6828.376245	8.725235	-0.064944	4.456321
325.259953	6836.343205	8.730240	-0.064956	4.458884
325.310199	6844.443708	8.735245	-0.064970	4.461488
325.367798	6852.314617	8.740250	-0.064986	4.464017
325.568107	6860.437900	8.745255	-0.065029	4.466627
325.481025	6868.469887	8.750259	-0.065018	4.469204
325.483066	6876.495494	8.755264	-0.065024	4.471778
325.894937	6884.481079	8.760269	-0.065105	4.474340
325.946627	6892.483161	8.765274	-0.065120	4.476904
326.135223	6900.472407	8.770279	-0.065161	4.479462
326.026573	6908.528808	8.775283	-0.065146	4.482040
326.470098	6916.452709	8.780288	-0.065233	4.484576
326.726490	6924.555654	8.785293	-0.065286	4.487167
326.869791	6932.536759	8.790298	-0.065318	4.489717
326.941862	6940.629001	8.795303	-0.065337	4.492301
327.030046	6948.601438	8.800307	-0.065359	4.494845
326.929867	6956.617931	8.805312	-0.065345	4.497401
327.256418	6964.638764	8.810317	-0.065411	4.499958
327.454326	6972.602079	8.815322	-0.065453	4.502496
327.729339	6980.631864	8.820327	-0.065510	4.505053
327.705180	6988.755116	8.825331	-0.065511	4.507637
327.365188	6996.754943	8.830336	-0.065452	4.510180
327.629796	7004.763349	8.835341	-0.065507	4.512726
327.356037	7012.732035	8.840346	-0.065461	4.515256
328.234977	7020.708657	8.845351	-0.065630	4.517791
327.992633	7028.758828	8.850355	-0.065590	4.520344
327.671252	7036.740401	8.855360	-0.065535	4.522874
328.138680	7044.773637	8.860365	-0.065628	4.525421
328.374731	7052.782303	8.865370	-0.065677	4.527958
328.223802	7060.815057	8.870375	-0.065654	4.530501
328.287915	7068.815703	8.875379	-0.065671	4.533032
328.794660	7076.791102	8.880384	-0.065771	4.535555
328.914158	7084.858636	8.885389	-0.065798	4.538105
328.675563	7092.870634	8.890394	-0.065759	4.540635
329.094603	7100.828914	8.895399	-0.065842	4.543148
329.459952	7108.857559	8.900403	-0.065916	4.545682
329.360385	7116.893668	8.905408	-0.065902	4.548215
329.548519	7124.939844	8.910413	-0.065943	4.550751
329.753762	7132.926005	8.915418	-0.065986	4.553267
330.086283	7140.947446	8.920423	-0.066053	4.555792
329.718190	7148.951891	8.925427	-0.065990	4.558310
329.566345	7157.051426	8.930432	-0.065967	4.560856
330.190090	7164.937295	8.935437	-0.066088	4.563336
330.223325	7172.987864	8.940442	-0.066100	4.565864
330.755165	7180.993830	8.945447	-0.066204	4.568378
330.755312	7189.096456	8.950451	-0.066209	4.570920
331.024905	7197.005700	8.955456	-0.066264	4.573401
331.163110	7205.125437	8.960461	-0.066295	4.575945
331.253445	7213.059593	8.965466	-0.066317	4.578430
331.677613	7221.116917	8.970471	-0.066402	4.580953
331.465711	7229.062568	8.975475	-0.066367	4.583439
331.649905	7237.164164	8.980480	-0.066407	4.585972
332.029947	7245.171390	8.985485	-0.066483	4.588475
331.824978	7253.187016	8.990490	-0.066450	4.590978
332.191623	7261.167234	8.995495	-0.066524	4.593470
332.474715	7269.246404	9.000499	-0.066582	4.595991
332.531140	7277.175876	9.005504	-0.066597	4.598464
332.605335	7285.267896	9.010509	-0.066616	4.600986
332.630739	7293.153036	9.015514	-0.066626	4.603442
332.882442	7301.248204	9.020519	-0.066678	4.605962
333.098669	7309.269750	9.025523	-0.066724	4.608458
333.197224	7317.288098	9.030528	-0.066747	4.610952
333.114110	7325.346574	9.035533	-0.066737	4.613456
333.067502	7333.357019	9.040538	-0.066734	4.615944
333.448606	7341.330357	9.045543	-0.066810	4.618420
333.742995	7349.355655	9.050547	-0.066870	4.620911
333.740701	7357.287427	9.055552	-0.066875	4.623370
333.919737	7365.403379	9.060557	-0.066913	4.625886
334.281829	7373.374269	9.065562	-0.066986	4.628356
334.284112	7381.458132	9.070567	-0.066992	4.630859
334.234653	7389.407197	9.075571	-0.066988	4.633318
334.472937	7397.421661	9.080576	-0.067037	4.635797
334.776810	7405.417201	9.085581	-0.067099	4.638269
334.691245	7413.449872	9.090586	-0.067088	4.640751
334.555543	7421.443372	9.095591	-0.067068	4.643219
335.032970	7429.479146	9.100595	-0.067162	4.645699
334.792890	7437.466061	9.105600	-0.067123	4.648163
334.886162	7445.586706	9.110605	-0.067146	4.650666
335.142646	7453.506024	9.115610	-0.067198	4.653106
335.341717	7461.593871	9.120615	-0.067241	4.655597
335.377041	7469.571431	9.125619	-0.067253	4.658052
335.403852	7477.600927	9.130624	-0.067263	4.660523
335.783184	7485.579100	9.135629	-0.067339	4.662976
335.804735	7493.607025	9.140634	-0.067348	4.665443
335.724738	7501.643167	9.145639	-0.067338	4.667911
336.061006	7509.687142	9.150643	-0.067406	4.670380
336.077167	7517.727902	9.155648	-0.067414	4.672847
336.393504	7525.755109	9.160653	-0.067479	4.675308
336.289528	7533.673797	9.165658	-0.067464	4.677735
336.487127	7541.710354	9.170663	-0.067506	4.680197
336.555581	7549.661173	9.175667	-0.067524	4.682631
336.846719	7557.732036	9.180672	-0.067584	4.685101
336.909982	7565.758677	9.185677	-0.067601	4.687556
336.767843	7573.779772	9.190682	-0.067580	4.690008
336.820319	7581.804593	9.195687	-0.067595	4.692459
337.109711	7589.783281	9.200691	-0.067654	4.694895
337.077491	7597.836743	9.205696	-0.067653	4.697353
337.297365	7605.849272	9.210701	-0.067699	4.699797
337.491829	7613.853676	9.215706	-0.067740	4.702238
337.474986	7621.832770	9.220711	-0.067743	4.704669
337.509779	7629.902342	9.225715	-0.067754	4.707127
337.660011	7637.856636	9.230720	-0.067787	4.709548
338.053980	7645.979419	9.235725	-0.067866	4.712018
337.695633	7653.916089	9.240730	-0.067805	4.714432
337.538894	7661.999500	9.245735	-0.067781	4.716889
337.739767	7669.909035	9.250739	-0.067823	4.719292
337.831570	7678.045290	9.255744	-0.067846	4.721762
338.428946	7685.927294	9.260749	-0.067962	4.724153
338.450315	7693.999638	9.265754	-0.067971	4.726601
338.599225	7702.032651	9.270759	-0.068004	4.729036
338.747154	7710.128614	9.275763	-0.068037	4.731488
338.833610	7718.070672	9.280768	-0.068058	4.733893
338.901302	7726.164227	9.285773	-0.068076	4.736343
338.780244	7734.083174	9.290778	-0.068059	4.738739
339.107438	7742.144511	9.295783	-0.068125	4.741175
339.018067	7750.142046	9.300787	-0.068114	4.743592
339.535985	7758.151201	9.305792	-0.068215	4.746010
339.622821	7766.201736	9.310797	-0.068237	4.748441
339.715502	7774.214049	9.315802	-0.068259	4.750858
340.096963	7782.250383	9.320807	-0.068335	4.753281
340.010810	7790.278879	9.325811	-0.068325	4.755701
339.835837	7798.212228	9.330816	-0.068297	4.758091
340.214945	7806.224750	9.335821	-0.068373	4.760503
340.340995	7814.239284	9.340826	-0.068402	4.762915
340.134994	7822.302730	9.345831	-0.068369	4.765341
340.570333	7830.327239	9.350835	-0.068455	4.767752
340.735581	7838.332689	9.355840	-0.068491	4.770158
340.882640	7846.362873	9.360845	-0.068524	4.772569
340.939722	7854.351579	9.365850	-0.068539	4.774967
341.120152	7862.361163	9.370855	-0.068578	4.777370
341.328987	7870.413671	9.375859	-0.068622	4.779784
341.193721	7878.439714	9.380864	-0.068602	4.782190
341.483816	7886.441897	9.385869	-0.068662	4.784587
341.390986	7894.461855	9.390874	-0.068650	4.786988
341.500176	7902.480703	9.395879	-0.068675	4.789388
341.774898	7910.488751	9.400883	-0.068731	4.791782
341.980047	7918.479245	9.405888	-0.068775	4.794171
342.134198	7926.526521	9.410893	-0.068809	4.796575
342.196889	7934.447192	9.415898	-0.068826	4.798941
342.407479	7942.552427	9.420903	-0.068870	4.801360
342.319951	7950.502312	9.425907	-0.068859	4.803732
342.435953	7958.550734	9.430912	-0.068886	4.806132
342.665657	7966.614072	9.435917	-0.068934	4.808535
342.725626	7974.631183	9.440922	-0.068950	4.810923
342.810834	7982.585517	9.445927	-0.068971	4.813291
343.104247	7990.051304	9.450931	-0.069031	4.815512
343.073023	7994.594415	9.455936	-0.069028	4.816864

343.274809	7997.175797	9.460941	-0.069067	4.817631
343.170352	7998.420379	9.465946	-0.069049	4.818002
343.401709	7998.892663	9.470951	-0.069092	4.818141
343.272608	7999.850451	9.475955	-0.069069	4.818427
343.310074	7999.768013	9.480960	-0.069076	4.818402
343.677637	7999.821167	9.485965	-0.069144	4.818416
343.850136	7999.759412	9.490970	-0.069176	4.818397
343.930826	7999.767829	9.495975	-0.069191	4.818399
343.896730	7999.809370	9.500979	-0.069185	4.818412
344.045988	7999.800848	9.505984	-0.069213	4.818409
344.236902	7999.829621	9.510989	-0.069248	4.818417
343.955597	7999.774457	9.515994	-0.069196	4.818401
343.943004	7999.802635	9.520999	-0.069193	4.818410
344.032875	7999.867864	9.526003	-0.069210	4.818429
343.811672	7999.849189	9.531008	-0.069169	4.818424
343.920371	7999.931465	9.536013	-0.069189	4.818448
344.042161	7999.829145	9.541018	-0.069212	4.818417
343.568190	7999.872213	9.546023	-0.069124	4.818432
343.988518	7999.872528	9.551027	-0.069202	4.818430
344.405430	7999.785662	9.556032	-0.069280	4.818403
344.357146	7999.809169	9.561037	-0.069271	4.818410
343.980058	7999.844072	9.566042	-0.069200	4.818422
344.158967	7999.829643	9.571047	-0.069234	4.818417
344.690208	7999.803081	9.576051	-0.069333	4.818407
344.416282	7999.847747	9.581056	-0.069282	4.818421
344.579913	7999.871961	9.586061	-0.069312	4.818428
344.464524	7999.801144	9.591066	-0.069291	4.818407
344.581533	7999.784846	9.596071	-0.069312	4.818402
344.684657	7999.873349	9.601075	-0.069332	4.818428
344.374285	7999.836695	9.606080	-0.069274	4.818418
344.778940	7999.846252	9.611085	-0.069349	4.818419
344.532809	7999.891286	9.616090	-0.069303	4.818434
344.561327	7999.865418	9.621095	-0.069309	4.818426
344.479920	7999.913683	9.626099	-0.069294	4.818441
344.368384	7999.879661	9.631104	-0.069273	4.818431
344.674574	7999.862719	9.636109	-0.069330	4.818425
345.058441	7999.785914	9.641114	-0.069401	4.818400
344.805411	7999.915894	9.646119	-0.069354	4.818440
344.826535	7999.899377	9.651123	-0.069358	4.818435
345.128658	7999.846687	9.656128	-0.069414	4.818418
345.130097	7999.900248	9.661133	-0.069415	4.818434
344.819907	7999.894041	9.666138	-0.069357	4.818433
344.876165	7999.876939	9.671143	-0.069367	4.818428
345.089068	7999.880809	9.676147	-0.069407	4.818428
344.771640	7999.883954	9.681152	-0.069348	4.818431
344.817318	7999.925503	9.686157	-0.069357	4.818443
344.922246	7999.895398	9.691162	-0.069376	4.818433
345.086401	7999.912270	9.696167	-0.069407	4.818438
345.044586	7999.861324	9.701171	-0.069399	4.818423
345.018114	7999.805332	9.706176	-0.069394	4.818406
345.449729	7999.859342	9.711181	-0.069474	4.818421
345.361304	7999.846622	9.716186	-0.069458	4.818417
345.301860	7999.810140	9.721191	-0.069447	4.818407
345.295544	7999.908743	9.726195	-0.069446	4.818436
345.235136	7999.855451	9.731200	-0.069434	4.818420
345.427157	7999.927285	9.736205	-0.069470	4.818441
345.726056	7999.852505	9.741210	-0.069526	4.818418
345.483709	7999.849295	9.746215	-0.069481	4.818418
345.488033	7999.946990	9.751219	-0.069481	4.818447
345.468067	7999.903681	9.756224	-0.069478	4.818434
345.694763	7999.888837	9.761229	-0.069520	4.818428
345.725220	7999.862994	9.766234	-0.069526	4.818421
345.522381	7999.844560	9.771239	-0.069488	4.818416
345.636217	7999.889112	9.776243	-0.069509	4.818429
345.440453	7999.840326	9.781248	-0.069473	4.818415
345.604431	7999.840398	9.786253	-0.069503	4.818414
345.424267	7999.870558	9.791258	-0.069470	4.818424
345.674438	7999.825578	9.796263	-0.069516	4.818410
345.882435	7999.838833	9.801267	-0.069555	4.818413
345.723941	7999.830434	9.806272	-0.069525	4.818411
345.847784	7999.882469	9.811277	-0.069548	4.818426
345.741864	7999.815974	9.816282	-0.069529	4.818407
345.691060	7999.833149	9.821287	-0.069519	4.818412
345.553702	7999.923718	9.826291	-0.069494	4.818439
345.758685	7999.847694	9.831296	-0.069532	4.818416
345.794536	7999.845020	9.836301	-0.069539	4.818415
345.552637	7999.938403	9.841306	-0.069494	4.818444
345.524264	7999.939077	9.846311	-0.069488	4.818444
345.640422	7999.889173	9.851315	-0.069510	4.818429
345.559600	7999.852407	9.856320	-0.069495	4.818418
345.690757	7999.910838	9.861325	-0.069519	4.818435
345.497564	7999.920877	9.866330	-0.069483	4.818439
345.793889	7999.855512	9.871335	-0.069538	4.818418
345.869857	7999.880666	9.876339	-0.069553	4.818425
345.816774	7999.897810	9.881344	-0.069543	4.818431
345.557584	7999.976266	9.886349	-0.069495	4.818455
345.564150	7999.897614	9.891354	-0.069496	4.818432
345.763537	7999.878208	9.896359	-0.069533	4.818425
345.837553	7999.914885	9.901363	-0.069547	4.818436
345.960738	7999.855625	9.906368	-0.069570	4.818418
346.186421	7999.913209	9.911373	-0.069612	4.818434
346.068677	7999.886452	9.916378	-0.069590	4.818426
345.970694	7999.925049	9.921383	-0.069571	4.818438
345.428234	7999.999752	9.926387	-0.069471	4.818462
345.946142	7999.815538	9.931392	-0.069567	4.818406
346.117476	7999.861903	9.936397	-0.069599	4.818419
346.030720	7999.836607	9.941402	-0.069583	4.818412
346.035094	7999.845064	9.946407	-0.069583	4.818414
345.812079	7999.932398	9.951411	-0.069542	4.818441
345.832952	7999.852885	9.956416	-0.069546	4.818417
345.843121	7999.942259	9.961421	-0.069548	4.818444
346.187502	7999.807190	9.966426	-0.069612	4.818402
345.723091	7999.873478	9.971431	-0.069525	4.818424
346.047709	7999.875679	9.976435	-0.069586	4.818423
346.128480	7999.853653	9.981440	-0.069601	4.818416
346.023552	7999.855412	9.986445	-0.069581	4.818417
346.119984	7999.887137	9.991450	-0.069599	4.818426
346.128368	7999.857852	9.996455	-0.069601	4.818418
346.391733	7999.898088	10.001459	-0.069650	4.818428
345.998331	7999.863478	10.006464	-0.069577	4.818420
346.201723	7999.845176	10.011469	-0.069615	4.818413
346.383513	7999.823438	10.016474	-0.069648	4.818406
346.470992	7999.830897	10.021479	-0.069665	4.818408
346.318945	7999.859329	10.026483	-0.069636	4.818417
346.380691	7999.808704	10.031488	-0.069648	4.818402
346.574040	7999.875309	10.036493	-0.069684	4.818421
346.275686	7999.840909	10.041498	-0.069628	4.818412
346.316689	7999.885548	10.046503	-0.069636	4.818425
346.102531	7999.942553	10.051507	-0.069596	4.818443
345.924231	7999.926542	10.056512	-0.069563	4.818439
345.834052	7999.980991	10.061517	-0.069546	4.818455
345.771781	7999.928722	10.066522	-0.069535	4.818440
346.108318	7999.856541	10.071527	-0.069597	4.818417
346.453167	7999.902057	10.076531	-0.069661	4.818429
346.220805	7999.897927	10.081536	-0.069618	4.818429
346.095772	7999.887872	10.086541	-0.069595	4.818427
345.985712	7999.873815	10.091546	-0.069574	4.818423
345.841357	7999.920197	10.096551	-0.069548	4.818437
346.304936	7999.875946	10.101555	-0.069634	4.818422
346.329954	7999.817485	10.106560	-0.069638	4.818405
346.341426	7999.871181	10.111565	-0.069641	4.818421
346.594607	7999.834641	10.116570	-0.069688	4.818409
346.539127	7999.818158	10.121575	-0.069677	4.818404
346.654478	7999.811288	10.126579	-0.069699	4.818402
346.542242	7999.827649	10.131584	-0.069678	4.818407
346.659910	7999.862805	10.136589	-0.069700	4.818417
346.636062	7999.865639	10.141594	-0.069696	4.818418
346.587541	7999.829300	10.146599	-0.069686	4.818407
346.241786	7999.924457	10.151603	-0.069622	4.818437
345.959530	7999.923866	10.156608	-0.069570	4.818438
346.157997	7999.965342	10.161613	-0.069607	4.818449
346.281469	7999.891388	10.166618	-0.069630	4.818427
346.577026	7999.873258	10.171623	-0.069685	4.818420
346.623978	7999.932674	10.176627	-0.069693	4.818438
346.655677	7999.843854	10.181632	-0.069699	4.818411
346.617778	7999.879048	10.186637	-0.069692	4.818422
346.185176	7999.869115	10.191642	-0.069612	4.818421
346.247694	7999.949735	10.196647	-0.069623	4.818444
346.950855	7999.868766	10.201651	-0.069754	4.818418
346.856318	7999.828667	10.206656	-0.069737	4.818406
346.832411	7999.840949	10.211661	-0.069732	4.818410
346.424308	7999.912182	10.216666	-0.069656	4.818433
346.578342	7999.849131	10.221671	-0.069685	4.818413
346.630639	7999.870822	10.226675	-0.069695	4.818419
346.268382	7999.882819	10.231680	-0.069627	4.818424
346.521056	7999.900867	10.236685	-0.069674	4.818429
346.592029	7999.871361	10.241690	-0.069687	4.818420
346.643736	7999.859448	10.246695	-0.069697	4.818416
346.522940	7999.911391	10.251699	-0.069675	4.818432
346.295741	7999.884233	10.256704	-0.069632	4.818425
346.548643	7999.882336	10.261709	-0.069679	4.818423
346.567571	7999.886787	10.266714	-0.069683	4.818424
346.698290	7999.890619	10.271719	-0.069707	4.818425
346.826172	7999.956359	10.276723	-0.069731	4.818444
346.671613	7999.856670	10.281728	-0.069702	4.818415
346.888428	7999.873193	10.286733	-0.069743	4.818419
346.509657	7999.857674	10.291738	-0.069672	4.818416
346.376135	7999.945145	10.296743	-0.069647	4.818443
346.221605	8000.016589	10.301747	-0.069619	4.818464
346.323541	7999.958097	10.306752	-0.069638	4.818447
346.491743	7999.941429	10.311757	-0.069669	4.818441
346.392875	7999.910722	10.316762	-0.069650	4.818432
346.598347	7999.874599	10.321767	-0.069689	4.818421
346.528694	7999.977616	10.326771	-0.069676	4.818452
346.285006	7999.893545	10.331776	-0.069630	4.818428
346.321064	7999.959116	10.336781	-0.069637	4.818447
346.595024	7999.891355	10.341786	-0.069688	4.818426
346.387426	7999.892803	10.346791	-0.069649	4.818427
346.941136	7999.868646	10.351795	-0.069753	4.818418
346.691455	7999.880035	10.356800	-0.069706	4.818422
346.857509	7999.863339	10.361805	-0.069737	4.818416
347.072782	7999.945985	10.366810	-0.069777	4.818440
347.342848	7999.845626	10.371815	-0.069827	4.818409
346.945989	7999.878161	10.376819	-0.069753	4.818420
346.635373	7999.941237	10.381824	-0.069696	4.818440
346.546611	7999.979957	10.386829	-0.069679	4.818452
346.729708	7999.966636	10.391834	-0.069713	4.818448
346.610452	7999.937758	10.396839	-0.069691	4.818439
346.639443	7999.979088	10.401843	-0.069696	4.818452
346.810914	7999.888971	10.406848	-0.069728	4.818424
346.787379	7999.922256	10.411853	-0.069724	4.818434
346.602126	7999.961796	10.416858	-0.069690	4.818447
346.934868	7999.888516	10.421863	-0.069751	4.818423
346.847397	7999.970298	10.426867	-0.069735	4.818448
346.768531	7999.913608	10.431872	-0.069720	4.818432
347.070716	7999.895567	10.436877	-0.069777	4.818425
346.893111	7999.853317	10.441882	-0.069744	4.818413
347.268620	7999.814199	10.446887	-0.069814	4.818400
346.965010	7999.934063	10.451891	-0.069757	4.818437
346.924903	7999.844290	10.456896	-0.069750	4.818410
346.671816	7999.967973	10.461901	-0.069703	4.818448
347.068326	7999.909186	10.466906	-0.069776	4.818429
346.560233	7999.970694	10.471911	-0.069682	4.818449
346.770712	7999.993432	10.476915	-0.069721	4.818455
346.691716	7999.884246	10.481920	-0.069706	4.818423
346.076330	8000.068219	10.486925	-0.069592	4.818480
346.241340	8000.050459	10.491930	-0.069622	4.818474
346.994700	7999.938659	10.496935	-0.069763	4.818438
346.814159	7999.986661	10.501939	-0.069729	4.818453
347.084120	7999.946144	10.506944	-0.069779	4.818440
347.219935	7999.923798	10.511949	-0.069805	4.818433
347.046559	7999.893152	10.516954	-0.069772	4.818424
347.105564	7999.877136	10.521959	-0.069783	4.818419
346.848787	8000.007069	10.526963	-0.069736	4.818459
346.917144	7999.864140	10.531968	-0.069748	4.818416
347.153593	7999.847327	10.536973	-0.069792	4.818410
347.203667	7999.927784	10.541978	-0.069802	4.818434
347.315769	7999.891474	10.546983	-0.069822	4.818423
347.228834	7999.887172	10.551987	-0.069806	4.818422
347.317028	7999.899890	10.556992	-0.069823	4.818425
347.363126	7999.896302	10.561997	-0.069831	4.818424
347.066105	7999.877666	10.567002	-0.069776	4.818420
347.154325	7999.890385	10.572007	-0.069792	4.818423
347.621923	7999.880837	10.577011	-0.069879	4.818418
347.563992	7999.808675	10.582016	-0.069869	4.818397
347.664174	7999.846751	10.587021	-0.069887	4.818408
347.548101	7999.784317	10.592026	-0.069866	4.818390
347.568075	7999.811880	10.597031	-0.069869	4.818398
347.673379	7999.876271	10.602035	-0.069889	4.818417
347.752522	7999.802777	10.607040	-0.069904	4.818395
347.620803	7999.816779	10.612045	-0.069879	4.818399
347.694695	7999.798861	10.617050	-0.069893	4.818394
347.795712	7999.823299	10.622055	-0.069912	4.818401
347.867077	7999.846294	10.627059	-0.069925	4.818407
347.630558	7999.794862	10.632064	-0.069881	4.818393
347.650877	7999.843428	10.637069	-0.069885	4.818407
347.668348	7999.822661	10.642074	-0.069888	4.818401
347.667295	7999.817398	10.647079	-0.069888	4.818399
347.720719	7999.891601	10.652083	-0.069898	4.818421
347.584642	7999.833101	10.657088	-0.069873	4.818404
347.710132	7999.878862	10.662093	-0.069896	4.818418
347.639841	7999.834884	10.667098	-0.069883	4.818405
347.635838	7999.811733	10.672103	-0.069882	4.818398
347.737516	7999.826730	10.677107	-0.069901	4.818402
347.385118	7999.806309	10.682112	-0.069835	4.818397
347.507416	7999.873026	10.687117	-0.069858	4.818417
347.529741	7999.850224	10.692122	-0.069862	4.818410
347.550558	7999.824253	10.697127	-0.069866	4.818402
347.645573	7999.871709	10.702131	-0.069884	4.818416
347.546700	7999.812653	10.707136	-0.069866	4.818398
347.786183	7999.834727	10.712141	-0.069910	4.818404
347.798967	7999.790801	10.717146	-0.069913	4.818391
347.556170	7999.826428	10.722151	-0.069867	4.818403
347.718962	7999.835937	10.727155	-0.069898	4.818405
347.634820	7999.842171	10.732160	-0.069882	4.818407
347.670246	7999.870988	10.737165	-0.069889	4.818415
347.716334	7999.825404	10.742170	-0.069897	4.818402
347.712351	7999.819052	10.747175	-0.069896	4.818400
347.723226	7999.833895	10.752179	-0.069898	4.818404
347.693669	7999.798856	10.757184	-0.069893	4.818394
347.797858	7999.807588	10.762189	-0.069912	4.818396
347.655748	7999.803604	10.767194	-0.069886	4.818395
347.776511	7999.792606	10.772199	-0.069908	4.818392
347.819899	7999.829929	10.777203	-0.069916	4.818403
347.509889	7999.839467	10.782208	-0.069859	4.818407
347.783781	7999.813702	10.787213	-0.069910	4.818398
347.844069	7999.797703	10.792218	-0.069921	4.818393
347.879388	7999.834919	10.797223	-0.069928	4.818404
347.634368	7999.869467	10.802227	-0.069882	4.818415
347.648879	7999.803515	10.807232	-0.069885	4.818395
347.873599	7999.829594	10.812237	-0.069927	4.818402
347.883977	7999.806633	10.817242	-0.069928	4.818395
347.559494	7999.782383	10.822247	-0.069868	4.818389
347.950519	7999.793867	10.827251	-0.069941	4.818391
347.637090	7999.822259	10.832256	-0.069883	4.818401
347.439097	7999.856380	10.837261	-0.069846	4.818412
347.449403	7999.854418	10.842266	-0.069848	4.818411
347.342026	7999.844595	10.847271	-0.069828	4.818409
347.383907	7999.908145	10.852275	-0.069835	4.818428
347.265898	7999.934928	10.857280	-0.069813	4.818436
347.588933	7999.880417	10.862285	-0.069874	4.818418
347.534287	7999.857645	10.867290	-0.069863	4.818412
347.476131	7999.842175	10.872295	-0.069853	4.818408
347.888462	7999.806697	10.877299	-0.069929	4.818395
347.676153	7999.814381	10.882304	-0.069890	4.818398
347.552446	7999.882035	10.887309	-0.069867	4.818419
347.711519	7999.846348	10.892314	-0.069896	4.818408
347.620953	7999.816799	10.897319	-0.069880	4.818399
347.715618	7999.836953	10.902323	-0.069897	4.818405
347.607550	7999.785125	10.907328	-0.069877	4.818390
347.901989	7999.832076	10.912333	-0.069932	4.818403
347.648718	7999.895912	10.917338	-0.069885	4.818423
347.538960	7999.848261	10.922343	-0.069864	4.818409
347.784524	7999.929212	10.927347	-0.069910	4.818432
347.490137	7999.906409	10.932352	-0.069855	4.818427
347.421598	7999.863504	10.937357	-0.069842	4.818414
347.770448	7999.851332	10.942362	-0.069907	4.818409
347.916076	7999.839615	10.947367	-0.069935	4.818405
347.556513	7999.919889	10.952371	-0.069868	4.818430
347.536281	7999.870276	10.957376	-0.069864	4.818416
347.781442	7999.842030	10.962381	-0.069910	4.818406
347.874685	7999.811769	10.967386	-0.069927	4.818397
347.762561	7999.811332	10.972391	-0.069906	4.818397
347.634610	7999.938775	10.977395	-0.069882	4.818436
347.522873	7999.864850	10.982400	-0.069861	4.818414
347.955130	7999.840135	10.987405	-0.069942	4.818405
347.851414	7999.832460	10.992410	-0.069923	4.818403
347.658902	7999.887653	10.997415	-0.069887	4.818420
347.418063	7999.932755	11.002419	-0.069842	4.818435
347.535338	7999.862917	11.007424	-0.069864	4.818413
347.593730	7999.917237	11.012429	-0.069875	4.818429
347.493962	7999.911715	11.017434	-0.069856	4.818428
347.505999	7999.886677	11.022439	-0.069858	4.818421
347.619149	7999.917575	11.027443	-0.069879	4.818429
347.706149	7999.874633	11.032448	-0.069896	4.818416
347.765163	7999.878565	11.037453	-0.069907	4.818417
347.799140	7999.887416	11.042458	-0.069913	4.818420
347.895957	7999.854053	11.047463	-0.069931	4.818409
347.915577	7999.907859	11.052467	-0.069935	4.818425
347.766645	7999.892235	11.057472	-0.069907	4.818421
347.739224	7999.905521	11.062477	-0.069902	4.818425
347.899102	7999.879294	11.067482	-0.069932	4.818417
347.824222	7999.828955	11.072487	-0.069918	4.818402
347.898253	7999.921280	11.077491	-0.069931	4.818429
348.031538	7999.850604	11.082496	-0.069956	4.818408
348.215969	7999.860400	11.087501	-0.069991	4.818410
347.973570	7999.864534	11.092506	-0.069945	4.818412
347.646791	7999.874900	11.097511	-0.069885	4.818417
347.654710	7999.896003	11.102515	-0.069886	4.818423
347.034763	8000.028470	11.107520	-0.069771	4.818465
347.189482	8000.031572	11.112525	-0.069800	4.818465
347.520134	7999.979263	11.117530	-0.069861	4.818448
347.572228	7999.939007	11.122535	-0.069871	4.818436
347.835111	7999.989741	11.127539	-0.069920	4.818450
347.686231	7999.981467	11.132544	-0.069892	4.818448
347.542540	7999.942814	11.137549	-0.069865	4.818437
347.325604	8000.044929	11.142554	-0.069825	4.818468
347.562942	7999.938885	11.147559	-0.069869	4.818436
347.908920	7999.908827	11.152563	-0.069933	4.818426
347.862670	7999.859918	11.157568	-0.069925	4.818411
347.733201	7999.949544	11.162573	-0.069901	4.818438
347.663725	8000.002169	11.167578	-0.069888	4.818454
347.693121	7999.882868	11.172583	-0.069893	4.818419
347.797433	7999.953547	11.177587	-0.069913	4.818439
347.790400	7999.890458	11.182592	-0.069911	4.818421
347.976694	7999.899229	11.187597	-0.069946	4.818423
347.919757	7999.917373	11.192602	-0.069936	4.818428
347.321123	7999.926232	11.197607	-0.069824	4.818433
347.576023	7999.974760	11.202611	-0.069872	4.818447
346.848279	8000.052251	11.207616	-0.069736	4.818472
347.089341	8000.072247	11.212621	-0.069781	4.818477
347.319651	8000.042754	11.217626	-0.069824	4.818468
346.848061	8000.041750	11.222631	-0.069736	4.818469
347.482303	7999.980867	11.227635	-0.069854	4.818449
347.462256	7999.960653	11.232640	-0.069850	4.818443
347.262188	8000.018895	11.237645	-0.069813	4.818461
347.128935	7999.984581	11.242650	-0.069788	4.818451
347.528174	7999.932131	11.247655	-0.069863	4.818434
347.395554	8000.023815	11.252659	-0.069838	4.818462
346.977753	8000.006725	11.257664	-0.069760	4.818458
347.321203	7999.995532	11.262669	-0.069824	4.818454
347.255045	8000.028252	11.267674	-0.069812	4.818464
347.559799	7999.927302	11.272679	-0.069869	4.818433
347.715998	7999.949323	11.277683	-0.069898	4.818438
347.667184	7999.899330	11.282688	-0.069889	4.818424
347.754621	7999.941436	11.287693	-0.069905	4.818436
347.336820	7999.984192	11.292698	-0.069827	4.818450
347.362025	7999.939380	11.297703	-0.069832	4.818437
347.203297	8000.012869	11.302707	-0.069802	4.818459
347.197794	7999.954001	11.307712	-0.069801	4.818442
347.451551	7999.932169	11.312717	-0.069848	4.818434
347.748297	7999.948704	11.317722	-0.069904	4.818438
347.643162	7999.934711	11.322727	-0.069884	4.818434
347.078562	8000.115158	11.327731	-0.069779	4.818490
347.305709	8000.008979	11.332736	-0.069821	4.818458
347.459110	8000.006815	11.337741	-0.069850	4.818457
347.263484	7999.993721	11.342746	-0.069813	4.818453
346.850570	8000.032342	11.347751	-0.069737	4.818467
346.896464	8000.109594	11.352755	-0.069745	4.818489
347.624655	7999.920819	11.357760	-0.069881	4.818430
347.593102	7999.939299	11.362765	-0.069875	4.818436
347.702297	7999.924999	11.367770	-0.069895	4.818431
347.595631	7999.899436	11.372775	-0.069875	4.818424
347.381563	7999.967992	11.377779	-0.069835	4.818445
347.629295	7999.938730	11.382784	-0.069882	4.818436
347.886007	7999.888590	11.387789	-0.069929	4.818420
347.654882	7999.920172	11.392794	-0.069886	4.818430
347.758339	7999.831251	11.397799	-0.069906	4.818403
347.950343	7999.937740	11.402803	-0.069941	4.818434
347.668059	7999.967594	11.407808	-0.069889	4.818444
347.628688	7999.981771	11.412813	-0.069882	4.818448
347.580079	7999.955928	11.417818	-0.069872	4.818441
347.417447	7999.976870	11.422823	-0.069842	4.818448
347.566286	7999.968345	11.427827	-0.069870	4.818445
347.632636	7999.919879	11.432832	-0.069882	4.818430
347.735971	7999.985295	11.437837	-0.069902	4.818449
347.252095	7999.991477	11.442842	-0.069811	4.818453
346.910841	8000.020549	11.447847	-0.069748	4.818463
347.562879	7999.965152	11.452851	-0.069869	4.818444
347.226031	8000.022629	11.457856	-0.069807	4.818462
347.549224	7999.968121	11.462861	-0.069867	4.818445
347.418582	7999.973738	11.467866	-0.069842	4.818447
347.523825	7999.905840	11.472871	-0.069862	4.818426
347.948394	7999.914621	11.477875	-0.069941	4.818427
347.689828	7999.919591	11.482880	-0.069893	4.818430
347.721465	7999.915811	11.487885	-0.069899	4.818428
347.949679	7999.938787	11.492890	-0.069941	4.818434
347.700499	7999.934432	11.497895	-0.069895	4.818434
348.142202	7999.927693	11.502899	-0.069977	4.818430
347.874580	7999.885296	11.507904	-0.069927	4.818419
347.595060	7999.948783	11.512909	-0.069875	4.818439
347.598738	7999.954082	11.517914	-0.069876	4.818440
347.483429	8000.010299	11.522919	-0.069855	4.818458
347.271807	8000.053688	11.527923	-0.069815	4.818471
346.637984	8000.093579	11.532928	-0.069697	4.818486
347.284554	8000.043359	11.537933	-0.069818	4.818468
347.274736	8000.034830	11.542938	-0.069816	4.818466
347.420071	7999.956964	11.547943	-0.069843	4.818442
347.180535	8000.064028	11.552947	-0.069798	4.818475
347.243551	8000.032317	11.557952	-0.069810	4.818465
347.030636	8000.003246	11.562957	-0.069770	4.818457
347.176096	8000.002026	11.567962	-0.069797	4.818456
347.488087	7999.877024	11.572967	-0.069855	4.818418
347.718292	7999.892676	11.577971	-0.069898	4.818422
347.555031	7999.906260	11.582976	-0.069868	4.818426
347.292981	8000.030875	11.587981	-0.069819	4.818464
347.730627	7999.941137	11.592986	-0.069901	4.818436
347.656365	7999.834111	11.597991	-0.069887	4.818404
347.514656	7999.947723	11.602995	-0.069860	4.818439
347.399090	7999.912593	11.608000	-0.069839	4.818429
347.452891	7999.991001	11.613005	-0.069849	4.818452
347.263161	8000.007383	11.618010	-0.069814	4.818458
347.372557	7999.920642	11.623015	-0.069834	4.818431
347.626607	7999.972307	11.628019	-0.069881	4.818446
347.869437	7999.898884	11.633024	-0.069927	4.818423
347.747789	7999.917220	11.638029	-0.069904	4.818429
347.791603	8000.004945	11.643034	-0.069912	4.818455
347.774547	7999.938574	11.648039	-0.069909	4.818435
347.576389	8000.019939	11.653043	-0.069872	4.818460
347.540314	8000.013161	11.658048	-0.069865	4.818458
347.598847	7999.997139	11.663053	-0.069876	4.818453
347.922760	7999.916392	11.668058	-0.069936	4.818428
347.983985	7999.902506	11.673063	-0.069948	4.818423
347.789012	7999.987064	11.678067	-0.069912	4.818449
347.591907	7999.977100	11.683072	-0.069875	4.818447
347.778361	7999.970124	11.688077	-0.069910	4.818444
347.840442	8000.010845	11.693082	-0.069921	4.818456
347.821831	7999.909806	11.698087	-0.069918	4.818426
347.686215	7999.974153	11.703091	-0.069893	4.818446
347.793230	7999.931476	11.708096	-0.069912	4.818433
347.834379	7999.904724	11.713101	-0.069920	4.818425
348.102060	7999.901975	11.718106	-0.069970	4.818423
348.058599	7999.864652	11.723111	-0.069962	4.818412
348.278882	7999.863374	11.728115	-0.070003	4.818411
347.910414	7999.853238	11.733120	-0.069934	4.818409
347.618512	7999.996355	11.738125	-0.069880	4.818453
347.740224	8000.021068	11.743130	-0.069903	4.818460
347.836104	7999.963545	11.748135	-0.069920	4.818442
347.834441	7999.960373	11.753139	-0.069920	4.818441
347.828180	7999.976039	11.758144	-0.069919	4.818446
347.699775	8000.023683	11.763149	-0.069895	4.818461
347.933559	7999.937540	11.768154	-0.069939	4.818434
347.830005	7999.943517	11.773159	-0.069919	4.818436
347.710876	8000.028030	11.778163	-0.069897	4.818462
347.873774	7999.887402	11.783168	-0.069927	4.818419
347.902200	7999.940276	11.788173	-0.069933	4.818435
347.775755	8000.026792	11.793178	-0.069909	4.818461
347.581723	8000.022119	11.798183	-0.069873	4.818461
347.736143	8000.035717	11.803187	-0.069902	4.818464
347.679723	8000.003471	11.808192	-0.069891	4.818455
347.834694	7999.971929	11.813197	-0.069920	4.818445
347.602836	8000.010851	11.818202	-0.069877	4.818457
347.646076	8000.022974	11.823207	-0.069885	4.818461
347.683942	8000.043425	11.828211	-0.069892	4.818467
347.581254	8000.004266	11.833216	-0.069873	4.818455
347.454578	7999.992087	11.838221	-0.069850	4.818452
347.511957	8000.021196	11.843226	-0.069860	4.818461
347.756379	7999.957244	11.848231	-0.069906	4.818441
347.932889	7999.946986	11.853235	-0.069939	4.818437
348.050318	7999.997891	11.858240	-0.069960	4.818452
348.156223	7999.927901	11.863245	-0.069980	4.818430
347.833421	8000.029662	11.868250	-0.069920	4.818462
348.109766	7999.924136	11.873255	-0.069971	4.818429
348.133030	7999.954893	11.878259	-0.069976	4.818438
348.038353	7999.962036	11.883264	-0.069958	4.818441
347.789578	7999.976585	11.888269	-0.069912	4.818446
347.925853	7999.964744	11.893274	-0.069937	4.818442
347.804317	7999.980981	11.898279	-0.069915	4.818448
347.815485	8000.009477	11.903283	-0.069917	4.818456
347.858786	7999.981704	11.908288	-0.069925	4.818448
347.599998	8000.020269	11.913293	-0.069877	4.818460
347.282550	8000.059105	11.918298	-0.069818	4.818473
347.537277	7999.984790	11.923303	-0.069865	4.818450
348.003663	7999.992027	11.928307	-0.069952	4.818450
347.840165	7999.968860	11.933312	-0.069921	4.818444
347.581702	8000.064124	11.938317	-0.069873	4.818473
347.495822	8000.057736	11.943322	-0.069857	4.818472
347.648760	8000.000969	11.948327	-0.069886	4.818454
347.944333	7999.933495	11.953331	-0.069941	4.818433
347.949876	7999.959817	11.958336	-0.069942	4.818441
347.904229	7999.970761	11.963341	-0.069933	4.818444
348.008985	7999.952203	11.968346	-0.069953	4.818438
347.783442	7999.960760	11.973351	-0.069911	4.818442
348.097518	7999.958627	11.978355	-0.069969	4.818440
347.957801	7999.914777	11.983360	-0.069943	4.818427
348.082374	7999.900681	11.988365	-0.069966	4.818423
348.039517	7999.945260	11.993370	-0.069959	4.818436
347.976699	7999.944427	11.998375	-0.069947	4.818436
347.753570	8000.011812	12.003379	-0.069905	4.818457
347.982335	7999.915104	12.008384	-0.069948	4.818427
348.165900	7999.910190	12.013389	-0.069982	4.818425
347.626999	8000.023783	12.018394	-0.069882	4.818461
347.512626	7999.984469	12.023399	-0.069860	4.818450
347.688366	8000.037197	12.028403	-0.069893	4.818465
347.327840	8000.033465	12.033408	-0.069826	4.818465
347.718795	8000.005053	12.038413	-0.069899	4.818455
347.796358	7999.986134	12.043418	-0.069913	4.818449
348.282804	7999.868696	12.048423	-0.070004	4.818412
348.278117	7999.921131	12.053427	-0.070003	4.818428
348.378071	7999.957105	12.058432	-0.070022	4.818438
348.532397	7999.907706	12.063437	-0.070050	4.818423
348.447537	7999.924429	12.068442	-0.070035	4.818428
348.253684	7999.898759	12.073447	-0.069998	4.818421
348.192836	7999.926300	12.078451	-0.069987	4.818430
348.294779	7999.865707	12.083456	-0.070006	4.818411
348.318695	7999.912222	12.088461	-0.070011	4.818425
348.246430	7999.953261	12.093466	-0.069997	4.818438
348.073930	7999.971971	12.098471	-0.069965	4.818444
348.114171	7999.972505	12.103475	-0.069973	4.818444
348.333891	7999.944973	12.108480	-0.070013	4.818435
348.550468	7999.939447	12.113485	-0.070054	4.818432
348.239765	8000.042418	12.118490	-0.069996	4.818464
348.069590	8000.032811	12.123495	-0.069964	4.818462
348.083683	8000.026699	12.128499	-0.069967	4.818460
347.930176	8000.045661	12.133504	-0.069938	4.818466
348.024197	7999.950315	12.138509	-0.069956	4.818438
347.956730	8000.050214	12.143514	-0.069943	4.818467
348.105445	7999.979742	12.148519	-0.069971	4.818446
347.881657	7999.980973	12.153523	-0.069929	4.818447
347.719638	7999.969375	12.158528	-0.069899	4.818444
347.579732	7999.957020	12.163533	-0.069873	4.818441
347.974874	7999.862519	12.168538	-0.069947	4.818412
347.761836	7999.876493	12.173543	-0.069907	4.818417
347.875962	7999.965150	12.178547	-0.069928	4.818443
347.527715	7999.948982	12.183552	-0.069863	4.818439
347.717011	7999.901097	12.188557	-0.069899	4.818424
347.648247	7999.982079	12.193562	-0.069886	4.818448
347.905511	7999.901498	12.198567	-0.069934	4.818423
348.063225	8000.022232	12.203571	-0.069963	4.818459
347.935372	7999.934442	12.208576	-0.069939	4.818433
348.088451	7999.912325	12.213581	-0.069968	4.818426
347.937710	7999.949173	12.218586	-0.069940	4.818438
347.758476	7999.953095	12.223591	-0.069906	4.818439
347.811149	8000.061937	12.228595	-0.069916	4.818472
348.276211	7999.961014	12.233600	-0.070003	4.818440
348.152491	7999.942574	12.238605	-0.069980	4.818435
348.029341	7999.993437	12.243610	-0.069957	4.818450
347.989844	7999.908919	12.248615	-0.069949	4.818425
348.257251	7999.954464	12.253619	-0.069999	4.818438
347.965799	7999.998895	12.258624	-0.069945	4.818452
347.953861	7999.967239	12.263629	-0.069943	4.818443
348.166910	8000.034112	12.268634	-0.069983	4.818462
348.087641	7999.980563	12.273639	-0.069968	4.818446
348.049310	7999.996854	12.278643	-0.069961	4.818451
348.179243	7999.933482	12.283648	-0.069985	4.818432
347.960285	7999.969425	12.288653	-0.069944	4.818443
348.098037	7999.984902	12.293658	-0.069970	4.818448
347.957985	7999.916899	12.298663	-0.069944	4.818428
348.051270	7999.949635	12.303667	-0.069961	4.818437
348.033832	7999.925255	12.308672	-0.069958	4.818430
348.311531	7999.874343	12.313677	-0.070009	4.818414
348.192820	7999.996661	12.318682	-0.069987	4.818451
347.881693	7999.906439	12.323687	-0.069929	4.818425
348.076201	7999.956267	12.328691	-0.069966	4.818439
348.174129	7999.912419	12.333696	-0.069984	4.818426
348.505044	7999.882162	12.338701	-0.070045	4.818415
348.526107	7999.965387	12.343706	-0.070049	4.818440
348.562303	7999.909171	12.348711	-0.070056	4.818423
348.569920	7999.949170	12.353715	-0.070058	4.818435
348.411756	7999.884075	12.358720	-0.070028	4.818416
348.265450	7999.859036	12.363725	-0.070001	4.818409
348.380749	7999.971859	12.368730	-0.070022	4.818443
348.097068	7999.929248	12.373735	-0.069970	4.818431
348.049755	7999.982167	12.378739	-0.069961	4.818447
348.268508	7999.991369	12.383744	-0.070002	4.818449
348.177273	7999.928213	12.388749	-0.069985	4.818430
348.282102	7999.993650	12.393754	-0.070004	4.818449
348.324627	7999.955367	12.398759	-0.070012	4.818438
348.193442	7999.944178	12.403763	-0.069988	4.818435
348.674628	7999.929564	12.408768	-0.070077	4.818429
348.628750	7999.901657	12.413773	-0.070069	4.818421
348.580939	7999.961919	12.418778	-0.070060	4.818439
348.555399	7999.887035	12.423783	-0.070055	4.818417
348.441501	7999.959020	12.428787	-0.070034	4.818438
348.676378	7999.874992	12.433792	-0.070077	4.818413
348.538061	7999.895205	12.438797	-0.070052	4.818419
348.209539	7999.976942	12.443802	-0.069991	4.818445
348.464156	7999.941473	12.448807	-0.070038	4.818433
348.544154	7999.953034	12.453811	-0.070053	4.818436
348.537889	7999.909904	12.458816	-0.070052	4.818423
348.426021	7999.888471	12.463821	-0.070031	4.818418
348.618684	7999.874228	12.468826	-0.070067	4.818413
348.682260	7999.891871	12.473831	-0.070079	4.818418
348.611471	7999.893032	12.478835	-0.070065	4.818418
348.734662	7999.862119	12.483840	-0.070088	4.818408
348.699049	7999.887895	12.488845	-0.070082	4.818416
348.717511	7999.965836	12.493850	-0.070085	4.818439
348.547346	7999.871184	12.498855	-0.070053	4.818412
348.918382	7999.934905	12.503859	-0.070123	4.818429
348.642737	7999.909198	12.508864	-0.070071	4.818423
348.577260	7999.882081	12.513869	-0.070059	4.818415
348.767665	7999.899307	12.518874	-0.070095	4.818419
348.763874	7999.867759	12.523879	-0.070094	4.818410
348.767255	7999.905602	12.528883	-0.070094	4.818421
348.661705	7999.897902	12.533888	-0.070075	4.818419
348.525555	7999.912895	12.538893	-0.070049	4.818424
348.393998	8000.007744	12.543898	-0.070025	4.818453
348.284386	7999.918095	12.548903	-0.070005	4.818427
348.577422	7999.976580	12.553907	-0.070059	4.818443
348.721497	7999.854599	12.558912	-0.070086	4.818406
348.703930	7999.866966	12.563917	-0.070083	4.818410
348.912587	7999.893884	12.568922	-0.070122	4.818417
349.019970	7999.873260	12.573927	-0.070142	4.818411
348.808629	7999.873606	12.578931	-0.070102	4.818412
348.858299	7999.837517	12.583936	-0.070111	4.818401
348.790646	7999.840820	12.588941	-0.070099	4.818402
348.703095	7999.855407	12.593946	-0.070083	4.818407
348.587886	7999.838130	12.598951	-0.070061	4.818402
348.629022	7999.957319	12.603955	-0.070069	4.818437
348.467914	7999.924734	12.608960	-0.070039	4.818428
348.779452	7999.869021	12.613965	-0.070097	4.818410
348.786285	7999.923709	12.618970	-0.070098	4.818427
348.385986	7999.950946	12.623975	-0.070024	4.818436
348.360112	8000.038798	12.628979	-0.070019	4.818462
348.250720	7999.998499	12.633984	-0.069998	4.818451
348.037034	8000.010363	12.638989	-0.069959	4.818455
348.451594	7999.951818	12.643994	-0.070036	4.818436
348.371390	7999.910856	12.648999	-0.070021	4.818424
348.504125	7999.952515	12.654003	-0.070046	4.818436
348.141555	8000.001252	12.659008	-0.069978	4.818452
348.023935	7999.976593	12.664013	-0.069956	4.818445
348.430367	8000.032383	12.669018	-0.070032	4.818460
348.366085	7999.963284	12.674023	-0.070020	4.818440
348.154405	7999.985674	12.679027	-0.069981	4.818448
348.324372	7999.951182	12.684032	-0.070012	4.818437
348.418891	7999.960836	12.689037	-0.070030	4.818439
348.534619	7999.981271	12.694042	-0.070051	4.818445
348.653895	7999.893609	12.699047	-0.070074	4.818418
348.752625	7999.987315	12.704051	-0.070092	4.818446
348.175003	8000.018497	12.709056	-0.069984	4.818457
348.540197	7999.962447	12.714061	-0.070052	4.818439
348.576112	7999.963974	12.719066	-0.070059	4.818439
348.683794	7999.873008	12.724071	-0.070079	4.818412
348.507443	7999.899017	12.729075	-0.070046	4.818420
348.360728	7999.983166	12.734080	-0.070019	4.818446
348.695052	7999.877358	12.739085	-0.070081	4.818413
348.663008	7999.886383	12.744090	-0.070075	4.818416
348.304531	7999.911025	12.749095	-0.070009	4.818425
348.428295	7999.941016	12.754099	-0.070032	4.818433
347.961565	8000.033517	12.759104	-0.069945	4.818462
347.855790	7999.955470	12.764109	-0.069925	4.818440
347.969617	8000.039925	12.769114	-0.069946	4.818464
347.986778	7999.972957	12.774119	-0.069949	4.818444
348.225427	8000.001322	12.779123	-0.069994	4.818452
347.984319	7999.943527	12.784128	-0.069949	4.818436
347.943824	7999.941940	12.789133	-0.069941	4.818435
348.379449	8000.025415	12.794138	-0.070023	4.818458
348.183545	8000.009167	12.799143	-0.069986	4.818454
347.990348	8000.012904	12.804147	-0.069950	4.818456
347.948949	8000.037553	12.809152	-0.069942	4.818464
347.911709	8000.011861	12.814157	-0.069935	4.818456
348.433733	8000.006188	12.819162	-0.070033	4.818453
348.243574	7999.995266	12.824167	-0.069997	4.818450
348.348349	8000.023955	12.829171	-0.070017	4.818458
348.033649	8000.018730	12.834176	-0.069958	4.818458
348.180218	7999.977627	12.839181	-0.069985	4.818445
348.457607	8000.038005	12.844186	-0.070037	4.818462
348.339815	7999.912550	12.849191	-0.070015	4.818425
348.298360	7999.983396	12.854195	-0.070008	4.818446
348.331986	8000.002741	12.859200	-0.070014	4.818452
348.106721	7999.969304	12.864205	-0.069972	4.818443
347.884104	8000.017798	12.869210	-0.069930	4.818458
348.275855	7999.964199	12.874215	-0.070003	4.818441
348.309366	8000.001392	12.879219	-0.070010	4.818452
348.409700	7999.943927	12.884224	-0.070028	4.818434
348.401342	7999.944867	12.889229	-0.070027	4.818434
348.641059	7999.944898	12.894234	-0.070071	4.818433
348.619305	7999.911011	12.899239	-0.070067	4.818423
348.328008	7999.985892	12.904243	-0.070013	4.818447
348.710047	7999.930065	12.909248	-0.070084	4.818429
348.606268	7999.880391	12.914253	-0.070065	4.818414
348.624875	7999.894288	12.919258	-0.070068	4.818418
348.055914	8000.010631	12.924263	-0.069962	4.818455
348.345339	7999.963025	12.929267	-0.070016	4.818440
348.282305	7999.971638	12.934272	-0.070005	4.818443
347.925306	7999.985801	12.939277	-0.069938	4.818448
348.207888	8000.022098	12.944282	-0.069991	4.818458
347.821905	8000.068424	12.949287	-0.069919	4.818473
348.110972	8000.040762	12.954291	-0.069973	4.818464
348.500068	7999.974529	12.959296	-0.070045	4.818443
348.285599	8000.030480	12.964301	-0.070005	4.818460
348.278114	7999.991534	12.969306	-0.070004	4.818449
347.923492	8000.015177	12.974311	-0.069938	4.818457
347.701740	8000.063682	12.979315	-0.069897	4.818472
347.421290	8000.100909	12.984320	-0.069844	4.818485
347.399432	8000.089070	12.989325	-0.069840	4.818481
348.159772	8000.101258	12.994330	-0.069982	4.818482
347.728069	8000.103930	12.999335	-0.069902	4.818484
347.395285	8000.131013	13.004339	-0.069840	4.818494
348.195499	8000.000939	13.009344	-0.069989	4.818452
347.890044	8000.004236	13.014349	-0.069932	4.818454
348.206133	8000.010530	13.019354	-0.069990	4.818455
348.065663	8000.009717	13.024359	-0.069964	4.818455
348.686632	8000.021107	13.029363	-0.070080	4.818456
348.678005	7999.978995	13.034368	-0.070078	4.818443
348.708650	7999.914306	13.039373	-0.070084	4.818424
348.737830	7999.931492	13.044378	-0.070089	4.818429
348.767361	7999.878337	13.049383	-0.070095	4.818413
348.623985	7999.899534	13.054387	-0.070068	4.818420
348.368464	8000.014787	13.059392	-0.070021	4.818455
348.661943	7999.916837	13.064397	-0.070075	4.818425
348.473556	7999.990983	13.069402	-0.070040	4.818448
348.365532	7999.919204	13.074407	-0.070020	4.818427
348.766356	7999.945522	13.079411	-0.070095	4.818433
348.853888	7999.915186	13.084416	-0.070111	4.818424
348.609530	7999.887795	13.089421	-0.070066	4.818417
348.617113	7999.915194	13.094426	-0.070067	4.818425
348.939617	7999.862777	13.099431	-0.070127	4.818408
348.943270	7999.882775	13.104435	-0.070128	4.818414
348.999703	7999.920272	13.109440	-0.070138	4.818425
348.698955	7999.903682	13.114445	-0.070082	4.818421
348.725194	7999.937629	13.119450	-0.070087	4.818431
348.434244	7999.928519	13.124455	-0.070033	4.818429
348.654397	7999.956639	13.129459	-0.070074	4.818437
348.667002	7999.919009	13.134464	-0.070076	4.818426
348.640469	7999.835712	13.139469	-0.070071	4.818401
348.309728	7999.975165	13.144474	-0.070010	4.818444
348.274563	7999.925352	13.149479	-0.070003	4.818429
348.524333	7999.875119	13.154483	-0.070050	4.818413
348.564519	7999.884052	13.159488	-0.070057	4.818416
348.293781	7999.923508	13.164493	-0.070007	4.818428
348.388262	7999.988808	13.169498	-0.070025	4.818448
348.123905	7999.971651	13.174503	-0.069975	4.818443
348.065891	8000.020229	13.179507	-0.069965	4.818458
348.473363	7999.958440	13.184512	-0.070040	4.818438
348.325314	7999.944926	13.189517	-0.070013	4.818435
348.630474	7999.975225	13.194522	-0.070070	4.818443
348.579797	7999.926255	13.199527	-0.070060	4.818428
348.236553	8000.037194	13.204531	-0.069996	4.818462
348.201616	8000.019932	13.209536	-0.069990	4.818458
348.431553	7999.947388	13.214541	-0.070033	4.818435
348.746229	7999.908516	13.219546	-0.070091	4.818422
348.567492	7999.845248	13.224551	-0.070058	4.818404
348.651996	7999.909366	13.229555	-0.070074	4.818423
348.770088	7999.927732	13.234560	-0.070096	4.818428
348.717983	7999.897643	13.239565	-0.070086	4.818419
348.562579	8000.039423	13.244570	-0.070057	4.818462
348.879540	7999.923936	13.249575	-0.070116	4.818426
348.508224	7999.971506	13.254579	-0.070047	4.818442
348.632769	7999.935361	13.259584	-0.070070	4.818431
348.760122	7999.860406	13.264589	-0.070094	4.818408
348.786071	7999.910098	13.269594	-0.070099	4.818423
348.889298	7999.856871	13.274599	-0.070118	4.818406
349.121698	7999.904053	13.279603	-0.070161	4.818419
349.042255	7999.944997	13.284608	-0.070146	4.818432
348.673918	7999.875013	13.289613	-0.070078	4.818413
348.580427	7999.985066	13.294618	-0.070060	4.818446
348.335676	7999.972369	13.299623	-0.070015	4.818443
348.570529	7999.925089	13.304627	-0.070059	4.818428
348.452682	7999.920375	13.309632	-0.070037	4.818427
348.545355	7999.925805	13.314637	-0.070054	4.818428
348.787719	7999.925872	13.319642	-0.070099	4.818427
348.487587	7999.897741	13.324647	-0.070043	4.818420
348.491911	7999.935596	13.329651	-0.070044	4.818431
348.808202	7999.876797	13.334656	-0.070103	4.818413
348.544229	7999.832347	13.339661	-0.070054	4.818400
348.869789	7999.872365	13.344666	-0.070114	4.818411
348.952733	7999.895515	13.349671	-0.070130	4.818418
348.868970	7999.913303	13.354675	-0.070114	4.818423
348.705100	7999.883830	13.359680	-0.070084	4.818415
348.813585	7999.945117	13.364685	-0.070104	4.818433
348.982449	7999.978857	13.369690	-0.070135	4.818442
348.878173	7999.876678	13.374695	-0.070116	4.818412
349.009432	7999.898370	13.379699	-0.070140	4.818418
349.055897	7999.902136	13.384704	-0.070149	4.818419
348.576811	7999.909428	13.389709	-0.070060	4.818423
348.458968	7999.956162	13.394714	-0.070038	4.818438
348.396622	7999.910188	13.399719	-0.070026	4.818424
348.808824	7999.904108	13.404723	-0.070103	4.818421
348.726124	7999.932410	13.409728	-0.070088	4.818429
348.784350	7999.899584	13.414733	-0.070098	4.818419
348.858061	7999.970909	13.419738	-0.070112	4.818440
348.828120	7999.850819	13.424743	-0.070107	4.818405
348.624892	7999.898519	13.429747	-0.070069	4.818420
348.565164	7999.928175	13.434752	-0.070058	4.818429
348.661110	7999.904250	13.439757	-0.070076	4.818421
348.564013	7999.943910	13.444762	-0.070057	4.818433
348.492041	7999.886259	13.449767	-0.070044	4.818417
348.495813	7999.947205	13.454771	-0.070045	4.818435
348.506303	7999.914797	13.459776	-0.070047	4.818425
348.391621	7999.948973	13.464781	-0.070025	4.818436
348.791553	7999.960580	13.469786	-0.070100	4.818438
348.542512	7999.976175	13.474791	-0.070054	4.818443
347.988697	8000.091669	13.479795	-0.069950	4.818480
348.043345	8000.070346	13.484800	-0.069961	4.818473
348.038426	8000.054532	13.489805	-0.069960	4.818468
348.167503	8000.025797	13.494810	-0.069984	4.818459
348.421791	7999.979824	13.499815	-0.070031	4.818445
348.391580	8000.026671	13.504819	-0.070025	4.818459
348.802963	7999.917686	13.509824	-0.070102	4.818425
348.555146	7999.995244	13.514829	-0.070056	4.818449
349.165009	7999.930892	13.519834	-0.070169	4.818427
348.759829	7999.923415	13.524839	-0.070094	4.818427
348.374218	7999.930897	13.529843	-0.070022	4.818430
348.559804	7999.977458	13.534848	-0.070057	4.818443
348.906088	7999.867610	13.539853	-0.070121	4.818409
348.749238	7999.883378	13.544858	-0.070092	4.818415
348.911180	7999.888677	13.549863	-0.070122	4.818416
349.005101	7999.852125	13.554867	-0.070140	4.818404
348.758131	7999.889796	13.559872	-0.070094	4.818417
348.676878	7999.893968	13.564877	-0.070079	4.818418
349.003074	7999.931895	13.569882	-0.070139	4.818428
348.640472	7999.944933	13.574887	-0.070072	4.818433
348.725741	7999.977563	13.579891	-0.070088	4.818443
348.089961	8000.060471	13.584896	-0.069969	4.818470
348.561255	7999.982730	13.589901	-0.070057	4.818445
348.312463	8000.024577	13.594906	-0.070011	4.818458
348.472563	7999.964755	13.599911	-0.070041	4.818440
348.321918	8000.019453	13.604915	-0.070013	4.818457
348.664308	7999.944201	13.609920	-0.070076	4.818433
348.120404	7999.974782	13.614925	-0.069975	4.818444
348.115823	7999.989421	13.619930	-0.069974	4.818449
348.147384	8000.007689	13.624935	-0.069980	4.818454
348.055549	7999.988622	13.629939	-0.069963	4.818449
348.390431	8000.015114	13.634944	-0.070025	4.818455
347.907706	8000.051757	13.639949	-0.069936	4.818468
348.230647	8000.046593	13.644954	-0.069996	4.818465
348.071840	8000.060235	13.649959	-0.069966	4.818470
348.501011	7999.996634	13.654963	-0.070046	4.818449
348.516958	8000.022045	13.659968	-0.070049	4.818457
348.276660	7999.942211	13.664973	-0.070004	4.818434
348.813835	7999.956689	13.669978	-0.070104	4.818436
348.812843	7999.904179	13.674983	-0.070104	4.818421
348.594795	7999.949583	13.679987	-0.070063	4.818435
348.609143	7999.960273	13.684992	-0.070066	4.818438
348.418459	7999.987141	13.689997	-0.070031	4.818447
348.803794	7999.977556	13.695002	-0.070102	4.818443
348.611158	7999.918303	13.700007	-0.070066	4.818426
348.562188	7999.935502	13.705011	-0.070057	4.818431
348.680415	7999.945471	13.710016	-0.070079	4.818433
348.233295	7999.974187	13.715021	-0.069996	4.818444
348.556657	7999.983727	13.720026	-0.070056	4.818445
348.537108	8000.038065	13.725031	-0.070053	4.818462
348.456529	8000.036996	13.730035	-0.070038	4.818462
348.525939	7999.989620	13.735040	-0.070051	4.818447
348.818809	7999.901112	13.740045	-0.070105	4.818420
348.720421	8000.002701	13.745050	-0.070087	4.818450
348.534828	7999.937242	13.750055	-0.070052	4.818432
348.896279	7999.917890	13.755059	-0.070120	4.818424
348.699758	8000.025527	13.760064	-0.070083	4.818457
348.824330	7999.899087	13.765069	-0.070106	4.818419
348.597731	8000.052522	13.770074	-0.070064	4.818466
348.200114	8000.054595	13.775079	-0.069990	4.818468
348.411863	8000.043756	13.780083	-0.070029	4.818464
348.393766	8000.027767	13.785088	-0.070026	4.818459
348.231387	8000.014063	13.790093	-0.069996	4.818456
348.334107	8000.105722	13.795098	-0.070015	4.818482
348.137831	8000.068469	13.800103	-0.069979	4.818472
347.986801	8000.083265	13.805107	-0.069950	4.818477
348.148296	8000.051810	13.810112	-0.069980	4.818467
348.528193	7999.934008	13.815117	-0.070051	4.818431
348.700029	7999.979337	13.820122	-0.070083	4.818443
348.434452	8000.018860	13.825127	-0.070034	4.818456
347.849976	8000.084600	13.830131	-0.069925	4.818478
347.747402	8000.094789	13.835136	-0.069906	4.818482
347.773464	8000.104585	13.840141	-0.069911	4.818484
348.107831	8000.098522	13.845146	-0.069973	4.818481
347.911420	8000.047619	13.850151	-0.069936	4.818467
347.683023	8000.130684	13.855155	-0.069894	4.818492
348.059549	8000.085283	13.860160	-0.069964	4.818477
347.801644	8000.058763	13.865165	-0.069916	4.818471
348.031981	8000.089118	13.870170	-0.069959	4.818479
348.180610	8000.028094	13.875175	-0.069987	4.818460
348.351797	8000.049265	13.880179	-0.070018	4.818466
348.261058	8000.061710	13.885184	-0.070002	4.818470
348.142988	8000.090592	13.890189	-0.069980	4.818479
347.550048	8000.186668	13.895194	-0.069869	4.818510
347.950766	8000.078593	13.900199	-0.069944	4.818476
348.091247	8000.047909	13.905203	-0.069970	4.818466
347.980671	8000.098939	13.910208	-0.069949	4.818482
347.766030	8000.113940	13.915213	-0.069909	4.818487
347.789464	8000.111101	13.920218	-0.069914	4.818486
348.016964	8000.076323	13.925223	-0.069956	4.818475
347.904144	8000.087425	13.930227	-0.069935	4.818479
347.852897	8000.081496	13.935232	-0.069926	4.818477
348.160974	8000.019438	13.940237	-0.069983	4.818458
347.649078	8000.141788	13.945242	-0.069888	4.818496
347.546656	8000.116281	13.950247	-0.069869	4.818489
347.913528	8000.089651	13.955251	-0.069937	4.818479
347.947854	8000.103756	13.960256	-0.069943	4.818483
347.631250	8000.103755	13.965261	-0.069884	4.818485
347.829253	8000.090634	13.970266	-0.069921	4.818480
347.567092	8000.119704	13.975271	-0.069872	4.818490
347.667765	8000.107391	13.980275	-0.069891	4.818486
347.796219	8000.092296	13.985280	-0.069915	4.818481
347.788323	8000.065944	13.990285	-0.069914	4.818473
347.844283	8000.133882	13.995290	-0.069924	4.818493
347.993181	8000.056063	14.000295	-0.069952	4.818469
347.577388	8000.124042	14.005299	-0.069874	4.818491
347.468121	8000.160390	14.010304	-0.069854	4.818502
347.821014	8000.048530	14.015309	-0.069920	4.818467
348.280011	8000.033622	14.020314	-0.070005	4.818461
348.116086	8000.072395	14.025319	-0.069975	4.818473
348.486022	8000.076254	14.030323	-0.070044	4.818473
348.412215	8000.056376	14.035328	-0.070030	4.818467
348.530915	7999.976056	14.040333	-0.070052	4.818443
348.636887	8000.066708	14.045338	-0.070072	4.818470
348.306096	8000.018221	14.050343	-0.070010	4.818457
348.166871	8000.058371	14.055347	-0.069984	4.818469
348.183909	8000.063847	14.060352	-0.069987	4.818471
348.051616	8000.054743	14.065357	-0.069963	4.818468
348.151443	8000.082316	14.070362	-0.069981	4.818476
348.195502	8000.039854	14.075367	-0.069989	4.818463
347.844167	8000.082439	14.080371	-0.069924	4.818477
348.070739	8000.103295	14.085376	-0.069966	4.818483
347.850980	8000.083580	14.090381	-0.069925	4.818478
347.629427	8000.142587	14.095386	-0.069884	4.818496
347.775302	8000.089926	14.100391	-0.069911	4.818480
347.767959	8000.100328	14.105395	-0.069910	4.818483
348.029921	8000.084906	14.110400	-0.069959	4.818477
347.886896	8000.043111	14.115405	-0.069932	4.818466
347.886949	8000.080909	14.120410	-0.069932	4.818477
347.977243	8000.032761	14.125415	-0.069949	4.818462
348.154071	8000.021458	14.130419	-0.069982	4.818458
348.460988	8000.028681	14.135424	-0.070039	4.818459
348.360660	8000.033650	14.140429	-0.070020	4.818461
348.409273	8000.022746	14.145434	-0.070029	4.818458
348.290860	8000.014875	14.150439	-0.070007	4.818456
348.637384	7999.978526	14.155443	-0.070072	4.818443
348.704425	8000.024564	14.160448	-0.070084	4.818457
348.504573	7999.961015	14.165453	-0.070047	4.818439
348.433965	8000.052474	14.170458	-0.070034	4.818466
348.325760	8000.010090	14.175463	-0.070014	4.818454
348.167936	8000.064693	14.180467	-0.069984	4.818471
348.123878	8000.055709	14.185472	-0.069976	4.818468
348.375117	7999.967698	14.190477	-0.070023	4.818441
348.310325	8000.066583	14.195482	-0.070011	4.818471
348.375634	8000.023353	14.200487	-0.070023	4.818458
348.328934	8000.013284	14.205491	-0.070014	4.818455
348.632207	8000.028858	14.210496	-0.070071	4.818458
348.538491	7999.970918	14.215501	-0.070053	4.818442
348.330339	8000.078400	14.220506	-0.070015	4.818474
347.975139	8000.020140	14.225511	-0.069949	4.818458
348.062233	8000.100041	14.230515	-0.069965	4.818482
348.183406	8000.054402	14.235520	-0.069987	4.818468
348.307987	8000.000409	14.240525	-0.070011	4.818451
348.112947	8000.096515	14.245530	-0.069974	4.818481
348.364607	8000.045258	14.250535	-0.070021	4.818464
348.176385	8000.064810	14.255539	-0.069986	4.818471
348.442249	8000.049439	14.260544	-0.070036	4.818465
348.171431	8000.059495	14.265549	-0.069985	4.818469
348.621288	7999.968870	14.270554	-0.070069	4.818441
348.901084	7999.872839	14.275559	-0.070121	4.818411
348.715827	7999.965926	14.280563	-0.070086	4.818439
348.634912	7999.993201	14.285568	-0.070071	4.818448
348.548269	7999.980502	14.290573	-0.070055	4.818444
348.791952	7999.955388	14.295578	-0.070101	4.818436
348.731804	7999.992388	14.300583	-0.070089	4.818447
348.545843	8000.009869	14.305587	-0.070055	4.818453
348.455714	8000.034922	14.310592	-0.070038	4.818461
348.254982	7999.968212	14.315597	-0.070001	4.818442
348.399566	8000.007929	14.320602	-0.070028	4.818453
348.164877	8000.024764	14.325607	-0.069984	4.818459
348.355043	7999.997889	14.330611	-0.070019	4.818450
348.322795	8000.035259	14.335616	-0.070013	4.818462
348.050678	8000.034799	14.340621	-0.069963	4.818462
348.420078	8000.034451	14.345626	-0.070032	4.818461
348.162000	8000.071974	14.350631	-0.069983	4.818473
348.487805	7999.952405	14.355635	-0.070044	4.818436
348.840882	7999.922443	14.360640	-0.070110	4.818426
348.720733	7999.901950	14.365645	-0.070087	4.818420
348.950697	7999.956449	14.370650	-0.070130	4.818436
348.802041	7999.936627	14.375655	-0.070103	4.818430
348.741345	7999.943172	14.380659	-0.070091	4.818433
349.098021	7999.888059	14.385664	-0.070158	4.818415
348.599581	7999.916093	14.390669	-0.070065	4.818425
348.833227	7999.959091	14.395674	-0.070108	4.818437
348.530832	7999.993927	14.400679	-0.070052	4.818448
348.423690	7999.969406	14.405683	-0.070032	4.818442
348.520189	7999.982237	14.410688	-0.070050	4.818445
348.986444	7999.877130	14.415693	-0.070137	4.818412
348.828506	8000.009428	14.420698	-0.070108	4.818452
348.707366	7999.964773	14.425703	-0.070085	4.818439
348.541364	7999.998268	14.430707	-0.070054	4.818450
348.405490	8000.054212	14.435712	-0.070029	4.818467
348.078311	8000.074019	14.440717	-0.069968	4.818474
348.336844	8000.057501	14.445722	-0.070016	4.818468
348.221477	8000.047571	14.450727	-0.069995	4.818466
347.941721	8000.096356	14.455731	-0.069943	4.818481
348.257150	7999.213364	14.460736	-0.070001	4.818217

348.413691	7996.046130	14.465741	-0.070028	4.817275
348.300891	7990.639688	14.470746	-0.070003	4.815667
347.832949	7984.027379	14.475751	-0.069912	4.813701
348.191326	7976.772109	14.480755	-0.069974	4.811540
348.226691	7969.131340	14.485760	-0.069975	4.809264
347.960315	7961.389908	14.490765	-0.069921	4.806958
348.324246	7953.416022	14.495770	-0.069983	4.804579
347.850519	7945.642085	14.500775	-0.069890	4.802262
347.767063	7937.615206	14.505779	-0.069869	4.799867
347.848931	7929.629828	14.510784	-0.069879	4.797482
347.294437	7921.638029	14.515789	-0.069771	4.795097
347.441756	7913.635295	14.520794	-0.069793	4.792704
347.148637	7905.600361	14.525799	-0.069733	4.790303
347.297373	7897.597293	14.530803	-0.069756	4.787908
347.078930	7889.551542	14.535808	-0.069710	4.785500
347.397992	7881.515520	14.540813	-0.069764	4.783092
347.501757	7873.568735	14.545818	-0.069778	4.780711
347.808334	7865.521712	14.550823	-0.069830	4.778298
347.832770	7857.485241	14.555827	-0.069829	4.775887
347.798078	7849.545868	14.560832	-0.069818	4.773505
347.687266	7841.557782	14.565837	-0.069792	4.771107
347.950361	7833.508640	14.570842	-0.069836	4.768688
347.602391	7825.546238	14.575847	-0.069766	4.766296
347.971753	7817.480143	14.580851	-0.069829	4.763870
348.068986	7809.610716	14.585856	-0.069842	4.761502
347.765070	7801.509499	14.590861	-0.069780	4.759064
347.317613	7793.715044	14.595866	-0.069692	4.756718
347.386573	7785.547572	14.600871	-0.069700	4.754257
347.654079	7777.525649	14.605875	-0.069744	4.751838
347.352551	7769.535423	14.610880	-0.069683	4.749429
347.444132	7761.529566	14.615885	-0.069695	4.747013
347.515005	7753.496594	14.620890	-0.069703	4.744587
347.657871	7745.531252	14.625895	-0.069724	4.742181
347.533123	7737.490601	14.630899	-0.069696	4.739751
347.670880	7729.547760	14.635904	-0.069716	4.737349
347.135393	7721.514756	14.640909	-0.069611	4.734920
347.330940	7713.550521	14.645914	-0.069642	4.732508
347.563655	7705.476109	14.650919	-0.069680	4.730063
347.774398	7697.489099	14.655923	-0.069714	4.727642
347.485461	7689.486761	14.660928	-0.069655	4.725217
347.309600	7681.528382	14.665933	-0.069617	4.722803
347.072804	7673.636558	14.670938	-0.069568	4.720409
346.984761	7665.595413	14.675943	-0.069547	4.717967
347.170822	7657.526959	14.680947	-0.069576	4.715516
347.071580	7649.534182	14.685952	-0.069552	4.713086
347.207111	7641.508675	14.690957	-0.069572	4.710646
347.059325	7633.545537	14.695962	-0.069540	4.708223
346.621898	7625.557664	14.700967	-0.069453	4.705792
346.701327	7617.528002	14.705971	-0.069463	4.703346
346.537591	7609.555853	14.710976	-0.069427	4.700917
346.441498	7601.509316	14.715981	-0.069404	4.698464
346.309471	7593.549780	14.720986	-0.069374	4.696036
346.440154	7585.479712	14.725991	-0.069393	4.693572
346.539556	7577.499598	14.730995	-0.069406	4.691135
346.122854	7569.526223	14.736000	-0.069324	4.688700
346.081742	7561.489746	14.741005	-0.069311	4.686243
346.374135	7553.498122	14.746010	-0.069360	4.683798
346.414441	7545.545696	14.751015	-0.069362	4.681365
345.909523	7537.544283	14.756019	-0.069263	4.678915
345.836219	7529.618373	14.761024	-0.069244	4.676487
345.772583	7521.505186	14.766029	-0.069227	4.674001
345.829415	7513.449452	14.771034	-0.069232	4.671530
345.351052	7505.458315	14.776039	-0.069138	4.669078
345.171303	7497.450543	14.781043	-0.069099	4.666620
345.322005	7489.439234	14.786048	-0.069122	4.664159
345.421387	7481.435115	14.791053	-0.069136	4.661700
345.890684	7473.432334	14.796058	-0.069218	4.659239
345.832159	7465.505475	14.801063	-0.069202	4.656800
345.958853	7457.422606	14.806067	-0.069220	4.654312
346.324530	7449.488930	14.811072	-0.069283	4.651869
346.040137	7441.393336	14.816077	-0.069225	4.649375
346.010284	7433.471161	14.821082	-0.069214	4.646932
345.980815	7425.401389	14.826087	-0.069203	4.644443
346.398614	7417.448856	14.831091	-0.069276	4.641989
346.105738	7409.419237	14.836096	-0.069216	4.639509
346.288866	7401.485380	14.841101	-0.069245	4.637058
346.202672	7393.439921	14.846106	-0.069224	4.634571
346.274796	7385.438934	14.851111	-0.069232	4.632097
346.286553	7377.417096	14.856115	-0.069229	4.629614
346.512698	7369.438450	14.861120	-0.069266	4.627144
346.179109	7361.386626	14.866125	-0.069198	4.624650
346.481689	7353.463640	14.871130	-0.069250	4.622194
346.912621	7345.381375	14.876135	-0.069325	4.619688
346.412779	7337.494030	14.881139	-0.069226	4.617241
346.769572	7329.381306	14.886144	-0.069288	4.614722
346.471068	7321.447786	14.891149	-0.069227	4.612258
346.316801	7313.412695	14.896154	-0.069193	4.609761
345.937863	7305.443051	14.901159	-0.069117	4.607282
346.247663	7297.350872	14.906163	-0.069170	4.604765
346.543251	7289.434518	14.911168	-0.069219	4.602301
346.261641	7281.397412	14.916173	-0.069162	4.599797
346.371410	7273.494313	14.921178	-0.069177	4.597335
346.154139	7265.435725	14.926183	-0.069131	4.594822
345.822737	7257.425198	14.931187	-0.069064	4.592322
346.148377	7249.320950	14.936192	-0.069120	4.589793
345.772925	7241.358547	14.941197	-0.069045	4.587306
346.003965	7233.388414	14.946202	-0.069083	4.584816
346.258200	7225.370491	14.951207	-0.069125	4.582310
345.687302	7217.372530	14.956211	-0.069013	4.579807
346.052914	7209.412558	14.961216	-0.069076	4.577316
345.807124	7201.380763	14.966221	-0.069025	4.574800
345.644895	7193.404765	14.971226	-0.068990	4.572301
345.572483	7185.373883	14.976231	-0.068971	4.569783
345.621792	7177.341678	14.981235	-0.068975	4.567263
345.741127	7169.325348	14.986240	-0.068992	4.564748
345.603474	7161.363911	14.991245	-0.068961	4.562247
345.529264	7153.367699	14.996250	-0.068942	4.559735
345.996450	7145.354041	15.001255	-0.069024	4.557216
345.927043	7137.347735	15.006259	-0.069006	4.554698
345.469205	7129.443141	15.011264	-0.068915	4.552209
345.217193	7121.340204	15.016269	-0.068863	4.549657
345.070713	7113.385683	15.021274	-0.068831	4.547150
345.054892	7105.331551	15.026279	-0.068822	4.544611
344.992320	7097.363475	15.031283	-0.068806	4.542097
344.756414	7089.337085	15.036288	-0.068756	4.539564
344.833789	7081.377696	15.041293	-0.068766	4.537050
345.410522	7073.278828	15.046298	-0.068868	4.534493
345.327170	7065.349449	15.051303	-0.068847	4.531986
345.182669	7057.271151	15.056307	-0.068815	4.529431
345.822470	7049.304224	15.061312	-0.068929	4.526911
345.687973	7041.264427	15.066317	-0.068899	4.524365
346.033712	7033.330738	15.071322	-0.068958	4.521852
345.832451	7025.316404	15.076327	-0.068915	4.519311
345.633353	7017.357811	15.081331	-0.068873	4.516786
345.224495	7009.336180	15.086336	-0.068792	4.514239
345.107948	7001.347508	15.091341	-0.068765	4.511701
344.856663	6993.336393	15.096346	-0.068713	4.509155
345.272633	6985.262482	15.101351	-0.068785	4.506590
345.363487	6977.217355	15.106355	-0.068796	4.504031
345.599905	6969.312360	15.111360	-0.068835	4.501516
345.942904	6961.181091	15.116365	-0.068894	4.498928
345.951092	6953.243549	15.121370	-0.068890	4.496399
345.574531	6945.253522	15.126375	-0.068815	4.493850
345.437598	6937.280854	15.131379	-0.068784	4.491306
345.129015	6929.322760	15.136384	-0.068722	4.488765
344.961416	6921.316671	15.141389	-0.068685	4.486207
344.839159	6913.245283	15.146394	-0.068657	4.483627
345.012940	6905.272294	15.151399	-0.068684	4.481079
344.934732	6897.228141	15.156403	-0.068665	4.478505
344.939506	6889.315251	15.161408	-0.068660	4.475972
345.145573	6881.212090	15.166413	-0.068693	4.473378
344.986701	6873.272551	15.171418	-0.068659	4.470833
344.895098	6865.275326	15.176423	-0.068636	4.468268
345.120466	6857.204238	15.181427	-0.068673	4.465680
344.859487	6849.260546	15.186432	-0.068619	4.463128
344.818143	6841.253155	15.191437	-0.068606	4.460556
344.976136	6833.239651	15.196442	-0.068631	4.457981
344.854558	6825.243701	15.201447	-0.068603	4.455409
344.205395	6817.293516	15.206451	-0.068477	4.452848
344.344491	6809.260283	15.211456	-0.068497	4.450263
344.543065	6801.187135	15.216461	-0.068529	4.447663
344.651211	6793.171400	15.221466	-0.068544	4.445080
344.818112	6785.225146	15.226471	-0.068570	4.442518
344.434712	6777.243086	15.231475	-0.068493	4.439940
344.773635	6769.221012	15.236480	-0.068551	4.437351
344.972511	6761.136280	15.241485	-0.068583	4.434741
345.020849	6753.247056	15.246490	-0.068587	4.432191
344.897374	6745.194509	15.251495	-0.068559	4.429585
344.892849	6737.138912	15.256499	-0.068553	4.426978
344.902311	6729.189023	15.261504	-0.068549	4.424404
344.762603	6721.223288	15.266509	-0.068518	4.421822
344.622446	6713.198742	15.271514	-0.068487	4.419219
344.437072	6705.271202	15.276519	-0.068447	4.416646
344.508676	6697.179247	15.281523	-0.068455	4.414020
344.602772	6689.240618	15.286528	-0.068467	4.411442
343.967720	6681.210728	15.291533	-0.068344	4.408829
344.073952	6673.225627	15.296538	-0.068358	4.406233
343.792838	6665.241069	15.301543	-0.068301	4.403633
343.604021	6657.264362	15.306547	-0.068261	4.401035
343.668842	6649.291349	15.311552	-0.068267	4.398438
343.835206	6641.191768	15.316557	-0.068293	4.395799
343.837181	6633.210301	15.321562	-0.068288	4.393196
344.195981	6625.213038	15.326567	-0.068350	4.390589
344.601522	6617.124820	15.331571	-0.068420	4.387950
344.524805	6609.156233	15.336576	-0.068401	4.385346
344.507503	6601.180692	15.341581	-0.068392	4.382739
344.765848	6593.164107	15.346586	-0.068435	4.380118
344.521619	6585.255267	15.351591	-0.068384	4.377528
344.147832	6577.251037	15.356595	-0.068310	4.374904
344.175593	6569.312707	15.361600	-0.068310	4.372302
344.510869	6561.164968	15.366605	-0.068367	4.369633
344.565174	6553.217494	15.371610	-0.068372	4.367026
344.558507	6545.235211	15.376615	-0.068365	4.364405
344.706146	6537.260967	15.381619	-0.068388	4.361787
344.772329	6529.258147	15.386624	-0.068395	4.359157
344.775192	6521.337482	15.391629	-0.068390	4.356552
344.647881	6513.280364	15.396634	-0.068361	4.353899
344.425258	6505.238930	15.401639	-0.068314	4.351250
344.189945	6497.245411	15.406643	-0.068265	4.348614
343.996723	6489.306979	15.411648	-0.068224	4.345995
343.460012	6481.302021	15.416653	-0.068119	4.343350
343.619289	6473.296067	15.421658	-0.068144	4.340709
343.607305	6465.305637	15.426663	-0.068136	4.338070
343.927223	6457.211989	15.431667	-0.068190	4.335397
343.746014	6449.284492	15.436672	-0.068152	4.332774
343.951128	6441.154353	15.441677	-0.068184	4.330085
343.571466	6433.301886	15.446682	-0.068109	4.327482
343.394472	6425.255208	15.451687	-0.068070	4.324815
343.223980	6417.319794	15.456691	-0.068034	4.322183
343.344064	6409.284102	15.461696	-0.068051	4.319518
343.542797	6401.307745	15.466701	-0.068082	4.316872
343.477752	6393.237721	15.471706	-0.068065	4.314191
343.530703	6385.257977	15.476711	-0.068070	4.311540
343.369569	6377.186400	15.481715	-0.068034	4.308854
343.007904	6369.311838	15.486720	-0.067962	4.306231
343.411842	6361.142668	15.491725	-0.068032	4.303514
343.550832	6353.251597	15.496730	-0.068053	4.300887
343.131599	6345.252936	15.501735	-0.067969	4.298216
342.976896	6337.237312	15.506739	-0.067935	4.295541
342.815115	6329.268087	15.511744	-0.067900	4.292880
342.366155	6321.236986	15.516749	-0.067811	4.290193
342.472658	6313.263956	15.521754	-0.067826	4.287529
342.741238	6305.159754	15.526759	-0.067871	4.284822
342.484406	6297.259006	15.531763	-0.067818	4.282175
342.764499	6289.203657	15.536768	-0.067865	4.279481
343.375640	6281.161589	15.541773	-0.067973	4.276792
343.277106	6273.183696	15.546778	-0.067950	4.274117
343.142267	6265.226776	15.551783	-0.067919	4.271446
343.168154	6257.187494	15.556787	-0.067919	4.268748
342.832154	6249.285556	15.561792	-0.067851	4.266090
342.892641	6241.188555	15.566797	-0.067857	4.263369
343.280278	6233.148299	15.571802	-0.067924	4.260669
342.677148	6225.264842	15.576807	-0.067807	4.258010
342.634973	6217.225204	15.581811	-0.067794	4.255303
342.547048	6209.232838	15.586816	-0.067772	4.252609
342.455764	6201.174408	15.591821	-0.067750	4.249891
342.590239	6193.218827	15.596826	-0.067770	4.247208
342.460728	6185.176481	15.601831	-0.067740	4.244491
342.653409	6177.237491	15.606835	-0.067771	4.241811
342.596613	6169.191171	15.611840	-0.067755	4.239091
342.838569	6161.178538	15.616845	-0.067795	4.236383
343.440011	6153.145801	15.621850	-0.067902	4.233671
343.350933	6145.175764	15.626855	-0.067880	4.230971
342.953599	6137.162653	15.631859	-0.067801	4.228251
342.907554	6129.218164	15.636864	-0.067787	4.225556
342.859297	6121.164792	15.641869	-0.067773	4.222823
343.078387	6113.173254	15.646874	-0.067808	4.220112
343.297339	6105.198716	15.651879	-0.067844	4.217405
343.148773	6097.143968	15.656883	-0.067811	4.214664
342.892512	6089.214586	15.661888	-0.067758	4.211964
343.198339	6081.104892	15.666893	-0.067810	4.209206
343.028378	6073.219670	15.671898	-0.067773	4.206518
343.145646	6065.165115	15.676903	-0.067790	4.203774
342.930073	6057.220348	15.681907	-0.067744	4.201062
343.258345	6049.180040	15.686912	-0.067800	4.198321
342.883670	6041.220039	15.691917	-0.067725	4.195598
342.756544	6033.207551	15.696922	-0.067696	4.192858
343.048540	6025.104659	15.701927	-0.067745	4.190091
342.602806	6017.192238	15.706931	-0.067657	4.187378
342.730200	6009.133870	15.711936	-0.067676	4.184620
342.345724	6001.159776	15.716941	-0.067599	4.181883
342.901660	5993.096866	15.721946	-0.067697	4.179125
342.875876	5985.187063	15.726951	-0.067687	4.176410
342.732047	5977.171190	15.731955	-0.067655	4.173657
342.874175	5969.229441	15.736960	-0.067677	4.170930
342.439604	5961.196542	15.741965	-0.067590	4.168163
342.049878	5953.232855	15.746970	-0.067513	4.165418
342.299029	5945.230424	15.751975	-0.067554	4.162666
342.467441	5937.144646	15.756979	-0.067580	4.159883
342.374830	5929.225947	15.761984	-0.067558	4.157152
342.365754	5921.138395	15.766989	-0.067551	4.154363
342.459386	5913.235106	15.771994	-0.067563	4.151636
342.683221	5905.167648	15.776999	-0.067599	4.148852
342.213344	5897.221932	15.782003	-0.067507	4.146100
342.631057	5889.151554	15.787008	-0.067579	4.143314
341.729786	5881.314252	15.792013	-0.067406	4.140590
341.651386	5873.272599	15.797018	-0.067386	4.137804
341.802587	5865.231183	15.802023	-0.067409	4.135019
341.633161	5857.238109	15.807027	-0.067373	4.132245
341.867838	5849.171843	15.812032	-0.067411	4.129449
341.767953	5841.183316	15.817037	-0.067387	4.126673
341.952216	5833.194463	15.822042	-0.067416	4.123900
341.485998	5825.311032	15.827047	-0.067324	4.121152
341.620564	5817.224514	15.832051	-0.067344	4.118340
342.042124	5809.200173	15.837056	-0.067417	4.115552
341.428239	5801.283397	15.842061	-0.067298	4.112785
341.564292	5793.206037	15.847066	-0.067318	4.109970
341.701608	5785.202089	15.852071	-0.067338	4.107179
341.841024	5777.106910	15.857075	-0.067359	4.104355
341.765874	5769.251988	15.862080	-0.067340	4.101609
341.777333	5761.165836	15.867085	-0.067337	4.098782
341.282477	5753.253276	15.872090	-0.067240	4.096007
341.078083	5745.243363	15.877095	-0.067196	4.093200
340.831120	5737.217645	15.882099	-0.067145	4.090384
341.326875	5729.200407	15.887104	-0.067232	4.087581
341.523684	5721.122717	15.892109	-0.067264	4.084750
341.472242	5713.215683	15.897114	-0.067249	4.081973
341.267831	5705.225474	15.902119	-0.067206	4.079163
341.281556	5697.262665	15.907123	-0.067203	4.076364
341.127748	5689.261025	15.912128	-0.067169	4.073546
341.556251	5681.146941	15.917133	-0.067244	4.070696
341.400842	5673.191086	15.922138	-0.067210	4.067891
341.507492	5665.146236	15.927143	-0.067224	4.065057
341.481039	5657.202981	15.932147	-0.067214	4.062254
341.488930	5649.193001	15.937152	-0.067210	4.059426
341.141084	5641.277528	15.942157	-0.067140	4.056625
341.234707	5633.189329	15.947162	-0.067153	4.053767
341.426684	5625.234780	15.952167	-0.067183	4.050956
341.554662	5617.173917	15.957171	-0.067202	4.048104
341.598524	5609.178822	15.962176	-0.067205	4.045273
341.490324	5601.230461	15.967181	-0.067179	4.042453
341.739527	5593.160768	15.972186	-0.067220	4.039594
341.672613	5585.265701	15.977191	-0.067203	4.036790
341.661640	5577.181224	15.982195	-0.067196	4.033918
341.681755	5569.196788	15.987200	-0.067194	4.031080
341.454596	5561.171395	15.992205	-0.067147	4.028221
341.263884	5553.219379	15.997210	-0.067106	4.025387
341.340009	5545.258104	16.002215	-0.067115	4.022552
341.526617	5537.190500	16.007219	-0.067144	4.019679
341.299417	5529.281693	16.012224	-0.067097	4.016853
341.174291	5521.236542	16.017229	-0.067068	4.013979
341.241895	5513.254553	16.022234	-0.067076	4.011128
341.537461	5505.187169	16.027239	-0.067126	4.008249
341.110239	5497.247768	16.032243	-0.067041	4.005401
341.268688	5489.283755	16.037248	-0.067065	4.002552
341.308204	5481.235216	16.042253	-0.067067	3.999669
341.218584	5473.300492	16.047258	-0.067045	3.996822
340.899948	5465.310291	16.052263	-0.066981	3.993950
340.678992	5457.331692	16.057267	-0.066935	3.991081
341.133267	5449.241946	16.062272	-0.067014	3.988182
341.061174	5441.232122	16.067277	-0.066995	3.985300
341.015558	5433.262392	16.072282	-0.066982	3.982431
340.899532	5425.304485	16.077287	-0.066955	3.979563
340.931431	5417.276671	16.082291	-0.066955	3.976671
340.955682	5409.248147	16.087296	-0.066955	3.973776
340.601721	5401.290943	16.092301	-0.066884	3.970898
340.265695	5393.343955	16.097306	-0.066816	3.968021
340.203658	5385.305414	16.102311	-0.066799	3.965115
340.393655	5377.310185	16.107315	-0.066829	3.962226
340.140831	5369.312002	16.112320	-0.066777	3.959327
339.850962	5361.366469	16.117325	-0.066718	3.956443
339.704196	5353.321443	16.122330	-0.066685	3.953524
339.816842	5345.292423	16.127335	-0.066701	3.950613
340.363520	5337.149917	16.132339	-0.066798	3.947668
340.276961	5329.253688	16.137344	-0.066776	3.944797
340.735515	5321.214097	16.142349	-0.066856	3.941883
340.712429	5313.214638	16.147354	-0.066847	3.938972
340.829119	5305.265272	16.152359	-0.066863	3.936080
340.540974	5297.253750	16.157363	-0.066805	3.933155
340.664081	5289.290116	16.162368	-0.066822	3.930253
340.678613	5281.238820	16.167373	-0.066820	3.927315
340.809459	5273.242105	16.172378	-0.066839	3.924398
340.731281	5265.331524	16.177383	-0.066819	3.921505
340.350304	5257.323445	16.182387	-0.066743	3.918569
340.164425	5249.390431	16.187392	-0.066703	3.915662
339.962364	5241.350091	16.192397	-0.066660	3.912713
339.972191	5233.325808	16.197402	-0.066657	3.909771
339.559502	5225.403507	16.202407	-0.066575	3.906857
339.591946	5217.317002	16.207411	-0.066576	3.903889
339.910696	5209.377392	16.212416	-0.066630	3.900978
339.899555	5201.296037	16.217421	-0.066623	3.898007
339.844322	5193.304689	16.222426	-0.066607	3.895065
339.909656	5185.334828	16.227431	-0.066614	3.892132
340.165158	5177.247001	16.232435	-0.066656	3.889157
340.268637	5169.352216	16.237440	-0.066671	3.886247
340.328165	5161.289858	16.242445	-0.066676	3.883273
340.069166	5153.394180	16.247450	-0.066623	3.880351
339.766733	5145.460554	16.252455	-0.066562	3.877412
339.621734	5137.412051	16.257459	-0.066529	3.874432
339.575464	5129.269843	16.262464	-0.066515	3.871417
339.768648	5121.209781	16.267469	-0.066546	3.868435
340.052617	5113.222263	16.272474	-0.066594	3.865479
340.062235	5105.317722	16.277479	-0.066590	3.862546
339.837023	5097.319958	16.282483	-0.066543	3.859572
339.519497	5089.409322	16.287488	-0.066479	3.856625
339.519212	5081.370030	16.292493	-0.066474	3.853635
339.653644	5073.329227	16.297498	-0.066494	3.850645
339.759469	5065.333134	16.302503	-0.066508	3.847669
339.775696	5057.321594	16.307507	-0.066506	3.844683
340.017115	5049.365082	16.312512	-0.066546	3.841720
339.642207	5041.389560	16.317517	-0.066471	3.838734
339.733518	5033.393114	16.322522	-0.066482	3.835748
339.556127	5025.430331	16.327527	-0.066444	3.832767
339.327439	5017.385120	16.332531	-0.066396	3.829751
339.433883	5009.384030	16.337536	-0.066411	3.826756
339.252880	5001.367916	16.342541	-0.066372	3.823748
339.344620	4993.406022	16.347546	-0.066384	3.820763
339.135328	4985.425896	16.352551	-0.066340	3.817763
339.324430	4977.349365	16.357555	-0.066370	3.814732
339.397716	4969.413121	16.362560	-0.066378	3.811750
339.215765	4961.405569	16.367565	-0.066339	3.808732
339.104801	4953.363694	16.372570	-0.066313	3.805701
339.010680	4945.434898	16.377575	-0.066291	3.802711
338.886875	4937.431460	16.382579	-0.066262	3.799689
338.661801	4929.521647	16.387584	-0.066215	3.796698
338.699892	4921.423629	16.392589	-0.066217	3.793639
338.956347	4913.407850	16.397594	-0.066260	3.790614
338.988147	4905.385824	16.402599	-0.066260	3.787579
338.983747	4897.346914	16.407603	-0.066254	3.784535
339.278079	4889.422749	16.412608	-0.066304	3.781538
338.938356	4881.461927	16.417613	-0.066235	3.778511
338.792035	4873.469262	16.422618	-0.066203	3.775473
338.754579	4865.481212	16.427623	-0.066191	3.772437
338.786531	4857.423031	16.432627	-0.066192	3.769374
338.837440	4849.465326	16.437632	-0.066196	3.766347
338.559945	4841.472483	16.442637	-0.066139	3.763296
338.959282	4833.472818	16.447642	-0.066208	3.760256
339.096106	4825.482238	16.452647	-0.066228	3.757211
339.018724	4817.434089	16.457651	-0.066209	3.754137
338.997261	4809.509874	16.462656	-0.066200	3.751108
339.089241	4801.472176	16.467661	-0.066211	3.748037
338.940639	4793.487501	16.472666	-0.066179	3.744977
338.701958	4785.535605	16.477671	-0.066129	3.741926
338.727625	4777.491787	16.482675	-0.066129	3.738843
338.327808	4769.604236	16.487680	-0.066049	3.735807
338.276981	4761.529065	16.492685	-0.066034	3.732705
338.383440	4753.516136	16.497690	-0.066049	3.729628
338.140665	4745.581343	16.502695	-0.065998	3.726570
337.718737	4737.581446	16.507699	-0.065915	3.723480
337.878988	4729.581603	16.512704	-0.065939	3.720402
338.378153	4721.510879	16.517709	-0.066027	3.717302
337.857292	4713.550683	16.522714	-0.065925	3.714217
338.044045	4705.479185	16.527719	-0.065954	3.711105
338.365854	4697.444128	16.532723	-0.066009	3.708007
338.539525	4689.472342	16.537728	-0.066036	3.704927
338.068493	4681.564859	16.542733	-0.065943	3.701854
338.303315	4673.509577	16.547738	-0.065982	3.698738
338.171179	4665.573441	16.552743	-0.065952	3.695657
338.487881	4657.470521	16.557747	-0.066006	3.692520
338.348501	4649.545867	16.562752	-0.065975	3.689437
338.305197	4641.544316	16.567757	-0.065961	3.686325
338.266730	4633.582899	16.572762	-0.065949	3.683226
338.122203	4625.624245	16.577767	-0.065917	3.680122
337.964618	4617.638847	16.582771	-0.065882	3.677005
337.606388	4609.643707	16.587776	-0.065810	3.673876
337.515866	4601.652256	16.592781	-0.065788	3.670753
337.694207	4593.618704	16.597786	-0.065816	3.667619
337.305123	4585.651266	16.602791	-0.065739	3.664492
337.113876	4577.687406	16.607795	-0.065698	3.661369
337.454736	4569.635957	16.612800	-0.065756	3.658223
337.571794	4561.618883	16.617805	-0.065773	3.655082
337.679662	4553.607708	16.622810	-0.065788	3.651941
337.897145	4545.566279	16.627815	-0.065823	3.648788
337.960716	4537.583841	16.632819	-0.065830	3.645652
338.046422	4529.616994	16.637824	-0.065840	3.642519
337.915915	4521.657250	16.642829	-0.065811	3.639380
337.899262	4513.683672	16.647834	-0.065803	3.636237
337.958831	4505.691791	16.652839	-0.065808	3.633085
337.299134	4497.727441	16.657843	-0.065680	3.629922
337.643837	4489.700680	16.662848	-0.065739	3.626759
337.550257	4481.654696	16.667853	-0.065717	3.623574
337.681535	4473.661891	16.672858	-0.065736	3.620413
337.582261	4465.715518	16.677863	-0.065712	3.617262
337.801257	4457.631093	16.682867	-0.065748	3.614062
337.757327	4449.756013	16.687872	-0.065734	3.610934
337.398590	4441.696292	16.692877	-0.065662	3.607722
337.331285	4433.695606	16.697882	-0.065645	3.604538
337.322255	4425.774593	16.702887	-0.065638	3.601385
337.602167	4417.703781	16.707891	-0.065685	3.598178
337.619857	4409.738404	16.712896	-0.065683	3.595003
337.597202	4401.705625	16.717901	-0.065673	3.591797
337.720872	4393.685609	16.722906	-0.065691	3.588597
337.729947	4385.711644	16.727911	-0.065688	3.585409
337.475791	4377.757342	16.732915	-0.065635	3.582219
337.463579	4369.779727	16.737920	-0.065628	3.579024
337.250365	4361.804822	16.742925	-0.065583	3.575820
337.510804	4353.765865	16.747930	-0.065626	3.572603
337.594346	4345.751223	16.752935	-0.065636	3.569387
337.193765	4337.805110	16.757939	-0.065557	3.566181
337.448317	4329.809062	16.762944	-0.065599	3.562972
337.386059	4321.826287	16.767949	-0.065582	3.559756
337.324939	4313.862287	16.772954	-0.065565	3.556544
337.371763	4305.806786	16.777959	-0.065569	3.553296
337.132509	4297.756519	16.782963	-0.065519	3.550038
337.344717	4289.815098	16.787968	-0.065553	3.546835
337.151035	4281.776130	16.792973	-0.065512	3.543577
337.307209	4273.803287	16.797978	-0.065536	3.540354
337.215616	4265.878308	16.802983	-0.065514	3.537140
337.105851	4257.845815	16.807987	-0.065488	3.533878
337.330421	4249.867898	16.812992	-0.065525	3.530646
336.975734	4241.870782	16.817997	-0.065454	3.527385
337.063498	4233.847531	16.823002	-0.065465	3.524125
336.834697	4225.954504	16.828007	-0.065417	3.520904
336.913600	4217.895390	16.833011	-0.065426	3.517623
336.774512	4209.969513	16.838016	-0.065395	3.514385
336.455925	4201.958118	16.843021	-0.065331	3.511104
336.710169	4193.907660	16.848026	-0.065373	3.507823
336.594532	4185.906073	16.853031	-0.065346	3.504546
336.832222	4177.892410	16.858035	-0.065385	3.501273
336.405614	4169.957187	16.863040	-0.065301	3.498008
336.512052	4161.935391	16.868045	-0.065315	3.494721
336.614420	4153.923704	16.873050	-0.065329	3.491435
336.362746	4145.963795	16.878055	-0.065277	3.488156
336.581404	4137.900934	16.883059	-0.065312	3.484846
336.327468	4130.018548	16.888064	-0.065260	3.481592
336.686422	4121.939781	16.893069	-0.065322	3.478275
335.932893	4114.069649	16.898074	-0.065176	3.475003
336.076971	4106.034822	16.903079	-0.065198	3.471691
336.175085	4097.981133	16.908083	-0.065211	3.468365
336.532177	4089.925366	16.913088	-0.065272	3.465045
336.217024	4082.002834	16.918093	-0.065208	3.461754
336.188267	4074.036714	16.923098	-0.065198	3.458451
336.183392	4066.028879	16.928103	-0.065192	3.455128
336.148348	4058.047764	16.933107	-0.065180	3.451813
336.160484	4050.059943	16.938112	-0.065177	3.448493
336.035883	4042.052102	16.943117	-0.065148	3.445157
336.113716	4034.074292	16.948122	-0.065158	3.441837
335.904561	4026.099504	16.953127	-0.065114	3.438505
335.990419	4018.111765	16.958131	-0.065124	3.435175
335.904331	4010.125892	16.963136	-0.065103	3.431836
335.660107	4002.118499	16.968141	-0.065052	3.428480
335.718526	3994.110884	16.973146	-0.065058	3.425130
336.093236	3986.103911	16.978151	-0.065123	3.421789
335.443306	3978.148330	16.983155	-0.064996	3.418430
335.926379	3970.101672	16.988160	-0.065081	3.415070
335.777541	3962.154711	16.993165	-0.065048	3.411725
335.384506	3954.178420	16.998170	-0.064970	3.408357
335.345823	3946.196440	17.003175	-0.064958	3.404995
335.478649	3938.180381	17.008179	-0.064977	3.401622
335.540524	3930.210813	17.013184	-0.064983	3.398262
335.688807	3922.164862	17.018189	-0.065006	3.394870
336.304537	3914.061757	17.023194	-0.065115	3.391467
336.027356	3906.151550	17.028199	-0.065058	3.388111
335.658486	3898.134896	17.033203	-0.064984	3.384702
335.684064	3890.221300	17.038208	-0.064984	3.381348
336.113297	3882.130664	17.043213	-0.065059	3.377930
335.803892	3874.205273	17.048218	-0.064996	3.374552
335.467828	3866.291750	17.053223	-0.064928	3.371175
335.470096	3858.256457	17.058227	-0.064923	3.367755
335.375123	3850.301522	17.063232	-0.064901	3.364362
335.377995	3842.310994	17.068237	-0.064896	3.360954
335.222157	3834.320546	17.073242	-0.064862	3.357537
335.348165	3826.313577	17.078247	-0.064880	3.354119
335.221488	3818.315056	17.083251	-0.064851	3.350692
335.248457	3810.325811	17.088256	-0.064851	3.347272
335.421889	3802.272827	17.093261	-0.064878	3.343826
335.191526	3794.391789	17.098266	-0.064830	3.340435
335.259267	3786.378375	17.103271	-0.064837	3.336996
335.431238	3778.316035	17.108275	-0.064864	3.333535
335.253925	3770.382999	17.113280	-0.064826	3.330113
335.181000	3762.371401	17.118285	-0.064807	3.326658
335.277974	3754.351513	17.123290	-0.064820	3.323203
335.472908	3746.397621	17.128295	-0.064851	3.319776
334.874821	3738.480541	17.133299	-0.064735	3.316330
334.974346	3730.457941	17.138304	-0.064748	3.312863
334.653445	3722.478768	17.143309	-0.064683	3.309394
334.711522	3714.441454	17.148314	-0.064689	3.305911
334.516493	3706.472911	17.153319	-0.064647	3.302444
334.556672	3698.429710	17.158323	-0.064649	3.298951
334.607229	3690.490189	17.163328	-0.064654	3.295499
334.748327	3682.461134	17.168333	-0.064675	3.292008
334.520428	3674.490017	17.173338	-0.064627	3.288524
333.941072	3666.625447	17.178343	-0.064514	3.285069
334.153847	3658.514560	17.183347	-0.064548	3.281535
334.059179	3650.584730	17.188352	-0.064525	3.278063
334.223407	3642.548958	17.193357	-0.064551	3.274552
334.243501	3634.540744	17.198362	-0.064549	3.271043
334.252250	3626.584840	17.203367	-0.064546	3.267553
334.347980	3618.493667	17.208371	-0.064558	3.264003
334.677344	3610.545662	17.213376	-0.064615	3.260522
334.269327	3602.620813	17.218381	-0.064533	3.257017
334.448695	3594.578330	17.223386	-0.064562	3.253481
334.655068	3586.582302	17.228391	-0.064595	3.249962
334.333375	3578.627384	17.233395	-0.064530	3.246436
334.588901	3570.629865	17.238400	-0.064572	3.242912
334.697850	3562.639208	17.243405	-0.064587	3.239380
334.436241	3554.703437	17.248410	-0.064533	3.235853
334.440533	3546.733728	17.253415	-0.064529	3.232319
334.103243	3538.721459	17.258419	-0.064461	3.228747
334.518359	3530.667172	17.263424	-0.064533	3.225185
334.357429	3522.724051	17.268429	-0.064498	3.221644
334.298681	3514.711364	17.273434	-0.064482	3.218072
334.236833	3506.738687	17.278439	-0.064465	3.214514
334.161264	3498.748928	17.283443	-0.064446	3.210943
334.318371	3490.719259	17.288448	-0.064470	3.207361
334.162997	3482.745940	17.293453	-0.064436	3.203787
334.108444	3474.784431	17.298458	-0.064420	3.200218
333.950069	3466.867591	17.303463	-0.064386	3.196661
334.225311	3458.761363	17.308467	-0.064431	3.193033
334.464506	3450.781553	17.313472	-0.064471	3.189457
334.167497	3442.825163	17.318477	-0.064410	3.185864
333.935568	3434.875035	17.323482	-0.064362	3.182272
333.941200	3426.881800	17.328487	-0.064358	3.178668
333.833194	3418.900431	17.333491	-0.064333	3.175059
333.900460	3410.895173	17.338496	-0.064340	3.171444
333.825959	3402.907390	17.343501	-0.064321	3.167826
333.904411	3394.864857	17.348506	-0.064330	3.164185
333.641923	3386.993038	17.353511	-0.064276	3.160603
333.677581	3378.968957	17.358515	-0.064278	3.156961
334.041991	3370.918218	17.363520	-0.064340	3.153317
333.675995	3363.000990	17.368525	-0.064267	3.149697
333.448863	3355.027925	17.373530	-0.064219	3.146054
333.593372	3347.004719	17.378535	-0.064241	3.142400
333.605825	3338.993672	17.383539	-0.064238	3.138742
333.562750	3331.016606	17.388544	-0.064225	3.135092
333.643966	3323.015305	17.393549	-0.064235	3.131433
333.076440	3315.109377	17.398554	-0.064124	3.127783
333.093482	3307.104685	17.403559	-0.064122	3.124111
332.790249	3299.152457	17.408563	-0.064060	3.120444
332.708594	3291.172496	17.413568	-0.064040	3.116769
333.020597	3283.109419	17.418573	-0.064093	3.113071
333.117437	3275.075491	17.423578	-0.064106	3.109371
333.153436	3267.111315	17.428583	-0.064107	3.105696
333.260147	3259.116292	17.433587	-0.064122	3.102007
333.440430	3251.104368	17.438592	-0.064150	3.098308
333.018629	3243.210401	17.443597	-0.064066	3.094631
333.154324	3235.175626	17.448602	-0.064086	3.090911
332.983738	3227.244262	17.453607	-0.064050	3.087220
332.924812	3219.215067	17.458611	-0.064033	3.083484
333.121057	3211.238483	17.463616	-0.064065	3.079780
332.835832	3203.320907	17.468621	-0.064006	3.076077
332.936763	3195.240835	17.473626	-0.064020	3.072311
332.848602	3187.270945	17.478631	-0.063998	3.068584
333.160203	3179.218086	17.483635	-0.064051	3.064832
332.852045	3171.325747	17.488640	-0.063989	3.061121
332.867934	3163.321004	17.493645	-0.063986	3.057368
332.867842	3155.323758	17.498650	-0.063981	3.053614
333.174055	3147.298463	17.503655	-0.064033	3.049856
332.734614	3139.362057	17.508659	-0.063946	3.046100
333.037354	3131.363357	17.513664	-0.063997	3.042345
332.788452	3123.434813	17.518669	-0.063946	3.038592
332.568165	3115.482147	17.523674	-0.063899	3.034825
332.782249	3107.468733	17.528679	-0.063934	3.031045
332.509963	3099.469661	17.533683	-0.063878	3.027244
332.531443	3091.476756	17.538688	-0.063877	3.023455
332.527085	3083.508422	17.543693	-0.063871	3.019672
332.445178	3075.555667	17.548698	-0.063851	3.015887
332.632728	3067.533213	17.553703	-0.063880	3.012078
332.298752	3059.569706	17.558707	-0.063813	3.008266
332.389276	3051.581066	17.563712	-0.063824	3.004459
332.287762	3043.608630	17.568717	-0.063800	3.000645
332.308906	3035.622186	17.573722	-0.063799	2.996825
332.645093	3027.580914	17.578727	-0.063856	2.992991
332.874703	3019.555351	17.583731	-0.063894	2.989154
332.584395	3011.630281	17.588736	-0.063835	2.985333
332.777911	3003.640063	17.593741	-0.063866	2.981501
332.812968	2995.668035	17.598746	-0.063867	2.977665
332.464715	2987.763856	17.603751	-0.063797	2.973836
332.201155	2979.741944	17.608755	-0.063743	2.969950
332.490383	2971.726246	17.613760	-0.063791	2.966091
332.364542	2963.780742	17.618765	-0.063763	2.962239
332.529421	2955.761212	17.623770	-0.063788	2.958362
332.579713	2947.807680	17.628775	-0.063792	2.954505
332.606857	2939.798326	17.633779	-0.063792	2.950615
332.729700	2931.805084	17.638784	-0.063810	2.946733
332.612059	2923.837137	17.643789	-0.063783	2.942845
332.383259	2915.876636	17.648794	-0.063735	2.938950
332.561304	2907.935086	17.653799	-0.063763	2.935080
332.473462	2899.911365	17.658803	-0.063741	2.931151
332.315377	2891.956530	17.663808	-0.063707	2.927247
332.003407	2884.023042	17.668813	-0.063644	2.923339
331.968492	2876.004842	17.673818	-0.063632	2.919400
332.136137	2868.025770	17.678823	-0.063658	2.915486
332.132552	2859.986380	17.683827	-0.063652	2.911527
332.037355	2852.013050	17.688832	-0.063629	2.907590
331.882024	2844.019994	17.693837	-0.063595	2.903635
332.004608	2836.025796	17.698842	-0.063613	2.899690
332.117131	2828.076940	17.703847	-0.063628	2.895761
331.820564	2820.091528	17.708851	-0.063568	2.891786
332.064761	2812.074761	17.713856	-0.063608	2.887819
331.926398	2804.136383	17.718861	-0.063577	2.883865
331.868281	2796.183003	17.723866	-0.063561	2.879903
331.569377	2788.266526	17.728871	-0.063500	2.875940
331.622066	2780.241998	17.733875	-0.063505	2.871937
331.546432	2772.263133	17.738880	-0.063486	2.867944
331.472806	2764.272132	17.743885	-0.063467	2.863940
331.384287	2756.307109	17.748890	-0.063445	2.859942
331.372805	2748.345745	17.753895	-0.063438	2.855945
331.503384	2740.320374	17.758899	-0.063457	2.851919
331.275978	2732.365747	17.763904	-0.063409	2.847901
331.522550	2724.329250	17.768909	-0.063450	2.843864
331.528216	2716.378607	17.773914	-0.063446	2.839851
331.337692	2708.477766	17.778919	-0.063405	2.835845
331.376521	2700.460753	17.783923	-0.063407	2.831789
331.474219	2692.443502	17.788928	-0.063420	2.827730
331.387888	2684.452181	17.793933	-0.063399	2.823668
331.267938	2676.507585	17.798938	-0.063371	2.819621
331.221798	2668.560400	17.803943	-0.063358	2.815572
331.016428	2660.567271	17.808947	-0.063314	2.811484
330.829909	2652.600186	17.813952	-0.063274	2.807405
331.074987	2644.571389	17.818957	-0.063315	2.803313
331.299022	2636.559065	17.823962	-0.063351	2.799223
331.420860	2628.635948	17.828967	-0.063369	2.795167
331.308378	2620.645977	17.833971	-0.063343	2.791056
331.423926	2612.656296	17.838976	-0.063359	2.786953
331.307362	2604.709781	17.843981	-0.063332	2.782852
331.087298	2596.760598	17.848986	-0.063286	2.778738
331.240504	2588.790249	17.853991	-0.063309	2.774629
331.241040	2580.763403	17.858995	-0.063304	2.770475
331.359187	2572.794302	17.864000	-0.063321	2.766353
331.291994	2564.836692	17.869005	-0.063303	2.762219
330.926082	2556.918015	17.874010	-0.063230	2.758080
331.102096	2548.905777	17.879015	-0.063258	2.753920
331.001848	2540.863581	17.884019	-0.063234	2.749721
331.162712	2532.883298	17.889024	-0.063258	2.745564
330.964946	2524.963138	17.894029	-0.063216	2.741410
331.093277	2516.944075	17.899034	-0.063235	2.737218
330.968098	2509.026425	17.904039	-0.063207	2.733057
330.877974	2501.025847	17.909043	-0.063185	2.728848
330.758927	2493.070184	17.914048	-0.063157	2.724655
330.483010	2485.150426	17.919053	-0.063101	2.720464
330.451807	2477.172192	17.924058	-0.063090	2.716251
330.653488	2469.154663	17.929063	-0.063122	2.712026
330.437644	2461.182261	17.934067	-0.063077	2.707791
330.575728	2453.198463	17.939072	-0.063097	2.703566
330.542370	2445.221990	17.944077	-0.063086	2.699328
330.191263	2437.310111	17.949082	-0.063015	2.695097
330.132148	2429.334963	17.954087	-0.062999	2.690844
330.425745	2421.276318	17.959091	-0.063048	2.686563
330.367351	2413.342137	17.964096	-0.063032	2.682318
330.384611	2405.379837	17.969101	-0.063030	2.678057
330.259974	2397.419627	17.974106	-0.063002	2.673781
330.295894	2389.440352	17.979111	-0.063004	2.669498
330.240290	2381.442753	17.984115	-0.062988	2.665192
330.328477	2373.470544	17.989120	-0.062999	2.660903
330.214734	2365.511710	17.994125	-0.062973	2.656601
329.984199	2357.575038	17.999130	-0.062925	2.652295
329.917454	2349.601773	18.004135	-0.062907	2.647974
330.019284	2341.586773	18.009139	-0.062921	2.643635
330.127412	2333.620845	18.014144	-0.062936	2.639315
329.790271	2325.730868	18.019149	-0.062868	2.635000
329.622774	2317.740488	18.024154	-0.062832	2.630634
330.007933	2309.704411	18.029159	-0.062898	2.626273
329.587605	2301.786402	18.034163	-0.062815	2.621915
329.458761	2293.830609	18.039168	-0.062785	2.617549
329.665963	2285.822270	18.044173	-0.062819	2.613170
329.482747	2277.846879	18.049178	-0.062779	2.608775
329.705206	2269.850877	18.054183	-0.062816	2.604389
329.660188	2261.912552	18.059187	-0.062802	2.600008
329.508198	2253.997693	18.064192	-0.062769	2.595626
329.356772	2245.944267	18.069197	-0.062735	2.591160
329.263795	2237.920515	18.074202	-0.062713	2.586707
329.401135	2229.969459	18.079207	-0.062733	2.582302
329.436533	2221.989814	18.084211	-0.062735	2.577867
329.431423	2214.026770	18.089216	-0.062728	2.573431
329.473913	2206.071693	18.094221	-0.062731	2.568995
329.250804	2198.124195	18.099226	-0.062684	2.564536
329.316824	2190.190598	18.104231	-0.062692	2.560098
329.361622	2182.212530	18.109235	-0.062695	2.555626
328.954580	2174.338295	18.114240	-0.062614	2.551172
329.012463	2166.296681	18.119245	-0.062619	2.546649
329.043131	2158.328663	18.124250	-0.062620	2.542158
329.369404	2150.343127	18.129255	-0.062675	2.537671
328.994360	2142.406227	18.134259	-0.062600	2.533152
329.159583	2134.408142	18.139264	-0.062626	2.528629
329.121802	2126.460305	18.144269	-0.062614	2.524113
329.159730	2118.498848	18.149274	-0.062616	2.519586
328.893385	2110.598661	18.154279	-0.062561	2.515063
328.745514	2102.615024	18.159283	-0.062528	2.510493
328.951014	2094.606468	18.164288	-0.062561	2.505927
328.424410	2086.722665	18.169293	-0.062458	2.501369
328.571079	2078.703806	18.174298	-0.062480	2.496776
328.747768	2070.715488	18.179303	-0.062508	2.492194
328.509677	2062.767149	18.184307	-0.062458	2.487596
328.902668	2054.739072	18.189312	-0.062526	2.482990
328.895173	2046.821157	18.194317	-0.062520	2.478410
328.474878	2038.908706	18.199322	-0.062436	2.473793
328.796161	2030.919107	18.204327	-0.062491	2.469179
328.628250	2022.949782	18.209331	-0.062454	2.464530
328.567882	2015.018105	18.214336	-0.062438	2.459903
328.706545	2007.026010	18.219341	-0.062459	2.455248
328.793768	1999.029907	18.224346	-0.062470	2.450577
328.663925	1991.119977	18.229351	-0.062440	2.445931
328.386950	1983.203190	18.234355	-0.062384	2.441260
328.126400	1975.294243	18.239360	-0.062330	2.436587
328.426141	1967.231556	18.244365	-0.062380	2.431858
327.876881	1959.323864	18.249370	-0.062273	2.427144
328.163447	1951.297960	18.254375	-0.062321	2.422417
328.040614	1943.353674	18.259379	-0.062293	2.417697
327.597891	1935.464262	18.264384	-0.062206	2.412975
328.078487	1927.391951	18.269389	-0.062290	2.408208
327.755633	1919.491758	18.274394	-0.062225	2.403470
327.884641	1911.533714	18.279399	-0.062243	2.398724
327.936825	1903.556066	18.284403	-0.062248	2.393951
327.872943	1895.602872	18.289408	-0.062231	2.389174
327.724767	1887.668927	18.294413	-0.062198	2.384392
327.576531	1879.737014	18.299418	-0.062165	2.379602
327.592135	1871.768812	18.304423	-0.062163	2.374793
327.598695	1863.794748	18.309427	-0.062159	2.369970
327.501031	1855.845355	18.314432	-0.062136	2.365144
326.650972	1848.054326	18.319437	-0.061972	2.360342
326.817377	1840.017906	18.324442	-0.061998	2.355465
326.839067	1832.055021	18.329447	-0.061997	2.350611
327.062328	1823.994351	18.334451	-0.062033	2.345703
327.081855	1816.050745	18.339456	-0.062032	2.340840
326.626694	1808.174475	18.344461	-0.061942	2.335969
326.540237	1800.211760	18.349466	-0.061921	2.331065
326.924511	1792.174049	18.354471	-0.061987	2.326144
326.781302	1784.235521	18.359475	-0.061955	2.321229
326.912703	1776.282474	18.364480	-0.061974	2.316318
326.725260	1768.384511	18.369485	-0.061934	2.311404
326.911652	1760.363659	18.374490	-0.061964	2.306435
326.670536	1752.478498	18.379495	-0.061914	2.301503
326.452809	1744.565440	18.384499	-0.061868	2.296545
326.289111	1736.627237	18.389504	-0.061832	2.291565
326.695107	1728.581475	18.394509	-0.061903	2.286556
326.417161	1720.672473	18.399514	-0.061846	2.281563
326.557351	1712.708283	18.404519	-0.061867	2.276561
326.326781	1704.759184	18.409523	-0.061819	2.271524
326.699532	1696.713023	18.414528	-0.061883	2.266468
326.647586	1688.800348	18.419533	-0.061868	2.261448
326.252648	1680.910948	18.424538	-0.061789	2.256401
326.427427	1672.952198	18.429543	-0.061817	2.251349
326.345582	1664.996534	18.434547	-0.061796	2.246265
326.244613	1657.070625	18.439552	-0.061772	2.241186
326.526281	1649.074227	18.444557	-0.061820	2.236085
326.487231	1641.152362	18.449562	-0.061807	2.230992
326.393288	1633.225096	18.454567	-0.061784	2.225879
325.992767	1625.344104	18.459571	-0.061705	2.220755
326.123420	1617.380064	18.464576	-0.061724	2.215615
325.888461	1609.457233	18.469581	-0.061675	2.210455
325.779088	1601.484899	18.474586	-0.061649	2.205263
325.844622	1593.547768	18.479591	-0.061656	2.200098
325.616752	1585.643406	18.484595	-0.061609	2.194915
325.705834	1577.662554	18.489600	-0.061620	2.189699
325.355959	1569.750523	18.494605	-0.061550	2.184475
325.451511	1561.777339	18.499610	-0.061563	2.179239
325.542498	1553.828846	18.504615	-0.061574	2.174007
325.323846	1545.895533	18.509619	-0.061528	2.168743
325.656926	1537.896077	18.514624	-0.061585	2.163475
325.256518	1530.035272	18.519629	-0.061506	2.158216
325.614743	1522.022520	18.524634	-0.061567	2.152915
325.675153	1514.089763	18.529639	-0.061573	2.147626
325.617804	1506.171520	18.534643	-0.061557	2.142323
325.425754	1498.264885	18.539648	-0.061516	2.137001
325.697969	1490.282345	18.544653	-0.061562	2.131660
325.434525	1482.384244	18.549658	-0.061508	2.126311
325.091507	1474.518858	18.554663	-0.061439	2.120962
325.026652	1466.574356	18.559667	-0.061421	2.115573
325.144598	1458.573120	18.564672	-0.061438	2.110150
324.999735	1450.650652	18.569677	-0.061406	2.104740
324.918518	1442.717464	18.574682	-0.061386	2.099316
324.911205	1434.792467	18.579687	-0.061379	2.093890
325.030751	1426.805669	18.584691	-0.061396	2.088421
325.121410	1418.853412	18.589696	-0.061408	2.082958
325.095072	1410.967273	18.594701	-0.061398	2.077514
324.808071	1403.070538	18.599706	-0.061339	2.072023
324.780338	1395.148846	18.604711	-0.061329	2.066526
324.575700	1387.230927	18.609715	-0.061286	2.060999
324.371865	1379.345666	18.614720	-0.061243	2.055479
324.350721	1371.405119	18.619725	-0.061234	2.049925
324.316796	1363.426153	18.624730	-0.061222	2.044328
324.421324	1355.516026	18.629735	-0.061236	2.038778
324.479750	1347.573771	18.634739	-0.061242	2.033185
324.261753	1339.670362	18.639744	-0.061196	2.027576
324.534608	1331.691870	18.644749	-0.061242	2.021949
324.433862	1323.762233	18.649754	-0.061218	2.016302
324.834576	1315.795500	18.654759	-0.061288	2.010666
324.781593	1307.872413	18.659763	-0.061273	2.004997
324.632298	1300.003483	18.664768	-0.061240	1.999340
324.670496	1292.099479	18.669773	-0.061242	1.993662
324.380106	1284.205565	18.674778	-0.061182	1.987940
324.074367	1276.340761	18.679783	-0.061120	1.982221
323.640184	1268.496382	18.684787	-0.061034	1.976485
323.922107	1260.472220	18.689792	-0.061082	1.970681
323.551566	1252.625942	18.694797	-0.061008	1.964917
323.333409	1244.730638	18.699802	-0.060962	1.959118
323.580223	1236.752397	18.704807	-0.061003	1.953291
323.260442	1228.872452	18.709811	-0.060938	1.947457
323.457308	1220.883133	18.714816	-0.060969	1.941582
323.604622	1212.934121	18.719821	-0.060992	1.935713
323.396821	1205.036922	18.724826	-0.060948	1.929826
323.283841	1197.144382	18.729831	-0.060922	1.923934
323.023686	1189.287119	18.734835	-0.060868	1.918034
323.204174	1181.328926	18.739840	-0.060896	1.912090
322.888345	1173.449960	18.744845	-0.060832	1.906130
322.809274	1165.532577	18.749850	-0.060813	1.900150
322.667239	1157.662927	18.754855	-0.060781	1.894180
322.606711	1149.717238	18.759859	-0.060765	1.888142
322.821938	1141.766337	18.764864	-0.060799	1.882114
323.255458	1133.805682	18.769869	-0.060875	1.876084
322.823374	1125.975450	18.774874	-0.060789	1.870033
322.585772	1118.104404	18.779879	-0.060740	1.863954
322.965954	1110.120764	18.784883	-0.060806	1.857841
323.203884	1102.180650	18.789888	-0.060845	1.851724
322.823237	1094.355052	18.794893	-0.060769	1.845603
322.648085	1086.493255	18.799898	-0.060731	1.839458
322.422115	1078.644949	18.804903	-0.060684	1.833296
322.230254	1070.744203	18.809907	-0.060643	1.827077
322.238276	1062.823945	18.814912	-0.060639	1.820845
322.180052	1054.938440	18.819917	-0.060623	1.814611
322.189709	1047.022716	18.824922	-0.060620	1.808340
322.379856	1039.096982	18.829927	-0.060650	1.802062
322.446654	1031.202775	18.834931	-0.060658	1.795771
322.430483	1023.286169	18.839936	-0.060649	1.789430
321.838181	1015.490229	18.844941	-0.060534	1.783091
322.164434	1007.532716	18.849946	-0.060590	1.776715
321.943970	999.690309	18.854951	-0.060543	1.770340
321.659259	991.828036	18.859955	-0.060485	1.763918
322.631551	983.761578	18.864960	-0.060661	1.757466
322.281136	975.981105	18.869965	-0.060591	1.751055
322.292510	968.076460	18.874970	-0.060588	1.744565
322.198407	960.239849	18.879975	-0.060565	1.738093
322.198858	952.364303	18.884979	-0.060560	1.731577
322.148464	944.472512	18.889984	-0.060546	1.725016
322.230654	936.619552	18.894989	-0.060556	1.718480
321.888675	928.801474	18.899994	-0.060487	1.711892
322.193036	920.856369	18.904999	-0.060539	1.705257
321.941657	913.029011	18.910003	-0.060487	1.698622
321.750088	905.179899	18.915008	-0.060446	1.691951
321.840241	897.289707	18.920013	-0.060458	1.685256
322.023721	889.382495	18.925018	-0.060487	1.678532
321.880710	881.566983	18.930023	-0.060455	1.671816
321.876519	873.678117	18.935027	-0.060449	1.665028
322.010074	865.820508	18.940032	-0.060469	1.658259
321.890061	857.976332	18.945037	-0.060441	1.651438
321.219867	850.226393	18.950042	-0.060311	1.644595
321.949666	842.250186	18.955047	-0.060442	1.637720
321.584759	834.433675	18.960051	-0.060369	1.630803
321.176126	826.617212	18.965056	-0.060288	1.623851
321.321873	818.742097	18.970061	-0.060310	1.616895
321.348910	810.853190	18.975066	-0.060310	1.609880
321.350365	803.012964	18.980071	-0.060305	1.602874
321.166296	795.198989	18.985075	-0.060266	1.595835
321.334070	787.317617	18.990080	-0.060292	1.588754
321.156273	779.500764	18.995085	-0.060253	1.581650
321.181291	771.642365	19.000090	-0.060253	1.574505
321.461719	763.768310	19.005095	-0.060300	1.567351
320.975285	756.017063	19.010099	-0.060204	1.560164
321.079725	748.169514	19.015104	-0.060219	1.552942
321.322372	740.288757	19.020109	-0.060259	1.545677
321.024114	732.509711	19.025114	-0.060198	1.538390
320.700875	724.741871	19.030119	-0.060133	1.531076
320.509020	716.921761	19.035123	-0.060092	1.523697
320.949247	709.020877	19.040128	-0.060169	1.516303
320.999326	701.195558	19.045133	-0.060173	1.508884
320.779790	693.410044	19.050138	-0.060127	1.501425
320.920180	685.583179	19.055143	-0.060148	1.493945
320.418416	677.855560	19.060147	-0.060050	1.486422
320.372549	670.054969	19.065152	-0.060036	1.478862
320.373091	662.228359	19.070157	-0.060031	1.471245
320.267106	654.403194	19.075162	-0.060006	1.463573
320.122419	646.632421	19.080167	-0.059974	1.455908
319.989019	638.840468	19.085171	-0.059945	1.448182
319.811579	631.063740	19.090176	-0.059906	1.440424
320.029431	623.238628	19.095181	-0.059942	1.432640
319.759841	615.472445	19.100186	-0.059887	1.424792
319.907346	607.671272	19.105191	-0.059909	1.416935
319.377732	599.973681	19.110195	-0.059805	1.409025
319.502207	592.157995	19.115200	-0.059823	1.401061
318.866713	584.509254	19.120205	-0.059700	1.393093
318.733082	576.708395	19.125210	-0.059670	1.385008
318.706180	568.938351	19.130215	-0.059660	1.376925
318.398436	561.189658	19.135219	-0.059598	1.368769
318.532538	553.378027	19.140224	-0.059618	1.360575
319.145652	545.513376	19.145229	-0.059727	1.352360
318.895886	537.786669	19.150234	-0.059675	1.344088
319.101022	530.024280	19.155239	-0.059708	1.335808
319.345525	522.227340	19.160243	-0.059749	1.327447
318.830461	514.601924	19.165248	-0.059648	1.319080
318.821815	506.825719	19.170253	-0.059641	1.310588
318.459994	499.115498	19.175258	-0.059569	1.302048
319.120667	491.270592	19.180263	-0.059687	1.293493
319.269865	483.517191	19.185267	-0.059709	1.284887
319.153603	475.858751	19.190272	-0.059683	1.276279
319.006162	468.193562	19.195277	-0.059650	1.267599
318.680742	460.547437	19.200282	-0.059585	1.258847
318.915854	452.813800	19.205287	-0.059624	1.250042
318.852294	445.135327	19.210291	-0.059607	1.241180
318.701354	437.481873	19.215296	-0.059574	1.232266
318.942919	429.753366	19.220301	-0.059614	1.223277
318.641440	422.130715	19.225306	-0.059552	1.214238
318.090587	414.565826	19.230311	-0.059445	1.205148
318.149166	406.887061	19.235315	-0.059451	1.195978
317.868294	399.275170	19.240320	-0.059394	1.186747
317.972360	391.601675	19.245325	-0.059408	1.177449
318.077155	383.922136	19.250330	-0.059423	1.168070
317.946908	376.322159	19.255335	-0.059393	1.158664
317.869127	368.687473	19.260339	-0.059374	1.149148
317.706489	361.082934	19.265344	-0.059339	1.139573
317.941000	353.423563	19.270349	-0.059377	1.129933
317.736628	345.848754	19.275354	-0.059334	1.120222
317.396671	338.328939	19.280359	-0.059266	1.110467
317.212615	330.758326	19.285363	-0.059227	1.100595
317.339507	323.150285	19.290368	-0.059246	1.090654
317.209172	315.620320	19.295373	-0.059216	1.080666
316.712848	308.142483	19.300378	-0.059119	1.070570
316.357048	300.643143	19.305383	-0.059048	1.060382
316.645008	293.027323	19.310387	-0.059097	1.050088
316.423389	285.537343	19.315392	-0.059051	1.039744
316.557864	277.993414	19.320397	-0.059071	1.029306
316.488183	270.492116	19.325402	-0.059053	1.018772
316.219376	263.063261	19.330407	-0.058998	1.008182
316.535520	255.516641	19.335411	-0.059052	0.997456
316.008116	248.130830	19.340416	-0.058949	0.986634
316.030064	240.670473	19.345421	-0.058948	0.975722
315.601069	233.290247	19.350426	-0.058863	0.964690
315.601723	225.873341	19.355431	-0.058859	0.953587
315.176525	218.530608	19.360435	-0.058775	0.942353
315.692874	211.029645	19.365440	-0.058866	0.930994
315.385308	203.724079	19.370445	-0.058804	0.919574
315.200505	196.389136	19.375450	-0.058765	0.907998
315.429552	189.011092	19.380455	-0.058803	0.896319
315.374155	181.695196	19.385459	-0.058788	0.884507
315.376709	174.401417	19.390464	-0.058783	0.872587
315.426467	167.124407	19.395469	-0.058788	0.860544
315.357031	159.890099	19.400474	-0.058770	0.848367
315.136084	152.717085	19.405479	-0.058724	0.836072
314.841172	145.546416	19.410483	-0.058665	0.823575
314.553989	138.412863	19.415488	-0.058607	0.810953
314.377129	131.293683	19.420493	-0.058569	0.798192
314.190826	124.192624	19.425498	-0.058530	0.785254
314.843950	116.977854	19.430503	-0.058647	0.772164
314.452734	109.993781	19.435507	-0.058569	0.758935
314.344024	102.984764	19.440512	-0.058545	0.745519
314.124609	96.032867	19.445517	-0.058499	0.731930
314.078698	89.075589	19.450522	-0.058486	0.718136
313.950732	82.186133	19.455527	-0.058458	0.704179
313.678070	75.537190	19.460531	-0.058403	0.690387