Fri Apr 16 18:33:02 2021

Number of Points = 3642
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.672809	0.086253	0.000000	0.000094	0.307355

1.278780	-0.024867	0.005005	-0.000018	0.307350
1.004184	0.025789	0.010010	0.000033	0.307353
0.875024	0.049227	0.015014	0.000057	0.307352
0.384724	0.144745	0.020019	0.000148	0.307382
0.806248	0.063064	0.025024	0.000070	0.307357
0.701522	0.085279	0.030029	0.000090	0.307372
0.624034	0.097140	0.035034	0.000104	0.307361
0.968622	0.031635	0.040038	0.000040	0.307347
0.996754	-0.013101	0.045043	0.000035	0.307159
1.098598	-0.060736	0.050048	0.000016	0.307022
0.893446	-0.021341	0.055053	0.000055	0.307031
1.120413	-0.063203	0.060058	0.000013	0.307027
1.077462	-0.057304	0.065062	0.000021	0.307018
1.351623	-0.106134	0.070067	-0.000030	0.307022
1.213257	-0.083374	0.075072	-0.000004	0.307010
1.840481	-0.197921	0.080077	-0.000121	0.307007
1.732783	-0.181711	0.085082	-0.000101	0.306991
1.370978	-0.172019	0.090086	-0.000033	0.306726
1.414352	-0.177791	0.095091	-0.000041	0.306735
1.457148	-0.188769	0.100096	-0.000049	0.306719
1.614225	-0.215946	0.105101	-0.000078	0.306725
1.658993	-0.225318	0.110106	-0.000086	0.306719
1.852356	-0.314546	0.115110	-0.000122	0.306463
2.026992	-0.364043	0.120115	-0.000155	0.306379
1.726009	-0.310139	0.125120	-0.000098	0.306374
1.935524	-0.347085	0.130125	-0.000137	0.306379
1.765894	-0.366767	0.135130	-0.000106	0.306140
1.685258	-0.366852	0.140134	-0.000090	0.306070
1.665006	-0.360597	0.145139	-0.000087	0.306081
1.438809	-0.320520	0.150144	-0.000044	0.306076
1.410767	-0.380959	0.155149	-0.000039	0.305765
1.726712	-0.440306	0.160154	-0.000098	0.305756
1.439312	-0.386311	0.165158	-0.000044	0.305763
1.362373	-0.400434	0.170163	-0.000030	0.305630
1.300717	-0.415439	0.175168	-0.000018	0.305505
1.380432	-0.428066	0.180173	-0.000033	0.305513
1.785032	-0.526704	0.185178	-0.000108	0.305394
1.866472	-0.594292	0.190182	-0.000123	0.305143
1.739298	-0.567344	0.195187	-0.000099	0.305161
1.700206	-0.597345	0.200192	-0.000092	0.304984
1.585961	-0.606192	0.205197	-0.000070	0.304843
1.836354	-0.653302	0.210202	-0.000117	0.304835
1.600478	-0.667746	0.215206	-0.000073	0.304562
1.581178	-0.673459	0.220211	-0.000069	0.304518
1.526333	-0.680693	0.225216	-0.000059	0.304436
1.576757	-0.732411	0.230221	-0.000068	0.304233
1.525726	-0.723638	0.235226	-0.000058	0.304230
1.600044	-0.795961	0.240230	-0.000072	0.303949
1.844623	-0.852913	0.245235	-0.000117	0.303889
1.898554	-0.899819	0.250240	-0.000127	0.303712
1.904354	-0.930117	0.255245	-0.000128	0.303572
1.824908	-0.942952	0.260250	-0.000113	0.303441
1.841026	-0.987397	0.265254	-0.000116	0.303243
1.804490	-0.997194	0.270259	-0.000109	0.303164
1.649658	-1.013863	0.275264	-0.000080	0.302949
1.701898	-1.037804	0.280269	-0.000090	0.302880
1.539638	-1.061426	0.285274	-0.000059	0.302625
1.632091	-1.094278	0.290278	-0.000076	0.302548
1.599717	-1.136944	0.295283	-0.000070	0.302315
1.715189	-1.180526	0.300288	-0.000092	0.302206
1.577388	-1.201176	0.305293	-0.000066	0.301987
1.513791	-1.213767	0.310298	-0.000054	0.301871
1.754864	-1.296196	0.315302	-0.000099	0.301685
1.617957	-1.310303	0.320307	-0.000073	0.301497
1.509594	-1.319279	0.325312	-0.000053	0.301359
1.566274	-1.378575	0.330317	-0.000063	0.301123
1.303697	-1.343422	0.335322	-0.000014	0.301062
1.116454	-1.373576	0.340326	0.000021	0.300753
1.668118	-1.489033	0.345331	-0.000082	0.300679
1.265412	-1.451426	0.350336	-0.000006	0.300508
1.690953	-1.571336	0.355341	-0.000085	0.300302
1.443549	-1.555669	0.360346	-0.000039	0.300160
1.444014	-1.617006	0.365350	-0.000039	0.299864
1.489460	-1.651579	0.370355	-0.000048	0.299737
1.238784	-1.651994	0.375360	-0.000001	0.299514
1.411412	-1.724675	0.380365	-0.000033	0.299314
1.263320	-1.726261	0.385370	-0.000005	0.299175
1.087425	-1.750350	0.390374	0.000028	0.298904
1.113380	-1.792488	0.395379	0.000023	0.298722
1.077345	-1.816536	0.400384	0.000030	0.298573
0.600217	-1.786866	0.405389	0.000119	0.298296
0.490644	-1.794301	0.410394	0.000140	0.298163
0.999151	-1.922411	0.415398	0.000045	0.297989
1.241573	-2.031011	0.420403	0.000000	0.297675
0.911693	-2.006890	0.425408	0.000062	0.297500
1.052040	-2.069057	0.430413	0.000036	0.297321
1.112106	-2.145271	0.435418	0.000025	0.297002
1.204446	-2.202017	0.440422	0.000008	0.296807
1.264566	-2.250442	0.445427	-0.000003	0.296624
0.950058	-2.241446	0.450432	0.000055	0.296388
1.100876	-2.325432	0.455437	0.000027	0.296111
0.924280	-2.336386	0.460442	0.000060	0.295900
0.684531	-2.329770	0.465446	0.000105	0.295719
0.429933	-2.321033	0.470451	0.000153	0.295534
0.761487	-2.442595	0.475456	0.000091	0.295233
0.763544	-2.485228	0.480461	0.000091	0.295026
0.166803	-2.416850	0.485466	0.000202	0.294828
0.557625	-2.549861	0.490470	0.000130	0.294524
0.578937	-2.599742	0.495475	0.000126	0.294297
0.357798	-2.607235	0.500480	0.000167	0.294062
0.588770	-2.696578	0.505485	0.000124	0.293828
0.661666	-2.757824	0.510490	0.000111	0.293591
0.424289	-2.779677	0.515494	0.000155	0.293270
0.310231	-2.800570	0.520499	0.000176	0.293064
-0.104033	-2.774956	0.525504	0.000254	0.292818
-0.240628	-2.795853	0.530509	0.000279	0.292591
-1.110644	-2.688102	0.535514	0.000441	0.292341
-1.921239	-2.594537	0.540518	0.000592	0.292074
-1.825112	-2.644013	0.545523	0.000575	0.291915
-2.634462	-2.533727	0.550528	0.000725	0.291732
-2.999534	-2.524325	0.555533	0.000793	0.291449
-2.797635	-2.593634	0.560538	0.000756	0.291286
-2.664331	-2.662411	0.565542	0.000731	0.291064
-3.185959	-2.617325	0.570547	0.000829	0.290816
-3.469947	-2.592978	0.575552	0.000882	0.290680
-3.597812	-2.604532	0.580557	0.000905	0.290506
-4.173993	-2.547478	0.585562	0.001013	0.290268
-4.387896	-2.533780	0.590566	0.001053	0.290142
-4.083864	-2.649649	0.595571	0.000996	0.289839
-4.693074	-2.568474	0.600576	0.001110	0.289690
-5.858520	-2.386366	0.605581	0.001327	0.289541
-5.634089	-2.467203	0.610586	0.001285	0.289340
-6.142895	-2.393253	0.615590	0.001380	0.289247
-6.149940	-2.443929	0.620595	0.001382	0.288986
-6.821808	-2.333687	0.625600	0.001507	0.288926
-6.474008	-2.454054	0.630605	0.001442	0.288639
-6.979968	-2.369816	0.635610	0.001536	0.288600
-7.001876	-2.429287	0.640614	0.001541	0.288281
-6.919254	-2.447309	0.645619	0.001525	0.288265
-7.486466	-2.400573	0.650624	0.001631	0.287981
-7.569007	-2.389688	0.655629	0.001647	0.287960
-7.754317	-2.418311	0.660634	0.001681	0.287646
-7.727949	-2.430946	0.665638	0.001676	0.287606
-8.081485	-2.420243	0.670643	0.001742	0.287336
-8.306532	-2.385177	0.675648	0.001784	0.287306
-8.401792	-2.427067	0.680653	0.001802	0.287007
-8.628859	-2.387319	0.685658	0.001845	0.286998
-9.161866	-2.345133	0.690662	0.001944	0.286722
-8.609615	-2.444744	0.695667	0.001841	0.286725
-8.994995	-2.437994	0.700672	0.001913	0.286405
-9.252867	-2.395920	0.705677	0.001961	0.286380
-9.468736	-2.408164	0.710682	0.002002	0.286119
-9.639712	-2.387209	0.715686	0.002034	0.286067
-9.785308	-2.401987	0.720691	0.002061	0.285858
-10.051435	-2.376045	0.725696	0.002111	0.285743
-10.140295	-2.382498	0.730701	0.002127	0.285628
-10.348245	-2.368874	0.735706	0.002166	0.285505
-10.431315	-2.377226	0.740710	0.002182	0.285385
-10.407716	-2.425641	0.745715	0.002177	0.285161
-11.051099	-2.315227	0.750720	0.002297	0.285127
-11.179215	-2.346753	0.755725	0.002321	0.284848
-11.219028	-2.339387	0.760730	0.002329	0.284848
-11.765777	-2.289468	0.765734	0.002431	0.284596
-11.927156	-2.272863	0.770739	0.002461	0.284531
-11.905904	-2.298084	0.775744	0.002457	0.284421
-11.561844	-2.397895	0.780749	0.002393	0.284231
-11.791384	-2.362844	0.785754	0.002436	0.284196
-12.681251	-2.259048	0.790758	0.002602	0.283900
-12.353390	-2.317222	0.795763	0.002541	0.283907
-12.249217	-2.378977	0.800768	0.002522	0.283688
-12.450875	-2.362604	0.805773	0.002559	0.283584
-12.464704	-2.382013	0.810778	0.002562	0.283471
-12.982490	-2.328462	0.815782	0.002658	0.283263
-13.148879	-2.295261	0.820787	0.002690	0.283278
-13.607103	-2.267944	0.825792	0.002775	0.282991
-13.643776	-2.263274	0.830797	0.002782	0.282980
-13.719164	-2.275172	0.835802	0.002796	0.282849
-13.671580	-2.327659	0.840806	0.002787	0.282623
-13.450184	-2.366559	0.845811	0.002746	0.282630
-14.004637	-2.325520	0.850816	0.002850	0.282323
-14.146774	-2.299409	0.855821	0.002876	0.282324
-14.291905	-2.304667	0.860826	0.002903	0.282161
-14.251732	-2.346683	0.865830	0.002896	0.281982
-14.362737	-2.324966	0.870835	0.002917	0.281989
-14.977671	-2.268178	0.875840	0.003031	0.281706
-14.640943	-2.329664	0.880845	0.002969	0.281704
-15.033267	-2.290642	0.885850	0.003042	0.281537
-15.577268	-2.223142	0.890854	0.003143	0.281375
-15.711517	-2.193890	0.895859	0.003168	0.281400
-15.629851	-2.260669	0.900864	0.003153	0.281132
-16.318207	-2.141834	0.905869	0.003282	0.281099
-16.496688	-2.110111	0.910874	0.003315	0.281094
-16.220157	-2.224073	0.915878	0.003264	0.280765
-16.098361	-2.247939	0.920883	0.003241	0.280756
-16.390401	-2.207986	0.925888	0.003296	0.280688
-16.626829	-2.193882	0.930893	0.003340	0.280538
-16.616594	-2.196818	0.935898	0.003338	0.280532
-16.507075	-2.256980	0.940902	0.003318	0.280323
-16.799686	-2.231867	0.945907	0.003372	0.280178
-17.373532	-2.125187	0.950912	0.003479	0.280189
-16.855929	-2.275162	0.955917	0.003383	0.279900
-17.573952	-2.151632	0.960922	0.003517	0.279863
-17.558345	-2.160412	0.965926	0.003514	0.279831
-17.260128	-2.272444	0.970931	0.003459	0.279532
-17.793582	-2.175705	0.975936	0.003558	0.279530
-17.216204	-2.307755	0.980941	0.003451	0.279389
-17.902487	-2.208866	0.985946	0.003579	0.279254
-17.638696	-2.262573	0.990950	0.003530	0.279224
-17.975916	-2.255982	0.995955	0.003593	0.278939
-17.745732	-2.307516	1.000960	0.003550	0.278888
-17.768387	-2.325873	1.005965	0.003554	0.278771
-17.852144	-2.349540	1.010970	0.003570	0.278568
-18.041501	-2.314564	1.015974	0.003605	0.278570
-18.475286	-2.289901	1.020979	0.003686	0.278288
-19.087947	-2.182918	1.025984	0.003800	0.278264
-19.002261	-2.209806	1.030989	0.003785	0.278205
-18.606552	-2.326301	1.035994	0.003711	0.277972
-18.675847	-2.316114	1.040998	0.003724	0.277959
-19.076212	-2.289026	1.046003	0.003799	0.277720
-19.202126	-2.283380	1.051008	0.003822	0.277630
-18.861865	-2.360752	1.056013	0.003759	0.277548
-19.705857	-2.249964	1.061018	0.003916	0.277325
-19.793439	-2.234199	1.066022	0.003933	0.277324
-19.808530	-2.269154	1.071027	0.003936	0.277126
-20.531321	-2.162136	1.076032	0.004070	0.276998
-20.387722	-2.186047	1.081037	0.004044	0.277009
-20.300452	-2.248190	1.086042	0.004028	0.276766
-20.872528	-2.153339	1.091046	0.004134	0.276718
-20.913607	-2.149222	1.096051	0.004142	0.276699
-20.971641	-2.199598	1.101056	0.004153	0.276380
-20.694103	-2.249755	1.106061	0.004101	0.276381
-21.208454	-2.174623	1.111066	0.004197	0.276284
-21.639462	-2.135017	1.116070	0.004278	0.276080
-21.419678	-2.173603	1.121075	0.004237	0.276087
-21.467034	-2.198735	1.126080	0.004246	0.275909
-22.046085	-2.118818	1.131085	0.004354	0.275775
-21.325101	-2.252989	1.136090	0.004220	0.275758
-21.455997	-2.266769	1.141094	0.004244	0.275560
-22.310654	-2.117961	1.146099	0.004403	0.275525
-22.565019	-2.071024	1.151104	0.004451	0.275528
-22.238752	-2.191968	1.156109	0.004390	0.275203
-22.625230	-2.125816	1.161114	0.004462	0.275181
-22.876882	-2.084914	1.166118	0.004509	0.275155
-22.275800	-2.249305	1.171123	0.004398	0.274864
-22.447669	-2.220531	1.176128	0.004430	0.274850
-22.822182	-2.178502	1.181133	0.004499	0.274712
-22.798629	-2.217343	1.186138	0.004495	0.274530
-22.676953	-2.240605	1.191142	0.004473	0.274523
-23.375198	-2.155985	1.196147	0.004603	0.274299
-23.525600	-2.139325	1.201152	0.004631	0.274242
-23.353086	-2.171928	1.206157	0.004599	0.274235
-23.472127	-2.211898	1.211162	0.004621	0.273909
-23.718073	-2.167745	1.216166	0.004667	0.273905
-23.455423	-2.236093	1.221171	0.004618	0.273795
-23.839051	-2.205730	1.226176	0.004690	0.273586
-23.723658	-2.224885	1.231181	0.004669	0.273595
-23.894340	-2.241189	1.236186	0.004700	0.273344
-24.035452	-2.230932	1.241190	0.004727	0.273262
-24.147197	-2.218551	1.246195	0.004748	0.273219
-24.577972	-2.183864	1.251200	0.004828	0.272987
-24.340427	-2.227692	1.256205	0.004784	0.272983
-24.572319	-2.222239	1.261210	0.004827	0.272788
-25.186814	-2.137603	1.266214	0.004942	0.272643
-24.876687	-2.190622	1.271219	0.004884	0.272660
-25.401215	-2.145815	1.276224	0.004982	0.272391
-25.195903	-2.194774	1.281229	0.004944	0.272329
-25.198625	-2.200570	1.286234	0.004945	0.272295
-25.070951	-2.279669	1.291238	0.004921	0.271997
-25.571959	-2.184436	1.296243	0.005014	0.272018
-26.085303	-2.120109	1.301248	0.005110	0.271863
-26.306914	-2.102883	1.306253	0.005151	0.271739
-26.163951	-2.129980	1.311258	0.005125	0.271733
-26.732573	-2.067893	1.316262	0.005231	0.271512
-26.756449	-2.083409	1.321267	0.005235	0.271405
-26.391640	-2.153244	1.326272	0.005168	0.271386
-26.397867	-2.198024	1.331277	0.005169	0.271140
-26.902261	-2.116140	1.336282	0.005263	0.271087
-26.785307	-2.143111	1.341286	0.005241	0.271056
-26.900807	-2.174986	1.346291	0.005263	0.270773
-27.119189	-2.137195	1.351296	0.005304	0.270762
-27.063488	-2.163963	1.356301	0.005293	0.270672
-27.326400	-2.145162	1.361306	0.005343	0.270516
-27.494598	-2.115268	1.366310	0.005374	0.270512
-27.191503	-2.211976	1.371315	0.005318	0.270288
-27.298529	-2.217525	1.376320	0.005338	0.270154
-27.573037	-2.173253	1.381325	0.005389	0.270123
-27.956074	-2.154942	1.386330	0.005460	0.269847
-28.070730	-2.133980	1.391334	0.005482	0.269847
-27.855188	-2.199584	1.396339	0.005442	0.269704
-28.362830	-2.142058	1.401344	0.005536	0.269517
-27.846343	-2.236916	1.406349	0.005440	0.269511
-27.978199	-2.258959	1.411354	0.005465	0.269263
-28.550801	-2.161588	1.416358	0.005572	0.269226
-28.649829	-2.159690	1.421363	0.005590	0.269139
-29.134851	-2.114729	1.426368	0.005681	0.268905
-29.051755	-2.129666	1.431373	0.005665	0.268906
-29.559152	-2.063499	1.436378	0.005760	0.268764
-29.355814	-2.132025	1.441382	0.005722	0.268594
-29.397920	-2.122684	1.446387	0.005730	0.268602
-29.748060	-2.105542	1.451392	0.005796	0.268350
-29.445844	-2.175714	1.456397	0.005740	0.268268
-29.643235	-2.143629	1.461402	0.005776	0.268247
-29.949315	-2.138017	1.466406	0.005833	0.267976
-30.069476	-2.112510	1.471411	0.005856	0.267995
-30.392108	-2.076461	1.476416	0.005916	0.267872
-30.697025	-2.060636	1.481421	0.005973	0.267657
-29.981492	-2.194368	1.486426	0.005840	0.267637
-30.262976	-2.181742	1.491430	0.005893	0.267427
-30.423261	-2.171078	1.496435	0.005922	0.267326
-30.872729	-2.091247	1.501440	0.006006	0.267315
-30.907435	-2.141199	1.506445	0.006013	0.267010
-30.775533	-2.167046	1.511450	0.005988	0.266999
-31.037702	-2.139712	1.516454	0.006037	0.266888
-31.106147	-2.159294	1.521459	0.006050	0.266713
-30.850147	-2.208276	1.526464	0.006003	0.266700
-30.964272	-2.238238	1.531469	0.006024	0.266424
-31.390708	-2.170575	1.536474	0.006104	0.266369
-31.575956	-2.153236	1.541478	0.006138	0.266279
-31.688566	-2.170652	1.546483	0.006159	0.266073
-32.083450	-2.098134	1.551488	0.006233	0.266076
-32.104790	-2.131123	1.556493	0.006237	0.265874
-32.009573	-2.171389	1.561498	0.006219	0.265749
-32.511487	-2.079232	1.566502	0.006313	0.265753
-32.337773	-2.155326	1.571507	0.006281	0.265509
-32.505622	-2.127852	1.576512	0.006312	0.265492
-32.689754	-2.117140	1.581517	0.006347	0.265367
-33.025804	-2.093098	1.586522	0.006409	0.265164
-33.101030	-2.080199	1.591526	0.006423	0.265159
-33.000285	-2.133874	1.596531	0.006405	0.264965
-33.831902	-2.005209	1.601536	0.006560	0.264841
-33.972065	-1.975954	1.606541	0.006586	0.264861
-33.276057	-2.152334	1.611546	0.006456	0.264588
-34.400638	-1.959695	1.616550	0.006666	0.264522
-34.315432	-1.973204	1.621555	0.006650	0.264532
-33.979694	-2.084785	1.626560	0.006588	0.264255
-33.744415	-2.132641	1.631565	0.006544	0.264227
-34.166387	-2.071489	1.636570	0.006623	0.264141
-34.766286	-2.006670	1.641574	0.006735	0.263897
-34.195094	-2.109948	1.646579	0.006628	0.263900
-35.023045	-1.986488	1.651584	0.006783	0.263750
-35.025380	-2.014983	1.656589	0.006783	0.263590
-34.718701	-2.070889	1.661594	0.006726	0.263589
-35.136482	-2.035852	1.666598	0.006804	0.263363
-35.375078	-2.008977	1.671603	0.006849	0.263272
-35.339710	-2.015983	1.676608	0.006842	0.263268
-35.178205	-2.089916	1.681613	0.006812	0.263022
-35.515787	-2.037962	1.686618	0.006875	0.262969
-35.167345	-2.115621	1.691622	0.006811	0.262890
-34.941952	-2.205546	1.696627	0.006769	0.262620
-35.533125	-2.097950	1.701632	0.006879	0.262619
-35.753364	-2.096758	1.706637	0.006920	0.262404
-35.691116	-2.124512	1.711642	0.006909	0.262313
-35.831013	-2.109722	1.716646	0.006935	0.262254
-36.256312	-2.078953	1.721651	0.007014	0.261995
-36.128300	-2.104619	1.726656	0.006990	0.261982
-36.177301	-2.121886	1.731661	0.007000	0.261836
-36.741923	-2.042134	1.736666	0.007105	0.261708
-36.820963	-2.028651	1.741670	0.007120	0.261703
-36.567183	-2.126406	1.746675	0.007073	0.261417
-37.177655	-2.023551	1.751680	0.007186	0.261370
-36.817481	-2.103396	1.756685	0.007119	0.261290
-37.091966	-2.091956	1.761690	0.007171	0.261076
-37.286184	-2.058970	1.766694	0.007207	0.261063
-37.138265	-2.124937	1.771699	0.007180	0.260845
-37.164149	-2.141180	1.776704	0.007184	0.260728
-36.973154	-2.184559	1.781709	0.007149	0.260680
-37.618736	-2.098955	1.786714	0.007269	0.260502
-38.074661	-2.015536	1.791718	0.007354	0.260504
-37.569373	-2.146252	1.796723	0.007260	0.260287
-38.501017	-1.998475	1.801728	0.007434	0.260166
-37.965683	-2.101997	1.806733	0.007334	0.260131
-38.329846	-2.086751	1.811738	0.007402	0.259846
-38.342003	-2.085806	1.816742	0.007405	0.259839
-38.417843	-2.101580	1.821747	0.007419	0.259673
-38.759978	-2.069921	1.826752	0.007483	0.259502
-38.255003	-2.161655	1.831757	0.007389	0.259502
-38.463954	-2.174506	1.836762	0.007428	0.259217
-38.817292	-2.111887	1.841766	0.007494	0.259207
-38.302741	-2.239588	1.846771	0.007398	0.259016
-39.002677	-2.137452	1.851776	0.007529	0.258874
-39.240079	-2.103423	1.856781	0.007573	0.258822
-39.418941	-2.114395	1.861786	0.007606	0.258578
-39.584912	-2.084506	1.866790	0.007637	0.258576
-39.745413	-2.090668	1.871795	0.007667	0.258377
-39.757861	-2.111408	1.876800	0.007670	0.258247
-40.092458	-2.051574	1.881805	0.007732	0.258241
-40.700742	-1.986053	1.886810	0.007846	0.257987
-41.134086	-1.905844	1.891814	0.007926	0.257994
-40.480076	-2.042515	1.896819	0.007805	0.257894
-40.733524	-2.042488	1.901824	0.007852	0.257634
-40.918407	-2.007691	1.906829	0.007887	0.257640
-40.769317	-2.069665	1.911834	0.007859	0.257443
-41.104201	-2.032401	1.916838	0.007921	0.257310
-40.619498	-2.125984	1.921843	0.007831	0.257279
-41.323090	-2.049841	1.926848	0.007962	0.256986
-41.309288	-2.049948	1.931853	0.007960	0.256999
-41.472057	-2.044184	1.936858	0.007990	0.256864
-41.579794	-2.054106	1.941862	0.008011	0.256696
-41.546754	-2.056463	1.946867	0.008005	0.256716
-41.531948	-2.115115	1.951872	0.008002	0.256400
-42.135362	-2.007920	1.956877	0.008114	0.256384
-42.350793	-1.982415	1.961882	0.008155	0.256306
-42.697254	-1.959157	1.966886	0.008219	0.256081
-41.849886	-2.116636	1.971891	0.008062	0.256061
-42.413851	-2.054288	1.976896	0.008167	0.255833
-42.570274	-2.041039	1.981901	0.008196	0.255746
-42.349654	-2.088218	1.986906	0.008155	0.255705
-42.940923	-2.019104	1.991910	0.008265	0.255487
-42.870992	-2.028145	1.996915	0.008252	0.255507
-43.278256	-2.001249	2.001920	0.008328	0.255239

-43.394646	-2.011049	2.011917	0.008350	0.255061
-43.813519	-1.972856	2.021914	0.008428	0.254844
-43.031394	-2.154955	2.031910	0.008283	0.254616
-43.501800	-2.088786	2.041907	0.008371	0.254505
-43.295992	-2.174513	2.051904	0.008333	0.254228
-43.680752	-2.108048	2.061901	0.008405	0.254207
-43.879028	-2.124289	2.071898	0.008442	0.253907
-43.819265	-2.139215	2.081894	0.008431	0.253883
-44.123652	-2.090908	2.091891	0.008488	0.253841
-44.229649	-2.118698	2.101888	0.008508	0.253571
-44.377481	-2.093744	2.111885	0.008536	0.253558
-44.454158	-2.076602	2.121882	0.008550	0.253575
-44.937549	-1.985911	2.131878	0.008640	0.253589
-44.539401	-2.060786	2.141875	0.008567	0.253574
-44.779524	-2.014952	2.151872	0.008612	0.253585
-45.072809	-1.960861	2.161869	0.008666	0.253588
-44.777345	-2.015744	2.171866	0.008612	0.253580
-44.538453	-2.058174	2.181862	0.008567	0.253585
-44.944941	-1.983578	2.191859	0.008643	0.253587
-45.135315	-1.945404	2.201856	0.008679	0.253606
-44.909429	-1.989361	2.211853	0.008637	0.253588
-45.000059	-1.959667	2.221850	0.008654	0.253662
-44.494131	-2.010520	2.231846	0.008560	0.253896
-44.745897	-1.963993	2.241843	0.008607	0.253899
-44.381442	-2.032029	2.251840	0.008540	0.253887
-44.311706	-2.031621	2.261837	0.008527	0.253961
-44.043110	-2.033962	2.271834	0.008477	0.254225
-43.751364	-2.088695	2.281830	0.008423	0.254214
-43.506029	-2.134034	2.291827	0.008378	0.254209
-43.228996	-2.152377	2.301824	0.008327	0.254390
-43.572756	-2.070531	2.311821	0.008391	0.254498
-43.226006	-2.133341	2.321818	0.008326	0.254499
-43.715746	-2.008687	2.331814	0.008418	0.254699
-43.577233	-2.007361	2.341811	0.008392	0.254849
-43.423006	-2.017597	2.351808	0.008364	0.254949
-43.176012	-2.025450	2.361805	0.008318	0.255158
-43.200528	-2.009788	2.371802	0.008323	0.255220
-43.285492	-1.940938	2.381798	0.008339	0.255522
-43.168460	-1.947887	2.391795	0.008317	0.255602
-42.821699	-1.982331	2.401792	0.008253	0.255763
-42.659728	-1.982912	2.411789	0.008223	0.255925
-41.947755	-2.087900	2.421786	0.008091	0.256062
-42.226216	-2.002699	2.431782	0.008143	0.256256
-42.217579	-1.980220	2.441779	0.008142	0.256391
-42.118918	-1.945646	2.451776	0.008123	0.256686
-41.834179	-1.980683	2.461773	0.008071	0.256779
-41.775490	-1.949383	2.471770	0.008060	0.257015
-41.273714	-2.005494	2.481766	0.007967	0.257212
-41.223776	-1.992189	2.491763	0.007958	0.257336
-41.475991	-1.888574	2.501760	0.008005	0.257660
-41.107465	-1.922366	2.511757	0.007937	0.257845
-40.943270	-1.919520	2.521754	0.007906	0.258028
-40.555260	-1.946087	2.531750	0.007834	0.258273
-40.346108	-1.947622	2.541747	0.007795	0.258477
-39.977687	-1.989166	2.551744	0.007727	0.258618
-39.622554	-2.003891	2.561741	0.007661	0.258896
-39.531571	-1.984488	2.571738	0.007645	0.259096
-39.183181	-2.019697	2.581734	0.007580	0.259252
-39.630048	-1.886533	2.591731	0.007663	0.259540
-39.307789	-1.901515	2.601728	0.007604	0.259782
-38.830094	-1.957567	2.611725	0.007515	0.259953
-38.487625	-1.980810	2.621722	0.007451	0.260169
-38.209880	-1.975694	2.631718	0.007400	0.260477
-38.270197	-1.935211	2.641715	0.007411	0.260640
-38.366999	-1.883934	2.651712	0.007430	0.260826
-37.918896	-1.918708	2.661709	0.007346	0.261084
-37.122100	-2.021429	2.671706	0.007198	0.261317
-37.284181	-1.956595	2.681702	0.007229	0.261511
-36.790404	-2.010449	2.691699	0.007137	0.261709
-37.152258	-1.890079	2.701696	0.007205	0.262009
-36.392419	-1.986550	2.711693	0.007063	0.262239
-36.243318	-1.980686	2.721690	0.007036	0.262419
-35.827845	-2.016841	2.731686	0.006959	0.262636
-36.004330	-1.926122	2.741683	0.006992	0.262957
-35.848747	-1.915183	2.751680	0.006963	0.263172
-35.559619	-1.930476	2.761677	0.006910	0.263376
-35.242845	-1.946730	2.771674	0.006851	0.263602
-34.951613	-1.943699	2.781670	0.006797	0.263908
-35.217690	-1.847902	2.791667	0.006847	0.264167
-34.429080	-1.953069	2.801664	0.006700	0.264375
-33.980711	-2.002871	2.811661	0.006617	0.264548
-33.435771	-2.047742	2.821658	0.006516	0.264843
-33.115817	-2.068389	2.831654	0.006456	0.265047
-33.176554	-2.019648	2.841651	0.006468	0.265252
-32.727617	-2.055518	2.851648	0.006385	0.265500
-32.704162	-2.020092	2.861645	0.006380	0.265716
-32.446565	-2.034082	2.871642	0.006333	0.265893
-31.877595	-2.104660	2.881638	0.006227	0.266071
-31.744190	-2.071715	2.891635	0.006202	0.266381
-31.952748	-1.996419	2.901632	0.006241	0.266583
-31.448587	-2.051915	2.911629	0.006148	0.266778
-31.377669	-2.023720	2.921626	0.006135	0.267000
-30.536455	-2.125079	2.931622	0.005979	0.267279
-30.598641	-2.081835	2.941619	0.005990	0.267450
-30.414465	-2.078784	2.951616	0.005956	0.267647
-30.087143	-2.077221	2.961613	0.005896	0.267976
-30.188188	-2.023700	2.971610	0.005915	0.268164
-30.164660	-1.984934	2.981606	0.005910	0.268395
-29.738003	-2.021997	2.991603	0.005831	0.268613
-29.451477	-2.019682	3.001600	0.005778	0.268905
-29.042091	-2.047313	3.011597	0.005702	0.269155
-29.269393	-1.965929	3.021594	0.005745	0.269369
-28.770370	-2.016722	3.031590	0.005652	0.269583
-28.508863	-2.012575	3.041587	0.005604	0.269859
-28.044040	-2.047435	3.051584	0.005517	0.270124
-28.023329	-2.009278	3.061581	0.005514	0.270348
-27.546015	-2.057523	3.071578	0.005425	0.270553
-27.602219	-2.003620	3.081574	0.005436	0.270785
-27.215778	-2.024910	3.091571	0.005364	0.271046
-26.691384	-2.082832	3.101568	0.005267	0.271245
-26.672534	-2.048774	3.111565	0.005263	0.271443
-26.204978	-2.082299	3.121562	0.005177	0.271717
-26.276886	-2.021531	3.131558	0.005190	0.271970
-26.016829	-2.027190	3.141555	0.005142	0.272190
-26.191106	-1.947939	3.151552	0.005175	0.272441
-25.805352	-1.973685	3.161549	0.005103	0.272676
-25.219869	-2.018858	3.171546	0.004994	0.273000
-25.051002	-2.007413	3.181542	0.004963	0.273222
-25.196338	-1.935596	3.191539	0.004990	0.273461
-24.976209	-1.928438	3.201536	0.004950	0.273710
-25.023860	-1.869245	3.211533	0.004959	0.273976
-24.498101	-1.908512	3.221530	0.004861	0.274272
-24.166250	-1.918182	3.231526	0.004800	0.274538
-24.274039	-1.848389	3.241523	0.004820	0.274802
-23.680739	-1.906602	3.251520	0.004710	0.275062
-23.630485	-1.867468	3.261517	0.004701	0.275315
-22.930004	-1.948193	3.271514	0.004570	0.275559
-23.028669	-1.885455	3.281510	0.004589	0.275793
-22.512688	-1.927607	3.291507	0.004493	0.276063
-21.862399	-2.004534	3.301504	0.004372	0.276278
-21.686457	-1.996594	3.311501	0.004340	0.276486
-21.347255	-2.013655	3.321498	0.004277	0.276718
-20.962894	-2.030178	3.331494	0.004206	0.276996
-20.694947	-2.040151	3.341491	0.004156	0.277197
-20.271515	-2.081255	3.351488	0.004077	0.277384
-20.546414	-1.979482	3.361485	0.004129	0.277652
-20.004892	-2.021048	3.371482	0.004028	0.277948
-19.731455	-2.033945	3.381478	0.003978	0.278138
-19.399779	-2.058347	3.391475	0.003916	0.278324
-19.074394	-2.064380	3.401472	0.003856	0.278599
-18.700654	-2.091885	3.411469	0.003786	0.278808
-18.980737	-1.997819	3.421466	0.003839	0.279030
-18.975447	-1.948411	3.431462	0.003838	0.279290
-18.033520	-2.071808	3.441459	0.003663	0.279537
-18.048818	-2.023659	3.451456	0.003666	0.279771
-17.627207	-2.063845	3.461453	0.003588	0.279958
-16.929605	-2.150355	3.471450	0.003458	0.280165
-16.704934	-2.135695	3.481446	0.003417	0.280451
-16.698928	-2.108357	3.491443	0.003416	0.280596
-16.227341	-2.166312	3.501440	0.003328	0.280738
-16.253527	-2.105584	3.511437	0.003333	0.281026
-15.929067	-2.130322	3.521434	0.003273	0.281201
-16.052665	-2.067433	3.531430	0.003296	0.281408
-15.728604	-2.066126	3.541427	0.003236	0.281716
-15.369693	-2.090681	3.551424	0.003170	0.281924
-14.983948	-2.128542	3.561421	0.003098	0.282088
-15.068797	-2.066200	3.571418	0.003114	0.282328
-15.040478	-2.009545	3.581414	0.003109	0.282643
-14.553725	-2.053892	3.591411	0.003019	0.282868
-14.314178	-2.055999	3.601408	0.002974	0.283079
-14.214836	-2.034981	3.611405	0.002956	0.283277
-13.700638	-2.067071	3.621402	0.002861	0.283590
-13.594309	-2.046846	3.631398	0.002841	0.283790
-13.576182	-2.003140	3.641395	0.002838	0.284029
-12.966320	-2.073413	3.651392	0.002725	0.284234
-12.877675	-2.031516	3.661389	0.002708	0.284528
-12.683720	-2.023002	3.671386	0.002672	0.284750
-12.039201	-2.101186	3.681382	0.002553	0.284947
-11.784279	-2.103422	3.691379	0.002505	0.285170
-11.733984	-2.050427	3.701376	0.002496	0.285484
-11.149084	-2.127610	3.711373	0.002388	0.285630
-11.073058	-2.109869	3.721370	0.002374	0.285789
-10.951439	-2.074641	3.731366	0.002351	0.286078
-11.134014	-1.991759	3.741363	0.002386	0.286328
-10.937430	-1.978439	3.751360	0.002349	0.286575
-10.683608	-1.979176	3.761357	0.002302	0.286803
-10.243007	-2.016637	3.771354	0.002220	0.287017
-10.036649	-1.990885	3.781350	0.002182	0.287334
-9.635138	-2.020904	3.791347	0.002108	0.287549
-9.496325	-2.001396	3.801344	0.002082	0.287773
-9.114228	-2.025824	3.811341	0.002011	0.287998
-8.987412	-1.991325	3.821338	0.001988	0.288286
-8.882313	-1.961569	3.831334	0.001968	0.288530
-8.950812	-1.900545	3.841331	0.001981	0.288773
-8.632575	-1.907518	3.851328	0.001922	0.289026
-7.917657	-1.992079	3.861325	0.001790	0.289252
-7.882469	-1.942031	3.871322	0.001783	0.289534
-7.509627	-1.962241	3.881318	0.001714	0.289770
-7.287177	-1.956548	3.891315	0.001673	0.289999
-7.430666	-1.878722	3.901312	0.001700	0.290256
-7.110925	-1.880762	3.911309	0.001641	0.290534
-6.740693	-1.899923	3.921306	0.001572	0.290773
-6.327733	-1.927659	3.931302	0.001495	0.291007
-5.974346	-1.948400	3.941299	0.001430	0.291222
-5.379474	-2.017530	3.951296	0.001319	0.291415
-5.139433	-1.998586	3.961293	0.001275	0.291724
-5.000834	-1.981708	3.971290	0.001249	0.291932
-4.646654	-2.008073	3.981286	0.001183	0.292119
-4.262735	-2.036820	3.991283	0.001112	0.292321
-3.996481	-2.024862	4.001280	0.001063	0.292618
-3.941210	-1.993036	4.011277	0.001053	0.292824
-3.639905	-2.006998	4.021274	0.000997	0.293025
-3.580464	-1.967394	4.031270	0.000986	0.293272
-3.370491	-1.950450	4.041267	0.000947	0.293543
-3.626383	-1.856035	4.051264	0.000995	0.293778
-3.210384	-1.883387	4.061261	0.000918	0.294014
-2.651166	-1.940490	4.071258	0.000814	0.294232
-2.642587	-1.882909	4.081254	0.000813	0.294522
-2.413293	-1.874705	4.091251	0.000770	0.294766
-2.047765	-1.894351	4.101248	0.000702	0.294994
-2.492851	-1.756807	4.111245	0.000785	0.295271
-2.304340	-1.734726	4.121242	0.000751	0.295545
-2.290901	-1.689371	4.131238	0.000748	0.295778
-2.127550	-1.656125	4.141235	0.000718	0.296085
-1.892776	-1.639837	4.151232	0.000675	0.296372
-1.985743	-1.558988	4.161229	0.000692	0.296683
-1.518512	-1.586730	4.171226	0.000605	0.296960
-1.371148	-1.552983	4.181222	0.000578	0.297254
-1.459293	-1.471579	4.191219	0.000595	0.297571
-1.415423	-1.409941	4.201216	0.000587	0.297908
-1.139502	-1.398020	4.211213	0.000536	0.298208
-1.157397	-1.328224	4.221210	0.000539	0.298530
-1.468880	-1.200278	4.231206	0.000597	0.298874
-0.959149	-1.216008	4.241203	0.000503	0.299245
-0.761799	-1.182628	4.251200	0.000466	0.299579
-0.405055	-1.177056	4.261197	0.000400	0.299917
-0.633190	-1.059315	4.271194	0.000443	0.300284
-0.758572	-0.964660	4.281190	0.000466	0.300629
-0.651516	-0.913282	4.291187	0.000446	0.300969
-0.683515	-0.827266	4.301184	0.000453	0.301353
-0.612999	-0.748975	4.311181	0.000440	0.301789
-0.490402	-0.694311	4.321178	0.000417	0.302156
-0.229227	-0.660732	4.331174	0.000369	0.302543
-0.504805	-0.509113	4.341171	0.000420	0.303027
-0.446089	-0.434917	4.351168	0.000409	0.303431
0.077940	-0.448572	4.361165	0.000312	0.303819
0.042866	-0.339240	4.371162	0.000319	0.304307
0.017857	-0.250253	4.381158	0.000324	0.304708
0.330079	-0.207367	4.391155	0.000266	0.305179
-0.011725	-0.047287	4.401152	0.000329	0.305642
0.091877	0.028068	4.411149	0.000310	0.306087
0.000000	0.138836	4.421146	0.000328	0.306530

0.227310	0.362030	4.426150	0.000285	0.307775
0.588142	0.853846	4.431155	0.000218	0.310384
0.551465	1.703688	4.436160	0.000224	0.314290
0.459938	2.846505	4.441165	0.000241	0.319432
0.889467	4.177471	4.446170	0.000160	0.325751
1.056722	5.853158	4.451174	0.000128	0.333243
1.070264	7.854657	4.456179	0.000124	0.341833
1.457401	10.092017	4.461184	0.000051	0.351465
1.664909	12.670020	4.466189	0.000011	0.362072
1.519821	15.629655	4.471194	0.000036	0.373610
2.087810	18.776979	4.476198	-0.000072	0.385992
3.158460	22.171068	4.481203	-0.000273	0.399215
3.177226	26.101037	4.486208	-0.000279	0.413225
3.558648	30.311718	4.491213	-0.000353	0.427947
3.917555	34.862462	4.496218	-0.000423	0.443277
4.640806	39.698380	4.501222	-0.000560	0.459202
4.737832	45.005671	4.506227	-0.000582	0.475683
5.303650	50.556426	4.511232	-0.000691	0.492576
5.655241	56.512636	4.516237	-0.000760	0.509950
6.045366	62.769250	4.521242	-0.000836	0.527594
5.972740	69.436419	4.526246	-0.000827	0.545535
6.270520	76.344901	4.531251	-0.000887	0.563696
6.564818	83.546508	4.536256	-0.000946	0.582017
6.812574	91.042037	4.541261	-0.000997	0.600467
7.632073	98.695397	4.546266	-0.001155	0.618975
7.669255	106.751787	4.551270	-0.001167	0.637541
7.828531	115.020694	4.556275	-0.001202	0.656099
7.915568	123.502228	4.561280	-0.001223	0.674575
9.010969	131.982590	4.566285	-0.001433	0.692931
9.330671	140.797835	4.571290	-0.001498	0.711212
9.524964	149.780715	4.576294	-0.001540	0.729323
9.876266	158.888076	4.581299	-0.001611	0.747290
10.472255	168.043936	4.586304	-0.001728	0.765008
10.666366	177.395283	4.591309	-0.001770	0.782555
11.079255	186.777463	4.596314	-0.001853	0.799842
12.427866	196.063472	4.601318	-0.002110	0.816886
14.667973	205.303069	4.606323	-0.002533	0.833773
15.242880	214.847679	4.611328	-0.002646	0.850342
15.743284	224.447283	4.616333	-0.002745	0.866664
16.288927	234.042707	4.621338	-0.002853	0.882690
16.322447	243.750086	4.626342	-0.002865	0.898465
16.956084	253.339818	4.631347	-0.002989	0.913948
17.880063	262.839858	4.636352	-0.003168	0.929112
18.460085	272.412967	4.641357	-0.003282	0.944052
19.316496	281.898937	4.646362	-0.003447	0.958700
20.012082	291.397785	4.651366	-0.003583	0.973104
20.458060	300.922393	4.656371	-0.003672	0.987272
21.221218	310.327863	4.661376	-0.003820	1.001146
21.461061	319.793993	4.666381	-0.003871	1.014788
21.671875	329.197279	4.671386	-0.003916	1.028152
22.840518	338.379863	4.676390	-0.004139	1.041269
23.768650	347.604879	4.681395	-0.004318	1.054223
24.690697	356.766468	4.686400	-0.004496	1.066932
25.007859	366.009808	4.691405	-0.004561	1.079461
25.363156	375.175223	4.696410	-0.004633	1.091750
26.244733	384.209585	4.701414	-0.004803	1.103850
26.555193	393.330008	4.706419	-0.004866	1.115803
27.201460	402.305155	4.711424	-0.004992	1.127516
28.071673	411.238465	4.716429	-0.005160	1.139104
28.699625	420.180932	4.721434	-0.005283	1.150534
28.976979	429.119108	4.726438	-0.005340	1.161772
29.817915	437.932807	4.731443	-0.005502	1.172866
30.221478	446.772205	4.736448	-0.005583	1.183797
31.153819	455.501863	4.741453	-0.005762	1.194604
31.321225	464.329764	4.746458	-0.005799	1.205275
31.510030	473.127253	4.751462	-0.005840	1.215820
32.481443	481.756715	4.756467	-0.006026	1.226233
32.697050	490.477222	4.761472	-0.006072	1.236515
33.348230	499.085369	4.766477	-0.006199	1.246666
33.808759	507.729049	4.771482	-0.006290	1.256740
33.907984	516.403356	4.776486	-0.006314	1.266698
34.333738	525.002933	4.781491	-0.006399	1.276556
34.833354	533.534400	4.786496	-0.006497	1.286276
35.434893	542.068436	4.791501	-0.006615	1.295945
35.871432	550.599379	4.796506	-0.006701	1.305508
35.955652	559.243908	4.801510	-0.006722	1.315061
36.863808	567.624633	4.806515	-0.006897	1.324407
37.044241	576.138084	4.811520	-0.006936	1.333700
37.091468	584.648032	4.816525	-0.006950	1.342900
37.691953	593.043285	4.821530	-0.007067	1.352015
38.070646	601.448945	4.826534	-0.007143	1.361039
38.637316	609.836693	4.831539	-0.007254	1.370018
39.334628	618.180209	4.836544	-0.007389	1.378915
39.830001	626.580321	4.841549	-0.007487	1.387778
40.196957	634.986061	4.846554	-0.007560	1.396569
40.184144	643.425011	4.851558	-0.007563	1.405274
41.039174	651.720393	4.856563	-0.007728	1.413925
41.667510	660.036488	4.861568	-0.007850	1.422507
42.467512	668.340933	4.866573	-0.008004	1.431053
43.188970	676.632737	4.871578	-0.008144	1.439523
43.353109	685.031581	4.876582	-0.008180	1.447958
43.918382	693.360132	4.881587	-0.008291	1.456340
44.025276	701.744340	4.886592	-0.008316	1.464654
44.569952	710.070564	4.891597	-0.008422	1.472935
45.031718	718.347538	4.896602	-0.008514	1.481108
45.518006	726.628142	4.901606	-0.008610	1.489244
45.914200	734.942176	4.906611	-0.008689	1.497353
46.427933	743.190291	4.911616	-0.008790	1.505373
46.871664	751.502094	4.916621	-0.008877	1.513401
47.263757	759.763907	4.921626	-0.008956	1.521330
47.439626	768.088127	4.926630	-0.008994	1.529244
47.634127	776.397777	4.931635	-0.009035	1.537107
47.817952	784.679434	4.936640	-0.009075	1.544901
48.401618	792.898696	4.941645	-0.009189	1.552659
49.233429	801.054028	4.946650	-0.009349	1.560355
49.204485	809.386086	4.951654	-0.009349	1.568049
49.658920	817.616883	4.956659	-0.009439	1.575683
50.093106	825.815369	4.961664	-0.009525	1.583248
50.864475	834.001281	4.966669	-0.009673	1.590815
51.605844	842.182590	4.971674	-0.009817	1.598337
52.076490	850.400115	4.976678	-0.009910	1.605817
52.283440	858.708378	4.981683	-0.009953	1.613305
52.731946	866.919221	4.986688	-0.010042	1.620707
52.953140	875.196013	4.991693	-0.010089	1.628101
53.160697	883.461685	4.996698	-0.010133	1.635449
53.535341	891.646868	5.001702	-0.010207	1.642717
54.300080	899.777554	5.006707	-0.010355	1.649961
54.438599	908.027987	5.011712	-0.010386	1.657189
55.010744	916.187442	5.016717	-0.010498	1.664367
54.973137	924.472111	5.021722	-0.010496	1.671538
55.185989	932.682900	5.026726	-0.010541	1.678649
55.646106	940.835969	5.031731	-0.010632	1.685715
56.327684	948.959028	5.036736	-0.010764	1.692755
56.751248	957.151487	5.041741	-0.010848	1.699790
56.813363	965.395368	5.046746	-0.010865	1.706791
57.208434	973.575230	5.051750	-0.010944	1.713753
57.728753	981.727217	5.056755	-0.011046	1.720681
57.851019	989.930024	5.061760	-0.011074	1.727571
58.406761	998.084762	5.066765	-0.011182	1.734450
58.809816	1006.245881	5.071770	-0.011263	1.741287
59.176901	1014.425720	5.076774	-0.011336	1.748108
59.260200	1022.653795	5.081779	-0.011357	1.754905
59.431969	1030.820852	5.086784	-0.011394	1.761638
59.973467	1038.965728	5.091789	-0.011500	1.768373
60.649888	1047.071096	5.096794	-0.011631	1.775069
61.008927	1055.229379	5.101798	-0.011703	1.781741
61.466215	1063.406609	5.106803	-0.011794	1.788416
62.075138	1071.529980	5.111808	-0.011912	1.795042
62.092983	1079.744529	5.116813	-0.011921	1.801643
62.420159	1087.892971	5.121818	-0.011987	1.808205
63.024822	1096.002257	5.126822	-0.012105	1.814746
63.529853	1104.133817	5.131827	-0.012204	1.821269
63.504559	1112.347235	5.136832	-0.012204	1.827769
63.990056	1120.483453	5.141837	-0.012300	1.834247
64.433277	1128.585625	5.146842	-0.012388	1.840670
64.544497	1136.765097	5.151846	-0.012413	1.847091
64.857292	1144.950565	5.156851	-0.012477	1.853518
64.872664	1153.126857	5.161856	-0.012485	1.859881
64.845884	1161.328990	5.166861	-0.012485	1.866237
64.890429	1169.517803	5.171866	-0.012499	1.872569
65.512712	1177.547900	5.176870	-0.012620	1.878827
66.113325	1185.597873	5.181875	-0.012737	1.885075
65.870159	1193.830321	5.186880	-0.012697	1.891344
66.582929	1201.896553	5.191885	-0.012834	1.897577
66.931668	1210.007139	5.196890	-0.012905	1.903781
67.039476	1218.171665	5.201894	-0.012930	1.909977
67.095315	1226.356227	5.206899	-0.012945	1.916163
67.508255	1234.423184	5.211904	-0.013027	1.922281
67.721933	1242.577680	5.216909	-0.013072	1.928423
68.240206	1250.666511	5.221914	-0.013174	1.934530
69.204862	1258.672404	5.226918	-0.013359	1.940606
69.178560	1266.896924	5.231923	-0.013359	1.946715
69.290571	1275.043066	5.236928	-0.013385	1.952761
69.886616	1283.116321	5.241933	-0.013501	1.958789
70.345520	1291.172522	5.246938	-0.013592	1.964771
70.976613	1299.239982	5.251942	-0.013715	1.970761
71.349249	1307.384973	5.256947	-0.013789	1.976762
71.480335	1315.534211	5.261952	-0.013819	1.982721
71.544618	1323.716584	5.266957	-0.013836	1.988679
71.871672	1331.827200	5.271962	-0.013902	1.994595
72.184830	1339.918208	5.276966	-0.013965	2.000478
72.573198	1348.039034	5.281971	-0.014043	2.006374
72.838562	1356.138437	5.286976	-0.014097	2.012223
73.277973	1364.239724	5.291981	-0.014184	2.018076
73.889887	1372.301911	5.296986	-0.014304	2.023901
73.946621	1380.461104	5.301990	-0.014319	2.029721
74.279991	1388.582169	5.306995	-0.014387	2.035525
74.701877	1396.638384	5.312000	-0.014470	2.041277
75.178720	1404.731923	5.317005	-0.014564	2.047044
74.987968	1412.942409	5.322010	-0.014534	2.052808
75.419062	1420.998873	5.327014	-0.014619	2.058511
76.235713	1429.033881	5.332019	-0.014776	2.064224
76.392124	1437.178207	5.337024	-0.014811	2.069929
76.586685	1445.324522	5.342029	-0.014852	2.075624
76.984561	1453.408724	5.347034	-0.014931	2.081281
77.493719	1461.452060	5.352038	-0.015031	2.086905
77.642588	1469.617843	5.357043	-0.015064	2.092562
78.458438	1477.623562	5.362048	-0.015221	2.098161
79.009576	1485.708738	5.367053	-0.015329	2.103773
79.297981	1493.853010	5.372058	-0.015388	2.109384
79.837117	1501.946679	5.377062	-0.015493	2.114970
80.291879	1510.033839	5.382067	-0.015583	2.120528
80.510133	1518.132471	5.387072	-0.015629	2.126057
81.067874	1526.221484	5.392077	-0.015738	2.131598
82.085906	1534.201750	5.397082	-0.015933	2.137095
81.873817	1542.406237	5.402086	-0.015898	2.142610
82.272408	1550.510329	5.407091	-0.015978	2.148103
81.928847	1558.726613	5.412096	-0.015919	2.153585
82.710336	1566.700932	5.417101	-0.016070	2.158999
82.729377	1574.813182	5.422106	-0.016078	2.164419
83.237108	1582.865713	5.427110	-0.016178	2.169831
83.660279	1590.970130	5.432115	-0.016262	2.175257
83.944846	1599.050779	5.437120	-0.016320	2.180640
83.931971	1607.196651	5.442125	-0.016323	2.186025
85.033649	1615.152438	5.447130	-0.016533	2.191377
84.463375	1623.400296	5.452134	-0.016432	2.196750
85.190883	1631.389302	5.457139	-0.016573	2.202062
85.503427	1639.450089	5.462144	-0.016636	2.207369
85.550712	1647.627193	5.467149	-0.016650	2.212714
86.482636	1655.583617	5.472154	-0.016829	2.217985
86.543836	1663.686509	5.477158	-0.016845	2.223258
87.145312	1671.783811	5.482163	-0.016962	2.228564
87.353332	1679.885515	5.487168	-0.017006	2.233825
87.858129	1687.947301	5.492173	-0.017105	2.239074
88.430460	1695.984434	5.497178	-0.017217	2.244301
88.481535	1704.130396	5.502182	-0.017232	2.249539
88.806850	1712.228693	5.507187	-0.017297	2.254759
89.070685	1720.300592	5.512192	-0.017352	2.259944
89.343196	1728.390019	5.517197	-0.017408	2.265129
89.348876	1736.571504	5.522202	-0.017414	2.270337
89.535665	1744.627707	5.527206	-0.017454	2.275470
90.490260	1752.577436	5.532211	-0.017637	2.280591
90.324497	1760.721864	5.537216	-0.017611	2.285726
90.534207	1768.828949	5.542221	-0.017655	2.290858
90.898789	1776.882021	5.547226	-0.017728	2.295958
91.719163	1784.861851	5.552230	-0.017886	2.301040
92.137778	1792.929868	5.557235	-0.017969	2.306132
92.313326	1801.020299	5.562240	-0.018007	2.311205
92.622242	1809.124051	5.567245	-0.018070	2.316286
92.977960	1817.181394	5.572250	-0.018141	2.321332
93.286208	1825.234362	5.577254	-0.018203	2.326360
94.235394	1833.245822	5.582259	-0.018385	2.331405
94.392183	1841.364362	5.587264	-0.018420	2.336439
94.640430	1849.466245	5.592269	-0.018471	2.341459
95.062285	1857.529505	5.597274	-0.018555	2.346459
95.501758	1865.598199	5.602278	-0.018642	2.351454
95.923012	1873.670272	5.607283	-0.018725	2.356438
96.148104	1881.737365	5.612288	-0.018772	2.361392
96.453692	1889.817034	5.617293	-0.018834	2.366350
96.269174	1897.999548	5.622298	-0.018805	2.371320
96.392969	1906.068960	5.627302	-0.018833	2.376236
97.066101	1914.065720	5.632307	-0.018964	2.381143
97.591255	1922.080572	5.637312	-0.019067	2.386038
97.665419	1930.227865	5.642317	-0.019086	2.390967
98.344021	1938.218934	5.647322	-0.019217	2.395840
98.130259	1946.360431	5.652326	-0.019183	2.400721
98.603531	1954.394681	5.657331	-0.019276	2.405584
98.911421	1962.450987	5.662336	-0.019338	2.410437
99.521546	1970.487481	5.667341	-0.019457	2.415292
99.717390	1978.585442	5.672346	-0.019499	2.420141
99.879197	1986.655009	5.677350	-0.019534	2.424961
100.528673	1994.694703	5.682355	-0.019660	2.429791
100.609336	2002.828610	5.687360	-0.019680	2.434623
100.946909	2010.869669	5.692365	-0.019748	2.439411
101.434374	2018.849762	5.697370	-0.019844	2.444165
101.613633	2026.946411	5.702374	-0.019882	2.448955
101.647617	2035.068958	5.707379	-0.019894	2.453738
101.884289	2043.090729	5.712384	-0.019943	2.458469
102.536097	2051.109886	5.717389	-0.020070	2.463222
102.966870	2059.154838	5.722394	-0.020155	2.467963
103.174238	2067.261504	5.727398	-0.020199	2.472714
103.748220	2075.296650	5.732403	-0.020311	2.477442
103.902797	2083.362215	5.737408	-0.020345	2.482147
104.211313	2091.438112	5.742413	-0.020407	2.486860
104.789927	2099.463512	5.747418	-0.020520	2.491556
105.070828	2107.524913	5.752422	-0.020577	2.496241
105.064854	2115.678799	5.757427	-0.020582	2.500949
105.460453	2123.681687	5.762432	-0.020660	2.505591
106.103483	2131.732990	5.767437	-0.020785	2.510271
106.206371	2139.841493	5.772442	-0.020809	2.514935
106.942201	2147.803282	5.777446	-0.020952	2.519553
106.809169	2155.931826	5.782451	-0.020932	2.524193
106.893967	2164.023873	5.787456	-0.020953	2.528820
107.389771	2172.040814	5.792461	-0.021050	2.533426
107.615976	2180.126590	5.797466	-0.021098	2.538043
108.223173	2188.114448	5.802470	-0.021216	2.542624
108.758149	2196.163574	5.807475	-0.021320	2.547226
108.646563	2204.304370	5.812480	-0.021305	2.551824
108.818960	2212.368690	5.817485	-0.021342	2.556392
109.508246	2220.329148	5.822490	-0.021475	2.560930
109.293179	2228.465588	5.827494	-0.021441	2.565494
109.917202	2236.475886	5.832499	-0.021562	2.570039
110.226211	2244.539977	5.837504	-0.021625	2.574583
110.725476	2252.585989	5.842509	-0.021723	2.579123
110.523581	2260.737333	5.847514	-0.021690	2.583664
111.059172	2268.745426	5.852518	-0.021795	2.588169
111.442679	2276.883540	5.857523	-0.021872	2.592728
111.243468	2284.995640	5.862528	-0.021840	2.597224
112.191589	2292.879170	5.867533	-0.022021	2.601665
112.820713	2300.878356	5.872538	-0.022144	2.606140
112.833803	2308.978655	5.877542	-0.022151	2.610621
113.309400	2317.031496	5.882547	-0.022245	2.615099
113.891939	2324.994621	5.887552	-0.022358	2.619528
114.569749	2333.015329	5.892557	-0.022490	2.623988
114.744413	2341.133661	5.897562	-0.022527	2.628458
115.095813	2349.208290	5.902566	-0.022598	2.632910
115.527668	2357.258824	5.907571	-0.022683	2.637346
115.724988	2365.281410	5.912576	-0.022725	2.641743
116.067236	2373.362233	5.917581	-0.022794	2.646175
116.639909	2381.372920	5.922586	-0.022906	2.650576
116.558550	2389.511460	5.927590	-0.022896	2.654996
116.942699	2397.539289	5.932595	-0.022973	2.659379
117.298982	2405.567889	5.937600	-0.023044	2.663754
117.778991	2413.632802	5.942605	-0.023139	2.668149
117.768673	2421.744351	5.947610	-0.023142	2.672529
117.592387	2429.829886	5.952614	-0.023114	2.676877
118.212615	2437.823970	5.957619	-0.023235	2.681222
118.368535	2445.859675	5.962624	-0.023269	2.685551
118.820460	2453.875808	5.967629	-0.023358	2.689882
119.211249	2461.914918	5.972634	-0.023436	2.694215
119.224892	2470.020105	5.977638	-0.023444	2.698551
119.570038	2478.057118	5.982643	-0.023513	2.702865
120.314035	2486.009581	5.987648	-0.023657	2.707153
120.583163	2494.103619	5.992653	-0.023712	2.711479
120.953109	2502.150940	5.997658	-0.023786	2.715780
121.138023	2510.218853	6.002662	-0.023825	2.720073
121.910481	2518.194620	6.007667	-0.023974	2.724347
121.976605	2526.294336	6.012672	-0.023992	2.728636
122.737520	2534.308601	6.017677	-0.024139	2.732916
123.250621	2542.353744	6.022682	-0.024239	2.737191
123.424845	2550.425630	6.027686	-0.024277	2.741451
123.920952	2558.475870	6.032691	-0.024374	2.745713
124.327785	2566.500748	6.037696	-0.024455	2.749950
124.802471	2574.608274	6.042701	-0.024549	2.754228
125.132397	2582.637211	6.047706	-0.024615	2.758449
125.291046	2590.679240	6.052710	-0.024650	2.762660
126.230750	2598.645245	6.057715	-0.024830	2.766872
126.504711	2606.720721	6.062720	-0.024886	2.771095
126.699056	2614.803663	6.067725	-0.024928	2.775309
126.908206	2622.870786	6.072730	-0.024972	2.779510
127.163492	2630.900207	6.077734	-0.025024	2.783688
127.505370	2638.972710	6.082739	-0.025093	2.787887
127.759774	2647.014653	6.087744	-0.025146	2.792059
128.170175	2655.030517	6.092749	-0.025227	2.796220
128.915106	2663.000634	6.097754	-0.025371	2.800372
129.345907	2671.048838	6.102758	-0.025456	2.804538
130.075350	2679.095125	6.107763	-0.025597	2.808716
130.391226	2687.141645	6.112768	-0.025661	2.812862
130.989002	2695.193699	6.117773	-0.025777	2.817022
131.257956	2703.281479	6.122778	-0.025833	2.821174
131.244614	2711.379150	6.127782	-0.025835	2.825308
131.366539	2719.471821	6.132787	-0.025863	2.829442
131.773476	2727.459450	6.137792	-0.025944	2.833533
132.664180	2735.412953	6.142797	-0.026115	2.837629
132.569067	2743.527527	6.147802	-0.026102	2.841744
132.938201	2751.556139	6.152806	-0.026176	2.845835
133.487744	2759.593738	6.157811	-0.026284	2.849936
133.788881	2767.629624	6.162816	-0.026345	2.854016
134.202926	2775.667379	6.167821	-0.026427	2.858097
134.638576	2783.718735	6.172826	-0.026513	2.862180
134.960877	2791.744462	6.177830	-0.026578	2.866238
135.683492	2799.772931	6.182835	-0.026718	2.870314
135.867784	2807.816399	6.187840	-0.026758	2.874362
136.212667	2815.876191	6.192845	-0.026827	2.878421
136.335876	2823.950146	6.197850	-0.026855	2.882468
136.327156	2832.018532	6.202854	-0.026859	2.886500
136.866498	2840.062746	6.207859	-0.026964	2.890545
136.862231	2848.123878	6.212864	-0.026968	2.894562
137.411795	2856.091971	6.217869	-0.027076	2.898558
137.895905	2864.130252	6.222874	-0.027171	2.902580
138.131728	2872.196401	6.227878	-0.027220	2.906596
138.591230	2880.270925	6.232883	-0.027311	2.910623
138.884745	2888.317319	6.237888	-0.027371	2.914621
139.390523	2896.325388	6.242893	-0.027470	2.918607
139.815633	2904.337822	6.247898	-0.027554	2.922585
139.800752	2912.407671	6.252902	-0.027556	2.926561
140.527760	2920.423500	6.257907	-0.027697	2.930546
140.668071	2928.469078	6.262912	-0.027728	2.934508
141.309118	2936.444914	6.267917	-0.027853	2.938458
141.364761	2944.530078	6.272922	-0.027868	2.942424
141.870888	2952.535824	6.277926	-0.027967	2.946370
142.069622	2960.622101	6.282931	-0.028010	2.950334
142.601632	2968.609270	6.287936	-0.028114	2.954262
142.664406	2976.704162	6.292941	-0.028131	2.958212
143.280551	2984.665463	6.297946	-0.028250	2.962121
143.499166	2992.745176	6.302950	-0.028296	2.966061
143.714253	3000.826492	6.307955	-0.028341	2.969997
143.792386	3008.881980	6.312960	-0.028361	2.973907
143.931974	3016.939526	6.317965	-0.028392	2.977817
144.307510	3024.957677	6.322970	-0.028467	2.981715
144.686203	3032.983599	6.327974	-0.028543	2.985611
144.589342	3041.121981	6.332979	-0.028530	2.989532
144.988391	3049.102877	6.337984	-0.028609	2.993398
145.558961	3057.083680	6.342989	-0.028721	2.997267
145.951666	3065.114324	6.347994	-0.028799	3.001146
146.616145	3073.057491	6.352998	-0.028928	3.004992
146.768949	3081.182515	6.358003	-0.028961	3.008894
147.082516	3089.214883	6.363008	-0.029025	3.012755
147.063205	3097.322556	6.368013	-0.029026	3.016630
147.557521	3105.330476	6.373018	-0.029124	3.020478
147.714094	3113.336853	6.378022	-0.029158	3.024303
148.420718	3121.360850	6.383027	-0.029295	3.028160
148.500255	3129.441987	6.388032	-0.029314	3.032007
149.025727	3137.444328	6.393037	-0.029417	3.035834
149.455635	3145.448668	6.398042	-0.029503	3.039653
149.617575	3153.478263	6.403046	-0.029538	3.043465
150.480156	3161.491435	6.408051	-0.029704	3.047300
150.477871	3169.618887	6.413056	-0.029708	3.051140
150.966094	3177.649752	6.418061	-0.029804	3.054955
151.518002	3185.633248	6.423066	-0.029912	3.058745
152.019829	3193.632152	6.428070	-0.030011	3.062536
152.585230	3201.682465	6.433075	-0.030121	3.066349
152.660299	3209.771315	6.438080	-0.030140	3.070151
153.067257	3217.857877	6.443085	-0.030221	3.073963
153.598265	3225.861862	6.448090	-0.030325	3.077739
153.431468	3233.929190	6.453094	-0.030299	3.081505
153.864280	3241.904508	6.458099	-0.030385	3.085253
154.418183	3249.886687	6.463104	-0.030493	3.089005
154.380575	3258.019909	6.468109	-0.030491	3.092794
154.490406	3266.090977	6.473114	-0.030517	3.096557
155.162569	3274.039271	6.478118	-0.030647	3.100285
155.393533	3282.090199	6.483123	-0.030695	3.104035
155.770315	3290.093059	6.488128	-0.030770	3.107765
156.073192	3298.163130	6.493133	-0.030832	3.111519
156.959323	3306.132033	6.498138	-0.031002	3.115248
157.026967	3314.175466	6.503142	-0.031020	3.118969
156.906702	3322.301647	6.508147	-0.031002	3.122714
157.095105	3330.334621	6.513152	-0.031043	3.126427
157.263920	3338.394818	6.518157	-0.031079	3.130147
158.200067	3346.317749	6.523162	-0.031259	3.133835
158.943822	3354.298321	6.528166	-0.031402	3.137536
159.292121	3362.366348	6.533171	-0.031472	3.141254
159.715072	3370.389646	6.538176	-0.031556	3.144951
159.777676	3378.514436	6.543181	-0.031573	3.148673
160.444698	3386.520505	6.548186	-0.031702	3.152364
160.904902	3394.532874	6.553190	-0.031793	3.156044
160.976456	3402.619323	6.558195	-0.031811	3.159736
161.076790	3410.667867	6.563200	-0.031835	3.163408
161.983600	3418.570814	6.568205	-0.032009	3.167046
162.211734	3426.674462	6.573210	-0.032057	3.170740
162.520941	3434.687531	6.578214	-0.032119	3.174392
163.063407	3442.748435	6.583219	-0.032226	3.178072
163.635058	3450.723704	6.588224	-0.032337	3.181710
164.125700	3458.778436	6.593229	-0.032434	3.185376
164.617511	3466.805956	6.598234	-0.032530	3.189026
164.418006	3474.906668	6.603238	-0.032498	3.192674
165.061906	3482.947200	6.608243	-0.032623	3.196327
165.624344	3490.904581	6.613248	-0.032733	3.199936
165.601257	3498.972245	6.618253	-0.032734	3.203564
165.879964	3507.042890	6.623258	-0.032791	3.207203
166.067953	3515.066853	6.628262	-0.032831	3.210812
167.066866	3523.021372	6.633267	-0.033022	3.214422
167.163046	3531.070459	6.638272	-0.033045	3.218030
167.110942	3539.191003	6.643277	-0.033041	3.221661
167.609594	3547.176534	6.648282	-0.033138	3.225250
168.048190	3555.202133	6.653286	-0.033225	3.228851
168.737573	3563.241804	6.658291	-0.033359	3.232464
169.426116	3571.214440	6.663296	-0.033492	3.236043
170.043952	3579.201541	6.668301	-0.033612	3.239622
170.819047	3587.194882	6.673306	-0.033762	3.243206
171.219782	3595.236971	6.678310	-0.033841	3.246792
171.768808	3603.324940	6.683315	-0.033949	3.250401
172.047270	3611.349523	6.688320	-0.034006	3.253966
172.233383	3619.445373	6.693325	-0.034045	3.257554
172.695700	3627.482717	6.698330	-0.034137	3.261125
172.969686	3635.468821	6.703334	-0.034193	3.264661
173.485182	3643.533349	6.708339	-0.034294	3.268237
173.687835	3651.592767	6.713344	-0.034337	3.271795
174.263344	3659.610878	6.718349	-0.034449	3.275345
174.604104	3667.624862	6.723354	-0.034518	3.278881
174.617635	3675.660796	6.728358	-0.034525	3.282409
174.888483	3683.750077	6.733363	-0.034581	3.285967
174.973426	3691.776206	6.738368	-0.034602	3.289485
175.327397	3699.795582	6.743373	-0.034673	3.293008
176.070807	3707.765923	6.748378	-0.034816	3.296521
176.519547	3715.756309	6.753382	-0.034905	3.300028
176.639870	3723.827609	6.758387	-0.034932	3.303552
176.519480	3731.922316	6.763392	-0.034915	3.307074
177.262912	3739.931418	6.768397	-0.035059	3.310589
177.542669	3747.945399	6.773402	-0.035116	3.314084
177.782211	3755.978090	6.778406	-0.035166	3.317581
178.083587	3764.031808	6.783411	-0.035227	3.321087
178.378395	3771.989534	6.788416	-0.035287	3.324546
178.650742	3780.028433	6.793421	-0.035343	3.328037
178.984074	3788.091396	6.798426	-0.035410	3.331536
179.175853	3796.140223	6.803430	-0.035451	3.335020
179.401695	3804.180051	6.808435	-0.035498	3.338498
179.117596	3812.265788	6.813440	-0.035450	3.341973
179.876429	3820.182329	6.818445	-0.035596	3.345411
180.333276	3828.203126	6.823450	-0.035687	3.348878
180.463621	3836.262781	6.828454	-0.035716	3.352347
180.690441	3844.363820	6.833459	-0.035763	3.355833
181.356676	3852.280296	6.838464	-0.035892	3.359252
181.446119	3860.341862	6.843469	-0.035914	3.362709
181.670195	3868.410925	6.848474	-0.035961	3.366170
182.404362	3876.357589	6.853478	-0.036103	3.369595
182.641706	3884.453318	6.858483	-0.036152	3.373061
182.704192	3892.503154	6.863488	-0.036169	3.376497
183.065255	3900.502316	6.868493	-0.036241	3.379920
183.774098	3908.468625	6.873498	-0.036378	3.383337
183.775699	3916.544871	6.878502	-0.036384	3.386772
184.362237	3924.581811	6.883507	-0.036498	3.390208
184.981476	3932.609659	6.888512	-0.036618	3.393638
185.189717	3940.637018	6.893517	-0.036662	3.397049
185.570391	3948.635657	6.898522	-0.036738	3.400451
185.650600	3956.655624	6.903526	-0.036758	3.403847
186.227808	3964.701118	6.908531	-0.036871	3.407269
185.971564	3972.803701	6.913536	-0.036828	3.410681
186.119887	3980.831814	6.918541	-0.036861	3.414074
186.944920	3988.798078	6.923546	-0.037020	3.417460
187.256336	3996.819750	6.928550	-0.037083	3.420849
187.898529	4004.790454	6.933555	-0.037208	3.424224
188.065913	4012.862789	6.938560	-0.037244	3.427621
187.951651	4020.961644	6.943565	-0.037228	3.431017
188.502325	4028.934600	6.948570	-0.037335	3.434380
189.020925	4036.913095	6.953574	-0.037437	3.437740
189.537299	4044.981187	6.958579	-0.037538	3.441135
189.773502	4052.961251	6.963584	-0.037587	3.444479
190.228975	4061.004292	6.968589	-0.037677	3.447855
190.403378	4069.125850	6.973594	-0.037715	3.451249
190.841420	4077.092865	6.978598	-0.037802	3.454586
191.127703	4085.147042	6.983603	-0.037860	3.457950
191.557046	4093.177932	6.988608	-0.037945	3.461305
191.578732	4101.211906	6.993613	-0.037954	3.464645
192.233398	4109.170305	6.998618	-0.038081	3.467972
192.295280	4117.269338	7.003622	-0.038098	3.471334
192.666655	4125.312639	7.008627	-0.038172	3.474680
192.859729	4133.302149	7.013632	-0.038213	3.477994
193.471451	4141.284355	7.018637	-0.038332	3.481316
194.186184	4149.263134	7.023642	-0.038470	3.484637
194.294293	4157.343389	7.028646	-0.038496	3.487976
194.858033	4165.370583	7.033651	-0.038606	3.491306
195.238546	4173.370370	7.038656	-0.038682	3.494614
195.719572	4181.380505	7.043661	-0.038776	3.497927
195.900641	4189.483924	7.048666	-0.038815	3.501266
196.182149	4197.465531	7.053670	-0.038873	3.504554
196.832155	4205.501610	7.058675	-0.038999	3.507874
197.021304	4213.572213	7.063680	-0.039039	3.511189
197.337135	4221.549038	7.068685	-0.039103	3.514467
197.927833	4229.591167	7.073690	-0.039218	3.517778
198.104985	4237.642348	7.078694	-0.039256	3.521076
198.255999	4245.698629	7.083699	-0.039289	3.524372
198.867949	4253.664477	7.088704	-0.039408	3.527642
199.184061	4261.770638	7.093709	-0.039472	3.530958
199.086362	4269.781832	7.098714	-0.039459	3.534218
199.262409	4277.808293	7.103718	-0.039497	3.537490
199.596013	4285.856957	7.108723	-0.039565	3.540773
199.712925	4293.832344	7.113728	-0.039591	3.544017
200.390671	4301.817284	7.118733	-0.039723	3.547278
200.504247	4309.918737	7.123738	-0.039749	3.550567
200.520957	4317.981985	7.128742	-0.039757	3.553834
200.537224	4326.033406	7.133747	-0.039765	3.557093
200.747778	4334.002477	7.138752	-0.039810	3.560322
201.397177	4341.950133	7.143757	-0.039936	3.563552
201.801470	4349.985818	7.148762	-0.040016	3.566808
201.896593	4358.011386	7.153766	-0.040039	3.570047
202.785097	4366.006102	7.158771	-0.040209	3.573295
202.934676	4374.026901	7.163776	-0.040242	3.576528
203.543709	4382.032952	7.168781	-0.040361	3.579765
204.000577	4390.043942	7.173786	-0.040451	3.582998
204.274471	4398.104845	7.178790	-0.040507	3.586241
204.642076	4406.166196	7.183795	-0.040581	3.589485
204.755002	4414.202491	7.188800	-0.040607	3.592708
205.276146	4422.229065	7.193805	-0.040709	3.595937
205.446811	4430.224969	7.198810	-0.040746	3.599140
205.649986	4438.232717	7.203814	-0.040789	3.602345
206.154223	4446.295190	7.208819	-0.040888	3.605579
206.390739	4454.286886	7.213824	-0.040937	3.608773
206.606726	4462.380551	7.218829	-0.040982	3.612005
207.111198	4470.368738	7.223834	-0.041081	3.615200
207.433905	4478.386874	7.228838	-0.041146	3.618399
207.599908	4486.472356	7.233843	-0.041183	3.621617
207.367440	4494.518436	7.238848	-0.041144	3.624805
207.797827	4502.505552	7.243853	-0.041230	3.627986
208.301471	4510.520610	7.248858	-0.041328	3.631177
208.679578	4518.496757	7.253862	-0.041404	3.634347
209.002142	4526.555856	7.258867	-0.041469	3.637545
208.818113	4534.651255	7.263872	-0.041440	3.640740
209.137094	4542.558930	7.268877	-0.041504	3.643872
209.806677	4550.604583	7.273882	-0.041634	3.647066
210.138573	4558.639525	7.278886	-0.041701	3.650243
210.518359	4566.675072	7.283891	-0.041777	3.653419
210.595356	4574.740698	7.288896	-0.041796	3.656596
210.739834	4582.726038	7.293901	-0.041828	3.659740
211.416456	4590.691387	7.298906	-0.041960	3.662888
211.938377	4598.697777	7.303910	-0.042062	3.666045
212.363101	4606.757099	7.308915	-0.042146	3.669218
212.644687	4614.817595	7.313920	-0.042204	3.672384
213.156593	4622.810999	7.318925	-0.042304	3.675528
213.507722	4630.804220	7.323930	-0.042374	3.678664
213.676147	4638.844975	7.328934	-0.042411	3.681811
214.441039	4646.838146	7.333939	-0.042558	3.684953
214.400812	4654.922424	7.338944	-0.042556	3.688107
215.010956	4662.947583	7.343949	-0.042675	3.691251
215.198158	4670.971768	7.348954	-0.042715	3.694382
215.140570	4679.016253	7.353958	-0.042709	3.697511
215.327994	4687.096737	7.358963	-0.042749	3.700658
215.723396	4695.045548	7.363968	-0.042828	3.703757
216.037797	4703.101591	7.368973	-0.042892	3.706892
216.849235	4711.029791	7.373978	-0.043048	3.709988
217.155317	4719.142251	7.378982	-0.043110	3.713140
217.587653	4727.227514	7.383987	-0.043195	3.716282
217.675419	4735.161886	7.388992	-0.043217	3.719353
218.113977	4743.168486	7.393997	-0.043304	3.722459
218.377233	4751.248556	7.399002	-0.043358	3.725587
218.410379	4759.238203	7.404006	-0.043369	3.728671
218.802922	4767.299972	7.409011	-0.043447	3.731789
219.026134	4775.316524	7.414016	-0.043494	3.734883
219.115146	4783.329121	7.419021	-0.043516	3.737969
219.644597	4791.358681	7.424026	-0.043619	3.741071
219.879260	4799.329760	7.429030	-0.043668	3.744139
219.738061	4807.444893	7.434035	-0.043647	3.747252
220.263897	4815.388516	7.439040	-0.043750	3.750312
220.952992	4823.382952	7.444045	-0.043883	3.753394
221.338278	4831.441275	7.449050	-0.043960	3.756489
221.917933	4839.386257	7.454054	-0.044073	3.759544
222.407031	4847.418070	7.459059	-0.044169	3.762627
222.831417	4855.435465	7.464064	-0.044253	3.765700
223.036720	4863.501306	7.469069	-0.044297	3.768784
222.955503	4871.616519	7.474074	-0.044287	3.771878
223.549263	4879.588495	7.479078	-0.044403	3.774930
223.914947	4887.633185	7.484083	-0.044476	3.778002
223.980404	4895.661517	7.489088	-0.044493	3.781058
224.613623	4903.557439	7.494093	-0.044616	3.784075
224.625425	4911.713197	7.499098	-0.044623	3.787173
224.841883	4919.705784	7.504102	-0.044669	3.790212
224.849593	4927.765555	7.509107	-0.044675	3.793269
225.335726	4935.753731	7.514112	-0.044771	3.796307
225.979137	4943.672050	7.519117	-0.044896	3.799320
226.088567	4951.786492	7.524122	-0.044921	3.802392
226.116967	4959.795999	7.529126	-0.044932	3.805421
226.777825	4967.796583	7.534131	-0.045060	3.808458
227.147573	4975.825641	7.539136	-0.045134	3.811496
227.231836	4983.877702	7.544141	-0.045155	3.814535
227.633399	4991.903849	7.549146	-0.045234	3.817568
228.027791	4999.927868	7.554150	-0.045313	3.820598
228.727704	5007.870411	7.559155	-0.045448	3.823602
228.993562	5015.933480	7.564160	-0.045503	3.826638
229.227189	5024.020795	7.569165	-0.045552	3.829681
229.651157	5032.015154	7.574170	-0.045636	3.832691
230.112432	5040.024613	7.579174	-0.045727	3.835704
230.701340	5048.035567	7.584179	-0.045841	3.838719
230.501234	5056.128575	7.589184	-0.045809	3.841745
230.939528	5064.087025	7.594189	-0.045896	3.844731
231.570599	5072.094933	7.599194	-0.046019	3.847738
231.746060	5080.116622	7.604198	-0.046056	3.850738
231.826250	5088.179455	7.609203	-0.046076	3.853749
231.979521	5096.246094	7.614208	-0.046110	3.856761
232.307675	5104.220210	7.619213	-0.046176	3.859739
232.972571	5112.212372	7.624218	-0.046305	3.862729
233.043662	5120.270120	7.629222	-0.046324	3.865728
233.761008	5128.269657	7.634227	-0.046462	3.868717
233.836884	5136.375144	7.639232	-0.046481	3.871730
233.991835	5144.463161	7.644237	-0.046515	3.874735
234.648031	5152.381085	7.649242	-0.046643	3.877685
234.994216	5160.368240	7.654246	-0.046712	3.880652
235.103310	5168.339504	7.659251	-0.046738	3.883607
235.681966	5176.367524	7.664256	-0.046850	3.886589
236.005530	5184.388264	7.669261	-0.046916	3.889561
235.769037	5192.502925	7.674266	-0.046877	3.892554
236.256100	5200.427313	7.679270	-0.046973	3.895489
236.675905	5208.480971	7.684275	-0.047056	3.898469
237.097865	5216.465449	7.689280	-0.047140	3.901420
237.028850	5224.515178	7.694285	-0.047132	3.904384
237.707032	5232.491334	7.699290	-0.047263	3.907333
238.042402	5240.522113	7.704294	-0.047331	3.910293
238.409294	5248.543828	7.709299	-0.047404	3.913248
238.724010	5256.614555	7.714304	-0.047468	3.916217
238.916838	5264.569549	7.719309	-0.047509	3.919140
239.335910	5272.615601	7.724314	-0.047592	3.922098
239.861341	5280.573595	7.729318	-0.047695	3.925024
240.295594	5288.631321	7.734323	-0.047781	3.927982
240.198224	5296.780596	7.739328	-0.047768	3.930961
240.806214	5304.698963	7.744333	-0.047886	3.933867
241.041378	5312.803753	7.749338	-0.047935	3.936831
241.727048	5320.714094	7.754342	-0.048068	3.939731
242.029740	5328.739553	7.759347	-0.048129	3.942664
242.343960	5336.757671	7.764352	-0.048193	3.945592
242.526934	5344.833262	7.769357	-0.048232	3.948536
242.649995	5352.923198	7.774362	-0.048260	3.951482
242.915506	5360.883086	7.779366	-0.048315	3.954381
243.421431	5368.920044	7.784371	-0.048414	3.957310
243.406474	5376.921709	7.789376	-0.048416	3.960215
243.657125	5384.913211	7.794381	-0.048468	3.963119
244.163929	5392.946008	7.799386	-0.048568	3.966040
244.155154	5400.970345	7.804390	-0.048571	3.968946
244.642420	5409.046481	7.809395	-0.048667	3.971879
244.874753	5417.031857	7.814400	-0.048715	3.974771
245.060397	5425.033251	7.819405	-0.048755	3.977667
245.608357	5433.066733	7.824410	-0.048862	3.980578
245.727881	5441.021881	7.829414	-0.048889	3.983451
245.939006	5449.138540	7.834419	-0.048934	3.986382
246.068136	5457.133552	7.839424	-0.048963	3.989265
246.539783	5465.181038	7.844429	-0.049056	3.992172
246.989648	5473.187051	7.849434	-0.049145	3.995060
247.156367	5481.138910	7.854438	-0.049181	3.997923
247.368778	5489.224721	7.859443	-0.049226	4.000832
247.561578	5497.202641	7.864448	-0.049267	4.003700
248.042252	5505.253581	7.869453	-0.049361	4.006597
248.242665	5513.279455	7.874458	-0.049404	4.009478
248.234749	5521.305364	7.879462	-0.049407	4.012353
248.803951	5529.332509	7.884467	-0.049518	4.015236
248.909330	5537.362132	7.889472	-0.049543	4.018111
249.497671	5545.325182	7.894477	-0.049658	4.020967
249.480526	5553.390528	7.899482	-0.049660	4.023848
249.901861	5561.373962	7.904486	-0.049743	4.026705
250.073799	5569.429045	7.909491	-0.049780	4.029582
250.265826	5577.485535	7.914496	-0.049821	4.032457
251.044522	5585.471913	7.919501	-0.049971	4.035314
251.350055	5593.441983	7.924506	-0.050033	4.038156
251.638152	5601.445813	7.929510	-0.050092	4.041008
251.905911	5609.422076	7.934515	-0.050147	4.043847
252.331769	5617.483121	7.939520	-0.050231	4.046717
252.392855	5625.540018	7.944525	-0.050248	4.049578
252.410131	5633.621329	7.949530	-0.050256	4.052445
252.677540	5641.585364	7.954534	-0.050311	4.055272
253.245153	5649.587657	7.959539	-0.050422	4.058115
253.448082	5657.635682	7.964544	-0.050465	4.060967
253.476675	5665.657360	7.969549	-0.050475	4.063804
253.841989	5673.695601	7.974554	-0.050548	4.066651
254.036954	5681.676292	7.979558	-0.050590	4.069472
254.565932	5689.728695	7.984563	-0.050693	4.072323
254.782575	5697.720714	7.989568	-0.050739	4.075145
255.168553	5705.723523	7.994573	-0.050816	4.077971
255.304638	5713.782613	7.999578	-0.050846	4.080811
255.639406	5721.745773	8.004582	-0.050914	4.083619
255.680948	5729.885014	8.009587	-0.050927	4.086482
255.451436	5737.853891	8.014592	-0.050889	4.089279
255.917539	5745.898606	8.019597	-0.050981	4.092112
256.167891	5753.908255	8.024602	-0.051033	4.094926
256.769640	5761.843060	8.029606	-0.051150	4.097718
256.690381	5769.967584	8.034611	-0.051140	4.100564
257.122139	5777.907309	8.039616	-0.051226	4.103352
257.357021	5785.980239	8.044621	-0.051274	4.106180
258.219251	5793.925269	8.049626	-0.051440	4.108971
258.501322	5801.981769	8.054630	-0.051498	4.111791
258.730861	5810.024582	8.059635	-0.051545	4.114604
258.831914	5818.032518	8.064640	-0.051569	4.117400
259.196184	5826.024698	8.069645	-0.051642	4.120193
259.758024	5834.014612	8.074650	-0.051752	4.122985
260.076869	5842.028754	8.079654	-0.051816	4.125781
260.491491	5850.066240	8.084659	-0.051899	4.128584
260.503482	5858.108063	8.089664	-0.051906	4.131381
260.742286	5866.115969	8.094669	-0.051956	4.134168
260.994472	5874.170225	8.099674	-0.052008	4.136969
261.432470	5882.131120	8.104678	-0.052094	4.139738
261.493528	5890.211024	8.109683	-0.052111	4.142542
261.805232	5898.206689	8.114688	-0.052174	4.145318
262.160349	5906.217020	8.119693	-0.052245	4.148097
262.370085	5914.296106	8.124698	-0.052289	4.150897
262.925340	5922.198943	8.129702	-0.052398	4.153638
263.074116	5930.322074	8.134707	-0.052431	4.156448
263.445583	5938.294238	8.139712	-0.052505	4.159207
263.445696	5946.338958	8.144717	-0.052510	4.161984
263.529314	5954.298182	8.149722	-0.052531	4.164731
263.929940	5962.322663	8.154726	-0.052610	4.167503
264.195123	5970.361215	8.159731	-0.052665	4.170276
264.177577	5978.413653	8.164736	-0.052667	4.173048
264.194399	5986.467486	8.169741	-0.052675	4.175820
264.899006	5994.416682	8.174746	-0.052811	4.178562
265.305351	6002.423826	8.179750	-0.052892	4.181318
265.456331	6010.396361	8.184755	-0.052925	4.184058
265.760989	6018.481626	8.189760	-0.052987	4.186836
266.057667	6026.488893	8.194765	-0.053048	4.189586
266.047937	6034.628864	8.199770	-0.053051	4.192375
266.434264	6042.599140	8.204774	-0.053128	4.195109
267.169615	6050.551814	8.209779	-0.053270	4.197840
267.109140	6058.616663	8.214784	-0.053264	4.200598
267.281176	6066.591164	8.219789	-0.053301	4.203325
267.637279	6074.686294	8.224794	-0.053372	4.206094
267.769167	6082.619712	8.229798	-0.053402	4.208804
268.114495	6090.709543	8.234803	-0.053471	4.211568
268.315314	6098.649326	8.239808	-0.053514	4.214277
268.689558	6106.726077	8.244813	-0.053589	4.217032
268.827710	6114.785762	8.249818	-0.053619	4.219778
269.545695	6122.684948	8.254822	-0.053758	4.222473
269.887636	6130.739474	8.259827	-0.053827	4.225216
269.883542	6138.781140	8.264832	-0.053831	4.227948
270.141487	6146.799372	8.269837	-0.053884	4.230674
270.298954	6154.864745	8.274842	-0.053919	4.233412
270.328086	6162.911854	8.279846	-0.053929	4.236142
270.956710	6170.803372	8.284851	-0.054052	4.238823
270.949073	6178.898959	8.289856	-0.054055	4.241564
271.267250	6186.856782	8.294861	-0.054120	4.244261
271.625269	6194.913670	8.299866	-0.054191	4.246990
271.964949	6202.880373	8.304870	-0.054260	4.249687
272.370973	6211.016667	8.309875	-0.054341	4.252439
272.477595	6219.020397	8.314880	-0.054365	4.255142
272.463988	6227.018079	8.319885	-0.054368	4.257840
272.727478	6235.008833	8.324890	-0.054422	4.260537
273.048508	6242.990076	8.329894	-0.054487	4.263230
273.466474	6251.030214	8.334899	-0.054570	4.265941
273.527442	6259.068493	8.339904	-0.054586	4.268647
274.368716	6267.042717	8.344909	-0.054748	4.271336
274.372615	6275.076308	8.349914	-0.054754	4.274036
274.566725	6283.143921	8.354918	-0.054795	4.276748
275.022231	6291.072496	8.359923	-0.054885	4.279413
275.221050	6299.112179	8.364928	-0.054927	4.282112
275.731437	6307.056943	8.369933	-0.055027	4.284780
276.097890	6315.151667	8.374938	-0.055101	4.287495
276.282555	6323.163449	8.379942	-0.055140	4.290179
276.627901	6331.195499	8.384947	-0.055210	4.292870
276.649804	6339.264947	8.389952	-0.055219	4.295568
277.168157	6347.186727	8.394957	-0.055320	4.298220
277.237630	6355.272562	8.399962	-0.055338	4.300921
277.651928	6363.208290	8.404966	-0.055421	4.303573
278.087518	6371.295530	8.409971	-0.055507	4.306274
278.408917	6379.260813	8.414976	-0.055572	4.308932
278.701484	6387.312536	8.419981	-0.055631	4.311617
279.120232	6395.323903	8.424986	-0.055715	4.314287
279.233358	6403.333287	8.429990	-0.055741	4.316953
279.721473	6411.331485	8.434995	-0.055837	4.319616
279.468516	6419.404434	8.440000	-0.055795	4.322296
279.808806	6427.346940	8.445005	-0.055863	4.324937
279.992824	6435.438576	8.450010	-0.055903	4.327623
280.071320	6443.454139	8.455014	-0.055922	4.330282
280.588190	6451.455377	8.460019	-0.056024	4.332939
280.777806	6459.497089	8.465024	-0.056064	4.335604
281.152100	6467.410106	8.470029	-0.056139	4.338226
281.146873	6475.565649	8.475034	-0.056143	4.340924
281.408788	6483.460136	8.480038	-0.056197	4.343537
281.617573	6491.586635	8.485043	-0.056241	4.346223
282.163663	6499.495650	8.490048	-0.056347	4.348839
282.485565	6507.564394	8.495053	-0.056413	4.351505
282.992332	6515.562935	8.500058	-0.056512	4.354146
282.914894	6523.646249	8.505062	-0.056503	4.356810
282.826690	6531.661730	8.510067	-0.056491	4.359450
282.925957	6539.656001	8.515072	-0.056515	4.362082
283.140181	6547.590884	8.520077	-0.056560	4.364694
283.828846	6555.640740	8.525082	-0.056693	4.367346
284.157007	6563.635252	8.530086	-0.056759	4.369976
284.558361	6571.706353	8.535091	-0.056839	4.372629
284.441697	6579.724219	8.540096	-0.056823	4.375260
284.792230	6587.689293	8.545101	-0.056893	4.377875
284.976694	6595.773303	8.550106	-0.056933	4.380526
285.217364	6603.689524	8.555110	-0.056982	4.383121
285.497734	6611.768055	8.560115	-0.057040	4.385768
285.914569	6619.802014	8.565120	-0.057122	4.388399
286.257002	6627.828161	8.570125	-0.057191	4.391026
286.559877	6635.839033	8.575130	-0.057253	4.393646
286.605135	6643.859962	8.580135	-0.057266	4.396266
287.013875	6651.848852	8.585139	-0.057348	4.398876
287.135118	6659.919132	8.590144	-0.057375	4.401510
287.314485	6667.850446	8.595149	-0.057414	4.404097
287.622061	6675.969985	8.600154	-0.057476	4.406744
287.747888	6683.935911	8.605159	-0.057505	4.409339
287.769940	6692.015056	8.610163	-0.057514	4.411968
288.268249	6700.012399	8.615168	-0.057612	4.414572
288.701609	6708.033161	8.620173	-0.057698	4.417182
288.699626	6716.062932	8.625178	-0.057702	4.419790
289.125738	6724.058958	8.630183	-0.057787	4.422389
289.741101	6732.078629	8.635187	-0.057906	4.424994
289.552469	6740.127083	8.640192	-0.057876	4.427603
289.672030	6748.198935	8.645197	-0.057904	4.430220
290.041694	6756.214415	8.650202	-0.057978	4.432818
289.810002	6764.245000	8.655207	-0.057940	4.435416
290.164766	6772.221096	8.660211	-0.058011	4.437998
290.136472	6780.268252	8.665216	-0.058011	4.440600
290.906837	6788.157172	8.670221	-0.058159	4.443153
290.889988	6796.272631	8.675226	-0.058161	4.445773
290.759790	6804.295034	8.680231	-0.058142	4.448362
291.403988	6812.295251	8.685235	-0.058267	4.450946
291.680182	6820.286775	8.690240	-0.058324	4.453523
292.179063	6828.337759	8.695245	-0.058422	4.456119
292.493005	6836.352826	8.700250	-0.058485	4.458702
292.076152	6844.433193	8.705255	-0.058413	4.461300
292.965929	6852.329688	8.710259	-0.058583	4.463844
293.241045	6860.412060	8.715264	-0.058640	4.466443
293.573159	6868.392461	8.720269	-0.058707	4.469008
293.598386	6876.485089	8.725274	-0.058717	4.471606
293.950237	6884.388034	8.730279	-0.058787	4.474143
294.688419	6892.467484	8.735283	-0.058930	4.476737
294.531516	6900.477473	8.740288	-0.058906	4.479303
294.862369	6908.518556	8.745293	-0.058972	4.481880
295.547231	6916.442617	8.750298	-0.059105	4.484420
295.532108	6924.529016	8.755303	-0.059107	4.487007
295.536992	6932.595406	8.760307	-0.059113	4.489586
295.915116	6940.589370	8.765312	-0.059189	4.492142
296.151570	6948.580042	8.770317	-0.059238	4.494695
296.383215	6956.604770	8.775322	-0.059286	4.497257
296.490700	6964.578902	8.780327	-0.059311	4.499801
296.692965	6972.681844	8.785331	-0.059354	4.502385
297.081313	6980.658947	8.790336	-0.059431	4.504928
297.182803	6988.684244	8.795341	-0.059455	4.507484
297.499566	6996.716602	8.800346	-0.059520	4.510042
297.826695	7004.669102	8.805351	-0.059585	4.512572
298.039406	7012.684435	8.810355	-0.059630	4.515121
298.764362	7020.665445	8.815360	-0.059770	4.517659
298.813810	7028.701665	8.820365	-0.059785	4.520211
298.874536	7036.749224	8.825370	-0.059801	4.522765
299.124997	7044.704907	8.830375	-0.059853	4.525290
299.638711	7052.709791	8.835379	-0.059953	4.527829
299.505958	7060.803593	8.840384	-0.059934	4.530392
299.971198	7068.758106	8.845389	-0.060026	4.532913
300.105049	7076.856541	8.850394	-0.060056	4.535476
299.912263	7084.863892	8.855399	-0.060025	4.538008
300.279177	7092.841941	8.860403	-0.060098	4.540531
300.639474	7100.779166	8.865408	-0.060170	4.543039
300.623671	7108.910121	8.870413	-0.060173	4.545606
300.227629	7117.010289	8.875418	-0.060104	4.548161
300.309009	7124.980222	8.880423	-0.060124	4.550675
301.735799	7132.869458	8.885427	-0.060395	4.553166
301.467500	7140.924606	8.890432	-0.060350	4.555703
301.757539	7148.897544	8.895437	-0.060409	4.558214
302.082783	7156.962067	8.900442	-0.060475	4.560752
302.381615	7164.885447	8.905447	-0.060536	4.563245
302.523102	7172.980314	8.910451	-0.060567	4.565789
302.890132	7180.969854	8.915456	-0.060640	4.568300
303.202942	7189.009062	8.920461	-0.060704	4.570825
303.686518	7197.046762	8.925466	-0.060799	4.573348
303.677312	7205.074278	8.930471	-0.060802	4.575866
304.268642	7213.051744	8.935475	-0.060918	4.578367
304.345672	7221.149494	8.940480	-0.060937	4.580904
304.688442	7229.086679	8.945485	-0.061006	4.583390
305.132896	7237.156491	8.950490	-0.061094	4.585916
305.360161	7245.145218	8.955495	-0.061141	4.588415
305.404106	7253.249233	8.960499	-0.061155	4.590948
305.564368	7261.182243	8.965504	-0.061189	4.593427
305.766205	7269.220426	8.970509	-0.061232	4.595937
306.229388	7277.178846	8.975514	-0.061323	4.598421
306.368654	7285.182213	8.980519	-0.061355	4.600917
306.949133	7293.176139	8.985523	-0.061468	4.603410
307.018507	7301.252831	8.990528	-0.061486	4.605926
307.117144	7309.247613	8.995533	-0.061509	4.608416
306.870684	7317.380450	9.000538	-0.061468	4.610946
307.042683	7325.313447	9.005543	-0.061506	4.613414
307.842830	7333.278912	9.010547	-0.061660	4.615891
308.158924	7341.255440	9.015552	-0.061724	4.618370
308.217348	7349.309508	9.020557	-0.061740	4.620871
308.892558	7357.303992	9.025562	-0.061870	4.623352
309.049097	7365.342538	9.030567	-0.061905	4.625846
309.167270	7373.384567	9.035571	-0.061932	4.628339
309.589410	7381.407199	9.040576	-0.062015	4.630825
309.395627	7389.415254	9.045581	-0.061984	4.633305
309.719246	7397.449907	9.050586	-0.062050	4.635792
310.294755	7405.344296	9.055591	-0.062162	4.638234
310.612164	7413.476711	9.060595	-0.062226	4.640749
310.655667	7421.445176	9.065600	-0.062239	4.643211
310.598413	7429.525159	9.070605	-0.062234	4.645706
311.134432	7437.474546	9.075610	-0.062339	4.648160
310.861482	7445.556239	9.080615	-0.062293	4.650654
311.434016	7453.567026	9.085619	-0.062405	4.653124
311.540794	7461.571172	9.090624	-0.062430	4.655590
312.002760	7469.517821	9.095629	-0.062521	4.658038
311.867206	7477.625861	9.100634	-0.062501	4.660534
312.423378	7485.543709	9.105639	-0.062609	4.662970
312.811740	7493.621168	9.110643	-0.062687	4.665454
312.774321	7501.640712	9.115648	-0.062685	4.667919
313.217663	7509.653850	9.120653	-0.062773	4.670380
313.541192	7517.706837	9.125658	-0.062838	4.672853
313.806295	7525.723426	9.130663	-0.062893	4.675312
314.062196	7533.711748	9.135667	-0.062945	4.677762
314.231980	7541.723557	9.140672	-0.062982	4.680218
314.535490	7549.672655	9.145677	-0.063044	4.682653
314.630617	7557.734658	9.150682	-0.063066	4.685122
314.958706	7565.727052	9.155687	-0.063133	4.687568
315.434562	7573.799704	9.160691	-0.063226	4.690036
315.593515	7581.792124	9.165696	-0.063261	4.692480
315.553714	7589.781011	9.170701	-0.063259	4.694921
315.993371	7597.821636	9.175706	-0.063346	4.697376
316.216529	7605.756423	9.180711	-0.063392	4.699798
316.463158	7613.871546	9.185715	-0.063443	4.702273
316.688148	7621.851678	9.190720	-0.063490	4.704706
316.645239	7629.897453	9.195725	-0.063487	4.707158
317.185349	7637.830970	9.200730	-0.063593	4.709574
317.427908	7645.911060	9.205735	-0.063643	4.712033
317.772488	7653.907685	9.210739	-0.063713	4.714466
317.960563	7661.963273	9.215744	-0.063753	4.716916
318.060086	7669.899394	9.220749	-0.063776	4.719328
318.327980	7678.009084	9.225754	-0.063831	4.721791
318.031813	7685.934931	9.230759	-0.063781	4.724198
318.291504	7694.075699	9.235763	-0.063835	4.726668
318.921769	7701.969725	9.240768	-0.063957	4.729061
319.059862	7710.076203	9.245773	-0.063988	4.731519
319.187534	7718.053942	9.250778	-0.064017	4.733936
319.249072	7726.124070	9.255783	-0.064033	4.736380
319.683570	7734.126580	9.260787	-0.064119	4.738801
320.137134	7742.205745	9.265792	-0.064209	4.741244
320.037858	7750.091232	9.270797	-0.064196	4.743629
320.383094	7758.169844	9.275802	-0.064265	4.746070
320.283547	7766.222591	9.280807	-0.064252	4.748502
320.220697	7774.254891	9.285811	-0.064245	4.750928
320.592512	7782.209798	9.290816	-0.064319	4.753327
320.737515	7790.288210	9.295821	-0.064351	4.755763
321.317339	7798.282181	9.300826	-0.064465	4.758172
321.723246	7806.219899	9.305831	-0.064545	4.760562
322.230632	7814.243526	9.310835	-0.064645	4.762977
322.214054	7822.266840	9.315840	-0.064647	4.765392
322.487346	7830.286439	9.320845	-0.064703	4.767804
323.001131	7838.338378	9.325850	-0.064804	4.770223
322.947118	7846.413206	9.330855	-0.064799	4.772650
323.309744	7854.403574	9.335859	-0.064871	4.775049
323.982031	7862.350151	9.340864	-0.065001	4.777433
324.029734	7870.375937	9.345869	-0.065015	4.779841
324.527283	7878.395775	9.350874	-0.065113	4.782244
324.591464	7886.407038	9.355879	-0.065130	4.784645
324.990856	7894.476960	9.360883	-0.065210	4.787062
324.840434	7902.506642	9.365888	-0.065187	4.789467
324.836645	7910.483480	9.370893	-0.065191	4.791854
325.695819	7918.470752	9.375898	-0.065356	4.794240
325.666256	7926.521233	9.380903	-0.065356	4.796648
325.888440	7934.516995	9.385907	-0.065402	4.799036
326.460655	7942.536608	9.390912	-0.065514	4.801429
326.746946	7950.450354	9.395917	-0.065572	4.803791
326.898707	7958.611384	9.400922	-0.065606	4.806225
326.729138	7966.572674	9.405927	-0.065579	4.808600
327.285920	7974.645381	9.410931	-0.065688	4.811005
327.546717	7982.582336	9.415936	-0.065742	4.813368
327.963984	7990.058651	9.420941	-0.065824	4.815593
327.928342	7994.800928	9.425946	-0.065821	4.817005

328.123214	7997.089324	9.430951	-0.065858	4.817685
328.324877	7998.695089	9.435955	-0.065897	4.818162
328.526784	7999.489913	9.440960	-0.065935	4.818398
328.728955	7999.977331	9.445965	-0.065972	4.818542
328.693205	8000.318937	9.450970	-0.065966	4.818644
328.232142	8000.266715	9.455975	-0.065880	4.818630
328.955014	8000.190134	9.460979	-0.066014	4.818605
329.013370	8000.389218	9.465984	-0.066025	4.818664
329.321225	8000.382753	9.470989	-0.066082	4.818660
329.338632	8000.207729	9.475994	-0.066085	4.818608
329.503869	8000.364143	9.480999	-0.066116	4.818654
329.660610	8000.388227	9.486003	-0.066145	4.818661
329.766990	8000.436836	9.491008	-0.066165	4.818675
329.783857	8000.356246	9.496013	-0.066168	4.818651
330.186664	8000.264978	9.501018	-0.066243	4.818622
330.034996	8000.499092	9.506023	-0.066215	4.818692
330.165576	8000.407401	9.511027	-0.066239	4.818664
329.973227	8000.221227	9.516032	-0.066203	4.818610
329.680716	8000.178557	9.521037	-0.066148	4.818598
329.799065	8000.070966	9.526042	-0.066170	4.818566
329.686139	8000.179660	9.531047	-0.066149	4.818599
329.974696	8000.035475	9.536051	-0.066202	4.818555
329.482271	7999.991235	9.541056	-0.066110	4.818543
329.589758	7999.963253	9.546061	-0.066130	4.818535
330.122769	8000.186400	9.551066	-0.066230	4.818599
330.441743	8000.408848	9.556071	-0.066289	4.818664
330.386511	8000.194040	9.561075	-0.066278	4.818600
330.435396	8000.194672	9.566080	-0.066287	4.818600
330.616788	8000.106796	9.571085	-0.066321	4.818573
330.289168	8000.095145	9.576090	-0.066260	4.818571
330.822403	8000.187130	9.581095	-0.066359	4.818596
330.772356	7999.995477	9.586099	-0.066350	4.818540
331.069248	8000.149425	9.591104	-0.066405	4.818584
331.388784	8000.218672	9.596109	-0.066464	4.818604
331.641030	8000.209381	9.601114	-0.066511	4.818600
331.320412	8000.203066	9.606119	-0.066451	4.818599
331.314471	8000.037175	9.611123	-0.066450	4.818550
331.209597	8000.187952	9.616128	-0.066430	4.818595
331.031591	8000.042891	9.621133	-0.066397	4.818553
331.578011	8000.087829	9.626138	-0.066499	4.818564
331.675253	8000.254903	9.631143	-0.066517	4.818613
332.048056	8000.165341	9.636147	-0.066586	4.818585
331.791044	8000.324618	9.641152	-0.066538	4.818634
331.765746	8000.142729	9.646157	-0.066533	4.818580
332.136755	8000.244137	9.651162	-0.066602	4.818608
331.788735	8000.244806	9.656167	-0.066537	4.818610
332.065800	8000.225348	9.661171	-0.066589	4.818603
331.754575	8000.035508	9.666176	-0.066530	4.818548
332.038413	8000.176697	9.671181	-0.066583	4.818589
332.182665	7999.973946	9.676186	-0.066610	4.818528
331.485589	7999.986829	9.681191	-0.066480	4.818534
332.088481	7999.900284	9.686195	-0.066592	4.818506
332.365341	8000.186202	9.691200	-0.066644	4.818590
332.312062	8000.124627	9.696205	-0.066634	4.818572
332.521689	8000.128420	9.701210	-0.066673	4.818572
332.299821	8000.082473	9.706215	-0.066631	4.818560
332.490315	8000.006258	9.711219	-0.066666	4.818536
332.304501	8000.183261	9.716224	-0.066632	4.818590
331.953889	8000.026485	9.721229	-0.066566	4.818544
332.244732	8000.097456	9.726234	-0.066620	4.818564
331.946427	7999.973900	9.731239	-0.066565	4.818529
331.948264	7999.838543	9.736243	-0.066565	4.818488
332.131263	7999.987852	9.741248	-0.066599	4.818532
332.537111	8000.120150	9.746253	-0.066674	4.818570
332.463001	7999.992188	9.751258	-0.066660	4.818532
332.407115	7999.978853	9.756263	-0.066650	4.818528
332.639152	8000.092079	9.761267	-0.066693	4.818561
332.341595	7999.911863	9.766272	-0.066637	4.818509
332.826034	8000.075626	9.771277	-0.066727	4.818556
332.740073	8000.047204	9.776282	-0.066711	4.818547
333.067026	8000.272920	9.781287	-0.066772	4.818613
333.014400	8000.077024	9.786291	-0.066762	4.818555
333.001667	8000.145062	9.791296	-0.066760	4.818576
333.064186	7999.970618	9.796301	-0.066771	4.818523
333.407575	8000.073766	9.801306	-0.066835	4.818553
332.977195	8000.132121	9.806311	-0.066755	4.818572
333.259269	8000.141064	9.811315	-0.066807	4.818573
333.263846	8000.113830	9.816320	-0.066808	4.818565
333.086393	8000.117788	9.821325	-0.066775	4.818567
332.871934	7999.946005	9.826330	-0.066735	4.818517
332.653282	7999.984053	9.831335	-0.066694	4.818529
332.847501	7999.928876	9.836339	-0.066730	4.818512
333.071839	7999.973789	9.841344	-0.066771	4.818524
333.180742	8000.080154	9.846349	-0.066792	4.818556
333.491358	8000.182873	9.851354	-0.066849	4.818585
333.364446	8000.178049	9.856359	-0.066826	4.818584
333.323550	7999.894155	9.861363	-0.066818	4.818500
332.975869	7999.970388	9.866368	-0.066753	4.818524
332.963815	7999.889415	9.871373	-0.066751	4.818500
333.626530	8000.136331	9.876378	-0.066874	4.818571
333.353002	8000.006796	9.881383	-0.066823	4.818533
333.661020	7999.804093	9.886387	-0.066880	4.818472
333.538620	8000.126755	9.891392	-0.066857	4.818568
333.514053	8000.125374	9.896397	-0.066853	4.818568
333.696741	8000.116221	9.901402	-0.066886	4.818564
333.715784	8000.162639	9.906407	-0.066890	4.818578
333.866251	8000.115282	9.911411	-0.066918	4.818563
333.647550	8000.144934	9.916416	-0.066877	4.818573
333.727241	8000.161714	9.921421	-0.066892	4.818578
333.549303	8000.094302	9.926426	-0.066858	4.818558
333.857538	8000.293542	9.931431	-0.066916	4.818616
333.964818	8000.197343	9.936435	-0.066936	4.818587
333.857198	8000.137150	9.941440	-0.066915	4.818570
333.933752	8000.309211	9.946445	-0.066930	4.818621
334.022252	8000.144549	9.951450	-0.066946	4.818571
334.062775	8000.183903	9.956455	-0.066953	4.818583
334.103291	8000.045897	9.961459	-0.066961	4.818542
333.998318	8000.112725	9.966464	-0.066941	4.818562
334.180681	8000.271483	9.971469	-0.066975	4.818609
334.161487	8000.089664	9.976474	-0.066971	4.818555
334.006840	8000.097069	9.981479	-0.066942	4.818557
334.137726	8000.157550	9.986483	-0.066966	4.818575
334.226038	8000.158702	9.991488	-0.066983	4.818575
333.913712	8000.006616	9.996493	-0.066924	4.818531
334.225399	7999.952981	10.001498	-0.066982	4.818514
334.109423	8000.177083	10.006503	-0.066961	4.818581
334.190949	8000.058507	10.011507	-0.066976	4.818545
334.197857	7999.911665	10.016512	-0.066977	4.818502
334.109640	8000.041680	10.021517	-0.066960	4.818541
334.322283	8000.096938	10.026522	-0.067000	4.818556
334.222358	8000.151238	10.031527	-0.066981	4.818573
334.402066	8000.005616	10.036531	-0.067014	4.818529
334.509831	8000.174939	10.041536	-0.067034	4.818579
334.306606	8000.109291	10.046541	-0.066996	4.818560
334.115633	8000.091031	10.051546	-0.066961	4.818555
334.349294	8000.196941	10.056551	-0.067004	4.818586
334.552085	8000.095699	10.061555	-0.067042	4.818555
334.082106	8000.090565	10.066560	-0.066954	4.818555
334.524500	8000.178228	10.071565	-0.067036	4.818580
334.649958	8000.315252	10.076570	-0.067060	4.818620
334.124004	8000.037567	10.081575	-0.066962	4.818539
334.428446	7999.980689	10.086579	-0.067018	4.818521
334.462177	8000.007360	10.091584	-0.067024	4.818529
333.925983	7999.885918	10.096589	-0.066924	4.818495
333.831368	7999.830096	10.101594	-0.066906	4.818479
333.940282	7999.933313	10.106599	-0.066927	4.818509
334.329577	7999.825077	10.111603	-0.066999	4.818475
333.926649	8000.011826	10.116608	-0.066924	4.818532
333.892483	7999.908523	10.121613	-0.066917	4.818502
333.879722	7999.827539	10.126618	-0.066915	4.818478
333.903201	8000.073410	10.131623	-0.066919	4.818551
333.739368	7999.763763	10.136627	-0.066888	4.818459
333.622715	7999.889204	10.141632	-0.066867	4.818497
333.728952	7999.873799	10.146637	-0.066886	4.818492
333.786078	7999.862997	10.151642	-0.066897	4.818489
333.767273	7999.847000	10.156647	-0.066893	4.818484
333.689844	7999.865914	10.161651	-0.066879	4.818490
334.181628	8000.019287	10.166656	-0.066970	4.818534
334.308959	7999.845692	10.171661	-0.066994	4.818482
334.771782	8000.137219	10.176666	-0.067080	4.818566
334.671296	8000.037239	10.181671	-0.067061	4.818537
334.484795	8000.006444	10.186675	-0.067026	4.818529
334.804949	8000.086205	10.191680	-0.067086	4.818551
334.622240	7999.900138	10.196685	-0.067051	4.818497
334.229496	7999.984174	10.201690	-0.066978	4.818523
333.830112	7999.824651	10.206695	-0.066904	4.818477
334.041055	7999.856797	10.211699	-0.066943	4.818486
334.127804	7999.922993	10.216704	-0.066959	4.818505
334.131380	7999.934576	10.221709	-0.066959	4.818509
333.916357	7999.886617	10.226714	-0.066919	4.818495
333.907461	7999.980942	10.231719	-0.066918	4.818523
334.250593	7999.865802	10.236723	-0.066981	4.818488
334.551544	7999.997781	10.241728	-0.067037	4.818526
334.517639	8000.051899	10.246733	-0.067031	4.818542
334.487073	7999.780728	10.251738	-0.067025	4.818462
334.647711	7999.941298	10.256743	-0.067055	4.818509
334.652965	7999.907775	10.261747	-0.067056	4.818499
334.713561	8000.028202	10.266752	-0.067067	4.818534
334.379898	7999.856946	10.271757	-0.067004	4.818485
334.935873	7999.911467	10.276762	-0.067108	4.818499
334.448515	7999.969072	10.281767	-0.067017	4.818518
334.056564	7999.811745	10.286771	-0.066944	4.818472
334.560863	7999.862436	10.291776	-0.067038	4.818486
335.010864	8000.142254	10.296781	-0.067121	4.818567
335.035678	7999.924279	10.301786	-0.067126	4.818502
334.893014	8000.086114	10.306791	-0.067099	4.818551
334.609092	7999.984773	10.311795	-0.067046	4.818522
334.791301	8000.075315	10.316800	-0.067080	4.818548
334.542477	7999.826462	10.321805	-0.067033	4.818475
334.737715	7999.996932	10.326810	-0.067070	4.818525
335.116739	8000.038636	10.331815	-0.067140	4.818536
335.109753	8000.029090	10.336819	-0.067139	4.818533
335.082899	8000.037125	10.341824	-0.067134	4.818536
335.236080	7999.933132	10.346829	-0.067162	4.818504
335.137636	8000.148023	10.351834	-0.067144	4.818568
334.929859	8000.005702	10.356839	-0.067105	4.818527
335.407122	8000.041352	10.361843	-0.067194	4.818536
334.971709	8000.048214	10.366848	-0.067112	4.818539
335.013186	8000.017266	10.371853	-0.067120	4.818530
335.255367	7999.874563	10.376858	-0.067165	4.818487
335.075355	8000.070540	10.381863	-0.067131	4.818546
334.825570	8000.111327	10.386867	-0.067085	4.818559
334.920592	7999.872237	10.391872	-0.067102	4.818487
334.747530	7999.908785	10.396877	-0.067070	4.818499
334.928054	7999.926890	10.401882	-0.067103	4.818503
334.780636	7999.979517	10.406887	-0.067076	4.818520
335.701371	8000.004204	10.411891	-0.067247	4.818523
335.693882	8000.145779	10.416896	-0.067246	4.818566
335.754383	8000.248368	10.421901	-0.067257	4.818596
335.715725	8000.133455	10.426906	-0.067250	4.818562
335.482393	8000.129329	10.431911	-0.067206	4.818561
335.189804	7999.809580	10.436915	-0.067151	4.818467
335.306467	8000.056683	10.441920	-0.067173	4.818541
335.298929	7999.800502	10.446925	-0.067171	4.818464
335.626397	8000.006297	10.451930	-0.067232	4.818524
335.624307	8000.117508	10.456935	-0.067232	4.818557
335.797040	8000.048405	10.461939	-0.067264	4.818536
335.405998	7999.998127	10.466944	-0.067191	4.818523
335.440427	8000.117163	10.471949	-0.067197	4.818558
335.524220	7999.927249	10.476954	-0.067213	4.818501
335.592040	8000.176862	10.481959	-0.067225	4.818575
335.613612	8000.032306	10.486963	-0.067229	4.818532
335.748698	7999.993143	10.491968	-0.067254	4.818520
335.771912	8000.135122	10.496973	-0.067258	4.818562
335.885754	8000.065245	10.501978	-0.067279	4.818541
335.822836	8000.092745	10.506983	-0.067268	4.818549
336.022783	8000.107960	10.511987	-0.067305	4.818553
336.111280	8000.243453	10.516992	-0.067321	4.818593
335.913628	8000.194666	10.521997	-0.067284	4.818579
335.759067	8000.140149	10.527002	-0.067255	4.818564
336.117297	8000.336914	10.532007	-0.067322	4.818621
336.349020	8000.165733	10.537011	-0.067365	4.818569
335.974160	8000.170239	10.542016	-0.067295	4.818572
336.040765	8000.377862	10.547021	-0.067307	4.818633
336.027939	8000.232851	10.552026	-0.067305	4.818590
335.779151	8000.183391	10.557031	-0.067258	4.818576
336.137200	8000.125121	10.562035	-0.067325	4.818558
336.244317	8000.232523	10.567040	-0.067345	4.818589
335.899470	8000.157661	10.572045	-0.067280	4.818568
336.224660	8000.101057	10.577050	-0.067341	4.818550
336.143566	8000.254261	10.582055	-0.067325	4.818596
336.283511	8000.226707	10.587059	-0.067351	4.818587
335.979281	7999.984458	10.592064	-0.067294	4.818517
336.120892	8000.206708	10.597069	-0.067321	4.818582
336.082999	8000.112795	10.602074	-0.067314	4.818554
335.906814	8000.001321	10.607079	-0.067281	4.818522
335.966133	8000.097597	10.612083	-0.067292	4.818550
336.359767	8000.186727	10.617088	-0.067365	4.818575
336.206157	8000.137469	10.622093	-0.067336	4.818561
336.298562	8000.121884	10.627098	-0.067353	4.818556
336.352835	8000.260076	10.632103	-0.067363	4.818597
336.320954	8000.252302	10.637107	-0.067357	4.818595
335.976394	7999.997977	10.642112	-0.067293	4.818521
335.880131	8000.031336	10.647117	-0.067275	4.818531
336.043776	8000.096450	10.652122	-0.067305	4.818550
336.133047	8000.115457	10.657127	-0.067322	4.818555
336.236812	8000.058040	10.662131	-0.067341	4.818537
336.217692	8000.154335	10.667136	-0.067337	4.818566
335.964067	7999.967328	10.672141	-0.067290	4.818512
336.383830	8000.031611	10.677146	-0.067368	4.818529
336.267839	8000.154969	10.682151	-0.067346	4.818566
336.419523	8000.006875	10.687155	-0.067374	4.818522
336.428227	8000.200092	10.692160	-0.067376	4.818579
336.636498	8000.172387	10.697165	-0.067414	4.818570
336.407422	7999.955264	10.702170	-0.067371	4.818506
336.197554	7999.998674	10.707175	-0.067332	4.818520
336.433097	8000.000713	10.712179	-0.067376	4.818520
336.290257	8000.055500	10.717184	-0.067349	4.818536
336.213545	8000.139493	10.722189	-0.067335	4.818562
336.366763	7999.979874	10.727194	-0.067363	4.818514
335.964728	8000.143549	10.732199	-0.067288	4.818564
336.182638	7999.929159	10.737203	-0.067329	4.818499
336.170565	7999.846081	10.742208	-0.067326	4.818475
336.247296	8000.042289	10.747213	-0.067341	4.818533
336.452669	7999.824584	10.752218	-0.067379	4.818467
336.100686	7999.999413	10.757223	-0.067313	4.818521
336.283931	7999.913655	10.762227	-0.067347	4.818494
336.617154	8000.054465	10.767232	-0.067409	4.818535
336.323795	8000.074737	10.772237	-0.067354	4.818542
336.549465	7999.896131	10.777242	-0.067396	4.818488
336.386900	8000.189947	10.782247	-0.067366	4.818576
336.419245	8000.103254	10.787251	-0.067372	4.818550
336.527306	8000.218015	10.792256	-0.067392	4.818584
336.281943	7999.998579	10.797261	-0.067346	4.818520
336.491867	8000.022321	10.802266	-0.067385	4.818526
336.510425	8000.042497	10.807271	-0.067388	4.818532
336.668775	8000.070809	10.812275	-0.067418	4.818540
336.907467	8000.198835	10.817280	-0.067462	4.818577
336.714179	8000.138559	10.822285	-0.067426	4.818560
336.643534	8000.023223	10.827290	-0.067412	4.818526
336.630250	8000.129041	10.832295	-0.067410	4.818557
336.696849	8000.023907	10.837299	-0.067422	4.818526
336.589247	8000.070761	10.842304	-0.067402	4.818540
336.536178	8000.136174	10.847309	-0.067392	4.818560
336.567404	8000.040020	10.852314	-0.067398	4.818531
336.574189	8000.070537	10.857319	-0.067399	4.818540
336.493048	8000.034827	10.862323	-0.067384	4.818530
336.513569	8000.025643	10.867328	-0.067387	4.818527
336.553686	7999.964240	10.872333	-0.067395	4.818508
336.503211	7999.984558	10.877338	-0.067385	4.818515
336.478224	8000.147945	10.882343	-0.067380	4.818563
336.369392	7999.977533	10.887347	-0.067360	4.818513
336.296624	8000.012251	10.892352	-0.067346	4.818524
336.505163	8000.259524	10.897357	-0.067385	4.818596
336.426430	7999.955168	10.902362	-0.067370	4.818506
336.339319	8000.068411	10.907367	-0.067354	4.818540
336.487645	7999.959105	10.912371	-0.067381	4.818507
336.453000	8000.089830	10.917376	-0.067375	4.818546
336.106727	7999.943584	10.922381	-0.067310	4.818504
336.380126	7999.953467	10.927386	-0.067361	4.818506
336.456000	8000.095091	10.932391	-0.067375	4.818548
336.688181	8000.077146	10.937395	-0.067418	4.818541
336.643554	7999.953757	10.942400	-0.067410	4.818505
336.490244	8000.035693	10.947405	-0.067381	4.818530
336.652116	8000.060903	10.952410	-0.067411	4.818537
336.667173	8000.175490	10.957415	-0.067414	4.818571
336.393614	7999.897960	10.962419	-0.067363	4.818489
336.438856	8000.033933	10.967424	-0.067371	4.818530
336.246894	7999.998865	10.972429	-0.067335	4.818520
335.882949	7999.856587	10.977434	-0.067267	4.818479
335.915125	7999.975594	10.982439	-0.067273	4.818514
336.240560	7999.893805	10.987443	-0.067333	4.818489
335.834861	7999.869573	10.992448	-0.067258	4.818483
335.320510	7999.892190	10.997453	-0.067162	4.818492
335.542263	7999.792247	11.002458	-0.067203	4.818461
335.598720	7999.845454	11.007463	-0.067213	4.818477
336.404815	7999.921110	11.012467	-0.067363	4.818496
336.467552	8000.043670	11.017472	-0.067375	4.818532
336.247558	7999.933718	11.022477	-0.067334	4.818501
336.744703	7999.887771	11.027482	-0.067426	4.818485
336.565272	8000.037582	11.032487	-0.067393	4.818530
336.911528	8000.092506	11.037491	-0.067457	4.818545
336.412830	8000.081739	11.042496	-0.067364	4.818544
336.526909	8000.026557	11.047501	-0.067385	4.818527
336.451238	7999.910107	11.052506	-0.067371	4.818493
336.523185	8000.088412	11.057511	-0.067384	4.818546
336.622695	8000.041434	11.062515	-0.067403	4.818531
336.185165	7999.949612	11.067520	-0.067321	4.818506
336.626546	8000.154816	11.072525	-0.067403	4.818565
336.611378	8000.080092	11.077530	-0.067400	4.818543
336.632796	8000.113950	11.082535	-0.067404	4.818553
336.944211	7999.958510	11.087539	-0.067462	4.818505
336.566206	7999.821292	11.092544	-0.067391	4.818466
336.344654	7999.917024	11.097549	-0.067350	4.818495
336.499014	7999.880213	11.102554	-0.067379	4.818484
336.847298	7999.977142	11.107559	-0.067444	4.818511
336.806929	7999.969255	11.112563	-0.067436	4.818509
336.652373	7999.988204	11.117568	-0.067407	4.818515
336.316130	7999.865180	11.122573	-0.067344	4.818480
336.566846	7999.918844	11.127578	-0.067391	4.818495
336.347548	7999.812051	11.132583	-0.067350	4.818464
336.569248	7999.802363	11.137587	-0.067391	4.818460
336.293732	7999.874296	11.142592	-0.067340	4.818483
335.897529	7999.943593	11.147597	-0.067266	4.818505
335.999739	7999.799049	11.152602	-0.067284	4.818462
335.944472	7999.863382	11.157607	-0.067274	4.818481
336.067790	7999.721215	11.162611	-0.067297	4.818438
336.235524	7999.950101	11.167616	-0.067328	4.818506
335.796963	7999.883457	11.172621	-0.067246	4.818487
336.320222	7999.824208	11.177626	-0.067344	4.818468
336.824045	8000.040727	11.182631	-0.067437	4.818530
336.827896	8000.011382	11.187635	-0.067438	4.818522
336.837812	7999.963226	11.192640	-0.067440	4.818507
336.496153	7999.928289	11.197645	-0.067376	4.818498
336.407258	7999.787528	11.202650	-0.067359	4.818457
336.405635	7999.892447	11.207655	-0.067359	4.818488
336.531143	7999.880445	11.212659	-0.067382	4.818484
336.569098	7999.957550	11.217664	-0.067389	4.818507
336.581625	8000.068955	11.222669	-0.067391	4.818540
336.694874	7999.906711	11.227674	-0.067412	4.818491
336.748454	8000.040696	11.232679	-0.067422	4.818531
337.031463	7999.991934	11.237683	-0.067475	4.818515
336.981602	8000.016458	11.242688	-0.067465	4.818522
336.958206	8000.189314	11.247693	-0.067461	4.818574
337.032689	8000.062242	11.252698	-0.067475	4.818536
336.906605	8000.075268	11.257703	-0.067451	4.818540
336.819510	8000.146531	11.262707	-0.067435	4.818562
336.830716	8000.186552	11.267712	-0.067437	4.818574
337.030135	8000.210158	11.272717	-0.067474	4.818580
337.124490	8000.019327	11.277722	-0.067491	4.818523
336.789968	8000.168148	11.282727	-0.067429	4.818568
336.808993	8000.002565	11.287731	-0.067432	4.818519
336.988442	8000.125612	11.292736	-0.067465	4.818555
337.148513	8000.036401	11.297741	-0.067495	4.818528
337.476890	8000.124676	11.302746	-0.067556	4.818553
337.354358	8000.208068	11.307751	-0.067533	4.818578
337.701775	8000.320737	11.312755	-0.067598	4.818610
337.518794	8000.212314	11.317760	-0.067564	4.818579
337.277432	8000.294142	11.322765	-0.067519	4.818604
337.153535	8000.168656	11.327770	-0.067495	4.818567
337.215201	8000.215639	11.332775	-0.067507	4.818581
337.133321	8000.031934	11.337779	-0.067491	4.818526
337.108401	8000.086173	11.342784	-0.067486	4.818543
336.930445	8000.069129	11.347789	-0.067453	4.818538
336.894603	8000.092788	11.352794	-0.067446	4.818546
337.541213	8000.150617	11.357799	-0.067567	4.818560
337.541396	8000.128570	11.362803	-0.067567	4.818554
337.378337	8000.144257	11.367808	-0.067536	4.818559
337.218909	8000.170488	11.372813	-0.067506	4.818567
337.659943	8000.115411	11.377818	-0.067588	4.818549
337.545071	8000.240885	11.382823	-0.067567	4.818587
337.148673	8000.133854	11.387827	-0.067493	4.818557
337.349299	8000.231994	11.392832	-0.067530	4.818585
337.026752	8000.028329	11.397837	-0.067470	4.818526
337.007199	7999.904219	11.402842	-0.067466	4.818489
336.594581	7999.902983	11.407847	-0.067389	4.818490
337.049797	7999.935198	11.412851	-0.067474	4.818498
336.896002	7999.916375	11.417856	-0.067445	4.818493
336.647948	7999.934094	11.422861	-0.067399	4.818499
336.873278	7999.867781	11.427866	-0.067440	4.818479
336.535395	7999.846537	11.432871	-0.067377	4.818474
336.713809	8000.048282	11.437875	-0.067411	4.818533
337.213375	7999.939397	11.442880	-0.067503	4.818499
336.955732	8000.061943	11.447885	-0.067455	4.818536
337.041603	7999.989597	11.452890	-0.067471	4.818514
336.972770	7999.925711	11.457895	-0.067458	4.818496
337.342388	8000.005081	11.462899	-0.067527	4.818518
337.220231	8000.101072	11.467904	-0.067504	4.818547
337.092957	8000.050061	11.472909	-0.067480	4.818532
337.290791	7999.987584	11.477914	-0.067517	4.818513
337.274456	8000.201466	11.482919	-0.067514	4.818576
337.258815	7999.932571	11.487923	-0.067511	4.818497
337.020921	7999.929433	11.492928	-0.067466	4.818497
337.216765	8000.166046	11.497933	-0.067503	4.818566
337.108364	8000.067004	11.502938	-0.067483	4.818537
336.882216	7999.986356	11.507943	-0.067440	4.818514
336.763260	7999.811613	11.512947	-0.067418	4.818462
336.797155	8000.008309	11.517952	-0.067424	4.818521
336.819789	8000.039034	11.522957	-0.067428	4.818530
337.054484	7999.931913	11.527962	-0.067472	4.818497
337.150517	8000.100042	11.532967	-0.067490	4.818547
337.182106	8000.072112	11.537971	-0.067495	4.818538
337.376000	8000.289811	11.542976	-0.067532	4.818602
337.448848	8000.173212	11.547981	-0.067545	4.818567
337.397745	8000.148391	11.552986	-0.067535	4.818560
337.218042	8000.203742	11.557991	-0.067502	4.818577
337.205896	7999.931745	11.562995	-0.067499	4.818497
337.188420	7999.917863	11.568000	-0.067496	4.818492
337.058519	8000.168032	11.573005	-0.067472	4.818567
337.311842	7999.918419	11.578010	-0.067518	4.818492
337.235391	8000.114717	11.583015	-0.067504	4.818551
337.182617	8000.185382	11.588019	-0.067494	4.818572
337.200951	7999.985154	11.593024	-0.067498	4.818512
337.474964	8000.051723	11.598029	-0.067548	4.818531
337.421138	8000.101383	11.603034	-0.067538	4.818546
337.022477	8000.057297	11.608039	-0.067464	4.818535
337.304837	8000.104034	11.613043	-0.067516	4.818547
337.674225	8000.039617	11.618048	-0.067585	4.818527
337.429239	8000.146586	11.623053	-0.067539	4.818560
337.387876	8000.048426	11.628058	-0.067531	4.818531
337.308940	8000.064171	11.633063	-0.067517	4.818536
337.518466	8000.119396	11.638067	-0.067556	4.818551
337.549088	8000.225795	11.643072	-0.067561	4.818583
337.504508	8000.260884	11.648077	-0.067553	4.818593
337.522375	7999.909515	11.653082	-0.067556	4.818489
337.441498	8000.345051	11.658087	-0.067541	4.818619
337.471731	8000.173314	11.663091	-0.067546	4.818567
337.618972	8000.239266	11.668096	-0.067574	4.818586
337.464274	8000.268708	11.673101	-0.067545	4.818596
337.418229	7999.981568	11.678106	-0.067536	4.818511
337.343172	8000.146399	11.683111	-0.067522	4.818560
337.252231	7999.961525	11.688115	-0.067505	4.818505
337.308036	8000.021024	11.693120	-0.067515	4.818523
337.430757	8000.311255	11.698125	-0.067538	4.818609
337.375635	8000.064928	11.703130	-0.067527	4.818536
337.400451	8000.325533	11.708135	-0.067532	4.818613
337.292900	8000.111051	11.713139	-0.067512	4.818550
337.504188	7999.984729	11.718144	-0.067551	4.818511
337.443391	8000.229513	11.723149	-0.067540	4.818584
337.415687	8000.166167	11.728154	-0.067534	4.818566
337.603795	8000.113008	11.733159	-0.067569	4.818549
337.456352	8000.345109	11.738163	-0.067542	4.818619
337.472434	8000.204672	11.743168	-0.067545	4.818577
337.595296	8000.312285	11.748173	-0.067567	4.818608
337.715321	8000.137532	11.753178	-0.067589	4.818556
337.411511	8000.194398	11.758183	-0.067533	4.818574
337.253039	7999.962456	11.763187	-0.067503	4.818506
337.222093	8000.054399	11.768192	-0.067497	4.818533
337.495135	7999.986614	11.773197	-0.067548	4.818512
337.604156	8000.014279	11.778202	-0.067568	4.818520
337.722828	7999.979098	11.783207	-0.067590	4.818509
337.718448	8000.108125	11.788211	-0.067589	4.818547
337.701024	8000.034419	11.793216	-0.067586	4.818525
337.597939	8000.123314	11.798221	-0.067567	4.818552
337.681744	8000.049891	11.803226	-0.067582	4.818530
337.445997	8000.039434	11.808231	-0.067538	4.818528
337.587924	7999.991964	11.813235	-0.067564	4.818513
337.656849	8000.083123	11.818240	-0.067577	4.818540
337.536378	8000.146601	11.823245	-0.067554	4.818559
337.507843	7999.909021	11.828250	-0.067549	4.818489
337.189494	8000.092690	11.833255	-0.067490	4.818545
337.235197	7999.835100	11.838259	-0.067498	4.818468
337.459461	8000.118266	11.843264	-0.067540	4.818551
337.501741	8000.060039	11.848269	-0.067547	4.818534
337.769193	8000.189496	11.853274	-0.067597	4.818571
337.502544	8000.048488	11.858279	-0.067547	4.818530
337.521310	8000.046627	11.863283	-0.067551	4.818530
337.350074	8000.063257	11.868288	-0.067519	4.818535
337.558482	8000.198233	11.873293	-0.067557	4.818575
337.688858	7999.948050	11.878298	-0.067581	4.818500
337.445577	8000.031952	11.883303	-0.067536	4.818526
337.687296	8000.050867	11.888307	-0.067581	4.818530
337.498005	7999.933968	11.893312	-0.067545	4.818496
337.242523	7999.903311	11.898317	-0.067498	4.818488
337.627913	7999.772983	11.903322	-0.067569	4.818448
337.344253	8000.113489	11.908327	-0.067517	4.818550
336.950236	7999.902589	11.913331	-0.067443	4.818489
337.388552	8000.122451	11.918336	-0.067525	4.818553
337.551048	8000.253675	11.923341	-0.067555	4.818591
337.280636	8000.080081	11.928346	-0.067504	4.818541
337.092154	8000.038760	11.933351	-0.067469	4.818529
337.505181	8000.006403	11.938355	-0.067546	4.818518
337.669646	8000.211120	11.943360	-0.067576	4.818578
337.341006	8000.101832	11.948365	-0.067515	4.818547
337.776413	8000.314316	11.953370	-0.067596	4.818608
337.683197	8000.300485	11.958375	-0.067579	4.818605
337.725126	8000.192924	11.963379	-0.067586	4.818572
337.884218	8000.114194	11.968384	-0.067616	4.818548
337.775240	8000.172575	11.973389	-0.067595	4.818566
337.703640	8000.098156	11.978394	-0.067582	4.818544
337.442795	7999.960374	11.983399	-0.067533	4.818504
337.485924	8000.116264	11.988403	-0.067541	4.818551
337.613444	7999.918522	11.993408	-0.067564	4.818491
337.593183	8000.138649	11.998413	-0.067561	4.818557
337.590207	8000.046242	12.003418	-0.067560	4.818529
337.048619	7999.901620	12.008423	-0.067459	4.818488
337.504678	8000.164747	12.013427	-0.067544	4.818565
337.550119	8000.041490	12.018432	-0.067552	4.818528
337.720295	8000.111941	12.023437	-0.067584	4.818548
337.437707	7999.816444	12.028442	-0.067531	4.818462
337.311563	8000.056168	12.033447	-0.067507	4.818533
337.462646	7999.915410	12.038451	-0.067535	4.818491
337.557794	7999.954437	12.043456	-0.067553	4.818502
337.358953	8000.080904	12.048461	-0.067516	4.818541
337.503533	7999.911724	12.053466	-0.067543	4.818490
337.600535	8000.132345	12.058471	-0.067561	4.818555
337.334151	7999.818171	12.063475	-0.067511	4.818462
337.324564	7999.810689	12.068480	-0.067509	4.818460
337.581218	8000.031309	12.073485	-0.067557	4.818525
337.255238	7999.910514	12.078490	-0.067496	4.818490
337.414854	8000.063737	12.083495	-0.067525	4.818535
337.504605	7999.930569	12.088499	-0.067542	4.818495
337.794710	8000.212507	12.093504	-0.067596	4.818578
337.631067	8000.005683	12.098509	-0.067565	4.818517
337.854715	8000.030658	12.103514	-0.067607	4.818524
337.890346	8000.158114	12.108519	-0.067613	4.818561
337.933399	8000.073658	12.113523	-0.067621	4.818536
337.991836	8000.144739	12.118528	-0.067632	4.818557
337.853983	8000.114578	12.123533	-0.067606	4.818549
337.831390	7999.923255	12.128538	-0.067602	4.818492
337.789082	8000.132598	12.133543	-0.067594	4.818554
337.498100	7999.945091	12.138547	-0.067539	4.818500
337.685724	8000.037811	12.143552	-0.067574	4.818526
337.547150	8000.086357	12.148557	-0.067548	4.818541
337.872542	7999.919555	12.153562	-0.067609	4.818491
337.718960	7999.952160	12.158567	-0.067580	4.818501
337.872196	8000.064370	12.163571	-0.067609	4.818534
337.442224	7999.991533	12.168576	-0.067528	4.818514
337.859059	8000.053684	12.173581	-0.067606	4.818531
337.782986	7999.962414	12.178586	-0.067592	4.818504
337.467107	8000.076847	12.183591	-0.067533	4.818539
337.354746	7999.799334	12.188595	-0.067511	4.818457
337.878426	8000.061252	12.193600	-0.067609	4.818533
337.674022	7999.928410	12.198605	-0.067571	4.818494
337.724309	8000.015125	12.203610	-0.067580	4.818520
337.974628	8000.129663	12.208615	-0.067627	4.818553
337.839071	8000.027114	12.213619	-0.067601	4.818523
337.701115	8000.078816	12.218624	-0.067575	4.818539
337.472011	8000.064248	12.223629	-0.067533	4.818535
337.591738	7999.967158	12.228634	-0.067555	4.818506
337.733163	8000.085509	12.233639	-0.067581	4.818541
337.468755	7999.932987	12.238643	-0.067532	4.818496
337.598278	8000.091064	12.243648	-0.067556	4.818543
337.479167	8000.005525	12.248653	-0.067533	4.818518
337.366234	7999.786779	12.253658	-0.067512	4.818453
337.311864	7999.939285	12.258663	-0.067502	4.818499
337.710926	7999.937180	12.263667	-0.067576	4.818497
337.678024	7999.929391	12.268672	-0.067570	4.818494
337.700652	8000.261336	12.273677	-0.067574	4.818593
337.736563	8000.053990	12.278682	-0.067581	4.818531
337.619332	8000.209870	12.283687	-0.067559	4.818578
337.704379	8000.178445	12.288691	-0.067574	4.818568
337.641327	8000.102039	12.293696	-0.067562	4.818546
337.520553	8000.117234	12.298701	-0.067540	4.818551
337.507294	7999.931283	12.303706	-0.067537	4.818496
337.596459	8000.033203	12.308711	-0.067554	4.818526
337.328714	7999.898480	12.313715	-0.067504	4.818487
336.487985	7999.935693	12.318720	-0.067347	4.818501
336.721129	7999.867383	12.323725	-0.067390	4.818480
337.066946	7999.778516	12.328730	-0.067454	4.818452
336.490472	7999.937799	12.333735	-0.067347	4.818502
337.508513	7999.908149	12.338739	-0.067537	4.818489
337.046840	7999.798166	12.343744	-0.067450	4.818458
337.022519	7999.853462	12.348749	-0.067446	4.818474
337.546884	8000.106990	12.353754	-0.067543	4.818548
337.805660	8000.155517	12.358759	-0.067592	4.818561
337.650240	7999.957199	12.363763	-0.067562	4.818503
337.570833	7999.927808	12.368768	-0.067547	4.818494
337.228209	7999.906500	12.373773	-0.067483	4.818489
337.140451	7999.867555	12.378778	-0.067467	4.818478
337.349963	7999.822024	12.383783	-0.067506	4.818464
337.215886	7999.962987	12.388787	-0.067481	4.818506
337.581689	7999.904818	12.393792	-0.067549	4.818487
337.429856	7999.954239	12.398797	-0.067520	4.818503
337.240460	7999.792212	12.403802	-0.067485	4.818455
337.256535	7999.833346	12.408807	-0.067488	4.818467
337.400019	7999.849918	12.413811	-0.067514	4.818472
337.246288	7999.842640	12.418816	-0.067486	4.818470
337.357486	7999.914412	12.423821	-0.067506	4.818491
337.673020	7999.907009	12.428826	-0.067565	4.818488
337.560902	7999.956952	12.433831	-0.067544	4.818503
337.309161	7999.845531	12.438835	-0.067497	4.818471
337.205640	7999.856755	12.443840	-0.067478	4.818475
337.325785	7999.797455	12.448845	-0.067500	4.818457
337.427550	7999.899539	12.453850	-0.067519	4.818487
337.598086	7999.934309	12.458855	-0.067550	4.818496
337.666096	7999.890065	12.463859	-0.067563	4.818483
337.626526	7999.953557	12.468864	-0.067555	4.818502
337.987203	7999.907916	12.473869	-0.067622	4.818487
337.878024	7999.926412	12.478874	-0.067602	4.818493
337.780488	8000.076254	12.483879	-0.067584	4.818538
337.990087	7999.990842	12.488883	-0.067623	4.818512
338.082772	8000.127445	12.493888	-0.067640	4.818552
338.146867	8000.124082	12.498893	-0.067652	4.818551
337.621559	7999.811745	12.503898	-0.067553	4.818460
337.342711	7999.922467	12.508903	-0.067501	4.818494
337.201727	7999.866029	12.513907	-0.067475	4.818477
337.446278	7999.914366	12.518912	-0.067521	4.818491
337.201138	7999.900638	12.523917	-0.067475	4.818488
337.484061	7999.958926	12.528922	-0.067527	4.818504
337.231772	7999.831755	12.533927	-0.067480	4.818467
337.453581	7999.835713	12.538931	-0.067521	4.818467
337.314070	7999.807632	12.543936	-0.067495	4.818460
337.375233	7999.840963	12.548941	-0.067507	4.818469
337.462482	7999.838953	12.553946	-0.067523	4.818468
337.638647	8000.099447	12.558951	-0.067555	4.818545
337.489458	7999.849786	12.563955	-0.067527	4.818472
337.455848	7999.999417	12.568960	-0.067521	4.818516
337.752818	7999.914105	12.573965	-0.067576	4.818490
337.893067	7999.904397	12.578970	-0.067602	4.818486
337.767951	8000.007696	12.583975	-0.067579	4.818517
337.857989	7999.904968	12.588979	-0.067595	4.818487
337.929167	8000.063327	12.593984	-0.067609	4.818533
337.959781	7999.992352	12.598989	-0.067614	4.818512
337.819042	8000.015681	12.603994	-0.067588	4.818520
337.673266	8000.086172	12.608999	-0.067561	4.818541
337.848059	8000.049630	12.614003	-0.067593	4.818530
337.887522	7999.830788	12.619008	-0.067600	4.818464
337.616255	8000.036067	12.624013	-0.067550	4.818526
337.831642	7999.868868	12.629018	-0.067590	4.818476
338.047919	8000.203362	12.634023	-0.067630	4.818575
338.047140	8000.112032	12.639027	-0.067630	4.818547
337.803473	7999.961880	12.644032	-0.067584	4.818504
337.917683	8000.205820	12.649037	-0.067605	4.818576
338.077140	8000.045229	12.654042	-0.067635	4.818527
337.731072	8000.184454	12.659047	-0.067570	4.818570
337.656177	7999.853905	12.664051	-0.067556	4.818472
337.929194	7999.853290	12.669056	-0.067607	4.818471
337.415748	8000.029145	12.674061	-0.067511	4.818525
337.816064	7999.803506	12.679066	-0.067585	4.818457
337.806335	7999.926164	12.684071	-0.067584	4.818493
337.786451	7999.994114	12.689075	-0.067580	4.818513
338.033966	8000.101268	12.694080	-0.067626	4.818544
337.929031	8000.014865	12.699085	-0.067606	4.818519
338.124577	7999.925070	12.704090	-0.067642	4.818492
337.787820	8000.121092	12.709095	-0.067580	4.818551
337.750195	7999.830916	12.714099	-0.067572	4.818465
337.646487	8000.067787	12.719104	-0.067553	4.818536
337.282102	7999.901357	12.724109	-0.067485	4.818488
337.687116	7999.867844	12.729114	-0.067560	4.818476
337.615028	7999.992830	12.734119	-0.067547	4.818514
337.465718	7999.890103	12.739123	-0.067519	4.818484
337.551063	7999.953139	12.744128	-0.067535	4.818502
337.692489	7999.914059	12.749133	-0.067561	4.818490
337.584239	7999.839159	12.754138	-0.067540	4.818468
337.615586	7999.873148	12.759143	-0.067546	4.818478
337.903680	7999.801363	12.764147	-0.067600	4.818456
338.017482	7999.967629	12.769152	-0.067621	4.818505
337.596986	7999.851887	12.774157	-0.067542	4.818472
337.668361	7999.752063	12.779162	-0.067555	4.818442
337.161385	7999.980479	12.784167	-0.067461	4.818512
337.567829	7999.830487	12.789171	-0.067536	4.818466
337.734131	7999.907182	12.794176	-0.067567	4.818488
337.851611	7999.890877	12.799181	-0.067589	4.818482
338.019179	7999.920361	12.804186	-0.067620	4.818491
337.531668	7999.826828	12.809191	-0.067529	4.818465
337.860153	7999.959184	12.814195	-0.067590	4.818503
337.840919	7999.968368	12.819200	-0.067587	4.818506
337.919358	8000.073296	12.824205	-0.067601	4.818536
337.936875	7999.964365	12.829210	-0.067604	4.818504
337.650826	7999.946949	12.834215	-0.067551	4.818500
337.759986	7999.822433	12.839219	-0.067571	4.818462
337.530238	7999.924355	12.844224	-0.067528	4.818494
337.795605	8000.028593	12.849229	-0.067578	4.818524
338.398229	7999.958849	12.854234	-0.067690	4.818501
338.213475	8000.259730	12.859239	-0.067655	4.818591
338.094674	8000.055593	12.864243	-0.067633	4.818531
337.923152	7999.884351	12.869248	-0.067601	4.818480
338.081009	8000.091080	12.874253	-0.067630	4.818541
338.079918	7999.984003	12.879258	-0.067630	4.818509
337.917754	7999.946176	12.884263	-0.067599	4.818499
337.710411	7999.971777	12.889267	-0.067561	4.818507
337.692479	7999.863431	12.894272	-0.067557	4.818475
337.911787	7999.968112	12.899277	-0.067598	4.818505
338.039706	7999.911013	12.904282	-0.067622	4.818488
337.962553	7999.918385	12.909287	-0.067607	4.818490
337.680596	7999.809714	12.914291	-0.067554	4.818459
337.996563	7999.903072	12.919296	-0.067613	4.818486
337.877977	8000.101966	12.924301	-0.067591	4.818545
337.826181	7999.960637	12.929306	-0.067581	4.818503
338.175683	8000.031349	12.934311	-0.067646	4.818523
337.991182	7999.915561	12.939315	-0.067612	4.818489
337.715263	7999.952854	12.944320	-0.067560	4.818502
337.806481	7999.917312	12.949325	-0.067577	4.818491
337.833217	7999.943894	12.954330	-0.067582	4.818498
337.774087	7999.929463	12.959335	-0.067571	4.818494
337.734326	7999.890099	12.964339	-0.067563	4.818483
338.120350	8000.065195	12.969344	-0.067635	4.818533
338.447499	8000.152408	12.974349	-0.067696	4.818558
338.584477	8000.081783	12.979354	-0.067721	4.818536
338.418228	8000.013464	12.984359	-0.067690	4.818517
338.363455	8000.019032	12.989363	-0.067680	4.818519
338.582334	7999.909602	12.994368	-0.067720	4.818485
338.515555	8000.074544	12.999373	-0.067708	4.818535
338.500867	7999.773121	13.004378	-0.067705	4.818445
338.533962	8000.101008	13.009383	-0.067711	4.818542
338.420460	7999.887495	13.014387	-0.067690	4.818479
338.778437	8000.104210	13.019392	-0.067756	4.818542
338.545770	8000.082245	13.024397	-0.067713	4.818537
338.507069	7999.777358	13.029402	-0.067705	4.818446
338.760913	8000.000046	13.034407	-0.067753	4.818512
338.979442	7999.915801	13.039411	-0.067793	4.818486
338.816908	7999.893711	13.044416	-0.067763	4.818480
338.822330	8000.081645	13.049421	-0.067764	4.818536
338.870741	7999.925889	13.054426	-0.067773	4.818489
338.633523	7999.909114	13.059431	-0.067728	4.818485
338.666340	7999.822424	13.064435	-0.067734	4.818459
338.676988	8000.036665	13.069440	-0.067736	4.818523
338.766850	8000.103962	13.074445	-0.067753	4.818542
338.642797	7999.985819	13.079450	-0.067730	4.818508
338.675779	8000.061813	13.084455	-0.067736	4.818530
338.723118	8000.062427	13.089459	-0.067744	4.818530
338.589884	7999.872794	13.094464	-0.067719	4.818474
338.686307	8000.176328	13.099469	-0.067737	4.818564
338.921063	8000.089148	13.104474	-0.067781	4.818537
338.863895	8000.195443	13.109479	-0.067770	4.818569
338.579755	8000.021663	13.114483	-0.067717	4.818519
338.943438	8000.052681	13.119488	-0.067785	4.818526
338.727325	8000.113851	13.124493	-0.067744	4.818546
338.668446	7999.982921	13.129498	-0.067733	4.818507
338.305685	7999.981286	13.134503	-0.067666	4.818508
338.718520	7999.988811	13.139507	-0.067742	4.818508
338.538645	7999.936056	13.144512	-0.067709	4.818493
338.258360	7999.933408	13.149517	-0.067656	4.818494
338.694529	7999.883514	13.154522	-0.067737	4.818477
338.579512	8000.020532	13.159527	-0.067716	4.818518
338.449529	8000.047151	13.164531	-0.067692	4.818527
338.517195	8000.056429	13.169536	-0.067704	4.818529
338.803361	8000.033949	13.174541	-0.067757	4.818522
338.455258	7999.729187	13.179546	-0.067692	4.818432
338.263567	7999.938664	13.184551	-0.067656	4.818495
338.410446	7999.905953	13.189555	-0.067684	4.818485
338.489263	7999.962608	13.194560	-0.067698	4.818502
338.754189	8000.080489	13.199565	-0.067748	4.818536
338.565098	7999.869129	13.204570	-0.067712	4.818473
338.477618	7999.952983	13.209575	-0.067696	4.818499
338.668656	8000.013214	13.214579	-0.067731	4.818516
338.500848	7999.866159	13.219584	-0.067700	4.818473
338.570719	8000.001412	13.224589	-0.067713	4.818513
338.554508	7999.940316	13.229594	-0.067710	4.818495
338.373888	7999.935831	13.234599	-0.067676	4.818494
338.427326	7999.781193	13.239603	-0.067686	4.818448
338.722947	8000.013877	13.244608	-0.067741	4.818516
338.397837	7999.928773	13.249613	-0.067680	4.818492
338.623506	8000.072376	13.254618	-0.067722	4.818534
338.819630	8000.116932	13.259623	-0.067758	4.818546
338.820030	7999.920660	13.264627	-0.067758	4.818488
339.012007	7999.907435	13.269632	-0.067794	4.818483
338.889160	8000.088434	13.274637	-0.067771	4.818537
338.771164	8000.103664	13.279642	-0.067749	4.818542
338.512555	8000.045674	13.284647	-0.067700	4.818526
338.647813	8000.107271	13.289651	-0.067726	4.818544
338.811419	8000.168192	13.294656	-0.067756	4.818561
338.872267	8000.306480	13.299661	-0.067767	4.818602
338.594084	8000.174759	13.304666	-0.067715	4.818564
338.541552	8000.213942	13.309671	-0.067705	4.818576
338.512588	8000.106497	13.314675	-0.067700	4.818544
338.460463	8000.246443	13.319680	-0.067690	4.818586
338.602456	7999.902999	13.324685	-0.067716	4.818483
338.652716	8000.020152	13.329690	-0.067725	4.818518
338.265583	7999.998255	13.334695	-0.067653	4.818513
338.556045	8000.200437	13.339699	-0.067707	4.818572
338.919474	8000.131744	13.344704	-0.067775	4.818550
338.609125	8000.163334	13.349709	-0.067717	4.818561
338.564933	8000.065134	13.354714	-0.067708	4.818532
338.908107	8000.139965	13.359719	-0.067772	4.818553
338.736707	8000.240557	13.364723	-0.067740	4.818583
338.634038	8000.000945	13.369728	-0.067721	4.818512
338.866523	8000.203416	13.374733	-0.067764	4.818572
338.851581	8000.146533	13.379738	-0.067761	4.818555
338.668679	8000.165107	13.384743	-0.067727	4.818561
338.700581	7999.928318	13.389747	-0.067733	4.818491
338.690411	7999.937621	13.394752	-0.067731	4.818493
338.324467	8000.074486	13.399757	-0.067663	4.818536
338.658395	7999.894151	13.404762	-0.067725	4.818481
338.901422	8000.093609	13.409767	-0.067770	4.818539
338.750534	8000.014996	13.414771	-0.067742	4.818516
338.691792	8000.091882	13.419776	-0.067731	4.818539
338.712333	8000.039665	13.424781	-0.067734	4.818524
338.841617	7999.929056	13.429786	-0.067758	4.818490
338.559313	7999.949471	13.434791	-0.067705	4.818497
338.826826	8000.091526	13.439795	-0.067755	4.818539
338.621963	7999.865265	13.444800	-0.067717	4.818472
338.505199	7999.962377	13.449805	-0.067695	4.818502
338.410581	7999.907596	13.454810	-0.067677	4.818486
338.930297	8000.276530	13.459815	-0.067774	4.818593
338.779070	7999.987997	13.464819	-0.067746	4.818508
339.046626	8000.088071	13.469824	-0.067795	4.818537
339.031701	8000.168683	13.474829	-0.067793	4.818561
339.038163	8000.066951	13.479834	-0.067794	4.818531
338.728977	8000.215058	13.484839	-0.067736	4.818576
338.699305	8000.040431	13.489843	-0.067730	4.818524
338.938206	8000.108641	13.494848	-0.067775	4.818543
338.897698	7999.968507	13.499853	-0.067767	4.818502
338.952600	7999.896801	13.504858	-0.067777	4.818480
338.990796	8000.167034	13.509863	-0.067784	4.818561
338.895682	8000.021982	13.514867	-0.067766	4.818518
338.908792	8000.123954	13.519872	-0.067769	4.818548
339.036573	8000.195950	13.524877	-0.067792	4.818569
339.135654	7999.934853	13.529882	-0.067810	4.818491
338.821478	8000.004177	13.534887	-0.067752	4.818513
338.876267	8000.077310	13.539891	-0.067762	4.818534
338.979907	8000.010444	13.544896	-0.067781	4.818514
338.580010	8000.057649	13.549901	-0.067707	4.818530
338.906072	7999.953828	13.554906	-0.067767	4.818497
339.002585	8000.141913	13.559911	-0.067785	4.818553
339.054782	8000.177228	13.564915	-0.067795	4.818563
338.769361	7999.875385	13.569920	-0.067741	4.818475
338.775521	7999.904845	13.574925	-0.067742	4.818483
338.946951	7999.878755	13.579930	-0.067774	4.818475
338.933026	8000.040195	13.584935	-0.067771	4.818523
338.727742	8000.076317	13.589939	-0.067733	4.818535
339.019849	8000.010883	13.594944	-0.067787	4.818514
339.014231	8000.156691	13.599949	-0.067786	4.818557
338.940641	8000.082243	13.604954	-0.067772	4.818536
338.985427	8000.183584	13.609959	-0.067781	4.818566
339.241497	7999.942397	13.614963	-0.067828	4.818493
339.043960	7999.920895	13.619968	-0.067791	4.818487
338.902244	8000.170917	13.624973	-0.067765	4.818562
339.135456	8000.225409	13.629978	-0.067808	4.818577
339.035439	8000.186298	13.634983	-0.067789	4.818566
338.950817	8000.201968	13.639987	-0.067773	4.818571
339.192449	7999.968988	13.644992	-0.067818	4.818501
339.204173	8000.145462	13.649997	-0.067820	4.818553
339.201845	8000.174811	13.655002	-0.067820	4.818562
339.161299	8000.195260	13.660007	-0.067812	4.818568
338.843767	8000.100806	13.665011	-0.067753	4.818541
338.874285	8000.109596	13.670016	-0.067758	4.818544
339.117961	8000.168424	13.675021	-0.067804	4.818561
338.977234	7999.926210	13.680026	-0.067777	4.818489
339.012599	8000.054714	13.685031	-0.067784	4.818527
338.890100	8000.113968	13.690035	-0.067761	4.818545
338.945045	7999.902670	13.695040	-0.067771	4.818482
338.657170	8000.055256	13.700045	-0.067717	4.818529
338.853235	8000.011648	13.705050	-0.067754	4.818515
338.962170	8000.273368	13.710055	-0.067774	4.818592
339.082453	8000.025145	13.715059	-0.067796	4.818518
339.174737	8000.044194	13.720064	-0.067813	4.818523
339.040845	7999.922772	13.725069	-0.067788	4.818488
339.373074	8000.025797	13.730074	-0.067850	4.818517
338.968186	7999.994218	13.735079	-0.067774	4.818509
338.437922	7999.892770	13.740083	-0.067675	4.818481
338.465228	7999.898368	13.745088	-0.067680	4.818483
338.929898	7999.879286	13.750093	-0.067767	4.818475
338.733849	7999.896638	13.755098	-0.067730	4.818481
338.872084	8000.103114	13.760103	-0.067756	4.818542
338.952714	7999.889006	13.765107	-0.067771	4.818478
339.199643	7999.909041	13.770112	-0.067816	4.818483
338.846086	7999.972599	13.775117	-0.067751	4.818503
339.141084	7999.956533	13.780122	-0.067805	4.818497
339.065538	8000.021652	13.785127	-0.067791	4.818517
339.164073	8000.006148	13.790131	-0.067809	4.818512
339.194485	8000.045374	13.795136	-0.067815	4.818524
339.191144	8000.087304	13.800141	-0.067814	4.818536
339.153965	7999.759342	13.805146	-0.067807	4.818439
339.042148	7999.902700	13.810151	-0.067786	4.818482
338.916417	7999.874798	13.815155	-0.067763	4.818474
339.092928	7999.886559	13.820160	-0.067795	4.818477
339.044230	8000.005559	13.825165	-0.067786	4.818512
339.205383	7999.921608	13.830170	-0.067816	4.818487
339.082057	8000.097352	13.835175	-0.067793	4.818540
339.338811	7999.967429	13.840179	-0.067841	4.818500
339.201683	7999.969813	13.845184	-0.067815	4.818501
338.940907	7999.917042	13.850189	-0.067766	4.818487
338.982195	7999.902883	13.855194	-0.067774	4.818482
339.024825	8000.163728	13.860199	-0.067782	4.818560
339.023914	8000.057701	13.865203	-0.067781	4.818528
339.334097	8000.052331	13.870208	-0.067839	4.818525
338.874221	7999.907724	13.875213	-0.067753	4.818484
339.102914	7999.935916	13.880218	-0.067796	4.818492
339.011805	7999.806662	13.885223	-0.067779	4.818453
338.968575	7999.995004	13.890227	-0.067771	4.818510
338.941692	8000.004088	13.895232	-0.067765	4.818512
338.941886	7999.806765	13.900237	-0.067765	4.818454
339.047146	7999.838579	13.905242	-0.067785	4.818463
338.866597	7999.821500	13.910247	-0.067751	4.818458
338.890071	7999.874278	13.915251	-0.067755	4.818474
339.208081	7999.967669	13.920256	-0.067814	4.818501
339.186291	8000.078627	13.925261	-0.067810	4.818534
339.389213	7999.879773	13.930266	-0.067848	4.818474
339.204492	8000.051561	13.935271	-0.067813	4.818526
339.242913	7999.928209	13.940275	-0.067820	4.818489
339.033297	7999.936986	13.945280	-0.067781	4.818492
339.105310	8000.036585	13.950285	-0.067795	4.818522
339.434254	8000.045106	13.955290	-0.067856	4.818523
338.980643	8000.011835	13.960295	-0.067771	4.818515
339.015105	8000.009132	13.965299	-0.067777	4.818514
339.114515	7999.915971	13.970304	-0.067796	4.818486
339.131671	8000.074673	13.975309	-0.067799	4.818533
339.255835	7999.952450	13.980314	-0.067822	4.818496
339.154079	8000.110636	13.985319	-0.067803	4.818543
339.306011	8000.079042	13.990323	-0.067831	4.818533
339.315545	8000.087556	13.995328	-0.067833	4.818536
339.375505	8000.097783	14.000333	-0.067844	4.818539
339.524478	8000.080844	14.005338	-0.067871	4.818533
339.304431	7999.903708	14.010343	-0.067830	4.818481
339.444819	8000.018902	14.015347	-0.067856	4.818515
339.403452	7999.914441	14.020352	-0.067848	4.818484
339.213468	8000.070416	14.025357	-0.067813	4.818531
339.203989	7999.994713	14.030362	-0.067811	4.818509
339.221132	7999.955047	14.035367	-0.067814	4.818497
339.480278	8000.114837	14.040371	-0.067862	4.818543
339.412960	8000.149628	14.045376	-0.067850	4.818554
339.316809	8000.188237	14.050381	-0.067832	4.818566
339.272744	8000.016567	14.055386	-0.067823	4.818515
339.260371	7999.936628	14.060391	-0.067821	4.818491
339.454391	8000.140693	14.065395	-0.067857	4.818551
339.473384	7999.954109	14.070400	-0.067860	4.818496
339.353407	8000.071123	14.075405	-0.067838	4.818531
339.383165	7999.840600	14.080410	-0.067843	4.818462
339.461712	8000.101920	14.085415	-0.067858	4.818540
339.478345	7999.931049	14.090419	-0.067861	4.818489
339.659005	8000.097154	14.095424	-0.067894	4.818537
339.263279	8000.239925	14.100429	-0.067820	4.818581
339.387120	7999.925624	14.105434	-0.067843	4.818487
339.717350	8000.143029	14.110439	-0.067905	4.818551
339.616317	8000.304377	14.115443	-0.067886	4.818599
339.624382	7999.946565	14.120448	-0.067887	4.818493
339.515710	8000.104661	14.125453	-0.067867	4.818540
339.706155	7999.900394	14.130458	-0.067902	4.818479
339.681021	8000.158251	14.135463	-0.067897	4.818556
339.637851	8000.060062	14.140467	-0.067889	4.818526
339.613369	8000.063930	14.145472	-0.067884	4.818528
339.433328	8000.148665	14.150477	-0.067851	4.818554
339.457228	8000.192004	14.155482	-0.067855	4.818566
339.295810	8000.120597	14.160487	-0.067825	4.818546
339.333134	7999.996180	14.165491	-0.067832	4.818509
339.612425	8000.141543	14.170496	-0.067884	4.818551
339.566113	8000.297314	14.175501	-0.067875	4.818597
339.480779	8000.060024	14.180506	-0.067859	4.818527
339.462135	8000.334761	14.185511	-0.067855	4.818609
339.483206	8000.041146	14.190515	-0.067859	4.818522
339.369069	7999.904239	14.195520	-0.067838	4.818481
339.352621	8000.105532	14.200525	-0.067835	4.818541
339.622311	7999.932746	14.205530	-0.067885	4.818489
339.423886	7999.895489	14.210535	-0.067847	4.818478
339.122857	8000.078340	14.215539	-0.067791	4.818534
339.242704	7999.917226	14.220544	-0.067813	4.818486
338.979490	7999.947339	14.225549	-0.067764	4.818496
339.176627	7999.807185	14.230554	-0.067801	4.818453
339.025001	7999.932177	14.235559	-0.067773	4.818491
339.077016	7999.891920	14.240563	-0.067782	4.818479
339.270011	7999.932237	14.245568	-0.067818	4.818490
339.310301	8000.232937	14.250573	-0.067826	4.818579
339.589561	8000.072872	14.255578	-0.067877	4.818531
339.354922	8000.127500	14.260583	-0.067834	4.818548
339.310308	8000.090168	14.265587	-0.067825	4.818537
339.231964	8000.018807	14.270592	-0.067810	4.818516
339.439658	8000.103400	14.275597	-0.067849	4.818540
339.320180	7999.890854	14.280602	-0.067826	4.818477
339.215974	8000.075247	14.285607	-0.067807	4.818533
339.335973	8000.065273	14.290611	-0.067829	4.818529
339.409235	8000.099816	14.295616	-0.067843	4.818539
339.423095	8000.212295	14.300621	-0.067845	4.818573
339.542252	8000.031229	14.305626	-0.067867	4.818518
339.715794	8000.030357	14.310631	-0.067899	4.818517
339.507537	7999.987722	14.315635	-0.067860	4.818506
339.510779	7999.803032	14.320640	-0.067861	4.818451
339.457998	7999.935623	14.325645	-0.067851	4.818490
339.514246	7999.951049	14.330650	-0.067861	4.818495
339.489443	7999.942317	14.335655	-0.067857	4.818492
339.541597	7999.914657	14.340659	-0.067866	4.818484
339.348737	7999.934150	14.345664	-0.067830	4.818490
339.403346	8000.006231	14.350669	-0.067840	4.818512
339.586552	7999.968751	14.355674	-0.067874	4.818500
339.631204	8000.123619	14.360679	-0.067883	4.818546
339.563897	7999.997824	14.365683	-0.067870	4.818508
339.574817	8000.081925	14.370688	-0.067872	4.818533
339.430943	8000.177633	14.375693	-0.067845	4.818562
339.707848	8000.054272	14.380698	-0.067896	4.818525
339.774392	8000.249314	14.385703	-0.067909	4.818582
339.665690	8000.071542	14.390707	-0.067888	4.818530
339.732818	8000.099707	14.395712	-0.067901	4.818538
339.520470	8000.267984	14.400717	-0.067861	4.818589
339.467939	7999.879988	14.405722	-0.067851	4.818474
339.614378	8000.040394	14.410727	-0.067878	4.818521
339.600962	7999.959391	14.415731	-0.067875	4.818497
339.530084	7999.933259	14.420736	-0.067862	4.818489
339.299032	7999.958547	14.425741	-0.067819	4.818498
339.505959	7999.528845	14.430746	-0.067857	4.818369

339.485573	7996.386538	14.435751	-0.067851	4.817434
339.344609	7990.770663	14.440755	-0.067821	4.815764
339.601202	7984.039894	14.445760	-0.067864	4.813759
339.238820	7976.856513	14.450765	-0.067792	4.811621
339.346981	7969.187847	14.455770	-0.067807	4.809336
339.475354	7961.418335	14.460775	-0.067826	4.807019
339.407457	7953.467019	14.465779	-0.067808	4.804648
339.323272	7945.595829	14.470784	-0.067787	4.802300
339.369527	7937.523040	14.475789	-0.067790	4.799890
339.239820	7929.603802	14.480794	-0.067761	4.797525
339.187611	7921.578688	14.485799	-0.067746	4.795127
339.289692	7913.566633	14.490803	-0.067759	4.792731
339.307229	7905.629630	14.495808	-0.067757	4.790357
339.158371	7897.538352	14.500813	-0.067724	4.787936
338.981559	7889.559345	14.505818	-0.067686	4.785547
339.132625	7881.563812	14.510823	-0.067709	4.783151
339.022643	7873.570640	14.515827	-0.067683	4.780756
338.995842	7865.554249	14.520832	-0.067673	4.778352
338.873517	7857.591955	14.525837	-0.067644	4.775963
339.019879	7849.540604	14.530842	-0.067666	4.773546
338.937254	7841.530637	14.535847	-0.067646	4.771140
339.000505	7833.497000	14.540851	-0.067652	4.768726
338.986131	7825.582996	14.545856	-0.067644	4.766347
338.954398	7817.471504	14.550861	-0.067633	4.763907
339.028043	7809.641999	14.555866	-0.067641	4.761550
338.913319	7801.558735	14.560871	-0.067615	4.759117
338.933151	7793.580220	14.565875	-0.067613	4.756713
338.829303	7785.563332	14.570880	-0.067588	4.754297
338.869616	7777.511323	14.575885	-0.067590	4.751869
338.965814	7769.525917	14.580890	-0.067603	4.749459
338.463269	7761.489446	14.585895	-0.067504	4.747034
338.452549	7753.429821	14.590899	-0.067497	4.744600
338.788466	7745.532738	14.595904	-0.067554	4.742213
338.882666	7737.519144	14.600909	-0.067566	4.739790
338.822010	7729.519945	14.605914	-0.067549	4.737370
338.596059	7721.501114	14.610919	-0.067502	4.734944
338.631705	7713.532443	14.615923	-0.067503	4.732531
338.588557	7705.508631	14.620928	-0.067490	4.730100
338.565471	7697.448928	14.625933	-0.067480	4.727657
338.729159	7689.485032	14.630938	-0.067505	4.725242
338.647021	7681.545414	14.635943	-0.067485	4.722833
338.447431	7673.577398	14.640947	-0.067442	4.720414
338.595253	7665.557766	14.645952	-0.067465	4.717978
338.222092	7657.524282	14.650957	-0.067390	4.715537
338.089707	7649.561936	14.655962	-0.067360	4.713116
338.190560	7641.586318	14.660967	-0.067373	4.710690
338.332462	7633.544199	14.665971	-0.067394	4.708242
338.449221	7625.477416	14.670976	-0.067411	4.705785
338.332345	7617.470238	14.675981	-0.067384	4.703346
338.446845	7609.532631	14.680986	-0.067400	4.700926
338.385247	7601.532963	14.685991	-0.067383	4.698486
338.223730	7593.555560	14.690995	-0.067347	4.696052
338.268341	7585.503273	14.696000	-0.067350	4.693593
338.187110	7577.514088	14.701005	-0.067330	4.691153
338.303678	7569.479605	14.706010	-0.067346	4.688697
337.910588	7561.533730	14.711015	-0.067268	4.686268
337.759479	7553.486615	14.716019	-0.067234	4.683806
338.030507	7545.610902	14.721024	-0.067279	4.681394
338.198663	7537.433231	14.726029	-0.067305	4.678890
338.319907	7529.552114	14.731034	-0.067323	4.676474
338.213050	7521.489394	14.736039	-0.067297	4.674002
338.023838	7513.482766	14.741043	-0.067257	4.671546
338.125202	7505.420779	14.746048	-0.067270	4.669072
337.846541	7497.476490	14.751053	-0.067213	4.666632
337.996501	7489.430154	14.756058	-0.067236	4.664160
337.703200	7481.521782	14.761063	-0.067176	4.661729
337.771035	7473.436167	14.766067	-0.067183	4.659242
337.767957	7465.528267	14.771072	-0.067177	4.656808
337.602216	7457.417715	14.776077	-0.067141	4.654311
337.818559	7449.484772	14.781082	-0.067176	4.651867
337.922710	7441.427362	14.786087	-0.067190	4.649384
337.690632	7433.489786	14.791091	-0.067141	4.646936
337.740502	7425.431864	14.796096	-0.067145	4.644449
337.694943	7417.490554	14.801101	-0.067132	4.641998
337.583386	7409.438351	14.806106	-0.067105	4.639510
337.475412	7401.492513	14.811111	-0.067080	4.637054
337.528313	7393.414426	14.816115	-0.067084	4.634557
337.336725	7385.495451	14.821120	-0.067043	4.632106
336.818374	7377.439206	14.826125	-0.066942	4.629612
337.127545	7369.429103	14.831130	-0.066994	4.627131
337.296447	7361.390271	14.836135	-0.067020	4.624640
337.284990	7353.443740	14.841139	-0.067012	4.622177
337.295716	7345.484296	14.846144	-0.067009	4.619707
337.254940	7337.463898	14.851149	-0.066996	4.617218
337.324647	7329.367110	14.856154	-0.067004	4.614703
337.193447	7321.418008	14.861159	-0.066974	4.612233
336.831000	7313.414792	14.866163	-0.066901	4.609745
337.158346	7305.421554	14.871168	-0.066957	4.607259
337.099017	7297.394888	14.876173	-0.066940	4.604760
337.326122	7289.448630	14.881178	-0.066977	4.602286
337.205556	7281.402853	14.886183	-0.066950	4.599779
337.053158	7273.424734	14.891187	-0.066916	4.597292
337.308008	7265.418100	14.896192	-0.066958	4.594795
337.014618	7257.385362	14.901197	-0.066898	4.592288
337.071586	7249.425349	14.906202	-0.066903	4.589802
337.066913	7241.382041	14.911207	-0.066897	4.587289
336.659181	7233.405235	14.916211	-0.066816	4.584795
336.945974	7225.478951	14.921216	-0.066864	4.582317
336.891815	7217.337405	14.926221	-0.066848	4.579769
336.911449	7209.385388	14.931226	-0.066847	4.577279
336.839628	7201.357564	14.936231	-0.066828	4.574764
336.832467	7193.373609	14.941235	-0.066821	4.572261
336.984804	7185.359154	14.946240	-0.066844	4.569748
336.997462	7177.371883	14.951245	-0.066841	4.567242
336.805867	7169.357613	14.956250	-0.066800	4.564725
336.687123	7161.419855	14.961255	-0.066773	4.562231
336.865459	7153.350260	14.966259	-0.066801	4.559695
336.653335	7145.415064	14.971264	-0.066756	4.557199
336.730143	7137.295601	14.976269	-0.066765	4.554645
336.736385	7129.382471	14.981274	-0.066761	4.552153
336.949799	7121.290684	14.986279	-0.066795	4.549605
336.687706	7113.328113	14.991283	-0.066741	4.547094
336.701714	7105.314262	14.996288	-0.066738	4.544567
336.727776	7097.381920	15.001293	-0.066738	4.542064
336.792086	7089.315205	15.006298	-0.066745	4.539517
336.561085	7081.354485	15.011303	-0.066696	4.537002
336.645303	7073.303521	15.016307	-0.066707	4.534458
336.661353	7065.342571	15.021312	-0.066704	4.531940
336.538569	7057.264092	15.026317	-0.066676	4.529383
336.446500	7049.347659	15.031322	-0.066654	4.526877
336.661154	7041.215816	15.036327	-0.066688	4.524301
336.782989	7033.330730	15.041331	-0.066705	4.521803
336.610760	7025.344773	15.046336	-0.066668	4.519269
336.562992	7017.361064	15.051341	-0.066654	4.516736
336.647057	7009.316537	15.056346	-0.066664	4.514182
336.328357	7001.336976	15.061351	-0.066599	4.511646
336.452468	6993.257897	15.066355	-0.066617	4.509079
336.353502	6985.313502	15.071360	-0.066593	4.506552
336.277138	6977.236033	15.076365	-0.066574	4.503981
336.103458	6969.365315	15.081370	-0.066536	4.501474
336.015530	6961.268778	15.086375	-0.066515	4.498895
336.021506	6953.259011	15.091379	-0.066510	4.496341
335.958228	6945.260529	15.096384	-0.066493	4.493790
335.905670	6937.252795	15.101389	-0.066478	4.491234
336.190858	6929.268799	15.106394	-0.066526	4.488686
336.025581	6921.250128	15.111399	-0.066490	4.486124
335.992637	6913.222658	15.116403	-0.066478	4.483557
336.225194	6905.297746	15.121408	-0.066516	4.481024
335.898223	6897.256073	15.126413	-0.066450	4.478449
335.896491	6889.255635	15.131418	-0.066444	4.475887
335.910859	6881.236184	15.136423	-0.066442	4.473317
335.910999	6873.240042	15.141427	-0.066436	4.470754
335.707688	6865.249460	15.146432	-0.066393	4.468190
335.815334	6857.196807	15.151437	-0.066408	4.465606
336.012823	6849.238817	15.156442	-0.066439	4.463051
335.792455	6841.248798	15.161447	-0.066393	4.460482
335.608373	6833.251281	15.166451	-0.066353	4.457910
335.646614	6825.237601	15.171456	-0.066355	4.455332
335.488679	6817.217043	15.176461	-0.066320	4.452750
335.750326	6809.229523	15.181466	-0.066364	4.450179
335.660386	6801.221107	15.186471	-0.066342	4.447597
335.667313	6793.134524	15.191475	-0.066338	4.444990
335.336881	6785.288405	15.196480	-0.066271	4.442457
335.116375	6777.225629	15.201485	-0.066224	4.439853
335.266060	6769.250413	15.206490	-0.066247	4.437277
335.273808	6761.183667	15.211495	-0.066243	4.434670
335.275523	6753.216353	15.216499	-0.066238	4.432093
335.237601	6745.196490	15.221504	-0.066226	4.429498
335.298778	6737.194085	15.226509	-0.066232	4.426907
335.278859	6729.142862	15.231514	-0.066223	4.424299
335.236094	6721.189242	15.236519	-0.066209	4.421721
334.971624	6713.179803	15.241523	-0.066155	4.419121
335.246790	6705.222118	15.246528	-0.066201	4.416540
335.132201	6697.137742	15.251533	-0.066174	4.413914
335.354974	6689.223908	15.256538	-0.066210	4.411344
335.313935	6681.181314	15.261543	-0.066197	4.408729
334.995907	6673.204416	15.266547	-0.066133	4.406132
335.141040	6665.144857	15.271552	-0.066154	4.403510
335.076033	6657.198570	15.276557	-0.066137	4.400921
335.062543	6649.241619	15.281562	-0.066129	4.398328
334.975358	6641.209471	15.286567	-0.066107	4.395709
334.826105	6633.231219	15.291571	-0.066074	4.393105
334.939571	6625.274468	15.296576	-0.066090	4.390508
334.736226	6617.226592	15.301581	-0.066047	4.387877
334.987948	6609.207717	15.306586	-0.066088	4.385258
334.821144	6601.266145	15.311591	-0.066052	4.382660
334.684970	6593.248603	15.316595	-0.066021	4.380035
334.710602	6585.282082	15.321600	-0.066021	4.377427
334.857981	6577.179591	15.326605	-0.066043	4.374773
334.830488	6569.271363	15.331610	-0.066032	4.372180
334.770122	6561.263899	15.336615	-0.066016	4.369553
334.838184	6553.248016	15.341619	-0.066023	4.366922
334.805919	6545.288572	15.346624	-0.066012	4.364308
334.603535	6537.317759	15.351629	-0.065969	4.361687
334.890405	6529.309525	15.356634	-0.066017	4.359056
334.715249	6521.343986	15.361639	-0.065979	4.356434
334.641125	6513.233127	15.366643	-0.065960	4.353763
334.504245	6505.222523	15.371648	-0.065929	4.351123
334.354732	6497.236073	15.376653	-0.065896	4.348489
334.137115	6489.275997	15.381658	-0.065850	4.345862
334.047372	6481.256341	15.386663	-0.065828	4.343214
333.942014	6473.281685	15.391667	-0.065803	4.340580
334.187255	6465.273283	15.396672	-0.065843	4.337936
334.273264	6457.234825	15.401677	-0.065854	4.335279
334.280949	6449.283364	15.406682	-0.065850	4.332648
334.245258	6441.247295	15.411687	-0.065838	4.329987
334.177516	6433.221693	15.416691	-0.065820	4.327328
334.265367	6425.225424	15.421696	-0.065831	4.324679
334.004104	6417.303038	15.426701	-0.065777	4.322049
334.175073	6409.242023	15.431706	-0.065804	4.319375
334.006562	6401.309277	15.436711	-0.065767	4.316740
333.851974	6393.230802	15.441715	-0.065733	4.314054
333.866734	6385.278827	15.446720	-0.065730	4.311411
333.875902	6377.210856	15.451725	-0.065727	4.308727
333.944932	6369.232597	15.456730	-0.065734	4.306071
334.009715	6361.188141	15.461735	-0.065741	4.303392
333.769001	6353.255158	15.466739	-0.065691	4.300746
333.778682	6345.250239	15.471744	-0.065687	4.298076
333.845983	6337.182335	15.476749	-0.065694	4.295385
333.860835	6329.226517	15.481754	-0.065692	4.292728
333.574937	6321.164330	15.486759	-0.065633	4.290032
333.919165	6313.220583	15.491763	-0.065692	4.287379
333.883803	6305.210105	15.496768	-0.065680	4.284699
333.757917	6297.262209	15.501773	-0.065651	4.282037
333.685839	6289.255367	15.506778	-0.065633	4.279354
333.643739	6281.238763	15.511783	-0.065619	4.276667
333.858951	6273.194729	15.516787	-0.065654	4.273971
333.764340	6265.218563	15.521792	-0.065631	4.271293
333.680644	6257.140249	15.526797	-0.065610	4.268579
333.856091	6249.192358	15.531802	-0.065637	4.265910
333.712846	6241.211415	15.536807	-0.065605	4.263226
333.516084	6233.236222	15.541811	-0.065564	4.260540
333.309596	6225.270144	15.546816	-0.065520	4.257856
333.190413	6217.211137	15.551821	-0.065492	4.255140
332.989942	6209.255149	15.556826	-0.065450	4.252456
333.293056	6201.141855	15.561831	-0.065501	4.249723
333.376954	6193.144857	15.566835	-0.065511	4.247024
333.036332	6185.193702	15.571840	-0.065442	4.244335
333.099715	6177.204746	15.576845	-0.065449	4.241636
333.328961	6169.163083	15.581850	-0.065486	4.238919
333.410967	6161.182758	15.586855	-0.065496	4.236219
333.265389	6153.179648	15.591859	-0.065463	4.233508
333.627289	6145.172073	15.596864	-0.065526	4.230799
333.347304	6137.164211	15.601869	-0.065468	4.228081
333.416728	6129.141195	15.606874	-0.065476	4.225359
333.347950	6121.224326	15.611879	-0.065458	4.222671
333.448152	6113.187601	15.616883	-0.065471	4.219942
333.510341	6105.217884	15.621888	-0.065477	4.217234
333.381656	6097.126501	15.626893	-0.065448	4.214480
333.509476	6089.170440	15.631898	-0.065466	4.211774
333.556064	6081.122268	15.636903	-0.065470	4.209033
333.343611	6073.184157	15.641907	-0.065425	4.206325
333.496245	6065.189537	15.646912	-0.065448	4.203601
333.279567	6057.230846	15.651917	-0.065402	4.200883
333.217666	6049.205408	15.656922	-0.065385	4.198141
333.230233	6041.199135	15.661927	-0.065382	4.195406
333.143185	6033.120279	15.666931	-0.065361	4.192643
332.955292	6025.148805	15.671936	-0.065320	4.189913
332.958004	6017.121273	15.676941	-0.065315	4.187165
333.088616	6009.093627	15.681946	-0.065334	4.184416
332.858964	6001.211357	15.686951	-0.065286	4.181711
332.885930	5993.140508	15.691955	-0.065286	4.178943
332.850199	5985.228165	15.696960	-0.065274	4.176227
332.747449	5977.107143	15.701965	-0.065250	4.173436
332.964933	5969.139882	15.706970	-0.065285	4.170700
332.354157	5961.187784	15.711975	-0.065166	4.167957
332.587163	5953.149718	15.716979	-0.065204	4.165194
332.477542	5945.262644	15.721984	-0.065178	4.162476
332.621301	5937.124227	15.726989	-0.065199	4.159673
332.808451	5929.215888	15.731994	-0.065229	4.156948
332.477813	5921.211621	15.736999	-0.065162	4.154182
331.939560	5913.287467	15.742003	-0.065057	4.151438
332.286078	5905.191047	15.747008	-0.065116	4.148645
332.424590	5897.152021	15.752013	-0.065136	4.145867
332.540716	5889.168792	15.757018	-0.065152	4.143106
332.577585	5881.202880	15.762023	-0.065154	4.140349
332.452613	5873.210638	15.767027	-0.065125	4.137578
332.619682	5865.186456	15.772032	-0.065151	4.134798
332.485300	5857.188273	15.777037	-0.065121	4.132021
332.512412	5849.173066	15.782042	-0.065120	4.129239
332.420297	5841.202056	15.787047	-0.065098	4.126469
332.147176	5833.187000	15.792051	-0.065042	4.123679
332.525998	5825.239666	15.797056	-0.065107	4.120919
332.618441	5817.181563	15.802061	-0.065119	4.118115
332.550399	5809.226699	15.807066	-0.065101	4.115343
332.275384	5801.236281	15.812071	-0.065044	4.112554
332.142864	5793.222407	15.817075	-0.065014	4.109757
332.165517	5785.208668	15.822080	-0.065013	4.106960
332.084255	5777.176020	15.827085	-0.064993	4.104153
332.376713	5769.225610	15.832090	-0.065042	4.101378
332.219684	5761.200763	15.837095	-0.065007	4.098569
331.966228	5753.203300	15.842099	-0.064955	4.095766
332.038113	5745.210422	15.847104	-0.064963	4.092967
331.970515	5737.158450	15.852109	-0.064945	4.090144
331.985358	5729.168244	15.857114	-0.064942	4.087342
332.162081	5721.125146	15.862119	-0.064970	4.084521
332.075739	5713.196381	15.867123	-0.064948	4.081735
332.130390	5705.202275	15.872128	-0.064953	4.078926
332.146998	5697.209069	15.877133	-0.064951	4.076115
332.280749	5689.212820	15.882138	-0.064971	4.073303
332.281941	5681.178118	15.887143	-0.064966	4.070473
332.085358	5673.196509	15.892147	-0.064924	4.067657
331.986061	5665.196832	15.897152	-0.064900	4.064834
332.044410	5657.209159	15.902157	-0.064905	4.062016
331.921103	5649.212867	15.907162	-0.064877	4.059190
331.791776	5641.237480	15.912167	-0.064848	4.056369
331.767112	5633.202195	15.917171	-0.064838	4.053527
331.704868	5625.229783	15.922176	-0.064821	4.050704
331.368651	5617.194972	15.927181	-0.064753	4.047853
331.344735	5609.215405	15.932186	-0.064743	4.045025
331.576808	5601.219383	15.937191	-0.064781	4.042192
331.526181	5593.191503	15.942195	-0.064766	4.039342
331.498891	5585.270191	15.947200	-0.064756	4.036528
331.390693	5577.208827	15.952205	-0.064730	4.033662
331.162888	5569.195564	15.957210	-0.064682	4.030808
331.091529	5561.185287	15.962215	-0.064664	4.027955
330.876515	5553.177701	15.967219	-0.064618	4.025100
331.199470	5545.234187	15.972224	-0.064673	4.022274
330.960926	5537.175219	15.977229	-0.064624	4.019395
330.831363	5529.267434	15.982234	-0.064594	4.016570
331.081952	5521.198060	15.987239	-0.064635	4.013692
330.823464	5513.223804	15.992243	-0.064582	4.010838
330.897786	5505.230897	15.997248	-0.064590	4.007980
330.819442	5497.232598	16.002253	-0.064571	4.005115
331.047125	5489.270794	16.007258	-0.064608	4.002267
331.057015	5481.190909	16.012263	-0.064604	3.999371
331.019530	5473.270529	16.017267	-0.064592	3.996529
331.274132	5465.237406	16.022272	-0.064634	3.993649
331.221072	5457.238765	16.027277	-0.064619	3.990775
331.008652	5449.253658	16.032282	-0.064574	3.987900
331.187852	5441.236219	16.037287	-0.064602	3.985019
330.941960	5433.300805	16.042291	-0.064551	3.982158
330.917323	5425.250318	16.047296	-0.064541	3.979257
330.996922	5417.268956	16.052301	-0.064550	3.976381
331.045213	5409.250782	16.057306	-0.064554	3.973488
330.771924	5401.276037	16.062311	-0.064498	3.970604
330.850157	5393.228334	16.067315	-0.064507	3.967697
330.679778	5385.260242	16.072320	-0.064470	3.964813
330.361367	5377.310653	16.077325	-0.064405	3.961930
330.281291	5369.328235	16.082330	-0.064385	3.959038
330.162159	5361.344199	16.087335	-0.064357	3.956143
330.254352	5353.275280	16.092339	-0.064369	3.953218
330.466351	5345.228535	16.097344	-0.064403	3.950301
330.614174	5337.186646	16.102349	-0.064426	3.947383
330.273036	5329.270272	16.107354	-0.064357	3.944499
330.306125	5321.283871	16.112359	-0.064358	3.941595
330.348287	5313.235148	16.117363	-0.064360	3.938666
330.382265	5305.271646	16.122368	-0.064361	3.935766
330.272311	5297.247906	16.127373	-0.064335	3.932838
330.323439	5289.249973	16.132378	-0.064339	3.929921
330.378775	5281.269710	16.137383	-0.064344	3.927009
330.375028	5273.230993	16.142387	-0.064338	3.924072
330.327785	5265.321812	16.147392	-0.064324	3.921179
330.220656	5257.276691	16.152397	-0.064299	3.918233
330.399960	5249.297368	16.157402	-0.064327	3.915315
330.008639	5241.332378	16.162407	-0.064249	3.912388
330.042106	5233.268121	16.167411	-0.064250	3.909431
330.196690	5225.300354	16.172416	-0.064273	3.906510
330.056410	5217.280546	16.177421	-0.064242	3.903561
330.094679	5209.333566	16.182426	-0.064244	3.900641
329.878256	5201.347043	16.187431	-0.064198	3.897699
330.085766	5193.302735	16.192435	-0.064231	3.894742
329.662077	5185.401653	16.197440	-0.064147	3.891822
329.667917	5177.318778	16.202445	-0.064143	3.888842
329.753610	5169.362864	16.207450	-0.064153	3.885909
329.654527	5161.339520	16.212455	-0.064130	3.882944
329.654734	5153.338776	16.217459	-0.064124	3.879987
330.076342	5145.338286	16.222464	-0.064197	3.877038
329.635711	5137.389581	16.227469	-0.064110	3.874087
329.781512	5129.206819	16.232474	-0.064132	3.871059
329.912301	5121.233315	16.237479	-0.064151	3.868106
329.636214	5113.264530	16.242483	-0.064094	3.865144
329.609825	5105.370152	16.247488	-0.064084	3.862213
329.625034	5097.275289	16.252493	-0.064081	3.859206
329.435911	5089.385617	16.257498	-0.064041	3.856268
329.386287	5081.332994	16.262503	-0.064026	3.853271
329.493036	5073.319548	16.267507	-0.064041	3.850289
329.545657	5065.366484	16.272512	-0.064045	3.847326
328.928726	5057.338757	16.277517	-0.063925	3.844319
329.232438	5049.354242	16.282522	-0.063976	3.841345
329.074198	5041.345981	16.287527	-0.063941	3.838350
329.264827	5033.326922	16.292531	-0.063972	3.835357
329.226367	5025.385920	16.297536	-0.063959	3.832385
329.206752	5017.329966	16.302541	-0.063950	3.829368
329.456749	5009.325203	16.307546	-0.063991	3.826374
329.117590	5001.367439	16.312551	-0.063923	3.823382
328.999223	4993.367139	16.317555	-0.063896	3.820377
329.124727	4985.391840	16.322560	-0.063914	3.817384
329.139026	4977.339758	16.327565	-0.063911	3.814358
328.994490	4969.413130	16.332570	-0.063879	3.811372
328.925215	4961.361415	16.337575	-0.063860	3.808339
328.951647	4953.360875	16.342579	-0.063860	3.805325
329.032078	4945.426284	16.347584	-0.063870	3.802335
328.942809	4937.383386	16.352589	-0.063848	3.799298
328.906504	4929.455272	16.357594	-0.063836	3.796303
328.804102	4921.377325	16.362599	-0.063811	3.793247
328.814670	4913.380655	16.367603	-0.063808	3.790222
328.784888	4905.422536	16.372608	-0.063797	3.787208
328.686692	4897.362996	16.377613	-0.063773	3.784152
328.690585	4889.432055	16.382618	-0.063769	3.781145
328.724627	4881.405228	16.387623	-0.063770	3.778099
328.406312	4873.450442	16.392627	-0.063705	3.775070
328.534581	4865.441340	16.397632	-0.063724	3.772029
327.842845	4857.491054	16.402637	-0.063590	3.768987
328.482885	4849.440506	16.407642	-0.063703	3.765938
328.533023	4841.426174	16.412647	-0.063707	3.762885
328.560142	4833.431247	16.417651	-0.063707	3.759837
328.634930	4825.484735	16.422656	-0.063716	3.756805
328.374292	4817.443487	16.427661	-0.063662	3.753727
328.355632	4809.526511	16.432666	-0.063653	3.750700
328.280478	4801.477649	16.437671	-0.063634	3.747619
328.149145	4793.469222	16.442675	-0.063604	3.744549
328.513061	4785.476938	16.447680	-0.063666	3.741495
328.349197	4777.481312	16.452685	-0.063630	3.738424
328.527612	4769.486334	16.457690	-0.063658	3.735360
328.329815	4761.522385	16.462695	-0.063616	3.732295
328.142261	4753.461323	16.467699	-0.063576	3.729191
328.424092	4745.500339	16.472704	-0.063623	3.726135
328.275331	4737.501181	16.477709	-0.063590	3.723050
328.335090	4729.529774	16.482714	-0.063596	3.719979
328.074296	4721.555409	16.487719	-0.063542	3.716896
328.199473	4713.478907	16.492723	-0.063560	3.713781
328.107950	4705.473631	16.497728	-0.063538	3.710685
327.761688	4697.464659	16.502733	-0.063468	3.707579
328.075346	4689.444968	16.507738	-0.063521	3.704483
327.957785	4681.521230	16.512743	-0.063494	3.701410
327.785352	4673.533776	16.517747	-0.063456	3.698308
327.836524	4665.560517	16.522752	-0.063460	3.695216
328.034887	4657.510021	16.527757	-0.063492	3.692094
327.940231	4649.494187	16.532762	-0.063469	3.688976
327.939411	4641.532531	16.537767	-0.063464	3.685879
327.927467	4633.538259	16.542771	-0.063456	3.682766
327.980770	4625.562304	16.547776	-0.063461	3.679659
327.858251	4617.573143	16.552781	-0.063432	3.676540
328.085471	4609.578716	16.557786	-0.063469	3.673425
327.885554	4601.591732	16.562791	-0.063427	3.670300
328.051906	4593.532796	16.567795	-0.063452	3.667153
327.999262	4585.579654	16.572800	-0.063437	3.664039
327.834781	4577.610818	16.577805	-0.063401	3.660913
327.800251	4569.609539	16.582810	-0.063390	3.657776
327.732058	4561.607961	16.587815	-0.063372	3.654634
327.617611	4553.625290	16.592819	-0.063345	3.651497
327.726724	4545.625055	16.597824	-0.063360	3.648355
327.804342	4537.573601	16.602829	-0.063369	3.645190
327.802246	4529.647311	16.607834	-0.063363	3.642069
327.470369	4521.682346	16.612839	-0.063296	3.638921
327.606831	4513.675247	16.617843	-0.063316	3.635767
327.610325	4505.671098	16.622848	-0.063312	3.632608
327.638867	4497.636579	16.627853	-0.063312	3.629434
327.698077	4489.642391	16.632858	-0.063317	3.626275
327.414477	4481.671947	16.637863	-0.063259	3.623112
327.432457	4473.660827	16.642867	-0.063257	3.619939
327.523176	4465.683735	16.647872	-0.063269	3.616779
327.390590	4457.659009	16.652877	-0.063239	3.613591
327.217703	4449.711150	16.657882	-0.063201	3.610429
327.090207	4441.714428	16.662887	-0.063172	3.607247
326.981898	4433.692050	16.667891	-0.063147	3.604052
326.996361	4425.772843	16.672896	-0.063144	3.600899
326.682459	4417.717172	16.677901	-0.063080	3.597679
326.857837	4409.714134	16.682906	-0.063107	3.594491
326.770715	4401.753941	16.687911	-0.063086	3.591310
326.904076	4393.697048	16.692915	-0.063105	3.588094
326.897788	4385.695930	16.697920	-0.063099	3.584893
326.793988	4377.717806	16.702925	-0.063074	3.581696
326.625797	4369.753227	16.707930	-0.063038	3.578499
326.855614	4361.735692	16.712935	-0.063075	3.575291
326.874818	4353.734075	16.717939	-0.063073	3.572079
326.796980	4345.733755	16.722944	-0.063053	3.568862
326.405787	4337.829521	16.727949	-0.062975	3.565671
326.836877	4329.769537	16.732954	-0.063050	3.562440
326.770238	4321.795488	16.737959	-0.063033	3.559225
326.354639	4313.880758	16.742963	-0.062950	3.556021
326.695755	4305.763346	16.747968	-0.063008	3.552755
326.747246	4297.714011	16.752973	-0.063012	3.549505
326.778020	4289.737671	16.757978	-0.063013	3.546280
326.847957	4281.740125	16.762983	-0.063020	3.543046
327.035866	4273.734606	16.767987	-0.063050	3.539808
326.975661	4265.838609	16.772992	-0.063033	3.536605
326.870449	4257.807189	16.777997	-0.063009	3.533342
326.819218	4249.809780	16.783002	-0.062994	3.530092
326.624759	4241.857771	16.788007	-0.062952	3.526852
326.625488	4233.812826	16.793011	-0.062947	3.523578
326.629273	4225.875481	16.798016	-0.062942	3.520345
326.455676	4217.891216	16.803021	-0.062905	3.517084
326.441620	4209.871320	16.808026	-0.062897	3.513811
326.457584	4201.912313	16.813031	-0.062894	3.510560
326.357444	4193.876729	16.818035	-0.062870	3.507272
326.276762	4185.857869	16.823040	-0.062850	3.503987
326.349492	4177.893055	16.828045	-0.062858	3.500727
326.550591	4169.876714	16.833050	-0.062890	3.497447
326.478209	4161.866800	16.838055	-0.062872	3.494157
326.325729	4153.927085	16.843059	-0.062838	3.490890
326.576231	4145.867723	16.848064	-0.062879	3.487585
326.518805	4137.858820	16.853069	-0.062863	3.484287
326.398645	4129.981509	16.858074	-0.062835	3.481038
326.222381	4121.988243	16.863079	-0.062797	3.477736
326.417321	4113.965068	16.868083	-0.062828	3.474431
326.445861	4105.983328	16.873088	-0.062828	3.471134
326.160146	4097.966035	16.878093	-0.062770	3.467809
326.147609	4089.961452	16.883098	-0.062762	3.464496
326.247587	4082.011086	16.888103	-0.062775	3.461205
326.002422	4074.009959	16.893107	-0.062724	3.457879
325.962398	4066.051688	16.898112	-0.062712	3.454574
325.927945	4058.028502	16.903117	-0.062700	3.451239
325.966281	4050.017595	16.908122	-0.062702	3.447908
326.125921	4041.990151	16.913127	-0.062726	3.444572
326.246583	4034.020820	16.918131	-0.062743	3.441255
326.075539	4026.085582	16.923136	-0.062706	3.437939
325.780644	4018.093653	16.928141	-0.062646	3.434592
325.549093	4010.132747	16.933146	-0.062597	3.431257
325.538030	4002.081450	16.938151	-0.062590	3.427888
325.355239	3994.081529	16.943155	-0.062550	3.424532
325.230414	3986.189640	16.948160	-0.062522	3.421219
324.969720	3978.149559	16.953165	-0.062468	3.417836
325.013216	3970.116417	16.958170	-0.062471	3.414464
325.125699	3962.118763	16.963175	-0.062486	3.411106
325.609698	3954.047024	16.968179	-0.062571	3.407726
325.557361	3946.103453	16.973184	-0.062556	3.404378
324.868883	3938.225591	16.978189	-0.062423	3.401032
325.182975	3930.186709	16.983194	-0.062476	3.397650
325.306332	3922.151322	16.988199	-0.062493	3.394259
325.130876	3914.114110	16.993203	-0.062455	3.390854
325.052394	3906.162969	16.998208	-0.062435	3.387485
325.085630	3898.112223	17.003213	-0.062436	3.384075
324.961093	3890.205311	17.008218	-0.062408	3.380716
325.221916	3882.153935	17.013223	-0.062451	3.377307
325.284365	3874.117491	17.018227	-0.062457	3.373893
325.057413	3866.227242	17.023232	-0.062410	3.370528
325.059958	3858.172609	17.028237	-0.062405	3.367097
324.957700	3850.218041	17.033242	-0.062381	3.363702
325.301550	3842.232537	17.038247	-0.062439	3.360307
324.994607	3834.292271	17.043251	-0.062377	3.356903
324.930006	3826.274707	17.048256	-0.062359	3.353472
324.878886	3818.283149	17.053261	-0.062345	3.350049
324.924361	3810.305828	17.058266	-0.062348	3.346632
324.936219	3802.292326	17.063271	-0.062345	3.343195
324.734664	3794.316877	17.068275	-0.062302	3.339763
324.714252	3786.376470	17.073280	-0.062293	3.336349
324.443211	3778.365712	17.078285	-0.062237	3.332892
324.695533	3770.325405	17.083290	-0.062278	3.329438
324.584589	3762.359815	17.088295	-0.062252	3.325999
324.720429	3754.313176	17.093299	-0.062272	3.322531
324.610708	3746.379977	17.098304	-0.062247	3.319099
324.555741	3738.394564	17.103309	-0.062231	3.315643
324.238524	3730.440434	17.108314	-0.062167	3.312187
324.501066	3722.361742	17.113319	-0.062210	3.308696
324.219690	3714.399683	17.118323	-0.062153	3.305230
324.255789	3706.458970	17.123328	-0.062154	3.301782
324.227272	3698.424050	17.128333	-0.062143	3.298287
324.173696	3690.452997	17.133338	-0.062128	3.294816
324.247302	3682.440088	17.138343	-0.062136	3.291327
324.295772	3674.407899	17.143347	-0.062140	3.287826
324.341397	3666.440248	17.148352	-0.062143	3.284348
324.424608	3658.452578	17.153357	-0.062153	3.280860
324.425401	3650.501637	17.158362	-0.062148	3.277381
324.048083	3642.570534	17.163367	-0.062073	3.273892
323.911047	3634.574618	17.168371	-0.062042	3.270380
324.004439	3626.567426	17.173376	-0.062054	3.266868
323.437955	3618.595298	17.178381	-0.061943	3.263342
323.491055	3610.617667	17.183386	-0.061948	3.259834
323.594343	3602.634708	17.188391	-0.061962	3.256322
323.322964	3594.608282	17.193395	-0.061906	3.252772
323.134814	3586.635274	17.198400	-0.061865	3.249246
322.885406	3578.678885	17.203405	-0.061814	3.245720
322.858543	3570.687768	17.208410	-0.061803	3.242184
322.833727	3562.673483	17.213415	-0.061793	3.238634
323.229575	3554.614907	17.218419	-0.061862	3.235078
323.751359	3546.555897	17.223424	-0.061953	3.231523
323.434620	3538.607480	17.228429	-0.061889	3.227978
323.488082	3530.608929	17.233434	-0.061894	3.224423
323.540575	3522.669725	17.238439	-0.061898	3.220890
323.530303	3514.661897	17.243443	-0.061891	3.217320
323.387845	3506.680496	17.248448	-0.061859	3.213752
323.280468	3498.713751	17.253453	-0.061834	3.210188
323.241737	3490.730485	17.258458	-0.061821	3.206616
322.916607	3482.746745	17.263463	-0.061755	3.203027
322.798904	3474.795983	17.268467	-0.061728	3.199458
323.035053	3466.795654	17.273472	-0.061767	3.195878
322.979297	3458.781020	17.278477	-0.061751	3.192275
323.162466	3450.737738	17.283482	-0.061780	3.188666
323.278613	3442.733545	17.288487	-0.061796	3.185066
323.446501	3434.774842	17.293491	-0.061822	3.181486
322.890902	3426.911471	17.298496	-0.061713	3.177913
322.782641	3418.875390	17.303501	-0.061688	3.174277
322.932293	3410.864713	17.308506	-0.061710	3.170661
323.188597	3402.824392	17.313511	-0.061753	3.167031
323.017740	3394.880573	17.318515	-0.061716	3.163422
323.020846	3386.934963	17.323520	-0.061711	3.159816
322.849475	3378.943541	17.328525	-0.061674	3.156177
322.720875	3370.947594	17.333530	-0.061644	3.152533
322.853142	3362.903603	17.338535	-0.061664	3.148876
322.832897	3354.923037	17.343539	-0.061655	3.145236
322.540648	3347.028667	17.348544	-0.061595	3.141619
322.442972	3338.999901	17.353549	-0.061571	3.137945
322.724137	3330.967316	17.358554	-0.061618	3.134282
322.389587	3323.025323	17.363559	-0.061551	3.130628
322.385692	3314.999088	17.368563	-0.061545	3.126947
322.629962	3306.991365	17.373568	-0.061585	3.123281
322.484514	3299.040955	17.378573	-0.061552	3.119619
322.644073	3291.051586	17.383578	-0.061577	3.115949
322.605774	3283.094242	17.388583	-0.061564	3.112280
322.611778	3275.069457	17.393587	-0.061560	3.108578
322.113779	3267.171525	17.398592	-0.061462	3.104907
321.948453	3259.189351	17.403597	-0.061426	3.101208
322.345121	3251.136011	17.408602	-0.061494	3.097497
322.289278	3243.146336	17.413607	-0.061479	3.093791
322.199714	3235.142821	17.418611	-0.061457	3.090072
322.185165	3227.181598	17.423616	-0.061449	3.086372
322.222369	3219.187070	17.428621	-0.061450	3.082654
322.110223	3211.228230	17.433626	-0.061424	3.078941
321.761733	3203.324114	17.438631	-0.061354	3.075238
322.035822	3195.195109	17.443635	-0.061400	3.071456
322.365359	3187.159678	17.448640	-0.061456	3.067715
322.235538	3179.183428	17.453645	-0.061426	3.063975
322.025688	3171.287200	17.458650	-0.061382	3.060264
322.224762	3163.273062	17.463655	-0.061413	3.056514
322.234601	3155.245190	17.468659	-0.061410	3.052743
322.243187	3147.275786	17.473664	-0.061406	3.048994
322.209684	3139.310640	17.478669	-0.061395	3.045241
322.166143	3131.361676	17.483674	-0.061381	3.041491
322.126033	3123.367992	17.488679	-0.061368	3.037715
322.037262	3115.422383	17.493683	-0.061347	3.033954
321.954800	3107.440524	17.498688	-0.061326	3.030172
321.577907	3099.477991	17.503693	-0.061250	3.026380
321.647730	3091.490287	17.508698	-0.061258	3.022593
321.895486	3083.459580	17.513703	-0.061299	3.018790
321.681918	3075.495643	17.518707	-0.061254	3.014991
321.787484	3067.513203	17.523712	-0.061268	3.011195
321.096053	3059.595483	17.528717	-0.061134	3.007384
321.225227	3051.574555	17.533722	-0.061153	3.003560
321.316857	3043.561910	17.538727	-0.061165	2.999734
321.242905	3035.618868	17.543731	-0.061145	2.995927
321.320864	3027.604590	17.548736	-0.061155	2.992090
321.067617	3019.622464	17.553741	-0.061102	2.988246
320.987001	3011.629578	17.558746	-0.061082	2.984400
321.422975	3003.573867	17.563751	-0.061158	2.980547
321.318737	2995.623572	17.568755	-0.061133	2.976711
321.184592	2987.684874	17.573760	-0.061103	2.972874
321.078516	2979.690808	17.578765	-0.061078	2.969006
321.060542	2971.720229	17.583770	-0.061069	2.965150
320.968977	2963.749348	17.588775	-0.061047	2.961285
321.406342	2955.692719	17.593779	-0.061123	2.957401
321.390440	2947.758861	17.598784	-0.061114	2.953547
320.964929	2939.801853	17.603789	-0.061030	2.949656
320.916170	2931.831624	17.608794	-0.061015	2.945772
320.860180	2923.854166	17.613799	-0.061000	2.941880
321.105332	2915.803719	17.618803	-0.061040	2.937963
320.939417	2907.885076	17.623808	-0.061004	2.934084
321.002069	2899.865743	17.628813	-0.061010	2.930162
320.944126	2891.899716	17.633818	-0.060994	2.926254
320.737129	2883.974203	17.638823	-0.060950	2.922353
320.833197	2875.950880	17.643827	-0.060963	2.918416
320.842409	2867.997431	17.648832	-0.060959	2.914502
320.533954	2859.950069	17.653837	-0.060896	2.910520
320.536630	2851.970269	17.658842	-0.060891	2.906582
320.860445	2843.930710	17.663847	-0.060946	2.902628
320.731039	2835.962696	17.668851	-0.060917	2.898678
320.698172	2828.025655	17.673856	-0.060906	2.894744
320.762104	2820.036998	17.678861	-0.060912	2.890784
320.697394	2812.088154	17.683866	-0.060895	2.886831
320.549740	2804.124452	17.688871	-0.060862	2.882861
320.285230	2796.186231	17.693875	-0.060807	2.878891
320.357350	2788.216073	17.698880	-0.060816	2.874919
319.967967	2780.236671	17.703885	-0.060738	2.870911
320.216457	2772.198194	17.708890	-0.060779	2.866903
319.986440	2764.248193	17.713895	-0.060731	2.862907
320.118492	2756.243362	17.718899	-0.060750	2.858899
320.281163	2748.255513	17.723904	-0.060775	2.854895
320.124486	2740.287318	17.728909	-0.060740	2.850878
320.618938	2732.223188	17.733914	-0.060827	2.846843
320.260772	2724.329067	17.738919	-0.060755	2.842840
320.320766	2716.327904	17.743923	-0.060761	2.838801
320.257087	2708.413966	17.748928	-0.060744	2.834793
319.986294	2700.444574	17.753933	-0.060688	2.830740
320.268991	2692.386051	17.758938	-0.060735	2.826667
320.230734	2684.424548	17.763943	-0.060723	2.822620
320.320880	2676.438790	17.768947	-0.060734	2.818561
320.098006	2668.498911	17.773952	-0.060687	2.814502
319.763473	2660.544443	17.778957	-0.060620	2.810423
320.085784	2652.507653	17.783962	-0.060674	2.806335
319.876072	2644.572380	17.788967	-0.060630	2.802261
319.916934	2636.580584	17.793971	-0.060632	2.798167
320.081717	2628.595708	17.798976	-0.060658	2.794078
320.070706	2620.604159	17.803981	-0.060650	2.789969
319.820309	2612.668201	17.808986	-0.060598	2.785868
320.072909	2604.660812	17.813991	-0.060640	2.781755
320.179033	2596.683557	17.818995	-0.060655	2.777643
320.168304	2588.731216	17.824000	-0.060647	2.773530
320.230206	2580.686328	17.829005	-0.060653	2.769367
319.834060	2572.820103	17.834010	-0.060574	2.765263
319.491898	2564.904733	17.839015	-0.060505	2.761130
319.796685	2556.852146	17.844019	-0.060557	2.756960
319.937023	2548.845468	17.849024	-0.060578	2.752797
319.979674	2540.814011	17.854029	-0.060580	2.748609
319.897836	2532.841240	17.859034	-0.060560	2.744437
319.651697	2524.938985	17.864039	-0.060509	2.740286
319.619115	2516.964993	17.869043	-0.060497	2.736104
319.761878	2508.961422	17.874048	-0.060518	2.731911
319.690924	2500.970167	17.879053	-0.060500	2.727705
319.788310	2492.989425	17.884058	-0.060513	2.723508
319.300349	2485.120319	17.889063	-0.060417	2.719327
319.634105	2477.084865	17.894067	-0.060473	2.715104
319.871360	2469.082800	17.899072	-0.060512	2.710885
319.457956	2461.162275	17.904077	-0.060430	2.706662
319.534058	2453.169814	17.909082	-0.060439	2.702425
319.544252	2445.190203	17.914087	-0.060435	2.698184
319.399190	2437.234367	17.919091	-0.060403	2.693939
319.432272	2429.257197	17.924096	-0.060404	2.689687
319.084763	2421.312703	17.929101	-0.060334	2.685422
319.281924	2413.328563	17.934106	-0.060365	2.681164
319.199681	2405.359114	17.939111	-0.060345	2.676888
318.981957	2397.399843	17.944115	-0.060299	2.672603
319.129293	2389.406965	17.949120	-0.060321	2.668316
319.263326	2381.367634	17.954125	-0.060340	2.663997
319.109747	2373.450102	17.959130	-0.060307	2.659717
319.246364	2365.465759	17.964135	-0.060327	2.655414
318.911623	2357.533400	17.969139	-0.060259	2.651100
318.879349	2349.553742	17.974144	-0.060248	2.646774
319.002036	2341.537508	17.979149	-0.060265	2.642431
319.453725	2333.542944	17.984154	-0.060344	2.638116
319.190171	2325.623633	17.989159	-0.060290	2.633785
318.794693	2317.708737	17.994163	-0.060211	2.629441
318.500391	2309.764577	17.999168	-0.060151	2.625081
318.686742	2301.710283	18.004173	-0.060180	2.620686
318.838759	2293.757325	18.009178	-0.060203	2.616337
318.871298	2285.770805	18.014183	-0.060204	2.611954
318.865505	2277.792831	18.019187	-0.060197	2.607565
318.680519	2269.888708	18.024192	-0.060158	2.603198
318.571779	2261.907262	18.029197	-0.060132	2.598785
318.829126	2253.913381	18.034202	-0.060175	2.594384
318.848404	2245.823502	18.039207	-0.060173	2.589906
318.733256	2237.846392	18.044211	-0.060146	2.585472
318.812249	2229.918545	18.049216	-0.060155	2.581073
318.769083	2221.967236	18.054221	-0.060142	2.576644
318.596891	2214.023048	18.059226	-0.060105	2.572202
318.378874	2206.102691	18.064231	-0.060059	2.567763
318.428358	2198.095225	18.069235	-0.060063	2.563286
318.434887	2190.159778	18.074240	-0.060059	2.558839
318.128896	2182.209388	18.079245	-0.059996	2.554353
318.246655	2174.253649	18.084250	-0.060013	2.549887
318.184135	2166.263155	18.089255	-0.059996	2.545380
318.194729	2158.296540	18.094259	-0.059993	2.540884
318.097676	2150.359212	18.099264	-0.059969	2.536389
318.299406	2142.334818	18.104269	-0.060002	2.531858
318.050643	2134.418671	18.109274	-0.059950	2.527347
318.278289	2126.399947	18.114279	-0.059987	2.522806
317.964734	2118.507313	18.119283	-0.059923	2.518288
317.913003	2110.562909	18.124288	-0.059908	2.513751
317.900321	2102.562055	18.129293	-0.059901	2.509177
317.735867	2094.608009	18.134298	-0.059865	2.504610
317.888616	2086.625452	18.139303	-0.059888	2.500042
317.892351	2078.642308	18.144307	-0.059883	2.495454
317.901939	2070.678762	18.149312	-0.059880	2.490870
317.896858	2062.699606	18.154317	-0.059873	2.486267
317.678024	2054.795542	18.159322	-0.059827	2.481683
317.411816	2046.893559	18.164327	-0.059773	2.477087
317.426888	2038.882419	18.169331	-0.059770	2.472441
317.643643	2030.883996	18.174336	-0.059805	2.467810
317.535274	2022.901404	18.179341	-0.059780	2.463153
317.676804	2014.943306	18.184346	-0.059801	2.458522
317.492925	2007.022198	18.189351	-0.059761	2.453878
317.401278	1999.037433	18.194355	-0.059739	2.449196
317.567768	1991.058842	18.199360	-0.059764	2.444528
317.511350	1983.128610	18.204365	-0.059749	2.439862
317.283532	1975.216446	18.209370	-0.059701	2.435184
317.459211	1967.187275	18.214375	-0.059728	2.430460
317.532678	1959.184022	18.219379	-0.059737	2.425734
317.392550	1951.263197	18.224384	-0.059705	2.421031
317.127709	1943.329812	18.229389	-0.059651	2.416301
317.028507	1935.377935	18.234394	-0.059627	2.411565
316.931651	1927.429122	18.239399	-0.059604	2.406820
316.688252	1919.492683	18.244403	-0.059553	2.402062
316.971271	1911.491849	18.249408	-0.059600	2.397299
316.651816	1903.578302	18.254413	-0.059535	2.392529
316.795413	1895.598441	18.259418	-0.059557	2.387748
316.608888	1887.647587	18.264423	-0.059517	2.382948
316.809938	1879.645057	18.269427	-0.059549	2.378138
317.144989	1871.651048	18.274432	-0.059606	2.373335
316.798710	1863.744323	18.279437	-0.059536	2.368519
316.617675	1855.811716	18.284442	-0.059497	2.363691
316.590408	1847.883536	18.289447	-0.059487	2.358869
316.561351	1839.920628	18.294451	-0.059476	2.354015
316.582342	1831.947672	18.299456	-0.059475	2.349150
316.654299	1823.949087	18.304461	-0.059483	2.344262
316.718158	1816.003841	18.309466	-0.059489	2.339397
316.639138	1808.079365	18.314471	-0.059469	2.334522
316.655606	1800.096100	18.319475	-0.059467	2.329609
316.789341	1792.141895	18.324480	-0.059487	2.324714
316.498935	1784.237326	18.329485	-0.059427	2.319802
316.537551	1776.288355	18.334490	-0.059429	2.314881
316.370869	1768.371944	18.339495	-0.059393	2.309952
316.469007	1760.355834	18.344499	-0.059406	2.304973
316.319960	1752.475859	18.349504	-0.059373	2.300047
316.077542	1744.513458	18.354509	-0.059322	2.295051
316.373256	1736.493333	18.359514	-0.059372	2.290054
316.275438	1728.572612	18.364519	-0.059349	2.285075
316.330573	1720.612283	18.369523	-0.059354	2.280073
316.487509	1712.668584	18.374528	-0.059378	2.275079
316.379801	1704.676843	18.379533	-0.059352	2.270021
316.190266	1696.732603	18.384538	-0.059312	2.264975
316.314657	1688.790885	18.389543	-0.059329	2.259946
316.141986	1680.848919	18.394547	-0.059292	2.254880
315.994691	1672.947287	18.399552	-0.059259	2.249830
315.906932	1664.974354	18.404557	-0.059238	2.244729
316.037933	1657.037846	18.409562	-0.059257	2.239659
316.220414	1649.056331	18.414567	-0.059285	2.234553
316.066794	1641.135352	18.419571	-0.059251	2.229444
316.063328	1633.188736	18.424576	-0.059246	2.224321
315.826200	1625.279385	18.429581	-0.059196	2.219188
315.750294	1617.348136	18.434586	-0.059177	2.214044
315.859099	1609.368399	18.439591	-0.059192	2.208874
315.718277	1601.436144	18.444595	-0.059160	2.203699
315.763864	1593.501662	18.449600	-0.059163	2.198528
315.629455	1585.563670	18.454605	-0.059133	2.193326
315.482769	1577.645386	18.459610	-0.059100	2.188123
315.436083	1569.689061	18.464615	-0.059086	2.182892
315.467849	1561.728798	18.469619	-0.059087	2.177653
315.548294	1553.775502	18.474624	-0.059097	2.172410
315.253579	1545.874239	18.479629	-0.059037	2.167154
315.365193	1537.907834	18.484634	-0.059052	2.161881
315.413649	1529.977093	18.489639	-0.059056	2.156612
315.281265	1522.044393	18.494643	-0.059026	2.151312
315.191242	1514.112165	18.499648	-0.059004	2.146003
315.103049	1506.165835	18.504653	-0.058982	2.140671
315.239355	1498.225792	18.509658	-0.059002	2.135353
315.153458	1490.289545	18.514663	-0.058981	2.130002
315.155025	1482.327382	18.519667	-0.058976	2.124628
315.221055	1474.420482	18.524672	-0.058983	2.119284
315.085323	1466.508681	18.529677	-0.058952	2.113904
314.980771	1458.543118	18.534682	-0.058927	2.108477
314.820569	1450.616499	18.539687	-0.058892	2.103056
314.742718	1442.694558	18.544691	-0.058873	2.097633
314.862821	1434.735414	18.549696	-0.058890	2.092190
314.793392	1426.787536	18.554701	-0.058871	2.086722
314.908448	1418.863219	18.559706	-0.058888	2.081274
314.801384	1410.964266	18.564711	-0.058862	2.075807
314.719544	1403.036796	18.569715	-0.058842	2.070308
314.625274	1395.112944	18.574720	-0.058819	2.064796
314.530753	1387.185710	18.579725	-0.058796	2.059267
314.535541	1379.261199	18.584730	-0.058792	2.053735
314.128649	1371.396349	18.589735	-0.058711	2.048187
314.669265	1363.338817	18.594739	-0.058806	2.042587
314.716685	1355.442167	18.599744	-0.058810	2.037033
314.307242	1347.580176	18.604749	-0.058728	2.031441
314.229463	1339.637530	18.609754	-0.058708	2.025812
314.135046	1331.733083	18.614759	-0.058685	2.020191
313.843925	1323.823138	18.619763	-0.058626	2.014531
314.248151	1315.833424	18.624768	-0.058696	2.008871
314.141949	1307.912837	18.629773	-0.058671	2.003191
314.100323	1300.015580	18.634778	-0.058658	1.997518
314.375477	1292.046316	18.639783	-0.058704	1.991811
314.237310	1284.141493	18.644787	-0.058673	1.986089
313.961950	1276.286935	18.649792	-0.058616	1.980373
314.199489	1268.300969	18.654797	-0.058655	1.974600
314.226803	1260.385056	18.659802	-0.058655	1.968839
314.247633	1252.480643	18.664807	-0.058653	1.963068
313.869025	1244.618597	18.669811	-0.058578	1.957267
313.938879	1236.704387	18.674816	-0.058585	1.951461
313.898727	1228.752801	18.679821	-0.058573	1.945597
313.939947	1220.838642	18.684826	-0.058575	1.939752
313.883997	1212.931831	18.689831	-0.058559	1.933884
313.817355	1205.003488	18.694835	-0.058542	1.927981
313.763488	1197.092920	18.699840	-0.058526	1.922074
313.556728	1189.212362	18.704845	-0.058483	1.916155
313.793820	1181.264414	18.709850	-0.058521	1.910217
313.644051	1173.366001	18.714855	-0.058488	1.904253
313.401112	1165.492570	18.719859	-0.058438	1.898279
313.454786	1157.582854	18.724864	-0.058443	1.892293
313.517566	1149.631485	18.729869	-0.058449	1.886257
313.490152	1141.752982	18.734874	-0.058439	1.880247
313.418291	1133.863871	18.739879	-0.058420	1.874204
313.317203	1125.964086	18.744883	-0.058396	1.868130
313.399634	1118.042066	18.749888	-0.058406	1.862041
313.181757	1110.163909	18.754893	-0.058360	1.855929
313.211909	1102.245775	18.759898	-0.058360	1.849797
313.215014	1094.345369	18.764903	-0.058356	1.843654
313.009414	1086.477442	18.769907	-0.058312	1.837491
313.075056	1078.569318	18.774912	-0.058319	1.831309
313.130173	1070.644187	18.779917	-0.058324	1.825091
312.808540	1062.813736	18.784922	-0.058259	1.818881
312.804629	1054.904520	18.789927	-0.058253	1.812625
312.869904	1046.973939	18.794931	-0.058260	1.806340
312.769909	1039.113734	18.799936	-0.058236	1.800068
312.746786	1031.221831	18.804941	-0.058226	1.793759
312.685716	1023.303535	18.809946	-0.058210	1.787401
312.615910	1015.418461	18.814951	-0.058192	1.781047
312.428888	1007.549545	18.819955	-0.058151	1.774668
312.334605	999.681685	18.824960	-0.058129	1.768278
312.414692	991.763322	18.829965	-0.058138	1.761846
312.445767	983.880658	18.834970	-0.058139	1.755414
312.297446	976.017667	18.839975	-0.058106	1.748951
312.216591	968.138011	18.844979	-0.058086	1.742459
312.412278	960.238437	18.849984	-0.058117	1.735962
312.145560	952.384738	18.854989	-0.058062	1.729418
312.002675	944.540524	18.859994	-0.058030	1.722874
312.005733	936.668667	18.864999	-0.058025	1.716301
311.794118	928.805236	18.870003	-0.057981	1.709681
311.988644	920.885432	18.875008	-0.058012	1.703042
312.093028	912.993562	18.880013	-0.058026	1.696388
312.073814	905.122507	18.885018	-0.058017	1.689710
312.003840	897.270643	18.890023	-0.057999	1.683014
311.851277	889.421792	18.895027	-0.057965	1.676283
311.872556	881.568743	18.900032	-0.057964	1.669545
311.875776	873.687830	18.905037	-0.057959	1.662753
311.618947	865.875651	18.910042	-0.057906	1.655957
311.790000	857.977965	18.915047	-0.057933	1.649118
311.555215	850.147844	18.920051	-0.057884	1.642252
311.621105	842.303245	18.925056	-0.057891	1.635388
311.510360	834.415655	18.930061	-0.057865	1.628431
311.394495	826.568808	18.935066	-0.057838	1.621480
310.954144	818.779860	18.940071	-0.057751	1.614504
311.000979	810.893009	18.945075	-0.057754	1.607481
311.201143	803.016347	18.950080	-0.057786	1.600457
311.058666	795.198006	18.955085	-0.057755	1.593406
311.022496	787.343402	18.960090	-0.057743	1.586306
311.014978	779.506596	18.965095	-0.057736	1.579194
310.923212	771.675753	18.970099	-0.057714	1.572044
310.847288	763.839385	18.975104	-0.057694	1.564857
310.761361	756.031664	18.980109	-0.057673	1.557663
310.736519	748.197030	18.985114	-0.057663	1.550419
310.533299	740.390192	18.990119	-0.057620	1.543140
310.505107	732.546790	18.995123	-0.057610	1.535819
310.525618	724.710868	19.000128	-0.057608	1.528478
310.430124	716.889727	19.005133	-0.057585	1.521097
310.317737	709.096820	19.010138	-0.057559	1.513704
310.438240	701.248133	19.015143	-0.057576	1.506258
310.314497	693.443764	19.020147	-0.057548	1.498780
310.180483	685.654957	19.025152	-0.057518	1.491277
309.863279	677.876745	19.030157	-0.057454	1.483717
309.935139	670.063033	19.035162	-0.057462	1.476146
309.618976	662.279407	19.040167	-0.057398	1.468503
309.427587	654.468260	19.045171	-0.057357	1.460813
309.649195	646.632706	19.050176	-0.057393	1.453125
309.514119	638.832800	19.055181	-0.057363	1.445374
309.275208	631.095844	19.060186	-0.057313	1.437626
309.039722	623.323600	19.065191	-0.057264	1.429802
308.949370	615.530190	19.070195	-0.057242	1.421937
308.741934	607.782694	19.075200	-0.057198	1.414055
308.343429	600.029077	19.080205	-0.057119	1.406091
308.400333	592.244774	19.085210	-0.057124	1.398127
308.289580	584.471450	19.090215	-0.057098	1.390100
307.933928	576.727622	19.095219	-0.057027	1.382014
307.893718	568.957185	19.100224	-0.057014	1.373908
307.881000	561.153865	19.105229	-0.057007	1.365725
307.668200	553.441967	19.110234	-0.056962	1.357553
307.271903	545.731219	19.115239	-0.056883	1.349300
306.922296	538.011484	19.120243	-0.056813	1.340995
306.828758	530.275282	19.125248	-0.056790	1.332666
306.227635	522.588797	19.130253	-0.056673	1.324247
306.134951	514.848070	19.135258	-0.056651	1.315808
305.895791	507.032490	19.140263	-0.056601	1.307204
305.287163	499.364745	19.145267	-0.056483	1.298639
305.163151	491.630000	19.150272	-0.056454	1.290032
304.902580	483.921316	19.155277	-0.056401	1.281371
304.419752	476.262317	19.160282	-0.056306	1.272665
304.221339	468.556688	19.165287	-0.056263	1.263900
303.670034	460.903724	19.170291	-0.056156	1.255066
303.412490	453.213418	19.175296	-0.056103	1.246183
302.862344	445.580989	19.180301	-0.055995	1.237246
302.373304	437.930268	19.185306	-0.055899	1.228234
301.838581	430.292634	19.190311	-0.055794	1.219162
301.377276	422.629664	19.195315	-0.055703	1.210006
301.166994	414.954279	19.200320	-0.055659	1.200817
300.567747	407.345970	19.205325	-0.055542	1.191557
300.353480	399.671402	19.210330	-0.055497	1.182224
299.745152	392.089994	19.215335	-0.055379	1.172848
299.319004	384.457299	19.220339	-0.055295	1.163372
298.907455	376.852749	19.225344	-0.055213	1.153856
298.387130	369.225736	19.230349	-0.055111	1.144208
298.009870	361.622261	19.235354	-0.055036	1.134540
297.581600	354.026837	19.240359	-0.054951	1.124787
296.873166	346.498681	19.245363	-0.054814	1.114973
296.518163	338.906060	19.250368	-0.054743	1.105067
295.882273	331.377600	19.255373	-0.054619	1.095092
295.536133	323.797602	19.260378	-0.054550	1.085022
294.859153	316.302262	19.265383	-0.054419	1.074895
294.445922	308.743986	19.270387	-0.054337	1.064648
293.885571	301.250118	19.275392	-0.054227	1.054354
293.122230	293.772902	19.280397	-0.054080	1.043933
292.804059	286.256140	19.285402	-0.054016	1.033459
292.031397	278.822121	19.290407	-0.053867	1.022883
291.596105	271.324334	19.295411	-0.053781	1.012189
291.132931	263.865852	19.300416	-0.053690	1.001429
290.691514	256.396616	19.305421	-0.053603	0.990542
290.416882	248.902829	19.310426	-0.053546	0.979541
290.054861	241.466606	19.315431	-0.053474	0.968478
289.679183	234.040040	19.320435	-0.053399	0.957297
289.307886	226.648977	19.325440	-0.053325	0.946039
288.374413	219.359074	19.330445	-0.053146	0.934649
287.578137	212.062427	19.335450	-0.052993	0.923145
287.351535	204.685948	19.340455	-0.052946	0.911528
286.825071	197.361009	19.345459	-0.052843	0.899758
286.419132	190.047084	19.350464	-0.052763	0.887884
286.197626	182.726688	19.355469	-0.052717	0.875892
285.696436	175.486119	19.360474	-0.052618	0.863784
285.194262	168.257089	19.365479	-0.052520	0.851522
284.687553	161.058689	19.370483	-0.052421	0.839132
284.381487	153.840781	19.375488	-0.052359	0.826584
283.823659	146.696773	19.380493	-0.052250	0.813894
283.071881	139.620923	19.385498	-0.052106	0.801063
282.747340	132.486823	19.390503	-0.052041	0.788055
281.943200	125.476015	19.395507	-0.051886	0.774899
281.541451	118.424733	19.400512	-0.051807	0.761574
281.301254	111.377330	19.405517	-0.051757	0.748074
280.878908	104.394710	19.410522	-0.051674	0.734388
280.322537	97.478062	19.415527	-0.051566	0.720527
279.666650	90.617995	19.420531	-0.051439	0.706472
279.153299	83.782708	19.425536	-0.051339	0.692236
278.571055	77.162273	19.430541	-0.051226	0.678130