Fri Apr 16 18:36:13 2021

Number of Points = 3641
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.965000	-0.052823	0.000000	-0.000051	0.306726

2.553298	-0.160132	0.005005	-0.000160	0.306723
2.112191	-0.079991	0.010010	-0.000078	0.306723
2.074069	-0.071977	0.015014	-0.000071	0.306728
2.070324	-0.070511	0.020019	-0.000070	0.306731
1.959194	-0.051056	0.025024	-0.000049	0.306727
1.307683	0.073371	0.030029	0.000072	0.306755
1.189453	0.094812	0.035034	0.000094	0.306754
1.608878	-0.005387	0.040038	0.000016	0.306641
1.852719	-0.099243	0.045043	-0.000029	0.306407
1.869775	-0.105338	0.050048	-0.000032	0.306392
2.191988	-0.161506	0.055053	-0.000092	0.306403
1.906234	-0.108799	0.060058	-0.000039	0.306406
1.444425	-0.023417	0.065062	0.000047	0.306413
1.629542	-0.055500	0.070067	0.000013	0.306419
1.312570	0.001805	0.075072	0.000072	0.306418
1.670318	-0.062753	0.080077	0.000006	0.306419
1.525299	-0.046758	0.085082	0.000033	0.306370
1.915030	-0.175674	0.090086	-0.000040	0.306095
1.702937	-0.135250	0.095091	-0.000000	0.306104
1.786658	-0.153579	0.100096	-0.000016	0.306088
1.731751	-0.139983	0.105101	-0.000005	0.306105
1.721763	-0.140240	0.110106	-0.000003	0.306095
1.658824	-0.150720	0.115110	0.000008	0.305991
2.142177	-0.285497	0.120115	-0.000081	0.305768
1.857590	-0.233250	0.125120	-0.000028	0.305770
1.926722	-0.244881	0.130125	-0.000041	0.305774
1.775968	-0.218156	0.135130	-0.000013	0.305771
2.011060	-0.308585	0.140134	-0.000057	0.305545
1.894205	-0.292943	0.145139	-0.000035	0.305518
1.402557	-0.202203	0.150144	0.000057	0.305524
1.095372	-0.141593	0.155149	0.000114	0.305546
1.549904	-0.275953	0.160154	0.000030	0.305300
1.815111	-0.351274	0.165158	-0.000020	0.305171
1.932936	-0.371495	0.170163	-0.000042	0.305177
2.034333	-0.404322	0.175168	-0.000060	0.305108
1.810027	-0.415163	0.180173	-0.000018	0.304863
1.705725	-0.396625	0.185178	0.000001	0.304860
1.969624	-0.446417	0.190182	-0.000048	0.304851
2.097242	-0.538113	0.195187	-0.000072	0.304525
1.937498	-0.510342	0.200192	-0.000042	0.304519
1.953308	-0.519802	0.205197	-0.000045	0.304487
1.769446	-0.538103	0.210202	-0.000010	0.304241
1.665911	-0.518128	0.215206	0.000009	0.304246
1.914606	-0.589589	0.220211	-0.000037	0.304121
1.835520	-0.621626	0.225216	-0.000022	0.303899
1.783152	-0.609401	0.230221	-0.000012	0.303912
1.800838	-0.664609	0.235226	-0.000016	0.303664
1.732750	-0.667120	0.240230	-0.000003	0.303592
2.015689	-0.737372	0.245235	-0.000055	0.303502
1.854114	-0.759151	0.250240	-0.000025	0.303258
1.772009	-0.740947	0.255245	-0.000010	0.303273
1.987416	-0.837843	0.260250	-0.000050	0.302997
2.124814	-0.868270	0.265254	-0.000075	0.302970
2.265823	-0.945891	0.270259	-0.000101	0.302722
2.211655	-0.958381	0.275264	-0.000091	0.302614
2.044122	-0.967688	0.280269	-0.000060	0.302424
2.188964	-1.017809	0.285274	-0.000087	0.302309
2.033272	-1.032510	0.290278	-0.000058	0.302103
2.116567	-1.071243	0.295283	-0.000073	0.301990
2.231065	-1.134482	0.300288	-0.000094	0.301786
2.023900	-1.111703	0.305293	-0.000055	0.301714
2.117366	-1.184014	0.310298	-0.000073	0.301448
2.210825	-1.218869	0.315302	-0.000090	0.301362
2.169863	-1.269512	0.320307	-0.000082	0.301083
1.882616	-1.231486	0.325312	-0.000029	0.301014
2.207637	-1.345377	0.330317	-0.000089	0.300750
1.816393	-1.293881	0.335322	-0.000016	0.300655
1.715355	-1.303884	0.340326	0.000003	0.300518
1.919495	-1.385443	0.345331	-0.000035	0.300304
1.695894	-1.373123	0.350336	0.000007	0.300167
1.960974	-1.479472	0.355341	-0.000043	0.299886
1.714942	-1.454579	0.360346	0.000003	0.299790
1.561466	-1.479101	0.365350	0.000032	0.299536
1.481529	-1.492538	0.370355	0.000047	0.299401
1.348518	-1.499783	0.375360	0.000072	0.299248
1.578329	-1.598952	0.380365	0.000029	0.298970
1.676017	-1.644400	0.385370	0.000011	0.298836
1.067045	-1.579521	0.390374	0.000125	0.298613
1.307823	-1.662786	0.395379	0.000080	0.298421
1.327369	-1.695292	0.400384	0.000076	0.298281
1.125076	-1.713461	0.405389	0.000114	0.298014
1.437719	-1.804888	0.410394	0.000056	0.297845
1.279726	-1.813485	0.415398	0.000086	0.297663
1.180921	-1.853485	0.420403	0.000104	0.297381
1.162241	-1.883519	0.425408	0.000108	0.297218
1.450433	-1.976548	0.430413	0.000054	0.297019
1.275590	-2.002265	0.435418	0.000087	0.296739
1.493089	-2.081441	0.440422	0.000047	0.296545
1.292538	-2.080635	0.445427	0.000084	0.296371
1.402651	-2.161784	0.450432	0.000064	0.296071
1.740088	-2.267545	0.455437	0.000001	0.295854
1.773229	-2.312828	0.460442	-0.000005	0.295661
1.354804	-2.270219	0.465446	0.000073	0.295497
0.774932	-2.230032	0.470451	0.000181	0.295177
0.553669	-2.232543	0.475456	0.000222	0.294967
1.100257	-2.372760	0.480461	0.000121	0.294766
1.287473	-2.457830	0.485466	0.000086	0.294515
0.878545	-2.436302	0.490470	0.000162	0.294255
0.637251	-2.434343	0.495475	0.000207	0.294049
0.325668	-2.419793	0.500480	0.000265	0.293841
0.390378	-2.479917	0.505485	0.000253	0.293602
0.179991	-2.500231	0.510490	0.000293	0.293313
0.262956	-2.555172	0.515494	0.000277	0.293116
-0.070347	-2.530648	0.520499	0.000339	0.292937
-0.113655	-2.580650	0.525504	0.000348	0.292651
-0.438055	-2.573609	0.530509	0.000408	0.292394
-0.685350	-2.571418	0.535514	0.000454	0.292181
-1.152838	-2.523279	0.540518	0.000541	0.291999
-1.401249	-2.531554	0.545523	0.000588	0.291733
-1.674241	-2.526389	0.550528	0.000639	0.291512
-1.922924	-2.512964	0.555533	0.000685	0.291354
-2.597059	-2.440383	0.560538	0.000811	0.291105
-2.107890	-2.575560	0.565542	0.000720	0.290875
-2.672253	-2.499383	0.570547	0.000825	0.290743
-2.644960	-2.552266	0.575552	0.000820	0.290504
-2.406180	-2.638995	0.580557	0.000775	0.290287
-3.152446	-2.536393	0.585562	0.000914	0.290122
-3.340569	-2.557487	0.590566	0.000950	0.289846
-3.547166	-2.554772	0.595571	0.000988	0.289671
-3.986816	-2.507262	0.600576	0.001070	0.289509
-4.227521	-2.512703	0.605581	0.001115	0.289262
-4.403835	-2.503782	0.610586	0.001148	0.289146
-4.783329	-2.484000	0.615590	0.001219	0.288899
-4.843286	-2.506294	0.620595	0.001230	0.288733
-5.168047	-2.476413	0.625600	0.001290	0.288586
-4.928269	-2.577082	0.630605	0.001246	0.288299
-5.465974	-2.495615	0.635610	0.001346	0.288217
-5.732262	-2.495565	0.640614	0.001396	0.287974
-5.901739	-2.492015	0.645619	0.001427	0.287836
-6.202024	-2.479275	0.650624	0.001483	0.287625
-6.048060	-2.543879	0.655629	0.001455	0.287440
-6.441646	-2.496755	0.660634	0.001528	0.287317
-6.763116	-2.492123	0.665638	0.001588	0.287045
-7.027064	-2.451276	0.670643	0.001637	0.287009
-7.106641	-2.492962	0.675648	0.001652	0.286725
-7.411510	-2.442901	0.680653	0.001709	0.286698
-7.663728	-2.459880	0.685658	0.001756	0.286380
-7.241666	-2.549895	0.690662	0.001678	0.286312
-7.839617	-2.490171	0.695667	0.001789	0.286064
-7.792040	-2.516758	0.700672	0.001780	0.285973
-7.911082	-2.540525	0.705677	0.001803	0.285742
-8.223946	-2.500429	0.710682	0.001861	0.285657
-8.873123	-2.415779	0.715686	0.001982	0.285487
-9.154327	-2.381243	0.720691	0.002034	0.285403
-9.291025	-2.407055	0.725696	0.002060	0.285145
-9.026134	-2.468946	0.730701	0.002011	0.285075
-9.523083	-2.426346	0.735706	0.002103	0.284832
-9.569346	-2.427306	0.740710	0.002112	0.284784
-10.048770	-2.391812	0.745715	0.002201	0.284521
-10.082886	-2.388392	0.750720	0.002208	0.284506
-10.226119	-2.414882	0.755725	0.002235	0.284238
-10.257455	-2.412317	0.760730	0.002241	0.284222
-10.660595	-2.393846	0.765734	0.002316	0.283942
-10.857149	-2.369410	0.770739	0.002352	0.283884
-10.754547	-2.424740	0.775744	0.002333	0.283697
-11.063308	-2.392977	0.780749	0.002391	0.283572
-11.355043	-2.360526	0.785754	0.002445	0.283466
-11.319865	-2.411127	0.790758	0.002439	0.283240
-11.382590	-2.402045	0.795763	0.002451	0.283227
-11.784114	-2.383058	0.800768	0.002526	0.282951
-11.863890	-2.365927	0.805773	0.002541	0.282964
-12.187071	-2.359082	0.810778	0.002601	0.282698
-12.481812	-2.319131	0.815782	0.002656	0.282627
-12.334321	-2.368290	0.820787	0.002628	0.282512
-12.365716	-2.404970	0.825792	0.002634	0.282295
-12.386630	-2.406755	0.830797	0.002638	0.282266
-12.664640	-2.412718	0.835802	0.002690	0.281975
-12.421204	-2.458240	0.840806	0.002645	0.281968
-12.588599	-2.474830	0.845811	0.002676	0.281726
-13.161410	-2.378560	0.850816	0.002783	0.281685
-13.068035	-2.432329	0.855821	0.002766	0.281496
-13.134061	-2.447651	0.860826	0.002778	0.281355
-13.324896	-2.433058	0.865830	0.002814	0.281251
-13.668565	-2.409036	0.870835	0.002878	0.281052
-13.883716	-2.370677	0.875840	0.002918	0.281048
-13.842986	-2.434008	0.880845	0.002910	0.280759
-14.353195	-2.345454	0.885850	0.003005	0.280737
-14.406111	-2.360153	0.890854	0.003015	0.280611
-14.484129	-2.364205	0.895859	0.003030	0.280517
-14.809223	-2.310636	0.900864	0.003091	0.280488
-14.591474	-2.412316	0.905869	0.003050	0.280167
-14.391734	-2.451052	0.910874	0.003013	0.280154
-14.770211	-2.427954	0.915878	0.003084	0.279917
-15.119151	-2.378091	0.920883	0.003149	0.279846
-15.101949	-2.405322	0.925888	0.003146	0.279721
-15.175092	-2.430800	0.930893	0.003159	0.279520
-15.352395	-2.399284	0.935898	0.003192	0.279515
-15.921677	-2.347656	0.940902	0.003299	0.279246
-15.800013	-2.369929	0.945907	0.003276	0.279245
-16.185482	-2.330953	0.950912	0.003348	0.279083
-16.031533	-2.395015	0.955917	0.003319	0.278895
-16.097647	-2.383218	0.960922	0.003332	0.278894
-16.085902	-2.445833	0.965926	0.003330	0.278579
-16.682400	-2.336886	0.970931	0.003441	0.278581
-16.600778	-2.386113	0.975936	0.003426	0.278402
-16.808381	-2.374872	0.980941	0.003464	0.278264
-17.150688	-2.313452	0.985946	0.003528	0.278259
-17.810546	-2.244409	0.990950	0.003651	0.277993
-16.926645	-2.408020	0.995955	0.003487	0.277978
-17.320339	-2.365569	1.000960	0.003560	0.277826
-17.928493	-2.289249	1.005965	0.003673	0.277646
-18.019174	-2.272070	1.010970	0.003690	0.277650
-17.994831	-2.322249	1.015974	0.003686	0.277410
-18.304882	-2.279510	1.020979	0.003744	0.277339
-18.815168	-2.185536	1.025984	0.003839	0.277345
-18.260358	-2.349048	1.030989	0.003736	0.277017
-19.294959	-2.157616	1.035994	0.003928	0.277034
-18.898220	-2.243261	1.040998	0.003855	0.276963
-18.925070	-2.283908	1.046003	0.003860	0.276724
-18.806470	-2.308261	1.051008	0.003838	0.276709
-18.986407	-2.306728	1.056013	0.003871	0.276545
-19.225525	-2.294001	1.061018	0.003916	0.276384
-19.090274	-2.318967	1.066022	0.003891	0.276381
-19.497012	-2.292346	1.071027	0.003967	0.276133
-19.572702	-2.289841	1.076032	0.003981	0.276073
-19.491566	-2.316348	1.081037	0.003966	0.276011
-20.119156	-2.246463	1.086042	0.004083	0.275779
-19.832864	-2.302041	1.091046	0.004030	0.275760
-19.724996	-2.344085	1.096051	0.004010	0.275641
-19.777902	-2.359664	1.101056	0.004020	0.275509
-20.169630	-2.285971	1.106061	0.004093	0.275521
-20.337215	-2.321456	1.111066	0.004124	0.275174
-20.019383	-2.381616	1.116070	0.004065	0.275161
-20.118376	-2.390353	1.121075	0.004083	0.275020
-20.473694	-2.359892	1.126080	0.004150	0.274839
-20.415228	-2.368667	1.131085	0.004139	0.274849
-20.822145	-2.356540	1.136090	0.004215	0.274522
-20.919696	-2.339523	1.141094	0.004233	0.274518
-20.827882	-2.381368	1.146099	0.004216	0.274385
-21.144022	-2.353898	1.151104	0.004275	0.274226
-21.333880	-2.317214	1.156109	0.004310	0.274237
-21.691688	-2.312319	1.161114	0.004377	0.273918
-21.652732	-2.321768	1.166118	0.004370	0.273905
-21.740456	-2.324054	1.171123	0.004386	0.273808
-22.267454	-2.270289	1.176128	0.004484	0.273585
-21.792246	-2.355603	1.181133	0.004396	0.273591
-22.333903	-2.297941	1.186138	0.004497	0.273374
-22.936181	-2.205135	1.191142	0.004609	0.273285
-22.493255	-2.286819	1.196147	0.004527	0.273278
-22.672300	-2.309810	1.201152	0.004560	0.272983
-22.854207	-2.276785	1.206157	0.004594	0.272983
-22.945382	-2.277409	1.211162	0.004611	0.272891
-23.093904	-2.297090	1.216166	0.004639	0.272643
-23.176934	-2.280374	1.221171	0.004655	0.272651
-23.474776	-2.265466	1.226176	0.004710	0.272442
-23.697613	-2.243256	1.231181	0.004752	0.272344
-23.504700	-2.281205	1.236186	0.004716	0.272328
-23.607065	-2.318415	1.241190	0.004735	0.272031
-23.655328	-2.313220	1.246195	0.004744	0.272011
-23.824183	-2.298552	1.251200	0.004776	0.271925
-24.597916	-2.194600	1.256205	0.004920	0.271729
-24.708778	-2.173069	1.261210	0.004941	0.271736
-24.579117	-2.223630	1.266214	0.004917	0.271592
-24.454422	-2.283008	1.271219	0.004893	0.271395
-24.522531	-2.273734	1.276224	0.004906	0.271378
-24.576590	-2.304246	1.281229	0.004916	0.271162
-24.971190	-2.246342	1.286234	0.004990	0.271088
-24.917858	-2.260974	1.291238	0.004980	0.271061
-25.147113	-2.272574	1.296243	0.005023	0.270776
-25.407048	-2.225540	1.301248	0.005071	0.270774
-25.559603	-2.212006	1.306253	0.005100	0.270697
-25.919174	-2.178936	1.311258	0.005167	0.270524
-25.643144	-2.228906	1.316262	0.005116	0.270525
-25.591746	-2.273340	1.321267	0.005106	0.270336
-25.837961	-2.263289	1.326272	0.005152	0.270150
-25.684427	-2.287460	1.331277	0.005124	0.270170
-25.854231	-2.311983	1.336282	0.005155	0.269872
-26.007015	-2.289246	1.341286	0.005184	0.269844
-26.007309	-2.310142	1.346291	0.005184	0.269731
-26.578408	-2.246407	1.351296	0.005290	0.269515
-26.484923	-2.262321	1.356301	0.005273	0.269521
-26.597668	-2.279215	1.361306	0.005294	0.269319
-26.793270	-2.259250	1.366310	0.005331	0.269235
-26.772087	-2.267413	1.371315	0.005327	0.269211
-27.107225	-2.265126	1.376320	0.005389	0.268895
-26.758757	-2.328325	1.381325	0.005325	0.268895
-26.720026	-2.366918	1.386330	0.005317	0.268725
-27.771384	-2.200703	1.391334	0.005513	0.268590
-27.736973	-2.204406	1.396339	0.005507	0.268603
-27.857504	-2.234980	1.401344	0.005529	0.268319
-27.880484	-2.239694	1.406349	0.005534	0.268271
-27.871287	-2.249551	1.411354	0.005532	0.268226
-28.148684	-2.243527	1.416358	0.005584	0.267986
-27.881242	-2.291164	1.421363	0.005534	0.267991
-28.481852	-2.218367	1.426368	0.005646	0.267793
-28.813297	-2.184081	1.431373	0.005708	0.267652
-28.679329	-2.209548	1.436378	0.005683	0.267646
-28.824191	-2.228837	1.441382	0.005710	0.267398
-29.366416	-2.137922	1.446387	0.005811	0.267356
-29.569346	-2.103119	1.451392	0.005849	0.267344
-29.787130	-2.113450	1.456397	0.005890	0.267073
-29.638429	-2.151091	1.461402	0.005862	0.267015
-29.459252	-2.184796	1.466406	0.005829	0.267008
-29.339549	-2.257138	1.471411	0.005807	0.266734
-30.401379	-2.063074	1.476416	0.006004	0.266738
-30.161706	-2.114996	1.481421	0.005960	0.266692
-30.440715	-2.116128	1.486426	0.006012	0.266410
-30.166131	-2.170387	1.491430	0.005961	0.266386
-30.232020	-2.174264	1.496435	0.005973	0.266299
-30.624571	-2.142245	1.501440	0.006046	0.266085
-30.171963	-2.224561	1.506445	0.005962	0.266084
-30.867486	-2.126521	1.511450	0.006092	0.265929
-31.030588	-2.127190	1.516454	0.006122	0.265763
-30.372095	-2.246627	1.521459	0.006000	0.265764
-31.176116	-2.138067	1.526464	0.006150	0.265558
-31.351324	-2.114175	1.531469	0.006182	0.265514
-31.112792	-2.159974	1.536474	0.006138	0.265501
-31.674241	-2.117300	1.541478	0.006243	0.265176
-31.771686	-2.098784	1.546483	0.006261	0.265180
-32.105725	-2.043716	1.551488	0.006323	0.265148
-31.934659	-2.127265	1.556493	0.006291	0.264861
-32.251808	-2.069906	1.561498	0.006351	0.264859
-32.351158	-2.064689	1.566502	0.006369	0.264788
-32.125352	-2.153801	1.571507	0.006327	0.264525
-32.371542	-2.109598	1.576512	0.006373	0.264521
-32.451146	-2.115314	1.581517	0.006388	0.264410
-32.826881	-2.074821	1.586522	0.006458	0.264257
-32.659421	-2.108916	1.591526	0.006427	0.264236
-32.632245	-2.148883	1.596531	0.006422	0.264044
-33.094709	-2.091525	1.601536	0.006508	0.263897
-32.646988	-2.171600	1.606541	0.006425	0.263904
-33.005730	-2.156567	1.611546	0.006492	0.263627
-33.580560	-2.057843	1.616550	0.006599	0.263595
-33.029354	-2.166323	1.621555	0.006496	0.263549
-33.350677	-2.158871	1.626560	0.006556	0.263268
-33.394909	-2.150948	1.631565	0.006565	0.263267
-34.015789	-2.057930	1.636570	0.006680	0.263157
-33.898954	-2.109583	1.641574	0.006659	0.262989
-33.985508	-2.090577	1.646579	0.006675	0.263006
-33.810353	-2.171134	1.651584	0.006642	0.262738
-33.947524	-2.163094	1.656589	0.006668	0.262644
-33.811255	-2.196635	1.661594	0.006643	0.262595
-34.351883	-2.148158	1.666598	0.006744	0.262320
-33.451827	-2.312976	1.671603	0.006576	0.262313
-34.072160	-2.241518	1.676608	0.006692	0.262084
-34.344112	-2.209710	1.681613	0.006742	0.261986
-34.282449	-2.231885	1.686618	0.006731	0.261925
-34.215994	-2.285346	1.691622	0.006719	0.261695
-34.275764	-2.272880	1.696627	0.006730	0.261704
-34.786083	-2.235179	1.701632	0.006825	0.261398
-34.572994	-2.279977	1.706637	0.006786	0.261364
-34.795143	-2.263143	1.711642	0.006827	0.261233
-35.437694	-2.177986	1.716646	0.006947	0.261056
-34.857324	-2.284517	1.721651	0.006839	0.261051
-35.485285	-2.226564	1.726656	0.006956	0.260738
-35.355170	-2.249610	1.731661	0.006932	0.260741
-35.211785	-2.300929	1.736666	0.006905	0.260600
-35.790296	-2.213089	1.741670	0.007013	0.260503
-35.788005	-2.222389	1.746675	0.007012	0.260453
-36.690377	-2.107614	1.751680	0.007181	0.260177
-36.406236	-2.160228	1.756685	0.007128	0.260172
-36.361741	-2.200949	1.761690	0.007120	0.259990
-36.501190	-2.202342	1.766694	0.007146	0.259840
-35.967659	-2.305974	1.771699	0.007046	0.259803
-36.925966	-2.181488	1.776704	0.007225	0.259524
-36.704658	-2.223967	1.781709	0.007184	0.259511
-36.853194	-2.228412	1.786714	0.007212	0.259335
-36.883558	-2.243833	1.791718	0.007217	0.259218
-36.705163	-2.289826	1.796723	0.007184	0.259142
-37.713086	-2.151488	1.801728	0.007372	0.258889
-37.391822	-2.209618	1.806733	0.007312	0.258891
-37.387500	-2.249083	1.811738	0.007312	0.258674
-37.824641	-2.186767	1.816742	0.007393	0.258577
-37.693853	-2.222317	1.821747	0.007369	0.258510
-38.434289	-2.131110	1.826752	0.007507	0.258266
-38.210507	-2.171343	1.831757	0.007465	0.258268
-38.156518	-2.214872	1.836762	0.007455	0.258079
-38.496850	-2.173270	1.841766	0.007519	0.257964
-38.453776	-2.187702	1.846771	0.007511	0.257927
-39.206227	-2.101143	1.851776	0.007651	0.257643
-38.681804	-2.198034	1.856781	0.007553	0.257634
-38.697775	-2.227348	1.861786	0.007556	0.257453
-38.957393	-2.207368	1.866790	0.007605	0.257299
-38.929244	-2.214721	1.871795	0.007600	0.257286
-38.966508	-2.262483	1.876800	0.007607	0.256978
-39.261441	-2.207107	1.881805	0.007662	0.256987
-39.116693	-2.267814	1.886810	0.007635	0.256793
-39.668727	-2.184821	1.891814	0.007738	0.256694
-39.359277	-2.254844	1.896819	0.007680	0.256616
-39.980980	-2.186846	1.901824	0.007796	0.256361
-40.051196	-2.172516	1.906829	0.007809	0.256369
-39.663141	-2.284626	1.911834	0.007737	0.256134
-40.248610	-2.192841	1.916838	0.007846	0.256050
-40.086202	-2.239073	1.921843	0.007816	0.255955
-40.284272	-2.241914	1.926848	0.007853	0.255735
-40.656849	-2.171787	1.931853	0.007922	0.255747
-40.849426	-2.173973	1.936858	0.007958	0.255536
-40.911650	-2.171435	1.941862	0.007970	0.255486
-40.467547	-2.273304	1.946867	0.007888	0.255366
-41.129255	-2.191877	1.951872	0.008011	0.255144
-40.958479	-2.222755	1.956877	0.007979	0.255145
-40.792490	-2.306212	1.961882	0.007948	0.254841
-41.570243	-2.166873	1.966886	0.008093	0.254829
-41.360548	-2.233872	1.971891	0.008054	0.254664
-41.862777	-2.170231	1.976896	0.008148	0.254506
-41.628805	-2.217469	1.981901	0.008104	0.254479
-41.957782	-2.203384	1.986906	0.008166	0.254218
-42.220237	-2.154958	1.991910	0.008215	0.254221
-41.815370	-2.261143	1.996915	0.008139	0.254035
-42.395596	-2.182254	2.001920	0.008248	0.253882

-42.755691	-2.169303	2.011917	0.008315	0.253581
-43.067962	-2.138326	2.021914	0.008373	0.253432
-43.320787	-2.120325	2.031910	0.008420	0.253271
-43.633611	-2.092659	2.041907	0.008479	0.253103
-43.384461	-2.161043	2.051904	0.008433	0.252970
-43.315886	-2.201003	2.061901	0.008420	0.252811
-43.583962	-2.183803	2.071898	0.008470	0.252629
-43.524610	-2.194970	2.081894	0.008459	0.252626
-43.785526	-2.182758	2.091891	0.008508	0.252423
-43.749168	-2.210354	2.101888	0.008501	0.252302
-43.724286	-2.213762	2.111885	0.008497	0.252307
-43.964717	-2.169098	2.121882	0.008542	0.252311
-43.691006	-2.219388	2.131878	0.008491	0.252307
-43.998446	-2.199266	2.141875	0.008549	0.252101
-44.583016	-2.110499	2.151872	0.008658	0.251998
-44.563015	-2.113512	2.161869	0.008654	0.252001
-44.301630	-2.104394	2.171866	0.008606	0.252326
-44.453081	-2.075203	2.181862	0.008634	0.252334
-44.451813	-2.075277	2.191859	0.008634	0.252334
-44.369674	-2.091505	2.201856	0.008619	0.252325
-43.675320	-2.220940	2.211853	0.008490	0.252307
-44.083616	-2.146045	2.221850	0.008566	0.252309
-43.822339	-2.192487	2.231846	0.008517	0.252314
-43.417918	-2.239622	2.241843	0.008442	0.252465
-43.240875	-2.245915	2.251840	0.008410	0.252613
-43.371508	-2.221198	2.261837	0.008434	0.252617
-43.526619	-2.191926	2.271834	0.008463	0.252622
-43.291091	-2.231854	2.281830	0.008419	0.252638
-42.976583	-2.233488	2.291827	0.008361	0.252955
-42.796289	-2.267075	2.301824	0.008328	0.252950
-43.109072	-2.208160	2.311821	0.008386	0.252960
-43.088150	-2.172461	2.321818	0.008382	0.253185
-42.838116	-2.206735	2.331814	0.008336	0.253248
-43.061686	-2.150881	2.341811	0.008378	0.253334
-42.400635	-2.231188	2.351808	0.008255	0.253562
-42.280138	-2.253109	2.361805	0.008233	0.253561
-42.496319	-2.167044	2.371802	0.008273	0.253826
-41.828992	-2.280873	2.381798	0.008149	0.253869
-41.951748	-2.222710	2.391795	0.008172	0.254072
-41.694292	-2.245556	2.401792	0.008124	0.254208
-42.192084	-2.129818	2.411789	0.008217	0.254350
-41.917006	-2.152555	2.421786	0.008166	0.254504
-41.244602	-2.236924	2.431782	0.008041	0.254719
-41.215653	-2.223738	2.441779	0.008036	0.254823
-41.053853	-2.210413	2.451776	0.008006	0.255065
-40.601096	-2.281240	2.461773	0.007922	0.255130
-40.324522	-2.279915	2.471770	0.007871	0.255422
-40.291152	-2.276313	2.481766	0.007865	0.255476
-40.226567	-2.246312	2.491763	0.007853	0.255711
-40.003530	-2.275734	2.501760	0.007811	0.255773
-39.871949	-2.253003	2.511757	0.007787	0.256037
-39.565383	-2.284292	2.521754	0.007730	0.256174
-39.586940	-2.247740	2.531750	0.007734	0.256357
-39.517694	-2.213351	2.541747	0.007722	0.256622
-39.553085	-2.181448	2.551744	0.007728	0.256764
-39.419630	-2.165984	2.561741	0.007704	0.256987
-39.064510	-2.185470	2.571738	0.007638	0.257241
-38.891128	-2.187576	2.581734	0.007606	0.257405
-38.508816	-2.219080	2.591731	0.007535	0.257618
-38.131280	-2.239110	2.601728	0.007465	0.257891
-38.053929	-2.227025	2.611725	0.007450	0.258037
-37.721414	-2.250626	2.621722	0.007389	0.258243
-37.601798	-2.225280	2.631718	0.007367	0.258506
-37.607437	-2.191038	2.641715	0.007368	0.258691
-37.471585	-2.181885	2.651712	0.007343	0.258879
-37.111387	-2.188300	2.661709	0.007276	0.259209
-37.013377	-2.174777	2.671706	0.007258	0.259383
-36.940635	-2.149115	2.681702	0.007244	0.259599
-36.424401	-2.200820	2.691699	0.007148	0.259833
-36.337193	-2.164470	2.701696	0.007132	0.260123
-36.153643	-2.159030	2.711693	0.007098	0.260338
-35.521240	-2.240204	2.721690	0.006981	0.260526
-35.979687	-2.116891	2.731686	0.007066	0.260746
-35.194976	-2.212094	2.741683	0.006920	0.261009
-35.335567	-2.149094	2.751680	0.006947	0.261216
-35.378383	-2.097319	2.761677	0.006955	0.261459
-34.998691	-2.120493	2.771674	0.006884	0.261712
-34.645821	-2.133470	2.781670	0.006819	0.261994
-34.337912	-2.147365	2.791667	0.006762	0.262226
-34.232525	-2.122670	2.801664	0.006742	0.262467
-34.292065	-2.068433	2.811661	0.006754	0.262705
-33.422392	-2.178394	2.821658	0.006592	0.262970
-33.572663	-2.101332	2.831654	0.006620	0.263243
-32.948309	-2.171547	2.841651	0.006504	0.263480
-32.843674	-2.151009	2.851648	0.006485	0.263697
-32.701776	-2.135358	2.861645	0.006458	0.263923
-31.969355	-2.216290	2.871642	0.006322	0.264209
-31.615467	-2.241078	2.881638	0.006257	0.264425
-31.390136	-2.248372	2.891635	0.006215	0.264608
-31.434329	-2.199433	2.901632	0.006223	0.264831
-31.230601	-2.178479	2.911629	0.006185	0.265147
-30.920058	-2.190114	2.921626	0.006128	0.265391
-30.761798	-2.182700	2.931622	0.006098	0.265588
-30.704236	-2.155444	2.941619	0.006088	0.265792
-30.464374	-2.147676	2.951616	0.006043	0.266071
-30.035821	-2.177646	2.961613	0.005964	0.266331
-30.110805	-2.116875	2.971610	0.005978	0.266586
-29.607155	-2.167024	2.981606	0.005884	0.266810
-29.229387	-2.198993	2.991603	0.005814	0.267009
-29.287968	-2.128434	3.001600	0.005825	0.267332
-28.864907	-2.159453	3.011597	0.005747	0.267580
-28.758381	-2.135002	3.021594	0.005727	0.267816
-28.373479	-2.159966	3.031590	0.005656	0.268059
-28.129982	-2.162021	3.041587	0.005610	0.268286
-28.310205	-2.071381	3.051584	0.005644	0.268597
-27.637446	-2.149127	3.061581	0.005519	0.268836
-27.369844	-2.155214	3.071578	0.005469	0.269065
-27.050778	-2.170949	3.081574	0.005410	0.269291
-26.895760	-2.156178	3.091571	0.005382	0.269521
-26.542454	-2.164617	3.101568	0.005316	0.269820
-26.367706	-2.152799	3.111565	0.005284	0.270053
-25.869697	-2.202804	3.121562	0.005191	0.270269
-25.505062	-2.225076	3.131558	0.005123	0.270504
-25.546246	-2.170188	3.141555	0.005131	0.270757
-25.195706	-2.191849	3.151552	0.005066	0.270981
-24.735793	-2.239559	3.161549	0.004981	0.271172
-24.635295	-2.218598	3.171546	0.004962	0.271380
-24.072760	-2.260612	3.181542	0.004858	0.271701
-23.937251	-2.251867	3.191539	0.004833	0.271878
-23.686263	-2.262806	3.201536	0.004786	0.272062
-23.595230	-2.229886	3.211533	0.004769	0.272324
-23.184314	-2.252648	3.221530	0.004693	0.272599
-23.169689	-2.214610	3.231526	0.004690	0.272814
-22.897670	-2.219730	3.241523	0.004640	0.273048
-22.610156	-2.229307	3.251520	0.004587	0.273274
-22.195348	-2.253822	3.261517	0.004510	0.273543
-22.134060	-2.228049	3.271514	0.004498	0.273737
-21.883590	-2.231471	3.281510	0.004452	0.273959
-21.703676	-2.211785	3.291507	0.004419	0.274235
-21.422247	-2.214864	3.301504	0.004366	0.274487
-21.207849	-2.210839	3.311501	0.004327	0.274713
-21.159401	-2.177697	3.321498	0.004318	0.274933
-20.385529	-2.274142	3.331494	0.004174	0.275165
-20.348459	-2.222072	3.341491	0.004167	0.275474
-20.131340	-2.228114	3.351488	0.004127	0.275649
-20.061866	-2.203641	3.361485	0.004114	0.275842
-19.557767	-2.252077	3.371482	0.004020	0.276068
-19.417992	-2.220780	3.381478	0.003995	0.276365
-19.715224	-2.119508	3.391475	0.004050	0.276611
-19.190113	-2.170689	3.401472	0.003953	0.276842
-18.709485	-2.218052	3.411469	0.003863	0.277050
-18.376359	-2.225990	3.421466	0.003801	0.277324
-18.136039	-2.218663	3.431462	0.003757	0.277589
-18.280510	-2.147803	3.441459	0.003784	0.277821
-17.648791	-2.219134	3.451456	0.003666	0.278047
-17.346044	-2.232876	3.461453	0.003610	0.278261
-17.002562	-2.239394	3.471450	0.003547	0.278551
-16.617422	-2.271406	3.481446	0.003475	0.278747
-16.584835	-2.236169	3.491443	0.003469	0.278960
-16.147145	-2.263169	3.501440	0.003388	0.279232
-15.745533	-2.292982	3.511437	0.003313	0.279455
-15.649029	-2.274484	3.521434	0.003295	0.279641
-15.272651	-2.302753	3.531430	0.003226	0.279847
-15.178480	-2.258333	3.541427	0.003208	0.280165
-14.781797	-2.290025	3.551424	0.003135	0.280373
-14.552316	-2.298922	3.561421	0.003092	0.280541
-14.127291	-2.340320	3.571418	0.003013	0.280725
-13.800107	-2.351910	3.581414	0.002952	0.280971
-13.790787	-2.319597	3.591411	0.002951	0.281145
-13.607763	-2.310720	3.601408	0.002917	0.281362
-13.374969	-2.293037	3.611405	0.002874	0.281669
-12.967694	-2.334884	3.621402	0.002798	0.281834
-12.967683	-2.295258	3.631398	0.002798	0.282036
-12.599265	-2.309832	3.641395	0.002730	0.282304
-12.460298	-2.287698	3.651392	0.002704	0.282546
-12.160993	-2.302672	3.661389	0.002649	0.282747
-11.621378	-2.361768	3.671386	0.002548	0.282946
-11.658626	-2.296786	3.681382	0.002555	0.283243
-11.407645	-2.303698	3.691379	0.002509	0.283440
-11.328795	-2.277828	3.701376	0.002494	0.283644
-10.741153	-2.339602	3.711373	0.002385	0.283873
-10.683463	-2.291755	3.721370	0.002375	0.284169
-10.541728	-2.279939	3.731366	0.002348	0.284360
-9.988250	-2.345355	3.741363	0.002246	0.284538
-9.843091	-2.314280	3.751360	0.002219	0.284829
-9.707701	-2.294178	3.761357	0.002194	0.285055
-9.384799	-2.312367	3.771354	0.002134	0.285260
-9.281777	-2.285287	3.781350	0.002115	0.285492
-9.155761	-2.256935	3.791347	0.002091	0.285750
-8.825522	-2.275709	3.801344	0.002030	0.285958
-8.525032	-2.291957	3.811341	0.001974	0.286152
-8.047128	-2.338632	3.821338	0.001886	0.286354
-7.527421	-2.370057	3.831334	0.001789	0.286672
-7.538120	-2.335709	3.841331	0.001791	0.286834
-7.358410	-2.331593	3.851328	0.001758	0.287019
-6.971857	-2.345989	3.861325	0.001686	0.287300
-6.830194	-2.326928	3.871322	0.001660	0.287524
-6.677232	-2.313039	3.881318	0.001632	0.287733
-6.410689	-2.315625	3.891315	0.001582	0.287963
-6.390832	-2.263939	3.901312	0.001579	0.288240
-6.366112	-2.221929	3.911309	0.001574	0.288472
-5.986669	-2.247336	3.921306	0.001504	0.288690
-5.782398	-2.239115	3.931302	0.001466	0.288916
-5.561984	-2.217902	3.941299	0.001425	0.289222
-5.396798	-2.200354	3.951296	0.001394	0.289459
-5.055088	-2.215849	3.961293	0.001331	0.289691
-4.663249	-2.243366	3.971290	0.001258	0.289909
-4.356270	-2.251134	3.981286	0.001201	0.290148
-4.443116	-2.170138	3.991283	0.001218	0.290472
-4.156859	-2.182244	4.001280	0.001164	0.290670
-4.149647	-2.138877	4.011277	0.001163	0.290891
-4.500092	-2.017231	4.021274	0.001229	0.291178
-3.700640	-2.113619	4.031270	0.001080	0.291421
-3.514501	-2.089769	4.041267	0.001046	0.291706
-3.453113	-2.046651	4.051264	0.001034	0.291974
-3.143052	-2.048763	4.061261	0.000977	0.292242
-3.057452	-2.008414	4.071258	0.000961	0.292518
-3.157181	-1.930228	4.081254	0.000980	0.292814
-2.683461	-1.960998	4.091251	0.000892	0.293087
-2.672135	-1.906051	4.101248	0.000890	0.293367
-2.364940	-1.904278	4.111245	0.000833	0.293650
-2.596358	-1.799586	4.121242	0.000876	0.293958
-2.224537	-1.802590	4.131238	0.000807	0.294275
-2.271128	-1.732801	4.141235	0.000816	0.294575
-2.110021	-1.695588	4.151232	0.000786	0.294901
-2.300212	-1.589053	4.161229	0.000821	0.295253
-2.149478	-1.547759	4.171226	0.000793	0.295588
-2.181980	-1.478512	4.181222	0.000800	0.295897
-2.203030	-1.401350	4.191219	0.000804	0.296255
-1.718300	-1.417704	4.201216	0.000714	0.296604
-1.704047	-1.350993	4.211213	0.000711	0.296941
-1.766722	-1.257641	4.221210	0.000723	0.297340
-1.533430	-1.219024	4.231206	0.000680	0.297733
-1.310947	-1.182698	4.241203	0.000638	0.298105
-1.494984	-1.073304	4.251200	0.000673	0.298472
-1.222671	-1.041700	4.261197	0.000622	0.298864
-1.104286	-0.969862	4.271194	0.000600	0.299315
-1.138200	-0.887789	4.281190	0.000607	0.299681
-0.983020	-0.832197	4.291187	0.000578	0.300085
-0.893346	-0.749246	4.301184	0.000561	0.300562
-0.680983	-0.716521	4.311181	0.000522	0.300904
-0.368609	-0.690918	4.321178	0.000464	0.301299
-0.513021	-0.562124	4.331174	0.000491	0.301790
-0.284749	-0.521712	4.341171	0.000449	0.302182
-0.328266	-0.415845	4.351168	0.000457	0.302650
-0.137731	-0.355800	4.361165	0.000422	0.303101
-0.070592	-0.274079	4.371162	0.000409	0.303548
-0.119716	-0.161489	4.381158	0.000418	0.304041
0.038698	-0.093255	4.391155	0.000389	0.304502
0.063745	0.006990	4.401152	0.000385	0.304999
0.000000	0.111299	4.411149	0.000397	0.305437

-0.083169	0.396141	4.416154	0.000412	0.306712
-0.021054	0.940944	4.421158	0.000400	0.309324
0.353027	1.703673	4.426163	0.000330	0.313186
0.779559	2.746702	4.431168	0.000250	0.318320
1.061362	4.099371	4.436173	0.000197	0.324639
1.370768	5.748559	4.441178	0.000138	0.332152
1.721517	7.681536	4.446182	0.000072	0.340739
1.976989	9.942287	4.451187	0.000023	0.350399
2.545687	12.450177	4.456192	-0.000085	0.361020
3.107247	15.276004	4.461197	-0.000191	0.372569
3.268843	18.506301	4.466202	-0.000223	0.385019
3.657734	22.025161	4.471206	-0.000298	0.398279
4.313953	25.835747	4.476211	-0.000422	0.412307
4.793081	30.031057	4.481216	-0.000514	0.427069
4.973569	34.617323	4.486221	-0.000551	0.442440
5.478190	39.498695	4.491226	-0.000648	0.458412
5.798567	44.761332	4.496230	-0.000711	0.474908
6.106681	50.365057	4.501235	-0.000772	0.491847
6.765387	56.262808	4.506240	-0.000898	0.509237
7.174924	62.518912	4.511245	-0.000978	0.526914
7.671464	69.088223	4.516250	-0.001075	0.544890
8.168268	75.971052	4.521254	-0.001172	0.563097
8.458287	83.191105	4.526259	-0.001230	0.581481
9.174506	90.621323	4.531264	-0.001369	0.599992
9.085555	98.460293	4.536269	-0.001357	0.618567
9.968018	106.374214	4.541274	-0.001526	0.637165
10.464900	114.599083	4.546278	-0.001624	0.655769
10.587900	123.102510	4.551283	-0.001653	0.674314
11.177622	131.699777	4.556288	-0.001768	0.692732
11.549303	140.517366	4.561293	-0.001843	0.711042
12.575177	149.374131	4.566298	-0.002039	0.729200
15.735922	158.017256	4.571302	-0.002633	0.747238
18.284141	166.926582	4.576307	-0.003114	0.765145
18.465672	176.381388	4.581312	-0.003154	0.782873
18.529313	185.913861	4.586317	-0.003171	0.800310
19.547394	195.350437	4.591322	-0.003367	0.817505
21.939731	204.621553	4.596326	-0.003819	0.834478
23.236058	214.135026	4.601331	-0.004066	0.851195
24.058720	223.756703	4.606336	-0.004225	0.867629
24.963272	233.372433	4.611341	-0.004400	0.883771
25.594658	243.050665	4.616346	-0.004524	0.899647
26.586428	252.657977	4.621350	-0.004715	0.915234
27.092193	262.315785	4.626355	-0.004815	0.930505
28.024165	271.896984	4.631360	-0.004995	0.945527
29.171573	281.401173	4.636365	-0.005214	0.960253
30.171936	290.918496	4.641370	-0.005407	0.974738
31.561141	300.342652	4.646374	-0.005671	0.988973
31.702030	309.930573	4.651379	-0.005704	1.002927
33.093419	319.256499	4.656384	-0.005969	1.016627
33.935171	328.631539	4.661389	-0.006132	1.030078
34.964402	337.932771	4.666394	-0.006329	1.043299
35.698116	347.245160	4.671398	-0.006472	1.056298
36.344358	356.513052	4.676403	-0.006598	1.069058
36.881977	365.754262	4.681408	-0.006704	1.081607
36.795781	375.051848	4.686413	-0.006694	1.093943
37.710209	384.110217	4.691418	-0.006870	1.106055
38.653714	393.130317	4.696422	-0.007052	1.117992
38.965500	402.213472	4.701427	-0.007116	1.129744
39.538050	411.220298	4.706432	-0.007228	1.141335
40.239641	420.157595	4.711437	-0.007364	1.152750
40.992736	429.037244	4.716442	-0.007510	1.163991
42.472744	437.763356	4.721446	-0.007791	1.175089
43.111431	446.611339	4.726451	-0.007916	1.186056
44.310347	455.332860	4.731456	-0.008145	1.196884
45.506781	464.018551	4.736461	-0.008373	1.207571
46.043382	472.811713	4.741466	-0.008479	1.218158
47.260036	481.463278	4.746470	-0.008711	1.228623
47.728684	490.193098	4.751475	-0.008804	1.238943
48.500160	498.856769	4.756480	-0.008953	1.249159
49.127269	507.502301	4.761485	-0.009075	1.259244
49.729626	516.138552	4.766490	-0.009193	1.269232
50.886390	524.663306	4.771494	-0.009414	1.279123
51.646412	533.225555	4.776499	-0.009561	1.288903
52.405451	541.786252	4.781504	-0.009708	1.298608
52.584855	550.434007	4.786509	-0.009746	1.308229
53.370581	558.984239	4.791514	-0.009898	1.317784
54.354559	567.408086	4.796518	-0.010087	1.327169
55.018777	575.872398	4.801523	-0.010216	1.336473
55.413527	584.375360	4.806528	-0.010295	1.345706
56.033918	592.816185	4.811533	-0.010416	1.354850
56.800182	601.226829	4.816538	-0.010564	1.363926
57.668352	609.628121	4.821542	-0.010731	1.372949
57.940496	618.089123	4.826547	-0.010787	1.381872
58.730393	626.478793	4.831552	-0.010940	1.390753
59.265395	634.869722	4.836557	-0.011045	1.399535
60.158189	643.200405	4.841562	-0.011216	1.408260
60.871038	651.565310	4.846566	-0.011354	1.416937
61.712704	659.881353	4.851571	-0.011516	1.425532
61.846183	668.345690	4.856576	-0.011547	1.434106
62.881908	676.592113	4.861581	-0.011745	1.442561
63.609761	684.925433	4.866586	-0.011886	1.451002
64.252087	693.267121	4.871590	-0.012010	1.459388
65.280392	701.533988	4.876595	-0.012207	1.467715
66.389614	709.824503	4.881600	-0.012419	1.476031
66.751199	718.169774	4.886605	-0.012492	1.484233
66.644760	726.605761	4.891610	-0.012477	1.492404
67.280583	734.874305	4.896614	-0.012601	1.500486
67.646957	743.204194	4.901619	-0.012675	1.508541
68.005114	751.516259	4.906624	-0.012747	1.516535
68.941048	759.703347	4.911629	-0.012926	1.524458
69.851425	767.935629	4.916634	-0.013101	1.532378
70.651842	776.173179	4.921638	-0.013255	1.540245
71.088706	784.470333	4.926643	-0.013342	1.548072
71.807063	792.715638	4.931648	-0.013481	1.555854
72.394385	800.948708	4.936653	-0.013596	1.563566
73.270801	809.168248	4.941658	-0.013764	1.571271
74.390512	817.347247	4.946662	-0.013978	1.578937
74.586568	825.668556	4.951667	-0.014020	1.586559
74.901566	833.968779	4.956672	-0.014084	1.594142
75.280114	842.218741	4.961677	-0.014159	1.601654
76.040954	850.422074	4.966682	-0.014306	1.609143
76.983533	858.606354	4.971686	-0.014487	1.616607
77.158454	866.886277	4.976691	-0.014525	1.624012
77.636585	875.170809	4.981696	-0.014619	1.631430
78.197124	883.357694	4.986701	-0.014729	1.638740
78.899700	891.517647	4.991706	-0.014865	1.646013
79.461116	899.742075	4.996710	-0.014975	1.653291
80.073554	907.912170	5.001715	-0.015094	1.660497
80.652184	916.126748	5.006720	-0.015207	1.667705
81.045920	924.345043	5.011725	-0.015285	1.674859
81.900300	932.475575	5.016730	-0.015450	1.681971
82.491846	940.690319	5.021734	-0.015565	1.689089
82.918326	948.907881	5.026739	-0.015650	1.696156
83.447237	957.109573	5.031744	-0.015754	1.703195
83.844833	965.314235	5.036749	-0.015833	1.710189
84.254827	973.514975	5.041754	-0.015914	1.717154
84.743096	981.683639	5.046758	-0.016011	1.724073
85.363141	989.836092	5.051763	-0.016131	1.730968
85.862198	998.043960	5.056768	-0.016229	1.737866
86.432684	1006.182660	5.061773	-0.016341	1.744688
87.240581	1014.332116	5.066778	-0.016497	1.751524
87.821482	1022.502500	5.071782	-0.016610	1.758320
87.781246	1030.742216	5.076787	-0.016608	1.765068
88.944849	1038.828549	5.081792	-0.016830	1.771817
89.463451	1046.989336	5.086797	-0.016931	1.778520
89.842546	1055.182170	5.091802	-0.017007	1.785206
90.290577	1063.393069	5.096806	-0.017096	1.791889
90.628109	1071.576244	5.101811	-0.017164	1.798512
90.713166	1079.765723	5.106816	-0.017185	1.805084
91.259160	1087.896037	5.111821	-0.017292	1.811642
91.800974	1096.034211	5.116826	-0.017398	1.818182
92.453588	1104.132807	5.121830	-0.017525	1.824680
92.673097	1112.323494	5.126835	-0.017571	1.831175
92.870339	1120.528656	5.131840	-0.017613	1.837656
93.128336	1128.662305	5.136845	-0.017666	1.844065
93.818269	1136.762840	5.141850	-0.017800	1.850478
94.156332	1144.929375	5.146854	-0.017868	1.856878
94.511750	1153.069576	5.151859	-0.017939	1.863237
95.029579	1161.211628	5.156864	-0.018041	1.869595
95.115900	1169.389758	5.161869	-0.018062	1.875909
95.848083	1177.457284	5.166874	-0.018204	1.882192
96.167070	1185.607811	5.171878	-0.018268	1.888469
96.252185	1193.784155	5.176883	-0.018289	1.894718
96.621301	1201.914521	5.181888	-0.018363	1.900944
97.349855	1209.974520	5.186893	-0.018504	1.907138
97.636996	1218.146266	5.191898	-0.018563	1.913346
98.005002	1226.281283	5.196902	-0.018637	1.919514
98.311861	1234.406686	5.201907	-0.018699	1.925649
98.989667	1242.502779	5.206912	-0.018830	1.931784
99.316895	1250.645317	5.211917	-0.018896	1.937895
99.808382	1258.738609	5.216922	-0.018993	1.943968
100.502543	1266.853261	5.221926	-0.019128	1.950061
100.887915	1274.955569	5.226931	-0.019205	1.956091
101.293602	1283.076997	5.231936	-0.019285	1.962118
101.878341	1291.155797	5.236941	-0.019399	1.968116
102.471379	1299.264070	5.241946	-0.019515	1.974118
102.646404	1307.420745	5.246950	-0.019553	1.980090
102.845913	1315.561824	5.251955	-0.019595	1.986037
103.068926	1323.718810	5.256960	-0.019642	1.991979
103.269689	1331.836689	5.261965	-0.019684	1.997873
103.585140	1339.938236	5.266970	-0.019748	2.003750
104.649143	1347.948131	5.271974	-0.019952	2.009624
104.908500	1356.089939	5.276979	-0.020005	2.015490
105.309464	1364.217194	5.281984	-0.020085	2.021343
105.607072	1372.349247	5.286989	-0.020146	2.027171
105.956686	1380.482539	5.291994	-0.020216	2.032989
106.441380	1388.574260	5.296998	-0.020311	2.038775
106.624939	1396.678758	5.302003	-0.020351	2.044522
107.436113	1404.745210	5.307008	-0.020507	2.050292
107.573932	1412.880580	5.312013	-0.020538	2.056023
107.715573	1421.028184	5.317018	-0.020569	2.061748
108.061989	1429.134059	5.322022	-0.020639	2.067449
108.689340	1437.180593	5.327027	-0.020761	2.073121
108.625904	1445.375792	5.332032	-0.020754	2.078810
108.904198	1453.442189	5.337037	-0.020811	2.084430
109.654152	1461.482745	5.342042	-0.020956	2.090064
110.087193	1469.594090	5.347046	-0.021042	2.095699
110.476277	1477.672647	5.352051	-0.021120	2.101293
110.725952	1485.811107	5.357056	-0.021171	2.106898
111.786493	1493.831517	5.362061	-0.021374	2.112489
112.102716	1501.948287	5.367066	-0.021438	2.118056
112.801651	1509.986209	5.372070	-0.021573	2.123593
113.570184	1518.033296	5.377075	-0.021722	2.129128
113.953608	1526.171883	5.382080	-0.021798	2.134673
114.017209	1534.317872	5.387085	-0.021815	2.140178
114.295490	1542.425416	5.392090	-0.021872	2.145663
114.578401	1550.536976	5.397094	-0.021930	2.151137
114.885916	1558.613626	5.402099	-0.021993	2.156577
115.072948	1566.726798	5.407104	-0.022033	2.162015
115.128862	1574.853542	5.412109	-0.022048	2.167436
115.122999	1582.995658	5.417114	-0.022052	2.172848
115.660077	1591.038793	5.422118	-0.022158	2.178232
116.106322	1599.073148	5.427123	-0.022246	2.183589
116.561704	1607.188099	5.432128	-0.022336	2.188986
116.781949	1615.275208	5.437133	-0.022382	2.194330
117.253017	1623.320861	5.442138	-0.022475	2.199657
117.381137	1631.433611	5.447142	-0.022504	2.204983
117.596120	1639.517660	5.452147	-0.022549	2.210285
117.972319	1647.600398	5.457152	-0.022624	2.215588
118.202517	1655.699152	5.462157	-0.022672	2.220876
118.663137	1663.745367	5.467162	-0.022763	2.226138
119.383871	1671.784699	5.472166	-0.022903	2.231407
119.914177	1679.846405	5.477171	-0.023006	2.236660
120.534956	1687.906743	5.482176	-0.023127	2.241909
120.795997	1696.020375	5.487181	-0.023181	2.247146
121.198276	1704.112629	5.492186	-0.023261	2.252371
121.470383	1712.221178	5.497190	-0.023317	2.257582
121.647100	1720.310084	5.502195	-0.023355	2.262759
121.820955	1728.450946	5.507200	-0.023393	2.267958
122.383586	1736.521275	5.512205	-0.023503	2.273135
122.924710	1744.530804	5.517210	-0.023608	2.278259
123.304819	1752.592995	5.522214	-0.023684	2.283390
123.649498	1760.665392	5.527219	-0.023754	2.288514
124.050752	1768.749289	5.532224	-0.023834	2.293638
124.241510	1776.841870	5.537229	-0.023874	2.298737
124.584420	1784.895890	5.542234	-0.023943	2.303815
124.813336	1793.014894	5.547238	-0.023991	2.308912
124.922160	1801.107194	5.552243	-0.024017	2.313970
125.636935	1809.129410	5.557248	-0.024155	2.319026
125.771486	1817.199544	5.562253	-0.024185	2.324051
126.062589	1825.286948	5.567258	-0.024244	2.329089
126.337893	1833.382366	5.572262	-0.024301	2.334119
126.635000	1841.442338	5.577267	-0.024361	2.339119
126.922863	1849.523824	5.582272	-0.024420	2.344121
126.976035	1857.647924	5.587277	-0.024435	2.349118
127.358767	1865.683077	5.592282	-0.024512	2.354077
127.930638	1873.699253	5.597286	-0.024623	2.359031
127.917590	1881.787293	5.602291	-0.024626	2.363969
128.470998	1889.839019	5.607296	-0.024734	2.368921
128.689826	1897.924766	5.612301	-0.024780	2.373856
128.845353	1906.012112	5.617306	-0.024814	2.378777
129.422945	1914.036880	5.622310	-0.024927	2.383684
129.883930	1922.079826	5.627315	-0.025018	2.388582
130.226480	1930.172907	5.632320	-0.025087	2.393491
130.238075	1938.274890	5.637325	-0.025094	2.398368
130.596097	1946.300052	5.642330	-0.025166	2.403217
130.661185	1954.440634	5.647334	-0.025183	2.408102
131.139377	1962.447686	5.652339	-0.025278	2.412930
131.608227	1970.518939	5.657344	-0.025370	2.417786
131.751352	1978.586744	5.662349	-0.025402	2.422604
131.963645	1986.683308	5.667354	-0.025447	2.427435
132.145599	1994.806510	5.672358	-0.025486	2.432270
132.237765	2002.871399	5.677363	-0.025508	2.437054
132.941142	2010.841769	5.682368	-0.025644	2.441820
132.655225	2018.985994	5.687373	-0.025596	2.446602
133.077489	2027.006385	5.692378	-0.025680	2.451358
133.475657	2035.073735	5.697382	-0.025759	2.456129
133.454125	2043.141798	5.702387	-0.025760	2.460859
133.858083	2051.178952	5.707392	-0.025841	2.465595
134.298867	2059.218697	5.712397	-0.025928	2.470326
134.820273	2067.240784	5.717402	-0.026030	2.475044
134.848559	2075.353111	5.722406	-0.026040	2.479767
135.000124	2083.393513	5.727411	-0.026074	2.484449
135.321038	2091.481758	5.732416	-0.026139	2.489163
135.410827	2099.578459	5.737421	-0.026161	2.493855
135.765167	2107.615420	5.742426	-0.026232	2.498524
135.681182	2115.727129	5.747430	-0.026221	2.503194
135.477305	2123.833954	5.752435	-0.026189	2.507844
136.399431	2131.783769	5.757440	-0.026365	2.512479
136.856296	2139.798774	5.762445	-0.026456	2.517108
137.136007	2147.843828	5.767450	-0.026513	2.521732
136.842373	2155.995941	5.772454	-0.026463	2.526367
137.212660	2164.027627	5.777459	-0.026537	2.530973
137.460346	2172.072130	5.782464	-0.026589	2.535570
137.776386	2180.130581	5.787469	-0.026653	2.540171
138.045550	2188.161374	5.792474	-0.026708	2.544744
138.459200	2196.221393	5.797478	-0.026790	2.549336
138.513818	2204.284369	5.802483	-0.026805	2.553896
138.890961	2212.325845	5.807488	-0.026881	2.558458
139.271239	2220.365700	5.812493	-0.026957	2.563012
139.417165	2228.453012	5.817498	-0.026989	2.567567
139.262687	2236.596618	5.822502	-0.026966	2.572125
139.339450	2244.635096	5.827507	-0.026985	2.576632
140.208010	2252.600988	5.832512	-0.027152	2.581146
140.347228	2260.647397	5.837517	-0.027183	2.585646
140.369749	2268.786339	5.842522	-0.027192	2.590181
140.929951	2276.895582	5.847526	-0.027302	2.594730
140.995405	2284.897687	5.852531	-0.027319	2.599176
141.215300	2292.936964	5.857536	-0.027365	2.603647
141.277360	2300.991955	5.862541	-0.027382	2.608107
141.884434	2308.980247	5.867546	-0.027500	2.612560
142.149872	2317.042622	5.872550	-0.027555	2.617024
142.309577	2325.104048	5.877555	-0.027590	2.621471
142.928554	2333.108845	5.882560	-0.027710	2.625912
142.630097	2341.261598	5.887565	-0.027660	2.630363
142.926590	2349.291167	5.892570	-0.027720	2.634780
143.466479	2357.279568	5.897574	-0.027826	2.639183
143.509831	2365.327793	5.902579	-0.027839	2.643578
143.850227	2373.403691	5.907584	-0.027907	2.648001
144.126715	2381.452663	5.912589	-0.027964	2.652397
144.124370	2389.525429	5.917594	-0.027969	2.656781
144.737763	2397.535039	5.922598	-0.028088	2.661164
145.016129	2405.575222	5.927603	-0.028145	2.665533
145.446447	2413.637275	5.932608	-0.028230	2.669918
145.615470	2421.704941	5.937613	-0.028267	2.674281
145.829370	2429.750223	5.942618	-0.028312	2.678628
146.188637	2437.764193	5.947622	-0.028384	2.682960
146.577818	2445.783027	5.952627	-0.028462	2.687290
146.706884	2453.881728	5.957632	-0.028491	2.691639
147.183051	2461.920991	5.962637	-0.028585	2.695971
147.349045	2469.981926	5.967642	-0.028621	2.700288
147.586912	2478.024882	5.972646	-0.028670	2.704593
147.354938	2486.150042	5.977651	-0.028632	2.708904
147.610207	2494.206166	5.982656	-0.028685	2.713204
148.005281	2502.184173	5.987661	-0.028764	2.717464
148.146745	2510.232632	5.992666	-0.028795	2.721738
148.239740	2518.341593	5.997670	-0.028818	2.726034
148.557398	2526.345922	6.002675	-0.028882	2.730283
148.889171	2534.393205	6.007680	-0.028949	2.734549
148.869111	2542.471071	6.012685	-0.028950	2.738801
149.350893	2550.440272	6.017690	-0.029045	2.743022
149.563543	2558.517247	6.022694	-0.029090	2.747276
149.845466	2566.589078	6.027699	-0.029147	2.751525
150.406469	2574.645121	6.032704	-0.029257	2.755776
150.482454	2582.681274	6.037709	-0.029276	2.759980
150.657943	2590.686791	6.042714	-0.029314	2.764168
151.385068	2598.683614	6.047718	-0.029455	2.768379
151.704991	2606.740574	6.052723	-0.029519	2.772589
151.807653	2614.849451	6.057728	-0.029544	2.776807
152.119678	2622.868938	6.062733	-0.029607	2.780985
152.258164	2630.933754	6.067738	-0.029638	2.785169
152.776969	2638.957662	6.072742	-0.029740	2.789350
152.893529	2646.995677	6.077747	-0.029766	2.793506
153.377492	2655.030617	6.082752	-0.029862	2.797677
153.427268	2663.088500	6.087757	-0.029876	2.801828
153.938699	2671.089923	6.092762	-0.029976	2.805970
154.096120	2679.201315	6.097766	-0.030011	2.810142
154.165056	2687.252832	6.102771	-0.030029	2.814272
154.265864	2695.307638	6.107776	-0.030053	2.818399
154.456088	2703.339494	6.112781	-0.030093	2.822514
154.805228	2711.357453	6.117786	-0.030164	2.826625
155.060242	2719.449062	6.122790	-0.030216	2.830762
155.233291	2727.485332	6.127795	-0.030254	2.834860
155.463567	2735.503990	6.132800	-0.030302	2.838947
155.859705	2743.499879	6.137805	-0.030381	2.843025
155.922412	2751.572249	6.142810	-0.030397	2.847117
156.413846	2759.620774	6.147814	-0.030494	2.851216
156.650529	2767.661408	6.152819	-0.030543	2.855290
156.902496	2775.695194	6.157824	-0.030595	2.859356
157.064481	2783.737783	6.162829	-0.030631	2.863415
157.274409	2791.798856	6.167834	-0.030675	2.867481
157.669608	2799.838636	6.172838	-0.030754	2.871540
157.859722	2807.875879	6.177843	-0.030794	2.875581
158.275925	2815.895214	6.182848	-0.030877	2.879620
158.701038	2823.891298	6.187853	-0.030961	2.883642
159.097745	2831.934525	6.192858	-0.031040	2.887680
159.319952	2840.035195	6.197862	-0.031087	2.891732
159.685188	2848.065400	6.202867	-0.031160	2.895750
160.022679	2856.106937	6.207872	-0.031228	2.899768
160.048939	2864.161945	6.212877	-0.031238	2.903768
160.521784	2872.188249	6.217882	-0.031331	2.907774
160.977184	2880.258752	6.222886	-0.031421	2.911795
160.904363	2888.354639	6.227891	-0.031413	2.915794
160.951456	2896.389433	6.232896	-0.031426	2.919764
161.499753	2904.318111	6.237901	-0.031534	2.923704
161.863498	2912.362612	6.242906	-0.031607	2.927685
162.350216	2920.422455	6.247910	-0.031702	2.931675
162.595507	2928.443864	6.252915	-0.031753	2.935628
162.693668	2936.502630	6.257920	-0.031777	2.939585
162.901335	2944.543684	6.262925	-0.031820	2.943534
163.059539	2952.592145	6.267930	-0.031855	2.947479
163.379502	2960.675324	6.272934	-0.031920	2.951445
163.329465	2968.728702	6.277939	-0.031916	2.955370
163.573438	2976.726021	6.282944	-0.031966	2.959279
163.993577	2984.721263	6.287949	-0.032049	2.963191
164.295815	2992.733705	6.292954	-0.032111	2.967099
164.528593	3000.830747	6.297958	-0.032159	2.971040
164.630437	3008.866478	6.302963	-0.032184	2.974939
164.835264	3016.925550	6.307968	-0.032227	2.978850
165.038172	3024.948994	6.312973	-0.032270	2.982738
165.260792	3032.988015	6.317978	-0.032316	2.986630
165.805949	3041.005511	6.322982	-0.032423	2.990523
165.702520	3049.081393	6.327987	-0.032409	2.994405
166.155097	3057.067771	6.332992	-0.032498	2.998268
166.230241	3065.138295	6.337997	-0.032517	3.002146
166.478388	3073.166934	6.343002	-0.032569	3.006009
166.865126	3081.180159	6.348006	-0.032646	3.009866
166.656558	3089.272503	6.353011	-0.032612	3.013726
167.011293	3097.319812	6.358016	-0.032683	3.017588
167.161936	3105.331831	6.363021	-0.032717	3.021418
167.401572	3113.333529	6.368026	-0.032766	3.025242
167.999771	3121.361411	6.373030	-0.032883	3.029092
168.331208	3129.377362	6.378035	-0.032950	3.032918
168.632201	3137.453554	6.383040	-0.033011	3.036766
168.802784	3145.483350	6.388045	-0.033048	3.040581
169.324265	3153.438992	6.393050	-0.033150	3.044373
169.421731	3161.565528	6.398054	-0.033173	3.048221
169.764079	3169.592773	6.403059	-0.033242	3.052028
170.022188	3177.649616	6.408064	-0.033295	3.055841
169.974341	3185.706086	6.413069	-0.033292	3.059633
170.256714	3193.701683	6.418074	-0.033349	3.063409
170.538134	3201.789835	6.423078	-0.033407	3.067223
170.715897	3209.823059	6.428083	-0.033445	3.071002
171.095662	3217.867387	6.433088	-0.033521	3.074790
171.370337	3225.861949	6.438093	-0.033577	3.078546
171.660934	3233.876809	6.443098	-0.033637	3.082308
171.716260	3241.954565	6.448102	-0.033652	3.086082
171.766358	3249.987862	6.453107	-0.033667	3.089832
172.545817	3257.969001	6.458112	-0.033817	3.093587
172.443545	3266.039623	6.463117	-0.033803	3.097337
172.497296	3274.069781	6.468122	-0.033818	3.101071
173.215600	3282.056795	6.473126	-0.033957	3.104812
173.333883	3290.111425	6.478131	-0.033984	3.108552
173.668674	3298.172078	6.483136	-0.034052	3.112300
174.116834	3306.177787	6.488141	-0.034140	3.116023
174.368896	3314.192154	6.493146	-0.034192	3.119737
174.288130	3322.267374	6.498150	-0.034182	3.123458
174.476282	3330.292586	6.503155	-0.034223	3.127165
174.932158	3338.316818	6.508160	-0.034313	3.130879
175.056849	3346.374508	6.513165	-0.034341	3.134589
175.158599	3354.429823	6.518170	-0.034365	3.138293
175.929409	3362.370678	6.523174	-0.034514	3.141970
175.864756	3370.490431	6.528179	-0.034507	3.145686
176.319307	3378.477988	6.533184	-0.034597	3.149361
176.413231	3386.549879	6.538189	-0.034619	3.153054
176.657199	3394.556196	6.543194	-0.034670	3.156720
177.056238	3402.606631	6.548198	-0.034749	3.160408
177.376767	3410.557813	6.553203	-0.034814	3.164044
177.577077	3418.638657	6.558208	-0.034856	3.167728
177.869976	3426.680725	6.563213	-0.034916	3.171395
178.000120	3434.733767	6.568218	-0.034946	3.175055
178.230417	3442.783611	6.573222	-0.034994	3.178714
178.597267	3450.760513	6.578227	-0.035067	3.182342
178.388590	3458.898851	6.583232	-0.035033	3.186013
178.525960	3466.911831	6.588237	-0.035064	3.189639
178.589121	3474.959213	6.593242	-0.035081	3.193272
178.691162	3482.975988	6.598246	-0.035105	3.196890
178.981866	3490.945484	6.603251	-0.035164	3.200490
179.526471	3498.922513	6.608256	-0.035271	3.204101
179.958930	3506.971787	6.613261	-0.035357	3.207735
180.336334	3515.005767	6.618266	-0.035432	3.211355
180.399234	3523.109165	6.623270	-0.035449	3.214989
180.451768	3531.112500	6.628275	-0.035464	3.218574
180.818181	3539.142997	6.633280	-0.035537	3.222180
180.793499	3547.216486	6.638285	-0.035538	3.225785
181.376297	3555.198463	6.643290	-0.035651	3.229371
181.711212	3563.268533	6.648294	-0.035719	3.232981
181.775097	3571.296293	6.653299	-0.035736	3.236557
181.877579	3579.318077	6.658304	-0.035760	3.240128
182.249926	3587.277574	6.663309	-0.035835	3.243678
182.338735	3595.347331	6.668314	-0.035856	3.247262
182.831180	3603.380351	6.673318	-0.035953	3.250842
183.321055	3611.369087	6.678323	-0.036049	3.254399
183.100940	3619.500397	6.683328	-0.036014	3.257985
183.698264	3627.460227	6.688333	-0.036130	3.261526
184.080367	3635.465356	6.693338	-0.036206	3.265073
184.476982	3643.508514	6.698342	-0.036285	3.268634
184.249107	3651.622883	6.703347	-0.036248	3.272197
184.930535	3659.614152	6.708352	-0.036380	3.275739
185.238670	3667.573546	6.713357	-0.036442	3.279248
185.215125	3675.644121	6.718362	-0.036443	3.282788
185.667028	3683.718116	6.723366	-0.036533	3.286345
185.978092	3691.682756	6.728371	-0.036596	3.289845
186.421202	3699.731775	6.733376	-0.036683	3.293383
186.408657	3707.792033	6.738381	-0.036686	3.296904
186.478566	3715.846225	6.743386	-0.036704	3.300422
187.009377	3723.841990	6.748390	-0.036808	3.303929
186.612143	3731.930152	6.753395	-0.036739	3.307436
187.058515	3739.960250	6.758400	-0.036828	3.310947
187.386374	3747.958068	6.763405	-0.036894	3.314435
187.795849	3755.938400	6.768410	-0.036975	3.317916
187.944610	3764.005553	6.773414	-0.037008	3.321420
188.217906	3771.963387	6.778419	-0.037064	3.324878
188.475307	3780.024187	6.783424	-0.037117	3.328376
188.385033	3788.136287	6.788429	-0.037105	3.331879
189.145512	3796.049960	6.793434	-0.037252	3.335326
189.248643	3804.144472	6.798438	-0.037277	3.338821
189.490323	3812.123571	6.803443	-0.037327	3.342269
189.874371	3820.171684	6.808448	-0.037403	3.345748
189.956043	3828.226088	6.813453	-0.037424	3.349215
190.306869	3836.237470	6.818458	-0.037494	3.352670
190.431614	3844.320896	6.823462	-0.037523	3.356143
190.636509	3852.337949	6.828467	-0.037566	3.359588
190.860975	3860.332441	6.833472	-0.037613	3.363020
191.012573	3868.397087	6.838477	-0.037646	3.366475
191.662142	3876.366651	6.843482	-0.037772	3.369906
191.967297	3884.421507	6.848486	-0.037834	3.373356
192.037210	3892.474466	6.853491	-0.037852	3.376793
192.315990	3900.471351	6.858496	-0.037909	3.380210
192.736318	3908.475953	6.863501	-0.037993	3.383632
192.993369	3916.520607	6.868506	-0.038046	3.387062
193.079884	3924.602219	6.873510	-0.038067	3.390498
193.138552	3932.660609	6.878515	-0.038083	3.393919
193.408226	3940.665581	6.883520	-0.038138	3.397322
193.671532	3948.693274	6.888525	-0.038193	3.400731
193.846376	3956.651059	6.893530	-0.038230	3.404104
194.307766	3964.701790	6.898534	-0.038321	3.407523
194.248668	3972.765144	6.903539	-0.038315	3.410925
194.310649	3980.801814	6.908544	-0.038332	3.414317
194.714226	3988.820560	6.913549	-0.038412	3.417710
194.859872	3996.841799	6.918554	-0.038445	3.421091
195.078526	4004.872326	6.923558	-0.038491	3.424476
195.666684	4012.853822	6.928563	-0.038605	3.427849
196.081870	4020.942823	6.933568	-0.038688	3.431259
196.142170	4028.961736	6.938573	-0.038704	3.434623
196.309472	4036.952019	6.943578	-0.038740	3.437975
196.591907	4044.982403	6.948582	-0.038798	3.441345
196.531605	4052.985760	6.953587	-0.038792	3.444688
196.958222	4061.005125	6.958592	-0.038876	3.448052
197.366940	4069.093157	6.963597	-0.038958	3.451440
197.602355	4077.073232	6.968602	-0.039007	3.454774
198.088710	4085.098241	6.973606	-0.039102	3.458132
198.317198	4093.126178	6.978611	-0.039150	3.461479
198.873924	4101.124588	6.983616	-0.039259	3.464822
198.998785	4109.208417	6.988621	-0.039287	3.468182
199.339422	4117.238126	6.993626	-0.039356	3.471524
199.814530	4125.246710	6.998630	-0.039449	3.474858
200.159304	4133.220969	7.003635	-0.039519	3.478171
200.309512	4141.282192	7.008640	-0.039552	3.481509
200.463259	4149.316922	7.013645	-0.039586	3.484834
200.272187	4157.380369	7.018650	-0.039555	3.488156
200.616817	4165.414432	7.023654	-0.039625	3.491480
200.680086	4173.423526	7.028659	-0.039641	3.494782
201.093534	4181.444101	7.033664	-0.039724	3.498096
201.184609	4189.491363	7.038669	-0.039746	3.501408
200.852701	4197.545737	7.043674	-0.039689	3.504706
201.678863	4205.514095	7.048678	-0.039848	3.508003
201.794791	4213.567914	7.053683	-0.039875	3.511309
201.948620	4221.586738	7.058688	-0.039909	3.514599
202.127841	4229.614969	7.063693	-0.039947	3.517890
202.477872	4237.636617	7.068698	-0.040017	3.521181
202.686146	4245.631173	7.073702	-0.040061	3.524453
202.413410	4253.725992	7.078707	-0.040016	3.527748
202.939708	4261.723782	7.083712	-0.040119	3.531025
203.160592	4269.746121	7.088717	-0.040165	3.534300
203.170472	4277.757849	7.093722	-0.040172	3.537560
203.336055	4285.846358	7.098726	-0.040208	3.540854
203.627546	4293.778195	7.103731	-0.040267	3.544085
203.919844	4301.827410	7.108736	-0.040327	3.547361
204.087516	4309.906882	7.113741	-0.040363	3.550641
204.225598	4317.952226	7.118746	-0.040394	3.553905
204.318819	4325.985310	7.123750	-0.040417	3.557158
204.587982	4333.949034	7.128755	-0.040472	3.560386
204.718846	4341.953060	7.133760	-0.040501	3.563624
204.618519	4350.044661	7.138765	-0.040488	3.566886
204.796986	4358.004011	7.143770	-0.040526	3.570101
205.204192	4366.052599	7.148774	-0.040607	3.573356
205.676877	4374.038601	7.153779	-0.040700	3.576584
205.928309	4382.049434	7.158784	-0.040752	3.579813
206.072496	4390.083429	7.163789	-0.040784	3.583045
206.500452	4398.112888	7.168794	-0.040869	3.586280
206.950155	4406.123258	7.173798	-0.040958	3.589506
206.661079	4414.204524	7.178803	-0.040909	3.592735
207.340714	4422.214110	7.183808	-0.041041	3.595961
207.624684	4430.183919	7.188813	-0.041099	3.599157
207.613469	4438.223359	7.193818	-0.041102	3.602369
208.019950	4446.265862	7.198822	-0.041183	3.605592
208.280544	4454.263803	7.203827	-0.041236	3.608789
208.777965	4462.315913	7.208832	-0.041334	3.612012
208.993670	4470.369326	7.213837	-0.041380	3.615225
209.253675	4478.356115	7.218842	-0.041433	3.618409
209.624655	4486.425320	7.223846	-0.041507	3.621627
209.596936	4494.419814	7.228851	-0.041507	3.624800
209.789441	4502.484933	7.233856	-0.041548	3.628005
210.038699	4510.555558	7.238861	-0.041600	3.631211
210.215009	4518.517210	7.243866	-0.041638	3.634369
210.523891	4526.551376	7.248870	-0.041700	3.637557
210.840141	4534.561395	7.253875	-0.041764	3.640732
211.208647	4542.528971	7.258880	-0.041838	3.643889
211.482599	4550.587909	7.263885	-0.041894	3.647077
211.625769	4558.616550	7.268890	-0.041926	3.650247
211.882078	4566.697375	7.273894	-0.041979	3.653437
211.909038	4574.683294	7.278899	-0.041989	3.656581
211.961910	4582.710026	7.283904	-0.042004	3.659739
212.343482	4590.739782	7.288909	-0.042080	3.662904
212.683830	4598.713504	7.293914	-0.042149	3.666044
212.784169	4606.767473	7.298918	-0.042173	3.669205
213.312621	4614.778788	7.303923	-0.042276	3.672359
213.432163	4622.821559	7.308928	-0.042304	3.675512
213.671358	4630.829502	7.313933	-0.042353	3.678651
213.692380	4638.846635	7.318938	-0.042362	3.681785
214.097065	4646.870666	7.323942	-0.042443	3.684929
214.234218	4654.889639	7.328947	-0.042473	3.688062
214.339480	4662.959334	7.333952	-0.042498	3.691211
214.683999	4670.965163	7.338957	-0.042568	3.694339
214.878750	4678.957608	7.343962	-0.042609	3.697454
215.128953	4687.046305	7.348966	-0.042661	3.700606
215.452051	4694.997223	7.353971	-0.042726	3.703704
215.775114	4703.051497	7.358976	-0.042791	3.706839
215.728650	4711.131899	7.363981	-0.042788	3.709972
215.854021	4719.160072	7.368986	-0.042816	3.713086
216.327032	4727.213801	7.373990	-0.042909	3.716217
216.479127	4735.173984	7.378995	-0.042943	3.719301
216.557197	4743.198274	7.384000	-0.042963	3.722405
216.873787	4751.204636	7.389005	-0.043027	3.725505
217.000867	4759.219789	7.394010	-0.043055	3.728602
217.294698	4767.287406	7.399014	-0.043115	3.731720
217.355872	4775.307438	7.404019	-0.043132	3.734811
217.528343	4783.340670	7.409024	-0.043169	3.737908
217.899151	4791.327935	7.414029	-0.043243	3.740989
218.155418	4799.263568	7.419034	-0.043296	3.744045
218.385013	4807.364513	7.424038	-0.043344	3.747162
218.386583	4815.411327	7.429043	-0.043349	3.750249
218.628027	4823.424081	7.434048	-0.043399	3.753327
219.065473	4831.440733	7.439053	-0.043486	3.756408
219.089657	4839.448988	7.444058	-0.043496	3.759474
219.382642	4847.470337	7.449062	-0.043555	3.762548
219.540552	4855.490624	7.454067	-0.043590	3.765617
219.615600	4863.513783	7.459072	-0.043609	3.768682
220.066418	4871.564797	7.464077	-0.043698	3.771764
220.265984	4879.554850	7.469082	-0.043740	3.774814
220.779201	4887.558822	7.474086	-0.043841	3.777874
220.586847	4895.640784	7.479091	-0.043810	3.780945
220.773367	4903.611944	7.484096	-0.043850	3.783980
221.026221	4911.661921	7.489101	-0.043903	3.787045
221.301477	4919.651325	7.494106	-0.043959	3.790084
221.461160	4927.696411	7.499110	-0.043994	3.793139
221.826825	4935.746077	7.504115	-0.044067	3.796198
221.969774	4943.714642	7.509120	-0.044099	3.799219
222.195437	4951.763794	7.514125	-0.044146	3.802270
222.372062	4959.766335	7.519130	-0.044184	3.805300
222.963526	4967.779854	7.524134	-0.044299	3.808340
223.123843	4975.831166	7.529139	-0.044334	3.811383
223.275957	4983.815783	7.534144	-0.044368	3.814398
223.806480	4991.897523	7.539149	-0.044472	3.817456
223.774263	4999.874640	7.544154	-0.044471	3.820459
223.925687	5007.914267	7.549158	-0.044504	3.823487
224.224572	5015.978953	7.554163	-0.044565	3.826526
224.347808	5024.010753	7.559168	-0.044593	3.829546
224.401200	5032.049767	7.564173	-0.044608	3.832564
224.574292	5040.058929	7.569178	-0.044645	3.835572
224.590692	5048.082858	7.574182	-0.044654	3.838579
224.930844	5056.079070	7.579187	-0.044722	3.841581
225.095070	5064.076128	7.584192	-0.044758	3.844577
225.426352	5072.106514	7.589197	-0.044825	3.847587
225.493755	5080.154498	7.594202	-0.044842	3.850595
225.842886	5088.182450	7.599206	-0.044912	3.853599
225.891210	5096.202375	7.604211	-0.044927	3.856592
226.089685	5104.219917	7.609216	-0.044969	3.859584
226.348499	5112.228572	7.614221	-0.045022	3.862572
226.516141	5120.237849	7.619226	-0.045058	3.865556
226.800069	5128.287087	7.624230	-0.045116	3.868555
226.936006	5136.350263	7.629235	-0.045147	3.871554
227.231920	5144.403134	7.634240	-0.045207	3.874550
227.429189	5152.413211	7.639245	-0.045249	3.877525
227.726512	5160.332914	7.644250	-0.045309	3.880467
227.942332	5168.342587	7.649254	-0.045355	3.883438
227.901883	5176.381231	7.654259	-0.045352	3.886413
228.183202	5184.352394	7.659264	-0.045410	3.889366
228.292339	5192.452536	7.664269	-0.045435	3.892362
228.286713	5200.459582	7.669274	-0.045439	3.895318
228.602548	5208.442334	7.674278	-0.045503	3.898270
228.873469	5216.509981	7.679283	-0.045559	3.901250
228.985763	5224.441686	7.684288	-0.045585	3.904175
229.233928	5232.536584	7.689293	-0.045636	3.907160
229.169995	5240.518019	7.694298	-0.045629	3.910094
229.683686	5248.573626	7.699302	-0.045730	3.913065
229.857714	5256.614758	7.704307	-0.045768	3.916022
230.394696	5264.543013	7.709312	-0.045873	3.918943
230.462713	5272.625121	7.714317	-0.045891	3.921908
230.605319	5280.586682	7.719322	-0.045922	3.924828
231.062086	5288.640772	7.724326	-0.046013	3.927786
231.319978	5296.680923	7.729331	-0.046066	3.930733
231.506415	5304.717323	7.734336	-0.046106	3.933675
231.739794	5312.762492	7.739341	-0.046154	3.936619
232.139719	5320.709266	7.744346	-0.046234	3.939528
232.501342	5328.776241	7.749350	-0.046306	3.942477
232.624895	5336.784663	7.754355	-0.046334	3.945399
233.071987	5344.826083	7.759360	-0.046423	3.948336
232.941796	5352.928306	7.764365	-0.046404	3.951283
233.132751	5360.863766	7.769370	-0.046444	3.954173
233.630824	5368.927776	7.774374	-0.046542	3.957113
233.882414	5376.904775	7.779379	-0.046594	3.960014
233.911363	5384.913662	7.784384	-0.046605	3.962921
234.189467	5392.950310	7.789389	-0.046662	3.965840
234.574284	5400.947125	7.794394	-0.046738	3.968745
234.800102	5409.026945	7.799398	-0.046786	3.971675
234.739716	5417.035630	7.804403	-0.046779	3.974571
234.827622	5425.079042	7.809408	-0.046801	3.977481
235.349548	5433.087000	7.814413	-0.046903	3.980384
235.499621	5441.011251	7.819418	-0.046936	3.983247
235.772019	5449.136105	7.824422	-0.046992	3.986183
236.100677	5457.084983	7.829427	-0.047059	3.989054
236.198349	5465.160239	7.834432	-0.047082	3.991965
236.463258	5473.171713	7.839437	-0.047136	3.994853
236.742458	5481.171916	7.844442	-0.047193	3.997736
237.039308	5489.226696	7.849446	-0.047254	4.000636
237.151334	5497.167634	7.854451	-0.047280	4.003490
237.361782	5505.237501	7.859456	-0.047324	4.006391
237.526798	5513.233620	7.864461	-0.047360	4.009261
237.474301	5521.293786	7.869466	-0.047355	4.012149
237.791512	5529.302175	7.874470	-0.047420	4.015023
238.041294	5537.294306	7.879475	-0.047471	4.017887
238.171078	5545.341536	7.884480	-0.047501	4.020767
238.340649	5553.338559	7.889485	-0.047537	4.023628
238.434664	5561.395585	7.894490	-0.047560	4.026507
238.728154	5569.377435	7.899494	-0.047620	4.029360
238.745463	5577.478508	7.904499	-0.047628	4.032249
239.087110	5585.474127	7.909504	-0.047697	4.035104
239.385649	5593.473142	7.914509	-0.047758	4.037957
239.228276	5601.481997	7.919514	-0.047733	4.040804
239.255082	5609.467025	7.924518	-0.047743	4.043644
239.404714	5617.517189	7.929523	-0.047776	4.046507
239.741410	5625.489968	7.934528	-0.047844	4.049343
239.812151	5633.609754	7.939533	-0.047863	4.052225
240.131261	5641.547268	7.944538	-0.047927	4.055045
240.280282	5649.622261	7.949542	-0.047960	4.057908
240.402249	5657.612488	7.954547	-0.047988	4.060739
240.608792	5665.585217	7.959552	-0.048031	4.063563
240.810891	5673.675074	7.964557	-0.048074	4.066427
240.858497	5681.660773	7.969562	-0.048088	4.069249
241.203653	5689.739104	7.974566	-0.048158	4.072107
241.289328	5697.723808	7.979571	-0.048179	4.074925
241.864134	5705.713458	7.984576	-0.048291	4.077751
241.991474	5713.755498	7.989581	-0.048320	4.080586
242.241855	5721.711030	7.994586	-0.048371	4.083391
242.517808	5729.800655	7.999590	-0.048428	4.086242
242.551619	5737.820097	8.004595	-0.048439	4.089062
242.788904	5745.834782	8.009600	-0.048489	4.091881
243.451068	5753.828465	8.014605	-0.048617	4.094698
243.598399	5761.869805	8.019610	-0.048650	4.097521
243.918722	5769.902480	8.024614	-0.048715	4.100342
244.084831	5777.907956	8.029619	-0.048751	4.103150
244.208336	5785.952849	8.034624	-0.048779	4.105968
244.533545	5794.004028	8.039629	-0.048844	4.108790
244.622760	5801.995434	8.044634	-0.048866	4.111585
244.972180	5810.000583	8.049638	-0.048936	4.114387
245.006481	5817.992703	8.054643	-0.048948	4.117178
245.120194	5825.990671	8.059648	-0.048974	4.119971
245.367323	5834.021947	8.064653	-0.049025	4.122774
245.427062	5842.059053	8.069658	-0.049042	4.125576
245.670687	5850.080953	8.074662	-0.049092	4.128372
245.821921	5858.152413	8.079667	-0.049125	4.131183
246.157093	5866.111794	8.084672	-0.049193	4.133956
245.840018	5874.217027	8.089677	-0.049139	4.136768
245.981468	5882.149856	8.094682	-0.049170	4.139525
246.426651	5890.182552	8.099686	-0.049258	4.142318
246.508591	5898.171720	8.104691	-0.049279	4.145090
246.895260	5906.193428	8.109696	-0.049356	4.147875
246.806659	5914.299107	8.114701	-0.049345	4.150681
246.851976	5922.227432	8.119706	-0.049358	4.153426
247.588592	5930.289531	8.124710	-0.049501	4.156224
247.532042	5938.235138	8.129715	-0.049495	4.158969
247.849136	5946.299615	8.134720	-0.049559	4.161759
247.845824	5954.281931	8.139725	-0.049564	4.164514
248.089403	5962.354642	8.144730	-0.049614	4.167301
248.291518	5970.357370	8.149734	-0.049657	4.170062
248.264998	5978.391017	8.154739	-0.049657	4.172829
248.694240	5986.389949	8.159744	-0.049742	4.175588
249.125161	5994.403375	8.164749	-0.049828	4.178350
249.459941	6002.444799	8.169754	-0.049895	4.181119
249.610757	6010.403692	8.174758	-0.049928	4.183855
249.400158	6018.537091	8.179763	-0.049894	4.186645
249.920200	6026.469937	8.184768	-0.049996	4.189373
250.156909	6034.596602	8.189773	-0.050046	4.192162
250.260875	6042.594852	8.194778	-0.050070	4.194904
250.487364	6050.587768	8.199782	-0.050117	4.197643
251.038655	6058.559334	8.204787	-0.050225	4.200378
250.757584	6066.580282	8.209792	-0.050178	4.203117
250.891105	6074.615122	8.214797	-0.050208	4.205865
251.402685	6082.570270	8.219802	-0.050308	4.208587
251.780096	6090.677127	8.224806	-0.050384	4.211358
251.850356	6098.642241	8.229811	-0.050402	4.214076
252.069966	6106.736771	8.234816	-0.050448	4.216837
252.523613	6114.686869	8.239821	-0.050537	4.219550
252.623395	6122.705259	8.244826	-0.050561	4.222281
253.129241	6130.719324	8.249830	-0.050660	4.225013
253.279808	6138.794399	8.254835	-0.050694	4.227759
253.461100	6146.788311	8.259840	-0.050733	4.230477
253.459696	6154.846645	8.264845	-0.050737	4.233213
253.951514	6162.811667	8.269850	-0.050834	4.235920
253.998313	6170.863301	8.274854	-0.050848	4.238651
254.176641	6178.888371	8.279859	-0.050886	4.241372
254.143307	6186.847815	8.284864	-0.050885	4.244067
254.396029	6194.935401	8.289869	-0.050937	4.246807
254.468976	6202.888883	8.294874	-0.050956	4.249497
254.758708	6210.941520	8.299878	-0.051015	4.252222
255.059044	6218.958440	8.304883	-0.051076	4.254933
255.153252	6226.952605	8.309888	-0.051099	4.257632
255.449438	6234.965261	8.314893	-0.051159	4.260338
255.678883	6242.944369	8.319898	-0.051207	4.263030
256.094498	6251.034340	8.324902	-0.051290	4.265759
256.315921	6259.022225	8.329907	-0.051336	4.268451
256.248116	6267.107255	8.334912	-0.051329	4.271170
256.482229	6275.054891	8.339917	-0.051377	4.273845
256.411292	6283.084265	8.344922	-0.051369	4.276542
256.735846	6291.083159	8.349926	-0.051435	4.279232
256.841788	6299.123232	8.354931	-0.051460	4.281931
256.900814	6307.101783	8.359936	-0.051476	4.284607
257.134994	6315.127950	8.364941	-0.051524	4.287300
257.297930	6323.111839	8.369946	-0.051560	4.289976
257.709814	6331.189976	8.374950	-0.051642	4.292684
257.748444	6339.194980	8.379955	-0.051654	4.295362
257.841463	6347.244618	8.384960	-0.051677	4.298054
258.429784	6355.235434	8.389965	-0.051791	4.300730
258.081670	6363.234253	8.394970	-0.051731	4.303397
258.556680	6371.286076	8.399974	-0.051825	4.306088
258.671325	6379.272170	8.404979	-0.051852	4.308753
258.746491	6387.362689	8.409984	-0.051871	4.311450
259.106851	6395.296144	8.414989	-0.051943	4.314095
259.075103	6403.356449	8.419994	-0.051942	4.316778
259.354193	6411.320812	8.424998	-0.051999	4.319430
259.352134	6419.379106	8.430003	-0.052004	4.322109
259.459489	6427.344693	8.435008	-0.052029	4.324756
259.834825	6435.423207	8.440013	-0.052104	4.327442
259.723809	6443.406120	8.445018	-0.052089	4.330090
260.023823	6451.462792	8.450022	-0.052150	4.332764
260.120798	6459.482452	8.455027	-0.052173	4.335423
260.411195	6467.494816	8.460032	-0.052232	4.338079
260.860776	6475.461190	8.465037	-0.052321	4.340720
261.138180	6483.428242	8.470042	-0.052378	4.343358
261.477877	6491.516849	8.475046	-0.052446	4.346034
261.718663	6499.511789	8.480051	-0.052496	4.348678
262.087868	6507.538008	8.485056	-0.052570	4.351331
262.286861	6515.639484	8.490061	-0.052612	4.354006
261.841962	6523.648177	8.495066	-0.052534	4.356644
261.842187	6531.615377	8.500070	-0.052539	4.359270
262.241036	6539.615333	8.505075	-0.052619	4.361908
262.564929	6547.593524	8.510080	-0.052684	4.364536
262.551114	6555.657273	8.515085	-0.052687	4.367189
262.913165	6563.609351	8.520090	-0.052759	4.369806
262.826510	6571.705420	8.525094	-0.052748	4.372466
262.839612	6579.706277	8.530099	-0.052756	4.375093
263.521388	6587.672848	8.535104	-0.052888	4.377713
263.740997	6595.767617	8.540109	-0.052934	4.380369
263.968373	6603.701457	8.545114	-0.052982	4.382972
263.786618	6611.767824	8.550118	-0.052953	4.385613
263.903976	6619.749807	8.555123	-0.052980	4.388227
264.208977	6627.826292	8.560128	-0.053042	4.390871
264.673307	6635.755554	8.565133	-0.053133	4.393467
265.217296	6643.754989	8.570138	-0.053240	4.396085
265.583659	6651.784950	8.575143	-0.053313	4.398710
265.688155	6659.848947	8.580147	-0.053338	4.401343
265.839366	6667.822133	8.585152	-0.053371	4.403945
266.119709	6675.862742	8.590157	-0.053428	4.406568
266.222911	6683.914529	8.595162	-0.053453	4.409192
266.580528	6691.943324	8.600167	-0.053524	4.411809
266.678609	6699.983822	8.605171	-0.053548	4.414426
266.600934	6708.021837	8.610176	-0.053538	4.417039
267.349209	6716.001385	8.615181	-0.053683	4.419638
266.866852	6724.053474	8.620186	-0.053598	4.422250
266.968447	6732.122732	8.625191	-0.053622	4.424871
267.142317	6740.149337	8.630195	-0.053660	4.427476
267.060432	6748.177538	8.635200	-0.053650	4.430079
267.659604	6756.204376	8.640205	-0.053766	4.432683
267.844363	6764.196060	8.645210	-0.053806	4.435273
267.777095	6772.224758	8.650215	-0.053799	4.437871
267.999721	6780.205969	8.655219	-0.053845	4.440454
268.419489	6788.172228	8.660224	-0.053928	4.443032
268.514106	6796.244308	8.665229	-0.053951	4.445641
268.685927	6804.234821	8.670234	-0.053988	4.448222
269.015672	6812.300093	8.675239	-0.054055	4.450827
269.228193	6820.309151	8.680243	-0.054100	4.453411
269.457038	6828.302354	8.685248	-0.054147	4.455989
269.106998	6836.379982	8.690253	-0.054087	4.458590
269.003848	6844.428364	8.695258	-0.054073	4.461181
269.397344	6852.340965	8.700263	-0.054152	4.463729
269.411728	6860.431868	8.705267	-0.054159	4.466331
269.545306	6868.390705	8.710272	-0.054189	4.468890
270.095942	6876.474511	8.715277	-0.054297	4.471489
270.144138	6884.396300	8.720282	-0.054311	4.474033
270.498157	6892.479883	8.725287	-0.054382	4.476628
270.792822	6900.387994	8.730291	-0.054442	4.479165
270.852167	6908.485172	8.735296	-0.054458	4.481761
271.285160	6916.445538	8.740301	-0.054544	4.484312
270.966845	6924.553279	8.745306	-0.054490	4.486906
271.166626	6932.549482	8.750311	-0.054532	4.489466
271.211867	6940.634369	8.755315	-0.054546	4.492051
271.532790	6948.555283	8.760320	-0.054611	4.494583
271.691519	6956.596251	8.765325	-0.054645	4.497152
271.756226	6964.546190	8.770330	-0.054663	4.499690
272.277088	6972.603776	8.775335	-0.054765	4.502263
272.369295	6980.608614	8.780339	-0.054787	4.504815
272.066722	6988.687351	8.785344	-0.054736	4.507388
272.453461	6996.666538	8.790349	-0.054813	4.509931
272.504050	7004.667938	8.795354	-0.054828	4.512478
273.116632	7012.650930	8.800359	-0.054947	4.515019
273.090750	7020.682010	8.805363	-0.054947	4.517573
273.205453	7028.696460	8.810368	-0.054974	4.520120
273.877017	7036.669280	8.815373	-0.055104	4.522654
273.840856	7044.687639	8.820378	-0.055102	4.525198
274.392696	7052.727165	8.825383	-0.055210	4.527750
274.415795	7060.760969	8.830387	-0.055219	4.530297
274.561548	7068.766570	8.835392	-0.055252	4.532834
274.765525	7076.836321	8.840397	-0.055295	4.535390
274.946766	7084.777713	8.845402	-0.055334	4.537904
275.190829	7092.854322	8.850407	-0.055384	4.540459
275.169248	7100.854008	8.855411	-0.055385	4.542988
275.411999	7108.878555	8.860416	-0.055436	4.545524
275.803554	7116.881680	8.865421	-0.055514	4.548052
275.662037	7124.918647	8.870426	-0.055493	4.550588
275.987695	7132.931454	8.875431	-0.055558	4.553117
275.964332	7141.006140	8.880435	-0.055559	4.555662
276.436201	7148.914937	8.885440	-0.055652	4.558155
276.589651	7156.974493	8.890445	-0.055686	4.560693
276.598084	7164.901756	8.895450	-0.055692	4.563188
276.764007	7172.953353	8.900455	-0.055728	4.565721
276.863836	7181.025856	8.905459	-0.055752	4.568259
277.113702	7189.031294	8.910464	-0.055804	4.570774
277.494812	7197.069214	8.915469	-0.055880	4.573299
277.343616	7205.057464	8.920474	-0.055857	4.575806
277.585000	7213.083420	8.925479	-0.055907	4.578324
277.887877	7221.100572	8.930483	-0.055969	4.580837
278.053586	7229.048308	8.935488	-0.056005	4.583328
278.402300	7237.098127	8.940493	-0.056075	4.585849
278.569882	7245.124580	8.945498	-0.056111	4.588362
279.019184	7253.156009	8.950503	-0.056200	4.590874
278.848459	7261.177207	8.955507	-0.056173	4.593382
279.042795	7269.201935	8.960512	-0.056214	4.595889
279.115247	7277.154701	8.965517	-0.056233	4.598373
279.359524	7285.215086	8.970522	-0.056284	4.600889
279.703849	7293.156413	8.975527	-0.056353	4.603366
279.850419	7301.228189	8.980531	-0.056385	4.605883
279.660968	7309.292738	8.985536	-0.056355	4.608396
279.951219	7317.331749	8.990541	-0.056414	4.610900
280.163749	7325.210981	8.995546	-0.056459	4.613352
280.481612	7333.325032	9.000551	-0.056523	4.615877
280.323485	7341.324630	9.005555	-0.056499	4.618364
280.852237	7349.321425	9.010560	-0.056603	4.620849
281.295225	7357.292811	9.015565	-0.056690	4.623325
281.305984	7365.349243	9.020570	-0.056697	4.625826
281.727377	7373.337600	9.025575	-0.056781	4.628304
281.866106	7381.411602	9.030579	-0.056812	4.630808
282.249377	7389.363584	9.035584	-0.056888	4.633272
282.311949	7397.459672	9.040589	-0.056905	4.635780
282.310891	7405.381718	9.045594	-0.056910	4.638232
282.391405	7413.493569	9.050599	-0.056930	4.640742
282.584830	7421.411774	9.055603	-0.056971	4.643191
282.534753	7429.499189	9.060608	-0.056967	4.645690
282.700168	7437.515958	9.065613	-0.057003	4.648167
283.124940	7445.557145	9.070618	-0.057087	4.650649
283.322085	7453.528005	9.075623	-0.057129	4.653109
283.300220	7461.623718	9.080627	-0.057130	4.655605
283.061258	7469.552562	9.085632	-0.057091	4.658049
283.603668	7477.621440	9.090637	-0.057197	4.660535
283.914106	7485.536543	9.095642	-0.057260	4.662972
284.385477	7493.557479	9.100647	-0.057353	4.665440
284.548628	7501.599887	9.105651	-0.057388	4.667914
284.743893	7509.621265	9.110656	-0.057430	4.670380
285.312192	7517.711423	9.115661	-0.057541	4.672865
285.326907	7525.707753	9.120666	-0.057549	4.675321
285.372173	7533.703259	9.125671	-0.057562	4.677774
285.564833	7541.682882	9.130675	-0.057603	4.680222
285.771747	7549.699385	9.135680	-0.057647	4.682680
286.024676	7557.735572	9.140685	-0.057699	4.685142
286.025781	7565.735745	9.145690	-0.057704	4.687592
286.195089	7573.740532	9.150695	-0.057741	4.690042
286.318026	7581.767826	9.155699	-0.057769	4.692498
286.294286	7589.763213	9.160704	-0.057770	4.694943
286.774052	7597.825627	9.165709	-0.057864	4.697407
286.625793	7605.805554	9.170714	-0.057842	4.699844
286.885218	7613.871796	9.175719	-0.057895	4.702307
287.039362	7621.807921	9.180723	-0.057929	4.704728
286.912237	7629.917092	9.185728	-0.057911	4.707201
286.526632	7637.976164	9.190733	-0.057844	4.709658
286.889603	7645.912307	9.195738	-0.057917	4.712076
287.346772	7653.911547	9.200743	-0.058007	4.714511
287.453867	7661.974023	9.205747	-0.058032	4.716964
287.318332	7669.911246	9.210752	-0.058012	4.719379
287.628787	7678.008803	9.215757	-0.058075	4.721840
288.043374	7685.898525	9.220762	-0.058157	4.724237
288.112581	7694.037324	9.225767	-0.058175	4.726709
288.475675	7701.990717	9.230771	-0.058248	4.729122
288.800584	7710.030442	9.235776	-0.058314	4.731561
288.850917	7718.044994	9.240781	-0.058328	4.733991
288.914928	7726.044199	9.245786	-0.058345	4.736415
288.869376	7734.073638	9.250791	-0.058342	4.738848
289.196077	7742.087984	9.255795	-0.058408	4.741273
289.538861	7750.005544	9.260800	-0.058477	4.743669
289.811018	7758.169392	9.265805	-0.058532	4.746137
290.076648	7766.131979	9.270810	-0.058587	4.748544
290.001633	7774.300854	9.275815	-0.058578	4.751012
290.297186	7782.187207	9.280819	-0.058638	4.753393
290.720135	7790.202780	9.285824	-0.058722	4.755811
290.583915	7798.253350	9.290829	-0.058702	4.758240
290.585225	7806.262504	9.295834	-0.058707	4.760655
291.038980	7814.226660	9.300839	-0.058797	4.763054
290.808757	7822.285591	9.305843	-0.058759	4.765482
290.940258	7830.261466	9.310848	-0.058789	4.767883
291.588544	7838.335287	9.315853	-0.058915	4.770310
291.676645	7846.323221	9.320858	-0.058936	4.772712
291.776293	7854.409868	9.325863	-0.058960	4.775143
291.876592	7862.378035	9.330867	-0.058984	4.777536
292.216472	7870.354651	9.335872	-0.059052	4.779931
292.612128	7878.398385	9.340877	-0.059131	4.782344
292.280579	7886.402561	9.345882	-0.059074	4.784746
292.514867	7894.479999	9.350887	-0.059123	4.787167
292.668313	7902.473242	9.355891	-0.059157	4.789562
292.428702	7910.542462	9.360896	-0.059117	4.791979
292.943326	7918.473670	9.365901	-0.059218	4.794352
293.270736	7926.472688	9.370906	-0.059284	4.796745
293.749883	7934.465012	9.375911	-0.059379	4.799133
293.755751	7942.593984	9.380915	-0.059385	4.801563
294.071225	7950.402492	9.385920	-0.059449	4.803895
294.474182	7958.606023	9.390925	-0.059529	4.806343
294.422483	7966.535338	9.395930	-0.059525	4.808710
294.666636	7974.586273	9.400935	-0.059575	4.811111
294.703190	7982.623037	9.405939	-0.059587	4.813507
294.869292	7990.054571	9.410944	-0.059623	4.815721
294.996249	7994.822402	9.415949	-0.059649	4.817141

295.137843	7997.257123	9.420954	-0.059677	4.817866
295.553786	7998.554013	9.425959	-0.059755	4.818250
295.424024	7998.988479	9.430963	-0.059731	4.818380
295.369583	8000.133736	9.435968	-0.059722	4.818721
295.693636	8000.169356	9.440973	-0.059782	4.818731
295.970006	8000.152986	9.445978	-0.059834	4.818725
295.871507	8000.195749	9.450983	-0.059815	4.818738
296.027530	8000.154762	9.455987	-0.059844	4.818725
296.202979	8000.147579	9.460992	-0.059877	4.818722
296.337833	8000.144066	9.465997	-0.059902	4.818721
296.401006	8000.111321	9.471002	-0.059913	4.818711
296.415508	8000.167073	9.476007	-0.059916	4.818727
296.379501	8000.169748	9.481011	-0.059909	4.818728
296.409227	8000.172222	9.486016	-0.059915	4.818729
296.730293	8000.155380	9.491021	-0.059974	4.818723
296.549338	8000.103762	9.496026	-0.059941	4.818708
296.603288	8000.108645	9.501031	-0.059951	4.818709
296.796645	8000.164604	9.506035	-0.059986	4.818725
296.623907	8000.145596	9.511040	-0.059954	4.818720
296.716141	8000.178233	9.516045	-0.059971	4.818729
296.941760	8000.110882	9.521050	-0.060013	4.818709
296.876771	8000.153028	9.526055	-0.060001	4.818721
296.893397	8000.133313	9.531059	-0.060004	4.818715
296.882126	8000.119531	9.536064	-0.060002	4.818711
296.281450	8000.209301	9.541069	-0.059890	4.818740
296.501702	8000.185918	9.546074	-0.059931	4.818733
296.751916	8000.217445	9.551079	-0.059977	4.818741
296.558989	8000.173012	9.556083	-0.059941	4.818728
296.900114	8000.188934	9.561088	-0.060005	4.818732
296.945222	8000.212576	9.566093	-0.060013	4.818739
296.799840	8000.169804	9.571098	-0.059986	4.818727
296.794026	8000.206421	9.576103	-0.059985	4.818738
296.955037	8000.169694	9.581107	-0.060015	4.818726
296.969574	8000.140515	9.586112	-0.060017	4.818717
297.067850	8000.191056	9.591117	-0.060035	4.818732
296.741911	8000.177414	9.596122	-0.059975	4.818729
296.850662	8000.176712	9.601127	-0.059995	4.818728
297.223215	8000.180456	9.606131	-0.060064	4.818728
297.299207	8000.115371	9.611136	-0.060078	4.818709
297.189637	8000.199933	9.616141	-0.060058	4.818734
297.116174	8000.170670	9.621146	-0.060044	4.818726
297.424736	8000.200853	9.626151	-0.060101	4.818733
297.408061	8000.174418	9.631155	-0.060098	4.818726
297.071007	8000.162729	9.636160	-0.060035	4.818723
297.280263	8000.182195	9.641165	-0.060074	4.818728
297.280812	8000.167516	9.646170	-0.060074	4.818724
297.439422	8000.210447	9.651175	-0.060103	4.818736
297.487506	8000.170167	9.656179	-0.060112	4.818724
297.328175	8000.190127	9.661184	-0.060083	4.818731
297.260821	8000.227000	9.666189	-0.060070	4.818742
297.451601	8000.203238	9.671194	-0.060105	4.818734
297.397676	8000.213023	9.676199	-0.060095	4.818737
297.184859	8000.237536	9.681203	-0.060056	4.818745
296.959162	8000.236719	9.686208	-0.060013	4.818746
297.143659	8000.264254	9.691213	-0.060048	4.818753
297.173022	8000.227927	9.696218	-0.060053	4.818743
297.318256	8000.245521	9.701223	-0.060080	4.818747
297.614834	8000.211588	9.706227	-0.060135	4.818736
297.554027	8000.166759	9.711232	-0.060124	4.818723
297.212572	8000.267208	9.716237	-0.060060	4.818754
297.709254	8000.210689	9.721242	-0.060152	4.818735
297.884472	8000.224475	9.726247	-0.060185	4.818739
297.662550	8000.200637	9.731251	-0.060144	4.818733
297.693987	8000.170628	9.736256	-0.060149	4.818723
297.930998	8000.209327	9.741261	-0.060193	4.818734
298.041177	8000.182430	9.746266	-0.060214	4.818726
297.675860	8000.266842	9.751271	-0.060146	4.818752
297.853009	8000.237662	9.756275	-0.060179	4.818743
297.946988	8000.221042	9.761280	-0.060196	4.818738
297.553569	8000.212819	9.766285	-0.060123	4.818737
297.710707	8000.227421	9.771290	-0.060152	4.818740
298.164409	8000.250040	9.776295	-0.060236	4.818745
297.980100	8000.243463	9.781299	-0.060202	4.818744
298.153524	8000.185924	9.786304	-0.060234	4.818726
298.434250	8000.219945	9.791309	-0.060286	4.818735
298.100616	8000.196763	9.796314	-0.060224	4.818730
298.439674	8000.196934	9.801319	-0.060287	4.818728
298.546294	8000.183622	9.806323	-0.060307	4.818724
298.111673	8000.195838	9.811328	-0.060226	4.818729
298.332000	8000.180846	9.816333	-0.060267	4.818724
298.344584	8000.163177	9.821338	-0.060269	4.818719
298.473410	8000.220405	9.826343	-0.060293	4.818735
298.518644	8000.223079	9.831347	-0.060301	4.818736
298.455761	8000.194999	9.836352	-0.060289	4.818728
298.269991	8000.231395	9.841357	-0.060255	4.818739
298.191207	8000.210450	9.846362	-0.060240	4.818733
298.293934	8000.224351	9.851367	-0.060259	4.818737
298.511499	8000.205129	9.856371	-0.060299	4.818731
298.239653	8000.185890	9.861376	-0.060249	4.818726
298.602934	8000.218878	9.866381	-0.060316	4.818734
298.524707	8000.150755	9.871386	-0.060301	4.818714
298.489272	8000.237323	9.876391	-0.060295	4.818740
298.364177	8000.206344	9.881395	-0.060271	4.818732
298.587293	8000.195582	9.886400	-0.060313	4.818728
298.807175	8000.240355	9.891405	-0.060354	4.818740
298.622217	8000.202311	9.896410	-0.060319	4.818729
298.473647	8000.231847	9.901415	-0.060291	4.818739
298.462339	8000.221209	9.906419	-0.060289	4.818736
298.466058	8000.221250	9.911424	-0.060290	4.818736
298.527788	8000.249303	9.916429	-0.060301	4.818744
298.526235	8000.206285	9.921434	-0.060301	4.818731
298.452669	8000.213718	9.926439	-0.060287	4.818733
298.434979	8000.230261	9.931443	-0.060284	4.818738
298.369542	8000.235702	9.936448	-0.060271	4.818740
298.223951	8000.267373	9.941453	-0.060244	4.818750
298.452483	8000.213690	9.946458	-0.060287	4.818733
298.464329	8000.242148	9.951463	-0.060289	4.818742
298.592261	8000.210237	9.956467	-0.060312	4.818732
298.635808	8000.208695	9.961472	-0.060321	4.818731
299.023200	8000.224170	9.966477	-0.060393	4.818734
298.622511	8000.227385	9.971482	-0.060318	4.818737
299.004347	8000.213428	9.976487	-0.060389	4.818731
298.730164	8000.218274	9.981491	-0.060338	4.818734
298.873440	8000.173978	9.986496	-0.060364	4.818720
298.948341	8000.233658	9.991501	-0.060378	4.818738
298.870080	8000.212719	9.996506	-0.060363	4.818732
299.153234	8000.234191	10.001511	-0.060416	4.818737
298.990114	8000.206915	10.006515	-0.060386	4.818729
299.125326	8000.190826	10.011520	-0.060411	4.818724
299.150575	8000.229943	10.016525	-0.060415	4.818736
299.093372	8000.188304	10.021530	-0.060405	4.818723
299.141089	8000.222468	10.026535	-0.060413	4.818733
299.333855	8000.230191	10.031539	-0.060449	4.818735
299.198934	8000.207472	10.036544	-0.060424	4.818729
299.222090	8000.238174	10.041549	-0.060428	4.818738
299.258339	8000.195643	10.046554	-0.060435	4.818725
299.487281	8000.167131	10.051559	-0.060477	4.818716
299.497769	8000.201864	10.056563	-0.060479	4.818726
299.134951	8000.170963	10.061568	-0.060412	4.818718
299.189013	8000.218840	10.066573	-0.060422	4.818732
299.371388	8000.201263	10.071578	-0.060455	4.818726
299.427798	8000.207227	10.076583	-0.060466	4.818728
299.477353	8000.195277	10.081587	-0.060475	4.818724
299.199302	8000.219996	10.086592	-0.060423	4.818733
299.213864	8000.228566	10.091597	-0.060426	4.818735
299.124468	8000.192803	10.096602	-0.060409	4.818725
299.254144	8000.201809	10.101607	-0.060433	4.818727
298.953173	8000.210504	10.106611	-0.060377	4.818731
299.025944	8000.219825	10.111616	-0.060390	4.818733
299.403067	8000.227829	10.116621	-0.060461	4.818734
299.091080	8000.217507	10.121626	-0.060402	4.818732
299.171780	8000.199666	10.126631	-0.060417	4.818727
299.110308	8000.225082	10.131635	-0.060406	4.818734
299.112506	8000.203083	10.136640	-0.060406	4.818728
298.925617	8000.237367	10.141645	-0.060371	4.818739
298.943705	8000.196699	10.146650	-0.060374	4.818727
299.210442	8000.230542	10.151655	-0.060424	4.818736
298.993193	8000.241365	10.156659	-0.060383	4.818740
299.573628	8000.200611	10.161664	-0.060491	4.818725
299.370422	8000.226295	10.166669	-0.060454	4.818734
299.116201	8000.231398	10.171674	-0.060406	4.818736
299.030852	8000.266992	10.176679	-0.060390	4.818747
299.291590	8000.248328	10.181683	-0.060439	4.818741
299.308670	8000.136343	10.186688	-0.060442	4.818707
299.506842	8000.186079	10.191693	-0.060478	4.818721
299.512755	8000.188246	10.196698	-0.060479	4.818722
299.474148	8000.207665	10.201703	-0.060472	4.818728
299.415032	8000.211090	10.206707	-0.060461	4.818729
299.356158	8000.190401	10.211712	-0.060450	4.818723
299.836705	8000.237490	10.216717	-0.060539	4.818735
299.539919	8000.210585	10.221722	-0.060484	4.818728
299.293989	8000.234670	10.226727	-0.060438	4.818737
299.421388	8000.220578	10.231731	-0.060462	4.818732
299.445879	8000.191526	10.236736	-0.060466	4.818723
299.437170	8000.246983	10.241741	-0.060465	4.818740
299.193557	8000.230203	10.246746	-0.060419	4.818736
299.142479	8000.279870	10.251751	-0.060410	4.818751
299.112589	8000.249069	10.256755	-0.060404	4.818742
298.636562	8000.272283	10.261760	-0.060315	4.818750
299.186013	8000.229031	10.266765	-0.060417	4.818735
299.535666	8000.188445	10.271770	-0.060482	4.818722
299.438238	8000.232272	10.276775	-0.060464	4.818735
299.359864	8000.198748	10.281779	-0.060449	4.818726
299.508845	8000.178643	10.286784	-0.060477	4.818719
299.412506	8000.225629	10.291789	-0.060459	4.818733
299.639527	8000.191850	10.296794	-0.060501	4.818723
299.909534	8000.212105	10.301799	-0.060551	4.818728
299.827249	8000.173287	10.306803	-0.060536	4.818716
299.771855	8000.153691	10.311808	-0.060526	4.818711
299.697374	8000.175793	10.316813	-0.060512	4.818718
299.883642	8000.123663	10.321818	-0.060546	4.818701
299.632200	8000.158162	10.326823	-0.060499	4.818713
299.742784	8000.195235	10.331827	-0.060520	4.818723
299.716691	8000.142462	10.336832	-0.060515	4.818708
299.927302	8000.171387	10.341837	-0.060554	4.818715
299.653288	8000.135339	10.346842	-0.060503	4.818706
299.647749	8000.198177	10.351847	-0.060502	4.818724
299.857497	8000.182002	10.356851	-0.060541	4.818719
299.848114	8000.137833	10.361856	-0.060539	4.818706
299.843252	8000.187049	10.366861	-0.060538	4.818720
299.808362	8000.162474	10.371866	-0.060531	4.818713
299.932250	8000.193427	10.376871	-0.060554	4.818722
299.841957	8000.167089	10.381875	-0.060537	4.818714
299.963550	8000.142436	10.386880	-0.060560	4.818707
300.033421	8000.187373	10.391885	-0.060573	4.818720
299.857058	8000.148390	10.396890	-0.060540	4.818709
300.207510	8000.179120	10.401895	-0.060605	4.818717
300.015795	8000.185029	10.406899	-0.060569	4.818719
299.864478	8000.161050	10.411904	-0.060541	4.818713
299.789827	8000.216705	10.416909	-0.060527	4.818729
299.798073	8000.195833	10.421914	-0.060528	4.818723
299.468678	8000.256590	10.426919	-0.060467	4.818743
299.541318	8000.265909	10.431923	-0.060480	4.818745
299.860353	8000.200811	10.436928	-0.060540	4.818724
299.973463	8000.242112	10.441933	-0.060561	4.818736
299.939564	8000.196578	10.446938	-0.060554	4.818723
299.689959	8000.230052	10.451943	-0.060508	4.818734
299.832100	8000.225588	10.456947	-0.060534	4.818732
299.961616	8000.197891	10.461952	-0.060558	4.818723
299.979910	8000.225385	10.466957	-0.060561	4.818731
299.990551	8000.201398	10.471962	-0.060563	4.818724
299.845390	8000.222588	10.476967	-0.060536	4.818731
299.783134	8000.224924	10.481971	-0.060525	4.818732
299.748612	8000.215035	10.486976	-0.060518	4.818729
299.835456	8000.283260	10.491981	-0.060534	4.818749
299.533299	8000.248945	10.496986	-0.060478	4.818740
299.665418	8000.255886	10.501991	-0.060502	4.818742
299.763722	8000.223593	10.506995	-0.060520	4.818732
299.831173	8000.196144	10.512000	-0.060533	4.818723
300.016347	8000.224742	10.517005	-0.060567	4.818731
299.936608	8000.199589	10.522010	-0.060552	4.818724
299.846040	8000.199463	10.527015	-0.060535	4.818724
299.840920	8000.209876	10.532019	-0.060534	4.818727
299.624636	8000.214420	10.537024	-0.060494	4.818729
299.747596	8000.248506	10.542029	-0.060517	4.818739
299.598748	8000.200441	10.547034	-0.060489	4.818725
299.611468	8000.256175	10.552039	-0.060491	4.818742
299.683463	8000.292750	10.557043	-0.060505	4.818753
299.472438	8000.314138	10.562048	-0.060465	4.818760
299.541837	8000.254208	10.567053	-0.060478	4.818742
299.657379	8000.229478	10.572058	-0.060499	4.818734
299.916025	8000.262169	10.577063	-0.060548	4.818743
299.694665	8000.257210	10.582067	-0.060506	4.818742
299.661423	8000.241045	10.587072	-0.060500	4.818737
299.944738	8000.261472	10.592077	-0.060553	4.818742
299.666848	8000.232714	10.597082	-0.060501	4.818735
299.705127	8000.261513	10.602087	-0.060508	4.818743
299.457092	8000.272987	10.607091	-0.060462	4.818748
299.421859	8000.249457	10.612096	-0.060455	4.818741
299.841175	8000.230743	10.617101	-0.060533	4.818733
299.895214	8000.150691	10.622106	-0.060543	4.818709
299.945434	8000.113583	10.627111	-0.060552	4.818698
299.894733	8000.197859	10.632115	-0.060543	4.818723
299.860668	8000.199510	10.637120	-0.060536	4.818724
300.267070	8000.233061	10.642125	-0.060612	4.818733
300.093541	8000.200405	10.647130	-0.060579	4.818723
299.955604	8000.193376	10.652135	-0.060553	4.818722
300.233812	8000.183327	10.657139	-0.060605	4.818718
300.289339	8000.187183	10.662144	-0.060615	4.818719
300.086747	8000.231750	10.667149	-0.060578	4.818733
299.882401	8000.223864	10.672154	-0.060539	4.818731
300.241707	8000.247369	10.677159	-0.060606	4.818737
300.157211	8000.219008	10.682163	-0.060590	4.818729
300.323388	8000.143549	10.687168	-0.060621	4.818706
300.324007	8000.221148	10.692173	-0.060621	4.818729
300.175112	8000.163643	10.697178	-0.060593	4.818712
300.288527	8000.117913	10.702183	-0.060614	4.818698
300.433899	8000.193186	10.707187	-0.060642	4.818720
300.340661	8000.162615	10.712192	-0.060624	4.818711
300.358435	8000.189053	10.717197	-0.060627	4.818719
300.296366	8000.190343	10.722202	-0.060616	4.818720
300.337100	8000.161501	10.727207	-0.060623	4.818711
300.426614	8000.200400	10.732211	-0.060640	4.818722
300.361146	8000.147118	10.737216	-0.060627	4.818707
300.486020	8000.203251	10.742221	-0.060651	4.818723
300.238421	8000.172785	10.747226	-0.060604	4.818715
300.209232	8000.166110	10.752231	-0.060599	4.818713
300.251977	8000.206503	10.757235	-0.060607	4.818725
300.269180	8000.208816	10.762240	-0.060610	4.818725
300.489318	8000.217942	10.767245	-0.060651	4.818727
300.454031	8000.179730	10.772250	-0.060644	4.818716
300.687495	8000.176445	10.777255	-0.060687	4.818714
300.542912	8000.219663	10.782259	-0.060660	4.818728
300.386363	8000.200858	10.787264	-0.060631	4.818723
300.597419	8000.215111	10.792269	-0.060670	4.818726
300.487253	8000.178029	10.797274	-0.060650	4.818715
300.506520	8000.211827	10.802279	-0.060653	4.818725
300.535683	8000.247851	10.807283	-0.060659	4.818736
300.384867	8000.215488	10.812288	-0.060630	4.818727
300.395429	8000.236590	10.817293	-0.060632	4.818733
300.430571	8000.203481	10.822298	-0.060639	4.818723
300.578727	8000.209582	10.827303	-0.060666	4.818724
300.410358	8000.214742	10.832307	-0.060635	4.818727
300.265834	8000.196093	10.837312	-0.060608	4.818722
300.650012	8000.224114	10.842317	-0.060679	4.818728
300.551425	8000.187182	10.847322	-0.060661	4.818718
300.276548	8000.225573	10.852327	-0.060610	4.818730
300.287989	8000.242492	10.857331	-0.060612	4.818735
300.246782	8000.256635	10.862336	-0.060604	4.818740
300.385618	8000.253177	10.867341	-0.060630	4.818738
300.275546	8000.219243	10.872346	-0.060609	4.818728
300.402129	8000.206189	10.877351	-0.060632	4.818724
300.425902	8000.180274	10.882355	-0.060637	4.818716
300.498617	8000.183304	10.887360	-0.060650	4.818717
300.400897	8000.235516	10.892365	-0.060632	4.818733
300.418184	8000.191690	10.897370	-0.060635	4.818720
300.358727	8000.202451	10.902375	-0.060624	4.818723
300.463702	8000.202751	10.907379	-0.060643	4.818723
300.412632	8000.205232	10.912384	-0.060634	4.818724
300.496516	8000.228329	10.917389	-0.060649	4.818730
300.337857	8000.213691	10.922394	-0.060620	4.818727
300.264213	8000.213783	10.927399	-0.060606	4.818727
300.375297	8000.235134	10.932403	-0.060626	4.818733
300.048226	8000.252928	10.937408	-0.060565	4.818739
300.306085	8000.278270	10.942413	-0.060613	4.818746
300.368715	8000.228738	10.947418	-0.060625	4.818731
300.265923	8000.270398	10.952423	-0.060606	4.818744
300.460592	8000.243543	10.957427	-0.060642	4.818735
300.400901	8000.216551	10.962432	-0.060631	4.818727
300.490646	8000.241821	10.967437	-0.060647	4.818734
300.326791	8000.207193	10.972442	-0.060617	4.818725
300.659380	8000.191555	10.977447	-0.060679	4.818719
300.670422	8000.232587	10.982451	-0.060680	4.818731
300.520231	8000.193941	10.987456	-0.060652	4.818720
300.479901	8000.234310	10.992461	-0.060645	4.818732
300.481544	8000.191331	10.997466	-0.060645	4.818719
300.376959	8000.176343	11.002471	-0.060625	4.818715
300.464404	8000.222556	11.007475	-0.060642	4.818729
300.592187	8000.195886	11.012480	-0.060665	4.818720
300.565911	8000.247971	11.017485	-0.060660	4.818736
300.604436	8000.206517	11.022490	-0.060667	4.818723
300.515398	8000.203264	11.027495	-0.060651	4.818723
300.751926	8000.230429	11.032499	-0.060695	4.818730
300.437329	8000.202244	11.037504	-0.060636	4.818723
300.468108	8000.225704	11.042509	-0.060642	4.818730
300.623672	8000.203588	11.047514	-0.060671	4.818723
300.587443	8000.194725	11.052519	-0.060664	4.818720
300.470463	8000.165944	11.057523	-0.060642	4.818712
300.587720	8000.160111	11.062528	-0.060664	4.818710
300.789439	8000.237160	11.067533	-0.060701	4.818732
300.405626	8000.216471	11.072538	-0.060630	4.818727
300.681463	8000.105725	11.077543	-0.060681	4.818693
300.715082	8000.185847	11.082547	-0.060687	4.818717
300.728921	8000.138832	11.087552	-0.060689	4.818703
300.645885	8000.157677	11.092557	-0.060674	4.818709
300.651541	8000.143063	11.097562	-0.060675	4.818704
300.587400	8000.160055	11.102567	-0.060663	4.818710
300.598096	8000.172771	11.107571	-0.060665	4.818714
300.505644	8000.089779	11.112576	-0.060647	4.818689
300.626289	8000.201434	11.117581	-0.060670	4.818722
300.603745	8000.167581	11.122586	-0.060665	4.818712
300.551418	8000.132295	11.127591	-0.060656	4.818702
300.933322	8000.173919	11.132595	-0.060727	4.818713
300.653460	8000.102140	11.137600	-0.060674	4.818692
300.536495	8000.128937	11.142605	-0.060653	4.818701
300.817834	8000.152486	11.147610	-0.060705	4.818707
300.890150	8000.112516	11.152615	-0.060718	4.818694
300.485309	8000.201661	11.157619	-0.060643	4.818723
300.747346	8000.148411	11.162624	-0.060691	4.818706
301.005114	8000.147537	11.167629	-0.060739	4.818704
300.987310	8000.084383	11.172634	-0.060736	4.818686
300.927726	8000.139185	11.177639	-0.060725	4.818702
301.060734	8000.176549	11.182643	-0.060749	4.818713
301.017624	8000.120408	11.187648	-0.060741	4.818696
300.817243	8000.192268	11.192653	-0.060704	4.818719
301.020847	8000.202230	11.197658	-0.060742	4.818721
301.109165	8000.163516	11.202663	-0.060758	4.818709
301.094763	8000.213658	11.207667	-0.060755	4.818724
301.057180	8000.202680	11.212672	-0.060748	4.818721
301.164982	8000.218746	11.217677	-0.060768	4.818725
300.952712	8000.206562	11.222682	-0.060729	4.818722
301.059674	8000.200596	11.227687	-0.060748	4.818720
301.173448	8000.209399	11.232691	-0.060770	4.818722
301.087916	8000.185218	11.237696	-0.060753	4.818715
300.882959	8000.231851	11.242701	-0.060715	4.818730
301.100506	8000.210535	11.247706	-0.060756	4.818723
300.761284	8000.234462	11.252711	-0.060692	4.818731
301.018400	8000.232532	11.257715	-0.060740	4.818730
301.024669	8000.132987	11.262720	-0.060741	4.818700
300.977506	8000.186900	11.267725	-0.060732	4.818716
300.640694	8000.210859	11.272730	-0.060670	4.818725
300.890545	8000.196251	11.277735	-0.060716	4.818719
300.919641	8000.236468	11.282739	-0.060721	4.818731
300.888146	8000.207742	11.287744	-0.060715	4.818723
300.935258	8000.257630	11.292749	-0.060724	4.818738
300.893977	8000.232972	11.297754	-0.060716	4.818730
300.717718	8000.284170	11.302759	-0.060683	4.818746
300.740193	8000.262433	11.307763	-0.060687	4.818740
300.788346	8000.202227	11.312768	-0.060696	4.818722
300.762753	8000.245933	11.317773	-0.060691	4.818735
300.872422	8000.207494	11.322778	-0.060712	4.818723
300.416975	8000.226776	11.327783	-0.060627	4.818730
300.636160	8000.253717	11.332787	-0.060668	4.818738
300.633538	8000.238996	11.337792	-0.060667	4.818733
300.720056	8000.243252	11.342797	-0.060683	4.818734
300.590284	8000.216404	11.347802	-0.060659	4.818727
300.554874	8000.243205	11.352807	-0.060652	4.818735
300.412881	8000.242414	11.357811	-0.060626	4.818735
300.111950	8000.239573	11.362816	-0.060569	4.818735
299.854274	8000.296012	11.367821	-0.060521	4.818753
299.841867	8000.285359	11.372826	-0.060519	4.818750
300.041337	8000.271149	11.377831	-0.060556	4.818745
300.261309	8000.253009	11.382835	-0.060597	4.818739
300.328482	8000.260161	11.387840	-0.060609	4.818741
300.490714	8000.286367	11.392845	-0.060639	4.818748
300.797505	8000.238938	11.397850	-0.060696	4.818733
300.770972	8000.214471	11.402855	-0.060691	4.818725
300.460578	8000.280716	11.407859	-0.060634	4.818746
300.614285	8000.205095	11.412864	-0.060662	4.818723
300.918958	8000.223703	11.417869	-0.060719	4.818728
300.968564	8000.227482	11.422874	-0.060728	4.818728
300.735282	8000.230756	11.427879	-0.060684	4.818730
300.852937	8000.238560	11.432883	-0.060706	4.818732
300.990786	8000.083039	11.437888	-0.060732	4.818685
300.954755	8000.174847	11.442893	-0.060725	4.818713
301.026145	8000.174713	11.447898	-0.060738	4.818713
301.118318	8000.187432	11.452903	-0.060755	4.818716
301.193736	8000.196788	11.457907	-0.060769	4.818719
300.972741	8000.155130	11.462912	-0.060728	4.818707
301.065538	8000.206655	11.467917	-0.060745	4.818722
301.166095	8000.181731	11.472922	-0.060764	4.818714
301.155555	8000.176346	11.477927	-0.060762	4.818713
300.968776	8000.231603	11.482931	-0.060727	4.818730
301.231258	8000.201429	11.487936	-0.060776	4.818720
300.997705	8000.251887	11.492941	-0.060732	4.818736
300.876351	8000.230390	11.497946	-0.060709	4.818730
300.906306	8000.249646	11.502951	-0.060715	4.818735
300.959773	8000.242989	11.507955	-0.060725	4.818733
301.217305	8000.182341	11.512960	-0.060772	4.818714
301.103610	8000.210229	11.517965	-0.060751	4.818723
300.716959	8000.214668	11.522970	-0.060679	4.818726
300.885345	8000.196912	11.527975	-0.060710	4.818720
301.082941	8000.246645	11.532979	-0.060747	4.818734
300.998812	8000.225628	11.537984	-0.060731	4.818728
301.103613	8000.245850	11.542989	-0.060751	4.818733
300.959473	8000.214621	11.547994	-0.060724	4.818725
301.000393	8000.215143	11.552999	-0.060731	4.818725
301.320822	8000.245489	11.558003	-0.060791	4.818733
301.253216	8000.212102	11.563008	-0.060778	4.818723
301.426609	8000.253135	11.568013	-0.060810	4.818734
301.117062	8000.234450	11.573018	-0.060753	4.818730
300.852166	8000.220538	11.578023	-0.060703	4.818727
300.847048	8000.260313	11.583027	-0.060702	4.818739
301.025599	8000.190256	11.588032	-0.060735	4.818717
301.228110	8000.257880	11.593037	-0.060773	4.818737
300.758015	8000.232929	11.598042	-0.060685	4.818731
300.856408	8000.197491	11.603047	-0.060704	4.818720
301.180728	8000.246762	11.608051	-0.060764	4.818733
301.231899	8000.214909	11.613056	-0.060773	4.818724
301.214967	8000.261873	11.618061	-0.060770	4.818738
300.733354	8000.256697	11.623066	-0.060680	4.818738
301.047614	8000.253407	11.628071	-0.060739	4.818736
301.160071	8000.219199	11.633075	-0.060760	4.818725
301.193153	8000.205987	11.638080	-0.060766	4.818721
301.173640	8000.219361	11.643085	-0.060762	4.818725
301.144558	8000.189618	11.648090	-0.060756	4.818717
301.051664	8000.203093	11.653095	-0.060739	4.818721
301.215097	8000.230364	11.658099	-0.060769	4.818728
300.899599	8000.205312	11.663104	-0.060711	4.818722
301.100024	8000.240400	11.668109	-0.060748	4.818732
301.060308	8000.239881	11.673114	-0.060740	4.818732
300.931502	8000.214093	11.678119	-0.060716	4.818725
300.957372	8000.255317	11.683123	-0.060721	4.818737
301.239297	8000.193935	11.688128	-0.060773	4.818718
301.421908	8000.243476	11.693133	-0.060807	4.818732
300.717066	8000.236466	11.698138	-0.060676	4.818732
300.909048	8000.213771	11.703143	-0.060712	4.818725
300.953820	8000.251045	11.708147	-0.060720	4.818736
301.021373	8000.231987	11.713152	-0.060732	4.818730
300.905050	8000.285007	11.718157	-0.060711	4.818746
300.726997	8000.264876	11.723162	-0.060677	4.818741
301.112667	8000.278237	11.728167	-0.060749	4.818743
301.281172	8000.241607	11.733171	-0.060780	4.818732
301.155268	8000.247315	11.738176	-0.060757	4.818734
301.258579	8000.266470	11.743181	-0.060776	4.818739
301.271959	8000.245663	11.748186	-0.060778	4.818733
301.397931	8000.220019	11.753191	-0.060802	4.818725
301.286723	8000.263668	11.758195	-0.060781	4.818738
301.165075	8000.273626	11.763200	-0.060758	4.818742
301.252744	8000.263216	11.768205	-0.060774	4.818738
301.306772	8000.246081	11.773210	-0.060784	4.818733
301.126507	8000.274157	11.778215	-0.060751	4.818742
301.087214	8000.272595	11.783219	-0.060743	4.818742
300.824038	8000.283872	11.788224	-0.060694	4.818746
300.984211	8000.292225	11.793229	-0.060724	4.818748
300.619225	8000.311625	11.798234	-0.060656	4.818755
300.957726	8000.268800	11.803239	-0.060719	4.818741
301.236002	8000.261900	11.808243	-0.060771	4.818738
301.167987	8000.218021	11.813248	-0.060758	4.818725
301.338201	8000.284180	11.818253	-0.060789	4.818744
301.117296	8000.254056	11.823258	-0.060748	4.818736
301.259431	8000.273712	11.828263	-0.060775	4.818741
301.096466	8000.276845	11.833267	-0.060744	4.818743
301.106396	8000.253896	11.838272	-0.060746	4.818736
301.029653	8000.263386	11.843277	-0.060731	4.818739
300.990924	8000.235615	11.848282	-0.060724	4.818731
301.117935	8000.249832	11.853287	-0.060748	4.818735
301.380276	8000.244823	11.858291	-0.060796	4.818732
301.105822	8000.229738	11.863296	-0.060745	4.818729
301.133555	8000.262598	11.868301	-0.060750	4.818738
301.037975	8000.242482	11.873306	-0.060732	4.818733
301.215426	8000.246864	11.878311	-0.060765	4.818733
301.079082	8000.263972	11.883315	-0.060740	4.818739
300.693250	8000.266325	11.888320	-0.060668	4.818741
300.882221	8000.280293	11.893325	-0.060703	4.818745
301.121803	8000.265553	11.898330	-0.060748	4.818739
301.229409	8000.210310	11.903335	-0.060768	4.818723
301.440338	8000.230854	11.908339	-0.060807	4.818728
301.528979	8000.212068	11.913344	-0.060823	4.818722
301.333770	8000.228416	11.918349	-0.060787	4.818728
301.505048	8000.200211	11.923354	-0.060818	4.818719
301.439664	8000.220333	11.928359	-0.060806	4.818725
301.752098	8000.222264	11.933363	-0.060864	4.818724
301.670626	8000.190795	11.938368	-0.060849	4.818715
301.644770	8000.212476	11.943373	-0.060844	4.818722
301.692996	8000.176390	11.948378	-0.060853	4.818711
301.537317	8000.178568	11.953383	-0.060824	4.818712
301.589151	8000.211738	11.958387	-0.060833	4.818722
301.673476	8000.168778	11.963392	-0.060849	4.818709
301.661393	8000.200075	11.968397	-0.060847	4.818718
301.766800	8000.159484	11.973402	-0.060866	4.818705
301.841969	8000.149961	11.978407	-0.060880	4.818702
301.807178	8000.201938	11.983411	-0.060874	4.818718
301.578281	8000.187441	11.988416	-0.060831	4.818714
301.466292	8000.244712	11.993421	-0.060810	4.818732
301.765506	8000.228646	11.998426	-0.060866	4.818726
301.632652	8000.169248	12.003431	-0.060841	4.818709
301.652348	8000.230317	12.008435	-0.060844	4.818727
301.884138	8000.158850	12.013440	-0.060887	4.818705
301.704182	8000.211050	12.018445	-0.060854	4.818721
301.590418	8000.161336	12.023450	-0.060832	4.818707
301.567247	8000.201928	12.028455	-0.060828	4.818719
301.586012	8000.214748	12.033459	-0.060832	4.818723
301.552455	8000.191238	12.038464	-0.060825	4.818716
301.738365	8000.211459	12.043469	-0.060860	4.818721
301.812866	8000.213463	12.048474	-0.060873	4.818721
301.584756	8000.220998	12.053479	-0.060831	4.818724
301.822264	8000.199939	12.058483	-0.060875	4.818717
301.737877	8000.170530	12.063488	-0.060859	4.818709
301.770225	8000.217082	12.068493	-0.060865	4.818723
301.813137	8000.187218	12.073498	-0.060873	4.818714
301.630678	8000.198488	12.078503	-0.060839	4.818718
301.827385	8000.210460	12.083507	-0.060876	4.818720
301.730389	8000.182985	12.088512	-0.060857	4.818713
301.687037	8000.196051	12.093517	-0.060849	4.818717
301.782123	8000.177348	12.098522	-0.060867	4.818711
301.654710	8000.172550	12.103527	-0.060843	4.818710
301.582835	8000.206221	12.108531	-0.060830	4.818720
301.641923	8000.143010	12.113536	-0.060840	4.818701
301.732281	8000.210235	12.118541	-0.060857	4.818721
301.725176	8000.196505	12.123546	-0.060856	4.818717
301.662334	8000.178909	12.128551	-0.060844	4.818712
301.858040	8000.222327	12.133555	-0.060880	4.818724
301.603481	8000.211692	12.138560	-0.060833	4.818722
301.736881	8000.227041	12.143565	-0.060858	4.818726
301.846395	8000.210622	12.148570	-0.060878	4.818720
301.832091	8000.217771	12.153575	-0.060875	4.818723
301.716469	8000.242488	12.158579	-0.060854	4.818730
301.723460	8000.205869	12.163584	-0.060855	4.818719
301.756993	8000.228317	12.168589	-0.060861	4.818726
301.551672	8000.244535	12.173594	-0.060823	4.818732
301.622026	8000.196151	12.178599	-0.060836	4.818717
301.732003	8000.234267	12.183603	-0.060856	4.818728
301.495902	8000.219677	12.188608	-0.060812	4.818724
301.342799	8000.182040	12.193613	-0.060783	4.818714
301.579923	8000.180901	12.198618	-0.060827	4.818713
301.426478	8000.173670	12.203623	-0.060799	4.818711
301.551435	8000.191006	12.208627	-0.060822	4.818716
301.678826	8000.171672	12.213632	-0.060845	4.818709
301.622940	8000.240154	12.218637	-0.060835	4.818730
301.308028	8000.197282	12.223642	-0.060776	4.818719
301.210086	8000.178184	12.228647	-0.060758	4.818713
301.500469	8000.222824	12.233651	-0.060812	4.818725
301.634459	8000.166872	12.238656	-0.060837	4.818708
301.496575	8000.219615	12.243661	-0.060811	4.818724
301.415193	8000.192342	12.248666	-0.060796	4.818717
301.722813	8000.177432	12.253671	-0.060853	4.818711
301.660249	8000.230098	12.258675	-0.060841	4.818727
301.674643	8000.182040	12.263680	-0.060844	4.818713
301.728457	8000.218383	12.268685	-0.060854	4.818723
301.679759	8000.216699	12.273690	-0.060845	4.818723
301.762647	8000.172671	12.278695	-0.060860	4.818709
301.849651	8000.232512	12.283699	-0.060876	4.818727
301.568759	8000.200565	12.288704	-0.060824	4.818719
301.628852	8000.224405	12.293709	-0.060835	4.818725
301.773845	8000.228368	12.298714	-0.060862	4.818726
301.818045	8000.197473	12.303719	-0.060870	4.818717
301.710810	8000.228590	12.308723	-0.060850	4.818726
301.703928	8000.188646	12.313728	-0.060848	4.818714
301.628010	8000.217021	12.318733	-0.060834	4.818723
301.564218	8000.194170	12.323738	-0.060822	4.818717
301.408198	8000.143911	12.328743	-0.060793	4.818702
301.661498	8000.206948	12.333747	-0.060840	4.818720
301.726927	8000.158500	12.338752	-0.060852	4.818705
301.651112	8000.217288	12.343757	-0.060838	4.818723
301.543220	8000.204353	12.348762	-0.060818	4.818720
301.606432	8000.250254	12.353767	-0.060829	4.818733
301.744074	8000.236296	12.358771	-0.060855	4.818728
301.550366	8000.205474	12.363776	-0.060819	4.818720
301.801653	8000.229686	12.368781	-0.060865	4.818726
301.620845	8000.203226	12.373786	-0.060832	4.818719
301.590777	8000.140961	12.378791	-0.060826	4.818701
301.995582	8000.189177	12.383795	-0.060901	4.818714
301.746571	8000.202733	12.388800	-0.060855	4.818719
301.569565	8000.227705	12.393805	-0.060822	4.818727
301.800098	8000.208654	12.398810	-0.060865	4.818720
301.952912	8000.208524	12.403815	-0.060893	4.818719
301.675739	8000.214376	12.408819	-0.060841	4.818722
301.634517	8000.127849	12.413824	-0.060833	4.818697
301.888615	8000.157339	12.418829	-0.060881	4.818704
301.854932	8000.199893	12.423834	-0.060874	4.818717
301.551555	8000.229525	12.428839	-0.060818	4.818727
301.514907	8000.258408	12.433843	-0.060811	4.818736
301.642927	8000.193990	12.438848	-0.060835	4.818716
301.641269	8000.255832	12.443853	-0.060834	4.818735
301.539069	8000.248214	12.448858	-0.060815	4.818733
301.750862	8000.216337	12.453863	-0.060854	4.818723
301.559070	8000.229584	12.458867	-0.060819	4.818727
301.532395	8000.208260	12.463872	-0.060814	4.818721
302.013179	8000.210268	12.468877	-0.060903	4.818720
301.918772	8000.214285	12.473882	-0.060885	4.818721
301.864267	8000.180018	12.478887	-0.060875	4.818711
301.738966	8000.238167	12.483891	-0.060852	4.818729
301.688182	8000.151516	12.488896	-0.060842	4.818704
301.606499	8000.217568	12.493901	-0.060827	4.818723
301.510867	8000.212132	12.498906	-0.060809	4.818722
301.798124	8000.191716	12.503911	-0.060862	4.818715
301.783119	8000.234510	12.508915	-0.060859	4.818728
301.742869	8000.139606	12.513920	-0.060852	4.818700
301.815154	8000.198208	12.518925	-0.060865	4.818717
301.780576	8000.241799	12.523930	-0.060859	4.818730
301.564939	8000.226424	12.528935	-0.060818	4.818726
301.889338	8000.237947	12.533939	-0.060879	4.818728
301.402506	8000.256821	12.538944	-0.060788	4.818736
301.466046	8000.276511	12.543949	-0.060800	4.818742
301.731843	8000.249526	12.548954	-0.060849	4.818733
301.615457	8000.267941	12.553959	-0.060827	4.818738
301.725215	8000.264109	12.558963	-0.060848	4.818737
301.516149	8000.249868	12.563968	-0.060809	4.818733
301.837334	8000.273934	12.568973	-0.060868	4.818739
301.771296	8000.256296	12.573978	-0.060856	4.818734
301.741755	8000.238081	12.578983	-0.060850	4.818729
301.923751	8000.208965	12.583987	-0.060884	4.818720
301.999271	8000.181621	12.588992	-0.060898	4.818711
302.009175	8000.256197	12.593997	-0.060900	4.818733
301.748298	8000.231848	12.599002	-0.060851	4.818727
301.921998	8000.222549	12.604007	-0.060884	4.818724
301.795113	8000.269142	12.609011	-0.060860	4.818738
301.395643	8000.208399	12.614016	-0.060785	4.818722
301.831849	8000.244436	12.619021	-0.060866	4.818731
301.491219	8000.244225	12.624026	-0.060803	4.818732
301.654216	8000.231643	12.629031	-0.060833	4.818728
301.463388	8000.238610	12.634035	-0.060798	4.818730
301.517959	8000.171147	12.639040	-0.060808	4.818710
301.740785	8000.198136	12.644045	-0.060849	4.818717
301.549839	8000.223977	12.649050	-0.060813	4.818726
301.611262	8000.212180	12.654055	-0.060825	4.818722
301.772246	8000.258296	12.659059	-0.060855	4.818735
301.440916	8000.220454	12.664064	-0.060793	4.818725
301.484623	8000.270299	12.669069	-0.060801	4.818740
301.869090	8000.238555	12.674074	-0.060872	4.818729
301.902268	8000.167669	12.679079	-0.060878	4.818708
301.307238	8000.238627	12.684083	-0.060768	4.818731
301.810858	8000.116140	12.689088	-0.060861	4.818693
301.980932	8000.169714	12.694093	-0.060893	4.818708
301.877947	8000.169426	12.699098	-0.060874	4.818708
301.896568	8000.208460	12.704103	-0.060877	4.818720
302.029781	8000.232196	12.709107	-0.060902	4.818726
301.896093	8000.186420	12.714112	-0.060877	4.818713
301.932434	8000.215196	12.719117	-0.060883	4.818722
302.021198	8000.191168	12.724122	-0.060900	4.818714
301.986438	8000.137232	12.729127	-0.060893	4.818698
302.001357	8000.170975	12.734131	-0.060896	4.818708
302.244501	8000.141600	12.739136	-0.060941	4.818699
302.214658	8000.194690	12.744141	-0.060935	4.818714
302.004384	8000.196162	12.749146	-0.060896	4.818716
301.735215	8000.190583	12.754151	-0.060846	4.818715
301.990639	8000.230578	12.759155	-0.060893	4.818726
301.795882	8000.192402	12.764160	-0.060857	4.818715
301.772873	8000.239287	12.769165	-0.060853	4.818729
302.065605	8000.218943	12.774170	-0.060907	4.818722
301.884254	8000.137945	12.779175	-0.060873	4.818699
301.842236	8000.233872	12.784179	-0.060865	4.818728
301.846016	8000.186725	12.789184	-0.060866	4.818714
302.202784	8000.209154	12.794189	-0.060932	4.818719
301.826762	8000.215826	12.799194	-0.060862	4.818722
301.940149	8000.155413	12.804199	-0.060883	4.818704
302.319933	8000.173945	12.809203	-0.060954	4.818708
301.896616	8000.167422	12.814208	-0.060875	4.818708
301.955485	8000.174468	12.819213	-0.060886	4.818709
302.036863	8000.217459	12.824218	-0.060901	4.818722
302.028981	8000.178550	12.829223	-0.060899	4.818710
302.023932	8000.169041	12.834227	-0.060898	4.818708
301.958454	8000.178675	12.839232	-0.060886	4.818711
301.978018	8000.225062	12.844237	-0.060890	4.818724
301.930267	8000.215001	12.849242	-0.060881	4.818722
301.806043	8000.212342	12.854247	-0.060857	4.818721
301.803911	8000.252156	12.859251	-0.060857	4.818733
301.700790	8000.238235	12.864256	-0.060838	4.818729
301.485262	8000.229153	12.869261	-0.060797	4.818728
301.424187	8000.268206	12.874266	-0.060786	4.818739
301.777921	8000.199363	12.879271	-0.060852	4.818718
301.755006	8000.264077	12.884275	-0.060847	4.818737
301.940512	8000.220325	12.889280	-0.060882	4.818723
301.878972	8000.242594	12.894285	-0.060870	4.818730
302.126708	8000.211182	12.899290	-0.060916	4.818720
301.706494	8000.208895	12.904295	-0.060838	4.818721
301.948439	8000.222499	12.909299	-0.060883	4.818724
301.780147	8000.205638	12.914304	-0.060851	4.818719
302.218926	8000.210250	12.919309	-0.060933	4.818719
301.981090	8000.219756	12.924314	-0.060889	4.818723
301.926149	8000.212748	12.929319	-0.060878	4.818721
302.219335	8000.204993	12.934323	-0.060933	4.818718
301.699330	8000.165763	12.939328	-0.060836	4.818708
301.739895	8000.237588	12.944333	-0.060843	4.818729
301.719064	8000.245702	12.949338	-0.060839	4.818732
301.964175	8000.193283	12.954343	-0.060885	4.818715
301.734428	8000.234352	12.959347	-0.060842	4.818728
301.665865	8000.219828	12.964352	-0.060829	4.818724
301.631161	8000.277049	12.969357	-0.060823	4.818741
301.889912	8000.264655	12.974362	-0.060871	4.818737
302.005825	8000.193788	12.979367	-0.060892	4.818715
302.154541	8000.234503	12.984371	-0.060920	4.818727
301.857208	8000.199197	12.989376	-0.060864	4.818717
302.073893	8000.184162	12.994381	-0.060905	4.818712
302.004851	8000.171728	12.999386	-0.060892	4.818709
301.820739	8000.146274	13.004391	-0.060857	4.818702
302.043068	8000.233031	13.009395	-0.060899	4.818727
302.156290	8000.219806	13.014400	-0.060920	4.818722
301.888265	8000.239408	13.019405	-0.060870	4.818729
302.114483	8000.225545	13.024410	-0.060912	4.818724
301.953613	8000.228704	13.029415	-0.060882	4.818726
302.371064	8000.241430	13.034419	-0.060959	4.818728
302.214923	8000.211093	13.039424	-0.060930	4.818719
302.263253	8000.167667	13.044429	-0.060939	4.818706
302.265650	8000.201249	13.049434	-0.060939	4.818716
302.136129	8000.184888	13.054439	-0.060915	4.818712
302.324496	8000.229261	13.059443	-0.060950	4.818724
302.361238	8000.210854	13.064448	-0.060957	4.818719
302.356508	8000.229662	13.069453	-0.060956	4.818724
302.202454	8000.246542	13.074458	-0.060927	4.818730
302.075997	8000.208199	13.079463	-0.060903	4.818719
302.091551	8000.225172	13.084467	-0.060906	4.818724
301.940375	8000.183364	13.089472	-0.060878	4.818712
301.997701	8000.227093	13.094477	-0.060889	4.818725
302.118697	8000.170973	13.099482	-0.060911	4.818708
302.046961	8000.172137	13.104487	-0.060898	4.818709
302.067736	8000.194421	13.109491	-0.060901	4.818715
302.354240	8000.216991	13.114496	-0.060955	4.818721
302.365308	8000.243344	13.119501	-0.060957	4.818728
302.227894	8000.228979	13.124506	-0.060931	4.818725
302.228168	8000.195419	13.129511	-0.060931	4.818715
302.242825	8000.221818	13.134515	-0.060933	4.818723
302.123015	8000.192999	13.139520	-0.060911	4.818714
302.239810	8000.214426	13.144525	-0.060933	4.818720
302.257942	8000.220946	13.149530	-0.060936	4.818722
301.946120	8000.208522	13.154535	-0.060878	4.818720
302.284226	8000.255878	13.159539	-0.060941	4.818733
302.055818	8000.221462	13.164544	-0.060898	4.818723
302.122555	8000.210782	13.169549	-0.060910	4.818720
302.000561	8000.199762	13.174554	-0.060888	4.818717
302.089090	8000.168391	13.179559	-0.060904	4.818707
302.158133	8000.217514	13.184563	-0.060917	4.818722
301.843123	8000.217634	13.189568	-0.060858	4.818723
302.169732	8000.204019	13.194573	-0.060919	4.818718
302.280024	8000.182366	13.199578	-0.060939	4.818711
302.042682	8000.140494	13.204583	-0.060895	4.818699
302.088994	8000.194567	13.209587	-0.060903	4.818715
302.150520	8000.153409	13.214592	-0.060915	4.818703
302.334784	8000.187242	13.219597	-0.060949	4.818712
302.145095	8000.205759	13.224602	-0.060914	4.818718
302.080338	8000.189186	13.229607	-0.060901	4.818714
302.117899	8000.221125	13.234611	-0.060908	4.818723
301.958820	8000.139366	13.239616	-0.060879	4.818699
302.144492	8000.242429	13.244621	-0.060913	4.818729
302.098399	8000.237632	13.249626	-0.060904	4.818728
301.677926	8000.219612	13.254631	-0.060826	4.818724
301.706343	8000.296523	13.259635	-0.060831	4.818747
301.806322	8000.242230	13.264640	-0.060850	4.818730
301.696824	8000.276463	13.269645	-0.060829	4.818741
301.332076	8000.272795	13.274650	-0.060761	4.818741
301.449379	8000.216628	13.279655	-0.060783	4.818724
301.508045	8000.274006	13.284659	-0.060794	4.818741
301.586864	8000.232023	13.289664	-0.060808	4.818728
301.536781	8000.267024	13.294669	-0.060799	4.818739
301.554082	8000.278776	13.299674	-0.060802	4.818742
301.770949	8000.227041	13.304679	-0.060842	4.818726
301.828249	8000.285450	13.309683	-0.060853	4.818743
301.635497	8000.228425	13.314688	-0.060817	4.818727
301.607852	8000.289931	13.319693	-0.060812	4.818745
301.834192	8000.263486	13.324698	-0.060854	4.818737
301.963387	8000.237883	13.329703	-0.060878	4.818728
301.854424	8000.283659	13.334707	-0.060857	4.818743
301.754010	8000.229923	13.339712	-0.060839	4.818727
301.540405	8000.232401	13.344717	-0.060799	4.818728
301.931660	8000.244788	13.349722	-0.060872	4.818731
301.524152	8000.257346	13.354727	-0.060796	4.818736
301.737714	8000.251708	13.359731	-0.060835	4.818733
301.891526	8000.228521	13.364736	-0.060864	4.818726
302.097032	8000.248996	13.369741	-0.060902	4.818731
301.880408	8000.268213	13.374746	-0.060862	4.818738
302.149562	8000.225542	13.379751	-0.060912	4.818724
302.170707	8000.246782	13.384755	-0.060915	4.818730
301.973868	8000.234795	13.389760	-0.060879	4.818728
302.041644	8000.204205	13.394765	-0.060891	4.818718
301.861492	8000.230185	13.399770	-0.060858	4.818727
301.687936	8000.242619	13.404775	-0.060825	4.818731
302.025888	8000.221809	13.409779	-0.060888	4.818723
301.846040	8000.220529	13.414784	-0.060854	4.818724
301.947497	8000.222881	13.419789	-0.060873	4.818724
302.019826	8000.209128	13.424794	-0.060887	4.818720
301.779668	8000.200777	13.429799	-0.060842	4.818718
302.331036	8000.223621	13.434803	-0.060944	4.818723
302.425196	8000.184982	13.439808	-0.060962	4.818711
301.945304	8000.219675	13.444813	-0.060872	4.818723
301.837158	8000.219320	13.449818	-0.060852	4.818723
302.176287	8000.116731	13.454823	-0.060915	4.818692
302.281170	8000.203020	13.459827	-0.060935	4.818717
302.029038	8000.210244	13.464832	-0.060888	4.818720
302.189257	8000.242718	13.469837	-0.060917	4.818729
302.243133	8000.253894	13.474842	-0.060927	4.818732
301.660257	8000.235873	13.479847	-0.060819	4.818729
302.058870	8000.218993	13.484851	-0.060893	4.818723
301.818393	8000.197005	13.489856	-0.060848	4.818717
301.939279	8000.165003	13.494861	-0.060870	4.818707
301.959275	8000.237612	13.499866	-0.060874	4.818728
302.040062	8000.172584	13.504871	-0.060889	4.818709
302.074008	8000.219156	13.509875	-0.060895	4.818723
302.224603	8000.209560	13.514880	-0.060923	4.818719
302.218893	8000.238842	13.519885	-0.060922	4.818728
302.056047	8000.230440	13.524890	-0.060891	4.818726
302.045881	8000.222962	13.529895	-0.060889	4.818724
302.229527	8000.231619	13.534899	-0.060924	4.818726
301.942347	8000.244682	13.539904	-0.060870	4.818731
301.967548	8000.199909	13.544909	-0.060875	4.818717
302.085312	8000.214008	13.549914	-0.060896	4.818721
302.334816	8000.208835	13.554919	-0.060943	4.818719
302.306488	8000.195878	13.559923	-0.060937	4.818715
302.118459	8000.196589	13.564928	-0.060902	4.818716
301.891573	8000.206237	13.569933	-0.060860	4.818719
301.890934	8000.231389	13.574938	-0.060860	4.818727
301.974356	8000.221974	13.579943	-0.060875	4.818724
301.728914	8000.278571	13.584947	-0.060829	4.818742
301.688346	8000.229803	13.589952	-0.060822	4.818727
301.573692	8000.239851	13.594957	-0.060800	4.818731
301.596036	8000.270544	13.599962	-0.060804	4.818740
301.840256	8000.218113	13.604967	-0.060850	4.818723
301.926227	8000.273746	13.609971	-0.060866	4.818739
302.010895	8000.207720	13.614976	-0.060881	4.818719
301.963296	8000.176688	13.619981	-0.060872	4.818710
301.803071	8000.250115	13.624986	-0.060843	4.818733
301.883779	8000.185086	13.629991	-0.060857	4.818713
302.005826	8000.232796	13.634995	-0.060880	4.818727
301.875761	8000.237402	13.640000	-0.060856	4.818729
301.507013	8000.291358	13.645005	-0.060787	4.818746
301.846005	8000.265318	13.650010	-0.060850	4.818737
301.790007	8000.223691	13.655015	-0.060840	4.818725
302.053129	8000.257494	13.660019	-0.060888	4.818734
301.905846	8000.233564	13.665024	-0.060861	4.818728
301.968344	8000.169348	13.670029	-0.060872	4.818708
302.236666	8000.177002	13.675034	-0.060922	4.818709
301.873723	8000.181746	13.680039	-0.060855	4.818712
301.995947	8000.238896	13.685043	-0.060877	4.818729
302.064253	8000.236626	13.690048	-0.060890	4.818728
301.879414	8000.194384	13.695053	-0.060855	4.818716
302.098580	8000.211889	13.700058	-0.060896	4.818720
301.949695	8000.188987	13.705063	-0.060868	4.818714
302.133207	8000.206032	13.710067	-0.060902	4.818719
302.375087	8000.148327	13.715072	-0.060947	4.818700
302.182193	8000.244403	13.720077	-0.060911	4.818730
302.102467	8000.245464	13.725082	-0.060896	4.818730
302.253351	8000.153028	13.730087	-0.060924	4.818702
302.315951	8000.209408	13.735091	-0.060936	4.818719
301.986338	8000.219826	13.740096	-0.060875	4.818723
302.209565	8000.237384	13.745101	-0.060916	4.818728
302.149119	8000.231353	13.750106	-0.060905	4.818726
302.033831	8000.213079	13.755111	-0.060883	4.818721
302.068788	8000.203038	13.760115	-0.060889	4.818718
302.052417	8000.194431	13.765120	-0.060886	4.818715
301.752033	8000.259756	13.770125	-0.060830	4.818736
301.526718	8000.307175	13.775130	-0.060788	4.818751
301.569954	8000.259489	13.780135	-0.060796	4.818737
302.005073	8000.261956	13.785139	-0.060877	4.818736
302.407574	8000.227300	13.790144	-0.060952	4.818724
302.367479	8000.207900	13.795149	-0.060944	4.818718
302.136654	8000.242663	13.800154	-0.060901	4.818729
301.979788	8000.239582	13.805159	-0.060872	4.818729
302.188679	8000.221301	13.810163	-0.060911	4.818723
302.179593	8000.197058	13.815168	-0.060909	4.818716
302.067982	8000.198756	13.820173	-0.060888	4.818717
302.178867	8000.216960	13.825178	-0.060909	4.818722
302.100918	8000.264185	13.830183	-0.060894	4.818736
302.193051	8000.243347	13.835187	-0.060911	4.818729
302.270935	8000.191914	13.840192	-0.060926	4.818714
302.263286	8000.258923	13.845197	-0.060924	4.818734
302.145513	8000.246908	13.850202	-0.060902	4.818731
302.206476	8000.231959	13.855207	-0.060913	4.818726
302.306310	8000.248972	13.860211	-0.060932	4.818731
302.172256	8000.217872	13.865216	-0.060907	4.818722
301.881485	8000.261300	13.870221	-0.060853	4.818736
301.910250	8000.283686	13.875226	-0.060858	4.818743
301.826138	8000.273156	13.880231	-0.060842	4.818740
301.854595	8000.278760	13.885235	-0.060847	4.818741
301.643765	8000.251912	13.890240	-0.060808	4.818734
302.137592	8000.262478	13.895245	-0.060900	4.818735
302.163880	8000.229254	13.900250	-0.060905	4.818725
302.056250	8000.231004	13.905255	-0.060884	4.818726
302.188858	8000.263121	13.910259	-0.060909	4.818735
301.704824	8000.268398	13.915264	-0.060819	4.818739
301.919564	8000.255435	13.920269	-0.060859	4.818734
301.753875	8000.258532	13.925274	-0.060828	4.818736
301.929474	8000.223042	13.930279	-0.060860	4.818724
301.926073	8000.289057	13.935283	-0.060860	4.818744
301.689377	8000.287042	13.940288	-0.060816	4.818744
302.117388	8000.276834	13.945293	-0.060895	4.818740
301.910762	8000.261575	13.950298	-0.060857	4.818736
301.448309	8000.283910	13.955303	-0.060770	4.818744
301.947054	8000.296636	13.960307	-0.060863	4.818746
301.997992	8000.256390	13.965312	-0.060873	4.818734
301.927921	8000.253382	13.970317	-0.060859	4.818733
302.064635	8000.242557	13.975322	-0.060885	4.818730
301.792919	8000.261063	13.980327	-0.060834	4.818736
301.810694	8000.294843	13.985331	-0.060837	4.818746
301.672786	8000.272083	13.990336	-0.060812	4.818740
301.953271	8000.277796	13.995341	-0.060864	4.818741
302.286489	8000.269510	14.000346	-0.060926	4.818737
301.976286	8000.228794	14.005351	-0.060868	4.818726
301.888044	8000.312588	14.010355	-0.060851	4.818751
301.650386	8000.308464	14.015360	-0.060807	4.818751
301.517722	8000.337155	14.020365	-0.060782	4.818760
301.230454	8000.382725	14.025370	-0.060729	4.818775
301.269663	8000.325550	14.030375	-0.060736	4.818758
301.440837	8000.364456	14.035379	-0.060768	4.818768
301.401741	8000.298929	14.040384	-0.060760	4.818749
300.888225	8000.359405	14.045389	-0.060664	4.818769
300.999902	8000.353500	14.050394	-0.060685	4.818767
300.794335	8000.327770	14.055399	-0.060647	4.818760
301.092446	8000.387190	14.060403	-0.060702	4.818777
301.125901	8000.357205	14.065408	-0.060708	4.818768
301.024308	8000.363227	14.070413	-0.060689	4.818770
301.190412	8000.353831	14.075418	-0.060720	4.818766
301.212991	8000.324754	14.080423	-0.060724	4.818758
301.632246	8000.331210	14.085427	-0.060802	4.818758
301.425040	8000.264561	14.090432	-0.060764	4.818739
301.914673	8000.298142	14.095437	-0.060855	4.818747
301.814988	8000.283216	14.100442	-0.060836	4.818743
301.562000	8000.317693	14.105447	-0.060789	4.818754
301.621781	8000.318459	14.110451	-0.060800	4.818754
301.626722	8000.283911	14.115456	-0.060801	4.818744
301.666605	8000.295955	14.120461	-0.060808	4.818747
302.073699	8000.273941	14.125466	-0.060884	4.818739
301.946552	8000.268098	14.130471	-0.060860	4.818738
301.910355	8000.287549	14.135475	-0.060853	4.818744
301.880418	8000.270377	14.140480	-0.060847	4.818739
302.090253	8000.229037	14.145485	-0.060886	4.818726
302.017734	8000.266894	14.150490	-0.060873	4.818737
301.653458	8000.263232	14.155495	-0.060805	4.818738
301.914364	8000.286520	14.160499	-0.060853	4.818743
302.016001	8000.237490	14.165504	-0.060872	4.818728
302.161344	8000.276064	14.170509	-0.060899	4.818739
302.125249	8000.236791	14.175514	-0.060892	4.818728
302.149578	8000.194104	14.180519	-0.060897	4.818715
302.246924	8000.278199	14.185523	-0.060915	4.818740
302.192643	8000.270151	14.190528	-0.060905	4.818738
302.302353	8000.234859	14.195533	-0.060925	4.818727
302.005289	8000.249891	14.200538	-0.060870	4.818732
301.819240	8000.253774	14.205543	-0.060835	4.818734
301.856393	8000.282561	14.210547	-0.060842	4.818743
301.634413	8000.290174	14.215552	-0.060800	4.818746
301.392702	8000.328992	14.220557	-0.060755	4.818758
301.691159	8000.297186	14.225562	-0.060811	4.818748
301.228398	8000.310079	14.230567	-0.060724	4.818753
301.413138	8000.335528	14.235571	-0.060759	4.818760
301.215575	8000.305706	14.240576	-0.060722	4.818752
301.626605	8000.274305	14.245581	-0.060798	4.818741
302.068807	8000.259036	14.250586	-0.060880	4.818735
301.863146	8000.244839	14.255591	-0.060842	4.818731
302.027988	8000.274226	14.260595	-0.060873	4.818739
302.097890	8000.249955	14.265600	-0.060886	4.818732
302.204109	8000.269148	14.270605	-0.060905	4.818737
301.855401	8000.308681	14.275610	-0.060840	4.818750
301.930041	8000.278179	14.280615	-0.060854	4.818741
302.058872	8000.303955	14.285619	-0.060878	4.818748
302.102146	8000.253124	14.290624	-0.060886	4.818733
301.940287	8000.291924	14.295629	-0.060856	4.818745
302.198482	8000.296302	14.300634	-0.060904	4.818745
302.339908	8000.248835	14.305639	-0.060930	4.818731
302.223067	8000.285071	14.310643	-0.060908	4.818742
301.749282	8000.304113	14.315648	-0.060820	4.818749
302.111534	8000.294104	14.320653	-0.060887	4.818745
302.249152	8000.264416	14.325658	-0.060913	4.818736
302.032168	8000.266850	14.330663	-0.060872	4.818737
302.177788	8000.293892	14.335667	-0.060899	4.818745
301.922753	8000.262278	14.340672	-0.060852	4.818736
302.106599	8000.258354	14.345677	-0.060886	4.818734
302.045363	8000.291114	14.350682	-0.060874	4.818744
302.016001	8000.259268	14.355687	-0.060869	4.818735
301.779682	8000.344296	14.360691	-0.060825	4.818761
301.499851	8000.293487	14.365696	-0.060772	4.818747
301.981488	8000.291311	14.370701	-0.060862	4.818745
301.983035	8000.275595	14.375706	-0.060862	4.818740
302.027410	8000.284551	14.380711	-0.060870	4.818743
302.400556	8000.275732	14.385715	-0.060940	4.818738
301.951540	8000.268877	14.390720	-0.060856	4.818738
302.031221	8000.280387	14.395725	-0.060871	4.818741
302.173283	8000.283264	14.400730	-0.060897	4.818742
301.818442	8000.271334	14.405735	-0.060831	4.818739
301.705280	8000.311812	14.410739	-0.060810	4.818752
301.676239	8000.277874	14.415744	-0.060804	4.818742
301.748507	7999.225993	14.420749	-0.060817	4.818428

301.794072	7996.184929	14.425754	-0.060823	4.817523
301.513628	7990.673056	14.430759	-0.060768	4.815882
301.312564	7984.113373	14.435763	-0.060726	4.813928
301.824184	7976.787203	14.440768	-0.060816	4.811743
301.796814	7969.149921	14.445773	-0.060806	4.809465
301.733434	7961.426924	14.450778	-0.060789	4.807161
301.818899	7953.453241	14.455783	-0.060800	4.804781
301.576211	7945.627039	14.460787	-0.060749	4.802444
301.615982	7937.564582	14.465792	-0.060751	4.800035
301.693209	7929.594284	14.470797	-0.060760	4.797652
301.958884	7921.615393	14.475802	-0.060805	4.795264
301.849201	7913.588343	14.480807	-0.060779	4.792863
302.160047	7905.578176	14.485811	-0.060831	4.790463
302.005746	7897.544137	14.490816	-0.060797	4.788057
301.435585	7889.626587	14.495821	-0.060686	4.785686
301.626102	7881.593836	14.500826	-0.060716	4.783277
301.370806	7873.619980	14.505831	-0.060663	4.780885
301.423251	7865.566883	14.510835	-0.060668	4.778468
301.467779	7857.612353	14.515840	-0.060671	4.776079
301.241183	7849.582412	14.520845	-0.060623	4.773667
300.275629	7841.711891	14.525850	-0.060438	4.771304
300.905050	7833.498673	14.530855	-0.060550	4.768832
301.265914	7825.569269	14.535859	-0.060612	4.766445
301.266147	7817.530756	14.540864	-0.060607	4.764024
301.257269	7809.610240	14.545869	-0.060600	4.761639
301.001379	7801.566391	14.550874	-0.060547	4.759215
300.673028	7793.626579	14.555879	-0.060480	4.756822
300.850133	7785.593408	14.560883	-0.060508	4.754398
301.004383	7777.593057	14.565888	-0.060531	4.751983
301.108992	7769.494039	14.570893	-0.060545	4.749536
301.316555	7761.433985	14.575898	-0.060579	4.747101
301.189143	7753.427296	14.580903	-0.060550	4.744681
300.953090	7745.569521	14.585907	-0.060501	4.742304
301.137943	7737.560735	14.590912	-0.060530	4.739880
301.462505	7729.553779	14.595917	-0.060585	4.737456
301.175786	7721.605767	14.600922	-0.060526	4.735049
300.820895	7713.576031	14.605927	-0.060455	4.732616
301.152962	7705.513369	14.610931	-0.060511	4.730170
300.832709	7697.565307	14.615936	-0.060446	4.727759
301.403092	7689.490506	14.620941	-0.060547	4.725307
301.134937	7681.537623	14.625946	-0.060492	4.722892
301.112140	7673.499755	14.630951	-0.060482	4.720450
301.213295	7665.564194	14.635955	-0.060496	4.718037
300.805017	7657.577975	14.640960	-0.060415	4.715609
300.816318	7649.543537	14.645965	-0.060411	4.713164
300.638666	7641.624205	14.650970	-0.060373	4.710752
300.678264	7633.521369	14.655975	-0.060375	4.708284
301.003385	7625.459712	14.660979	-0.060430	4.705826
300.815135	7617.522068	14.665984	-0.060390	4.703406
300.862650	7609.552581	14.670989	-0.060393	4.700974
300.947524	7601.545412	14.675994	-0.060404	4.698530
300.600410	7593.524709	14.680999	-0.060334	4.696080
300.865322	7585.524393	14.686003	-0.060378	4.693635
301.172533	7577.504788	14.691008	-0.060430	4.691182
301.132498	7569.496565	14.696013	-0.060417	4.688733
301.011883	7561.591279	14.701018	-0.060389	4.686313
300.552024	7553.529403	14.706023	-0.060298	4.683845
300.808325	7545.586403	14.711027	-0.060341	4.681411
300.885111	7537.480162	14.716032	-0.060350	4.678926
300.673996	7529.600620	14.721037	-0.060305	4.676509
300.970951	7521.479790	14.726042	-0.060355	4.674016
300.731241	7513.476424	14.731047	-0.060305	4.671559
300.892444	7505.420854	14.736051	-0.060330	4.669084
300.694083	7497.490069	14.741056	-0.060288	4.666647
300.759113	7489.389096	14.746061	-0.060294	4.664155
300.819692	7481.541967	14.751066	-0.060301	4.661741
300.588817	7473.432201	14.756071	-0.060252	4.659244
300.958657	7465.520402	14.761075	-0.060316	4.656807
300.572676	7457.474029	14.766080	-0.060239	4.654327
300.465372	7449.523086	14.771085	-0.060213	4.651876
300.779687	7441.442588	14.776090	-0.060267	4.649383
300.519661	7433.480017	14.781095	-0.060213	4.646925
300.525935	7425.444699	14.786099	-0.060209	4.644443
300.723376	7417.477088	14.791104	-0.060240	4.641981
300.201748	7409.473239	14.796109	-0.060138	4.639506
300.283681	7401.513280	14.801114	-0.060148	4.637044
300.164261	7393.423761	14.806119	-0.060120	4.634540
300.185171	7385.495623	14.811123	-0.060119	4.632085
300.044153	7377.439069	14.816128	-0.060087	4.629589
300.175111	7369.446692	14.821133	-0.060106	4.627111
300.364784	7361.423185	14.826138	-0.060136	4.624622
300.330701	7353.465893	14.831143	-0.060125	4.622153
300.344288	7345.429306	14.836147	-0.060122	4.619657
300.220754	7337.474850	14.841152	-0.060093	4.617186
300.285115	7329.385521	14.846157	-0.060100	4.614672
300.331997	7321.447164	14.851162	-0.060104	4.612203
300.400363	7313.388596	14.856167	-0.060111	4.609695
300.235555	7305.452591	14.861171	-0.060075	4.607224
300.033169	7297.406852	14.866176	-0.060032	4.604717
300.285873	7289.428719	14.871181	-0.060074	4.602231
300.362460	7281.446590	14.876186	-0.060083	4.599742
300.235957	7273.419695	14.881191	-0.060054	4.597237
300.260296	7265.447485	14.886195	-0.060053	4.594748
300.162542	7257.425256	14.891200	-0.060030	4.592242
300.352747	7249.391959	14.896205	-0.060060	4.589732
300.164553	7241.386013	14.901210	-0.060019	4.587228
299.960177	7233.354685	14.906215	-0.059976	4.584715
299.953367	7225.412438	14.911219	-0.059969	4.582228
300.205776	7217.391241	14.916224	-0.060011	4.579716
299.915468	7209.420556	14.921229	-0.059952	4.577218
299.769568	7201.396683	14.926234	-0.059919	4.574702
299.533931	7193.389822	14.931239	-0.059870	4.572189
299.837559	7185.331096	14.936243	-0.059921	4.569660
299.496485	7177.418367	14.941248	-0.059852	4.567174
299.440105	7169.371976	14.946253	-0.059837	4.564645
299.050317	7161.492348	14.951258	-0.059759	4.562166
299.450150	7153.327447	14.956263	-0.059828	4.559599
299.555089	7145.411217	14.961267	-0.059842	4.557107
299.589105	7137.346249	14.966272	-0.059843	4.554567
299.598848	7129.375111	14.971277	-0.059840	4.552055
299.275452	7121.404232	14.976282	-0.059774	4.549541
299.345503	7113.320760	14.981287	-0.059782	4.546991
299.352064	7105.300695	14.986291	-0.059778	4.544459
299.444602	7097.349558	14.991296	-0.059790	4.541948
299.186337	7089.303278	14.996301	-0.059736	4.539404
299.320678	7081.392202	15.001306	-0.059756	4.536903
299.391523	7073.254209	15.006311	-0.059764	4.534329
299.345546	7065.341829	15.011315	-0.059750	4.531824
299.011481	7057.335202	15.016320	-0.059683	4.529287
299.129988	7049.300069	15.021325	-0.059699	4.526741
299.176829	7041.313466	15.026330	-0.059703	4.524209
299.414730	7033.328338	15.031335	-0.059742	4.521676
299.379775	7025.298401	15.036339	-0.059730	4.519127
299.314313	7017.353928	15.041344	-0.059712	4.516604
299.098751	7009.330146	15.046349	-0.059667	4.514053
299.016920	7001.414513	15.051354	-0.059646	4.511536
298.667174	6993.307264	15.056359	-0.059576	4.508955
298.947055	6985.259235	15.061363	-0.059623	4.506394
298.782150	6977.238586	15.066368	-0.059587	4.503839
298.667438	6969.293448	15.071373	-0.059560	4.501306
298.926931	6961.262127	15.076378	-0.059603	4.498746
299.055972	6953.248643	15.081383	-0.059622	4.496190
299.102267	6945.253427	15.086387	-0.059625	4.493638
298.816274	6937.292405	15.091392	-0.059567	4.491094
298.869130	6929.233955	15.096397	-0.059571	4.488518
298.593465	6921.293763	15.101402	-0.059514	4.485978
298.693497	6913.222448	15.106407	-0.059528	4.483396
298.489199	6905.318788	15.111411	-0.059484	4.480864
298.582235	6897.270415	15.116416	-0.059496	4.478287
298.855522	6889.212444	15.121421	-0.059542	4.475705
298.837974	6881.291603	15.126426	-0.059533	4.473165
298.641415	6873.295173	15.131431	-0.059492	4.470598
298.399481	6865.253536	15.136435	-0.059441	4.468015
298.872945	6857.159471	15.141440	-0.059524	4.465416
298.934912	6849.200366	15.146445	-0.059530	4.462858
299.034417	6841.234566	15.151450	-0.059543	4.460297
298.638404	6833.262479	15.156455	-0.059464	4.457729
298.943270	6825.194131	15.161459	-0.059516	4.455133
298.609048	6817.232443	15.166464	-0.059448	4.452566
298.344798	6809.204670	15.171469	-0.059394	4.449976
298.769011	6801.237357	15.176474	-0.059468	4.447408
299.059164	6793.128719	15.181479	-0.059516	4.444793
298.596821	6785.282631	15.186483	-0.059425	4.442256
298.506800	6777.229271	15.191488	-0.059403	4.439654
298.765269	6769.273258	15.196493	-0.059446	4.437083
298.666945	6761.174457	15.201498	-0.059422	4.434462
298.209844	6753.260237	15.206503	-0.059332	4.431898
298.288940	6745.190140	15.211507	-0.059341	4.429284
298.169842	6737.195693	15.216512	-0.059313	4.426693
298.201226	6729.141700	15.221517	-0.059314	4.424081
297.843415	6721.288013	15.226522	-0.059242	4.421531
298.013853	6713.161161	15.231527	-0.059268	4.418893
298.265260	6705.164430	15.236531	-0.059310	4.416297
298.099970	6697.201193	15.241536	-0.059274	4.413708
298.336783	6689.190036	15.246541	-0.059313	4.411104
298.351961	6681.140741	15.251546	-0.059310	4.408484
298.044050	6673.228958	15.256551	-0.059248	4.405906
298.058296	6665.198821	15.261555	-0.059245	4.403290
298.118431	6657.216598	15.266560	-0.059251	4.400688
297.753377	6649.246535	15.271565	-0.059178	4.398086
297.622262	6641.294837	15.276570	-0.059148	4.395489
297.939879	6633.176387	15.281575	-0.059202	4.392840
298.107572	6625.242458	15.286579	-0.059228	4.390249
297.933143	6617.225690	15.291584	-0.059190	4.387626
297.928849	6609.193092	15.296589	-0.059184	4.384998
297.980462	6601.280461	15.301594	-0.059188	4.382408
297.622178	6593.224898	15.306599	-0.059116	4.379767
298.016359	6585.244948	15.311603	-0.059184	4.377154
298.127895	6577.232873	15.316608	-0.059200	4.374527
298.127298	6569.244178	15.321613	-0.059194	4.371906
298.097642	6561.264721	15.326618	-0.059183	4.369285
298.274269	6553.248465	15.331623	-0.059211	4.366653
298.028705	6545.263480	15.336627	-0.059160	4.364026
297.837831	6537.334364	15.341632	-0.059119	4.361416
297.818663	6529.284811	15.346637	-0.059110	4.358767
297.906220	6521.364712	15.351642	-0.059121	4.356159
297.604930	6513.267937	15.356647	-0.059060	4.353488
297.701808	6505.259752	15.361651	-0.059072	4.350848
297.674076	6497.224322	15.366656	-0.059062	4.348197
297.679349	6489.220446	15.371661	-0.059058	4.345554
298.115278	6481.221569	15.376666	-0.059134	4.342915
297.674463	6473.242796	15.381671	-0.059046	4.340274
297.555554	6465.306558	15.386675	-0.059019	4.337648
297.622266	6457.271629	15.391680	-0.059026	4.334990
297.350269	6449.241467	15.396685	-0.058970	4.332328
297.827548	6441.232616	15.401690	-0.059053	4.329678
297.546037	6433.263459	15.406695	-0.058996	4.327034
297.323884	6425.221603	15.411699	-0.058949	4.324364
297.456399	6417.308364	15.416704	-0.058968	4.321738
297.546975	6409.244055	15.421709	-0.058980	4.319060
297.282235	6401.333787	15.426714	-0.058925	4.316428
297.157957	6393.247452	15.431719	-0.058897	4.313738
297.341447	6385.268828	15.436723	-0.058926	4.311084
297.147754	6377.246886	15.441728	-0.058884	4.308411
297.156216	6369.185301	15.446733	-0.058881	4.305725
297.322087	6361.248101	15.451738	-0.058906	4.303080
297.007781	6353.187402	15.456743	-0.058842	4.300388
297.274160	6345.239533	15.461747	-0.058887	4.297737
297.225702	6337.190152	15.466752	-0.058872	4.295047
297.235746	6329.237604	15.471757	-0.058869	4.292389
297.237467	6321.170773	15.476762	-0.058864	4.289691
297.169008	6313.221957	15.481767	-0.058846	4.287030
297.067380	6305.206351	15.486771	-0.058822	4.284345
297.085310	6297.246456	15.491776	-0.058820	4.281678
297.077147	6289.166606	15.496781	-0.058813	4.278969
297.172948	6281.271226	15.501786	-0.058825	4.276321
297.308717	6273.199200	15.506791	-0.058845	4.273612
297.150571	6265.216042	15.511795	-0.058811	4.270929
296.977297	6257.191065	15.516800	-0.058773	4.268229
296.971683	6249.183933	15.521805	-0.058767	4.265536
297.097570	6241.180751	15.526810	-0.058785	4.262844
297.085203	6233.194123	15.531815	-0.058777	4.260154
297.330595	6225.216849	15.536819	-0.058818	4.257468
297.030844	6217.211944	15.541824	-0.058756	4.254766
296.901933	6209.221855	15.546829	-0.058727	4.252068
296.893613	6201.186988	15.551834	-0.058720	4.249355
296.813800	6193.218587	15.556839	-0.058700	4.246662
296.848409	6185.156647	15.561843	-0.058701	4.243937
296.798487	6177.233521	15.566848	-0.058687	4.241256
296.817485	6169.170362	15.571853	-0.058685	4.238527
296.862359	6161.229517	15.576858	-0.058688	4.235837
296.670904	6153.211898	15.581863	-0.058647	4.233118
296.526833	6145.219166	15.586867	-0.058615	4.230405
296.387007	6137.203902	15.591872	-0.058584	4.227684
296.546014	6129.117106	15.596877	-0.058608	4.224939
296.661200	6121.192148	15.601882	-0.058624	4.222247
296.348813	6113.189834	15.606887	-0.058561	4.219523
296.675345	6105.203879	15.611891	-0.058616	4.216809
296.554341	6097.147938	15.616896	-0.058588	4.214065
296.443106	6089.167513	15.621901	-0.058562	4.211345
296.122977	6081.221270	15.626906	-0.058497	4.208632
296.479425	6073.131226	15.631911	-0.058558	4.205876
296.616550	6065.173553	15.636915	-0.058579	4.203161
296.222237	6057.224477	15.641920	-0.058500	4.200441
296.361265	6049.209469	15.646925	-0.058520	4.197703
296.365241	6041.194262	15.651930	-0.058516	4.194962
296.099764	6033.179969	15.656935	-0.058461	4.192216
296.335209	6025.110742	15.661939	-0.058500	4.189455
296.239587	6017.115729	15.666944	-0.058476	4.186714
296.310550	6009.093732	15.671949	-0.058484	4.183964
295.875331	6001.252277	15.676954	-0.058398	4.181268
295.840027	5993.157318	15.681959	-0.058386	4.178487
296.124159	5985.159860	15.686963	-0.058434	4.175743
296.380223	5977.164933	15.691968	-0.058476	4.172997
295.933102	5969.176158	15.696973	-0.058388	4.170243
296.062613	5961.178192	15.701978	-0.058406	4.167491
296.248038	5953.140840	15.706983	-0.058436	4.164724
296.270085	5945.217072	15.711987	-0.058434	4.161993
295.754125	5937.217994	15.716992	-0.058333	4.159227
296.035425	5929.213784	15.721997	-0.058380	4.156467
295.637224	5921.252840	15.727002	-0.058301	4.153712
295.659734	5913.219238	15.732007	-0.058300	4.150935
295.730727	5905.181058	15.737011	-0.058307	4.148156
295.766021	5897.170338	15.742016	-0.058309	4.145383
295.771275	5889.186840	15.747021	-0.058304	4.142618
295.957404	5881.202641	15.752026	-0.058334	4.139853
295.651410	5873.252578	15.757031	-0.058272	4.137092
295.689638	5865.189408	15.762035	-0.058273	4.134294
295.733826	5857.189867	15.767040	-0.058276	4.131516
295.925532	5849.169267	15.772045	-0.058307	4.128732
295.892001	5841.249019	15.777050	-0.058295	4.125977
295.551656	5833.202715	15.782055	-0.058226	4.123172
295.802818	5825.223683	15.787059	-0.058268	4.120397
295.750112	5817.235190	15.792064	-0.058253	4.117612
295.513989	5809.210260	15.797069	-0.058203	4.114811
295.141140	5801.296581	15.802074	-0.058129	4.112044
295.029225	5793.203541	15.807079	-0.058103	4.109216
295.133188	5785.184153	15.812083	-0.058117	4.106415
294.805497	5777.212837	15.817088	-0.058050	4.103623
295.249863	5769.168999	15.822093	-0.058128	4.100815
295.508835	5761.204103	15.827098	-0.058171	4.098030
295.155901	5753.184381	15.832103	-0.058100	4.095215
295.116671	5745.207997	15.837107	-0.058087	4.092418
294.627260	5737.243477	15.842112	-0.057991	4.089616
295.092670	5729.137820	15.847117	-0.058072	4.086777
294.695442	5721.220604	15.852122	-0.057993	4.083989
295.038079	5713.199463	15.857127	-0.058051	4.081174
294.872805	5705.201821	15.862131	-0.058015	4.078358
294.780356	5697.235913	15.867136	-0.057993	4.075552
294.867414	5689.196067	15.872141	-0.058003	4.072720
294.599578	5681.219604	15.877146	-0.057948	4.069904
294.557824	5673.200934	15.882151	-0.057935	4.067074
294.266555	5665.197863	15.887155	-0.057876	4.064244
294.470675	5657.230921	15.892160	-0.057908	4.061432
294.533481	5649.159115	15.897165	-0.057915	4.058579
294.674393	5641.197132	15.902170	-0.057936	4.055765
295.098166	5633.146098	15.907175	-0.058009	4.052921
294.963956	5625.172974	15.912179	-0.057979	4.050094
294.825207	5617.224168	15.917184	-0.057948	4.047273
294.891970	5609.152101	15.922189	-0.057955	4.044411
295.281348	5601.249611	15.927194	-0.058022	4.041611
295.006242	5593.224444	15.932199	-0.057966	4.038755
294.928022	5585.257559	15.937203	-0.057946	4.035922
295.102933	5577.162813	15.942208	-0.057973	4.033044
295.040011	5569.121510	15.947213	-0.057956	4.030180
294.843114	5561.206878	15.952218	-0.057914	4.027357
294.659594	5553.182603	15.957223	-0.057875	4.024493
294.869602	5545.217553	15.962227	-0.057908	4.021654
294.822502	5537.214109	15.967232	-0.057894	4.018796
294.745120	5529.209945	15.972237	-0.057875	4.015934
294.819516	5521.255004	15.977242	-0.057883	4.013091
294.937283	5513.184137	15.982247	-0.057900	4.010205
294.626161	5505.254437	15.987251	-0.057837	4.007361
295.046552	5497.181557	15.992256	-0.057909	4.004475
294.951499	5489.248646	15.997261	-0.057886	4.001629
294.977727	5481.275594	16.002266	-0.057886	3.998768
294.939054	5473.252278	16.007271	-0.057874	3.995886
294.929053	5465.255965	16.012275	-0.057866	3.993012
294.672567	5457.262650	16.017280	-0.057813	3.990133
294.661439	5449.258908	16.022285	-0.057806	3.987252
294.772005	5441.261932	16.027290	-0.057821	3.984374
294.690864	5433.291383	16.032295	-0.057801	3.981500
294.394729	5425.271486	16.037299	-0.057740	3.978602
294.501821	5417.271294	16.042304	-0.057755	3.975717
294.640815	5409.228627	16.047309	-0.057776	3.972814
294.654259	5401.240366	16.052314	-0.057773	3.969927
294.396291	5393.266356	16.057319	-0.057719	3.967038
294.656521	5385.226484	16.062323	-0.057763	3.964132
294.654333	5377.310773	16.067328	-0.057757	3.961264
294.401953	5369.244764	16.072333	-0.057705	3.958336
294.631614	5361.263515	16.077338	-0.057742	3.955444
294.292469	5353.263798	16.082343	-0.057674	3.952534
294.223991	5345.260529	16.087347	-0.057656	3.949625
294.219334	5337.241879	16.092352	-0.057649	3.946709
294.126401	5329.204568	16.097357	-0.057627	3.943783
293.959538	5321.309092	16.102362	-0.057590	3.940905
293.719936	5313.275091	16.107367	-0.057540	3.937972
293.777954	5305.313774	16.112371	-0.057546	3.935070
293.942022	5297.285190	16.117376	-0.057571	3.932143
293.928731	5289.203503	16.122381	-0.057563	3.929192
293.853442	5281.290000	16.127386	-0.057544	3.926298
293.748961	5273.266172	16.132391	-0.057519	3.923361
293.591675	5265.298962	16.137395	-0.057485	3.920441
293.817081	5257.290893	16.142400	-0.057521	3.917512
293.992908	5249.241157	16.147405	-0.057549	3.914565
294.076541	5241.304461	16.152410	-0.057559	3.911655
293.883121	5233.294256	16.157415	-0.057518	3.908710
293.846714	5225.282513	16.162419	-0.057506	3.905766
293.949693	5217.304897	16.167424	-0.057520	3.902835
293.625159	5209.337078	16.172429	-0.057454	3.899896
293.739059	5201.360703	16.177434	-0.057470	3.896961
293.725611	5193.323624	16.182439	-0.057462	3.893999
293.152984	5185.436926	16.187443	-0.057350	3.891079
292.828960	5177.413264	16.192448	-0.057284	3.888111
292.888391	5169.362733	16.197453	-0.057290	3.885138
293.304322	5161.351648	16.202458	-0.057362	3.882185
293.208503	5153.285706	16.207463	-0.057339	3.879200
293.249395	5145.397052	16.212467	-0.057341	3.876280
293.083181	5137.308683	16.217472	-0.057305	3.873280
293.275749	5129.198797	16.222477	-0.057336	3.870277
293.476101	5121.193085	16.227482	-0.057368	3.867310
293.515139	5113.227833	16.232487	-0.057370	3.864353
293.371857	5105.316871	16.237491	-0.057338	3.861410
293.310241	5097.321741	16.242496	-0.057321	3.858435
293.251646	5089.324252	16.247501	-0.057305	3.855457
293.307005	5081.359073	16.252506	-0.057310	3.852491
293.032954	5073.324487	16.257511	-0.057253	3.849490
293.048804	5065.367281	16.262515	-0.057251	3.846521
292.909876	5057.342492	16.267520	-0.057220	3.843522
292.927236	5049.350807	16.272525	-0.057218	3.840536
292.918132	5041.367723	16.277530	-0.057211	3.837550
292.983911	5033.322246	16.282535	-0.057218	3.834541
292.382776	5025.459100	16.287539	-0.057101	3.831582
292.306635	5017.399677	16.292544	-0.057081	3.828560
292.771385	5009.287881	16.297549	-0.057162	3.825527
292.911454	5001.342169	16.302554	-0.057183	3.822547
292.887934	4993.338464	16.307559	-0.057173	3.819539
293.152640	4985.344526	16.312563	-0.057217	3.816539
293.124657	4977.336246	16.317568	-0.057207	3.813525
293.010958	4969.363524	16.322573	-0.057180	3.810520
292.885746	4961.387083	16.327578	-0.057152	3.807511
292.836999	4953.345346	16.332583	-0.057137	3.804476
292.668871	4945.452081	16.337587	-0.057101	3.801492
292.864952	4937.386692	16.342592	-0.057132	3.798450
292.633533	4929.439762	16.347597	-0.057084	3.795439
292.582956	4921.464194	16.352602	-0.057069	3.792420
292.495896	4913.395904	16.357607	-0.057047	3.789362
292.346975	4905.463978	16.362611	-0.057014	3.786352
292.618106	4897.356008	16.367616	-0.057059	3.783283
292.518359	4889.401758	16.372621	-0.057036	3.780261
292.508572	4881.449113	16.377626	-0.057028	3.777239
292.182706	4873.450450	16.382631	-0.056962	3.774190
292.424068	4865.471907	16.387635	-0.057002	3.771159
292.494383	4857.410510	16.392640	-0.057010	3.768091
292.465426	4849.388141	16.397645	-0.056999	3.765032
292.112230	4841.503340	16.402650	-0.056928	3.762016
291.989566	4833.464842	16.407655	-0.056900	3.758944
292.270485	4825.494577	16.412659	-0.056947	3.755905
292.381989	4817.461529	16.417664	-0.056962	3.752836
292.361481	4809.428005	16.422669	-0.056953	3.749761
292.321146	4801.475690	16.427674	-0.056941	3.746714
292.566433	4793.423479	16.432679	-0.056981	3.743633
292.687743	4785.455787	16.437683	-0.056998	3.740579
292.367220	4777.502169	16.442688	-0.056933	3.737517
292.215348	4769.463007	16.447693	-0.056900	3.734423
292.207254	4761.535573	16.452698	-0.056893	3.731374
292.062813	4753.521430	16.457703	-0.056861	3.728286
292.207710	4745.476320	16.462707	-0.056882	3.725190
292.253267	4737.512385	16.467712	-0.056885	3.722120
292.213816	4729.464400	16.472717	-0.056873	3.719014
292.118367	4721.547278	16.477722	-0.056850	3.715953
291.993117	4713.469168	16.482727	-0.056821	3.712828
292.081167	4705.453047	16.487731	-0.056832	3.709729
292.140376	4697.458420	16.492736	-0.056838	3.706635
291.893528	4689.466045	16.497741	-0.056787	3.703531
292.071561	4681.512206	16.502746	-0.056814	3.700451
291.940742	4673.520665	16.507751	-0.056785	3.697346
292.038406	4665.489895	16.512755	-0.056798	3.694228
291.982248	4657.544541	16.517760	-0.056782	3.691138
291.981970	4649.487389	16.522765	-0.056777	3.688002
291.674360	4641.564665	16.527770	-0.056714	3.684908
291.578685	4633.577372	16.532775	-0.056691	3.681792
291.834402	4625.531943	16.537779	-0.056733	3.678660
291.933360	4617.550418	16.542784	-0.056746	3.675546
291.651999	4609.546007	16.547789	-0.056689	3.672411
291.579973	4601.590703	16.552794	-0.056670	3.669297
291.531499	4593.598303	16.557799	-0.056656	3.666167
291.304784	4585.632347	16.562803	-0.056608	3.663040
291.429027	4577.627286	16.567808	-0.056626	3.659904
291.146029	4569.648831	16.572813	-0.056568	3.656765
291.212059	4561.606755	16.577818	-0.056575	3.653607
291.061295	4553.624983	16.582823	-0.056542	3.650465
291.148617	4545.637299	16.587827	-0.056553	3.647324
291.180236	4537.598604	16.592832	-0.056553	3.644159
291.134277	4529.643649	16.597837	-0.056539	3.641022
291.286243	4521.652207	16.602842	-0.056562	3.637874
291.102845	4513.667870	16.607847	-0.056523	3.634716
291.010520	4505.666666	16.612851	-0.056500	3.631551
291.253828	4497.611297	16.617856	-0.056540	3.628372
291.143013	4489.608095	16.622861	-0.056514	3.625200
290.960325	4481.705347	16.627866	-0.056475	3.622063
291.080227	4473.631039	16.632871	-0.056492	3.618864
290.985264	4465.687126	16.637875	-0.056469	3.615708
290.538767	4457.752220	16.642880	-0.056381	3.612543
290.510844	4449.681705	16.647885	-0.056370	3.609333
290.804789	4441.687354	16.652890	-0.056420	3.606160
290.736010	4433.665423	16.657895	-0.056401	3.602962
290.583365	4425.689693	16.662899	-0.056368	3.599778
290.593722	4417.730186	16.667904	-0.056364	3.596602
290.848036	4409.658882	16.672909	-0.056406	3.593385
290.727954	4401.713785	16.677914	-0.056379	3.590206
290.486489	4393.717738	16.682919	-0.056328	3.586999
290.844687	4385.681925	16.687923	-0.056390	3.583792
291.080638	4377.707439	16.692928	-0.056428	3.580602
290.852042	4369.702422	16.697933	-0.056381	3.577384
290.872265	4361.731102	16.702938	-0.056379	3.574183
290.686073	4353.781686	16.707943	-0.056339	3.570983
290.374412	4345.796211	16.712947	-0.056276	3.567761
290.013899	4337.831095	16.717952	-0.056203	3.564543
290.426173	4329.809279	16.722957	-0.056275	3.561322
290.609922	4321.794130	16.727962	-0.056304	3.558095
290.368802	4313.827082	16.732967	-0.056254	3.554871
290.350920	4305.769226	16.737971	-0.056245	3.551614
290.413743	4297.744992	16.742976	-0.056251	3.548370
290.051800	4289.754550	16.747981	-0.056179	3.545124
290.587351	4281.758666	16.752986	-0.056273	3.541900
290.262332	4273.824750	16.757991	-0.056207	3.538672
290.264503	4265.801407	16.762995	-0.056202	3.535415
290.498092	4257.790538	16.768000	-0.056240	3.532167
290.455047	4249.751686	16.773005	-0.056227	3.528896
290.226121	4241.885822	16.778010	-0.056179	3.525687
290.032262	4233.881275	16.783015	-0.056138	3.522419
289.923155	4225.876841	16.788019	-0.056112	3.519151
289.848437	4217.957459	16.793024	-0.056093	3.515915
289.783365	4209.856776	16.798029	-0.056076	3.512603
290.048679	4201.868908	16.803034	-0.056120	3.509345
289.790999	4193.872577	16.808039	-0.056066	3.506063
290.009099	4185.855999	16.813043	-0.056102	3.502785
290.283582	4177.815713	16.818048	-0.056147	3.499497
289.933042	4169.890481	16.823053	-0.056077	3.496232
289.726685	4161.961291	16.828058	-0.056033	3.492967
289.599722	4153.946003	16.833063	-0.056004	3.489666
289.935654	4145.886776	16.838067	-0.056062	3.486359
289.653600	4137.968108	16.843072	-0.056004	3.483086
289.503248	4129.958626	16.848077	-0.055970	3.479778
289.512345	4121.992309	16.853082	-0.055967	3.476489
289.634213	4113.947364	16.858087	-0.055984	3.473168
288.921495	4106.048069	16.863091	-0.055846	3.469877
288.916114	4098.019075	16.868096	-0.055840	3.466552
289.233464	4089.909690	16.873101	-0.055894	3.463202
289.021735	4082.003273	16.878106	-0.055849	3.459915
289.425177	4073.952536	16.883111	-0.055919	3.456586
289.641165	4065.940558	16.888115	-0.055954	3.453263
289.333063	4058.023665	16.893120	-0.055891	3.449958
289.435633	4049.975657	16.898125	-0.055905	3.446610
289.364544	4042.029913	16.903130	-0.055886	3.443296
289.251286	4034.066192	16.908135	-0.055860	3.439969
289.337192	4026.056299	16.913139	-0.055871	3.436627
289.280193	4018.066832	16.918144	-0.055855	3.433284
289.246045	4010.068352	16.923149	-0.055843	3.429936
289.039274	4002.115264	16.928154	-0.055799	3.426597
288.829845	3994.075736	16.933159	-0.055755	3.423219
288.745029	3986.129665	16.938163	-0.055734	3.419881
289.283545	3978.072690	16.943168	-0.055829	3.416515
288.567617	3970.154738	16.948173	-0.055690	3.413160
288.135878	3962.194877	16.953178	-0.055605	3.409794
287.894871	3954.225396	16.958183	-0.055554	3.406427
288.413961	3946.127417	16.963187	-0.055646	3.403030
288.318453	3938.137046	16.968192	-0.055623	3.399653
288.492075	3930.148622	16.973197	-0.055650	3.396283
288.627535	3922.104937	16.978202	-0.055670	3.392885
288.663960	3914.063024	16.983207	-0.055671	3.389481
288.641730	3906.072508	16.988211	-0.055662	3.386093
288.859178	3898.114910	16.993216	-0.055697	3.382724
288.496062	3890.174962	16.998221	-0.055624	3.379338
288.956887	3882.121799	17.003226	-0.055704	3.375931
288.823193	3874.158277	17.008231	-0.055674	3.372537
288.649240	3866.185105	17.013235	-0.055636	3.369134
288.786698	3858.199479	17.018240	-0.055657	3.365733
288.536187	3850.243377	17.023245	-0.055605	3.362328
288.858773	3842.232071	17.028250	-0.055660	3.358916
288.045787	3834.379595	17.033255	-0.055503	3.355527
288.631098	3826.261465	17.038259	-0.055607	3.352072
288.611460	3818.256503	17.043264	-0.055598	3.348640
288.335790	3810.280224	17.048269	-0.055541	3.345207
288.690763	3802.289788	17.053274	-0.055602	3.341789
288.573430	3794.270214	17.058279	-0.055575	3.338336
288.527619	3786.317878	17.063283	-0.055561	3.334912
288.617999	3778.324651	17.068288	-0.055572	3.331471
288.729438	3770.287838	17.073293	-0.055588	3.328009
289.031078	3762.280601	17.078298	-0.055639	3.324564
288.731056	3754.390422	17.083303	-0.055578	3.321142
288.590473	3746.396808	17.088307	-0.055546	3.317678
288.523641	3738.394875	17.093312	-0.055528	3.314210
288.758594	3730.353930	17.098317	-0.055567	3.310733
288.815499	3722.351108	17.103322	-0.055572	3.307262
288.540587	3714.390372	17.108327	-0.055516	3.303793
288.580825	3706.426690	17.113331	-0.055518	3.300331
288.507017	3698.456659	17.118336	-0.055499	3.296858
287.984400	3690.495967	17.123341	-0.055396	3.293367
288.156669	3682.474645	17.128346	-0.055423	3.289874
288.108695	3674.459103	17.133351	-0.055409	3.286371
287.943505	3666.475041	17.138355	-0.055373	3.282874
287.801096	3658.568763	17.143360	-0.055341	3.279407
287.681527	3650.581928	17.148365	-0.055313	3.275903
287.818133	3642.570046	17.153370	-0.055333	3.272394
287.585077	3634.522084	17.158375	-0.055285	3.268851
287.719711	3626.519795	17.163379	-0.055304	3.265338
287.768096	3618.548973	17.168384	-0.055308	3.261833
287.432297	3610.573662	17.173389	-0.055240	3.258306
288.017438	3602.533813	17.178394	-0.055344	3.254784
287.626173	3594.597368	17.183399	-0.055266	3.251264
287.258774	3586.601110	17.188403	-0.055192	3.247714
287.852669	3578.545231	17.193408	-0.055297	3.244175
287.255400	3570.700283	17.198413	-0.055181	3.240675
287.606390	3562.642969	17.203418	-0.055241	3.237117
287.845873	3554.572563	17.208423	-0.055280	3.233544
287.699010	3546.629042	17.213427	-0.055248	3.230008
287.748020	3538.621681	17.218432	-0.055251	3.226448
287.761496	3530.616713	17.223437	-0.055249	3.222883
287.712616	3522.658038	17.228442	-0.055234	3.219332
287.351634	3514.759676	17.233447	-0.055162	3.215791
287.139685	3506.766541	17.238451	-0.055117	3.212210
287.172644	3498.719166	17.243456	-0.055118	3.208612
287.320533	3490.664876	17.248461	-0.055140	3.205011
287.254098	3482.729299	17.253466	-0.055122	3.201450
287.358752	3474.722115	17.258471	-0.055137	3.197860
287.239511	3466.753867	17.263475	-0.055109	3.194274
287.138688	3458.815038	17.268480	-0.055085	3.190698
287.326519	3450.749049	17.273485	-0.055115	3.187074
287.265514	3442.781412	17.278490	-0.055098	3.183478
287.423118	3434.743429	17.283495	-0.055122	3.179857
287.018596	3426.881996	17.288499	-0.055041	3.176286
287.386025	3418.813337	17.293504	-0.055105	3.172652
287.222230	3410.819635	17.298509	-0.055069	3.169024
287.054740	3402.878883	17.303514	-0.055032	3.165415
287.252978	3394.870704	17.308519	-0.055064	3.161789
287.232263	3386.889105	17.313523	-0.055055	3.158160
287.478588	3378.892347	17.318528	-0.055095	3.154532
286.963627	3370.959537	17.323533	-0.054994	3.150895
287.327851	3362.908518	17.328538	-0.055057	3.147239
286.807882	3354.977158	17.333543	-0.054955	3.143594
286.969064	3346.964865	17.338547	-0.054979	3.139939
287.149893	3338.968044	17.343552	-0.055008	3.136287
287.021103	3330.965798	17.348557	-0.054978	3.132614
287.046688	3322.974535	17.353562	-0.054978	3.128949
287.083892	3314.986703	17.358567	-0.054979	3.125282
286.758169	3307.082064	17.363571	-0.054914	3.121632
286.721476	3299.106871	17.368576	-0.054901	3.117959
286.587676	3291.091336	17.373581	-0.054871	3.114258
286.369310	3283.135199	17.378586	-0.054825	3.110576
285.948818	3275.180725	17.383591	-0.054742	3.106881
286.130929	3267.147064	17.388595	-0.054770	3.103174
286.598154	3259.061560	17.393600	-0.054852	3.099451
286.803914	3251.097653	17.398605	-0.054885	3.095768
286.615837	3243.147734	17.403610	-0.054845	3.092068
286.810472	3235.076290	17.408615	-0.054875	3.088326
286.682796	3227.130052	17.413619	-0.054846	3.084622
286.730257	3219.220971	17.418624	-0.054850	3.080939
286.481252	3211.253515	17.423629	-0.054798	3.077211
286.089314	3203.314592	17.428634	-0.054720	3.073484
285.948236	3195.260167	17.433639	-0.054689	3.069711
286.047303	3187.232847	17.438643	-0.054702	3.065957
286.254065	3179.229434	17.443648	-0.054735	3.062215
286.392136	3171.210926	17.448653	-0.054755	3.058459
286.383964	3163.283156	17.453658	-0.054748	3.054733
285.874438	3155.339756	17.458663	-0.054648	3.050971
286.091554	3147.297388	17.463667	-0.054683	3.047193
286.204813	3139.316768	17.468672	-0.054699	3.043434
286.060628	3131.349161	17.473677	-0.054667	3.039664
285.772576	3123.460077	17.478682	-0.054608	3.035920
286.010644	3115.389742	17.483687	-0.054647	3.032111
286.077555	3107.372485	17.488691	-0.054654	3.028314
286.228192	3099.371525	17.493696	-0.054677	3.024524
286.045953	3091.460391	17.498701	-0.054638	3.020755
286.076782	3083.497948	17.503706	-0.054638	3.016968
285.740309	3075.513111	17.508711	-0.054570	3.013147
285.716260	3067.503376	17.513715	-0.054561	3.009326
286.165593	3059.477542	17.518720	-0.054639	3.005515
285.867046	3051.540212	17.523725	-0.054578	3.001704
285.229820	3043.689098	17.528730	-0.054454	2.997912
285.547286	3035.583896	17.533735	-0.054508	2.994042
285.745278	3027.571375	17.538739	-0.054540	2.990206
285.565438	3019.625901	17.543744	-0.054501	2.986378
285.436891	3011.606747	17.548749	-0.054472	2.982511
285.820093	3003.590080	17.553754	-0.054538	2.978668
285.751297	2995.625326	17.558759	-0.054519	2.974821
285.760719	2987.641130	17.563763	-0.054516	2.970964
285.868024	2979.647648	17.568768	-0.054531	2.967102
285.768190	2971.688325	17.573773	-0.054507	2.963241
285.899139	2963.728446	17.578778	-0.054526	2.959387
285.762288	2955.768900	17.583783	-0.054495	2.955514
285.678571	2947.785827	17.588787	-0.054474	2.951627
285.453982	2939.803753	17.593792	-0.054427	2.947728
285.531659	2931.787051	17.598797	-0.054436	2.943823
285.725234	2923.823803	17.603802	-0.054467	2.939945
285.816758	2915.840714	17.608807	-0.054479	2.936047
285.491171	2907.889314	17.613811	-0.054413	2.932136
285.600609	2899.877735	17.618816	-0.054428	2.928215
285.608499	2891.867093	17.623821	-0.054424	2.924283
285.560026	2883.971851	17.628826	-0.054410	2.920400
285.312400	2875.999587	17.633831	-0.054358	2.916462
285.334542	2867.966441	17.638835	-0.054357	2.912504
285.236993	2859.960700	17.643840	-0.054334	2.908548
284.951051	2851.977462	17.648845	-0.054275	2.904586
284.784747	2844.079522	17.653850	-0.054239	2.900669
284.813758	2836.067219	17.658855	-0.054239	2.896700
284.793535	2828.042486	17.663859	-0.054230	2.892716
284.692701	2820.084336	17.668864	-0.054206	2.888756
284.345776	2812.144167	17.673869	-0.054136	2.884785
284.375143	2804.172685	17.678874	-0.054136	2.880815
284.630270	2796.131029	17.683879	-0.054178	2.876816
284.967180	2788.091785	17.688883	-0.054236	2.872818
284.937440	2780.128801	17.693888	-0.054225	2.868832
284.771172	2772.168119	17.698893	-0.054189	2.864834
284.978473	2764.212839	17.703898	-0.054222	2.860854
285.142776	2756.192077	17.708903	-0.054247	2.856833
284.951526	2748.265874	17.713907	-0.054206	2.852834
284.989011	2740.265305	17.718912	-0.054208	2.848805
284.521008	2732.344424	17.723917	-0.054116	2.844781
284.496066	2724.410120	17.728922	-0.054106	2.840770
284.629435	2716.372670	17.733927	-0.054125	2.836710
284.597388	2708.402627	17.738931	-0.054114	2.832669
284.320419	2700.460525	17.743936	-0.054057	2.828623
284.501908	2692.380015	17.748941	-0.054086	2.824527
284.884283	2684.390258	17.753946	-0.054152	2.820483
284.869860	2676.429561	17.758951	-0.054144	2.816424
284.568586	2668.485517	17.763955	-0.054082	2.812352
284.927066	2660.451436	17.768960	-0.054144	2.808266
284.762256	2652.500743	17.773965	-0.054108	2.804187
284.494206	2644.623043	17.778970	-0.054053	2.800132
284.711519	2636.584141	17.783975	-0.054088	2.796018
285.027856	2628.547182	17.788979	-0.054141	2.791905
284.843470	2620.620562	17.793984	-0.054102	2.787812
284.639672	2612.641415	17.798989	-0.054058	2.783685
284.542136	2604.729375	17.803994	-0.054035	2.779593
284.483622	2596.746030	17.808999	-0.054019	2.775460
284.530791	2588.755514	17.814003	-0.054022	2.771324
284.559880	2580.773623	17.819008	-0.054022	2.767185
284.274826	2572.813815	17.824013	-0.053964	2.763033
284.515187	2564.821834	17.829018	-0.054004	2.758889
284.311456	2556.860929	17.834023	-0.053960	2.754728
284.481878	2548.821040	17.839027	-0.053987	2.750543
283.817902	2540.955359	17.844032	-0.053858	2.746390
283.556231	2532.961575	17.849037	-0.053804	2.742189
284.160879	2524.909972	17.854042	-0.053911	2.738006
283.958486	2516.963373	17.859047	-0.053868	2.733820
283.875910	2508.976132	17.864051	-0.053847	2.729615
283.763340	2501.017878	17.869056	-0.053821	2.725416
284.025452	2492.994357	17.874061	-0.053865	2.721200
283.741574	2485.117390	17.879066	-0.053807	2.717020
283.542895	2477.128052	17.884071	-0.053764	2.712780
283.387045	2469.147318	17.889075	-0.053730	2.708540
283.442938	2461.149421	17.894080	-0.053735	2.704298
283.514597	2453.175622	17.899085	-0.053743	2.700064
283.920298	2445.145602	17.904090	-0.053813	2.695814
283.846907	2437.176338	17.909095	-0.053794	2.691559
283.404014	2429.274658	17.914099	-0.053707	2.687309
283.289185	2421.340453	17.919104	-0.053680	2.683057
282.924392	2413.400539	17.924109	-0.053607	2.678778
283.160278	2405.384883	17.929114	-0.053645	2.674491
282.948137	2397.393926	17.934119	-0.053601	2.670181
283.162775	2389.371118	17.939123	-0.053635	2.665876
283.628574	2381.333726	17.944128	-0.053717	2.661572
283.596695	2373.375559	17.949133	-0.053706	2.657270
283.560522	2365.461378	17.954138	-0.053694	2.652986
283.658367	2357.461131	17.959143	-0.053706	2.648656
283.164821	2349.570362	17.964147	-0.053609	2.644340
282.930215	2341.658089	17.969152	-0.053560	2.640022
282.852676	2333.683839	17.974157	-0.053541	2.635673
283.463651	2325.591158	17.979162	-0.053649	2.631300
282.963365	2317.694755	17.984167	-0.053551	2.626951
283.148300	2309.669842	17.989171	-0.053580	2.622571
282.964841	2301.748047	17.994176	-0.053540	2.618215
282.691237	2293.810203	17.999181	-0.053484	2.613837
282.704464	2285.816708	18.004186	-0.053481	2.609441
282.966499	2277.792713	18.009191	-0.053525	2.605037
282.879607	2269.855646	18.014195	-0.053503	2.600650
283.191467	2261.862648	18.019200	-0.053556	2.596253
283.012184	2253.840438	18.024205	-0.053517	2.591797
283.155116	2245.817870	18.029210	-0.053539	2.587356
282.913600	2237.903905	18.034215	-0.053488	2.582941
282.894161	2229.939347	18.039219	-0.053480	2.578506
283.053995	2221.967999	18.044224	-0.053504	2.574072
282.967788	2214.015015	18.049229	-0.053483	2.569623
282.999516	2206.057504	18.054234	-0.053483	2.565172
283.171971	2198.080546	18.059239	-0.053510	2.560713
282.919920	2190.190151	18.064243	-0.053458	2.556264
282.811769	2182.241739	18.069248	-0.053433	2.551785
282.649216	2174.260060	18.074253	-0.053397	2.547275
282.688199	2166.288049	18.079258	-0.053399	2.542778
282.431133	2158.363154	18.084263	-0.053346	2.538278
281.931159	2150.445155	18.089267	-0.053248	2.533755
281.923740	2142.459486	18.094272	-0.053241	2.529223
281.851313	2134.454273	18.099277	-0.053222	2.524666
281.885420	2126.505649	18.104282	-0.053223	2.520141
282.071261	2118.491794	18.109287	-0.053252	2.515581
282.290571	2110.473824	18.114291	-0.053288	2.511014
282.213707	2102.516073	18.119296	-0.053268	2.506451
282.138342	2094.549555	18.124301	-0.053249	2.501875
282.025824	2086.658653	18.129306	-0.053223	2.497330
282.047562	2078.658788	18.134311	-0.053222	2.492725
282.032461	2070.682277	18.139315	-0.053213	2.488122
282.128680	2062.712458	18.144320	-0.053226	2.483523
281.883731	2054.783671	18.149325	-0.053175	2.478913
281.631250	2046.881251	18.154330	-0.053123	2.474310
281.800215	2038.868607	18.159335	-0.053149	2.469665
282.115474	2030.839906	18.164339	-0.053203	2.465014
281.751504	2022.949251	18.169344	-0.053129	2.460383
281.930539	2014.941256	18.174349	-0.053158	2.455716
282.065112	2006.986456	18.179354	-0.053177	2.451068
281.612165	1999.105464	18.184359	-0.053088	2.446408
281.278590	1991.168516	18.189363	-0.053020	2.441716
281.408853	1983.202465	18.194368	-0.053039	2.437034
281.275086	1975.215081	18.199373	-0.053009	2.432310
280.850143	1967.289666	18.204378	-0.052925	2.427591
281.026548	1959.247193	18.209383	-0.052952	2.422840
281.200623	1951.256410	18.214387	-0.052979	2.418110
281.577781	1943.252442	18.219392	-0.053044	2.413379
281.394025	1935.310683	18.224397	-0.053005	2.408632
281.758557	1927.306283	18.229402	-0.053067	2.403881
280.866107	1919.537429	18.234407	-0.052896	2.399162
280.983260	1911.537205	18.239411	-0.052913	2.394375
281.427020	1903.501685	18.244416	-0.052990	2.389584
281.466849	1895.512564	18.249421	-0.052992	2.384779
280.969915	1887.691566	18.254426	-0.052894	2.380021
281.444458	1879.633726	18.259431	-0.052977	2.375191
281.203097	1871.712768	18.264435	-0.052927	2.370374
281.405576	1863.728132	18.269440	-0.052959	2.365546
281.407824	1855.779898	18.274445	-0.052955	2.360713
281.726730	1847.809765	18.279450	-0.053009	2.355884
281.760658	1839.844977	18.284455	-0.053010	2.351024
281.305739	1831.973431	18.289459	-0.052920	2.346170
281.357786	1823.989260	18.294464	-0.052924	2.341280
281.211974	1816.067291	18.299469	-0.052892	2.336401
281.259266	1808.116536	18.304474	-0.052895	2.331510
281.360770	1800.111296	18.309479	-0.052909	2.326580
281.261845	1792.169364	18.314483	-0.052885	2.321661
281.086348	1784.277995	18.319488	-0.052847	2.316757
280.750525	1776.361959	18.324493	-0.052780	2.311814
280.584159	1768.429446	18.329498	-0.052743	2.306864
280.446365	1760.462354	18.334503	-0.052712	2.301884
280.293391	1752.528156	18.339507	-0.052679	2.296913
280.344418	1744.535940	18.344512	-0.052683	2.291912
280.401643	1736.546596	18.349517	-0.052688	2.286903
280.740309	1728.544826	18.354522	-0.052746	2.281899
280.646196	1720.635089	18.359527	-0.052723	2.276905
280.605390	1712.689928	18.364531	-0.052710	2.271881
280.487675	1704.734653	18.369536	-0.052683	2.266834
280.182320	1696.796317	18.374541	-0.052621	2.261769
280.490184	1688.814799	18.379546	-0.052673	2.256720
280.337434	1680.876711	18.384551	-0.052639	2.251646
279.846999	1673.010020	18.389555	-0.052543	2.246577
279.900854	1665.032945	18.394560	-0.052547	2.241473
280.224333	1657.013754	18.399565	-0.052602	2.236356
280.677793	1649.028811	18.404570	-0.052682	2.231260
280.080977	1641.174175	18.409575	-0.052565	2.226142
280.504264	1633.157197	18.414579	-0.052639	2.221000
280.482022	1625.252456	18.419584	-0.052629	2.215878
280.336406	1617.304430	18.424589	-0.052597	2.210704
280.471861	1609.359727	18.429594	-0.052617	2.205547
280.376521	1601.449016	18.434599	-0.052594	2.200378
280.037988	1593.551182	18.439603	-0.052526	2.195183
280.081315	1585.595603	18.444608	-0.052528	2.189973
280.157062	1577.606349	18.449613	-0.052537	2.184732
280.100066	1569.698451	18.454618	-0.052521	2.179519
280.043101	1561.759419	18.459623	-0.052505	2.174273
280.197548	1553.777533	18.464627	-0.052529	2.169006
279.999273	1545.874570	18.469632	-0.052487	2.163745
279.833916	1537.960678	18.474637	-0.052451	2.158467
279.980224	1530.021271	18.479642	-0.052473	2.153189
279.773413	1522.079633	18.484647	-0.052429	2.147863
279.628706	1514.141442	18.489651	-0.052397	2.142531
279.374013	1506.272382	18.494656	-0.052344	2.137222
279.394794	1498.298758	18.499661	-0.052343	2.131856
279.694610	1490.296072	18.504666	-0.052393	2.126484
279.754387	1482.356163	18.509671	-0.052399	2.121118
279.827112	1474.429580	18.514675	-0.052407	2.115748
279.567376	1466.511448	18.519680	-0.052354	2.110338
279.347659	1458.567054	18.524685	-0.052308	2.104899
279.513398	1450.615315	18.529690	-0.052333	2.099480
279.728707	1442.647623	18.534695	-0.052368	2.094041
279.645174	1434.724069	18.539699	-0.052347	2.088588
279.345589	1426.866381	18.544704	-0.052286	2.083145
279.525449	1418.899516	18.549709	-0.052314	2.077660
279.393792	1411.012650	18.554714	-0.052285	2.072184
279.141811	1403.087347	18.559719	-0.052232	2.066655
279.238847	1395.130841	18.564723	-0.052245	2.061125
279.682909	1387.136314	18.569728	-0.052323	2.055589
279.257020	1379.279426	18.574733	-0.052238	2.050045
278.932864	1371.398236	18.579738	-0.052172	2.044480
278.520807	1363.556359	18.584743	-0.052091	2.038918
278.984966	1355.515923	18.589747	-0.052172	2.033291
278.952478	1347.589557	18.594752	-0.052160	2.027678
279.014880	1339.625614	18.599757	-0.052167	2.022032
278.732313	1331.778599	18.604762	-0.052109	2.016418
278.749687	1323.812763	18.609767	-0.052107	2.010735
278.770685	1315.866908	18.614771	-0.052105	2.005050
279.177245	1307.905889	18.619776	-0.052176	1.999379
278.559462	1300.106198	18.624781	-0.052056	1.993699
278.851786	1292.110835	18.629786	-0.052105	1.987959
278.676361	1284.228893	18.634791	-0.052067	1.982234
278.548011	1276.325648	18.639795	-0.052038	1.976482
278.408578	1268.430021	18.644800	-0.052007	1.970718
278.121637	1260.530200	18.649805	-0.051948	1.964917
278.299343	1252.594736	18.654810	-0.051976	1.959124
278.037708	1244.710474	18.659815	-0.051922	1.953303
278.004029	1236.765003	18.664819	-0.051910	1.947445
278.533732	1228.740744	18.669824	-0.052004	1.941574
278.028941	1220.904086	18.674829	-0.051904	1.935708
278.125218	1212.970078	18.679834	-0.051917	1.929819
278.023792	1205.061476	18.684839	-0.051893	1.923909
277.872819	1197.191822	18.689843	-0.051860	1.918005
277.598732	1189.324893	18.694848	-0.051803	1.912070
277.965709	1181.295510	18.699853	-0.051866	1.906067
278.207945	1173.374238	18.704858	-0.051906	1.900113
277.890918	1165.522230	18.709863	-0.051842	1.894128
277.920693	1157.591100	18.714867	-0.051842	1.888105
277.996722	1149.693689	18.719872	-0.051851	1.882093
277.917082	1141.795699	18.724877	-0.051831	1.876043
278.203201	1133.851570	18.729882	-0.051879	1.869981
277.720592	1126.016960	18.734887	-0.051784	1.863893
277.922698	1118.086679	18.739891	-0.051816	1.857793
277.953913	1110.178326	18.744896	-0.051817	1.851668
277.920889	1102.255238	18.749901	-0.051805	1.845505
278.322868	1094.315557	18.754906	-0.051875	1.839360
278.157089	1086.469685	18.759911	-0.051839	1.833199
278.008409	1078.588713	18.764915	-0.051806	1.826993
278.332871	1070.647996	18.769920	-0.051861	1.820775
278.185315	1062.782712	18.774925	-0.051829	1.814538
277.737893	1054.984961	18.779930	-0.051740	1.808297
277.707890	1047.081984	18.784935	-0.051729	1.802001
278.084776	1039.125818	18.789939	-0.051794	1.795691
278.159108	1031.196682	18.794944	-0.051803	1.789343
277.682335	1023.378716	18.799949	-0.051709	1.782993
277.768018	1015.485057	18.804954	-0.051719	1.776630
277.842720	1007.562428	18.809959	-0.051728	1.770219
277.603596	999.721091	18.814963	-0.051678	1.763811
277.577523	991.848160	18.819968	-0.051668	1.757381
277.890000	983.895800	18.824973	-0.051721	1.750905
277.633212	976.071130	18.829978	-0.051668	1.744438
277.492746	968.216246	18.834983	-0.051637	1.737936
277.552407	960.317043	18.839987	-0.051643	1.731399
277.578569	952.437661	18.844992	-0.051642	1.724850
277.539250	944.584269	18.849997	-0.051630	1.718288
277.476915	936.719499	18.855002	-0.051613	1.711689
277.522567	928.810770	18.860007	-0.051616	1.705042
277.255610	920.987421	18.865011	-0.051561	1.698399
277.440774	913.084293	18.870016	-0.051591	1.691723
277.240028	905.236188	18.875021	-0.051548	1.685015
277.075220	897.412310	18.880026	-0.051512	1.678306
276.846695	889.574219	18.885031	-0.051464	1.671549
276.925189	881.668663	18.890035	-0.051474	1.664748
276.676390	873.874449	18.895040	-0.051422	1.657971
276.513949	865.987866	18.900045	-0.051387	1.651098
276.842736	858.076271	18.905050	-0.051443	1.644242
276.702937	850.255330	18.910055	-0.051412	1.637372
276.808214	842.347467	18.915059	-0.051426	1.630431
276.583911	834.523127	18.920064	-0.051379	1.623487
276.556045	826.645764	18.925069	-0.051368	1.616494
276.888399	818.748041	18.930074	-0.051425	1.609505
276.642276	810.937952	18.935079	-0.051374	1.602480
276.774444	803.078829	18.940083	-0.051394	1.595434
276.977331	795.217089	18.945088	-0.051426	1.588366
276.768009	787.409044	18.950093	-0.051382	1.581254
276.649967	779.606988	18.955098	-0.051355	1.574129
276.326463	771.809065	18.960103	-0.051289	1.566945
276.092630	763.997927	18.965107	-0.051241	1.559729
276.248475	756.148258	18.970112	-0.051264	1.552502
276.400051	748.268275	18.975117	-0.051287	1.545212
276.532309	740.428691	18.980122	-0.051307	1.537923
276.469278	732.598155	18.985127	-0.051290	1.530577
276.158297	724.830223	18.990131	-0.051227	1.523218
276.190661	717.012793	18.995136	-0.051228	1.515828
276.224171	709.167472	19.000141	-0.051229	1.508376
276.258699	701.345460	19.005146	-0.051230	1.500910
276.384166	693.514902	19.010151	-0.051248	1.493412
276.266609	685.716464	19.015155	-0.051221	1.485869
276.437995	677.910242	19.020160	-0.051248	1.478326
276.417222	670.087116	19.025165	-0.051239	1.470697
276.176648	662.323185	19.030170	-0.051189	1.463050
275.983754	654.544761	19.035175	-0.051148	1.455357
275.954231	646.751728	19.040179	-0.051137	1.447635
275.987523	638.953395	19.045184	-0.051138	1.439877
275.909077	631.170921	19.050189	-0.051118	1.432074
275.937126	623.373936	19.055194	-0.051118	1.424232
275.985354	615.582405	19.060199	-0.051122	1.416355
275.889196	607.822796	19.065203	-0.051099	1.408442
276.097381	600.019308	19.070208	-0.051133	1.400491
276.035369	592.264566	19.075213	-0.051116	1.392499
276.084192	584.482627	19.080218	-0.051120	1.384452
275.757418	576.773326	19.085223	-0.051054	1.376368
275.742701	568.994131	19.090227	-0.051046	1.368217
275.903492	561.220939	19.095232	-0.051071	1.360055
275.619354	553.515707	19.100237	-0.051013	1.351837
275.635553	545.758295	19.105242	-0.051011	1.343566
275.859444	537.973518	19.110247	-0.051047	1.335252
275.701409	530.257935	19.115251	-0.051013	1.326892
275.629628	522.554730	19.120256	-0.050994	1.318508
275.368042	514.798632	19.125261	-0.050940	1.309977
275.523558	507.012914	19.130266	-0.050964	1.301435
275.535010	499.286946	19.135271	-0.050961	1.292876
275.172084	491.622154	19.140275	-0.050888	1.284257
275.227130	483.918738	19.145280	-0.050894	1.275617
275.101301	476.215545	19.150285	-0.050865	1.266883
275.201865	468.508867	19.155290	-0.050879	1.258128
275.020803	460.837725	19.160295	-0.050840	1.249297
274.800264	453.180587	19.165299	-0.050794	1.240413
274.919811	445.484351	19.170304	-0.050811	1.231485
274.856805	437.789247	19.175309	-0.050794	1.222458
274.819995	430.131921	19.180314	-0.050782	1.213413
274.523695	422.503334	19.185319	-0.050722	1.204282
274.687883	414.814969	19.190323	-0.050747	1.195104
274.757600	407.148806	19.195328	-0.050755	1.185862
274.517097	399.544202	19.200333	-0.050705	1.176557
274.417075	391.915682	19.205338	-0.050682	1.167179
274.368272	384.301719	19.210343	-0.050668	1.157754
274.237273	376.676077	19.215347	-0.050638	1.148219
274.296524	369.036209	19.220352	-0.050644	1.138627
274.229348	361.424427	19.225357	-0.050627	1.128962
274.122424	353.851805	19.230362	-0.050602	1.119255
274.134841	346.254296	19.235367	-0.050599	1.109457
273.911185	338.701626	19.240371	-0.050552	1.099577
274.150664	331.089007	19.245376	-0.050592	1.089635
273.802429	323.582922	19.250381	-0.050522	1.079607
274.108288	315.979604	19.255386	-0.050574	1.069506
273.851170	308.473899	19.260391	-0.050521	1.059310
273.536002	300.996454	19.265395	-0.050457	1.049039
273.479662	293.485197	19.270400	-0.050442	1.038682
273.601101	285.944537	19.275405	-0.050459	1.028222
273.526063	278.468119	19.280410	-0.050440	1.017697
273.274659	271.021444	19.285415	-0.050389	1.007062
273.064718	263.584776	19.290419	-0.050345	0.996337
273.292497	256.058951	19.295424	-0.050382	0.985477
273.044803	248.652570	19.300429	-0.050331	0.974549
273.108149	241.197641	19.305434	-0.050338	0.963506
273.139025	233.775341	19.310439	-0.050339	0.952376
273.154131	226.367777	19.315443	-0.050337	0.941133
273.199336	218.983461	19.320448	-0.050340	0.929797
272.828197	211.688899	19.325453	-0.050266	0.918348
273.193021	204.274954	19.330458	-0.050329	0.906770
273.034675	196.977520	19.335463	-0.050295	0.895082
272.824220	189.702680	19.340467	-0.050251	0.883260
272.792001	182.432855	19.345472	-0.050240	0.871339
272.663548	175.180345	19.350477	-0.050211	0.859252
272.505400	167.968612	19.355482	-0.050177	0.847053
272.218902	160.802955	19.360487	-0.050119	0.834716
272.225429	153.578430	19.365491	-0.050115	0.822182
272.237803	146.404851	19.370496	-0.050113	0.809545
272.131063	139.266070	19.375501	-0.050088	0.796733
272.042311	132.167724	19.380506	-0.050067	0.783792
271.935931	125.105438	19.385511	-0.050043	0.770694
271.968052	118.038843	19.390515	-0.050044	0.757409
272.136989	110.991918	19.395520	-0.050071	0.743971
271.804575	104.063310	19.400525	-0.050004	0.730344
272.027404	97.075703	19.405530	-0.050041	0.716537
272.106013	90.155370	19.410535	-0.050051	0.702544
271.945150	83.322356	19.415539	-0.050016	0.688360
271.801824	76.711332	19.420544	-0.049985	0.674357