Fri Apr 16 18:39:23 2021

Number of Points = 3635
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.011763	0.071619	0.000000	0.000008	0.306714

3.166106	0.044550	0.005005	-0.000020	0.306718
3.104734	0.054213	0.010010	-0.000009	0.306710
2.978318	0.065714	0.015014	0.000015	0.306656
2.964927	0.008445	0.020019	0.000018	0.306373
3.172622	-0.029633	0.025024	-0.000021	0.306371
2.991042	0.005352	0.030029	0.000013	0.306380
2.907266	0.019951	0.035034	0.000029	0.306377
3.163803	-0.026316	0.040038	-0.000019	0.306378
2.743521	0.052513	0.045043	0.000059	0.306389
2.122359	0.167917	0.050048	0.000175	0.306400
2.549214	0.089175	0.055053	0.000096	0.306394
2.501422	0.096152	0.060058	0.000105	0.306386
2.372367	0.122738	0.065062	0.000129	0.306400
2.633718	0.072663	0.070067	0.000080	0.306387
2.837260	0.034791	0.075072	0.000042	0.306383
2.765296	0.048553	0.080077	0.000056	0.306385
2.458453	0.104691	0.085082	0.000113	0.306387
2.880636	-0.009038	0.090086	0.000035	0.306211
2.920020	-0.045369	0.095091	0.000028	0.306073
2.728727	-0.010342	0.100096	0.000063	0.306074
2.706038	-0.004651	0.105101	0.000068	0.306081
2.967674	-0.055485	0.110106	0.000019	0.306065
2.793890	-0.021159	0.115110	0.000051	0.306077
2.649308	-0.016012	0.120115	0.000078	0.305977
2.730026	-0.078297	0.125120	0.000064	0.305751
2.479244	-0.028675	0.130125	0.000110	0.305770
2.637810	-0.061215	0.135130	0.000081	0.305752
2.828327	-0.094072	0.140134	0.000046	0.305759
2.876931	-0.118702	0.145139	0.000037	0.305684
2.765319	-0.137574	0.150144	0.000058	0.305498
2.447103	-0.075005	0.155149	0.000117	0.305520
2.482173	-0.083853	0.160154	0.000110	0.305508
2.405999	-0.066844	0.165158	0.000125	0.305523
2.622668	-0.170745	0.170163	0.000085	0.305216
2.892037	-0.232124	0.175168	0.000035	0.305157
2.814362	-0.214615	0.180173	0.000049	0.305173
2.260355	-0.122254	0.185178	0.000152	0.305133
2.689908	-0.258763	0.190182	0.000073	0.304855
2.837325	-0.287162	0.195187	0.000045	0.304847
2.013512	-0.134173	0.200192	0.000199	0.304862
2.085722	-0.187145	0.205197	0.000185	0.304672
1.905394	-0.182415	0.210202	0.000219	0.304538
1.829547	-0.165174	0.215206	0.000233	0.304554
1.753985	-0.152474	0.220211	0.000247	0.304549
2.096933	-0.274168	0.225216	0.000184	0.304266
2.490013	-0.349378	0.230221	0.000111	0.304248
2.446390	-0.343506	0.235226	0.000119	0.304238
2.352832	-0.391514	0.240230	0.000136	0.303928
1.896364	-0.309148	0.245235	0.000221	0.303924
2.038407	-0.338090	0.250240	0.000195	0.303909
1.999008	-0.391881	0.255245	0.000203	0.303618
1.852461	-0.366097	0.260250	0.000230	0.303614
2.385340	-0.482108	0.265254	0.000131	0.303522
2.212992	-0.502347	0.270259	0.000163	0.303275
2.505193	-0.556511	0.275264	0.000109	0.303270
2.761662	-0.648661	0.280269	0.000061	0.303052
2.428940	-0.603390	0.285274	0.000123	0.302979
2.406976	-0.630747	0.290278	0.000128	0.302829
2.306368	-0.649879	0.295283	0.000146	0.302649
2.080124	-0.619958	0.300288	0.000189	0.302595
2.444748	-0.740745	0.305293	0.000121	0.302334
2.309924	-0.716479	0.310298	0.000146	0.302332
2.307536	-0.781131	0.315302	0.000147	0.302020
2.292968	-0.781256	0.320307	0.000150	0.302006
2.219347	-0.819856	0.325312	0.000163	0.301757
2.445841	-0.867895	0.330317	0.000121	0.301723
2.332494	-0.907511	0.335322	0.000143	0.301434
1.858215	-0.826409	0.340326	0.000231	0.301409
1.802600	-0.869006	0.345331	0.000241	0.301155
1.663085	-0.855689	0.350336	0.000268	0.301097
1.679846	-0.904877	0.355341	0.000265	0.300875
1.453858	-0.882316	0.360346	0.000307	0.300785
1.927287	-1.004062	0.365350	0.000219	0.300613
1.885075	-1.011969	0.370355	0.000227	0.300537
1.953657	-1.085892	0.375360	0.000214	0.300241
2.059835	-1.116885	0.380365	0.000194	0.300184
1.452316	-1.068875	0.385370	0.000308	0.299882
1.273724	-1.041786	0.390374	0.000341	0.299856
1.493262	-1.142110	0.395379	0.000300	0.299564
1.614752	-1.184143	0.400384	0.000278	0.299467
1.982056	-1.292171	0.405389	0.000210	0.299267
1.676936	-1.279022	0.410394	0.000266	0.299062
1.444432	-1.260601	0.415398	0.000310	0.298946
1.547223	-1.338292	0.420403	0.000291	0.298660
1.582329	-1.366812	0.425408	0.000284	0.298552
1.840494	-1.464583	0.430413	0.000237	0.298305
1.783034	-1.492975	0.435418	0.000247	0.298116
1.765336	-1.511681	0.440422	0.000251	0.298009
1.855690	-1.598998	0.445427	0.000234	0.297664
1.485929	-1.562470	0.450432	0.000303	0.297514
1.603227	-1.615656	0.455437	0.000281	0.297359
1.138708	-1.592818	0.460442	0.000368	0.297058
1.236148	-1.633064	0.465446	0.000350	0.296948
1.360351	-1.696060	0.470451	0.000327	0.296751
1.501715	-1.781972	0.475456	0.000301	0.296456
1.734474	-1.859058	0.480461	0.000258	0.296286
1.625296	-1.879183	0.485466	0.000278	0.296090
1.177910	-1.857876	0.490470	0.000361	0.295796
0.503871	-1.762470	0.495475	0.000487	0.295663
-0.224389	-1.658456	0.500480	0.000623	0.295524
-0.737329	-1.624223	0.505485	0.000718	0.295234
-0.904694	-1.616208	0.510490	0.000750	0.295124
-0.871652	-1.676209	0.515494	0.000743	0.294859
-1.070927	-1.668099	0.520499	0.000781	0.294720
-1.490126	-1.629439	0.525504	0.000859	0.294535
-0.893435	-1.778783	0.530509	0.000748	0.294334
-1.450609	-1.696710	0.535514	0.000852	0.294239
-1.658058	-1.724013	0.540518	0.000890	0.293918
-1.371586	-1.795333	0.545523	0.000837	0.293823
-1.341029	-1.845188	0.550528	0.000832	0.293604
-1.748250	-1.811890	0.555533	0.000908	0.293403
-2.370190	-1.721117	0.560538	0.001024	0.293293
-2.530827	-1.745213	0.565542	0.001054	0.293029
-2.516475	-1.764848	0.570547	0.001051	0.292944
-2.790327	-1.772638	0.575552	0.001102	0.292659
-2.267398	-1.897527	0.580557	0.001005	0.292511
-2.379235	-1.913972	0.585562	0.001026	0.292329
-2.093667	-2.018854	0.590566	0.000973	0.292066
-1.959872	-2.067982	0.595571	0.000948	0.291943
-1.991576	-2.108587	0.600576	0.000954	0.291712
-2.142276	-2.125507	0.605581	0.000982	0.291492
-2.448963	-2.104628	0.610586	0.001039	0.291318
-2.595698	-2.127793	0.615590	0.001067	0.291070
-2.988212	-2.093540	0.620595	0.001140	0.290885
-3.512036	-2.024158	0.625600	0.001238	0.290756
-4.381585	-1.912368	0.630605	0.001400	0.290525
-4.911538	-1.824788	0.635610	0.001498	0.290481
-3.865500	-2.078910	0.640614	0.001304	0.290161
-3.890515	-2.101247	0.645619	0.001309	0.290027
-4.247516	-2.074614	0.650624	0.001375	0.289835
-4.386039	-2.091986	0.655629	0.001401	0.289622
-4.935052	-2.011694	0.660634	0.001503	0.289524
-5.538544	-1.953991	0.665638	0.001616	0.289263
-5.059729	-2.055866	0.670643	0.001527	0.289189
-5.551989	-2.024255	0.675648	0.001619	0.288898
-5.611419	-2.032566	0.680653	0.001630	0.288802
-6.079715	-1.993227	0.685658	0.001717	0.288572
-5.732823	-2.083596	0.690662	0.001653	0.288434
-5.970540	-2.074656	0.695667	0.001697	0.288262
-6.589956	-1.997713	0.700672	0.001812	0.288082
-6.758495	-1.987183	0.705677	0.001844	0.287981
-6.771087	-2.035319	0.710682	0.001846	0.287727
-7.076475	-1.997930	0.715686	0.001903	0.287635
-7.535213	-1.959441	0.720691	0.001989	0.287408
-7.532697	-1.977109	0.725696	0.001988	0.287321
-7.329986	-2.060020	0.730701	0.001951	0.287088
-8.167738	-1.925307	0.735706	0.002107	0.286999
-7.541739	-2.082062	0.740710	0.001990	0.286782
-8.010747	-2.009786	0.745715	0.002078	0.286716
-8.279255	-2.013331	0.750720	0.002128	0.286451
-8.275520	-2.029298	0.755725	0.002127	0.286373
-8.198940	-2.090171	0.760730	0.002113	0.286135
-8.623301	-2.026834	0.765734	0.002192	0.286065
-8.731921	-2.054884	0.770739	0.002213	0.285822
-8.835583	-2.052828	0.775744	0.002232	0.285737
-8.610785	-2.128918	0.780749	0.002190	0.285558
-9.625740	-1.957539	0.785754	0.002379	0.285491
-9.431776	-2.038039	0.790758	0.002343	0.285261
-9.852397	-1.981991	0.795763	0.002422	0.285157
-9.381355	-2.104911	0.800768	0.002334	0.284967
-10.102637	-1.997796	0.805773	0.002469	0.284844
-9.643461	-2.117397	0.810778	0.002383	0.284660
-10.285382	-2.030783	0.815782	0.002503	0.284507
-10.608694	-1.990419	0.820787	0.002563	0.284412
-10.770577	-1.999407	0.825792	0.002593	0.284216
-10.598585	-2.038864	0.830797	0.002562	0.284174
-11.526638	-1.926252	0.835802	0.002734	0.283887
-10.951803	-2.032426	0.840806	0.002628	0.283878
-11.020511	-2.073204	0.845811	0.002640	0.283606
-11.403887	-2.011123	0.850816	0.002712	0.283567
-11.848718	-1.973283	0.855821	0.002795	0.283346
-12.065540	-1.951710	0.860826	0.002835	0.283255
-11.771559	-2.027784	0.865830	0.002781	0.283139
-12.521104	-1.924127	0.870835	0.002920	0.282971
-12.222721	-1.985361	0.875840	0.002865	0.282935
-12.109448	-2.065773	0.880845	0.002844	0.282628
-13.186641	-1.868790	0.885850	0.003045	0.282633
-13.217982	-1.904477	0.890854	0.003050	0.282421
-13.086763	-1.947336	0.895859	0.003026	0.282323
-13.262376	-1.931132	0.900864	0.003059	0.282242
-13.551941	-1.925570	0.905869	0.003113	0.282000
-13.452509	-1.945549	0.910874	0.003095	0.281989
-13.351741	-2.006563	0.915878	0.003076	0.281770
-13.747689	-1.949000	0.920883	0.003150	0.281695
-13.785324	-1.969633	0.925888	0.003157	0.281553
-13.830246	-1.996847	0.930893	0.003165	0.281371
-14.230346	-1.924489	0.935898	0.003240	0.281368
-14.992730	-1.839032	0.940902	0.003382	0.281094
-14.891234	-1.859123	0.945907	0.003363	0.281085
-14.541848	-1.950581	0.950912	0.003298	0.280941
-14.973826	-1.909958	0.955917	0.003379	0.280745
-14.711146	-1.959718	0.960922	0.003330	0.280734
-14.781559	-1.984631	0.965926	0.003343	0.280539
-15.434765	-1.870218	0.970931	0.003465	0.280516
-15.017367	-1.973344	0.975936	0.003387	0.280375
-15.191335	-1.981744	0.980941	0.003420	0.280167
-15.759776	-1.878495	0.985946	0.003526	0.280166
-15.637285	-1.957794	0.990950	0.003503	0.279871
-15.561612	-1.976656	0.995955	0.003489	0.279844
-15.972260	-1.931493	1.000960	0.003566	0.279691
-16.179120	-1.924849	1.005965	0.003604	0.279530
-16.266258	-1.911550	1.010970	0.003621	0.279516
-16.071936	-1.998745	1.015974	0.003585	0.279247
-16.093918	-1.998524	1.020979	0.003589	0.279227
-16.677637	-1.924100	1.025984	0.003698	0.279062
-16.525961	-1.982625	1.030989	0.003669	0.278901
-16.779142	-1.939913	1.035994	0.003717	0.278883
-17.242428	-1.911756	1.040998	0.003803	0.278591
-17.276361	-1.904975	1.046003	0.003809	0.278594
-17.412353	-1.908223	1.051008	0.003835	0.278448
-17.563532	-1.913849	1.056013	0.003863	0.278275
-17.371870	-1.951886	1.061018	0.003828	0.278258
-17.706858	-1.936563	1.066022	0.003890	0.278020
-18.032731	-1.883213	1.071027	0.003951	0.277989
-17.998870	-1.909507	1.076032	0.003945	0.277883
-17.994289	-1.955821	1.081037	0.003944	0.277646
-18.171656	-1.925104	1.086042	0.003977	0.277637
-18.547188	-1.897586	1.091046	0.004047	0.277424
-18.492892	-1.926239	1.096051	0.004037	0.277325
-18.560541	-1.921313	1.101056	0.004050	0.277286
-19.110459	-1.872546	1.106061	0.004152	0.277018
-19.358291	-1.829197	1.111066	0.004198	0.277009
-18.910810	-1.934561	1.116070	0.004115	0.276883
-19.112943	-1.931223	1.121075	0.004153	0.276707
-19.043035	-1.945921	1.126080	0.004140	0.276696
-19.119327	-1.983059	1.131085	0.004154	0.276429
-19.542189	-1.915759	1.136090	0.004233	0.276378
-19.754620	-1.895044	1.141094	0.004273	0.276283
-19.595840	-1.964380	1.146099	0.004243	0.276071
-19.925701	-1.905344	1.151104	0.004305	0.276065
-20.353393	-1.867246	1.156109	0.004385	0.275857
-20.358986	-1.886358	1.161114	0.004386	0.275750
-20.300485	-1.897978	1.166118	0.004375	0.275745
-20.260653	-1.950019	1.171123	0.004368	0.275509
-20.420292	-1.922719	1.176128	0.004398	0.275499
-20.380066	-1.960001	1.181133	0.004390	0.275341
-21.052524	-1.870755	1.186138	0.004515	0.275167
-20.607699	-1.952765	1.191142	0.004433	0.275160
-20.837341	-1.966097	1.196147	0.004476	0.274870
-20.942571	-1.951943	1.201152	0.004495	0.274843
-20.793927	-2.008952	1.206157	0.004468	0.274685
-21.510082	-1.910952	1.211162	0.004601	0.274514
-21.125913	-1.979632	1.216166	0.004530	0.274520
-21.446438	-1.973812	1.221171	0.004590	0.274242
-22.043385	-1.868201	1.226176	0.004701	0.274226
-22.032780	-1.891269	1.231181	0.004699	0.274114
-22.148586	-1.911559	1.236186	0.004721	0.273895
-22.051203	-1.929738	1.241190	0.004703	0.273892
-22.311277	-1.925555	1.246195	0.004751	0.273663
-22.592389	-1.889226	1.251200	0.004804	0.273585
-22.843337	-1.844569	1.256205	0.004850	0.273579
-23.132652	-1.848708	1.261210	0.004904	0.273278
-22.981072	-1.876064	1.266214	0.004876	0.273278
-22.883448	-1.914696	1.271219	0.004858	0.273167
-23.627860	-1.814054	1.276224	0.004997	0.272982
-23.222710	-1.885425	1.281229	0.004922	0.272994
-23.393507	-1.897941	1.286234	0.004954	0.272762
-23.959554	-1.816050	1.291238	0.005059	0.272650
-23.803930	-1.842663	1.296243	0.005030	0.272658
-23.626875	-1.932875	1.301248	0.004997	0.272350
-24.240129	-1.821729	1.306253	0.005112	0.272347
-24.552949	-1.777570	1.311258	0.005170	0.272279
-24.087326	-1.912690	1.316262	0.005083	0.272010
-24.057680	-1.917715	1.321267	0.005078	0.272011
-24.804151	-1.812630	1.326272	0.005217	0.271847
-25.315294	-1.740047	1.331277	0.005312	0.271738
-24.756869	-1.845404	1.336282	0.005208	0.271717
-24.483723	-1.941877	1.341286	0.005158	0.271467
-25.171707	-1.831094	1.346291	0.005286	0.271390
-25.406527	-1.789186	1.351296	0.005330	0.271386
-25.454481	-1.834868	1.356301	0.005339	0.271095
-25.791729	-1.774586	1.361306	0.005402	0.271088
-25.536242	-1.834960	1.366310	0.005354	0.271014
-25.626825	-1.864816	1.371315	0.005371	0.270765
-25.880059	-1.819962	1.376320	0.005418	0.270758
-25.632573	-1.888701	1.381325	0.005372	0.270631
-25.710735	-1.898588	1.386330	0.005387	0.270501
-25.925348	-1.858796	1.391334	0.005427	0.270505
-26.255143	-1.858304	1.396339	0.005489	0.270186
-26.196932	-1.875079	1.401344	0.005478	0.270152
-25.935834	-1.942391	1.406349	0.005429	0.270045
-27.249400	-1.740388	1.411354	0.005674	0.269847
-26.620486	-1.855722	1.416358	0.005557	0.269841
-26.385573	-1.934581	1.421363	0.005514	0.269646
-26.858755	-1.874832	1.426368	0.005602	0.269505
-26.682452	-1.911203	1.431373	0.005569	0.269481
-27.345793	-1.836928	1.436378	0.005693	0.269231
-27.097154	-1.883248	1.441382	0.005646	0.269225
-27.582597	-1.819925	1.446387	0.005737	0.269090
-27.555580	-1.863175	1.451392	0.005732	0.268883
-27.313779	-1.905841	1.456397	0.005687	0.268889
-27.743697	-1.877255	1.461402	0.005767	0.268621
-28.145871	-1.811183	1.466406	0.005842	0.268583
-27.769630	-1.890227	1.471411	0.005772	0.268525
-28.270366	-1.849104	1.476416	0.005866	0.268255
-28.477785	-1.808245	1.481421	0.005904	0.268271
-28.534334	-1.825564	1.486426	0.005915	0.268122
-28.777233	-1.806958	1.491430	0.005960	0.267983
-29.033007	-1.758809	1.496435	0.006008	0.267991
-28.802671	-1.852771	1.501440	0.005965	0.267709
-28.881077	-1.850930	1.506445	0.005980	0.267641
-29.202977	-1.798847	1.511450	0.006040	0.267606
-29.443871	-1.808431	1.516454	0.006085	0.267316
-29.057013	-1.878042	1.521459	0.006013	0.267320
-29.327594	-1.854826	1.526464	0.006063	0.267178
-29.744793	-1.812912	1.531469	0.006141	0.266993
-29.438544	-1.870455	1.536474	0.006084	0.266983
-29.502054	-1.901289	1.541478	0.006096	0.266752
-29.836189	-1.848848	1.546483	0.006159	0.266707
-29.723309	-1.887731	1.551488	0.006138	0.266606
-30.043770	-1.870636	1.556493	0.006197	0.266382
-30.122475	-1.859996	1.561498	0.006212	0.266361
-30.519946	-1.826025	1.566502	0.006286	0.266152
-30.224658	-1.895632	1.571507	0.006232	0.266065
-30.534470	-1.846309	1.576512	0.006289	0.266026
-30.635672	-1.879207	1.581517	0.006308	0.265746
-30.827198	-1.844928	1.586522	0.006344	0.265743
-30.766528	-1.881316	1.591526	0.006333	0.265604
-31.345360	-1.795707	1.596531	0.006441	0.265496
-31.399550	-1.786977	1.601536	0.006451	0.265489
-31.224201	-1.870858	1.606541	0.006418	0.265205
-31.706113	-1.792603	1.611546	0.006508	0.265153
-31.720410	-1.804462	1.616550	0.006511	0.265074
-31.762181	-1.840938	1.621555	0.006519	0.264832
-31.861266	-1.823678	1.626560	0.006537	0.264828
-31.866880	-1.859403	1.631565	0.006539	0.264626
-32.275337	-1.807593	1.636570	0.006615	0.264502
-31.942814	-1.869915	1.641574	0.006553	0.264492
-32.138101	-1.884115	1.646579	0.006589	0.264219
-32.380454	-1.841920	1.651584	0.006635	0.264208
-32.067906	-1.928731	1.656589	0.006577	0.264043
-33.072622	-1.774825	1.661594	0.006764	0.263884
-32.922905	-1.803172	1.666598	0.006736	0.263877
-33.098016	-1.818289	1.671603	0.006769	0.263619
-33.067745	-1.833399	1.676608	0.006763	0.263566
-33.053573	-1.850200	1.681613	0.006761	0.263487
-33.314705	-1.846637	1.686618	0.006809	0.263245
-33.557911	-1.800420	1.691622	0.006855	0.263255
-33.411360	-1.863551	1.696627	0.006827	0.263054
-33.789983	-1.813988	1.701632	0.006898	0.262947
-33.347737	-1.901935	1.706637	0.006816	0.262905
-33.597427	-1.911488	1.711642	0.006862	0.262601
-33.962192	-1.844948	1.716646	0.006930	0.262602
-33.867698	-1.896666	1.721651	0.006913	0.262411
-34.058653	-1.883508	1.726656	0.006949	0.262291
-33.992473	-1.907146	1.731661	0.006936	0.262226
-34.660085	-1.832857	1.736666	0.007061	0.261965
-34.537999	-1.854235	1.741670	0.007038	0.261969
-34.661546	-1.863412	1.746675	0.007061	0.261794
-35.096007	-1.803644	1.751680	0.007142	0.261686
-34.817694	-1.858703	1.756685	0.007091	0.261661
-35.126808	-1.857326	1.761690	0.007148	0.261357
-35.403864	-1.806417	1.766694	0.007200	0.261359
-35.414069	-1.832854	1.771699	0.007202	0.261202
-35.512090	-1.844529	1.776704	0.007220	0.261038
-35.381284	-1.866611	1.781709	0.007196	0.261046
-35.593258	-1.884949	1.786714	0.007236	0.260730
-35.781061	-1.851647	1.791718	0.007271	0.260725
-35.853732	-1.856680	1.796723	0.007284	0.260623
-36.439078	-1.773852	1.801728	0.007393	0.260491
-35.672418	-1.913974	1.806733	0.007251	0.260486
-35.957904	-1.921265	1.811738	0.007304	0.260156
-36.666568	-1.794431	1.816742	0.007436	0.260144
-36.676528	-1.816037	1.821747	0.007438	0.260013
-36.890814	-1.809845	1.826752	0.007478	0.259830
-36.609645	-1.861428	1.831757	0.007426	0.259827
-37.111264	-1.822573	1.836762	0.007519	0.259534
-36.727645	-1.900762	1.841766	0.007448	0.259487
-36.814277	-1.904635	1.846771	0.007464	0.259376
-37.323281	-1.842381	1.851776	0.007559	0.259206
-37.371115	-1.830764	1.856781	0.007568	0.259222
-37.283326	-1.903656	1.861786	0.007552	0.258903
-37.592184	-1.853896	1.866790	0.007610	0.258867
-37.418656	-1.909363	1.871795	0.007577	0.258732
-37.745813	-1.882048	1.876800	0.007638	0.258551
-37.876277	-1.859167	1.881805	0.007663	0.258546
-38.558525	-1.787323	1.886810	0.007790	0.258252
-38.029102	-1.885332	1.891814	0.007691	0.258242
-38.148923	-1.888632	1.896819	0.007714	0.258101
-38.712713	-1.813400	1.901824	0.007819	0.257947
-38.291488	-1.891210	1.906829	0.007741	0.257940
-38.714096	-1.872019	1.911834	0.007819	0.257615
-39.002273	-1.819366	1.916838	0.007873	0.257616
-38.771393	-1.891058	1.921843	0.007830	0.257448
-39.279165	-1.825240	1.926848	0.007925	0.257298
-39.192012	-1.841828	1.931853	0.007909	0.257293
-39.876702	-1.772074	1.936858	0.008036	0.256984
-39.873278	-1.772115	1.941862	0.008036	0.256987
-39.634608	-1.835295	1.946867	0.007992	0.256875
-40.072501	-1.788578	1.951872	0.008073	0.256688
-39.650542	-1.864339	1.956877	0.007995	0.256693
-40.161302	-1.820620	1.961882	0.008090	0.256415
-40.593879	-1.750916	1.966886	0.008171	0.256363
-40.446543	-1.787801	1.971891	0.008143	0.256306
-40.371702	-1.847612	1.976896	0.008129	0.256044
-40.301205	-1.858472	1.981901	0.008116	0.256055
-40.892838	-1.792682	1.986906	0.008227	0.255817
-40.885207	-1.808214	1.991910	0.008225	0.255737
-40.397378	-1.906880	1.996915	0.008135	0.255680
-41.204091	-1.793204	2.001920	0.008285	0.255492

-41.090677	-1.862230	2.011917	0.008264	0.255216
-41.543761	-1.805776	2.021914	0.008349	0.255067
-41.959491	-1.769737	2.031910	0.008426	0.254841
-42.093627	-1.765967	2.041907	0.008451	0.254723
-42.260354	-1.771965	2.051904	0.008483	0.254515
-42.162210	-1.795283	2.061901	0.008465	0.254483
-42.514744	-1.775453	2.071898	0.008530	0.254229
-42.821781	-1.717071	2.081894	0.008588	0.254242
-42.519201	-1.773605	2.091891	0.008532	0.254233
-43.085464	-1.693988	2.101888	0.008637	0.254098
-42.974878	-1.749687	2.111885	0.008617	0.253894
-43.030804	-1.740308	2.121882	0.008628	0.253888
-42.454110	-1.846653	2.131878	0.008520	0.253879
-42.613349	-1.818624	2.141875	0.008550	0.253872
-42.592007	-1.821023	2.151872	0.008547	0.253880
-42.528083	-1.832948	2.161869	0.008535	0.253877
-42.707961	-1.799119	2.171866	0.008569	0.253882
-42.435101	-1.848281	2.181862	0.008518	0.253883
-42.225911	-1.888612	2.191859	0.008479	0.253869
-42.387565	-1.858164	2.201856	0.008510	0.253874
-42.506551	-1.835983	2.211853	0.008532	0.253876
-42.533690	-1.831397	2.221850	0.008537	0.253873
-42.166552	-1.897747	2.231846	0.008469	0.253874
-42.420509	-1.811260	2.241843	0.008516	0.254103
-42.258212	-1.820502	2.251840	0.008486	0.254217
-42.237401	-1.824705	2.261837	0.008483	0.254214
-42.032117	-1.862104	2.271834	0.008445	0.254212
-41.902625	-1.859278	2.281830	0.008421	0.254361
-42.047170	-1.808359	2.291827	0.008448	0.254500
-41.955436	-1.825159	2.301824	0.008431	0.254498
-41.856974	-1.814017	2.311821	0.008413	0.254663
-41.356531	-1.876696	2.321818	0.008320	0.254823
-41.512328	-1.846813	2.331814	0.008349	0.254830
-41.390125	-1.828371	2.341811	0.008327	0.255060
-41.001142	-1.885308	2.351808	0.008255	0.255138
-41.155315	-1.839445	2.361805	0.008283	0.255238
-40.731951	-1.873395	2.371802	0.008205	0.255481
-40.770807	-1.865602	2.381798	0.008212	0.255484
-40.427122	-1.886238	2.391795	0.008149	0.255720
-40.399709	-1.890122	2.401792	0.008144	0.255725
-40.193472	-1.881070	2.411789	0.008105	0.255987
-40.136633	-1.880987	2.421786	0.008095	0.256045
-40.145282	-1.835967	2.431782	0.008097	0.256290
-40.026230	-1.844701	2.441779	0.008075	0.256362
-40.024807	-1.788258	2.451776	0.008075	0.256681
-39.961680	-1.782430	2.461773	0.008063	0.256777
-39.450939	-1.838338	2.471770	0.007968	0.256985
-39.134778	-1.864801	2.481766	0.007910	0.257159
-39.082802	-1.848663	2.491763	0.007900	0.257302
-38.656325	-1.880246	2.501760	0.007821	0.257559
-38.787495	-1.837439	2.511757	0.007846	0.257665
-38.443589	-1.848399	2.521754	0.007782	0.257953
-38.159324	-1.873227	2.531750	0.007729	0.258103
-38.279090	-1.825151	2.541747	0.007752	0.258249
-37.786316	-1.862769	2.551744	0.007660	0.258540
-37.715657	-1.854201	2.561741	0.007647	0.258659
-37.154575	-1.918178	2.571738	0.007543	0.258871
-36.784832	-1.945370	2.581734	0.007474	0.259094
-36.943774	-1.893538	2.591731	0.007504	0.259221
-36.414600	-1.941749	2.601728	0.007406	0.259488
-36.603756	-1.880149	2.611725	0.007441	0.259639
-36.237964	-1.913176	2.621722	0.007373	0.259824
-36.254984	-1.857848	2.631718	0.007377	0.260114
-36.094352	-1.853262	2.641715	0.007347	0.260301
-35.742226	-1.883720	2.651712	0.007282	0.260487
-35.852678	-1.818966	2.661709	0.007302	0.260734
-35.563140	-1.835725	2.671706	0.007249	0.260932
-35.454559	-1.819746	2.681702	0.007229	0.261129
-35.223777	-1.819712	2.691699	0.007186	0.261361
-34.768825	-1.848135	2.701696	0.007101	0.261661
-34.850438	-1.801306	2.711693	0.007117	0.261837
-34.336861	-1.859195	2.721690	0.007021	0.262032
-34.172156	-1.840551	2.731686	0.006991	0.262299
-33.796779	-1.861541	2.741683	0.006921	0.262559
-33.654688	-1.849977	2.751680	0.006895	0.262765
-33.619561	-1.815661	2.761677	0.006889	0.262988
-33.660417	-1.758381	2.771674	0.006897	0.263261
-33.260214	-1.782255	2.781670	0.006822	0.263529
-32.719752	-1.842086	2.791667	0.006722	0.263739
-32.531252	-1.837345	2.801664	0.006687	0.263952
-32.355510	-1.820626	2.811661	0.006654	0.264218
-32.055015	-1.828766	2.821658	0.006599	0.264472
-31.960335	-1.805725	2.831654	0.006581	0.264691
-31.196015	-1.907973	2.841651	0.006439	0.264891
-31.114057	-1.876720	2.851648	0.006424	0.265142
-31.222321	-1.801201	2.861645	0.006444	0.265446
-31.120327	-1.783525	2.871642	0.006426	0.265642
-30.471526	-1.867837	2.881638	0.006305	0.265825
-30.294134	-1.855235	2.891635	0.006272	0.266068
-30.194261	-1.819762	2.901632	0.006254	0.266359
-29.855624	-1.838117	2.911629	0.006191	0.266592
-29.503504	-1.864153	2.921626	0.006126	0.266798
-29.387765	-1.848035	2.931622	0.006104	0.266998
-28.942922	-1.870166	2.941619	0.006022	0.267316
-28.746247	-1.866787	2.951616	0.005985	0.267527
-28.481094	-1.875252	2.961613	0.005936	0.267741
-28.222400	-1.879255	2.971610	0.005888	0.267972
-27.928339	-1.880291	2.981606	0.005834	0.268254
-27.722169	-1.878458	2.991603	0.005796	0.268466
-27.627602	-1.854913	3.001600	0.005778	0.268684
-27.303514	-1.874344	3.011597	0.005718	0.268896
-27.042612	-1.859974	3.021594	0.005670	0.269228
-26.799652	-1.869251	3.031590	0.005625	0.269414
-26.455969	-1.892341	3.041587	0.005561	0.269625
-26.149862	-1.908991	3.051584	0.005504	0.269833
-25.638651	-1.944565	3.061581	0.005409	0.270140
-26.009095	-1.836322	3.071578	0.005478	0.270358
-25.697694	-1.849841	3.081574	0.005420	0.270588
-25.577334	-1.836014	3.091571	0.005398	0.270778
-25.024008	-1.881137	3.101568	0.005295	0.271073
-24.764143	-1.886885	3.111565	0.005247	0.271294
-24.894172	-1.819923	3.121562	0.005272	0.271524
-24.290538	-1.888944	3.131558	0.005160	0.271740
-24.426968	-1.812356	3.141555	0.005185	0.272014
-24.476162	-1.749565	3.151552	0.005194	0.272300
-23.837304	-1.818674	3.161549	0.005076	0.272549
-23.963200	-1.748387	3.171546	0.005099	0.272799
-23.181445	-1.845194	3.181542	0.004954	0.273039
-22.966553	-1.840490	3.191539	0.004914	0.273270
-22.658124	-1.841307	3.201536	0.004857	0.273562
-22.709815	-1.786412	3.211533	0.004867	0.273801
-22.343404	-1.809999	3.221530	0.004799	0.274028
-22.033424	-1.819404	3.231526	0.004741	0.274275
-21.904716	-1.794164	3.241523	0.004718	0.274530
-21.003491	-1.907074	3.251520	0.004550	0.274798
-20.756207	-1.914070	3.261517	0.004504	0.274997
-20.674130	-1.890838	3.271514	0.004489	0.275197
-20.089020	-1.939640	3.281510	0.004380	0.275498
-20.269655	-1.872303	3.291507	0.004414	0.275678
-19.953911	-1.893584	3.301504	0.004356	0.275867
-19.549412	-1.929959	3.311501	0.004281	0.276061
-19.400506	-1.898984	3.321498	0.004253	0.276364
-19.056870	-1.919883	3.331494	0.004189	0.276581
-18.926366	-1.903788	3.341491	0.004165	0.276788
-18.803741	-1.886881	3.351488	0.004143	0.276992
-18.753673	-1.835603	3.361485	0.004133	0.277307
-18.524977	-1.833436	3.371482	0.004091	0.277534
-18.293899	-1.825063	3.381478	0.004048	0.277795
-18.071959	-1.821536	3.391475	0.004007	0.278023
-17.715370	-1.838932	3.401472	0.003941	0.278269
-17.324826	-1.856757	3.411469	0.003868	0.278544
-17.185488	-1.840826	3.421466	0.003843	0.278758
-16.627688	-1.898323	3.431462	0.003739	0.278985
-16.385014	-1.896828	3.441459	0.003694	0.279220
-16.219171	-1.875741	3.451456	0.003663	0.279485
-15.942697	-1.885730	3.461453	0.003612	0.279692
-15.620678	-1.904994	3.471450	0.003552	0.279895
-15.365305	-1.900804	3.481446	0.003505	0.280155
-15.098675	-1.893839	3.491443	0.003456	0.280440
-14.954228	-1.887250	3.501440	0.003429	0.280609
-14.850308	-1.872742	3.511437	0.003410	0.280780
-14.734296	-1.840152	3.521434	0.003388	0.281056
-14.057788	-1.911267	3.531430	0.003263	0.281322
-14.140553	-1.852178	3.541427	0.003278	0.281547
-13.894659	-1.852747	3.551424	0.003233	0.281773
-13.811248	-1.825135	3.561421	0.003217	0.281992
-13.111649	-1.891948	3.571418	0.003087	0.282300
-12.850181	-1.899622	3.581414	0.003039	0.282504
-12.683547	-1.888906	3.591411	0.003008	0.282713
-12.139436	-1.940132	3.601408	0.002907	0.282956
-12.377525	-1.845544	3.611405	0.002951	0.283217
-12.080541	-1.855467	3.621402	0.002896	0.283441
-11.745863	-1.872660	3.631398	0.002834	0.283663
-11.555234	-1.861662	3.641395	0.002799	0.283895
-11.132120	-1.876725	3.651392	0.002720	0.284209
-11.026830	-1.858960	3.661389	0.002701	0.284396
-10.573548	-1.903303	3.671386	0.002617	0.284589
-10.112922	-1.937936	3.681382	0.002531	0.284837
-9.323182	-2.032300	3.691379	0.002385	0.285086
-9.423183	-1.982850	3.701376	0.002403	0.285244
-9.141003	-1.986463	3.711373	0.002351	0.285485
-8.929611	-1.983170	3.721370	0.002312	0.285695
-8.805100	-1.972819	3.731366	0.002289	0.285861
-8.363448	-2.013608	3.741363	0.002207	0.286060
-8.031403	-2.020487	3.751360	0.002145	0.286329
-7.953876	-2.003809	3.761357	0.002131	0.286484
-7.691440	-2.008120	3.771354	0.002082	0.286702
-7.738870	-1.945115	3.781350	0.002091	0.286975
-7.078059	-2.029346	3.791347	0.001969	0.287155
-6.985502	-2.012562	3.801344	0.001952	0.287324
-6.881240	-1.970271	3.811341	0.001932	0.287631
-6.695966	-1.962143	3.821338	0.001898	0.287840
-6.413981	-1.975634	3.831334	0.001846	0.288029
-5.850931	-2.032957	3.841331	0.001741	0.288254
-6.226401	-1.914913	3.851328	0.001811	0.288503
-5.699018	-1.969111	3.861325	0.001713	0.288711
-4.984095	-2.065179	3.871322	0.001580	0.288880
-5.002432	-1.998179	3.881318	0.001584	0.289198
-4.633355	-2.033868	3.891315	0.001516	0.289354
-4.589224	-2.008159	3.901312	0.001508	0.289521
-4.363011	-1.985961	3.911309	0.001466	0.289837
-4.425518	-1.934265	3.921306	0.001477	0.290037
-4.031856	-1.963012	3.931302	0.001404	0.290250
-3.972058	-1.924248	3.941299	0.001393	0.290496
-3.377062	-1.982543	3.951296	0.001283	0.290743
-4.291944	-1.778152	3.961293	0.001453	0.290932
-3.696950	-1.831099	3.971290	0.001343	0.291205
-3.502231	-1.817701	3.981286	0.001307	0.291446
-2.879490	-1.878002	3.991283	0.001191	0.291708
-2.544727	-1.884047	4.001280	0.001129	0.291979
-2.429562	-1.861264	4.011277	0.001108	0.292194
-2.342438	-1.829542	4.021274	0.001092	0.292429
-3.273610	-1.600143	4.031270	0.001265	0.292725
-3.072417	-1.572833	4.041267	0.001228	0.293040
-2.753114	-1.572387	4.051264	0.001169	0.293328
-2.212777	-1.612342	4.061261	0.001068	0.293614
-2.036322	-1.585601	4.071258	0.001035	0.293903
-2.139657	-1.499863	4.081254	0.001055	0.294231
-2.221828	-1.428443	4.091251	0.001070	0.294508
-2.701000	-1.267720	4.101248	0.001160	0.294868
-2.118879	-1.303132	4.111245	0.001052	0.295213
-2.081922	-1.236236	4.121242	0.001045	0.295572
-1.773450	-1.234440	4.131238	0.000988	0.295854
-1.546415	-1.206458	4.141235	0.000946	0.296192
-1.438260	-1.154853	4.151232	0.000926	0.296539
-1.612971	-1.053396	4.161229	0.000958	0.296878
-1.482113	-1.000872	4.171226	0.000934	0.297248
-1.342383	-0.948918	4.181222	0.000908	0.297624
-0.487117	-1.023261	4.191219	0.000749	0.298017
-0.729234	-0.908720	4.201216	0.000794	0.298358
-0.881227	-0.804699	4.211213	0.000823	0.298727
-0.809501	-0.736542	4.221210	0.000810	0.299120
-0.624498	-0.691029	4.231206	0.000775	0.299501
-0.630875	-0.598192	4.241203	0.000777	0.299943
-0.328867	-0.568133	4.251200	0.000721	0.300351
-0.389577	-0.485487	4.261197	0.000732	0.300695
0.018884	-0.467839	4.271194	0.000656	0.301136
-0.324025	-0.321581	4.281190	0.000720	0.301538
-0.134308	-0.268501	4.291187	0.000685	0.301957
-0.286952	-0.140420	4.301184	0.000714	0.302437
-0.355647	-0.035210	4.311181	0.000727	0.302879
-0.158945	0.035546	4.321178	0.000690	0.303386
0.296852	0.038969	4.331174	0.000605	0.303796
0.115761	0.185352	4.341171	0.000639	0.304336
0.000000	0.287373	4.351168	0.000661	0.304719

0.447104	0.477050	4.356173	0.000578	0.306003
0.616060	0.997831	4.361178	0.000546	0.308599
0.671412	1.824199	4.366182	0.000535	0.312496
1.060202	2.871681	4.371187	0.000462	0.317631
1.282947	4.235334	4.376192	0.000420	0.323964
1.862061	5.833096	4.381197	0.000311	0.331483
2.157388	7.769407	4.386202	0.000255	0.340058
3.005966	9.922739	4.391206	0.000096	0.349738
3.573237	12.435896	4.396211	-0.000011	0.360399
3.714138	15.339941	4.401216	-0.000039	0.371974
4.228939	18.504557	4.406221	-0.000137	0.384438
4.947636	21.964802	4.411226	-0.000273	0.397722
5.404063	25.817719	4.416230	-0.000360	0.411790
5.727901	30.038881	4.421235	-0.000423	0.426563
6.709094	34.484704	4.426240	-0.000609	0.441966
7.280880	39.368163	4.431245	-0.000718	0.458000
8.435189	44.486459	4.436250	-0.000937	0.474529
9.566832	49.969144	4.441254	-0.001151	0.491562
10.598395	55.824875	4.446259	-0.001347	0.509033
11.380704	62.053911	4.451264	-0.001496	0.526825
12.467645	68.560570	4.456269	-0.001703	0.544919
13.565283	75.379175	4.461274	-0.001911	0.563237
14.497202	82.542540	4.466278	-0.002090	0.581760
15.694359	89.945670	4.471283	-0.002317	0.600403
17.063190	97.594937	4.476288	-0.002577	0.619131
18.368851	105.524866	4.481293	-0.002825	0.637919
19.241137	113.765850	4.486298	-0.002993	0.656682
20.740391	122.118423	4.491302	-0.003277	0.675402
22.377044	130.644242	4.496307	-0.003587	0.694029
23.669456	139.421602	4.501312	-0.003834	0.712552
24.870589	148.379591	4.506317	-0.004063	0.730931
26.206384	157.460359	4.511322	-0.004318	0.749140
27.397227	166.689821	4.516326	-0.004545	0.767148
28.684247	176.004670	4.521331	-0.004791	0.784931
30.064651	185.386852	4.526336	-0.005054	0.802470
32.369058	194.695810	4.531341	-0.005489	0.819791
38.927337	203.371361	4.536346	-0.006716	0.836956
40.012047	213.082727	4.541350	-0.006924	0.853890
41.513984	222.743900	4.546355	-0.007210	0.870532
41.968763	232.593654	4.551360	-0.007301	0.886868
43.447000	242.255928	4.556365	-0.007582	0.902895
46.358803	251.673008	4.561370	-0.008130	0.918652
48.187800	261.281921	4.566374	-0.008477	0.934144
49.883804	270.891851	4.571379	-0.008799	0.949348
51.061043	280.553835	4.576384	-0.009024	0.964254
53.040943	290.072755	4.581389	-0.009399	0.978927
53.876314	299.753113	4.586394	-0.009561	0.993327
54.698978	309.347977	4.591398	-0.009720	1.007394
55.600866	318.876878	4.596403	-0.009894	1.021194
57.257636	328.227322	4.601408	-0.010209	1.034742
58.720952	337.568079	4.606413	-0.010487	1.048055
60.005402	346.890941	4.611418	-0.010732	1.061133
61.081586	356.210915	4.616422	-0.010939	1.073999
62.257642	365.443622	4.621427	-0.011164	1.086619
63.308588	374.653944	4.626432	-0.011365	1.099036
64.743991	383.754745	4.631437	-0.011638	1.111256
65.777054	392.860967	4.636442	-0.011836	1.123261
66.646805	401.964718	4.641446	-0.012004	1.135100
67.545469	411.003917	4.646451	-0.012177	1.146741
68.989289	419.913773	4.651456	-0.012452	1.158219
71.088680	428.666951	4.656461	-0.012848	1.169529
72.347765	437.544167	4.661466	-0.013089	1.180706
73.410358	446.417025	4.666470	-0.013292	1.191731
74.798059	455.198294	4.671475	-0.013556	1.202611
76.313589	463.924974	4.676480	-0.013844	1.213354
77.325828	472.719624	4.681485	-0.014038	1.223981
77.498485	481.621980	4.686490	-0.014076	1.234475
78.764766	490.256258	4.691494	-0.014317	1.244785
80.202528	498.883487	4.696499	-0.014590	1.255034
80.802322	507.594878	4.701504	-0.014708	1.265134
82.127116	516.156839	4.706509	-0.014960	1.275124
82.905890	524.776902	4.711514	-0.015110	1.284997
83.146109	533.492921	4.716518	-0.015161	1.294800
83.855907	542.080021	4.721523	-0.015298	1.304474
85.248837	550.594756	4.726528	-0.015563	1.314123
86.783597	559.005227	4.731533	-0.015854	1.323613
87.360444	567.558998	4.736538	-0.015967	1.333016
88.815883	575.942812	4.741542	-0.016243	1.342329
90.221628	584.346084	4.746547	-0.016511	1.351589
91.164025	592.791548	4.751552	-0.016691	1.360748
92.587038	601.171490	4.756557	-0.016962	1.369860
93.617758	609.597836	4.761562	-0.017159	1.378892
94.633079	618.028314	4.766566	-0.017353	1.387866
94.995006	626.556253	4.771571	-0.017426	1.396771
95.569198	634.973937	4.776576	-0.017539	1.405542
96.561080	643.360766	4.781581	-0.017729	1.414297
98.139098	651.610807	4.786586	-0.018028	1.422958
100.212316	659.795501	4.791590	-0.018419	1.431582
101.459848	668.139391	4.796595	-0.018657	1.440177
102.927511	676.436469	4.801600	-0.018935	1.448710
103.901650	684.840239	4.806605	-0.019122	1.457218
105.375298	693.111232	4.811610	-0.019402	1.465626
106.910375	701.419976	4.816614	-0.019693	1.474032
107.968051	709.751511	4.821619	-0.019895	1.482335
108.684397	718.120158	4.826624	-0.020034	1.490574
109.464894	726.502295	4.831629	-0.020184	1.498791
110.728836	734.758916	4.836634	-0.020425	1.506917
111.758073	743.064604	4.841638	-0.020622	1.515010
112.577773	751.374667	4.846643	-0.020780	1.523031
112.951423	759.756955	4.851648	-0.020855	1.531010
113.293854	768.147646	4.856653	-0.020924	1.538950
114.728754	776.299544	4.861658	-0.021196	1.546792
115.714751	784.556083	4.866662	-0.021385	1.554623
116.578060	792.822859	4.871667	-0.021551	1.562406
117.289334	801.087114	4.876672	-0.021689	1.570125
119.028142	809.225444	4.881677	-0.022018	1.577843
120.235838	817.438714	4.886682	-0.022248	1.585513
122.399418	825.513740	4.891686	-0.022656	1.593159
124.238632	833.651959	4.896691	-0.023004	1.600779
124.725265	842.033480	4.901696	-0.023100	1.608384
125.465959	850.337545	4.906701	-0.023243	1.615921
125.994891	858.649229	4.911706	-0.023347	1.623399
126.400347	866.997461	4.916710	-0.023428	1.630857
127.195191	875.236471	4.921715	-0.023581	1.638241
127.962762	883.404523	4.926720	-0.023729	1.645524
129.016647	891.597228	4.931725	-0.023930	1.652837
130.169860	899.742253	4.936730	-0.024150	1.660089
131.627425	907.870514	4.941734	-0.024427	1.667337
133.271519	916.003410	4.946739	-0.024738	1.674583
134.286450	924.217634	4.951744	-0.024933	1.681780
134.981017	932.498741	4.956749	-0.025067	1.688961
135.779861	940.729053	4.961754	-0.025221	1.696082
136.805488	948.922650	4.966758	-0.025417	1.703171
137.770960	957.109757	4.971763	-0.025602	1.710218
138.404495	965.328142	4.976768	-0.025726	1.717218
139.197119	973.516681	4.981773	-0.025878	1.724185
140.298654	981.684576	4.986778	-0.026089	1.731147
141.876014	989.778037	4.991782	-0.026388	1.738081
142.782836	997.970560	4.996787	-0.026562	1.744982
143.528770	1006.193840	5.001792	-0.026706	1.751860
143.944031	1014.472717	5.006797	-0.026788	1.758714
144.713354	1022.638168	5.011802	-0.026937	1.765494
146.590686	1030.660401	5.016806	-0.027292	1.772271
148.135466	1038.762148	5.021811	-0.027584	1.779045
148.828557	1046.993502	5.026816	-0.027719	1.785790
149.259113	1055.292324	5.031821	-0.027804	1.792531
149.907874	1063.472042	5.036826	-0.027930	1.799178
150.833142	1071.585007	5.041830	-0.028108	1.805782
152.394954	1079.659748	5.046835	-0.028404	1.812409
153.192454	1087.832327	5.051840	-0.028557	1.818995
154.056017	1095.996252	5.056845	-0.028723	1.825559
154.975732	1104.180362	5.061850	-0.028900	1.832121
156.266871	1112.245253	5.066854	-0.029145	1.838612
156.659180	1120.491130	5.071859	-0.029224	1.845112
157.262288	1128.660067	5.076864	-0.029341	1.851554
158.342724	1136.782107	5.081869	-0.029548	1.857995
158.621978	1145.011871	5.086874	-0.029605	1.864401
159.419710	1153.163027	5.091878	-0.029759	1.870786
160.166847	1161.293410	5.096883	-0.029903	1.877127
161.186640	1169.379934	5.101888	-0.030098	1.883444
162.703686	1177.400255	5.106893	-0.030386	1.889748
163.100314	1185.632282	5.111898	-0.030465	1.896061
163.819041	1193.777164	5.116902	-0.030604	1.902325
164.866298	1201.887631	5.121907	-0.030804	1.908579
165.607309	1210.012845	5.126912	-0.030947	1.914789
166.241787	1218.190018	5.131917	-0.031070	1.921005
167.625998	1226.213100	5.136922	-0.031333	1.927171
168.486980	1234.366131	5.141926	-0.031499	1.933354
168.818403	1242.612372	5.146931	-0.031566	1.939527
169.769333	1250.691434	5.151936	-0.031748	1.945626
170.501670	1258.866421	5.156941	-0.031890	1.951753
171.632084	1266.923243	5.161946	-0.032105	1.957816
172.844844	1274.948995	5.166950	-0.032336	1.963847
174.462991	1282.953968	5.171955	-0.032643	1.969889
174.775129	1291.197308	5.176960	-0.032706	1.975943
175.871580	1299.286805	5.181965	-0.032915	1.981951
176.481096	1307.455186	5.186970	-0.033034	1.987946
177.764642	1315.488768	5.191974	-0.033278	1.993898
178.371742	1323.658671	5.196979	-0.033396	1.999857
179.025287	1331.807443	5.201984	-0.033523	2.005788
180.480019	1339.854417	5.206989	-0.033799	2.011713
180.475445	1348.135307	5.211994	-0.033804	2.017634
181.265093	1356.208567	5.216998	-0.033956	2.023473
181.544552	1364.424446	5.222003	-0.034013	2.029342
181.884722	1372.570697	5.227008	-0.034082	2.035152
183.510001	1380.506345	5.232013	-0.034389	2.040930
185.085214	1388.502491	5.237018	-0.034688	2.046729
186.036639	1396.634930	5.242022	-0.034870	2.052542
186.954539	1404.768490	5.247027	-0.035046	2.058336
187.529895	1412.894822	5.252032	-0.035159	2.064073
189.202677	1420.881311	5.257037	-0.035475	2.069809
190.192919	1429.005217	5.262042	-0.035665	2.075554
191.158210	1437.094286	5.267046	-0.035850	2.081257
192.335661	1445.185531	5.272051	-0.036074	2.086966
193.115264	1453.321620	5.277056	-0.036224	2.092651
193.679556	1461.499090	5.282061	-0.036335	2.098327
194.314206	1469.627127	5.287066	-0.036458	2.103961
194.915115	1477.773221	5.292070	-0.036575	2.109588
195.721505	1485.894559	5.297075	-0.036730	2.115204
196.672496	1493.922692	5.302080	-0.036913	2.120755
198.238159	1501.930050	5.307085	-0.037209	2.126338
199.141082	1510.046400	5.312090	-0.037383	2.131915
200.110719	1518.113687	5.317094	-0.037568	2.137450
200.634707	1526.283106	5.322099	-0.037671	2.142997
201.256967	1534.403137	5.327104	-0.037792	2.148505
201.591669	1542.569456	5.332109	-0.037860	2.154003
202.415712	1550.613668	5.337114	-0.038018	2.159451
203.218619	1558.686090	5.342118	-0.038173	2.164903
203.971656	1566.796267	5.347123	-0.038318	2.170361
204.513263	1574.901733	5.352128	-0.038424	2.175782
204.829193	1583.060975	5.357133	-0.038488	2.181203
205.426383	1591.161583	5.362138	-0.038605	2.186599
205.865378	1599.291381	5.367142	-0.038692	2.191985
207.130617	1607.263630	5.372147	-0.038932	2.197333
207.766055	1615.323614	5.377152	-0.039056	2.202665
208.671727	1623.384253	5.382157	-0.039230	2.208010
208.938716	1631.547773	5.387162	-0.039285	2.213350
209.703661	1639.616609	5.392166	-0.039432	2.218662
210.255633	1647.739740	5.397171	-0.039540	2.223976
210.774895	1655.822294	5.402176	-0.039642	2.229248
211.801455	1663.838961	5.407181	-0.039838	2.234511
212.690994	1671.890650	5.412186	-0.040009	2.239771
213.840844	1679.903503	5.417190	-0.040228	2.245018
214.511861	1688.067940	5.422195	-0.040358	2.250306
215.147534	1696.150852	5.427200	-0.040482	2.255526
216.118140	1704.192206	5.432205	-0.040668	2.260738
217.248065	1712.224217	5.437210	-0.040883	2.265945
218.115249	1720.337989	5.442214	-0.041050	2.271169
218.725820	1728.481580	5.447219	-0.041169	2.276377
218.815065	1736.627077	5.452224	-0.041191	2.281528
219.558771	1744.674754	5.457229	-0.041334	2.286663
220.273528	1752.748799	5.462234	-0.041472	2.291801
221.365938	1760.746901	5.467238	-0.041681	2.296912
221.974001	1768.858697	5.472243	-0.041799	2.302040
222.696916	1776.941152	5.477248	-0.041939	2.307149
223.098639	1785.124645	5.482253	-0.042019	2.312282
223.445752	1793.206913	5.487258	-0.042089	2.317335
224.296489	1801.184272	5.492262	-0.042252	2.322356
225.106557	1809.246678	5.497267	-0.042408	2.327414
225.543990	1817.343540	5.502272	-0.042495	2.332451
226.515945	1825.388706	5.507277	-0.042681	2.337490
227.118656	1833.469023	5.512282	-0.042799	2.342509
227.283544	1841.608176	5.517286	-0.042834	2.347516
228.467166	1849.598108	5.522291	-0.043060	2.352507
229.018185	1857.682845	5.527296	-0.043168	2.357491
229.886837	1865.714039	5.532301	-0.043335	2.362459
230.780861	1873.756733	5.537306	-0.043506	2.367425
231.727802	1881.800509	5.542310	-0.043688	2.372386
232.609061	1889.889740	5.547315	-0.043857	2.377358
233.298841	1897.947897	5.552320	-0.043991	2.382285
234.132006	1906.020738	5.557325	-0.044151	2.387222
234.855822	1914.122460	5.562330	-0.044291	2.392158
234.971833	1922.255415	5.567334	-0.044318	2.397053
235.744428	1930.312855	5.572339	-0.044467	2.401945
236.467372	1938.341922	5.577344	-0.044606	2.406806
237.037195	1946.451113	5.582349	-0.044718	2.411693
237.716484	1954.534990	5.587354	-0.044849	2.416564
238.743763	1962.507516	5.592358	-0.045046	2.421386
239.448860	1970.612981	5.597363	-0.045182	2.426251
240.166857	1978.708151	5.602368	-0.045321	2.431102
240.956297	1986.803354	5.607373	-0.045473	2.435948
242.081003	1994.777000	5.612378	-0.045688	2.440739
242.480232	2002.853507	5.617382	-0.045767	2.445524
242.896520	2010.981352	5.622387	-0.045850	2.450332
243.589551	2019.008718	5.627392	-0.045984	2.455092
243.901780	2027.121249	5.632397	-0.046047	2.459864
244.468510	2035.170789	5.637402	-0.046158	2.464609
244.970174	2043.254951	5.642406	-0.046257	2.469360
245.282681	2051.370424	5.647411	-0.046320	2.474105
245.602038	2059.430027	5.652416	-0.046384	2.478809
246.167070	2067.478156	5.657421	-0.046495	2.483517
247.051593	2075.480768	5.662426	-0.046665	2.488213
247.934722	2083.492493	5.667430	-0.046834	2.492905
248.414940	2091.618423	5.672435	-0.046929	2.497624
249.401670	2099.596691	5.677440	-0.047118	2.502286
250.264827	2107.655774	5.682445	-0.047283	2.506977
250.936965	2115.739449	5.687450	-0.047414	2.511659
251.607604	2123.802232	5.692454	-0.047544	2.516320
252.147237	2131.869132	5.697459	-0.047649	2.520965
252.604156	2139.907910	5.702464	-0.047740	2.525579
252.963876	2148.037111	5.707469	-0.047812	2.530229
253.517356	2156.099897	5.712474	-0.047920	2.534847
254.277430	2164.104624	5.717478	-0.048067	2.539438
254.920478	2172.168604	5.722483	-0.048192	2.544046
255.612223	2180.219246	5.727488	-0.048326	2.548642
255.975410	2188.338767	5.732493	-0.048398	2.553244
256.326973	2196.403282	5.737498	-0.048469	2.557806
256.800168	2204.439939	5.742502	-0.048562	2.562353
257.729761	2212.470192	5.747507	-0.048740	2.566921
258.291678	2220.547510	5.752512	-0.048850	2.571480
259.274881	2228.567642	5.757517	-0.049038	2.576029
259.993974	2236.619193	5.762522	-0.049177	2.580569
260.801344	2244.651479	5.767526	-0.049333	2.585096
261.095722	2252.789530	5.772531	-0.049393	2.589638
261.675011	2260.933485	5.777536	-0.049506	2.594195
262.276893	2268.939995	5.782541	-0.049623	2.598670
263.112023	2276.907918	5.787546	-0.049784	2.603131
263.507109	2284.970419	5.792550	-0.049862	2.607607
264.479808	2292.975260	5.797555	-0.050049	2.612082
264.943684	2301.047247	5.802560	-0.050140	2.616552
265.418583	2309.113449	5.807565	-0.050234	2.621012
266.012745	2317.154871	5.812570	-0.050350	2.625458
266.449583	2325.234725	5.817574	-0.050436	2.629907
266.964646	2333.315383	5.822579	-0.050537	2.634355
267.276799	2341.367260	5.827584	-0.050600	2.638765
267.637969	2349.411805	5.832589	-0.050673	2.643167
268.272393	2357.447127	5.837594	-0.050796	2.647575
268.825817	2365.496148	5.842598	-0.050904	2.651978
269.723764	2373.525657	5.847603	-0.051077	2.656386
270.218586	2381.596110	5.852608	-0.051174	2.660781
270.900930	2389.615487	5.857613	-0.051306	2.665154
271.436071	2397.700723	5.862618	-0.051411	2.669545
271.817416	2405.789388	5.867622	-0.051487	2.673921
273.087948	2413.731624	5.872627	-0.051729	2.678270
273.690449	2421.763241	5.877632	-0.051846	2.682615
273.712645	2429.925664	5.882637	-0.051855	2.686985
274.641481	2437.917416	5.887642	-0.052033	2.691316
275.275852	2445.953093	5.892646	-0.052157	2.695644
276.144334	2453.995382	5.897651	-0.052323	2.699983
276.389811	2462.062513	5.902656	-0.052374	2.704289
276.773392	2470.163625	5.907661	-0.052451	2.708615
277.806541	2478.150605	5.912666	-0.052648	2.712914
278.494585	2486.180641	5.917670	-0.052782	2.717208
278.938360	2494.269726	5.922675	-0.052869	2.721510
279.110082	2502.361312	5.927680	-0.052907	2.725789
279.868924	2510.381094	5.932685	-0.053053	2.730061
280.767854	2518.376919	5.937690	-0.053225	2.734322
281.110973	2526.473586	5.942694	-0.053294	2.738594
281.775615	2534.506006	5.947699	-0.053423	2.742847
282.370857	2542.545818	5.952704	-0.053539	2.747092
283.072515	2550.623434	5.957709	-0.053675	2.751356
283.126357	2558.793891	5.962714	-0.053690	2.755623
283.542789	2566.782939	5.967718	-0.053773	2.759810
284.302394	2574.741962	5.972723	-0.053920	2.763997
284.890246	2582.782511	5.977728	-0.054034	2.768209
285.427248	2590.830199	5.982733	-0.054139	2.772415
286.086460	2598.856726	5.987738	-0.054267	2.776610
286.213936	2606.962502	5.992742	-0.054296	2.780809
287.245470	2614.924299	5.997747	-0.054493	2.784981
287.520815	2623.005995	6.002752	-0.054550	2.789163
287.560801	2631.153005	6.007757	-0.054562	2.793358
288.084463	2639.171923	6.012762	-0.054665	2.797510
288.638687	2647.172094	6.017766	-0.054773	2.801648
289.286384	2655.210129	6.022771	-0.054899	2.805804
289.606280	2663.280208	6.027776	-0.054964	2.809952
290.635854	2671.248305	6.032781	-0.055160	2.814083
291.093504	2679.324916	6.037786	-0.055251	2.818229
291.417031	2687.375814	6.042790	-0.055316	2.822348
291.835470	2695.457819	6.047795	-0.055399	2.826483
292.160046	2703.530715	6.052800	-0.055465	2.830601
292.983479	2711.502135	6.057805	-0.055623	2.834691
293.543811	2719.553371	6.062810	-0.055733	2.838800
293.871524	2727.583301	6.067814	-0.055799	2.842878
294.369540	2735.661792	6.072819	-0.055897	2.846985
294.926884	2743.698358	6.077824	-0.056006	2.851068
295.628185	2751.721044	6.082829	-0.056141	2.855147
296.619443	2759.685315	6.087834	-0.056331	2.859207
296.878193	2767.792594	6.092838	-0.056384	2.863291
297.572088	2775.857896	6.097843	-0.056519	2.867372
298.012902	2783.901930	6.102848	-0.056606	2.871423
298.654450	2791.923014	6.107853	-0.056731	2.875468
299.305145	2799.935317	6.112858	-0.056857	2.879503
299.422146	2808.032482	6.117862	-0.056884	2.883545
300.026801	2816.085012	6.122867	-0.057002	2.887586
301.048354	2824.061521	6.127872	-0.057197	2.891607
301.133901	2832.192944	6.132877	-0.057218	2.895647
302.325414	2840.128900	6.137882	-0.057445	2.899645
302.772411	2848.187978	6.142886	-0.057533	2.903658
303.340746	2856.287929	6.147891	-0.057644	2.907692
304.498175	2864.268723	6.152896	-0.057865	2.911694
305.130724	2872.330821	6.157901	-0.057988	2.915701
305.333720	2880.417049	6.162906	-0.058031	2.919692
305.741675	2888.380529	6.167910	-0.058112	2.923627
306.158949	2896.473619	6.172915	-0.058195	2.927621
306.832405	2904.472622	6.177920	-0.058325	2.931578
307.503077	2912.503537	6.182925	-0.058455	2.935544
307.899851	2920.577686	6.187930	-0.058534	2.939512
307.894487	2928.650090	6.192934	-0.058538	2.943452
308.852068	2936.633051	6.197939	-0.058722	2.947394
309.382455	2944.714329	6.202944	-0.058826	2.951356
309.742593	2952.776482	6.207949	-0.058898	2.955294
310.316851	2960.778659	6.212954	-0.059010	2.959209
310.644111	2968.833408	6.217958	-0.059076	2.963131
311.329321	2976.864706	6.222963	-0.059209	2.967055
312.034437	2984.875135	6.227968	-0.059345	2.970965
312.905422	2992.875990	6.232973	-0.059512	2.974874
313.753871	3000.885738	6.237978	-0.059676	2.978780
314.157770	3008.953029	6.242982	-0.059756	2.982686
314.688255	3017.043496	6.247987	-0.059860	2.986605
315.160476	3025.126415	6.252992	-0.059953	2.990511
316.110974	3033.059534	6.257997	-0.060135	2.994366
317.018970	3041.084880	6.263002	-0.060309	2.998256
317.905866	3049.053522	6.268006	-0.060479	3.002114
318.503124	3057.168351	6.273011	-0.060596	3.006022
318.711944	3065.237141	6.278016	-0.060640	3.009882
319.214152	3073.308229	6.283021	-0.060738	3.013754
319.751695	3081.365879	6.288026	-0.060844	3.017616
319.809592	3089.448032	6.293030	-0.060860	3.021460
320.225865	3097.490205	6.298035	-0.060942	3.025299
320.877398	3105.487735	6.303040	-0.061069	3.029123
321.757010	3113.508696	6.308045	-0.061238	3.032964
322.822155	3121.440899	6.313050	-0.061441	3.036768
322.873420	3129.569149	6.318054	-0.061456	3.040610
323.281350	3137.614804	6.323059	-0.061537	3.044425
323.802705	3145.641698	6.328064	-0.061639	3.048232
324.640022	3153.658626	6.333069	-0.061800	3.052045
325.662945	3161.655435	6.338074	-0.061996	3.055852
326.025877	3169.697933	6.343078	-0.062068	3.059644
326.511770	3177.759202	6.348083	-0.062164	3.063446
327.046202	3185.815054	6.353088	-0.062269	3.067243
327.596428	3193.886896	6.358093	-0.062376	3.071043
328.043711	3201.954206	6.363098	-0.062465	3.074832
328.972722	3209.873701	6.368102	-0.062643	3.078570
329.782208	3217.892690	6.373107	-0.062799	3.082344
330.413493	3225.934128	6.378112	-0.062921	3.086115
330.757951	3234.000243	6.383117	-0.062991	3.089879
330.971422	3242.109927	6.388122	-0.063035	3.093653
332.049155	3250.031161	6.393126	-0.063241	3.097375
332.621365	3258.131913	6.398131	-0.063353	3.101152
333.213640	3266.128657	6.403136	-0.063468	3.104877
333.716980	3274.175428	6.408141	-0.063567	3.108617
334.618636	3282.193297	6.413146	-0.063740	3.112357
334.782378	3290.274613	6.418150	-0.063776	3.116087
335.546680	3298.261181	6.423155	-0.063923	3.119798
335.738431	3306.326675	6.428160	-0.063964	3.123513
336.368275	3314.345743	6.433165	-0.064086	3.127223
336.953905	3322.451991	6.438170	-0.064201	3.130966
337.685437	3330.407702	6.443174	-0.064342	3.134643
338.285990	3338.464720	6.448179	-0.064459	3.138355
338.808322	3346.474403	6.453184	-0.064561	3.142038
339.612636	3354.496596	6.458189	-0.064716	3.145735
340.384500	3362.538711	6.463194	-0.064865	3.149434
340.487359	3370.626578	6.468198	-0.064889	3.153121
341.181310	3378.645767	6.473203	-0.065024	3.156798
341.648690	3386.659813	6.478208	-0.065116	3.160458
342.017817	3394.668937	6.483213	-0.065190	3.164107
342.665825	3402.730498	6.488218	-0.065316	3.167788
342.775881	3410.820561	6.493222	-0.065341	3.171454
343.378057	3418.847825	6.498227	-0.065458	3.175109
343.605797	3426.892755	6.503232	-0.065506	3.178751
344.433558	3434.847832	6.508237	-0.065665	3.182375
345.013801	3442.914087	6.513242	-0.065778	3.186034
345.054317	3450.976904	6.518246	-0.065791	3.189663
345.639601	3459.002551	6.523251	-0.065905	3.193295
346.769126	3466.969151	6.528256	-0.066121	3.196920
346.968594	3475.045317	6.533261	-0.066163	3.200550
347.655625	3483.020463	6.538266	-0.066296	3.204151
348.726508	3490.997475	6.543270	-0.066500	3.207765
349.077938	3499.122744	6.548275	-0.066571	3.211411
349.918387	3507.135170	6.553280	-0.066733	3.215023
350.457287	3515.157025	6.558285	-0.066838	3.218622
350.752240	3523.242888	6.563290	-0.066898	3.222235
351.111176	3531.274324	6.568294	-0.066970	3.225822
351.620977	3539.354042	6.573299	-0.067070	3.229434
352.443904	3547.335359	6.578304	-0.067229	3.233010
353.207499	3555.329410	6.583309	-0.067376	3.236586
354.124467	3563.291453	6.588314	-0.067552	3.240150
354.277736	3571.340762	6.593318	-0.067585	3.243716
354.537617	3579.447002	6.598323	-0.067639	3.247308
355.371374	3587.447845	6.603328	-0.067799	3.250874
355.711148	3595.489792	6.608333	-0.067868	3.254433
356.333132	3603.516580	6.613338	-0.067989	3.257993
356.901399	3611.531175	6.618342	-0.068100	3.261541
357.550454	3619.555830	6.623347	-0.068225	3.265093
358.252103	3627.561200	6.628352	-0.068361	3.268635
358.361940	3635.691497	6.633357	-0.068387	3.272204
358.699580	3643.766957	6.638362	-0.068455	3.275754
359.185065	3651.697805	6.643366	-0.068550	3.279243
360.211948	3659.693496	6.648371	-0.068747	3.282778
360.613597	3667.759819	6.653376	-0.068827	3.286315
360.785695	3675.848830	6.658381	-0.068864	3.289849
361.450639	3683.869458	6.663386	-0.068993	3.293368
361.724875	3691.923747	6.668390	-0.069049	3.296884
362.964101	3699.850366	6.673395	-0.069285	3.300377
363.543442	3707.867309	6.678400	-0.069398	3.303881
363.942612	3715.938134	6.683405	-0.069477	3.307396
364.355600	3724.028041	6.688410	-0.069559	3.310917
364.470416	3732.090780	6.693414	-0.069586	3.314410
365.413477	3740.060318	6.698419	-0.069767	3.317892
365.894276	3748.057652	6.703424	-0.069861	3.321364
366.505326	3756.072235	6.708429	-0.069980	3.324845
367.182037	3764.069371	6.713434	-0.070111	3.328317
367.389311	3772.153225	6.718438	-0.070155	3.331804
367.898976	3780.226814	6.723443	-0.070255	3.335295
368.289977	3788.228723	6.728448	-0.070333	3.338747
368.745914	3796.248660	6.733453	-0.070423	3.342206
369.479607	3804.267951	6.738458	-0.070565	3.345671
369.587690	3812.390333	6.743462	-0.070590	3.349153
370.094598	3820.435842	6.748467	-0.070689	3.352613
371.160535	3828.336434	6.753472	-0.070893	3.356029
371.976582	3836.329624	6.758477	-0.071050	3.359472
372.969276	3844.332867	6.763482	-0.071240	3.362921
373.180943	3852.426666	6.768486	-0.071285	3.366376
373.912694	3860.447062	6.773491	-0.071426	3.369816
374.334309	3868.512413	6.778496	-0.071510	3.373260
374.241253	3876.624048	6.783501	-0.071497	3.376701
374.688001	3884.664267	6.788506	-0.071586	3.380128
375.538546	3892.546947	6.793510	-0.071749	3.383500
376.308336	3900.597561	6.798515	-0.071898	3.386936
376.857610	3908.626853	6.803520	-0.072005	3.390351
377.393507	3916.683399	6.808525	-0.072110	3.393774
378.088298	3924.717044	6.813530	-0.072244	3.397190
378.010909	3932.813628	6.818534	-0.072235	3.400601
378.588712	3940.768569	6.823539	-0.072348	3.403972
379.334469	3948.784280	6.828544	-0.072492	3.407371
379.490351	3956.887870	6.833549	-0.072526	3.410783
379.411217	3964.988945	6.838554	-0.072517	3.414182
380.286631	3972.877143	6.843558	-0.072685	3.417521
381.074964	3980.914193	6.848563	-0.072836	3.420917
381.112020	3988.962741	6.853568	-0.072849	3.424288
381.192150	3997.032828	6.858573	-0.072869	3.427666
381.944515	4005.046753	6.863578	-0.073014	3.431041
382.269695	4013.037049	6.868582	-0.073079	3.434387
382.941640	4021.011071	6.873587	-0.073210	3.437735
383.315611	4029.065800	6.878592	-0.073284	3.441104
383.781896	4037.048193	6.883597	-0.073376	3.444442
384.591203	4045.088479	6.888602	-0.073532	3.447812
385.168961	4053.123683	6.893606	-0.073645	3.451169
385.298269	4061.214986	6.898611	-0.073674	3.454531
385.731871	4069.208769	6.903616	-0.073760	3.457860
385.899188	4077.301543	6.908621	-0.073796	3.461217
386.581598	4085.264525	6.913626	-0.073928	3.464534
386.931314	4093.288128	6.918630	-0.073999	3.467862
387.094909	4101.418624	6.923635	-0.074034	3.471225
387.405657	4109.377883	6.928640	-0.074097	3.474519
388.130377	4117.348670	6.933645	-0.074237	3.477828
387.977213	4125.507867	6.938650	-0.074214	3.481182
388.543044	4133.380372	6.943654	-0.074324	3.484439
389.041484	4141.449834	6.948659	-0.074422	3.487771
389.456528	4149.498902	6.953664	-0.074505	3.491089
389.512458	4157.544013	6.958669	-0.074520	3.494391
390.458582	4165.529228	6.963674	-0.074702	3.497694
390.748458	4173.553746	6.968678	-0.074761	3.500988
391.115846	4181.572973	6.973683	-0.074834	3.504279
391.202856	4189.653329	6.978688	-0.074856	3.507584
391.918693	4197.662141	6.983693	-0.074994	3.510876
392.068495	4205.676418	6.988698	-0.075027	3.514149
392.394806	4213.732752	6.993702	-0.075093	3.517442
392.589614	4221.815481	6.998707	-0.075134	3.520738
392.778410	4229.781922	7.003712	-0.075175	3.523984
392.941079	4237.870069	7.008717	-0.075210	3.527275
393.734530	4245.844740	7.013722	-0.075363	3.530537
394.427139	4253.783334	7.018726	-0.075497	3.533778
394.384019	4261.901789	7.023731	-0.075494	3.537065
395.158385	4269.872450	7.028736	-0.075643	3.540316
395.569419	4277.877066	7.033741	-0.075725	3.543565
396.026506	4285.972300	7.038746	-0.075815	3.546850
396.326611	4293.971136	7.043750	-0.075876	3.550088
396.961581	4302.022469	7.048755	-0.076000	3.553354
397.067225	4310.063467	7.053760	-0.076024	3.556597
397.261453	4318.042311	7.058765	-0.076066	3.559815
397.621705	4326.071877	7.063770	-0.076138	3.563055
398.138732	4334.085479	7.068774	-0.076239	3.566290
398.879718	4342.064912	7.073779	-0.076382	3.569515
398.966298	4350.177948	7.078784	-0.076404	3.572771
399.618134	4358.156494	7.083789	-0.076530	3.575988
399.759114	4366.191452	7.088794	-0.076561	3.579208
400.392028	4374.179261	7.093798	-0.076684	3.582422
401.126599	4382.187340	7.098803	-0.076826	3.585644
401.513854	4390.219207	7.103808	-0.076904	3.588861
401.857353	4398.289879	7.108813	-0.076973	3.592090
402.455011	4406.343053	7.113818	-0.077089	3.595317
403.099712	4414.271637	7.118822	-0.077214	3.598492
403.199088	4422.411448	7.123827	-0.077238	3.601733
403.612631	4430.388013	7.128832	-0.077320	3.604915
403.758668	4438.437656	7.133837	-0.077352	3.608115
404.449989	4446.459756	7.138842	-0.077486	3.611318
404.787104	4454.445531	7.143846	-0.077554	3.614492
405.413041	4462.495771	7.148851	-0.077676	3.617698
405.287610	4470.627939	7.153856	-0.077658	3.620912
406.012565	4478.501716	7.158861	-0.077798	3.624045
406.580446	4486.574176	7.163866	-0.077908	3.627249
407.026695	4494.585132	7.168870	-0.077997	3.630422
407.240333	4502.639638	7.173875	-0.078042	3.633604
407.693534	4510.654995	7.178880	-0.078131	3.636773
407.758952	4518.669239	7.183885	-0.078148	3.639929
408.517844	4526.644793	7.188890	-0.078295	3.643086
408.406537	4534.716581	7.193894	-0.078279	3.646254
408.979524	4542.707614	7.198899	-0.078391	3.649406
409.687595	4550.719482	7.203904	-0.078528	3.652568
409.887289	4558.790777	7.208909	-0.078570	3.655736
410.274937	4566.800263	7.213914	-0.078648	3.658882
410.449115	4574.818837	7.218918	-0.078685	3.662023
410.711788	4582.860645	7.223923	-0.078739	3.665172
411.030307	4590.875252	7.228928	-0.078804	3.668310
411.224575	4598.917415	7.233933	-0.078845	3.671453
411.595657	4606.952050	7.238938	-0.078919	3.674595
411.869201	4614.941850	7.243942	-0.078975	3.677714
412.233287	4622.999018	7.248947	-0.079048	3.680858
412.531226	4630.935183	7.253952	-0.079109	3.683952
412.654877	4639.048357	7.258957	-0.079137	3.687106
413.031957	4647.105563	7.263962	-0.079212	3.690243
413.233454	4655.103493	7.268966	-0.079255	3.693350
413.616496	4663.156528	7.273971	-0.079331	3.696480
414.330061	4671.110539	7.278976	-0.079469	3.699578
414.647112	4679.125456	7.283981	-0.079533	3.702686
414.964285	4687.217560	7.288986	-0.079598	3.705822
415.311239	4695.184463	7.293990	-0.079667	3.708907
415.187462	4703.345538	7.298995	-0.079650	3.712052
415.601665	4711.328116	7.304000	-0.079732	3.715140
416.257297	4719.247321	7.309005	-0.079859	3.718207
416.637234	4727.274218	7.314010	-0.079935	3.721305
416.769227	4735.279510	7.319014	-0.079964	3.724387
417.064703	4743.358075	7.324019	-0.080025	3.727498
417.251106	4751.394474	7.329024	-0.080064	3.730587
417.415450	4759.438238	7.334029	-0.080100	3.733676
418.356173	4767.394602	7.339034	-0.080280	3.736749
418.980006	4775.357131	7.344038	-0.080402	3.739813
419.268861	4783.426345	7.349043	-0.080461	3.742907
419.749002	4791.477060	7.354048	-0.080555	3.745996
420.301396	4799.438446	7.359053	-0.080663	3.749051
420.869949	4807.506214	7.364058	-0.080774	3.752143
421.219786	4815.532512	7.369062	-0.080844	3.755212
421.861013	4823.502855	7.374067	-0.080969	3.758264
422.293316	4831.568612	7.379072	-0.081054	3.761345
422.995270	4839.501898	7.384077	-0.081190	3.764379
423.411005	4847.592952	7.389082	-0.081273	3.767464
424.061699	4855.583227	7.394086	-0.081399	3.770514
424.429756	4863.620895	7.399091	-0.081473	3.773572
424.819361	4871.707582	7.404096	-0.081550	3.776647
425.178842	4879.703134	7.409101	-0.081623	3.779684
425.526969	4887.738989	7.414106	-0.081692	3.782734
425.768008	4895.749250	7.419110	-0.081742	3.785769
426.438714	4903.762890	7.424115	-0.081872	3.788812
426.513785	4911.856024	7.429120	-0.081892	3.791870
426.405382	4919.921358	7.434125	-0.081877	3.794910
426.829753	4927.902814	7.439130	-0.081961	3.797928
427.462771	4935.868252	7.444134	-0.082084	3.800943
427.822061	4943.828572	7.449139	-0.082156	3.803947
428.227459	4951.923807	7.454144	-0.082236	3.807000
428.623319	4959.914913	7.459149	-0.082315	3.810012
429.152373	4967.965306	7.464154	-0.082419	3.813046
429.465316	4976.038530	7.469158	-0.082482	3.816081
430.085150	4983.953492	7.474163	-0.082603	3.819062
430.339945	4992.060752	7.479168	-0.082655	3.822104
430.937725	4999.966622	7.484173	-0.082772	3.825076
431.423427	5008.075081	7.489178	-0.082867	3.828119
431.601880	5016.167218	7.494182	-0.082906	3.831146
431.603444	5024.169070	7.499187	-0.082911	3.834133
432.263972	5032.186618	7.504192	-0.083039	3.837139
432.736840	5040.136983	7.509197	-0.083132	3.840112
433.434873	5048.127692	7.514202	-0.083267	3.843104
433.806440	5056.188187	7.519206	-0.083342	3.846111
434.345313	5064.187623	7.524211	-0.083447	3.849097
434.551463	5072.285639	7.529216	-0.083491	3.852111
434.758454	5080.285735	7.534221	-0.083534	3.855085
435.248000	5088.321545	7.539226	-0.083631	3.858077
435.611445	5096.329655	7.544230	-0.083703	3.861053
435.740166	5104.311796	7.549235	-0.083732	3.864013
436.535061	5112.353024	7.554240	-0.083886	3.867005
436.564557	5120.413234	7.559245	-0.083896	3.869987
436.962454	5128.525920	7.564250	-0.083975	3.872993
437.306438	5136.562655	7.569254	-0.084045	3.875968
437.475737	5144.478259	7.574259	-0.084081	3.878892
437.949006	5152.478878	7.579264	-0.084174	3.881851
438.125738	5160.426654	7.584269	-0.084212	3.884783
438.553462	5168.527975	7.589274	-0.084297	3.887773
438.885859	5176.514416	7.594278	-0.084364	3.890718
438.981369	5184.561568	7.599283	-0.084387	3.893677
439.511610	5192.557333	7.604288	-0.084491	3.896625
439.613425	5200.546762	7.609293	-0.084515	3.899559
440.227732	5208.588801	7.614298	-0.084635	3.902520
440.511630	5216.569687	7.619302	-0.084693	3.905450
440.963483	5224.618529	7.624307	-0.084782	3.908406
441.453517	5232.649443	7.629312	-0.084878	3.911354
441.787514	5240.650477	7.634317	-0.084946	3.914285
442.367433	5248.704526	7.639322	-0.085059	3.917239
442.443678	5256.709260	7.644326	-0.085078	3.920162
442.880662	5264.717378	7.649331	-0.085164	3.923091
443.230107	5272.780803	7.654336	-0.085235	3.926037
443.481122	5280.762947	7.659341	-0.085286	3.928949
443.989238	5288.807322	7.664346	-0.085386	3.931886
444.357435	5296.812769	7.669350	-0.085460	3.934804
444.921429	5304.835746	7.674355	-0.085570	3.937730
445.280613	5312.901233	7.679360	-0.085642	3.940665
445.433322	5320.900793	7.684365	-0.085676	3.943571
445.780566	5329.009285	7.689370	-0.085745	3.946517
446.368144	5336.955795	7.694374	-0.085860	3.949407
446.761614	5345.000989	7.699379	-0.085938	3.952326
447.054626	5353.020230	7.704384	-0.085998	3.955233
447.363073	5361.000666	7.709389	-0.086061	3.958123
447.948598	5369.039842	7.714394	-0.086175	3.961037
448.125948	5376.990376	7.719398	-0.086213	3.963910
448.808857	5385.065507	7.724403	-0.086345	3.966835
449.209515	5393.107936	7.729408	-0.086425	3.969741
449.522351	5401.061882	7.734413	-0.086488	3.972611
450.172204	5409.150188	7.739418	-0.086614	3.975533
450.089804	5417.166583	7.744422	-0.086604	3.978414
450.187006	5425.216562	7.749427	-0.086627	3.981309
450.162728	5433.228735	7.754432	-0.086628	3.984185
450.438139	5441.216622	7.759437	-0.086684	3.987056
450.736066	5449.253735	7.764442	-0.086745	3.989943
450.886038	5457.241970	7.769446	-0.086778	3.992808
451.353460	5465.251468	7.774451	-0.086870	3.995684
451.834769	5473.245336	7.779456	-0.086965	3.998552
452.092343	5481.284518	7.784461	-0.087018	4.001430
452.237646	5489.289412	7.789466	-0.087050	4.004293
452.651368	5497.326934	7.794470	-0.087132	4.007169
453.228307	5505.333935	7.799475	-0.087245	4.010035
453.333420	5513.414321	7.804480	-0.087270	4.012917
453.654901	5521.413439	7.809485	-0.087334	4.015772
454.001846	5529.427752	7.814490	-0.087404	4.018630
454.370864	5537.453062	7.819494	-0.087478	4.021491
454.726007	5545.430407	7.824499	-0.087549	4.024332
455.290473	5553.468246	7.829504	-0.087659	4.027196
455.123444	5561.546822	7.834509	-0.087634	4.030061
455.615590	5569.618197	7.839514	-0.087730	4.032932
455.932978	5577.633745	7.844518	-0.087795	4.035778
456.428065	5585.553709	7.849523	-0.087892	4.038591
456.890013	5593.615005	7.854528	-0.087983	4.041451
457.127613	5601.537587	7.859533	-0.088032	4.044257
457.536733	5609.647342	7.864538	-0.088114	4.047130
457.896882	5617.616621	7.869542	-0.088186	4.049950
457.941202	5625.655809	7.874547	-0.088199	4.052788
458.294293	5633.755457	7.879552	-0.088270	4.055649
458.620462	5641.672503	7.884557	-0.088336	4.058445
459.007648	5649.716679	7.889562	-0.088413	4.061283
459.306439	5657.716302	7.894566	-0.088474	4.064103
459.632244	5665.767530	7.899571	-0.088540	4.066940
459.582597	5673.842213	7.904576	-0.088536	4.069777
459.893248	5681.806826	7.909581	-0.088598	4.072578
460.333842	5689.846358	7.914586	-0.088686	4.075406
460.490710	5697.855435	7.919590	-0.088720	4.078217
460.651985	5705.877947	7.924595	-0.088755	4.081031
461.272047	5713.839813	7.929600	-0.088876	4.083828
461.537060	5721.834528	7.934605	-0.088930	4.086630
461.502260	5729.933765	7.939610	-0.088929	4.089462
461.987311	5737.966454	7.944614	-0.089024	4.092276
462.451102	5746.010220	7.949619	-0.089116	4.095092
462.778549	5753.996328	7.954624	-0.089182	4.097884
462.856321	5762.043739	7.959629	-0.089201	4.100691
463.326070	5770.046963	7.964634	-0.089294	4.103487
463.542229	5778.077606	7.969638	-0.089339	4.106287
464.041308	5786.054157	7.974643	-0.089437	4.109070
464.761320	5794.097662	7.979648	-0.089577	4.111877
464.987588	5802.069297	7.984653	-0.089624	4.114651
465.381941	5810.131570	7.989658	-0.089702	4.117456
465.247399	5818.149874	7.994662	-0.089682	4.120237
465.599619	5826.124115	7.999667	-0.089753	4.123008
466.016865	5834.142822	8.004672	-0.089836	4.125792
465.974835	5842.181995	8.009677	-0.089833	4.128576
466.340238	5850.267017	8.014682	-0.089906	4.131380
466.440615	5858.233194	8.019686	-0.089930	4.134136
467.117783	5866.257093	8.024691	-0.090061	4.136919
467.361860	5874.320095	8.029696	-0.090112	4.139707
467.312332	5882.330827	8.034701	-0.090108	4.142471
467.534873	5890.334090	8.039706	-0.090154	4.145235
467.884134	5898.285573	8.044710	-0.090225	4.147981
468.198883	5906.321707	8.049715	-0.090288	4.150753
468.386797	5914.367981	8.054720	-0.090328	4.153525
468.765167	5922.371044	8.059725	-0.090404	4.156283
469.111643	5930.309882	8.064730	-0.090474	4.159017
469.417672	5938.397352	8.069734	-0.090536	4.161799
469.329085	5946.369839	8.074739	-0.090524	4.164535
469.779049	5954.456750	8.079744	-0.090613	4.167315
470.468063	5962.389612	8.084749	-0.090747	4.170044
470.739113	5970.485743	8.089754	-0.090802	4.172821
470.999456	5978.512060	8.094758	-0.090856	4.175572
471.022485	5986.526474	8.099763	-0.090865	4.178315
471.316846	5994.639086	8.104768	-0.090925	4.181093
471.395071	6002.557193	8.109773	-0.090945	4.183800
471.409542	6010.681086	8.114778	-0.090953	4.186574
471.995954	6018.601539	8.119782	-0.091067	4.189284
472.273279	6026.716363	8.124787	-0.091124	4.192055
472.649039	6034.746326	8.129792	-0.091199	4.194796
472.745539	6042.727754	8.134797	-0.091222	4.197515
473.139645	6050.665998	8.139802	-0.091300	4.200222
473.668324	6058.673951	8.144806	-0.091404	4.202952
473.923791	6066.686186	8.149811	-0.091457	4.205678
474.055527	6074.750052	8.154816	-0.091486	4.208419
474.512302	6082.777434	8.159821	-0.091577	4.211149
474.871585	6090.799551	8.164826	-0.091649	4.213875
475.743326	6098.801413	8.169830	-0.091816	4.216597
475.677346	6106.811894	8.174835	-0.091809	4.219310
476.191505	6114.851610	8.179840	-0.091910	4.222038
476.757016	6122.785299	8.184845	-0.092020	4.224729
476.885812	6130.895841	8.189850	-0.092049	4.227473
477.120299	6138.899385	8.194854	-0.092098	4.230180
477.604581	6146.881967	8.199859	-0.092193	4.232881
477.942930	6154.927066	8.204864	-0.092261	4.235599
478.038476	6162.836714	8.209869	-0.092284	4.238268
478.427433	6170.958410	8.214874	-0.092362	4.241009
478.671655	6178.905371	8.219878	-0.092412	4.243689
479.061003	6187.005282	8.224883	-0.092490	4.246419
479.535175	6194.987376	8.229888	-0.092583	4.249109
479.580403	6203.036590	8.234893	-0.092597	4.251816
479.855514	6211.110264	8.239898	-0.092653	4.254531
480.045084	6219.087524	8.244902	-0.092694	4.257211
480.605141	6227.052692	8.249907	-0.092803	4.259889
480.971952	6235.094771	8.254912	-0.092877	4.262589
480.806350	6243.109729	8.259917	-0.092851	4.265274
481.227760	6251.181159	8.264922	-0.092935	4.267981
481.485897	6259.179429	8.269926	-0.092988	4.270660
481.797353	6267.153337	8.274931	-0.093051	4.273330
481.798414	6275.276430	8.279936	-0.093056	4.276045
482.382906	6283.131564	8.284941	-0.093170	4.278674
483.013713	6291.197253	8.289946	-0.093293	4.281373
483.293831	6299.113043	8.294950	-0.093350	4.284016
483.564314	6307.251412	8.299955	-0.093405	4.286732
483.762403	6315.249839	8.304960	-0.093447	4.289399
483.686879	6323.322481	8.309965	-0.093438	4.292086
484.176014	6331.296155	8.314970	-0.093535	4.294744
484.149119	6339.367325	8.319974	-0.093535	4.297428
484.556812	6347.315762	8.324979	-0.093616	4.300073
484.636369	6355.377368	8.329984	-0.093636	4.302752
484.924391	6363.354984	8.334989	-0.093694	4.305402
485.458333	6371.416139	8.339994	-0.093799	4.308081
485.490503	6379.438625	8.344998	-0.093810	4.310741
486.128441	6387.383118	8.350003	-0.093934	4.313378
486.694155	6395.468457	8.355008	-0.094044	4.316060
486.749957	6403.385652	8.360013	-0.094060	4.318680
487.209065	6411.495236	8.365018	-0.094151	4.321366
487.595035	6419.392599	8.370022	-0.094228	4.323979
487.903105	6427.450888	8.375027	-0.094290	4.326643
488.173180	6435.496256	8.380032	-0.094345	4.329301
488.359877	6443.471019	8.385037	-0.094385	4.331933
488.862024	6451.529550	8.390042	-0.094484	4.334594
488.996268	6459.535414	8.395046	-0.094514	4.337232
488.823974	6467.591194	8.400051	-0.094487	4.339883
489.197361	6475.580570	8.405056	-0.094562	4.342515
489.357666	6483.595906	8.410061	-0.094597	4.345152
489.696091	6491.634051	8.415066	-0.094665	4.347797
489.965310	6499.639787	8.420070	-0.094720	4.350428
490.166648	6507.712867	8.425075	-0.094763	4.353080
490.580016	6515.716845	8.430080	-0.094845	4.355709
490.701122	6523.658800	8.435085	-0.094872	4.358313
491.424766	6531.697508	8.440090	-0.095012	4.360952
491.471179	6539.677543	8.445094	-0.095026	4.363566
491.790877	6547.691955	8.450099	-0.095091	4.366191
492.078844	6555.745406	8.455104	-0.095149	4.368827
492.262014	6563.814605	8.460109	-0.095189	4.371465
492.582260	6571.792272	8.465114	-0.095253	4.374073
493.024466	6579.790544	8.470118	-0.095341	4.376688
493.274010	6587.818701	8.475123	-0.095392	4.379308
493.539426	6595.847629	8.480128	-0.095447	4.381928
493.667465	6603.815174	8.485133	-0.095476	4.384525
493.940786	6611.891116	8.490138	-0.095532	4.387157
494.340251	6619.885162	8.495142	-0.095611	4.389762
494.422151	6627.920895	8.500147	-0.095632	4.392376
495.003632	6635.962605	8.505152	-0.095745	4.394994
495.186868	6643.983138	8.510157	-0.095785	4.397601
495.435373	6652.023657	8.515162	-0.095836	4.400213
495.882224	6659.997110	8.520166	-0.095924	4.402803
496.101392	6668.020965	8.525171	-0.095970	4.405406
496.474502	6676.104724	8.530176	-0.096045	4.408028
496.309794	6684.178856	8.535181	-0.096019	4.410643
496.635800	6692.187403	8.540186	-0.096085	4.413237
496.954723	6700.228916	8.545190	-0.096150	4.415841
497.208782	6708.164380	8.550195	-0.096202	4.418408
497.443792	6716.213128	8.555200	-0.096251	4.421010
497.507939	6724.186411	8.560205	-0.096268	4.423585
497.977686	6732.265080	8.565210	-0.096361	4.426195
498.173687	6740.231192	8.570215	-0.096402	4.428766
498.633559	6748.286888	8.575219	-0.096493	4.431365
498.918996	6756.269831	8.580224	-0.096551	4.433939
498.899195	6764.335069	8.585229	-0.096553	4.436536
499.193852	6772.288553	8.590234	-0.096613	4.439097
499.645656	6780.358925	8.595239	-0.096702	4.441695
499.828568	6788.262422	8.600243	-0.096741	4.444236
500.418226	6796.392903	8.605248	-0.096856	4.446850
500.557522	6804.332723	8.610253	-0.096887	4.449400
500.977421	6812.431726	8.615258	-0.096970	4.452001
501.219557	6820.405745	8.620263	-0.097020	4.454559
501.243459	6828.454773	8.625267	-0.097030	4.457139
501.728971	6836.445493	8.630272	-0.097126	4.459700
501.814844	6844.468943	8.635277	-0.097147	4.462269
502.512737	6852.454595	8.640282	-0.097282	4.464827
502.571732	6860.492717	8.645287	-0.097298	4.467397
502.628254	6868.488623	8.650291	-0.097313	4.469953
503.037552	6876.532473	8.655296	-0.097395	4.472523
503.282058	6884.502997	8.660301	-0.097445	4.475068
503.843423	6892.498652	8.665306	-0.097555	4.477621
504.145360	6900.542474	8.670311	-0.097616	4.480187
504.217987	6908.592849	8.675315	-0.097635	4.482752
504.200093	6916.622479	8.680320	-0.097637	4.485309
504.184251	6924.604661	8.685325	-0.097639	4.487850
505.175814	6932.609137	8.690330	-0.097829	4.490399
505.285228	6940.658094	8.695335	-0.097854	4.492958
505.369060	6948.651035	8.700339	-0.097875	4.495498
505.623405	6956.714521	8.705344	-0.097927	4.498059
506.282172	6964.666157	8.710349	-0.098055	4.500585
506.659823	6972.650127	8.715354	-0.098131	4.503119
507.055619	6980.719348	8.720359	-0.098209	4.505678
507.355435	6988.695726	8.725363	-0.098270	4.508206
507.754721	6996.815769	8.730368	-0.098350	4.510778
507.981658	7004.760719	8.735373	-0.098397	4.513293
508.438880	7012.780062	8.740378	-0.098488	4.515830
508.632586	7020.728538	8.745383	-0.098529	4.518343
508.896669	7028.734255	8.750387	-0.098583	4.520873
509.505469	7036.740461	8.755392	-0.098701	4.523402
509.715677	7044.809359	8.760397	-0.098746	4.525949
510.040204	7052.836350	8.765402	-0.098811	4.528481
510.289305	7060.916169	8.770407	-0.098863	4.531028
510.595148	7068.892110	8.775411	-0.098925	4.533542
510.980880	7076.962229	8.780416	-0.099002	4.536083
511.124766	7084.878150	8.785421	-0.099034	4.538574
511.418420	7092.968141	8.790426	-0.099093	4.541119
511.758488	7100.911416	8.795431	-0.099162	4.543616
511.827497	7109.007320	8.800435	-0.099180	4.546160
512.106944	7116.994891	8.805440	-0.099237	4.548668
512.509961	7125.021968	8.810445	-0.099317	4.551187
512.978085	7132.965589	8.815450	-0.099409	4.553679
513.059057	7141.056761	8.820455	-0.099430	4.556215
513.341647	7148.969761	8.825459	-0.099487	4.558694
513.681611	7157.107292	8.830464	-0.099556	4.561243
513.804017	7164.962350	8.835469	-0.099584	4.563701
514.080580	7173.055498	8.840474	-0.099640	4.566232
514.428911	7181.077917	8.845479	-0.099710	4.568740
514.615080	7189.143743	8.850483	-0.099750	4.571259
514.787348	7197.154153	8.855488	-0.099787	4.573761
515.093012	7205.136337	8.860493	-0.099849	4.576252
515.078434	7213.161566	8.865498	-0.099852	4.578754
515.591336	7221.215848	8.870503	-0.099952	4.581265
516.162883	7229.087033	8.875507	-0.100064	4.583718
516.452245	7237.220621	8.880512	-0.100123	4.586250
516.579163	7245.223975	8.885517	-0.100152	4.588741
516.983284	7253.294965	8.890522	-0.100232	4.591251
517.299151	7261.236216	8.895527	-0.100296	4.593720
517.504890	7269.264673	8.900531	-0.100339	4.596214
517.777968	7277.275238	8.905536	-0.100395	4.598701
518.026149	7285.318508	8.910541	-0.100447	4.601197
518.386990	7293.209860	8.915546	-0.100519	4.603645
518.531402	7301.319707	8.920551	-0.100551	4.606159
518.806892	7309.255311	8.925555	-0.100607	4.608617
519.005369	7317.397156	8.930560	-0.100649	4.611138
518.959246	7325.363389	8.935565	-0.100646	4.613604
519.241817	7333.431225	8.940570	-0.100704	4.616099
519.817997	7341.385889	8.945575	-0.100816	4.618558
519.789566	7349.431786	8.950579	-0.100816	4.621044
520.198960	7357.388443	8.955584	-0.100897	4.623501
520.492714	7365.464973	8.960589	-0.100957	4.625994
520.815038	7373.462937	8.965594	-0.101022	4.628461
520.952881	7381.533286	8.970599	-0.101053	4.630948
521.117253	7389.479305	8.975603	-0.101089	4.633397
521.485250	7397.586738	8.980608	-0.101162	4.635893
521.764256	7405.490693	8.985613	-0.101219	4.638326
522.145749	7413.514662	8.990618	-0.101296	4.640794
522.427733	7421.525755	8.995623	-0.101353	4.643257
522.631488	7429.537110	9.000627	-0.101396	4.645719
522.733144	7437.632036	9.005632	-0.101420	4.648205
523.185575	7445.643169	9.010637	-0.101510	4.650664
523.496424	7453.625988	9.015642	-0.101573	4.653113
523.813712	7461.670184	9.020647	-0.101637	4.655579
524.139630	7469.629118	9.025651	-0.101703	4.658018
524.538133	7477.643461	9.030656	-0.101782	4.660473
524.742642	7485.634274	9.035661	-0.101825	4.662919
524.938243	7493.654866	9.040666	-0.101867	4.665373
525.232464	7501.762713	9.045671	-0.101927	4.667852
525.411972	7509.770484	9.050675	-0.101965	4.670299
525.694939	7517.845176	9.055680	-0.102023	4.672765
525.913889	7525.811553	9.060685	-0.102069	4.675198
526.395217	7533.785035	9.065690	-0.102164	4.677630
526.645800	7541.785648	9.070695	-0.102215	4.680070
526.759834	7549.757279	9.075699	-0.102242	4.682500
527.151667	7557.776156	9.080704	-0.102320	4.684943
527.201876	7565.809326	9.085709	-0.102334	4.687389
527.345840	7573.822478	9.090714	-0.102366	4.689827
527.657290	7581.903207	9.095719	-0.102429	4.692285
528.117864	7589.878038	9.100723	-0.102520	4.694709
528.402483	7597.944735	9.105728	-0.102578	4.697160
528.423212	7605.912679	9.110733	-0.102587	4.699579
528.697871	7613.980682	9.115738	-0.102644	4.702028
528.869003	7621.941292	9.120743	-0.102681	4.704443
529.173812	7630.018022	9.125747	-0.102742	4.706891
529.450919	7638.015465	9.130752	-0.102799	4.709315
529.879682	7645.962360	9.135757	-0.102884	4.711721
529.865185	7653.994355	9.140762	-0.102886	4.714153
529.919758	7662.127941	9.145767	-0.102902	4.716614
530.421562	7670.014681	9.150771	-0.103000	4.718998
530.692257	7678.107593	9.155776	-0.103056	4.721444
530.902359	7686.012144	9.160781	-0.103100	4.723832
531.201923	7694.135483	9.165786	-0.103161	4.726284
531.907180	7702.082958	9.170791	-0.103297	4.728681
532.095477	7710.139606	9.175795	-0.103338	4.731111
532.611891	7718.193657	9.180800	-0.103439	4.733538
532.662187	7726.231821	9.185805	-0.103453	4.735960
532.965926	7734.195286	9.190810	-0.103515	4.738358
533.351578	7742.243461	9.195815	-0.103592	4.740780
533.682409	7750.176084	9.200819	-0.103659	4.743165
534.117635	7758.312084	9.205824	-0.103745	4.745611
534.335303	7766.240661	9.210829	-0.103790	4.747993
534.470803	7774.336818	9.215834	-0.103821	4.750425
534.752985	7782.306443	9.220839	-0.103879	4.752817
534.969275	7790.329530	9.225843	-0.103924	4.755224
535.259703	7798.353320	9.230848	-0.103983	4.757630
535.453026	7806.351174	9.235853	-0.104024	4.760027
535.716625	7814.390320	9.240858	-0.104078	4.762435
536.154103	7822.332183	9.245863	-0.104165	4.764812
536.471127	7830.377093	9.250867	-0.104229	4.767219
536.931723	7838.450681	9.255872	-0.104320	4.769633
537.104018	7846.453380	9.260877	-0.104357	4.772026
537.357145	7854.430754	9.265882	-0.104409	4.774409
537.679161	7862.516484	9.270887	-0.104475	4.776823
537.933711	7870.401710	9.275891	-0.104527	4.779176
538.125893	7878.530895	9.280896	-0.104568	4.781602
538.658458	7886.431666	9.285901	-0.104672	4.783956
538.978420	7894.520463	9.290906	-0.104737	4.786366
539.212577	7902.543253	9.295911	-0.104786	4.788756
539.559561	7910.591464	9.300915	-0.104855	4.791152
539.879459	7918.563771	9.305920	-0.104920	4.793523
540.075894	7926.600515	9.310925	-0.104962	4.795914
540.509951	7934.546755	9.315930	-0.105048	4.798275
540.809608	7942.583580	9.320935	-0.105109	4.800662
541.112266	7950.556237	9.325939	-0.105170	4.803029
541.469015	7958.598893	9.330944	-0.105242	4.805416
541.677913	7966.667868	9.335949	-0.105286	4.807809
541.920683	7974.655090	9.340954	-0.105336	4.810177
542.399761	7982.687604	9.345959	-0.105430	4.812557
542.567440	7990.152836	9.350963	-0.105466	4.814768
542.904588	7994.813318	9.355968	-0.105532	4.816147

542.956080	7997.434972	9.360973	-0.105543	4.816923
543.260141	7998.809044	9.365978	-0.105601	4.817329
543.570395	7999.327069	9.370983	-0.105659	4.817481
543.204264	8000.143208	9.375987	-0.105591	4.817724
543.638645	8000.182208	9.380992	-0.105672	4.817734
543.799672	8000.131815	9.385997	-0.105701	4.817718
543.874741	8000.208827	9.391002	-0.105715	4.817740
544.175503	8000.189994	9.396007	-0.105771	4.817734
544.205563	8000.147186	9.401011	-0.105777	4.817721
544.359297	8000.204252	9.406016	-0.105805	4.817737
544.273244	8000.132335	9.411021	-0.105789	4.817716
544.610686	8000.127746	9.416026	-0.105852	4.817713
544.894018	8000.148734	9.421031	-0.105905	4.817718
544.678271	8000.065438	9.426035	-0.105864	4.817694
545.132344	8000.106839	9.431040	-0.105949	4.817705
544.991972	8000.090024	9.436045	-0.105922	4.817700
545.195132	8000.067662	9.441050	-0.105960	4.817693
545.081471	8000.158803	9.446055	-0.105939	4.817720
545.097191	8000.126331	9.451059	-0.105942	4.817711
545.505798	8000.163909	9.456064	-0.106018	4.817720
545.488291	8000.178410	9.461069	-0.106014	4.817724
545.623196	8000.136072	9.466074	-0.106039	4.817711
545.801465	8000.204045	9.471079	-0.106072	4.817731
545.707193	8000.115132	9.476083	-0.106055	4.817705
545.761054	8000.203440	9.481088	-0.106065	4.817731
545.791002	8000.162738	9.486093	-0.106070	4.817719
546.105777	8000.092436	9.491098	-0.106129	4.817696
545.936571	8000.184879	9.496103	-0.106097	4.817724
545.955129	8000.090226	9.501107	-0.106100	4.817696
546.203452	8000.143400	9.506112	-0.106147	4.817711
546.328234	8000.104079	9.511117	-0.106170	4.817699
546.301051	8000.083637	9.516122	-0.106164	4.817693
546.358666	8000.102397	9.521127	-0.106175	4.817698
546.348980	8000.098029	9.526131	-0.106173	4.817697
546.575237	8000.123462	9.531136	-0.106215	4.817704
546.675404	8000.155497	9.536141	-0.106234	4.817713
546.762591	8000.093481	9.541146	-0.106250	4.817694
546.746056	8000.159674	9.546151	-0.106247	4.817714
546.424551	8000.142327	9.551155	-0.106187	4.817710
546.841025	8000.192679	9.556160	-0.106264	4.817723
546.913368	8000.165250	9.561165	-0.106278	4.817714
546.950074	8000.095116	9.566170	-0.106284	4.817694
547.377262	8000.138243	9.571175	-0.106364	4.817704
547.195220	8000.170386	9.576179	-0.106330	4.817715
547.410629	8000.211484	9.581184	-0.106370	4.817726
547.276328	8000.136748	9.586189	-0.106345	4.817704
547.075985	8000.232957	9.591194	-0.106307	4.817734
547.281309	8000.235940	9.596199	-0.106345	4.817734
547.034441	8000.181712	9.601203	-0.106299	4.817719
547.302622	8000.249945	9.606208	-0.106349	4.817738
547.268345	8000.175612	9.611213	-0.106343	4.817716
547.405878	8000.160733	9.616218	-0.106368	4.817711
547.680297	8000.138358	9.621223	-0.106419	4.817703
547.533587	8000.165742	9.626227	-0.106392	4.817712
547.482322	8000.139675	9.631232	-0.106382	4.817704
547.541224	8000.150017	9.636237	-0.106393	4.817707
547.637486	8000.219963	9.641242	-0.106411	4.817728
547.718670	8000.226412	9.646247	-0.106426	4.817729
547.492689	8000.192525	9.651251	-0.106384	4.817720
547.709177	8000.194617	9.656256	-0.106424	4.817720
547.671243	8000.191947	9.661261	-0.106417	4.817719
547.764496	8000.088887	9.666266	-0.106434	4.817688
548.005570	8000.147234	9.671271	-0.106479	4.817704
548.064306	8000.055272	9.676275	-0.106489	4.817677
547.973025	8000.144634	9.681280	-0.106472	4.817704
547.846671	8000.194462	9.686285	-0.106449	4.817719
547.883731	8000.172846	9.691290	-0.106456	4.817713
548.122657	8000.216397	9.696295	-0.106500	4.817724
547.922469	8000.103787	9.701299	-0.106462	4.817692
547.938996	8000.199993	9.706304	-0.106465	4.817720
547.880711	8000.203354	9.711309	-0.106455	4.817722
547.876272	8000.211718	9.716314	-0.106454	4.817724
548.154377	8000.244239	9.721319	-0.106505	4.817733
548.151762	8000.195678	9.726323	-0.106505	4.817718
548.198442	8000.210061	9.731328	-0.106513	4.817722
548.223560	8000.201982	9.736333	-0.106518	4.817720
548.354876	8000.181740	9.741338	-0.106542	4.817713
548.442715	8000.263167	9.746343	-0.106558	4.817737
548.138670	8000.227086	9.751347	-0.106502	4.817728
548.166118	8000.242243	9.756352	-0.106507	4.817732
548.441561	8000.196681	9.761357	-0.106558	4.817717
548.456596	8000.165252	9.766362	-0.106561	4.817708
548.528118	8000.252770	9.771367	-0.106574	4.817734
548.665547	8000.252656	9.776371	-0.106599	4.817733
548.631016	8000.265855	9.781376	-0.106593	4.817737
548.527373	8000.264335	9.786381	-0.106573	4.817737
548.909304	8000.228764	9.791386	-0.106644	4.817725
548.663239	8000.304268	9.796391	-0.106599	4.817748
548.634681	8000.242672	9.801395	-0.106593	4.817730
548.763618	8000.243489	9.806400	-0.106617	4.817730
548.925408	8000.199434	9.811405	-0.106647	4.817716
548.765367	8000.218186	9.816410	-0.106617	4.817722
548.911740	8000.207656	9.821415	-0.106644	4.817719
549.046986	8000.187471	9.826419	-0.106669	4.817712
549.080846	8000.166863	9.831424	-0.106675	4.817706
548.981050	8000.233954	9.836429	-0.106657	4.817726
548.897929	8000.207421	9.841434	-0.106641	4.817719
548.857547	8000.260613	9.846439	-0.106634	4.817734
548.871620	8000.159560	9.851443	-0.106636	4.817704
549.159810	8000.184848	9.856448	-0.106690	4.817711
548.902995	8000.143126	9.861453	-0.106642	4.817699
548.981388	8000.153753	9.866458	-0.106656	4.817702
549.191434	8000.214816	9.871463	-0.106695	4.817719
549.117888	8000.147290	9.876467	-0.106681	4.817700
549.112504	8000.111344	9.881472	-0.106680	4.817689
549.180482	8000.208303	9.886477	-0.106693	4.817718
549.222387	8000.239492	9.891482	-0.106701	4.817727
549.418138	8000.238120	9.896487	-0.106737	4.817725
549.307207	8000.208017	9.901491	-0.106716	4.817717
549.349686	8000.194917	9.906496	-0.106724	4.817713
549.320020	8000.210297	9.911501	-0.106718	4.817718
549.145796	8000.239388	9.916506	-0.106686	4.817727
549.188019	8000.254761	9.921511	-0.106694	4.817731
549.242753	8000.213364	9.926515	-0.106704	4.817719
549.383374	8000.214352	9.931520	-0.106730	4.817719
549.479557	8000.187269	9.936525	-0.106747	4.817710
549.361754	8000.219293	9.941530	-0.106725	4.817720
549.653151	8000.241465	9.946535	-0.106780	4.817725
549.449543	8000.222666	9.951539	-0.106742	4.817721
549.484851	8000.267470	9.956544	-0.106748	4.817734
549.183819	8000.298931	9.961549	-0.106692	4.817744
549.392199	8000.192274	9.966554	-0.106731	4.817712
549.434490	8000.247726	9.971559	-0.106738	4.817728
549.394563	8000.260847	9.976563	-0.106731	4.817732
549.854768	8000.257005	9.981568	-0.106816	4.817729
549.672803	8000.252233	9.986573	-0.106782	4.817729
549.569033	8000.257039	9.991578	-0.106763	4.817730
549.378549	8000.291166	9.996583	-0.106727	4.817741
549.285442	8000.243393	10.001587	-0.106710	4.817728
549.454740	8000.224760	10.006592	-0.106741	4.817721
549.461122	8000.180548	10.011597	-0.106742	4.817708
549.577012	8000.136878	10.016602	-0.106764	4.817695
549.713899	8000.231680	10.021607	-0.106789	4.817722
549.549866	8000.193419	10.026611	-0.106759	4.817712
549.824427	8000.235385	10.031616	-0.106810	4.817723
549.758849	8000.181685	10.036621	-0.106797	4.817707
549.915455	8000.121734	10.041626	-0.106826	4.817689
549.931131	8000.191565	10.046631	-0.106829	4.817709
550.035699	8000.134018	10.051635	-0.106849	4.817692
549.915193	8000.219793	10.056640	-0.106826	4.817718
549.795995	8000.186404	10.061645	-0.106804	4.817709
549.656155	8000.197013	10.066650	-0.106778	4.817712
549.829876	8000.232234	10.071655	-0.106810	4.817722
549.874966	8000.176984	10.076659	-0.106818	4.817705
549.912120	8000.248183	10.081664	-0.106825	4.817726
549.821523	8000.261619	10.086669	-0.106808	4.817731
549.800240	8000.187471	10.091674	-0.106804	4.817709
550.038688	8000.262662	10.096679	-0.106848	4.817730
549.895923	8000.225765	10.101683	-0.106822	4.817720
550.046005	8000.293339	10.106688	-0.106849	4.817739
550.128830	8000.250241	10.111693	-0.106865	4.817726
550.157785	8000.178935	10.116698	-0.106870	4.817705
550.097587	8000.235002	10.121703	-0.106859	4.817722
549.959119	8000.138050	10.126707	-0.106833	4.817694
550.189508	8000.165661	10.131712	-0.106876	4.817701
550.048478	8000.261684	10.136717	-0.106849	4.817730
550.159818	8000.245370	10.141722	-0.106870	4.817724
550.069219	8000.274626	10.146727	-0.106853	4.817734
550.197432	8000.227972	10.151731	-0.106877	4.817719
550.285342	8000.244012	10.156736	-0.106893	4.817724
550.339532	8000.253233	10.161741	-0.106903	4.817726
550.398712	8000.214008	10.166746	-0.106914	4.817714
550.462732	8000.259233	10.171751	-0.106926	4.817727
550.264750	8000.189888	10.176755	-0.106889	4.817708
550.372167	8000.231526	10.181760	-0.106909	4.817719
550.333846	8000.264710	10.186765	-0.106901	4.817729
550.244309	8000.214878	10.191770	-0.106884	4.817715
550.501641	8000.209132	10.196775	-0.106932	4.817712
550.388903	8000.186385	10.201779	-0.106911	4.817706
550.212298	8000.281888	10.206784	-0.106878	4.817735
550.449653	8000.265304	10.211789	-0.106922	4.817729
550.480299	8000.175037	10.216794	-0.106928	4.817702
550.313141	8000.206340	10.221799	-0.106897	4.817712
550.238330	8000.230554	10.226803	-0.106883	4.817720
550.444199	8000.272574	10.231808	-0.106921	4.817731
550.427356	8000.247007	10.236813	-0.106918	4.817724
550.334147	8000.168644	10.241818	-0.106900	4.817701
550.622265	8000.244561	10.246823	-0.106954	4.817722
550.721673	8000.148969	10.251827	-0.106972	4.817694
550.474173	8000.185428	10.256832	-0.106926	4.817705
550.342813	8000.243622	10.261837	-0.106901	4.817723
550.715882	8000.210033	10.266842	-0.106971	4.817712
550.731992	8000.275653	10.271847	-0.106974	4.817731
550.329457	8000.205432	10.276851	-0.106899	4.817712
550.350538	8000.288000	10.281856	-0.106902	4.817736
550.425299	8000.273262	10.286861	-0.106916	4.817732
550.273777	8000.223580	10.291866	-0.106888	4.817718
550.559396	8000.189770	10.296871	-0.106941	4.817706
550.480264	8000.221303	10.301875	-0.106926	4.817716
550.633132	8000.256222	10.306880	-0.106954	4.817726
550.435533	8000.212196	10.311885	-0.106918	4.817714
550.646171	8000.208933	10.316890	-0.106957	4.817712
550.690259	8000.260195	10.321895	-0.106965	4.817727
550.546433	8000.257033	10.326899	-0.106938	4.817726
550.474406	8000.249645	10.331904	-0.106924	4.817724
550.714295	8000.242591	10.336909	-0.106969	4.817721
550.560267	8000.160175	10.341914	-0.106940	4.817698
550.544442	8000.203180	10.346919	-0.106937	4.817710
550.735263	8000.188026	10.351923	-0.106973	4.817705
550.575967	8000.203623	10.356928	-0.106943	4.817710
550.543286	8000.167278	10.361933	-0.106937	4.817700
550.795308	8000.151962	10.366938	-0.106983	4.817694
551.002708	8000.220374	10.371943	-0.107022	4.817714
550.930138	8000.143366	10.376947	-0.107008	4.817691
551.029532	8000.201763	10.381952	-0.107027	4.817708
550.731120	8000.248027	10.386957	-0.106971	4.817723
550.744138	8000.209184	10.391962	-0.106973	4.817711
550.804216	8000.242749	10.396967	-0.106984	4.817721
550.733341	8000.145726	10.401971	-0.106971	4.817693
550.820032	8000.180734	10.406976	-0.106987	4.817703
550.720352	8000.259430	10.411981	-0.106969	4.817726
550.760128	8000.135545	10.416986	-0.106976	4.817689
550.895978	8000.227171	10.421991	-0.107001	4.817716
550.745637	8000.154302	10.426995	-0.106973	4.817695
550.787110	8000.159117	10.432000	-0.106980	4.817696
550.847465	8000.188468	10.437005	-0.106992	4.817705
550.970286	8000.155446	10.442010	-0.107014	4.817694
550.979733	8000.193546	10.447015	-0.107016	4.817706
550.980547	8000.153469	10.452019	-0.107016	4.817694
551.016981	8000.205675	10.457024	-0.107023	4.817709
550.855157	8000.240220	10.462029	-0.106993	4.817720
550.946834	8000.152953	10.467034	-0.107009	4.817694
551.134948	8000.192605	10.472039	-0.107044	4.817705
551.083754	8000.161263	10.477043	-0.107035	4.817696
550.854668	8000.235961	10.482048	-0.106992	4.817719
551.048294	8000.242998	10.487053	-0.107028	4.817720
550.974490	8000.264062	10.492058	-0.107014	4.817727
550.589344	8000.315387	10.497063	-0.106942	4.817743
550.780133	8000.249606	10.502067	-0.106978	4.817723
550.962352	8000.267024	10.507072	-0.107012	4.817728
551.063826	8000.240019	10.512077	-0.107030	4.817719
550.995716	8000.281206	10.517082	-0.107018	4.817732
550.887998	8000.305993	10.522087	-0.106997	4.817739
550.811495	8000.229982	10.527091	-0.106983	4.817717
550.752740	8000.262868	10.532096	-0.106972	4.817727
550.927005	8000.247473	10.537101	-0.107004	4.817722
550.947331	8000.186587	10.542106	-0.107008	4.817704
551.157493	8000.259259	10.547111	-0.107047	4.817724
550.788318	8000.268628	10.552115	-0.106978	4.817729
550.889369	8000.302791	10.557120	-0.106997	4.817739
550.850513	8000.279011	10.562125	-0.106990	4.817732
550.691478	8000.265080	10.567130	-0.106960	4.817728
551.196951	8000.247136	10.572135	-0.107054	4.817721
551.193998	8000.250249	10.577139	-0.107053	4.817722
550.831386	8000.315615	10.582144	-0.106986	4.817743
550.841182	8000.298874	10.587149	-0.106987	4.817738
551.057076	8000.246116	10.592154	-0.107027	4.817721
550.971756	8000.323967	10.597159	-0.107011	4.817744
550.900447	8000.245922	10.602163	-0.106998	4.817722
550.601915	8000.341756	10.607168	-0.106942	4.817751
550.553265	8000.316779	10.612173	-0.106933	4.817744
550.857131	8000.234718	10.617178	-0.106990	4.817719
550.958289	8000.327948	10.622183	-0.107008	4.817746
550.980439	8000.224899	10.627187	-0.107012	4.817715
551.104807	8000.243582	10.632192	-0.107035	4.817720
551.225958	8000.268547	10.637197	-0.107058	4.817727
550.854609	8000.300033	10.642202	-0.106989	4.817738
551.113997	8000.320687	10.647207	-0.107037	4.817743
551.158369	8000.275973	10.652211	-0.107045	4.817729
551.263016	8000.315463	10.657216	-0.107064	4.817741
551.149836	8000.299036	10.662221	-0.107043	4.817736
551.075300	8000.259969	10.667226	-0.107029	4.817725
551.145627	8000.329545	10.672231	-0.107042	4.817745
551.175321	8000.301493	10.677235	-0.107048	4.817737
550.856071	8000.328466	10.682240	-0.106988	4.817746
551.017485	8000.331869	10.687245	-0.107018	4.817747
551.048287	8000.301723	10.692250	-0.107024	4.817738
550.935448	8000.277918	10.697255	-0.107003	4.817731
550.828003	8000.299545	10.702259	-0.106982	4.817738
551.325389	8000.271991	10.707264	-0.107075	4.817728
551.127591	8000.299683	10.712269	-0.107038	4.817737
551.349214	8000.166849	10.717274	-0.107079	4.817696
551.199520	8000.313373	10.722279	-0.107051	4.817740
551.272164	8000.230046	10.727283	-0.107065	4.817715
551.464400	8000.214914	10.732288	-0.107100	4.817710
551.393281	8000.262385	10.737293	-0.107087	4.817724
551.505157	8000.197562	10.742298	-0.107108	4.817705
551.564549	8000.277526	10.747303	-0.107119	4.817728
551.468279	8000.220211	10.752307	-0.107101	4.817712
551.624662	8000.179241	10.757312	-0.107130	4.817699
551.583441	8000.157536	10.762317	-0.107122	4.817693
551.491060	8000.186767	10.767322	-0.107104	4.817702
551.487098	8000.298504	10.772327	-0.107104	4.817735
551.218228	8000.317774	10.777331	-0.107054	4.817742
550.994963	8000.331382	10.782336	-0.107012	4.817747
551.183936	8000.320421	10.787341	-0.107047	4.817743
551.313218	8000.327574	10.792346	-0.107071	4.817744
551.302580	8000.310535	10.797351	-0.107069	4.817739
551.089508	8000.301087	10.802355	-0.107029	4.817737
551.592692	8000.308425	10.807360	-0.107123	4.817737
551.688056	8000.305591	10.812365	-0.107140	4.817736
551.330443	8000.275047	10.817370	-0.107074	4.817729
551.576357	8000.342969	10.822375	-0.107119	4.817748
551.514523	8000.312525	10.827379	-0.107108	4.817739
551.031867	8000.333948	10.832384	-0.107018	4.817747
551.351909	8000.375528	10.837389	-0.107077	4.817758
551.467874	8000.355063	10.842394	-0.107099	4.817752
551.115126	8000.386821	10.847399	-0.107033	4.817763
550.692238	8000.367982	10.852403	-0.106954	4.817759
551.082547	8000.393712	10.857408	-0.107027	4.817765
551.254649	8000.367738	10.862413	-0.107059	4.817756
551.252537	8000.280155	10.867418	-0.107058	4.817730
551.606464	8000.326449	10.872423	-0.107124	4.817743
551.768316	8000.264465	10.877427	-0.107154	4.817724
551.575741	8000.312272	10.882432	-0.107118	4.817739
551.828762	8000.310685	10.887437	-0.107165	4.817737
552.011213	8000.261658	10.892442	-0.107199	4.817722
551.781275	8000.340563	10.897447	-0.107156	4.817746
551.279414	8000.324789	10.902451	-0.107062	4.817743
551.112234	8000.362420	10.907456	-0.107031	4.817755
550.856121	8000.359727	10.912461	-0.106983	4.817756
551.004882	8000.370328	10.917466	-0.107011	4.817758
551.296844	8000.380911	10.922471	-0.107065	4.817760
551.059693	8000.379550	10.927475	-0.107021	4.817761
551.214764	8000.369149	10.932480	-0.107050	4.817757
551.133324	8000.356349	10.937485	-0.107034	4.817753
551.343489	8000.323548	10.942490	-0.107073	4.817743
551.047764	8000.365631	10.947495	-0.107018	4.817757
551.235268	8000.325116	10.952499	-0.107053	4.817744
551.337170	8000.310774	10.957504	-0.107072	4.817739
551.347055	8000.358374	10.962509	-0.107074	4.817753
551.364793	8000.333310	10.967514	-0.107077	4.817746
551.606426	8000.336830	10.972519	-0.107122	4.817746
551.508739	8000.295315	10.977523	-0.107103	4.817734
551.891284	8000.278743	10.982528	-0.107174	4.817727
551.727049	8000.298486	10.987533	-0.107144	4.817734
551.841295	8000.260066	10.992538	-0.107165	4.817722
552.046001	8000.245116	10.997543	-0.107203	4.817717
552.005692	8000.262450	11.002547	-0.107195	4.817722
552.212977	8000.199019	11.007552	-0.107234	4.817702
552.210970	8000.261212	11.012557	-0.107233	4.817721
551.873336	8000.256273	11.017562	-0.107170	4.817721
552.042115	8000.266113	11.022567	-0.107202	4.817723
552.054945	8000.281058	11.027571	-0.107204	4.817727
551.979336	8000.278891	11.032576	-0.107190	4.817727
551.967206	8000.269213	11.037581	-0.107187	4.817724
552.097397	8000.196218	11.042586	-0.107212	4.817702
552.134589	8000.271641	11.047591	-0.107218	4.817724
551.867825	8000.273010	11.052595	-0.107169	4.817726
551.833945	8000.294657	11.057600	-0.107162	4.817732
552.123461	8000.270399	11.062605	-0.107216	4.817724
552.114103	8000.232282	11.067610	-0.107214	4.817713
552.191082	8000.272424	11.072615	-0.107228	4.817724
552.141793	8000.250601	11.077619	-0.107219	4.817718
552.142274	8000.290681	11.082624	-0.107219	4.817730
552.269345	8000.315733	11.087629	-0.107243	4.817737
552.476859	8000.186910	11.092634	-0.107281	4.817698
552.655605	8000.268620	11.097639	-0.107314	4.817721
552.424580	8000.253635	11.102643	-0.107271	4.817718
552.140131	8000.292717	11.107648	-0.107218	4.817730
552.480967	8000.261825	11.112653	-0.107282	4.817720
552.431687	8000.192537	11.117658	-0.107272	4.817699
552.304889	8000.264511	11.122663	-0.107249	4.817721
552.356214	8000.238883	11.127667	-0.107258	4.817714
552.404447	8000.183676	11.132672	-0.107267	4.817697
552.463088	8000.208784	11.137677	-0.107278	4.817704
552.220091	8000.261129	11.142682	-0.107232	4.817721
552.388481	8000.262526	11.147687	-0.107264	4.817720
552.314753	8000.306796	11.152691	-0.107250	4.817734
552.267471	8000.235427	11.157696	-0.107241	4.817713
552.615153	8000.299565	11.162701	-0.107305	4.817730
552.577077	8000.217783	11.167706	-0.107298	4.817706
552.318479	8000.296269	11.172711	-0.107250	4.817731
552.229281	8000.284410	11.177715	-0.107233	4.817728
552.264535	8000.314450	11.182720	-0.107240	4.817736
552.195858	8000.322932	11.187725	-0.107227	4.817739
552.337086	8000.255372	11.192730	-0.107253	4.817719
552.390431	8000.281457	11.197735	-0.107263	4.817726
552.239933	8000.283470	11.202739	-0.107235	4.817727
552.180206	8000.249891	11.207744	-0.107223	4.817718
552.342382	8000.290223	11.212749	-0.107254	4.817729
552.155847	8000.288545	11.217754	-0.107219	4.817729
552.261101	8000.259486	11.222759	-0.107238	4.817720
552.125318	8000.249056	11.227763	-0.107213	4.817718
552.439565	8000.179804	11.232768	-0.107271	4.817696
552.427490	8000.289315	11.237773	-0.107269	4.817728
552.419815	8000.249114	11.242778	-0.107267	4.817716
552.540725	8000.313103	11.247783	-0.107290	4.817735
552.505719	8000.267228	11.252787	-0.107283	4.817721
552.468760	8000.210777	11.257792	-0.107276	4.817705
552.543671	8000.273040	11.262797	-0.107290	4.817723
552.477536	8000.228820	11.267802	-0.107278	4.817710
552.408584	8000.300583	11.272807	-0.107265	4.817732
552.560289	8000.263765	11.277811	-0.107293	4.817720
552.710114	8000.210042	11.282816	-0.107321	4.817704
552.555664	8000.293214	11.287821	-0.107292	4.817729
552.291272	8000.200744	11.292826	-0.107242	4.817703
552.706745	8000.222625	11.297831	-0.107320	4.817707
552.592721	8000.237828	11.302835	-0.107298	4.817712
552.488835	8000.231028	11.307840	-0.107279	4.817711
552.604970	8000.251702	11.312845	-0.107300	4.817716
552.689381	8000.204407	11.317850	-0.107316	4.817702
552.730428	8000.211327	11.322855	-0.107323	4.817704
552.490116	8000.215192	11.327859	-0.107279	4.817706
552.572950	8000.214284	11.332864	-0.107294	4.817705
552.795287	8000.296632	11.337869	-0.107335	4.817729
552.468627	8000.254934	11.342874	-0.107274	4.817718
552.506364	8000.294504	11.347879	-0.107281	4.817729
552.427362	8000.318656	11.352883	-0.107266	4.817737
551.973376	8000.337331	11.357888	-0.107182	4.817744
552.680115	8000.271702	11.362893	-0.107313	4.817722
552.773708	8000.190789	11.367898	-0.107331	4.817698
552.686439	8000.286545	11.372903	-0.107314	4.817726
552.557229	8000.314183	11.377907	-0.107290	4.817735
552.474039	8000.247564	11.382912	-0.107274	4.817716
552.541881	8000.308668	11.387917	-0.107287	4.817734
552.501839	8000.279596	11.392922	-0.107279	4.817725
552.571614	8000.252128	11.397927	-0.107292	4.817717
552.723655	8000.208986	11.402931	-0.107321	4.817703
552.737659	8000.217620	11.407936	-0.107323	4.817706
552.621994	8000.267606	11.412941	-0.107301	4.817721
552.844784	8000.190689	11.417946	-0.107343	4.817697
552.784445	8000.272072	11.422951	-0.107331	4.817722
552.822394	8000.220934	11.427955	-0.107338	4.817706
552.766747	8000.219058	11.432960	-0.107328	4.817706
552.630476	8000.258195	11.437965	-0.107302	4.817718
552.864470	8000.168785	11.442970	-0.107346	4.817691
553.006326	8000.236245	11.447975	-0.107372	4.817710
552.924177	8000.201284	11.452979	-0.107357	4.817700
552.886477	8000.221820	11.457984	-0.107350	4.817706
552.578299	8000.303802	11.462989	-0.107292	4.817732
552.676863	8000.299960	11.467994	-0.107310	4.817730
552.598141	8000.304075	11.472999	-0.107296	4.817732
552.537457	8000.229346	11.478003	-0.107284	4.817710
552.831692	8000.189335	11.483008	-0.107339	4.817697
552.768054	8000.240081	11.488013	-0.107327	4.817712
552.535335	8000.170223	11.493018	-0.107284	4.817693
552.635505	8000.261334	11.498023	-0.107302	4.817719
552.765867	8000.244244	11.503027	-0.107326	4.817714
552.704062	8000.205361	11.508032	-0.107315	4.817702
552.845638	8000.292857	11.513037	-0.107341	4.817728
552.747386	8000.248168	11.518042	-0.107323	4.817715
552.450321	8000.358790	11.523047	-0.107267	4.817749
552.366354	8000.334351	11.528051	-0.107251	4.817742
552.575403	8000.276219	11.533056	-0.107290	4.817724
552.706728	8000.283403	11.538061	-0.107315	4.817725
552.663141	8000.159350	11.543066	-0.107306	4.817689
552.639689	8000.270805	11.548071	-0.107302	4.817722
552.667641	8000.276479	11.553075	-0.107307	4.817724
552.802063	8000.177176	11.558080	-0.107332	4.817694
552.739438	8000.193129	11.563085	-0.107320	4.817699
552.747614	8000.100420	11.568090	-0.107321	4.817671
552.919215	8000.247422	11.573095	-0.107353	4.817714
552.673354	8000.279685	11.578099	-0.107308	4.817724
552.614910	8000.253508	11.583104	-0.107296	4.817717
553.079386	8000.257121	11.588109	-0.107383	4.817716
552.864576	8000.220222	11.593114	-0.107343	4.817706
552.961222	8000.270145	11.598119	-0.107361	4.817720
552.862365	8000.248652	11.603123	-0.107342	4.817714
552.991443	8000.209393	11.608128	-0.107366	4.817702
552.969814	8000.278684	11.613133	-0.107362	4.817723
552.919019	8000.223085	11.618138	-0.107352	4.817707
553.186330	8000.240694	11.623143	-0.107402	4.817711
552.902369	8000.244975	11.628147	-0.107349	4.817713
552.935990	8000.232801	11.633152	-0.107355	4.817709
552.890712	8000.277487	11.638157	-0.107347	4.817723
552.695844	8000.276741	11.643162	-0.107310	4.817724
552.785317	8000.265383	11.648167	-0.107327	4.817720
552.666342	8000.287896	11.653171	-0.107305	4.817727
552.727061	8000.258186	11.658176	-0.107316	4.817718
552.831963	8000.314559	11.663181	-0.107335	4.817734
552.972428	8000.180536	11.668186	-0.107361	4.817694
553.147524	8000.242154	11.673191	-0.107394	4.817711
553.095418	8000.246658	11.678195	-0.107384	4.817713
552.784778	8000.253714	11.683200	-0.107326	4.817716
552.920738	8000.284171	11.688205	-0.107351	4.817725
553.098389	8000.184444	11.693210	-0.107384	4.817694
552.950020	8000.251884	11.698215	-0.107356	4.817715
553.045363	8000.210023	11.703219	-0.107374	4.817702
553.098044	8000.186524	11.708224	-0.107384	4.817695
552.963450	8000.240453	11.713229	-0.107359	4.817712
552.695829	8000.247083	11.718234	-0.107309	4.817715
552.881806	8000.283544	11.723239	-0.107343	4.817725
552.734287	8000.287709	11.728243	-0.107316	4.817727
552.646653	8000.277983	11.733248	-0.107299	4.817724
553.391129	8000.268810	11.738253	-0.107438	4.817718
553.131374	8000.169021	11.743258	-0.107389	4.817690
552.996480	8000.218727	11.748263	-0.107364	4.817705
553.008182	8000.301162	11.753267	-0.107366	4.817729
553.180622	8000.223510	11.758272	-0.107398	4.817706
552.914129	8000.267073	11.763277	-0.107348	4.817720
552.836506	8000.256438	11.768282	-0.107334	4.817717
553.044602	8000.305880	11.773287	-0.107373	4.817731
553.014094	8000.307536	11.778291	-0.107367	4.817731
552.958249	8000.242370	11.783296	-0.107356	4.817712
553.107804	8000.250875	11.788301	-0.107384	4.817714
553.073807	8000.171262	11.793306	-0.107377	4.817691
553.008055	8000.212484	11.798311	-0.107365	4.817703
553.028583	8000.243364	11.803315	-0.107369	4.817712
552.887575	8000.303528	11.808320	-0.107343	4.817731
553.004427	8000.284131	11.813325	-0.107364	4.817724
552.902644	8000.215130	11.818330	-0.107345	4.817704
552.697788	8000.313388	11.823335	-0.107307	4.817734
552.868089	8000.277895	11.828339	-0.107338	4.817723
552.963988	8000.197015	11.833344	-0.107356	4.817699
553.169495	8000.282282	11.838349	-0.107394	4.817723
553.143380	8000.196455	11.843354	-0.107389	4.817698
552.957854	8000.235928	11.848359	-0.107355	4.817710
553.039672	8000.256101	11.853363	-0.107370	4.817716
553.049990	8000.269955	11.858368	-0.107372	4.817720
552.919105	8000.327102	11.863373	-0.107347	4.817738
552.747859	8000.268689	11.868378	-0.107315	4.817721
552.756865	8000.313113	11.873383	-0.107317	4.817734
552.896700	8000.299326	11.878387	-0.107343	4.817729
553.025083	8000.204153	11.883392	-0.107366	4.817701
553.181536	8000.247567	11.888397	-0.107396	4.817713
553.137228	8000.209994	11.893402	-0.107387	4.817702
553.001562	8000.315592	11.898407	-0.107362	4.817734
553.019982	8000.245182	11.903411	-0.107365	4.817713
553.076330	8000.206970	11.908416	-0.107376	4.817701
553.183174	8000.247550	11.913421	-0.107395	4.817713
553.110544	8000.172646	11.918426	-0.107382	4.817691
553.384593	8000.226216	11.923431	-0.107433	4.817706
553.226747	8000.201751	11.928435	-0.107403	4.817699
553.130155	8000.131771	11.933440	-0.107385	4.817679
553.233215	8000.250349	11.938445	-0.107404	4.817714
552.919930	8000.189860	11.943450	-0.107346	4.817697
553.325415	8000.206324	11.948455	-0.107421	4.817700
553.120972	8000.186452	11.953459	-0.107383	4.817695
553.057757	8000.161260	11.958464	-0.107371	4.817688
553.250073	8000.257937	11.963469	-0.107407	4.817716
553.078308	8000.198461	11.968474	-0.107375	4.817699
553.390290	8000.192463	11.973479	-0.107433	4.817696
553.250833	8000.198855	11.978483	-0.107407	4.817698
553.254812	8000.227384	11.983488	-0.107407	4.817707
553.273213	8000.312028	11.988493	-0.107411	4.817732
553.293120	8000.251133	11.993498	-0.107414	4.817714
553.261320	8000.247496	11.998503	-0.107408	4.817713
552.978175	8000.333007	12.003507	-0.107355	4.817739
553.134251	8000.289923	12.008512	-0.107384	4.817726
553.189651	8000.327642	12.013517	-0.107394	4.817737
552.921821	8000.334268	12.018522	-0.107344	4.817740
553.106322	8000.268395	12.023527	-0.107379	4.817719
552.891726	8000.320100	12.028531	-0.107339	4.817736
553.127509	8000.303495	12.033536	-0.107382	4.817730
553.032345	8000.349562	12.038541	-0.107365	4.817744
552.817184	8000.323205	12.043546	-0.107324	4.817737
553.252820	8000.317959	12.048551	-0.107405	4.817734
553.006226	8000.290088	12.053555	-0.107359	4.817726
553.004270	8000.322749	12.058560	-0.107359	4.817736
553.165870	8000.302951	12.063565	-0.107389	4.817729
552.806487	8000.269213	12.068570	-0.107322	4.817721
552.996112	8000.281468	12.073575	-0.107357	4.817724
552.798103	8000.339744	12.078579	-0.107320	4.817742
552.912081	8000.258074	12.083584	-0.107341	4.817717
553.142537	8000.281473	12.088589	-0.107384	4.817723
553.082178	8000.278473	12.093594	-0.107373	4.817723
553.393150	8000.261913	12.098599	-0.107431	4.817716
553.309560	8000.279670	12.103603	-0.107415	4.817722
553.414074	8000.192586	12.108608	-0.107434	4.817696
553.445833	8000.293247	12.113613	-0.107440	4.817725
553.087752	8000.276404	12.118618	-0.107373	4.817722
552.937011	8000.287905	12.123623	-0.107345	4.817726
553.001489	8000.292003	12.128627	-0.107357	4.817727
553.280803	8000.173721	12.133632	-0.107409	4.817691
553.301708	8000.246798	12.138637	-0.107413	4.817712
553.371939	8000.208789	12.143642	-0.107426	4.817701
553.405398	8000.243023	12.148647	-0.107432	4.817711
553.284197	8000.287654	12.153651	-0.107409	4.817724
553.393821	8000.237563	12.158656	-0.107429	4.817709
553.497526	8000.291810	12.163661	-0.107449	4.817725
553.254405	8000.259770	12.168666	-0.107403	4.817716
553.467186	8000.213295	12.173671	-0.107443	4.817702
553.599654	8000.253195	12.178675	-0.107467	4.817713
553.440925	8000.226607	12.183680	-0.107438	4.817706
553.408162	8000.348476	12.188685	-0.107431	4.817742
553.568417	8000.308618	12.193690	-0.107461	4.817729
553.555868	8000.298933	12.198695	-0.107459	4.817727
553.427027	8000.295987	12.203699	-0.107435	4.817726
553.375234	8000.196072	12.208704	-0.107425	4.817697
553.574669	8000.234840	12.213709	-0.107462	4.817708
553.514125	8000.180153	12.218714	-0.107450	4.817692
553.561853	8000.269445	12.223719	-0.107459	4.817718
553.355761	8000.286466	12.228723	-0.107421	4.817724
553.349670	8000.243122	12.233728	-0.107420	4.817711
553.499158	8000.255846	12.238733	-0.107447	4.817714
553.573891	8000.204190	12.243738	-0.107461	4.817699
553.579031	8000.260161	12.248743	-0.107462	4.817715
553.420854	8000.270499	12.253747	-0.107432	4.817719
553.390269	8000.234181	12.258752	-0.107427	4.817708
553.576085	8000.346586	12.263757	-0.107461	4.817741
553.188440	8000.318762	12.268762	-0.107389	4.817734
553.233154	8000.325736	12.273767	-0.107397	4.817736
553.235769	8000.309944	12.278771	-0.107397	4.817731
553.310754	8000.216101	12.283776	-0.107411	4.817703
553.378611	8000.272988	12.288781	-0.107424	4.817720
553.295576	8000.251725	12.293786	-0.107408	4.817714
553.440412	8000.275984	12.298791	-0.107435	4.817720
553.155736	8000.335103	12.303795	-0.107382	4.817739
553.133620	8000.304183	12.308800	-0.107378	4.817730
553.165961	8000.358441	12.313805	-0.107384	4.817746
553.576534	8000.208323	12.318810	-0.107460	4.817700
553.466372	8000.287924	12.323815	-0.107439	4.817724
553.468340	8000.292164	12.328819	-0.107440	4.817725
553.540748	8000.291104	12.333824	-0.107453	4.817724
553.365866	8000.328622	12.338829	-0.107420	4.817736
553.357204	8000.286296	12.343834	-0.107419	4.817724
553.452093	8000.299277	12.348839	-0.107436	4.817727
553.400714	8000.320668	12.353843	-0.107427	4.817734
553.280784	8000.241908	12.358848	-0.107404	4.817711
553.606752	8000.222402	12.363853	-0.107465	4.817704
553.509132	8000.191434	12.368858	-0.107446	4.817695
553.488890	8000.209061	12.373863	-0.107442	4.817700
553.654999	8000.248398	12.378867	-0.107473	4.817711
553.653185	8000.210390	12.383872	-0.107473	4.817700
553.782396	8000.282942	12.388877	-0.107497	4.817721
553.585039	8000.289542	12.393882	-0.107460	4.817724
553.860076	8000.270348	12.398887	-0.107511	4.817717
553.711571	8000.316690	12.403891	-0.107483	4.817731
553.550391	8000.301668	12.408896	-0.107453	4.817728
553.644901	8000.363165	12.413901	-0.107471	4.817745
553.824400	8000.319369	12.418906	-0.107504	4.817732
553.783450	8000.235433	12.423911	-0.107496	4.817707
553.646232	8000.290378	12.428915	-0.107471	4.817724
553.866376	8000.220806	12.433920	-0.107512	4.817702
553.781370	8000.283898	12.438925	-0.107496	4.817721
553.646489	8000.210193	12.443930	-0.107470	4.817700
553.771962	8000.242607	12.448935	-0.107494	4.817709
553.806406	8000.294787	12.453939	-0.107500	4.817724
553.563113	8000.192073	12.458944	-0.107454	4.817695
553.765424	8000.262528	12.463949	-0.107492	4.817715
553.899268	8000.268695	12.468954	-0.107517	4.817716
553.771005	8000.220401	12.473959	-0.107493	4.817703
553.593970	8000.244175	12.478963	-0.107460	4.817710
553.360588	8000.229154	12.483968	-0.107416	4.817707
553.498478	8000.246982	12.488973	-0.107442	4.817712
553.356455	8000.222748	12.493978	-0.107415	4.817705
553.526857	8000.203079	12.498983	-0.107447	4.817699
553.704929	8000.282673	12.503987	-0.107480	4.817721
553.447649	8000.224056	12.508992	-0.107432	4.817705
553.586550	8000.252447	12.513997	-0.107458	4.817713
553.459866	8000.276957	12.519002	-0.107434	4.817721
553.766930	8000.239244	12.524007	-0.107491	4.817708
553.494372	8000.309089	12.529011	-0.107440	4.817730
553.514512	8000.271402	12.534016	-0.107444	4.817719
553.575295	8000.342954	12.539021	-0.107455	4.817740
553.318482	8000.330754	12.544026	-0.107407	4.817737
553.518946	8000.299922	12.549031	-0.107444	4.817727
553.752467	8000.315984	12.554035	-0.107488	4.817731
553.546500	8000.207486	12.559040	-0.107449	4.817700
553.476577	8000.287675	12.564045	-0.107436	4.817724
553.621619	8000.312992	12.569050	-0.107463	4.817731
553.550765	8000.284523	12.574055	-0.107450	4.817723
553.304180	8000.284076	12.579059	-0.107404	4.817724
553.441116	8000.290288	12.584064	-0.107429	4.817725
553.553437	8000.367866	12.589069	-0.107450	4.817747
553.579214	8000.291234	12.594074	-0.107455	4.817724
553.461142	8000.325364	12.599079	-0.107433	4.817735
553.632880	8000.298331	12.604083	-0.107464	4.817726
553.591830	8000.242873	12.609088	-0.107457	4.817710
553.763059	8000.286504	12.614093	-0.107489	4.817722
553.400813	8000.262216	12.619098	-0.107421	4.817717
553.635676	8000.268804	12.624103	-0.107465	4.817718
553.751390	8000.305295	12.629107	-0.107486	4.817728
553.733855	8000.207989	12.634112	-0.107483	4.817699
553.723063	8000.324906	12.639117	-0.107481	4.817734
553.649091	8000.274241	12.644122	-0.107467	4.817719
553.732577	8000.267014	12.649127	-0.107482	4.817717
553.796496	8000.325954	12.654131	-0.107494	4.817734
553.518803	8000.306065	12.659136	-0.107442	4.817729
553.516484	8000.337667	12.664141	-0.107442	4.817739
553.531856	8000.314678	12.669146	-0.107444	4.817732
553.665981	8000.315575	12.674151	-0.107469	4.817731
553.588543	8000.341860	12.679155	-0.107455	4.817739
553.320492	8000.351646	12.684160	-0.107405	4.817743
553.524777	8000.382048	12.689165	-0.107443	4.817752
553.351099	8000.315159	12.694170	-0.107410	4.817733
553.310598	8000.327217	12.699175	-0.107402	4.817736
553.619018	8000.321168	12.704179	-0.107460	4.817733
553.569183	8000.305664	12.709184	-0.107450	4.817729
553.276360	8000.372047	12.714189	-0.107396	4.817750
553.265429	8000.319140	12.719194	-0.107394	4.817734
553.409772	8000.349720	12.724199	-0.107420	4.817743
553.637616	8000.310850	12.729203	-0.107463	4.817730
553.372433	8000.279542	12.734208	-0.107413	4.817722
553.505821	8000.296250	12.739213	-0.107438	4.817726
553.422211	8000.289746	12.744218	-0.107422	4.817725
553.286131	8000.348927	12.749223	-0.107397	4.817743
553.334448	8000.329583	12.754227	-0.107406	4.817737
553.366984	8000.327941	12.759232	-0.107412	4.817736
553.643330	8000.293998	12.764237	-0.107463	4.817725
553.599327	8000.229005	12.769242	-0.107455	4.817706
553.768623	8000.226196	12.774247	-0.107486	4.817704
553.651147	8000.224471	12.779251	-0.107464	4.817704
553.742407	8000.166728	12.784256	-0.107481	4.817687
553.928159	8000.267530	12.789261	-0.107516	4.817716
553.583056	8000.285684	12.794266	-0.107451	4.817723
553.465460	8000.258642	12.799271	-0.107429	4.817715
553.594915	8000.291115	12.804275	-0.107453	4.817724
553.760511	8000.252390	12.809280	-0.107484	4.817712
553.847311	8000.301116	12.814285	-0.107500	4.817726
553.953248	8000.226710	12.819290	-0.107520	4.817704
553.970137	8000.234332	12.824295	-0.107523	4.817706
553.911162	8000.285147	12.829299	-0.107512	4.817721
553.980184	8000.143750	12.834304	-0.107524	4.817679
554.050429	8000.221768	12.839309	-0.107537	4.817702
553.919236	8000.262035	12.844314	-0.107513	4.817714
553.954430	8000.264650	12.849319	-0.107519	4.817715
554.095694	8000.321557	12.854323	-0.107545	4.817731
553.900462	8000.244859	12.859328	-0.107509	4.817709
553.793874	8000.336115	12.864333	-0.107489	4.817737
553.612646	8000.315526	12.869338	-0.107455	4.817732
553.581991	8000.299248	12.874343	-0.107449	4.817727
553.666015	8000.287810	12.879347	-0.107465	4.817723
553.669691	8000.238280	12.884352	-0.107465	4.817709
553.773897	8000.298863	12.889357	-0.107485	4.817726
553.620012	8000.295551	12.894362	-0.107456	4.817726
553.720378	8000.270640	12.899367	-0.107475	4.817718
553.751678	8000.308007	12.904371	-0.107480	4.817729
553.407083	8000.330387	12.909376	-0.107416	4.817737
553.366818	8000.409955	12.914381	-0.107408	4.817761
552.863247	8000.388876	12.919386	-0.107315	4.817757
552.898989	8000.429472	12.924391	-0.107321	4.817768
553.437416	8000.367715	12.929395	-0.107421	4.817748
553.245622	8000.341699	12.934400	-0.107385	4.817741
553.515588	8000.319266	12.939405	-0.107436	4.817733
553.703405	8000.249221	12.944410	-0.107470	4.817712
553.529421	8000.344766	12.949415	-0.107438	4.817741
553.299875	8000.356171	12.954419	-0.107395	4.817745
553.772297	8000.305052	12.959424	-0.107483	4.817728
553.806197	8000.332964	12.964429	-0.107489	4.817736
553.647435	8000.315869	12.969434	-0.107459	4.817732
553.755225	8000.340641	12.974439	-0.107479	4.817739
553.443299	8000.370882	12.979443	-0.107421	4.817749
553.497488	8000.290447	12.984448	-0.107431	4.817725
553.616741	8000.378675	12.989453	-0.107453	4.817750
553.803234	8000.312830	12.994458	-0.107488	4.817730
553.540893	8000.233043	12.999463	-0.107439	4.817708
553.513047	8000.342326	13.004467	-0.107434	4.817740
553.821088	8000.324669	13.009472	-0.107491	4.817734
554.099477	8000.275989	13.014477	-0.107543	4.817718
553.920857	8000.258603	13.019482	-0.107509	4.817714
554.180509	8000.248677	13.024487	-0.107558	4.817709
554.162525	8000.219927	13.029491	-0.107554	4.817701
553.948154	8000.207292	13.034496	-0.107514	4.817698
553.938654	8000.254611	13.039501	-0.107512	4.817712
553.713652	8000.270301	13.044506	-0.107470	4.817718
553.939267	8000.254603	13.049511	-0.107512	4.817712
553.975282	8000.292039	13.054515	-0.107519	4.817723
553.893967	8000.228609	13.059520	-0.107503	4.817705
554.063973	8000.307032	13.064525	-0.107535	4.817727
553.519642	8000.329657	13.069530	-0.107434	4.817736
553.666020	8000.257952	13.074535	-0.107461	4.817714
553.988967	8000.322787	13.079539	-0.107521	4.817732
553.752290	8000.276073	13.084544	-0.107477	4.817719
553.884167	8000.320184	13.089549	-0.107501	4.817732
554.009515	8000.298802	13.094554	-0.107524	4.817725
553.659702	8000.285243	13.099559	-0.107459	4.817723
553.902088	8000.313037	13.104563	-0.107504	4.817730
554.025478	8000.207243	13.109568	-0.107527	4.817698
553.909579	8000.294144	13.114573	-0.107505	4.817724
553.709628	8000.293323	13.119578	-0.107468	4.817725
553.949752	8000.278892	13.124583	-0.107512	4.817719
554.058146	8000.325825	13.129587	-0.107533	4.817733
553.919008	8000.300577	13.134592	-0.107507	4.817726
553.716245	8000.339797	13.139597	-0.107469	4.817739
553.728351	8000.247144	13.144602	-0.107471	4.817711
554.079189	8000.187920	13.149607	-0.107536	4.817692
554.079266	8000.328202	13.154611	-0.107536	4.817734
553.834865	8000.287703	13.159616	-0.107490	4.817723
553.973468	8000.341406	13.164621	-0.107516	4.817738
553.827309	8000.241165	13.169626	-0.107489	4.817709
553.816506	8000.181930	13.174631	-0.107487	4.817691
554.155717	8000.225907	13.179635	-0.107550	4.817703
554.242657	8000.234553	13.184640	-0.107566	4.817705
554.016058	8000.257602	13.189645	-0.107523	4.817713
554.327071	8000.244208	13.194650	-0.107581	4.817708
554.303785	8000.248079	13.199655	-0.107577	4.817709
554.039013	8000.264242	13.204659	-0.107527	4.817715
553.902602	8000.208445	13.209664	-0.107502	4.817699
554.070488	8000.308987	13.214669	-0.107533	4.817728
554.052190	8000.220108	13.219674	-0.107529	4.817702
554.034570	8000.282075	13.224679	-0.107526	4.817720
554.171868	8000.289348	13.229683	-0.107552	4.817722
554.118284	8000.222104	13.234688	-0.107541	4.817702
554.050119	8000.293881	13.239693	-0.107529	4.817724
554.137627	8000.275110	13.244698	-0.107545	4.817718
554.221302	8000.258393	13.249703	-0.107560	4.817712
553.977151	8000.281186	13.254707	-0.107515	4.817720
554.105082	8000.285157	13.259712	-0.107539	4.817721
554.351976	8000.342554	13.264717	-0.107584	4.817737
554.249540	8000.310458	13.269722	-0.107565	4.817728
554.201153	8000.300249	13.274727	-0.107556	4.817725
554.220992	8000.318463	13.279731	-0.107560	4.817730
554.177472	8000.250311	13.284736	-0.107551	4.817710
554.404848	8000.285270	13.289741	-0.107594	4.817719
554.051407	8000.245287	13.294746	-0.107528	4.817709
554.165477	8000.272261	13.299751	-0.107549	4.817717
554.212408	8000.304583	13.304755	-0.107558	4.817726
554.079477	8000.242508	13.309760	-0.107533	4.817708
554.243643	8000.328229	13.314765	-0.107563	4.817733
554.097808	8000.270184	13.319770	-0.107536	4.817716
553.587566	8000.343938	13.324775	-0.107441	4.817740
553.878881	8000.374558	13.329779	-0.107495	4.817748
553.521482	8000.372490	13.334784	-0.107428	4.817749
553.805324	8000.397726	13.339789	-0.107481	4.817755
553.917620	8000.347674	13.344794	-0.107502	4.817740
553.942749	8000.321663	13.349799	-0.107506	4.817732
554.162850	8000.294282	13.354803	-0.107547	4.817723
553.889419	8000.254414	13.359808	-0.107496	4.817713
554.045655	8000.299936	13.364813	-0.107525	4.817725
553.896384	8000.280870	13.369818	-0.107497	4.817720
554.037800	8000.234407	13.374823	-0.107524	4.817706
553.939409	8000.274098	13.379827	-0.107505	4.817718
553.853746	8000.300263	13.384832	-0.107489	4.817726
553.769778	8000.335945	13.389837	-0.107473	4.817737
554.048973	8000.311538	13.394842	-0.107525	4.817729
553.707800	8000.344516	13.399847	-0.107462	4.817740
553.763836	8000.380135	13.404851	-0.107472	4.817750
553.973999	8000.303034	13.409856	-0.107511	4.817727
554.123904	8000.346354	13.414861	-0.107539	4.817739
553.908581	8000.306280	13.419866	-0.107499	4.817728
553.699988	8000.289511	13.424871	-0.107460	4.817724
554.100491	8000.367083	13.429875	-0.107534	4.817745
553.935141	8000.330904	13.434880	-0.107503	4.817735
554.134428	8000.322206	13.439885	-0.107540	4.817732
553.798819	8000.337333	13.444890	-0.107478	4.817738
553.752024	8000.351408	13.449895	-0.107469	4.817742
553.727711	8000.394291	13.454899	-0.107464	4.817755
553.644383	8000.337161	13.459904	-0.107449	4.817738
553.840086	8000.349506	13.464909	-0.107485	4.817741
553.893272	8000.331288	13.469914	-0.107495	4.817735
553.847435	8000.281035	13.474919	-0.107486	4.817721
553.839548	8000.331541	13.479923	-0.107484	4.817736
554.007583	8000.329770	13.484928	-0.107516	4.817734
554.032192	8000.392355	13.489933	-0.107520	4.817753
553.933178	8000.385625	13.494938	-0.107502	4.817751
553.919602	8000.354829	13.499943	-0.107499	4.817742
553.708515	8000.377051	13.504947	-0.107460	4.817750
553.734270	8000.306747	13.509952	-0.107464	4.817729
553.773870	8000.337907	13.514957	-0.107471	4.817738
554.071963	8000.288461	13.519962	-0.107527	4.817722
553.930542	8000.331742	13.524967	-0.107500	4.817735
554.086999	8000.374103	13.529971	-0.107530	4.817747
553.933144	8000.302229	13.534976	-0.107501	4.817727
553.988523	8000.346277	13.539981	-0.107511	4.817739
553.868162	8000.345564	13.544986	-0.107488	4.817740
553.741157	8000.312055	13.549991	-0.107465	4.817730
553.959338	8000.354264	13.554995	-0.107505	4.817742
553.780808	8000.326331	13.560000	-0.107472	4.817734
553.773615	8000.343094	13.565005	-0.107470	4.817739
553.856248	8000.279951	13.570010	-0.107486	4.817720
553.943658	8000.244302	13.575015	-0.107502	4.817709
554.092729	8000.316089	13.580019	-0.107529	4.817730
553.897270	8000.334320	13.585024	-0.107493	4.817736
553.935943	8000.315891	13.590029	-0.107500	4.817731
553.909201	8000.349245	13.595034	-0.107495	4.817741
553.620759	8000.391432	13.600039	-0.107441	4.817754
553.434041	8000.382366	13.605043	-0.107406	4.817753
553.596318	8000.348867	13.610048	-0.107436	4.817742
553.898728	8000.353278	13.615053	-0.107493	4.817742
554.166505	8000.327649	13.620058	-0.107542	4.817733
553.860141	8000.310505	13.625063	-0.107485	4.817729
553.658835	8000.382446	13.630067	-0.107448	4.817752
553.867776	8000.325368	13.635072	-0.107486	4.817734
553.803972	8000.363454	13.640077	-0.107474	4.817745
553.804083	8000.329694	13.645082	-0.107474	4.817735
553.797561	8000.364399	13.650087	-0.107473	4.817746
554.103150	8000.403666	13.655091	-0.107530	4.817756
553.809573	8000.356119	13.660096	-0.107475	4.817743
553.863731	8000.389602	13.665101	-0.107485	4.817753
553.598613	8000.384663	13.670106	-0.107436	4.817753
553.666995	8000.336079	13.675111	-0.107448	4.817738
553.801580	8000.325380	13.680115	-0.107473	4.817734
553.559081	8000.310225	13.685120	-0.107428	4.817731
553.653294	8000.351676	13.690125	-0.107445	4.817743
553.946360	8000.301101	13.695130	-0.107500	4.817726
554.050528	8000.327931	13.700135	-0.107519	4.817734
554.269872	8000.337458	13.705139	-0.107560	4.817736
554.091843	8000.315860	13.710144	-0.107527	4.817730
553.927648	8000.324000	13.715149	-0.107496	4.817733
554.273090	8000.279465	13.720154	-0.107560	4.817719
554.143490	8000.298659	13.725159	-0.107536	4.817725
554.093302	8000.339054	13.730163	-0.107526	4.817737
553.938502	8000.297755	13.735168	-0.107497	4.817725
554.109767	8000.330840	13.740173	-0.107529	4.817734
554.022001	8000.284192	13.745178	-0.107513	4.817721
554.082259	8000.311435	13.750183	-0.107524	4.817729
554.157548	8000.370541	13.755187	-0.107538	4.817746
553.943561	8000.323103	13.760192	-0.107498	4.817733
554.158757	8000.319911	13.765197	-0.107538	4.817731
554.322883	8000.296987	13.770202	-0.107568	4.817724
554.379203	8000.221856	13.775207	-0.107579	4.817701
554.320128	8000.301149	13.780211	-0.107568	4.817725
554.324969	8000.278006	13.785216	-0.107568	4.817718
554.034386	8000.303285	13.790221	-0.107514	4.817727
553.974155	8000.308725	13.795226	-0.107503	4.817729
554.230503	8000.314573	13.800231	-0.107550	4.817729
554.331873	8000.287567	13.805235	-0.107569	4.817721
554.162156	8000.256598	13.810240	-0.107537	4.817712
554.219699	8000.251102	13.815245	-0.107548	4.817710
554.491338	8000.319408	13.820250	-0.107599	4.817729
554.426356	8000.275202	13.825255	-0.107586	4.817717
554.420950	8000.335239	13.830259	-0.107585	4.817734
554.370879	8000.312348	13.835264	-0.107576	4.817728
554.527108	8000.285089	13.840269	-0.107605	4.817719
554.424021	8000.319437	13.845274	-0.107586	4.817730
554.351608	8000.317315	13.850279	-0.107572	4.817729
554.480137	8000.314967	13.855283	-0.107596	4.817728
554.344800	8000.251801	13.860288	-0.107570	4.817710
554.271633	8000.345656	13.865293	-0.107557	4.817738
554.196260	8000.350875	13.870298	-0.107543	4.817740
554.193532	8000.289648	13.875303	-0.107542	4.817722
554.431424	8000.314213	13.880307	-0.107586	4.817728
554.237473	8000.320863	13.885312	-0.107550	4.817731
554.464182	8000.276702	13.890317	-0.107592	4.817717
554.599166	8000.241748	13.895322	-0.107617	4.817706
554.187020	8000.327484	13.900327	-0.107540	4.817733
554.310239	8000.330332	13.905331	-0.107563	4.817734
554.444282	8000.339667	13.910336	-0.107588	4.817736
554.422997	8000.325635	13.915341	-0.107584	4.817732
554.460728	8000.321959	13.920346	-0.107591	4.817730
554.469558	8000.296764	13.925351	-0.107592	4.817723
554.483835	8000.377130	13.930355	-0.107595	4.817747
554.349876	8000.324532	13.935360	-0.107570	4.817732
554.413513	8000.344441	13.940365	-0.107582	4.817737
554.367740	8000.291023	13.945370	-0.107573	4.817722
554.436512	8000.325774	13.950375	-0.107586	4.817732
554.462164	8000.359895	13.955379	-0.107590	4.817742
554.395242	8000.286126	13.960384	-0.107578	4.817720
554.543274	8000.310433	13.965389	-0.107605	4.817727
554.477549	8000.313683	13.970394	-0.107593	4.817728
554.629132	8000.311671	13.975399	-0.107621	4.817727
554.521214	8000.363881	13.980403	-0.107601	4.817743
554.071815	8000.344645	13.985408	-0.107517	4.817739
554.213653	8000.357258	13.990413	-0.107543	4.817742
554.295065	8000.283549	13.995418	-0.107558	4.817720
554.430283	8000.226448	14.000423	-0.107583	4.817702
554.325819	8000.354654	14.005427	-0.107564	4.817741
554.297834	8000.294112	14.010432	-0.107559	4.817723
554.145107	8000.334064	14.015437	-0.107530	4.817735
554.324691	8000.340900	14.020442	-0.107563	4.817737
554.377202	8000.380688	14.025447	-0.107573	4.817748
554.402080	8000.351508	14.030451	-0.107578	4.817739
554.298702	8000.259275	14.035456	-0.107558	4.817713
554.375813	8000.306805	14.040461	-0.107572	4.817726
554.176711	8000.362956	14.045466	-0.107535	4.817744
554.088948	8000.315253	14.050471	-0.107519	4.817730
554.351131	8000.315913	14.055475	-0.107568	4.817729
554.043944	8000.294537	14.060480	-0.107510	4.817724
554.037845	8000.328194	14.065485	-0.107509	4.817734
553.872140	8000.378504	14.070490	-0.107478	4.817750
554.238716	8000.343771	14.075495	-0.107546	4.817738
554.072609	8000.374034	14.080499	-0.107515	4.817748
554.151672	8000.238056	14.085504	-0.107530	4.817707
554.299174	8000.354123	14.090509	-0.107557	4.817741
554.213412	8000.363409	14.095514	-0.107541	4.817744
554.100823	8000.328001	14.100519	-0.107520	4.817734
553.930529	8000.371915	14.105523	-0.107488	4.817748
554.048804	8000.365197	14.110528	-0.107510	4.817745
554.215889	8000.380289	14.115533	-0.107541	4.817749
553.915765	8000.376948	14.120538	-0.107485	4.817749
553.708263	8000.407661	14.125543	-0.107446	4.817759
554.037233	8000.413516	14.130547	-0.107508	4.817759
554.224780	8000.316042	14.135552	-0.107542	4.817730
554.279313	8000.376956	14.140557	-0.107552	4.817748
554.231044	8000.393119	14.145562	-0.107543	4.817753
554.309831	8000.351015	14.150567	-0.107558	4.817740
554.286359	8000.378089	14.155571	-0.107553	4.817748
554.145240	8000.320112	14.160576	-0.107527	4.817731
554.162253	8000.322462	14.165581	-0.107530	4.817732
554.412754	8000.292362	14.170586	-0.107577	4.817722
554.440101	8000.246342	14.175591	-0.107582	4.817708
554.435063	8000.306384	14.180595	-0.107581	4.817726
554.092601	8000.318247	14.185600	-0.107517	4.817731
554.452115	8000.280246	14.190605	-0.107583	4.817718
554.480079	8000.297524	14.195610	-0.107589	4.817723
554.464342	8000.240326	14.200615	-0.107585	4.817706
554.051664	8000.373520	14.205619	-0.107509	4.817748
554.095689	8000.382593	14.210624	-0.107517	4.817750
554.450432	8000.360346	14.215629	-0.107583	4.817742
554.113841	8000.341705	14.220634	-0.107520	4.817738
554.515871	8000.267408	14.225639	-0.107595	4.817714
554.689353	8000.325841	14.230643	-0.107627	4.817731
554.528607	8000.306605	14.235648	-0.107597	4.817726
554.544789	8000.306833	14.240653	-0.107600	4.817726
554.542387	8000.317338	14.245658	-0.107599	4.817729
554.118998	8000.306922	14.250663	-0.107520	4.817728
554.418517	8000.343991	14.255667	-0.107576	4.817737
554.406340	8000.302667	14.260672	-0.107573	4.817725
554.403699	8000.321606	14.265677	-0.107573	4.817731
554.469019	8000.339430	14.270682	-0.107585	4.817736
554.309164	8000.320208	14.275687	-0.107555	4.817731
554.727287	8000.348464	14.280691	-0.107633	4.817737
554.506884	8000.262957	14.285696	-0.107592	4.817713
554.450336	8000.264232	14.290701	-0.107581	4.817714
554.332975	8000.304700	14.295706	-0.107559	4.817726
554.572566	8000.262838	14.300711	-0.107604	4.817713
554.424006	8000.339769	14.305715	-0.107576	4.817736
554.336165	8000.299448	14.310720	-0.107559	4.817724
554.506895	8000.320922	14.315725	-0.107591	4.817730
554.697163	8000.314202	14.320730	-0.107626	4.817727
554.331306	8000.288804	14.325735	-0.107558	4.817721
554.259725	8000.378463	14.330739	-0.107545	4.817748
554.494799	8000.339699	14.335744	-0.107588	4.817736
554.608907	8000.296002	14.340749	-0.107609	4.817722
554.646691	8000.321861	14.345754	-0.107616	4.817730
554.566708	8000.252121	14.350759	-0.107601	4.817709
554.499520	8000.329186	14.355763	-0.107589	4.817733
554.627413	7999.385958	14.360768	-0.107612	4.817453

554.663645	7996.127601	14.365773	-0.107616	4.816488
554.523118	7990.660776	14.370778	-0.107587	4.814870
554.278579	7984.027804	14.375783	-0.107537	4.812906
554.415252	7976.758363	14.380787	-0.107557	4.810751
554.490445	7969.090170	14.385792	-0.107566	4.808478
554.482931	7961.339219	14.390797	-0.107560	4.806179
554.501146	7953.423001	14.395802	-0.107558	4.803829
554.511674	7945.547348	14.400807	-0.107554	4.801491
554.433497	7937.566150	14.405811	-0.107535	4.799120
554.364890	7929.575405	14.410816	-0.107516	4.796746
554.494884	7921.534492	14.415821	-0.107535	4.794354
554.287676	7913.591952	14.420826	-0.107491	4.791992
554.488907	7905.512688	14.425831	-0.107524	4.789587
554.579060	7897.552408	14.430835	-0.107535	4.787216
554.154204	7889.457905	14.435840	-0.107451	4.784806
554.246903	7881.548585	14.440845	-0.107463	4.782448
554.250284	7873.484081	14.445850	-0.107458	4.780043
554.299577	7865.491109	14.450855	-0.107462	4.777657
554.216951	7857.523649	14.455859	-0.107441	4.775279
554.098832	7849.516965	14.460864	-0.107414	4.772888
554.159677	7841.531942	14.465869	-0.107420	4.770501
554.105561	7833.502708	14.470874	-0.107404	4.768101
554.014846	7825.451083	14.475879	-0.107382	4.765693
554.324008	7817.493158	14.480883	-0.107434	4.763310
554.248644	7809.546730	14.485888	-0.107415	4.760931
554.093731	7801.498310	14.490893	-0.107381	4.758520
554.238030	7793.562079	14.495898	-0.107402	4.756140
554.024169	7785.424497	14.500903	-0.107357	4.753701
553.785585	7777.554133	14.505907	-0.107308	4.751340
553.707306	7769.407468	14.510912	-0.107288	4.748894
553.829586	7761.504774	14.515917	-0.107305	4.746520
553.938224	7753.412692	14.520922	-0.107320	4.744088
553.675554	7745.462777	14.525927	-0.107266	4.741699
553.823435	7737.461220	14.530931	-0.107288	4.739291
553.811878	7729.488324	14.535936	-0.107280	4.736892
553.220565	7721.451704	14.540941	-0.107165	4.734473
553.647662	7713.466589	14.545946	-0.107239	4.732066
553.658709	7705.382874	14.550951	-0.107236	4.729630
553.741624	7697.469439	14.555955	-0.107246	4.727243
553.488006	7689.343478	14.560960	-0.107193	4.724791
553.633696	7681.503729	14.565965	-0.107215	4.722424
553.675110	7673.516299	14.570970	-0.107218	4.720012
553.635556	7665.443598	14.575975	-0.107205	4.717572
553.937984	7657.448477	14.580979	-0.107256	4.715154
553.788415	7649.475226	14.585984	-0.107223	4.712742
553.723701	7641.449908	14.590989	-0.107206	4.710314
553.710529	7633.444518	14.595994	-0.107198	4.707889
553.660827	7625.396707	14.600999	-0.107183	4.705451
553.795437	7617.459097	14.606003	-0.107203	4.703045
553.431668	7609.471495	14.611008	-0.107130	4.700622
553.370327	7601.455711	14.616013	-0.107113	4.698190
553.430103	7593.446740	14.621018	-0.107119	4.695758
553.147858	7585.415689	14.626023	-0.107061	4.693319
553.771117	7577.433951	14.631027	-0.107172	4.690892
553.571918	7569.448584	14.636032	-0.107129	4.688464
553.518136	7561.458784	14.641037	-0.107114	4.686034
553.418630	7553.418643	14.646042	-0.107090	4.683586
553.406977	7545.502969	14.651047	-0.107083	4.681176
553.527299	7537.441263	14.656051	-0.107100	4.678719
553.293184	7529.506496	14.661056	-0.107051	4.676300
553.256129	7521.423043	14.666061	-0.107039	4.673834
553.335440	7513.371817	14.671066	-0.107048	4.671377
553.454085	7505.324908	14.676071	-0.107065	4.668919
553.268727	7497.412228	14.681075	-0.107025	4.666502
553.376755	7489.374706	14.686080	-0.107040	4.664045
553.254359	7481.467463	14.691085	-0.107012	4.661627
553.080712	7473.412308	14.696090	-0.106974	4.659162
552.894767	7465.427736	14.701095	-0.106934	4.656717
553.230730	7457.402338	14.706099	-0.106991	4.654259
553.070561	7449.448671	14.711104	-0.106956	4.651821
553.083154	7441.372199	14.716109	-0.106953	4.649345
553.128212	7433.436377	14.721114	-0.106956	4.646910
552.930366	7425.348982	14.726119	-0.106914	4.644427
552.992633	7417.481554	14.731123	-0.106920	4.642011
552.873716	7409.388616	14.736128	-0.106893	4.639524
553.032576	7401.423939	14.741133	-0.106917	4.637075
552.980029	7393.410682	14.746138	-0.106902	4.634610
553.000932	7385.430089	14.751143	-0.106901	4.632153
553.154859	7377.392853	14.756147	-0.106924	4.629678
553.084014	7369.397499	14.761152	-0.106906	4.627215
552.998210	7361.364944	14.766157	-0.106884	4.624738
553.041539	7353.399330	14.771162	-0.106887	4.622281
552.822467	7345.358383	14.776167	-0.106841	4.619799
552.924268	7337.408306	14.781171	-0.106854	4.617345
552.585207	7329.382341	14.786176	-0.106786	4.614865
552.876106	7321.387929	14.791181	-0.106835	4.612394
552.960220	7313.356747	14.796186	-0.106845	4.609910
552.891059	7305.359465	14.801191	-0.106827	4.607435
552.773838	7297.365623	14.806195	-0.106800	4.604960
552.641069	7289.368115	14.811200	-0.106770	4.602482
552.588769	7281.373739	14.816205	-0.106755	4.600004
552.684096	7273.402375	14.821210	-0.106767	4.597532
552.584806	7265.345367	14.826215	-0.106743	4.595032
552.753652	7257.342142	14.831219	-0.106769	4.592548
552.770640	7249.282447	14.836224	-0.106767	4.590044
552.739779	7241.330770	14.841229	-0.106756	4.587573
552.462824	7233.315128	14.846234	-0.106699	4.585080
552.416148	7225.300989	14.851239	-0.106685	4.582586
552.506852	7217.377864	14.856243	-0.106697	4.580120
552.351942	7209.328834	14.861248	-0.106663	4.577613
552.274068	7201.320972	14.866253	-0.106643	4.575117
552.493754	7193.328051	14.871258	-0.106679	4.572625
552.408364	7185.296967	14.876263	-0.106657	4.570119
552.279321	7177.327556	14.881267	-0.106628	4.567631
552.226676	7169.312157	14.886272	-0.106613	4.565128
552.292508	7161.354435	14.891277	-0.106620	4.562641
552.237457	7153.322894	14.896282	-0.106604	4.560130
552.095574	7145.309310	14.901287	-0.106572	4.557623
552.173823	7137.321740	14.906291	-0.106582	4.555122
552.061158	7129.313868	14.911296	-0.106555	4.552614
552.121222	7121.282409	14.916301	-0.106561	4.550098
552.106465	7113.340510	14.921306	-0.106553	4.547608
551.979154	7105.265483	14.926311	-0.106524	4.545074
552.118723	7097.303441	14.931315	-0.106545	4.542575
552.027619	7089.258020	14.936320	-0.106523	4.540048
552.180722	7081.321524	14.941325	-0.106546	4.537555
551.969315	7073.261175	14.946330	-0.106501	4.535020
552.024561	7065.258831	14.951335	-0.106506	4.532503
552.325799	7057.274750	14.956339	-0.106557	4.529990
552.142990	7049.262417	14.961344	-0.106517	4.527467
552.094375	7041.263375	14.966349	-0.106503	4.524946
552.053843	7033.320224	14.971354	-0.106490	4.522441
552.013221	7025.252877	14.976359	-0.106477	4.519896
552.069004	7017.321711	14.981363	-0.106482	4.517393
551.743961	7009.258187	14.986368	-0.106417	4.514846
551.768247	7001.283892	14.991373	-0.106416	4.512326
551.576121	6993.268793	14.996378	-0.106375	4.509791
551.584518	6985.223717	15.001383	-0.106371	4.507246
551.750258	6977.194402	15.006387	-0.106396	4.504705
551.734191	6969.222698	15.011392	-0.106388	4.502180
551.568056	6961.206841	15.016397	-0.106352	4.499640
551.699026	6953.246518	15.021402	-0.106371	4.497116
551.478413	6945.226601	15.026407	-0.106325	4.494571
551.656095	6937.213749	15.031411	-0.106352	4.492028
551.740875	6929.186776	15.036416	-0.106363	4.489479
551.675494	6921.202414	15.041421	-0.106345	4.486941
551.568559	6913.174014	15.046426	-0.106320	4.484388
551.415624	6905.219458	15.051431	-0.106286	4.481857
551.607689	6897.183892	15.056435	-0.106317	4.479300
551.674796	6889.206326	15.061440	-0.106324	4.476759
551.485888	6881.169887	15.066445	-0.106283	4.474197
551.530022	6873.243811	15.071450	-0.106286	4.471670
551.570642	6865.168669	15.076455	-0.106288	4.469094
551.540530	6857.212515	15.081459	-0.106278	4.466553
551.323183	6849.157873	15.086464	-0.106232	4.463980
551.362123	6841.233410	15.091469	-0.106234	4.461447
551.325451	6833.190527	15.096474	-0.106222	4.458875
551.120431	6825.191715	15.101479	-0.106178	4.456315
551.182123	6817.219175	15.106483	-0.106184	4.453762
550.781187	6809.221753	15.111488	-0.106104	4.451199
551.199395	6801.126682	15.116493	-0.106177	4.448606
551.028163	6793.189827	15.121498	-0.106140	4.446059
551.074150	6785.138625	15.126503	-0.106143	4.443476
551.076647	6777.222031	15.131507	-0.106138	4.440934
550.795424	6769.168588	15.136512	-0.106080	4.438345
551.062905	6761.158084	15.141517	-0.106125	4.435771
551.137505	6753.150299	15.146522	-0.106133	4.433196
550.837399	6745.132719	15.151527	-0.106072	4.430614
551.149755	6737.130468	15.156531	-0.106125	4.428039
551.102248	6729.084356	15.161536	-0.106111	4.425446
550.798606	6721.118834	15.166541	-0.106049	4.422876
550.846199	6713.147392	15.171546	-0.106052	4.420305
550.683486	6705.157041	15.176551	-0.106017	4.417725
550.786759	6697.145645	15.181555	-0.106031	4.415138
550.750055	6689.126833	15.186560	-0.106019	4.412547
550.942348	6681.101049	15.191565	-0.106049	4.409952
551.056332	6673.128565	15.196570	-0.106065	4.407374
550.829312	6665.112788	15.201575	-0.106017	4.404777
550.971678	6657.175165	15.206579	-0.106039	4.402207
550.812310	6649.127244	15.211584	-0.106004	4.399598
550.790584	6641.170180	15.216589	-0.105994	4.397017
550.790615	6633.075051	15.221594	-0.105989	4.394390
550.703121	6625.120988	15.226599	-0.105967	4.391807
550.897120	6617.101946	15.231603	-0.105998	4.389203
550.685151	6609.142413	15.236608	-0.105953	4.386614
550.971345	6601.084961	15.241613	-0.106001	4.383995
550.779731	6593.193069	15.246618	-0.105960	4.381425
550.526855	6585.109670	15.251623	-0.105908	4.378791
550.209763	6577.244202	15.256627	-0.105844	4.376226
550.304481	6569.147369	15.261632	-0.105856	4.373587
550.288387	6561.153312	15.266637	-0.105848	4.370979
550.484074	6553.131015	15.271642	-0.105879	4.368361
550.348452	6545.125093	15.276647	-0.105848	4.365746
550.461847	6537.156071	15.281651	-0.105864	4.363142
550.302067	6529.210891	15.286656	-0.105829	4.360542
550.475751	6521.202380	15.291661	-0.105856	4.357923
550.638265	6513.196957	15.296666	-0.105881	4.355303
550.542237	6505.180938	15.301671	-0.105858	4.352676
550.483842	6497.131850	15.306675	-0.105841	4.350037
550.280651	6489.179364	15.311680	-0.105798	4.347427
550.314031	6481.137090	15.316685	-0.105799	4.344788
550.246941	6473.161826	15.321690	-0.105781	4.342168
550.395005	6465.182738	15.326695	-0.105804	4.339547
550.409482	6457.241846	15.331699	-0.105801	4.336936
550.212442	6449.178750	15.336704	-0.105759	4.334282
550.208634	6441.207204	15.341709	-0.105753	4.331658
550.173664	6433.156906	15.346714	-0.105741	4.329005
550.002755	6425.202833	15.351719	-0.105704	4.326382
550.131249	6417.141493	15.356723	-0.105723	4.323725
549.959209	6409.255889	15.361728	-0.105685	4.321121
550.057633	6401.207896	15.366733	-0.105698	4.318464
549.900697	6393.243784	15.371738	-0.105664	4.315831
549.957828	6385.167006	15.376743	-0.105669	4.313161
550.161901	6377.218933	15.381747	-0.105702	4.310534
549.760682	6369.212493	15.386752	-0.105622	4.307880
549.682241	6361.156864	15.391757	-0.105602	4.305211
549.587406	6353.174485	15.396762	-0.105579	4.302564
549.759429	6345.131898	15.401767	-0.105605	4.299898
549.638293	6337.178906	15.406771	-0.105578	4.297258
549.530313	6329.149686	15.411776	-0.105552	4.294591
549.436097	6321.155204	15.416781	-0.105529	4.291934
549.638679	6313.109089	15.421786	-0.105562	4.289261
549.686010	6305.137706	15.426791	-0.105565	4.286609
549.766835	6297.117845	15.431795	-0.105575	4.283940
549.688285	6289.168150	15.436800	-0.105555	4.281291
549.373312	6281.176450	15.441805	-0.105491	4.278625
549.429836	6273.228386	15.446810	-0.105496	4.275975
549.388757	6265.142024	15.451815	-0.105483	4.273276
549.385816	6257.147595	15.456819	-0.105477	4.270606
549.336022	6249.140799	15.461824	-0.105463	4.267930
549.402452	6241.102186	15.466829	-0.105470	4.265243
549.122059	6233.170779	15.471834	-0.105412	4.262587
549.243363	6225.142571	15.476839	-0.105430	4.259900
549.301009	6217.173385	15.481843	-0.105435	4.257231
548.970671	6209.155200	15.486848	-0.105368	4.254540
548.635715	6201.184238	15.491853	-0.105300	4.251864
549.043253	6193.143718	15.496858	-0.105371	4.249169
549.369128	6185.111475	15.501863	-0.105426	4.246475
549.311559	6177.050988	15.506867	-0.105410	4.243765
549.374891	6169.178634	15.511872	-0.105417	4.241119
549.095751	6161.098839	15.516877	-0.105359	4.238397
549.031100	6153.175460	15.521882	-0.105342	4.235729
548.948282	6145.142788	15.526887	-0.105321	4.233022
549.114240	6137.126199	15.531891	-0.105347	4.230321
549.188362	6129.120274	15.536896	-0.105355	4.227621
549.096709	6121.067254	15.541901	-0.105333	4.224902
549.258070	6113.121530	15.546906	-0.105358	4.222220
548.874043	6105.143430	15.551911	-0.105281	4.219519
548.930583	6097.145617	15.556915	-0.105286	4.216815
548.785682	6089.111363	15.561920	-0.105254	4.214095
548.916107	6081.127019	15.566925	-0.105273	4.211392
549.050659	6073.116307	15.571930	-0.105293	4.208679
548.860192	6065.121227	15.576935	-0.105252	4.205966
548.993184	6057.166858	15.581939	-0.105271	4.203269
548.686061	6049.163013	15.586944	-0.105209	4.200548
548.659372	6041.171788	15.591949	-0.105198	4.197833
548.654796	6033.180428	15.596954	-0.105192	4.195116
548.631863	6025.089360	15.601959	-0.105183	4.192363
548.552337	6017.074284	15.606963	-0.105163	4.189634
548.627123	6009.058352	15.611968	-0.105171	4.186904
548.297736	6001.053089	15.616973	-0.105104	4.184172
548.105312	5993.138203	15.621978	-0.105063	4.181470
548.200214	5985.093383	15.626983	-0.105076	4.178726
548.361243	5977.122818	15.631987	-0.105100	4.176006
548.361828	5969.078934	15.636992	-0.105095	4.173257
548.227797	5961.082471	15.641997	-0.105065	4.170520
548.385188	5953.088394	15.647002	-0.105089	4.167787
548.417726	5945.061981	15.652007	-0.105090	4.165039
548.128652	5937.200733	15.657011	-0.105031	4.162342
548.101213	5929.109635	15.662016	-0.105020	4.159567
548.496107	5921.118882	15.667021	-0.105088	4.156830
548.480703	5913.077118	15.672026	-0.105080	4.154069
548.271486	5905.094978	15.677031	-0.105036	4.151325
548.216896	5897.156154	15.682035	-0.105020	4.148595
548.308096	5889.091140	15.687040	-0.105032	4.145821
548.238331	5881.101789	15.692045	-0.105014	4.143070
548.321860	5873.162847	15.697050	-0.105024	4.140337
548.201974	5865.137091	15.702055	-0.104996	4.137569
548.129331	5857.146665	15.707059	-0.104977	4.134812
548.004815	5849.186161	15.712064	-0.104949	4.132062
548.146880	5841.109798	15.717069	-0.104970	4.129275
548.152821	5833.122568	15.722074	-0.104966	4.126514
547.989367	5825.119181	15.727079	-0.104930	4.123744
548.045500	5817.222840	15.732083	-0.104935	4.121012
547.933630	5809.152553	15.737088	-0.104909	4.118216
548.026926	5801.147394	15.742093	-0.104921	4.115443
548.168920	5793.151102	15.747098	-0.104942	4.112672
548.145224	5785.113572	15.752103	-0.104932	4.109882
548.179462	5777.140352	15.757107	-0.104934	4.107114
547.689545	5769.131253	15.762112	-0.104837	4.104324
547.859581	5761.176982	15.767117	-0.104863	4.101560
547.955987	5753.136773	15.772122	-0.104876	4.098764
547.677136	5745.169058	15.777127	-0.104819	4.095986
547.839176	5737.119237	15.782131	-0.104844	4.093183
548.018055	5729.138632	15.787136	-0.104872	4.090403
547.931848	5721.131241	15.792141	-0.104850	4.087608
547.794659	5713.109108	15.797146	-0.104819	4.084805
547.765186	5705.149755	15.802151	-0.104809	4.082024
547.804748	5697.137653	15.807155	-0.104811	4.079223
547.679096	5689.157522	15.812160	-0.104782	4.076429
547.785387	5681.122447	15.817165	-0.104796	4.073617
547.722127	5673.175697	15.822170	-0.104779	4.070832
547.517549	5665.110399	15.827175	-0.104736	4.068001
547.577779	5657.106335	15.832179	-0.104742	4.065194
547.728766	5649.145710	15.837184	-0.104765	4.062401
547.297475	5641.168251	15.842189	-0.104679	4.059592
547.417712	5633.175540	15.847194	-0.104696	4.056784
547.380931	5625.103708	15.852199	-0.104684	4.053944
547.434649	5617.163953	15.857203	-0.104688	4.051149
547.230010	5609.146094	15.862208	-0.104645	4.048321
547.290139	5601.125925	15.867213	-0.104651	4.045495
547.393392	5593.180223	15.872218	-0.104665	4.042693
547.140436	5585.164615	15.877223	-0.104612	4.039859
546.972622	5577.224301	15.882227	-0.104576	4.037051
546.877623	5569.168953	15.887232	-0.104553	4.034202
547.045590	5561.087331	15.892237	-0.104579	4.031345
547.235403	5553.096782	15.897242	-0.104609	4.028519
546.785609	5545.106179	15.902247	-0.104520	4.025681
546.893069	5537.156094	15.907251	-0.104534	4.022864
546.782031	5529.162517	15.912256	-0.104508	4.020026
546.767573	5521.164964	15.917261	-0.104500	4.017186
546.919925	5513.128558	15.922266	-0.104523	4.014333
546.967192	5505.145645	15.927271	-0.104527	4.011496
546.769728	5497.158608	15.932275	-0.104485	4.008651
546.666095	5489.144936	15.937280	-0.104460	4.005795
546.865603	5481.153581	15.942285	-0.104492	4.002951
546.881295	5473.194798	15.947290	-0.104490	4.000114
546.675373	5465.244186	15.952295	-0.104446	3.997273
546.922968	5457.166958	15.957299	-0.104487	3.994393
546.800179	5449.222150	15.962304	-0.104459	3.991552
546.668837	5441.190951	15.967309	-0.104429	3.988678
546.812745	5433.171664	15.972314	-0.104450	3.985811
546.729593	5425.189883	15.977319	-0.104430	3.982951
546.610827	5417.218200	15.982323	-0.104402	3.980092
546.553060	5409.229344	15.987328	-0.104386	3.977226
546.530295	5401.195013	15.992333	-0.104376	3.974343
546.415827	5393.237904	15.997338	-0.104350	3.971483
546.546768	5385.166050	16.002343	-0.104369	3.968584
546.726305	5377.192243	16.007347	-0.104397	3.965719
546.652456	5369.201922	16.012352	-0.104378	3.962842
546.515029	5361.232716	16.017357	-0.104347	3.959969
546.580990	5353.267923	16.022362	-0.104354	3.957099
546.474563	5345.184236	16.027367	-0.104329	3.954182
546.195967	5337.278580	16.032371	-0.104272	3.951323
546.066726	5329.201080	16.037376	-0.104242	3.948402
546.007868	5321.194269	16.042381	-0.104226	3.945507
546.354881	5313.185771	16.047386	-0.104285	3.942616
546.187926	5305.224629	16.052391	-0.104249	3.939730
546.368882	5297.234432	16.057395	-0.104277	3.936839
546.191708	5289.184011	16.062400	-0.104239	3.933917
545.874994	5281.240574	16.067405	-0.104175	3.931028
545.892753	5273.230004	16.072410	-0.104173	3.928120
545.829847	5265.182307	16.077415	-0.104156	3.925194
545.891970	5257.236272	16.082419	-0.104162	3.922306
545.798036	5249.221026	16.087424	-0.104139	3.919387
545.972017	5241.247476	16.092429	-0.104166	3.916487
546.001244	5233.224006	16.097434	-0.104166	3.913563
545.742867	5225.230249	16.102439	-0.104113	3.910642
545.935526	5217.189641	16.107443	-0.104143	3.907711
545.861926	5209.173406	16.112448	-0.104124	3.904781
545.603786	5201.246483	16.117453	-0.104071	3.901878
545.881352	5193.214164	16.122458	-0.104117	3.898945
545.820360	5185.263071	16.127463	-0.104101	3.896033
545.895174	5177.268900	16.132467	-0.104109	3.893106
545.767779	5169.232925	16.137472	-0.104080	3.890156
545.864836	5161.246204	16.142477	-0.104093	3.887228
545.891893	5153.243786	16.147482	-0.104093	3.884290
545.446523	5145.321651	16.152487	-0.104005	3.881369
545.621449	5137.302909	16.157491	-0.104032	3.878424
545.611624	5129.313930	16.162496	-0.104025	3.875483
545.651748	5121.201177	16.167501	-0.104027	3.872496
545.629254	5113.164181	16.172506	-0.104017	3.869533
545.601097	5105.173433	16.177511	-0.104007	3.866584
545.620567	5097.197975	16.182515	-0.104005	3.863640
545.313899	5089.258694	16.187520	-0.103943	3.860700
545.384027	5081.241111	16.192525	-0.103950	3.857737
545.364303	5073.281119	16.197530	-0.103941	3.854791
545.018972	5065.295099	16.202535	-0.103872	3.851827
545.261217	5057.204533	16.207539	-0.103911	3.848833
545.480107	5049.274633	16.212544	-0.103947	3.845897
545.343610	5041.264250	16.217549	-0.103916	3.842921
545.253011	5033.328915	16.222554	-0.103894	3.839971
545.108225	5025.336525	16.227559	-0.103862	3.836997
545.080979	5017.310058	16.232563	-0.103851	3.834010
545.253583	5009.310967	16.237568	-0.103878	3.831035
545.243523	5001.299333	16.242573	-0.103871	3.828050
545.260306	4993.298251	16.247578	-0.103869	3.825066
544.915959	4985.360514	16.252583	-0.103799	3.822096
545.093995	4977.276424	16.257587	-0.103827	3.819081
545.210597	4969.319154	16.262592	-0.103844	3.816109
545.204953	4961.288506	16.267597	-0.103837	3.813105
545.300174	4953.302393	16.272602	-0.103850	3.810117
545.312765	4945.256629	16.277607	-0.103847	3.807102
545.046373	4937.292157	16.282611	-0.103792	3.804110
545.291699	4929.354146	16.287616	-0.103832	3.801137
545.229294	4921.312774	16.292621	-0.103815	3.798115
545.301532	4913.336140	16.297626	-0.103823	3.795119
545.042868	4905.334360	16.302631	-0.103770	3.792103
545.028085	4897.354938	16.307635	-0.103762	3.789098
545.354990	4889.327924	16.312640	-0.103817	3.786082
544.978192	4881.335250	16.317645	-0.103742	3.783059
545.004534	4873.357516	16.322650	-0.103741	3.780049
544.972323	4865.357503	16.327655	-0.103730	3.777027
544.951935	4857.332635	16.332659	-0.103721	3.773994
544.883843	4849.374111	16.337664	-0.103703	3.770982
544.897221	4841.327899	16.342669	-0.103700	3.767936
544.926649	4833.381917	16.347674	-0.103700	3.764926
544.761312	4825.392716	16.352679	-0.103664	3.761892
544.907931	4817.377345	16.357683	-0.103686	3.758854
544.992288	4809.456120	16.362688	-0.103697	3.755848
544.795772	4801.393059	16.367693	-0.103655	3.752778
544.696902	4793.425677	16.372698	-0.103631	3.749745
544.779843	4785.399985	16.377703	-0.103641	3.746691
544.641324	4777.428470	16.382707	-0.103610	3.743650
544.399444	4769.466818	16.387712	-0.103560	3.740608
544.532199	4761.430550	16.392717	-0.103579	3.737544
544.662158	4753.429594	16.397722	-0.103598	3.734491
544.280757	4745.464781	16.402727	-0.103522	3.731437
544.350392	4737.438391	16.407731	-0.103529	3.728368
544.220696	4729.460835	16.412736	-0.103500	3.725310
544.266818	4721.460558	16.417741	-0.103503	3.722245
544.227600	4713.441498	16.422746	-0.103490	3.719168
544.201553	4705.536360	16.427751	-0.103480	3.716133
544.314928	4697.438486	16.432755	-0.103496	3.713025
544.253026	4689.388087	16.437760	-0.103479	3.709928
544.301348	4681.388267	16.442765	-0.103483	3.706850
544.272341	4673.415583	16.447770	-0.103472	3.703779
543.696787	4665.517347	16.452775	-0.103360	3.700720
543.909531	4657.456995	16.457779	-0.103394	3.697615
543.777780	4649.452973	16.462784	-0.103364	3.694521
543.803306	4641.454082	16.467789	-0.103364	3.691431
543.744959	4633.465898	16.472794	-0.103347	3.688340
543.960068	4625.388650	16.477799	-0.103382	3.685219
544.110761	4617.481993	16.482803	-0.103405	3.682160
543.824883	4609.485834	16.487808	-0.103346	3.679052
543.878805	4601.517733	16.492813	-0.103351	3.675961
544.109152	4593.488067	16.497818	-0.103389	3.672848
543.858645	4585.476254	16.502823	-0.103337	3.669727
543.910448	4577.499612	16.507827	-0.103341	3.666625
544.013748	4569.495714	16.512832	-0.103355	3.663511
543.891458	4561.542937	16.517837	-0.103327	3.660409
543.834782	4553.556431	16.522842	-0.103311	3.657292
543.837352	4545.514309	16.527847	-0.103306	3.654152
543.870727	4537.563224	16.532851	-0.103307	3.651047
543.556376	4529.558510	16.537856	-0.103243	3.647908
543.452525	4521.562087	16.542861	-0.103219	3.644775
543.633806	4513.598838	16.547866	-0.103247	3.641661
543.497387	4505.596173	16.552871	-0.103216	3.638519
543.431803	4497.609817	16.557875	-0.103199	3.635384
543.569369	4489.591417	16.562880	-0.103219	3.632238
543.588901	4481.553330	16.567885	-0.103217	3.629079
543.651551	4473.606431	16.572890	-0.103224	3.625954
543.320869	4465.611928	16.577895	-0.103157	3.622797
543.477075	4457.596935	16.582899	-0.103181	3.619642
543.394572	4449.639171	16.587904	-0.103160	3.616501
543.339461	4441.609727	16.592909	-0.103144	3.613329
543.625996	4433.604644	16.597914	-0.103192	3.610174
543.220209	4425.646114	16.602919	-0.103111	3.607015
543.232787	4417.603787	16.607923	-0.103108	3.603832
543.150661	4409.673100	16.612928	-0.103088	3.600687
543.136452	4401.649225	16.617933	-0.103080	3.597505
542.808672	4393.708788	16.622938	-0.103014	3.594344
542.833613	4385.637372	16.627943	-0.103013	3.591139
543.088657	4377.632424	16.632947	-0.103055	3.587963
542.858980	4369.672425	16.637952	-0.103007	3.584789
542.885673	4361.669360	16.642957	-0.103007	3.581602
543.170389	4353.644957	16.647962	-0.103054	3.578411
542.915887	4345.666744	16.652967	-0.103002	3.575220
542.909660	4337.682808	16.657971	-0.102995	3.572031
542.957086	4329.669228	16.662976	-0.102999	3.568829
542.969249	4321.685734	16.667981	-0.102996	3.565636
543.023967	4313.729588	16.672986	-0.103001	3.562451
542.835417	4305.696019	16.677991	-0.102960	3.559225
543.181944	4297.721358	16.682995	-0.103019	3.556037
543.134788	4289.694795	16.688000	-0.103005	3.552812
542.928260	4281.677504	16.693005	-0.102961	3.549584
543.018207	4273.686245	16.698010	-0.102973	3.546372
542.775552	4265.706544	16.703015	-0.102922	3.543151
542.707761	4257.751863	16.708019	-0.102904	3.539944
542.663980	4249.763913	16.713024	-0.102891	3.536720
542.685085	4241.725744	16.718029	-0.102890	3.533475
542.595100	4233.794604	16.723034	-0.102868	3.530268
542.432841	4225.794504	16.728039	-0.102832	3.527027
542.604360	4217.746019	16.733043	-0.102859	3.523774
542.399379	4209.855693	16.738048	-0.102815	3.520570
542.005728	4201.872644	16.743053	-0.102737	3.517319
542.253406	4193.816551	16.748058	-0.102777	3.514057
542.238474	4185.819787	16.753063	-0.102769	3.510807
542.115917	4177.823504	16.758067	-0.102741	3.507550
542.020457	4169.840253	16.763072	-0.102718	3.504297
542.181374	4161.826717	16.768077	-0.102743	3.501037
541.871962	4153.892796	16.773082	-0.102680	3.497791
541.872494	4145.834153	16.778087	-0.102674	3.494501
541.834678	4137.878540	16.783091	-0.102662	3.491249
542.179809	4129.793945	16.788096	-0.102721	3.487953
542.113642	4121.794504	16.793101	-0.102703	3.484676
542.415863	4113.873786	16.798106	-0.102754	3.481440
542.007202	4105.912857	16.803111	-0.102673	3.478161
541.919918	4097.943776	16.808115	-0.102651	3.474887
541.840721	4089.924651	16.813120	-0.102631	3.471589
541.859013	4081.866656	16.818125	-0.102629	3.468275
542.098706	4073.846248	16.823130	-0.102669	3.464980
541.790741	4065.903386	16.828135	-0.102606	3.461697
541.609086	4057.950407	16.833139	-0.102567	3.458410
541.501154	4049.967349	16.838144	-0.102542	3.455110
541.598451	4041.957139	16.843149	-0.102554	3.451802
541.443898	4033.985685	16.848154	-0.102520	3.448499
541.449195	4025.957625	16.853159	-0.102516	3.445175
541.212978	4018.024879	16.858163	-0.102467	3.441879
541.510831	4009.974713	16.863168	-0.102517	3.438549
541.445071	4001.978706	16.868173	-0.102499	3.435226
541.426976	3994.017311	16.873178	-0.102491	3.431915
541.464907	3985.977231	16.878183	-0.102492	3.428571
541.458147	3978.010874	16.883187	-0.102486	3.425253
541.485879	3970.010457	16.888192	-0.102486	3.421918
540.997191	3962.069111	16.893197	-0.102389	3.418587
540.671944	3954.153455	16.898202	-0.102323	3.415269
540.565890	3946.113112	16.903207	-0.102298	3.411903
541.141248	3937.999691	16.908211	-0.102400	3.408527
541.238987	3930.012437	16.913216	-0.102413	3.405184
541.321920	3922.049116	16.918221	-0.102423	3.401847
541.047279	3914.091095	16.923226	-0.102367	3.398497
540.598872	3906.153553	16.928231	-0.102278	3.395145
540.896606	3898.077611	16.933235	-0.102328	3.391759
540.826599	3890.067582	16.938240	-0.102310	3.388384
540.826384	3882.027781	16.943245	-0.102304	3.384995
540.990184	3874.073725	16.948250	-0.102329	3.381645
541.058624	3866.074322	16.953255	-0.102337	3.378269
541.029930	3858.102303	16.958259	-0.102326	3.374898
541.019231	3850.153680	16.963264	-0.102319	3.371534
540.921396	3842.115173	16.968269	-0.102295	3.368126
541.076385	3834.118923	16.973274	-0.102319	3.364741
540.973700	3826.148571	16.978279	-0.102295	3.361354
541.162939	3818.157276	16.983283	-0.102324	3.357966
541.155505	3810.188882	16.988288	-0.102318	3.354577
541.072344	3802.179452	16.993293	-0.102297	3.351164
541.178758	3794.198991	16.998298	-0.102311	3.347767
540.992328	3786.203240	17.003303	-0.102271	3.344349
540.693437	3778.302359	17.008307	-0.102211	3.340963
540.226154	3770.353648	17.013312	-0.102118	3.337548
540.139803	3762.282713	17.018317	-0.102097	3.334091
540.686131	3754.259684	17.023322	-0.102193	3.330675
540.665448	3746.229377	17.028327	-0.102184	3.327231
540.558249	3738.246340	17.033331	-0.102159	3.323800
540.617906	3730.316302	17.038336	-0.102165	3.320395
540.625264	3722.313435	17.043341	-0.102161	3.316953
540.810379	3714.287769	17.048346	-0.102190	3.313504
540.630431	3706.326239	17.053351	-0.102151	3.310066
540.795674	3698.304482	17.058355	-0.102176	3.306611
540.926875	3690.307821	17.063360	-0.102195	3.303162
540.655833	3682.324685	17.068365	-0.102140	3.299700
540.624134	3674.402693	17.073370	-0.102129	3.296269
540.569167	3666.377288	17.078375	-0.102113	3.292790
540.229859	3658.407059	17.083379	-0.102044	3.289320
540.534648	3650.381092	17.088384	-0.102096	3.285847
540.326547	3642.394411	17.093389	-0.102052	3.282367
540.294816	3634.421713	17.098394	-0.102041	3.278896
540.042994	3626.501254	17.103399	-0.101988	3.275436
540.157161	3618.461271	17.108403	-0.102004	3.271935
539.908132	3610.491097	17.113408	-0.101953	3.268446
540.086451	3602.430937	17.118413	-0.101981	3.264931
540.130065	3594.488813	17.123418	-0.101983	3.261458
540.066268	3586.485974	17.128423	-0.101966	3.257951
539.582475	3578.553486	17.133427	-0.101871	3.254454
539.413271	3570.591307	17.138432	-0.101834	3.250952
539.754457	3562.495836	17.143437	-0.101892	3.247409
539.603063	3554.550037	17.148442	-0.101859	3.243908
539.628602	3546.562343	17.153447	-0.101858	3.240392
540.037720	3538.549514	17.158451	-0.101929	3.236877
539.794027	3530.581701	17.163456	-0.101878	3.233351
539.834838	3522.557101	17.168461	-0.101881	3.229808
540.039408	3514.571724	17.173466	-0.101913	3.226285
539.890803	3506.577571	17.178471	-0.101880	3.222740
539.774132	3498.591383	17.183475	-0.101853	3.219196
539.749667	3490.638363	17.188480	-0.101844	3.215666
539.582917	3482.633847	17.193485	-0.101807	3.212103
539.342894	3474.665622	17.198490	-0.101757	3.208550
539.257526	3466.657950	17.203495	-0.101736	3.204981
539.365947	3458.672926	17.208499	-0.101751	3.201427
539.233129	3450.719125	17.213504	-0.101721	3.197873
539.299008	3442.658065	17.218509	-0.101728	3.194275
539.374673	3434.720252	17.223514	-0.101737	3.190729
539.256352	3426.711644	17.228519	-0.101709	3.187139
539.132809	3418.712626	17.233523	-0.101681	3.183548
539.346012	3410.745753	17.238528	-0.101715	3.179983
539.540970	3402.722101	17.243533	-0.101746	3.176387
539.462929	3394.776976	17.248538	-0.101726	3.172811
539.411964	3386.730788	17.253543	-0.101712	3.169186
539.234285	3378.824573	17.258547	-0.101673	3.165615
539.143933	3370.848995	17.263552	-0.101651	3.162012
538.823358	3362.885756	17.268557	-0.101586	3.158401
538.713658	3354.913862	17.273562	-0.101560	3.154791
538.805844	3346.881692	17.278567	-0.101572	3.151158
538.603979	3338.909727	17.283571	-0.101529	3.147535
538.544579	3330.877984	17.288576	-0.101513	3.143887
538.330700	3322.940229	17.293581	-0.101468	3.140271
538.357378	3314.956343	17.298586	-0.101467	3.136640
538.791728	3306.845306	17.303591	-0.101543	3.132966
538.877671	3298.875394	17.308595	-0.101554	3.129336
539.168054	3290.878597	17.313600	-0.101602	3.125699
538.592915	3282.966455	17.318605	-0.101490	3.122057
538.663002	3275.005430	17.323610	-0.101498	3.118418
538.890305	3266.962302	17.328615	-0.101535	3.114744
538.908632	3258.984236	17.333619	-0.101533	3.111086
538.754747	3251.016564	17.338624	-0.101499	3.107420
538.497868	3243.043644	17.343629	-0.101446	3.103743
538.735351	3235.071049	17.348634	-0.101485	3.100085
538.833694	3227.031093	17.353639	-0.101498	3.096384
539.143388	3218.996180	17.358643	-0.101550	3.092692
539.077538	3211.056143	17.363648	-0.101532	3.089022
539.071220	3203.068242	17.368653	-0.101526	3.085327
539.101827	3195.114453	17.373658	-0.101526	3.081646
538.933314	3187.149438	17.378663	-0.101490	3.077946
538.983608	3179.154887	17.383667	-0.101494	3.074238
538.971716	3171.142762	17.388672	-0.101486	3.070514
538.838444	3163.154176	17.393677	-0.101456	3.066791
538.918628	3155.152720	17.398682	-0.101466	3.063068
538.785729	3147.192296	17.403687	-0.101436	3.059349
538.761510	3139.229056	17.408691	-0.101426	3.055630
538.569548	3131.286885	17.413696	-0.101385	3.051907
538.568036	3123.243433	17.418701	-0.101379	3.048142
538.510681	3115.256335	17.423706	-0.101363	3.044396
538.466379	3107.312317	17.428711	-0.101350	3.040666
538.145503	3099.360428	17.433715	-0.101285	3.036914
538.227038	3091.347303	17.438720	-0.101295	3.033149
538.449877	3083.276964	17.443725	-0.101331	3.029359
538.642259	3075.315740	17.448730	-0.101361	3.025614
538.459732	3067.372608	17.453735	-0.101322	3.021854
538.302480	3059.393899	17.458739	-0.101287	3.018075
538.411264	3051.424898	17.463744	-0.101302	3.014308
538.309242	3043.430143	17.468749	-0.101278	3.010514
538.330924	3035.451495	17.473754	-0.101277	3.006729
538.558343	3027.434804	17.478759	-0.101314	3.002931
537.922586	3019.566393	17.483763	-0.101190	2.999156
537.869577	3011.595117	17.488768	-0.101175	2.995356
538.235075	3003.499747	17.493773	-0.101238	2.991513
537.886361	2995.567310	17.498778	-0.101167	2.987707
537.783539	2987.546428	17.503783	-0.101143	2.983867
537.804875	2979.576706	17.508787	-0.101142	2.980052
538.016979	2971.579773	17.513792	-0.101176	2.976229
537.750211	2963.573026	17.518797	-0.101121	2.972372
537.937169	2955.574650	17.523802	-0.101150	2.968537
538.121757	2947.564727	17.528807	-0.101179	2.964691
538.214295	2939.596423	17.533811	-0.101191	2.960856
538.227426	2931.650879	17.538816	-0.101188	2.957023
537.837729	2923.720612	17.543821	-0.101111	2.953171
537.984137	2915.705843	17.548826	-0.101132	2.949302
537.996461	2907.706462	17.553831	-0.101129	2.945427
538.080992	2899.735449	17.558835	-0.101140	2.941565
537.962378	2891.780368	17.563840	-0.101113	2.937695
538.140337	2883.748183	17.568845	-0.101140	2.933798
537.940439	2875.812877	17.573850	-0.101098	2.929923
537.633398	2867.890355	17.578855	-0.101035	2.926044
537.653852	2859.873441	17.583859	-0.101034	2.922130
537.687471	2851.912386	17.588864	-0.101035	2.918240
537.779133	2843.880322	17.593869	-0.101047	2.914312
537.516616	2835.901419	17.598874	-0.100992	2.910386
537.206712	2827.928510	17.603879	-0.100929	2.906455
537.036177	2819.957421	17.608883	-0.100892	2.902527
537.556028	2811.924206	17.613888	-0.100984	2.898602
537.418971	2803.924174	17.618893	-0.100953	2.894651
537.575892	2795.944667	17.623898	-0.100977	2.890721
537.666885	2787.953634	17.628903	-0.100988	2.886776
537.566309	2779.994936	17.633907	-0.100964	2.882831
537.489884	2772.052029	17.638912	-0.100945	2.878890
537.175030	2764.116041	17.643917	-0.100881	2.874934
537.471095	2756.097869	17.648922	-0.100931	2.870966
537.199976	2748.151470	17.653927	-0.100875	2.866996
537.219214	2740.122691	17.658931	-0.100873	2.862996
537.458591	2732.147721	17.663936	-0.100913	2.859029
537.271855	2724.179563	17.668941	-0.100872	2.855036
537.268589	2716.218025	17.673946	-0.100867	2.851052
537.267743	2708.193885	17.678951	-0.100861	2.847030
537.145473	2700.235328	17.683955	-0.100833	2.843029
536.956116	2692.327359	17.688960	-0.100793	2.839044
537.107678	2684.307308	17.693965	-0.100815	2.835016
537.274730	2676.307319	17.698970	-0.100841	2.830994
537.011171	2668.342055	17.703975	-0.100787	2.826958
536.937654	2660.346716	17.708979	-0.100768	2.822913
537.204375	2652.358841	17.713984	-0.100812	2.818885
536.771895	2644.451787	17.718989	-0.100726	2.814852
536.805903	2636.454482	17.723994	-0.100727	2.810794
536.873707	2628.442089	17.728999	-0.100735	2.806725
536.966456	2620.458609	17.734003	-0.100747	2.802666
536.791649	2612.510360	17.739008	-0.100709	2.798603
536.412570	2604.570619	17.744013	-0.100633	2.794527
536.522243	2596.602216	17.749018	-0.100648	2.790459
536.661386	2588.552376	17.754023	-0.100669	2.786345
536.490855	2580.594945	17.759027	-0.100632	2.782254
536.731011	2572.592126	17.764032	-0.100671	2.778158
536.648596	2564.624238	17.769037	-0.100650	2.774055
536.488028	2556.664645	17.774042	-0.100615	2.769945
536.358944	2548.692085	17.779047	-0.100586	2.765825
536.609642	2540.701219	17.784051	-0.100627	2.761711
536.730475	2532.747693	17.789056	-0.100644	2.757603
536.454345	2524.766186	17.794061	-0.100588	2.753451
536.383469	2516.764756	17.799066	-0.100569	2.749294
536.180526	2508.816339	17.804071	-0.100526	2.745150
536.341960	2500.790004	17.809075	-0.100551	2.740982
536.656791	2492.799418	17.814080	-0.100604	2.736835
536.373637	2484.863354	17.819085	-0.100546	2.732674
536.304680	2476.912775	17.824090	-0.100528	2.728512
536.202921	2468.917529	17.829095	-0.100504	2.724318
536.247343	2460.968885	17.834099	-0.100507	2.720152
536.097414	2453.038487	17.839104	-0.100474	2.715976
535.942201	2445.061120	17.844109	-0.100439	2.711769
535.944281	2437.069002	17.849114	-0.100434	2.707557
536.167336	2429.041994	17.854119	-0.100471	2.703335
536.157634	2421.077923	17.859123	-0.100463	2.699124
535.995356	2413.157696	17.864128	-0.100428	2.694920
536.170257	2405.116131	17.869133	-0.100455	2.690667
536.047352	2397.174404	17.874138	-0.100427	2.686441
535.831870	2389.230688	17.879143	-0.100382	2.682201
535.902955	2381.239017	17.884147	-0.100390	2.677948
536.110071	2373.259786	17.889152	-0.100423	2.673703
535.668500	2365.315103	17.894157	-0.100335	2.669428
535.726787	2357.327524	17.899162	-0.100341	2.665156
535.785079	2349.338172	17.904167	-0.100346	2.660875
535.582144	2341.402394	17.909171	-0.100303	2.656600
535.669984	2333.414209	17.914176	-0.100314	2.652308
535.655051	2325.402625	17.919181	-0.100306	2.647990
535.842246	2317.426309	17.924186	-0.100336	2.643698
535.652150	2309.505079	17.929191	-0.100295	2.639403
535.538531	2301.575008	17.934195	-0.100269	2.635102
535.621629	2293.579238	17.939200	-0.100279	2.630771
535.258964	2285.605641	17.944205	-0.100206	2.626415
535.564174	2277.609534	17.949210	-0.100258	2.622084
535.513041	2269.656188	17.954215	-0.100243	2.617745
535.352990	2261.698486	17.959219	-0.100208	2.613390
535.462115	2253.706862	17.964224	-0.100223	2.609027
535.123602	2245.763984	17.969229	-0.100154	2.604653
535.455959	2237.781084	17.974234	-0.100211	2.600295
535.318075	2229.837683	17.979239	-0.100180	2.595920
535.146603	2221.804889	17.984243	-0.100143	2.591485
535.114161	2213.780903	17.989248	-0.100131	2.587058
534.969743	2205.832765	17.994253	-0.100099	2.582657
535.113040	2197.853509	17.999258	-0.100121	2.578251
535.169442	2189.895404	18.004263	-0.100126	2.573843
534.951122	2181.953914	18.009267	-0.100080	2.569418
535.215493	2173.948803	18.014272	-0.100124	2.564983
535.179738	2166.003298	18.019277	-0.100112	2.560554
535.116823	2158.077807	18.024282	-0.100095	2.556125
534.938575	2150.139484	18.029287	-0.100056	2.551674
534.898357	2142.136542	18.034291	-0.100044	2.547188
535.098888	2134.152553	18.039296	-0.100076	2.542722
534.809233	2126.232662	18.044301	-0.100016	2.538249
534.871324	2118.265789	18.049306	-0.100023	2.533768
534.815110	2110.297179	18.054311	-0.100007	2.529268
534.923463	2102.301490	18.059315	-0.100022	2.524758
534.760233	2094.399035	18.064320	-0.099986	2.520272
534.570883	2086.443985	18.069325	-0.099945	2.515747
534.097665	2078.544108	18.074330	-0.099852	2.511223
534.330947	2070.484428	18.079335	-0.099890	2.506653
534.280974	2062.498929	18.084339	-0.099876	2.502096
534.313243	2054.564574	18.089344	-0.099876	2.497565
534.434534	2046.540109	18.094349	-0.099894	2.492982
534.375205	2038.592969	18.099354	-0.099877	2.488421
534.379512	2030.623637	18.104359	-0.099873	2.483843
534.143383	2022.695460	18.109363	-0.099824	2.479263
534.186514	2014.771305	18.114368	-0.099826	2.474697
534.063031	2006.800099	18.119373	-0.099798	2.470084
533.953498	1998.825592	18.124378	-0.099772	2.465460
534.188509	1990.825486	18.129383	-0.099811	2.460840
534.232035	1982.863523	18.134387	-0.099814	2.456218
534.319848	1974.898091	18.139392	-0.099825	2.451589
533.959996	1966.973985	18.144397	-0.099752	2.446941
533.740591	1959.043156	18.149402	-0.099706	2.442291
533.682255	1951.111878	18.154407	-0.099690	2.437644
533.585312	1943.132782	18.159411	-0.099667	2.432958
533.608427	1935.134096	18.164416	-0.099666	2.428260
533.342401	1927.169900	18.169421	-0.099611	2.423550
533.461940	1919.197072	18.174426	-0.099628	2.418857
533.805105	1911.180054	18.179431	-0.099686	2.414146
533.326414	1903.271932	18.184435	-0.099592	2.409425
533.849739	1895.234296	18.189440	-0.099684	2.404698
533.652671	1887.328613	18.194445	-0.099642	2.399982
533.437639	1879.435756	18.199450	-0.099597	2.395263
533.574425	1871.445573	18.204455	-0.099617	2.390506
533.548115	1863.465977	18.209459	-0.099607	2.385731
533.650557	1855.512637	18.214464	-0.099621	2.380974
533.512011	1847.578473	18.219469	-0.099589	2.376199
533.725040	1839.601533	18.224474	-0.099624	2.371417
533.688844	1831.632020	18.229479	-0.099612	2.366609
533.660182	1823.695766	18.234483	-0.099601	2.361813
533.731851	1815.762058	18.239488	-0.099609	2.357016
533.488369	1807.823672	18.244493	-0.099559	2.352181
533.139160	1799.913039	18.249498	-0.099488	2.347344
533.077246	1791.940947	18.254503	-0.099472	2.342484
533.286148	1783.930414	18.259507	-0.099505	2.337612
533.358862	1775.982538	18.264512	-0.099513	2.332757
533.186499	1768.024570	18.269517	-0.099476	2.327865
533.112823	1760.104721	18.274522	-0.099457	2.322995
533.009669	1752.178954	18.279527	-0.099433	2.318108
532.942168	1744.216273	18.284531	-0.099415	2.313191
533.077635	1736.243437	18.289536	-0.099435	2.308275
532.888350	1728.300175	18.294541	-0.099394	2.303339
532.916513	1720.341095	18.299546	-0.099394	2.298401
532.917131	1712.377570	18.304551	-0.099389	2.293447
532.954392	1704.408919	18.309555	-0.099390	2.288482
533.102270	1696.453206	18.314560	-0.099413	2.283525
532.775890	1688.561907	18.319565	-0.099347	2.278555
532.773797	1680.609515	18.324570	-0.099341	2.273565
532.326816	1672.698420	18.329575	-0.099253	2.268551
532.493217	1664.660189	18.334579	-0.099278	2.263499
532.661274	1656.702488	18.339584	-0.099304	2.258487
532.480667	1648.764887	18.344589	-0.099265	2.253446
532.296044	1640.851619	18.349594	-0.099226	2.248408
532.347796	1632.874600	18.354599	-0.099230	2.243340
532.420485	1624.933664	18.359603	-0.099238	2.238285
532.589582	1616.963400	18.364608	-0.099264	2.233208
532.437034	1609.032913	18.369613	-0.099231	2.228117
532.421763	1601.088223	18.374618	-0.099223	2.223017
532.225210	1593.185103	18.379623	-0.099181	2.217915
532.342257	1585.190778	18.384627	-0.099197	2.212772
532.405780	1577.248797	18.389632	-0.099204	2.207645
532.422350	1569.293567	18.394637	-0.099202	2.202494
532.338576	1561.384575	18.399642	-0.099181	2.197351
532.113647	1553.490194	18.404647	-0.099134	2.192193
531.742901	1545.579785	18.409651	-0.099059	2.186999
531.930842	1537.584920	18.414656	-0.099089	2.181789
531.607532	1529.669878	18.419661	-0.099023	2.176571
532.333158	1521.602692	18.424666	-0.099153	2.171338
532.294891	1513.686160	18.429671	-0.099141	2.166121
532.024832	1505.796333	18.434675	-0.099085	2.160887
532.038685	1497.868916	18.439680	-0.099083	2.155642
531.841398	1489.951068	18.444685	-0.099041	2.150370
531.990059	1481.966315	18.449690	-0.099063	2.145074
531.921634	1474.058069	18.454695	-0.099045	2.139796
531.822809	1466.122890	18.459699	-0.099021	2.134483
531.886962	1458.180783	18.464704	-0.099028	2.129168
531.673474	1450.250911	18.469709	-0.098983	2.123821
531.746515	1442.329394	18.474714	-0.098991	2.118494
531.878803	1434.366733	18.479719	-0.099011	2.113131
531.819305	1426.392973	18.484723	-0.098994	2.107729
531.687672	1418.489893	18.489728	-0.098964	2.102353
531.720137	1410.544313	18.494733	-0.098965	2.096951
531.623510	1402.624905	18.499738	-0.098942	2.091540
531.281232	1394.739698	18.504743	-0.098873	2.086114
531.352952	1386.776227	18.509747	-0.098881	2.080662
531.701283	1378.810407	18.514752	-0.098941	2.075221
531.334703	1370.922423	18.519757	-0.098867	2.069748
531.543672	1362.952591	18.524762	-0.098901	2.064261
531.448767	1355.064952	18.529767	-0.098878	2.058786
531.256792	1347.141457	18.534771	-0.098837	2.053262
531.230594	1339.219973	18.539776	-0.098827	2.047741
531.310725	1331.263583	18.544781	-0.098836	2.042192
531.433549	1323.340248	18.549786	-0.098854	2.036656
531.154227	1315.447058	18.554791	-0.098797	2.031083
531.165067	1307.482392	18.559795	-0.098793	2.025475
531.174747	1299.579433	18.564800	-0.098790	2.019895
530.966850	1291.669089	18.569805	-0.098746	2.014272
530.821158	1283.770871	18.574810	-0.098714	2.008648
531.326360	1275.746115	18.579815	-0.098802	2.002986
531.121272	1267.871705	18.584819	-0.098759	1.997341
530.995504	1259.984378	18.589824	-0.098730	1.991679
530.865307	1252.045338	18.594829	-0.098701	1.985963
530.972932	1244.123167	18.599834	-0.098715	1.980269
530.445951	1236.299089	18.604839	-0.098612	1.974560
530.469160	1228.333303	18.609843	-0.098611	1.968791
530.712707	1220.379682	18.614848	-0.098651	1.963039
530.552228	1212.484520	18.619853	-0.098616	1.957268
530.445635	1204.583113	18.624858	-0.098591	1.951481
530.597841	1196.618433	18.629863	-0.098614	1.945659
530.546681	1188.702551	18.634867	-0.098599	1.939833
530.588798	1180.783714	18.639872	-0.098602	1.933998
530.656303	1172.827142	18.644877	-0.098609	1.928120
530.650770	1164.929313	18.649882	-0.098603	1.922259
530.282810	1157.091345	18.654887	-0.098529	1.916384
530.109511	1149.191400	18.659891	-0.098491	1.910467
530.268067	1141.238628	18.664896	-0.098516	1.904529
530.377142	1133.306178	18.669901	-0.098531	1.898583
530.072389	1125.448588	18.674906	-0.098469	1.892627
529.927380	1117.549773	18.679911	-0.098437	1.886639
529.924031	1109.626775	18.684915	-0.098431	1.880630
529.936076	1101.736752	18.689920	-0.098428	1.874629
529.862256	1093.828107	18.694925	-0.098409	1.868584
529.784518	1085.916168	18.699930	-0.098389	1.862516
529.652013	1078.037624	18.704935	-0.098359	1.856448
529.664494	1070.098165	18.709939	-0.098356	1.850330
529.678362	1062.196388	18.714944	-0.098353	1.844222
529.487609	1054.327719	18.719949	-0.098313	1.838094
529.596112	1046.409092	18.724954	-0.098328	1.831942
529.566619	1038.500699	18.729959	-0.098317	1.825761
529.566205	1030.607622	18.734963	-0.098311	1.819575
529.369574	1022.756824	18.739968	-0.098270	1.813377
529.461473	1014.806579	18.744973	-0.098281	1.807115
529.487615	1006.930954	18.749978	-0.098281	1.800881
529.546549	999.042727	18.754983	-0.098287	1.794621
529.459548	991.127611	18.759987	-0.098265	1.788298
529.767214	983.192943	18.764992	-0.098317	1.781987
529.635657	975.328083	18.769997	-0.098288	1.775654
529.353537	967.486030	18.775002	-0.098230	1.769299
529.160471	959.634772	18.780007	-0.098189	1.762924
529.316402	951.713528	18.785011	-0.098212	1.756513
529.222735	943.861415	18.790016	-0.098190	1.750103
529.013701	935.991407	18.795021	-0.098146	1.743641
528.804891	928.147464	18.800026	-0.098102	1.737175
529.011461	920.204448	18.805031	-0.098135	1.730658
528.814296	912.341607	18.810035	-0.098093	1.724129
529.023396	904.454086	18.815040	-0.098126	1.717609
528.855209	896.590497	18.820045	-0.098090	1.711034
528.589356	888.756645	18.825050	-0.098035	1.704446
528.429404	880.905569	18.830055	-0.098000	1.697831
528.225009	873.042513	18.835059	-0.097957	1.691175
528.462712	865.111798	18.840064	-0.097996	1.684494
528.205130	857.294850	18.845069	-0.097943	1.677817
528.330580	849.384840	18.850074	-0.097961	1.671085
528.404387	841.498540	18.855079	-0.097969	1.664340
528.205573	833.672806	18.860083	-0.097927	1.657581
528.600610	825.745869	18.865088	-0.097995	1.650790
528.384975	817.920694	18.870093	-0.097950	1.643974
528.149417	810.113602	18.875098	-0.097901	1.637143
528.555631	802.152175	18.880103	-0.097971	1.630237
528.231750	794.340204	18.885107	-0.097906	1.623332
528.359892	786.469309	18.890112	-0.097924	1.616408
528.083333	778.655046	18.895117	-0.097868	1.609447
528.146259	770.793983	18.900122	-0.097874	1.602463
528.248709	762.943082	18.905127	-0.097888	1.595463
527.983974	755.133885	18.910131	-0.097834	1.588417
528.167831	747.258168	18.915136	-0.097863	1.581345
527.863236	739.474956	18.920141	-0.097801	1.574253
527.487505	731.686522	18.925146	-0.097726	1.567113
527.532241	723.842677	18.930151	-0.097729	1.559953
527.491509	716.001570	18.935155	-0.097716	1.552749
527.594660	708.129901	18.940160	-0.097730	1.545505
527.440953	700.320860	18.945165	-0.097696	1.538246
527.050664	692.545091	18.950170	-0.097618	1.530948
527.441851	684.640400	18.955175	-0.097686	1.523613
527.044906	676.879999	18.960179	-0.097607	1.516257
527.087226	669.052801	18.965184	-0.097609	1.508871
527.084266	661.213277	18.970189	-0.097604	1.501429
527.246185	653.377721	18.975194	-0.097629	1.493980
526.747011	645.647966	18.980199	-0.097530	1.486491
526.588751	637.852485	18.985203	-0.097496	1.478954
526.667744	630.011747	18.990208	-0.097505	1.471373
526.525092	622.187988	18.995213	-0.097474	1.463734
526.184094	614.446210	19.000218	-0.097405	1.456102
526.391094	606.589868	19.005223	-0.097438	1.448407
526.273847	598.798156	19.010227	-0.097411	1.440681
526.463887	590.982043	19.015232	-0.097441	1.432940
526.164642	583.227330	19.020237	-0.097380	1.425138
526.033301	575.465424	19.025242	-0.097351	1.417313
526.167391	567.646408	19.030247	-0.097371	1.409431
525.917479	559.898685	19.035251	-0.097319	1.401513
526.093077	552.107094	19.040256	-0.097346	1.393577
525.814241	544.344687	19.045261	-0.097289	1.385548
526.090692	536.526079	19.050266	-0.097336	1.377510
525.997107	528.785374	19.055271	-0.097313	1.369441
526.001052	521.009015	19.060275	-0.097309	1.361304
525.599330	513.340974	19.065280	-0.097229	1.353162
525.364608	505.609736	19.070285	-0.097180	1.344932
525.173061	497.893219	19.075290	-0.097139	1.336675
525.543558	490.061328	19.080295	-0.097203	1.328344
525.440652	482.334144	19.085299	-0.097179	1.319987
525.757628	474.508930	19.090304	-0.097232	1.311548
525.839078	466.699875	19.095309	-0.097242	1.303028
525.931663	458.972755	19.100314	-0.097254	1.294544
525.876083	451.271978	19.105319	-0.097239	1.286006
525.988041	443.548914	19.110323	-0.097255	1.277418
525.538033	435.948970	19.115328	-0.097166	1.268804
525.768717	428.182139	19.120333	-0.097204	1.260071
525.734130	420.501735	19.125338	-0.097192	1.251325
525.762668	412.809826	19.130343	-0.097192	1.242517
525.548794	405.169795	19.135347	-0.097147	1.233658
525.731780	397.453038	19.140352	-0.097176	1.224725
525.334515	389.843887	19.145357	-0.097097	1.215736
525.185443	382.192787	19.150362	-0.097064	1.206680
525.542779	374.468402	19.155367	-0.097126	1.197571
525.172668	366.870633	19.160371	-0.097052	1.188396
525.304896	359.194519	19.165376	-0.097071	1.179158
525.027474	351.597103	19.170381	-0.097015	1.169858
524.561685	344.044697	19.175386	-0.096923	1.160499
524.851653	336.346061	19.180391	-0.096972	1.151042
524.833407	328.697467	19.185395	-0.096963	1.141504
524.861613	321.085480	19.190400	-0.096963	1.131942
524.391162	313.547572	19.195405	-0.096871	1.122284
524.634725	305.903641	19.200410	-0.096911	1.112563
524.789953	298.288145	19.205415	-0.096935	1.102773
524.651077	290.732991	19.210419	-0.096904	1.092909
524.634551	283.161528	19.215424	-0.096896	1.082961
524.287392	275.667923	19.220429	-0.096826	1.072949
524.640035	268.042036	19.225434	-0.096887	1.062826
524.458742	260.539623	19.230439	-0.096848	1.052649
524.087823	253.068098	19.235443	-0.096774	1.042370
524.277953	245.525654	19.240448	-0.096804	1.032024
524.007198	238.059066	19.245453	-0.096749	1.021568
523.801606	230.597960	19.250458	-0.096706	1.011028
523.663752	223.139897	19.255463	-0.096675	1.000397
523.373302	215.701661	19.260467	-0.096616	0.989643
522.694782	208.344087	19.265472	-0.096485	0.978789
522.657023	200.866331	19.270477	-0.096473	0.967801
522.314018	193.488125	19.275482	-0.096404	0.956755
521.139745	186.258601	19.280487	-0.096181	0.945585
519.383190	179.118033	19.285491	-0.095849	0.934261
518.588485	171.811549	19.290496	-0.095696	0.922802
517.862362	164.506336	19.295501	-0.095556	0.911219
516.877321	157.253893	19.300506	-0.095368	0.899497
516.752702	149.861883	19.305511	-0.095340	0.887639
516.010845	142.620840	19.310515	-0.095197	0.875690
515.240458	135.402652	19.315520	-0.095048	0.863604
514.657257	128.161965	19.320525	-0.094935	0.851364
514.022386	120.968311	19.325530	-0.094812	0.839010
513.297319	113.795833	19.330535	-0.094672	0.826479
512.601484	106.639726	19.335539	-0.094538	0.813794
512.078519	99.494735	19.340544	-0.094436	0.800981
511.052729	92.462374	19.345549	-0.094240	0.788002
510.034225	85.458836	19.350554	-0.094046	0.774860
509.305613	78.430846	19.355559	-0.093905	0.761542
508.213429	71.685102	19.360563	-0.093697	0.748402