Fri Apr 16 18:42:23 2021

Number of Points = 3635
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.726184	0.037838	0.000000	0.000044	0.309221

1.727298	0.040584	0.005005	0.000043	0.309234
1.830536	0.019805	0.010010	0.000024	0.309225
1.829154	-0.029855	0.015014	0.000025	0.308991
1.737977	-0.034312	0.020019	0.000042	0.308892
1.751945	-0.036600	0.025024	0.000039	0.308893
1.716219	-0.028925	0.030029	0.000046	0.308899
1.659889	-0.021139	0.035034	0.000056	0.308887
1.815011	-0.048819	0.040038	0.000027	0.308889
1.851860	-0.053951	0.045043	0.000021	0.308896
1.673185	-0.022420	0.050048	0.000054	0.308892
1.715713	-0.029522	0.055053	0.000046	0.308894
1.777256	-0.042423	0.060058	0.000035	0.308886
1.952440	-0.074161	0.065062	0.000002	0.308886
1.832482	-0.051977	0.070067	0.000024	0.308888
1.742225	-0.036765	0.075072	0.000041	0.308882
1.911987	-0.064838	0.080077	0.000010	0.308895
1.897847	-0.112997	0.085082	0.000012	0.308657
1.926004	-0.134624	0.090086	0.000007	0.308580
2.113605	-0.167760	0.095091	-0.000028	0.308584
1.788491	-0.110965	0.100096	0.000033	0.308573
1.906304	-0.130347	0.105101	0.000011	0.308582
1.880235	-0.127071	0.110106	0.000016	0.308575
1.931884	-0.174376	0.115110	0.000006	0.308397
1.833062	-0.186213	0.120115	0.000025	0.308257
1.819685	-0.184489	0.125120	0.000027	0.308254
1.912573	-0.199070	0.130125	0.000010	0.308264
1.563074	-0.136375	0.135130	0.000075	0.308260
1.539402	-0.164894	0.140134	0.000080	0.308106
1.820913	-0.243386	0.145139	0.000027	0.307977
1.739360	-0.230246	0.150144	0.000043	0.307969
1.728473	-0.226971	0.155149	0.000045	0.307975
1.747060	-0.250193	0.160154	0.000041	0.307882
1.756051	-0.305102	0.165158	0.000040	0.307631
1.718330	-0.297886	0.170163	0.000047	0.307633
1.666833	-0.290171	0.175168	0.000056	0.307625
2.059324	-0.396184	0.180173	-0.000017	0.307461
1.633465	-0.350684	0.185178	0.000063	0.307311
1.873859	-0.394147	0.190182	0.000018	0.307312
1.777070	-0.389667	0.195187	0.000036	0.307250
1.787082	-0.447963	0.200192	0.000034	0.306984
1.721565	-0.433761	0.205197	0.000047	0.306994
1.649784	-0.427896	0.210202	0.000060	0.306960
1.865299	-0.520761	0.215206	0.000020	0.306707
1.753947	-0.500395	0.220211	0.000041	0.306707
1.669925	-0.502204	0.225216	0.000056	0.306626
1.896285	-0.596651	0.230221	0.000014	0.306375
1.428416	-0.511679	0.235226	0.000101	0.306374
1.319418	-0.522077	0.240230	0.000122	0.306231
1.512984	-0.592073	0.245235	0.000086	0.306066
1.653532	-0.619348	0.250240	0.000060	0.306058
1.577685	-0.658884	0.255245	0.000074	0.305806
1.848435	-0.722645	0.260250	0.000024	0.305737
1.976193	-0.766998	0.265254	-0.000000	0.305636
1.653842	-0.740006	0.270259	0.000060	0.305487
1.614540	-0.739562	0.275264	0.000067	0.305455
1.714387	-0.822556	0.280269	0.000049	0.305147
1.653837	-0.812606	0.285274	0.000060	0.305142
1.512558	-0.842283	0.290278	0.000086	0.304879
1.812932	-0.907729	0.295283	0.000031	0.304827
1.652278	-0.925917	0.300288	0.000061	0.304602
1.397729	-0.900698	0.305293	0.000108	0.304502
1.541381	-0.961471	0.310298	0.000081	0.304337
1.378088	-0.957423	0.315302	0.000112	0.304215
1.418439	-0.999187	0.320307	0.000104	0.304051
1.191844	-0.994862	0.325312	0.000147	0.303875
1.590364	-1.096126	0.330317	0.000072	0.303738
1.495625	-1.115896	0.335322	0.000090	0.303561
1.363168	-1.126744	0.340326	0.000115	0.303395
1.579102	-1.197099	0.345331	0.000075	0.303246
1.568238	-1.237947	0.350336	0.000077	0.303042
1.369236	-1.218603	0.355341	0.000114	0.302961
1.323679	-1.272506	0.360346	0.000123	0.302664
1.526385	-1.322919	0.365350	0.000085	0.302599
1.506812	-1.381196	0.370355	0.000089	0.302303
1.605163	-1.423854	0.375360	0.000070	0.302184
1.670862	-1.479211	0.380365	0.000058	0.301976
1.507260	-1.491497	0.385370	0.000089	0.301774
1.316565	-1.476373	0.390374	0.000124	0.301680
1.554430	-1.586817	0.395379	0.000080	0.301357
1.500327	-1.605719	0.400384	0.000090	0.301219
1.432280	-1.627988	0.405389	0.000103	0.301053
1.334743	-1.666366	0.410394	0.000121	0.300783
1.331539	-1.689369	0.415398	0.000122	0.300669
1.483807	-1.752890	0.420403	0.000094	0.300496
1.469097	-1.804552	0.425408	0.000096	0.300234
1.362189	-1.817116	0.430413	0.000116	0.300080
1.134774	-1.827191	0.435418	0.000159	0.299832
1.061190	-1.862170	0.440422	0.000172	0.299598
1.014758	-1.885030	0.445427	0.000181	0.299447
0.979880	-1.926554	0.450432	0.000188	0.299215
1.069070	-1.992559	0.455437	0.000171	0.298974
0.906182	-2.000842	0.460442	0.000202	0.298790
1.079862	-2.078054	0.465446	0.000169	0.298569
1.160644	-2.148089	0.470451	0.000154	0.298301
0.908605	-2.140381	0.475456	0.000201	0.298115
0.863702	-2.167732	0.480461	0.000210	0.297943
0.847163	-2.230235	0.485466	0.000213	0.297624
1.028332	-2.308109	0.490470	0.000179	0.297406
0.807992	-2.309449	0.495475	0.000220	0.297204
0.664988	-2.328939	0.500480	0.000247	0.296982
0.819652	-2.412899	0.505485	0.000218	0.296710
0.573878	-2.415453	0.510490	0.000264	0.296479
0.488847	-2.443350	0.515494	0.000280	0.296267
0.508708	-2.489952	0.520499	0.000276	0.296057
0.247865	-2.507926	0.525504	0.000325	0.295737
0.206449	-2.532413	0.530509	0.000333	0.295580
-0.156140	-2.507801	0.535514	0.000400	0.295378
-0.833891	-2.432030	0.540518	0.000527	0.295145
-1.053412	-2.450225	0.545523	0.000568	0.294860
-1.576221	-2.392692	0.550528	0.000665	0.294676
-2.009087	-2.347623	0.555533	0.000745	0.294511
-1.990863	-2.407614	0.560538	0.000742	0.294232
-2.022874	-2.435612	0.565542	0.000748	0.294065
-2.606047	-2.366012	0.570547	0.000857	0.293886
-2.774036	-2.393663	0.575552	0.000888	0.293599
-2.949940	-2.386600	0.580557	0.000921	0.293476
-3.467611	-2.337353	0.585562	0.001017	0.293255
-3.700583	-2.335486	0.590566	0.001061	0.293055
-3.889916	-2.318429	0.595571	0.001096	0.292969
-4.180469	-2.334401	0.600576	0.001150	0.292628
-4.170268	-2.354819	0.605581	0.001148	0.292536
-4.646574	-2.312766	0.610586	0.001237	0.292316
-4.693438	-2.343073	0.615590	0.001246	0.292123
-5.156836	-2.285564	0.620595	0.001332	0.291991
-5.340036	-2.298999	0.625600	0.001366	0.291759
-5.130943	-2.348058	0.630605	0.001327	0.291704
-5.684329	-2.315649	0.635610	0.001430	0.291365
-5.856291	-2.293324	0.640614	0.001463	0.291321
-6.003646	-2.318041	0.645619	0.001490	0.291064
-6.052235	-2.330830	0.650624	0.001499	0.290957
-6.274319	-2.333505	0.655629	0.001541	0.290742
-6.536745	-2.308989	0.660634	0.001589	0.290627
-6.498352	-2.345547	0.665638	0.001582	0.290479
-6.465123	-2.390217	0.670643	0.001576	0.290286
-7.112804	-2.303424	0.675648	0.001697	0.290132
-6.936077	-2.377382	0.680653	0.001664	0.289923
-7.452870	-2.303859	0.685658	0.001760	0.289821
-7.676483	-2.313277	0.690662	0.001802	0.289570
-7.837790	-2.298032	0.695667	0.001832	0.289500
-8.160844	-2.285401	0.700672	0.001892	0.289269
-8.192560	-2.291117	0.705677	0.001898	0.289212
-8.240059	-2.332822	0.710682	0.001907	0.288959
-8.494365	-2.304261	0.715686	0.001954	0.288871
-8.717532	-2.306157	0.720691	0.001996	0.288658
-9.060590	-2.263078	0.725696	0.002060	0.288561
-8.652182	-2.374960	0.730701	0.001984	0.288372
-9.447817	-2.256577	0.735706	0.002132	0.288240
-9.651243	-2.249380	0.740710	0.002170	0.288090
-9.599011	-2.285756	0.745715	0.002160	0.287954
-9.597161	-2.311796	0.750720	0.002160	0.287825
-10.016290	-2.276879	0.755725	0.002238	0.287617
-10.135446	-2.268698	0.760730	0.002260	0.287549
-10.443673	-2.262905	0.765734	0.002318	0.287296
-10.446951	-2.261066	0.770739	0.002318	0.287302
-10.643402	-2.289425	0.775744	0.002355	0.286979
-10.683434	-2.282554	0.780749	0.002363	0.286977
-11.204827	-2.231139	0.785754	0.002460	0.286758
-11.109107	-2.263200	0.790758	0.002442	0.286683
-10.904036	-2.330699	0.795763	0.002404	0.286531
-11.675091	-2.227299	0.800768	0.002547	0.286344
-11.570061	-2.256596	0.805773	0.002528	0.286293
-11.677512	-2.287798	0.810778	0.002548	0.286036
-11.679921	-2.287418	0.815782	0.002548	0.286035
-12.235386	-2.242956	0.820787	0.002652	0.285749
-12.571220	-2.188448	0.825792	0.002714	0.285716
-12.166342	-2.285595	0.830797	0.002639	0.285596
-12.552383	-2.240990	0.835802	0.002711	0.285466
-12.724811	-2.220451	0.840806	0.002743	0.285411
-12.813498	-2.259008	0.845811	0.002760	0.285134
-12.790564	-2.264826	0.850816	0.002755	0.285125
-13.183248	-2.242421	0.855821	0.002829	0.284876
-13.541752	-2.189280	0.860826	0.002895	0.284815
-13.280232	-2.259826	0.865830	0.002847	0.284697
-13.408915	-2.276792	0.870835	0.002871	0.284492
-13.679620	-2.229634	0.875840	0.002921	0.284481
-13.757328	-2.268854	0.880845	0.002936	0.284210
-14.165360	-2.197147	0.885850	0.003012	0.284197
-14.222328	-2.220510	0.890854	0.003022	0.284025
-14.231129	-2.249907	0.895859	0.003024	0.283866
-14.352211	-2.234318	0.900864	0.003047	0.283833
-14.810370	-2.204583	0.905869	0.003132	0.283560
-14.957940	-2.179002	0.910874	0.003160	0.283553
-14.870399	-2.228321	0.915878	0.003143	0.283383
-15.383387	-2.162251	0.920883	0.003239	0.283243
-15.541103	-2.136420	0.925888	0.003268	0.283229
-15.413606	-2.209367	0.930893	0.003245	0.282974
-15.643468	-2.173615	0.935898	0.003287	0.282943
-15.753877	-2.173817	0.940902	0.003308	0.282839
-15.903026	-2.191126	0.945907	0.003336	0.282611
-16.001684	-2.174773	0.950912	0.003354	0.282603
-16.134555	-2.192629	0.955917	0.003379	0.282387
-16.531992	-2.138715	0.960922	0.003453	0.282293
-16.128900	-2.219669	0.965926	0.003378	0.282254
-16.268415	-2.249904	0.970931	0.003404	0.281968
-16.997233	-2.117981	0.975936	0.003540	0.281965
-16.620867	-2.212769	0.980941	0.003470	0.281829
-17.022798	-2.169883	0.985946	0.003545	0.281674
-17.342993	-2.111393	0.990950	0.003604	0.281675
-17.174961	-2.193374	0.995955	0.003573	0.281411
-17.434726	-2.160031	1.000960	0.003621	0.281339
-17.461172	-2.165119	1.005965	0.003626	0.281288
-17.925313	-2.129204	1.010970	0.003713	0.281038
-17.693396	-2.172137	1.015974	0.003670	0.281034
-17.784885	-2.185133	1.020979	0.003687	0.280881
-18.323023	-2.119078	1.025984	0.003787	0.280717
-17.875540	-2.199516	1.030989	0.003704	0.280721
-18.132996	-2.191588	1.035994	0.003752	0.280521
-18.636204	-2.107269	1.040998	0.003845	0.280483
-18.782144	-2.087031	1.046003	0.003873	0.280451
-18.634123	-2.174140	1.051008	0.003845	0.280139
-18.645560	-2.171029	1.056013	0.003847	0.280145
-19.216706	-2.094297	1.061018	0.003954	0.280004
-19.199850	-2.132096	1.066022	0.003951	0.279824
-18.758004	-2.210951	1.071027	0.003868	0.279832
-19.349142	-2.156209	1.076032	0.003979	0.279559
-19.571286	-2.126779	1.081037	0.004020	0.279502
-19.459701	-2.153721	1.086042	0.003999	0.279467
-19.815799	-2.138780	1.091046	0.004066	0.279209
-19.896581	-2.123025	1.096051	0.004081	0.279214
-19.870424	-2.153325	1.101056	0.004076	0.279081
-19.979818	-2.172416	1.106061	0.004096	0.278879
-20.311129	-2.113197	1.111066	0.004158	0.278873
-20.202353	-2.176208	1.116070	0.004138	0.278648
-20.470934	-2.142646	1.121075	0.004188	0.278569
-20.812629	-2.082948	1.126080	0.004251	0.278556
-20.902961	-2.125031	1.131085	0.004268	0.278251
-20.897601	-2.126834	1.136090	0.004267	0.278247
-20.953503	-2.132930	1.141094	0.004278	0.278162
-21.443733	-2.083235	1.146099	0.004369	0.277957
-21.220135	-2.125819	1.151104	0.004328	0.277946
-20.969694	-2.204942	1.156109	0.004281	0.277771
-21.804471	-2.084362	1.161114	0.004436	0.277608
-21.606228	-2.118988	1.166118	0.004400	0.277615
-21.474892	-2.192030	1.171123	0.004375	0.277359
-22.017412	-2.105538	1.176128	0.004476	0.277295
-21.985258	-2.118451	1.181133	0.004470	0.277258
-21.984622	-2.172108	1.186138	0.004470	0.276978
-22.066394	-2.157924	1.191142	0.004486	0.276974
-22.230409	-2.155006	1.196147	0.004516	0.276833
-22.523304	-2.130555	1.201152	0.004571	0.276682
-22.370573	-2.156124	1.206157	0.004542	0.276694
-22.771425	-2.139027	1.211162	0.004617	0.276401
-22.815950	-2.139575	1.216166	0.004625	0.276356
-22.660453	-2.179013	1.221171	0.004596	0.276297
-23.260303	-2.118184	1.226176	0.004708	0.276044
-23.326977	-2.104596	1.231181	0.004721	0.276051
-23.373587	-2.125254	1.236186	0.004729	0.275898
-23.683669	-2.100432	1.241190	0.004787	0.275732
-23.725649	-2.090927	1.246195	0.004795	0.275742
-23.803322	-2.112117	1.251200	0.004809	0.275556
-23.784110	-2.126631	1.256205	0.004806	0.275498
-23.949851	-2.100246	1.261210	0.004837	0.275478
-24.044770	-2.145667	1.266214	0.004855	0.275148
-23.975307	-2.157163	1.271219	0.004842	0.275154
-24.262294	-2.130754	1.276224	0.004895	0.275018
-24.580984	-2.107420	1.281229	0.004954	0.274836
-24.400075	-2.141129	1.286234	0.004921	0.274831
-24.715838	-2.130461	1.291238	0.004980	0.274585
-24.754735	-2.137239	1.296243	0.004987	0.274511
-25.011877	-2.095480	1.301248	0.005035	0.274485
-25.015810	-2.144207	1.306253	0.005036	0.274224
-25.336892	-2.086635	1.311258	0.005095	0.274219
-25.571217	-2.066916	1.316262	0.005139	0.274098
-25.428020	-2.132487	1.321267	0.005113	0.273889
-25.734981	-2.078843	1.326272	0.005170	0.273877
-25.793093	-2.102942	1.331277	0.005181	0.273693
-26.090864	-2.071810	1.336282	0.005236	0.273571
-25.863228	-2.113576	1.341286	0.005194	0.273569
-26.026149	-2.136943	1.346291	0.005224	0.273288
-26.380637	-2.080387	1.351296	0.005290	0.273246
-25.996227	-2.162336	1.356301	0.005219	0.273182
-26.454760	-2.121159	1.361306	0.005304	0.272958
-26.304112	-2.148820	1.366310	0.005276	0.272957
-26.483578	-2.154956	1.371315	0.005310	0.272751
-27.027654	-2.080488	1.376320	0.005411	0.272620
-26.790594	-2.122082	1.381325	0.005367	0.272628
-27.261915	-2.095030	1.386330	0.005455	0.272316
-27.088970	-2.128691	1.391334	0.005422	0.272304
-27.126378	-2.139945	1.396339	0.005429	0.272208
-27.656572	-2.086908	1.401344	0.005528	0.271977
-27.336044	-2.143679	1.406349	0.005469	0.271985
-27.659531	-2.121226	1.411354	0.005529	0.271791
-28.135431	-2.052774	1.416358	0.005617	0.271694
-27.897491	-2.094944	1.421363	0.005573	0.271700
-28.036593	-2.130795	1.426368	0.005599	0.271374
-28.463525	-2.053950	1.431373	0.005679	0.271369
-28.290581	-2.100482	1.436378	0.005647	0.271288
-28.502237	-2.105429	1.441382	0.005686	0.271056
-28.822793	-2.044613	1.446387	0.005746	0.271069
-28.862285	-2.068688	1.451392	0.005753	0.270902
-28.759333	-2.116009	1.456397	0.005734	0.270749
-28.782651	-2.112992	1.461402	0.005738	0.270742
-29.257965	-2.067824	1.466406	0.005827	0.270521
-29.312653	-2.063321	1.471411	0.005837	0.270492
-29.342899	-2.066219	1.476416	0.005843	0.270447
-29.613407	-2.071820	1.481421	0.005893	0.270153
-29.704645	-2.056993	1.486426	0.005910	0.270143
-29.801196	-2.062782	1.491430	0.005928	0.270018
-29.846444	-2.088808	1.496435	0.005937	0.269834
-30.159839	-2.032609	1.501440	0.005995	0.269829
-30.194302	-2.065514	1.506445	0.006002	0.269619
-30.500589	-2.030408	1.511450	0.006059	0.269508
-30.410461	-2.047957	1.516454	0.006042	0.269501
-30.625480	-2.053649	1.521459	0.006082	0.269260
-30.860339	-2.017955	1.526464	0.006126	0.269222
-30.866340	-2.024210	1.531469	0.006127	0.269183
-31.100282	-2.037115	1.536474	0.006171	0.268884
-30.863278	-2.081147	1.541478	0.006126	0.268879
-31.068429	-2.065747	1.546483	0.006165	0.268760
-31.596097	-2.004729	1.551488	0.006263	0.268572
-31.071517	-2.098793	1.556493	0.006165	0.268579
-31.389663	-2.082803	1.561498	0.006225	0.268353
-31.879178	-2.012937	1.566502	0.006316	0.268249
-31.863006	-2.014174	1.571507	0.006313	0.268258
-31.788920	-2.081800	1.576512	0.006299	0.267965
-31.826999	-2.073405	1.581517	0.006306	0.267973
-32.624182	-1.943078	1.586522	0.006455	0.267894
-32.308516	-2.049676	1.591526	0.006396	0.267627
-32.220520	-2.064453	1.596531	0.006380	0.267634
-32.611469	-2.028595	1.601536	0.006452	0.267443
-32.514312	-2.070663	1.606541	0.006434	0.267310
-32.453421	-2.082770	1.611546	0.006423	0.267305
-33.013969	-2.036628	1.616550	0.006528	0.267002
-32.991120	-2.042336	1.621555	0.006523	0.266993
-33.106489	-2.034529	1.626560	0.006545	0.266921
-33.264418	-2.045157	1.631565	0.006574	0.266708
-33.399316	-2.020988	1.636570	0.006599	0.266705
-33.457336	-2.043447	1.641574	0.006610	0.266526
-33.464189	-2.069829	1.646579	0.006612	0.266375
-33.608490	-2.046511	1.651584	0.006639	0.266359
-33.845831	-2.051895	1.656589	0.006683	0.266095
-33.857048	-2.055560	1.661594	0.006685	0.266064
-33.961507	-2.052837	1.666598	0.006704	0.265975
-34.232410	-2.046413	1.671603	0.006755	0.265741
-34.170716	-2.059730	1.676608	0.006743	0.265730
-34.107877	-2.098831	1.681613	0.006732	0.265579
-34.926115	-1.967352	1.686618	0.006884	0.265484
-34.519185	-2.042364	1.691622	0.006808	0.265478
-34.739619	-2.059997	1.696627	0.006850	0.265163
-35.017308	-2.014159	1.701632	0.006901	0.265137
-35.048233	-2.025001	1.706637	0.006907	0.265047
-35.277348	-2.022946	1.711642	0.006950	0.264830
-35.363110	-2.008571	1.716646	0.006966	0.264823
-35.389572	-2.040814	1.721651	0.006971	0.264620
-35.711528	-2.004889	1.726656	0.007031	0.264496
-35.474563	-2.047210	1.731661	0.006987	0.264500
-36.213185	-1.964434	1.736666	0.007124	0.264217
-35.954795	-2.012857	1.741670	0.007076	0.264209
-35.613975	-2.092173	1.746675	0.007013	0.264114
-36.505254	-1.973751	1.751680	0.007179	0.263874
-36.310263	-2.009303	1.756685	0.007143	0.263873
-36.140127	-2.074989	1.761690	0.007111	0.263682
-36.648993	-2.004251	1.766694	0.007206	0.263562
-36.270031	-2.077011	1.771699	0.007135	0.263541
-36.827245	-2.030799	1.776704	0.007239	0.263237
-36.966624	-2.002533	1.781709	0.007265	0.263253
-36.896514	-2.038223	1.786714	0.007252	0.263127
-37.260779	-2.002631	1.791718	0.007320	0.262958
-37.084119	-2.032939	1.796723	0.007287	0.262968
-37.441851	-2.018949	1.801728	0.007354	0.262686
-37.645687	-1.993604	1.806733	0.007392	0.262621
-37.561524	-2.017307	1.811738	0.007376	0.262574
-37.840085	-2.016204	1.816742	0.007428	0.262301
-37.821048	-2.018426	1.821747	0.007424	0.262307
-37.780399	-2.057547	1.826752	0.007417	0.262132
-38.219219	-2.004652	1.831757	0.007499	0.261983
-38.499395	-1.953808	1.836762	0.007551	0.261982
-38.520695	-1.995713	1.841766	0.007555	0.261728
-38.430021	-2.017744	1.846771	0.007538	0.261697
-38.416983	-2.036769	1.851776	0.007536	0.261605
-38.773814	-2.016262	1.856781	0.007602	0.261359
-38.852511	-2.001214	1.861786	0.007617	0.261363
-38.786938	-2.048592	1.866790	0.007605	0.261166
-39.420586	-1.951762	1.871795	0.007723	0.261063
-39.589742	-1.922730	1.876800	0.007754	0.261054
-39.297663	-2.028623	1.881805	0.007700	0.260760
-39.473684	-2.001207	1.886810	0.007733	0.260735
-39.579451	-1.997146	1.891814	0.007752	0.260650
-39.646921	-2.012272	1.896819	0.007765	0.260498
-39.546937	-2.033353	1.901824	0.007746	0.260481
-39.704287	-2.052182	1.906829	0.007776	0.260217
-40.067663	-1.999442	1.911834	0.007843	0.260142
-39.748812	-2.074453	1.916838	0.007784	0.260047
-39.981249	-2.072178	1.921843	0.007828	0.259824
-40.198289	-2.033767	1.926848	0.007868	0.259818
-40.037463	-2.108113	1.931853	0.007838	0.259566
-40.427095	-2.048925	1.936858	0.007911	0.259501
-40.630780	-2.029473	1.941862	0.007949	0.259402
-40.485239	-2.089229	1.946867	0.007922	0.259216
-40.613179	-2.067706	1.951872	0.007945	0.259206
-41.068481	-2.038203	1.956877	0.008030	0.258908
-41.227983	-2.014961	1.961882	0.008060	0.258875
-41.117599	-2.056228	1.966886	0.008039	0.258756
-41.316627	-2.053783	1.971891	0.008077	0.258567
-41.357558	-2.048255	1.976896	0.008084	0.258556
-41.476708	-2.075652	1.981901	0.008106	0.258281
-41.471088	-2.083991	1.986906	0.008105	0.258240
-41.691771	-2.069680	1.991910	0.008147	0.258094
-42.096089	-2.018630	1.996915	0.008222	0.257968
-42.042635	-2.057797	2.001920	0.008212	0.257802

-42.301798	-2.047375	2.011917	0.008260	0.257595
-42.756419	-2.017070	2.021914	0.008345	0.257300
-42.594011	-2.071630	2.031910	0.008315	0.257159
-43.129503	-2.006109	2.041907	0.008415	0.256979
-43.261077	-2.004383	2.051904	0.008439	0.256853
-43.330436	-2.021026	2.061901	0.008452	0.256687
-43.481807	-1.991414	2.071898	0.008481	0.256699
-43.379230	-2.060521	2.081894	0.008462	0.256413
-43.677959	-2.015694	2.091891	0.008517	0.256359
-43.846917	-1.984686	2.101888	0.008549	0.256360
-43.907455	-1.973487	2.111885	0.008560	0.256361
-43.780680	-2.019789	2.121882	0.008537	0.256229
-43.850167	-2.039100	2.131878	0.008550	0.256048
-44.379522	-1.939603	2.141875	0.008648	0.256065
-44.525295	-1.913281	2.151872	0.008676	0.256064
-44.237841	-1.967592	2.161869	0.008622	0.256052
-44.093708	-1.992736	2.171866	0.008595	0.256057
-43.878557	-1.981127	2.181862	0.008555	0.256344
-43.723630	-2.006450	2.191859	0.008527	0.256359
-43.903549	-1.972756	2.201856	0.008560	0.256364
-44.332614	-1.893447	2.211853	0.008640	0.256371
-44.223546	-1.913244	2.221850	0.008620	0.256371
-43.851268	-1.981814	2.231846	0.008551	0.256366
-43.817303	-1.941379	2.241843	0.008544	0.256628
-43.581259	-1.972510	2.251840	0.008501	0.256694
-43.805544	-1.931011	2.261837	0.008542	0.256698
-43.674349	-1.943458	2.271834	0.008518	0.256762
-42.906512	-2.044267	2.281830	0.008375	0.256981
-42.911411	-2.044695	2.291827	0.008376	0.256973
-43.154238	-1.998529	2.301824	0.008422	0.256984
-43.195605	-1.933573	2.311821	0.008429	0.257307
-43.011639	-1.966277	2.321818	0.008395	0.257310
-42.538745	-2.024502	2.331814	0.008307	0.257466
-42.243173	-2.052297	2.341811	0.008252	0.257612
-42.423897	-2.019256	2.351808	0.008286	0.257612
-42.283663	-1.987309	2.361805	0.008260	0.257935
-41.893289	-2.054536	2.371802	0.008187	0.257956
-42.229297	-1.956385	2.381798	0.008250	0.258163
-42.204967	-1.945475	2.391795	0.008246	0.258249
-41.780989	-1.979378	2.401792	0.008167	0.258490
-41.767783	-1.967921	2.411789	0.008164	0.258568
-41.780224	-1.915697	2.421786	0.008167	0.258847
-41.469037	-1.960556	2.431782	0.008109	0.258912
-40.913688	-2.007914	2.441779	0.008006	0.259212
-40.800866	-2.017535	2.451776	0.007985	0.259272
-40.679199	-2.000145	2.461773	0.007962	0.259492
-40.460647	-2.013938	2.471770	0.007921	0.259637
-40.138744	-2.040101	2.481766	0.007862	0.259817
-39.933768	-2.040581	2.491763	0.007824	0.260022
-39.948538	-2.018254	2.501760	0.007826	0.260131
-39.727593	-1.999936	2.511757	0.007785	0.260456
-39.645161	-1.998096	2.521754	0.007770	0.260549
-39.422843	-2.006801	2.531750	0.007729	0.260725
-38.971580	-2.049084	2.541747	0.007645	0.260945
-38.998344	-2.024776	2.551744	0.007650	0.261053
-38.906860	-1.987863	2.561741	0.007633	0.261349
-38.744443	-1.983286	2.571738	0.007603	0.261538
-39.050180	-1.890721	2.581734	0.007660	0.261742
-38.158135	-2.010179	2.591731	0.007494	0.261978
-38.083089	-1.985377	2.601728	0.007480	0.262190
-37.595307	-2.049551	2.611725	0.007389	0.262325
-37.355219	-2.042553	2.621722	0.007345	0.262604
-37.236145	-2.028186	2.631718	0.007322	0.262803
-37.109866	-2.018905	2.641715	0.007299	0.262980
-37.082498	-1.976658	2.651712	0.007294	0.263239
-36.867463	-1.974989	2.661709	0.007254	0.263463
-36.645715	-1.980155	2.671706	0.007213	0.263656
-36.275139	-2.008092	2.681702	0.007144	0.263872
-35.954316	-2.012336	2.691699	0.007084	0.264168
-35.780033	-2.014190	2.701696	0.007052	0.264332
-35.467183	-2.041591	2.711693	0.006994	0.264493
-35.209655	-2.029609	2.721690	0.006946	0.264814
-35.243942	-1.986350	2.731686	0.006952	0.265016
-34.860632	-2.019746	2.741683	0.006881	0.265214
-34.727595	-1.994357	2.751680	0.006856	0.265484
-34.464885	-2.001611	2.761677	0.006808	0.265705
-34.211681	-2.013671	2.771674	0.006761	0.265890
-33.910269	-2.031050	2.781670	0.006705	0.266093
-33.808645	-1.998197	2.791667	0.006686	0.266372
-33.547873	-1.999087	2.801664	0.006637	0.266624
-33.567634	-1.957615	2.811661	0.006641	0.266829
-33.181443	-1.991369	2.821658	0.006569	0.267027
-32.750926	-2.017955	2.831654	0.006489	0.267307
-32.457711	-2.026300	2.841651	0.006435	0.267550
-32.623299	-1.953728	2.851648	0.006465	0.267779
-32.157597	-1.995607	2.861645	0.006379	0.268010
-31.896081	-1.999163	2.871642	0.006330	0.268247
-31.497393	-2.022850	2.881638	0.006256	0.268510
-31.222019	-2.033869	2.891635	0.006205	0.268720
-31.228991	-1.994794	2.901632	0.006206	0.268924
-30.776364	-2.022091	2.911629	0.006122	0.269219
-30.656357	-2.002540	2.921626	0.006100	0.269441
-30.423634	-2.005184	2.931622	0.006057	0.269654
-30.204607	-2.002719	2.941619	0.006016	0.269881
-30.048767	-1.979826	2.951616	0.005987	0.270155
-29.781966	-1.973694	2.961613	0.005937	0.270447
-29.690340	-1.952750	2.971610	0.005920	0.270648
-29.214573	-2.003657	2.981606	0.005832	0.270838
-29.299646	-1.941433	2.991603	0.005848	0.271088
-28.912508	-1.957226	3.001600	0.005776	0.271379
-29.007375	-1.890305	3.011597	0.005793	0.271643
-28.200252	-1.995980	3.021594	0.005643	0.271862
-28.078668	-1.977265	3.031590	0.005621	0.272079
-27.872022	-1.967777	3.041587	0.005582	0.272329
-27.681524	-1.946135	3.051584	0.005547	0.272627
-27.583799	-1.914416	3.061581	0.005529	0.272889
-27.416958	-1.899708	3.071578	0.005498	0.273128
-26.829683	-1.964372	3.081574	0.005389	0.273351
-26.652821	-1.951834	3.091571	0.005356	0.273587
-26.207612	-1.977042	3.101568	0.005273	0.273882
-25.989845	-1.972724	3.111565	0.005233	0.274113
-25.778741	-1.970115	3.121562	0.005193	0.274329
-25.423179	-1.995474	3.131558	0.005127	0.274536
-25.304030	-1.957685	3.141555	0.005105	0.274849
-24.771431	-2.010427	3.151552	0.005006	0.275081
-24.794691	-1.964320	3.161549	0.005010	0.275301
-24.722985	-1.931437	3.171546	0.004997	0.275542
-24.147760	-1.997254	3.181542	0.004890	0.275745
-23.879759	-1.994659	3.191539	0.004840	0.276014
-23.673397	-1.992171	3.201536	0.004802	0.276223
-23.635911	-1.956988	3.211533	0.004795	0.276443
-23.320133	-1.964470	3.221530	0.004736	0.276704
-23.063277	-1.957418	3.231526	0.004689	0.276985
-22.683863	-1.982863	3.241523	0.004618	0.277212
-22.706756	-1.935044	3.251520	0.004622	0.277439
-22.465204	-1.932208	3.261517	0.004578	0.277683
-22.177637	-1.928961	3.271514	0.004524	0.277971
-21.772907	-1.953176	3.281510	0.004449	0.278228
-21.403609	-1.979740	3.291507	0.004380	0.278439
-21.182598	-1.978278	3.301504	0.004339	0.278655
-20.967272	-1.973609	3.311501	0.004299	0.278882
-20.576025	-1.983003	3.321498	0.004226	0.279202
-20.495940	-1.958814	3.331494	0.004211	0.279402
-20.175728	-1.976033	3.341491	0.004152	0.279614
-19.871014	-1.988854	3.351488	0.004095	0.279834
-19.691838	-1.960809	3.361485	0.004062	0.280147
-19.371637	-1.973117	3.371482	0.004002	0.280384
-19.058859	-1.992871	3.381478	0.003944	0.280575
-18.885075	-1.992491	3.391475	0.003912	0.280740
-18.841422	-1.941397	3.401472	0.003904	0.281043
-18.698766	-1.923141	3.411469	0.003878	0.281270
-18.520687	-1.905949	3.421466	0.003844	0.281525
-18.194452	-1.918255	3.431462	0.003784	0.281766
-17.749646	-1.957647	3.441459	0.003701	0.281979
-17.932926	-1.861318	3.451456	0.003735	0.282302
-17.653552	-1.863027	3.461453	0.003683	0.282553
-17.186453	-1.899282	3.471450	0.003596	0.282802
-17.032931	-1.879041	3.481446	0.003568	0.283048
-16.575356	-1.920570	3.491443	0.003483	0.283260
-16.302924	-1.909803	3.501440	0.003432	0.283568
-16.193653	-1.882895	3.511437	0.003412	0.283806
-15.772392	-1.912310	3.521434	0.003334	0.284046
-15.869864	-1.844978	3.531430	0.003352	0.284298
-15.339720	-1.900826	3.541427	0.003253	0.284504
-14.999052	-1.899903	3.551424	0.003190	0.284823
-14.804726	-1.890973	3.561421	0.003154	0.285048
-14.312999	-1.935615	3.571418	0.003062	0.285274
-14.166721	-1.917771	3.581414	0.003035	0.285499
-13.859357	-1.927338	3.591411	0.002978	0.285734
-13.716203	-1.905148	3.601408	0.002951	0.285977
-13.529166	-1.897226	3.611405	0.002917	0.286189
-13.393853	-1.875838	3.621402	0.002892	0.286421
-13.157221	-1.863416	3.631398	0.002848	0.286701
-12.721659	-1.890809	3.641395	0.002767	0.286962
-12.518426	-1.882430	3.651392	0.002729	0.287190
-12.081390	-1.920301	3.661389	0.002648	0.287399
-11.765506	-1.934638	3.671386	0.002589	0.287615
-11.614090	-1.895503	3.681382	0.002561	0.287950
-11.476300	-1.881001	3.691379	0.002535	0.288148
-11.201886	-1.888580	3.701376	0.002484	0.288360
-10.821829	-1.914230	3.711373	0.002413	0.288578
-10.435828	-1.925627	3.721370	0.002342	0.288872
-10.083807	-1.942507	3.731366	0.002276	0.289108
-9.798775	-1.956786	3.741363	0.002223	0.289295
-9.669514	-1.939683	3.751360	0.002199	0.289498
-9.640604	-1.884587	3.761357	0.002194	0.289799
-9.388248	-1.886285	3.771354	0.002147	0.290019
-9.088359	-1.896109	3.781350	0.002091	0.290242
-8.751173	-1.908281	3.791347	0.002029	0.290486
-8.623923	-1.882905	3.801344	0.002005	0.290727
-8.437507	-1.872827	3.811341	0.001970	0.290945
-8.086798	-1.894578	3.821338	0.001905	0.291154
-8.016559	-1.863029	3.831334	0.001892	0.291374
-7.950988	-1.807431	3.841331	0.001880	0.291708
-7.428672	-1.858482	3.851328	0.001783	0.291926
-7.198994	-1.857509	3.861325	0.001740	0.292137
-7.099973	-1.827698	3.871322	0.001722	0.292373
-7.006064	-1.791965	3.881318	0.001704	0.292634
-7.017985	-1.723475	3.891315	0.001707	0.292961
-6.749114	-1.722435	3.901312	0.001657	0.293208
-6.452299	-1.728778	3.911309	0.001601	0.293442
-6.260693	-1.710807	3.921306	0.001566	0.293702
-5.982653	-1.708929	3.931302	0.001514	0.293960
-5.568168	-1.729596	3.941299	0.001437	0.294228
-5.589763	-1.668143	3.951296	0.001441	0.294511
-5.190115	-1.687108	3.961293	0.001367	0.294774
-5.197082	-1.632397	3.971290	0.001368	0.295036
-5.039394	-1.602366	3.981286	0.001339	0.295323
-4.852672	-1.582177	3.991283	0.001304	0.295588
-4.613742	-1.578059	4.001280	0.001260	0.295820
-4.242939	-1.592335	4.011277	0.001191	0.296079
-4.342972	-1.512548	4.021274	0.001209	0.296380
-4.328246	-1.447641	4.031270	0.001207	0.296709
-3.689156	-1.510641	4.041267	0.001088	0.296968
-3.506651	-1.485689	4.051264	0.001054	0.297251
-3.606545	-1.406577	4.061261	0.001073	0.297547
-3.045230	-1.445054	4.071258	0.000968	0.297855
-2.969573	-1.400584	4.081254	0.000954	0.298137
-2.780620	-1.375325	4.091251	0.000919	0.298426
-3.131519	-1.245965	4.101248	0.000984	0.298744
-2.944183	-1.210987	4.111245	0.000950	0.299077
-2.692941	-1.190800	4.121242	0.000903	0.299395
-2.762492	-1.111518	4.131238	0.000916	0.299717
-2.183968	-1.147407	4.141235	0.000808	0.300051
-2.068220	-1.098129	4.151232	0.000787	0.300389
-1.957780	-1.057328	4.161229	0.000766	0.300682
-1.752613	-1.029965	4.171226	0.000728	0.300992
-1.967580	-0.920654	4.181222	0.000768	0.301329
-1.471889	-0.929555	4.191219	0.000676	0.301719
-1.493228	-0.856176	4.201216	0.000680	0.302051
-1.517271	-0.773859	4.211213	0.000684	0.302424
-1.324291	-0.732556	4.221210	0.000649	0.302789
-1.234970	-0.673428	4.231206	0.000632	0.303148
-1.355067	-0.571443	4.241203	0.000654	0.303530
-1.250150	-0.498558	4.251200	0.000635	0.303968
-0.728475	-0.515396	4.261197	0.000538	0.304338
-0.887922	-0.408094	4.271194	0.000568	0.304710
-0.485813	-0.395585	4.281190	0.000493	0.305116
-0.594236	-0.279711	4.291187	0.000513	0.305571
-0.557399	-0.212125	4.301184	0.000506	0.305922
-0.307809	-0.172238	4.311181	0.000460	0.306325
-0.354447	-0.062727	4.321178	0.000468	0.306801
-0.097664	-0.027241	4.331174	0.000421	0.307188
0.182423	0.017569	4.341171	0.000369	0.307638
0.000000	0.149079	4.351168	0.000403	0.308100

-0.110300	0.441508	4.356173	0.000423	0.309376
0.169843	0.940934	4.361178	0.000371	0.311939
0.512925	1.725338	4.366182	0.000306	0.315842
0.730986	2.813604	4.371187	0.000265	0.320967
0.974088	4.187703	4.376192	0.000219	0.327298
1.609280	5.786792	4.381197	0.000100	0.334791
1.868454	7.750380	4.386202	0.000050	0.343370
2.406260	9.980042	4.391206	-0.000052	0.353040
2.868123	12.524270	4.396211	-0.000139	0.363651
3.520681	15.355545	4.401216	-0.000262	0.375202
4.003269	18.548424	4.406221	-0.000354	0.387645
4.803403	22.015496	4.411226	-0.000506	0.400899
5.347271	25.879584	4.416230	-0.000609	0.414953
6.053382	30.057116	4.421235	-0.000743	0.429701
6.785469	34.575139	4.426240	-0.000883	0.445082
7.740480	39.414508	4.431245	-0.001064	0.461085
8.537347	44.625284	4.436250	-0.001215	0.477590
9.466551	50.164983	4.441254	-0.001392	0.494575
10.868294	55.974083	4.446259	-0.001657	0.511998
11.920903	62.174637	4.451264	-0.001857	0.529745
13.423588	68.631387	4.456269	-0.002141	0.547806
15.114640	75.366459	4.461274	-0.002460	0.566087
16.840581	82.429364	4.466278	-0.002786	0.584622
19.834901	89.551979	4.471283	-0.003348	0.603274
22.445172	97.047486	4.476288	-0.003839	0.622072
29.531881	104.041120	4.481293	-0.005163	0.640992
31.898465	112.179563	4.486298	-0.005609	0.660022
32.704236	120.815879	4.491302	-0.005764	0.678983
33.965513	129.552711	4.496307	-0.006005	0.697804
35.105910	138.489991	4.501312	-0.006223	0.716491
36.837312	147.484461	4.506317	-0.006551	0.735021
38.807253	156.575347	4.511322	-0.006924	0.753361
40.852508	165.778254	4.516326	-0.007311	0.771497
42.791055	175.118618	4.521331	-0.007678	0.789433
43.783687	184.697596	4.526336	-0.007869	0.807095
46.023136	194.140350	4.531341	-0.008292	0.824526
48.338539	203.628797	4.536346	-0.008729	0.841696
50.967661	213.103643	4.541350	-0.009225	0.858591
52.831196	222.743043	4.546355	-0.009578	0.875206
56.186955	232.145146	4.551360	-0.010209	0.891551
57.854496	241.881109	4.556365	-0.010526	0.907659
59.342754	251.608290	4.561370	-0.010809	0.923422
62.142211	261.111479	4.566374	-0.011337	0.938928
63.421308	270.853534	4.571379	-0.011581	0.954138
65.310257	280.451346	4.576384	-0.011939	0.969053
67.007459	290.070229	4.581389	-0.012261	0.983722
70.167631	299.393628	4.586394	-0.012856	0.998116
72.213086	308.870756	4.591398	-0.013243	1.012245
74.925011	318.195077	4.596403	-0.013754	1.026127
76.362387	327.691505	4.601408	-0.014027	1.039753
77.650545	337.178420	4.606413	-0.014273	1.053154
78.683755	346.627552	4.611418	-0.014472	1.066274
80.169900	355.940331	4.616422	-0.014755	1.079157
82.157944	365.113579	4.621427	-0.015131	1.091816
83.742576	374.304577	4.626432	-0.015432	1.104262
85.290537	383.471133	4.631437	-0.015726	1.116528
86.259057	392.663735	4.636442	-0.015912	1.128566
87.838828	401.712963	4.641446	-0.016212	1.140428
89.669245	410.685412	4.646451	-0.016559	1.152124
90.555730	419.741780	4.651456	-0.016730	1.163605
92.100800	428.656566	4.656461	-0.017023	1.174938
92.988686	437.627138	4.661466	-0.017194	1.186093
94.144753	446.503754	4.666470	-0.017415	1.197086
95.554674	455.288707	4.671475	-0.017684	1.207920
96.543174	464.124948	4.676480	-0.017873	1.218633
97.998750	472.848860	4.681485	-0.018150	1.229213
99.561559	481.515863	4.686490	-0.018447	1.239657
100.555817	490.259951	4.691494	-0.018637	1.249991
101.342906	498.994262	4.696499	-0.018790	1.260188
102.733210	507.602081	4.701504	-0.019054	1.270275
104.258554	516.157260	4.706509	-0.019344	1.280248
105.147054	524.798963	4.711514	-0.019515	1.290121
106.735343	533.311801	4.716518	-0.019816	1.299905
107.912827	541.911312	4.721523	-0.020041	1.309635
108.562617	550.561675	4.726528	-0.020167	1.319252
109.958813	559.023985	4.731533	-0.020433	1.328730
111.300240	567.472122	4.736538	-0.020688	1.338115
112.678660	575.901051	4.741542	-0.020950	1.347420
113.651297	584.396383	4.746547	-0.021137	1.356660
115.170866	592.760115	4.751552	-0.021425	1.365794
116.286651	601.236689	4.756557	-0.021638	1.374914
116.932447	609.733296	4.761562	-0.021764	1.383913
118.742639	618.031803	4.766566	-0.022106	1.392849
119.892834	626.434001	4.771571	-0.022326	1.401721
121.174854	634.796581	4.776576	-0.022570	1.410519
122.561633	643.146395	4.781581	-0.022834	1.419266
123.580487	651.554776	4.786586	-0.023029	1.427957
124.606792	659.952688	4.791590	-0.023225	1.436585
125.635814	668.308051	4.796595	-0.023422	1.445120
127.506537	676.535643	4.801600	-0.023776	1.453614
129.633821	684.748078	4.806605	-0.024177	1.462086
130.984878	693.098209	4.811610	-0.024434	1.470517
132.991505	701.333082	4.816614	-0.024813	1.478893
134.602228	709.622971	4.821619	-0.025119	1.487211
135.515686	718.012595	4.826624	-0.025294	1.495468
136.744358	726.347696	4.831629	-0.025528	1.503677
137.251284	734.774648	4.836634	-0.025628	1.511815
138.426992	743.054539	4.841638	-0.025852	1.519874
139.832418	751.301337	4.846643	-0.026119	1.527894
140.720859	759.622944	4.851648	-0.026290	1.535863
141.516131	767.973194	4.856653	-0.026444	1.543803
142.735755	776.224516	4.861658	-0.026676	1.551674
144.200027	784.428991	4.866662	-0.026954	1.559498
145.811420	792.613510	4.871667	-0.027259	1.567286
146.497003	800.951299	4.876672	-0.027393	1.575038
147.840615	809.175404	4.881677	-0.027648	1.582746
149.067984	817.414737	4.886682	-0.027882	1.590412
150.072135	825.689963	4.891686	-0.028074	1.598041
151.372118	833.890563	4.896691	-0.028322	1.605609
152.533655	842.135871	4.901696	-0.028543	1.613161
153.516897	850.408433	4.906701	-0.028732	1.620676
154.465949	858.669824	4.911706	-0.028914	1.628142
155.665587	866.901637	4.916710	-0.029142	1.635582
156.794419	875.097733	4.921715	-0.029358	1.642947
157.796138	883.296826	4.926720	-0.029550	1.650263
158.728972	891.554882	4.931725	-0.029729	1.657589
159.594300	899.773677	4.936730	-0.029895	1.664839
161.178226	907.901205	4.941734	-0.030195	1.672077
162.562225	916.064948	4.946739	-0.030458	1.679287
163.822490	924.228158	4.951744	-0.030698	1.686448
164.932735	932.468688	4.956749	-0.030910	1.693624
166.326843	940.614627	4.961754	-0.031175	1.700728
167.315279	948.843828	4.966758	-0.031364	1.707817
168.373180	957.050725	4.971763	-0.031567	1.714868
169.202525	965.269277	4.976768	-0.031727	1.721869
170.175600	973.478579	4.981773	-0.031913	1.728852
171.396504	981.622784	4.986778	-0.032146	1.735785
171.897237	989.891701	4.991782	-0.032244	1.742700
172.497468	998.127986	4.996787	-0.032361	1.749573
173.563931	1006.276307	5.001792	-0.032565	1.756407
174.562227	1014.442933	5.006797	-0.032756	1.763220
175.449975	1022.603276	5.011802	-0.032927	1.769988
176.119259	1030.826411	5.016806	-0.033057	1.776753
176.993553	1039.002096	5.021811	-0.033225	1.783479
177.555682	1047.225943	5.026816	-0.033335	1.790179
178.910561	1055.318612	5.031821	-0.033592	1.796848
179.610454	1063.479133	5.036826	-0.033728	1.803465
180.547711	1071.629805	5.041830	-0.033908	1.810079
181.644725	1079.766017	5.046835	-0.034117	1.816677
182.502116	1087.905743	5.051840	-0.034282	1.823223
183.756483	1096.025169	5.056845	-0.034521	1.829779
184.212475	1104.251340	5.061850	-0.034611	1.836298
185.409468	1112.325736	5.066854	-0.034839	1.842764
185.905535	1120.569172	5.071859	-0.034937	1.849254
186.493623	1128.741843	5.076864	-0.035052	1.855678
187.195728	1136.906340	5.081869	-0.035188	1.862087
188.272808	1145.007952	5.086874	-0.035394	1.868470
189.074867	1153.136694	5.091878	-0.035548	1.874819
189.896600	1161.269545	5.096883	-0.035706	1.881151
190.720654	1169.371917	5.101888	-0.035865	1.887440
191.464412	1177.556004	5.106893	-0.036009	1.893759
191.861136	1185.742914	5.111898	-0.036088	1.900020
192.866747	1193.836932	5.116902	-0.036281	1.906260
193.622018	1201.976309	5.121907	-0.036426	1.912485
194.464263	1210.083539	5.126912	-0.036588	1.918675
194.734068	1218.297128	5.131917	-0.036644	1.924859
195.220664	1226.451013	5.136922	-0.036740	1.931004
195.884662	1234.586043	5.141926	-0.036869	1.937135
195.893672	1242.812142	5.146931	-0.036876	1.943240
196.540251	1250.912712	5.151936	-0.037001	1.949305
197.773393	1258.917125	5.156941	-0.037236	1.955345
198.946546	1266.927895	5.161946	-0.037460	1.961363
200.536691	1274.921777	5.166950	-0.037761	1.967397
201.696546	1283.037752	5.171955	-0.037982	1.973454
201.953190	1291.254126	5.176960	-0.038035	1.979466
202.828277	1299.371852	5.181965	-0.038204	1.985456
203.450396	1307.525844	5.186970	-0.038325	1.991426
204.113300	1315.659141	5.191974	-0.038453	1.997368
205.213611	1323.706500	5.196979	-0.038663	2.003277
206.095745	1331.805337	5.201984	-0.038833	2.009182
206.980093	1339.949193	5.206989	-0.039003	2.015102
207.715706	1348.053897	5.211994	-0.039145	2.020960
208.467903	1356.199638	5.216998	-0.039290	2.026833
209.010263	1364.371800	5.222003	-0.039397	2.032685
209.823254	1372.434939	5.227008	-0.039553	2.038471
210.604467	1380.546536	5.232013	-0.039704	2.044271
210.968572	1388.704350	5.237018	-0.039777	2.050044
211.690078	1396.790100	5.242022	-0.039917	2.055787
212.202086	1404.940345	5.247027	-0.040017	2.061538
213.337679	1412.948542	5.252032	-0.040234	2.067237
214.266127	1421.063851	5.257037	-0.040412	2.072973
214.828878	1429.196152	5.262042	-0.040522	2.078668
215.420773	1437.280269	5.267046	-0.040637	2.084317
216.391711	1445.366877	5.272051	-0.040823	2.089990
217.040432	1453.465450	5.277056	-0.040949	2.095624
217.798050	1461.585547	5.282061	-0.041096	2.101268
218.268564	1469.715868	5.287066	-0.041189	2.106875
218.923812	1477.854725	5.292070	-0.041316	2.112491
219.765718	1485.912442	5.297075	-0.041478	2.118056
220.231737	1494.005863	5.302080	-0.041570	2.123593
220.999509	1502.095431	5.307085	-0.041718	2.129142
221.734455	1510.177409	5.312090	-0.041860	2.134668
222.128965	1518.319754	5.317094	-0.041939	2.140187
222.779969	1526.406025	5.322099	-0.042065	2.145680
223.621435	1534.469822	5.327104	-0.042227	2.151161
224.663428	1542.513670	5.332109	-0.042426	2.156634
225.268085	1550.608122	5.337114	-0.042544	2.162085
225.912275	1558.713821	5.342118	-0.042669	2.167533
226.700547	1566.814642	5.347123	-0.042821	2.172978
226.851483	1574.959273	5.352128	-0.042855	2.178378
227.702899	1583.017308	5.357133	-0.043019	2.183773
227.814816	1591.224443	5.362138	-0.043045	2.189183
228.475554	1599.265638	5.367142	-0.043173	2.194523
229.415132	1607.269686	5.372147	-0.043353	2.199850
230.235811	1615.295862	5.377152	-0.043511	2.205169
230.834345	1623.421927	5.382157	-0.043628	2.210518
231.250146	1631.540339	5.387162	-0.043710	2.215833
232.108192	1639.593977	5.392166	-0.043875	2.221134
233.169414	1647.652880	5.397171	-0.044078	2.226443
234.398844	1655.655103	5.402176	-0.044312	2.231719
235.346408	1663.739119	5.407181	-0.044494	2.237009
235.928787	1671.847497	5.412186	-0.044608	2.242268
236.540012	1679.963017	5.417190	-0.044727	2.247523
236.870866	1688.122305	5.422195	-0.044794	2.252768
237.500716	1696.193405	5.427200	-0.044916	2.257971
238.290916	1704.259740	5.432205	-0.045068	2.263173
238.641537	1712.400309	5.437210	-0.045139	2.268371
239.716454	1720.438560	5.442214	-0.045344	2.273557
240.612332	1728.476793	5.447219	-0.045516	2.278714
241.481783	1736.490454	5.452224	-0.045683	2.283842
242.240122	1744.587839	5.457229	-0.045830	2.289001
242.799285	1752.704954	5.462234	-0.045939	2.294144
243.213410	1760.793338	5.467238	-0.046022	2.299244
244.193224	1768.817699	5.472243	-0.046209	2.304342
244.755791	1776.920260	5.477248	-0.046319	2.309441
245.574446	1784.985559	5.482253	-0.046477	2.314527
245.921378	1793.094695	5.487258	-0.046547	2.319589
247.125372	1801.073713	5.492262	-0.046776	2.324632
248.383031	1809.117178	5.497267	-0.047015	2.329708
248.715099	1817.266364	5.502272	-0.047082	2.334760
249.558890	1825.335876	5.507277	-0.047245	2.339795
250.416097	1833.382333	5.512282	-0.047410	2.344806
251.300803	1841.468883	5.517286	-0.047580	2.349833
252.038422	1849.550416	5.522291	-0.047722	2.354834
252.834920	1857.591433	5.527296	-0.047876	2.359804
253.381645	1865.684331	5.532301	-0.047983	2.364774
254.038313	1873.765349	5.537306	-0.048110	2.369736
254.748802	1881.843852	5.542310	-0.048248	2.374690
255.457409	1889.928604	5.547315	-0.048385	2.379637
255.785948	1898.015608	5.552320	-0.048451	2.384544
256.338106	1906.113280	5.557325	-0.048559	2.389466
257.007379	1914.163414	5.562330	-0.048689	2.394358
257.671639	1922.238439	5.567334	-0.048818	2.399254
257.987616	1930.314423	5.572339	-0.048882	2.404114
258.275766	1938.436588	5.577344	-0.048941	2.408988
258.666346	1946.537871	5.582349	-0.049019	2.413848
259.452858	1954.550146	5.587354	-0.049171	2.418677
259.961323	1962.608364	5.592358	-0.049270	2.423502
260.598282	1970.684358	5.597363	-0.049394	2.428337
261.223401	1978.759692	5.602368	-0.049516	2.433161
261.445446	1986.861235	5.607373	-0.049562	2.437960
262.412148	1994.814245	5.612378	-0.049748	2.442720
262.905407	2002.905806	5.617382	-0.049845	2.447514
263.551500	2010.969423	5.622387	-0.049970	2.452295
264.153106	2019.018779	5.627392	-0.050087	2.457055
265.300335	2027.010731	5.632397	-0.050306	2.461813
265.906320	2035.081455	5.637402	-0.050424	2.466567
266.655920	2043.153066	5.642406	-0.050569	2.471322
267.107647	2051.261729	5.647411	-0.050658	2.476068
267.369255	2059.339713	5.652416	-0.050712	2.480772
267.871182	2067.395067	5.657421	-0.050811	2.485472
268.403824	2075.476872	5.662426	-0.050915	2.490180
269.043871	2083.531342	5.667430	-0.051040	2.494872
269.312372	2091.638573	5.672435	-0.051095	2.499558
269.651755	2099.673925	5.677440	-0.051163	2.504198
270.155747	2107.790278	5.682445	-0.051262	2.508889
270.673201	2115.825391	5.687450	-0.051364	2.513525
271.485988	2123.815897	5.692454	-0.051521	2.518149
272.381581	2131.823260	5.697459	-0.051692	2.522780
272.866299	2139.907363	5.702464	-0.051788	2.527416
272.929511	2148.074054	5.707469	-0.051805	2.532060
273.420850	2156.092767	5.712474	-0.051902	2.536642
274.093039	2164.118286	5.717478	-0.052032	2.541233
274.671588	2172.175716	5.722483	-0.052145	2.545826
275.018704	2180.262146	5.727488	-0.052215	2.550411
275.462218	2188.344663	5.732493	-0.052303	2.554992
275.946664	2196.379191	5.737498	-0.052398	2.559541
276.360418	2204.408627	5.742502	-0.052480	2.564074
276.927717	2212.491630	5.747507	-0.052591	2.568640
277.414726	2220.542530	5.752512	-0.052687	2.573173
277.554028	2228.646385	5.757517	-0.052718	2.577704
277.718439	2236.694925	5.762522	-0.052754	2.582198
278.235444	2244.745950	5.767526	-0.052855	2.586710
278.668576	2252.875427	5.772531	-0.052941	2.591251
278.763189	2260.992961	5.777536	-0.052964	2.595754
279.538584	2268.947831	5.782541	-0.053114	2.600207
279.838320	2276.963493	5.787546	-0.053175	2.604653
279.685609	2285.084322	5.792550	-0.053152	2.609118
280.312996	2293.095537	5.797555	-0.053274	2.613568
280.892919	2301.082064	5.802560	-0.053387	2.617994
281.124302	2309.165542	5.807565	-0.053435	2.622442
281.204695	2317.258859	5.812570	-0.053455	2.626878
281.960591	2325.253338	5.817574	-0.053601	2.631297
282.157724	2333.346546	5.822579	-0.053643	2.635725
282.458303	2341.368375	5.827584	-0.053704	2.640114
282.981202	2349.389739	5.832589	-0.053807	2.644510
283.635850	2357.411661	5.837594	-0.053934	2.648908
283.891729	2365.502267	5.842598	-0.053987	2.653309
284.466031	2373.538086	5.847603	-0.054099	2.657694
284.859389	2381.564067	5.852608	-0.054177	2.662055
285.348644	2389.646734	5.857613	-0.054274	2.666445
285.590167	2397.729847	5.862618	-0.054324	2.670811
286.147357	2405.766784	5.867622	-0.054433	2.675167
286.604859	2413.804875	5.872627	-0.054523	2.679509
286.854727	2421.831440	5.877632	-0.054575	2.683825
287.444604	2429.885769	5.882637	-0.054690	2.688170
287.944809	2437.931617	5.887642	-0.054788	2.692498
287.854942	2446.046506	5.892646	-0.054777	2.696818
288.575200	2454.050945	5.897651	-0.054916	2.701124
288.977760	2462.089970	5.902656	-0.054996	2.705421
289.187207	2470.190673	5.907661	-0.055040	2.709732
289.190034	2478.266789	5.912666	-0.055046	2.714009
289.462462	2486.314924	5.917670	-0.055102	2.718282
290.055737	2494.304183	5.922675	-0.055218	2.722538
289.976970	2502.383979	5.927680	-0.055208	2.726792
290.639544	2510.409501	5.932685	-0.055337	2.731058
291.273467	2518.409768	5.937690	-0.055460	2.735301
291.245711	2526.511378	5.942694	-0.055460	2.739550
291.454195	2534.565183	5.947699	-0.055504	2.743782
291.719431	2542.617031	5.952704	-0.055559	2.748010
292.159177	2550.705575	5.957709	-0.055646	2.752261
292.569067	2558.731331	5.962714	-0.055727	2.756471
292.515466	2566.814292	5.967718	-0.055723	2.760676
293.051760	2574.810952	5.972723	-0.055828	2.764866
293.433598	2582.812404	5.977728	-0.055904	2.769042
293.417502	2590.943595	5.982733	-0.055906	2.773255
293.771248	2598.947028	5.987738	-0.055977	2.777418
294.453920	2606.904086	5.992742	-0.056109	2.781570
294.615644	2615.024149	5.997747	-0.056145	2.785769
294.876501	2623.047306	6.002752	-0.056199	2.789917
295.268081	2631.087327	6.007757	-0.056277	2.794076
295.665341	2639.113952	6.012762	-0.056356	2.798222
296.011453	2647.165373	6.017766	-0.056425	2.802372
296.190490	2655.248969	6.022771	-0.056464	2.806521
296.125789	2663.329546	6.027776	-0.056457	2.810649
296.384815	2671.382009	6.032781	-0.056511	2.814775
296.877610	2679.374043	6.037786	-0.056608	2.818879
297.350313	2687.380326	6.042790	-0.056701	2.822982
297.784720	2695.444743	6.047795	-0.056787	2.827106
298.155686	2703.476167	6.052800	-0.056861	2.831204
298.555429	2711.519219	6.057805	-0.056941	2.835304
298.888030	2719.531220	6.062810	-0.057008	2.839378
299.178337	2727.553582	6.067814	-0.057067	2.843449
299.860557	2735.594812	6.072819	-0.057199	2.847546
300.029223	2743.677480	6.077824	-0.057236	2.851628
300.362125	2751.753120	6.082829	-0.057303	2.855710
300.505780	2759.811043	6.087834	-0.057335	2.859767
301.143637	2767.780172	6.092838	-0.057459	2.863801
301.386842	2775.876719	6.097843	-0.057510	2.867872
301.664267	2783.896733	6.102848	-0.057566	2.871900
302.270208	2791.927332	6.107853	-0.057684	2.875946
302.400728	2799.988117	6.112858	-0.057714	2.879974
302.754484	2807.988734	6.117862	-0.057785	2.883980
303.078453	2816.079383	6.122867	-0.057850	2.888023
303.134603	2824.145562	6.127872	-0.057866	2.892033
303.598567	2832.186129	6.132877	-0.057958	2.896048
303.671540	2840.258483	6.137882	-0.057977	2.900051
303.760731	2848.285919	6.142886	-0.057998	2.904027
304.160041	2856.340461	6.147891	-0.058078	2.908028
304.547105	2864.398184	6.152896	-0.058155	2.912025
305.081464	2872.408995	6.157901	-0.058260	2.916000
305.171868	2880.433868	6.162906	-0.058282	2.919954
305.492148	2888.418179	6.167910	-0.058347	2.923894
305.905968	2896.473789	6.172915	-0.058429	2.927869
306.439906	2904.469957	6.177920	-0.058533	2.931816
306.834421	2912.547441	6.182925	-0.058612	2.935789
307.376990	2920.547588	6.187930	-0.058718	2.939728
307.481135	2928.591458	6.192934	-0.058743	2.943659
307.541589	2936.700285	6.197939	-0.058759	2.947614
307.856874	2944.711970	6.202944	-0.058823	2.951529
308.179374	2952.772893	6.207949	-0.058889	2.955464
308.314125	2960.814970	6.212954	-0.058919	2.959375
308.594198	2968.834576	6.217958	-0.058976	2.963277
309.173627	2976.835026	6.222963	-0.059089	2.967181
309.787424	2984.807069	6.227968	-0.059209	2.971067
310.198724	2992.893939	6.232973	-0.059291	2.974993
310.645280	3000.938028	6.237978	-0.059379	2.978895
311.024258	3008.948284	6.242982	-0.059455	2.982772
311.600055	3017.013631	6.247987	-0.059567	2.986680
311.359896	3025.118840	6.252992	-0.059528	2.990560
312.070515	3033.115070	6.257997	-0.059665	2.994432
312.514757	3041.124416	6.263002	-0.059753	2.998292
313.585172	3049.101687	6.268006	-0.059957	3.002163
314.509912	3057.119728	6.273011	-0.060135	3.006041
315.070857	3065.154550	6.278016	-0.060244	3.009903
315.578596	3073.233176	6.283021	-0.060344	3.013778
315.936021	3081.285878	6.288026	-0.060416	3.017628
316.335556	3089.313718	6.293030	-0.060496	3.021464
316.855806	3097.358329	6.298035	-0.060598	3.025309
316.709919	3105.438128	6.303040	-0.060576	3.029132
317.199306	3113.498247	6.308045	-0.060672	3.032973
317.418288	3121.539078	6.313050	-0.060718	3.036786
317.572350	3129.580398	6.318054	-0.060752	3.040591
317.866122	3137.608007	6.323059	-0.060812	3.044392
318.199255	3145.617830	6.328064	-0.060879	3.048182
318.389374	3153.686554	6.333069	-0.060920	3.051988
318.651335	3161.746024	6.338074	-0.060974	3.055788
318.859491	3169.751363	6.343078	-0.061017	3.059555
319.130888	3177.809451	6.348083	-0.061073	3.063346
319.075303	3185.875427	6.353088	-0.061068	3.067119
319.425422	3193.942204	6.358093	-0.061138	3.070908
319.582363	3201.984169	6.363098	-0.061173	3.074672
319.642950	3209.980343	6.368102	-0.061189	3.078404
320.239595	3217.964809	6.373107	-0.061306	3.082152
320.519958	3225.976243	6.378112	-0.061363	3.085894
320.793045	3234.015772	6.383117	-0.061419	3.089643
320.825423	3242.099854	6.388122	-0.061430	3.093397
321.080136	3250.119267	6.393126	-0.061483	3.097127
321.414706	3258.159938	6.398131	-0.061550	3.100865
321.634038	3266.130989	6.403136	-0.061596	3.104562
322.318664	3274.188333	6.408141	-0.061729	3.108316
322.460090	3282.246991	6.413146	-0.061761	3.112041
322.645414	3290.278418	6.418150	-0.061800	3.115750
323.113754	3298.281543	6.423155	-0.061893	3.119455
323.340554	3306.296938	6.428160	-0.061940	3.123151
323.295143	3314.390048	6.433165	-0.061937	3.126865
323.553716	3322.429664	6.438170	-0.061990	3.130564
323.819057	3330.444155	6.443174	-0.062045	3.134247
324.230544	3338.470041	6.448179	-0.062127	3.137938
324.521483	3346.476565	6.453184	-0.062186	3.141610
324.759901	3354.555995	6.458189	-0.062236	3.145308
324.997202	3362.595156	6.463194	-0.062285	3.148984
325.156267	3370.636479	6.468198	-0.062320	3.152653
325.527362	3378.660846	6.473203	-0.062394	3.156320
325.564169	3386.699459	6.478208	-0.062406	3.159973
325.885783	3394.691880	6.483213	-0.062471	3.163615
325.908920	3402.758786	6.488218	-0.062481	3.167272
326.209694	3410.807173	6.493222	-0.062542	3.170929
326.710980	3418.835756	6.498227	-0.062640	3.174582
326.697486	3426.844491	6.503232	-0.062643	3.178199
326.859372	3434.895832	6.508237	-0.062678	3.181838
327.349144	3442.890681	6.513242	-0.062775	3.185463
327.545800	3450.940637	6.518246	-0.062817	3.189095
327.755937	3458.993709	6.523251	-0.062861	3.192725
328.056334	3467.000051	6.528256	-0.062922	3.196333
328.192251	3475.060685	6.533261	-0.062953	3.199955
328.319738	3483.044892	6.538266	-0.062981	3.203538
328.490311	3491.084225	6.543270	-0.063018	3.207144
328.833740	3499.146196	6.548275	-0.063088	3.210763
329.024978	3507.187211	6.553280	-0.063128	3.214362
329.335127	3515.191692	6.558285	-0.063191	3.217946
329.605003	3523.242739	6.563290	-0.063247	3.221545
329.798092	3531.241439	6.568294	-0.063288	3.225113
330.394308	3539.281169	6.573299	-0.063404	3.228712
330.760189	3547.313264	6.578304	-0.063477	3.232294
331.216731	3555.348721	6.583309	-0.063568	3.235878
331.333640	3563.361141	6.588314	-0.063595	3.239433
331.584238	3571.358573	6.593318	-0.063646	3.242983
332.079271	3579.399918	6.598323	-0.063744	3.246558
332.190207	3587.434682	6.603328	-0.063770	3.250111
332.461155	3595.508679	6.608333	-0.063825	3.253684
332.664953	3603.553997	6.613338	-0.063868	3.257238
332.978188	3611.552613	6.618342	-0.063932	3.260771
333.097766	3619.580876	6.623347	-0.063959	3.264306
333.180030	3627.618517	6.628352	-0.063980	3.267839
333.597536	3635.661697	6.633357	-0.064063	3.271385
333.836414	3643.676828	6.638362	-0.064112	3.274907
334.242791	3651.666035	6.643366	-0.064193	3.278421
334.669996	3659.699965	6.648371	-0.064278	3.281951
334.877964	3667.721372	6.653376	-0.064322	3.285464
335.179001	3675.769449	6.658381	-0.064383	3.288987
335.698190	3683.817879	6.663386	-0.064485	3.292516
335.843005	3691.866237	6.668390	-0.064517	3.296026
336.088222	3699.919160	6.673395	-0.064568	3.299538
336.397328	3707.892321	6.678400	-0.064631	3.303015
336.659020	3715.953896	6.683405	-0.064685	3.306524
336.692678	3724.023854	6.688410	-0.064696	3.310024
337.159706	3732.004933	6.693414	-0.064788	3.313499
337.759888	3740.019482	6.698419	-0.064905	3.316990
337.783395	3748.077849	6.703424	-0.064915	3.320473
337.922858	3756.068483	6.708429	-0.064946	3.323928
338.271111	3764.122020	6.713434	-0.065016	3.327415
338.671683	3772.167921	6.718438	-0.065096	3.330896
338.945355	3780.197427	6.723443	-0.065152	3.334363
339.279785	3788.203157	6.728448	-0.065219	3.337817
339.692393	3796.253344	6.733453	-0.065301	3.341290
340.026494	3804.248419	6.738458	-0.065369	3.344733
340.035980	3812.300901	6.743462	-0.065376	3.348184
340.391150	3820.361964	6.748467	-0.065447	3.351648
340.760854	3828.364538	6.753472	-0.065521	3.355085
340.902634	3836.374243	6.758477	-0.065553	3.358512
341.215326	3844.430709	6.763482	-0.065616	3.361962
341.445742	3852.423651	6.768486	-0.065664	3.365379
341.777231	3860.468851	6.773491	-0.065731	3.368818
341.951310	3868.517001	6.778496	-0.065769	3.372248
342.136462	3876.590117	6.783501	-0.065808	3.375687
342.269116	3884.557654	6.788506	-0.065838	3.379075
342.387797	3892.587480	6.793510	-0.065866	3.382485
342.903669	3900.648098	6.798515	-0.065967	3.385920
343.104665	3908.655608	6.803520	-0.066009	3.389317
343.530532	3916.712584	6.808525	-0.066094	3.392739
343.735112	3924.781267	6.813530	-0.066137	3.396155
344.009814	3932.741190	6.818534	-0.066194	3.399525
344.216908	3940.757860	6.823539	-0.066237	3.402912
344.255280	3948.790992	6.828544	-0.066250	3.406297
344.663143	3956.797180	6.833549	-0.066331	3.409680
344.939977	3964.858987	6.838554	-0.066388	3.413079
344.859991	3972.920325	6.843558	-0.066378	3.416461
345.293502	3980.904057	6.848563	-0.066464	3.419826
345.774189	3988.874767	6.853568	-0.066558	3.423183
346.093195	3996.946133	6.858573	-0.066623	3.426574
346.459329	4004.980648	6.863578	-0.066696	3.429947
346.713596	4013.007892	6.868582	-0.066749	3.433310
347.072444	4021.028467	6.873587	-0.066821	3.436671
347.237584	4029.033412	6.878592	-0.066857	3.440015
347.568325	4037.082782	6.883597	-0.066924	3.443379
348.019608	4045.093481	6.888602	-0.067013	3.446729
348.234202	4053.108366	6.893606	-0.067058	3.450069
348.796320	4061.152248	6.898611	-0.067168	3.453429
348.988265	4069.185603	6.903616	-0.067209	3.456770
349.237585	4077.204060	6.908621	-0.067260	3.460102
349.752028	4085.216322	6.913626	-0.067361	3.463438
349.933068	4093.289310	6.918630	-0.067400	3.466785
350.137443	4101.326741	6.923635	-0.067444	3.470114
350.476304	4109.331622	6.928640	-0.067512	3.473431
350.891642	4117.365408	6.933645	-0.067594	3.476760
351.126357	4125.364791	6.938650	-0.067643	3.480065
351.334180	4133.375570	6.943654	-0.067687	3.483370
351.973699	4141.401256	6.948659	-0.067811	3.486693
351.747403	4149.475179	6.953664	-0.067774	3.490004
351.870539	4157.534914	6.958669	-0.067803	3.493317
352.428262	4165.487113	6.963674	-0.067912	3.496597
352.807260	4173.529048	6.968678	-0.067987	3.499905
353.238763	4181.525035	6.973683	-0.068073	3.503193
353.257519	4189.608647	6.978688	-0.068082	3.506500
353.695728	4197.642439	6.983693	-0.068168	3.509798
354.011914	4205.666033	6.988698	-0.068232	3.513083
354.364461	4213.675302	6.993702	-0.068303	3.516362
354.740017	4221.712646	6.998707	-0.068378	3.519649
355.207446	4229.631607	7.003712	-0.068470	3.522887
355.645842	4237.731585	7.008717	-0.068557	3.526196
355.891839	4245.771280	7.013722	-0.068608	3.529471
356.313406	4253.784213	7.018726	-0.068692	3.532737
356.542728	4261.865028	7.023731	-0.068740	3.536021
356.773839	4269.861605	7.028736	-0.068788	3.539269
357.147944	4277.871640	7.033741	-0.068863	3.542523
357.534209	4285.888290	7.038746	-0.068940	3.545778
358.089943	4293.884865	7.043750	-0.069049	3.549026
358.268502	4302.022973	7.048755	-0.069087	3.552317
358.741249	4310.009304	7.053760	-0.069180	3.555553
359.334516	4317.956023	7.058765	-0.069296	3.558773
359.451314	4326.007511	7.063770	-0.069323	3.562018
359.636473	4334.026306	7.068774	-0.069363	3.565249
360.020611	4342.074040	7.073779	-0.069439	3.568495
360.064743	4350.093317	7.078784	-0.069453	3.571716
360.241074	4358.201857	7.083789	-0.069491	3.574973
360.939800	4366.137853	7.088794	-0.069626	3.578175
361.222271	4374.153591	7.093798	-0.069684	3.581393
361.873474	4382.134482	7.098803	-0.069810	3.584604
362.063622	4390.187430	7.103808	-0.069851	3.587829
362.537976	4398.253338	7.108813	-0.069944	3.591063
362.974122	4406.255177	7.113818	-0.070031	3.594268
363.095967	4414.294488	7.118822	-0.070059	3.597476
363.554063	4422.327402	7.123827	-0.070149	3.600688
363.739135	4430.303640	7.128832	-0.070189	3.603867
363.905226	4438.396040	7.133837	-0.070225	3.607089
364.403783	4446.381171	7.138842	-0.070323	3.610275
364.457845	4454.415228	7.143846	-0.070338	3.613464
364.855824	4462.475693	7.148851	-0.070417	3.616671
365.115082	4470.454136	7.153856	-0.070471	3.619838
365.695204	4478.466363	7.158861	-0.070584	3.623026
365.735741	4486.599620	7.163866	-0.070597	3.626243
365.943878	4494.565275	7.168870	-0.070641	3.629395
366.609521	4502.597156	7.173875	-0.070770	3.632584
366.951751	4510.612653	7.178880	-0.070839	3.635754
367.149009	4518.602771	7.183885	-0.070881	3.638908
367.626422	4526.595989	7.188890	-0.070975	3.642068
367.949500	4534.604070	7.193894	-0.071040	3.645226
368.219911	4542.659512	7.198899	-0.071096	3.648399
368.343665	4550.737147	7.203904	-0.071124	3.651574
368.707458	4558.766883	7.208909	-0.071197	3.654734
369.046445	4566.758448	7.213914	-0.071265	3.657875
369.312214	4574.762928	7.218918	-0.071320	3.661017
369.630366	4582.778764	7.223923	-0.071384	3.664162
369.785014	4590.816928	7.228928	-0.071418	3.667308
369.771684	4598.891240	7.233933	-0.071421	3.670461
370.010524	4606.924756	7.238938	-0.071471	3.673602
370.116456	4614.944728	7.243942	-0.071496	3.676732
370.521820	4622.953539	7.248947	-0.071576	3.679863
370.796352	4630.924507	7.253952	-0.071632	3.682973
371.486609	4638.937551	7.258957	-0.071766	3.686107
371.497067	4646.989306	7.263962	-0.071773	3.689236
371.825543	4655.004709	7.268966	-0.071840	3.692357
372.490618	4663.056721	7.273971	-0.071969	3.695497
372.590141	4671.066017	7.278976	-0.071992	3.698604
372.719365	4679.122858	7.283981	-0.072022	3.701727
373.140416	4687.125920	7.288986	-0.072105	3.704835
373.333895	4695.140538	7.293990	-0.072146	3.707938
373.638680	4703.240292	7.298995	-0.072208	3.711074
373.659267	4711.287341	7.304000	-0.072218	3.714180
374.138528	4719.231508	7.309005	-0.072312	3.717256
374.371118	4727.261928	7.314010	-0.072360	3.720356
374.672083	4735.225709	7.319014	-0.072422	3.723429
375.011726	4743.313860	7.324019	-0.072490	3.726549
375.339259	4751.299209	7.329024	-0.072556	3.729626
375.473182	4759.330728	7.334029	-0.072586	3.732713
375.981021	4767.396023	7.339034	-0.072686	3.735820
376.416329	4775.337703	7.344038	-0.072772	3.738875
376.405714	4783.437109	7.349043	-0.072776	3.741977
376.681233	4791.410612	7.354048	-0.072832	3.745035
377.091861	4799.442556	7.359053	-0.072914	3.748117
377.345815	4807.506828	7.364058	-0.072966	3.751204
377.742736	4815.480410	7.369062	-0.073045	3.754258
378.120435	4823.504463	7.374067	-0.073121	3.757328
378.301076	4831.519030	7.379072	-0.073160	3.760387
378.486404	4839.504648	7.384077	-0.073199	3.763432
378.824821	4847.606223	7.389082	-0.073267	3.766523
379.233338	4855.582887	7.394086	-0.073349	3.769565
379.422030	4863.625127	7.399091	-0.073389	3.772625
379.601923	4871.651494	7.404096	-0.073428	3.775676
379.944577	4879.643047	7.409101	-0.073497	3.778715
380.219819	4887.695635	7.414106	-0.073553	3.781773
380.473177	4895.667960	7.419110	-0.073605	3.784797
380.871272	4903.717960	7.424115	-0.073685	3.787852
381.103405	4911.781504	7.429120	-0.073733	3.790906
381.136510	4919.807588	7.434125	-0.073745	3.793938
381.420719	4927.843034	7.439130	-0.073803	3.796977
381.887373	4935.803582	7.444134	-0.073895	3.799990
382.136912	4943.849272	7.449139	-0.073946	3.803028
382.214953	4951.888623	7.454144	-0.073966	3.806056
382.421690	4959.880195	7.459149	-0.074010	3.809067
383.035956	4967.927724	7.464154	-0.074129	3.812106
383.209767	4975.917611	7.469158	-0.074167	3.815111
383.601476	4983.973314	7.474163	-0.074245	3.818143
383.650987	4992.050066	7.479168	-0.074259	3.821173
384.008953	4999.963323	7.484173	-0.074331	3.824146
384.162278	5008.065129	7.489178	-0.074365	3.827183
384.641429	5016.055799	7.494182	-0.074459	3.830183
384.916059	5024.088315	7.499187	-0.074516	3.833192
384.855097	5032.171093	7.504192	-0.074510	3.836210
385.260170	5040.120988	7.509197	-0.074590	3.839185
385.563145	5048.154336	7.514202	-0.074652	3.842188
385.488175	5056.159776	7.519206	-0.074643	3.845169
386.019079	5064.184346	7.524211	-0.074747	3.848169
386.182419	5072.299457	7.529216	-0.074783	3.851191
386.733316	5080.210683	7.534221	-0.074890	3.854144
386.984366	5088.258806	7.539226	-0.074942	3.857139
387.478295	5096.226308	7.544230	-0.075039	3.860107
387.921240	5104.291467	7.549235	-0.075127	3.863107
387.949492	5112.341809	7.554240	-0.075138	3.866091
388.362877	5120.334584	7.559245	-0.075220	3.869060
388.692706	5128.457374	7.564250	-0.075286	3.872072
388.995781	5136.507040	7.569254	-0.075348	3.875055
389.314433	5144.447209	7.574259	-0.075412	3.877995
389.411211	5152.477750	7.579264	-0.075436	3.880961
389.651764	5160.365999	7.584269	-0.075486	3.883876
389.924150	5168.463584	7.589274	-0.075542	3.886866
390.227714	5176.425906	7.594278	-0.075603	3.889805
390.591792	5184.509040	7.599283	-0.075676	3.892787
390.682101	5192.538699	7.604288	-0.075698	3.895742
390.971528	5200.482960	7.609293	-0.075757	3.898667
391.381076	5208.576530	7.614298	-0.075839	3.901647
391.402832	5216.514333	7.619302	-0.075848	3.904560
391.789091	5224.585051	7.624307	-0.075925	3.907526
392.028936	5232.600845	7.629312	-0.075975	3.910467
392.175819	5240.679778	7.634317	-0.076007	3.913428
392.412820	5248.707182	7.639322	-0.076057	3.916369
393.037482	5256.628811	7.644326	-0.076178	3.919276
393.274117	5264.671093	7.649331	-0.076227	3.922218
393.281869	5272.680183	7.654336	-0.076234	3.925141
393.756579	5280.711955	7.659341	-0.076328	3.928079
394.055320	5288.779685	7.664346	-0.076388	3.931025
394.162329	5296.806081	7.669350	-0.076414	3.933949
394.255194	5304.883869	7.674355	-0.076436	3.936890
394.766894	5312.849115	7.679360	-0.076537	3.939796
394.985080	5320.863029	7.684365	-0.076582	3.942712
395.057546	5328.923112	7.689370	-0.076601	3.945639
395.302788	5336.908969	7.694374	-0.076652	3.948541
395.455255	5344.994256	7.699379	-0.076685	3.951474
395.528571	5352.991331	7.704384	-0.076704	3.954373
395.837375	5361.005761	7.709389	-0.076767	3.957279
396.142856	5368.989259	7.714394	-0.076829	3.960172
396.320942	5376.970403	7.719398	-0.076867	3.963060
396.564398	5385.039810	7.724403	-0.076918	3.965979
396.776367	5393.033755	7.729408	-0.076963	3.968868
397.514912	5401.037955	7.734413	-0.077105	3.971768
397.064373	5409.175222	7.739418	-0.077027	3.974692
397.526723	5417.107964	7.744422	-0.077118	3.977557
397.825334	5425.160497	7.749427	-0.077179	3.980459
397.694476	5433.130455	7.754432	-0.077159	3.983323
398.173260	5441.166146	7.759437	-0.077254	3.986219
398.631767	5449.186253	7.764442	-0.077344	3.989106
398.567353	5457.237454	7.769446	-0.077338	3.991994
398.800051	5465.236717	7.774451	-0.077386	3.994866
399.180313	5473.209541	7.779456	-0.077462	3.997729
399.536377	5481.246971	7.784461	-0.077533	4.000612
399.792938	5489.225214	7.789466	-0.077586	4.003471
399.883793	5497.300929	7.794470	-0.077609	4.006359
400.591075	5505.277613	7.799475	-0.077745	4.009220
400.501401	5513.367429	7.804480	-0.077734	4.012107
401.216776	5521.284725	7.809485	-0.077872	4.014943
401.159189	5529.383829	7.814490	-0.077867	4.017829
401.270663	5537.399418	7.819494	-0.077893	4.020686
401.737700	5545.407983	7.824499	-0.077985	4.023544
401.896482	5553.477778	7.829504	-0.078020	4.026417
402.201683	5561.458892	7.834509	-0.078082	4.029258
402.628721	5569.570405	7.839514	-0.078166	4.032146
402.436903	5577.561797	7.844518	-0.078136	4.034979
402.954599	5585.557741	7.849523	-0.078237	4.037823
402.881380	5593.571826	7.854528	-0.078229	4.040663
402.915992	5601.541759	7.859533	-0.078240	4.043486
403.148524	5609.640892	7.864538	-0.078289	4.046356
403.575187	5617.537755	7.869542	-0.078374	4.049155
403.844100	5625.646902	7.874547	-0.078429	4.052025
404.204568	5633.616430	7.879552	-0.078501	4.054846
404.645041	5641.624469	7.884557	-0.078588	4.057678
404.823846	5649.692128	7.889562	-0.078627	4.060526
404.809473	5657.682576	7.894566	-0.078629	4.063342
405.277424	5665.751889	7.899571	-0.078722	4.066191
405.355075	5673.745218	7.904576	-0.078741	4.069005
405.569252	5681.796932	7.909581	-0.078786	4.071840
406.017543	5689.801796	7.914586	-0.078875	4.074660
405.896678	5697.828356	7.919590	-0.078858	4.077477
406.153221	5705.849059	7.924595	-0.078911	4.080295
406.416308	5713.819045	7.929600	-0.078965	4.083094
406.843351	5721.861778	7.934605	-0.079050	4.085919
407.092955	5729.911352	7.939610	-0.079101	4.088741
407.224977	5737.894687	7.944614	-0.079131	4.091537
407.422927	5745.941573	7.949619	-0.079173	4.094354
407.727712	5753.966505	7.954624	-0.079235	4.097163
408.013585	5761.968335	7.959629	-0.079293	4.099962
408.405280	5769.967911	7.964634	-0.079371	4.102759
408.521864	5778.005652	7.969638	-0.079398	4.105564
409.006993	5786.032432	7.974643	-0.079494	4.108368
409.106646	5794.094577	7.979648	-0.079518	4.111177
409.213041	5802.064207	7.984653	-0.079543	4.113952
409.219810	5810.144660	7.989658	-0.079549	4.116763
409.318343	5818.062613	7.994662	-0.079573	4.119516
409.652204	5826.141289	7.999667	-0.079640	4.122326
409.913605	5834.121359	8.004672	-0.079694	4.125100
410.005071	5842.142284	8.009677	-0.079716	4.127883
410.184780	5850.221144	8.014682	-0.079755	4.130686
410.627836	5858.135025	8.019686	-0.079842	4.133433
410.454433	5866.284396	8.024691	-0.079815	4.136251
410.491652	5874.265174	8.029696	-0.079827	4.139012
410.589783	5882.283345	8.034701	-0.079851	4.141785
411.523984	5890.158131	8.039706	-0.080030	4.144518
411.490259	5898.243703	8.044710	-0.080029	4.147308
411.739364	5906.293465	8.049715	-0.080080	4.150089
412.191005	5914.276958	8.054720	-0.080170	4.152846
412.542583	5922.308599	8.059725	-0.080240	4.155618
412.746456	5930.317571	8.064730	-0.080283	4.158378
412.771634	5938.392895	8.069734	-0.080293	4.161156
413.186927	5946.289714	8.074739	-0.080376	4.163877
413.388882	5954.434940	8.079744	-0.080419	4.166678
413.791423	5962.382122	8.084749	-0.080499	4.169411
414.300094	5970.449254	8.089754	-0.080599	4.172185
414.387240	5978.439379	8.094758	-0.080620	4.174926
414.702090	5986.538006	8.099763	-0.080684	4.177705
415.110749	5994.541309	8.104768	-0.080765	4.180451
415.241197	6002.525013	8.109773	-0.080795	4.183184
415.653839	6010.528017	8.114778	-0.080877	4.185926
415.813350	6018.546949	8.119782	-0.080911	4.188668
416.329523	6026.655987	8.124787	-0.081013	4.191444
416.386179	6034.697429	8.129792	-0.081029	4.194189
416.418327	6042.697383	8.134797	-0.081040	4.196918
417.014799	6050.679084	8.139802	-0.081156	4.199645
417.103221	6058.649218	8.144806	-0.081178	4.202361
417.586504	6066.641757	8.149811	-0.081273	4.205087
417.651527	6074.725060	8.154816	-0.081290	4.207838
418.116706	6082.710569	8.159821	-0.081382	4.210558
418.276689	6090.766519	8.164826	-0.081417	4.213296
418.425838	6098.811576	8.169830	-0.081450	4.216029
418.773202	6106.759827	8.174835	-0.081520	4.218730
418.842082	6114.864054	8.179840	-0.081538	4.221478
418.756204	6122.812611	8.184845	-0.081527	4.224171
419.455209	6130.841063	8.189850	-0.081662	4.226897
419.419599	6138.836182	8.194854	-0.081661	4.229602
419.748390	6146.888783	8.199859	-0.081727	4.232329
419.941927	6154.909323	8.204864	-0.081768	4.235042
420.028493	6162.900471	8.209869	-0.081790	4.237742
420.400377	6170.916722	8.214874	-0.081864	4.240451
420.516454	6178.874737	8.219878	-0.081891	4.243137
420.955250	6186.965225	8.224883	-0.081978	4.245868
421.072640	6194.907586	8.229888	-0.082005	4.248545
421.344524	6202.998831	8.234893	-0.082061	4.251272
421.306724	6211.065564	8.239898	-0.082059	4.253986
421.369935	6219.037875	8.244902	-0.082076	4.256667
421.670413	6227.036201	8.249907	-0.082137	4.259357
421.999556	6235.063064	8.254912	-0.082203	4.262056
422.153533	6243.053671	8.259917	-0.082237	4.264739
422.548951	6251.097415	8.264922	-0.082316	4.267441
422.595934	6259.155391	8.269926	-0.082330	4.270142
423.064146	6267.104983	8.274931	-0.082422	4.272809
423.096814	6275.210955	8.279936	-0.082434	4.275522
423.344257	6283.114472	8.284941	-0.082485	4.278169
423.835476	6291.167589	8.289946	-0.082581	4.280865
423.908091	6299.140259	8.294950	-0.082600	4.283530
424.164307	6307.231717	8.299955	-0.082653	4.286234
424.232639	6315.208063	8.304960	-0.082671	4.288896
424.393122	6323.256227	8.309965	-0.082706	4.291581
424.721933	6331.295649	8.314970	-0.082772	4.294263
424.834497	6339.314077	8.319974	-0.082799	4.296935
425.348257	6347.244444	8.324979	-0.082899	4.299579
424.986094	6355.349201	8.329984	-0.082837	4.302271
425.349204	6363.319884	8.334989	-0.082910	4.304924
425.784654	6371.370865	8.339994	-0.082996	4.307603
425.914256	6379.356761	8.344998	-0.083025	4.310255
426.000573	6387.419321	8.350003	-0.083047	4.312931
426.147139	6395.416667	8.355008	-0.083079	4.315584
426.423108	6403.411069	8.360013	-0.083136	4.318236
426.959890	6411.395576	8.365018	-0.083241	4.320884
426.793461	6419.371297	8.370022	-0.083215	4.323523
427.213828	6427.487689	8.375027	-0.083299	4.326211
427.471182	6435.433736	8.380032	-0.083352	4.328839
427.416056	6443.540612	8.385037	-0.083347	4.331517
427.837977	6451.489830	8.390042	-0.083430	4.334145
427.798885	6459.566580	8.395046	-0.083428	4.336810
428.181648	6467.513435	8.400051	-0.083505	4.339433
428.380721	6475.569013	8.405056	-0.083547	4.342089
428.499370	6483.548011	8.410061	-0.083574	4.344718
428.736109	6491.643070	8.415066	-0.083623	4.347384
428.772886	6499.592957	8.420070	-0.083635	4.349999
429.458072	6507.669957	8.425075	-0.083768	4.352660
429.771962	6515.691017	8.430080	-0.083832	4.355297
429.217300	6523.726631	8.435085	-0.083734	4.357931
430.127203	6531.687435	8.440090	-0.083908	4.360550
429.994641	6539.665404	8.445094	-0.083889	4.363166
430.072402	6547.672205	8.450099	-0.083908	4.365790
430.158153	6555.701810	8.455104	-0.083930	4.368421
430.647156	6563.714480	8.460109	-0.084026	4.371047
431.188977	6571.733940	8.465114	-0.084132	4.373674
431.022909	6579.816006	8.470118	-0.084106	4.376315
431.733354	6587.772239	8.475123	-0.084244	4.378920
432.202538	6595.766109	8.480128	-0.084336	4.381533
432.073782	6603.756811	8.485133	-0.084317	4.384140
432.433018	6611.890976	8.490138	-0.084390	4.386795
432.754140	6619.851803	8.495142	-0.084454	4.389392
432.781702	6627.942056	8.500147	-0.084465	4.392028
432.872554	6635.943883	8.505152	-0.084487	4.394633
432.856059	6643.971741	8.510157	-0.084489	4.397245
433.628753	6651.942455	8.515162	-0.084638	4.399842
433.593860	6659.957266	8.520166	-0.084637	4.402446
434.041724	6668.009264	8.525171	-0.084725	4.405064
434.463758	6676.031111	8.530176	-0.084809	4.407670
434.352491	6684.084834	8.535181	-0.084794	4.410282
434.743004	6692.100625	8.540186	-0.084872	4.412883
434.921362	6700.116379	8.545190	-0.084910	4.415481
435.116280	6708.116390	8.550195	-0.084951	4.418073
435.183857	6716.181283	8.555200	-0.084969	4.420683
435.165782	6724.196435	8.560205	-0.084971	4.423275
435.630877	6732.220698	8.565210	-0.085063	4.425872
435.978634	6740.146450	8.570215	-0.085133	4.428434
436.461759	6748.243985	8.575219	-0.085228	4.431051
436.171543	6756.331998	8.580224	-0.085179	4.433659
436.386344	6764.340036	8.585229	-0.085224	4.436242
436.529181	6772.294868	8.590234	-0.085256	4.438807
436.586069	6780.314857	8.595239	-0.085272	4.441390
436.970750	6788.215138	8.600243	-0.085348	4.443935
437.196365	6796.337069	8.605248	-0.085396	4.446549
437.442377	6804.305250	8.610253	-0.085447	4.449112
437.233638	6812.422916	8.615258	-0.085413	4.451720
437.482157	6820.333356	8.620263	-0.085464	4.454262
438.160409	6828.370610	8.625267	-0.085596	4.456844
438.601779	6836.347078	8.630272	-0.085683	4.459405
438.357673	6844.419827	8.635277	-0.085643	4.461992
438.620672	6852.429673	8.640282	-0.085697	4.464559
439.331295	6860.440043	8.645287	-0.085835	4.467128
439.547691	6868.456152	8.650291	-0.085880	4.469694
439.254911	6876.543319	8.655296	-0.085831	4.472279
439.550996	6884.486628	8.660301	-0.085891	4.474820
439.945530	6892.580907	8.665306	-0.085970	4.477407
440.044195	6900.536117	8.670311	-0.085993	4.479947
439.539309	6908.654186	8.675315	-0.085905	4.482536
440.146561	6916.557359	8.680320	-0.086023	4.485059
439.869691	6924.574955	8.685325	-0.085976	4.487613
440.808799	6932.559895	8.690330	-0.086156	4.490160
440.774251	6940.640682	8.695335	-0.086155	4.492733
440.670814	6948.658190	8.700339	-0.086141	4.495284
441.055242	6956.660909	8.705344	-0.086218	4.497830
441.266699	6964.621131	8.710349	-0.086262	4.500361
441.861542	6972.641678	8.715354	-0.086378	4.502910
441.988569	6980.652397	8.720359	-0.086407	4.505454
442.018458	6988.766176	8.725363	-0.086418	4.508028
442.162404	6996.748501	8.730368	-0.086450	4.510560
442.257905	7004.769373	8.735373	-0.086473	4.513102
442.413975	7012.820827	8.740378	-0.086507	4.515653
442.918447	7020.717607	8.745383	-0.086606	4.518154
443.071916	7028.778310	8.750387	-0.086640	4.520705
443.507256	7036.651345	8.755392	-0.086726	4.523196
443.616875	7044.755242	8.760397	-0.086752	4.525757
443.681775	7052.836501	8.765402	-0.086769	4.528309
443.943551	7060.836517	8.770407	-0.086823	4.530835
444.458595	7068.856734	8.775411	-0.086924	4.533367
444.498808	7076.954995	8.780416	-0.086937	4.535921
444.673784	7084.874385	8.785421	-0.086974	4.538417
444.873423	7092.932862	8.790426	-0.087017	4.540955
445.007601	7100.876405	8.795431	-0.087047	4.543456
445.088418	7108.945900	8.800435	-0.087067	4.545995
445.743010	7116.886530	8.805440	-0.087194	4.548493
445.930100	7124.952467	8.810445	-0.087234	4.551028
445.819522	7133.034043	8.815450	-0.087219	4.553566
445.902678	7141.004342	8.820455	-0.087240	4.556068
446.058623	7148.986538	8.825459	-0.087274	4.558572
446.488042	7157.054080	8.830464	-0.087359	4.561103
446.679152	7164.929469	8.835469	-0.087400	4.563571
447.520623	7173.055500	8.840474	-0.087562	4.566118
447.236709	7181.064370	8.845479	-0.087514	4.568624
447.391427	7189.112955	8.850483	-0.087548	4.571142
448.042642	7197.060428	8.855488	-0.087674	4.573628
447.899824	7205.161627	8.860493	-0.087653	4.576159
448.398327	7213.101985	8.865498	-0.087751	4.578640
448.424792	7221.161235	8.870503	-0.087761	4.581156
448.380468	7229.146191	8.875507	-0.087758	4.583647
448.719219	7237.234893	8.880512	-0.087826	4.586170
448.856900	7245.180755	8.885517	-0.087857	4.588646
449.519900	7253.249103	8.890522	-0.087986	4.591160
449.653075	7261.194828	8.895527	-0.088016	4.593633
449.995889	7269.260541	8.900531	-0.088085	4.596143
450.000509	7277.243634	8.905536	-0.088091	4.598625
450.044038	7285.263073	8.910541	-0.088104	4.601118
450.433098	7293.259646	8.915546	-0.088182	4.603602
450.667644	7301.255123	8.920551	-0.088230	4.606084
450.806266	7309.276417	8.925555	-0.088261	4.608573
451.066659	7317.372288	8.930560	-0.088315	4.611084
450.980247	7325.360661	8.935565	-0.088304	4.613560
451.150941	7333.440441	8.940570	-0.088341	4.616062
451.670797	7341.328292	8.945575	-0.088443	4.618505
451.581083	7349.451741	8.950579	-0.088432	4.621018
451.973488	7357.375837	8.955584	-0.088510	4.623469
451.670581	7365.482096	8.960589	-0.088459	4.625974
452.171474	7373.473379	8.965594	-0.088557	4.628443
452.392653	7381.470432	8.970599	-0.088603	4.630913
452.724873	7389.403951	8.975603	-0.088670	4.633361
453.172903	7397.498671	8.980608	-0.088759	4.635857
453.352178	7405.447109	8.985613	-0.088798	4.638308
453.557813	7413.543755	8.990618	-0.088841	4.640802
453.332930	7421.483615	8.995623	-0.088804	4.643247
453.603466	7429.570723	9.000627	-0.088860	4.645736
454.029975	7437.541518	9.005632	-0.088945	4.648188
454.373385	7445.586743	9.010637	-0.089014	4.650661
454.903285	7453.583678	9.015642	-0.089118	4.653118
454.944612	7461.588669	9.020647	-0.089130	4.655576
454.914678	7469.638532	9.025651	-0.089130	4.658047
455.036614	7477.681668	9.030656	-0.089158	4.660514
455.132348	7485.621118	9.035661	-0.089181	4.662948
455.417456	7493.706734	9.040666	-0.089239	4.665426
455.479914	7501.721913	9.045671	-0.089256	4.667881
456.047384	7509.703637	9.050675	-0.089367	4.670324
455.789702	7517.793007	9.055680	-0.089324	4.672799
455.857516	7525.775048	9.060685	-0.089342	4.675240
456.203423	7533.825390	9.065690	-0.089411	4.677700
456.564534	7541.828019	9.070695	-0.089484	4.680144
456.343720	7549.817847	9.075699	-0.089448	4.682584
456.639580	7557.810383	9.080704	-0.089508	4.685022
456.906651	7565.794818	9.085709	-0.089563	4.687457
457.535572	7573.809428	9.090714	-0.089685	4.689899
457.821883	7581.805622	9.095719	-0.089744	4.692335
458.354294	7589.804010	9.100723	-0.089848	4.694770
458.518775	7597.892421	9.105728	-0.089884	4.697231
458.661344	7605.863904	9.110733	-0.089916	4.699656
459.188760	7613.942018	9.115738	-0.090019	4.702111
459.215863	7621.863875	9.120743	-0.090029	4.704518
459.390894	7629.946847	9.125747	-0.090067	4.706973
459.403325	7638.018861	9.130752	-0.090075	4.709423
459.604231	7646.014796	9.135757	-0.090117	4.711848
459.726893	7654.000079	9.140762	-0.090145	4.714269
459.535148	7662.068065	9.145767	-0.090115	4.716715
459.818303	7670.037869	9.150771	-0.090173	4.719128
460.337803	7678.072133	9.155776	-0.090274	4.721560
460.629196	7685.933843	9.160781	-0.090334	4.723938
461.023696	7694.067745	9.165786	-0.090413	4.726397
460.804416	7702.068605	9.170791	-0.090377	4.728816
461.310851	7710.152978	9.175795	-0.090476	4.731258
461.400735	7718.132219	9.180800	-0.090498	4.733667
461.766076	7726.153815	9.185805	-0.090572	4.736087
461.768872	7734.239031	9.190810	-0.090577	4.738526
462.067127	7742.220926	9.195815	-0.090638	4.740932
462.236845	7750.160377	9.200819	-0.090675	4.743324
462.473677	7758.236133	9.205824	-0.090724	4.745756
462.666851	7766.225516	9.210829	-0.090765	4.748160
463.080535	7774.297722	9.215834	-0.090847	4.750588
463.060142	7782.316427	9.220839	-0.090849	4.752999
463.235953	7790.326414	9.225843	-0.090887	4.755406
463.616485	7798.289392	9.230848	-0.090963	4.757798
463.686347	7806.314992	9.235853	-0.090981	4.760207
463.745422	7814.353954	9.240858	-0.090997	4.762620
463.875880	7822.342540	9.245863	-0.091027	4.765015
463.907992	7830.360269	9.250867	-0.091038	4.767419
464.662369	7838.369571	9.255872	-0.091183	4.769817
464.740906	7846.416897	9.260877	-0.091203	4.772227
464.487003	7854.474222	9.265882	-0.091161	4.774639
464.928262	7862.437558	9.270887	-0.091248	4.777020
465.059228	7870.445520	9.275891	-0.091278	4.779415
465.060400	7878.515670	9.280896	-0.091283	4.781827
465.421767	7886.325320	9.285901	-0.091356	4.784159
466.059279	7894.535340	9.290906	-0.091480	4.786608
465.719077	7902.533300	9.295911	-0.091422	4.788996
465.957828	7910.584931	9.300915	-0.091471	4.791397
466.323871	7918.540634	9.305920	-0.091545	4.793767
466.587030	7926.534792	9.310925	-0.091599	4.796148
466.907563	7934.544231	9.315930	-0.091664	4.798533
466.953661	7942.607812	9.320935	-0.091677	4.800933
467.555153	7950.525159	9.325939	-0.091794	4.803286
467.621972	7958.611863	9.330944	-0.091812	4.805691
467.491082	7966.628589	9.335949	-0.091793	4.808074
467.632381	7974.723337	9.340954	-0.091824	4.810478
467.736246	7982.704950	9.345959	-0.091849	4.812848
468.165668	7990.142652	9.350963	-0.091934	4.815054
468.511970	7994.891337	9.355968	-0.092001	4.816461

468.697467	7997.573776	9.360973	-0.092038	4.817256
468.756713	7998.902066	9.365978	-0.092049	4.817650
468.922723	7999.232856	9.370983	-0.092080	4.817747
469.049866	8000.279030	9.375987	-0.092105	4.818057
469.314196	8000.303804	9.380992	-0.092154	4.818063
469.517969	8000.189803	9.385997	-0.092192	4.818028
469.651363	8000.228527	9.391002	-0.092217	4.818039
469.836777	8000.195337	9.396007	-0.092251	4.818029
469.986215	8000.231129	9.401011	-0.092279	4.818039
469.903172	8000.265754	9.406016	-0.092263	4.818049
469.779881	8000.242957	9.411021	-0.092240	4.818043
469.959046	8000.303385	9.416026	-0.092274	4.818060
470.060333	8000.263746	9.421031	-0.092293	4.818048
470.386994	8000.234650	9.426035	-0.092353	4.818038
470.387720	8000.243080	9.431040	-0.092353	4.818040
470.201839	8000.258358	9.436045	-0.092319	4.818046
470.126806	8000.309942	9.441050	-0.092305	4.818061
470.390232	8000.233630	9.446055	-0.092354	4.818038
470.718103	8000.232980	9.451059	-0.092415	4.818036
470.674985	8000.268168	9.456064	-0.092407	4.818047
470.825168	8000.240799	9.461069	-0.092435	4.818038
470.798782	8000.270958	9.466074	-0.092430	4.818047
470.667473	8000.233307	9.471079	-0.092405	4.818036
470.923824	8000.262184	9.476083	-0.092453	4.818044
470.950722	8000.263612	9.481088	-0.092458	4.818044
470.871199	8000.265647	9.486093	-0.092443	4.818045
471.154026	8000.260152	9.491098	-0.092496	4.818042
471.198982	8000.281841	9.496103	-0.092504	4.818049
470.889255	8000.291161	9.501107	-0.092446	4.818053
471.286557	8000.244111	9.506112	-0.092520	4.818037
471.105607	8000.242611	9.511117	-0.092486	4.818037
471.388084	8000.277122	9.516122	-0.092539	4.818046
471.372111	8000.266364	9.521127	-0.092536	4.818043
471.499741	8000.230255	9.526131	-0.092560	4.818032
471.601483	8000.225368	9.531136	-0.092578	4.818030
471.329329	8000.263646	9.536141	-0.092528	4.818043
471.441997	8000.310505	9.541146	-0.092549	4.818056
471.764358	8000.207648	9.546151	-0.092609	4.818024
471.803617	8000.225044	9.551155	-0.092616	4.818029
471.969786	8000.301087	9.556160	-0.092647	4.818051
471.780455	8000.268934	9.561165	-0.092612	4.818042
471.677172	8000.278004	9.566170	-0.092592	4.818045
471.404301	8000.356282	9.571175	-0.092542	4.818070
471.637640	8000.327980	9.576179	-0.092585	4.818060
471.957836	8000.274579	9.581184	-0.092644	4.818043
471.829693	8000.290669	9.586189	-0.092621	4.818049
471.544333	8000.359295	9.591194	-0.092567	4.818070
471.875313	8000.338687	9.596199	-0.092629	4.818063
471.916899	8000.335058	9.601203	-0.092637	4.818061
471.999867	8000.289896	9.606208	-0.092652	4.818048
472.099382	8000.292348	9.611213	-0.092671	4.818048
472.313848	8000.326956	9.616218	-0.092710	4.818057
472.252285	8000.242904	9.621223	-0.092699	4.818033
472.327326	8000.276599	9.626227	-0.092713	4.818042
472.302756	8000.312049	9.631232	-0.092708	4.818053
472.232505	8000.284732	9.636237	-0.092695	4.818045
472.478885	8000.288202	9.641242	-0.092741	4.818045
472.319892	8000.285958	9.646247	-0.092711	4.818045
472.480430	8000.264000	9.651251	-0.092741	4.818038
472.467747	8000.331206	9.656256	-0.092739	4.818058
472.726544	8000.245352	9.661261	-0.092787	4.818031
472.430574	8000.381216	9.666266	-0.092732	4.818073
472.233506	8000.328946	9.671271	-0.092695	4.818058
472.511650	8000.299171	9.676275	-0.092747	4.818048
472.637927	8000.305159	9.681280	-0.092770	4.818049
472.644489	8000.248390	9.686285	-0.092771	4.818033
472.588329	8000.297083	9.691290	-0.092761	4.818047
472.113533	8000.401996	9.696295	-0.092673	4.818080
472.199547	8000.429529	9.701299	-0.092689	4.818088
472.114331	8000.411478	9.706304	-0.092673	4.818083
472.473922	8000.315463	9.711309	-0.092739	4.818053
472.627703	8000.397651	9.716314	-0.092768	4.818077
472.673293	8000.387761	9.721319	-0.092777	4.818074
472.690292	8000.327980	9.726323	-0.092780	4.818056
472.703987	8000.418723	9.731328	-0.092782	4.818083
472.345083	8000.376806	9.736333	-0.092715	4.818072
472.310107	8000.391050	9.741338	-0.092709	4.818076
472.262525	8000.369318	9.746343	-0.092700	4.818070
472.344505	8000.396794	9.751347	-0.092715	4.818078
472.279315	8000.450624	9.756352	-0.092703	4.818094
472.457887	8000.411021	9.761357	-0.092736	4.818082
472.654977	8000.380103	9.766362	-0.092773	4.818072
472.195787	8000.427324	9.771367	-0.092687	4.818088
472.088264	8000.435282	9.776371	-0.092667	4.818090
472.110931	8000.477715	9.781376	-0.092671	4.818103
472.141727	8000.398123	9.786381	-0.092677	4.818079
472.121824	8000.447327	9.791386	-0.092673	4.818094
472.369810	8000.396068	9.796391	-0.092719	4.818078
472.159065	8000.419417	9.801395	-0.092680	4.818085
472.220375	8000.453972	9.806400	-0.092692	4.818095
472.439258	8000.424414	9.811405	-0.092732	4.818086
472.845084	8000.441716	9.816410	-0.092808	4.818089
472.826950	8000.389863	9.821415	-0.092804	4.818074
472.655584	8000.389549	9.826419	-0.092772	4.818074
472.368408	8000.498160	9.831424	-0.092719	4.818108
472.830549	8000.354103	9.836429	-0.092805	4.818063
472.476255	8000.447027	9.841434	-0.092739	4.818092
472.269854	8000.471490	9.846439	-0.092700	4.818100
472.759404	8000.370990	9.851443	-0.092791	4.818068
472.770254	8000.376405	9.856448	-0.092793	4.818070
472.728209	8000.329479	9.861453	-0.092786	4.818056
472.726220	8000.485284	9.866458	-0.092785	4.818103
472.793546	8000.417788	9.871463	-0.092798	4.818082
472.586607	8000.386437	9.876467	-0.092759	4.818074
472.673231	8000.464520	9.881472	-0.092775	4.818097
472.561148	8000.442930	9.886477	-0.092754	4.818091
472.785346	8000.451354	9.891482	-0.092796	4.818092
472.555355	8000.449160	9.896487	-0.092753	4.818093
472.449067	8000.448711	9.901491	-0.092733	4.818093
472.547938	8000.500643	9.906496	-0.092752	4.818108
472.580217	8000.446342	9.911501	-0.092758	4.818092
472.618750	8000.446882	9.916506	-0.092765	4.818092
472.023114	8000.405839	9.921511	-0.092654	4.818082
472.442686	8000.478087	9.926515	-0.092732	4.818102
472.876028	8000.508413	9.931520	-0.092813	4.818109
472.698859	8000.459581	9.936525	-0.092779	4.818095
472.497837	8000.504125	9.941530	-0.092742	4.818109
472.606090	8000.420360	9.946535	-0.092762	4.818084
472.628539	8000.390138	9.951539	-0.092766	4.818075
472.732763	8000.469523	9.956544	-0.092786	4.818098
473.094065	8000.393538	9.961549	-0.092853	4.818074
473.487439	8000.375919	9.966554	-0.092926	4.818067
472.988142	8000.429944	9.971559	-0.092833	4.818085
472.923248	8000.489044	9.976563	-0.092821	4.818103
473.023555	8000.459920	9.981568	-0.092840	4.818094
473.012363	8000.415534	9.986573	-0.092837	4.818081
472.851741	8000.534355	9.991578	-0.092808	4.818117
473.148131	8000.471144	9.996583	-0.092863	4.818097
473.368008	8000.486878	10.001587	-0.092904	4.818100
473.528460	8000.474397	10.006592	-0.092933	4.818096
473.072282	8000.364769	10.011597	-0.092848	4.818065
473.189797	8000.389588	10.016602	-0.092870	4.818072
472.968039	8000.460163	10.021607	-0.092829	4.818094
472.747916	8000.438102	10.026611	-0.092788	4.818088
472.985795	8000.475149	10.031616	-0.092832	4.818098
473.168704	8000.424025	10.036621	-0.092866	4.818083
473.090885	8000.448195	10.041626	-0.092852	4.818090
473.036572	8000.448478	10.046631	-0.092841	4.818090
473.153617	8000.457497	10.051635	-0.092863	4.818093
473.018521	8000.484017	10.056640	-0.092838	4.818101
473.109806	8000.472666	10.061645	-0.092855	4.818097
473.292917	8000.483670	10.066650	-0.092889	4.818100
472.972967	8000.374911	10.071655	-0.092829	4.818069
472.942693	8000.542953	10.076659	-0.092824	4.818119
473.181534	8000.529472	10.081664	-0.092868	4.818114
472.850241	8000.487942	10.086669	-0.092806	4.818103
473.030994	8000.424152	10.091674	-0.092840	4.818083
472.629916	8000.530104	10.096679	-0.092765	4.818116
473.050090	8000.460215	10.101683	-0.092843	4.818094
473.191470	8000.417982	10.106688	-0.092870	4.818081
473.549555	8000.377753	10.111693	-0.092936	4.818067
473.376443	8000.472180	10.116698	-0.092904	4.818096
473.278537	8000.517126	10.121703	-0.092886	4.818110
473.296332	8000.439454	10.126707	-0.092889	4.818087
473.215970	8000.486754	10.131712	-0.092874	4.818101
473.517128	8000.363591	10.136717	-0.092930	4.818063
473.751977	8000.353212	10.141722	-0.092974	4.818059
473.556883	8000.395734	10.146727	-0.092937	4.818073
473.716080	8000.427460	10.151731	-0.092967	4.818081
473.703977	8000.478881	10.156736	-0.092965	4.818097
473.485456	8000.463159	10.161741	-0.092924	4.818093
473.453806	8000.395319	10.166746	-0.092918	4.818073
473.464589	8000.479706	10.171751	-0.092920	4.818098
473.625371	8000.388257	10.176755	-0.092950	4.818070
473.664220	8000.433026	10.181760	-0.092957	4.818083
473.330525	8000.478857	10.186765	-0.092895	4.818098
473.367677	8000.484643	10.191770	-0.092902	4.818100
473.214751	8000.500382	10.196775	-0.092873	4.818105
473.186933	8000.475769	10.201779	-0.092868	4.818098
473.756801	8000.481700	10.206784	-0.092974	4.818097
473.900418	8000.354207	10.211789	-0.093001	4.818059
474.155100	8000.395705	10.216794	-0.093048	4.818070
473.935530	8000.425246	10.221799	-0.093007	4.818080
474.011239	8000.403145	10.226803	-0.093021	4.818073
474.006323	8000.436768	10.231808	-0.093020	4.818083
473.936741	8000.368392	10.236813	-0.093007	4.818063
474.389718	8000.312655	10.241818	-0.093092	4.818044
474.360359	8000.309079	10.246823	-0.093086	4.818044
474.492281	8000.319361	10.251827	-0.093111	4.818046
474.509053	8000.369085	10.256832	-0.093114	4.818061
474.042641	8000.354075	10.261837	-0.093027	4.818058
474.568626	8000.367813	10.266842	-0.093125	4.818060
474.349666	8000.402627	10.271847	-0.093084	4.818071
474.228681	8000.394598	10.276851	-0.093061	4.818069
474.529124	8000.400941	10.281856	-0.093117	4.818070
474.440467	8000.348090	10.286861	-0.093101	4.818055
474.659481	8000.325906	10.291866	-0.093141	4.818047
474.452444	8000.352465	10.296871	-0.093103	4.818056
474.553747	8000.338096	10.301875	-0.093122	4.818051
474.613426	8000.434757	10.306880	-0.093133	4.818080
474.625639	8000.380171	10.311885	-0.093135	4.818064
474.763382	8000.373688	10.316890	-0.093161	4.818061
474.943790	8000.363595	10.321895	-0.093194	4.818057
474.607148	8000.368317	10.326899	-0.093131	4.818060
474.371873	8000.453444	10.331904	-0.093088	4.818086
474.095682	8000.447437	10.336909	-0.093036	4.818086
474.539557	8000.447381	10.341914	-0.093119	4.818084
474.437223	8000.424873	10.346919	-0.093100	4.818078
474.034588	8000.451830	10.351923	-0.093025	4.818087
474.133203	8000.412152	10.356928	-0.093043	4.818075
474.107110	8000.448635	10.361933	-0.093038	4.818086
474.105202	8000.461240	10.366938	-0.093038	4.818090
473.988669	8000.423791	10.371943	-0.093016	4.818079
474.191681	8000.422441	10.376947	-0.093054	4.818078
474.561597	8000.400281	10.381952	-0.093122	4.818070
474.365085	8000.383815	10.386957	-0.093086	4.818066
474.521064	8000.421815	10.391962	-0.093115	4.818076
474.382599	8000.423016	10.396967	-0.093089	4.818077
474.545918	8000.414788	10.401971	-0.093119	4.818074
474.264091	8000.477145	10.406976	-0.093067	4.818094
474.199058	8000.470959	10.411981	-0.093055	4.818092
474.246436	8000.504267	10.416986	-0.093064	4.818102
474.211038	8000.459539	10.421991	-0.093057	4.818089
474.168580	8000.455777	10.426995	-0.093049	4.818088
474.343902	8000.446666	10.432000	-0.093081	4.818084
474.248575	8000.383191	10.437005	-0.093064	4.818066
474.162183	8000.401975	10.442010	-0.093048	4.818072
474.331853	8000.450698	10.447015	-0.093079	4.818086
473.798109	8000.481069	10.452019	-0.092980	4.818097
473.871619	8000.503163	10.457024	-0.092993	4.818103
474.100884	8000.486389	10.462029	-0.093036	4.818097
474.438810	8000.472201	10.467034	-0.093099	4.818092
474.274259	8000.456186	10.472039	-0.093068	4.818088
474.166436	8000.385165	10.477043	-0.093048	4.818067
474.096467	8000.516850	10.482048	-0.093035	4.818106
474.269218	8000.448735	10.487053	-0.093067	4.818085
474.235358	8000.533545	10.492058	-0.093061	4.818111
474.015633	8000.397765	10.497063	-0.093020	4.818071
474.283284	8000.386797	10.502067	-0.093070	4.818067
474.260700	8000.543370	10.507072	-0.093065	4.818113
473.822956	8000.421361	10.512077	-0.092984	4.818079
473.764681	8000.445807	10.517082	-0.092973	4.818087
473.926229	8000.419653	10.522087	-0.093003	4.818078
474.081993	8000.474496	10.527091	-0.093032	4.818094
474.295005	8000.490136	10.532096	-0.093072	4.818098
473.972716	8000.510855	10.537101	-0.093012	4.818105
473.932710	8000.450267	10.542106	-0.093004	4.818087
474.362754	8000.450015	10.547111	-0.093084	4.818085
474.443323	8000.416401	10.552115	-0.093099	4.818075
474.714800	8000.434971	10.557120	-0.093149	4.818079
474.631116	8000.368501	10.562125	-0.093134	4.818060
474.561110	8000.421212	10.567130	-0.093121	4.818076
474.066214	8000.475297	10.572135	-0.093029	4.818094
474.428577	8000.440395	10.577139	-0.093096	4.818082
474.845320	8000.452593	10.582144	-0.093174	4.818084
474.479106	8000.463214	10.587149	-0.093105	4.818089
474.918233	8000.412548	10.592154	-0.093187	4.818072
474.513457	8000.512130	10.597159	-0.093112	4.818103
474.807394	8000.416242	10.602163	-0.093166	4.818073
475.135716	8000.391390	10.607168	-0.093227	4.818065
474.942932	8000.312849	10.612173	-0.093191	4.818042
474.666820	8000.374234	10.617178	-0.093140	4.818062
475.137113	8000.311372	10.622183	-0.093227	4.818041
474.912149	8000.325041	10.627187	-0.093186	4.818046
475.215010	8000.344055	10.632192	-0.093242	4.818050
474.858899	8000.327442	10.637197	-0.093176	4.818047
474.922688	8000.387307	10.642202	-0.093187	4.818064
474.762787	8000.405053	10.647207	-0.093158	4.818070
474.530262	8000.393344	10.652211	-0.093114	4.818068
474.886173	8000.435219	10.657216	-0.093181	4.818079
475.004792	8000.338962	10.662221	-0.093202	4.818050
475.315214	8000.368613	10.667226	-0.093260	4.818057
475.154443	8000.365287	10.672231	-0.093230	4.818057
475.296682	8000.362027	10.677235	-0.093257	4.818055
475.045037	8000.423757	10.682240	-0.093210	4.818075
474.985628	8000.382901	10.687245	-0.093199	4.818063
474.965083	8000.465794	10.692250	-0.093195	4.818088
475.066657	8000.404045	10.697255	-0.093214	4.818069
474.983490	8000.354430	10.702259	-0.093198	4.818054
475.228289	8000.390525	10.707264	-0.093244	4.818064
475.192421	8000.375274	10.712269	-0.093237	4.818060
475.014039	8000.448568	10.717274	-0.093204	4.818082
474.926872	8000.478924	10.722279	-0.093188	4.818092
474.999007	8000.474674	10.727283	-0.093201	4.818090
475.268208	8000.470048	10.732288	-0.093251	4.818088
475.239170	8000.389606	10.737293	-0.093246	4.818064
475.296048	8000.388300	10.742298	-0.093256	4.818063
475.104417	8000.444559	10.747303	-0.093220	4.818081
475.266751	8000.418417	10.752307	-0.093251	4.818072
475.248937	8000.484502	10.757312	-0.093247	4.818092
475.576095	8000.313266	10.762317	-0.093308	4.818040
475.681004	8000.316850	10.767322	-0.093327	4.818040
475.768397	8000.309656	10.772327	-0.093344	4.818038
476.003501	8000.316132	10.777331	-0.093387	4.818039
475.807112	8000.429187	10.782336	-0.093351	4.818073
475.457647	8000.340008	10.787341	-0.093286	4.818048
475.353062	8000.346952	10.792346	-0.093266	4.818051
475.802903	8000.363831	10.797351	-0.093350	4.818054
475.479176	8000.361362	10.802355	-0.093290	4.818054
475.589666	8000.401881	10.807360	-0.093310	4.818066
475.359466	8000.399680	10.812365	-0.093267	4.818066
475.790378	8000.345740	10.817370	-0.093347	4.818049
475.569697	8000.393165	10.822375	-0.093306	4.818064
475.948904	8000.336389	10.827379	-0.093377	4.818045
475.981590	8000.390551	10.832384	-0.093383	4.818061
475.117752	8000.479438	10.837389	-0.093222	4.818091
475.371104	8000.347174	10.842394	-0.093269	4.818051
475.784559	8000.385652	10.847399	-0.093346	4.818060
475.554190	8000.386608	10.852403	-0.093303	4.818062
475.365338	8000.487133	10.857408	-0.093268	4.818092
475.670204	8000.412459	10.862413	-0.093325	4.818069
475.469254	8000.466481	10.867418	-0.093287	4.818086
475.323334	8000.486530	10.872423	-0.093260	4.818092
475.351607	8000.454283	10.877427	-0.093265	4.818083
475.497549	8000.425803	10.882432	-0.093292	4.818073
475.308167	8000.423125	10.887437	-0.093257	4.818073
475.461378	8000.338939	10.892442	-0.093286	4.818048
475.737287	8000.438656	10.897447	-0.093337	4.818076
475.742489	8000.366068	10.902451	-0.093338	4.818055
475.603471	8000.390427	10.907456	-0.093312	4.818063
475.581431	8000.361681	10.912461	-0.093308	4.818054
475.531700	8000.399937	10.917466	-0.093298	4.818066
475.593407	8000.426077	10.922471	-0.093310	4.818073
475.486513	8000.434042	10.927475	-0.093290	4.818076
475.522148	8000.498776	10.932480	-0.093297	4.818095
475.417007	8000.469909	10.937485	-0.093277	4.818087
474.988506	8000.521770	10.942490	-0.093197	4.818104
475.184495	8000.416075	10.947495	-0.093234	4.818072
475.432347	8000.448002	10.952499	-0.093280	4.818080
475.587607	8000.527062	10.957504	-0.093309	4.818103
475.674762	8000.483010	10.962509	-0.093325	4.818090
475.340240	8000.390882	10.967514	-0.093262	4.818064
475.542084	8000.439009	10.972519	-0.093300	4.818077
475.394059	8000.431650	10.977523	-0.093272	4.818076
475.503699	8000.460574	10.982528	-0.093293	4.818084
475.033885	8000.504480	10.987533	-0.093205	4.818099
475.621032	8000.439058	10.992538	-0.093314	4.818077
475.888917	8000.466005	10.997543	-0.093364	4.818084
475.770890	8000.421160	11.002547	-0.093342	4.818071
475.655020	8000.478490	11.007552	-0.093321	4.818088
475.539861	8000.392619	11.012557	-0.093299	4.818064
475.626854	8000.529683	11.017562	-0.093315	4.818104
475.765515	8000.455821	11.022567	-0.093341	4.818081
475.311676	8000.336737	11.027571	-0.093256	4.818048
475.716656	8000.476185	11.032576	-0.093332	4.818088
475.892255	8000.417586	11.037581	-0.093365	4.818069
475.597809	8000.492401	11.042586	-0.093310	4.818093
475.157843	8000.451435	11.047591	-0.093228	4.818083
475.249508	8000.466415	11.052595	-0.093245	4.818087
475.281698	8000.482662	11.057600	-0.093251	4.818091
475.134204	8000.458462	11.062605	-0.093223	4.818085
475.357962	8000.487944	11.067610	-0.093265	4.818093
474.946851	8000.331557	11.072615	-0.093188	4.818048
474.676697	8000.397238	11.077619	-0.093138	4.818068
475.139014	8000.382701	11.082624	-0.093224	4.818062
475.368361	8000.447010	11.087629	-0.093267	4.818080
474.830758	8000.247772	11.092634	-0.093166	4.818024
474.740399	8000.337050	11.097639	-0.093149	4.818050
475.118908	8000.464538	11.102643	-0.093220	4.818087
475.015629	8000.412533	11.107648	-0.093201	4.818072
475.196528	8000.426666	11.112653	-0.093234	4.818075
475.485930	8000.473923	11.117658	-0.093288	4.818088
475.760220	8000.407242	11.122663	-0.093339	4.818067
475.509086	8000.487933	11.127667	-0.093292	4.818092
475.530440	8000.560890	11.132672	-0.093296	4.818113
475.303129	8000.347074	11.137677	-0.093254	4.818051
476.000339	8000.452741	11.142682	-0.093384	4.818079
476.244848	8000.466722	11.147687	-0.093429	4.818083
476.326430	8000.547902	11.152691	-0.093444	4.818106
476.311371	8000.336026	11.157696	-0.093441	4.818044
476.814630	8000.525309	11.162701	-0.093535	4.818098
476.995542	8000.430982	11.167706	-0.093569	4.818069
476.939561	8000.533387	11.172711	-0.093558	4.818099
476.830492	8000.533948	11.177715	-0.093538	4.818100
476.666213	8000.379985	11.182720	-0.093507	4.818055
477.120276	8000.463270	11.187725	-0.093592	4.818078
476.856513	8000.439532	11.192730	-0.093543	4.818072
476.988696	8000.524587	11.197735	-0.093567	4.818097
477.203852	8000.437062	11.202739	-0.093607	4.818070
476.919791	8000.448840	11.207744	-0.093554	4.818074
476.688456	8000.441356	11.212749	-0.093511	4.818073
477.346076	8000.361137	11.217754	-0.093634	4.818047
477.048127	8000.359029	11.222759	-0.093578	4.818047
477.138040	8000.515095	11.227763	-0.093595	4.818093
477.124368	8000.565445	11.232768	-0.093592	4.818108
476.793525	8000.395437	11.237773	-0.093531	4.818059
477.030310	8000.355605	11.242778	-0.093575	4.818046
477.646752	8000.483310	11.247783	-0.093689	4.818082
477.797508	8000.411723	11.252787	-0.093717	4.818060
477.641877	8000.496924	11.257792	-0.093688	4.818086
477.213157	8000.461375	11.262797	-0.093609	4.818077
477.506784	8000.513963	11.267802	-0.093663	4.818091
477.235844	8000.444840	11.272807	-0.093613	4.818072
476.831226	8000.484399	11.277811	-0.093537	4.818085
477.254913	8000.533560	11.282816	-0.093616	4.818098
477.693948	8000.434457	11.287821	-0.093698	4.818067
477.444776	8000.403551	11.292826	-0.093651	4.818059
477.197263	8000.542213	11.297831	-0.093605	4.818101
477.145073	8000.444590	11.302835	-0.093596	4.818072
477.716879	8000.495846	11.307840	-0.093702	4.818085
477.795935	8000.430617	11.312845	-0.093717	4.818065
477.322928	8000.473421	11.317850	-0.093629	4.818080
477.273384	8000.443232	11.322855	-0.093619	4.818071
477.543043	8000.472313	11.327859	-0.093669	4.818079
477.366566	8000.555114	11.332864	-0.093637	4.818104
477.492414	8000.429469	11.337869	-0.093660	4.818066
477.994036	8000.457618	11.342874	-0.093753	4.818073
477.781338	8000.499890	11.347879	-0.093714	4.818086
477.783159	8000.465161	11.352883	-0.093714	4.818076
478.069026	8000.414440	11.357888	-0.093767	4.818059
478.121165	8000.404643	11.362893	-0.093777	4.818056
478.054319	8000.422650	11.367898	-0.093764	4.818062
478.081814	8000.403027	11.372903	-0.093769	4.818056
478.171064	8000.464311	11.377907	-0.093786	4.818074
477.903467	8000.502647	11.382912	-0.093736	4.818086
477.711764	8000.474659	11.387917	-0.093700	4.818079
477.863160	8000.474690	11.392922	-0.093728	4.818078
477.754201	8000.428918	11.397927	-0.093708	4.818065
477.810022	8000.400218	11.402931	-0.093718	4.818056
477.566421	8000.544200	11.407936	-0.093673	4.818100
477.706437	8000.487204	11.412941	-0.093699	4.818083
477.987009	8000.452204	11.417946	-0.093751	4.818071
478.203424	8000.334157	11.422951	-0.093791	4.818035
478.148128	8000.495546	11.427955	-0.093781	4.818083
478.130798	8000.513200	11.432960	-0.093778	4.818088
478.041945	8000.441384	11.437965	-0.093761	4.818068
478.122992	8000.450951	11.442970	-0.093776	4.818070
478.153438	8000.456644	11.447975	-0.093782	4.818072
477.986633	8000.440592	11.452979	-0.093751	4.818068
478.430875	8000.440552	11.457984	-0.093834	4.818066
478.386370	8000.437813	11.462989	-0.093825	4.818065
478.179435	8000.465423	11.467994	-0.093787	4.818074
478.135859	8000.421627	11.472999	-0.093779	4.818061
478.321959	8000.416884	11.478003	-0.093813	4.818059
478.509930	8000.476406	11.483008	-0.093848	4.818076
478.137487	8000.470082	11.488013	-0.093779	4.818076
478.220149	8000.437549	11.493018	-0.093794	4.818066
478.581418	8000.445814	11.498023	-0.093861	4.818067
478.551615	8000.404319	11.503027	-0.093856	4.818054
478.608775	8000.441982	11.508032	-0.093866	4.818065
478.551962	8000.377990	11.513037	-0.093856	4.818047
478.588658	8000.394302	11.518042	-0.093862	4.818051
478.907878	8000.350371	11.523047	-0.093922	4.818037
478.772705	8000.353722	11.528051	-0.093897	4.818039
478.693033	8000.413671	11.533056	-0.093882	4.818057
478.509517	8000.381586	11.538061	-0.093848	4.818048
478.742319	8000.372238	11.543066	-0.093891	4.818044
478.584693	8000.383695	11.548071	-0.093861	4.818048
478.477575	8000.410611	11.553075	-0.093841	4.818057
478.716481	8000.408721	11.558080	-0.093886	4.818055
478.685220	8000.334559	11.563085	-0.093880	4.818033
478.748582	8000.367044	11.568090	-0.093892	4.818043
478.738096	8000.375318	11.573095	-0.093890	4.818045
478.746341	8000.376484	11.578099	-0.093891	4.818045
478.588988	8000.399529	11.583104	-0.093862	4.818053
478.727385	8000.341457	11.588109	-0.093888	4.818035
478.922796	8000.341058	11.593114	-0.093924	4.818034
478.791502	8000.433976	11.598119	-0.093900	4.818062
478.651666	8000.362492	11.603123	-0.093873	4.818042
478.510097	8000.486857	11.608128	-0.093847	4.818079
478.219801	8000.483801	11.613133	-0.093793	4.818079
478.382654	8000.429234	11.618138	-0.093823	4.818063
478.566897	8000.416040	11.623143	-0.093857	4.818058
478.371917	8000.485942	11.628147	-0.093821	4.818079
478.593538	8000.452215	11.633152	-0.093862	4.818068
478.889038	8000.403737	11.638157	-0.093917	4.818053
478.495000	8000.444497	11.643162	-0.093844	4.818067
478.646103	8000.483489	11.648167	-0.093872	4.818078
478.825894	8000.350179	11.653171	-0.093905	4.818037
478.809212	8000.377321	11.658176	-0.093902	4.818045
478.893161	8000.411150	11.663181	-0.093918	4.818055
478.899568	8000.398601	11.668186	-0.093919	4.818051
478.997870	8000.388404	11.673191	-0.093937	4.818048
478.888761	8000.415291	11.678195	-0.093917	4.818056
478.980680	8000.432384	11.683200	-0.093934	4.818061
479.144455	8000.324122	11.688205	-0.093964	4.818028
478.983507	8000.371338	11.693210	-0.093934	4.818043
478.786000	8000.429621	11.698215	-0.093898	4.818061
478.748750	8000.390126	11.703219	-0.093891	4.818049
479.201599	8000.385997	11.708224	-0.093975	4.818046
479.139978	8000.408290	11.713229	-0.093963	4.818053
478.801150	8000.408760	11.718234	-0.093900	4.818055
478.751331	8000.412264	11.723239	-0.093891	4.818056
478.741940	8000.377376	11.728243	-0.093889	4.818046
478.740350	8000.448961	11.733248	-0.093889	4.818067
478.850928	8000.389442	11.738253	-0.093909	4.818049
478.782680	8000.298961	11.743258	-0.093897	4.818022
478.670752	8000.442701	11.748263	-0.093876	4.818065
478.833151	8000.353376	11.753267	-0.093906	4.818038
478.893737	8000.415309	11.758272	-0.093917	4.818056
479.259648	8000.384676	11.763277	-0.093985	4.818046
479.264333	8000.369995	11.768282	-0.093986	4.818041
479.319427	8000.384462	11.773287	-0.093996	4.818045
479.182680	8000.343559	11.778291	-0.093971	4.818034
479.176115	8000.399277	11.783296	-0.093970	4.818050
479.029042	8000.389822	11.788301	-0.093942	4.818048
479.124416	8000.362734	11.793306	-0.093960	4.818040
479.315351	8000.353848	11.798311	-0.093995	4.818036
479.217362	8000.332449	11.803315	-0.093977	4.818030
479.433090	8000.380781	11.808320	-0.094017	4.818044
479.095879	8000.443406	11.813325	-0.093954	4.818064
479.367578	8000.338777	11.818330	-0.094005	4.818032
479.295686	8000.406208	11.823335	-0.093991	4.818052
479.503223	8000.339636	11.828339	-0.094030	4.818031
479.323037	8000.419226	11.833344	-0.093996	4.818056
479.103746	8000.353988	11.838349	-0.093956	4.818037
479.287918	8000.346058	11.843354	-0.093990	4.818034
479.436681	8000.350266	11.848359	-0.094017	4.818035
479.123405	8000.340565	11.853363	-0.093959	4.818033
479.345749	8000.370035	11.858368	-0.094000	4.818041
479.102694	8000.447682	11.863373	-0.093955	4.818065
478.750604	8000.404787	11.868378	-0.093890	4.818054
478.568138	8000.476973	11.873383	-0.093856	4.818076
478.450250	8000.437391	11.878387	-0.093834	4.818065
479.212970	8000.389202	11.883392	-0.093976	4.818047
479.279712	8000.369081	11.888397	-0.093988	4.818041
478.959976	8000.408785	11.893402	-0.093928	4.818054
479.263907	8000.421506	11.898407	-0.093985	4.818057
479.241461	8000.359052	11.903411	-0.093981	4.818038
479.249137	8000.418131	11.908416	-0.093982	4.818056
479.359405	8000.372298	11.913421	-0.094003	4.818042
479.250539	8000.449737	11.918426	-0.093982	4.818065
479.037378	8000.459356	11.923431	-0.093943	4.818069
479.437001	8000.348111	11.928435	-0.094017	4.818034
479.286394	8000.419695	11.933440	-0.093989	4.818056
479.214196	8000.350219	11.938445	-0.093975	4.818036
479.231841	8000.345199	11.943450	-0.093978	4.818034
479.286753	8000.381778	11.948455	-0.093989	4.818045
479.370247	8000.320823	11.953459	-0.094004	4.818026
479.327480	8000.345489	11.958464	-0.093996	4.818034
479.338569	8000.342484	11.963469	-0.093998	4.818033
479.192746	8000.349895	11.968474	-0.093971	4.818036
479.161440	8000.393679	11.973479	-0.093965	4.818049
479.011996	8000.372607	11.978483	-0.093937	4.818043
479.414427	8000.357234	11.983488	-0.094012	4.818037
479.048044	8000.431030	11.988493	-0.093944	4.818060
479.221203	8000.306051	11.993498	-0.093976	4.818023
479.497142	8000.337332	11.998503	-0.094027	4.818031
479.532706	8000.317823	12.003507	-0.094034	4.818025
479.476108	8000.357037	12.008512	-0.094023	4.818037
479.315374	8000.343176	12.013517	-0.093993	4.818033
479.404913	8000.366554	12.018522	-0.094010	4.818040
479.242069	8000.371619	12.023527	-0.093980	4.818042
479.280430	8000.301601	12.028531	-0.093987	4.818021
479.493706	8000.346738	12.033536	-0.094026	4.818034
479.662187	8000.285932	12.038541	-0.094058	4.818015
479.363324	8000.335409	12.043546	-0.094002	4.818031
479.249374	8000.472804	12.048551	-0.093981	4.818072
479.434242	8000.385902	12.053555	-0.094015	4.818045
479.409002	8000.418188	12.058560	-0.094011	4.818055
479.578900	8000.401632	12.063565	-0.094042	4.818049
479.642311	8000.375145	12.068570	-0.094054	4.818041
479.702849	8000.375999	12.073575	-0.094065	4.818041
479.629345	8000.320194	12.078579	-0.094051	4.818025
479.809910	8000.384879	12.083584	-0.094085	4.818044
479.696516	8000.423289	12.088589	-0.094064	4.818055
479.325762	8000.428571	12.093594	-0.093995	4.818059
479.491234	8000.434069	12.098599	-0.094026	4.818059
479.314718	8000.348373	12.103603	-0.093993	4.818035
479.268343	8000.430908	12.108608	-0.093984	4.818059
479.300647	8000.414513	12.113613	-0.093990	4.818054
479.486499	8000.390811	12.118618	-0.094024	4.818047
479.405589	8000.414937	12.123623	-0.094009	4.818054
479.410954	8000.296009	12.128627	-0.094010	4.818019
479.666602	8000.345959	12.133632	-0.094058	4.818033
479.204411	8000.382595	12.138637	-0.093972	4.818045
479.266311	8000.383467	12.143642	-0.093983	4.818045
479.349256	8000.404646	12.148647	-0.093999	4.818051
479.223187	8000.381797	12.153651	-0.093975	4.818045
479.175058	8000.411653	12.158656	-0.093966	4.818054
479.139314	8000.465906	12.163661	-0.093959	4.818070
479.234607	8000.461985	12.168666	-0.093977	4.818069
479.074919	8000.478678	12.173671	-0.093947	4.818074
479.145709	8000.364889	12.178675	-0.093960	4.818040
479.091222	8000.414663	12.183680	-0.093950	4.818055
479.350295	8000.399369	12.188685	-0.093998	4.818050
479.476075	8000.397986	12.193690	-0.094022	4.818049
479.582491	8000.404754	12.198695	-0.094042	4.818050
479.453569	8000.329209	12.203699	-0.094018	4.818029
479.666435	8000.341695	12.208704	-0.094057	4.818031
479.514591	8000.362712	12.213709	-0.094029	4.818038
479.429886	8000.378360	12.218714	-0.094013	4.818043
479.462777	8000.404097	12.223719	-0.094019	4.818051
479.176782	8000.354764	12.228723	-0.093966	4.818037
479.365470	8000.389023	12.233728	-0.094001	4.818047
479.484838	8000.378071	12.238733	-0.094023	4.818043
479.137732	8000.453193	12.243738	-0.093958	4.818067
478.990782	8000.453217	12.248743	-0.093931	4.818067
478.679189	8000.546745	12.253747	-0.093873	4.818096
479.297007	8000.520730	12.258752	-0.093988	4.818086
478.643071	8000.534643	12.263757	-0.093866	4.818093
478.872437	8000.384132	12.268762	-0.093909	4.818047
479.050110	8000.481421	12.273767	-0.093942	4.818075
478.984516	8000.456268	12.278771	-0.093930	4.818068
478.706244	8000.535524	12.283776	-0.093878	4.818093
478.933342	8000.449219	12.288781	-0.093920	4.818066
478.848275	8000.418526	12.293786	-0.093904	4.818058
479.396876	8000.377840	12.298791	-0.094006	4.818043
479.136691	8000.439449	12.303795	-0.093958	4.818063
479.110921	8000.503320	12.308800	-0.093953	4.818082
479.354082	8000.423562	12.313805	-0.093998	4.818057
479.657043	8000.354127	12.318810	-0.094054	4.818035
479.544141	8000.476794	12.323815	-0.094033	4.818072
479.285334	8000.414155	12.328819	-0.093985	4.818054
479.609632	8000.371349	12.333824	-0.094045	4.818040
479.338676	8000.426487	12.338829	-0.093995	4.818058
479.252047	8000.437895	12.343834	-0.093979	4.818062
479.410724	8000.468571	12.348839	-0.094008	4.818070
479.096778	8000.500984	12.353843	-0.093950	4.818081
479.302769	8000.366992	12.358848	-0.093988	4.818040
479.286215	8000.477330	12.363853	-0.093985	4.818073
479.142716	8000.404739	12.368858	-0.093958	4.818052
479.349291	8000.478216	12.373863	-0.093997	4.818073
478.938231	8000.487141	12.378867	-0.093920	4.818078
479.014140	8000.437663	12.383872	-0.093934	4.818063
479.117448	8000.464395	12.388877	-0.093953	4.818070
479.444513	8000.439532	12.393882	-0.094014	4.818061
479.674254	8000.451204	12.398887	-0.094057	4.818064
479.407828	8000.394776	12.403891	-0.094007	4.818048
479.125168	8000.500297	12.408896	-0.093955	4.818081
478.782647	8000.448059	12.413901	-0.093891	4.818067
479.388066	8000.401858	12.418906	-0.094004	4.818050
479.622558	8000.448350	12.423911	-0.094047	4.818063
479.343880	8000.419129	12.428915	-0.093995	4.818056
479.409734	8000.443226	12.433920	-0.094007	4.818063
479.597492	8000.369002	12.438925	-0.094042	4.818040
479.722663	8000.391832	12.443930	-0.094066	4.818046
479.831619	8000.376521	12.448935	-0.094086	4.818041
479.748631	8000.380609	12.453939	-0.094070	4.818043
479.831839	8000.416536	12.458944	-0.094086	4.818053
479.685339	8000.437628	12.463949	-0.094058	4.818060
479.746570	8000.375304	12.468954	-0.094070	4.818041
479.740002	8000.432076	12.473959	-0.094069	4.818058
479.540547	8000.388179	12.478963	-0.094031	4.818046
479.848846	8000.410441	12.483968	-0.094089	4.818051
479.882779	8000.332988	12.488973	-0.094095	4.818028
479.956651	8000.341401	12.493978	-0.094109	4.818030
479.743869	8000.422636	12.498983	-0.094069	4.818055
479.679983	8000.358543	12.503987	-0.094057	4.818036
479.873524	8000.383393	12.508992	-0.094093	4.818043
479.939727	8000.367477	12.513997	-0.094105	4.818038
479.998099	8000.373565	12.519002	-0.094116	4.818039
480.109646	8000.381459	12.524007	-0.094137	4.818041
479.531589	8000.348002	12.529011	-0.094029	4.818034
479.627188	8000.391475	12.534016	-0.094047	4.818046
479.677458	8000.406927	12.539021	-0.094056	4.818051
479.806894	8000.408755	12.544026	-0.094080	4.818051
479.840893	8000.447145	12.549031	-0.094087	4.818062
479.552217	8000.445163	12.554035	-0.094033	4.818063
479.838293	8000.454474	12.559040	-0.094086	4.818064
479.949220	8000.400225	12.564045	-0.094107	4.818048
479.785213	8000.348404	12.569050	-0.094076	4.818033
480.150864	8000.347256	12.574055	-0.094144	4.818031
479.846002	8000.343992	12.579059	-0.094087	4.818031
480.013854	8000.357948	12.584064	-0.094119	4.818035
479.694286	8000.379751	12.589069	-0.094059	4.818043
480.073671	8000.361948	12.594074	-0.094130	4.818036
479.884432	8000.438250	12.599079	-0.094094	4.818059
479.766276	8000.370229	12.604083	-0.094072	4.818039
480.038060	8000.390921	12.609088	-0.094123	4.818044
480.006673	8000.383102	12.614093	-0.094117	4.818042
479.774342	8000.360855	12.619098	-0.094074	4.818037
479.776934	8000.405119	12.624103	-0.094074	4.818050
480.047281	8000.342595	12.629107	-0.094124	4.818030
479.868235	8000.410617	12.634112	-0.094091	4.818051
479.918850	8000.372365	12.639117	-0.094100	4.818039
479.891554	8000.378294	12.644122	-0.094095	4.818041
480.056250	8000.425905	12.649127	-0.094126	4.818055
479.837390	8000.372255	12.654131	-0.094085	4.818040
479.708105	8000.459937	12.659136	-0.094061	4.818066
479.486529	8000.418887	12.664141	-0.094020	4.818055
479.681718	8000.392158	12.669146	-0.094056	4.818046
479.598896	8000.423629	12.674151	-0.094041	4.818056
479.603459	8000.368929	12.679155	-0.094041	4.818040
479.738894	8000.423498	12.684160	-0.094067	4.818055
479.741888	8000.427749	12.689165	-0.094067	4.818057
479.936656	8000.356784	12.694170	-0.094103	4.818035
479.992289	8000.381789	12.699175	-0.094114	4.818042
480.077132	8000.339809	12.704179	-0.094129	4.818029
480.275177	8000.395264	12.709184	-0.094166	4.818045
479.828003	8000.422632	12.714189	-0.094083	4.818055
479.617701	8000.409122	12.719194	-0.094044	4.818052
479.908739	8000.422715	12.724199	-0.094098	4.818054
479.752736	8000.344680	12.729203	-0.094069	4.818032
479.806192	8000.392823	12.734208	-0.094079	4.818046
479.980525	8000.366853	12.739213	-0.094111	4.818038
480.014239	8000.336786	12.744218	-0.094117	4.818029
480.088857	8000.356795	12.749223	-0.094131	4.818034
479.877829	8000.341168	12.754227	-0.094092	4.818030
480.244857	8000.350571	12.759232	-0.094160	4.818032
480.263184	8000.345561	12.764237	-0.094163	4.818030
480.156710	8000.308245	12.769242	-0.094144	4.818019
480.197951	8000.358322	12.774247	-0.094151	4.818034
480.309473	8000.298816	12.779251	-0.094172	4.818016
480.438760	8000.313280	12.784256	-0.094196	4.818020
480.112139	8000.313920	12.789261	-0.094135	4.818021
480.188779	8000.340276	12.794266	-0.094149	4.818029
480.192250	8000.372969	12.799271	-0.094150	4.818039
479.987833	8000.324789	12.804275	-0.094112	4.818025
480.006999	8000.349278	12.809280	-0.094115	4.818032
480.097472	8000.330546	12.814285	-0.094132	4.818026
480.019372	8000.345234	12.819290	-0.094118	4.818031
480.139962	8000.359575	12.824295	-0.094140	4.818035
480.107693	8000.319097	12.829299	-0.094134	4.818023
480.187478	8000.389728	12.834304	-0.094149	4.818044
480.124766	8000.379359	12.839309	-0.094137	4.818041
479.928030	8000.367094	12.844314	-0.094100	4.818038
479.834323	8000.349968	12.849319	-0.094083	4.818033
479.843600	8000.340618	12.854323	-0.094085	4.818030
480.197807	8000.360371	12.859328	-0.094150	4.818035
480.051089	8000.414106	12.864333	-0.094123	4.818051
479.991046	8000.359544	12.869338	-0.094112	4.818035
479.975249	8000.418292	12.874343	-0.094109	4.818053
480.021958	8000.403153	12.879347	-0.094118	4.818048
479.997450	8000.405962	12.884352	-0.094113	4.818049
479.863935	8000.399857	12.889357	-0.094088	4.818048
479.916579	8000.380590	12.894362	-0.094098	4.818042
479.995785	8000.406982	12.899367	-0.094113	4.818049
479.715478	8000.409331	12.904371	-0.094060	4.818051
479.962853	8000.412828	12.909376	-0.094106	4.818051
480.008660	8000.326064	12.914381	-0.094115	4.818025
480.127087	8000.359330	12.919386	-0.094137	4.818035
480.011125	8000.428245	12.924391	-0.094115	4.818056
480.069948	8000.410118	12.929395	-0.094126	4.818050
480.042058	8000.390764	12.934400	-0.094121	4.818044
480.015268	8000.416710	12.939405	-0.094116	4.818052
480.247379	8000.365229	12.944410	-0.094159	4.818036
480.407970	8000.358020	12.949415	-0.094189	4.818033
480.158669	8000.303939	12.954419	-0.094142	4.818018
480.002140	8000.405979	12.959424	-0.094113	4.818049
479.954822	8000.338960	12.964429	-0.094104	4.818029
480.081586	8000.340751	12.969434	-0.094128	4.818029
479.998147	8000.443825	12.974439	-0.094112	4.818060
479.938151	8000.360830	12.979443	-0.094101	4.818036
479.701196	8000.432245	12.984448	-0.094057	4.818058
479.874544	8000.463129	12.989453	-0.094089	4.818067
479.794923	8000.448308	12.994458	-0.094074	4.818063
479.589074	8000.494888	12.999463	-0.094036	4.818077
479.688508	8000.385715	13.004467	-0.094054	4.818044
480.077195	8000.404902	13.009472	-0.094127	4.818049
479.931212	8000.428108	13.014477	-0.094100	4.818056
479.817324	8000.398059	13.019482	-0.094078	4.818048
479.693413	8000.477392	13.024487	-0.094055	4.818072
479.708762	8000.410207	13.029491	-0.094058	4.818052
479.837973	8000.416244	13.034496	-0.094082	4.818053
479.925424	8000.362717	13.039501	-0.094098	4.818037
480.089981	8000.330289	13.044506	-0.094129	4.818026
480.262041	8000.354836	13.049511	-0.094161	4.818033
479.971715	8000.360202	13.054515	-0.094107	4.818036
479.821211	8000.447584	13.059520	-0.094079	4.818062
479.883551	8000.412657	13.064525	-0.094090	4.818052
480.040396	8000.263225	13.069530	-0.094119	4.818007
480.325275	8000.359927	13.074535	-0.094172	4.818034
480.177911	8000.313607	13.079539	-0.094145	4.818021
480.258110	8000.341067	13.084544	-0.094160	4.818029
480.296567	8000.333183	13.089549	-0.094167	4.818026
480.119737	8000.336996	13.094554	-0.094134	4.818028
480.215090	8000.390998	13.099559	-0.094152	4.818044
480.250384	8000.298819	13.104563	-0.094158	4.818016
480.239174	8000.334463	13.109568	-0.094156	4.818027
480.313884	8000.313402	13.114573	-0.094170	4.818020
480.233153	8000.331212	13.119578	-0.094155	4.818026
480.210310	8000.411976	13.124583	-0.094151	4.818050
479.966632	8000.383250	13.129587	-0.094105	4.818043
480.335869	8000.390578	13.134592	-0.094174	4.818043
480.280882	8000.328715	13.139597	-0.094163	4.818025
480.276700	8000.302325	13.144602	-0.094163	4.818017
480.308173	8000.343839	13.149607	-0.094168	4.818029
480.215768	8000.328837	13.154611	-0.094151	4.818025
480.252784	8000.373589	13.159616	-0.094158	4.818039
480.361478	8000.343530	13.164621	-0.094178	4.818029
480.094801	8000.358709	13.169626	-0.094129	4.818035
480.319704	8000.315551	13.174631	-0.094170	4.818021
480.219161	8000.335187	13.179635	-0.094152	4.818027
480.448173	8000.345797	13.184640	-0.094194	4.818029
480.300758	8000.328964	13.189645	-0.094167	4.818025
480.295786	8000.348899	13.194650	-0.094166	4.818031
480.376396	8000.393215	13.199655	-0.094181	4.818044
480.139152	8000.367739	13.204659	-0.094137	4.818037
480.065944	8000.391974	13.209664	-0.094123	4.818045
480.114095	8000.338943	13.214669	-0.094132	4.818029
480.318589	8000.333409	13.219674	-0.094170	4.818026
480.390666	8000.346010	13.224679	-0.094183	4.818030
480.391152	8000.333376	13.229683	-0.094183	4.818026
480.222129	8000.397327	13.234688	-0.094152	4.818046
479.997218	8000.425735	13.239693	-0.094110	4.818055
480.241456	8000.337566	13.244698	-0.094155	4.818028
480.335309	8000.401026	13.249703	-0.094173	4.818046
480.369264	8000.331997	13.254707	-0.094179	4.818026
480.392431	8000.351277	13.259712	-0.094183	4.818031
480.420241	8000.346402	13.264717	-0.094188	4.818030
480.542765	8000.347080	13.269722	-0.094211	4.818029
480.555321	8000.344095	13.274727	-0.094213	4.818029
480.332664	8000.312506	13.279731	-0.094172	4.818020
480.470976	8000.368170	13.284736	-0.094198	4.818036
480.444707	8000.335147	13.289741	-0.094193	4.818026
480.310944	8000.310082	13.294746	-0.094168	4.818019
480.410195	8000.343077	13.299751	-0.094186	4.818029
480.348678	8000.350629	13.304755	-0.094175	4.818031
480.483513	8000.396765	13.309760	-0.094200	4.818044
480.349528	8000.345368	13.314765	-0.094175	4.818030
480.397368	8000.351308	13.319770	-0.094184	4.818031
480.479397	8000.379847	13.324775	-0.094199	4.818039
480.358210	8000.324419	13.329779	-0.094176	4.818024
480.522036	8000.336212	13.334784	-0.094207	4.818026
480.404865	8000.346135	13.339789	-0.094185	4.818030
480.344152	8000.333688	13.344794	-0.094173	4.818026
480.595284	8000.326708	13.349799	-0.094220	4.818023
480.629130	8000.318759	13.354803	-0.094226	4.818021
480.327406	8000.347132	13.359808	-0.094170	4.818030
480.183975	8000.359843	13.364813	-0.094143	4.818035
480.296050	8000.366691	13.369818	-0.094164	4.818036
480.373891	8000.394118	13.374823	-0.094179	4.818044
480.497277	8000.357948	13.379827	-0.094202	4.818033
480.440058	8000.395047	13.384832	-0.094191	4.818044
480.464770	8000.332206	13.389837	-0.094196	4.818025
480.374249	8000.347772	13.394842	-0.094179	4.818030
480.463269	8000.399579	13.399847	-0.094195	4.818045
479.936159	8000.451090	13.404851	-0.094097	4.818063
480.228479	8000.427843	13.409856	-0.094151	4.818055
479.845709	8000.467707	13.414861	-0.094080	4.818068
480.237419	8000.401635	13.419866	-0.094153	4.818047
480.266670	8000.464180	13.424871	-0.094158	4.818065
479.973822	8000.411588	13.429875	-0.094104	4.818051
480.115532	8000.394634	13.434880	-0.094130	4.818045
480.185614	8000.393516	13.439885	-0.094143	4.818045
480.067243	8000.371829	13.444890	-0.094121	4.818039
480.327910	8000.350239	13.449895	-0.094170	4.818031
480.257037	8000.351339	13.454899	-0.094156	4.818032
480.461180	8000.371075	13.459904	-0.094194	4.818037
480.479641	8000.357642	13.464909	-0.094198	4.818033
480.492472	8000.380990	13.469914	-0.094200	4.818040
480.603050	8000.381498	13.474919	-0.094221	4.818039
480.149568	8000.429839	13.479923	-0.094136	4.818056
480.426866	8000.402167	13.484928	-0.094188	4.818046
480.615539	8000.380612	13.489933	-0.094223	4.818039
480.397803	8000.410174	13.494938	-0.094182	4.818049
480.261292	8000.436673	13.499943	-0.094157	4.818057
480.157826	8000.438365	13.504947	-0.094137	4.818058
480.495499	8000.451566	13.509952	-0.094200	4.818061
480.081461	8000.413056	13.514957	-0.094123	4.818051
480.234558	8000.436282	13.519962	-0.094152	4.818057
480.595114	8000.423478	13.524967	-0.094219	4.818052
480.049111	8000.468403	13.529971	-0.094117	4.818068
480.062423	8000.459110	13.534976	-0.094119	4.818065
480.212714	8000.430694	13.539981	-0.094147	4.818056
480.200997	8000.356806	13.544986	-0.094145	4.818034
480.384434	8000.394152	13.549991	-0.094179	4.818044
480.395860	8000.384832	13.554995	-0.094181	4.818041
480.156584	8000.445683	13.560000	-0.094137	4.818060
479.985873	8000.437998	13.565005	-0.094105	4.818059
480.108775	8000.375494	13.570010	-0.094128	4.818040
480.219058	8000.460248	13.575015	-0.094148	4.818064
480.298025	8000.405546	13.580019	-0.094163	4.818048
480.345260	8000.374618	13.585024	-0.094172	4.818039
480.280633	8000.462163	13.590029	-0.094160	4.818065
479.882831	8000.440733	13.595034	-0.094085	4.818060
479.961934	8000.481867	13.600039	-0.094100	4.818072
480.093665	8000.441603	13.605043	-0.094125	4.818059
480.403415	8000.423868	13.610048	-0.094182	4.818053
480.089149	8000.442586	13.615053	-0.094124	4.818060
480.360875	8000.420100	13.620058	-0.094174	4.818052
480.513431	8000.403300	13.625063	-0.094203	4.818046
480.569243	8000.347218	13.630067	-0.094213	4.818029
480.402316	8000.351171	13.635072	-0.094182	4.818031
480.578893	8000.372623	13.640077	-0.094215	4.818037
480.382486	8000.356149	13.645082	-0.094178	4.818033
480.493921	8000.366148	13.650087	-0.094199	4.818035
480.494863	8000.328245	13.655091	-0.094199	4.818024
480.398295	8000.364788	13.660096	-0.094181	4.818035
480.521007	8000.386531	13.665101	-0.094204	4.818041
480.347063	8000.314559	13.670106	-0.094171	4.818021
480.536750	8000.333037	13.675111	-0.094206	4.818025
480.205131	8000.369413	13.680115	-0.094145	4.818038
480.190151	8000.374463	13.685120	-0.094142	4.818039
479.867371	8000.445717	13.690125	-0.094082	4.818062
480.094401	8000.423652	13.695130	-0.094124	4.818054
480.249334	8000.431107	13.700135	-0.094153	4.818056
480.666540	8000.341174	13.705139	-0.094230	4.818027
480.676333	8000.393966	13.710144	-0.094232	4.818043
480.629254	8000.393296	13.715149	-0.094223	4.818043
480.481545	8000.340652	13.720154	-0.094196	4.818028
480.677471	8000.372909	13.725159	-0.094232	4.818037
480.501818	8000.399907	13.730163	-0.094200	4.818045
480.474662	8000.440592	13.735168	-0.094194	4.818058
480.314610	8000.516255	13.740173	-0.094165	4.818081
480.499501	8000.377749	13.745178	-0.094199	4.818039
480.670972	8000.375960	13.750183	-0.094231	4.818038
480.553765	8000.336385	13.755187	-0.094209	4.818026
480.309010	8000.405584	13.760192	-0.094163	4.818048
480.202360	8000.418815	13.765197	-0.094143	4.818052
480.338066	8000.380713	13.770202	-0.094169	4.818040
480.605924	8000.400298	13.775207	-0.094219	4.818045
480.671395	8000.339087	13.780211	-0.094231	4.818027
480.525574	8000.375985	13.785216	-0.094203	4.818038
480.512461	8000.386328	13.790221	-0.094201	4.818041
480.727238	8000.347239	13.795226	-0.094241	4.818029
480.724915	8000.358787	13.800231	-0.094240	4.818032
480.560447	8000.378572	13.805235	-0.094210	4.818039
480.813253	8000.387413	13.810240	-0.094257	4.818040
480.646889	8000.410330	13.815245	-0.094226	4.818048
480.333220	8000.393249	13.820250	-0.094167	4.818044
480.608079	8000.388711	13.825255	-0.094219	4.818042
480.569803	8000.328138	13.830259	-0.094211	4.818024
480.623707	8000.367863	13.835264	-0.094221	4.818035
480.563199	8000.341728	13.840269	-0.094210	4.818028
480.571899	8000.317626	13.845274	-0.094212	4.818021
480.836986	8000.365607	13.850279	-0.094261	4.818034
480.692822	8000.333022	13.855283	-0.094234	4.818025
480.448896	8000.434879	13.860288	-0.094189	4.818056
480.788306	8000.385970	13.865293	-0.094252	4.818040
480.645476	8000.376573	13.870298	-0.094225	4.818038
480.725250	8000.435622	13.875303	-0.094240	4.818055
480.720283	8000.423964	13.880307	-0.094239	4.818052
480.662785	8000.421040	13.885312	-0.094228	4.818051
480.616557	8000.461455	13.890317	-0.094220	4.818063
480.701901	8000.351027	13.895322	-0.094235	4.818030
480.714086	8000.394375	13.900327	-0.094238	4.818043
480.451374	8000.384334	13.905331	-0.094189	4.818041
480.510527	8000.376743	13.910336	-0.094200	4.818039
480.526457	8000.412772	13.915341	-0.094203	4.818049
480.157602	8000.459151	13.920346	-0.094134	4.818064
480.508868	8000.466226	13.925351	-0.094199	4.818065
480.523766	8000.392714	13.930355	-0.094202	4.818043
480.361427	8000.388307	13.935360	-0.094172	4.818043
480.608097	8000.293854	13.940365	-0.094217	4.818014
480.637649	8000.375360	13.945370	-0.094223	4.818038
480.505879	8000.454583	13.950375	-0.094198	4.818062
480.474054	8000.391994	13.955379	-0.094192	4.818043
480.828976	8000.402281	13.960384	-0.094258	4.818045
480.850108	8000.374142	13.965389	-0.094262	4.818036
480.592676	8000.337847	13.970394	-0.094214	4.818027
480.590192	8000.425219	13.975399	-0.094214	4.818053
480.634953	8000.367927	13.980403	-0.094222	4.818035
480.565894	8000.374318	13.985408	-0.094209	4.818038
480.504207	8000.430311	13.990413	-0.094198	4.818054
480.484680	8000.372109	13.995418	-0.094194	4.818037
480.585645	8000.469370	14.000423	-0.094213	4.818066
480.049456	8000.450193	14.005427	-0.094113	4.818062
480.452631	8000.446418	14.010432	-0.094188	4.818059
480.675928	8000.458000	14.015437	-0.094230	4.818062
480.381065	8000.442239	14.020442	-0.094175	4.818059
480.326584	8000.445677	14.025447	-0.094164	4.818060
480.299438	8000.468458	14.030451	-0.094159	4.818067
480.409703	8000.423678	14.035456	-0.094180	4.818053
480.446602	8000.471588	14.040461	-0.094187	4.818067
480.708647	8000.385777	14.045466	-0.094235	4.818040
480.639125	8000.479572	14.050471	-0.094222	4.818068
480.417649	8000.410087	14.055475	-0.094181	4.818049
480.624973	8000.419337	14.060480	-0.094220	4.818051
480.662403	8000.465148	14.065485	-0.094227	4.818064
480.565023	8000.344762	14.070490	-0.094208	4.818029
480.662176	8000.393525	14.075495	-0.094226	4.818043
480.669638	8000.378883	14.080499	-0.094228	4.818039
480.845422	8000.417175	14.085504	-0.094260	4.818049
480.552669	8000.457259	14.090509	-0.094206	4.818062
480.553099	8000.370905	14.095514	-0.094206	4.818037
480.695025	8000.471906	14.100519	-0.094232	4.818066
480.615643	8000.433919	14.105523	-0.094218	4.818055
480.752770	8000.439016	14.110528	-0.094243	4.818056
480.768059	8000.448708	14.115533	-0.094246	4.818059
480.749214	8000.405259	14.120538	-0.094242	4.818046
480.653856	8000.455509	14.125543	-0.094224	4.818061
480.603028	8000.343154	14.130547	-0.094215	4.818028
480.707120	8000.400441	14.135552	-0.094234	4.818045
480.617288	8000.428653	14.140557	-0.094218	4.818054
480.664471	8000.397724	14.145562	-0.094226	4.818044
480.964444	8000.418817	14.150567	-0.094282	4.818049
480.719283	8000.379537	14.155571	-0.094236	4.818039
480.785856	8000.422601	14.160576	-0.094249	4.818051
481.025246	8000.387021	14.165581	-0.094293	4.818039
480.892295	8000.414623	14.170586	-0.094268	4.818048
480.835097	8000.430661	14.175591	-0.094258	4.818053
480.659523	8000.405003	14.180595	-0.094225	4.818046
480.759611	8000.408523	14.185600	-0.094244	4.818047
480.547302	8000.444480	14.190605	-0.094204	4.818059
480.558253	8000.450951	14.195610	-0.094206	4.818060
480.730071	8000.499718	14.200615	-0.094238	4.818074
480.586300	8000.399737	14.205619	-0.094211	4.818045
480.697644	8000.436064	14.210624	-0.094232	4.818055
480.554249	8000.438243	14.215629	-0.094205	4.818057
480.609266	8000.429540	14.220634	-0.094215	4.818054
480.668391	8000.445118	14.225639	-0.094226	4.818058
480.876463	8000.375394	14.230643	-0.094265	4.818037
480.959361	8000.439752	14.235648	-0.094280	4.818055
480.805483	8000.488121	14.240653	-0.094252	4.818070
480.678180	8000.398905	14.245658	-0.094228	4.818044
480.598627	8000.454645	14.250663	-0.094213	4.818061
480.435302	8000.492349	14.255667	-0.094183	4.818073
480.619488	8000.465465	14.260672	-0.094217	4.818064
481.046276	8000.347233	14.265677	-0.094296	4.818028
480.809187	8000.352299	14.270682	-0.094252	4.818030
480.864327	8000.398361	14.275687	-0.094262	4.818044
480.786802	8000.383570	14.280691	-0.094248	4.818039
480.806599	8000.377528	14.285696	-0.094251	4.818038
480.814630	8000.425030	14.290701	-0.094253	4.818052
480.473058	8000.415979	14.295706	-0.094189	4.818050
480.415129	8000.551010	14.300711	-0.094179	4.818091
480.386668	8000.410537	14.305715	-0.094173	4.818049
480.486463	8000.467762	14.310720	-0.094192	4.818066
480.746795	8000.542005	14.315725	-0.094240	4.818087
480.690792	8000.441160	14.320730	-0.094230	4.818057
480.377296	8000.569414	14.325735	-0.094171	4.818096
480.350087	8000.535325	14.330739	-0.094166	4.818086
480.845819	8000.434920	14.335744	-0.094258	4.818054
480.923596	8000.465506	14.340749	-0.094273	4.818063
480.903126	8000.407290	14.345754	-0.094269	4.818046
480.783658	8000.489846	14.350759	-0.094247	4.818071
480.934683	8000.476184	14.355763	-0.094275	4.818066
480.926080	7999.362922	14.360768	-0.094272	4.817736

480.712240	7996.317868	14.365773	-0.094231	4.816834
480.692483	7990.681501	14.370778	-0.094223	4.815163
480.751195	7984.078140	14.375783	-0.094230	4.813203
480.781909	7976.731474	14.380787	-0.094231	4.811023
480.852477	7969.105921	14.385792	-0.094239	4.808758
480.744941	7961.362871	14.390797	-0.094214	4.806458
480.595479	7953.427714	14.395802	-0.094181	4.804100
480.537957	7945.632042	14.400807	-0.094165	4.801782
480.624407	7937.555592	14.405811	-0.094176	4.799379
480.518227	7929.589814	14.410816	-0.094151	4.797008
480.444630	7921.566590	14.415821	-0.094132	4.794619
480.417375	7913.596144	14.420826	-0.094121	4.792244
480.579564	7905.512562	14.425831	-0.094146	4.789833
480.021379	7897.585746	14.430835	-0.094037	4.787471
480.468991	7889.496794	14.435840	-0.094115	4.785055
480.650871	7881.550939	14.440845	-0.094144	4.782682
480.446864	7873.496027	14.445850	-0.094100	4.780277
480.429246	7865.571560	14.450855	-0.094092	4.777908
480.525336	7857.495683	14.455859	-0.094105	4.775493
480.596688	7849.541494	14.460864	-0.094113	4.773113
480.638308	7841.563835	14.465869	-0.094115	4.770725
480.613981	7833.490484	14.470874	-0.094105	4.768308
480.659553	7825.491734	14.475879	-0.094108	4.765911
480.479462	7817.475022	14.480883	-0.094070	4.763508
480.444552	7809.551231	14.485888	-0.094058	4.761132
480.361658	7801.534238	14.490893	-0.094037	4.758726
480.313557	7793.546608	14.495898	-0.094023	4.756328
480.289012	7785.475962	14.500903	-0.094013	4.753904
480.324689	7777.534603	14.505907	-0.094015	4.751517
480.209532	7769.453730	14.510912	-0.093988	4.749088
480.155792	7761.490645	14.515917	-0.093973	4.746692
480.166473	7753.370370	14.520922	-0.093969	4.744248
480.217844	7745.526152	14.525927	-0.093974	4.741885
480.064110	7737.449086	14.530931	-0.093940	4.739452
480.036357	7729.501435	14.535936	-0.093929	4.737056
480.006451	7721.510206	14.540941	-0.093919	4.734646
479.778259	7713.493712	14.545946	-0.093871	4.732227
479.942854	7705.426272	14.550951	-0.093896	4.729791
479.863509	7697.458399	14.555955	-0.093876	4.727385
480.058703	7689.421049	14.560960	-0.093907	4.724955
479.862488	7681.504988	14.565965	-0.093865	4.722562
479.874365	7673.462268	14.570970	-0.093862	4.720128
479.550194	7665.547468	14.575975	-0.093797	4.717733
479.675057	7657.499282	14.580979	-0.093815	4.715296
479.597200	7649.495277	14.585984	-0.093795	4.712870
479.707919	7641.461453	14.590989	-0.093810	4.710435
479.665197	7633.404192	14.595994	-0.093797	4.707991
479.931399	7625.423666	14.600999	-0.093841	4.705568
479.729023	7617.471601	14.606003	-0.093799	4.703154
479.657527	7609.461647	14.611008	-0.093780	4.700721
479.542440	7601.495728	14.616013	-0.093753	4.698300
479.613944	7593.468057	14.621018	-0.093761	4.695858
480.016559	7585.510522	14.626023	-0.093831	4.693437
479.505347	7577.486743	14.631027	-0.093731	4.690995
479.249813	7569.482641	14.636032	-0.093678	4.688557
478.768119	7561.573170	14.641037	-0.093583	4.686147
479.044185	7553.394086	14.646042	-0.093629	4.683653
479.250667	7545.485051	14.651047	-0.093662	4.681240
479.139127	7537.433887	14.656051	-0.093636	4.678783
479.151089	7529.531449	14.661056	-0.093633	4.676369
479.233343	7521.456551	14.666061	-0.093643	4.673902
478.721680	7513.441678	14.671066	-0.093543	4.671452
479.158683	7505.359781	14.676071	-0.093619	4.668980
479.102927	7497.418728	14.681075	-0.093603	4.666550
479.117776	7489.380030	14.686080	-0.093601	4.664088
478.900368	7481.516376	14.691085	-0.093555	4.661679
478.865119	7473.359790	14.696090	-0.093543	4.659179
479.115902	7465.458305	14.701095	-0.093584	4.656756
479.160667	7457.390767	14.706099	-0.093588	4.654280
479.190059	7449.448484	14.711104	-0.093588	4.651842
478.826336	7441.426805	14.716109	-0.093515	4.649378
478.783027	7433.462467	14.721114	-0.093501	4.646931
478.937627	7425.421187	14.726119	-0.093525	4.644458
478.788094	7417.476455	14.731123	-0.093492	4.642014
478.676645	7409.414291	14.736128	-0.093466	4.639532
478.696935	7401.467919	14.741133	-0.093464	4.637085
478.417233	7393.422600	14.746138	-0.093407	4.634606
478.303234	7385.445354	14.751143	-0.093381	4.632146
478.478442	7377.354751	14.756147	-0.093408	4.629650
478.758619	7369.378557	14.761152	-0.093455	4.627189
478.471230	7361.373919	14.766157	-0.093396	4.624717
478.309294	7353.409853	14.771162	-0.093361	4.622256
478.563526	7345.405964	14.776167	-0.093403	4.619782
478.417662	7337.400989	14.781171	-0.093370	4.617306
478.243765	7329.366143	14.786176	-0.093333	4.614819
478.634695	7321.393867	14.791181	-0.093400	4.612351
478.391695	7313.356785	14.796186	-0.093350	4.609861
478.352324	7305.390054	14.801191	-0.093337	4.607391
478.596375	7297.331191	14.806195	-0.093377	4.604892
478.510070	7289.405378	14.811200	-0.093356	4.602432
478.606504	7281.395784	14.816205	-0.093369	4.599946
478.385550	7273.377529	14.821210	-0.093322	4.597455
478.322278	7265.383220	14.826215	-0.093305	4.594970
478.382020	7257.377737	14.831219	-0.093311	4.592480
478.461994	7249.310294	14.836224	-0.093321	4.589970
478.241654	7241.415946	14.841229	-0.093274	4.587512
478.233626	7233.311550	14.846234	-0.093268	4.584988
478.363425	7225.365213	14.851239	-0.093287	4.582512
478.086856	7217.338016	14.856243	-0.093230	4.580008
477.931572	7209.389742	14.861248	-0.093196	4.577528
478.144317	7201.322942	14.866253	-0.093230	4.575010
477.995964	7193.340409	14.871258	-0.093197	4.572516
478.057976	7185.360117	14.876263	-0.093203	4.570023
478.179171	7177.326926	14.881267	-0.093221	4.567511
478.187490	7169.282830	14.886272	-0.093217	4.564994
478.254483	7161.331551	14.891277	-0.093224	4.562505
478.128286	7153.321053	14.896282	-0.093195	4.559996
477.826602	7145.418764	14.901287	-0.093134	4.557519
477.905445	7137.330181	14.906291	-0.093143	4.554983
478.061036	7129.320160	14.911296	-0.093167	4.552471
477.907730	7121.315729	14.916301	-0.093133	4.549958
477.843019	7113.298243	14.921306	-0.093116	4.547440
478.066279	7105.266170	14.926311	-0.093152	4.544916
477.930669	7097.325637	14.931315	-0.093122	4.542419
477.635678	7089.307461	14.936320	-0.093062	4.539896
477.695442	7081.340557	14.941325	-0.093068	4.537388
477.671231	7073.234055	14.946330	-0.093058	4.534835
477.824384	7065.292066	14.951335	-0.093081	4.532333
477.524748	7057.253432	14.956339	-0.093020	4.529797
477.585491	7049.291402	14.961344	-0.093026	4.527286
477.490623	7041.237301	14.966349	-0.093003	4.524743
477.276864	7033.273868	14.971354	-0.092958	4.522228
477.617564	7025.251419	14.976359	-0.093016	4.519693
477.477720	7017.308087	14.981363	-0.092985	4.517181
477.310671	7009.277755	14.986368	-0.092949	4.514640
477.323497	7001.323169	14.991373	-0.092946	4.512123
477.382951	6993.250351	14.996378	-0.092952	4.509566
477.380990	6985.238878	15.001383	-0.092946	4.507027
477.225852	6977.218797	15.006387	-0.092912	4.504484
477.019300	6969.307171	15.011392	-0.092868	4.501973
476.914642	6961.295682	15.016397	-0.092843	4.499429
476.712401	6953.275131	15.021402	-0.092800	4.496881
476.844287	6945.241641	15.026407	-0.092820	4.494329
476.721952	6937.265689	15.031411	-0.092792	4.491792
476.827660	6929.211160	15.036416	-0.092806	4.489230
476.808385	6921.221525	15.041421	-0.092797	4.486686
477.157129	6913.116313	15.046426	-0.092857	4.484106
477.042475	6905.311269	15.051431	-0.092830	4.481618
476.755643	6897.267110	15.056435	-0.092772	4.479052
476.491550	6889.268476	15.061440	-0.092717	4.476499
476.638177	6881.199770	15.066445	-0.092739	4.473923
476.745290	6873.223140	15.071450	-0.092754	4.471376
476.864325	6865.193248	15.076455	-0.092771	4.468810
477.248697	6857.148712	15.081459	-0.092837	4.466239
477.012028	6849.173789	15.086464	-0.092788	4.463686
476.556005	6841.295303	15.091469	-0.092698	4.461161
476.791833	6833.190509	15.096474	-0.092736	4.458566
476.687536	6825.225707	15.101479	-0.092712	4.456013
476.393662	6817.187507	15.106483	-0.092652	4.453433
476.494758	6809.178416	15.111488	-0.092665	4.450864
476.546172	6801.201877	15.116493	-0.092670	4.448303
476.306708	6793.127462	15.121498	-0.092620	4.445707
476.236643	6785.202843	15.126503	-0.092601	4.443159
476.289522	6777.212004	15.131507	-0.092606	4.440589
475.792938	6769.245080	15.136512	-0.092508	4.438023
475.891801	6761.215346	15.141517	-0.092521	4.435437
475.925810	6753.151594	15.146522	-0.092522	4.432839
476.551069	6745.131332	15.151527	-0.092634	4.430257
475.749911	6737.192240	15.156531	-0.092479	4.427691
475.655169	6729.132192	15.161536	-0.092456	4.425089
475.877537	6721.190441	15.166541	-0.092492	4.422525
475.930213	6713.122832	15.171546	-0.092497	4.419919
475.651250	6705.225924	15.176551	-0.092440	4.417363
475.626368	6697.131512	15.181555	-0.092430	4.414744
475.855449	6689.128062	15.186560	-0.092467	4.412155
475.901099	6681.151772	15.191565	-0.092471	4.409571
475.807667	6673.136434	15.196570	-0.092448	4.406973
475.913153	6665.085671	15.201575	-0.092462	4.404363
475.762521	6657.200181	15.206579	-0.092429	4.401803
476.185610	6649.052007	15.211584	-0.092502	4.399160
476.139460	6641.150844	15.216589	-0.092489	4.396592
475.916708	6633.106941	15.221594	-0.092442	4.393976
475.670183	6625.223827	15.226599	-0.092391	4.391411
475.655169	6617.169280	15.231603	-0.092383	4.388789
475.407555	6609.222832	15.236608	-0.092331	4.386200
475.503024	6601.174780	15.241613	-0.092344	4.383578
475.493970	6593.169020	15.246618	-0.092337	4.380967
475.964946	6585.156446	15.251623	-0.092419	4.378357
475.991414	6577.136490	15.256627	-0.092419	4.375739
475.927969	6569.131780	15.261632	-0.092402	4.373124
475.720742	6561.188354	15.266637	-0.092358	4.370526
475.460860	6553.184037	15.271642	-0.092304	4.367907
475.307627	6545.218624	15.276647	-0.092271	4.365299
475.387804	6537.257824	15.281651	-0.092280	4.362693
475.614424	6529.209053	15.286656	-0.092317	4.360058
475.960931	6521.249103	15.291661	-0.092377	4.357451
475.378980	6513.196145	15.296666	-0.092263	4.354806
475.247393	6505.228705	15.301671	-0.092233	4.352190
475.540048	6497.145458	15.306675	-0.092282	4.349537
475.587195	6489.145690	15.311680	-0.092286	4.346909
475.330925	6481.202251	15.316685	-0.092233	4.344295
475.120288	6473.230404	15.321690	-0.092188	4.341671
475.062282	6465.213491	15.326695	-0.092172	4.339031
475.142069	6457.229547	15.331699	-0.092182	4.336402
475.067930	6449.181124	15.336704	-0.092163	4.333748
475.221105	6441.247739	15.341709	-0.092186	4.331133
474.872548	6433.204333	15.346714	-0.092116	4.328476
474.833371	6425.271993	15.351719	-0.092104	4.325856
474.929744	6417.190060	15.356723	-0.092116	4.323187
475.119993	6409.188203	15.361728	-0.092146	4.320543
475.118984	6401.219472	15.366733	-0.092141	4.317906
474.868283	6393.211846	15.371738	-0.092089	4.315254
474.914240	6385.237635	15.376743	-0.092092	4.312613
475.167790	6377.159478	15.381747	-0.092134	4.309938
475.131063	6369.140673	15.386752	-0.092122	4.307278
475.351794	6361.112728	15.391757	-0.092158	4.304616
475.184190	6353.151383	15.396762	-0.092121	4.301971
475.163358	6345.142349	15.401767	-0.092112	4.299310
474.907210	6337.179187	15.406771	-0.092059	4.296660
474.443727	6329.171165	15.411776	-0.091968	4.293992
474.992271	6321.152670	15.416781	-0.092065	4.291328
475.094445	6313.089985	15.421786	-0.092078	4.288643
474.971123	6305.111438	15.426791	-0.092050	4.285983
474.664454	6297.196225	15.431795	-0.091988	4.283340
474.202373	6289.251932	15.436800	-0.091897	4.280685
474.595051	6281.184534	15.441805	-0.091964	4.277995
474.492720	6273.121780	15.446810	-0.091940	4.275300
474.617945	6265.180090	15.451815	-0.091958	4.272646
474.717526	6257.154454	15.456819	-0.091972	4.269962
474.423503	6249.144047	15.461824	-0.091911	4.267278
474.587287	6241.113639	15.466829	-0.091937	4.264589
474.815077	6233.119921	15.471834	-0.091974	4.261912
474.632567	6225.135556	15.476839	-0.091935	4.259232
474.439767	6217.187286	15.481843	-0.091894	4.256563
474.317266	6209.123996	15.486848	-0.091865	4.253854
474.913525	6201.125512	15.491853	-0.091971	4.251172
474.554002	6193.131434	15.496858	-0.091899	4.248481
474.635520	6185.161867	15.501863	-0.091909	4.245800
474.380682	6177.153653	15.506867	-0.091856	4.243102
474.564471	6169.141077	15.511872	-0.091885	4.240404
474.593589	6161.172500	15.516877	-0.091885	4.237718
474.586027	6153.114793	15.521882	-0.091879	4.235000
474.395629	6145.168698	15.526887	-0.091838	4.232316
474.083662	6137.150184	15.531891	-0.091775	4.229605
474.211069	6129.153698	15.536896	-0.091793	4.226904
473.966971	6121.161035	15.541901	-0.091742	4.224198
474.106918	6113.174368	15.546906	-0.091763	4.221497
474.054910	6105.120526	15.551911	-0.091748	4.218769
474.168873	6097.147666	15.556915	-0.091764	4.216069
474.538193	6089.121945	15.561920	-0.091828	4.213352
474.362326	6081.140997	15.566925	-0.091790	4.210643
474.101304	6073.118398	15.571930	-0.091736	4.207916
474.279113	6065.107858	15.576935	-0.091764	4.205197
473.879348	6057.173815	15.581939	-0.091684	4.202495
473.925058	6049.105482	15.586944	-0.091687	4.199751
474.119455	6041.161236	15.591949	-0.091718	4.197050
474.022802	6033.108095	15.596954	-0.091695	4.194306
474.304244	6025.040183	15.601959	-0.091742	4.191559
474.144105	6017.056502	15.606963	-0.091707	4.188835
473.701594	6009.119740	15.611968	-0.091619	4.186121
473.504908	6001.158851	15.616973	-0.091578	4.183400
473.681474	5993.084392	15.621978	-0.091605	4.180643
473.730606	5985.086250	15.626983	-0.091609	4.177909
473.586788	5977.095509	15.631987	-0.091577	4.175173
473.700120	5969.138416	15.636992	-0.091593	4.172450
474.057948	5961.057601	15.641997	-0.091654	4.169686
473.598906	5953.098398	15.647002	-0.091563	4.166952
473.949788	5945.041105	15.652007	-0.091623	4.164192
473.649887	5937.197840	15.657011	-0.091562	4.161496
473.607142	5929.132456	15.662016	-0.091549	4.158725
473.429128	5921.210848	15.667021	-0.091511	4.155999
473.142293	5913.137886	15.672026	-0.091452	4.153219
473.128052	5905.162015	15.677031	-0.091444	4.150473
473.337304	5897.135173	15.682035	-0.091478	4.147711
473.279615	5889.102663	15.687040	-0.091462	4.144942
472.995700	5881.213381	15.692045	-0.091404	4.142218
473.201951	5873.085888	15.697050	-0.091437	4.139415
473.047002	5865.176230	15.702055	-0.091403	4.136682
472.785037	5857.168450	15.707059	-0.091349	4.133911
473.241834	5849.119872	15.712064	-0.091429	4.131134
472.882296	5841.189796	15.717069	-0.091356	4.128385
472.405954	5833.218271	15.722074	-0.091263	4.125618
472.718801	5825.159685	15.727079	-0.091315	4.122830
472.481961	5817.188960	15.732083	-0.091266	4.120063
472.733749	5809.149775	15.737088	-0.091308	4.117277
472.561779	5801.178383	15.742093	-0.091270	4.114506
472.619091	5793.148615	15.747098	-0.091276	4.111717
472.671095	5785.108333	15.752103	-0.091280	4.108922
472.604778	5777.160738	15.757107	-0.091263	4.106156
472.581799	5769.151364	15.762112	-0.091253	4.103367
472.916521	5761.115172	15.767117	-0.091310	4.100572
472.676987	5753.120927	15.772122	-0.091260	4.097782
472.550822	5745.146425	15.777127	-0.091232	4.094998
472.526044	5737.141986	15.782131	-0.091222	4.092203
472.414152	5729.131412	15.787136	-0.091196	4.089403
472.555323	5721.169535	15.792141	-0.091217	4.086622
472.528597	5713.078117	15.797146	-0.091206	4.083791
472.767969	5705.143536	15.802151	-0.091246	4.081016
472.931999	5697.117620	15.807155	-0.091271	4.078207
472.850209	5689.129730	15.812160	-0.091251	4.075406
472.825430	5681.155650	15.817165	-0.091241	4.072608
472.709367	5673.124248	15.822170	-0.091214	4.069787
472.813119	5665.149547	15.827175	-0.091228	4.066987
472.513117	5657.140711	15.832179	-0.091167	4.064168
472.566751	5649.158781	15.837184	-0.091172	4.061361
472.331539	5641.201885	15.842189	-0.091122	4.058556
472.373117	5633.146481	15.847194	-0.091125	4.055719
472.318299	5625.146930	15.852199	-0.091109	4.052898
472.665033	5617.092099	15.857203	-0.091169	4.050062
472.369752	5609.171709	15.862208	-0.091109	4.047262
472.517972	5601.126964	15.867213	-0.091131	4.044422
472.335008	5593.182804	15.872218	-0.091092	4.041611
472.575810	5585.153967	15.877223	-0.091131	4.038775
472.024733	5577.262106	15.882227	-0.091023	4.035973
472.034461	5569.159652	15.887232	-0.091020	4.033103
472.188761	5561.129535	15.892237	-0.091043	4.030259
471.854281	5553.135920	15.897242	-0.090976	4.027418
472.097000	5545.068264	15.902247	-0.091016	4.024557
472.157220	5537.150738	15.907251	-0.091022	4.021746
472.534994	5529.045101	15.912256	-0.091087	4.018870
472.486400	5521.138417	15.917261	-0.091072	4.016057
472.186192	5513.143718	15.922266	-0.091011	4.013206
472.275266	5505.170951	15.927271	-0.091023	4.010367
472.107972	5497.180717	15.932275	-0.090986	4.007516
472.100413	5489.137168	15.937280	-0.090980	4.004646
472.402971	5481.203724	15.942285	-0.091031	4.001819
471.973876	5473.191452	15.947290	-0.090945	3.998949
471.809012	5465.255539	15.952295	-0.090910	3.996109
471.703429	5457.238788	15.957299	-0.090885	3.993239
472.039095	5449.187621	15.962304	-0.090942	3.990362
472.096167	5441.181604	15.967309	-0.090947	3.987494
471.508501	5433.204512	15.972314	-0.090833	3.984624
471.553007	5425.225503	15.977319	-0.090836	3.981762
471.839938	5417.176147	15.982323	-0.090884	3.978876
471.174855	5409.266587	15.987328	-0.090755	3.976022
471.895162	5401.156412	15.992333	-0.090884	3.973119
471.583138	5393.184052	15.997338	-0.090820	3.970244
471.505354	5385.204331	16.002343	-0.090800	3.967369
471.416380	5377.187689	16.007347	-0.090779	3.964479
470.892057	5369.286823	16.012352	-0.090676	3.961620
471.658587	5361.203881	16.017357	-0.090813	3.958716
471.626984	5353.173408	16.022362	-0.090802	3.955815
471.271258	5345.247158	16.027367	-0.090731	3.952944
471.144177	5337.235051	16.032371	-0.090702	3.950044
471.247131	5329.143959	16.037376	-0.090716	3.947117
471.160567	5321.172709	16.042381	-0.090694	3.944228
470.784696	5313.253096	16.047386	-0.090619	3.941350
471.037058	5305.259946	16.052391	-0.090661	3.938455
470.697485	5297.239389	16.057395	-0.090592	3.935537
470.875192	5289.198240	16.062400	-0.090620	3.932619
471.040907	5281.185072	16.067405	-0.090646	3.929708
471.052631	5273.171200	16.072410	-0.090643	3.926793
471.045320	5265.176275	16.077415	-0.090636	3.923881
471.245341	5257.226966	16.082419	-0.090668	3.920988
470.876552	5249.260285	16.087424	-0.090594	3.918076
470.924190	5241.240092	16.092429	-0.090598	3.915150
471.458773	5233.153096	16.097434	-0.090692	3.912207
471.256536	5225.191391	16.102439	-0.090649	3.909293
471.149088	5217.243458	16.107443	-0.090624	3.906384
471.056720	5209.223955	16.112448	-0.090601	3.903447
470.943535	5201.253400	16.117453	-0.090575	3.900525
470.764140	5193.262646	16.122458	-0.090536	3.897592
470.809649	5185.266670	16.127463	-0.090540	3.894660
470.882758	5177.244603	16.132467	-0.090548	3.891716
470.697688	5169.228213	16.137472	-0.090508	3.888767
470.951405	5161.221999	16.142477	-0.090550	3.885828
470.874232	5153.232270	16.147482	-0.090530	3.882887
470.512174	5145.318566	16.152487	-0.090458	3.879965
470.476244	5137.326904	16.157491	-0.090446	3.877019
470.702780	5129.242161	16.162496	-0.090483	3.874042
471.067830	5121.089034	16.167501	-0.090545	3.871040
470.560454	5113.211330	16.172506	-0.090446	3.868120
469.976993	5105.260485	16.177511	-0.090332	3.865169
470.476057	5097.261825	16.182515	-0.090420	3.862220
469.942056	5089.281860	16.187520	-0.090315	3.859255
470.291617	5081.272539	16.192525	-0.090375	3.856294
470.447842	5073.231398	16.197530	-0.090399	3.853316
470.489347	5065.226503	16.202535	-0.090401	3.850346
470.020076	5057.300697	16.207539	-0.090308	3.847393
470.310434	5049.214978	16.212544	-0.090357	3.844394
470.722814	5041.281965	16.217549	-0.090429	3.841452
470.499081	5033.264188	16.222554	-0.090382	3.838463
470.301236	5025.319955	16.227559	-0.090340	3.835499
470.250836	5017.315615	16.232563	-0.090325	3.832514
470.061760	5009.306399	16.237568	-0.090285	3.829521
470.495697	5001.277068	16.242573	-0.090360	3.826533
470.376855	4993.261262	16.247578	-0.090333	3.823535
470.765454	4985.296148	16.252583	-0.090400	3.820564
470.748847	4977.307673	16.257587	-0.090392	3.817574
470.295393	4969.323903	16.262592	-0.090302	3.814573
470.348822	4961.340579	16.267597	-0.090307	3.811582
470.140797	4953.310914	16.272602	-0.090263	3.808565
469.821776	4945.361688	16.277607	-0.090198	3.805573
469.877351	4937.348994	16.282611	-0.090203	3.802563
470.078188	4929.316437	16.287616	-0.090235	3.799547
470.016128	4921.394812	16.292621	-0.090218	3.796564
470.197921	4913.264133	16.297626	-0.090247	3.793506
469.950614	4905.364762	16.302631	-0.090196	3.790523
470.119371	4897.305676	16.307635	-0.090222	3.787486
469.936534	4889.295199	16.312640	-0.090182	3.784458
470.190808	4881.354369	16.317645	-0.090225	3.781463
470.209169	4873.300585	16.322650	-0.090223	3.778418
469.927165	4865.374125	16.327655	-0.090165	3.775411
470.036504	4857.390271	16.332659	-0.090180	3.772390
469.954684	4849.320943	16.337664	-0.090160	3.769329
469.955572	4841.378902	16.342669	-0.090155	3.766316
469.864682	4833.356095	16.347674	-0.090132	3.763268
469.558849	4825.441216	16.352679	-0.090070	3.760253
469.652336	4817.435442	16.357683	-0.090082	3.757210
469.752474	4809.340586	16.362688	-0.090096	3.754132
469.807443	4801.426422	16.367693	-0.090101	3.751118
469.560731	4793.416639	16.372698	-0.090049	3.748059
469.611108	4785.377377	16.377703	-0.090054	3.744993
469.604784	4777.430038	16.382707	-0.090047	3.741958
469.527197	4769.408805	16.387712	-0.090027	3.738890
469.505414	4761.491776	16.392717	-0.090018	3.735862
469.335688	4753.448068	16.397722	-0.089981	3.732779
469.684496	4745.354691	16.402727	-0.090041	3.729686
469.557083	4737.437181	16.407731	-0.090012	3.726648
469.275356	4729.446791	16.412736	-0.089954	3.723574
469.285366	4721.503378	16.417741	-0.089951	3.720524
469.195145	4713.483745	16.422746	-0.089929	3.717439
469.312936	4705.435236	16.427751	-0.089946	3.714346
469.416008	4697.415430	16.432755	-0.089959	3.711260
469.492114	4689.360304	16.437760	-0.089968	3.708158
469.356480	4681.411710	16.442765	-0.089938	3.705089
469.106971	4673.497554	16.447770	-0.089886	3.702028
469.519959	4665.420648	16.452775	-0.089958	3.698919
469.423484	4657.466775	16.457779	-0.089935	3.695841
469.333312	4649.418342	16.462784	-0.089913	3.692724
469.417126	4641.421448	16.467789	-0.089923	3.689630
469.290870	4633.442995	16.472794	-0.089894	3.686534
469.178331	4625.452679	16.477799	-0.089868	3.683431
469.231305	4617.479619	16.482803	-0.089873	3.680337
468.984640	4609.516779	16.487808	-0.089821	3.677236
469.151141	4601.488434	16.492813	-0.089847	3.674118
469.101325	4593.512111	16.497818	-0.089833	3.671012
469.064130	4585.507255	16.502823	-0.089820	3.667893
469.264650	4577.475258	16.507827	-0.089852	3.664766
469.104612	4569.522905	16.512832	-0.089817	3.661659
469.134982	4561.541027	16.517837	-0.089818	3.658542
468.828932	4553.568544	16.522842	-0.089756	3.655417
468.953747	4545.533939	16.527847	-0.089774	3.652277
469.043715	4537.500659	16.532851	-0.089785	3.649134
469.032164	4529.534722	16.537856	-0.089778	3.646011
468.918725	4521.562087	16.542861	-0.089751	3.642881
468.902630	4513.576792	16.547866	-0.089743	3.639746
468.847169	4505.611494	16.552871	-0.089727	3.636614
468.908720	4497.613064	16.557875	-0.089734	3.633470
468.904579	4489.565944	16.562880	-0.089728	3.630303
468.931013	4481.600515	16.567885	-0.089727	3.627166
468.702154	4473.565218	16.572890	-0.089679	3.623991
468.591734	4465.613206	16.577895	-0.089654	3.620849
468.392232	4457.633459	16.582899	-0.089611	3.617692
468.505523	4449.613011	16.587904	-0.089627	3.614524
468.459630	4441.623650	16.592909	-0.089613	3.611362
468.638909	4433.567505	16.597914	-0.089641	3.608176
468.382256	4425.628744	16.602919	-0.089588	3.605022
468.355967	4417.681873	16.607923	-0.089578	3.601869
468.323452	4409.642625	16.612928	-0.089567	3.598675
468.328305	4401.660409	16.617933	-0.089563	3.595503
468.436536	4393.648637	16.622938	-0.089577	3.592319
468.252053	4385.644275	16.627943	-0.089538	3.589127
468.453105	4377.639857	16.632947	-0.089570	3.585943
468.301111	4369.649769	16.637952	-0.089536	3.582752
468.501242	4361.654080	16.642957	-0.089568	3.579566
468.384469	4353.675684	16.647962	-0.089541	3.576375
468.169364	4345.707889	16.652967	-0.089496	3.573182
468.209379	4337.694748	16.657971	-0.089498	3.569975
467.836526	4329.706457	16.662976	-0.089424	3.566764
467.930371	4321.688177	16.667981	-0.089436	3.563551
467.740919	4313.741169	16.672986	-0.089395	3.560356
467.424986	4305.793061	16.677991	-0.089331	3.557153
467.728519	4297.700640	16.682995	-0.089383	3.553909
467.709452	4289.696539	16.688000	-0.089374	3.550687
467.709307	4281.705251	16.693005	-0.089368	3.547468
467.739753	4273.626788	16.698010	-0.089369	3.544211
467.779168	4265.725173	16.703015	-0.089371	3.541024
467.719181	4257.735524	16.708019	-0.089355	3.537795
467.687064	4249.717100	16.713024	-0.089343	3.534552
467.875162	4241.746167	16.718029	-0.089373	3.531332
467.923965	4233.722293	16.723034	-0.089377	3.528084
467.883727	4225.718839	16.728039	-0.089364	3.524838
467.856296	4217.784078	16.733043	-0.089354	3.521617
467.908519	4209.755898	16.738048	-0.089358	3.518358
467.950288	4201.795825	16.743053	-0.089361	3.515123
467.884586	4193.806984	16.748058	-0.089343	3.511871
467.900974	4185.777776	16.753063	-0.089341	3.508601
467.845212	4177.778557	16.758067	-0.089326	3.505338
467.523191	4169.848309	16.763072	-0.089260	3.502092
467.686738	4161.810844	16.768077	-0.089286	3.498814
467.582834	4153.868407	16.773082	-0.089261	3.495564
467.553587	4145.853517	16.778087	-0.089250	3.492283
467.535458	4137.850627	16.783091	-0.089242	3.489005
467.639135	4129.822729	16.788096	-0.089256	3.485717
467.426093	4121.893825	16.793101	-0.089211	3.482457
467.642328	4113.818034	16.798106	-0.089246	3.479147
467.517418	4105.919155	16.803111	-0.089217	3.475895
467.552482	4097.868505	16.808115	-0.089218	3.472583
467.121103	4089.910118	16.813120	-0.089133	3.469291
467.521365	4081.876354	16.818125	-0.089202	3.465992
467.521343	4073.849987	16.823130	-0.089197	3.462679
467.575675	4065.863149	16.828135	-0.089202	3.459382
467.355057	4057.943277	16.833139	-0.089155	3.456100
467.153986	4049.917854	16.838144	-0.089113	3.452771
467.363128	4041.937506	16.843149	-0.089146	3.449472
467.268057	4033.956541	16.848154	-0.089124	3.446160
467.199697	4025.948777	16.853159	-0.089106	3.442833
467.269042	4017.984006	16.858163	-0.089113	3.439527
467.024144	4010.010054	16.863168	-0.089062	3.436202
467.001686	4002.016528	16.868173	-0.089053	3.432874
466.624994	3994.062412	16.873178	-0.088978	3.429546
466.960305	3986.037521	16.878183	-0.089035	3.426211
466.730592	3978.051705	16.883187	-0.088987	3.422869
466.757763	3970.025454	16.888192	-0.088987	3.419515
466.869399	3962.058923	16.893197	-0.089002	3.416186
466.490573	3954.040681	16.898202	-0.088926	3.412816
466.187020	3946.073347	16.903207	-0.088864	3.409465
466.291811	3938.086243	16.908211	-0.088879	3.406118
466.430400	3930.038704	16.913216	-0.088899	3.402743
466.502072	3922.053007	16.918221	-0.088907	3.399389
466.377566	3914.098497	16.923226	-0.088879	3.396037
466.251717	3906.093495	16.928231	-0.088850	3.392660
466.462457	3898.030807	16.933235	-0.088884	3.389268
466.392052	3890.038581	16.938240	-0.088866	3.385892
466.331256	3882.085299	16.943245	-0.088849	3.382530
466.370370	3874.045049	16.948250	-0.088851	3.379131
466.373891	3866.084489	16.953255	-0.088847	3.375761
466.314157	3858.127030	16.958259	-0.088830	3.372387
466.099364	3850.129919	16.963264	-0.088785	3.368987
465.883239	3842.169030	16.968269	-0.088740	3.365598
466.004000	3834.170116	16.973274	-0.088757	3.362203
466.116132	3826.151379	16.978279	-0.088772	3.358795
466.024534	3818.211257	16.983283	-0.088750	3.355410
465.920769	3810.199018	16.988288	-0.088726	3.351990
466.188801	3802.174857	16.993293	-0.088770	3.348576
465.855551	3794.204264	16.998298	-0.088703	3.345158
466.031147	3786.227105	17.003303	-0.088730	3.341753
465.855117	3778.262775	17.008307	-0.088692	3.338337
465.794353	3770.255718	17.013312	-0.088676	3.334904
465.732493	3762.262130	17.018317	-0.088659	3.331472
465.643437	3754.239260	17.023322	-0.088637	3.328024
465.754447	3746.241792	17.028327	-0.088653	3.324590
465.698848	3738.345713	17.033331	-0.088637	3.321190
465.870115	3730.273033	17.038336	-0.088664	3.317719
465.747454	3722.315374	17.043341	-0.088636	3.314283
465.789574	3714.299914	17.048346	-0.088638	3.310825
465.602279	3706.305507	17.053351	-0.088598	3.307363
465.619725	3698.303270	17.058355	-0.088596	3.303903
465.545378	3690.344369	17.063360	-0.088577	3.300454
465.522867	3682.366100	17.068365	-0.088568	3.296994
465.417515	3674.358431	17.073370	-0.088543	3.293516
465.862389	3666.288415	17.078375	-0.088620	3.290028
465.852525	3658.364339	17.083379	-0.088613	3.286582
465.334091	3650.427639	17.088384	-0.088511	3.283106
465.390043	3642.442025	17.093389	-0.088517	3.279629
465.390668	3634.440604	17.098394	-0.088511	3.276138
465.174784	3626.470467	17.103399	-0.088466	3.272649
465.485235	3618.422641	17.108403	-0.088519	3.269143
465.659052	3610.400186	17.113408	-0.088546	3.265639
465.421758	3602.484108	17.118413	-0.088496	3.262162
465.373813	3594.482202	17.123418	-0.088482	3.258651
464.949914	3586.557263	17.128423	-0.088398	3.255154
464.828763	3578.572411	17.133427	-0.088370	3.251639
464.635566	3570.542694	17.138432	-0.088329	3.248098
464.667883	3562.558137	17.143437	-0.088330	3.244583
464.979546	3554.538376	17.148442	-0.088382	3.241059
465.021614	3546.552483	17.153447	-0.088385	3.237536
464.742397	3538.593472	17.158451	-0.088328	3.234007
464.931682	3530.552596	17.163456	-0.088358	3.230458
464.985434	3522.567083	17.168461	-0.088362	3.226923
464.420318	3514.614358	17.173466	-0.088252	3.223373
464.336199	3506.618048	17.178471	-0.088231	3.219821
464.539434	3498.618761	17.183475	-0.088264	3.216275
464.599732	3490.559037	17.188480	-0.088270	3.212692
464.570396	3482.584788	17.193485	-0.088259	3.209139
464.787196	3474.572068	17.198490	-0.088294	3.205576
464.423224	3466.681098	17.203495	-0.088221	3.202039
463.964494	3458.767621	17.208499	-0.088130	3.198483
464.187757	3450.674833	17.213504	-0.088167	3.194872
464.234148	3442.741203	17.218509	-0.088170	3.191321
464.260380	3434.684010	17.223514	-0.088170	3.187710
464.252762	3426.657287	17.228519	-0.088163	3.184107
464.119877	3418.746234	17.233523	-0.088133	3.180546
464.143520	3410.740125	17.238528	-0.088132	3.176946
464.492440	3402.704502	17.243533	-0.088192	3.173342
464.588807	3394.699002	17.248538	-0.088205	3.169737
464.515877	3386.769568	17.253543	-0.088186	3.166154
464.501633	3378.809569	17.258547	-0.088178	3.162557
464.421501	3370.796824	17.263552	-0.088158	3.158928
464.295659	3362.879798	17.268557	-0.088129	3.155336
464.215125	3354.862112	17.273562	-0.088109	3.151697
464.249119	3346.847929	17.278567	-0.088110	3.148060
464.545352	3338.805397	17.283571	-0.088160	3.144418
464.160725	3330.887479	17.288576	-0.088083	3.140798
464.181773	3322.904378	17.293581	-0.088082	3.137162
464.463894	3314.836836	17.298586	-0.088129	3.133495
464.498945	3306.834647	17.303591	-0.088130	3.129843
464.367098	3298.926696	17.308595	-0.088100	3.126221
464.134492	3290.943978	17.313600	-0.088052	3.122557
463.982254	3282.993337	17.318605	-0.088018	3.118907
463.879247	3275.034218	17.323610	-0.087994	3.115251
464.083183	3266.969384	17.328615	-0.088027	3.111556
464.355988	3258.943726	17.333619	-0.088072	3.107878
463.898007	3251.010723	17.338624	-0.087982	3.104204
464.186624	3243.048355	17.343629	-0.088030	3.100547
464.039488	3235.077210	17.348634	-0.087997	3.096862
463.837709	3227.089444	17.353639	-0.087955	3.093162
464.034185	3219.045183	17.358643	-0.087986	3.089450
464.204435	3211.053587	17.363648	-0.088012	3.085756
464.095562	3203.108734	17.368653	-0.087987	3.082067
464.095132	3195.109260	17.373658	-0.087982	3.078353
464.014268	3187.155883	17.378663	-0.087961	3.074652
464.108719	3179.129084	17.383667	-0.087974	3.070921
463.535693	3171.176005	17.388672	-0.087862	3.067188
463.658961	3163.164449	17.393677	-0.087879	3.063456
463.510255	3155.222755	17.398682	-0.087846	3.059739
463.581328	3147.213334	17.403687	-0.087854	3.055997
463.355536	3139.259800	17.408691	-0.087807	3.052262
463.542326	3131.213360	17.413696	-0.087837	3.048499
463.360460	3123.284926	17.418701	-0.087798	3.044768
463.311940	3115.297296	17.423706	-0.087783	3.041012
463.641771	3107.251526	17.428711	-0.087839	3.037242
463.248131	3099.348912	17.433715	-0.087761	3.033499
463.069508	3091.347064	17.438720	-0.087722	3.029716
463.339974	3083.316057	17.443725	-0.087767	3.025936
463.344699	3075.325552	17.448730	-0.087763	3.022157
463.236316	3067.375416	17.453735	-0.087738	3.018387
463.411935	3059.361836	17.458739	-0.087765	3.014597
463.277506	3051.398286	17.463744	-0.087735	3.010810
463.338063	3043.414308	17.468749	-0.087741	3.007018
463.248475	3035.438616	17.473754	-0.087719	3.003218
463.231751	3027.468588	17.478759	-0.087711	2.999420
463.443164	3019.483040	17.483763	-0.087745	2.995621
463.348092	3011.487341	17.488768	-0.087722	2.991796
463.146816	3003.535456	17.493773	-0.087679	2.987982
462.969016	2995.522913	17.498778	-0.087641	2.984136
463.068850	2987.559950	17.503783	-0.087654	2.980322
463.076717	2979.585181	17.508787	-0.087650	2.976493
462.789084	2971.605142	17.513792	-0.087591	2.972642
462.829609	2963.626096	17.518797	-0.087594	2.968803
462.439342	2955.657985	17.523802	-0.087516	2.964941
462.890753	2947.621556	17.528807	-0.087595	2.961086
462.754641	2939.674616	17.533811	-0.087564	2.957238
462.826782	2931.644530	17.538816	-0.087572	2.953356
462.878963	2923.673499	17.543821	-0.087577	2.949496
462.681528	2915.702172	17.548826	-0.087535	2.945618
462.667118	2907.744562	17.553831	-0.087527	2.941751
462.704499	2899.765458	17.558835	-0.087528	2.937871
462.819492	2891.723033	17.563840	-0.087545	2.933960
462.903904	2883.764992	17.568845	-0.087555	2.930083
462.606425	2875.798794	17.573850	-0.087494	2.926176
462.372234	2867.864484	17.578855	-0.087446	2.922283
462.575317	2859.863902	17.583859	-0.087478	2.918375
462.585631	2851.893350	17.588864	-0.087475	2.914467
462.578363	2843.841400	17.593869	-0.087468	2.910513
462.532846	2835.864287	17.598874	-0.087455	2.906588
462.308553	2827.901387	17.603879	-0.087408	2.902655
462.562580	2819.926473	17.608883	-0.087450	2.898737
461.738209	2812.032661	17.613888	-0.087291	2.894794
462.146247	2803.963020	17.618893	-0.087362	2.890827
462.135966	2795.993315	17.623898	-0.087354	2.886881
462.042928	2788.015480	17.628903	-0.087332	2.882920
462.029163	2780.023408	17.633907	-0.087324	2.878952
461.944873	2772.060973	17.638912	-0.087303	2.874989
462.011685	2764.086253	17.643917	-0.087310	2.871023
461.991213	2756.079182	17.648922	-0.087301	2.867030
461.978611	2748.099259	17.653927	-0.087294	2.863046
462.006604	2740.137708	17.658931	-0.087294	2.859067
461.867665	2732.175018	17.663936	-0.087263	2.855073
461.964459	2724.182416	17.668941	-0.087275	2.851072
462.016252	2716.172550	17.673946	-0.087280	2.847054
461.677936	2708.256966	17.678951	-0.087212	2.843055
461.995779	2700.252895	17.683955	-0.087265	2.839044
462.064984	2692.283485	17.688960	-0.087273	2.835031
462.023498	2684.292292	17.693965	-0.087260	2.830994
461.814593	2676.334225	17.698970	-0.087216	2.826958
461.794684	2668.315970	17.703975	-0.087207	2.822898
461.906800	2660.346958	17.708979	-0.087223	2.818864
461.447624	2652.441138	17.713984	-0.087132	2.814823
461.304001	2644.469312	17.718989	-0.087100	2.810761
461.434014	2636.446749	17.723994	-0.087119	2.806683
461.477378	2628.450111	17.728999	-0.087122	2.802607
461.077420	2620.556328	17.734003	-0.087042	2.798552
461.201877	2612.519201	17.739008	-0.087060	2.794449
461.223174	2604.554567	17.744013	-0.087059	2.790371
461.014991	2596.569993	17.749018	-0.087015	2.786262
460.857001	2588.616334	17.754023	-0.086980	2.782167
461.225759	2580.586648	17.759027	-0.087043	2.778058
460.790615	2572.655766	17.764032	-0.086957	2.773946
461.011578	2564.651254	17.769037	-0.086993	2.769829
460.891163	2556.680625	17.774042	-0.086965	2.765702
460.546225	2548.770756	17.779047	-0.086896	2.761587
460.372300	2540.833996	17.784051	-0.086858	2.757463
460.600559	2532.751015	17.789056	-0.086896	2.753281
460.773832	2524.719107	17.794061	-0.086923	2.749116
460.964583	2516.693600	17.799066	-0.086953	2.744949
460.941863	2508.760006	17.804071	-0.086943	2.740810
460.620720	2500.878149	17.809075	-0.086878	2.736674
460.763362	2492.825397	17.814080	-0.086900	2.732471
460.926650	2484.831911	17.819085	-0.086925	2.728294
460.946876	2476.843919	17.824090	-0.086923	2.724104
460.805010	2468.939294	17.829095	-0.086892	2.719941
460.454239	2461.064236	17.834099	-0.086821	2.715775
460.445924	2453.027092	17.839104	-0.086814	2.711538
460.534634	2445.038683	17.844109	-0.086826	2.707326
460.368156	2437.039765	17.849114	-0.086789	2.703086
460.611180	2429.064656	17.854119	-0.086829	2.698879
460.812238	2421.058696	17.859123	-0.086862	2.694645
460.514931	2413.118009	17.864128	-0.086801	2.690408
460.409587	2405.183099	17.869133	-0.086776	2.686179
460.554589	2397.189306	17.874138	-0.086798	2.681928
460.424636	2389.249204	17.879143	-0.086769	2.677682
460.254765	2381.306804	17.884147	-0.086732	2.673425
460.291894	2373.265040	17.889152	-0.086733	2.669121
460.168941	2365.315731	17.894157	-0.086705	2.664849
460.309779	2357.299268	17.899162	-0.086726	2.660552
460.121736	2349.369114	17.904167	-0.086686	2.656273
460.140280	2341.412540	17.909171	-0.086684	2.651986
459.788747	2333.455760	17.914176	-0.086613	2.647668
459.804711	2325.472870	17.919181	-0.086611	2.643352
459.829584	2317.489806	17.924186	-0.086611	2.639031
460.057473	2309.497543	17.929191	-0.086648	2.634710
459.906733	2301.553142	17.934195	-0.086614	2.630384
459.770563	2293.577960	17.939200	-0.086584	2.626034
460.054545	2285.577546	17.944205	-0.086631	2.621692
459.760132	2277.663407	17.949210	-0.086571	2.617350
459.824543	2269.671322	17.954215	-0.086578	2.612983
459.579849	2261.743990	17.959219	-0.086527	2.608623
459.426484	2253.741323	17.964224	-0.086494	2.604220
459.290577	2245.840592	17.969229	-0.086463	2.599868
459.054337	2237.892971	17.974234	-0.086414	2.595475
459.420306	2229.746659	17.979239	-0.086477	2.591007
459.217498	2221.768499	17.984243	-0.086434	2.586584
459.284975	2213.798473	17.989248	-0.086441	2.582177
459.409276	2205.836237	17.994253	-0.086459	2.577772
459.145773	2197.923394	17.999258	-0.086405	2.573358
459.363641	2189.904982	18.004263	-0.086440	2.568913
459.278220	2181.981054	18.009267	-0.086419	2.564490
459.115920	2174.046248	18.014272	-0.086383	2.560049
458.986770	2166.101286	18.019277	-0.086354	2.555597
459.194762	2158.075210	18.024282	-0.086388	2.551115
458.892044	2150.168597	18.029287	-0.086326	2.546656
459.178193	2142.148016	18.034291	-0.086374	2.542167
459.215392	2134.175788	18.039296	-0.086376	2.537680
459.068707	2126.240661	18.044301	-0.086343	2.533192
458.907221	2118.282672	18.049306	-0.086308	2.528683
458.585770	2110.354315	18.054311	-0.086243	2.524170
458.881409	2102.361661	18.059315	-0.086293	2.519658
458.824586	2094.395946	18.064320	-0.086277	2.515128
458.817220	2086.417128	18.069325	-0.086270	2.510585
458.826650	2078.444834	18.074330	-0.086267	2.506039
458.667115	2070.498242	18.079335	-0.086232	2.501487
458.851953	2062.500536	18.084339	-0.086261	2.496923
458.572859	2054.566206	18.089344	-0.086204	2.492352
458.775793	2046.562952	18.094349	-0.086236	2.487770
458.836657	2038.596082	18.099354	-0.086242	2.483189
458.775783	2030.650295	18.104359	-0.086226	2.478603
458.657853	2022.733185	18.109363	-0.086199	2.474020
458.521339	2014.781236	18.114368	-0.086168	2.469408
458.285628	2006.847279	18.119373	-0.086119	2.464789
458.074957	1998.914845	18.124378	-0.086075	2.460165
457.948804	1990.951771	18.129383	-0.086046	2.455520
458.221739	1982.918912	18.134387	-0.086091	2.450857
457.992975	1974.961196	18.139392	-0.086043	2.446190
458.031710	1967.029560	18.144397	-0.086045	2.441550
457.604269	1959.128368	18.149402	-0.085961	2.436883
457.646343	1951.110844	18.154407	-0.085963	2.432175
458.051169	1943.045582	18.159411	-0.086033	2.427458
457.797590	1935.112024	18.164416	-0.085981	2.422758
458.098567	1927.121281	18.169421	-0.086032	2.418059
457.690438	1919.226402	18.174426	-0.085951	2.413352
457.764168	1911.251604	18.179431	-0.085959	2.408626
457.907402	1903.269212	18.184435	-0.085980	2.403891
457.821752	1895.321032	18.189440	-0.085959	2.399150
457.809042	1887.401567	18.194445	-0.085952	2.394422
457.976431	1879.404211	18.199450	-0.085978	2.389652
457.957855	1871.439370	18.204455	-0.085969	2.384878
457.773122	1863.536479	18.209459	-0.085929	2.380118
457.678942	1855.585207	18.214464	-0.085907	2.375326
457.697477	1847.616453	18.219469	-0.085905	2.370523
457.353040	1839.698177	18.224474	-0.085835	2.365712
457.421081	1831.731890	18.229479	-0.085843	2.360895
457.430065	1823.812177	18.234483	-0.085839	2.356092
457.475583	1815.798707	18.239488	-0.085843	2.351224
457.398645	1807.846342	18.244493	-0.085823	2.346374
457.251381	1799.897041	18.249498	-0.085790	2.341510
457.281439	1791.929461	18.254503	-0.085791	2.336640
457.294890	1783.975897	18.259507	-0.085788	2.331766
457.041082	1776.032572	18.264512	-0.085736	2.326866
457.148145	1768.070158	18.269517	-0.085750	2.321974
456.910875	1760.177212	18.274522	-0.085701	2.317086
457.141128	1752.168259	18.279527	-0.085738	2.312155
457.546668	1744.153633	18.284531	-0.085809	2.307226
456.699603	1736.336348	18.289536	-0.085646	2.302301
456.895502	1728.352197	18.294541	-0.085677	2.297351
456.977759	1720.381039	18.299546	-0.085687	2.292389
456.892313	1712.419559	18.304551	-0.085666	2.287407
457.018493	1704.474309	18.309555	-0.085684	2.282443
456.836026	1696.552508	18.314560	-0.085645	2.277457
456.989915	1688.564774	18.319565	-0.085669	2.272447
456.423389	1680.670697	18.324570	-0.085558	2.267422
456.285442	1672.709159	18.329575	-0.085527	2.262380
456.611200	1664.704249	18.334579	-0.085582	2.257341
456.305918	1656.781725	18.339584	-0.085520	2.252287
456.080490	1648.888821	18.344589	-0.085473	2.247248
455.930338	1640.941334	18.349594	-0.085440	2.242169
456.431119	1632.886277	18.354599	-0.085528	2.237068
456.474504	1624.958243	18.359603	-0.085531	2.231996
456.362660	1617.009018	18.364608	-0.085505	2.226885
456.304055	1609.073524	18.369613	-0.085489	2.221775
456.059423	1601.188094	18.374618	-0.085438	2.216669
456.162056	1593.203930	18.379623	-0.085452	2.211520
456.424081	1585.219358	18.384627	-0.085495	2.206372
456.203990	1577.313525	18.389632	-0.085449	2.201219
456.228236	1569.389560	18.394637	-0.085448	2.196065
456.150321	1561.462088	18.399642	-0.085429	2.190887
456.116353	1553.493735	18.404647	-0.085417	2.185674
455.930106	1545.604133	18.409651	-0.085377	2.180486
456.397017	1537.555153	18.414656	-0.085459	2.175242
456.438211	1529.624560	18.419661	-0.085461	2.170024
456.181487	1521.705963	18.424666	-0.085408	2.164772
455.976843	1513.818148	18.429671	-0.085365	2.159533
456.139999	1505.877405	18.434675	-0.085390	2.154282
456.352466	1497.875192	18.439680	-0.085425	2.148981
456.269426	1489.959788	18.444685	-0.085404	2.143696
456.178933	1482.033052	18.449690	-0.085382	2.138391
456.066559	1474.115457	18.454695	-0.085356	2.133076
456.116991	1466.180019	18.459699	-0.085360	2.127751
456.074221	1458.226440	18.464704	-0.085347	2.122392
456.135803	1450.308822	18.469709	-0.085353	2.117054
455.765790	1442.407478	18.474714	-0.085279	2.111671
455.568488	1434.458067	18.479719	-0.085237	2.106259
455.172161	1426.589514	18.484723	-0.085158	2.100868
455.456754	1418.579121	18.489728	-0.085206	2.095433
455.595098	1410.616716	18.494733	-0.085226	2.090003
455.717989	1402.638011	18.499738	-0.085244	2.084546
455.773770	1394.731388	18.504743	-0.085249	2.079118
455.715723	1386.830990	18.509747	-0.085233	2.073668
455.266781	1378.965034	18.514752	-0.085144	2.068188
455.265572	1371.023364	18.519757	-0.085139	2.062687
454.862851	1363.155485	18.524762	-0.085059	2.057181
454.980862	1355.178961	18.529767	-0.085075	2.051637
454.940082	1347.255497	18.534771	-0.085063	2.046100
454.903542	1339.303221	18.539776	-0.085051	2.040528
454.952364	1331.378731	18.544781	-0.085054	2.034968
454.845880	1323.454929	18.549786	-0.085029	2.029378
454.849137	1315.494620	18.554791	-0.085025	2.023758
454.887318	1307.571480	18.559795	-0.085027	2.018153
454.878017	1299.636278	18.564800	-0.085020	2.012518
454.901480	1291.711411	18.569805	-0.085019	2.006878
454.627126	1283.830117	18.574810	-0.084963	2.001222
454.703674	1275.888376	18.579815	-0.084972	1.995544
454.903312	1267.943643	18.584819	-0.085004	1.989861
454.637244	1260.059953	18.589824	-0.084949	1.984155
454.672996	1252.142162	18.594829	-0.084950	1.978441
454.589836	1244.231189	18.599834	-0.084930	1.972702
454.332950	1236.343975	18.604839	-0.084877	1.966945
454.613201	1228.376582	18.609843	-0.084924	1.961171
454.520197	1220.478630	18.614848	-0.084901	1.955390
454.560449	1212.562562	18.619853	-0.084903	1.949593
454.635610	1204.612764	18.624858	-0.084912	1.943758
454.321416	1196.736557	18.629863	-0.084848	1.937917
454.389480	1188.808506	18.634867	-0.084856	1.932062
454.308679	1180.882136	18.639872	-0.084836	1.926174
454.375453	1172.963574	18.644877	-0.084843	1.920290
454.270872	1165.079699	18.649882	-0.084818	1.914394
454.011654	1157.200110	18.654887	-0.084765	1.908466
454.061700	1149.270195	18.659891	-0.084769	1.902517
454.257995	1141.322693	18.664896	-0.084800	1.896553
454.171209	1133.429689	18.669901	-0.084779	1.890578
454.068025	1125.520999	18.674906	-0.084754	1.884571
453.949827	1117.650527	18.679911	-0.084727	1.878572
454.014248	1109.745276	18.684915	-0.084734	1.872549
453.924582	1101.821756	18.689920	-0.084712	1.866473
453.794043	1093.944341	18.694925	-0.084683	1.860409
454.134438	1085.978964	18.699930	-0.084741	1.854313
454.024889	1078.077510	18.704935	-0.084715	1.848192
453.745557	1070.241262	18.709939	-0.084658	1.842082
453.543946	1062.384807	18.714944	-0.084615	1.835945
453.482922	1054.481784	18.719949	-0.084599	1.829767
453.258510	1046.598062	18.724954	-0.084552	1.823564
452.966635	1038.722611	18.729959	-0.084492	1.817339
453.499464	1030.732705	18.734963	-0.084586	1.811102
453.384758	1022.837449	18.739968	-0.084560	1.804839
453.139523	1015.019733	18.744973	-0.084509	1.798600
453.245272	1007.088383	18.749978	-0.084523	1.792291
453.422776	999.120073	18.754983	-0.084551	1.785940
453.387595	991.243882	18.759987	-0.084540	1.779614
452.919730	983.439932	18.764992	-0.084447	1.773269
453.067537	975.513263	18.769997	-0.084470	1.766880
452.711760	967.676310	18.775002	-0.084398	1.760476
453.023743	959.744914	18.780007	-0.084451	1.754057
453.220660	951.828966	18.785011	-0.084483	1.747612
452.939045	943.986084	18.790016	-0.084425	1.741142
452.963069	936.110567	18.795021	-0.084424	1.734661
452.382662	928.334949	18.800026	-0.084311	1.728159
452.718566	920.365588	18.805031	-0.084368	1.721591
452.628189	912.525253	18.810035	-0.084346	1.715050
452.553746	904.638919	18.815040	-0.084327	1.708447
452.865334	896.700371	18.820045	-0.084380	1.701826
452.752474	888.861718	18.825050	-0.084354	1.695207
452.551806	881.005384	18.830055	-0.084311	1.688535
452.536567	873.150105	18.835059	-0.084303	1.681863
452.645681	865.260161	18.840064	-0.084319	1.675151
452.460004	857.432330	18.845069	-0.084279	1.668425
452.150657	849.608383	18.850074	-0.084216	1.661658
452.278226	841.715349	18.855079	-0.084235	1.654864
452.468561	833.823846	18.860083	-0.084265	1.648052
452.260811	825.985144	18.865088	-0.084221	1.641203
452.335547	818.126833	18.870093	-0.084230	1.634347
452.203879	810.257528	18.875098	-0.084200	1.627424
451.997882	802.419376	18.880103	-0.084157	1.620487
452.233496	794.532972	18.885107	-0.084195	1.613541
452.245412	786.658489	18.890112	-0.084192	1.606544
452.344177	778.806351	18.895117	-0.084206	1.599549
452.112097	771.017519	18.900122	-0.084157	1.592531
451.975787	763.179612	18.905127	-0.084127	1.585453
451.918454	755.374706	18.910131	-0.084111	1.578384
451.816931	747.522940	18.915136	-0.084087	1.571234
451.548452	739.736862	18.920141	-0.084032	1.564086
451.938106	731.829874	18.925146	-0.084099	1.556893
451.727542	724.016704	18.930151	-0.084055	1.549663
451.800039	716.176689	18.935155	-0.084063	1.542417
451.576697	708.383933	18.940160	-0.084016	1.535136
451.570827	700.546592	18.945165	-0.084010	1.527811
451.385637	692.744295	18.950170	-0.083971	1.520457
451.650096	684.872516	18.955175	-0.084015	1.513070
451.829319	677.034301	18.960179	-0.084043	1.505666
451.772793	669.230883	18.965184	-0.084027	1.498222
451.416030	661.481222	18.970189	-0.083956	1.490745
451.337282	653.679257	18.975194	-0.083936	1.483224
451.246589	645.884534	18.980199	-0.083914	1.475670
451.317910	638.029139	18.985203	-0.083922	1.468043
451.188038	630.230414	18.990208	-0.083893	1.460400
451.136601	622.447454	18.995213	-0.083878	1.452745
451.055053	614.644709	19.000218	-0.083858	1.445024
451.145098	606.843735	19.005223	-0.083869	1.437292
451.070606	599.076144	19.010227	-0.083850	1.429525
450.740592	591.326023	19.015232	-0.083784	1.421690
451.012640	583.494404	19.020237	-0.083829	1.413830
451.222185	575.668224	19.025242	-0.083863	1.405921
451.222647	567.907730	19.030247	-0.083858	1.397999
450.721220	560.231885	19.035251	-0.083760	1.390033
450.516344	552.469996	19.040256	-0.083717	1.381983
450.749993	544.658565	19.045261	-0.083755	1.373910
450.497581	536.922681	19.050266	-0.083703	1.365784
450.565962	529.151215	19.055271	-0.083710	1.357628
450.450211	521.419741	19.060275	-0.083684	1.349433
450.160938	513.706570	19.065280	-0.083625	1.341176
450.199405	505.956027	19.070285	-0.083627	1.332886
450.423711	498.156600	19.075290	-0.083664	1.324526
450.438707	490.427937	19.080295	-0.083661	1.316151
450.471103	482.608148	19.085299	-0.083662	1.307626
450.338119	474.890196	19.090304	-0.083632	1.299127
450.345332	467.169536	19.095309	-0.083629	1.290595
450.153136	459.497642	19.100314	-0.083588	1.282022
450.293216	451.750185	19.105319	-0.083609	1.273371
450.340363	444.049793	19.110323	-0.083612	1.264695
450.287912	436.354374	19.115328	-0.083598	1.255946
449.861126	428.737906	19.120333	-0.083513	1.247154
449.869823	421.042232	19.125338	-0.083510	1.238293
449.872961	413.348200	19.130343	-0.083505	1.229368
449.827598	405.671211	19.135347	-0.083492	1.220389
449.685762	398.012557	19.140352	-0.083460	1.211346
449.862100	390.309990	19.145357	-0.083488	1.202246
449.704660	382.685614	19.150362	-0.083454	1.193103
449.384159	375.077040	19.155367	-0.083389	1.183874
449.789369	367.366205	19.160371	-0.083459	1.174600
449.778139	359.712644	19.165376	-0.083452	1.165234
449.600867	352.133238	19.170381	-0.083414	1.155849
449.365329	344.523902	19.175386	-0.083366	1.146338
449.226156	336.920114	19.180391	-0.083335	1.136775
449.172174	329.317896	19.185395	-0.083320	1.127151
449.076904	321.723230	19.190400	-0.083297	1.117444
449.059895	314.133908	19.195405	-0.083289	1.107677
448.960841	306.564803	19.200410	-0.083265	1.097831
448.958870	298.975661	19.205415	-0.083260	1.087891
448.984050	291.421006	19.210419	-0.083260	1.077912
448.829905	283.880918	19.215424	-0.083226	1.067817
448.620113	276.370849	19.220429	-0.083182	1.057654
448.569267	268.845757	19.225434	-0.083168	1.047409
448.508749	261.329592	19.230439	-0.083151	1.037072
448.361456	253.837773	19.235443	-0.083119	1.026645
448.353957	246.330756	19.240448	-0.083113	1.016123
448.347029	238.840518	19.245453	-0.083106	1.005515
448.438315	231.358534	19.250458	-0.083119	0.994831
448.058523	223.938155	19.255463	-0.083043	0.984000
448.249008	216.452874	19.260467	-0.083073	0.973100
448.189923	209.013967	19.265472	-0.083058	0.962081
447.966392	201.649370	19.270477	-0.083011	0.951002
448.075089	194.223083	19.275482	-0.083026	0.939788
447.857126	186.869413	19.280487	-0.082981	0.928461
447.508527	179.579110	19.285491	-0.082911	0.917058
447.478171	172.217750	19.290496	-0.082901	0.905487
447.483414	164.880478	19.295501	-0.082897	0.893814
447.500719	157.554941	19.300506	-0.082895	0.882010
447.373124	150.288406	19.305511	-0.082867	0.870101
447.472928	143.000122	19.310515	-0.082881	0.858057
447.167130	135.801413	19.315520	-0.082819	0.845872
446.938806	128.623548	19.320525	-0.082772	0.833567
446.886626	121.412485	19.325530	-0.082757	0.821075
446.850190	114.231329	19.330535	-0.082746	0.808448
446.802676	107.101721	19.335539	-0.082732	0.795709
446.450033	100.030923	19.340544	-0.082662	0.782772
446.432119	92.947516	19.345549	-0.082654	0.769704
446.506435	85.875462	19.350554	-0.082663	0.756463
446.143086	78.906943	19.355559	-0.082591	0.743035
445.995839	72.127789	19.360563	-0.082559	0.729807