Fri Apr 16 18:45:14 2021

Number of Points = 3643
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.414918	-0.144106	0.000000	-0.000076	0.309512

1.387473	-0.140402	0.005005	-0.000071	0.309506
1.257732	-0.114709	0.010010	-0.000047	0.309516
1.177103	-0.101171	0.015014	-0.000032	0.309511
1.202657	-0.106436	0.020019	-0.000036	0.309508
1.352001	-0.133349	0.025024	-0.000064	0.309509
1.342454	-0.130905	0.030029	-0.000062	0.309512
1.284449	-0.119854	0.035034	-0.000052	0.309515
0.982813	-0.065539	0.040038	0.000005	0.309512
1.194229	-0.104076	0.045043	-0.000035	0.309511
1.221791	-0.107035	0.050048	-0.000040	0.309521
1.215587	-0.108855	0.055053	-0.000039	0.309507
1.300773	-0.123155	0.060058	-0.000054	0.309513
1.290276	-0.141282	0.065062	-0.000052	0.309419
1.190306	-0.163314	0.070067	-0.000034	0.309231
1.162505	-0.156903	0.075072	-0.000029	0.309237
0.910604	-0.111399	0.080077	0.000018	0.309236
0.885547	-0.104870	0.085082	0.000023	0.309245
0.532539	-0.040520	0.090086	0.000089	0.309246
1.035114	-0.134318	0.095091	-0.000005	0.309234
1.053705	-0.145228	0.100096	-0.000008	0.309199
0.567012	-0.119667	0.105101	0.000082	0.308904
0.752018	-0.151940	0.110106	0.000048	0.308911
0.871568	-0.175061	0.115110	0.000026	0.308904
0.707846	-0.145177	0.120115	0.000056	0.308905
0.873706	-0.175204	0.125120	0.000025	0.308905
0.879031	-0.209363	0.130125	0.000024	0.308749
0.737854	-0.215396	0.135130	0.000051	0.308601
0.821970	-0.232861	0.140134	0.000035	0.308590
0.960110	-0.258347	0.145139	0.000009	0.308589
1.174410	-0.301437	0.150144	-0.000031	0.308569
1.256480	-0.383448	0.155149	-0.000046	0.308254
1.173705	-0.366838	0.160154	-0.000030	0.308261
1.189331	-0.370641	0.165158	-0.000033	0.308257
1.143212	-0.391000	0.170163	-0.000025	0.308122
1.189968	-0.430318	0.175168	-0.000033	0.307977
1.118304	-0.418331	0.180173	-0.000020	0.307972
1.148255	-0.435726	0.185178	-0.000025	0.307916
1.088288	-0.485133	0.190182	-0.000014	0.307632
1.113718	-0.490559	0.195187	-0.000019	0.307628
1.340698	-0.541093	0.200192	-0.000061	0.307585
1.177036	-0.569576	0.205197	-0.000031	0.307311
1.099445	-0.553696	0.210202	-0.000016	0.307319
1.101492	-0.577813	0.215206	-0.000017	0.307207
1.270514	-0.655917	0.220211	-0.000048	0.306984
1.332262	-0.665493	0.225216	-0.000059	0.306991
0.996250	-0.647836	0.230221	0.000003	0.306787
1.148991	-0.690855	0.235226	-0.000025	0.306715
0.967968	-0.671000	0.240230	0.000008	0.306653
0.648074	-0.670021	0.245235	0.000068	0.306383
1.152655	-0.762560	0.250240	-0.000026	0.306379
1.200449	-0.817903	0.255245	-0.000035	0.306159
1.239238	-0.845358	0.260250	-0.000042	0.306062
1.212606	-0.866068	0.265254	-0.000037	0.305941
1.244219	-0.914759	0.270259	-0.000043	0.305738
1.001874	-0.880586	0.275264	0.000002	0.305691
1.064318	-0.937308	0.280269	-0.000009	0.305476
1.109479	-0.947829	0.285274	-0.000018	0.305465
0.910207	-0.979784	0.290278	0.000020	0.305142
0.781963	-0.955284	0.295283	0.000043	0.305148
0.898347	-1.039399	0.300288	0.000022	0.304849
0.927143	-1.050544	0.305293	0.000017	0.304821
0.876656	-1.102626	0.310298	0.000026	0.304530
0.709892	-1.077280	0.315302	0.000057	0.304506
0.715854	-1.132655	0.320307	0.000056	0.304248
0.865090	-1.164447	0.325312	0.000028	0.304226
0.908031	-1.243986	0.330317	0.000020	0.303884
0.825631	-1.237373	0.335322	0.000036	0.303844
0.708924	-1.273263	0.340326	0.000057	0.303572
0.160107	-1.187558	0.345331	0.000160	0.303505
0.593544	-1.318598	0.350336	0.000079	0.303256
0.454131	-1.317839	0.355341	0.000105	0.303139
0.489122	-1.360352	0.360346	0.000098	0.302966
0.407770	-1.387243	0.365350	0.000114	0.302767
0.536454	-1.441607	0.370355	0.000090	0.302619
0.520428	-1.492854	0.375360	0.000093	0.302360
0.578086	-1.525922	0.380365	0.000082	0.302251
0.560889	-1.579366	0.385370	0.000085	0.301980
0.610353	-1.617781	0.390374	0.000076	0.301839
0.314236	-1.594980	0.395379	0.000131	0.301691
0.672017	-1.717906	0.400384	0.000065	0.301413
0.629774	-1.739607	0.405389	0.000073	0.301271
0.375627	-1.739146	0.410394	0.000120	0.301052
0.424441	-1.795822	0.415398	0.000111	0.300822
0.691351	-1.873653	0.420403	0.000061	0.300681
0.543468	-1.885346	0.425408	0.000089	0.300495
0.377262	-1.905490	0.430413	0.000120	0.300252
0.331984	-1.930282	0.435418	0.000128	0.300093
0.221916	-1.963779	0.440422	0.000149	0.299835
0.023502	-1.975343	0.445427	0.000186	0.299605
-0.023041	-1.997807	0.450432	0.000195	0.299456
-0.012977	-2.050068	0.455437	0.000193	0.299212
-0.308600	-2.044838	0.460442	0.000248	0.298977
-0.301623	-2.081246	0.465446	0.000247	0.298807
-0.329257	-2.126329	0.470451	0.000252	0.298564
-0.554125	-2.134141	0.475456	0.000294	0.298328
-0.781711	-2.127071	0.480461	0.000336	0.298162
-0.903110	-2.145517	0.485466	0.000359	0.297965
-1.089419	-2.168625	0.490470	0.000393	0.297688
-1.521333	-2.122033	0.495475	0.000474	0.297533
-1.586839	-2.155210	0.500480	0.000486	0.297313
-1.982761	-2.133488	0.505485	0.000560	0.297069
-2.234839	-2.110419	0.510490	0.000607	0.296958
-2.488130	-2.116664	0.515494	0.000654	0.296703
-2.397423	-2.172157	0.520499	0.000637	0.296512
-2.643469	-2.156588	0.525504	0.000683	0.296370
-2.930246	-2.165398	0.530509	0.000736	0.296072
-3.153520	-2.147506	0.535514	0.000778	0.295961
-3.585145	-2.114345	0.540518	0.000858	0.295740
-3.279421	-2.201668	0.545523	0.000801	0.295584
-3.584636	-2.163585	0.550528	0.000858	0.295499
-4.502651	-2.067101	0.555533	0.001029	0.295154
-4.207217	-2.133637	0.560538	0.000974	0.295091
-4.668617	-2.100068	0.565542	0.001060	0.294844
-4.628674	-2.139071	0.570547	0.001053	0.294688
-5.126524	-2.082614	0.575552	0.001145	0.294521
-4.967263	-2.152858	0.580557	0.001116	0.294318
-5.292401	-2.113103	0.585562	0.001176	0.294223
-5.345607	-2.161086	0.590566	0.001186	0.293939
-5.444757	-2.157276	0.595571	0.001205	0.293869
-5.761811	-2.159210	0.600576	0.001264	0.293576
-5.981718	-2.132196	0.605581	0.001305	0.293512
-6.097782	-2.163224	0.610586	0.001326	0.293255
-6.295192	-2.145274	0.615590	0.001363	0.293166
-6.862238	-2.083418	0.620595	0.001469	0.292962
-6.671053	-2.140847	0.625600	0.001433	0.292850
-7.080948	-2.110699	0.630605	0.001509	0.292631
-6.914821	-2.168423	0.635610	0.001479	0.292495
-7.719465	-2.058216	0.640614	0.001628	0.292316
-7.581398	-2.109687	0.645619	0.001603	0.292185
-7.316126	-2.196550	0.650624	0.001553	0.291994
-7.772856	-2.142569	0.655629	0.001638	0.291850
-8.015701	-2.128332	0.660634	0.001684	0.291701
-8.150769	-2.131848	0.665638	0.001709	0.291562
-8.567053	-2.095267	0.670643	0.001786	0.291368
-8.496269	-2.130224	0.675648	0.001773	0.291258
-8.604717	-2.153363	0.680653	0.001793	0.291045
-8.723980	-2.149614	0.685658	0.001816	0.290956
-9.190267	-2.108278	0.690662	0.001902	0.290740
-9.211646	-2.115958	0.695667	0.001906	0.290682
-9.217453	-2.152770	0.700672	0.001907	0.290493
-9.981746	-2.017876	0.705677	0.002050	0.290473
-9.770847	-2.122074	0.710682	0.002011	0.290145
-9.746787	-2.127331	0.715686	0.002006	0.290140
-10.042227	-2.131273	0.720691	0.002061	0.289852
-10.013139	-2.141683	0.725696	0.002056	0.289827
-10.199850	-2.158445	0.730701	0.002091	0.289573
-10.399637	-2.137026	0.735706	0.002128	0.289499
-10.926302	-2.072002	0.740710	0.002226	0.289345
-11.061707	-2.073015	0.745715	0.002251	0.289217
-10.519426	-2.193731	0.750720	0.002150	0.289106
-11.272274	-2.104585	0.755725	0.002290	0.288867
-11.143102	-2.133448	0.760730	0.002266	0.288840
-11.483181	-2.127025	0.765734	0.002330	0.288562
-11.397251	-2.144349	0.770739	0.002314	0.288553
-11.700582	-2.143128	0.775744	0.002370	0.288283
-12.141389	-2.072443	0.780749	0.002452	0.288235
-11.945650	-2.139693	0.785754	0.002416	0.288076
-12.411838	-2.079910	0.790758	0.002503	0.287951
-12.250071	-2.125081	0.795763	0.002472	0.287871
-12.275556	-2.172334	0.800768	0.002477	0.287610
-12.595008	-2.115882	0.805773	0.002537	0.287602
-12.900589	-2.117259	0.810778	0.002594	0.287315
-12.923999	-2.117344	0.815782	0.002598	0.287293
-12.934794	-2.154948	0.820787	0.002600	0.287094
-13.307357	-2.111630	0.825792	0.002669	0.286971
-13.344488	-2.119273	0.830797	0.002676	0.286898
-13.510271	-2.131003	0.835802	0.002707	0.286687
-13.699898	-2.097007	0.840806	0.002743	0.286684
-14.012480	-2.096706	0.845811	0.002801	0.286398
-13.874410	-2.130513	0.850816	0.002775	0.286354
-14.338889	-2.074201	0.855821	0.002862	0.286212
-14.561885	-2.066678	0.860826	0.002903	0.286045
-14.440043	-2.087965	0.865830	0.002880	0.286049
-14.556095	-2.127786	0.870835	0.002902	0.285741
-14.834228	-2.080096	0.875840	0.002954	0.285726
-14.996148	-2.074781	0.880845	0.002984	0.285604
-14.844900	-2.127164	0.885850	0.002956	0.285478
-14.984396	-2.104392	0.890854	0.002982	0.285464
-15.291052	-2.115035	0.895859	0.003039	0.285127
-15.346349	-2.102897	0.900864	0.003049	0.285138
-15.582853	-2.098148	0.905869	0.003093	0.284944
-15.690786	-2.103548	0.910874	0.003114	0.284816
-15.416801	-2.161246	0.915878	0.003063	0.284776
-16.113942	-2.091490	0.920883	0.003192	0.284486
-16.306298	-2.054300	0.925888	0.003228	0.284498
-16.568561	-2.038452	0.930893	0.003277	0.284336
-16.458755	-2.082822	0.935898	0.003257	0.284211
-16.391764	-2.096993	0.940902	0.003244	0.284201
-16.852727	-2.079746	0.945907	0.003330	0.283862
-16.650623	-2.115036	0.950912	0.003292	0.283869
-17.280940	-2.028060	0.955917	0.003410	0.283728
-17.596472	-2.002607	0.960922	0.003468	0.283565
-17.282786	-2.059490	0.965926	0.003410	0.283566
-17.429391	-2.082757	0.970931	0.003437	0.283311
-17.639668	-2.058214	0.975936	0.003477	0.283241
-17.821232	-2.035640	0.980941	0.003510	0.283187
-17.749954	-2.095659	0.985946	0.003497	0.282947
-17.929064	-2.063009	0.990950	0.003531	0.282947
-18.141566	-2.063323	0.995955	0.003570	0.282747
-18.283113	-2.064557	1.000960	0.003596	0.282609
-18.227842	-2.076133	1.005965	0.003586	0.282601
-18.278809	-2.125889	1.010970	0.003596	0.282299
-18.450747	-2.095265	1.015974	0.003628	0.282295
-18.742089	-2.070314	1.020979	0.003682	0.282152
-19.047267	-2.048574	1.025984	0.003739	0.281978
-19.247557	-2.014337	1.030989	0.003776	0.281967
-18.822137	-2.132331	1.035994	0.003697	0.281758
-19.521565	-2.019325	1.040998	0.003827	0.281685
-19.757709	-1.980906	1.046003	0.003871	0.281662
-19.442757	-2.097967	1.051008	0.003813	0.281355
-19.578909	-2.074545	1.056013	0.003838	0.281348
-19.893275	-2.043470	1.061018	0.003896	0.281213
-20.243089	-2.012127	1.066022	0.003962	0.281047
-20.024802	-2.052532	1.071027	0.003921	0.281043
-20.217815	-2.061617	1.076032	0.003957	0.280816
-20.793254	-1.974462	1.081037	0.004064	0.280725
-20.309750	-2.063216	1.086042	0.003974	0.280721
-20.528068	-2.065375	1.091046	0.004015	0.280505
-21.084339	-1.966160	1.096051	0.004118	0.280495
-20.804812	-2.039133	1.101056	0.004066	0.280381
-21.094193	-2.031922	1.106061	0.004120	0.280146
-21.321321	-1.987257	1.111066	0.004162	0.280163
-21.095456	-2.068917	1.116070	0.004121	0.279953
-21.362655	-2.044446	1.121075	0.004170	0.279829
-21.361312	-2.043278	1.126080	0.004170	0.279836
-21.624637	-2.059073	1.131085	0.004219	0.279506
-21.470571	-2.085907	1.136090	0.004190	0.279512
-21.655855	-2.074507	1.141094	0.004225	0.279397
-22.585778	-1.940312	1.146099	0.004398	0.279216
-22.174030	-2.012460	1.151104	0.004321	0.279230
-22.072924	-2.074835	1.156109	0.004303	0.279001
-22.673287	-1.986841	1.161114	0.004414	0.278891
-22.650331	-1.991006	1.166118	0.004410	0.278891
-22.809550	-2.018339	1.171123	0.004440	0.278599
-22.733473	-2.034736	1.176128	0.004426	0.278586
-23.099012	-1.983032	1.181133	0.004494	0.278509
-23.346865	-1.984421	1.186138	0.004540	0.278267
-22.933268	-2.060956	1.191142	0.004463	0.278260
-23.491703	-1.987268	1.196147	0.004567	0.278115
-23.315655	-2.048241	1.201152	0.004534	0.277964
-23.173902	-2.076773	1.206157	0.004508	0.277950
-23.522957	-2.067710	1.211162	0.004573	0.277666
-23.720494	-2.041469	1.216166	0.004610	0.277616
-23.442589	-2.107604	1.221171	0.004558	0.277534
-23.562832	-2.128876	1.226176	0.004580	0.277309
-23.865210	-2.076113	1.231181	0.004637	0.277297
-23.870127	-2.120179	1.236186	0.004638	0.277062
-24.090578	-2.095014	1.241190	0.004679	0.276984
-24.366405	-2.057035	1.246195	0.004730	0.276920
-24.640988	-2.050480	1.251200	0.004781	0.276694
-24.376680	-2.099530	1.256205	0.004732	0.276688
-24.435977	-2.129096	1.261210	0.004743	0.276477
-25.072724	-2.035105	1.266214	0.004862	0.276363
-24.870356	-2.076578	1.271219	0.004824	0.276338
-24.871173	-2.130179	1.276224	0.004824	0.276056
-25.469551	-2.023464	1.281229	0.004935	0.276045
-25.340967	-2.073593	1.286234	0.004912	0.275905
-25.306435	-2.112098	1.291238	0.004905	0.275736
-25.592376	-2.060678	1.296243	0.004958	0.275733
-25.807460	-2.060584	1.301248	0.004998	0.275527
-26.063057	-2.021795	1.306253	0.005046	0.275487
-25.750898	-2.095259	1.311258	0.004988	0.275399
-26.097493	-2.079624	1.316262	0.005053	0.275150
-26.356899	-2.032593	1.321267	0.005101	0.275149
-26.068731	-2.122670	1.326272	0.005047	0.274951
-26.666119	-2.037063	1.331277	0.005158	0.274829
-26.503740	-2.069992	1.336282	0.005128	0.274811
-26.528479	-2.122624	1.341286	0.005133	0.274510
-27.112181	-2.017423	1.346291	0.005242	0.274505
-27.338428	-1.999789	1.351296	0.005284	0.274381
-27.418755	-2.016536	1.356301	0.005299	0.274215
-26.864398	-2.116392	1.361306	0.005196	0.274220
-27.357865	-2.078924	1.366310	0.005287	0.273944
-27.750942	-2.020295	1.371315	0.005361	0.273876
-27.385920	-2.097763	1.376320	0.005293	0.273817
-27.990732	-2.033760	1.381325	0.005405	0.273574
-28.056788	-2.022007	1.386330	0.005418	0.273572
-27.869245	-2.086970	1.391334	0.005383	0.273409
-28.171601	-2.062692	1.396339	0.005439	0.273246
-28.050897	-2.082731	1.401344	0.005417	0.273256
-28.406717	-2.073515	1.406349	0.005483	0.272962
-28.566090	-2.043720	1.411354	0.005513	0.272966
-28.798700	-2.021195	1.416358	0.005556	0.272861
-29.330846	-1.968012	1.421363	0.005655	0.272630
-28.750741	-2.071943	1.426368	0.005547	0.272638
-29.085211	-2.051268	1.431373	0.005609	0.272424
-29.390394	-2.016642	1.436378	0.005666	0.272313
-29.146911	-2.060918	1.441382	0.005621	0.272313
-29.428675	-2.070446	1.446387	0.005673	0.271990
-29.564359	-2.044155	1.451392	0.005699	0.271998
-29.906026	-2.001251	1.456397	0.005762	0.271896
-30.336122	-1.955691	1.461402	0.005842	0.271722
-30.306756	-1.960982	1.466406	0.005837	0.271722
-30.797085	-1.903352	1.471411	0.005928	0.271554
-30.809855	-1.928766	1.476416	0.005930	0.271406
-30.465547	-1.995766	1.481421	0.005866	0.271382
-31.080586	-1.917427	1.486426	0.005981	0.271203
-31.161121	-1.925133	1.491430	0.005996	0.271084
-30.698648	-2.011994	1.496435	0.005910	0.271069
-30.875309	-2.025759	1.501440	0.005943	0.270824
-31.179505	-1.983354	1.506445	0.005999	0.270755
-30.696995	-2.081765	1.511450	0.005910	0.270697
-30.906299	-2.080837	1.516454	0.005949	0.270499
-31.369919	-1.998511	1.521459	0.006035	0.270488
-31.530419	-2.004066	1.526464	0.006065	0.270302
-31.698707	-2.001969	1.531469	0.006096	0.270149
-31.410066	-2.055259	1.536474	0.006042	0.270145
-31.421927	-2.109935	1.541478	0.006045	0.269840
-31.922996	-2.020977	1.546483	0.006138	0.269828
-32.303060	-1.973156	1.551488	0.006209	0.269713
-32.633360	-1.950124	1.556493	0.006270	0.269514
-31.975909	-2.071508	1.561498	0.006148	0.269505
-32.331064	-2.044677	1.566502	0.006214	0.269302
-32.936187	-1.949887	1.571507	0.006327	0.269219
-32.358807	-2.059315	1.576512	0.006219	0.269196
-32.885569	-2.021008	1.581517	0.006317	0.268886
-33.145854	-1.973545	1.586522	0.006366	0.268887
-33.033320	-2.016786	1.591526	0.006345	0.268764
-33.228893	-2.016548	1.596531	0.006381	0.268573
-33.271335	-2.005917	1.601536	0.006389	0.268589
-33.544182	-2.005190	1.606541	0.006440	0.268325
-33.807188	-1.968041	1.611546	0.006489	0.268267
-33.905440	-1.953075	1.616550	0.006507	0.268251
-34.039291	-1.980799	1.621555	0.006532	0.267970
-33.913288	-2.002387	1.626560	0.006509	0.267977
-34.266952	-1.961968	1.631565	0.006575	0.267848
-34.353779	-1.986973	1.636570	0.006591	0.267627
-33.709126	-2.104796	1.641574	0.006471	0.267624
-34.003146	-2.100768	1.646579	0.006526	0.267356
-34.234367	-2.067366	1.651584	0.006569	0.267309
-34.506567	-2.038215	1.656589	0.006619	0.267199
-34.410860	-2.096233	1.661594	0.006602	0.266979
-34.485401	-2.081730	1.666598	0.006616	0.266984
-35.180366	-2.003208	1.671603	0.006745	0.266724
-35.115525	-2.018662	1.676608	0.006733	0.266704
-34.935430	-2.068234	1.681613	0.006699	0.266612
-35.567379	-1.997783	1.686618	0.006817	0.266371
-35.293155	-2.048784	1.691622	0.006766	0.266364
-35.419925	-2.067308	1.696627	0.006790	0.266138
-35.864746	-1.998808	1.701632	0.006872	0.266070
-36.013903	-1.979827	1.706637	0.006900	0.266026
-35.974844	-2.039419	1.711642	0.006893	0.265740
-36.093390	-2.017814	1.716646	0.006915	0.265740
-36.368909	-1.993052	1.721651	0.006966	0.265602
-36.308470	-2.025050	1.726656	0.006955	0.265487
-36.314034	-2.024823	1.731661	0.006956	0.265483
-36.693333	-2.016069	1.736666	0.007027	0.265154
-36.598980	-2.035194	1.741670	0.007009	0.265143
-36.507313	-2.076740	1.746675	0.006992	0.265007
-36.782862	-2.060101	1.751680	0.007044	0.264824
-37.067319	-2.009605	1.756685	0.007097	0.264817
-37.131554	-2.050281	1.761690	0.007109	0.264531
-37.292075	-2.027431	1.766694	0.007138	0.264496
-37.597520	-1.990895	1.771699	0.007195	0.264391
-37.488206	-2.044227	1.776704	0.007175	0.264208
-37.379943	-2.065072	1.781709	0.007155	0.264202
-37.971025	-2.005160	1.786714	0.007265	0.263941
-38.074303	-1.998980	1.791718	0.007284	0.263871
-37.874205	-2.048672	1.796723	0.007247	0.263798
-37.879392	-2.090477	1.801728	0.007248	0.263563
-38.476942	-1.982703	1.806733	0.007359	0.263558
-38.449357	-2.027599	1.811738	0.007354	0.263339
-38.513046	-2.033568	1.816742	0.007366	0.263242
-38.789150	-1.989468	1.821747	0.007417	0.263208
-38.508694	-2.088034	1.826752	0.007365	0.262947
-38.746287	-2.045474	1.831757	0.007409	0.262943
-38.749878	-2.082945	1.836762	0.007410	0.262733
-39.330562	-2.000045	1.841766	0.007518	0.262607
-39.010380	-2.065725	1.846771	0.007459	0.262566
-39.327053	-2.056840	1.851776	0.007518	0.262297
-39.657661	-1.997965	1.856781	0.007579	0.262290
-39.677691	-2.026325	1.861786	0.007583	0.262113
-39.861771	-2.018288	1.866790	0.007617	0.261973
-39.935634	-2.006611	1.871795	0.007631	0.261963
-40.077662	-2.029516	1.876800	0.007658	0.261693
-39.909859	-2.062480	1.881805	0.007626	0.261679
-39.968658	-2.082737	1.886810	0.007637	0.261508
-40.480036	-2.018110	1.891814	0.007732	0.261351
-40.436173	-2.028080	1.896819	0.007724	0.261339
-40.245366	-2.114154	1.901824	0.007689	0.261055
-40.701545	-2.034133	1.906829	0.007774	0.261038
-41.012630	-2.004738	1.911834	0.007832	0.260887
-41.026303	-2.030499	1.916838	0.007834	0.260730
-40.949505	-2.047169	1.921843	0.007820	0.260715
-41.245797	-2.032148	1.926848	0.007875	0.260499
-41.574694	-1.973997	1.931853	0.007936	0.260489
-41.348761	-2.041343	1.936858	0.007894	0.260343
-42.005619	-1.955655	1.941862	0.008017	0.260155
-42.016610	-1.954313	1.946867	0.008019	0.260151
-41.822530	-2.032382	1.951872	0.007983	0.259913
-42.268731	-1.966183	1.956877	0.008066	0.259830
-42.487479	-1.933502	1.961882	0.008106	0.259790
-42.537535	-1.972350	1.966886	0.008116	0.259522
-42.785692	-1.929715	1.971891	0.008162	0.259508
-42.638147	-1.981612	1.976896	0.008135	0.259368
-42.822036	-1.975654	1.981901	0.008169	0.259214
-42.494056	-2.035306	1.986906	0.008108	0.259214
-42.923380	-2.011927	1.991910	0.008188	0.258908
-43.342002	-1.941567	1.996915	0.008266	0.258876
-43.089052	-2.023364	2.001920	0.008219	0.258676

-43.341095	-2.011145	2.011917	0.008266	0.258487
-43.634329	-2.000952	2.021914	0.008320	0.258245
-43.570371	-2.046758	2.031910	0.008308	0.258053
-43.885563	-2.007741	2.041907	0.008367	0.257950
-44.049649	-2.026206	2.051904	0.008398	0.257678
-44.367437	-1.978050	2.061901	0.008457	0.257624
-44.154334	-2.041715	2.071898	0.008417	0.257484
-44.637226	-1.986176	2.081894	0.008507	0.257302
-44.238774	-2.059528	2.091891	0.008433	0.257297
-44.267568	-2.059452	2.101888	0.008438	0.257267
-44.611624	-2.049714	2.111885	0.008503	0.256969
-44.387815	-2.091828	2.121882	0.008461	0.256961
-44.448788	-2.081004	2.131878	0.008472	0.256960
-44.603588	-2.052392	2.141875	0.008501	0.256962
-44.555062	-2.060249	2.151872	0.008492	0.256967
-44.649725	-2.043143	2.161869	0.008510	0.256966
-44.392850	-2.091037	2.171866	0.008462	0.256960
-44.659496	-2.042260	2.181862	0.008512	0.256961
-44.551143	-2.060894	2.191859	0.008492	0.256967
-44.776751	-2.018793	2.201856	0.008534	0.256973
-44.578177	-2.055290	2.211853	0.008497	0.256970
-44.529632	-2.064980	2.221850	0.008488	0.256965
-44.641408	-2.044958	2.231846	0.008508	0.256963
-44.568330	-2.028204	2.241843	0.008495	0.257133
-44.290885	-2.049289	2.251840	0.008443	0.257298
-44.379977	-2.033242	2.261837	0.008460	0.257297
-44.266100	-2.054552	2.271834	0.008439	0.257293
-44.341844	-2.001647	2.281830	0.008453	0.257513
-44.217602	-2.006878	2.291827	0.008430	0.257611
-43.903751	-2.064428	2.301824	0.008371	0.257608
-43.927828	-2.017960	2.311821	0.008376	0.257844
-43.620995	-2.056471	2.321818	0.008319	0.257941
-43.787335	-2.020929	2.331814	0.008350	0.257971
-43.261602	-2.071008	2.341811	0.008252	0.258226
-43.307136	-2.062224	2.351808	0.008260	0.258229
-43.196123	-2.046667	2.361805	0.008240	0.258429
-42.971901	-2.066125	2.371802	0.008198	0.258549
-43.101533	-2.018721	2.381798	0.008222	0.258682
-42.432407	-2.108739	2.391795	0.008098	0.258859
-42.609767	-2.059756	2.401792	0.008131	0.258953
-42.361075	-2.061072	2.411789	0.008084	0.259198
-42.386511	-2.040672	2.421786	0.008089	0.259286
-42.139987	-2.050232	2.431782	0.008043	0.259483
-42.059339	-2.041487	2.441779	0.008028	0.259613
-41.688369	-2.072538	2.451776	0.007959	0.259816
-41.697892	-2.039018	2.461773	0.007961	0.259993
-41.308783	-2.085570	2.471770	0.007889	0.260128
-41.419281	-2.016883	2.481766	0.007909	0.260398
-41.163363	-2.045119	2.491763	0.007862	0.260500
-41.110358	-2.015682	2.501760	0.007852	0.260717
-40.876489	-2.029482	2.511757	0.007808	0.260876
-40.652239	-2.041125	2.521754	0.007767	0.261038
-40.440037	-2.030048	2.531750	0.007727	0.261313
-40.248976	-2.040044	2.541747	0.007692	0.261450
-39.939477	-2.054984	2.551744	0.007634	0.261679
-39.675122	-2.064872	2.561741	0.007585	0.261890
-39.635315	-2.047315	2.571738	0.007577	0.262027
-39.356282	-2.051886	2.581734	0.007526	0.262282
-39.095106	-2.059212	2.591731	0.007477	0.262504
-39.252792	-1.998814	2.601728	0.007506	0.262678
-38.528108	-2.082049	2.611725	0.007371	0.262946
-38.729853	-2.006855	2.621722	0.007409	0.263158
-38.495797	-2.019966	2.631718	0.007365	0.263320
-38.136882	-2.042041	2.641715	0.007299	0.263557
-38.300423	-1.962280	2.651712	0.007329	0.263832
-37.713533	-2.032263	2.661709	0.007220	0.264033
-37.670352	-2.002469	2.671706	0.007212	0.264239
-37.496001	-1.989166	2.681702	0.007179	0.264486
-37.334280	-1.970038	2.691699	0.007149	0.264751
-36.927980	-2.007397	2.701696	0.007074	0.264951
-36.386820	-2.072093	2.711693	0.006973	0.265135
-36.693416	-1.953232	2.721690	0.007030	0.265479
-36.388329	-1.976201	2.731686	0.006973	0.265657
-36.270721	-1.958001	2.741683	0.006951	0.265872
-35.913252	-1.984709	2.751680	0.006885	0.266081
-35.487858	-2.009789	2.761677	0.006806	0.266365
-35.257457	-2.007248	2.771674	0.006763	0.266606
-35.305449	-1.960479	2.781670	0.006772	0.266813
-35.092214	-1.958743	2.791667	0.006732	0.267032
-34.765472	-1.965051	2.801664	0.006671	0.267320
-34.330975	-1.995843	2.811661	0.006591	0.267581
-34.040200	-2.008869	2.821658	0.006536	0.267796
-33.720685	-2.028970	2.831654	0.006477	0.268002
-33.445235	-2.034733	2.841651	0.006426	0.268241
-33.260036	-2.020458	2.851648	0.006391	0.268500
-33.118147	-2.005170	2.861645	0.006365	0.268721
-32.877638	-2.009749	2.871642	0.006320	0.268932
-32.654812	-1.994891	2.881638	0.006279	0.269230
-32.237772	-2.028743	2.891635	0.006201	0.269455
-31.979815	-2.039210	2.901632	0.006153	0.269651
-31.745929	-2.040371	2.911629	0.006110	0.269873
-31.637214	-2.007946	2.921626	0.006089	0.270153
-31.267193	-2.024291	2.931622	0.006021	0.270425
-31.059384	-2.029536	2.941619	0.005982	0.270599
-30.811727	-2.040709	2.951616	0.005936	0.270780
-30.390861	-2.063961	2.961613	0.005857	0.271065
-30.424997	-2.014956	2.971610	0.005864	0.271293
-30.169431	-2.019702	2.981606	0.005816	0.271516
-29.928172	-2.022160	2.991603	0.005771	0.271736
-29.526632	-2.047564	3.001600	0.005697	0.271990
-29.323210	-2.034677	3.011597	0.005659	0.272255
-29.170044	-2.023319	3.021594	0.005630	0.272463
-28.870412	-2.037340	3.031590	0.005575	0.272678
-28.939899	-1.970420	3.041587	0.005588	0.272966
-28.073691	-2.078025	3.051584	0.005426	0.273231
-28.003799	-2.053373	3.061581	0.005413	0.273428
-27.973947	-2.019105	3.071578	0.005408	0.273638
-27.326020	-2.091496	3.081574	0.005287	0.273878
-27.432477	-2.017390	3.091571	0.005307	0.274168
-27.150336	-2.028047	3.101568	0.005255	0.274382
-26.889592	-2.035788	3.111565	0.005206	0.274591
-26.590048	-2.043304	3.121562	0.005150	0.274838
-26.149678	-2.068679	3.131558	0.005068	0.275126
-26.413426	-1.978028	3.141555	0.005117	0.275351
-26.208131	-1.970486	3.151552	0.005079	0.275586
-25.931879	-1.985958	3.161549	0.005028	0.275769
-25.301370	-2.046993	3.171546	0.004910	0.276050
-25.178022	-2.022849	3.181542	0.004888	0.276294
-25.113496	-1.992844	3.191539	0.004876	0.276512
-24.667372	-2.029080	3.201536	0.004793	0.276747
-24.382186	-2.034968	3.211533	0.004739	0.276987
-23.950439	-2.060542	3.221530	0.004659	0.277264
-24.078565	-1.994487	3.231526	0.004683	0.277487
-23.675803	-2.024993	3.241523	0.004608	0.277709
-23.228308	-2.056952	3.251520	0.004525	0.277967
-23.094311	-2.031443	3.261517	0.004500	0.278226
-22.697786	-2.062913	3.271514	0.004426	0.278437
-22.482682	-2.063121	3.281510	0.004386	0.278639
-22.333705	-2.044622	3.291507	0.004358	0.278876
-21.855798	-2.071625	3.301504	0.004269	0.279187
-21.857755	-2.036330	3.311501	0.004270	0.279367
-21.351727	-2.090638	3.321498	0.004176	0.279563
-21.498883	-2.012899	3.331494	0.004203	0.279826
-20.870703	-2.072807	3.341491	0.004086	0.280107
-20.658862	-2.070713	3.351488	0.004047	0.280317
-20.396889	-2.079132	3.361485	0.003998	0.280519
-20.141423	-2.086960	3.371482	0.003950	0.280718
-19.888569	-2.084962	3.381478	0.003903	0.280965
-19.834490	-2.057017	3.391475	0.003893	0.281159
-19.468665	-2.081120	3.401472	0.003825	0.281378
-19.413297	-2.032432	3.411469	0.003815	0.281680
-19.071050	-2.049577	3.421466	0.003751	0.281911
-18.936610	-2.033568	3.431462	0.003726	0.282118
-18.469390	-2.077251	3.441459	0.003639	0.282330
-18.194216	-2.074283	3.451456	0.003588	0.282601
-17.854800	-2.084436	3.461453	0.003525	0.282865
-17.847372	-2.044004	3.471450	0.003524	0.283079
-17.651695	-2.041614	3.481446	0.003487	0.283273
-17.263190	-2.057212	3.491443	0.003415	0.283554
-16.944912	-2.065917	3.501440	0.003356	0.283804
-16.817458	-2.047401	3.511437	0.003332	0.284017
-16.531169	-2.054728	3.521434	0.003279	0.284244
-16.404512	-2.028661	3.531430	0.003255	0.284494
-15.923295	-2.063453	3.541427	0.003166	0.284762
-15.749422	-2.054954	3.551424	0.003133	0.284965
-15.449333	-2.069127	3.561421	0.003077	0.285170
-15.228624	-2.048303	3.571418	0.003036	0.285479
-15.163439	-2.021881	3.581414	0.003024	0.285673
-14.514690	-2.102466	3.591411	0.002903	0.285862
-14.630074	-2.038249	3.601408	0.002925	0.286081
-13.952073	-2.107466	3.611405	0.002799	0.286354
-14.072733	-2.036729	3.621402	0.002821	0.286600
-13.815656	-2.042878	3.631398	0.002773	0.286805
-13.323426	-2.097218	3.641395	0.002682	0.286982
-13.249953	-2.047094	3.651392	0.002668	0.287302
-12.671097	-2.111248	3.661389	0.002560	0.287509
-12.602399	-2.083474	3.671386	0.002548	0.287711
-12.446415	-2.063280	3.681382	0.002519	0.287955
-11.845271	-2.120123	3.691379	0.002407	0.288219
-12.018444	-2.051031	3.701376	0.002439	0.288407
-11.465238	-2.111884	3.711373	0.002336	0.288606
-11.294161	-2.089398	3.721370	0.002304	0.288875
-10.851259	-2.120699	3.731366	0.002222	0.289121
-10.696459	-2.114247	3.741363	0.002193	0.289294
-10.519388	-2.106003	3.751360	0.002160	0.289496
-9.984373	-2.143426	3.761357	0.002061	0.289795
-9.923595	-2.118152	3.771354	0.002049	0.289976
-9.599697	-2.141913	3.781350	0.001989	0.290151
-9.369347	-2.118368	3.791347	0.001946	0.290477
-9.171814	-2.122537	3.801344	0.001909	0.290635
-8.890574	-2.140954	3.811341	0.001857	0.290798
-8.910908	-2.085770	3.821338	0.001861	0.291053
-8.358877	-2.135122	3.831334	0.001758	0.291307
-8.290718	-2.108732	3.841331	0.001745	0.291499
-7.932011	-2.133386	3.851328	0.001679	0.291700
-7.639098	-2.129360	3.861325	0.001624	0.291984
-7.663833	-2.085102	3.871322	0.001629	0.292181
-7.324055	-2.107099	3.881318	0.001566	0.292378
-7.037496	-2.109729	3.891315	0.001512	0.292622
-6.930925	-2.070023	3.901312	0.001492	0.292914
-6.639537	-2.081896	3.911309	0.001438	0.293117
-6.370587	-2.092778	3.921306	0.001388	0.293304
-6.125219	-2.082379	3.931302	0.001342	0.293575
-5.971520	-2.062010	3.941299	0.001314	0.293813
-5.720102	-2.064767	3.951296	0.001267	0.294024
-5.456844	-2.066332	3.961293	0.001218	0.294252
-5.229351	-2.055689	3.971290	0.001176	0.294507
-5.101754	-2.027544	3.981286	0.001152	0.294759
-4.867673	-2.023321	3.991283	0.001108	0.294989
-4.739825	-2.000335	4.001280	0.001085	0.295215
-4.282251	-2.026360	4.011277	0.001000	0.295495
-4.143513	-2.009222	4.021274	0.000974	0.295702
-3.962759	-1.998280	4.031270	0.000940	0.295916
-4.091531	-1.924851	4.041267	0.000964	0.296161
-3.544246	-1.977281	4.051264	0.000862	0.296390
-3.118276	-1.991767	4.061261	0.000783	0.296697
-2.820048	-2.002736	4.071258	0.000727	0.296908
-2.678639	-1.984246	4.081254	0.000701	0.297123
-2.597570	-1.949665	4.091251	0.000686	0.297363
-2.412939	-1.930660	4.101248	0.000652	0.297618
-2.228671	-1.897935	4.111245	0.000617	0.297940
-2.016650	-1.889358	4.121242	0.000578	0.298168
-2.108277	-1.821580	4.131238	0.000595	0.298416
-1.891778	-1.805494	4.141235	0.000555	0.298685
-1.675075	-1.790100	4.151232	0.000514	0.298950
-1.413641	-1.778362	4.161229	0.000466	0.299236
-1.449526	-1.717038	4.171226	0.000472	0.299501
-1.301137	-1.678566	4.181222	0.000445	0.299817
-1.215229	-1.634557	4.191219	0.000429	0.300104
-1.185969	-1.572493	4.201216	0.000423	0.300429
-1.218971	-1.514105	4.211213	0.000429	0.300681
-0.982477	-1.493933	4.221210	0.000385	0.300984
-0.997404	-1.425529	4.231206	0.000388	0.301300
-0.826325	-1.385148	4.241203	0.000356	0.301643
-0.922761	-1.301719	4.251200	0.000374	0.301959
-0.786969	-1.246706	4.261197	0.000349	0.302340
-0.703423	-1.188119	4.271194	0.000333	0.302693
-0.663536	-1.119556	4.281190	0.000326	0.303055
-0.567865	-1.062817	4.291187	0.000308	0.303408
-0.300032	-1.035598	4.301184	0.000258	0.303770
-0.343852	-0.946005	4.311181	0.000266	0.304158
-0.351576	-0.858623	4.321178	0.000268	0.304567
-0.197499	-0.805078	4.331174	0.000239	0.304954
-0.212052	-0.716951	4.341171	0.000242	0.305359
-0.158396	-0.643872	4.351168	0.000232	0.305751
-0.151130	-0.555043	4.361165	0.000231	0.306177
-0.188164	-0.461347	4.371162	0.000237	0.306588
-0.147483	-0.372331	4.381158	0.000230	0.307042
-0.044146	-0.297546	4.391155	0.000211	0.307482
-0.160823	-0.172169	4.401152	0.000232	0.307972
0.071524	-0.118679	4.411149	0.000189	0.308421
-0.084514	0.013454	4.421146	0.000218	0.308908
0.000000	0.092648	4.431142	0.000202	0.309350

0.105334	0.341802	4.436147	0.000182	0.310602
0.107192	0.897618	4.441152	0.000182	0.313182
0.471147	1.677143	4.446157	0.000113	0.317065
0.888007	2.736002	4.451162	0.000035	0.322200
1.240927	4.095357	4.456166	-0.000031	0.328530
1.610901	5.752346	4.461171	-0.000101	0.336037
2.172347	7.669105	4.466176	-0.000207	0.344619
2.690142	9.910770	4.471181	-0.000305	0.354289
3.330130	12.432312	4.476186	-0.000426	0.364900
4.165604	15.241718	4.481190	-0.000583	0.376457
6.426588	18.133345	4.486195	-0.001006	0.388937
9.563774	21.214727	4.491200	-0.001592	0.402282
12.653009	24.676057	4.496205	-0.002170	0.416489
16.571001	28.366177	4.501210	-0.002902	0.431496
21.152570	32.307065	4.506214	-0.003757	0.447196
25.280257	36.729594	4.511219	-0.004529	0.463608
33.805697	40.756461	4.516224	-0.006119	0.480655
38.772573	45.855515	4.521229	-0.007047	0.498361
44.035388	51.297893	4.526234	-0.008030	0.516565
52.131486	56.609704	4.531238	-0.009541	0.535172
56.944921	62.927839	4.536243	-0.010442	0.554231
60.834560	69.755875	4.541248	-0.011170	0.573518
65.358597	76.805245	4.546253	-0.012017	0.592992
74.075119	83.462002	4.551258	-0.013645	0.612689
81.177990	90.750522	4.556262	-0.014972	0.632548
87.779376	98.466808	4.561267	-0.016206	0.652543
93.585357	106.606934	4.566272	-0.017292	0.672543
97.827080	115.258156	4.571277	-0.018088	0.692443
101.905430	124.166094	4.576282	-0.018853	0.712244
105.223950	133.373202	4.581286	-0.019477	0.731829
109.915334	142.528055	4.586291	-0.020356	0.751269
113.145281	152.056241	4.591296	-0.020964	0.770427
116.354159	161.705566	4.596301	-0.021568	0.789332
117.931954	171.714442	4.601306	-0.021868	0.807918
119.372562	181.792415	4.606310	-0.022143	0.826164
120.641397	191.914739	4.611315	-0.022386	0.844037
122.357816	201.954748	4.616320	-0.022712	0.861533
123.762356	212.032591	4.621325	-0.022980	0.878651
124.720885	222.182630	4.626330	-0.023165	0.895431
125.580214	232.299180	4.631334	-0.023332	0.911821
126.347944	242.377177	4.636339	-0.023481	0.927836
126.643971	252.489536	4.641344	-0.023543	0.943505
126.870977	262.534732	4.646349	-0.023591	0.958798
127.618371	272.423698	4.651354	-0.023737	0.973754
128.210132	282.271922	4.656358	-0.023854	0.988385
128.895926	292.028243	4.661363	-0.023988	1.002693
129.425362	301.734137	4.666368	-0.024093	1.016689
129.703145	311.407607	4.671373	-0.024151	1.030387
129.892267	321.015423	4.676378	-0.024192	1.043795
130.065219	330.550098	4.681382	-0.024230	1.056928
130.740841	339.934219	4.686387	-0.024362	1.069814
130.857561	349.333296	4.691392	-0.024390	1.082438
131.136210	358.643399	4.696397	-0.024448	1.094835
132.390613	367.733247	4.701402	-0.024688	1.107026
132.738946	376.921054	4.706406	-0.024758	1.119008
133.204398	386.041210	4.711411	-0.024851	1.130803
133.957634	395.050624	4.716416	-0.024997	1.142398
134.827786	404.024725	4.721421	-0.025165	1.153857
134.961111	413.058465	4.726426	-0.025196	1.165121
135.524258	421.942787	4.731430	-0.025306	1.176184
135.984865	430.815555	4.736435	-0.025398	1.187108
136.399481	439.654768	4.741440	-0.025481	1.197882
137.045009	448.415315	4.746445	-0.025607	1.208513
138.801998	456.989687	4.751450	-0.025939	1.219054
139.222639	465.757994	4.756454	-0.026023	1.229466
139.941411	474.437944	4.761459	-0.026163	1.239745
140.374828	483.141400	4.766464	-0.026249	1.249912
140.900641	491.786372	4.771469	-0.026353	1.259947
141.532795	500.404803	4.776474	-0.026476	1.269892
142.241793	508.954514	4.781478	-0.026614	1.279697
142.649944	517.559741	4.786483	-0.026695	1.289433
143.296261	526.098800	4.791488	-0.026821	1.299067
143.711468	534.675563	4.796493	-0.026904	1.308628
144.814176	543.165047	4.801498	-0.027115	1.318150
145.351915	551.639965	4.806502	-0.027221	1.327485
145.970706	560.108932	4.811507	-0.027341	1.336762
146.786218	568.518962	4.816512	-0.027499	1.345948
147.117101	577.010836	4.821517	-0.027566	1.355072
147.513898	585.458311	4.826522	-0.027645	1.364099
148.000184	593.884379	4.831526	-0.027741	1.373060
148.821732	602.242891	4.836531	-0.027899	1.381950
149.366574	610.656818	4.841536	-0.028006	1.390793
149.702285	619.068121	4.846541	-0.028074	1.399541
150.185650	627.445643	4.851546	-0.028170	1.408226
150.545463	635.830803	4.856550	-0.028242	1.416844
151.033627	644.184655	4.861555	-0.028339	1.425399
151.788284	652.503674	4.866560	-0.028485	1.433912
152.838380	660.747666	4.871565	-0.028685	1.442349
153.426893	669.094963	4.876570	-0.028800	1.450763
154.016374	677.416409	4.881574	-0.028916	1.459103
154.523521	685.761922	4.886579	-0.029015	1.467406
155.011650	694.114494	4.891584	-0.029112	1.475665
155.207345	702.446879	4.896589	-0.029154	1.483812
155.877517	710.723415	4.901594	-0.029284	1.491936
156.519080	718.977435	4.906598	-0.029409	1.499989
157.121158	727.262764	4.911603	-0.029526	1.508023
157.216540	735.621344	4.916608	-0.029549	1.516005
157.788352	743.848610	4.921613	-0.029661	1.523895
158.400501	752.123356	4.926618	-0.029780	1.531794
159.022469	760.354844	4.931622	-0.029902	1.539614
159.425854	768.652635	4.936627	-0.029982	1.547423
159.837723	776.921794	4.941632	-0.030064	1.555167
160.439658	785.128298	4.946637	-0.030182	1.562843
161.281055	793.339396	4.951642	-0.030344	1.570521
162.165631	801.526992	4.956646	-0.030514	1.578146
162.773750	809.759229	4.961651	-0.030632	1.585734
162.914678	818.087863	4.966656	-0.030664	1.593305
163.125105	826.342834	4.971661	-0.030708	1.600784
163.899358	834.538359	4.976666	-0.030858	1.608256
164.644437	842.719528	4.981670	-0.031002	1.615677
165.206776	850.944100	4.986675	-0.031112	1.623075
165.977951	859.158240	4.991680	-0.031261	1.630460
165.959405	867.454265	4.996685	-0.031263	1.637773
166.188760	875.687182	5.001690	-0.031311	1.645032
166.643726	883.899991	5.006694	-0.031401	1.652273
167.043599	892.097221	5.011699	-0.031481	1.659461
167.552742	900.280400	5.016704	-0.031581	1.666621
168.145469	908.452896	5.021709	-0.031696	1.673753
168.646555	916.640166	5.026714	-0.031795	1.680854
169.197410	924.814700	5.031718	-0.031903	1.687921
169.435668	933.056216	5.036723	-0.031953	1.694973
169.951889	941.226775	5.041728	-0.032054	1.701973
170.180516	949.439246	5.046733	-0.032102	1.708941
170.623554	957.624345	5.051738	-0.032190	1.715886
170.863798	965.807511	5.056742	-0.032240	1.722775
171.175906	973.989918	5.061747	-0.032303	1.729645
171.424868	982.189561	5.066752	-0.032355	1.736494
171.876055	990.329476	5.071757	-0.032444	1.743292
172.517794	998.477275	5.076762	-0.032569	1.750095
172.639676	1006.693221	5.081766	-0.032597	1.756861
173.090351	1014.837195	5.086771	-0.032686	1.763584
173.450727	1023.016487	5.091776	-0.032759	1.770299
173.548115	1031.224755	5.096781	-0.032782	1.776978
173.988567	1039.377712	5.101786	-0.032870	1.783630
174.134079	1047.579168	5.106790	-0.032902	1.790260
174.617801	1055.708778	5.111795	-0.032997	1.796850
174.979670	1063.847009	5.116800	-0.033070	1.803408
175.326201	1071.977612	5.121805	-0.033140	1.809933
175.738444	1080.136212	5.126810	-0.033222	1.816466
176.261955	1088.241220	5.131814	-0.033325	1.822946
176.548945	1096.403413	5.136819	-0.033383	1.829419
177.033742	1104.532667	5.141824	-0.033479	1.835867
177.357717	1112.666659	5.146829	-0.033544	1.842277
177.334334	1120.885173	5.151834	-0.033545	1.848689
177.992265	1128.969017	5.156838	-0.033673	1.855055
178.478371	1137.098365	5.161843	-0.033769	1.861415
178.808262	1145.256257	5.166848	-0.033836	1.867755
179.325697	1153.364546	5.171853	-0.033937	1.874059
179.770005	1161.493679	5.176858	-0.034025	1.880348
180.052130	1169.634948	5.181862	-0.034083	1.886607
180.353904	1177.790693	5.186867	-0.034145	1.892858
180.645537	1185.943547	5.191872	-0.034204	1.899085
180.907822	1194.060597	5.196877	-0.034258	1.905262
181.232879	1202.226201	5.201882	-0.034324	1.911461
181.567946	1210.323588	5.206886	-0.034392	1.917591
182.209965	1218.402575	5.211891	-0.034517	1.923722
182.531367	1226.542010	5.216896	-0.034582	1.929843
182.602791	1234.709278	5.221901	-0.034600	1.935936
183.321938	1242.784615	5.226906	-0.034740	1.942015
183.391937	1250.966222	5.231910	-0.034758	1.948081
183.927923	1259.055191	5.236915	-0.034863	1.954111
184.402611	1267.134656	5.241920	-0.034957	1.960109
184.768791	1275.235344	5.246925	-0.035030	1.966092
185.113544	1283.387343	5.251930	-0.035100	1.972092
185.732010	1291.451459	5.256934	-0.035220	1.978039
186.132467	1299.568048	5.261939	-0.035300	1.983983
186.340808	1307.722930	5.266944	-0.035344	1.989916
186.542668	1315.839493	5.271949	-0.035387	1.995803
186.937356	1323.953878	5.276954	-0.035465	2.001691
187.667983	1331.994009	5.281958	-0.035607	2.007545
188.154562	1340.119153	5.286963	-0.035703	2.013416
188.903525	1348.193835	5.291968	-0.035847	2.019262
189.474254	1356.273959	5.296973	-0.035959	2.025076
190.194325	1364.377276	5.301978	-0.036098	2.030906
190.810367	1372.467750	5.306982	-0.036218	2.036698
191.630418	1380.520234	5.311987	-0.036376	2.042468
191.995916	1388.688255	5.316992	-0.036449	2.048256
192.195279	1396.844690	5.321997	-0.036492	2.054002
192.714728	1404.938920	5.327002	-0.036594	2.059722
193.020896	1413.052009	5.332006	-0.036656	2.065417
193.345984	1421.204966	5.337011	-0.036722	2.071125
194.034503	1429.261978	5.342016	-0.036855	2.076789
194.751400	1437.287729	5.347021	-0.036994	2.082418
195.023054	1445.441529	5.352026	-0.037050	2.088075
195.349262	1453.569996	5.357030	-0.037116	2.093705
195.869932	1461.663399	5.362035	-0.037218	2.099314
196.083013	1469.781376	5.367040	-0.037263	2.104895
196.387960	1477.910491	5.372045	-0.037325	2.110478
196.561705	1486.073069	5.377050	-0.037363	2.116056
197.246936	1494.085280	5.382054	-0.037496	2.121568
197.199508	1502.223890	5.387059	-0.037492	2.127079
197.718743	1510.308003	5.392064	-0.037594	2.132594
197.952657	1518.391080	5.397069	-0.037643	2.138066
198.486651	1526.457658	5.402074	-0.037748	2.143542
198.720770	1534.571636	5.407078	-0.037796	2.149007
199.194419	1542.633750	5.412083	-0.037890	2.154446
199.498946	1550.729157	5.417088	-0.037952	2.159878
199.732296	1558.808659	5.422093	-0.038000	2.165278
200.158009	1566.921025	5.427098	-0.038085	2.170705
200.473756	1575.003192	5.432102	-0.038149	2.176088
200.924120	1583.075067	5.437107	-0.038238	2.181464
201.216823	1591.180412	5.442112	-0.038298	2.186833
201.617403	1599.265606	5.447117	-0.038378	2.192186
201.936094	1607.367255	5.452122	-0.038442	2.197529
202.098651	1615.436964	5.457126	-0.038478	2.202824
202.463405	1623.510752	5.462131	-0.038551	2.208127
202.844157	1631.609652	5.467136	-0.038627	2.213435
202.965495	1639.718973	5.472141	-0.038655	2.218713
203.520947	1647.759220	5.477146	-0.038764	2.223974
203.853763	1655.863581	5.482150	-0.038831	2.229243
203.957200	1663.956633	5.487155	-0.038855	2.234472
204.145616	1672.059466	5.492160	-0.038896	2.239702
204.367727	1680.119937	5.497165	-0.038942	2.244897
205.213446	1688.140693	5.502170	-0.039105	2.250109
205.440171	1696.245240	5.507174	-0.039153	2.255307
205.830829	1704.313157	5.512179	-0.039231	2.260485
206.247473	1712.393292	5.517184	-0.039313	2.265661
206.448955	1720.513072	5.522189	-0.039356	2.270831
206.862043	1728.602580	5.527194	-0.039438	2.275989
207.374198	1736.617566	5.532198	-0.039539	2.281096
207.740468	1744.685009	5.537203	-0.039612	2.286213
207.876162	1752.798258	5.542208	-0.039643	2.291326
207.981908	1760.886557	5.547213	-0.039668	2.296410
208.411449	1768.953390	5.552218	-0.039753	2.301497
208.619544	1777.028895	5.557222	-0.039797	2.306559
208.911919	1785.104424	5.562227	-0.039857	2.311618
209.357593	1793.157678	5.567232	-0.039945	2.316664
209.663287	1801.203965	5.572237	-0.040007	2.321683
209.924496	1809.295440	5.577242	-0.040061	2.326716
210.396012	1817.356859	5.582246	-0.040154	2.331736
210.820666	1825.431498	5.587251	-0.040238	2.336750
210.924082	1833.530560	5.592256	-0.040263	2.341741
211.307570	1841.581306	5.597261	-0.040339	2.346716
211.783763	1849.657450	5.602266	-0.040433	2.351702
211.996105	1857.724824	5.607270	-0.040478	2.356651
212.390934	1865.765069	5.612275	-0.040557	2.361589
212.831654	1873.826466	5.617280	-0.040644	2.366532
213.057956	1881.913473	5.622285	-0.040692	2.371463
213.647443	1889.960137	5.627290	-0.040807	2.376389
213.811157	1898.043398	5.632294	-0.040842	2.381292
214.033444	1906.128557	5.637299	-0.040889	2.386190
214.381560	1914.214077	5.642304	-0.040959	2.391089
214.857533	1922.233482	5.647309	-0.041053	2.395949
215.110049	1930.323442	5.652314	-0.041105	2.400823
215.227986	1938.401859	5.657318	-0.041132	2.405669
215.489394	1946.499951	5.662323	-0.041186	2.410529
216.087227	1954.527175	5.667328	-0.041303	2.415363
216.180621	1962.611660	5.672333	-0.041325	2.420182
216.308983	1970.705305	5.677338	-0.041355	2.424999
216.452107	1978.795777	5.682342	-0.041387	2.429806
216.992915	1986.850351	5.687347	-0.041492	2.434614
217.198827	1994.913487	5.692352	-0.041536	2.439390
217.357964	2002.938306	5.697357	-0.041571	2.444131
217.813931	2010.992445	5.702362	-0.041661	2.448904
217.721913	2019.112323	5.707366	-0.041649	2.453662
217.802211	2027.169454	5.712371	-0.041669	2.458389
218.377434	2035.174597	5.717376	-0.041782	2.463113
218.386932	2043.276546	5.722381	-0.041789	2.467842
218.624951	2051.354133	5.727386	-0.041838	2.472565
219.125085	2059.368092	5.732390	-0.041937	2.477262
219.447682	2067.394433	5.737395	-0.042002	2.481944
219.568364	2075.496790	5.742400	-0.042030	2.486645
220.079260	2083.530954	5.747405	-0.042130	2.491328
220.233553	2091.618898	5.752410	-0.042164	2.496005
220.723742	2099.633392	5.757414	-0.042260	2.500657
220.876858	2107.709356	5.762419	-0.042294	2.505311
221.377080	2115.769318	5.767424	-0.042393	2.509972
221.650940	2123.831609	5.772429	-0.042449	2.514609
221.863118	2131.889605	5.777434	-0.042494	2.519231
222.219958	2139.911551	5.782438	-0.042565	2.523834
222.454307	2147.997362	5.787443	-0.042614	2.528456
222.827065	2156.059697	5.792448	-0.042689	2.533066
222.819822	2164.150550	5.797453	-0.042693	2.537656
223.166503	2172.193267	5.802458	-0.042762	2.542237
223.614218	2180.221189	5.807462	-0.042851	2.546808
223.780196	2188.323672	5.812467	-0.042887	2.551392
224.059039	2196.377056	5.817472	-0.042944	2.555949
224.432682	2204.396229	5.822477	-0.043019	2.560485
224.813912	2212.440866	5.827482	-0.043095	2.565028
225.086001	2220.522528	5.832486	-0.043151	2.569576
225.428649	2228.534868	5.837491	-0.043220	2.574081
225.595547	2236.647820	5.842496	-0.043257	2.578623
225.722072	2244.686391	5.847501	-0.043285	2.583112
226.066816	2252.766217	5.852506	-0.043355	2.587632
226.163493	2260.911658	5.857510	-0.043378	2.592163
226.544837	2268.931302	5.862515	-0.043454	2.596636
226.779766	2276.963668	5.867520	-0.043503	2.601098
227.092057	2284.974251	5.872525	-0.043567	2.605546
227.123550	2293.053184	5.877530	-0.043578	2.610004
227.347244	2301.106863	5.882534	-0.043625	2.614454
227.780412	2309.102753	5.887539	-0.043710	2.618879
228.020222	2317.155356	5.892544	-0.043760	2.623315
228.115028	2325.221840	5.897549	-0.043783	2.627740
228.498367	2333.277523	5.902554	-0.043860	2.632172
228.573452	2341.342387	5.907558	-0.043879	2.636581
228.861057	2349.362347	5.912563	-0.043938	2.640972
229.187895	2357.400739	5.917568	-0.044004	2.645368
229.404165	2365.449694	5.922573	-0.044049	2.649755
229.723415	2373.500282	5.927578	-0.044114	2.654143
230.076866	2381.532478	5.932582	-0.044185	2.658515
230.421298	2389.581538	5.937587	-0.044254	2.662889
230.868820	2397.638331	5.942592	-0.044343	2.667267
231.065471	2405.716202	5.947597	-0.044385	2.671632
231.525706	2413.755969	5.952602	-0.044476	2.675987
231.921144	2421.775725	5.957606	-0.044555	2.680320
232.069427	2429.825458	5.962611	-0.044587	2.684645
232.310057	2437.898032	5.967616	-0.044638	2.688982
232.520716	2445.955862	5.972621	-0.044682	2.693302
232.708570	2454.024847	5.977626	-0.044722	2.697619
232.930052	2462.051770	5.982630	-0.044769	2.701910
233.186690	2470.086745	5.987635	-0.044822	2.706200
233.670643	2478.146575	5.992640	-0.044917	2.710511
233.577705	2486.222549	5.997645	-0.044905	2.714786
233.605837	2494.281275	6.002650	-0.044915	2.719054
233.764519	2502.316291	6.007654	-0.044950	2.723310
233.692739	2510.395207	6.012659	-0.044942	2.727569
233.966384	2518.458941	6.017664	-0.044998	2.731834
234.310250	2526.467641	6.022669	-0.045068	2.736068
234.548829	2534.505105	6.027674	-0.045117	2.740305
234.877281	2542.516426	6.032678	-0.045184	2.744526
235.041987	2550.589621	6.037683	-0.045219	2.748763
235.455755	2558.679228	6.042688	-0.045302	2.753018
235.512056	2566.698928	6.047693	-0.045317	2.757208
235.679666	2574.780622	6.052698	-0.045354	2.761430
236.042745	2582.779006	6.057702	-0.045427	2.765614
236.137624	2590.832227	6.062707	-0.045450	2.769804
236.445035	2598.874446	6.067712	-0.045512	2.773995
236.761774	2606.879055	6.072717	-0.045576	2.778161
237.110655	2614.914438	6.077722	-0.045646	2.782338
237.000538	2623.003265	6.082726	-0.045631	2.786509
237.468620	2631.009148	6.087731	-0.045724	2.790665
238.008268	2639.047390	6.092736	-0.045829	2.794837
238.113758	2647.070257	6.097741	-0.045854	2.798968
238.153128	2655.151702	6.102746	-0.045867	2.803119
238.452944	2663.200828	6.107750	-0.045928	2.807263
238.597862	2671.253772	6.112755	-0.045960	2.811393
238.748373	2679.333283	6.117760	-0.045993	2.815531
239.116055	2687.318815	6.122765	-0.046067	2.819628
239.319824	2695.376813	6.127770	-0.046110	2.823746
239.299311	2703.478720	6.132774	-0.046111	2.827868
239.754638	2711.476132	6.137779	-0.046201	2.831958
240.115914	2719.533133	6.142784	-0.046274	2.836067
240.600528	2727.508930	6.147789	-0.046369	2.840136
241.081345	2735.506758	6.152794	-0.046464	2.844210
241.036864	2743.615399	6.157798	-0.046461	2.848303
241.202096	2751.657848	6.162803	-0.046497	2.852370
241.248630	2759.750839	6.167808	-0.046511	2.856449
241.463381	2767.762369	6.172813	-0.046556	2.860491
242.074030	2775.762135	6.177818	-0.046675	2.864544
242.157864	2783.842063	6.182822	-0.046696	2.868601
242.458515	2791.862146	6.187827	-0.046757	2.872635
242.713962	2799.938139	6.192832	-0.046810	2.876689
242.452396	2808.018343	6.197837	-0.046766	2.880710
242.632827	2816.029833	6.202842	-0.046805	2.884715
243.091943	2824.045057	6.207846	-0.046896	2.888733
243.269978	2832.082529	6.212851	-0.046934	2.892741
243.480309	2840.159083	6.217856	-0.046979	2.896764
243.548707	2848.195468	6.222861	-0.046997	2.900753
243.918574	2856.223167	6.227866	-0.047071	2.904750
244.384904	2864.250744	6.232870	-0.047163	2.908746
244.326915	2872.371383	6.237875	-0.047157	2.912754
244.894418	2880.370347	6.242880	-0.047268	2.916730
245.121508	2888.366922	6.247885	-0.047316	2.920681
245.463795	2896.377580	6.252890	-0.047385	2.924640
245.691504	2904.414492	6.257894	-0.047432	2.928601
245.828999	2912.499751	6.262899	-0.047463	2.932574
245.955805	2920.562798	6.267904	-0.047492	2.936531
246.080342	2928.570634	6.272909	-0.047520	2.940455
246.418206	2936.587572	6.277914	-0.047588	2.944390
246.594831	2944.645893	6.282918	-0.047627	2.948332
246.837484	2952.679668	6.287923	-0.047677	2.952259
247.169903	2960.725394	6.292928	-0.047744	2.956192
247.280883	2968.751505	6.297933	-0.047770	2.960098
247.509697	2976.764524	6.302938	-0.047818	2.963999
247.716782	2984.847955	6.307942	-0.047862	2.967928
248.013178	2992.871222	6.312947	-0.047922	2.971827
248.165794	3000.947887	6.317952	-0.047956	2.975739
248.043535	3008.987945	6.322957	-0.047938	2.979614
248.345504	3017.005643	6.327962	-0.048000	2.983495
248.791423	3025.026248	6.332966	-0.048088	2.987380
249.154141	3033.045685	6.337971	-0.048161	2.991255
249.276150	3041.124292	6.342976	-0.048188	2.995141
249.592614	3049.087786	6.347981	-0.048253	2.998977
249.800810	3057.145608	6.352986	-0.048297	3.002847
250.122766	3065.171774	6.357990	-0.048362	3.006703
250.095102	3073.265898	6.362995	-0.048362	3.010569
250.418701	3081.301678	6.368000	-0.048427	3.014420
250.772894	3089.279112	6.373005	-0.048498	3.018239
250.783830	3097.362903	6.378010	-0.048506	3.022087
251.184926	3105.398049	6.383014	-0.048586	3.025926
251.359949	3113.420076	6.388019	-0.048623	3.029743
251.791219	3121.479378	6.393024	-0.048709	3.033586
251.946471	3129.469271	6.398029	-0.048743	3.037377
252.012409	3137.557207	6.403034	-0.048761	3.041205
252.405917	3145.559582	6.408038	-0.048839	3.045004
252.633409	3153.583545	6.413043	-0.048887	3.048801
252.675835	3161.682685	6.418048	-0.048900	3.052619
253.108589	3169.669710	6.423053	-0.048986	3.056398
253.497081	3177.705352	6.428058	-0.049063	3.060194
253.532328	3185.759853	6.433062	-0.049075	3.063976
253.693466	3193.811970	6.438067	-0.049110	3.067758
254.237653	3201.870578	6.443072	-0.049217	3.071558
254.183114	3209.941059	6.448077	-0.049212	3.075329
254.344202	3217.917638	6.453082	-0.049247	3.079063
254.615142	3225.930876	6.458086	-0.049303	3.082814
254.731776	3233.951065	6.463091	-0.049330	3.086556
255.032754	3242.012540	6.468096	-0.049391	3.090322
255.294918	3250.010681	6.473101	-0.049445	3.094052
255.616220	3258.059019	6.478106	-0.049510	3.097803
255.681804	3266.121068	6.483110	-0.049527	3.101544
255.704369	3274.160832	6.488115	-0.049537	3.105268
256.077057	3282.190993	6.493120	-0.049611	3.109000
256.077744	3290.224000	6.498125	-0.049617	3.112711
256.056425	3298.287101	6.503130	-0.049618	3.116431
256.230258	3306.297466	6.508134	-0.049656	3.120131
256.329980	3314.306566	6.513139	-0.049679	3.123822
256.804166	3322.327697	6.518144	-0.049773	3.127532
256.972913	3330.346344	6.523149	-0.049810	3.131222
257.266042	3338.412504	6.528154	-0.049869	3.134936
257.555486	3346.423295	6.533158	-0.049928	3.138619
257.740335	3354.460210	6.538163	-0.049968	3.142305
257.710686	3362.567625	6.543168	-0.049968	3.146009
257.875512	3370.576341	6.548173	-0.050004	3.149673
258.164000	3378.606206	6.553178	-0.050063	3.153348
258.456972	3386.597137	6.558182	-0.050122	3.157000
258.782601	3394.621723	6.563187	-0.050188	3.160666
259.132994	3402.621736	6.568192	-0.050259	3.164316
259.188582	3410.673205	6.573197	-0.050274	3.167973
259.447828	3418.741610	6.578202	-0.050328	3.171643
259.631194	3426.782769	6.583206	-0.050367	3.175292
259.533578	3434.802698	6.588211	-0.050354	3.178915
259.889755	3442.842139	6.593216	-0.050426	3.182563
260.333170	3450.859662	6.598221	-0.050513	3.186200
260.114348	3458.943226	6.603226	-0.050478	3.189834
260.374689	3466.975618	6.608230	-0.050532	3.193462
263.687724	3474.705540	6.613235	-0.051154	3.197082
264.904876	3482.769084	6.618240	-0.051385	3.200757
265.394382	3490.814384	6.623245	-0.051482	3.204387
266.178752	3498.866530	6.628250	-0.051633	3.208029
266.568760	3506.985574	6.633254	-0.051711	3.211680
266.513088	3515.102896	6.638259	-0.051706	3.215307
266.998679	3523.098649	6.643264	-0.051802	3.218899
267.288642	3531.118718	6.648269	-0.051861	3.222489
267.384420	3539.199293	6.653274	-0.051884	3.226093
267.723894	3547.250398	6.658278	-0.051952	3.229691
267.820004	3555.281004	6.663283	-0.051975	3.233266
268.275210	3563.297874	6.668288	-0.052065	3.236845
268.250446	3571.334605	6.673293	-0.052066	3.240409
268.393595	3579.324196	6.678298	-0.052098	3.243955
268.536694	3587.417884	6.683302	-0.052130	3.247544
268.740027	3595.428058	6.688307	-0.052173	3.251094
268.697658	3603.509679	6.693312	-0.052170	3.254661
268.996812	3611.478359	6.698317	-0.052231	3.258189
269.307173	3619.493770	6.703322	-0.052294	3.261734
269.487027	3627.557864	6.708326	-0.052333	3.265291
269.671125	3635.577176	6.713331	-0.052372	3.268825
269.832869	3643.650711	6.718336	-0.052408	3.272378
269.854786	3651.696185	6.723341	-0.052417	3.275909
270.164754	3659.651831	6.728346	-0.052480	3.279408
270.125156	3667.712489	6.733350	-0.052478	3.282936
270.116022	3675.759725	6.738355	-0.052481	3.286455
270.372098	3683.790588	6.743360	-0.052534	3.289974
270.771703	3691.772690	6.748365	-0.052614	3.293473
271.081183	3699.807527	6.753370	-0.052676	3.296988
270.975071	3707.897516	6.758374	-0.052662	3.300507
270.894206	3715.884658	6.763379	-0.052652	3.303979
271.260665	3723.950338	6.768384	-0.052726	3.307498
271.272094	3732.005800	6.773389	-0.052733	3.310995
271.276346	3740.030820	6.778394	-0.052739	3.314475
271.625482	3748.031077	6.783398	-0.052809	3.317955
271.410558	3756.086237	6.788403	-0.052774	3.321432
271.836893	3764.058308	6.793408	-0.052859	3.324894
271.973426	3772.066988	6.798413	-0.052890	3.328358
272.206655	3780.143524	6.803418	-0.052938	3.331851
272.460801	3788.164451	6.808422	-0.052991	3.335317
272.497314	3796.179081	6.813427	-0.053003	3.338768
272.746592	3804.243459	6.818432	-0.053054	3.342246
272.915189	3812.230423	6.823437	-0.053091	3.345683
272.861809	3820.299144	6.828442	-0.053086	3.349143
272.995923	3828.332721	6.833446	-0.053116	3.352592
273.123478	3836.368652	6.838451	-0.053145	3.356038
273.545717	3844.358600	6.843456	-0.053229	3.359472
274.003564	3852.324579	6.848461	-0.053320	3.362894
274.056780	3860.394944	6.853466	-0.053335	3.366341
274.232544	3868.429982	6.858470	-0.053373	3.369774
273.982742	3876.494887	6.863475	-0.053332	3.373201
274.278228	3884.523541	6.868480	-0.053392	3.376629
274.453785	3892.550306	6.873485	-0.053430	3.380048
274.303851	3900.578083	6.878490	-0.053407	3.383452
274.508605	3908.623825	6.883494	-0.053450	3.386874
274.681990	3916.665027	6.888499	-0.053488	3.390289
275.094320	3924.701320	6.893504	-0.053570	3.393707
275.084043	3932.708224	6.898509	-0.053573	3.397093
275.338739	3940.729335	6.903514	-0.053626	3.400492
275.372891	3948.744823	6.908518	-0.053637	3.403877
275.777907	3956.730143	6.913523	-0.053718	3.407260
276.063109	3964.800474	6.918528	-0.053776	3.410670
275.771121	3972.837294	6.923533	-0.053727	3.414043
275.847431	3980.888744	6.928538	-0.053747	3.417431
276.486341	3988.868158	6.933542	-0.053871	3.420805
276.731828	3996.803202	6.938547	-0.053922	3.424144
277.038824	4004.896672	6.943552	-0.053984	3.427548
277.065937	4012.962071	6.948557	-0.053994	3.430927
277.444746	4020.957591	6.953562	-0.054070	3.434286
277.650472	4028.980006	6.958566	-0.054114	3.437646
277.806049	4037.004065	6.963571	-0.054148	3.441002
277.872197	4045.047186	6.968576	-0.054165	3.444360
278.071646	4053.066947	6.973581	-0.054208	3.447709
277.970484	4061.149389	6.978586	-0.054194	3.451071
278.410888	4069.136574	6.983590	-0.054281	3.454409
278.631389	4077.151988	6.988595	-0.054327	3.457747
278.865606	4085.200470	6.993600	-0.054376	3.461096
278.812772	4093.180887	6.998605	-0.054372	3.464404
279.079364	4101.253714	7.003610	-0.054427	3.467758
279.290040	4109.314131	7.008614	-0.054471	3.471102
279.471645	4117.274509	7.013619	-0.054510	3.474400
279.698709	4125.323540	7.018624	-0.054557	3.477733
279.861070	4133.362923	7.023629	-0.054593	3.481057
280.027770	4141.345338	7.028634	-0.054629	3.484354
280.276090	4149.391776	7.033638	-0.054681	3.487677
280.451525	4157.408590	7.038643	-0.054719	3.490982
280.854406	4165.449866	7.043648	-0.054799	3.494302
280.802859	4173.451552	7.048653	-0.054794	3.497587
280.935483	4181.529064	7.053658	-0.054824	3.500906
281.265332	4189.515635	7.058662	-0.054891	3.504192
281.185536	4197.549125	7.063667	-0.054881	3.507480
281.491924	4205.606974	7.068672	-0.054944	3.510787
281.686030	4213.611124	7.073677	-0.054985	3.514066
281.891762	4221.639520	7.078682	-0.055028	3.517352
282.164708	4229.671028	7.083686	-0.055084	3.520638
282.161152	4237.651332	7.088691	-0.055089	3.523892
282.463722	4245.729418	7.093696	-0.055151	3.527191
282.498018	4253.786179	7.098701	-0.055162	3.530471
282.530933	4261.788333	7.103706	-0.055173	3.533726
282.943002	4269.817005	7.108710	-0.055255	3.537000
282.999904	4277.836842	7.113715	-0.055271	3.540256
283.131353	4285.838328	7.118720	-0.055301	3.543504
283.146046	4293.919417	7.123725	-0.055309	3.546778
283.295332	4301.944425	7.128730	-0.055342	3.550030
283.348510	4310.010474	7.133734	-0.055357	3.553293
283.434005	4318.012687	7.138739	-0.055378	3.556528
283.820231	4325.984678	7.143744	-0.055455	3.559757
283.897158	4333.972038	7.148749	-0.055475	3.562980
283.811642	4342.045632	7.153754	-0.055464	3.566229
284.082643	4350.041473	7.158758	-0.055520	3.569456
284.294582	4358.040576	7.163763	-0.055564	3.572678
284.275445	4366.153749	7.168768	-0.055566	3.575937
284.195012	4374.137277	7.173773	-0.055556	3.579139
284.811163	4382.084511	7.178778	-0.055676	3.582344
284.869010	4390.164121	7.183782	-0.055692	3.585583
285.150285	4398.136166	7.188787	-0.055750	3.588783
285.096148	4406.256661	7.193792	-0.055745	3.592029
285.264074	4414.255521	7.198797	-0.055781	3.595230
285.551787	4422.237123	7.203802	-0.055840	3.598424
285.620539	4430.329748	7.208806	-0.055858	3.601654
285.435326	4438.324436	7.213811	-0.055829	3.604834
285.567843	4446.387621	7.218816	-0.055859	3.608049
285.895914	4454.402982	7.223821	-0.055925	3.611246
286.335037	4462.389242	7.228826	-0.056012	3.614433
286.662646	4470.416796	7.233830	-0.056078	3.617630
286.687398	4478.475859	7.238835	-0.056088	3.620828
286.807594	4486.473721	7.243840	-0.056116	3.624001
287.079772	4494.515051	7.248845	-0.056172	3.627194
287.035717	4502.561796	7.253850	-0.056169	3.630376
287.679167	4510.538779	7.258854	-0.056294	3.633548
287.766537	4518.536585	7.263859	-0.056315	3.636709
287.896524	4526.589021	7.268864	-0.056345	3.639890
288.092017	4534.586094	7.273869	-0.056386	3.643049
288.001782	4542.638159	7.278874	-0.056375	3.646218
288.218023	4550.673201	7.283878	-0.056420	3.649387
288.301359	4558.685760	7.288883	-0.056441	3.652540
288.634474	4566.734671	7.293888	-0.056508	3.655712
288.603187	4574.726309	7.298893	-0.056507	3.658848
289.049334	4582.719368	7.303898	-0.056596	3.661996
289.435737	4590.738013	7.308902	-0.056673	3.665148
289.377871	4598.778603	7.313907	-0.056667	3.668295
289.659724	4606.840106	7.318912	-0.056725	3.671456
289.762902	4614.849896	7.323917	-0.056749	3.674590
290.009558	4622.847912	7.328922	-0.056801	3.677720
289.997472	4630.929836	7.333926	-0.056804	3.680873
290.176741	4638.854193	7.338931	-0.056842	3.683968
290.327101	4646.969281	7.343936	-0.056875	3.687133
290.644568	4654.960481	7.348941	-0.056940	3.690251
290.725400	4662.992304	7.353946	-0.056960	3.693377
291.020771	4671.038978	7.358950	-0.057020	3.696511
291.080148	4679.048186	7.363955	-0.057036	3.699622
291.193989	4687.087887	7.368960	-0.057063	3.702743
291.438124	4695.102326	7.373965	-0.057114	3.705855
291.429467	4703.170354	7.378970	-0.057117	3.708979
291.527306	4711.230827	7.383974	-0.057141	3.712100
291.736790	4719.227697	7.388979	-0.057185	3.715197
292.095290	4727.224702	7.393984	-0.057257	3.718295
291.995234	4735.253163	7.398989	-0.057243	3.721391
292.330394	4743.174564	7.403994	-0.057311	3.724454
292.588884	4751.226842	7.408998	-0.057364	3.727563
292.571246	4759.293493	7.414003	-0.057366	3.730667
292.879545	4767.299305	7.419008	-0.057429	3.733754
292.954038	4775.345793	7.424013	-0.057448	3.736849
293.143305	4783.377717	7.429018	-0.057488	3.739938
293.177748	4791.392196	7.434022	-0.057500	3.743013
293.450526	4799.359628	7.439027	-0.057556	3.746074
293.776488	4807.401225	7.444032	-0.057622	3.749163
293.794718	4815.459535	7.449037	-0.057630	3.752247
294.151790	4823.422798	7.454042	-0.057702	3.755301
294.060707	4831.470303	7.459046	-0.057690	3.758374
294.362889	4839.487113	7.464051	-0.057752	3.761442
294.437045	4847.510308	7.469056	-0.057771	3.764504
294.680238	4855.539240	7.474061	-0.057821	3.767570
295.001997	4863.554300	7.479066	-0.057887	3.770631
295.059309	4871.591790	7.484070	-0.057902	3.773690
295.113507	4879.628637	7.489075	-0.057918	3.776748
295.455718	4887.623654	7.494080	-0.057987	3.779793
295.572344	4895.623663	7.499085	-0.058014	3.782833
295.650924	4903.707455	7.504090	-0.058033	3.785901
295.899748	4911.714811	7.509094	-0.058085	3.788941
296.360903	4919.738737	7.514099	-0.058176	3.791990
296.179231	4927.807129	7.519104	-0.058147	3.795039
296.009676	4935.804368	7.524109	-0.058121	3.798059
296.542085	4943.799823	7.529114	-0.058225	3.801091
296.703111	4951.756629	7.534118	-0.058261	3.804098
296.658095	4959.808476	7.539123	-0.058257	3.807134
296.927538	4967.860176	7.544128	-0.058313	3.810175
297.125722	4975.889547	7.549133	-0.058355	3.813203
297.091289	4983.949313	7.554138	-0.058354	3.816235
296.992444	4991.983611	7.559142	-0.058341	3.819253
297.413106	4999.952520	7.564147	-0.058424	3.822256
297.793417	5007.960238	7.569152	-0.058500	3.825270
297.876031	5016.007066	7.574157	-0.058521	3.828290
298.034118	5024.077503	7.579162	-0.058555	3.831318
298.057522	5032.087262	7.584166	-0.058565	3.834318
298.232994	5040.086047	7.589171	-0.058603	3.837315
298.620993	5048.075405	7.594176	-0.058680	3.840311
298.638473	5056.116168	7.599181	-0.058689	3.843315
298.813875	5064.142356	7.604186	-0.058727	3.846315
298.944213	5072.176664	7.609190	-0.058756	3.849314
299.024571	5080.209291	7.614195	-0.058776	3.852310
299.219855	5088.206385	7.619200	-0.058818	3.855292
299.330073	5096.233100	7.624205	-0.058844	3.858282
299.302873	5104.284858	7.629210	-0.058844	3.861275
299.564497	5112.272631	7.634214	-0.058898	3.864249
299.722140	5120.290238	7.639219	-0.058932	3.867228
299.828568	5128.337204	7.644224	-0.058957	3.870216
300.276053	5136.426847	7.649229	-0.059046	3.873224
300.316259	5144.456451	7.654234	-0.059059	3.876199
300.589049	5152.375450	7.659238	-0.059114	3.879135
300.634975	5160.395130	7.664243	-0.059128	3.882102
300.684747	5168.416534	7.669248	-0.059143	3.885068
300.871177	5176.420462	7.674253	-0.059183	3.888027
301.310799	5184.406459	7.679258	-0.059270	3.890983
301.534698	5192.469027	7.684262	-0.059317	3.893960
301.497401	5200.486044	7.689267	-0.059315	3.896912
301.647715	5208.479385	7.694272	-0.059348	3.899858
301.808784	5216.506275	7.699277	-0.059383	3.902814
301.739977	5224.499097	7.704282	-0.059376	3.905751
302.063980	5232.561745	7.709286	-0.059441	3.908718
302.032751	5240.611476	7.714291	-0.059441	3.911672
302.352318	5248.601651	7.719296	-0.059505	3.914609
302.250254	5256.634966	7.724301	-0.059492	3.917550
302.355305	5264.641092	7.729306	-0.059516	3.920484
302.842332	5272.653509	7.734310	-0.059612	3.923425
302.862518	5280.647261	7.739315	-0.059621	3.926349
303.223913	5288.707682	7.744320	-0.059694	3.929300
303.433780	5296.722384	7.749325	-0.059738	3.932230
303.558809	5304.739029	7.754330	-0.059766	3.935157
303.461625	5312.822955	7.759334	-0.059754	3.938102
303.722875	5320.835162	7.764339	-0.059807	3.941026
304.110941	5328.797981	7.769344	-0.059885	3.943931
304.181974	5336.852704	7.774349	-0.059903	3.946862
304.310039	5344.877876	7.779354	-0.059932	3.949781
304.648641	5352.930979	7.784358	-0.060001	3.952712
304.807826	5360.957165	7.789363	-0.060035	3.955628
305.059537	5368.955379	7.794368	-0.060088	3.958533
305.367996	5376.937757	7.799373	-0.060150	3.961431
305.640688	5384.907217	7.804378	-0.060206	3.964322
305.710463	5393.006713	7.809382	-0.060224	3.967254
305.853385	5400.979020	7.814387	-0.060256	3.970139
305.993149	5409.074914	7.819392	-0.060287	3.973066
306.102013	5417.114359	7.824397	-0.060313	3.975971
306.474486	5425.018619	7.829402	-0.060387	3.978829
306.473135	5433.132476	7.834406	-0.060392	3.981754
306.501542	5441.105199	7.839411	-0.060403	3.984626
306.601593	5449.162627	7.844416	-0.060427	3.987529
306.920239	5457.176300	7.849421	-0.060491	3.990417
306.730890	5465.192661	7.854426	-0.060461	3.993295
306.935096	5473.260138	7.859430	-0.060505	3.996196
307.170180	5481.151105	7.864435	-0.060553	3.999033
307.414455	5489.215396	7.869440	-0.060604	4.001929
307.676810	5497.203742	7.874445	-0.060658	4.004797
307.633217	5505.253401	7.879450	-0.060655	4.007679
308.057428	5513.285916	7.884454	-0.060740	4.010561
308.019506	5521.294569	7.889459	-0.060738	4.013424
308.185462	5529.377179	7.894464	-0.060774	4.016316
308.341436	5537.310487	7.899469	-0.060808	4.019151
308.450973	5545.352268	7.904474	-0.060834	4.022023
308.626817	5553.364383	7.909478	-0.060872	4.024883
308.983676	5561.366068	7.914483	-0.060943	4.027740
309.313142	5569.469569	7.919488	-0.061010	4.030631
309.414018	5577.560493	7.924493	-0.061034	4.033512
309.416314	5585.560719	7.929498	-0.061039	4.036357
309.966152	5593.449562	7.934502	-0.061147	4.039169
310.004760	5601.501718	7.939507	-0.061159	4.042028
309.978401	5609.485055	7.944512	-0.061160	4.044861
310.320082	5617.519221	7.949517	-0.061229	4.047715
310.470618	5625.561529	7.954522	-0.061262	4.050567
310.631311	5633.598541	7.959526	-0.061297	4.053415
310.864920	5641.633658	7.964531	-0.061346	4.056262
311.029102	5649.624571	7.969536	-0.061381	4.059090
311.393661	5657.671611	7.974541	-0.061455	4.061938
311.262512	5665.669039	7.979546	-0.061435	4.064760
311.678574	5673.754533	7.984550	-0.061518	4.067619
311.596442	5681.707016	7.989555	-0.061508	4.070422
311.762744	5689.735856	7.994560	-0.061544	4.073253
311.876925	5697.798306	7.999565	-0.061571	4.076094
312.172634	5705.740669	8.004570	-0.061631	4.078892
312.309866	5713.811680	8.009574	-0.061662	4.081732
312.515811	5721.771708	8.014579	-0.061705	4.084532
312.583434	5729.864945	8.019584	-0.061723	4.087375
312.684959	5737.852954	8.024589	-0.061747	4.090179
312.859506	5745.861280	8.029594	-0.061785	4.092989
313.088060	5753.948724	8.034598	-0.061833	4.095826
313.202988	5761.894914	8.039603	-0.061859	4.098610
313.451865	5769.961581	8.044608	-0.061911	4.101436
313.553450	5777.917551	8.049613	-0.061935	4.104219
313.884779	5785.967981	8.054618	-0.062002	4.107037
313.945086	5794.055586	8.059622	-0.062018	4.109862
313.996309	5801.991624	8.064627	-0.062033	4.112632
314.394422	5810.055327	8.069632	-0.062112	4.115449
314.499656	5818.024334	8.074637	-0.062137	4.118227
314.197329	5826.088434	8.079642	-0.062086	4.121031
314.748866	5834.015712	8.084646	-0.062194	4.123797
314.829101	5842.090940	8.089651	-0.062214	4.126606
315.094653	5850.094392	8.094656	-0.062269	4.129391
315.221904	5858.150095	8.099661	-0.062298	4.132190
315.414161	5866.135918	8.104666	-0.062339	4.134964
315.498980	5874.188949	8.109670	-0.062360	4.137758
315.619681	5882.184816	8.114675	-0.062387	4.140531
315.699722	5890.195760	8.119680	-0.062407	4.143306
315.973980	5898.241775	8.124685	-0.062464	4.146095
316.024555	5906.213244	8.129690	-0.062478	4.148852
316.374091	5914.300848	8.134694	-0.062549	4.151652
316.503641	5922.231354	8.139699	-0.062578	4.154393
316.350288	5930.322398	8.144704	-0.062555	4.157184
316.331060	5938.326964	8.149709	-0.062556	4.159944
316.839803	5946.287613	8.154714	-0.062656	4.162695
316.995487	5954.311031	8.159718	-0.062690	4.165461
317.036114	5962.340393	8.164723	-0.062703	4.168225
317.349999	5970.374340	8.169728	-0.062767	4.170993
317.735826	5978.393013	8.174733	-0.062844	4.173754
317.800432	5986.427706	8.179738	-0.062861	4.176515
317.954530	5994.462757	8.184742	-0.062895	4.179276
318.109076	6002.459484	8.189747	-0.062929	4.182021
318.362991	6010.479003	8.194752	-0.062981	4.184774
318.330426	6018.543981	8.199757	-0.062981	4.187537
318.690396	6026.555066	8.204762	-0.063053	4.190284
318.765691	6034.664433	8.209766	-0.063072	4.193060
318.794598	6042.681255	8.214771	-0.063083	4.195802
319.010057	6050.602852	8.219776	-0.063128	4.198511
319.257141	6058.642898	8.224781	-0.063179	4.201260
319.412072	6066.559653	8.229786	-0.063213	4.203964
319.402324	6074.677552	8.234790	-0.063217	4.206732
319.804808	6082.637718	8.239795	-0.063297	4.209450
319.784932	6090.729963	8.244800	-0.063298	4.212206
319.954713	6098.730433	8.249805	-0.063335	4.214931
320.159561	6106.712059	8.254810	-0.063378	4.217649
320.331375	6114.737664	8.259814	-0.063416	4.220379
320.309288	6122.765621	8.264819	-0.063417	4.223106
320.034330	6130.854725	8.269824	-0.063371	4.225849
320.318328	6138.812385	8.274829	-0.063429	4.228552
320.799178	6146.830721	8.279834	-0.063524	4.231276
321.045441	6154.836024	8.284838	-0.063575	4.233991
321.035092	6162.885979	8.289843	-0.063578	4.236717
321.307436	6170.864942	8.294848	-0.063634	4.239420
321.434054	6178.876716	8.299853	-0.063663	4.242131
321.441052	6186.880723	8.304858	-0.063669	4.244836
321.753883	6194.923950	8.309862	-0.063733	4.247556
321.940022	6202.936534	8.314867	-0.063772	4.250263
322.145009	6210.930594	8.319872	-0.063816	4.252961
322.421982	6219.001777	8.324877	-0.063873	4.255685
322.272504	6226.988987	8.329882	-0.063850	4.258374
322.526342	6235.037896	8.334886	-0.063902	4.261087
322.875813	6242.972278	8.339891	-0.063973	4.263760
323.110241	6251.073045	8.344896	-0.064022	4.266486
322.919212	6259.067835	8.349901	-0.063991	4.269170
322.990631	6267.109309	8.354906	-0.064010	4.271872
323.501517	6275.116342	8.359910	-0.064110	4.274564
323.586177	6283.117479	8.364915	-0.064131	4.277248
323.796221	6291.134119	8.369920	-0.064175	4.279937
323.658531	6299.159120	8.374925	-0.064155	4.282624
323.674219	6307.142859	8.379930	-0.064163	4.285297
323.944307	6315.182437	8.384934	-0.064219	4.287989
324.207001	6323.163870	8.389939	-0.064273	4.290659
324.408695	6331.223089	8.394944	-0.064315	4.293354
324.341401	6339.255462	8.399949	-0.064308	4.296036
324.375603	6347.204007	8.404954	-0.064320	4.298688
324.798830	6355.300678	8.409958	-0.064404	4.301392
324.802546	6363.186974	8.414963	-0.064410	4.304021
324.854741	6371.331854	8.419968	-0.064425	4.306734
324.944826	6379.310158	8.424973	-0.064447	4.309391
325.085194	6387.345637	8.429978	-0.064478	4.312065
325.594108	6395.302483	8.434982	-0.064578	4.314715
325.397903	6403.376420	8.439987	-0.064547	4.317395
325.676264	6411.342649	8.444992	-0.064604	4.320043
325.846811	6419.371179	8.449997	-0.064641	4.322708
325.958167	6427.372316	8.455002	-0.064666	4.325363
326.192735	6435.463005	8.460006	-0.064715	4.328046
326.037275	6443.475045	8.465011	-0.064692	4.330699
326.491067	6451.469560	8.470016	-0.064781	4.333349
326.606301	6459.530204	8.475021	-0.064808	4.336016
326.854789	6467.453813	8.480026	-0.064859	4.338638
327.098905	6475.533658	8.485030	-0.064910	4.341309
327.138812	6483.461668	8.490035	-0.064923	4.343927
327.661005	6491.516651	8.495040	-0.065025	4.346589
327.464087	6499.562207	8.500045	-0.064994	4.349241
327.392390	6507.624884	8.505050	-0.064986	4.351898
327.826155	6515.629752	8.510054	-0.065072	4.354538
328.047306	6523.594182	8.515059	-0.065118	4.357161
328.064561	6531.587061	8.520064	-0.065126	4.359791
328.130078	6539.660645	8.525069	-0.065144	4.362446
328.272667	6547.608228	8.530074	-0.065176	4.365058
328.277410	6555.694882	8.535078	-0.065182	4.367714
328.486305	6563.643122	8.540083	-0.065226	4.370324
328.603488	6571.745754	8.545088	-0.065253	4.372982
328.912180	6579.729261	8.550093	-0.065315	4.375601
328.850798	6587.726421	8.555098	-0.065309	4.378221
329.290443	6595.810438	8.560103	-0.065396	4.380870
329.317499	6603.727657	8.565107	-0.065407	4.383461
329.254264	6611.805185	8.570112	-0.065400	4.386102
329.719945	6619.770778	8.575117	-0.065492	4.388708
329.557947	6627.861940	8.580122	-0.065467	4.391350
329.968764	6635.844163	8.585127	-0.065549	4.393958
330.031653	6643.875482	8.590131	-0.065566	4.396578
330.371112	6651.825773	8.595136	-0.065634	4.399172
330.585463	6659.891622	8.600141	-0.065679	4.401802
330.552404	6667.835717	8.605146	-0.065678	4.404388
330.968412	6675.943929	8.610151	-0.065761	4.407029
331.268274	6683.927802	8.615155	-0.065822	4.409628
331.336843	6691.997654	8.620160	-0.065840	4.412251
331.667492	6700.047358	8.625165	-0.065907	4.414868
331.824439	6708.069532	8.630170	-0.065941	4.417473
332.017386	6716.097793	8.635175	-0.065982	4.420079
331.825740	6724.111687	8.640179	-0.065952	4.422677
332.114952	6732.143961	8.645184	-0.066011	4.425282
332.362520	6740.173135	8.650189	-0.066062	4.427883
332.436112	6748.260288	8.655194	-0.066081	4.430502
332.622285	6756.248026	8.660199	-0.066121	4.433087
332.725700	6764.257349	8.665203	-0.066145	4.435677
332.834591	6772.244249	8.670208	-0.066171	4.438258
332.881305	6780.330672	8.675213	-0.066185	4.440869
333.135705	6788.226933	8.680218	-0.066237	4.443419
333.284850	6796.292176	8.685223	-0.066270	4.446021
333.234656	6804.244258	8.690227	-0.066266	4.448584
333.498899	6812.352079	8.695232	-0.066321	4.451198
333.692921	6820.342681	8.700237	-0.066362	4.453772
333.637390	6828.374774	8.705242	-0.066357	4.456356
334.140902	6836.377889	8.710247	-0.066456	4.458932
334.223098	6844.401790	8.715251	-0.066476	4.461512
334.259144	6852.355219	8.720256	-0.066488	4.464067
334.407910	6860.461404	8.725261	-0.066521	4.466670
334.420199	6868.428328	8.730266	-0.066529	4.469226
334.580644	6876.521430	8.735271	-0.066564	4.471822
334.714900	6884.439399	8.740275	-0.066594	4.474360
334.856289	6892.505150	8.745280	-0.066625	4.476944
335.104331	6900.473710	8.750285	-0.066677	4.479496
335.151821	6908.503262	8.755290	-0.066691	4.482065
335.364194	6916.512832	8.760295	-0.066736	4.484627
335.826507	6924.505297	8.765299	-0.066827	4.487183
335.849390	6932.521758	8.770304	-0.066836	4.489744
335.969501	6940.618892	8.775309	-0.066864	4.492329
336.176650	6948.594375	8.780314	-0.066908	4.494874
336.202595	6956.649136	8.785319	-0.066918	4.497442
336.251127	6964.605345	8.790323	-0.066932	4.499977
336.587154	6972.600954	8.795328	-0.067000	4.502525
336.764369	6980.640341	8.800333	-0.067038	4.505084
336.604891	6988.707812	8.805338	-0.067014	4.507650
336.762282	6996.744876	8.810343	-0.067048	4.510206
336.921596	7004.749199	8.815347	-0.067083	4.512749
336.965862	7012.726888	8.820352	-0.067096	4.515283
337.364037	7020.653212	8.825357	-0.067176	4.517800
337.678052	7028.672612	8.830362	-0.067239	4.520345
337.962757	7036.697945	8.835367	-0.067298	4.522890
337.807390	7044.743127	8.840371	-0.067274	4.525438
338.263125	7052.751343	8.845376	-0.067364	4.527975
338.339315	7060.836930	8.850381	-0.067383	4.530535
338.487047	7068.797118	8.855386	-0.067416	4.533053
338.746444	7076.867469	8.860391	-0.067470	4.535605
339.141151	7084.774218	8.865395	-0.067548	4.538104
339.468305	7092.834429	8.870400	-0.067614	4.540650
339.571906	7100.813142	8.875405	-0.067639	4.543168
339.912305	7108.884452	8.880410	-0.067707	4.545715
340.004606	7116.917875	8.885415	-0.067730	4.548247
340.193892	7124.914406	8.890419	-0.067770	4.550767
340.209546	7132.960440	8.895424	-0.067778	4.553300
340.582555	7140.973529	8.900429	-0.067853	4.555823
340.583272	7148.953253	8.905434	-0.067858	4.558333
340.733204	7157.010819	8.910439	-0.067892	4.560866
340.888220	7164.940694	8.915443	-0.067926	4.563358
341.112082	7172.998821	8.920448	-0.067972	4.565888
340.813876	7181.075910	8.925453	-0.067922	4.568423
341.133684	7189.056833	8.930458	-0.067987	4.570926
341.619019	7197.066143	8.935463	-0.068083	4.573438
341.614896	7205.103931	8.940467	-0.068087	4.575956
341.628107	7213.054300	8.945472	-0.068095	4.578446
341.572068	7221.164067	8.950477	-0.068089	4.580984
341.950389	7229.059299	8.955482	-0.068165	4.583454
342.080665	7237.149050	8.960487	-0.068194	4.585983
342.394843	7245.099466	8.965491	-0.068258	4.588467
342.735875	7253.169200	8.970496	-0.068327	4.590988
342.861790	7261.187476	8.975501	-0.068356	4.593490
342.923554	7269.240503	8.980506	-0.068372	4.596002
343.193591	7277.204921	8.985511	-0.068428	4.598486
343.364434	7285.231290	8.990515	-0.068465	4.600987
343.581813	7293.165650	8.995520	-0.068510	4.603458
343.823167	7301.285888	9.000525	-0.068561	4.605985
343.814218	7309.242900	9.005530	-0.068564	4.608460
343.768677	7317.324851	9.010535	-0.068561	4.610973
344.068204	7325.284506	9.015539	-0.068622	4.613446
344.315705	7333.340214	9.020544	-0.068673	4.615948
344.628087	7341.324763	9.025549	-0.068737	4.618427
344.698883	7349.349571	9.030554	-0.068755	4.620917
345.143822	7357.328522	9.035559	-0.068843	4.623391
345.177547	7365.413576	9.040563	-0.068854	4.625896
345.211278	7373.429428	9.045568	-0.068866	4.628379
345.414810	7381.487648	9.050573	-0.068909	4.630873
345.581019	7389.370684	9.055578	-0.068945	4.633312
345.552413	7397.457163	9.060583	-0.068945	4.635813
345.619628	7405.427648	9.065587	-0.068963	4.638276
345.939001	7413.472936	9.070592	-0.069027	4.640761
346.120803	7421.467137	9.075597	-0.069067	4.643229
346.224593	7429.504172	9.080602	-0.069091	4.645709
346.501421	7437.534349	9.085607	-0.069148	4.648185
346.382706	7445.609518	9.090611	-0.069131	4.650674
346.518536	7453.564291	9.095616	-0.069161	4.653124
346.721175	7461.615632	9.100621	-0.069204	4.655603
346.972815	7469.551621	9.105626	-0.069256	4.658045
346.920207	7477.669384	9.110631	-0.069252	4.660542
347.081021	7485.589492	9.115635	-0.069287	4.662976
347.306612	7493.617551	9.120640	-0.069334	4.665443
347.733978	7501.647145	9.125645	-0.069419	4.667908
347.601578	7509.642730	9.130650	-0.069400	4.670362
347.893758	7517.777538	9.135655	-0.069459	4.672857
347.929587	7525.733005	9.140659	-0.069471	4.675296
348.282376	7533.707542	9.145664	-0.069542	4.677739
348.629769	7541.719012	9.150669	-0.069612	4.680193
348.666503	7549.685120	9.155674	-0.069624	4.682631
348.718978	7557.735065	9.160679	-0.069639	4.685094
348.672287	7565.771637	9.165683	-0.069635	4.687551
348.733554	7573.787188	9.170688	-0.069652	4.690001
349.068567	7581.825203	9.175693	-0.069720	4.692455
348.821490	7589.822657	9.180698	-0.069679	4.694897
349.058524	7597.875024	9.185703	-0.069728	4.697354
349.110852	7605.824522	9.190707	-0.069743	4.699778
349.161439	7613.889819	9.195712	-0.069758	4.702236
349.397380	7621.827893	9.200717	-0.069807	4.704654
349.420327	7629.870766	9.205722	-0.069816	4.707103
349.792577	7637.876320	9.210727	-0.069891	4.709539
349.690645	7645.961970	9.215731	-0.069877	4.711998
349.895639	7653.939293	9.220736	-0.069920	4.714423
350.184808	7661.983933	9.225741	-0.069979	4.716867
350.415247	7669.936923	9.230746	-0.070028	4.719282
350.647720	7678.042246	9.235751	-0.070076	4.721742
350.826785	7685.972480	9.240755	-0.070115	4.724147
350.901219	7694.013327	9.245760	-0.070134	4.726585
351.360893	7702.011239	9.250765	-0.070224	4.729008
351.205761	7710.086911	9.255770	-0.070201	4.731455
351.582982	7718.049462	9.260775	-0.070276	4.733865
351.645626	7726.143136	9.265779	-0.070293	4.736314
352.018005	7734.059353	9.270784	-0.070368	4.738707
352.105790	7742.178142	9.275789	-0.070389	4.741161
352.523274	7750.096837	9.280794	-0.070472	4.743552
352.674853	7758.215247	9.285799	-0.070506	4.746003
352.832439	7766.181724	9.290803	-0.070540	4.748407
352.827256	7774.275262	9.295808	-0.070544	4.750849
352.800234	7782.253680	9.300813	-0.070545	4.753254
352.860887	7790.264837	9.305818	-0.070561	4.755668
353.641406	7798.189724	9.310823	-0.070712	4.758053
353.681338	7806.275389	9.315827	-0.070724	4.760487
353.597436	7814.276941	9.320832	-0.070714	4.762895
353.673546	7822.355608	9.325837	-0.070733	4.765324
353.910422	7830.325628	9.330842	-0.070783	4.767719
353.775251	7838.379420	9.335847	-0.070763	4.770139
354.222686	7846.371078	9.340851	-0.070851	4.772537
354.599900	7854.350642	9.345856	-0.070927	4.774931
354.591664	7862.410682	9.350861	-0.070930	4.777348
354.901969	7870.382220	9.355866	-0.070993	4.779737
355.181077	7878.434669	9.360871	-0.071050	4.782149
355.331413	7886.391927	9.365875	-0.071084	4.784532
355.420941	7894.476704	9.370880	-0.071105	4.786952
355.599752	7902.457001	9.375885	-0.071144	4.789339
355.884178	7910.502055	9.380890	-0.071202	4.791744
355.904605	7918.486631	9.385895	-0.071211	4.794130
355.832251	7926.587025	9.390899	-0.071203	4.796550
355.589866	7934.486605	9.395904	-0.071163	4.798910
355.778692	7942.629511	9.400909	-0.071203	4.801340
355.967336	7950.487681	9.405914	-0.071244	4.803683
356.211250	7958.550499	9.410919	-0.071294	4.806086
356.589383	7966.574073	9.415923	-0.071370	4.808476
356.859244	7974.596222	9.420928	-0.071425	4.810864
356.886183	7982.614091	9.425933	-0.071436	4.813251
357.207501	7989.976530	9.430938	-0.071500	4.815440
357.521779	7994.634720	9.435943	-0.071562	4.816824

357.590681	7997.235112	9.440947	-0.071576	4.817597
357.789764	7998.330798	9.445952	-0.071614	4.817922
357.578917	7998.836217	9.450957	-0.071575	4.818073
357.550362	7999.827123	9.455962	-0.071570	4.818368
357.947661	7999.852367	9.460967	-0.071644	4.818374
358.002092	7999.805835	9.465971	-0.071654	4.818360
357.847568	7999.885685	9.470976	-0.071626	4.818384
357.967114	7999.857873	9.475981	-0.071648	4.818376
357.947705	7999.852363	9.480986	-0.071644	4.818374
357.993740	7999.839323	9.485991	-0.071653	4.818370
358.316310	7999.853071	9.490995	-0.071713	4.818373
358.554324	7999.840489	9.496000	-0.071757	4.818368
358.680243	7999.848467	9.501005	-0.071781	4.818370
358.587837	7999.830432	9.506010	-0.071763	4.818365
358.813920	7999.873350	9.511015	-0.071805	4.818377
358.442205	7999.857893	9.516019	-0.071736	4.818374
358.565593	7999.855336	9.521024	-0.071759	4.818373
358.725650	7999.855367	9.526029	-0.071789	4.818372
358.727480	7999.807084	9.531034	-0.071789	4.818358
358.590764	7999.851467	9.536039	-0.071764	4.818371
358.942744	7999.853007	9.541043	-0.071829	4.818370
358.961531	7999.840654	9.546048	-0.071833	4.818367
359.015230	7999.883375	9.551053	-0.071843	4.818379
359.076392	7999.814878	9.556058	-0.071854	4.818359
359.209155	7999.880707	9.561063	-0.071879	4.818378
358.979125	7999.871338	9.566067	-0.071836	4.818376
358.964794	7999.904751	9.571072	-0.071833	4.818386
359.151802	7999.884140	9.576077	-0.071868	4.818379
359.188434	7999.893028	9.581082	-0.071875	4.818381
359.178099	7999.922294	9.586087	-0.071873	4.818390
359.327418	7999.861273	9.591091	-0.071901	4.818371
359.746234	7999.854254	9.596096	-0.071979	4.818368
359.470837	7999.879986	9.601101	-0.071927	4.818376
359.239997	7999.907362	9.606106	-0.071885	4.818385
359.564737	7999.914841	9.611111	-0.071945	4.818386
359.295383	7999.928051	9.616115	-0.071895	4.818391
359.347831	7999.901445	9.621120	-0.071905	4.818383
359.467104	7999.921937	9.626125	-0.071927	4.818389
359.974403	7999.866740	9.631130	-0.072021	4.818370
359.959445	7999.877042	9.636135	-0.072018	4.818374
360.012279	7999.845189	9.641139	-0.072028	4.818364
359.652016	7999.896043	9.646144	-0.071961	4.818380
360.135029	7999.870978	9.651149	-0.072051	4.818371
359.951499	7999.862228	9.656154	-0.072017	4.818369
360.250365	7999.896669	9.661159	-0.072072	4.818378
360.247621	7999.897681	9.666163	-0.072072	4.818379
360.233280	7999.889087	9.671168	-0.072069	4.818376
360.300610	7999.892085	9.676173	-0.072082	4.818377
360.312360	7999.869136	9.681178	-0.072084	4.818370
360.657452	7999.892642	9.686183	-0.072148	4.818375
360.552690	7999.841884	9.691187	-0.072129	4.818361
360.604126	7999.849920	9.696192	-0.072138	4.818363
360.669752	7999.875999	9.701197	-0.072150	4.818370
360.527123	7999.865693	9.706202	-0.072124	4.818368
360.750308	7999.890724	9.711207	-0.072165	4.818374
360.625168	7999.876451	9.716211	-0.072142	4.818371
360.762915	7999.873037	9.721216	-0.072168	4.818369
360.789435	7999.881791	9.726221	-0.072173	4.818372
360.862105	7999.818697	9.731226	-0.072186	4.818353
360.880902	7999.863055	9.736231	-0.072190	4.818366
360.727230	7999.856803	9.741235	-0.072161	4.818364
360.554037	7999.851340	9.746240	-0.072129	4.818364
360.543414	7999.880603	9.751245	-0.072127	4.818372
360.856146	7999.867971	9.756250	-0.072185	4.818367
361.116970	7999.910308	9.761255	-0.072233	4.818379
360.819509	7999.892685	9.766259	-0.072178	4.818375
360.811675	7999.881027	9.771264	-0.072177	4.818371
360.758812	7999.860366	9.776269	-0.072167	4.818365
360.714603	7999.881829	9.781274	-0.072158	4.818372
360.762422	7999.905571	9.786279	-0.072167	4.818379
360.583578	7999.897932	9.791283	-0.072134	4.818377
360.783100	7999.864886	9.796288	-0.072171	4.818367
360.591022	7999.917983	9.801293	-0.072135	4.818383
360.461685	7999.875299	9.806298	-0.072111	4.818371
360.966299	7999.861026	9.811303	-0.072205	4.818365
360.979963	7999.860157	9.816307	-0.072208	4.818364
360.982666	7999.884346	9.821312	-0.072208	4.818372
360.942342	7999.896410	9.826317	-0.072201	4.818375
361.248664	7999.821730	9.831322	-0.072258	4.818352
361.362224	7999.879956	9.836327	-0.072279	4.818369
360.963189	7999.870429	9.841331	-0.072205	4.818368
361.062215	7999.889603	9.846336	-0.072223	4.818373
361.195500	7999.911335	9.851341	-0.072248	4.818379
361.064373	7999.870725	9.856346	-0.072223	4.818367
361.316418	7999.906645	9.861351	-0.072270	4.818377
361.361920	7999.873644	9.866355	-0.072279	4.818367
361.119302	7999.883007	9.871360	-0.072234	4.818371
361.270146	7999.902873	9.876365	-0.072262	4.818376
361.255547	7999.855417	9.881370	-0.072259	4.818362
361.485634	7999.892094	9.886375	-0.072302	4.818372
361.450712	7999.865371	9.891379	-0.072295	4.818364
361.339717	7999.896445	9.896384	-0.072274	4.818374
361.541708	7999.906491	9.901389	-0.072312	4.818376
361.505437	7999.860846	9.906394	-0.072305	4.818363
361.406826	7999.901538	9.911399	-0.072287	4.818375
361.383199	7999.881267	9.916403	-0.072283	4.818369
361.579395	7999.862880	9.921408	-0.072319	4.818363
361.691593	7999.861226	9.926413	-0.072340	4.818362
361.598143	7999.849475	9.931418	-0.072322	4.818359
361.732196	7999.883820	9.936423	-0.072347	4.818369
361.590152	7999.833613	9.941427	-0.072321	4.818354
361.768351	7999.874849	9.946432	-0.072354	4.818366
361.779838	7999.904407	9.951437	-0.072356	4.818374
361.657241	7999.874413	9.956442	-0.072333	4.818366
361.777098	7999.892816	9.961447	-0.072356	4.818371
361.733332	7999.870175	9.966451	-0.072348	4.818364
361.750610	7999.862003	9.971456	-0.072351	4.818362
361.730380	7999.889038	9.976461	-0.072347	4.818370
361.762050	7999.855852	9.981466	-0.072353	4.818360
361.838177	7999.883123	9.986471	-0.072367	4.818368
361.729165	7999.849109	9.991475	-0.072347	4.818358
361.735255	7999.863892	9.996480	-0.072348	4.818363
362.001331	7999.865343	10.001485	-0.072397	4.818362
362.070763	7999.836862	10.006490	-0.072410	4.818353
361.807508	7999.836497	10.011495	-0.072361	4.818354
361.892109	7999.830274	10.016499	-0.072377	4.818352
361.915220	7999.847385	10.021504	-0.072381	4.818357
362.065959	7999.867250	10.026509	-0.072409	4.818362
362.114107	7999.841636	10.031514	-0.072418	4.818354
361.900813	7999.878696	10.036519	-0.072378	4.818366
361.830139	7999.849395	10.041523	-0.072365	4.818358
362.015198	7999.839261	10.046528	-0.072400	4.818354
362.222588	7999.878787	10.051533	-0.072438	4.818365
361.964717	7999.859590	10.056538	-0.072390	4.818360
361.971747	7999.882788	10.061543	-0.072392	4.818367
361.981387	7999.886066	10.066547	-0.072393	4.818368
362.086587	7999.825505	10.071552	-0.072413	4.818350
362.055297	7999.883899	10.076557	-0.072407	4.818367
362.015926	7999.825610	10.081562	-0.072400	4.818350
361.918010	7999.899918	10.086567	-0.072382	4.818373
362.017310	7999.870786	10.091571	-0.072400	4.818364
361.832475	7999.883020	10.096576	-0.072366	4.818368
362.000110	7999.881056	10.101581	-0.072397	4.818367
361.925948	7999.860110	10.106586	-0.072383	4.818361
361.813434	7999.905868	10.111591	-0.072362	4.818375
361.750347	7999.887170	10.116595	-0.072350	4.818369
361.948126	7999.813142	10.121600	-0.072387	4.818347
361.897708	7999.864980	10.126605	-0.072378	4.818362
362.004334	7999.823342	10.131610	-0.072397	4.818349
362.043353	7999.883726	10.136615	-0.072405	4.818367
362.077707	7999.854776	10.141619	-0.072411	4.818359
362.024332	7999.860364	10.146624	-0.072401	4.818360
362.095500	7999.889669	10.151629	-0.072414	4.818369
362.321900	7999.849631	10.156634	-0.072456	4.818356
362.039547	7999.886819	10.161639	-0.072404	4.818368
362.159948	7999.884225	10.166643	-0.072426	4.818367
362.089796	7999.878036	10.171648	-0.072413	4.818365
362.022973	7999.916001	10.176653	-0.072401	4.818377
361.775561	7999.872788	10.181658	-0.072355	4.818365
361.902015	7999.892329	10.186663	-0.072378	4.818370
361.613665	7999.906332	10.191667	-0.072325	4.818376
361.926418	7999.872698	10.196672	-0.072383	4.818364
362.138148	7999.884976	10.201677	-0.072422	4.818367
362.237120	7999.822231	10.206682	-0.072441	4.818348
362.230751	7999.886210	10.211687	-0.072439	4.818367
362.197457	7999.880513	10.216691	-0.072433	4.818366
362.160896	7999.865320	10.221696	-0.072426	4.818361
362.333551	7999.881277	10.226701	-0.072458	4.818365
362.194750	7999.862619	10.231706	-0.072433	4.818360
362.361566	7999.870096	10.236711	-0.072464	4.818362
362.204037	7999.895298	10.241715	-0.072434	4.818370
362.172979	7999.849722	10.246720	-0.072428	4.818357
362.314359	7999.871563	10.251725	-0.072455	4.818363
362.300267	7999.858771	10.256730	-0.072452	4.818359
362.355377	7999.895214	10.261735	-0.072462	4.818369
362.429967	7999.882555	10.266739	-0.072476	4.818365
362.321858	7999.874809	10.271744	-0.072456	4.818364
362.517278	7999.891071	10.276749	-0.072492	4.818368
362.180652	7999.872921	10.281754	-0.072430	4.818364
362.583342	7999.877247	10.286759	-0.072505	4.818363
362.569389	7999.855004	10.291763	-0.072502	4.818357
362.493721	7999.807782	10.296768	-0.072488	4.818343
362.493903	7999.901255	10.301773	-0.072488	4.818371
362.545327	7999.823172	10.306778	-0.072498	4.818347
362.570596	7999.837161	10.311783	-0.072502	4.818351
362.593999	7999.860578	10.316787	-0.072507	4.818358
362.537064	7999.835661	10.321792	-0.072496	4.818351
362.628490	7999.870489	10.326797	-0.072513	4.818361
362.690491	7999.869215	10.331802	-0.072525	4.818360
362.642056	7999.878019	10.336807	-0.072516	4.818363
362.700901	7999.857799	10.341811	-0.072526	4.818357
362.694770	7999.838811	10.346816	-0.072525	4.818351
362.736969	7999.896087	10.351821	-0.072533	4.818368
362.683752	7999.841812	10.356826	-0.072523	4.818352
362.636012	7999.876882	10.361831	-0.072514	4.818363
362.540278	7999.851447	10.366835	-0.072496	4.818356
362.554586	7999.861089	10.371840	-0.072499	4.818359
362.709759	7999.864210	10.376845	-0.072528	4.818359
362.623952	7999.802149	10.381850	-0.072512	4.818341
362.688992	7999.860780	10.386855	-0.072524	4.818358
362.755827	7999.848018	10.391859	-0.072536	4.818354
362.876162	7999.856975	10.396864	-0.072559	4.818356
362.860066	7999.863061	10.401869	-0.072556	4.818358
362.844127	7999.801932	10.406874	-0.072553	4.818340
362.934913	7999.839902	10.411879	-0.072570	4.818351
362.882709	7999.818199	10.416883	-0.072560	4.818344
363.004070	7999.840824	10.421888	-0.072583	4.818351
362.978394	7999.866736	10.426893	-0.072578	4.818359
362.717089	7999.863245	10.431898	-0.072529	4.818359
362.758166	7999.859591	10.436903	-0.072537	4.818357
362.720543	7999.855937	10.441907	-0.072530	4.818356
362.783428	7999.804263	10.446912	-0.072541	4.818341
362.802246	7999.827618	10.451917	-0.072545	4.818348
362.962432	7999.805601	10.456922	-0.072575	4.818340
362.741922	7999.838363	10.461927	-0.072534	4.818351
362.747831	7999.837390	10.466931	-0.072535	4.818351
362.973000	7999.797336	10.471936	-0.072577	4.818338
362.951208	7999.859009	10.476941	-0.072573	4.818356
362.716100	7999.796003	10.481946	-0.072529	4.818339
362.809525	7999.843461	10.486951	-0.072546	4.818352
362.773871	7999.853486	10.491955	-0.072540	4.818355
362.695122	7999.833529	10.496960	-0.072525	4.818350
362.822773	7999.900348	10.501965	-0.072549	4.818369
362.664326	7999.843617	10.506970	-0.072519	4.818353
362.827885	7999.845801	10.511975	-0.072550	4.818353
362.813610	7999.825654	10.516979	-0.072547	4.818347
362.746760	7999.848916	10.521984	-0.072534	4.818354
362.819658	7999.833084	10.526989	-0.072548	4.818349
362.830168	7999.850027	10.531994	-0.072550	4.818354
362.749264	7999.846845	10.536999	-0.072535	4.818354
362.790714	7999.841096	10.542003	-0.072542	4.818352
362.721354	7999.818113	10.547008	-0.072530	4.818345
363.012599	7999.829353	10.552013	-0.072584	4.818347
362.941119	7999.790588	10.557018	-0.072570	4.818336
362.859312	7999.835706	10.562023	-0.072555	4.818350
362.916259	7999.856420	10.567027	-0.072566	4.818356
363.091100	7999.831447	10.572032	-0.072598	4.818348
363.089749	7999.838780	10.577037	-0.072598	4.818350
362.919453	7999.836504	10.582042	-0.072566	4.818350
362.758785	7999.875317	10.587047	-0.072536	4.818362
363.135511	7999.895052	10.592051	-0.072607	4.818366
362.914439	7999.849037	10.597056	-0.072565	4.818354
362.951586	7999.845331	10.602061	-0.072572	4.818352
363.021577	7999.844164	10.607066	-0.072585	4.818352
363.129258	7999.845601	10.612071	-0.072605	4.818352
363.165041	7999.864982	10.617075	-0.072612	4.818357
362.867014	7999.844196	10.622080	-0.072556	4.818352
363.017056	7999.860903	10.627085	-0.072584	4.818357
362.817544	7999.882393	10.632090	-0.072547	4.818364
362.918716	7999.924703	10.637095	-0.072566	4.818376
363.055266	7999.904470	10.642099	-0.072591	4.818369
363.144657	7999.892010	10.647104	-0.072608	4.818365
362.900775	7999.932862	10.652109	-0.072563	4.818379
362.844489	7999.872244	10.657114	-0.072552	4.818361
362.928531	7999.898572	10.662119	-0.072568	4.818368
362.774679	7999.898616	10.667123	-0.072539	4.818369
362.845264	7999.884854	10.672128	-0.072552	4.818364
363.077481	7999.919462	10.677133	-0.072595	4.818374
362.897103	7999.863488	10.682138	-0.072562	4.818358
362.964960	7999.910605	10.687143	-0.072574	4.818372
362.987322	7999.872043	10.692147	-0.072579	4.818360
363.056277	7999.875063	10.697152	-0.072591	4.818361
362.982249	7999.905581	10.702157	-0.072578	4.818370
362.907850	7999.855224	10.707162	-0.072564	4.818355
363.090149	7999.877613	10.712167	-0.072598	4.818361
363.210892	7999.882375	10.717171	-0.072620	4.818362
363.098738	7999.870373	10.722176	-0.072599	4.818359
363.265943	7999.878907	10.727181	-0.072630	4.818361
363.075455	7999.866909	10.732186	-0.072595	4.818358
362.920508	7999.880592	10.737191	-0.072566	4.818363
362.964028	7999.867519	10.742195	-0.072574	4.818359
363.189836	7999.824322	10.747200	-0.072616	4.818345
363.140616	7999.892981	10.752205	-0.072607	4.818366
363.136565	7999.870870	10.757210	-0.072606	4.818359
363.316571	7999.897430	10.762215	-0.072640	4.818366
363.300404	7999.908766	10.767219	-0.072637	4.818370
363.202306	7999.892750	10.772224	-0.072618	4.818365
363.230982	7999.921489	10.777229	-0.072624	4.818374
363.346663	7999.897827	10.782234	-0.072645	4.818366
363.107483	7999.890429	10.787239	-0.072601	4.818365
363.280335	7999.887486	10.792243	-0.072633	4.818364
363.309854	7999.862673	10.797248	-0.072638	4.818356
363.388041	7999.929883	10.802253	-0.072653	4.818376
363.172238	7999.882888	10.807258	-0.072613	4.818363
363.243645	7999.903795	10.812263	-0.072626	4.818369
363.070778	7999.909887	10.817267	-0.072594	4.818371
363.052606	7999.865532	10.822272	-0.072590	4.818358
363.088065	7999.924819	10.827277	-0.072597	4.818375
363.058953	7999.869815	10.832282	-0.072591	4.818359
363.119237	7999.880072	10.837287	-0.072603	4.818362
363.118205	7999.893710	10.842291	-0.072602	4.818366
362.994828	7999.906765	10.847296	-0.072580	4.818370
363.157278	7999.934140	10.852301	-0.072610	4.818378
363.048461	7999.911680	10.857306	-0.072589	4.818372
363.177080	7999.896593	10.862311	-0.072613	4.818367
363.257714	7999.886116	10.867315	-0.072628	4.818363
363.117810	7999.875843	10.872320	-0.072602	4.818361
363.311505	7999.898385	10.877325	-0.072638	4.818367
363.323169	7999.884886	10.882330	-0.072641	4.818363
363.307207	7999.882571	10.887335	-0.072638	4.818362
363.103724	7999.900857	10.892339	-0.072600	4.818368
363.244441	7999.857574	10.897344	-0.072626	4.818355
363.466800	7999.894152	10.902349	-0.072667	4.818365
363.135067	7999.900222	10.907354	-0.072605	4.818368
363.254780	7999.907071	10.912359	-0.072628	4.818369
363.308469	7999.900435	10.917363	-0.072638	4.818367
363.422967	7999.877807	10.922368	-0.072659	4.818360
363.466154	7999.915143	10.927373	-0.072667	4.818371
363.259063	7999.871414	10.932378	-0.072628	4.818359
363.246214	7999.915353	10.937383	-0.072626	4.818372
363.319220	7999.891120	10.942387	-0.072640	4.818364
363.380702	7999.850980	10.947392	-0.072651	4.818352
363.602384	7999.893851	10.952397	-0.072692	4.818364
363.453627	7999.860354	10.957402	-0.072665	4.818355
363.491944	7999.881870	10.962407	-0.072672	4.818361
363.518718	7999.892730	10.967411	-0.072677	4.818364
363.387967	7999.879428	10.972416	-0.072652	4.818361
363.297806	7999.916032	10.977421	-0.072635	4.818372
363.387080	7999.884666	10.982426	-0.072652	4.818362
363.294710	7999.901285	10.987431	-0.072635	4.818368
363.289425	7999.887560	10.992435	-0.072634	4.818364
362.987530	7999.894028	10.997440	-0.072578	4.818367
363.329789	7999.925906	11.002445	-0.072641	4.818375
362.855494	7999.906966	11.007450	-0.072553	4.818371
363.270329	7999.929310	11.012455	-0.072630	4.818376
363.318157	7999.920496	11.017459	-0.072639	4.818373
363.374399	7999.872934	11.022464	-0.072650	4.818359
363.330073	7999.920653	11.027469	-0.072641	4.818373
363.231687	7999.911985	11.032474	-0.072623	4.818371
363.282720	7999.930520	11.037479	-0.072632	4.818376
363.047865	7999.952588	11.042483	-0.072589	4.818384
363.119018	7999.933582	11.047488	-0.072602	4.818378
363.293409	7999.947464	11.052493	-0.072634	4.818381
363.456411	7999.877172	11.057498	-0.072665	4.818360
363.289231	7999.920099	11.062503	-0.072634	4.818373
363.368019	7999.898044	11.067507	-0.072648	4.818366
363.389505	7999.847917	11.072512	-0.072652	4.818351
363.535570	7999.878225	11.077517	-0.072679	4.818360
363.622129	7999.874128	11.082522	-0.072696	4.818358
363.542577	7999.843657	11.087527	-0.072681	4.818349
363.427666	7999.841070	11.092531	-0.072659	4.818349
363.503832	7999.842086	11.097536	-0.072673	4.818349
363.594021	7999.901055	11.102541	-0.072690	4.818366
363.355445	7999.863208	11.107546	-0.072646	4.818356
363.366716	7999.842352	11.112551	-0.072648	4.818350
363.521923	7999.850725	11.117555	-0.072677	4.818352
363.365872	7999.872796	11.122560	-0.072648	4.818359
363.548109	7999.913039	11.127565	-0.072682	4.818370
363.582543	7999.913498	11.132570	-0.072688	4.818370
363.605859	7999.924311	11.137575	-0.072692	4.818373
363.567014	7999.895433	11.142579	-0.072685	4.818365
363.462582	7999.847825	11.147584	-0.072666	4.818351
363.573432	7999.901818	11.152589	-0.072686	4.818367
363.535149	7999.869798	11.157594	-0.072679	4.818357
363.328465	7999.874387	11.162599	-0.072641	4.818359
363.386500	7999.890915	11.167603	-0.072651	4.818364
363.042615	7999.888420	11.172608	-0.072587	4.818365
363.051680	7999.906395	11.177613	-0.072589	4.818370
363.321442	7999.895294	11.182618	-0.072639	4.818366
363.371244	7999.868651	11.187623	-0.072648	4.818358
363.414393	7999.909136	11.192627	-0.072656	4.818369
363.362124	7999.875878	11.197632	-0.072647	4.818360
363.519881	7999.911594	11.202637	-0.072676	4.818370
363.467081	7999.887781	11.207642	-0.072666	4.818363
363.289860	7999.917970	11.212647	-0.072633	4.818373
363.368077	7999.924266	11.217651	-0.072648	4.818374
363.431363	7999.877848	11.222656	-0.072660	4.818360
363.160525	7999.918339	11.227661	-0.072609	4.818373
363.218655	7999.900210	11.232666	-0.072620	4.818368
363.182680	7999.919683	11.237671	-0.072613	4.818374
363.195390	7999.944008	11.242675	-0.072616	4.818381
363.112115	7999.907185	11.247680	-0.072600	4.818370
363.162470	7999.917309	11.252685	-0.072609	4.818373
363.266228	7999.849377	11.257690	-0.072629	4.818352
363.542501	7999.886675	11.262695	-0.072680	4.818362
363.457397	7999.923347	11.267699	-0.072664	4.818374
363.488027	7999.902749	11.272704	-0.072670	4.818367
363.674143	7999.905235	11.277709	-0.072705	4.818367
363.035319	7999.901950	11.282714	-0.072586	4.818369
363.465885	7999.936058	11.287719	-0.072666	4.818377
363.475345	7999.923580	11.292723	-0.072668	4.818374
363.321738	7999.883717	11.297728	-0.072639	4.818362
363.464871	7999.883528	11.302733	-0.072665	4.818362
363.415876	7999.895475	11.307738	-0.072656	4.818365
363.010807	7999.933123	11.312743	-0.072581	4.818378
363.286343	7999.904245	11.317747	-0.072632	4.818369
363.468788	7999.862570	11.322752	-0.072666	4.818355
363.550734	7999.896222	11.327757	-0.072681	4.818365
363.278784	7999.865280	11.332762	-0.072631	4.818357
363.420744	7999.900784	11.337767	-0.072657	4.818367
363.626341	7999.883575	11.342771	-0.072695	4.818361
363.417710	7999.860831	11.347776	-0.072657	4.818355
363.575203	7999.867135	11.352781	-0.072686	4.818356
363.761522	7999.886428	11.357786	-0.072721	4.818361
363.542530	7999.897154	11.362791	-0.072680	4.818365
363.428477	7999.918735	11.367795	-0.072659	4.818372
363.617872	7999.889756	11.372800	-0.072694	4.818363
363.800650	7999.902700	11.377805	-0.072728	4.818366
363.631766	7999.871034	11.382810	-0.072696	4.818357
363.520663	7999.910510	11.387815	-0.072676	4.818369
363.711142	7999.908852	11.392819	-0.072711	4.818368
363.426577	7999.903999	11.397824	-0.072658	4.818368
363.438985	7999.925169	11.402829	-0.072660	4.818374
363.562630	7999.901613	11.407834	-0.072683	4.818367
363.493219	7999.900684	11.412839	-0.072670	4.818367
363.579538	7999.897635	11.417843	-0.072686	4.818365
363.556624	7999.913082	11.422848	-0.072682	4.818370
363.703776	7999.902444	11.427853	-0.072710	4.818366
363.567004	7999.842850	11.432858	-0.072684	4.818349
363.518660	7999.908370	11.437863	-0.072675	4.818369
363.746161	7999.890403	11.442867	-0.072717	4.818363
363.526314	7999.868560	11.447872	-0.072676	4.818357
363.624959	7999.899284	11.452877	-0.072695	4.818366
363.580858	7999.845130	11.457882	-0.072687	4.818350
363.568146	7999.864914	11.462887	-0.072684	4.818356
363.514165	7999.916705	11.467891	-0.072674	4.818371
363.529509	7999.862295	11.472896	-0.072677	4.818355
363.589638	7999.909309	11.477901	-0.072688	4.818369
363.593007	7999.870493	11.482906	-0.072689	4.818357
363.879323	7999.882720	11.487911	-0.072742	4.818360
363.672570	7999.914615	11.492915	-0.072704	4.818370
363.543629	7999.863528	11.497920	-0.072679	4.818355
363.767501	7999.909579	11.502925	-0.072721	4.818368
363.438443	7999.907282	11.507930	-0.072660	4.818369
363.399990	7999.930923	11.512935	-0.072653	4.818376
363.478828	7999.924623	11.517939	-0.072667	4.818374
363.455337	7999.932710	11.522944	-0.072663	4.818376
363.685902	7999.937891	11.527949	-0.072706	4.818377
363.559524	7999.895240	11.532954	-0.072682	4.818365
363.773963	7999.904406	11.537959	-0.072722	4.818367
364.019626	7999.877229	11.542963	-0.072768	4.818358
363.762816	7999.876947	11.547968	-0.072720	4.818359
363.721090	7999.922601	11.552973	-0.072712	4.818372
363.561505	7999.914165	11.557978	-0.072683	4.818370
363.589404	7999.910336	11.562983	-0.072688	4.818369
363.284239	7999.930413	11.567987	-0.072631	4.818376
363.357837	7999.916692	11.572992	-0.072645	4.818372
363.234930	7999.952858	11.577997	-0.072622	4.818383
363.417810	7999.921692	11.583002	-0.072656	4.818373
363.380251	7999.929591	11.588007	-0.072649	4.818376
363.729251	7999.906946	11.593011	-0.072714	4.818368
363.718584	7999.896299	11.598016	-0.072712	4.818364
363.746116	7999.937627	11.603021	-0.072717	4.818377
363.785983	7999.920304	11.608026	-0.072724	4.818371
363.904156	7999.895625	11.613031	-0.072746	4.818364
363.797692	7999.904704	11.618035	-0.072726	4.818367
363.625917	7999.898206	11.623040	-0.072694	4.818365
363.769133	7999.911672	11.628045	-0.072721	4.818369
363.604530	7999.922074	11.633050	-0.072690	4.818373
363.643743	7999.912094	11.638055	-0.072698	4.818369
363.707638	7999.923450	11.643059	-0.072710	4.818373
363.656548	7999.897559	11.648064	-0.072700	4.818365
363.812565	7999.936403	11.653069	-0.072729	4.818376
363.523896	7999.929393	11.658074	-0.072675	4.818375
363.753704	7999.926161	11.663079	-0.072718	4.818373
363.659753	7999.922804	11.668083	-0.072701	4.818373
363.554812	7999.878339	11.673088	-0.072681	4.818360
363.663135	7999.906042	11.678093	-0.072701	4.818368
363.798882	7999.875296	11.683098	-0.072726	4.818358
363.552989	7999.877261	11.688103	-0.072681	4.818359
363.836611	7999.903105	11.693107	-0.072733	4.818366
363.574378	7999.902751	11.698112	-0.072685	4.818367
363.934029	7999.928561	11.703117	-0.072752	4.818373
363.954830	7999.886827	11.708122	-0.072755	4.818361
363.794709	7999.874183	11.713127	-0.072726	4.818358
363.873778	7999.914099	11.718131	-0.072740	4.818369
363.619536	7999.868689	11.723136	-0.072693	4.818357
363.828774	7999.904042	11.728141	-0.072732	4.818366
363.822617	7999.892406	11.733146	-0.072731	4.818363
363.635154	7999.884648	11.738151	-0.072696	4.818361
363.653406	7999.890142	11.743155	-0.072699	4.818363
363.792100	7999.878341	11.748160	-0.072725	4.818359
363.918490	7999.893682	11.753165	-0.072748	4.818363
363.871645	7999.875200	11.758170	-0.072740	4.818358
364.033395	7999.847953	11.763175	-0.072770	4.818349
364.109445	7999.911985	11.768179	-0.072784	4.818368
363.975786	7999.876588	11.773184	-0.072759	4.818358
364.002819	7999.910558	11.778189	-0.072764	4.818368
364.095769	7999.884491	11.783194	-0.072781	4.818359
363.854873	7999.918030	11.788199	-0.072737	4.818370
363.925485	7999.911621	11.793203	-0.072750	4.818368
363.798661	7999.914126	11.798208	-0.072726	4.818369
363.703450	7999.911802	11.803213	-0.072708	4.818369
363.722203	7999.908901	11.808218	-0.072712	4.818368
363.948149	7999.848902	11.813223	-0.072754	4.818349
363.922724	7999.870617	11.818227	-0.072749	4.818356
363.905213	7999.816818	11.823232	-0.072746	4.818340
364.085428	7999.895895	11.828237	-0.072779	4.818363
364.250932	7999.866597	11.833242	-0.072810	4.818354
364.060352	7999.873502	11.838247	-0.072775	4.818356
363.919077	7999.917825	11.843251	-0.072748	4.818370
363.832860	7999.875711	11.848256	-0.072732	4.818358
363.618754	7999.927463	11.853261	-0.072692	4.818374
363.851186	7999.870702	11.858266	-0.072736	4.818356
363.853016	7999.874926	11.863271	-0.072736	4.818358
364.106395	7999.881462	11.868275	-0.072783	4.818359
363.912052	7999.848405	11.873280	-0.072747	4.818349
363.985326	7999.927104	11.878285	-0.072761	4.818373
364.115766	7999.893137	11.883290	-0.072785	4.818362
363.932989	7999.886492	11.888295	-0.072751	4.818361
363.836134	7999.874693	11.893299	-0.072733	4.818358
364.068649	7999.891453	11.898304	-0.072776	4.818362
364.111460	7999.863666	11.903309	-0.072784	4.818353
363.796250	7999.879408	11.908314	-0.072725	4.818359
364.157211	7999.912589	11.913319	-0.072792	4.818368
364.310448	7999.907284	11.918323	-0.072821	4.818365
364.161960	7999.864336	11.923328	-0.072793	4.818353
364.217217	7999.918639	11.928333	-0.072804	4.818369
364.036141	7999.897312	11.933338	-0.072770	4.818364
363.849004	7999.886408	11.938343	-0.072735	4.818361
363.750111	7999.902940	11.943347	-0.072716	4.818366
364.009349	7999.904302	11.948352	-0.072765	4.818366
363.970846	7999.942647	11.953357	-0.072758	4.818377
363.943939	7999.901325	11.958362	-0.072753	4.818365
363.993638	7999.904089	11.963367	-0.072762	4.818366
364.233591	7999.891540	11.968371	-0.072806	4.818361
364.037026	7999.879459	11.973376	-0.072770	4.818358
363.925829	7999.915782	11.978381	-0.072749	4.818369
363.861126	7999.917017	11.983386	-0.072737	4.818370
363.840767	7999.906241	11.988391	-0.072733	4.818367
363.988910	7999.896666	11.993395	-0.072761	4.818364
363.748777	7999.907110	11.998400	-0.072716	4.818368
363.784458	7999.918088	12.003405	-0.072723	4.818371
363.711871	7999.881408	12.008410	-0.072709	4.818360
363.852608	7999.914795	12.013415	-0.072735	4.818369
364.113616	7999.897277	12.018419	-0.072784	4.818363
363.712224	7999.842548	12.023424	-0.072709	4.818349
363.878949	7999.890987	12.028429	-0.072740	4.818362
363.942074	7999.852969	12.033434	-0.072752	4.818351
363.792820	7999.886683	12.038439	-0.072724	4.818361
363.810526	7999.898472	12.043443	-0.072727	4.818365
363.935108	7999.891733	12.048448	-0.072751	4.818362
364.031378	7999.957086	12.053453	-0.072769	4.818381
363.581150	7999.925861	12.058458	-0.072685	4.818374
363.877336	7999.902510	12.063463	-0.072740	4.818366
363.889033	7999.939426	12.068467	-0.072742	4.818377
363.626537	7999.924363	12.073472	-0.072693	4.818373
363.956899	7999.889916	12.078477	-0.072755	4.818362
363.774586	7999.892730	12.083482	-0.072721	4.818363
364.124852	7999.882706	12.088487	-0.072786	4.818359
364.151308	7999.901964	12.093491	-0.072791	4.818364
364.215205	7999.882861	12.098496	-0.072803	4.818359
364.058346	7999.911222	12.103501	-0.072773	4.818368
364.056395	7999.888088	12.108506	-0.072773	4.818361
364.284208	7999.885880	12.113511	-0.072815	4.818359
364.074095	7999.919831	12.118515	-0.072776	4.818370
363.834959	7999.907181	12.123520	-0.072732	4.818367
363.854267	7999.917941	12.128525	-0.072735	4.818370
363.843951	7999.889444	12.133530	-0.072733	4.818362
363.685936	7999.926192	12.138535	-0.072704	4.818374
363.769244	7999.952511	12.143539	-0.072719	4.818381
363.653387	7999.905799	12.148544	-0.072698	4.818368
363.658288	7999.953126	12.153549	-0.072699	4.818382
363.826415	7999.922813	12.158554	-0.072730	4.818372
363.724629	7999.927753	12.163559	-0.072711	4.818374
364.219386	7999.922811	12.168563	-0.072803	4.818370
364.213262	7999.894370	12.173568	-0.072802	4.818362
364.231014	7999.922964	12.178573	-0.072805	4.818370
364.257408	7999.907561	12.183578	-0.072810	4.818366
364.174869	7999.907507	12.188583	-0.072795	4.818366
364.113874	7999.904590	12.193587	-0.072783	4.818365
364.190747	7999.890913	12.198592	-0.072798	4.818361
364.354081	7999.935106	12.203597	-0.072828	4.818374
364.101819	7999.900224	12.208602	-0.072781	4.818364
364.151461	7999.881982	12.213607	-0.072790	4.818359
364.278043	7999.895225	12.218611	-0.072814	4.818362
364.114592	7999.838425	12.223616	-0.072783	4.818346
364.116923	7999.901472	12.228621	-0.072784	4.818364
363.856094	7999.911638	12.233626	-0.072735	4.818369
364.215184	7999.895431	12.238631	-0.072802	4.818362
364.335895	7999.864484	12.243635	-0.072825	4.818353
364.242902	7999.864290	12.248640	-0.072807	4.818353
364.199297	7999.893114	12.253645	-0.072799	4.818362
364.329636	7999.910610	12.258650	-0.072823	4.818366
364.054281	7999.886972	12.263655	-0.072772	4.818360
364.150286	7999.900858	12.268659	-0.072790	4.818364
364.176634	7999.861298	12.273664	-0.072795	4.818352
364.159861	7999.926190	12.278669	-0.072792	4.818372
364.222455	7999.897618	12.283674	-0.072803	4.818363
364.359435	7999.888944	12.288679	-0.072829	4.818360
364.343743	7999.891884	12.293683	-0.072826	4.818361
364.252159	7999.855999	12.298688	-0.072809	4.818350
364.372563	7999.882815	12.303693	-0.072831	4.818358
364.239668	7999.875786	12.308698	-0.072806	4.818356
364.042548	7999.902558	12.313703	-0.072770	4.818365
364.260451	7999.902318	12.318707	-0.072810	4.818364
364.245581	7999.872710	12.323712	-0.072807	4.818355
364.315306	7999.872591	12.328717	-0.072820	4.818355
364.384238	7999.874561	12.333722	-0.072833	4.818355
364.351257	7999.891974	12.338727	-0.072827	4.818361
364.359567	7999.923593	12.343731	-0.072829	4.818370
364.351221	7999.856261	12.348736	-0.072827	4.818350
364.380516	7999.902865	12.353741	-0.072832	4.818364
364.553592	7999.903076	12.358746	-0.072865	4.818363
364.393336	7999.824261	12.363751	-0.072835	4.818340
364.498575	7999.857176	12.368755	-0.072854	4.818350
364.498378	7999.879228	12.373760	-0.072854	4.818356
364.291215	7999.878558	12.378765	-0.072816	4.818357
364.160060	7999.913564	12.383770	-0.072791	4.818368
364.243521	7999.881069	12.388775	-0.072807	4.818358
364.422804	7999.904471	12.393779	-0.072840	4.818364
364.178398	7999.863392	12.398784	-0.072795	4.818353
364.195245	7999.903527	12.403789	-0.072798	4.818365
364.468047	7999.907172	12.408794	-0.072849	4.818365
364.148121	7999.855632	12.413799	-0.072789	4.818351
364.155418	7999.907192	12.418803	-0.072790	4.818366
364.018993	7999.883312	12.423808	-0.072765	4.818359
364.267665	7999.909740	12.428813	-0.072811	4.818366
364.094876	7999.908480	12.433818	-0.072779	4.818367
364.220060	7999.901750	12.438823	-0.072802	4.818364
364.297177	7999.908031	12.443827	-0.072817	4.818366
364.285068	7999.875309	12.448832	-0.072814	4.818356
364.335083	7999.892781	12.453837	-0.072824	4.818361
364.474059	7999.897788	12.458842	-0.072850	4.818362
364.370710	7999.937367	12.463847	-0.072830	4.818374
364.383646	7999.904979	12.468851	-0.072833	4.818364
364.397454	7999.885207	12.473856	-0.072835	4.818359
364.520278	7999.901552	12.478861	-0.072858	4.818363
364.266546	7999.867701	12.483866	-0.072811	4.818354
364.352566	7999.875151	12.488871	-0.072827	4.818356
364.530210	7999.902731	12.493875	-0.072860	4.818363
364.241409	7999.895719	12.498880	-0.072806	4.818362
364.189634	7999.916031	12.503885	-0.072796	4.818369
363.983250	7999.924825	12.508890	-0.072758	4.818372
364.121764	7999.911971	12.513895	-0.072784	4.818368
364.180413	7999.925357	12.518899	-0.072795	4.818371
364.077747	7999.881972	12.523904	-0.072776	4.818359
364.120238	7999.930852	12.528909	-0.072783	4.818373
364.223959	7999.925936	12.533914	-0.072803	4.818371
364.281793	7999.895199	12.538919	-0.072813	4.818362
364.331764	7999.925274	12.543923	-0.072823	4.818371
363.914028	7999.914438	12.548928	-0.072745	4.818369
364.028697	7999.932774	12.553933	-0.072766	4.818374
364.330395	7999.884290	12.558938	-0.072822	4.818359
364.083553	7999.925102	12.563943	-0.072777	4.818372
364.217526	7999.930043	12.568947	-0.072801	4.818373
364.058756	7999.920567	12.573952	-0.072772	4.818370
364.027515	7999.942204	12.578957	-0.072766	4.818377
364.207302	7999.896293	12.583962	-0.072799	4.818363
364.165625	7999.928294	12.588967	-0.072792	4.818372
364.523413	7999.924673	12.593971	-0.072858	4.818370
364.351425	7999.919222	12.598976	-0.072826	4.818369
364.071331	7999.939633	12.603981	-0.072774	4.818376
364.304667	7999.923846	12.608986	-0.072818	4.818370
364.321834	7999.879962	12.613991	-0.072821	4.818357
364.360814	7999.914091	12.618995	-0.072828	4.818367
363.958438	7999.916064	12.624000	-0.072753	4.818369
364.270541	7999.888725	12.629005	-0.072811	4.818360
364.284980	7999.905722	12.634010	-0.072814	4.818365
364.243893	7999.933529	12.639015	-0.072806	4.818374
364.258677	7999.956832	12.644019	-0.072809	4.818380
364.390901	7999.885078	12.649024	-0.072833	4.818359
364.250284	7999.906303	12.654029	-0.072807	4.818365
364.295732	7999.911111	12.659034	-0.072816	4.818367
364.520420	7999.896258	12.664039	-0.072858	4.818361
364.778186	7999.876596	12.669043	-0.072905	4.818354
364.238434	7999.898788	12.674048	-0.072805	4.818363
364.501222	7999.926456	12.679053	-0.072854	4.818370
364.344832	7999.903359	12.684058	-0.072825	4.818364
364.213494	7999.893200	12.689063	-0.072800	4.818362
364.483784	7999.895761	12.694067	-0.072851	4.818361
364.289927	7999.865861	12.699072	-0.072814	4.818353
364.372290	7999.907922	12.704077	-0.072830	4.818365
364.501199	7999.922248	12.709082	-0.072854	4.818369
364.260947	7999.891727	12.714087	-0.072809	4.818361
364.290054	7999.917322	12.719091	-0.072814	4.818369
364.358798	7999.912988	12.724096	-0.072827	4.818367
364.164529	7999.986012	12.729101	-0.072791	4.818389
364.418727	7999.930592	12.734106	-0.072838	4.818372
364.378919	7999.944763	12.739111	-0.072831	4.818376
364.613648	7999.935296	12.744115	-0.072875	4.818373
364.360025	7999.907747	12.749120	-0.072827	4.818365
364.261307	7999.911678	12.754125	-0.072809	4.818367
364.423486	7999.926448	12.759130	-0.072839	4.818371
364.560352	7999.883114	12.764135	-0.072865	4.818357
364.445746	7999.920442	12.769139	-0.072843	4.818369
364.394982	7999.898756	12.774144	-0.072834	4.818363
364.546106	7999.906026	12.779149	-0.072862	4.818364
364.308232	7999.907047	12.784154	-0.072818	4.818365
364.165199	7999.892530	12.789159	-0.072791	4.818362
364.151854	7999.965871	12.794163	-0.072788	4.818384
364.011625	7999.913582	12.799168	-0.072762	4.818369
363.904083	7999.923696	12.804173	-0.072742	4.818372
363.919304	7999.934401	12.809178	-0.072745	4.818375
364.391625	7999.917607	12.814183	-0.072833	4.818368
364.167782	7999.921966	12.819187	-0.072791	4.818370
364.432170	7999.911845	12.824192	-0.072841	4.818366
364.193363	7999.947512	12.829197	-0.072796	4.818378
363.895405	7999.944579	12.834202	-0.072741	4.818378
363.970953	7999.942436	12.839207	-0.072755	4.818377
364.409578	7999.934644	12.844211	-0.072836	4.818373
364.343759	7999.918009	12.849216	-0.072824	4.818369
364.422399	7999.923260	12.854221	-0.072839	4.818370
364.296559	7999.921577	12.859226	-0.072815	4.818370
364.494874	7999.918975	12.864231	-0.072852	4.818368
364.453283	7999.948877	12.869235	-0.072844	4.818377
364.421257	7999.917989	12.874240	-0.072838	4.818368
364.467409	7999.938560	12.879245	-0.072847	4.818374
364.236345	7999.962778	12.884250	-0.072804	4.818382
364.029556	7999.952660	12.889255	-0.072765	4.818380
364.321348	7999.979666	12.894259	-0.072820	4.818387
364.339364	7999.917938	12.899264	-0.072823	4.818369
364.240988	7999.943930	12.904269	-0.072805	4.818377
364.614983	7999.913218	12.909274	-0.072874	4.818366
364.426214	7999.911743	12.914279	-0.072839	4.818366
364.735024	7999.956833	12.919283	-0.072897	4.818379
364.598773	7999.898293	12.924288	-0.072871	4.818362
364.717043	7999.920879	12.929293	-0.072893	4.818368
364.638313	7999.925077	12.934298	-0.072879	4.818369
364.491913	7999.922068	12.939303	-0.072851	4.818369
364.604762	7999.928827	12.944307	-0.072872	4.818371
364.493639	7999.944145	12.949312	-0.072852	4.818376
364.574921	7999.950482	12.954317	-0.072867	4.818377
364.291281	7999.936186	12.959322	-0.072814	4.818374
364.385684	7999.943749	12.964327	-0.072831	4.818376
364.346316	7999.922215	12.969331	-0.072824	4.818370
364.428742	7999.908612	12.974336	-0.072839	4.818365
364.736976	7999.893826	12.979341	-0.072897	4.818360
364.718870	7999.897784	12.984346	-0.072893	4.818361
364.544354	7999.851337	12.989351	-0.072861	4.818348
364.426000	7999.926426	12.994355	-0.072839	4.818371
364.717023	7999.918762	12.999360	-0.072893	4.818367
364.856151	7999.917470	13.004365	-0.072919	4.818366
364.698883	7999.920617	13.009370	-0.072890	4.818368
364.749845	7999.884537	13.014375	-0.072899	4.818357
364.847181	7999.929950	13.019379	-0.072917	4.818370
364.727925	7999.881091	13.024384	-0.072895	4.818356
364.800421	7999.897813	13.029389	-0.072908	4.818361
365.008679	7999.883792	13.034394	-0.072947	4.818356
364.834658	7999.912973	13.039399	-0.072915	4.818365
364.936614	7999.933240	13.044403	-0.072934	4.818371
364.911659	7999.873038	13.049408	-0.072929	4.818353
364.927515	7999.926815	13.054413	-0.072932	4.818369
364.763175	7999.892056	13.059418	-0.072901	4.818359
364.902807	7999.859262	13.064423	-0.072927	4.818349
364.867546	7999.914456	13.069427	-0.072921	4.818365
364.757217	7999.897225	13.074432	-0.072900	4.818361
364.683870	7999.913048	13.079437	-0.072887	4.818366
364.862246	7999.911230	13.084442	-0.072920	4.818364
364.935453	7999.881749	13.089447	-0.072933	4.818355
364.958531	7999.908314	13.094451	-0.072938	4.818363
364.883717	7999.871602	13.099456	-0.072924	4.818353
364.788964	7999.910246	13.104461	-0.072906	4.818364
364.687919	7999.913095	13.109466	-0.072887	4.818366
364.746768	7999.899176	13.114471	-0.072898	4.818361
364.914866	7999.944485	13.119475	-0.072929	4.818374
364.738016	7999.875950	13.124480	-0.072896	4.818354
364.835842	7999.908766	13.129485	-0.072915	4.818364
364.946995	7999.898697	13.134490	-0.072935	4.818360
364.743698	7999.901230	13.139495	-0.072897	4.818362
364.857170	7999.910098	13.144499	-0.072919	4.818364
364.827850	7999.891849	13.149504	-0.072913	4.818359
364.701720	7999.913268	13.154509	-0.072890	4.818366
364.691890	7999.933092	13.159514	-0.072888	4.818372
364.547957	7999.898607	13.164519	-0.072861	4.818362
364.817427	7999.895906	13.169523	-0.072911	4.818360
364.741698	7999.888591	13.174528	-0.072897	4.818358
364.596110	7999.885593	13.179533	-0.072870	4.818358
364.756367	7999.918193	13.184538	-0.072900	4.818367
364.525959	7999.852094	13.189543	-0.072857	4.818348
364.720191	7999.900902	13.194547	-0.072893	4.818362
364.929565	7999.837531	13.199552	-0.072932	4.818342
364.785271	7999.838752	13.204557	-0.072905	4.818343
364.610699	7999.860574	13.209562	-0.072872	4.818350
364.550790	7999.869224	13.214567	-0.072861	4.818353
364.604977	7999.929815	13.219571	-0.072871	4.818371
364.538285	7999.893212	13.224576	-0.072859	4.818360
364.723976	7999.882039	13.229581	-0.072894	4.818356
364.484783	7999.908248	13.234586	-0.072849	4.818365
364.579975	7999.885363	13.239591	-0.072867	4.818358
364.594933	7999.941228	13.244595	-0.072869	4.818374
364.728468	7999.906251	13.249600	-0.072894	4.818364
364.697078	7999.925786	13.254605	-0.072888	4.818369
364.501820	7999.929476	13.259610	-0.072852	4.818371
364.484300	7999.908235	13.264615	-0.072849	4.818365
364.883270	7999.912517	13.269619	-0.072923	4.818365
364.772773	7999.883731	13.274624	-0.072902	4.818357
364.796067	7999.908198	13.279629	-0.072907	4.818364
365.040059	7999.909359	13.284634	-0.072952	4.818363
364.613317	7999.912054	13.289639	-0.072873	4.818366
364.699966	7999.926865	13.294643	-0.072889	4.818370
364.847892	7999.897333	13.299648	-0.072916	4.818360
364.725622	7999.900948	13.304653	-0.072894	4.818362
364.795679	7999.880878	13.309658	-0.072907	4.818356
364.704750	7999.837649	13.314663	-0.072890	4.818343
365.015643	7999.901672	13.319667	-0.072948	4.818361
364.590836	7999.874985	13.324672	-0.072868	4.818355
364.588152	7999.926412	13.329677	-0.072868	4.818370
364.701321	7999.946830	13.334682	-0.072889	4.818376
364.758353	7999.905579	13.339687	-0.072900	4.818363
364.755555	7999.929697	13.344691	-0.072899	4.818370
364.641134	7999.876701	13.349696	-0.072878	4.818355
364.972897	7999.868532	13.354701	-0.072939	4.818351
364.795851	7999.886120	13.359706	-0.072906	4.818357
364.706883	7999.903834	13.364711	-0.072890	4.818363
365.029572	7999.928104	13.369715	-0.072950	4.818369
364.893030	7999.877962	13.374720	-0.072924	4.818354
364.404358	7999.954402	13.379725	-0.072834	4.818379
364.506146	7999.910599	13.384730	-0.072852	4.818366
364.494662	7999.946154	13.389735	-0.072850	4.818376
364.692189	7999.959297	13.394739	-0.072887	4.818379
364.710915	7999.934339	13.399744	-0.072891	4.818372
364.620908	7999.926832	13.404749	-0.072874	4.818370
364.634481	7999.966924	13.409754	-0.072876	4.818382
364.432528	7999.914859	13.414759	-0.072839	4.818367
364.731835	7999.943016	13.419763	-0.072894	4.818374
364.859619	7999.919516	13.424768	-0.072918	4.818367
364.966001	7999.917786	13.429773	-0.072938	4.818366
364.872434	7999.932289	13.434778	-0.072920	4.818371
364.815929	7999.911576	13.439783	-0.072910	4.818365
364.922677	7999.947662	13.444787	-0.072930	4.818375
364.738527	7999.898986	13.449792	-0.072895	4.818361
364.791271	7999.877633	13.454797	-0.072905	4.818355
364.901651	7999.886460	13.459802	-0.072926	4.818357
364.660975	7999.887442	13.464807	-0.072881	4.818358
365.108310	7999.913378	13.469811	-0.072964	4.818364
365.162654	7999.914103	13.474816	-0.072974	4.818364
364.944215	7999.916433	13.479821	-0.072934	4.818366
365.008361	7999.923591	13.484826	-0.072946	4.818368
364.727583	7999.899880	13.489831	-0.072893	4.818362
364.899868	7999.924239	13.494835	-0.072925	4.818368
364.824987	7999.891727	13.499840	-0.072911	4.818359
364.933154	7999.888971	13.504845	-0.072932	4.818358
364.772893	7999.908883	13.509850	-0.072902	4.818364
364.561527	7999.903956	13.514855	-0.072862	4.818364
364.902164	7999.905358	13.519859	-0.072926	4.818363
364.770391	7999.884689	13.524864	-0.072901	4.818357
364.757856	7999.913929	13.529869	-0.072899	4.818366
364.910671	7999.924374	13.534874	-0.072927	4.818368
364.830088	7999.911741	13.539879	-0.072912	4.818365
364.698362	7999.915231	13.544883	-0.072888	4.818366
364.621003	7999.879535	13.549888	-0.072873	4.818356
365.045400	7999.887309	13.554893	-0.072952	4.818357
365.109010	7999.890259	13.559898	-0.072964	4.818357
364.575506	7999.886276	13.564903	-0.072865	4.818358
364.846110	7999.934005	13.569907	-0.072915	4.818371
364.947907	7999.917510	13.574912	-0.072934	4.818366
364.997523	7999.951782	13.579917	-0.072943	4.818376
365.067463	7999.912804	13.584922	-0.072956	4.818364
364.909648	7999.922246	13.589927	-0.072927	4.818368
364.740983	7999.963052	13.594931	-0.072896	4.818380
364.443772	7999.948574	13.599936	-0.072840	4.818377
364.479472	7999.961654	13.604941	-0.072847	4.818381
364.751515	7999.934831	13.609946	-0.072897	4.818372
364.880348	7999.918697	13.614951	-0.072921	4.818367
364.815918	7999.924136	13.619955	-0.072909	4.818369
364.828412	7999.883340	13.624960	-0.072912	4.818356
364.843154	7999.903492	13.629965	-0.072914	4.818362
364.960020	7999.908204	13.634970	-0.072936	4.818363
364.910972	7999.920151	13.639975	-0.072927	4.818367
365.099187	7999.928969	13.644979	-0.072962	4.818369
365.073056	7999.905511	13.649984	-0.072957	4.818362
364.802235	7999.926046	13.654989	-0.072907	4.818369
365.070777	7999.919132	13.659994	-0.072957	4.818366
364.836092	7999.907591	13.664999	-0.072913	4.818364
364.951360	7999.926986	13.670003	-0.072934	4.818369
365.012445	7999.887890	13.675008	-0.072946	4.818357
364.975059	7999.906294	13.680013	-0.072939	4.818363
364.902478	7999.897970	13.685018	-0.072925	4.818360
365.109418	7999.871327	13.690023	-0.072964	4.818352
365.150725	7999.906539	13.695027	-0.072971	4.818362
365.015529	7999.898428	13.700032	-0.072946	4.818360
365.014620	7999.906817	13.705037	-0.072946	4.818363
365.184018	7999.902779	13.710042	-0.072978	4.818361
365.001081	7999.874074	13.715047	-0.072943	4.818353
365.099356	7999.905846	13.720051	-0.072962	4.818362
365.013848	7999.893148	13.725056	-0.072946	4.818359
365.145782	7999.919068	13.730061	-0.072970	4.818366
365.138918	7999.914774	13.735066	-0.072969	4.818364
365.115107	7999.901851	13.740071	-0.072965	4.818361
365.170212	7999.924643	13.745075	-0.072975	4.818367
365.091487	7999.882627	13.750080	-0.072960	4.818355
365.049568	7999.886266	13.755085	-0.072952	4.818356
365.227979	7999.904405	13.760090	-0.072986	4.818361
364.946692	7999.876486	13.765095	-0.072933	4.818354
365.007483	7999.928763	13.770099	-0.072945	4.818369
364.759938	7999.901294	13.775104	-0.072898	4.818362
364.799386	7999.883965	13.780109	-0.072906	4.818357
365.045637	7999.920867	13.785114	-0.072952	4.818367
365.014318	7999.897340	13.790119	-0.072946	4.818360
365.246344	7999.934051	13.795123	-0.072989	4.818370
365.404640	7999.898356	13.800128	-0.073018	4.818359
365.068661	7999.889660	13.805133	-0.072956	4.818357
365.236671	7999.900308	13.810138	-0.072987	4.818360
365.019003	7999.892145	13.815143	-0.072946	4.818358
365.128638	7999.904113	13.820147	-0.072967	4.818361
365.211758	7999.902072	13.825152	-0.072982	4.818360
365.110404	7999.888112	13.830157	-0.072963	4.818357
365.220744	7999.923196	13.835162	-0.072984	4.818367
364.955199	7999.911242	13.840167	-0.072935	4.818364
365.116816	7999.914452	13.845171	-0.072965	4.818364
365.061833	7999.863301	13.850176	-0.072954	4.818349
365.015486	7999.859529	13.855181	-0.072946	4.818349
365.085969	7999.897231	13.860186	-0.072959	4.818359
364.997190	7999.883439	13.865191	-0.072942	4.818356
365.006034	7999.829990	13.870195	-0.072944	4.818340
364.983771	7999.846496	13.875200	-0.072940	4.818345
365.148390	7999.912765	13.880205	-0.072970	4.818364
365.131286	7999.899931	13.885210	-0.072967	4.818360
365.178159	7999.819683	13.890215	-0.072976	4.818336
365.084364	7999.914006	13.895219	-0.072958	4.818364
365.063136	7999.904268	13.900224	-0.072954	4.818362
364.917591	7999.881315	13.905229	-0.072927	4.818355
365.020995	7999.884797	13.910234	-0.072947	4.818356
365.088367	7999.890948	13.915239	-0.072959	4.818358
365.139546	7999.919989	13.920243	-0.072969	4.818366
365.100661	7999.895311	13.925248	-0.072961	4.818359
364.982975	7999.884283	13.930253	-0.072939	4.818356
365.063552	7999.927372	13.935258	-0.072954	4.818369
364.801187	7999.904957	13.940263	-0.072906	4.818363
365.058222	7999.907343	13.945267	-0.072953	4.818363
365.113761	7999.866072	13.950272	-0.072964	4.818350
364.918580	7999.855058	13.955277	-0.072927	4.818348
365.167092	7999.897241	13.960282	-0.072974	4.818359
365.116684	7999.826195	13.965287	-0.072964	4.818338
365.107000	7999.901687	13.970291	-0.072962	4.818361
364.824574	7999.869551	13.975296	-0.072910	4.818352
365.170119	7999.838460	13.980301	-0.072974	4.818342
365.073808	7999.910692	13.985306	-0.072956	4.818364
364.947335	7999.887994	13.990311	-0.072933	4.818357
365.109829	7999.910121	13.995315	-0.072963	4.818363
365.070473	7999.907493	14.000320	-0.072955	4.818363
365.203610	7999.896669	14.005325	-0.072980	4.818359
365.161671	7999.876151	14.010330	-0.072972	4.818353
365.149729	7999.878090	14.015335	-0.072970	4.818354
365.179580	7999.900545	14.020339	-0.072976	4.818360
365.203344	7999.895610	14.025344	-0.072980	4.818359
365.165869	7999.879353	14.030349	-0.072973	4.818354
365.197979	7999.877680	14.035354	-0.072979	4.818353
365.145965	7999.846525	14.040359	-0.072969	4.818344
365.276019	7999.862967	14.045363	-0.072994	4.818349
365.194981	7999.875536	14.050368	-0.072978	4.818353
365.162786	7999.833092	14.055373	-0.072972	4.818340
365.313993	7999.913886	14.060378	-0.073001	4.818364
365.172621	7999.843724	14.065383	-0.072974	4.818343
365.150288	7999.872833	14.070387	-0.072970	4.818352
365.228785	7999.851825	14.075392	-0.072985	4.818345
365.279714	7999.885064	14.080397	-0.072994	4.818355
365.077302	7999.919118	14.085402	-0.072956	4.818366
364.855880	7999.913005	14.090407	-0.072915	4.818365
365.116765	7999.908089	14.095411	-0.072964	4.818363
365.203626	7999.892445	14.100416	-0.072980	4.818358
365.251710	7999.915143	14.105421	-0.072989	4.818364
365.280299	7999.923927	14.110426	-0.072994	4.818367
365.244642	7999.882486	14.115431	-0.072988	4.818354
365.381555	7999.930530	14.120435	-0.073013	4.818368
365.171385	7999.898309	14.125440	-0.072974	4.818359
365.200540	7999.865088	14.130445	-0.072979	4.818349
365.303186	7999.897969	14.135450	-0.072998	4.818359
364.904834	7999.850629	14.140455	-0.072924	4.818346
365.050410	7999.893536	14.145459	-0.072951	4.818359
365.124289	7999.896623	14.150464	-0.072965	4.818359
364.984987	7999.886357	14.155469	-0.072939	4.818357
365.262143	7999.911068	14.160474	-0.072991	4.818363
365.160312	7999.876095	14.165479	-0.072972	4.818353
365.326985	7999.872021	14.170483	-0.073003	4.818351
365.165829	7999.878267	14.175488	-0.072973	4.818354
365.056907	7999.855803	14.180493	-0.072952	4.818347
365.246877	7999.909808	14.185498	-0.072988	4.818363
365.216530	7999.855835	14.190503	-0.072982	4.818347
365.323487	7999.891924	14.195507	-0.073002	4.818357
365.362430	7999.884041	14.200512	-0.073009	4.818354
365.129809	7999.904036	14.205517	-0.072966	4.818361
365.215533	7999.898879	14.210522	-0.072982	4.818359
365.302225	7999.886383	14.215527	-0.072998	4.818355
365.293671	7999.908325	14.220531	-0.072996	4.818362
365.086394	7999.880344	14.225536	-0.072958	4.818354
365.219391	7999.902077	14.230541	-0.072982	4.818360
365.393771	7999.926465	14.235546	-0.073015	4.818367
365.246683	7999.887735	14.240551	-0.072987	4.818356
365.360767	7999.931273	14.245555	-0.073009	4.818369
365.243998	7999.920257	14.250560	-0.072987	4.818366
365.235027	7999.911733	14.255565	-0.072985	4.818363
365.345466	7999.903756	14.260570	-0.073006	4.818360
365.314629	7999.862380	14.265575	-0.073000	4.818348
365.384268	7999.924229	14.270579	-0.073013	4.818366
365.321731	7999.905536	14.275584	-0.073001	4.818361
365.238917	7999.893924	14.280589	-0.072986	4.818358
365.110298	7999.915310	14.285594	-0.072962	4.818365
364.960188	7999.894396	14.290599	-0.072934	4.818359
365.034937	7999.925853	14.295603	-0.072948	4.818368
364.999042	7999.900164	14.300608	-0.072941	4.818361
365.188649	7999.907950	14.305613	-0.072976	4.818362
365.265927	7999.905831	14.310618	-0.072991	4.818361
365.145385	7999.887413	14.315623	-0.072968	4.818356
365.457469	7999.917843	14.320627	-0.073026	4.818364
365.213564	7999.883071	14.325632	-0.072981	4.818355
365.066367	7999.897906	14.330637	-0.072954	4.818360
365.285823	7999.933400	14.335642	-0.072994	4.818369
365.146495	7999.937837	14.340647	-0.072969	4.818371
365.071865	7999.960995	14.345651	-0.072955	4.818379
365.227707	7999.952575	14.350656	-0.072984	4.818375
365.151906	7999.935805	14.355661	-0.072969	4.818371
365.065053	7999.948297	14.360666	-0.072953	4.818375
365.058060	7999.928246	14.365671	-0.072952	4.818369
365.295018	7999.948219	14.370675	-0.072996	4.818374
365.029644	7999.932065	14.375680	-0.072947	4.818370
365.004926	7999.946437	14.380685	-0.072942	4.818374
365.348886	7999.941583	14.385690	-0.073006	4.818372
365.170801	7999.926597	14.390695	-0.072973	4.818368
365.169742	7999.932883	14.395699	-0.072973	4.818370
365.264840	7999.914198	14.400704	-0.072990	4.818364
365.396925	7999.904409	14.405709	-0.073015	4.818360
365.154823	7999.908523	14.410714	-0.072970	4.818363
365.097173	7999.885694	14.415719	-0.072959	4.818356
365.270984	7999.907973	14.420723	-0.072991	4.818362
365.519039	7999.886082	14.425728	-0.073038	4.818354
365.317773	7999.862383	14.430733	-0.073000	4.818348
365.356256	7999.918563	14.435738	-0.073007	4.818365
365.213002	7999.435608	14.440743	-0.072980	4.818222

365.086251	7996.236122	14.445747	-0.072955	4.817271
365.150006	7990.733410	14.450752	-0.072963	4.815635
365.186254	7984.025479	14.455757	-0.072965	4.813639
365.176790	7976.844617	14.460762	-0.072959	4.811502
365.003845	7969.133388	14.465767	-0.072921	4.809207
365.036994	7961.424284	14.470771	-0.072923	4.806910
364.892494	7953.445435	14.475776	-0.072890	4.804533
364.641409	7945.566664	14.480781	-0.072839	4.802184
364.920789	7937.597702	14.485786	-0.072885	4.799806
364.961449	7929.614121	14.490791	-0.072888	4.797423
364.714877	7921.643746	14.495795	-0.072837	4.795044
364.643694	7913.615683	14.500800	-0.072818	4.792645
364.990719	7905.549324	14.505805	-0.072877	4.790233
364.863636	7897.609063	14.510810	-0.072849	4.787859
364.488848	7889.504294	14.515815	-0.072774	4.785435
364.544630	7881.593885	14.520819	-0.072779	4.783066
364.683383	7873.586114	14.525824	-0.072799	4.780668
364.799525	7865.548761	14.530829	-0.072816	4.778259
364.812942	7857.571662	14.535834	-0.072813	4.775867
364.846135	7849.558176	14.540839	-0.072814	4.773463
365.056555	7841.553533	14.545843	-0.072848	4.771060
364.825566	7833.532095	14.550848	-0.072800	4.768652
364.731230	7825.547224	14.555853	-0.072777	4.766253
364.916472	7817.498310	14.560858	-0.072806	4.763833
364.899257	7809.567891	14.565863	-0.072798	4.761448
364.822932	7801.526846	14.570867	-0.072778	4.759029
364.737308	7793.620489	14.575872	-0.072757	4.756649
364.598297	7785.473129	14.580877	-0.072726	4.754196
364.760724	7777.579989	14.585882	-0.072751	4.751817
364.444218	7769.515168	14.590887	-0.072687	4.749386
364.451136	7761.546047	14.595891	-0.072683	4.746982
364.546427	7753.448215	14.600896	-0.072695	4.744538
364.652294	7745.569602	14.605901	-0.072710	4.742159
364.504665	7737.541263	14.610906	-0.072677	4.739733
364.465229	7729.477566	14.615911	-0.072664	4.737296
364.532536	7721.493058	14.620915	-0.072672	4.734881
364.435211	7713.523925	14.625920	-0.072648	4.732470
364.473015	7705.503038	14.630925	-0.072650	4.730042
364.458211	7697.490068	14.635930	-0.072642	4.727615
364.145243	7689.477422	14.640935	-0.072579	4.725187
364.125459	7681.532446	14.645939	-0.072570	4.722778
364.277463	7673.541035	14.650944	-0.072593	4.720354
364.033780	7665.478583	14.655949	-0.072542	4.717907
364.089849	7657.523689	14.660954	-0.072548	4.715491
364.029116	7649.511680	14.665959	-0.072531	4.713057
364.024499	7641.552362	14.670963	-0.072525	4.710637
363.931886	7633.539279	14.675968	-0.072502	4.708200
363.764335	7625.499298	14.680973	-0.072466	4.705754
363.872125	7617.512884	14.685978	-0.072481	4.703322
363.973905	7609.506977	14.690983	-0.072495	4.700883
364.003009	7601.479323	14.695987	-0.072495	4.698436
363.681900	7593.539566	14.700992	-0.072430	4.696016
363.803676	7585.486842	14.705997	-0.072447	4.693559
363.655054	7577.570370	14.711002	-0.072414	4.691142
363.615957	7569.462152	14.716007	-0.072402	4.688666
363.803397	7561.511054	14.721011	-0.072431	4.686236
363.929936	7553.482190	14.726016	-0.072450	4.683781
363.868966	7545.552963	14.731021	-0.072433	4.681356
363.777132	7537.459543	14.736026	-0.072411	4.678879
363.803170	7529.536826	14.741031	-0.072410	4.676453
364.037606	7521.482081	14.746035	-0.072449	4.673985
363.706668	7513.483555	14.751040	-0.072382	4.671533
363.871402	7505.433067	14.756045	-0.072407	4.669064
363.755100	7497.489174	14.761050	-0.072381	4.666626
363.753922	7489.415413	14.766055	-0.072375	4.664147
363.622155	7481.496220	14.771059	-0.072345	4.661715
363.625644	7473.428979	14.776064	-0.072341	4.659235
363.473349	7465.461379	14.781069	-0.072307	4.656785
363.554375	7457.449402	14.786074	-0.072317	4.654320
363.637127	7449.460910	14.791079	-0.072327	4.651861
363.629629	7441.456366	14.796083	-0.072321	4.649395
363.364869	7433.487567	14.801088	-0.072266	4.646939
363.568355	7425.398327	14.806093	-0.072299	4.644445
363.638443	7417.524913	14.811098	-0.072307	4.642016
363.271143	7409.421409	14.816103	-0.072233	4.639515
363.444182	7401.527992	14.821107	-0.072260	4.637077
363.492772	7393.441858	14.826112	-0.072264	4.634579
363.366785	7385.480476	14.831117	-0.072235	4.632117
363.331701	7377.423335	14.836122	-0.072223	4.629625
363.336996	7369.461242	14.841127	-0.072219	4.627161
363.387833	7361.384364	14.846131	-0.072223	4.624660
363.287222	7353.478411	14.851136	-0.072199	4.622210
362.913071	7345.386072	14.856141	-0.072124	4.619701
362.897282	7337.482485	14.861146	-0.072116	4.617250
363.132878	7329.373188	14.866151	-0.072155	4.614734
363.210482	7321.470765	14.871155	-0.072164	4.612280
363.157221	7313.359958	14.876160	-0.072149	4.609760
362.991036	7305.423703	14.881165	-0.072113	4.607293
363.217324	7297.383960	14.886170	-0.072150	4.604793
362.888744	7289.437899	14.891175	-0.072083	4.602320
362.830425	7281.424980	14.896179	-0.072067	4.599826
362.964140	7273.471738	14.901184	-0.072087	4.597348
362.699535	7265.421354	14.906189	-0.072032	4.594839
362.936929	7257.412196	14.911194	-0.072071	4.592341
362.749558	7249.361338	14.916199	-0.072031	4.589829
362.539820	7241.376068	14.921203	-0.071987	4.587336
362.624962	7233.370715	14.926208	-0.071997	4.584836
362.557640	7225.377517	14.931213	-0.071980	4.582337
362.703467	7217.324640	14.936218	-0.072002	4.579819
362.549401	7209.331745	14.941223	-0.071968	4.577318
362.698758	7201.385345	14.946227	-0.071990	4.574831
362.844698	7193.367504	14.951232	-0.072012	4.572320
362.598736	7185.372446	14.956237	-0.071961	4.569814
362.601183	7177.378260	14.961242	-0.071956	4.567307
362.276780	7169.346903	14.966247	-0.071891	4.564787
362.375787	7161.384789	14.971251	-0.071904	4.562288
362.359277	7153.380132	14.976256	-0.071896	4.559774
362.039346	7145.402986	14.981261	-0.071831	4.557266
361.902129	7137.364468	14.986266	-0.071800	4.554738
362.246709	7129.337669	14.991271	-0.071859	4.552214
362.329674	7121.318258	14.996275	-0.071869	4.549690
362.218208	7113.377191	15.001280	-0.071843	4.547188
361.968844	7105.276288	15.006285	-0.071792	4.544635
362.148463	7097.351607	15.011290	-0.071820	4.542137
361.700657	7089.367422	15.016295	-0.071731	4.539616
361.725474	7081.366848	15.021299	-0.071731	4.537091
361.899954	7073.286359	15.026304	-0.071758	4.534539
362.033795	7065.304563	15.031309	-0.071778	4.532017
361.928805	7057.257366	15.036314	-0.071753	4.529473
361.678486	7049.301974	15.041319	-0.071701	4.526955
361.814010	7041.258574	15.046323	-0.071721	4.524409
361.736480	7033.344977	15.051328	-0.071701	4.521903
361.499819	7025.312353	15.056333	-0.071652	4.519357
361.626093	7017.359319	15.061338	-0.071670	4.516835
361.924043	7009.249487	15.066343	-0.071720	4.514263
361.797525	7001.342456	15.071347	-0.071692	4.511753
361.921806	6993.270066	15.076352	-0.071710	4.509189
361.551282	6985.279466	15.081357	-0.071635	4.506649
361.308816	6977.273417	15.086362	-0.071585	4.504102
361.385869	6969.288895	15.091367	-0.071594	4.501562
361.332982	6961.235877	15.096371	-0.071579	4.498998
361.455539	6953.334317	15.101376	-0.071597	4.496482
361.152446	6945.239603	15.106381	-0.071535	4.493901
360.919005	6937.297578	15.111386	-0.071486	4.491367
361.071052	6929.233992	15.116391	-0.071509	4.488795
360.973571	6921.249528	15.121395	-0.071486	4.486246
361.430752	6913.117856	15.126400	-0.071566	4.483650
361.237113	6905.278564	15.131405	-0.071525	4.481144
361.521814	6897.248997	15.136410	-0.071572	4.478577
361.507701	6889.218218	15.141415	-0.071564	4.476008
361.165788	6881.249206	15.146419	-0.071496	4.473455
361.136229	6873.267873	15.151424	-0.071485	4.470898
361.522417	6865.202490	15.156429	-0.071551	4.468314
361.384695	6857.210433	15.161434	-0.071521	4.465750
361.021854	6849.225321	15.166439	-0.071448	4.463186
361.252081	6841.212904	15.171443	-0.071485	4.460615
361.185890	6833.225954	15.176448	-0.071468	4.458048
361.228696	6825.212865	15.181453	-0.071471	4.455473
361.487170	6817.199166	15.186458	-0.071514	4.452897
361.494982	6809.184190	15.191463	-0.071510	4.450317
361.394764	6801.218205	15.196467	-0.071486	4.447752
361.208700	6793.198167	15.201472	-0.071446	4.445166
361.068500	6785.195694	15.206477	-0.071415	4.442586
361.113652	6777.216210	15.211482	-0.071418	4.440012
361.418203	6769.226442	15.216487	-0.071469	4.437435
361.362611	6761.190173	15.221491	-0.071454	4.434839
361.101810	6753.235498	15.226496	-0.071400	4.432267
361.302213	6745.151249	15.231501	-0.071432	4.429655
361.271132	6737.207850	15.236506	-0.071421	4.427084
360.921973	6729.130962	15.241511	-0.071351	4.424468
361.017129	6721.206315	15.246515	-0.071363	4.421902
361.280100	6713.172504	15.251520	-0.071407	4.419299
360.819920	6705.220822	15.256525	-0.071316	4.416718
360.681137	6697.135397	15.261530	-0.071285	4.414094
360.853591	6689.176977	15.266535	-0.071312	4.411511
360.776725	6681.125949	15.271539	-0.071292	4.408895
360.722224	6673.159972	15.276544	-0.071277	4.406305
360.552507	6665.132762	15.281549	-0.071240	4.403693
360.628962	6657.296522	15.286554	-0.071249	4.401144
360.496120	6649.167889	15.291559	-0.071219	4.398496
360.554095	6641.214820	15.296563	-0.071225	4.395905
360.723210	6633.110101	15.301568	-0.071251	4.393264
360.754096	6625.134459	15.306573	-0.071251	4.390662
360.786804	6617.147248	15.311578	-0.071252	4.388055
360.667020	6609.180300	15.316583	-0.071225	4.385453
360.631774	6601.199212	15.321587	-0.071213	4.382844
360.640414	6593.262078	15.326592	-0.071209	4.380249
360.604362	6585.257134	15.331597	-0.071198	4.377629
360.814783	6577.214627	15.336602	-0.071231	4.374998
360.605147	6569.207735	15.341607	-0.071187	4.372374
360.583272	6561.201711	15.346611	-0.071178	4.369749
360.501966	6553.266510	15.351616	-0.071158	4.367146
360.603678	6545.250290	15.356621	-0.071171	4.364516
360.415344	6537.309898	15.361626	-0.071131	4.361907
360.293277	6529.298773	15.366631	-0.071103	4.359274
360.209809	6521.300224	15.371635	-0.071082	4.356644
360.412349	6513.271609	15.376640	-0.071115	4.354004
360.241742	6505.191835	15.381645	-0.071078	4.351343
360.351780	6497.176948	15.386650	-0.071093	4.348704
360.124607	6489.247639	15.391655	-0.071045	4.346089
360.284745	6481.170276	15.396659	-0.071070	4.343427
360.397156	6473.263515	15.401664	-0.071086	4.340819
360.400984	6465.196737	15.406669	-0.071081	4.338155
360.163797	6457.284297	15.411674	-0.071032	4.335540
360.271636	6449.231492	15.416679	-0.071047	4.332878
359.915326	6441.228883	15.421683	-0.070975	4.330228
359.573767	6433.241335	15.426688	-0.070906	4.327582
359.685147	6425.179748	15.431693	-0.070922	4.324913
360.153752	6417.264870	15.436698	-0.071004	4.322294
360.099464	6409.230344	15.441703	-0.070988	4.319629
360.104347	6401.273617	15.446707	-0.070984	4.316989
360.112026	6393.222043	15.451712	-0.070980	4.314316
359.902852	6385.217686	15.456717	-0.070936	4.311655
359.927133	6377.220759	15.461722	-0.070935	4.308997
359.996949	6369.170337	15.466727	-0.070943	4.306320
360.015080	6361.156269	15.471731	-0.070941	4.303653
359.891611	6353.246514	15.476736	-0.070913	4.301018
359.995211	6345.192303	15.481741	-0.070927	4.298335
360.007336	6337.232595	15.486746	-0.070924	4.295681
359.836333	6329.183617	15.491751	-0.070887	4.292994
359.907682	6321.151839	15.496755	-0.070895	4.290313
359.868951	6313.230853	15.501760	-0.070883	4.287666
359.869143	6305.140042	15.506765	-0.070877	4.284962
359.686267	6297.249795	15.511770	-0.070838	4.282321
359.723694	6289.179276	15.516775	-0.070840	4.279620
359.475722	6281.264490	15.521779	-0.070789	4.276967
359.304843	6273.254741	15.526784	-0.070752	4.274281
359.171993	6265.195964	15.531789	-0.070722	4.271577
359.516565	6257.149045	15.536794	-0.070780	4.268880
359.630916	6249.151875	15.541799	-0.070797	4.266196
359.423645	6241.157951	15.546803	-0.070753	4.263509
359.349835	6233.221864	15.551808	-0.070734	4.260840
359.248942	6225.157060	15.556813	-0.070710	4.258126
359.321413	6217.209105	15.561818	-0.070718	4.255451
359.357383	6209.143054	15.566823	-0.070719	4.252735
359.424488	6201.133993	15.571827	-0.070727	4.250036
359.389802	6193.195097	15.576832	-0.070715	4.247359
359.149015	6185.128806	15.581837	-0.070665	4.244634
359.343865	6177.201348	15.586842	-0.070696	4.241959
359.334434	6169.165069	15.591847	-0.070689	4.239244
359.167517	6161.206243	15.596851	-0.070653	4.236551
359.359994	6153.185934	15.601856	-0.070683	4.233839
359.217015	6145.191417	15.606861	-0.070651	4.231131
359.169398	6137.137330	15.611866	-0.070637	4.228402
359.137941	6129.136751	15.616871	-0.070626	4.225690
359.283361	6121.154968	15.621875	-0.070648	4.222984
359.079500	6113.182184	15.626880	-0.070605	4.220276
358.952559	6105.164323	15.631885	-0.070576	4.217551
358.993310	6097.199480	15.636890	-0.070578	4.214845
359.189710	6089.151109	15.641895	-0.070610	4.212110
358.929418	6081.118423	15.646899	-0.070556	4.209373
358.838656	6073.167919	15.651904	-0.070534	4.206665
358.524577	6065.135717	15.656909	-0.070470	4.203925
358.568070	6057.263436	15.661914	-0.070473	4.201241
358.523504	6049.138455	15.666919	-0.070460	4.198468
358.746062	6041.131346	15.671923	-0.070496	4.195737
358.796120	6033.112439	15.676928	-0.070500	4.192998
358.448947	6025.096927	15.681933	-0.070430	4.190254
358.753215	6017.097999	15.686938	-0.070481	4.187521
358.620768	6009.111187	15.691943	-0.070451	4.184786
358.536300	6001.128890	15.696947	-0.070431	4.182051
358.500821	5993.117351	15.701952	-0.070419	4.179304
358.606100	5985.137052	15.706957	-0.070433	4.176568
358.470202	5977.163262	15.711962	-0.070403	4.173830
358.405830	5969.150404	15.716967	-0.070385	4.171077
358.526834	5961.146185	15.721971	-0.070403	4.168328
358.480608	5953.136014	15.726976	-0.070389	4.165573
358.165243	5945.171801	15.731981	-0.070325	4.162828
358.501710	5937.172814	15.736986	-0.070382	4.160078
358.210996	5929.239190	15.741991	-0.070323	4.157341
358.293527	5921.164061	15.746995	-0.070333	4.154558
358.357040	5913.185478	15.752000	-0.070340	4.151806
358.332878	5905.114200	15.757005	-0.070330	4.149019
358.438936	5897.173554	15.762010	-0.070344	4.146277
358.296096	5889.131969	15.767015	-0.070313	4.143495
358.174434	5881.222248	15.772019	-0.070285	4.140757
358.124121	5873.189783	15.777024	-0.070270	4.137975
357.922438	5865.193774	15.782029	-0.070227	4.135202
357.768654	5857.240087	15.787034	-0.070194	4.132443
357.758171	5849.167475	15.792039	-0.070186	4.129643
357.900512	5841.182514	15.797043	-0.070208	4.126873
357.867763	5833.146815	15.802048	-0.070196	4.124081
357.943952	5825.176945	15.807053	-0.070205	4.121312
357.861872	5817.171103	15.812058	-0.070185	4.118526
357.851081	5809.209136	15.817063	-0.070177	4.115755
358.005722	5801.167989	15.822067	-0.070201	4.112956
357.891241	5793.197665	15.827072	-0.070174	4.110177
357.699147	5785.171485	15.832077	-0.070133	4.107375
357.913944	5777.151396	15.837082	-0.070168	4.104579
357.755130	5769.212645	15.842087	-0.070133	4.101804
357.838330	5761.118535	15.847091	-0.070144	4.098976
357.608470	5753.215956	15.852096	-0.070096	4.096209
357.690732	5745.157912	15.857101	-0.070106	4.093390
357.830745	5737.171620	15.862106	-0.070127	4.090596
357.692997	5729.149753	15.867111	-0.070096	4.087782
357.484395	5721.131986	15.872115	-0.070052	4.084968
357.748906	5713.174668	15.877120	-0.070096	4.082179
357.401789	5705.172956	15.882125	-0.070026	4.079364
357.418380	5697.217450	15.887130	-0.070024	4.076568
357.400831	5689.180106	15.892135	-0.070015	4.073742
357.435956	5681.176255	15.897139	-0.070016	4.070926
357.437786	5673.156323	15.902144	-0.070012	4.068102
357.264517	5665.118530	15.907149	-0.069974	4.065267
357.171609	5657.197106	15.912154	-0.069952	4.062472
357.200904	5649.182109	15.917159	-0.069952	4.059644
357.098471	5641.182874	15.922163	-0.069927	4.056817
357.087352	5633.179951	15.927168	-0.069920	4.053989
357.166514	5625.146869	15.932173	-0.069930	4.051150
357.075406	5617.175447	15.937178	-0.069907	4.048327
357.143928	5609.135542	15.942183	-0.069915	4.045481
357.119711	5601.169712	15.947187	-0.069905	4.042658
356.691508	5593.243451	15.952192	-0.069820	4.039841
356.709627	5585.240330	15.957197	-0.069819	4.037001
356.859298	5577.204363	15.962202	-0.069841	4.034149
356.797170	5569.119550	15.967207	-0.069824	4.031275
356.787994	5561.130263	15.972211	-0.069817	4.028434
356.967274	5553.137976	15.977216	-0.069845	4.025593
356.998114	5545.137948	15.982221	-0.069846	4.022744
357.123045	5537.179510	15.987226	-0.069864	4.019910
356.914126	5529.222024	15.992231	-0.069820	4.017069
356.801787	5521.223782	15.997235	-0.069794	4.014212
356.707580	5513.247041	16.002240	-0.069771	4.011362
356.702909	5505.175748	16.007245	-0.069765	4.008477
357.107906	5497.178183	16.012250	-0.069835	4.005624
356.970369	5489.223223	16.017255	-0.069804	4.002774
356.779841	5481.266060	16.022259	-0.069764	3.999921
356.841542	5473.273866	16.027264	-0.069770	3.997058
356.807946	5465.203205	16.032269	-0.069758	3.994162
356.599436	5457.256403	16.037274	-0.069714	3.991306
356.824776	5449.203157	16.042279	-0.069751	3.988417
356.807345	5441.207392	16.047283	-0.069743	3.985543
356.750538	5433.248830	16.052288	-0.069727	3.982679
356.652354	5425.195747	16.057293	-0.069703	3.979779
356.867001	5417.248424	16.062298	-0.069738	3.976919
356.781500	5409.202081	16.067303	-0.069717	3.974017
356.537885	5401.224862	16.072307	-0.069666	3.971135
356.619352	5393.221809	16.077312	-0.069676	3.968247
356.651629	5385.185548	16.082317	-0.069677	3.965344
356.624408	5377.269500	16.087322	-0.069667	3.962482
356.531804	5369.239136	16.092327	-0.069644	3.959575
356.666035	5361.250659	16.097331	-0.069664	3.956684
356.686060	5353.219501	16.102336	-0.069662	3.953775
356.525239	5345.240470	16.107341	-0.069627	3.950879
356.591306	5337.205888	16.112346	-0.069634	3.947964
356.375164	5329.208884	16.117351	-0.069589	3.945056
356.263259	5321.228823	16.122355	-0.069563	3.942154
356.411694	5313.201763	16.127360	-0.069585	3.939237
356.304495	5305.261596	16.132365	-0.069560	3.936345
356.291179	5297.212752	16.137370	-0.069552	3.933413
356.348631	5289.199613	16.142375	-0.069558	3.930494
356.386094	5281.201161	16.147379	-0.069559	3.927577
356.349214	5273.230509	16.152384	-0.069547	3.924666
356.217834	5265.268224	16.157389	-0.069518	3.921755
356.276556	5257.243782	16.162394	-0.069523	3.918823
356.138364	5249.304053	16.167399	-0.069493	3.915915
356.036726	5241.249853	16.172403	-0.069468	3.912964
356.119904	5233.259155	16.177408	-0.069479	3.910038
356.217029	5225.228551	16.182413	-0.069491	3.907095
356.200216	5217.227977	16.187418	-0.069483	3.904159
356.048387	5209.314688	16.192423	-0.069450	3.901250
355.982614	5201.282959	16.197427	-0.069432	3.898297
356.114781	5193.322911	16.202432	-0.069452	3.895372
355.981982	5185.301912	16.207437	-0.069422	3.892417
356.021940	5177.271639	16.212442	-0.069424	3.889460
355.912380	5169.325134	16.217447	-0.069398	3.886528
355.740419	5161.302691	16.222451	-0.069361	3.883565
355.825467	5153.361774	16.227456	-0.069372	3.880635
355.968733	5145.314617	16.232461	-0.069393	3.877665
355.947625	5137.343537	16.237466	-0.069384	3.874717
355.747836	5129.203030	16.242471	-0.069341	3.871700
355.852900	5121.164708	16.247475	-0.069356	3.868726
355.786249	5113.241601	16.252480	-0.069338	3.865788
355.605578	5105.237622	16.257485	-0.069299	3.862816
355.719507	5097.286178	16.262490	-0.069315	3.859866
355.765607	5089.312717	16.267495	-0.069319	3.856906
355.578860	5081.293230	16.272499	-0.069278	3.853920
355.555671	5073.355361	16.277504	-0.069269	3.850967
355.523303	5065.300916	16.282509	-0.069258	3.847967
355.637214	5057.302094	16.287514	-0.069274	3.844989
355.410511	5049.343436	16.292519	-0.069226	3.842016
355.557889	5041.288966	16.297523	-0.069248	3.839013
355.630697	5033.357067	16.302528	-0.069257	3.836052
355.307748	5025.321730	16.307533	-0.069191	3.833042
355.335812	5017.328924	16.312538	-0.069191	3.830053
355.394566	5009.310530	16.317543	-0.069197	3.827052
355.360106	5001.262280	16.322547	-0.069185	3.824036
355.353140	4993.375240	16.327552	-0.069179	3.821078
355.318184	4985.311358	16.332557	-0.069167	3.818052
355.213810	4977.335326	16.337562	-0.069143	3.815054
354.937554	4969.357664	16.342567	-0.069086	3.812049
355.050527	4961.282505	16.347571	-0.069102	3.809014
355.073944	4953.345158	16.352576	-0.069101	3.806027
354.981385	4945.339060	16.357581	-0.069078	3.803009
355.071202	4937.382906	16.362586	-0.069090	3.800011
355.323924	4929.395771	16.367591	-0.069132	3.797003
355.100129	4921.354763	16.372595	-0.069085	3.793961
355.031039	4913.387607	16.377600	-0.069067	3.790948
354.958201	4905.361046	16.382605	-0.069048	3.787911
355.034299	4897.372159	16.387610	-0.069057	3.784888
354.886981	4889.412529	16.392615	-0.069024	3.781869
354.830213	4881.382914	16.397619	-0.069008	3.778823
355.020512	4873.415952	16.402624	-0.069039	3.775805
354.719112	4865.376739	16.407629	-0.068977	3.772745
354.730171	4857.384526	16.412634	-0.068974	3.769707
354.727971	4849.423383	16.417639	-0.068968	3.766679
354.774410	4841.382785	16.422643	-0.068972	3.763619
354.599575	4833.440533	16.427648	-0.068934	3.760589
354.402292	4825.437443	16.432653	-0.068892	3.757532
354.672920	4817.438958	16.437658	-0.068937	3.754486
354.517208	4809.489614	16.442663	-0.068903	3.751447
354.504073	4801.433966	16.447667	-0.068895	3.748367
354.501592	4793.425868	16.452672	-0.068890	3.745303
354.481164	4785.470317	16.457677	-0.068881	3.742257
354.460746	4777.452034	16.462682	-0.068872	3.739184
354.472832	4769.496025	16.467687	-0.068869	3.736133
354.453639	4761.449354	16.472691	-0.068860	3.733044
354.537878	4753.425357	16.477696	-0.068870	3.729964
354.386238	4745.442874	16.482701	-0.068837	3.726891
354.184667	4737.467080	16.487706	-0.068794	3.723817
354.237711	4729.500657	16.492711	-0.068799	3.720751
354.064717	4721.473925	16.497715	-0.068761	3.717653
354.164288	4713.515205	16.502720	-0.068775	3.714586
354.150459	4705.448488	16.507725	-0.068767	3.711471
354.125009	4697.430520	16.512730	-0.068757	3.708373
354.022632	4689.422795	16.517735	-0.068733	3.705273
354.075959	4681.442839	16.522739	-0.068737	3.702186
354.112272	4673.451329	16.527744	-0.068739	3.699092
354.035664	4665.506303	16.532749	-0.068719	3.696010
353.989142	4657.468589	16.537754	-0.068705	3.692890
354.030032	4649.456684	16.542759	-0.068708	3.689780
353.850755	4641.503419	16.547763	-0.068669	3.686684
353.816942	4633.494860	16.552768	-0.068658	3.683568
353.684458	4625.511064	16.557773	-0.068628	3.680456
353.706836	4617.563517	16.562778	-0.068627	3.677360
353.676362	4609.536665	16.567783	-0.068616	3.674229
353.840507	4601.549636	16.572787	-0.068641	3.671116
353.820349	4593.531723	16.577792	-0.068632	3.667984
353.457276	4585.522890	16.582797	-0.068559	3.664842
353.715999	4577.572779	16.587802	-0.068602	3.661739
353.499395	4569.558043	16.592807	-0.068557	3.658594
353.432877	4561.582007	16.597811	-0.068539	3.655466
353.486626	4553.594065	16.602816	-0.068544	3.652333
353.537191	4545.527346	16.607821	-0.068548	3.649167
353.662712	4537.594941	16.612826	-0.068566	3.646053
353.567315	4529.621400	16.617831	-0.068543	3.642914
353.379002	4521.622520	16.622835	-0.068503	3.639760
353.462999	4513.652502	16.627840	-0.068513	3.636622
353.387121	4505.611301	16.632845	-0.068494	3.633449
353.493046	4497.603709	16.637850	-0.068508	3.630292
353.392448	4489.611516	16.642855	-0.068485	3.627131
353.270587	4481.601820	16.647859	-0.068457	3.623961
353.492637	4473.650130	16.652864	-0.068493	3.620821
353.229423	4465.606345	16.657869	-0.068438	3.617627
353.169879	4457.643992	16.662874	-0.068422	3.614469
353.297450	4449.612128	16.667879	-0.068441	3.611286
353.315391	4441.599989	16.672883	-0.068439	3.608104
353.301642	4433.645119	16.677888	-0.068431	3.604942
353.229116	4425.648985	16.682893	-0.068412	3.601759
353.326763	4417.663931	16.687898	-0.068425	3.598582
353.117567	4409.695934	16.692903	-0.068381	3.595401
353.013468	4401.708562	16.697907	-0.068357	3.592212
353.036653	4393.687658	16.702912	-0.068356	3.589010
353.008988	4385.658934	16.707917	-0.068345	3.585801
353.018141	4377.665108	16.712922	-0.068342	3.582604
353.096803	4369.670120	16.717927	-0.068351	3.579406
353.134450	4361.731264	16.722931	-0.068353	3.576226
353.021110	4353.711944	16.727936	-0.068327	3.573007
352.878587	4345.677224	16.732941	-0.068295	3.569777
352.907016	4337.722411	16.737946	-0.068295	3.566582
352.799037	4329.728367	16.742951	-0.068270	3.563364
352.812020	4321.755703	16.747955	-0.068267	3.560156
352.851175	4313.782818	16.752960	-0.068269	3.556945
352.764897	4305.756234	16.757965	-0.068247	3.553706
352.638400	4297.716110	16.762970	-0.068219	3.550457
352.410470	4289.763782	16.767975	-0.068171	3.547238
352.534691	4281.693767	16.772979	-0.068189	3.543979
352.489710	4273.806829	16.777984	-0.068175	3.540786
352.152167	4265.817064	16.782989	-0.068107	3.537539
352.286091	4257.781444	16.787994	-0.068127	3.534285
352.480268	4249.776956	16.792999	-0.068158	3.531043
352.225885	4241.777679	16.798003	-0.068105	3.527786
352.258381	4233.813478	16.803008	-0.068106	3.524549
352.336067	4225.797845	16.808013	-0.068115	3.521289
352.289043	4217.836132	16.813018	-0.068101	3.518045
352.156301	4209.821152	16.818023	-0.068071	3.514773
352.098850	4201.852137	16.823027	-0.068056	3.511519
352.393815	4193.801655	16.828032	-0.068105	3.508241
352.078418	4185.816697	16.833037	-0.068041	3.504966
352.078621	4177.879947	16.838042	-0.068036	3.501718
352.135422	4169.872933	16.843047	-0.068041	3.498440
351.973718	4161.861864	16.848051	-0.068006	3.495151
351.958187	4153.906833	16.853056	-0.067998	3.491886
351.775160	4145.835138	16.858061	-0.067959	3.488564
351.735853	4137.868996	16.863066	-0.067946	3.485288
351.793611	4129.895746	16.868071	-0.067952	3.482008
351.708817	4121.886921	16.873075	-0.067931	3.478706
351.889491	4113.930161	16.878080	-0.067959	3.475432
351.675505	4105.931093	16.883085	-0.067914	3.472123
351.634770	4097.924192	16.888090	-0.067901	3.468814
351.730933	4089.906278	16.893095	-0.067914	3.465502
351.577462	4081.908040	16.898099	-0.067880	3.462187
351.696101	4073.913389	16.903104	-0.067897	3.458879
351.673358	4065.968013	16.908109	-0.067887	3.455583
351.602203	4057.954517	16.913114	-0.067869	3.452254
351.429654	4049.980412	16.918119	-0.067832	3.448935
351.402628	4041.978808	16.923123	-0.067821	3.445607
351.623498	4033.982454	16.928128	-0.067857	3.442286
351.404644	4025.982222	16.933133	-0.067811	3.438944
351.407031	4018.050055	16.938138	-0.067807	3.435636
351.701971	4010.021955	16.943143	-0.067856	3.432294
351.665988	4002.019441	16.948147	-0.067844	3.428949
351.482106	3994.057267	16.953152	-0.067805	3.425612
351.415181	3986.047680	16.958157	-0.067787	3.422256
351.456943	3978.063658	16.963162	-0.067790	3.418911
351.229680	3970.100418	16.968167	-0.067742	3.415562
351.347830	3962.043131	16.973171	-0.067759	3.412182
351.303784	3954.083953	16.978176	-0.067746	3.408835
351.011440	3946.099534	16.983181	-0.067686	3.405465
351.205216	3938.104819	16.988186	-0.067717	3.402104
351.074187	3930.116717	16.993191	-0.067687	3.398731
351.183027	3922.099868	16.998195	-0.067702	3.395352
351.089357	3914.111973	17.003200	-0.067679	3.391974
350.743370	3906.116827	17.008205	-0.067610	3.388580
350.984012	3898.092709	17.013210	-0.067649	3.385192
350.915398	3890.131874	17.018215	-0.067631	3.381816
350.892503	3882.117695	17.023219	-0.067622	3.378416
350.876040	3874.166898	17.028224	-0.067614	3.375040
350.874671	3866.140532	17.033229	-0.067608	3.371628
350.871686	3858.141504	17.038234	-0.067602	3.368225
350.803951	3850.191376	17.043239	-0.067585	3.364837
350.785772	3842.199585	17.048243	-0.067576	3.361429
350.870101	3834.224491	17.053248	-0.067586	3.358029
350.670630	3826.239957	17.058253	-0.067544	3.354611
351.030650	3818.218143	17.063258	-0.067606	3.351194
350.879702	3810.225287	17.068263	-0.067572	3.347767
350.651856	3802.248935	17.073267	-0.067525	3.344340
350.836172	3794.299702	17.078272	-0.067554	3.340938
350.688741	3786.289782	17.083277	-0.067521	3.337493
350.584509	3778.287999	17.088282	-0.067497	3.334050
350.713886	3770.309273	17.093287	-0.067516	3.330622
350.675102	3762.298648	17.098291	-0.067503	3.327170
350.524233	3754.305657	17.103296	-0.067470	3.323718
350.496298	3746.354132	17.108301	-0.067459	3.320285
350.522892	3738.369839	17.113306	-0.067459	3.316837
350.498586	3730.347198	17.118311	-0.067449	3.313366
350.458430	3722.324318	17.123315	-0.067437	3.309891
350.449049	3714.333744	17.128320	-0.067430	3.306427
350.424584	3706.319115	17.133325	-0.067420	3.302949
350.144056	3698.394383	17.138330	-0.067362	3.299496
350.378141	3690.402563	17.143335	-0.067401	3.296031
350.500373	3682.361845	17.148339	-0.067418	3.292536
350.461435	3674.380141	17.153344	-0.067406	3.289057
350.272479	3666.415631	17.158349	-0.067365	3.285575
350.294745	3658.440280	17.163354	-0.067364	3.282094
350.397327	3650.429592	17.168359	-0.067378	3.278597
350.097604	3642.495134	17.173363	-0.067317	3.275113
350.059074	3634.501699	17.178368	-0.067305	3.271610
350.143184	3626.462094	17.183373	-0.067315	3.268088
349.932444	3618.486176	17.188378	-0.067271	3.264578
349.987989	3610.531126	17.193383	-0.067276	3.261085
350.005465	3602.532087	17.198387	-0.067274	3.257567
350.129418	3594.516164	17.203392	-0.067292	3.254042
349.782049	3586.556468	17.208397	-0.067222	3.250518
349.784714	3578.560062	17.213402	-0.067217	3.246989
349.946142	3570.548267	17.218407	-0.067242	3.243456
349.791769	3562.583297	17.223411	-0.067208	3.239926
349.809102	3554.610197	17.228416	-0.067206	3.236397
349.698379	3546.629024	17.233421	-0.067180	3.232854
349.853624	3538.594923	17.238426	-0.067204	3.229295
349.595338	3530.617953	17.243431	-0.067151	3.225741
349.701062	3522.615316	17.248435	-0.067165	3.222186
349.805489	3514.616678	17.253440	-0.067179	3.218629
349.712683	3506.636554	17.258445	-0.067157	3.215068
349.773088	3498.617806	17.263450	-0.067163	3.211492
349.754126	3490.647695	17.268455	-0.067154	3.207931
349.610152	3482.653098	17.273459	-0.067122	3.204350
349.681705	3474.683023	17.278464	-0.067130	3.200784
349.609546	3466.724508	17.283469	-0.067111	3.197214
349.455882	3458.743853	17.288474	-0.067078	3.193626
349.491023	3450.735223	17.293479	-0.067079	3.190030
349.312175	3442.749420	17.298483	-0.067040	3.186430
349.367545	3434.777003	17.303488	-0.067045	3.182843
349.358442	3426.751990	17.308493	-0.067039	3.179226
349.404117	3418.802684	17.313498	-0.067042	3.175640
349.392918	3410.792614	17.318503	-0.067035	3.172021
349.315123	3402.797526	17.323507	-0.067015	3.168401
349.184195	3394.825788	17.328512	-0.066985	3.164786
348.964994	3386.894620	17.333517	-0.066939	3.161180
348.966474	3378.884875	17.338522	-0.066934	3.157545
349.148884	3370.851391	17.343527	-0.066963	3.153903
349.103367	3362.855812	17.348531	-0.066949	3.150264
349.173461	3354.868319	17.353536	-0.066957	3.146629
349.127926	3346.870709	17.358541	-0.066943	3.142980
349.224713	3338.891493	17.363546	-0.066956	3.139342
349.280304	3330.931049	17.368551	-0.066961	3.135707
348.887607	3322.965250	17.373555	-0.066883	3.132044
349.044265	3314.939021	17.378560	-0.066907	3.128374
348.847332	3306.948054	17.383565	-0.066865	3.124700
348.829954	3299.011749	17.388570	-0.066857	3.121055
348.766899	3291.034346	17.393575	-0.066840	3.117385
348.746992	3283.049819	17.398579	-0.066831	3.113709
348.957209	3275.035913	17.403584	-0.066865	3.110026
348.858390	3267.036975	17.408589	-0.066841	3.106331
348.790085	3259.070181	17.413594	-0.066823	3.102648
348.702314	3251.103392	17.418599	-0.066802	3.098960
348.681224	3243.112390	17.423603	-0.066792	3.095259
348.800157	3235.116006	17.428608	-0.066809	3.091558
348.833458	3227.094191	17.433613	-0.066810	3.087837
348.768775	3219.102806	17.438618	-0.066793	3.084120
348.673294	3211.183266	17.443623	-0.066770	3.080431
348.691902	3203.175129	17.448627	-0.066768	3.076702
348.729994	3195.169335	17.453632	-0.066770	3.072970
348.620517	3187.131671	17.458637	-0.066744	3.069212
348.548826	3179.181428	17.463642	-0.066726	3.065492
348.677930	3171.213421	17.468647	-0.066745	3.061769
348.426532	3163.221939	17.473651	-0.066693	3.058011
348.458704	3155.260815	17.478656	-0.066693	3.054277
348.485956	3147.245502	17.483661	-0.066693	3.050513
348.443762	3139.281142	17.488666	-0.066680	3.046765
348.084897	3131.335186	17.493671	-0.066608	3.043005
348.271437	3123.311702	17.498675	-0.066638	3.039231
348.299909	3115.382076	17.503680	-0.066638	3.035489
348.015740	3107.397380	17.508685	-0.066580	3.031700
347.886737	3099.391978	17.513690	-0.066550	3.027905
348.179576	3091.365362	17.518695	-0.066600	3.024115
348.087848	3083.406383	17.523699	-0.066577	3.020334
347.992594	3075.451883	17.528704	-0.066555	3.016550
347.901882	3067.434783	17.533709	-0.066532	3.012732
347.751172	3059.470954	17.538714	-0.066499	3.008932
347.597222	3051.497330	17.543719	-0.066465	3.005121
347.913379	3043.470056	17.548723	-0.066519	3.001304
348.074972	3035.493486	17.553728	-0.066544	2.997499
347.892197	3027.514279	17.558733	-0.066504	2.993670
347.827657	3019.549627	17.563738	-0.066487	2.989849
347.859382	3011.558851	17.568743	-0.066488	2.986015
347.710836	3003.560709	17.573747	-0.066455	2.982164
347.645357	2995.617194	17.578752	-0.066438	2.978338
347.976589	2987.579570	17.583757	-0.066494	2.974483
348.046914	2979.593349	17.588762	-0.066502	2.970634
347.811770	2971.636332	17.593767	-0.066453	2.966778
347.537086	2963.658601	17.598771	-0.066397	2.962904
347.848735	2955.661830	17.603776	-0.066449	2.959048
347.673703	2947.730911	17.608781	-0.066412	2.955192
347.344359	2939.771377	17.613786	-0.066345	2.951310
347.407818	2931.755809	17.618791	-0.066352	2.947416
347.549068	2923.723058	17.623795	-0.066373	2.943512
347.495019	2915.785030	17.628800	-0.066357	2.939640
347.437730	2907.814388	17.633805	-0.066342	2.935746
347.516323	2899.794077	17.638810	-0.066351	2.931829
347.533011	2891.818039	17.643815	-0.066349	2.927926
347.291382	2883.842338	17.648819	-0.066299	2.924004
347.412527	2875.902796	17.653824	-0.066316	2.920114
347.447144	2867.909085	17.658829	-0.066317	2.916187
347.375720	2859.912539	17.663834	-0.066299	2.912248
347.370371	2851.885311	17.668839	-0.066293	2.908293
347.328414	2843.883204	17.673843	-0.066279	2.904342
347.271606	2835.954913	17.678848	-0.066264	2.900421
347.174817	2827.975006	17.683853	-0.066240	2.896467
347.404987	2819.971308	17.688858	-0.066278	2.892515
347.240888	2812.000662	17.693863	-0.066242	2.888551
346.995482	2804.033859	17.698867	-0.066191	2.884579
347.323324	2796.066286	17.703872	-0.066247	2.880633
347.310105	2788.064635	17.708877	-0.066240	2.876646
347.111568	2780.112533	17.713882	-0.066197	2.872668
346.997857	2772.146967	17.718887	-0.066171	2.868682
347.077852	2764.137520	17.723891	-0.066181	2.864680
346.916914	2756.229483	17.728896	-0.066146	2.860709
346.906723	2748.200937	17.733901	-0.066138	2.856680
346.983984	2740.209154	17.738906	-0.066148	2.852670
346.895501	2732.243764	17.743911	-0.066126	2.848658
346.875346	2724.247775	17.748915	-0.066117	2.844628
346.848292	2716.321424	17.753920	-0.066107	2.840627
346.833462	2708.323342	17.758925	-0.066099	2.836586
346.656556	2700.358992	17.763930	-0.066061	2.832546
346.541167	2692.378701	17.768935	-0.066034	2.828496
346.615964	2684.342475	17.773939	-0.066042	2.824422
346.575784	2676.409052	17.778944	-0.066030	2.820389
346.621860	2668.420004	17.783949	-0.066033	2.816326
346.575698	2660.443964	17.788954	-0.066019	2.812259
346.791367	2652.436869	17.793959	-0.066054	2.808185
346.449384	2644.465213	17.798963	-0.065985	2.804091
346.576508	2636.523899	17.803968	-0.066004	2.800034
346.473621	2628.549644	17.808973	-0.065980	2.795940
346.607831	2620.552126	17.813978	-0.065999	2.791843
346.433356	2612.581769	17.818983	-0.065962	2.787735
346.534872	2604.569087	17.823987	-0.065975	2.783616
346.546257	2596.641111	17.828992	-0.065972	2.779529
346.221714	2588.686968	17.833997	-0.065907	2.775402
346.181286	2580.696886	17.839002	-0.065894	2.771267
346.366918	2572.701107	17.844007	-0.065923	2.767137
346.127664	2564.735504	17.849011	-0.065873	2.762991
346.212941	2556.789211	17.854016	-0.065884	2.758868
346.163571	2548.808949	17.859021	-0.065870	2.754714
346.122057	2540.777551	17.864026	-0.065857	2.750526
345.883797	2532.835018	17.869031	-0.065807	2.746367
345.997443	2524.807203	17.874035	-0.065823	2.742179
346.205873	2516.832126	17.879040	-0.065857	2.738017
345.850070	2508.901991	17.884045	-0.065785	2.733838
346.062190	2500.890629	17.889050	-0.065819	2.729645
345.998057	2492.951877	17.894055	-0.065802	2.725466
345.906125	2484.976545	17.899059	-0.065780	2.721260
345.933982	2477.042947	17.904064	-0.065780	2.717078
345.957545	2469.048840	17.909069	-0.065779	2.712856
345.831013	2461.063463	17.914074	-0.065750	2.708623
345.694835	2453.094749	17.919079	-0.065720	2.704391
345.826071	2445.116193	17.924083	-0.065739	2.700165
345.816452	2437.163613	17.929088	-0.065732	2.695937
345.616176	2429.192183	17.934093	-0.065690	2.691680
345.554111	2421.201452	17.939098	-0.065673	2.687415
345.753508	2413.232460	17.944103	-0.065705	2.683171
345.675399	2405.259679	17.949107	-0.065685	2.678901
345.517894	2397.336140	17.954112	-0.065650	2.674645
345.301416	2389.352889	17.959117	-0.065605	2.670346
345.370305	2381.342978	17.964122	-0.065612	2.666045
345.302728	2373.362711	17.969127	-0.065595	2.661744
345.382553	2365.364520	17.974131	-0.065604	2.657436
345.322448	2357.435184	17.979136	-0.065588	2.653149
345.283197	2349.445780	17.984141	-0.065575	2.648823
345.205769	2341.480496	17.989146	-0.065556	2.644502
345.252113	2333.534791	17.994151	-0.065559	2.640192
345.021391	2325.586466	17.999155	-0.065511	2.635855
344.990775	2317.615051	18.004160	-0.065500	2.631511
344.928173	2309.628194	18.009165	-0.065483	2.627150
344.975104	2301.634423	18.014170	-0.065487	2.622786
345.059374	2293.660953	18.019175	-0.065497	2.618427
344.856242	2285.727226	18.024179	-0.065454	2.614064
345.148294	2277.723025	18.029184	-0.065503	2.609688
344.999445	2269.751604	18.034189	-0.065470	2.605293
345.039821	2261.811576	18.039194	-0.065473	2.600921
344.828055	2253.889442	18.044199	-0.065428	2.596534
344.574130	2245.849027	18.049203	-0.065376	2.592071
344.533874	2237.824951	18.054208	-0.065363	2.587624
344.577336	2229.841785	18.059213	-0.065366	2.583198
344.563873	2221.902203	18.064218	-0.065358	2.578785
344.742657	2213.924124	18.069223	-0.065386	2.574356
344.472226	2205.988968	18.074227	-0.065331	2.569912
344.583028	2198.002781	18.079232	-0.065346	2.565458
344.538450	2190.053228	18.084237	-0.065332	2.561007
344.362058	2182.121522	18.089242	-0.065294	2.556548
344.363545	2174.162440	18.094247	-0.065290	2.552079
344.435533	2166.150336	18.099251	-0.065298	2.547577
344.319995	2158.212610	18.104256	-0.065271	2.543095
344.275750	2150.257698	18.109261	-0.065258	2.538601
344.326910	2142.268238	18.114266	-0.065262	2.534087
344.345393	2134.310946	18.119271	-0.065260	2.529580
344.168173	2126.331471	18.124275	-0.065222	2.525038
344.279565	2118.386280	18.129280	-0.065237	2.520529
344.042795	2110.459413	18.134285	-0.065188	2.515996
344.105660	2102.478959	18.139290	-0.065195	2.511447
343.986342	2094.513609	18.144295	-0.065167	2.506885
343.941579	2086.527283	18.149299	-0.065154	2.502308
344.026631	2078.569978	18.154304	-0.065164	2.497748
343.964838	2070.591448	18.159309	-0.065148	2.493158
343.969888	2062.617037	18.164314	-0.065143	2.488566
343.947982	2054.657339	18.169319	-0.065134	2.483972
343.784428	2046.717938	18.174323	-0.065098	2.479371
343.811807	2038.778609	18.179328	-0.065098	2.474775
343.728550	2030.817164	18.184333	-0.065078	2.470150
343.681261	2022.826512	18.189338	-0.065064	2.465502
343.810938	2014.874278	18.194343	-0.065083	2.460881
343.811243	2006.908220	18.199347	-0.065077	2.456233
343.689233	1998.963493	18.204352	-0.065049	2.451579
343.697259	1990.992247	18.209357	-0.065046	2.446912
343.711487	1983.030329	18.214362	-0.065043	2.442241
343.752607	1975.094918	18.219367	-0.065046	2.437579
343.399831	1967.130800	18.224371	-0.064975	2.432860
343.508521	1959.134260	18.229376	-0.064990	2.428149
343.414781	1951.173761	18.234381	-0.064967	2.423434
343.191777	1943.258662	18.239386	-0.064920	2.418727
343.365711	1935.259122	18.244391	-0.064948	2.413992
343.238061	1927.293955	18.249395	-0.064919	2.409244
343.130942	1919.360917	18.254400	-0.064893	2.404507
342.875101	1911.448876	18.259405	-0.064841	2.399762
343.053779	1903.463838	18.264410	-0.064869	2.394999
343.050580	1895.503397	18.269415	-0.064863	2.390226
342.942271	1887.513809	18.274419	-0.064837	2.385417
343.112777	1879.565507	18.279424	-0.064864	2.380646
342.726759	1871.675294	18.284429	-0.064787	2.375856
342.596127	1863.701185	18.289434	-0.064757	2.371026
342.605649	1855.744001	18.294439	-0.064754	2.366207
342.389704	1847.810699	18.299443	-0.064709	2.361375
342.513352	1839.836903	18.304448	-0.064726	2.356536
342.278763	1831.900961	18.309453	-0.064678	2.351681
342.575160	1823.867905	18.314458	-0.064728	2.346800
342.297098	1815.957180	18.319463	-0.064671	2.341937
342.201502	1808.010690	18.324467	-0.064648	2.337056
342.287573	1800.046883	18.329472	-0.064658	2.332170
342.481353	1792.028480	18.334477	-0.064689	2.327249
342.387102	1784.094176	18.339482	-0.064666	2.322345
342.554554	1776.142775	18.344487	-0.064692	2.317442
342.266523	1768.228413	18.349491	-0.064634	2.312513
342.397765	1760.270630	18.354496	-0.064653	2.307583
342.394602	1752.300173	18.359501	-0.064647	2.302622
342.199914	1744.401072	18.364506	-0.064606	2.297679
342.384571	1736.421744	18.369511	-0.064635	2.292708
342.156498	1728.472905	18.374515	-0.064587	2.287709
342.339304	1720.505988	18.379520	-0.064616	2.282723
342.344610	1712.570814	18.384525	-0.064612	2.277732
342.237732	1704.621624	18.389530	-0.064587	2.272710
342.217991	1696.634505	18.394535	-0.064578	2.267661
342.159371	1688.684873	18.399539	-0.064562	2.262621
342.151354	1680.761148	18.404544	-0.064555	2.257591
342.080824	1672.808663	18.409549	-0.064537	2.252526
342.040685	1664.863488	18.414554	-0.064524	2.247457
342.420474	1656.874713	18.419559	-0.064590	2.242386
341.986689	1648.986509	18.424563	-0.064504	2.237294
342.005210	1641.048124	18.429568	-0.064502	2.232200
342.211532	1633.061904	18.434573	-0.064535	2.227080
342.052115	1625.138174	18.439578	-0.064500	2.221956
341.799507	1617.252968	18.444583	-0.064448	2.216836
341.828445	1609.272475	18.449587	-0.064448	2.211668
341.773171	1601.340041	18.454592	-0.064433	2.206512
341.736180	1593.378790	18.459597	-0.064421	2.201326
341.741346	1585.453507	18.464602	-0.064416	2.196155
341.601306	1577.532691	18.469607	-0.064385	2.190962
341.528348	1569.555317	18.474611	-0.064366	2.185726
341.467633	1561.650396	18.479616	-0.064350	2.180525
341.446501	1553.694096	18.484621	-0.064341	2.175282
341.344664	1545.749142	18.489626	-0.064317	2.170027
341.409146	1537.785569	18.494631	-0.064323	2.164761
341.509493	1529.822539	18.499635	-0.064337	2.159487
341.534489	1521.905384	18.504640	-0.064336	2.154224
341.401583	1513.989767	18.509645	-0.064306	2.148933
341.367252	1506.046893	18.514650	-0.064295	2.143620
341.430546	1498.101049	18.519655	-0.064301	2.138302
341.160232	1490.199570	18.524659	-0.064246	2.132968
340.869457	1482.298304	18.529664	-0.064187	2.127619
341.071432	1474.326241	18.534669	-0.064219	2.122256
341.084172	1466.400399	18.539674	-0.064216	2.116892
340.918254	1458.455494	18.544679	-0.064180	2.111485
340.613664	1450.511532	18.549683	-0.064118	2.106050
340.907791	1442.536006	18.554688	-0.064168	2.100639
340.794969	1434.608322	18.559693	-0.064142	2.095207
340.858477	1426.668519	18.564698	-0.064148	2.089769
340.860494	1418.737419	18.569703	-0.064143	2.084317
340.774204	1410.834293	18.574707	-0.064122	2.078862
340.762885	1402.910759	18.579712	-0.064115	2.073385
340.697217	1394.983933	18.584717	-0.064097	2.067886
340.494049	1387.067647	18.589722	-0.064054	2.062366
340.528876	1379.141315	18.594727	-0.064056	2.056848
340.666511	1371.175998	18.599731	-0.064076	2.051299
340.572836	1363.256817	18.604736	-0.064054	2.045743
340.605120	1355.330859	18.609741	-0.064054	2.040180
340.490253	1347.440887	18.614746	-0.064028	2.034612
340.575940	1339.497012	18.619751	-0.064039	2.029012
340.359101	1331.564720	18.624755	-0.063993	2.023372
340.060297	1323.711621	18.629760	-0.063932	2.017765
339.949938	1315.776414	18.634765	-0.063907	2.012103
340.114407	1307.801370	18.639770	-0.063932	2.006425
340.012105	1299.906934	18.644775	-0.063908	2.000762
340.142388	1291.953588	18.649779	-0.063927	1.995064
340.183397	1284.035063	18.654784	-0.063929	1.989366
340.100506	1276.111269	18.659789	-0.063909	1.983634
339.895905	1268.222810	18.664794	-0.063865	1.977898
340.153453	1260.263918	18.669799	-0.063908	1.972144
339.893563	1252.370725	18.674803	-0.063855	1.966365
339.867564	1244.479885	18.679808	-0.063845	1.960596
339.944725	1236.561873	18.684813	-0.063854	1.954802
340.005948	1228.631261	18.689818	-0.063860	1.948979
339.790385	1220.715876	18.694823	-0.063815	1.943119
339.826422	1212.788236	18.699827	-0.063816	1.937261
339.955380	1204.846730	18.704832	-0.063835	1.931385
339.543706	1196.988412	18.709837	-0.063753	1.925492
339.472984	1189.076090	18.714842	-0.063735	1.919579
339.540284	1181.168281	18.719847	-0.063742	1.913667
339.620158	1173.223548	18.724851	-0.063752	1.907710
339.597456	1165.318708	18.729856	-0.063743	1.901753
339.373989	1157.431234	18.734861	-0.063696	1.895767
339.295982	1149.526713	18.739866	-0.063676	1.889766
339.408276	1141.608245	18.744871	-0.063692	1.883758
339.358754	1133.716549	18.749875	-0.063677	1.877731
339.405505	1125.811435	18.754880	-0.063681	1.871687
339.149709	1117.923731	18.759885	-0.063628	1.865600
338.653757	1110.094947	18.764890	-0.063531	1.859511
339.121117	1102.094260	18.769895	-0.063612	1.853383
339.170746	1094.167935	18.774899	-0.063617	1.847242
339.200766	1086.274906	18.779904	-0.063617	1.841105
338.907310	1078.436032	18.784909	-0.063557	1.834950
338.766062	1070.546071	18.789914	-0.063526	1.828753
338.814893	1062.630566	18.794919	-0.063530	1.822538
338.669026	1054.742854	18.799923	-0.063497	1.816300
338.817264	1046.824363	18.804928	-0.063520	1.810052
338.738955	1038.938736	18.809933	-0.063500	1.803780
338.753238	1031.058360	18.814938	-0.063498	1.797502
338.600909	1023.175628	18.819943	-0.063464	1.791180
338.499893	1015.258077	18.824947	-0.063440	1.784814
338.487816	1007.386692	18.829952	-0.063433	1.778473
338.483359	999.486436	18.834957	-0.063427	1.772087
338.490879	991.577206	18.839962	-0.063423	1.765672
338.359165	983.747726	18.844967	-0.063393	1.759281
338.316235	975.844002	18.849971	-0.063380	1.752818
338.408565	967.948020	18.854976	-0.063392	1.746354
338.330908	960.078293	18.859981	-0.063372	1.739866
337.924503	952.279064	18.864986	-0.063292	1.733369
338.056560	944.357976	18.869991	-0.063311	1.726817
338.324860	936.425837	18.874995	-0.063356	1.720248
338.024998	928.628416	18.880000	-0.063295	1.713692
337.947997	920.735612	18.885005	-0.063275	1.707060
337.705745	912.893344	18.890010	-0.063225	1.700423
337.978827	904.979826	18.895015	-0.063271	1.693769
337.838468	897.104989	18.900019	-0.063240	1.687066
337.796227	889.251442	18.905024	-0.063227	1.680367
337.877379	881.383184	18.910029	-0.063237	1.673645
337.926344	873.496747	18.915034	-0.063241	1.666877
337.833729	865.656475	18.920039	-0.063218	1.660101
337.696398	857.822460	18.925043	-0.063187	1.653297
337.677549	849.954747	18.930048	-0.063179	1.646452
337.398548	842.147562	18.935053	-0.063122	1.639594
337.389746	834.283660	18.940058	-0.063115	1.632696
337.327522	826.398000	18.945063	-0.063098	1.625742
337.293838	818.532339	18.950067	-0.063087	1.618780
337.191023	810.702118	18.955072	-0.063063	1.611809
337.192980	802.825587	18.960077	-0.063058	1.604782
337.295152	794.977079	18.965082	-0.063072	1.597763
337.188411	787.153459	18.970087	-0.063047	1.590706
337.113007	779.298558	18.975091	-0.063028	1.583593
337.221608	771.454709	18.980096	-0.063043	1.576486
336.787852	763.685284	18.985101	-0.062957	1.569334
337.007883	755.794138	18.990106	-0.062993	1.562134
336.706194	748.024309	18.995111	-0.062931	1.554935
336.898126	740.137352	19.000115	-0.062962	1.547668
336.836191	732.311633	19.005120	-0.062945	1.540386
336.837532	724.483592	19.010125	-0.062940	1.533076
336.390904	716.724439	19.015130	-0.062852	1.525728
336.210423	708.935576	19.020135	-0.062813	1.518357
336.386431	701.062185	19.025139	-0.062841	1.510925
336.644676	693.195961	19.030144	-0.062884	1.503475
336.247279	685.450393	19.035149	-0.062805	1.496002
336.036831	677.660653	19.040154	-0.062761	1.488478
336.169207	669.827801	19.045159	-0.062780	1.480928
336.195410	662.000138	19.050163	-0.062780	1.473328
335.875453	654.217664	19.055168	-0.062715	1.465676
336.037269	646.379531	19.060173	-0.062740	1.458008
335.832541	638.602021	19.065178	-0.062697	1.450300
335.882929	630.795673	19.070183	-0.062701	1.442563
335.542183	623.069719	19.075187	-0.062633	1.434800
335.874203	615.210853	19.080192	-0.062690	1.426974
336.056172	607.385900	19.085197	-0.062718	1.419113
335.702548	599.671370	19.090202	-0.062647	1.411231
335.897408	591.860887	19.095207	-0.062679	1.403299
335.815817	584.104735	19.100211	-0.062658	1.395331
335.920707	576.310397	19.105216	-0.062673	1.387310
336.001300	568.526953	19.110221	-0.062683	1.379249
335.777058	560.800943	19.115226	-0.062636	1.371147
335.483744	553.101001	19.120231	-0.062576	1.363013
335.348464	545.362086	19.125235	-0.062546	1.354817
335.502773	537.572990	19.130240	-0.062570	1.346568
335.299903	529.863611	19.135245	-0.062527	1.338291
335.183472	522.121175	19.140250	-0.062500	1.329941
335.265838	514.370152	19.145255	-0.062510	1.321566
335.144089	506.642353	19.150259	-0.062483	1.313125
335.157271	498.829743	19.155264	-0.062480	1.304561
335.238399	491.088168	19.160269	-0.062490	1.296032
335.041194	483.399290	19.165274	-0.062448	1.287453
335.124830	475.682264	19.170279	-0.062459	1.278838
334.937724	467.997315	19.175283	-0.062419	1.270149
334.927703	460.302112	19.180288	-0.062412	1.261422
334.842658	452.619410	19.185293	-0.062391	1.252635
334.657245	444.944725	19.190298	-0.062352	1.243775
334.698241	437.269281	19.195303	-0.062354	1.234895
334.694366	429.562122	19.200307	-0.062348	1.225904
334.463290	421.924775	19.205312	-0.062300	1.216884
334.218843	414.290196	19.210317	-0.062250	1.207797
334.254827	406.609472	19.215322	-0.062252	1.198643
334.324779	398.947117	19.220327	-0.062260	1.189448
334.191082	391.302442	19.225331	-0.062230	1.180161
334.334065	383.635485	19.230336	-0.062251	1.170830
334.369528	375.991268	19.235341	-0.062253	1.161430
334.211078	368.390154	19.240346	-0.062219	1.151965
334.190193	360.759900	19.245351	-0.062210	1.142415
333.994679	353.171752	19.250355	-0.062168	1.132799
334.048218	345.558086	19.255360	-0.062173	1.123124
333.955104	337.980013	19.260365	-0.062151	1.113378
334.040794	330.372016	19.265370	-0.062162	1.103546
333.827897	322.840361	19.270375	-0.062117	1.093659
333.634552	315.291373	19.275379	-0.062076	1.083663
333.737640	307.727643	19.280384	-0.062091	1.073623
333.432361	300.220143	19.285389	-0.062029	1.063468
333.264119	292.707153	19.290394	-0.061993	1.053241
333.489420	285.136401	19.295399	-0.062030	1.042927
333.205618	277.668113	19.300403	-0.061972	1.032530
333.072170	270.184274	19.305408	-0.061942	1.022042
333.053931	262.688619	19.310413	-0.061934	1.011457
332.861467	255.239709	19.315418	-0.061893	1.000783
332.956016	247.750471	19.320423	-0.061906	0.990008
332.762813	240.303096	19.325427	-0.061865	0.979103
332.918186	232.831104	19.330432	-0.061889	0.968128
332.834846	225.424799	19.335437	-0.061869	0.957063
332.560800	218.058082	19.340442	-0.061813	0.945879
332.443940	210.692703	19.345447	-0.061786	0.934604
332.277415	203.333067	19.350451	-0.061751	0.923188
332.398600	195.958193	19.355456	-0.061768	0.911683
332.204637	188.645444	19.360461	-0.061727	0.900043
332.150322	181.322336	19.365466	-0.061712	0.888273
331.928678	174.066419	19.370471	-0.061666	0.876406
331.676365	166.823044	19.375475	-0.061615	0.864389
331.629826	159.576105	19.380480	-0.061601	0.852256
331.291296	152.399467	19.385485	-0.061534	0.839981
331.213931	145.172382	19.390490	-0.061514	0.827516
331.072042	138.004462	19.395495	-0.061483	0.814944
331.106477	130.818685	19.400499	-0.061485	0.802199
330.771966	123.751498	19.405504	-0.061418	0.789345
330.599574	116.668153	19.410509	-0.061381	0.776301
330.558475	109.595974	19.415514	-0.061369	0.763100
330.396486	102.586901	19.420519	-0.061334	0.749745
329.795119	95.669180	19.425523	-0.061218	0.736173
329.522650	88.735453	19.430528	-0.061163	0.722431
329.276937	81.836880	19.435533	-0.061112	0.708503
328.680006	75.208542	19.440538	-0.060997	0.694725