Fri Apr 16 18:48:04 2021

Number of Points = 3636
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.932848	0.058661	0.000000	0.000040	0.310383

2.059545	0.031942	0.005005	0.000017	0.310366
1.843332	0.081824	0.010010	0.000057	0.310415
1.868487	0.022435	0.015014	0.000052	0.310159
2.222158	-0.041089	0.020019	-0.000014	0.310163
1.906337	0.016822	0.025024	0.000045	0.310165
1.834372	0.029438	0.030029	0.000058	0.310163
2.143823	-0.025663	0.035034	0.000001	0.310168
2.133308	-0.026973	0.040038	0.000003	0.310153
2.224375	-0.042325	0.045043	-0.000014	0.310159
2.146141	-0.027668	0.050048	0.000000	0.310161
2.040051	-0.009087	0.055053	0.000020	0.310158
2.085227	-0.015558	0.060058	0.000012	0.310166
1.974228	0.002116	0.065062	0.000033	0.310154
1.953964	0.007622	0.070067	0.000036	0.310163
1.941434	0.009598	0.075072	0.000039	0.310161
1.869498	0.013931	0.080077	0.000052	0.310120
2.027999	-0.072617	0.085082	0.000023	0.309851
2.028308	-0.074921	0.090086	0.000023	0.309840
1.933143	-0.056381	0.095091	0.000040	0.309846
1.975748	-0.063871	0.100096	0.000032	0.309847
1.854427	-0.044243	0.105101	0.000055	0.309836
1.890229	-0.048695	0.110106	0.000048	0.309845
1.883092	-0.083058	0.115110	0.000050	0.309679
2.081399	-0.153781	0.120115	0.000013	0.309517
1.970106	-0.134219	0.125120	0.000033	0.309514
1.857792	-0.115207	0.130125	0.000054	0.309507
2.089120	-0.155495	0.135130	0.000011	0.309515
1.913407	-0.155370	0.140134	0.000044	0.309367
1.816511	-0.166009	0.145139	0.000062	0.309234
1.495665	-0.105826	0.150144	0.000122	0.309243
1.624106	-0.131246	0.155149	0.000098	0.309233
1.828636	-0.166605	0.160154	0.000060	0.309242
1.592604	-0.197302	0.165158	0.000104	0.308897
1.537622	-0.186395	0.170163	0.000114	0.308902
1.644552	-0.205694	0.175168	0.000094	0.308902
1.740672	-0.227840	0.180173	0.000076	0.308880
2.051326	-0.347704	0.185178	0.000018	0.308583
1.823839	-0.308319	0.190182	0.000061	0.308574
1.731433	-0.290222	0.195187	0.000078	0.308580
1.744070	-0.334229	0.200192	0.000076	0.308384
1.579678	-0.331105	0.205197	0.000106	0.308259
1.781930	-0.366996	0.210202	0.000069	0.308263
1.691261	-0.377277	0.215206	0.000086	0.308137
1.717956	-0.416468	0.220211	0.000081	0.307976
1.675880	-0.408565	0.225216	0.000088	0.307977
1.659548	-0.441179	0.230221	0.000092	0.307810
1.819951	-0.507832	0.235226	0.000062	0.307633
1.862860	-0.517834	0.240230	0.000054	0.307623
1.769380	-0.548542	0.245235	0.000071	0.307399
1.798515	-0.571751	0.250240	0.000066	0.307314
1.704676	-0.567145	0.255245	0.000083	0.307256
1.810584	-0.642454	0.260250	0.000064	0.306992
1.705192	-0.624873	0.265254	0.000083	0.306984
1.888482	-0.699597	0.270259	0.000049	0.306789
1.869316	-0.714073	0.275264	0.000053	0.306704
1.780962	-0.727260	0.280269	0.000069	0.306566
1.785361	-0.769729	0.285274	0.000068	0.306369
1.562656	-0.738100	0.290278	0.000110	0.306328
1.691793	-0.818216	0.295283	0.000086	0.306060
1.660958	-0.812786	0.300288	0.000092	0.306059
1.557464	-0.858496	0.305293	0.000111	0.305754
1.637606	-0.875618	0.310298	0.000096	0.305742
1.417311	-0.879421	0.315302	0.000137	0.305534
1.620168	-0.927208	0.320307	0.000099	0.305482
1.493305	-0.956045	0.325312	0.000123	0.305237
1.358711	-0.952331	0.330317	0.000148	0.305138
1.339645	-0.993538	0.335322	0.000152	0.304926
1.226928	-0.994074	0.340326	0.000173	0.304827
1.314986	-1.059096	0.345331	0.000156	0.304594
1.097327	-1.039583	0.350336	0.000197	0.304499
0.911096	-1.050791	0.355341	0.000231	0.304284
1.161052	-1.110043	0.360346	0.000185	0.304219
1.041103	-1.147446	0.365350	0.000207	0.303937
0.900377	-1.132186	0.370355	0.000233	0.303888
0.888995	-1.190620	0.375360	0.000236	0.303600
0.871418	-1.198700	0.380365	0.000239	0.303546
0.679655	-1.225375	0.385370	0.000275	0.303252
0.720714	-1.245926	0.390374	0.000267	0.303190
0.642712	-1.278812	0.395379	0.000282	0.302965
0.473335	-1.273919	0.400384	0.000313	0.302842
0.719902	-1.366055	0.405389	0.000267	0.302615
0.446102	-1.352410	0.410394	0.000318	0.302443
0.501405	-1.391371	0.415398	0.000308	0.302304
0.349611	-1.421146	0.420403	0.000336	0.302030
0.481936	-1.463437	0.425408	0.000312	0.301942
0.387888	-1.500183	0.430413	0.000329	0.301684
0.437860	-1.539107	0.435418	0.000320	0.301541
0.056951	-1.507908	0.440422	0.000391	0.301358
0.376672	-1.615243	0.445427	0.000331	0.301122
0.200132	-1.607302	0.450432	0.000364	0.301006
-0.180969	-1.595960	0.455437	0.000435	0.300727
-0.040085	-1.643385	0.460442	0.000409	0.300622
-0.203642	-1.641430	0.465446	0.000439	0.300489
-0.168564	-1.706446	0.470451	0.000433	0.300206
-0.692765	-1.633876	0.475456	0.000531	0.300097
-0.699461	-1.687605	0.480461	0.000532	0.299832
-0.783636	-1.706359	0.485466	0.000548	0.299667
-0.973656	-1.705406	0.490470	0.000583	0.299505
-0.859755	-1.777670	0.495475	0.000562	0.299256
-0.739603	-1.826264	0.500480	0.000539	0.299126
-0.931819	-1.843612	0.505485	0.000575	0.298873
-1.081782	-1.857365	0.510490	0.000603	0.298675
-1.507999	-1.806078	0.515494	0.000683	0.298548
-1.737047	-1.825977	0.520499	0.000725	0.298249
-1.585779	-1.876397	0.525504	0.000697	0.298138
-1.633941	-1.905433	0.530509	0.000706	0.297955
-1.823756	-1.923740	0.535514	0.000741	0.297698
-2.097134	-1.899781	0.540518	0.000792	0.297573
-2.045449	-1.964085	0.545523	0.000783	0.297306
-1.898555	-2.027765	0.550528	0.000755	0.297126
-2.444611	-1.959395	0.555533	0.000857	0.296975
-2.572765	-1.989842	0.560538	0.000881	0.296713
-2.626997	-2.006387	0.565542	0.000891	0.296585
-2.854800	-2.011302	0.570547	0.000933	0.296359
-2.982180	-2.030948	0.575552	0.000957	0.296149
-3.414718	-1.973713	0.580557	0.001038	0.296045
-3.382676	-2.041741	0.585562	0.001032	0.295741
-3.508470	-2.037015	0.590566	0.001055	0.295652
-4.040739	-1.974133	0.595571	0.001154	0.295486
-3.789229	-2.062211	0.600576	0.001108	0.295279
-4.131849	-2.027148	0.605581	0.001171	0.295145
-4.422796	-2.032335	0.610586	0.001225	0.294860
-4.941146	-1.953063	0.615590	0.001322	0.294787
-4.941741	-2.009508	0.620595	0.001322	0.294509
-4.844341	-2.047155	0.625600	0.001304	0.294411
-5.620904	-1.946502	0.630605	0.001449	0.294212
-5.280621	-2.041862	0.635610	0.001385	0.294047
-5.606621	-2.017226	0.640614	0.001446	0.293877
-5.997147	-1.989058	0.645619	0.001519	0.293666
-6.290642	-1.955014	0.650624	0.001573	0.293571
-6.150708	-2.030641	0.655629	0.001547	0.293323
-6.218445	-2.032011	0.660634	0.001560	0.293256
-6.884256	-1.964660	0.665638	0.001684	0.292991
-6.730682	-1.998160	0.670643	0.001655	0.292963
-6.858102	-2.038144	0.675648	0.001679	0.292651
-7.268480	-1.970631	0.680653	0.001755	0.292616
-7.396732	-2.006959	0.685658	0.001779	0.292321
-7.437039	-2.002824	0.690662	0.001787	0.292305
-7.625177	-2.032510	0.695667	0.001822	0.291988
-7.876376	-1.986812	0.700672	0.001869	0.291988
-8.139136	-1.996928	0.705677	0.001918	0.291701
-8.178957	-1.989709	0.710682	0.001925	0.291701
-8.712294	-1.956668	0.715686	0.002024	0.291384
-8.762395	-1.952141	0.720691	0.002034	0.291361
-8.399109	-2.066207	0.725696	0.001966	0.291123
-9.282852	-1.919917	0.730701	0.002130	0.291051
-9.189358	-1.977595	0.735706	0.002113	0.290849
-9.529118	-1.936429	0.740710	0.002176	0.290746
-9.526215	-1.963250	0.745715	0.002176	0.290615
-9.586302	-1.977707	0.750720	0.002187	0.290489
-9.985318	-1.924807	0.755725	0.002261	0.290391
-10.247831	-1.923200	0.760730	0.002310	0.290161
-10.287426	-1.922374	0.765734	0.002318	0.290129
-10.462587	-1.950877	0.770739	0.002350	0.289828
-9.934129	-2.047681	0.775744	0.002252	0.289824
-10.527977	-1.998022	0.780749	0.002362	0.289533
-10.689767	-1.974922	0.785754	0.002393	0.289502
-11.099985	-1.936262	0.790758	0.002469	0.289322
-11.096929	-1.959983	0.795763	0.002468	0.289206
-11.113617	-1.978815	0.800768	0.002471	0.289097
-11.669436	-1.922207	0.805773	0.002575	0.288874
-11.396253	-1.972659	0.810778	0.002524	0.288870
-11.934879	-1.934928	0.815782	0.002624	0.288568
-11.776627	-1.965170	0.820787	0.002595	0.288561
-11.711810	-2.020120	0.825792	0.002583	0.288344
-12.174416	-1.957619	0.830797	0.002669	0.288236
-12.366875	-1.942993	0.835802	0.002705	0.288134
-12.524883	-1.950666	0.840806	0.002734	0.287951
-12.283918	-1.999056	0.845811	0.002689	0.287928
-12.740515	-1.978674	0.850816	0.002774	0.287613
-13.027532	-1.927975	0.855821	0.002828	0.287605
-12.731018	-2.022016	0.860826	0.002773	0.287403
-13.272997	-1.945052	0.865830	0.002874	0.287294
-13.373961	-1.947986	0.870835	0.002892	0.287187
-13.320329	-1.999810	0.875840	0.002882	0.286975
-13.426231	-1.982378	0.880845	0.002902	0.286966
-13.630524	-1.997924	0.885850	0.002940	0.286700
-13.923562	-1.948340	0.890854	0.002995	0.286681
-14.021864	-1.965542	0.895859	0.003013	0.286504
-14.549603	-1.898176	0.900864	0.003111	0.286360
-14.464339	-1.917432	0.905869	0.003095	0.286341
-14.330140	-1.999352	0.910874	0.003071	0.286050
-14.719054	-1.930126	0.915878	0.003143	0.286042
-14.903690	-1.931094	0.920883	0.003177	0.285867
-14.689412	-1.997190	0.925888	0.003137	0.285730
-15.038960	-1.940118	0.930893	0.003202	0.285697
-15.190449	-1.955892	0.935898	0.003231	0.285478
-15.119961	-1.969522	0.940902	0.003218	0.285473
-15.224462	-1.995028	0.945907	0.003237	0.285248
-15.701707	-1.928860	0.950912	0.003326	0.285143
-15.905411	-1.900968	0.955917	0.003364	0.285097
-15.729641	-1.986896	0.960922	0.003331	0.284822
-15.977820	-1.943087	0.965926	0.003377	0.284816
-16.366628	-1.911696	0.970931	0.003450	0.284616
-16.105799	-1.982428	0.975936	0.003401	0.284497
-16.430213	-1.930130	0.980941	0.003462	0.284463
-16.699692	-1.929312	0.985946	0.003512	0.284218
-16.652371	-1.940608	0.990950	0.003503	0.284204
-16.586565	-1.988263	0.995955	0.003491	0.284022
-17.118663	-1.919945	1.000960	0.003590	0.283878
-17.320270	-1.884942	1.005965	0.003627	0.283869
-17.311454	-1.941219	1.010970	0.003626	0.283590
-17.667769	-1.880127	1.015974	0.003692	0.283571
-17.688610	-1.895191	1.020979	0.003696	0.283475
-17.630789	-1.949695	1.025984	0.003685	0.283250
-17.770656	-1.927112	1.030989	0.003711	0.283236
-17.800686	-1.960796	1.035994	0.003717	0.283036
-18.057344	-1.930949	1.040998	0.003765	0.282949
-17.835977	-1.984800	1.046003	0.003723	0.282880
-18.437896	-1.926962	1.051008	0.003835	0.282616
-18.549013	-1.909303	1.056013	0.003856	0.282603
-18.297285	-1.988291	1.061018	0.003809	0.282432
-18.735859	-1.935500	1.066022	0.003891	0.282294
-18.783940	-1.928092	1.071027	0.003900	0.282287
-18.862967	-1.974788	1.076032	0.003915	0.281974
-19.236367	-1.905295	1.081037	0.003984	0.281982
-19.296237	-1.916453	1.086042	0.003995	0.281869
-19.638112	-1.890177	1.091046	0.004059	0.281685
-19.379687	-1.936412	1.096051	0.004011	0.281688
-19.506710	-1.960902	1.101056	0.004035	0.281444
-19.852040	-1.916952	1.106061	0.004099	0.281347
-19.495931	-1.990297	1.111066	0.004033	0.281303
-20.050637	-1.939325	1.116070	0.004136	0.281046
-20.259770	-1.900373	1.121075	0.004175	0.281050
-19.860821	-2.007554	1.126080	0.004101	0.280872
-20.302532	-1.956684	1.131085	0.004183	0.280720
-20.326210	-1.952722	1.136090	0.004187	0.280718
-20.624988	-1.943752	1.141094	0.004243	0.280484
-20.199691	-2.020383	1.146099	0.004164	0.280488
-20.441903	-2.010391	1.151104	0.004209	0.280312
-20.982237	-1.944984	1.156109	0.004309	0.280142
-20.757350	-1.984636	1.161114	0.004267	0.280149
-21.187545	-1.966204	1.166118	0.004348	0.279840
-21.553146	-1.899899	1.171123	0.004416	0.279839
-21.246984	-1.980781	1.176128	0.004359	0.279708
-21.456836	-1.981844	1.181133	0.004398	0.279505
-21.522361	-1.967849	1.186138	0.004410	0.279516
-22.103817	-1.912475	1.191142	0.004518	0.279255
-21.978053	-1.942403	1.196147	0.004495	0.279218
-21.917673	-1.968449	1.201152	0.004484	0.279140
-22.681190	-1.880535	1.206157	0.004626	0.278876
-22.353891	-1.937734	1.211162	0.004565	0.278888
-22.338157	-1.975816	1.216166	0.004562	0.278705
-22.961048	-1.887877	1.221171	0.004678	0.278573
-22.544554	-1.964685	1.226176	0.004600	0.278568
-22.778904	-1.981650	1.231181	0.004644	0.278258
-22.856053	-1.968176	1.236186	0.004658	0.278255
-23.262069	-1.915669	1.241190	0.004734	0.278144
-23.218565	-1.959125	1.246195	0.004726	0.277959
-22.966762	-2.003534	1.251200	0.004679	0.277966
-23.674557	-1.930171	1.256205	0.004811	0.277678
-23.882242	-1.900846	1.261210	0.004849	0.277634
-23.637581	-1.955486	1.266214	0.004804	0.277581
-23.884418	-1.962376	1.271219	0.004850	0.277311
-24.226251	-1.899359	1.276224	0.004913	0.277315
-24.393262	-1.898716	1.281229	0.004945	0.277160
-24.289689	-1.950420	1.286234	0.004925	0.276988
-24.324786	-1.945448	1.291238	0.004932	0.276981
-24.554584	-1.949515	1.296243	0.004975	0.276741
-24.591908	-1.952014	1.301248	0.004982	0.276692
-24.780058	-1.931386	1.306253	0.005017	0.276621
-24.959257	-1.947582	1.311258	0.005050	0.276366
-24.869557	-1.965472	1.316262	0.005033	0.276357
-25.088426	-1.961206	1.321267	0.005074	0.276171
-25.605057	-1.888516	1.326272	0.005170	0.276060
-25.499086	-1.908534	1.331277	0.005151	0.276056
-25.204861	-2.014713	1.336282	0.005096	0.275779
-25.989535	-1.879685	1.341286	0.005242	0.275739
-25.963883	-1.895950	1.346291	0.005237	0.275678
-25.825334	-1.953593	1.351296	0.005211	0.275508
-26.138443	-1.899674	1.356301	0.005270	0.275492
-26.076754	-1.949622	1.361306	0.005258	0.275288
-26.493244	-1.898684	1.366310	0.005336	0.275158
-26.118824	-1.968008	1.371315	0.005266	0.275151
-26.614255	-1.935928	1.376320	0.005358	0.274846
-26.955129	-1.875882	1.381325	0.005422	0.274835
-26.481731	-1.982598	1.386330	0.005334	0.274727
-27.068395	-1.917764	1.391334	0.005443	0.274506
-26.977572	-1.934464	1.396339	0.005426	0.274505
-27.099779	-1.950042	1.401344	0.005449	0.274305
-27.446066	-1.903987	1.406349	0.005513	0.274216
-27.285812	-1.937486	1.411354	0.005483	0.274193
-27.608391	-1.937647	1.416358	0.005543	0.273882
-27.632031	-1.933424	1.421363	0.005548	0.273882
-27.749690	-1.938203	1.426368	0.005570	0.273743
-28.349497	-1.860971	1.431373	0.005681	0.273575
-27.680022	-1.981578	1.436378	0.005557	0.273581
-28.474644	-1.885862	1.441382	0.005705	0.273322
-28.600302	-1.875549	1.446387	0.005728	0.273256
-28.110440	-1.970638	1.451392	0.005637	0.273224
-28.606092	-1.929677	1.456397	0.005729	0.272963
-28.748472	-1.902171	1.461402	0.005756	0.272972
-29.006667	-1.884311	1.466406	0.005804	0.272818
-29.006255	-1.919455	1.471411	0.005804	0.272631
-29.116105	-1.899039	1.476416	0.005824	0.272634
-29.598025	-1.859152	1.481421	0.005914	0.272380
-29.388325	-1.908399	1.486426	0.005875	0.272321
-29.395233	-1.912716	1.491430	0.005876	0.272291
-29.630580	-1.927586	1.496435	0.005920	0.271984
-29.569078	-1.937429	1.501440	0.005909	0.271991
-29.780063	-1.925294	1.506445	0.005948	0.271852
-30.046150	-1.905533	1.511450	0.005997	0.271699
-29.934695	-1.926388	1.516454	0.005977	0.271696
-29.850681	-1.992583	1.521459	0.005961	0.271424
-30.254178	-1.929836	1.526464	0.006036	0.271368
-30.493512	-1.900275	1.531469	0.006081	0.271293
-30.221407	-1.992687	1.536474	0.006030	0.271064
-30.550952	-1.934014	1.541478	0.006091	0.271057
-30.864962	-1.917965	1.546483	0.006150	0.270838
-30.728079	-1.960325	1.551488	0.006124	0.270744
-30.798942	-1.953805	1.556493	0.006138	0.270710
-31.065342	-1.945553	1.561498	0.006187	0.270495
-31.291042	-1.905986	1.566502	0.006229	0.270487
-31.164259	-1.962975	1.571507	0.006206	0.270305
-31.594334	-1.913419	1.576512	0.006286	0.270152
-31.776328	-1.881584	1.581517	0.006320	0.270145
-31.447078	-1.994501	1.586522	0.006258	0.269860
-31.876692	-1.923129	1.591526	0.006338	0.269824
-31.967249	-1.928113	1.596531	0.006355	0.269709
-32.336118	-1.899213	1.601536	0.006424	0.269504
-32.347936	-1.898442	1.606541	0.006426	0.269496
-32.582158	-1.888572	1.611546	0.006470	0.269320
-32.841627	-1.858545	1.616550	0.006518	0.269228
-32.914840	-1.844887	1.621555	0.006532	0.269230
-33.237714	-1.843235	1.626560	0.006592	0.268923
-33.451482	-1.810724	1.631565	0.006631	0.268888
-33.015913	-1.897532	1.636570	0.006550	0.268848
-33.514358	-1.857477	1.641574	0.006643	0.268575
-33.409614	-1.877270	1.646579	0.006624	0.268571
-33.208127	-1.937915	1.651584	0.006586	0.268441
-33.442692	-1.932801	1.656589	0.006630	0.268239
-33.565730	-1.907222	1.661594	0.006653	0.268256
-34.153853	-1.846518	1.666598	0.006762	0.268006
-33.757347	-1.927285	1.671603	0.006689	0.267959
-33.621080	-1.967362	1.676608	0.006663	0.267877
-34.378944	-1.877928	1.681613	0.006804	0.267615
-33.981784	-1.949224	1.686618	0.006730	0.267620
-34.650207	-1.863433	1.691622	0.006855	0.267426
-35.135157	-1.794416	1.696627	0.006945	0.267322
-34.460789	-1.917090	1.701632	0.006820	0.267322
-35.090021	-1.860892	1.706637	0.006937	0.267006
-35.314255	-1.820946	1.711642	0.006978	0.267002
-35.161420	-1.860245	1.716646	0.006950	0.266939
-35.428298	-1.854071	1.721651	0.007000	0.266709
-35.329479	-1.870834	1.726656	0.006981	0.266716
-36.098716	-1.758101	1.731661	0.007124	0.266568
-35.547900	-1.893581	1.736666	0.007022	0.266376
-36.110239	-1.789366	1.741670	0.007127	0.266387
-36.099055	-1.835259	1.746675	0.007125	0.266148
-36.022159	-1.866380	1.751680	0.007110	0.266055
-35.737892	-1.923155	1.756685	0.007057	0.266027
-35.922023	-1.942937	1.761690	0.007092	0.265737
-36.560216	-1.826718	1.766694	0.007210	0.265738
-36.336068	-1.890800	1.771699	0.007169	0.265611
-36.627511	-1.860954	1.776704	0.007223	0.265484
-36.732539	-1.844288	1.781709	0.007243	0.265471
-36.639533	-1.908730	1.786714	0.007225	0.265212
-36.980850	-1.860331	1.791718	0.007289	0.265137
-37.119135	-1.848060	1.796723	0.007315	0.265067
-37.039567	-1.907319	1.801728	0.007300	0.264822
-37.080677	-1.902331	1.806733	0.007307	0.264808
-37.002572	-1.954870	1.811738	0.007293	0.264598
-37.393664	-1.905428	1.816742	0.007366	0.264480
-37.433115	-1.904701	1.821747	0.007373	0.264444
-37.309304	-1.971443	1.826752	0.007350	0.264202
-37.893009	-1.866784	1.831757	0.007459	0.264194
-37.619973	-1.954003	1.836762	0.007408	0.263988
-37.999280	-1.908854	1.841766	0.007479	0.263857
-38.108763	-1.895706	1.846771	0.007499	0.263820
-38.301970	-1.908636	1.851776	0.007535	0.263555
-38.456583	-1.881450	1.856781	0.007564	0.263550
-38.047125	-1.989353	1.861786	0.007488	0.263367
-38.613218	-1.912793	1.866790	0.007593	0.263221
-38.510133	-1.937402	1.871795	0.007574	0.263189
-38.524701	-1.980130	1.876800	0.007576	0.262939
-39.052382	-1.886299	1.881805	0.007675	0.262927
-39.009808	-1.929918	1.886810	0.007667	0.262730
-39.174342	-1.923697	1.891814	0.007697	0.262599
-38.867011	-1.990587	1.896819	0.007640	0.262538
-39.343565	-1.949621	1.901824	0.007729	0.262286
-39.417767	-1.937990	1.906829	0.007743	0.262275
-39.433287	-1.975955	1.911834	0.007746	0.262050
-39.950319	-1.898949	1.916838	0.007842	0.261956
-39.795765	-1.939439	1.921843	0.007813	0.261887
-39.662787	-2.001568	1.926848	0.007788	0.261677
-40.128379	-1.918875	1.931853	0.007875	0.261666
-40.284925	-1.936171	1.936858	0.007904	0.261413
-40.321559	-1.941349	1.941862	0.007911	0.261347
-40.791513	-1.871694	1.946867	0.007999	0.261259
-40.953356	-1.881976	1.951872	0.008029	0.261039
-40.937592	-1.885684	1.956877	0.008026	0.261034
-40.673293	-1.972668	1.961882	0.007977	0.260818
-41.161797	-1.902742	1.966886	0.008068	0.260713
-41.351833	-1.874786	1.971891	0.008103	0.260676
-41.067045	-1.962420	1.976896	0.008050	0.260477
-41.435400	-1.896927	1.981901	0.008118	0.260469
-41.676620	-1.890705	1.986906	0.008163	0.260259
-41.970898	-1.859330	1.991910	0.008218	0.260136
-41.754172	-1.904507	1.996915	0.008178	0.260104
-42.220558	-1.869957	2.001920	0.008265	0.259824

-42.125506	-1.926573	2.011917	0.008247	0.259604
-42.330734	-1.916415	2.021914	0.008285	0.259453
-42.600117	-1.912231	2.031910	0.008335	0.259202
-42.776937	-1.901904	2.041907	0.008368	0.259080
-43.341943	-1.835402	2.051904	0.008473	0.258877
-43.299833	-1.841269	2.061901	0.008466	0.258887
-43.748792	-1.811529	2.071898	0.008549	0.258596
-43.533396	-1.856426	2.081894	0.008509	0.258564
-43.551741	-1.853930	2.091891	0.008513	0.258559
-43.916532	-1.785497	2.101888	0.008581	0.258571
-43.720742	-1.870414	2.111885	0.008544	0.258295
-44.212062	-1.788874	2.121882	0.008636	0.258251
-44.004594	-1.828407	2.131878	0.008597	0.258240
-43.812026	-1.863992	2.141875	0.008561	0.258237
-43.964402	-1.835683	2.151872	0.008589	0.258241
-43.578570	-1.906989	2.161869	0.008518	0.258234
-43.746223	-1.875786	2.171866	0.008549	0.258238
-43.509649	-1.919561	2.181862	0.008505	0.258234
-43.834272	-1.860504	2.191859	0.008565	0.258234
-43.678272	-1.890244	2.201856	0.008536	0.258226
-43.265466	-1.915206	2.211853	0.008459	0.258507
-43.249442	-1.910408	2.221850	0.008456	0.258550
-43.381203	-1.886738	2.231846	0.008481	0.258549
-43.548302	-1.854536	2.241843	0.008512	0.258559
-43.516430	-1.860182	2.251840	0.008506	0.258560
-43.251149	-1.869181	2.261837	0.008457	0.258779
-43.408800	-1.823285	2.271834	0.008486	0.258876
-43.335414	-1.835376	2.281830	0.008473	0.258883
-43.442185	-1.779072	2.291827	0.008492	0.259089
-43.248632	-1.790728	2.301824	0.008456	0.259220
-43.293756	-1.774389	2.311821	0.008465	0.259266
-42.872579	-1.807409	2.321818	0.008386	0.259509
-42.772069	-1.827043	2.331814	0.008368	0.259502
-42.822841	-1.771063	2.341811	0.008377	0.259762
-42.865519	-1.748812	2.351808	0.008385	0.259843
-43.001435	-1.675499	2.361805	0.008410	0.260114
-42.574733	-1.745305	2.371802	0.008331	0.260157
-41.684987	-1.850103	2.381798	0.008165	0.260475
-41.903406	-1.807506	2.391795	0.008206	0.260490
-41.568572	-1.829364	2.401792	0.008144	0.260707
-41.371049	-1.862375	2.411789	0.008107	0.260724
-41.258899	-1.829123	2.421786	0.008086	0.261021
-41.059236	-1.858935	2.431782	0.008049	0.261058
-41.225611	-1.774948	2.441779	0.008080	0.261355
-40.943463	-1.806441	2.451776	0.008027	0.261465
-40.719237	-1.807154	2.461773	0.007986	0.261687
-40.823290	-1.753586	2.471770	0.008005	0.261879
-40.357329	-1.816798	2.481766	0.007918	0.261998
-40.354978	-1.761779	2.491763	0.007918	0.262304
-39.713894	-1.854609	2.501760	0.007798	0.262435
-39.354022	-1.889200	2.511757	0.007731	0.262606
-39.276077	-1.856736	2.521754	0.007717	0.262863
-39.413633	-1.807336	2.531750	0.007742	0.262997
-39.042939	-1.831415	2.541747	0.007673	0.263235
-38.656217	-1.870397	2.551744	0.007602	0.263408
-38.485081	-1.873892	2.561741	0.007570	0.263560
-38.445416	-1.828055	2.571738	0.007562	0.263851
-38.052829	-1.871359	2.581734	0.007489	0.264005
-37.842666	-1.873343	2.591731	0.007450	0.264204
-37.322325	-1.925647	2.601728	0.007353	0.264436
-37.667677	-1.838802	2.611725	0.007417	0.264567
-36.979494	-1.918248	2.621722	0.007289	0.264818
-37.049741	-1.864732	2.631718	0.007302	0.265040
-36.850978	-1.873509	2.641715	0.007265	0.265190
-36.339257	-1.913630	2.651712	0.007170	0.265479
-36.373924	-1.875911	2.661709	0.007177	0.265650
-36.084664	-1.902659	2.671706	0.007123	0.265791
-36.036633	-1.861520	2.681702	0.007114	0.266062
-35.685174	-1.885378	2.691699	0.007048	0.266280
-35.501735	-1.885449	2.701696	0.007014	0.266461
-35.074482	-1.919635	2.711693	0.006935	0.266698
-34.872254	-1.914036	2.721690	0.006897	0.266928
-35.063848	-1.845933	2.731686	0.006933	0.267108
-34.501960	-1.911746	2.741683	0.006828	0.267305
-34.491772	-1.856636	2.751680	0.006826	0.267613
-34.323312	-1.848973	2.761677	0.006795	0.267821
-34.094467	-1.850458	2.771674	0.006752	0.268037
-33.952261	-1.836601	2.781670	0.006726	0.268252
-33.425492	-1.879743	2.791667	0.006628	0.268536
-33.247653	-1.876023	2.801664	0.006595	0.268730
-32.968789	-1.891167	2.811661	0.006543	0.268922
-32.705376	-1.883297	2.821658	0.006494	0.269222
-32.224963	-1.933055	2.831654	0.006404	0.269424
-32.401730	-1.866592	2.841651	0.006437	0.269609
-32.176308	-1.866218	2.851648	0.006395	0.269831
-31.626851	-1.906657	2.861645	0.006293	0.270150
-31.504444	-1.888781	2.871642	0.006270	0.270365
-31.336195	-1.884645	2.881638	0.006239	0.270551
-31.127160	-1.886343	2.891635	0.006200	0.270745
-30.870017	-1.878541	2.901632	0.006152	0.271037
-30.476880	-1.914410	2.911629	0.006079	0.271227
-30.118572	-1.944608	2.921626	0.006012	0.271413
-30.051839	-1.903040	2.931622	0.006000	0.271700
-29.762264	-1.913051	2.941619	0.005946	0.271927
-29.597802	-1.905802	2.951616	0.005915	0.272125
-29.206753	-1.938875	2.961613	0.005842	0.272327
-29.032268	-1.913851	2.971610	0.005810	0.272628
-28.710151	-1.929673	2.981606	0.005750	0.272855
-28.647304	-1.902501	2.991603	0.005738	0.273060
-28.489160	-1.892740	3.001600	0.005709	0.273264
-28.251995	-1.876726	3.011597	0.005665	0.273577
-27.856539	-1.908051	3.021594	0.005591	0.273792
-28.016532	-1.835597	3.031590	0.005621	0.274021
-27.512132	-1.884462	3.041587	0.005527	0.274248
-27.251859	-1.880864	3.051584	0.005479	0.274516
-26.925501	-1.894228	3.061581	0.005418	0.274759
-26.455134	-1.940418	3.071578	0.005330	0.274966
-26.577497	-1.877302	3.081574	0.005353	0.275181
-26.133995	-1.897797	3.091571	0.005270	0.275497
-26.047442	-1.879473	3.101568	0.005254	0.275676
-25.730029	-1.898627	3.111565	0.005195	0.275878
-25.401392	-1.918716	3.121562	0.005134	0.276087
-25.323660	-1.879566	3.131558	0.005120	0.276366
-24.906418	-1.905249	3.141555	0.005042	0.276629
-24.792850	-1.887703	3.151552	0.005021	0.276828
-24.370063	-1.925678	3.161549	0.004942	0.277032
-24.240510	-1.895802	3.171546	0.004918	0.277311
-24.158332	-1.860366	3.181542	0.004903	0.277574
-23.660912	-1.904878	3.191539	0.004810	0.277813
-23.571598	-1.881034	3.201536	0.004793	0.278022
-23.161029	-1.911345	3.211533	0.004717	0.278253
-23.018577	-1.881276	3.221530	0.004690	0.278544
-22.616060	-1.913857	3.231526	0.004616	0.278755
-22.638289	-1.865975	3.241523	0.004620	0.278982
-22.421687	-1.858135	3.251520	0.004579	0.279227
-22.214042	-1.837840	3.261517	0.004541	0.279528
-22.274309	-1.780122	3.271514	0.004552	0.279770
-21.603952	-1.855324	3.281510	0.004427	0.280011
-21.337635	-1.860440	3.291507	0.004378	0.280235
-21.058226	-1.858987	3.301504	0.004325	0.280505
-20.930100	-1.839164	3.311501	0.004302	0.280727
-20.750499	-1.827350	3.321498	0.004268	0.280956
-20.377878	-1.851135	3.331494	0.004199	0.281183
-20.184403	-1.844281	3.341491	0.004163	0.281399
-20.177551	-1.786055	3.351488	0.004162	0.281705
-19.650161	-1.830502	3.361485	0.004063	0.281969
-19.375190	-1.838754	3.371482	0.004012	0.282183
-19.027335	-1.857814	3.381478	0.003947	0.282410
-18.819605	-1.852077	3.391475	0.003909	0.282632
-18.245506	-1.895617	3.401472	0.003802	0.282944
-18.233104	-1.856828	3.411469	0.003800	0.283154
-18.204905	-1.817388	3.421466	0.003794	0.283381
-17.701575	-1.866052	3.431462	0.003701	0.283600
-17.510216	-1.846800	3.441459	0.003665	0.283876
-17.173006	-1.855958	3.451456	0.003602	0.284141
-16.868180	-1.872643	3.461453	0.003545	0.284339
-16.828980	-1.837981	3.471450	0.003538	0.284551
-16.562216	-1.830330	3.481446	0.003488	0.284837
-16.428269	-1.802353	3.491443	0.003464	0.285102
-15.682947	-1.893110	3.501440	0.003325	0.285330
-15.762291	-1.835404	3.511437	0.003340	0.285549
-15.630341	-1.819743	3.521434	0.003315	0.285750
-15.155466	-1.849521	3.531430	0.003227	0.286036
-14.912558	-1.853671	3.541427	0.003181	0.286238
-14.597485	-1.869248	3.551424	0.003123	0.286449
-14.175067	-1.897693	3.561421	0.003044	0.286693
-14.076353	-1.863291	3.571418	0.003026	0.286957
-13.544843	-1.919684	3.581414	0.002927	0.287160
-13.441464	-1.903618	3.591411	0.002908	0.287336
-13.042132	-1.920818	3.601408	0.002833	0.287615
-12.941508	-1.888560	3.611405	0.002814	0.287869
-12.442637	-1.943842	3.621402	0.002722	0.288047
-12.253335	-1.937349	3.631398	0.002686	0.288252
-11.904865	-1.945735	3.641395	0.002622	0.288528
-11.824755	-1.924655	3.651392	0.002607	0.288707
-11.469051	-1.953695	3.661389	0.002540	0.288885
-11.190632	-1.939003	3.671386	0.002489	0.289212
-10.918146	-1.955602	3.681382	0.002438	0.289377
-11.172114	-1.870280	3.691379	0.002485	0.289573
-10.469138	-1.946474	3.701376	0.002354	0.289830
-10.350949	-1.917156	3.711373	0.002332	0.290084
-9.854239	-1.969505	3.721370	0.002240	0.290273
-9.882314	-1.920725	3.731366	0.002245	0.290491
-9.504700	-1.942194	3.741363	0.002175	0.290726
-9.356662	-1.931585	3.751360	0.002147	0.290912
-9.036687	-1.951931	3.761357	0.002088	0.291100
-8.749587	-1.951642	3.771354	0.002034	0.291361
-8.548616	-1.940156	3.781350	0.001997	0.291599
-8.608768	-1.891842	3.791347	0.002008	0.291785
-8.116344	-1.941405	3.801344	0.001916	0.291983
-7.889559	-1.919290	3.811341	0.001874	0.292297
-7.475888	-1.955240	3.821338	0.001797	0.292491
-7.726930	-1.867358	3.831334	0.001844	0.292700
-7.137291	-1.921374	3.841331	0.001734	0.292962
-6.999743	-1.896723	3.851328	0.001708	0.293207
-6.945357	-1.864259	3.861325	0.001698	0.293416
-6.503128	-1.903309	3.871322	0.001616	0.293620
-6.356940	-1.875676	3.881318	0.001589	0.293887
-6.169483	-1.854522	3.891315	0.001554	0.294159
-5.733763	-1.893481	3.901312	0.001473	0.294357
-5.664320	-1.866534	3.911309	0.001460	0.294551
-5.227618	-1.887563	3.921306	0.001378	0.294838
-4.853427	-1.906312	3.931302	0.001309	0.295079
-4.839659	-1.865838	3.941299	0.001306	0.295290
-4.556828	-1.873180	3.951296	0.001254	0.295506
-4.439388	-1.846044	3.961293	0.001232	0.295743
-4.122626	-1.855221	3.971290	0.001173	0.295980
-4.087725	-1.816844	3.981286	0.001166	0.296198
-3.952236	-1.794967	3.991283	0.001141	0.296425
-3.684894	-1.786520	4.001280	0.001091	0.296703
-3.353566	-1.794011	4.011277	0.001030	0.296960
-3.307967	-1.754372	4.021274	0.001021	0.297194
-3.418415	-1.678811	4.031270	0.001042	0.297464
-3.258291	-1.653116	4.041267	0.001012	0.297730
-2.761002	-1.689277	4.051264	0.000919	0.297993
-2.755117	-1.635668	4.061261	0.000918	0.298259
-2.891439	-1.546423	4.071258	0.000943	0.298571
-2.959299	-1.475081	4.081254	0.000956	0.298857
-2.517459	-1.492915	4.091251	0.000874	0.299159
-2.231058	-1.488726	4.101248	0.000820	0.299431
-2.268539	-1.419967	4.111245	0.000827	0.299730
-1.815232	-1.438893	4.121242	0.000743	0.300037
-1.829045	-1.370826	4.131238	0.000746	0.300352
-1.826431	-1.314135	4.141235	0.000745	0.300628
-1.890176	-1.240562	4.151232	0.000757	0.300926
-1.743354	-1.199398	4.161229	0.000729	0.301252
-1.491936	-1.173755	4.171226	0.000683	0.301594
-1.442956	-1.116339	4.181222	0.000674	0.301912
-1.304263	-1.069890	4.191219	0.000648	0.302255
-1.359453	-0.982542	4.201216	0.000658	0.302625
-1.339744	-0.901930	4.211213	0.000654	0.303027
-1.172267	-0.859849	4.221210	0.000623	0.303373
-0.759111	-0.861828	4.231206	0.000546	0.303722
-0.935793	-0.749460	4.241203	0.000579	0.304104
-0.866698	-0.683249	4.251200	0.000566	0.304478
-0.812280	-0.600782	4.261197	0.000556	0.304917
-0.629697	-0.551032	4.271194	0.000522	0.305310
-0.499060	-0.499384	4.281190	0.000497	0.305667
-0.220866	-0.462474	4.291187	0.000446	0.306081
-0.313366	-0.356719	4.301184	0.000463	0.306501
-0.307383	-0.273284	4.311181	0.000462	0.306900
-0.157088	-0.202858	4.321178	0.000434	0.307360
-0.128497	-0.113493	4.331174	0.000428	0.307805
-0.384218	0.023921	4.341171	0.000476	0.308232
-0.062639	0.069007	4.351168	0.000416	0.308717
0.000000	0.146541	4.361165	0.000404	0.309134

-0.118501	0.440241	4.366170	0.000426	0.310405
0.437936	0.899371	4.371174	0.000322	0.313006
1.301235	1.592179	4.376179	0.000161	0.316909
1.967443	2.610644	4.381184	0.000036	0.322069
2.768323	3.902636	4.386189	-0.000114	0.328462
3.969618	5.415591	4.391194	-0.000338	0.336001
5.122046	7.248630	4.396198	-0.000554	0.344682
6.886983	9.290124	4.401203	-0.000884	0.354456
9.503544	11.488045	4.406208	-0.001373	0.365200
12.607198	13.949793	4.411213	-0.001952	0.376990
16.188303	16.671668	4.416218	-0.002621	0.389708
18.323009	20.017568	4.421222	-0.003020	0.403323
19.970782	23.808039	4.426227	-0.003330	0.417727
21.683058	27.941853	4.431232	-0.003651	0.432838
23.317173	32.453390	4.436237	-0.003958	0.448611
24.809203	37.350113	4.441242	-0.004239	0.464966
26.210451	42.627974	4.446246	-0.004504	0.481859
27.316332	48.311905	4.451251	-0.004713	0.499202
29.385532	54.173682	4.456256	-0.005103	0.516946
31.357689	60.392248	4.461261	-0.005474	0.535016
33.029355	66.999007	4.466266	-0.005789	0.553367
34.343814	74.000566	4.471270	-0.006039	0.571964
35.628795	81.306260	4.476275	-0.006283	0.590706
36.892519	88.894076	4.481280	-0.006523	0.609530
38.132244	96.764541	4.486285	-0.006759	0.628430
39.059592	104.931343	4.491290	-0.006937	0.647313
40.001438	113.336246	4.496294	-0.007118	0.666183
40.719314	121.971775	4.501299	-0.007257	0.684934
41.656968	130.751098	4.506304	-0.007437	0.703561
42.323859	139.750355	4.511309	-0.007567	0.722051
43.102690	148.867359	4.516314	-0.007718	0.740346
44.344538	158.036431	4.521318	-0.007956	0.758456
45.015228	167.411669	4.526323	-0.008087	0.776337
45.842401	176.844828	4.531328	-0.008247	0.793971
47.143817	186.272388	4.536333	-0.008495	0.811361
48.137245	195.823246	4.541338	-0.008686	0.828504
49.000752	205.442757	4.546342	-0.008853	0.845378
49.691518	215.103960	4.551347	-0.008988	0.861939
50.490354	224.757046	4.556352	-0.009143	0.878205
51.337047	234.421701	4.561357	-0.009307	0.894207
51.940059	244.111819	4.566362	-0.009426	0.909900
52.476982	253.797395	4.571366	-0.009532	0.925301
53.403874	263.389240	4.576371	-0.009711	0.940410
54.264087	272.967213	4.581376	-0.009877	0.955241
54.773823	282.585307	4.586381	-0.009979	0.969813
55.219129	292.162694	4.591386	-0.010068	0.984093
55.970334	301.664973	4.596390	-0.010214	0.998136
56.989822	311.031061	4.601395	-0.010410	1.011856
57.565825	320.449305	4.606400	-0.010523	1.025357
58.490020	329.765573	4.611405	-0.010701	1.038625
59.074326	339.087090	4.616410	-0.010816	1.051651
59.778327	348.350332	4.621414	-0.010953	1.064465
60.522852	357.556758	4.626419	-0.011098	1.077061
60.970618	366.760451	4.631424	-0.011187	1.089438
61.530049	375.900510	4.636429	-0.011297	1.101618
62.644374	384.898234	4.641434	-0.011511	1.113604
63.798248	393.857459	4.646438	-0.011731	1.125421
64.284807	402.906251	4.651443	-0.011828	1.137083
64.990030	411.870658	4.656448	-0.011965	1.148567
66.033224	420.737933	4.661453	-0.012165	1.159888
66.873207	429.579381	4.666458	-0.012327	1.171024
67.486006	438.439909	4.671462	-0.012447	1.182031
68.150999	447.257201	4.676467	-0.012577	1.192894
68.827006	456.022776	4.681472	-0.012708	1.203599
69.460136	464.796818	4.686477	-0.012832	1.214211
69.908880	473.549078	4.691482	-0.012921	1.224668
70.453242	482.269378	4.696486	-0.013028	1.235018
71.039694	490.914284	4.701491	-0.013143	1.245202
71.774446	499.527861	4.706496	-0.013285	1.255296
72.578343	508.124096	4.711501	-0.013441	1.265303
72.961276	516.760717	4.716506	-0.013518	1.275196
73.874915	525.275594	4.721510	-0.013693	1.284976
74.253129	533.886804	4.726515	-0.013769	1.294689
75.157941	542.356171	4.731520	-0.013943	1.304271
75.892361	550.937528	4.736525	-0.014086	1.313874
76.350151	559.440606	4.741530	-0.014176	1.323271
77.059313	567.906556	4.746534	-0.014314	1.332606
77.605815	576.363365	4.751539	-0.014421	1.341838
77.982161	584.842165	4.756544	-0.014497	1.350999
78.576415	593.274919	4.761549	-0.014613	1.360088
79.545083	601.610306	4.766554	-0.014799	1.369079
80.294351	610.017652	4.771558	-0.014944	1.378049
80.614841	618.474284	4.776563	-0.015009	1.386937
81.083512	626.881162	4.781568	-0.015102	1.395742
81.574872	635.261647	4.786573	-0.015199	1.404469
81.812729	643.689309	4.791578	-0.015248	1.413147
82.903605	651.936951	4.796582	-0.015457	1.421732
83.358772	660.325029	4.801587	-0.015547	1.430302
83.786267	668.673686	4.806592	-0.015632	1.438775
84.543519	676.977789	4.811597	-0.015778	1.447209
84.905115	685.348057	4.816602	-0.015851	1.455595
85.154053	693.723687	4.821606	-0.015903	1.463919
85.596399	702.077106	4.826611	-0.015991	1.472206
86.018823	710.373983	4.831616	-0.016075	1.480387
86.855135	718.612510	4.836621	-0.016236	1.488533
87.352010	726.895663	4.841626	-0.016334	1.496623
88.112174	735.142571	4.846630	-0.016481	1.504677
88.142138	743.535556	4.851635	-0.016492	1.512713
88.553440	751.787571	4.856640	-0.016574	1.520631
89.113100	760.062982	4.861645	-0.016683	1.528553
89.701804	768.300122	4.866650	-0.016798	1.536403
90.510984	776.502433	4.871654	-0.016954	1.544213
90.778350	784.822406	4.876659	-0.017010	1.552012
91.444985	793.021028	4.881664	-0.017139	1.559719
91.916432	801.286086	4.886669	-0.017232	1.567420
92.245304	809.548556	4.891674	-0.017299	1.575059
92.915002	817.766404	4.896678	-0.017429	1.582671
93.453872	826.001075	4.901683	-0.017535	1.590243
94.029421	834.224333	4.906688	-0.017647	1.597773
94.330083	842.485021	4.911693	-0.017709	1.605262
94.939742	850.696989	4.916698	-0.017827	1.612717
95.446039	858.919108	4.921702	-0.017927	1.620131
95.691614	867.192654	4.926707	-0.017978	1.627520
96.326044	875.404539	4.931712	-0.018102	1.634876
96.949424	883.569808	4.936717	-0.018223	1.642157
97.474082	891.751979	4.941722	-0.018326	1.649406
98.191548	899.937501	4.946726	-0.018465	1.656652
98.780466	908.120809	4.951731	-0.018580	1.663848
98.783002	916.416051	4.956736	-0.018586	1.671028
99.208919	924.616547	4.961741	-0.018670	1.678154
99.839388	932.747562	4.966746	-0.018793	1.685217
100.177068	940.989684	4.971750	-0.018861	1.692307
100.709285	949.164094	4.976755	-0.018966	1.699335
101.264558	957.327042	4.981760	-0.019074	1.706327
101.742469	965.537995	4.986765	-0.019169	1.713321
102.096500	973.693177	4.991770	-0.019240	1.720224
102.446762	981.895942	4.996774	-0.019311	1.727137
102.940146	990.076066	5.001779	-0.019408	1.734023
103.176103	998.264564	5.006784	-0.019457	1.740855
103.482205	1006.475633	5.011789	-0.019519	1.747688
104.191616	1014.582122	5.016794	-0.019657	1.754460
104.825561	1022.711736	5.021798	-0.019780	1.761215
105.317776	1030.889091	5.026803	-0.019877	1.767965
106.155999	1038.997145	5.031808	-0.020038	1.774677
106.743902	1047.167527	5.036813	-0.020153	1.781382
106.762951	1055.419252	5.041818	-0.020162	1.788055
106.686077	1063.703780	5.046822	-0.020153	1.794719
107.386683	1071.773710	5.051827	-0.020289	1.801282
107.749152	1079.913357	5.056832	-0.020362	1.807835
108.035922	1088.112520	5.061837	-0.020420	1.814403
108.819153	1096.161220	5.066842	-0.020572	1.820888
109.220749	1104.319749	5.071846	-0.020652	1.827390
109.652922	1112.480609	5.076851	-0.020737	1.833875
109.772685	1120.644110	5.081856	-0.020765	1.840301
110.300621	1128.772823	5.086861	-0.020869	1.846726
110.714829	1136.913179	5.091866	-0.020951	1.853125
110.924336	1145.091201	5.096870	-0.020995	1.859506
111.084310	1153.263148	5.101875	-0.021030	1.865854
111.238465	1161.428346	5.106880	-0.021065	1.872175
111.489024	1169.587656	5.111885	-0.021116	1.878482
111.678412	1177.694061	5.116890	-0.021157	1.884720
111.864077	1185.853665	5.121894	-0.021197	1.890977
112.291815	1193.964589	5.126899	-0.021282	1.897205
112.236538	1202.130388	5.131904	-0.021277	1.903398
112.777907	1210.235144	5.136909	-0.021383	1.909593
112.454063	1218.455616	5.141914	-0.021328	1.915756
112.894579	1226.527326	5.146918	-0.021415	1.921875
113.474889	1234.587729	5.151923	-0.021529	1.927982
113.587137	1242.738743	5.156928	-0.021555	1.934084
114.252265	1250.791376	5.161933	-0.021684	1.940156
114.913802	1258.882175	5.166938	-0.021812	1.946236
115.784806	1266.947036	5.171942	-0.021980	1.952302
115.855420	1275.125554	5.176947	-0.021998	1.958344
116.161906	1283.215958	5.181952	-0.022061	1.964328
116.688691	1291.325549	5.186957	-0.022164	1.970332
116.710653	1299.500724	5.191962	-0.022173	1.976310
117.123166	1307.597835	5.196966	-0.022255	1.982257
117.398995	1315.734254	5.201971	-0.022312	1.988199
116.784020	1324.000200	5.206976	-0.022203	1.994120
117.079245	1332.070547	5.211981	-0.022263	1.999981
117.348204	1340.156374	5.216986	-0.022319	2.005834
118.165798	1348.170112	5.221990	-0.022476	2.011675
118.216486	1356.319545	5.226995	-0.022491	2.017516
118.313361	1364.457778	5.232000	-0.022514	2.023336
119.071717	1372.510158	5.237005	-0.022660	2.029148
119.116799	1380.659175	5.242010	-0.022674	2.034937
119.267427	1388.761757	5.247014	-0.022708	2.040688
119.599149	1396.849992	5.252019	-0.022775	2.046432
119.815457	1404.963584	5.257024	-0.022820	2.052165
119.839907	1413.116705	5.262029	-0.022830	2.057890
120.485040	1421.126111	5.267034	-0.022955	2.063562
120.538000	1429.281035	5.272038	-0.022970	2.069260
120.924899	1437.353423	5.277043	-0.023048	2.074918
121.110293	1445.444560	5.282048	-0.023088	2.080554
121.442468	1453.552832	5.287053	-0.023155	2.086201
121.431820	1461.703729	5.292058	-0.023158	2.091827
121.505149	1469.821439	5.297062	-0.023177	2.097424
121.884884	1477.882169	5.302067	-0.023253	2.102998
121.659447	1486.067396	5.307072	-0.023216	2.108581
121.820524	1494.197235	5.312077	-0.023252	2.114151
122.318213	1502.184231	5.317082	-0.023349	2.119642
122.705933	1510.223898	5.322086	-0.023427	2.125143
122.882331	1518.351470	5.327091	-0.023465	2.130669
123.211164	1526.404301	5.332096	-0.023531	2.136145
123.411752	1534.514402	5.337101	-0.023574	2.141633
123.397401	1542.634129	5.342106	-0.023577	2.147093
123.549000	1550.736222	5.347110	-0.023610	2.152543
123.683510	1558.825463	5.352115	-0.023641	2.157968
123.963549	1566.881765	5.357120	-0.023698	2.163373
124.112226	1575.002837	5.362125	-0.023731	2.168794
124.452293	1583.068272	5.367130	-0.023799	2.174183
124.753099	1591.149687	5.372134	-0.023861	2.179565
124.753546	1599.259389	5.377139	-0.023866	2.184924
124.716839	1607.381745	5.382144	-0.023865	2.190276
124.895154	1615.478162	5.387149	-0.023903	2.195617
125.234883	1623.501475	5.392154	-0.023971	2.200912
125.298200	1631.590504	5.397158	-0.023989	2.206212
125.719912	1639.649002	5.402163	-0.024072	2.211512
125.868125	1647.745443	5.407168	-0.024105	2.216799
126.052640	1655.833119	5.412173	-0.024145	2.222071
126.215954	1663.911557	5.417178	-0.024180	2.227322
126.440645	1672.006591	5.422182	-0.024228	2.232578
126.739712	1680.071899	5.427187	-0.024289	2.237808
126.565531	1688.193644	5.432192	-0.024261	2.243020
127.056497	1696.222619	5.437197	-0.024358	2.248220
127.297687	1704.308219	5.442202	-0.024408	2.253422
127.439507	1712.400916	5.447206	-0.024440	2.258608
127.654215	1720.481316	5.452211	-0.024485	2.263780
127.764856	1728.567615	5.457216	-0.024511	2.268935
127.717173	1736.756978	5.462221	-0.024507	2.274129
127.992613	1744.753802	5.467226	-0.024564	2.279219
128.038292	1752.818424	5.472230	-0.024578	2.284319
128.265853	1760.890510	5.477235	-0.024625	2.289429
128.379927	1768.957774	5.482240	-0.024652	2.294515
128.906720	1776.971754	5.487245	-0.024755	2.299591
129.220576	1785.007037	5.492250	-0.024819	2.304651
129.442935	1793.113337	5.497254	-0.024865	2.309737
129.551154	1801.210288	5.502259	-0.024891	2.314795
129.786031	1809.243076	5.507264	-0.024940	2.319814
130.169998	1817.292338	5.512269	-0.025017	2.324844
130.428200	1825.382613	5.517274	-0.025070	2.329878
130.422754	1833.506711	5.522278	-0.025074	2.334900
130.688038	1841.557330	5.527283	-0.025129	2.339889
130.864384	1849.624775	5.532288	-0.025167	2.344870
130.944899	1857.755391	5.537293	-0.025187	2.349871
131.470415	1865.756124	5.542298	-0.025290	2.354819
131.609698	1873.821456	5.547302	-0.025321	2.359763
132.031129	1881.859105	5.552307	-0.025405	2.364704
132.059122	1889.965661	5.557312	-0.025416	2.369644
132.466097	1898.035546	5.562317	-0.025497	2.374583
132.333833	1906.153676	5.567322	-0.025477	2.379496
132.805962	1914.164071	5.572326	-0.025570	2.384383
133.240638	1922.235080	5.577331	-0.025657	2.389294
133.288876	1930.302168	5.582336	-0.025671	2.394161
133.467379	1938.386130	5.587341	-0.025709	2.399039
133.625531	1946.434749	5.592346	-0.025744	2.403884
133.996081	1954.484819	5.597350	-0.025818	2.408737
134.015329	1962.601002	5.602355	-0.025827	2.413591
134.353950	1970.630390	5.607360	-0.025895	2.418410
134.715851	1978.692859	5.612365	-0.025968	2.423240
134.749391	1986.786229	5.617370	-0.025980	2.428053
135.209000	1994.848232	5.622374	-0.026070	2.432872
135.562465	2002.903149	5.627379	-0.026142	2.437668
135.454790	2010.979802	5.632384	-0.026127	2.442431
135.942581	2019.006280	5.637389	-0.026223	2.447203
136.255727	2027.061228	5.642394	-0.026286	2.451968
136.479911	2035.110022	5.647398	-0.026333	2.456713
137.067966	2043.139615	5.652403	-0.026448	2.461466
136.973364	2051.261110	5.657408	-0.026436	2.466210
137.238134	2059.353627	5.662413	-0.026490	2.470956
137.440091	2067.394264	5.667418	-0.026533	2.475658
137.666684	2075.432596	5.672422	-0.026581	2.480352
138.162443	2083.454310	5.677427	-0.026678	2.485048
138.407512	2091.524283	5.682432	-0.026729	2.489743
138.417518	2099.653837	5.687437	-0.026736	2.494446
138.494489	2107.715334	5.692442	-0.026756	2.499107
138.863919	2115.737351	5.697446	-0.026830	2.503757
139.448851	2123.760930	5.702451	-0.026944	2.508416
139.273435	2131.891352	5.707456	-0.026916	2.513071
139.814941	2139.896733	5.712461	-0.027023	2.517699
140.087099	2147.933177	5.717466	-0.027078	2.522316
140.267542	2156.012788	5.722470	-0.027117	2.526943
140.591042	2164.084775	5.727475	-0.027183	2.531567
140.780630	2172.134041	5.732480	-0.027223	2.536160
140.780089	2180.264012	5.737485	-0.027229	2.540776
141.497465	2188.205834	5.742490	-0.027367	2.545330
141.826770	2196.273364	5.747494	-0.027434	2.549918
142.003754	2204.349678	5.752499	-0.027472	2.554492
142.160292	2212.403013	5.757504	-0.027506	2.559044
142.242255	2220.505292	5.762509	-0.027527	2.563609
142.536848	2228.538813	5.767514	-0.027587	2.568143
142.215546	2236.691788	5.772518	-0.027533	2.572692
142.983504	2244.646738	5.777523	-0.027681	2.577200
143.252785	2252.674281	5.782528	-0.027736	2.581704
143.396851	2260.754277	5.787533	-0.027768	2.586222
143.351345	2268.912859	5.792538	-0.027765	2.590761
143.764061	2276.996713	5.797542	-0.027847	2.595284
144.077923	2284.993068	5.802547	-0.027911	2.599743
144.021457	2293.012143	5.807552	-0.027905	2.604181
144.692498	2300.995874	5.812557	-0.028036	2.608642
144.950991	2309.055614	5.817562	-0.028089	2.613109
145.138695	2317.115212	5.822566	-0.028129	2.617564
145.338838	2325.165523	5.827571	-0.028172	2.622007
145.586662	2333.204322	5.832576	-0.028223	2.626439
145.926145	2341.275639	5.837581	-0.028292	2.630887
146.221856	2349.296918	5.842586	-0.028352	2.635298
146.646618	2357.322364	5.847590	-0.028436	2.639712
146.859254	2365.380945	5.852595	-0.028481	2.644122
147.022575	2373.442300	5.857600	-0.028517	2.648524
147.524638	2381.485630	5.862605	-0.028615	2.652930
147.697308	2389.566901	5.867610	-0.028653	2.657328
148.106131	2397.591625	5.872614	-0.028734	2.661704
148.513877	2405.658240	5.877619	-0.028815	2.666095
148.723597	2413.722818	5.882624	-0.028860	2.670465
149.195344	2421.748892	5.887629	-0.028953	2.674824
149.266347	2429.812469	5.892634	-0.028971	2.679169
149.668458	2437.812657	5.897638	-0.029051	2.683496
149.968128	2445.881596	5.902643	-0.029112	2.687845
149.858358	2453.983949	5.907648	-0.029097	2.692178
150.301650	2462.018562	5.912653	-0.029185	2.696504
150.632289	2470.037904	5.917658	-0.029252	2.700808
150.782826	2478.087983	5.922662	-0.029285	2.705109
151.285248	2486.137120	5.927667	-0.029384	2.709426
151.499134	2494.186660	5.932672	-0.029429	2.713718
151.801280	2502.233120	5.937677	-0.029490	2.718006
152.053250	2510.270211	5.942682	-0.029542	2.722280
152.113130	2518.345561	5.947686	-0.029559	2.726555
152.579911	2526.390665	5.952691	-0.029651	2.730833
152.430001	2534.505440	5.957696	-0.029628	2.735102
153.068333	2542.482049	5.962701	-0.029752	2.739342
153.547188	2550.486888	5.967706	-0.029847	2.743579
153.642839	2558.563218	5.972710	-0.029870	2.747823
154.071030	2566.675684	5.977715	-0.029955	2.752101
154.362826	2574.703780	5.982720	-0.030014	2.756319
154.765099	2582.736015	5.987725	-0.030095	2.760540
154.774764	2590.760834	5.992730	-0.030102	2.764726
155.034306	2598.801249	5.997734	-0.030155	2.768929
155.442713	2606.836446	6.002739	-0.030236	2.773132
155.498497	2614.888365	6.007744	-0.030252	2.777316
156.151574	2622.895976	6.012749	-0.030379	2.781507
156.233632	2630.967495	6.017754	-0.030399	2.785690
157.428469	2638.932661	6.022758	-0.030627	2.789879
159.100926	2646.868443	6.027763	-0.030944	2.794075
159.604725	2654.943534	6.032768	-0.031043	2.798266
160.297379	2662.979818	6.037773	-0.031177	2.802442
160.363746	2671.084484	6.042778	-0.031195	2.806609
160.768879	2679.167900	6.047782	-0.031275	2.810780
161.361854	2687.225260	6.052787	-0.031391	2.814942
161.727336	2695.244911	6.057792	-0.031464	2.819064
162.411142	2703.283090	6.062797	-0.031597	2.823210
162.739052	2711.345212	6.067802	-0.031663	2.827340
162.594570	2719.488564	6.072806	-0.031641	2.831477
162.822809	2727.557791	6.077811	-0.031689	2.835593
163.280832	2735.515208	6.082816	-0.031780	2.839659
163.684511	2743.565107	6.087821	-0.031860	2.843764
164.062486	2751.597102	6.092826	-0.031936	2.847851
164.601121	2759.618143	6.097830	-0.032041	2.851937
164.673033	2767.729073	6.102835	-0.032060	2.856035
164.876936	2775.749244	6.107840	-0.032103	2.860088
165.012367	2783.799883	6.112845	-0.032134	2.864148
165.614241	2791.803416	6.117850	-0.032251	2.868205
165.837983	2799.862769	6.122854	-0.032298	2.872262
165.953190	2807.935346	6.127859	-0.032324	2.876314
166.206950	2815.969998	6.132864	-0.032377	2.880349
166.663274	2823.971318	6.137869	-0.032467	2.884374
166.681230	2832.078543	6.142874	-0.032476	2.888420
166.789310	2840.129339	6.147878	-0.032501	2.892438
167.111529	2848.162956	6.152883	-0.032566	2.896454
167.294688	2856.188918	6.157888	-0.032606	2.900453
167.702409	2864.221708	6.162893	-0.032687	2.904462
167.775520	2872.300683	6.167898	-0.032706	2.908470
167.875953	2880.395378	6.172902	-0.032730	2.912481
168.330203	2888.394269	6.177907	-0.032819	2.916459
168.438447	2896.405435	6.182912	-0.032845	2.920419
168.858369	2904.387894	6.187917	-0.032928	2.924376
168.814489	2912.467669	6.192922	-0.032925	2.928350
169.072253	2920.499636	6.197926	-0.032978	2.932312
169.599952	2928.538924	6.202931	-0.033082	2.936287
169.815694	2936.548551	6.207936	-0.033127	2.940224
170.006535	2944.595391	6.212941	-0.033168	2.944174
170.229758	2952.660456	6.217946	-0.033215	2.948128
170.288641	2960.710329	6.222950	-0.033231	2.952061
170.498264	2968.783966	6.227955	-0.033275	2.956009
170.619455	2976.778716	6.232960	-0.033303	2.959908
171.087254	2984.791281	6.237965	-0.033396	2.963829
171.240822	2992.832170	6.242970	-0.033429	2.967742
171.642643	3000.866467	6.247974	-0.033509	2.971659
172.329015	3008.874939	6.252979	-0.033642	2.975574
172.220220	3016.942257	6.257984	-0.033627	2.979470
172.342922	3024.995729	6.262989	-0.033656	2.983367
172.474533	3033.071147	6.267994	-0.033685	2.987269
172.966131	3041.069183	6.272998	-0.033782	2.991148
173.321847	3049.102203	6.278003	-0.033853	2.995031
173.501832	3057.114627	6.283008	-0.033892	2.998891
173.718651	3065.168034	6.288013	-0.033938	3.002767
174.130125	3073.202700	6.293018	-0.034020	3.006639
174.199164	3081.262273	6.298022	-0.034038	3.010500
174.641578	3089.297071	6.303027	-0.034125	3.014363
174.966723	3097.288133	6.308032	-0.034191	3.018195
175.433729	3105.324933	6.313037	-0.034283	3.022051
175.698742	3113.366734	6.318042	-0.034338	3.025894
176.173221	3121.386920	6.323046	-0.034431	3.029732
176.747763	3129.441182	6.328051	-0.034544	3.033586
176.525350	3137.522057	6.333056	-0.034508	3.037409
176.669120	3145.570572	6.338061	-0.034540	3.041229
177.149372	3153.565613	6.343066	-0.034634	3.045036
177.477581	3161.568323	6.348070	-0.034701	3.048834
177.914612	3169.639978	6.353075	-0.034787	3.052665
177.938714	3177.727962	6.358080	-0.034797	3.056479
178.244274	3185.768239	6.363085	-0.034859	3.060280
178.252154	3193.797785	6.368090	-0.034866	3.064056
178.687538	3201.816196	6.373094	-0.034952	3.067843
178.706685	3209.935117	6.378099	-0.034961	3.071652
179.047244	3217.942239	6.383104	-0.035029	3.075420
179.476402	3225.924189	6.388109	-0.035115	3.079175
179.946897	3233.922554	6.393114	-0.035207	3.082935
180.254381	3241.948348	6.398118	-0.035270	3.086696
180.739053	3249.982682	6.403123	-0.035365	3.090465
181.069993	3258.002557	6.408128	-0.035432	3.094215
181.562731	3266.019170	6.413133	-0.035529	3.097966
181.742910	3274.069554	6.418138	-0.035568	3.101714
181.943101	3282.135818	6.423142	-0.035611	3.105465
182.557737	3290.142216	6.428147	-0.035730	3.109204
182.644380	3298.198588	6.433152	-0.035752	3.112936
183.150274	3306.229028	6.438157	-0.035851	3.116672
183.752964	3314.216288	6.443162	-0.035968	3.120387
183.947812	3322.233480	6.448166	-0.036010	3.124093
184.639837	3330.269984	6.453171	-0.036144	3.127826
184.927418	3338.323773	6.458176	-0.036203	3.131544
185.076282	3346.402543	6.463181	-0.036236	3.135263
185.459351	3354.427408	6.468186	-0.036312	3.138963
186.008245	3362.418135	6.473190	-0.036420	3.142651
186.107857	3370.504220	6.478195	-0.036444	3.146357
186.301551	3378.566635	6.483200	-0.036485	3.150053
186.756107	3386.590176	6.488205	-0.036575	3.153738
186.979490	3394.594870	6.493210	-0.036621	3.157400
187.287058	3402.637678	6.498214	-0.036684	3.161078
187.427871	3410.685185	6.503219	-0.036715	3.164747
188.183324	3418.650006	6.508224	-0.036861	3.168402
188.647142	3426.710847	6.513229	-0.036953	3.172083
188.954956	3434.754570	6.518234	-0.037015	3.175745
189.279632	3442.793678	6.523238	-0.037081	3.179401
189.561134	3450.851258	6.528243	-0.037139	3.183059
189.867458	3458.834280	6.533248	-0.037201	3.186681
190.586063	3466.870179	6.538253	-0.037340	3.190340
191.064413	3474.858629	6.543258	-0.037434	3.193963
191.234524	3482.941041	6.548262	-0.037471	3.197611
191.398517	3491.042393	6.553267	-0.037507	3.201263
191.944847	3498.964663	6.558272	-0.037614	3.204846
192.349519	3507.030111	6.563277	-0.037695	3.208484
192.647084	3515.075500	6.568282	-0.037755	3.212104
192.770162	3523.160101	6.573286	-0.037783	3.215730
192.771774	3531.232697	6.578291	-0.037789	3.219341
193.143061	3539.177001	6.583296	-0.037863	3.222907
193.776342	3547.230604	6.588301	-0.037986	3.226528
194.135213	3555.267824	6.593306	-0.038059	3.230127
194.503407	3563.276130	6.598310	-0.038132	3.233709
194.629391	3571.338914	6.603315	-0.038161	3.237300
195.502207	3579.264217	6.608320	-0.038329	3.240859
195.450139	3587.325305	6.613325	-0.038324	3.244434
195.664063	3595.386439	6.618330	-0.038369	3.248017
196.145109	3603.420214	6.623334	-0.038464	3.251595
196.520408	3611.498414	6.628339	-0.038539	3.255184
196.528384	3619.477986	6.633344	-0.038546	3.258710
197.227788	3627.464662	6.638349	-0.038681	3.262264
197.614791	3635.533422	6.643354	-0.038759	3.265838
197.582164	3643.582839	6.648358	-0.038758	3.269381
198.214749	3651.621887	6.653363	-0.038881	3.272944
198.857284	3659.583794	6.658368	-0.039006	3.276469
199.168613	3667.656344	6.663373	-0.039069	3.280025
199.458513	3675.668554	6.668378	-0.039128	3.283550
199.999604	3683.672840	6.673382	-0.039234	3.287078
200.276409	3691.785212	6.678387	-0.039291	3.290639
200.451964	3699.760697	6.683392	-0.039329	3.294132
201.181446	3707.787849	6.688397	-0.039470	3.297666
201.829866	3715.819908	6.693402	-0.039596	3.301194
201.928113	3723.854297	6.698406	-0.039619	3.304699
202.185486	3731.938090	6.703411	-0.039672	3.308227
202.644430	3739.916821	6.708416	-0.039763	3.311713
203.222572	3747.934415	6.713421	-0.039876	3.315218
203.368024	3755.996208	6.718426	-0.039908	3.318721
203.789820	3763.993429	6.723430	-0.039992	3.322203
204.207844	3772.042886	6.728435	-0.040075	3.325703
204.440463	3780.084421	6.733440	-0.040124	3.329190
204.732051	3788.127062	6.738445	-0.040183	3.332675
205.204532	3796.141864	6.743450	-0.040276	3.336152
205.461353	3804.169967	6.748454	-0.040329	3.339622
206.064769	3812.163433	6.753459	-0.040447	3.343087
206.246976	3820.218073	6.758464	-0.040486	3.346559
206.782555	3828.266640	6.763469	-0.040591	3.350038
206.938606	3836.309302	6.768474	-0.040625	3.353496
207.268411	3844.350149	6.773478	-0.040692	3.356956
207.149485	3852.441067	6.778483	-0.040675	3.360418
207.741514	3860.315910	6.783488	-0.040791	3.363810
208.044424	3868.413527	6.788493	-0.040852	3.367283
208.794513	3876.421387	6.793498	-0.040997	3.370730
208.909419	3884.449183	6.798502	-0.041024	3.374159
209.154668	3892.520061	6.803507	-0.041075	3.377608
209.402426	3900.570480	6.808512	-0.041126	3.381044
210.230316	3908.505598	6.813517	-0.041285	3.384449
210.349460	3916.583785	6.818522	-0.041313	3.387886
210.603643	3924.665973	6.823526	-0.041365	3.391325
211.168613	3932.685598	6.828531	-0.041476	3.394746
211.213538	3940.696207	6.833536	-0.041489	3.398141
211.542202	3948.726027	6.838541	-0.041556	3.401550
211.915794	3956.689296	6.843546	-0.041631	3.404930
212.548891	3964.675558	6.848550	-0.041754	3.408325
212.943974	3972.759904	6.853555	-0.041833	3.411750
213.103032	3980.826611	6.858560	-0.041867	3.415155
213.564580	3988.798722	6.863565	-0.041959	3.418527
213.528504	3996.920413	6.868570	-0.041957	3.421942
213.530844	4004.934719	6.873574	-0.041963	3.425309
214.413818	4012.891930	6.878579	-0.042132	3.428680
215.191085	4020.907965	6.883584	-0.042282	3.432069
215.556814	4028.965935	6.888589	-0.042356	3.435457
216.073367	4036.944830	6.893594	-0.042457	3.438814
216.559400	4044.961207	6.898598	-0.042553	3.442183
217.308598	4053.025168	6.903603	-0.042697	3.445577
217.523025	4061.047373	6.908608	-0.042743	3.448931
217.613394	4069.169418	6.913613	-0.042765	3.452320
218.080618	4077.173942	6.918618	-0.042857	3.455669
218.668559	4085.093948	6.923622	-0.042972	3.458984
219.246321	4093.156446	6.928627	-0.043084	3.462355
219.361202	4101.225060	6.933632	-0.043111	3.465709
219.413990	4109.287039	6.938637	-0.043126	3.469054
220.127544	4117.254062	6.943642	-0.043264	3.472380
220.556284	4125.269541	6.948646	-0.043349	3.475713
220.959952	4133.285134	6.953651	-0.043430	3.479041
221.609173	4141.226770	6.958656	-0.043556	3.482345
222.105775	4149.292225	6.963661	-0.043653	3.485690
222.218717	4157.383640	6.968666	-0.043680	3.489031
222.700808	4165.403225	6.973670	-0.043775	3.492351
223.224886	4173.455392	6.978675	-0.043878	3.495682
223.554634	4181.437571	6.983680	-0.043944	3.498975
223.650712	4189.481771	6.988685	-0.043967	3.502283
224.207418	4197.508458	6.993690	-0.044076	3.505596
224.437000	4205.523214	6.998694	-0.044124	3.508889
224.803858	4213.606441	7.003699	-0.044198	3.512212
224.994027	4221.624423	7.008704	-0.044238	3.515500
225.644802	4229.593919	7.013709	-0.044365	3.518779
225.927186	4237.665055	7.018714	-0.044422	3.522085
225.956603	4245.697883	7.023718	-0.044433	3.525364
226.464757	4253.726124	7.028723	-0.044533	3.528654
226.845304	4261.768201	7.033728	-0.044609	3.531941
227.131442	4269.799958	7.038733	-0.044668	3.535219
227.467760	4277.806226	7.043738	-0.044735	3.538484
227.701780	4285.847950	7.048742	-0.044784	3.541758
228.142973	4293.845856	7.053747	-0.044872	3.545018
228.229528	4301.886302	7.058752	-0.044893	3.548280
228.744244	4309.956111	7.063757	-0.044994	3.551565
229.185350	4317.979063	7.068762	-0.045081	3.554825
229.431321	4325.959583	7.073766	-0.045132	3.558059
229.852369	4333.994476	7.078771	-0.045216	3.561317
230.134136	4341.957717	7.083776	-0.045274	3.564540
230.322670	4350.023673	7.088781	-0.045314	3.567798
231.093372	4358.010488	7.093786	-0.045463	3.571038
231.343168	4366.028628	7.098790	-0.045515	3.574273
231.991750	4374.085567	7.103795	-0.045641	3.577532
231.883980	4382.174169	7.108800	-0.045626	3.580778
232.497932	4390.110293	7.113805	-0.045745	3.583981
232.872951	4398.159635	7.118810	-0.045820	3.587220
233.047798	4406.214158	7.123814	-0.045858	3.590452
233.569588	4414.246401	7.128819	-0.045960	3.593682
233.846339	4422.250342	7.133824	-0.046017	3.596891
234.117608	4430.263531	7.138829	-0.046073	3.600100
234.536189	4438.247343	7.143834	-0.046156	3.603299
234.889381	4446.298068	7.148838	-0.046227	3.606520
235.297869	4454.328597	7.153843	-0.046308	3.609732
235.505920	4462.372465	7.158848	-0.046352	3.612940
235.901973	4470.445243	7.163853	-0.046431	3.616162
236.223277	4478.422364	7.168858	-0.046496	3.619341
236.276061	4486.478009	7.173862	-0.046511	3.622541
236.673110	4494.520682	7.178867	-0.046591	3.625743
236.937191	4502.506929	7.183872	-0.046645	3.628915
237.392852	4510.533077	7.188877	-0.046735	3.632106
237.584645	4518.588547	7.193882	-0.046776	3.635299
237.999980	4526.564112	7.198886	-0.046859	3.638463
238.696258	4534.571891	7.203891	-0.046993	3.641645
238.922175	4542.548360	7.208896	-0.047041	3.644798
239.415039	4550.604057	7.213901	-0.047138	3.647988
239.923596	4558.659584	7.218906	-0.047238	3.651175
239.945799	4566.687582	7.223910	-0.047247	3.654334
240.437976	4574.699870	7.228915	-0.047344	3.657498
240.738503	4582.744672	7.233920	-0.047405	3.660667
241.034208	4590.730077	7.238925	-0.047465	3.663809
241.482738	4598.787500	7.243930	-0.047554	3.666981
241.760410	4606.797810	7.248934	-0.047611	3.670127
242.013464	4614.843158	7.253939	-0.047663	3.673283
242.243613	4622.868381	7.258944	-0.047711	3.676429
242.501290	4630.857931	7.263949	-0.047765	3.679558
242.837755	4638.874591	7.268954	-0.047832	3.682697
243.034835	4646.894182	7.273958	-0.047874	3.685831
243.300759	4654.937629	7.278963	-0.047929	3.688973
243.687596	4662.986246	7.283968	-0.048006	3.692118
243.871020	4671.045278	7.288973	-0.048046	3.695259
243.966112	4679.064213	7.293978	-0.048069	3.698379
244.481246	4687.074486	7.298982	-0.048170	3.701504
244.845606	4695.070527	7.303987	-0.048243	3.704617
244.798100	4703.126872	7.308992	-0.048239	3.707740
244.972538	4711.208197	7.313997	-0.048277	3.710875
245.545036	4719.221483	7.319002	-0.048389	3.713992
245.730184	4727.214233	7.324006	-0.048429	3.717089
245.844487	4735.268541	7.329011	-0.048455	3.720205
246.244109	4743.227484	7.334016	-0.048535	3.723288
246.706830	4751.249762	7.339021	-0.048626	3.726395
246.859477	4759.292039	7.344026	-0.048660	3.729499
247.167907	4767.294393	7.349030	-0.048722	3.732590
247.738058	4775.319695	7.354035	-0.048834	3.735693
248.044059	4783.274920	7.359040	-0.048896	3.738759
248.463461	4791.368460	7.364045	-0.048979	3.741879
248.712186	4799.378303	7.369050	-0.049031	3.744961
249.271024	4807.387055	7.374054	-0.049140	3.748046
249.552070	4815.451508	7.379059	-0.049198	3.751144
249.649778	4823.448882	7.384064	-0.049221	3.754209
250.152820	4831.470994	7.389069	-0.049320	3.757291
250.306691	4839.500130	7.394074	-0.049354	3.760364
250.562205	4847.464037	7.399078	-0.049407	3.763412
251.014937	4855.570953	7.404083	-0.049496	3.766517
251.276239	4863.557634	7.409088	-0.049550	3.769569
251.600028	4871.573203	7.414093	-0.049615	3.772631
252.226599	4879.578883	7.419098	-0.049737	3.775694
252.290762	4887.579755	7.424102	-0.049755	3.778740
252.667505	4895.653065	7.429107	-0.049830	3.781817
253.185193	4903.629787	7.434112	-0.049932	3.784859
253.276734	4911.735058	7.439117	-0.049954	3.787937
253.698140	4919.749974	7.444122	-0.050038	3.790986
253.587644	4927.734241	7.449126	-0.050022	3.794008
254.301136	4935.764146	7.454131	-0.050160	3.797065
254.573030	4943.748614	7.459136	-0.050216	3.800091
254.872046	4951.746182	7.464141	-0.050277	3.803121
255.477321	4959.811029	7.469146	-0.050395	3.806181
255.552661	4967.829521	7.474150	-0.050414	3.809208
255.804229	4975.924960	7.479155	-0.050466	3.812266
256.127188	4983.885924	7.484160	-0.050532	3.815272
256.710651	4991.894920	7.489165	-0.050645	3.818300
256.751833	4999.964587	7.494170	-0.050658	3.821337
256.848413	5007.940161	7.499174	-0.050682	3.824336
257.370707	5016.030632	7.504179	-0.050784	3.827386
257.489724	5024.055141	7.509184	-0.050811	3.830400
257.895823	5032.057408	7.514189	-0.050892	3.833409
258.384466	5040.091299	7.519194	-0.050988	3.836430
258.813482	5048.065157	7.524198	-0.051074	3.839424
258.902779	5056.130434	7.529203	-0.051095	3.842443
259.233817	5064.081042	7.534208	-0.051162	3.845421
259.601874	5072.143700	7.539213	-0.051236	3.848440
260.011903	5080.197872	7.544218	-0.051318	3.851455
260.027833	5088.191654	7.549222	-0.051326	3.854435
260.661160	5096.250859	7.554227	-0.051449	3.857452
260.940244	5104.232088	7.559232	-0.051506	3.860429
261.160239	5112.246490	7.564237	-0.051552	3.863415
261.585079	5120.290827	7.569242	-0.051637	3.866414
261.831901	5128.297880	7.574246	-0.051688	3.869393
262.069719	5136.444698	7.579251	-0.051737	3.872421
262.118738	5144.505886	7.584256	-0.051752	3.875411
262.497369	5152.406474	7.589261	-0.051827	3.878347
263.081191	5160.410554	7.594266	-0.051941	3.881322
262.999975	5168.344990	7.599270	-0.051931	3.884256
263.710302	5176.396027	7.604275	-0.052069	3.887247
263.826241	5184.401935	7.609280	-0.052096	3.890206
264.171892	5192.443633	7.614285	-0.052165	3.893182
264.462655	5200.493810	7.619290	-0.052225	3.896157
264.611939	5208.463954	7.624294	-0.052258	3.899097
264.824696	5216.540189	7.629299	-0.052303	3.902075
264.795502	5224.559465	7.634304	-0.052302	3.905026
265.332001	5232.521019	7.639309	-0.052407	3.907964
265.738239	5240.610592	7.644314	-0.052488	3.910944
265.875048	5248.574693	7.649318	-0.052519	3.913871
265.891091	5256.723266	7.654323	-0.052527	3.916860
266.724804	5264.559214	7.659328	-0.052688	3.919749
267.355658	5272.531468	7.664333	-0.052810	3.922682
267.570818	5280.654880	7.669338	-0.052856	3.925659
267.734434	5288.669437	7.674342	-0.052891	3.928593
267.824075	5296.778561	7.679347	-0.052913	3.931559
268.322111	5304.726197	7.684352	-0.053011	3.934471
268.365686	5312.785842	7.689357	-0.053025	3.937412
268.592191	5320.826604	7.694362	-0.053072	3.940349
269.179360	5328.742483	7.699366	-0.053186	3.943244
269.621037	5336.841797	7.704371	-0.053274	3.946201
269.363268	5344.926712	7.709376	-0.053231	3.949138
269.624951	5352.939372	7.714381	-0.053285	3.952055
270.131970	5360.940387	7.719386	-0.053385	3.954971
270.285292	5368.924224	7.724390	-0.053419	3.957872
270.749074	5376.965419	7.729395	-0.053510	3.960798
270.925990	5384.915228	7.734400	-0.053548	3.963682
271.498122	5392.957964	7.739405	-0.053660	3.966606
271.911671	5400.964778	7.744410	-0.053742	3.969511
271.644386	5409.081555	7.749414	-0.053698	3.972442
271.758244	5417.128242	7.754419	-0.053724	3.975352
271.972451	5425.074727	7.759424	-0.053769	3.978225
272.691823	5433.086102	7.764429	-0.053908	3.981129
273.359290	5441.016978	7.769434	-0.054038	3.984001
273.357884	5449.120928	7.774438	-0.054043	3.986921
273.480230	5457.212654	7.779443	-0.054071	3.989836
273.786821	5465.141702	7.784448	-0.054133	3.992695
274.212730	5473.195021	7.789453	-0.054218	3.995597
274.853501	5481.148421	7.794458	-0.054342	3.998466
274.441653	5489.280056	7.799462	-0.054271	4.001378
274.958628	5497.205959	7.804467	-0.054372	4.004230
275.363156	5505.267667	7.809472	-0.054453	4.007127
275.648167	5513.269555	7.814477	-0.054511	4.009999
275.932527	5521.322707	7.819482	-0.054569	4.012886
276.075540	5529.325559	7.824486	-0.054601	4.015751
276.309271	5537.352670	7.829491	-0.054650	4.018624
276.670676	5545.377065	7.834496	-0.054722	4.021497
276.860437	5553.361940	7.839501	-0.054763	4.024350
277.526361	5561.389251	7.844506	-0.054892	4.027224
277.622926	5569.406702	7.849510	-0.054915	4.030083
277.807344	5577.525837	7.854515	-0.054955	4.032978
278.405083	5585.520607	7.859520	-0.055071	4.035833
278.943150	5593.445851	7.864525	-0.055177	4.038660
279.315967	5601.458167	7.869530	-0.055251	4.041514
279.505279	5609.459064	7.874534	-0.055292	4.044358
279.746662	5617.553111	7.879539	-0.055342	4.047234
279.986260	5625.543022	7.884544	-0.055392	4.050072
280.220574	5633.590875	7.889549	-0.055441	4.052927
280.673410	5641.615447	7.894554	-0.055530	4.055776
280.729605	5649.632429	7.899558	-0.055546	4.058614
281.219951	5657.643976	7.904563	-0.055643	4.061455
281.463783	5665.651773	7.909568	-0.055693	4.064288
281.781486	5673.662060	7.914573	-0.055758	4.067122
282.006459	5681.728990	7.919578	-0.055805	4.069972
282.316772	5689.717409	7.924582	-0.055868	4.072794
282.708387	5697.770948	7.929587	-0.055946	4.075637
282.758611	5705.772117	7.934592	-0.055960	4.078456
283.223722	5713.800287	7.939597	-0.056052	4.081288
283.780094	5721.757551	7.944602	-0.056161	4.084094
284.117454	5729.795509	7.949606	-0.056229	4.086924
284.350448	5737.883579	7.954611	-0.056278	4.089767
284.566812	5745.880174	7.959616	-0.056323	4.092576
284.980055	5753.929415	7.964621	-0.056405	4.095405
284.948804	5761.959969	7.969626	-0.056405	4.098218
285.259064	5769.956142	7.974630	-0.056468	4.101023
285.740706	5777.954487	7.979635	-0.056563	4.103829
285.843653	5785.981962	7.984640	-0.056587	4.106637
286.370533	5793.952236	7.989645	-0.056690	4.109430
286.910877	5802.027783	7.994650	-0.056796	4.112257
287.143517	5809.992586	7.999654	-0.056845	4.115040
287.405953	5818.059314	8.004659	-0.056899	4.117857
287.638726	5826.090739	8.009664	-0.056947	4.120659
287.954223	5834.042855	8.014669	-0.057011	4.123432
288.250398	5842.125966	8.019674	-0.057072	4.126249
288.459780	5850.066358	8.024678	-0.057116	4.129013
288.914646	5858.147292	8.029683	-0.057206	4.131828
289.099789	5866.141863	8.034688	-0.057246	4.134607
289.229110	5874.179144	8.039693	-0.057275	4.137398
289.773476	5882.183486	8.044698	-0.057381	4.140181
290.023896	5890.180332	8.049702	-0.057433	4.142956
290.314180	5898.255079	8.054707	-0.057493	4.145756
290.887793	5906.219143	8.059712	-0.057605	4.148520
291.222745	5914.301568	8.064717	-0.057672	4.151320
291.599170	5922.256125	8.069722	-0.057747	4.154074
291.815594	5930.295310	8.074726	-0.057793	4.156854
292.265132	5938.304210	8.079731	-0.057882	4.159624
292.369308	5946.347642	8.084736	-0.057907	4.162400
292.722913	5954.317605	8.089741	-0.057978	4.165152
293.217317	5962.352240	8.094746	-0.058075	4.167925
293.650948	5970.370145	8.099750	-0.058161	4.170691
293.830708	5978.435378	8.104755	-0.058200	4.173468
294.215288	5986.447860	8.109760	-0.058276	4.176227
294.557202	5994.404600	8.114765	-0.058345	4.178965
294.933744	6002.475551	8.119770	-0.058421	4.181740
294.848205	6010.492743	8.124774	-0.058410	4.184490
295.474248	6018.522146	8.129779	-0.058532	4.187250
296.156671	6026.521427	8.134784	-0.058664	4.189999
296.313770	6034.616494	8.139789	-0.058698	4.192773
296.687488	6042.648386	8.144794	-0.058773	4.195525
297.333631	6050.571358	8.149798	-0.058899	4.198242
297.687539	6058.619351	8.154803	-0.058970	4.200996
297.725197	6066.558188	8.159808	-0.058982	4.203708
298.137884	6074.631403	8.164813	-0.059064	4.206468
298.465933	6082.642416	8.169818	-0.059130	4.209203
298.740710	6090.671551	8.174822	-0.059187	4.211943
299.317411	6098.711644	8.179827	-0.059299	4.214688
299.626114	6106.718316	8.184832	-0.059362	4.217416
299.838010	6114.763769	8.189837	-0.059407	4.220155
299.495310	6122.862866	8.194842	-0.059348	4.222905
300.166934	6130.766134	8.199846	-0.059479	4.225597
300.640086	6138.809884	8.204851	-0.059572	4.228332
300.790356	6146.850007	8.209856	-0.059605	4.231062
300.921727	6154.855457	8.214861	-0.059635	4.233777
301.327046	6162.900806	8.219866	-0.059715	4.236507
301.491783	6170.834529	8.224870	-0.059751	4.239195
301.972822	6178.877971	8.229875	-0.059846	4.241922
302.470947	6186.837605	8.234880	-0.059944	4.244619
302.555051	6194.934439	8.239885	-0.059965	4.247356
302.889295	6202.949379	8.244890	-0.060032	4.250066
303.344962	6210.928885	8.249894	-0.060122	4.252764
303.749697	6219.058708	8.254899	-0.060203	4.255510
303.782763	6226.999382	8.259904	-0.060214	4.258187
304.062684	6235.025813	8.264909	-0.060272	4.260893
304.407211	6243.022163	8.269914	-0.060341	4.263589
304.621655	6251.043318	8.274918	-0.060386	4.266289
304.952708	6259.079259	8.279923	-0.060453	4.268994
305.112388	6267.095654	8.284928	-0.060488	4.271689
305.486932	6275.056130	8.289933	-0.060563	4.274365
305.613187	6283.131223	8.294938	-0.060592	4.277076
306.036285	6291.067111	8.299942	-0.060676	4.279742
306.474297	6299.135373	8.304947	-0.060763	4.282450
306.573523	6307.148467	8.309952	-0.060786	4.285134
306.993292	6315.144670	8.314957	-0.060870	4.287814
307.470580	6323.211693	8.319962	-0.060964	4.290517
307.518637	6331.218212	8.324966	-0.060978	4.293194
307.942439	6339.267220	8.329971	-0.061062	4.295887
308.223418	6347.230832	8.334976	-0.061120	4.298548
308.435822	6355.310853	8.339981	-0.061164	4.301246
308.774506	6363.269985	8.344986	-0.061233	4.303902
308.866213	6371.282874	8.349990	-0.061255	4.306573
309.561961	6379.314965	8.354995	-0.061390	4.309254
309.652227	6387.357772	8.360000	-0.061412	4.311932
309.990843	6395.336300	8.365005	-0.061480	4.314588
310.507556	6403.382038	8.370010	-0.061581	4.317267
310.794437	6411.321313	8.375014	-0.061640	4.319906
310.751844	6419.396173	8.380019	-0.061637	4.322587
311.273853	6427.358359	8.385024	-0.061740	4.325233
311.467061	6435.413866	8.390029	-0.061781	4.327905
311.813276	6443.444279	8.395034	-0.061851	4.330569
312.120579	6451.461874	8.400038	-0.061913	4.333226
312.613125	6459.496074	8.405043	-0.062010	4.335889
312.699052	6467.461159	8.410048	-0.062031	4.338524
313.215847	6475.521005	8.415053	-0.062133	4.341192
313.460989	6483.498854	8.420058	-0.062184	4.343829
313.670421	6491.544933	8.425062	-0.062228	4.346487
313.911488	6499.579201	8.430067	-0.062278	4.349139
314.064831	6507.662179	8.435072	-0.062312	4.351805
314.447170	6515.618891	8.440077	-0.062388	4.354430
314.786459	6523.666894	8.445082	-0.062456	4.357083
315.190787	6531.576144	8.450086	-0.062537	4.359689
315.561459	6539.647715	8.455091	-0.062611	4.362346
315.498215	6547.604739	8.460096	-0.062605	4.364961
315.765645	6555.637229	8.465101	-0.062660	4.367602
316.082413	6563.705017	8.470106	-0.062724	4.370253
316.494614	6571.677748	8.475110	-0.062806	4.372872
316.707928	6579.767293	8.480115	-0.062851	4.375526
316.948318	6587.755488	8.485120	-0.062901	4.378145
317.202557	6595.776890	8.490125	-0.062953	4.380774
317.421406	6603.729527	8.495130	-0.062999	4.383378
317.533829	6611.736911	8.500134	-0.063025	4.385998
318.214309	6619.774842	8.505139	-0.063157	4.388630
318.355523	6627.849770	8.510144	-0.063189	4.391269
318.500992	6635.839627	8.515149	-0.063221	4.393879
318.988194	6643.881147	8.520154	-0.063317	4.396506
319.083022	6651.840546	8.525158	-0.063340	4.399102
319.497616	6659.930735	8.530163	-0.063422	4.401742
319.795363	6667.856571	8.535168	-0.063483	4.404325
320.155709	6675.936619	8.540173	-0.063555	4.406958
320.489835	6683.970306	8.545178	-0.063623	4.409573
320.614689	6691.996463	8.550182	-0.063651	4.412183
321.183568	6700.018311	8.555187	-0.063762	4.414793
321.253534	6708.037863	8.560192	-0.063781	4.417398
321.449953	6716.058947	8.565197	-0.063822	4.420003
321.862690	6724.132994	8.570202	-0.063905	4.422624
322.069297	6732.132778	8.575207	-0.063948	4.425218
322.337965	6740.193142	8.580211	-0.064004	4.427831
322.842651	6748.224422	8.585216	-0.064103	4.430434
323.189542	6756.189005	8.590221	-0.064173	4.433013
323.459962	6764.250432	8.595226	-0.064228	4.435622
323.595898	6772.216530	8.600231	-0.064259	4.438197
323.987250	6780.277873	8.605235	-0.064337	4.440803
324.330127	6788.236553	8.610240	-0.064406	4.443374
324.494361	6796.306421	8.615245	-0.064442	4.445978
324.700390	6804.329101	8.620250	-0.064485	4.448566
325.048462	6812.315557	8.625255	-0.064555	4.451141
325.380888	6820.340965	8.630259	-0.064622	4.453728
325.716726	6828.372097	8.635264	-0.064690	4.456314
325.728229	6836.380878	8.640269	-0.064697	4.458890
326.516064	6844.412890	8.645274	-0.064849	4.461476
326.397046	6852.376666	8.650279	-0.064832	4.464035
326.851602	6860.486448	8.655283	-0.064922	4.466641
327.248545	6868.402491	8.660288	-0.065001	4.469183
327.286445	6876.488912	8.665293	-0.065014	4.471777
327.717634	6884.455738	8.670298	-0.065099	4.474333
328.170911	6892.466964	8.675303	-0.065189	4.476901
328.448098	6900.473647	8.680307	-0.065246	4.479466
328.820679	6908.493529	8.685312	-0.065320	4.482034
329.179159	6916.492961	8.690317	-0.065392	4.484593
329.619875	6924.544908	8.695322	-0.065479	4.487169
329.634540	6932.503441	8.700327	-0.065487	4.489711
330.102941	6940.609516	8.705331	-0.065580	4.492301
330.170547	6948.629472	8.710336	-0.065598	4.494860
330.394453	6956.611988	8.715341	-0.065645	4.497406
330.843900	6964.639554	8.720346	-0.065733	4.499966
331.051855	6972.620780	8.725351	-0.065777	4.502509
331.368142	6980.661279	8.730355	-0.065842	4.505070
331.357158	6988.724916	8.735360	-0.065845	4.507635
331.975380	6996.676146	8.740365	-0.065965	4.510165
332.266312	7004.715273	8.745370	-0.066024	4.512721
332.323076	7012.696696	8.750375	-0.066040	4.515256
332.823840	7020.695664	8.755379	-0.066139	4.517797
332.939674	7028.709229	8.760384	-0.066165	4.520339
333.123149	7036.701064	8.765389	-0.066205	4.522874
333.324400	7044.793866	8.770394	-0.066248	4.525439
333.618340	7052.729710	8.775399	-0.066307	4.527953
334.026953	7060.821922	8.780403	-0.066389	4.530515
334.052515	7068.825726	8.785408	-0.066399	4.533047
334.265536	7076.819463	8.790413	-0.066444	4.535575
334.729390	7084.817476	8.795418	-0.066535	4.538104
334.643577	7092.822989	8.800423	-0.066524	4.540632
335.270605	7100.817911	8.805427	-0.066646	4.543157
335.507323	7108.867342	8.810432	-0.066696	4.545697
335.664536	7116.915094	8.815437	-0.066730	4.548234
335.762091	7124.978789	8.820442	-0.066754	4.550775
336.188378	7132.931421	8.825447	-0.066838	4.553281
336.404649	7140.969585	8.830451	-0.066884	4.555811
336.634056	7148.959596	8.835456	-0.066932	4.558325
336.886501	7156.976796	8.840461	-0.066984	4.560846
337.225542	7164.961156	8.845466	-0.067052	4.563355
337.320896	7173.002433	8.850471	-0.067075	4.565881
337.493228	7181.026802	8.855475	-0.067112	4.568399
337.876629	7189.054316	8.860480	-0.067189	4.570918
338.073849	7197.033789	8.865485	-0.067231	4.573420
338.097923	7205.133380	8.870490	-0.067241	4.575958
338.302554	7213.038978	8.875495	-0.067284	4.578434
338.770652	7221.112085	8.880499	-0.067376	4.580962
338.817295	7229.088318	8.885504	-0.067390	4.583457
339.205334	7237.153030	8.890509	-0.067468	4.585979
339.577227	7245.152462	8.895514	-0.067542	4.588479
339.629472	7253.174969	8.900519	-0.067557	4.590984
339.869029	7261.161988	8.905523	-0.067607	4.593478
340.070862	7269.230702	8.910528	-0.067650	4.595995
340.505890	7277.163699	8.915533	-0.067736	4.598469
340.391737	7285.264744	8.920538	-0.067720	4.600993
340.630110	7293.163266	8.925543	-0.067770	4.603453
340.990284	7301.277356	8.930547	-0.067842	4.605979
341.150731	7309.224088	8.935552	-0.067877	4.608451
341.067453	7317.343698	8.940557	-0.067867	4.610976
341.344038	7325.327930	8.945562	-0.067923	4.613457
341.704714	7333.358562	8.950567	-0.067996	4.615952
341.914648	7341.320656	8.955571	-0.068040	4.618423
342.195282	7349.390604	8.960576	-0.068098	4.620927
342.365067	7357.304164	8.965581	-0.068134	4.623381
342.689654	7365.406077	8.970586	-0.068200	4.625892
342.706975	7373.399192	8.975591	-0.068209	4.628368
343.103790	7381.471598	8.980595	-0.068288	4.630867
343.368644	7389.401370	8.985600	-0.068342	4.633321
343.482417	7397.449776	8.990605	-0.068369	4.635809
343.945670	7405.410206	8.995610	-0.068460	4.638270
344.280284	7413.469196	9.000615	-0.068528	4.640759
344.547540	7421.431551	9.005619	-0.068583	4.643218
344.579347	7429.529941	9.010624	-0.068594	4.645716
344.761407	7437.529368	9.015629	-0.068633	4.648183
344.948367	7445.595939	9.020634	-0.068673	4.650670
344.806007	7453.574657	9.025639	-0.068652	4.653128
345.572966	7461.567876	9.030643	-0.068800	4.655589
345.678378	7469.572469	9.035648	-0.068824	4.658052
345.941224	7477.604794	9.040653	-0.068879	4.660523
346.202751	7485.617110	9.045658	-0.068933	4.662986
346.405229	7493.628630	9.050663	-0.068975	4.665447
346.680013	7501.655741	9.055667	-0.069032	4.667912
346.487527	7509.756771	9.060672	-0.069001	4.670398
347.023377	7517.738999	9.065677	-0.069106	4.672846
347.172110	7525.716793	9.070682	-0.069139	4.675292
347.272111	7533.657969	9.075687	-0.069163	4.677725
347.761092	7541.692878	9.080691	-0.069259	4.680186
348.023085	7549.721476	9.085696	-0.069313	4.682643
348.090855	7557.694702	9.090701	-0.069331	4.685082
348.364276	7565.781960	9.095706	-0.069387	4.687555
348.809926	7573.756599	9.100711	-0.069475	4.689992
349.068396	7581.796321	9.105715	-0.069529	4.692447
349.153733	7589.802959	9.110720	-0.069550	4.694891
349.282763	7597.826246	9.115725	-0.069579	4.697339
349.583719	7605.853393	9.120730	-0.069640	4.699787
349.519966	7613.843463	9.125735	-0.069634	4.702223
349.587741	7621.875101	9.130739	-0.069652	4.704669
350.035165	7629.904387	9.135744	-0.069740	4.707113
350.343950	7637.925089	9.140749	-0.069803	4.709554
350.493530	7646.020173	9.145754	-0.069836	4.712016
350.741929	7653.943356	9.150759	-0.069887	4.714424
351.054300	7661.972769	9.155763	-0.069951	4.716863
351.161114	7669.973502	9.160768	-0.069976	4.719293
351.651781	7677.968167	9.165773	-0.070072	4.721719
351.772323	7685.953714	9.170778	-0.070100	4.724141
351.718505	7693.994915	9.175783	-0.070095	4.726579
351.958529	7702.020400	9.180787	-0.070145	4.729011
352.366445	7710.087254	9.185792	-0.070226	4.731454
352.502898	7718.032905	9.190797	-0.070257	4.733859
352.723562	7726.178277	9.195802	-0.070303	4.736323
352.774637	7734.123401	9.200807	-0.070318	4.738726
352.820318	7742.179990	9.205811	-0.070332	4.741161
353.295749	7750.081577	9.210816	-0.070425	4.743547
353.277358	7758.202906	9.215821	-0.070427	4.746000
353.205133	7766.248352	9.220826	-0.070419	4.748428
353.500699	7774.251084	9.225831	-0.070479	4.750841
354.190320	7782.207309	9.230835	-0.070613	4.753238
354.128033	7790.302581	9.235840	-0.070607	4.755678
354.255736	7798.233549	9.240845	-0.070636	4.758066
354.632293	7806.307636	9.245850	-0.070711	4.760496
354.779171	7814.261504	9.250855	-0.070743	4.762888
354.723710	7822.352612	9.255859	-0.070738	4.765322
354.919725	7830.347296	9.260864	-0.070780	4.767724
355.032165	7838.334916	9.265869	-0.070806	4.770123
355.665412	7846.342002	9.270874	-0.070929	4.772526
355.708323	7854.359045	9.275879	-0.070943	4.774931
356.019384	7862.418229	9.280883	-0.071006	4.777348
356.390069	7870.418688	9.285888	-0.071080	4.779745
356.801683	7878.394558	9.290893	-0.071162	4.782134
356.831928	7886.385150	9.295898	-0.071173	4.784527
356.983276	7894.491648	9.300903	-0.071206	4.786953
357.371326	7902.448354	9.305907	-0.071283	4.789332
357.795620	7910.521316	9.310912	-0.071368	4.791745
357.778359	7918.447233	9.315917	-0.071370	4.794114
358.062632	7926.607391	9.320922	-0.071428	4.796551
358.186412	7934.461398	9.325927	-0.071456	4.798895
358.288677	7942.601571	9.330931	-0.071480	4.801324
358.587539	7950.508551	9.335936	-0.071541	4.803682
358.797787	7958.560898	9.340941	-0.071586	4.806082
359.242207	7966.617147	9.345946	-0.071674	4.808481
359.611562	7974.608490	9.350951	-0.071748	4.810859
359.675638	7982.618878	9.355955	-0.071765	4.813243
359.471826	7990.093442	9.360960	-0.071732	4.815468
359.825439	7994.670497	9.365965	-0.071800	4.816828

360.443100	7997.235240	9.370970	-0.071917	4.817588
360.320378	7998.352962	9.375975	-0.071895	4.817921
360.782585	7998.820108	9.380979	-0.071981	4.818058
361.128412	7999.812920	9.385984	-0.072046	4.818352
361.015704	7999.798813	9.390989	-0.072025	4.818348
361.127936	7999.866473	9.395994	-0.072046	4.818368
361.327584	7999.869136	9.400999	-0.072084	4.818368
361.829511	7999.833825	9.406003	-0.072177	4.818355
361.533626	7999.841429	9.411008	-0.072122	4.818359
361.494482	7999.865061	9.416013	-0.072115	4.818366
361.562903	7999.897480	9.421018	-0.072127	4.818375
361.615852	7999.859328	9.426023	-0.072137	4.818364
362.143675	7999.872674	9.431027	-0.072235	4.818366
362.235547	7999.844493	9.436032	-0.072253	4.818357
362.238700	7999.826681	9.441037	-0.072253	4.818352
362.277444	7999.857655	9.446042	-0.072260	4.818361
362.291455	7999.844188	9.451047	-0.072263	4.818357
362.248497	7999.871971	9.456051	-0.072255	4.818365
362.611400	7999.855811	9.461056	-0.072323	4.818359
362.554909	7999.880262	9.466061	-0.072312	4.818366
362.970922	7999.870063	9.471066	-0.072389	4.818362
362.854259	7999.877957	9.476071	-0.072368	4.818364
363.127876	7999.870058	9.481075	-0.072419	4.818361
363.112630	7999.877205	9.486080	-0.072416	4.818363
363.110809	7999.858276	9.491085	-0.072415	4.818358
363.227542	7999.890292	9.496090	-0.072437	4.818367
363.321831	7999.867395	9.501095	-0.072455	4.818359
363.725678	7999.815025	9.506099	-0.072530	4.818342
363.669904	7999.874145	9.511104	-0.072520	4.818360
363.665533	7999.865684	9.516109	-0.072519	4.818358
364.021367	7999.855733	9.521114	-0.072585	4.818353
363.707683	7999.858894	9.526119	-0.072527	4.818355
363.863455	7999.874628	9.531123	-0.072556	4.818359
363.730952	7999.894913	9.536128	-0.072531	4.818366
363.895749	7999.884512	9.541133	-0.072562	4.818362
364.230039	7999.884777	9.546138	-0.072624	4.818361
364.154678	7999.889021	9.551143	-0.072610	4.818363
364.264720	7999.878938	9.556147	-0.072630	4.818359
364.130508	7999.885546	9.561152	-0.072605	4.818362
364.351325	7999.910553	9.566157	-0.072646	4.818368
364.488374	7999.923937	9.571162	-0.072672	4.818372
364.746879	7999.862274	9.576167	-0.072720	4.818352
364.566982	7999.897680	9.581171	-0.072687	4.818364
364.755153	7999.863434	9.586176	-0.072722	4.818353
365.002990	7999.885652	9.591181	-0.072768	4.818358
365.158753	7999.866728	9.596186	-0.072797	4.818352
364.827042	7999.870696	9.601191	-0.072735	4.818354
365.031348	7999.904935	9.606195	-0.072773	4.818364
364.956547	7999.906036	9.611200	-0.072759	4.818364
365.217373	7999.854907	9.616205	-0.072808	4.818348
365.181376	7999.870180	9.621210	-0.072801	4.818353
365.407590	7999.909964	9.626215	-0.072843	4.818364
365.379587	7999.879131	9.631219	-0.072838	4.818355
365.456225	7999.891708	9.636224	-0.072852	4.818358
365.464943	7999.863466	9.641229	-0.072854	4.818350
365.577645	7999.901734	9.646234	-0.072875	4.818361
365.537105	7999.874934	9.651239	-0.072867	4.818353
365.411422	7999.922617	9.656243	-0.072844	4.818368
365.710378	7999.898256	9.661248	-0.072899	4.818359
365.585386	7999.875578	9.666253	-0.072876	4.818353
365.831596	7999.913531	9.671258	-0.072922	4.818363
365.682544	7999.878977	9.676263	-0.072894	4.818354
365.817757	7999.922798	9.681267	-0.072919	4.818366
365.926524	7999.880139	9.686272	-0.072940	4.818353
366.059563	7999.856710	9.691277	-0.072964	4.818345
366.060686	7999.872480	9.696282	-0.072965	4.818350
366.041181	7999.823904	9.701287	-0.072961	4.818336
366.113963	7999.867940	9.706291	-0.072974	4.818349
366.219288	7999.888254	9.711296	-0.072994	4.818354
366.143046	7999.822114	9.716301	-0.072980	4.818335
366.180655	7999.892988	9.721306	-0.072987	4.818356
366.090140	7999.885475	9.726311	-0.072970	4.818354
366.153362	7999.846408	9.731315	-0.072982	4.818342
366.229617	7999.893642	9.736320	-0.072996	4.818356
366.423380	7999.811157	9.741325	-0.073032	4.818330
366.414137	7999.877204	9.746330	-0.073030	4.818350
366.466573	7999.843244	9.751335	-0.073040	4.818340
366.575665	7999.895119	9.756339	-0.073060	4.818355
366.469810	7999.898954	9.761344	-0.073041	4.818356
366.484950	7999.869747	9.766349	-0.073043	4.818348
366.681652	7999.913342	9.771354	-0.073080	4.818360
366.498247	7999.873075	9.776359	-0.073046	4.818349
366.598645	7999.871267	9.781363	-0.073065	4.818348
366.492877	7999.887708	9.786368	-0.073045	4.818353
366.530108	7999.796826	9.791373	-0.073052	4.818326
366.580582	7999.897283	9.796378	-0.073061	4.818355
366.629793	7999.879035	9.801383	-0.073070	4.818350
366.932550	7999.891488	9.806387	-0.073127	4.818352
366.836249	7999.882847	9.811392	-0.073109	4.818350
366.770707	7999.880919	9.816397	-0.073097	4.818350
366.789361	7999.903226	9.821402	-0.073100	4.818356
366.735318	7999.872042	9.826407	-0.073090	4.818347
366.733931	7999.894081	9.831411	-0.073090	4.818354
366.729654	7999.910828	9.836416	-0.073089	4.818359
366.819036	7999.867910	9.841421	-0.073106	4.818346
367.048367	7999.847870	9.846426	-0.073148	4.818339
366.912755	7999.835552	9.851431	-0.073123	4.818336
367.010290	7999.888324	9.856435	-0.073141	4.818351
367.142268	7999.898492	9.861440	-0.073166	4.818354
366.974904	7999.923561	9.866445	-0.073135	4.818362
367.237862	7999.921828	9.871450	-0.073184	4.818360
367.166354	7999.903015	9.876455	-0.073170	4.818355
367.259852	7999.918971	9.881459	-0.073188	4.818359
367.045786	7999.933962	9.886464	-0.073148	4.818364
367.191509	7999.819322	9.891469	-0.073175	4.818330
367.192230	7999.920166	9.896474	-0.073175	4.818360
367.043803	7999.894021	9.901479	-0.073147	4.818353
367.125472	7999.914020	9.906483	-0.073163	4.818358
367.155128	7999.883956	9.911488	-0.073168	4.818349
367.240002	7999.864084	9.916493	-0.073184	4.818343
367.334239	7999.908410	9.921498	-0.073202	4.818356
367.206758	7999.870991	9.926503	-0.073178	4.818345
367.156544	7999.913383	9.931507	-0.073168	4.818358
367.222251	7999.920565	9.936512	-0.073181	4.818360
367.272166	7999.896024	9.941517	-0.073190	4.818352
367.393195	7999.942809	9.946522	-0.073212	4.818366
367.322392	7999.887242	9.951527	-0.073199	4.818349
367.413898	7999.933632	9.956531	-0.073216	4.818363
367.473042	7999.914466	9.961536	-0.073227	4.818357
367.338737	7999.917920	9.966541	-0.073202	4.818359
367.666077	7999.927553	9.971546	-0.073263	4.818360
367.672775	7999.907686	9.976551	-0.073264	4.818354
367.619952	7999.932187	9.981555	-0.073255	4.818362
367.660762	7999.911726	9.986560	-0.073262	4.818355
367.593545	7999.871962	9.991565	-0.073250	4.818344
367.774717	7999.883840	9.996570	-0.073283	4.818347
367.682523	7999.906764	10.001575	-0.073266	4.818354
367.781523	7999.915442	10.006579	-0.073285	4.818356
367.672912	7999.905584	10.011584	-0.073264	4.818354
367.664130	7999.869754	10.016589	-0.073263	4.818343
367.870982	7999.865170	10.021594	-0.073301	4.818341
367.839627	7999.848995	10.026599	-0.073295	4.818336
367.845752	7999.887940	10.031603	-0.073297	4.818348
367.848758	7999.904786	10.036608	-0.073297	4.818353
367.779125	7999.896500	10.041613	-0.073284	4.818350
367.813663	7999.931625	10.046618	-0.073291	4.818361
367.832832	7999.888816	10.051623	-0.073294	4.818348
367.856763	7999.908042	10.056627	-0.073299	4.818354
367.823676	7999.914952	10.061632	-0.073293	4.818356
367.972625	7999.919046	10.066637	-0.073320	4.818356
367.936822	7999.938524	10.071642	-0.073314	4.818362
367.935368	7999.912245	10.076647	-0.073313	4.818354
368.094666	7999.923831	10.081651	-0.073343	4.818357
367.822468	7999.938042	10.086656	-0.073292	4.818363
367.763333	7999.931998	10.091661	-0.073281	4.818361
368.131047	7999.948475	10.096666	-0.073350	4.818364
367.880219	7999.912555	10.101671	-0.073303	4.818355
367.880469	7999.893651	10.106675	-0.073303	4.818349
368.056635	7999.935924	10.111680	-0.073336	4.818361
368.175660	7999.934366	10.116685	-0.073358	4.818360
368.171824	7999.944818	10.121690	-0.073357	4.818363
367.943249	7999.920750	10.126695	-0.073315	4.818357
368.318704	7999.956238	10.131699	-0.073385	4.818366
368.317074	7999.927855	10.136704	-0.073384	4.818358
368.092790	7999.875484	10.141709	-0.073343	4.818343
368.342864	7999.947107	10.146714	-0.073389	4.818363
368.224610	7999.938170	10.151719	-0.073367	4.818361
368.023902	7999.916576	10.156723	-0.073330	4.818355
368.209636	7999.934818	10.161728	-0.073364	4.818360
368.007604	7999.939465	10.166733	-0.073327	4.818362
368.223669	7999.915048	10.171738	-0.073367	4.818354
368.421288	7999.906140	10.176743	-0.073404	4.818351
368.553443	7999.887952	10.181747	-0.073428	4.818345
368.568795	7999.948029	10.186752	-0.073431	4.818363
368.161414	7999.932069	10.191757	-0.073355	4.818359
368.427106	7999.957685	10.196762	-0.073405	4.818366
368.605349	7999.923308	10.201767	-0.073438	4.818355
368.461961	7999.931892	10.206771	-0.073411	4.818358
368.217902	7999.930724	10.211776	-0.073366	4.818359
368.248139	7999.914322	10.216781	-0.073371	4.818354
368.450065	7999.947487	10.221786	-0.073409	4.818363
368.277237	7999.924164	10.226791	-0.073377	4.818357
368.377660	7999.960172	10.231795	-0.073396	4.818367
368.379392	7999.944439	10.236800	-0.073396	4.818362
368.379174	7999.939183	10.241805	-0.073396	4.818361
368.435510	7999.958845	10.246810	-0.073406	4.818366
368.395823	7999.913146	10.251815	-0.073399	4.818353
368.516947	7999.925272	10.256819	-0.073421	4.818356
368.655339	7999.921873	10.261824	-0.073447	4.818354
368.724069	7999.933297	10.266829	-0.073460	4.818358
368.657260	7999.949208	10.271834	-0.073448	4.818363
368.557857	7999.891155	10.276839	-0.073429	4.818346
368.661984	7999.909356	10.281843	-0.073448	4.818351
368.804550	7999.940676	10.286848	-0.073475	4.818359
368.519955	7999.919007	10.291853	-0.073422	4.818354
368.494032	7999.944919	10.296858	-0.073417	4.818362
368.537588	7999.903487	10.301863	-0.073425	4.818349
368.856859	7999.898309	10.306867	-0.073485	4.818347
368.796499	7999.935315	10.311872	-0.073473	4.818358
368.670426	7999.854846	10.316877	-0.073450	4.818334
368.765426	7999.943301	10.321882	-0.073468	4.818360
368.821235	7999.918839	10.326887	-0.073478	4.818353
368.729885	7999.910262	10.331891	-0.073461	4.818351
368.888200	7999.940743	10.336896	-0.073490	4.818359
368.748025	7999.914706	10.341901	-0.073464	4.818352
368.856034	7999.946614	10.346906	-0.073484	4.818361
368.844979	7999.901298	10.351911	-0.073482	4.818348
368.903374	7999.916786	10.356915	-0.073493	4.818352
368.892895	7999.931350	10.361920	-0.073491	4.818356
368.809144	7999.877708	10.366925	-0.073476	4.818341
368.901896	7999.941974	10.371930	-0.073493	4.818359
368.833637	7999.923203	10.376935	-0.073480	4.818354
368.797022	7999.942669	10.381939	-0.073473	4.818360
368.731585	7999.933389	10.386944	-0.073461	4.818358
368.937000	7999.942443	10.391949	-0.073500	4.818359
368.809704	7999.986955	10.396954	-0.073476	4.818373
368.845089	7999.944362	10.401959	-0.073482	4.818360
368.834912	7999.925319	10.406963	-0.073480	4.818355
368.969839	7999.931327	10.411968	-0.073506	4.818356
368.956337	7999.941650	10.416973	-0.073503	4.818359
369.102895	7999.962520	10.421978	-0.073530	4.818365
369.069082	7999.900093	10.426983	-0.073524	4.818346
369.034383	7999.911182	10.431987	-0.073518	4.818350
368.924848	7999.963285	10.436992	-0.073497	4.818366
368.965582	7999.912361	10.441997	-0.073505	4.818350
369.167697	7999.936076	10.447002	-0.073542	4.818357
368.986605	7999.886382	10.452007	-0.073509	4.818343
369.044752	7999.897664	10.457011	-0.073519	4.818346
369.222871	7999.921058	10.462016	-0.073553	4.818352
368.974173	7999.905121	10.467021	-0.073506	4.818348
369.218764	7999.904196	10.472026	-0.073552	4.818347
368.963536	7999.897625	10.477031	-0.073504	4.818346
369.251381	7999.881524	10.482035	-0.073558	4.818340
369.322201	7999.909783	10.487040	-0.073571	4.818348
369.164163	7999.927623	10.492045	-0.073542	4.818354
369.219308	7999.935714	10.497050	-0.073552	4.818356
369.485450	7999.915120	10.502055	-0.073602	4.818349
369.411370	7999.935135	10.507059	-0.073588	4.818355
369.192329	7999.949007	10.512064	-0.073547	4.818360
369.303436	7999.911630	10.517069	-0.073568	4.818349
369.417777	7999.945724	10.522074	-0.073589	4.818359
369.429482	7999.924872	10.527079	-0.073591	4.818352
369.195011	7999.931184	10.532083	-0.073547	4.818355
369.213104	7999.963989	10.537088	-0.073551	4.818365
369.270885	7999.930099	10.542093	-0.073562	4.818354
369.333064	7999.971898	10.547098	-0.073573	4.818367
369.398152	7999.961215	10.552103	-0.073585	4.818363
369.371974	7999.970318	10.557107	-0.073580	4.818366
369.391410	7999.941166	10.562112	-0.073584	4.818357
369.372508	7999.907300	10.567117	-0.073580	4.818347
369.302644	7999.957833	10.572122	-0.073567	4.818363
369.388018	7999.922213	10.577127	-0.073583	4.818352
369.417770	7999.924712	10.582131	-0.073589	4.818352
369.533384	7999.969327	10.587136	-0.073610	4.818365
369.412168	7999.930938	10.592141	-0.073588	4.818354
369.320106	7999.961217	10.597146	-0.073571	4.818364
369.466362	7999.933765	10.602151	-0.073598	4.818355
369.543765	7999.900138	10.607155	-0.073612	4.818344
369.554088	7999.929687	10.612160	-0.073614	4.818353
369.394102	7999.927543	10.617165	-0.073584	4.818353
369.403565	7999.963384	10.622170	-0.073586	4.818364
369.345053	7999.914281	10.627175	-0.073575	4.818349
369.363904	7999.917684	10.632179	-0.073579	4.818350
369.392819	7999.942230	10.637184	-0.073584	4.818358
369.326592	7999.926637	10.642189	-0.073572	4.818353
369.128001	7999.951286	10.647194	-0.073535	4.818361
369.376901	7999.924159	10.652199	-0.073581	4.818352
369.400874	7999.916077	10.657203	-0.073586	4.818350
369.536595	7999.942054	10.662208	-0.073611	4.818357
369.467246	7999.912764	10.667213	-0.073598	4.818349
369.600895	7999.954470	10.672218	-0.073623	4.818360
369.464589	7999.915879	10.677223	-0.073597	4.818349
369.484586	7999.943457	10.682227	-0.073601	4.818358
369.578745	7999.927912	10.687232	-0.073619	4.818353
369.517877	7999.908188	10.692237	-0.073607	4.818347
369.541766	7999.931617	10.697242	-0.073612	4.818354
369.523165	7999.924015	10.702247	-0.073608	4.818352
369.679607	7999.928212	10.707251	-0.073637	4.818352
369.588547	7999.941697	10.712256	-0.073621	4.818357
369.430307	7999.912265	10.717261	-0.073591	4.818349
369.691428	7999.971436	10.722266	-0.073640	4.818365
369.689083	7999.937791	10.727271	-0.073639	4.818355
369.507366	7999.954263	10.732275	-0.073605	4.818361
369.546276	7999.952683	10.737280	-0.073613	4.818360
369.797083	7999.949741	10.742285	-0.073659	4.818358
369.816513	7999.952102	10.747290	-0.073663	4.818359
369.690071	7999.947256	10.752295	-0.073639	4.818358
369.875097	7999.943433	10.757299	-0.073674	4.818356
369.819365	7999.960543	10.762304	-0.073663	4.818361
369.618705	7999.925290	10.767309	-0.073626	4.818352
369.801716	7999.958205	10.772314	-0.073660	4.818361
369.725456	7999.957182	10.777319	-0.073646	4.818361
369.630400	7999.944354	10.782323	-0.073628	4.818357
369.687791	7999.947223	10.787328	-0.073639	4.818358
369.800227	7999.919318	10.792333	-0.073660	4.818349
369.757319	7999.970213	10.797338	-0.073652	4.818364
369.636018	7999.955982	10.802343	-0.073629	4.818361
369.713952	7999.972782	10.807347	-0.073644	4.818365
369.825092	7999.993179	10.812352	-0.073664	4.818371
369.775372	7999.916882	10.817357	-0.073655	4.818349
369.938285	7999.981040	10.822362	-0.073686	4.818367
369.902185	7999.928035	10.827367	-0.073679	4.818351
369.740709	7999.969988	10.832371	-0.073649	4.818364
369.976453	7999.974198	10.837376	-0.073693	4.818365
369.776898	7999.959968	10.842381	-0.073655	4.818361
369.977303	7999.978410	10.847386	-0.073693	4.818366
369.747196	7999.935410	10.852391	-0.073650	4.818354
369.810846	7999.968825	10.857395	-0.073662	4.818364
369.879452	7999.978148	10.862400	-0.073675	4.818366
369.579652	7999.959424	10.867405	-0.073619	4.818362
369.770274	7999.973533	10.872410	-0.073654	4.818365
369.971762	7999.959426	10.877415	-0.073692	4.818360
369.854725	7999.962059	10.882419	-0.073670	4.818362
369.941998	7999.952724	10.887424	-0.073686	4.818359
369.917569	7999.926136	10.892429	-0.073682	4.818351
369.958432	7999.980255	10.897434	-0.073689	4.818367
369.812610	7999.958342	10.902439	-0.073662	4.818361
369.985448	7999.971162	10.907443	-0.073694	4.818364
369.978364	7999.988924	10.912448	-0.073693	4.818369
369.834746	7999.951284	10.917453	-0.073666	4.818359
370.004965	7999.986129	10.922458	-0.073698	4.818368
370.151685	7999.946078	10.927463	-0.073725	4.818356
369.813521	7999.937343	10.932467	-0.073662	4.818354
370.067319	7999.955451	10.937472	-0.073709	4.818359
369.985292	7999.940695	10.942477	-0.073694	4.818355
370.209164	7999.998318	10.947482	-0.073736	4.818371
369.930982	7999.955723	10.952487	-0.073684	4.818359
369.991003	7999.955477	10.957491	-0.073695	4.818359
370.100073	7999.961140	10.962496	-0.073716	4.818360
369.888066	7999.934138	10.967501	-0.073676	4.818353
369.943329	7999.975845	10.972506	-0.073686	4.818365
370.025594	7999.960141	10.977511	-0.073702	4.818360
370.046202	7999.940458	10.982515	-0.073705	4.818354
370.068199	7999.920795	10.987520	-0.073710	4.818349
370.141202	7999.909168	10.992525	-0.073723	4.818345
370.224602	7999.958605	10.997530	-0.073739	4.818359
370.174964	7999.941133	11.002535	-0.073729	4.818354
369.971108	7999.965711	11.007539	-0.073691	4.818362
370.168391	7999.985162	11.012544	-0.073728	4.818367
370.163934	7999.978799	11.017549	-0.073727	4.818365
370.093246	7999.972599	11.022554	-0.073714	4.818364
370.194603	7999.921436	11.027559	-0.073733	4.818348
370.120430	7999.967711	11.032563	-0.073719	4.818362
370.298810	7999.969051	11.037568	-0.073752	4.818362
370.126574	7999.941532	11.042573	-0.073720	4.818354
370.087282	7999.999829	11.047578	-0.073713	4.818372
370.194686	7999.949797	11.052583	-0.073733	4.818357
370.208589	7999.937378	11.057587	-0.073736	4.818353
370.272541	7999.966596	11.062592	-0.073748	4.818361
370.262048	7999.925488	11.067597	-0.073746	4.818349
370.292497	7999.998376	11.072602	-0.073751	4.818371
370.194330	7999.946639	11.077607	-0.073733	4.818356
370.350802	7999.964493	11.082611	-0.073762	4.818360
370.330235	7999.987326	11.087616	-0.073758	4.818367
370.244883	7999.949417	11.092621	-0.073742	4.818356
370.369923	7999.973152	11.097626	-0.073766	4.818363
370.299111	7999.957496	11.102631	-0.073752	4.818359
370.339176	7999.932822	11.107635	-0.073760	4.818351
370.490742	7999.960064	11.112640	-0.073788	4.818359
370.116716	7999.905680	11.117645	-0.073718	4.818344
370.150046	7999.978606	11.122650	-0.073725	4.818365
370.189652	7999.972834	11.127655	-0.073732	4.818364
370.180992	7999.976919	11.132659	-0.073730	4.818365
370.293093	7999.977371	11.137664	-0.073751	4.818364
370.253540	7999.930621	11.142669	-0.073744	4.818351
370.191713	7999.960255	11.147674	-0.073732	4.818360
370.302489	7999.964891	11.152679	-0.073753	4.818361
370.207227	7999.928949	11.157683	-0.073735	4.818350
370.515405	7999.926777	11.162688	-0.073793	4.818349
370.431645	7999.913049	11.167693	-0.073777	4.818345
370.599141	7999.962564	11.172698	-0.073808	4.818359
370.535028	7999.949099	11.177703	-0.073796	4.818355
370.573865	7999.975880	11.182707	-0.073804	4.818363
370.449264	7999.976310	11.187712	-0.073780	4.818364
370.340104	7999.913921	11.192717	-0.073760	4.818345
370.419825	7999.959107	11.197722	-0.073775	4.818359
370.473771	7999.943023	11.202727	-0.073785	4.818354
370.384262	7999.932369	11.207731	-0.073768	4.818351
370.385547	7999.961798	11.212736	-0.073768	4.818359
370.413412	7999.934860	11.217741	-0.073774	4.818351
370.302433	7999.995348	11.222746	-0.073753	4.818370
370.259699	8000.004228	11.227751	-0.073745	4.818373
370.453798	7999.967964	11.232755	-0.073781	4.818361
370.339226	7999.962226	11.237760	-0.073760	4.818360
369.929632	7999.979844	11.242765	-0.073684	4.818367
369.934458	8000.000917	11.247770	-0.073684	4.818373
370.534315	7999.957487	11.252775	-0.073796	4.818358
370.476304	7999.959861	11.257779	-0.073785	4.818359
370.288898	7999.977306	11.262784	-0.073750	4.818364
370.498922	7999.949659	11.267789	-0.073789	4.818355
370.346101	7999.973870	11.272794	-0.073761	4.818363
370.218325	7999.953249	11.277799	-0.073737	4.818358
370.429766	7999.955033	11.282803	-0.073777	4.818357
370.592884	7999.967724	11.287808	-0.073807	4.818360
370.424911	7999.949715	11.292813	-0.073776	4.818356
370.577284	8000.001128	11.297818	-0.073804	4.818370
370.549677	7999.961892	11.302823	-0.073799	4.818359
370.360973	7999.983521	11.307827	-0.073764	4.818366
370.527719	8000.007816	11.312832	-0.073795	4.818373
370.490221	7999.965295	11.317837	-0.073788	4.818360
370.384389	7999.984885	11.322842	-0.073768	4.818366
370.335160	7999.963216	11.327847	-0.073759	4.818360
370.260373	7999.990574	11.332851	-0.073745	4.818369
370.484486	8000.009335	11.337856	-0.073787	4.818373
370.412234	8000.008366	11.342861	-0.073773	4.818373
370.549085	8000.033311	11.347866	-0.073799	4.818380
370.536231	7999.993221	11.352871	-0.073796	4.818368
370.395412	8000.009190	11.357875	-0.073770	4.818374
370.462948	8000.010095	11.362880	-0.073783	4.818374
370.555159	7999.981919	11.367885	-0.073800	4.818365
370.554769	7999.966157	11.372890	-0.073800	4.818360
370.659702	7999.941302	11.377895	-0.073819	4.818352
370.693364	7999.934400	11.382899	-0.073826	4.818350
370.532548	8000.004724	11.387904	-0.073796	4.818372
370.427084	7999.971796	11.392909	-0.073776	4.818362
370.413721	7999.987373	11.397914	-0.073774	4.818367
370.653227	7999.956970	11.402919	-0.073818	4.818357
370.688981	7999.988963	11.407923	-0.073825	4.818366
370.545574	7999.988090	11.412928	-0.073798	4.818367
370.792715	7999.947285	11.417933	-0.073844	4.818354
370.755039	7999.933123	11.422938	-0.073837	4.818349
370.567549	7999.974728	11.427943	-0.073802	4.818363
370.458314	7999.971162	11.432947	-0.073782	4.818362
370.716936	7999.980932	11.437952	-0.073830	4.818364
370.704959	7999.967115	11.442957	-0.073828	4.818360
370.771253	7999.985861	11.447962	-0.073840	4.818365
370.949028	7999.950429	11.452967	-0.073873	4.818354
370.674265	7999.941492	11.457971	-0.073822	4.818352
370.569559	8000.006265	11.462976	-0.073802	4.818372
370.337093	8000.001047	11.467981	-0.073759	4.818371
370.508322	8000.016999	11.472986	-0.073791	4.818375
370.690737	7999.980578	11.477991	-0.073825	4.818364
370.486882	7999.967340	11.482995	-0.073787	4.818361
370.801202	8000.021975	11.488000	-0.073846	4.818376
370.613707	7999.937526	11.493005	-0.073811	4.818351
370.687840	7999.977386	11.498010	-0.073824	4.818363
370.665438	7999.978136	11.503015	-0.073820	4.818363
370.498540	7999.989553	11.508019	-0.073789	4.818367
370.532623	7999.997363	11.513024	-0.073796	4.818369
370.711097	7999.941982	11.518029	-0.073829	4.818352
371.091281	7999.965987	11.523034	-0.073900	4.818358
370.913709	7999.958353	11.528039	-0.073866	4.818356
370.844831	7999.974237	11.533043	-0.073854	4.818361
370.985970	7999.993987	11.538048	-0.073880	4.818367
370.932023	7999.942841	11.543053	-0.073870	4.818352
370.802123	8000.005176	11.548058	-0.073846	4.818371
370.913163	7999.964647	11.553063	-0.073866	4.818358
371.047442	7999.968548	11.558067	-0.073891	4.818359
370.891345	7999.985363	11.563072	-0.073862	4.818364
370.818197	7999.956019	11.568077	-0.073849	4.818356
371.024527	7999.988199	11.573082	-0.073887	4.818365
370.968400	7999.961184	11.578087	-0.073877	4.818357
370.952571	7999.977779	11.583091	-0.073874	4.818362
371.120196	7999.945362	11.588096	-0.073905	4.818352
370.927519	7999.927021	11.593101	-0.073869	4.818347
371.087268	7999.974332	11.598106	-0.073899	4.818360
371.124284	7999.914952	11.603111	-0.073906	4.818343
371.054238	7999.927668	11.608115	-0.073893	4.818347
371.081813	7999.953249	11.613120	-0.073898	4.818354
370.942504	7999.941926	11.618125	-0.073872	4.818351
371.135765	7999.965527	11.623130	-0.073908	4.818358
371.052217	7999.943397	11.628135	-0.073892	4.818351
370.977958	7999.969712	11.633139	-0.073878	4.818359
371.088813	7999.981703	11.638144	-0.073899	4.818363
370.902594	7999.937187	11.643149	-0.073864	4.818350
370.999020	7999.977347	11.648154	-0.073882	4.818362
371.034564	7999.949461	11.653159	-0.073889	4.818353
371.041724	7999.962162	11.658163	-0.073890	4.818357
371.010716	7999.989058	11.663168	-0.073884	4.818365
371.046753	7999.954876	11.668173	-0.073891	4.818355
371.312615	7999.946886	11.673178	-0.073941	4.818351
371.273819	7999.968425	11.678183	-0.073933	4.818358
370.924669	7999.924875	11.683187	-0.073868	4.818346
371.113619	7999.967326	11.688192	-0.073904	4.818358
371.208286	7999.941283	11.693197	-0.073921	4.818350
371.127024	7999.962253	11.698202	-0.073906	4.818357
370.943440	7999.980799	11.703207	-0.073872	4.818363
371.093492	7999.969156	11.708211	-0.073900	4.818359
370.998267	7999.997291	11.713216	-0.073882	4.818368
370.899285	7999.961298	11.718221	-0.073864	4.818357
371.223621	7999.983505	11.723226	-0.073924	4.818363
371.170743	7999.971241	11.728231	-0.073914	4.818359
371.027509	7999.973521	11.733235	-0.073887	4.818360
371.053919	7999.965471	11.738240	-0.073892	4.818358
371.121845	7999.929616	11.743245	-0.073905	4.818347
370.990186	7999.985625	11.748250	-0.073881	4.818364
371.064418	7999.944602	11.753255	-0.073894	4.818352
371.212923	7999.970754	11.758259	-0.073922	4.818359
371.138771	7999.981314	11.763264	-0.073908	4.818362
371.146712	7999.965663	11.768269	-0.073910	4.818358
370.989401	8000.007672	11.773274	-0.073880	4.818371
370.966806	7999.988461	11.778279	-0.073876	4.818365
370.979514	7999.965521	11.783283	-0.073878	4.818358
371.129008	8000.008493	11.788288	-0.073906	4.818370
371.024018	7999.952461	11.793293	-0.073887	4.818354
370.947622	7999.990303	11.798298	-0.073873	4.818366
371.112520	7999.973606	11.803303	-0.073903	4.818360
370.612252	7999.961645	11.808307	-0.073810	4.818359
370.585798	8000.034821	11.813312	-0.073805	4.818380
370.622952	8000.018512	11.818317	-0.073812	4.818375
370.660759	8000.047380	11.823322	-0.073819	4.818384
370.758993	8000.020335	11.828327	-0.073837	4.818375
370.961217	7999.990483	11.833331	-0.073875	4.818366
371.080796	8000.002591	11.838336	-0.073897	4.818369
371.037809	7999.978904	11.843341	-0.073889	4.818362
371.127590	7999.979057	11.848346	-0.073906	4.818362
370.997641	7999.973112	11.853351	-0.073882	4.818360
370.974505	7999.973852	11.858355	-0.073877	4.818361
371.118601	7999.994692	11.863360	-0.073904	4.818366
370.850030	7999.960627	11.868365	-0.073854	4.818357
370.917907	8000.014060	11.873370	-0.073867	4.818373
370.957874	7999.994637	11.878375	-0.073874	4.818367
371.057679	7999.952906	11.883379	-0.073893	4.818354
371.086678	7999.998464	11.888384	-0.073898	4.818368
370.829269	7999.993961	11.893389	-0.073850	4.818367
370.948905	8000.019726	11.898394	-0.073873	4.818374
371.069754	7999.998236	11.903399	-0.073895	4.818368
371.298861	7999.967694	11.908403	-0.073938	4.818358
371.172346	8000.013267	11.913408	-0.073914	4.818372
371.227192	7999.949925	11.918413	-0.073924	4.818353
371.522594	8000.012713	11.923418	-0.073980	4.818370
371.332618	7999.978650	11.928423	-0.073944	4.818361
371.291450	7999.966543	11.933427	-0.073936	4.818357
371.432193	7999.987338	11.938432	-0.073963	4.818363
371.259011	7999.982914	11.943437	-0.073930	4.818362
371.195546	7999.978911	11.948442	-0.073919	4.818361
371.121475	7999.959009	11.953447	-0.073905	4.818356
370.766676	8000.017278	11.958451	-0.073839	4.818374
371.265420	8000.022916	11.963456	-0.073932	4.818374
371.125488	7999.987424	11.968461	-0.073906	4.818364
371.212659	8000.022208	11.973466	-0.073922	4.818374
371.332916	7999.982852	11.978471	-0.073944	4.818362
371.198554	7999.965293	11.983475	-0.073919	4.818357
371.310077	8000.010908	11.988480	-0.073940	4.818370
371.237828	7999.986828	11.993485	-0.073926	4.818364
371.272908	8000.016711	11.998490	-0.073933	4.818372
371.190651	7999.992498	12.003495	-0.073918	4.818365
371.071639	8000.012961	12.008499	-0.073895	4.818372
371.245108	8000.017388	12.013504	-0.073928	4.818373
371.175612	7999.977588	12.018509	-0.073915	4.818361
371.400577	8000.029977	12.023514	-0.073957	4.818376
371.146993	8000.025525	12.028519	-0.073909	4.818375
371.195591	8000.003066	12.033523	-0.073919	4.818369
371.328345	7999.993292	12.038528	-0.073943	4.818365
371.300796	7999.975064	12.043533	-0.073938	4.818360
371.502317	8000.004028	12.048538	-0.073976	4.818368
371.283723	7999.980086	12.053543	-0.073935	4.818361
371.243309	7999.984796	12.058547	-0.073927	4.818363
371.360684	7999.997925	12.063552	-0.073949	4.818366
371.211416	7999.987519	12.068557	-0.073921	4.818364
371.209362	8000.012702	12.073562	-0.073921	4.818371
371.348532	8000.011417	12.078567	-0.073947	4.818370
371.262312	7999.974545	12.083571	-0.073931	4.818360
371.337648	7999.999716	12.088576	-0.073945	4.818367
371.160993	7999.984740	12.093581	-0.073912	4.818363
371.296779	8000.036983	12.098586	-0.073937	4.818378
371.293958	7999.997028	12.103591	-0.073937	4.818366
371.330030	7999.968098	12.108595	-0.073943	4.818358
371.395888	8000.014151	12.113600	-0.073956	4.818371
371.371309	7999.970752	12.118605	-0.073951	4.818358
371.450041	8000.006473	12.123610	-0.073966	4.818369
371.692584	7999.991869	12.128615	-0.074011	4.818363
371.378299	8000.024418	12.133619	-0.073952	4.818374
371.138359	8000.013846	12.138624	-0.073908	4.818372
370.837370	8000.012961	12.143629	-0.073852	4.818373
371.099671	8000.041689	12.148634	-0.073901	4.818380
371.083027	8000.021507	12.153639	-0.073897	4.818374
371.068144	8000.022357	12.158643	-0.073895	4.818375
371.413885	8000.021742	12.163648	-0.073959	4.818373
371.262219	8000.022859	12.168653	-0.073931	4.818374
371.314628	8000.026713	12.173658	-0.073941	4.818375
371.310061	8000.006692	12.178663	-0.073940	4.818369
371.343921	7999.980885	12.183667	-0.073946	4.818361
371.127028	7999.994783	12.188672	-0.073906	4.818366
371.210824	7999.983301	12.193677	-0.073921	4.818363
371.523924	7999.974895	12.198682	-0.073979	4.818359
371.577755	7999.976667	12.203687	-0.073989	4.818359
371.569099	7999.979702	12.208691	-0.073988	4.818360
371.741665	8000.017733	12.213696	-0.074020	4.818371
371.565033	7999.965990	12.218701	-0.073987	4.818356
371.501838	8000.012413	12.223706	-0.073975	4.818370
371.694860	7999.984539	12.228711	-0.074011	4.818361
371.747210	7999.945323	12.233715	-0.074021	4.818349
371.624666	7999.986748	12.238720	-0.073998	4.818362
371.696292	7999.979305	12.243725	-0.074012	4.818359
371.840474	7999.998046	12.248730	-0.074038	4.818364
371.794468	7999.983773	12.253735	-0.074030	4.818360
371.473671	8000.013083	12.258739	-0.073970	4.818370
371.553536	8000.032013	12.263744	-0.073985	4.818376
371.502056	7999.987202	12.268749	-0.073975	4.818363
371.549171	8000.021449	12.273754	-0.073984	4.818373
371.384974	7999.995085	12.278759	-0.073954	4.818365
371.517612	7999.973754	12.283763	-0.073978	4.818359
371.741658	7999.996718	12.288768	-0.074020	4.818364
371.598879	7999.988499	12.293773	-0.073993	4.818363
371.716189	7999.975366	12.298778	-0.074015	4.818358
371.749878	7999.968464	12.303783	-0.074021	4.818356
371.463353	7999.966721	12.308787	-0.073968	4.818357
371.589732	7999.982072	12.313792	-0.073992	4.818361
371.554702	7999.975299	12.318797	-0.073985	4.818359
371.642120	8000.006935	12.323802	-0.074001	4.818368
371.789302	7999.992102	12.328807	-0.074029	4.818363
371.795248	7999.992181	12.333811	-0.074030	4.818363
371.976098	7999.998809	12.338816	-0.074064	4.818364
371.678647	7999.967506	12.343821	-0.074008	4.818356
371.647143	7999.971285	12.348826	-0.074002	4.818357
371.460969	7999.988746	12.353831	-0.073968	4.818363
371.614539	7999.982402	12.358835	-0.073996	4.818361
371.582195	8000.001926	12.363840	-0.073990	4.818367
371.684430	7999.991742	12.368845	-0.074009	4.818363
371.705714	8000.010936	12.373850	-0.074013	4.818369
371.713846	8000.000540	12.378855	-0.074015	4.818366
371.695348	7999.963525	12.383859	-0.074011	4.818355
371.547180	7999.998304	12.388864	-0.073984	4.818366
371.609522	7999.948717	12.393869	-0.073995	4.818351
371.587750	7999.978888	12.398874	-0.073991	4.818360
371.675955	7999.980071	12.403879	-0.074008	4.818360
371.427516	7999.965183	12.408883	-0.073961	4.818356
371.581348	8000.004012	12.413888	-0.073990	4.818367
371.625341	7999.957331	12.418893	-0.073998	4.818353
371.674675	7999.986355	12.423898	-0.074007	4.818362
371.505697	8000.000896	12.428903	-0.073976	4.818367
371.664070	8000.007222	12.433907	-0.074005	4.818368
371.797235	8000.022664	12.438912	-0.074030	4.818372
371.620058	7999.991924	12.443917	-0.073997	4.818364
371.748836	8000.003106	12.448922	-0.074021	4.818366
371.739632	7999.983023	12.453927	-0.074019	4.818360
371.489615	7999.992274	12.458931	-0.073973	4.818364
371.555495	8000.024672	12.463936	-0.073985	4.818374
371.636707	7999.987944	12.468941	-0.074000	4.818362
371.488696	8000.030077	12.473946	-0.073973	4.818375
371.437808	7999.995780	12.478951	-0.073963	4.818365
371.611355	7999.985502	12.483955	-0.073995	4.818362
371.793632	8000.011057	12.488960	-0.074029	4.818369
371.579913	7999.964070	12.493965	-0.073990	4.818355
371.799709	8000.003785	12.498970	-0.074031	4.818366
371.580530	8000.019752	12.503975	-0.073990	4.818372
371.627898	7999.959460	12.508979	-0.073999	4.818354
371.705430	8000.016175	12.513984	-0.074013	4.818370
371.921216	7999.959193	12.518989	-0.074053	4.818353
371.690975	7999.991819	12.523994	-0.074010	4.818363
371.797609	7999.997452	12.528999	-0.074030	4.818364
371.655550	8000.008151	12.534003	-0.074004	4.818368
371.811038	7999.970319	12.539008	-0.074033	4.818356
371.687180	7999.990717	12.544013	-0.074010	4.818363
371.739377	8000.010325	12.549018	-0.074019	4.818369
371.803488	8000.001731	12.554023	-0.074031	4.818366
371.661122	8000.010325	12.559027	-0.074005	4.818369
371.805440	7999.990201	12.564032	-0.074032	4.818362
371.770056	7999.942455	12.569037	-0.074025	4.818348
371.817922	8000.001923	12.574042	-0.074034	4.818366
371.837300	8000.004283	12.579047	-0.074037	4.818366
371.775599	8000.012910	12.584051	-0.074026	4.818369
372.012263	8000.016085	12.589056	-0.074070	4.818369
371.783942	7999.979406	12.594061	-0.074028	4.818359
371.899674	7999.990412	12.599066	-0.074049	4.818362
372.047935	8000.003957	12.604071	-0.074077	4.818365
371.878572	7999.963867	12.609075	-0.074045	4.818354
372.013459	8000.003493	12.614080	-0.074070	4.818365
371.837987	7999.934959	12.619085	-0.074038	4.818346
371.817585	7999.970401	12.624090	-0.074034	4.818356
371.726607	7999.982836	12.629095	-0.074017	4.818360
371.916769	8000.001144	12.634099	-0.074052	4.818365
371.831054	8000.036760	12.639104	-0.074036	4.818376
371.970007	7999.970343	12.644109	-0.074062	4.818356
371.869909	7999.998413	12.649114	-0.074043	4.818364
372.038052	7999.975458	12.654119	-0.074075	4.818357
371.813911	7999.941986	12.659123	-0.074033	4.818348
371.912337	7999.994780	12.664128	-0.074051	4.818363
371.844416	7999.953950	12.669133	-0.074039	4.818351
371.767253	7999.986529	12.674138	-0.074024	4.818361
371.722936	7999.998540	12.679143	-0.074016	4.818365
371.784659	7999.990964	12.684147	-0.074028	4.818363
372.093976	8000.007720	12.689152	-0.074085	4.818366
371.897534	7999.987226	12.694157	-0.074049	4.818361
371.833681	7999.996873	12.699162	-0.074037	4.818364
371.795804	7999.995314	12.704167	-0.074030	4.818364
371.796941	7999.992178	12.709171	-0.074030	4.818363
371.766034	8000.012772	12.714176	-0.074024	4.818369
371.877108	7999.999555	12.719181	-0.074045	4.818365
371.858433	7999.998254	12.724186	-0.074041	4.818364
371.938926	8000.002485	12.729191	-0.074056	4.818365
371.837904	7999.972767	12.734195	-0.074037	4.818357
372.030964	8000.016325	12.739200	-0.074073	4.818369
372.066624	7999.925412	12.744205	-0.074080	4.818342
372.026901	7999.986857	12.749210	-0.074073	4.818360
372.080566	7999.961314	12.754215	-0.074083	4.818353
371.835833	7999.958030	12.759219	-0.074037	4.818353
371.856973	7999.943607	12.764224	-0.074041	4.818348
371.810456	7999.970295	12.769229	-0.074032	4.818356
372.066613	8000.003145	12.774234	-0.074080	4.818365
372.228435	7999.982205	12.779239	-0.074110	4.818358
371.892978	7999.940937	12.784243	-0.074048	4.818347
372.209533	7999.955689	12.789248	-0.074107	4.818350
372.084966	7999.954017	12.794253	-0.074083	4.818350
371.875507	7999.984822	12.799258	-0.074044	4.818360
371.979685	7999.980967	12.804263	-0.074064	4.818359
371.948003	7999.953229	12.809267	-0.074058	4.818351
372.076166	7999.998018	12.814272	-0.074082	4.818364
372.008250	7999.970844	12.819277	-0.074069	4.818356
372.052216	7999.961980	12.824282	-0.074077	4.818353
372.032984	7999.977478	12.829287	-0.074074	4.818358
371.795675	7999.971143	12.834291	-0.074029	4.818357
371.942224	8000.002522	12.839296	-0.074057	4.818365
371.850368	7999.988683	12.844301	-0.074040	4.818362
371.810334	7999.974490	12.849306	-0.074032	4.818358
372.043927	7999.994431	12.854311	-0.074076	4.818363
372.089792	7999.959330	12.859315	-0.074084	4.818352
372.063164	8000.007294	12.864320	-0.074079	4.818366
371.844384	7999.991753	12.869325	-0.074038	4.818363
371.946403	8000.005727	12.874330	-0.074057	4.818366
371.911411	7999.995803	12.879335	-0.074051	4.818364
371.736672	7999.994508	12.884339	-0.074018	4.818364
371.814146	8000.022860	12.889344	-0.074033	4.818372
371.839619	7999.990636	12.894349	-0.074038	4.818362
371.886570	8000.026982	12.899354	-0.074046	4.818373
372.029575	8000.007891	12.904359	-0.074073	4.818367
371.865864	7999.984685	12.909363	-0.074042	4.818360
372.044018	8000.028043	12.914368	-0.074076	4.818373
371.932506	8000.001335	12.919373	-0.074055	4.818365
372.080270	8000.014873	12.924378	-0.074082	4.818369
371.829915	8000.015715	12.929383	-0.074036	4.818370
371.881836	7999.986998	12.934387	-0.074045	4.818361
372.025313	8000.035144	12.939392	-0.074072	4.818375
372.041417	7999.992290	12.944397	-0.074075	4.818362
371.991782	7999.996876	12.949402	-0.074066	4.818364
371.996422	7999.995888	12.954407	-0.074067	4.818363
372.122645	7999.973420	12.959411	-0.074090	4.818356
372.198649	8000.002802	12.964416	-0.074104	4.818364
371.925863	7999.952921	12.969421	-0.074054	4.818351
372.221319	7999.985248	12.974426	-0.074109	4.818359
372.039710	8000.000669	12.979431	-0.074075	4.818364
371.754993	8000.006302	12.984435	-0.074022	4.818367
371.913009	8000.047290	12.989440	-0.074051	4.818379
372.085625	7999.981325	12.994445	-0.074083	4.818359
371.872519	8000.036241	12.999450	-0.074044	4.818376
372.036349	8000.002723	13.004455	-0.074074	4.818365
371.669216	8000.007251	13.009459	-0.074006	4.818368
371.869844	7999.999437	13.014464	-0.074043	4.818365
371.920784	7999.973859	13.019469	-0.074053	4.818357
371.986444	8000.016758	13.024474	-0.074065	4.818369
371.937654	8000.026608	13.029479	-0.074056	4.818373
371.800694	7999.995357	13.034483	-0.074030	4.818364
372.038052	8000.010096	13.039488	-0.074074	4.818367
371.983550	8000.012516	13.044493	-0.074064	4.818368
371.938211	8000.024513	13.049498	-0.074056	4.818372
372.069768	8000.005269	13.054503	-0.074080	4.818366
371.932472	7999.995022	13.059507	-0.074055	4.818363
372.024934	8000.022524	13.064512	-0.074072	4.818371
372.001619	7999.969687	13.069517	-0.074068	4.818355
372.235375	7999.965470	13.074522	-0.074111	4.818353
372.356952	7999.968152	13.079527	-0.074134	4.818354
372.167721	7999.930946	13.084531	-0.074098	4.818343
372.275331	7999.927138	13.089536	-0.074118	4.818342
372.314036	7999.946565	13.094541	-0.074126	4.818347
372.389441	7999.982243	13.099546	-0.074140	4.818358
372.433371	8000.005943	13.104551	-0.074148	4.818364
372.252496	7999.961496	13.109555	-0.074114	4.818352
372.384782	7999.995836	13.114560	-0.074139	4.818362
372.282099	7999.969246	13.119565	-0.074120	4.818354
372.482788	7999.981393	13.124570	-0.074157	4.818357
372.367760	7999.986152	13.129575	-0.074136	4.818359
372.325629	7999.949869	13.134579	-0.074128	4.818348
372.479761	7999.992907	13.139584	-0.074157	4.818360
372.607968	7999.972567	13.144589	-0.074180	4.818354
372.534417	7999.968428	13.149594	-0.074167	4.818353
372.338708	8000.000467	13.154599	-0.074130	4.818363
372.191219	7999.945963	13.159603	-0.074103	4.818348
372.565648	7999.975149	13.164608	-0.074172	4.818355
372.227742	7999.960109	13.169613	-0.074110	4.818352
372.208376	7999.976656	13.174618	-0.074106	4.818357
372.387479	7999.995867	13.179623	-0.074139	4.818362
372.087513	7999.979236	13.184627	-0.074083	4.818358
372.214740	8000.021911	13.189632	-0.074107	4.818370
372.055170	8000.020820	13.194637	-0.074077	4.818370
371.997466	8000.032651	13.199642	-0.074067	4.818374
371.961242	8000.030064	13.204647	-0.074060	4.818374
371.901471	8000.011403	13.209651	-0.074049	4.818368
371.925178	8000.056892	13.214656	-0.074053	4.818382
372.050671	8000.018657	13.219661	-0.074077	4.818370
372.052279	8000.015527	13.224666	-0.074077	4.818369
372.248386	8000.004502	13.229671	-0.074113	4.818365
372.151856	7999.979045	13.234675	-0.074095	4.818358
372.131103	8000.032341	13.239680	-0.074092	4.818374
372.186149	8000.008918	13.244685	-0.074102	4.818366
372.214419	7999.993540	13.249690	-0.074107	4.818362
372.188506	8000.001596	13.254695	-0.074102	4.818364
372.183208	7999.951101	13.259699	-0.074101	4.818349
372.341771	8000.015207	13.264704	-0.074131	4.818368
372.037533	8000.006922	13.269709	-0.074074	4.818366
372.113829	8000.004794	13.274714	-0.074088	4.818365
372.001062	8000.007482	13.279719	-0.074067	4.818367
371.975808	7999.999790	13.284723	-0.074063	4.818364
372.075305	8000.015831	13.289728	-0.074081	4.818369
372.104230	8000.015169	13.294733	-0.074086	4.818369
372.140064	8000.009346	13.299738	-0.074093	4.818367
371.865529	8000.002511	13.304743	-0.074042	4.818366
371.813313	7999.980800	13.309747	-0.074032	4.818359
371.882904	8000.045813	13.314752	-0.074045	4.818379
371.876800	7999.985853	13.319757	-0.074044	4.818361
371.930824	8000.029647	13.324762	-0.074054	4.818374
372.093882	8000.029734	13.329767	-0.074085	4.818373
371.991469	8000.015754	13.334771	-0.074065	4.818369
372.038879	8000.025844	13.339776	-0.074074	4.818372
372.238194	7999.973893	13.344781	-0.074111	4.818356
372.509494	8000.021654	13.349786	-0.074162	4.818369
372.387610	8000.024220	13.354791	-0.074139	4.818370
372.307179	7999.987424	13.359795	-0.074124	4.818359
372.557787	8000.026503	13.364800	-0.074171	4.818370
371.921900	8000.019020	13.369805	-0.074052	4.818370
372.211509	8000.015552	13.374810	-0.074106	4.818368
372.332513	8000.017176	13.379815	-0.074129	4.818368
372.556136	7999.973955	13.384819	-0.074171	4.818354
372.403570	8000.014977	13.389824	-0.074142	4.818367
372.356020	7999.977572	13.394829	-0.074133	4.818356
372.546699	8000.005342	13.399834	-0.074169	4.818364
372.473617	8000.002260	13.404839	-0.074155	4.818363
372.378474	7999.969468	13.409843	-0.074137	4.818354
372.238547	8000.014862	13.414848	-0.074111	4.818368
372.386774	7999.955922	13.419853	-0.074139	4.818350
372.421519	8000.021519	13.424858	-0.074145	4.818369
372.516755	8000.004938	13.429863	-0.074163	4.818364
372.566109	7999.990893	13.434867	-0.074172	4.818359
372.493168	8000.029833	13.439872	-0.074159	4.818371
372.499975	7999.963743	13.444877	-0.074160	4.818352
372.564055	8000.001370	13.449882	-0.074172	4.818363
372.447126	8000.002951	13.454887	-0.074150	4.818364
372.495902	7999.959485	13.459891	-0.074159	4.818350
372.618748	8000.026264	13.464896	-0.074182	4.818370
372.616931	7999.991573	13.469901	-0.074182	4.818359
372.442010	8000.012336	13.474906	-0.074149	4.818366
372.531383	8000.009333	13.479911	-0.074166	4.818365
372.515000	7999.967093	13.484915	-0.074163	4.818353
372.343826	8000.055137	13.489920	-0.074131	4.818379
372.343683	7999.991055	13.494925	-0.074131	4.818360
372.345716	8000.001587	13.499930	-0.074131	4.818364
372.465817	8000.044168	13.504935	-0.074154	4.818376
372.214381	8000.032389	13.509939	-0.074107	4.818373
372.126549	8000.036462	13.514944	-0.074090	4.818375
372.456205	8000.020927	13.519949	-0.074152	4.818369
372.328068	8000.036015	13.524954	-0.074128	4.818374
372.491111	8000.032950	13.529959	-0.074158	4.818372
372.322857	8000.012833	13.534963	-0.074127	4.818367
372.119919	8000.074189	13.539968	-0.074089	4.818386
372.246979	8000.022319	13.544973	-0.074113	4.818370
372.346976	8000.000550	13.549978	-0.074131	4.818363
372.678103	8000.006045	13.554983	-0.074193	4.818364
372.486293	7999.964602	13.559987	-0.074157	4.818352
372.696159	7999.989478	13.564992	-0.074196	4.818359
372.352401	7999.984864	13.569997	-0.074132	4.818359
372.394697	7999.973876	13.575002	-0.074140	4.818355
372.422395	7999.972147	13.580007	-0.074145	4.818354
372.564349	7999.968799	13.585011	-0.074172	4.818353
372.739333	8000.004763	13.590016	-0.074204	4.818363
372.478744	7999.965548	13.595021	-0.074156	4.818352
372.460146	8000.002066	13.600026	-0.074152	4.818363
372.599451	8000.007086	13.605031	-0.074178	4.818364
372.334544	7999.974117	13.610035	-0.074129	4.818355
372.275218	8000.022693	13.615040	-0.074118	4.818370
372.286107	7999.995526	13.620045	-0.074120	4.818362
372.286942	8000.003941	13.625050	-0.074120	4.818364
372.327139	8000.008682	13.630055	-0.074128	4.818366
372.597088	7999.993396	13.635059	-0.074178	4.818360
372.657796	8000.021524	13.640064	-0.074189	4.818368
372.501959	7999.994220	13.645069	-0.074160	4.818361
372.405811	7999.993979	13.650074	-0.074142	4.818361
372.248207	8000.007621	13.655079	-0.074113	4.818366
372.016381	7999.999257	13.660083	-0.074070	4.818364
372.553342	7999.991756	13.665088	-0.074170	4.818360
372.489716	7999.981448	13.670093	-0.074158	4.818357
372.492201	7999.989885	13.675098	-0.074158	4.818359
372.612330	7999.994648	13.680103	-0.074181	4.818360
372.546350	7999.983257	13.685107	-0.074168	4.818357
372.816693	7999.990037	13.690112	-0.074219	4.818358
372.600565	7999.965075	13.695117	-0.074178	4.818352
372.456633	8000.002011	13.700122	-0.074152	4.818363
372.519620	8000.037523	13.705127	-0.074163	4.818374
372.517553	8000.007030	13.710131	-0.074163	4.818364
372.647199	8000.017174	13.715136	-0.074187	4.818367
372.528738	7999.999826	13.720141	-0.074165	4.818362
372.614126	8000.012527	13.725146	-0.074181	4.818366
372.470763	7999.999047	13.730151	-0.074154	4.818362
372.357518	7999.958659	13.735155	-0.074133	4.818351
372.393864	8000.008520	13.740160	-0.074140	4.818365
372.483845	7999.974010	13.745165	-0.074157	4.818355
372.564562	7999.981396	13.750170	-0.074172	4.818357
372.626614	8000.007440	13.755175	-0.074183	4.818364
372.608510	7999.985137	13.760179	-0.074180	4.818358
372.509154	8000.018469	13.765184	-0.074161	4.818368
372.677512	7999.971355	13.770189	-0.074193	4.818353
372.725072	7999.990902	13.775194	-0.074202	4.818359
372.698943	8000.001056	13.780199	-0.074197	4.818362
372.504700	7999.965883	13.785203	-0.074161	4.818352
372.699796	8000.004218	13.790208	-0.074197	4.818363
372.581817	8000.028897	13.795213	-0.074175	4.818371
372.551151	8000.032687	13.800218	-0.074169	4.818372
372.670420	8000.043742	13.805223	-0.074191	4.818375
372.694661	8000.004148	13.810227	-0.074196	4.818363
372.468511	8000.043132	13.815232	-0.074154	4.818375
372.392272	8000.013745	13.820237	-0.074140	4.818367
372.314932	8000.044221	13.825242	-0.074125	4.818376
372.270595	8000.091948	13.830247	-0.074117	4.818391
372.334568	8000.032929	13.835251	-0.074129	4.818373
372.513923	8000.070002	13.840256	-0.074162	4.818383
372.534552	8000.029309	13.845261	-0.074166	4.818371
372.592142	7999.990163	13.850266	-0.074177	4.818359
372.677143	7999.978698	13.855271	-0.074193	4.818355
372.383998	7999.982117	13.860275	-0.074138	4.818358
372.414296	8000.030845	13.865280	-0.074144	4.818372
372.318521	7999.999095	13.870285	-0.074126	4.818363
372.519562	8000.008096	13.875290	-0.074163	4.818365
372.413079	8000.019273	13.880295	-0.074143	4.818369
372.301000	8000.019869	13.885299	-0.074123	4.818369
372.674647	8000.047995	13.890304	-0.074192	4.818376
372.538461	8000.019904	13.895309	-0.074167	4.818368
372.317201	8000.031641	13.900314	-0.074126	4.818373
372.775238	8000.020980	13.905319	-0.074211	4.818368
372.913225	7999.968207	13.910323	-0.074236	4.818351
372.820324	8000.036292	13.915328	-0.074219	4.818372
372.813223	8000.021489	13.920333	-0.074218	4.818368
372.703526	7999.977997	13.925338	-0.074197	4.818355
372.511571	8000.030045	13.930343	-0.074162	4.818371
372.095226	8000.045467	13.935347	-0.074084	4.818378
372.477993	8000.005433	13.940352	-0.074155	4.818364
372.323815	8000.005464	13.945357	-0.074127	4.818365
372.543430	8000.029421	13.950362	-0.074168	4.818371
372.578579	8000.031994	13.955367	-0.074174	4.818372
372.675275	8000.002827	13.960371	-0.074192	4.818363
372.449950	8000.015559	13.965376	-0.074150	4.818367
372.411594	8000.008741	13.970381	-0.074143	4.818365
372.663769	7999.981661	13.975386	-0.074190	4.818356
372.723723	8000.000324	13.980391	-0.074201	4.818362
372.594990	7999.991243	13.985395	-0.074177	4.818359
372.915147	8000.032307	13.990400	-0.074237	4.818370
372.846223	7999.978857	13.995405	-0.074224	4.818355
372.655644	8000.004662	14.000410	-0.074188	4.818363
372.738790	8000.006828	14.005415	-0.074204	4.818364
372.708994	7999.964408	14.010419	-0.074198	4.818351
372.766839	7999.994598	14.015424	-0.074209	4.818360
372.702832	7999.995839	14.020429	-0.074197	4.818360
372.853465	7999.997861	14.025434	-0.074225	4.818360
372.805184	8000.004566	14.030439	-0.074216	4.818363
372.601849	7999.985028	14.035443	-0.074178	4.818358
372.829817	8000.017502	14.040448	-0.074221	4.818366
372.805436	7999.969902	14.045453	-0.074216	4.818352
372.725891	7999.986692	14.050458	-0.074201	4.818358
372.774765	8000.012560	14.055463	-0.074211	4.818365
372.885711	7999.976231	14.060467	-0.074231	4.818354
372.867640	7999.996998	14.065472	-0.074228	4.818360
372.753377	7999.955545	14.070477	-0.074207	4.818348
372.796097	7999.950865	14.075482	-0.074215	4.818347
372.878777	7999.988742	14.080487	-0.074230	4.818358
372.558680	7999.960284	14.085491	-0.074170	4.818350
372.589795	8000.015327	14.090496	-0.074176	4.818367
372.772906	7999.974714	14.095501	-0.074210	4.818354
372.635867	8000.003339	14.100506	-0.074185	4.818363
372.554065	8000.006442	14.105511	-0.074169	4.818364
372.700881	7999.961140	14.110515	-0.074197	4.818350
372.864156	7999.951776	14.115520	-0.074227	4.818347
372.748201	7999.974381	14.120525	-0.074206	4.818354
372.785991	8000.008503	14.125530	-0.074213	4.818364
372.749376	8000.027971	14.130535	-0.074206	4.818370
372.673846	7999.975483	14.135539	-0.074192	4.818354
372.705895	8000.010579	14.140544	-0.074198	4.818365
372.905889	7999.981748	14.145549	-0.074235	4.818355
372.881939	8000.020295	14.150554	-0.074230	4.818367
372.788906	8000.013793	14.155559	-0.074213	4.818365
372.718898	7999.985540	14.160563	-0.074200	4.818357
372.753046	8000.019614	14.165568	-0.074206	4.818367
372.595197	7999.960768	14.170573	-0.074177	4.818350
372.692013	7999.956815	14.175578	-0.074195	4.818349
373.020302	7999.994837	14.180583	-0.074256	4.818359
372.696155	8000.000990	14.185587	-0.074196	4.818362
372.722682	8000.019205	14.190592	-0.074201	4.818367
372.748110	7999.984879	14.195597	-0.074205	4.818357
372.843818	7999.968305	14.200602	-0.074223	4.818352
372.918324	7999.998719	14.205607	-0.074237	4.818360
372.805946	8000.002462	14.210611	-0.074216	4.818362
373.045968	8000.011987	14.215616	-0.074261	4.818364
372.814721	7999.987873	14.220621	-0.074218	4.818358
372.844609	8000.004031	14.225626	-0.074223	4.818362
372.831733	8000.030120	14.230631	-0.074221	4.818370
372.538758	8000.007278	14.235635	-0.074166	4.818364
372.594774	7999.998575	14.240640	-0.074177	4.818362
372.805773	7999.991953	14.245645	-0.074216	4.818359
372.781373	8000.016837	14.250650	-0.074212	4.818366
372.596082	8000.029056	14.255655	-0.074177	4.818371
372.659300	7999.983683	14.260659	-0.074189	4.818357
372.814113	8000.026730	14.265664	-0.074218	4.818369
372.502819	8000.013096	14.270669	-0.074160	4.818366
372.710532	8000.016934	14.275674	-0.074198	4.818367
372.833450	8000.040645	14.280679	-0.074221	4.818373
372.666051	7999.993226	14.285683	-0.074190	4.818360
372.733621	7999.999385	14.290688	-0.074203	4.818361
373.009996	7999.982085	14.295693	-0.074254	4.818355
373.029797	7999.990754	14.300698	-0.074258	4.818358
373.048020	8000.008857	14.305703	-0.074261	4.818363
372.923445	7999.942053	14.310707	-0.074238	4.818344
372.900758	8000.001627	14.315712	-0.074234	4.818361
372.986698	7999.983871	14.320717	-0.074250	4.818356
372.815538	7999.993129	14.325722	-0.074218	4.818359
372.927239	7999.988325	14.330727	-0.074239	4.818357
372.975924	7999.985826	14.335731	-0.074248	4.818356
372.836376	7999.997609	14.340736	-0.074222	4.818360
372.823977	7999.984837	14.345741	-0.074219	4.818357
372.967525	7999.982561	14.350746	-0.074246	4.818355
372.882640	7999.998229	14.355751	-0.074230	4.818360
372.761432	7999.979794	14.360755	-0.074208	4.818355
373.005984	8000.012490	14.365760	-0.074253	4.818364
373.056017	7999.123409	14.370765	-0.074262	4.818100

372.985682	7996.052307	14.375770	-0.074247	4.817187
372.941814	7990.643869	14.380775	-0.074235	4.815579
372.925464	7983.982411	14.385779	-0.074228	4.813598
372.839305	7976.772079	14.390784	-0.074207	4.811453
372.884725	7969.169285	14.395789	-0.074211	4.809190
372.922850	7961.367708	14.400794	-0.074213	4.806866
372.821080	7953.460286	14.405799	-0.074189	4.804510
372.682743	7945.551113	14.410803	-0.074158	4.802153
372.620758	7937.556801	14.415808	-0.074141	4.799768
372.803323	7929.588185	14.420813	-0.074170	4.797390
372.701741	7921.552236	14.425818	-0.074146	4.794991
372.797040	7913.620804	14.430823	-0.074158	4.792621
372.705737	7905.597198	14.435827	-0.074136	4.790223
372.481769	7897.594989	14.440832	-0.074089	4.787831
372.533534	7889.534110	14.445837	-0.074093	4.785420
372.455323	7881.587488	14.450842	-0.074074	4.783041
372.527285	7873.631822	14.455847	-0.074082	4.780658
372.415909	7865.527189	14.460851	-0.074056	4.778230
372.595804	7857.580604	14.465856	-0.074084	4.775848
372.521390	7849.566754	14.470861	-0.074065	4.773444
372.288312	7841.525292	14.475866	-0.074016	4.771032
372.430875	7833.525830	14.480871	-0.074038	4.768630
372.340716	7825.527174	14.485875	-0.074016	4.766228
372.240010	7817.525228	14.490880	-0.073992	4.763823
372.202572	7809.598514	14.495885	-0.073980	4.761440
372.223808	7801.487470	14.500890	-0.073978	4.759000
372.004547	7793.607734	14.505895	-0.073932	4.756628
371.933206	7785.472049	14.510899	-0.073914	4.754179
372.107764	7777.552861	14.515904	-0.073941	4.751792
372.085844	7769.458999	14.520909	-0.073932	4.749352
371.800698	7761.555646	14.525914	-0.073873	4.746969
371.964578	7753.453892	14.530919	-0.073899	4.744524
371.911365	7745.535602	14.535923	-0.073884	4.742134
371.908241	7737.483226	14.540928	-0.073878	4.739701
371.887844	7729.508200	14.545933	-0.073869	4.737291
371.846679	7721.471049	14.550938	-0.073856	4.734861
371.913785	7713.540888	14.555943	-0.073863	4.732462
371.688205	7705.490182	14.560947	-0.073816	4.730025
371.856369	7697.496619	14.565952	-0.073842	4.727604
371.745701	7689.481758	14.570957	-0.073816	4.725176
371.543407	7681.492166	14.575962	-0.073773	4.722754
371.371549	7673.594395	14.580967	-0.073736	4.720359
371.231220	7665.520886	14.585971	-0.073705	4.717909
371.210918	7657.526261	14.590976	-0.073696	4.715482
371.491758	7649.466361	14.595981	-0.073743	4.713033
371.408257	7641.488923	14.600986	-0.073722	4.710608
371.600335	7633.534334	14.605991	-0.073753	4.708189
371.507787	7625.439936	14.610995	-0.073730	4.705726
371.406142	7617.489225	14.616000	-0.073706	4.703306
371.568664	7609.550875	14.621005	-0.073731	4.700888
371.356359	7601.502473	14.626010	-0.073686	4.698436
371.359436	7593.587099	14.631015	-0.073682	4.696023
371.445705	7585.496002	14.636019	-0.073692	4.693554
371.362201	7577.504723	14.641024	-0.073672	4.691115
371.229165	7569.480697	14.646029	-0.073642	4.688665
371.302181	7561.486020	14.651034	-0.073650	4.686223
371.305520	7553.503479	14.656039	-0.073645	4.683782
371.015400	7545.576442	14.661043	-0.073586	4.681358
371.081321	7537.483067	14.666048	-0.073593	4.678881
370.936753	7529.557662	14.671053	-0.073561	4.676455
370.787465	7521.454044	14.676058	-0.073528	4.673973
370.851805	7513.468183	14.681063	-0.073535	4.671525
370.872806	7505.446735	14.686067	-0.073534	4.669065
370.845423	7497.469127	14.691072	-0.073523	4.666618
370.722029	7489.422418	14.696077	-0.073495	4.664148
370.726317	7481.498016	14.701082	-0.073491	4.661714
370.862298	7473.447842	14.706087	-0.073511	4.659240
370.533986	7465.519436	14.711091	-0.073444	4.656802
370.715250	7457.458487	14.716096	-0.073473	4.654322
370.646509	7449.508228	14.721101	-0.073455	4.651875
370.613641	7441.428399	14.726106	-0.073444	4.649387
370.642862	7433.461285	14.731111	-0.073444	4.646932
370.620974	7425.403235	14.736115	-0.073434	4.644448
370.832407	7417.532506	14.741120	-0.073469	4.642020
370.616660	7409.434596	14.746125	-0.073423	4.639521
370.428946	7401.441182	14.751130	-0.073383	4.637053
370.643498	7393.435428	14.756135	-0.073418	4.634580
370.304779	7385.501328	14.761139	-0.073350	4.632127
370.389845	7377.439670	14.766144	-0.073360	4.629634
370.512207	7369.455893	14.771149	-0.073378	4.627163
370.411949	7361.355824	14.776154	-0.073354	4.624655
370.385145	7353.489755	14.781159	-0.073344	4.622219
370.318756	7345.391299	14.786163	-0.073326	4.619709
370.345832	7337.468133	14.791168	-0.073326	4.617252
370.354616	7329.419468	14.796173	-0.073322	4.614754
370.238040	7321.430839	14.801178	-0.073295	4.612274
370.353203	7313.385526	14.806183	-0.073311	4.609775
370.100185	7305.397013	14.811187	-0.073259	4.607292
369.991311	7297.371240	14.816192	-0.073234	4.604797
370.139432	7289.423132	14.821197	-0.073256	4.602324
370.029908	7281.403067	14.826202	-0.073230	4.599827
369.891618	7273.450662	14.831207	-0.073200	4.597350
369.806331	7265.422247	14.836211	-0.073178	4.594848
369.949863	7257.415219	14.841216	-0.073200	4.592352
369.885470	7249.360463	14.846221	-0.073183	4.589839
369.846835	7241.334022	14.851226	-0.073170	4.587334
369.919650	7233.344395	14.856231	-0.073179	4.584839
369.722925	7225.425462	14.861235	-0.073137	4.582364
369.868412	7217.339287	14.866240	-0.073159	4.579836
369.862950	7209.416037	14.871245	-0.073152	4.577357
369.756982	7201.308217	14.876250	-0.073127	4.574820
369.691711	7193.407015	14.881255	-0.073110	4.572345
369.593755	7185.323064	14.886259	-0.073087	4.569812
369.479518	7177.377151	14.891264	-0.073060	4.567320
369.488188	7169.323362	14.896269	-0.073056	4.564794
369.371285	7161.383298	14.901274	-0.073030	4.562302
369.666371	7153.385071	14.906279	-0.073079	4.559791
369.528470	7145.396284	14.911283	-0.073048	4.557280
369.316018	7137.359900	14.916288	-0.073004	4.554753
369.475905	7129.365893	14.921293	-0.073028	4.552239
369.486183	7121.316931	14.926298	-0.073025	4.549706
369.521399	7113.343617	14.931303	-0.073026	4.547195
369.254910	7105.311813	14.936307	-0.072971	4.544664
369.424059	7097.336359	14.941312	-0.072998	4.542150
369.308402	7089.332101	14.946317	-0.072971	4.539625
369.228553	7081.366647	14.951322	-0.072951	4.537111
369.306807	7073.335033	14.956327	-0.072960	4.534575
369.183045	7065.318644	14.961331	-0.072932	4.532042
369.124448	7057.284459	14.966336	-0.072916	4.529502
369.084799	7049.353304	14.971341	-0.072903	4.526993
369.054022	7041.245026	14.976346	-0.072892	4.524427
369.068122	7033.339028	14.981351	-0.072890	4.521923
368.772565	7025.266211	14.986355	-0.072829	4.519364
368.964687	7017.336762	14.991360	-0.072860	4.516851
368.855652	7009.334162	14.996365	-0.072834	4.514312
368.670165	7001.318254	15.001370	-0.072795	4.511768
368.785281	6993.293824	15.006375	-0.072811	4.509220
368.742351	6985.274675	15.011379	-0.072798	4.506672
368.772305	6977.210172	15.016384	-0.072798	4.504108
368.694739	6969.288863	15.021389	-0.072778	4.501588
368.697732	6961.255369	15.026394	-0.072774	4.499031
368.632700	6953.300766	15.031399	-0.072756	4.496497
368.559550	6945.240095	15.036403	-0.072737	4.493928
368.657287	6937.293563	15.041408	-0.072750	4.491395
368.603273	6929.222280	15.046413	-0.072735	4.488820
368.454836	6921.249751	15.051418	-0.072702	4.486275
368.489427	6913.245247	15.056423	-0.072703	4.483719
368.483721	6905.286852	15.061427	-0.072697	4.481175
368.444675	6897.235815	15.066432	-0.072685	4.478601
368.289615	6889.276846	15.071437	-0.072651	4.476054
368.438296	6881.228619	15.076442	-0.072673	4.473478
368.386011	6873.247207	15.081447	-0.072658	4.470922
368.261839	6865.198358	15.086451	-0.072630	4.468342
368.099973	6857.237487	15.091456	-0.072594	4.465788
368.163647	6849.232260	15.096461	-0.072601	4.463220
368.153305	6841.228819	15.101466	-0.072594	4.460651
368.315157	6833.279914	15.106471	-0.072619	4.458098
368.099047	6825.225630	15.111475	-0.072573	4.455508
368.273251	6817.242967	15.116480	-0.072601	4.452942
368.134188	6809.196930	15.121485	-0.072569	4.450352
368.148042	6801.219170	15.126490	-0.072567	4.447784
368.126847	6793.217511	15.131495	-0.072558	4.445206
367.965274	6785.225662	15.136499	-0.072522	4.442629
368.035347	6777.218317	15.141504	-0.072530	4.440047
368.184805	6769.262667	15.146509	-0.072553	4.437480
368.077356	6761.203706	15.151514	-0.072528	4.434878
367.898608	6753.260850	15.156519	-0.072489	4.432310
367.847188	6745.144803	15.161523	-0.072474	4.429686
367.915651	6737.193632	15.166528	-0.072482	4.427115
367.681171	6729.148178	15.171533	-0.072433	4.424509
367.670180	6721.173029	15.176538	-0.072426	4.421927
367.916932	6713.144038	15.181543	-0.072466	4.419326
367.666458	6705.199840	15.186547	-0.072415	4.416749
367.705777	6697.139684	15.191552	-0.072417	4.414134
367.629327	6689.183527	15.196557	-0.072397	4.411551
367.498046	6681.144682	15.201562	-0.072367	4.408939
367.297305	6673.220479	15.206567	-0.072325	4.406363
367.447725	6665.132155	15.211571	-0.072348	4.403733
367.623933	6657.213098	15.216576	-0.072375	4.401158
367.336813	6649.192523	15.221581	-0.072317	4.398545
367.338301	6641.229652	15.226586	-0.072312	4.395951
367.684808	6633.158412	15.231591	-0.072371	4.393322
367.424949	6625.215891	15.236595	-0.072317	4.390730
367.216906	6617.154719	15.241600	-0.072273	4.388098
367.451015	6609.212805	15.246605	-0.072312	4.385506
367.211052	6601.177266	15.251610	-0.072262	4.382878
367.180379	6593.271199	15.256615	-0.072251	4.380293
367.205923	6585.261792	15.261619	-0.072251	4.377673
367.224727	6577.194390	15.266624	-0.072249	4.375033
367.020271	6569.253809	15.271629	-0.072206	4.372431
367.053544	6561.229143	15.276634	-0.072206	4.369801
367.154731	6553.284927	15.281639	-0.072220	4.367197
366.925531	6545.280335	15.286643	-0.072172	4.364569
366.997221	6537.297806	15.291648	-0.072180	4.361948
366.897978	6529.297248	15.296653	-0.072157	4.359319
366.747205	6521.280881	15.301658	-0.072123	4.356683
366.942649	6513.292923	15.306663	-0.072155	4.354057
366.795223	6505.263475	15.311667	-0.072122	4.351413
366.819002	6497.181966	15.316672	-0.072121	4.348752
366.915070	6489.262848	15.321677	-0.072134	4.346143
366.873562	6481.196430	15.326682	-0.072121	4.343483
366.804456	6473.283206	15.331687	-0.072103	4.340872
366.575172	6465.198006	15.336691	-0.072055	4.338201
366.535246	6457.263581	15.341696	-0.072042	4.335580
366.713834	6449.248438	15.346701	-0.072070	4.332932
366.630545	6441.225631	15.351706	-0.072049	4.330278
366.502801	6433.254144	15.356711	-0.072020	4.327639
366.431945	6425.226793	15.361715	-0.072002	4.324981
366.323623	6417.275052	15.366720	-0.071977	4.322345
366.509214	6409.257758	15.371725	-0.072006	4.319689
366.340555	6401.276875	15.376730	-0.071969	4.317039
366.500907	6393.239923	15.381735	-0.071994	4.314373
366.257564	6385.249265	15.386739	-0.071943	4.311717
366.284776	6377.204984	15.391744	-0.071943	4.309043
366.321834	6369.229251	15.396749	-0.071945	4.306391
366.346047	6361.195923	15.401754	-0.071944	4.303718
366.278448	6353.263746	15.406759	-0.071926	4.301076
366.125332	6345.183262	15.411763	-0.071893	4.298383
366.257754	6337.214451	15.416768	-0.071912	4.295727
366.142994	6329.231014	15.421773	-0.071886	4.293063
366.165279	6321.172185	15.426778	-0.071884	4.290373
366.225357	6313.221089	15.431783	-0.071890	4.287718
366.053485	6305.170189	15.436787	-0.071853	4.285025
365.963306	6297.244404	15.441792	-0.071831	4.282374
366.074755	6289.197612	15.446797	-0.071847	4.279682
365.910081	6281.245657	15.451802	-0.071811	4.277018
365.886651	6273.201572	15.456807	-0.071801	4.274322
365.840314	6265.220018	15.461811	-0.071787	4.271646
365.993380	6257.161466	15.466816	-0.071811	4.268943
365.665033	6249.227906	15.471821	-0.071744	4.266277
365.693664	6241.174746	15.476826	-0.071744	4.263572
365.798175	6233.238672	15.481831	-0.071759	4.260906
365.580828	6225.178787	15.486835	-0.071713	4.258193
365.669847	6217.200331	15.491840	-0.071724	4.255508
365.586922	6209.185694	15.496845	-0.071704	4.252808
365.552192	6201.166399	15.501850	-0.071692	4.250106
365.462214	6193.198332	15.506855	-0.071670	4.247418
365.451393	6185.129337	15.511859	-0.071663	4.244695
365.439367	6177.240278	15.516864	-0.071655	4.242031
365.428464	6169.164924	15.521869	-0.071648	4.239303
365.143302	6161.191022	15.526874	-0.071590	4.236605
365.224306	6153.174875	15.531879	-0.071600	4.233894
365.372463	6145.201366	15.536883	-0.071622	4.231196
365.303337	6137.143950	15.541888	-0.071604	4.228466
365.349013	6129.198612	15.546893	-0.071607	4.225774
365.233259	6121.117188	15.551898	-0.071580	4.223032
365.163922	6113.194990	15.556903	-0.071562	4.220343
365.041674	6105.195043	15.561907	-0.071534	4.217625
365.159487	6097.178688	15.566912	-0.071551	4.214902
365.033619	6089.172729	15.571917	-0.071522	4.212178
364.926524	6081.109930	15.576922	-0.071497	4.209434
365.010219	6073.185430	15.581927	-0.071508	4.206737
365.099634	6065.123801	15.586931	-0.071519	4.203991
364.937859	6057.189381	15.591936	-0.071484	4.201284
364.889357	6049.197762	15.596941	-0.071469	4.198558
364.885766	6041.174175	15.601946	-0.071464	4.195819
364.871260	6033.162607	15.606951	-0.071456	4.193082
364.517993	6025.088505	15.611955	-0.071385	4.190318
364.736953	6017.103185	15.616960	-0.071420	4.187589
364.815024	6009.138835	15.621965	-0.071430	4.184865
364.572823	6001.128891	15.626970	-0.071379	4.182118
364.729519	5993.148523	15.631975	-0.071403	4.179385
364.601668	5985.185210	15.636979	-0.071374	4.176653
364.386870	5977.152954	15.641984	-0.071329	4.173894
364.510112	5969.209444	15.646989	-0.071347	4.171168
364.474431	5961.155089	15.651994	-0.071335	4.168400
364.528929	5953.151860	15.656999	-0.071340	4.165649
364.504762	5945.168556	15.662003	-0.071330	4.162902
364.370932	5937.199080	15.667008	-0.071300	4.160156
364.369534	5929.230061	15.672013	-0.071294	4.157411
364.323673	5921.157511	15.677018	-0.071281	4.154627
364.147467	5913.221894	15.682023	-0.071243	4.151887
364.214429	5905.160467	15.687027	-0.071250	4.149105
364.230935	5897.188536	15.692032	-0.071248	4.146352
364.217952	5889.183287	15.697037	-0.071240	4.143584
364.215846	5881.214566	15.702042	-0.071235	4.140828
364.145987	5873.239314	15.707047	-0.071216	4.138067
363.983070	5865.181979	15.712051	-0.071181	4.135274
364.200497	5857.185758	15.717056	-0.071216	4.132505
364.177328	5849.194222	15.722061	-0.071206	4.129733
364.064615	5841.209751	15.727066	-0.071180	4.126960
363.926966	5833.171466	15.732071	-0.071149	4.124167
363.808179	5825.223264	15.737075	-0.071122	4.121403
363.774520	5817.219656	15.742080	-0.071111	4.118619
363.672672	5809.244811	15.747085	-0.071086	4.115842
363.666880	5801.183744	15.752090	-0.071080	4.113035
363.828340	5793.189557	15.757095	-0.071105	4.110251
363.615909	5785.184444	15.762099	-0.071060	4.107457
363.703456	5777.147706	15.767104	-0.071071	4.104654
363.859905	5769.222668	15.772109	-0.071095	4.101889
363.511152	5761.153839	15.777114	-0.071025	4.099064
363.478851	5753.249111	15.782119	-0.071014	4.096300
363.370759	5745.156640	15.787123	-0.070988	4.093466
363.413000	5737.159862	15.792128	-0.070991	4.090667
363.441460	5729.178027	15.797133	-0.070991	4.087870
363.237759	5721.149046	15.802138	-0.070948	4.085052
363.354015	5713.218112	15.807143	-0.070964	4.082271
363.215447	5705.187736	15.812147	-0.070933	4.079449
363.275067	5697.210544	15.817152	-0.070939	4.076647
363.174257	5689.171087	15.822157	-0.070915	4.073819
363.020574	5681.207822	15.827162	-0.070881	4.071015
363.189147	5673.209684	15.832167	-0.070908	4.068201
363.080408	5665.152802	15.837171	-0.070882	4.065361
363.195873	5657.185715	15.842176	-0.070898	4.062554
363.044112	5649.189729	15.847181	-0.070865	4.059730
363.032382	5641.156130	15.852186	-0.070858	4.056894
363.057144	5633.183090	15.857191	-0.070857	4.054077
362.922673	5625.202310	15.862195	-0.070827	4.051253
362.894454	5617.164235	15.867200	-0.070816	4.048409
362.904545	5609.190943	15.872205	-0.070813	4.045586
362.882228	5601.210574	15.877210	-0.070804	4.042758
362.857292	5593.244725	15.882215	-0.070794	4.039933
362.867539	5585.219549	15.887219	-0.070790	4.037086
362.860746	5577.205204	15.892224	-0.070784	4.034240
362.742782	5569.163808	15.897229	-0.070757	4.031381
362.748604	5561.145344	15.902234	-0.070753	4.028530
362.719413	5553.175389	15.907239	-0.070742	4.025694
362.515475	5545.198959	15.912243	-0.070699	4.022850
362.532838	5537.236420	15.917248	-0.070697	4.020013
362.641549	5529.268260	15.922253	-0.070712	4.017174
362.374385	5521.227012	15.927258	-0.070657	4.014300
362.439176	5513.269617	15.932263	-0.070664	4.011459
362.353509	5505.214867	15.937267	-0.070642	4.008580
362.418657	5497.207702	15.942272	-0.070649	4.005717
362.269382	5489.257393	15.947277	-0.070616	4.002870
362.386200	5481.255701	15.952282	-0.070633	4.000006
362.164661	5473.330730	15.957287	-0.070587	3.997163
362.229732	5465.233273	15.962291	-0.070593	3.994260
362.306103	5457.245489	15.967296	-0.070602	3.991394
362.212585	5449.233399	15.972301	-0.070580	3.988515
362.055646	5441.219801	15.977306	-0.070545	3.985632
362.045067	5433.283901	15.982311	-0.070538	3.982778
362.020100	5425.237347	15.987315	-0.070528	3.979881
362.030387	5417.252990	15.992320	-0.070525	3.977006
361.949235	5409.240825	15.997325	-0.070505	3.974116
361.881022	5401.252057	16.002330	-0.070487	3.971233
361.972434	5393.256001	16.007335	-0.070498	3.968349
361.797737	5385.218536	16.012339	-0.070461	3.965442
361.809676	5377.264023	16.017344	-0.070458	3.962567
361.903322	5369.303410	16.022349	-0.070470	3.959688
361.817719	5361.290365	16.027354	-0.070449	3.956786
361.872655	5353.244247	16.032359	-0.070454	3.953872
361.809611	5345.253087	16.037363	-0.070437	3.950973
361.900415	5337.213518	16.042368	-0.070449	3.948058
361.826820	5329.205476	16.047373	-0.070430	3.945149
361.672877	5321.234139	16.052378	-0.070396	3.942250
361.634612	5313.259329	16.057383	-0.070383	3.939349
361.695096	5305.267286	16.062387	-0.070389	3.936442
361.467017	5297.212166	16.067392	-0.070342	3.933504
361.628566	5289.244715	16.072397	-0.070367	3.930603
361.609991	5281.228351	16.077402	-0.070358	3.927679
361.542108	5273.257334	16.082407	-0.070340	3.924769
361.452609	5265.301952	16.087411	-0.070318	3.921861
361.496495	5257.231891	16.092416	-0.070321	3.918912
361.499587	5249.334718	16.097421	-0.070317	3.916023
361.392229	5241.287301	16.102426	-0.070291	3.913075
361.352143	5233.271359	16.107431	-0.070279	3.910138
361.235449	5225.263883	16.112435	-0.070252	3.907199
361.213380	5217.257378	16.117440	-0.070242	3.904261
361.198284	5209.332183	16.122445	-0.070234	3.901351
361.101343	5201.332435	16.127450	-0.070211	3.898409
360.909962	5193.346473	16.132455	-0.070170	3.895469
360.883252	5185.326237	16.137459	-0.070160	3.892517
361.014489	5177.299186	16.142464	-0.070179	3.889563
361.012381	5169.353275	16.147469	-0.070174	3.886634
360.872864	5161.339741	16.152474	-0.070142	3.883676
360.962183	5153.357717	16.157479	-0.070154	3.880731
360.804598	5145.364222	16.162483	-0.070119	3.877775
360.775290	5137.337647	16.167488	-0.070109	3.874807
360.603308	5129.280544	16.172493	-0.070071	3.871822
360.692344	5121.207451	16.177498	-0.070083	3.868834
360.726080	5113.282645	16.182503	-0.070084	3.865899
360.652324	5105.275695	16.187507	-0.070065	3.862928
360.813977	5097.308639	16.192512	-0.070090	3.859974
360.570759	5089.349724	16.197517	-0.070039	3.857013
360.366932	5081.304101	16.202522	-0.069996	3.854018
360.607062	5073.371025	16.207527	-0.070036	3.851072
360.521105	5065.331951	16.212531	-0.070014	3.848078
360.325716	5057.315563	16.217536	-0.069973	3.845087
360.371852	5049.365974	16.222541	-0.069976	3.842124
360.460264	5041.328881	16.227546	-0.069987	3.839126
360.332877	5033.412597	16.232551	-0.069958	3.836167
360.215271	5025.344088	16.237555	-0.069931	3.833149
360.261405	5017.364973	16.242560	-0.069935	3.830166
360.263514	5009.352141	16.247565	-0.069930	3.827167
360.013031	5001.320566	16.252570	-0.069878	3.824152
360.123049	4993.413035	16.257575	-0.069893	3.821190
360.100727	4985.366437	16.262579	-0.069884	3.818171
359.950273	4977.371282	16.267584	-0.069851	3.815165
359.976359	4969.386857	16.272589	-0.069850	3.812165
359.818243	4961.327692	16.277594	-0.069816	3.809131
359.942214	4953.378216	16.282599	-0.069834	3.806141
359.883725	4945.365628	16.287603	-0.069817	3.803122
359.841449	4937.391562	16.292608	-0.069804	3.800114
359.925369	4929.425239	16.297613	-0.069815	3.797111
359.768374	4921.337765	16.302618	-0.069780	3.794053
359.967225	4913.416739	16.307623	-0.069812	3.791065
359.726587	4905.401846	16.312627	-0.069762	3.788028
359.673593	4897.368716	16.317632	-0.069747	3.784986
359.571437	4889.414321	16.322637	-0.069723	3.781971
359.556643	4881.380222	16.327642	-0.069715	3.778925
359.526652	4873.436635	16.332647	-0.069704	3.775910
359.492527	4865.409265	16.337651	-0.069692	3.772861
359.407788	4857.418679	16.342656	-0.069671	3.769822
359.557282	4849.452668	16.347661	-0.069694	3.766796
359.257251	4841.400838	16.352666	-0.069633	3.763724
359.248324	4833.501958	16.357671	-0.069626	3.760715
359.355432	4825.489905	16.362675	-0.069641	3.757663
359.278380	4817.473963	16.367680	-0.069621	3.754602
359.297391	4809.474806	16.372685	-0.069620	3.751548
359.310516	4801.450694	16.377690	-0.069617	3.748482
359.319515	4793.460338	16.382695	-0.069613	3.745425
359.351694	4785.493761	16.387699	-0.069614	3.742376
359.215353	4777.485914	16.392704	-0.069583	3.739305
359.253216	4769.519810	16.397709	-0.069585	3.736251
359.161925	4761.477528	16.402714	-0.069563	3.733163
359.174237	4753.498568	16.407719	-0.069560	3.730099
359.177591	4745.496713	16.412723	-0.069556	3.727023
359.100435	4737.458079	16.417728	-0.069536	3.723928
358.932331	4729.573179	16.422733	-0.069499	3.720888
359.018135	4721.487737	16.427738	-0.069510	3.717774
359.103692	4713.510197	16.432743	-0.069521	3.714700
358.847235	4705.494019	16.437747	-0.069468	3.711599
358.983059	4697.444005	16.442752	-0.069488	3.708493
358.947178	4689.476716	16.447757	-0.069476	3.705411
358.810145	4681.501881	16.452762	-0.069445	3.702322
358.688280	4673.497297	16.457767	-0.069417	3.699219
358.606409	4665.548324	16.462771	-0.069397	3.696135
358.742936	4657.499570	16.467776	-0.069417	3.693016
358.605143	4649.517133	16.472781	-0.069386	3.689913
358.606326	4641.514370	16.477786	-0.069381	3.686804
358.673797	4633.494592	16.482791	-0.069389	3.683686
358.577242	4625.534473	16.487795	-0.069366	3.680585
358.426545	4617.571203	16.492800	-0.069332	3.677479
358.466494	4609.570423	16.497805	-0.069334	3.674360
358.343733	4601.590033	16.502810	-0.069306	3.671243
358.330143	4593.593760	16.507815	-0.069299	3.668119
358.300722	4585.591835	16.512819	-0.069288	3.664990
358.244601	4577.613772	16.517824	-0.069272	3.661867
358.245593	4569.575610	16.522829	-0.069267	3.658720
358.281770	4561.604816	16.527834	-0.069269	3.655597
358.207803	4553.627854	16.532839	-0.069250	3.652466
358.054707	4545.609278	16.537843	-0.069216	3.649313
358.000464	4537.633628	16.542848	-0.069201	3.646178
358.172901	4529.624259	16.547853	-0.069228	3.643033
358.035182	4521.628639	16.552858	-0.069197	3.639882
357.954742	4513.689807	16.557863	-0.069177	3.636752
357.945191	4505.669701	16.562867	-0.069170	3.633589
357.745990	4497.672502	16.567872	-0.069127	3.630428
357.909083	4489.653264	16.572877	-0.069152	3.627265
357.647516	4481.622502	16.577882	-0.069099	3.624083
357.814485	4473.693465	16.582887	-0.069124	3.620950
357.619222	4465.671290	16.587891	-0.069083	3.617767
357.530199	4457.669836	16.592896	-0.069061	3.614593
357.677495	4449.665385	16.597901	-0.069083	3.611422
357.627111	4441.650066	16.602906	-0.069069	3.608238
357.494091	4433.688711	16.607911	-0.069039	3.605070
357.527643	4425.689285	16.612915	-0.069040	3.601889
357.510671	4417.701405	16.617920	-0.069031	3.598708
357.396639	4409.741835	16.622925	-0.069005	3.595533
357.290034	4401.711345	16.627930	-0.068980	3.592327
357.484319	4393.702574	16.632935	-0.069011	3.589136
357.400843	4385.695659	16.637939	-0.068990	3.585934
357.094082	4377.725016	16.642944	-0.068928	3.582738
357.313379	4369.718537	16.647949	-0.068963	3.579539
357.323589	4361.733961	16.652954	-0.068960	3.576341
357.207473	4353.778441	16.657959	-0.068933	3.573147
357.156938	4345.738861	16.662963	-0.068919	3.569919
357.165898	4337.751820	16.667968	-0.068915	3.566711
357.133234	4329.748719	16.672973	-0.068904	3.563492
356.826180	4321.794569	16.677978	-0.068841	3.560282
357.167774	4313.809377	16.682983	-0.068900	3.557076
356.878389	4305.784792	16.687987	-0.068841	3.553832
356.759442	4297.739983	16.692992	-0.068813	3.550582
356.739182	4289.770772	16.697997	-0.068804	3.547362
356.886824	4281.727243	16.703002	-0.068826	3.544115
356.973734	4273.827565	16.708007	-0.068838	3.540921
356.759024	4265.814897	16.713011	-0.068792	3.537670
356.806491	4257.799464	16.718016	-0.068796	3.534422
356.718733	4249.855686	16.723021	-0.068774	3.531196
356.589444	4241.801800	16.728026	-0.068745	3.527921
356.758639	4233.820518	16.733031	-0.068771	3.524682
356.580167	4225.881283	16.738035	-0.068733	3.521446
356.422325	4217.871197	16.743040	-0.068698	3.518179
356.443916	4209.876000	16.748045	-0.068697	3.514920
356.481590	4201.873947	16.753050	-0.068699	3.511656
356.400460	4193.877981	16.758055	-0.068679	3.508388
356.269075	4185.846146	16.763059	-0.068649	3.505101
356.354054	4177.899358	16.768064	-0.068660	3.501852
356.283729	4169.907466	16.773069	-0.068641	3.498577
356.053402	4161.918314	16.778074	-0.068593	3.495294
355.991209	4153.930978	16.783079	-0.068576	3.492015
356.110676	4145.883472	16.788083	-0.068593	3.488714
355.986432	4137.892664	16.793088	-0.068565	3.485425
356.050223	4129.951238	16.798093	-0.068572	3.482159
356.105204	4121.907328	16.803098	-0.068577	3.478848
356.039038	4113.999672	16.808103	-0.068559	3.475586
355.934509	4105.959652	16.813107	-0.068535	3.472265
355.775508	4097.951439	16.818112	-0.068500	3.468951
355.894186	4089.972162	16.823117	-0.068517	3.465657
355.828016	4081.961191	16.828122	-0.068499	3.462339
355.858519	4073.971886	16.833127	-0.068499	3.459031
355.816838	4066.022466	16.838131	-0.068487	3.455733
355.833766	4058.019456	16.843136	-0.068484	3.452412
355.759236	4050.009132	16.848141	-0.068465	3.449082
355.698119	4042.028741	16.853146	-0.068449	3.445762
355.680417	4034.047241	16.858151	-0.068440	3.442439
355.465579	4026.041105	16.863155	-0.068395	3.439096
355.528681	4018.087126	16.868160	-0.068402	3.435781
355.553621	4010.100618	16.873165	-0.068401	3.432448
355.215072	4002.065551	16.878170	-0.068333	3.429078
355.092582	3994.112247	16.883175	-0.068305	3.425748
355.389641	3986.074193	16.888179	-0.068355	3.422393
355.390770	3978.056828	16.893184	-0.068350	3.419033
355.267344	3970.124037	16.898189	-0.068322	3.415701
354.941533	3962.132152	16.903194	-0.068256	3.412333
355.198562	3954.086403	16.908199	-0.068298	3.408961
355.105752	3946.118944	16.913203	-0.068276	3.405605
355.059154	3938.129528	16.918208	-0.068262	3.402239
355.179449	3930.122732	16.923213	-0.068279	3.398867
354.951303	3922.191277	16.928218	-0.068232	3.395512
354.979117	3914.139504	16.933223	-0.068231	3.392112
354.969828	3906.112260	16.938227	-0.068225	3.388718
354.834771	3898.134102	16.943232	-0.068194	3.385336
354.880964	3890.160895	16.948237	-0.068198	3.381959
354.797601	3882.158992	16.953242	-0.068177	3.378563
354.922691	3874.181693	16.958247	-0.068195	3.375181
354.676328	3866.223245	16.963251	-0.068144	3.371789
354.536609	3858.162431	16.968256	-0.068113	3.368355
354.734413	3850.203624	16.973261	-0.068144	3.364973
354.710209	3842.231109	16.978266	-0.068135	3.361574
354.454634	3834.292031	16.983271	-0.068082	3.358177
354.461871	3826.288395	16.988275	-0.068078	3.354759
354.616761	3818.277756	16.993280	-0.068101	3.351340
354.350122	3810.303589	16.998285	-0.068047	3.347917
354.189359	3802.282482	17.003290	-0.068011	3.344474
354.322955	3794.337539	17.008295	-0.068031	3.341072
354.336051	3786.329178	17.013299	-0.068028	3.337634
354.085745	3778.344475	17.018304	-0.067977	3.334193
354.274668	3770.340646	17.023309	-0.068007	3.330757
353.961404	3762.364430	17.028314	-0.067943	3.327310
353.927488	3754.352116	17.033319	-0.067931	3.323855
353.852597	3746.392316	17.038323	-0.067912	3.320417
354.014608	3738.360300	17.043328	-0.067937	3.316953
353.943983	3730.387117	17.048333	-0.067919	3.313502
353.661732	3722.397392	17.053338	-0.067861	3.310032
353.945537	3714.373670	17.058343	-0.067909	3.306566
353.640582	3706.403638	17.063347	-0.067847	3.303097
353.420443	3698.430122	17.068352	-0.067801	3.299626
353.718983	3690.433005	17.073357	-0.067851	3.296161
353.520880	3682.451422	17.078362	-0.067809	3.292679
353.399244	3674.441313	17.083367	-0.067781	3.289185
353.767514	3666.417116	17.088371	-0.067844	3.285700
353.767247	3658.446499	17.093376	-0.067839	3.282220
353.766633	3650.492938	17.098381	-0.067834	3.278744
353.295883	3642.564018	17.103386	-0.067741	3.275256
353.478092	3634.517247	17.108391	-0.067770	3.271740
353.486547	3626.495116	17.113395	-0.067766	3.268223
353.313036	3618.515549	17.118400	-0.067728	3.264713
353.354300	3610.595714	17.123405	-0.067731	3.261235
353.223547	3602.563413	17.128410	-0.067701	3.257696
353.253441	3594.575942	17.133415	-0.067702	3.254180
353.276145	3586.606967	17.138419	-0.067701	3.250669
353.268031	3578.573118	17.143424	-0.067694	3.247123
353.103234	3570.611492	17.148429	-0.067658	3.243599
353.053337	3562.621692	17.153434	-0.067644	3.240063
353.149220	3554.665665	17.158439	-0.067656	3.236545
353.106830	3546.641897	17.163443	-0.067643	3.232986
353.068550	3538.656132	17.168448	-0.067631	3.229441
353.145927	3530.650630	17.173453	-0.067640	3.225889
353.130651	3522.657104	17.178458	-0.067632	3.222333
353.057878	3514.683491	17.183463	-0.067613	3.218780
352.736711	3506.704612	17.188467	-0.067548	3.215211
352.712543	3498.691679	17.193472	-0.067538	3.211634
352.843677	3490.686782	17.198477	-0.067558	3.208064
352.604724	3482.714392	17.203482	-0.067508	3.204489
352.792882	3474.742006	17.208487	-0.067538	3.200928
352.531830	3466.773652	17.213491	-0.067484	3.197346
352.457858	3458.768480	17.218496	-0.067465	3.193751
352.471615	3450.788186	17.223501	-0.067462	3.190167
352.359261	3442.798552	17.228506	-0.067436	3.186569
352.462224	3434.795699	17.233511	-0.067450	3.182970
352.514655	3426.799151	17.238515	-0.067455	3.179369
352.426499	3418.834342	17.243520	-0.067433	3.175771
352.383759	3410.887982	17.248525	-0.067420	3.172179
352.087692	3402.871270	17.253530	-0.067360	3.168540
352.147384	3394.888281	17.258535	-0.067366	3.164929
352.160929	3386.931305	17.263539	-0.067363	3.161322
352.050573	3378.917226	17.268544	-0.067337	3.157681
351.731748	3370.980410	17.273549	-0.067273	3.154060
351.828026	3362.948715	17.278554	-0.067285	3.150411
351.685809	3354.965667	17.283559	-0.067254	3.146770
351.582377	3346.941548	17.288563	-0.067229	3.143106
351.494268	3338.963593	17.293568	-0.067207	3.139461
351.309045	3331.036721	17.298573	-0.067168	3.135830
351.532940	3322.958929	17.303578	-0.067204	3.132144
351.469149	3314.986751	17.308583	-0.067187	3.128490
351.445258	3306.984545	17.313587	-0.067177	3.124819
351.323806	3299.049124	17.318592	-0.067150	3.121170
351.089138	3291.110003	17.323597	-0.067101	3.117510
351.157312	3283.091490	17.328602	-0.067108	3.113823
351.262754	3275.098993	17.333607	-0.067123	3.110145
351.317881	3267.065529	17.338611	-0.067128	3.106442
351.211206	3259.099909	17.343616	-0.067103	3.102758
351.321605	3251.143347	17.348621	-0.067118	3.099084
351.227603	3243.134748	17.353626	-0.067095	3.095372
351.225055	3235.164849	17.358631	-0.067090	3.091677
351.355569	3227.149872	17.363635	-0.067109	3.087964
351.216256	3219.137843	17.368640	-0.067077	3.084235
351.004370	3211.276494	17.373645	-0.067033	3.080568
351.039797	3203.250483	17.378650	-0.067034	3.076831
350.796492	3195.271596	17.383655	-0.066984	3.073099
350.613572	3187.248186	17.388659	-0.066944	3.069344
350.828525	3179.217607	17.393664	-0.066979	3.065601
350.763509	3171.258378	17.398669	-0.066962	3.061872
350.630707	3163.249991	17.403674	-0.066932	3.058113
350.782429	3155.268509	17.408679	-0.066955	3.054376
350.962445	3147.287133	17.413683	-0.066983	3.050635
350.938843	3139.292244	17.418688	-0.066974	3.046874
350.643998	3131.352808	17.423693	-0.066914	3.043121
350.556198	3123.361283	17.428698	-0.066892	3.039348
350.771030	3115.402846	17.433703	-0.066927	3.035602
350.725477	3107.406889	17.438707	-0.066913	3.031820
350.583322	3099.428466	17.443712	-0.066882	3.028037
350.520235	3091.434631	17.448717	-0.066865	3.024246
350.591503	3083.460334	17.453722	-0.066873	3.020466
350.255183	3075.544375	17.458727	-0.066805	3.016689
350.260352	3067.517681	17.463731	-0.066801	3.012871
350.380143	3059.475225	17.468736	-0.066818	3.009047
350.336707	3051.517881	17.473741	-0.066804	3.005251
350.416873	3043.524112	17.478746	-0.066814	3.001438
350.343265	3035.571894	17.483751	-0.066795	2.997633
350.148638	3027.607564	17.488755	-0.066754	2.993810
350.085008	3019.596504	17.493760	-0.066737	2.989968
350.266362	3011.592225	17.498765	-0.066765	2.986136
350.102951	3003.631319	17.503770	-0.066730	2.982302
349.989927	2995.668174	17.508775	-0.066703	2.978465
350.024868	2987.676062	17.513779	-0.066705	2.974616
349.889407	2979.671313	17.518784	-0.066674	2.970748
349.893129	2971.691695	17.523789	-0.066670	2.966893
350.009311	2963.684435	17.528794	-0.066686	2.963027
350.009773	2955.730430	17.533799	-0.066681	2.959175
349.704939	2947.815532	17.538803	-0.066619	2.955321
349.686309	2939.807281	17.543808	-0.066610	2.951431
349.700580	2931.814985	17.548813	-0.066608	2.947546
349.514564	2923.800678	17.553818	-0.066568	2.943635
349.566098	2915.858106	17.558823	-0.066572	2.939766
349.531609	2907.874697	17.563827	-0.066561	2.935867
349.158549	2899.916842	17.568832	-0.066486	2.931957
349.137509	2891.915681	17.573837	-0.066477	2.928040
349.212128	2883.889845	17.578842	-0.066486	2.924111
349.400972	2875.946036	17.583847	-0.066516	2.920223
349.129536	2868.002781	17.588851	-0.066460	2.916305
348.948555	2859.986754	17.593856	-0.066421	2.912350
349.234164	2851.934238	17.598861	-0.066469	2.908398
349.127071	2843.938173	17.603866	-0.066444	2.904447
348.954777	2836.015261	17.608871	-0.066406	2.900523
349.263608	2828.012158	17.613875	-0.066459	2.896580
349.065886	2820.033705	17.618880	-0.066417	2.892617
348.870766	2812.082983	17.623885	-0.066375	2.888661
348.678554	2804.087036	17.628890	-0.066334	2.884678
348.766790	2796.137763	17.633895	-0.066345	2.880729
348.776295	2788.152487	17.638899	-0.066342	2.876751
348.678576	2780.172851	17.643904	-0.066319	2.872765
348.835157	2772.188055	17.648909	-0.066343	2.868785
348.796356	2764.171543	17.653914	-0.066330	2.864773
348.780043	2756.227254	17.658919	-0.066322	2.860792
348.716827	2748.255209	17.663923	-0.066305	2.856789
348.667399	2740.273549	17.668928	-0.066291	2.852777
348.469398	2732.315141	17.673933	-0.066248	2.848762
348.189920	2724.334025	17.678938	-0.066191	2.844725
348.355813	2716.368423	17.683943	-0.066217	2.840716
348.413903	2708.394229	17.688947	-0.066223	2.836691
348.044187	2700.416350	17.693952	-0.066148	2.832634
348.288165	2692.416411	17.698957	-0.066189	2.828595
348.149853	2684.410353	17.703962	-0.066158	2.824524
348.257331	2676.450151	17.708967	-0.066173	2.820486
348.051899	2668.496410	17.713971	-0.066129	2.816427
348.130544	2660.487658	17.718976	-0.066139	2.812351
348.099944	2652.508655	17.723981	-0.066128	2.808277
347.935459	2644.517743	17.728986	-0.066092	2.804183
347.913123	2636.602497	17.733991	-0.066082	2.800131
347.948511	2628.609816	17.738995	-0.066084	2.796037
347.875838	2620.615314	17.744000	-0.066065	2.791929
347.839718	2612.648973	17.749005	-0.066053	2.787831
347.777901	2604.644049	17.754010	-0.066036	2.783706
347.668112	2596.714744	17.759015	-0.066011	2.779612
347.692995	2588.729383	17.764019	-0.066010	2.775490
347.622071	2580.766552	17.769024	-0.065992	2.771368
347.403048	2572.818625	17.774029	-0.065946	2.767239
347.296017	2564.805088	17.779034	-0.065921	2.763076
347.299939	2556.857815	17.784039	-0.065916	2.758948
347.250247	2548.891610	17.789043	-0.065902	2.754800
346.734622	2540.909540	17.794048	-0.065801	2.750610
346.953672	2532.898557	17.799053	-0.065836	2.746443
346.642556	2524.944872	17.804058	-0.065773	2.742267
346.805855	2516.926589	17.809063	-0.065798	2.738081
346.561439	2509.003137	17.814067	-0.065748	2.733912
346.402976	2500.998427	17.819072	-0.065713	2.729699
346.307458	2493.056162	17.824077	-0.065690	2.725517
346.505399	2485.013286	17.829082	-0.065721	2.721294
346.530995	2477.063845	17.834087	-0.065721	2.717103
346.554685	2469.082592	17.839091	-0.065720	2.712888
346.669997	2461.077314	17.844096	-0.065736	2.708660
346.761005	2453.106832	17.849101	-0.065748	2.704442
346.677797	2445.158069	17.854106	-0.065728	2.700218
346.703938	2437.202659	17.859111	-0.065727	2.695991
346.359691	2429.246109	17.864115	-0.065658	2.691732
346.473444	2421.244282	17.869120	-0.065674	2.687473
346.485937	2413.296032	17.874125	-0.065671	2.683228
346.331405	2405.328252	17.879130	-0.065637	2.678956
346.332403	2397.385695	17.884135	-0.065632	2.674700
346.335357	2389.378225	17.889139	-0.065627	2.670403
346.370996	2381.381373	17.894144	-0.065629	2.666107
346.410906	2373.406712	17.899149	-0.065631	2.661816
346.142098	2365.475918	17.904154	-0.065576	2.657521
346.162056	2357.505772	17.909159	-0.065574	2.653218
346.170866	2349.509268	17.914163	-0.065571	2.648892
345.971807	2341.538558	17.919168	-0.065529	2.644559
346.049851	2333.604478	17.924173	-0.065538	2.640258
345.979387	2325.629971	17.929178	-0.065520	2.635918
345.875064	2317.658520	17.934183	-0.065495	2.631569
345.815251	2309.679898	17.939187	-0.065479	2.627213
345.605968	2301.733445	17.944192	-0.065434	2.622857
345.768870	2293.746472	17.949197	-0.065460	2.618497
345.638318	2285.783762	17.954202	-0.065430	2.614123
345.655891	2277.798876	17.959207	-0.065428	2.609739
345.515414	2269.842380	17.964211	-0.065397	2.605353
345.532363	2261.863466	17.969216	-0.065395	2.600958
345.670246	2253.913623	17.974221	-0.065415	2.596579
345.365880	2245.902733	17.979226	-0.065353	2.592129
345.199089	2237.904482	17.984231	-0.065317	2.587688
345.333771	2229.896320	17.989235	-0.065337	2.583255
345.226477	2221.957687	17.994240	-0.065312	2.578836
345.235518	2214.000332	17.999245	-0.065308	2.574407
345.193525	2206.035166	18.004250	-0.065295	2.569962
345.061133	2198.081606	18.009255	-0.065265	2.565510
344.950463	2190.157001	18.014259	-0.065240	2.561067
344.876380	2182.176160	18.019264	-0.065221	2.556588
344.985839	2174.210913	18.024269	-0.065236	2.552123
344.745240	2166.252437	18.029274	-0.065186	2.547629
344.834446	2158.257893	18.034279	-0.065197	2.543131
344.739479	2150.322876	18.039283	-0.065174	2.538644
344.727720	2142.327547	18.044288	-0.065167	2.534122
344.694607	2134.385026	18.049293	-0.065156	2.529620
344.789076	2126.391587	18.054298	-0.065168	2.525090
344.644425	2118.474817	18.059303	-0.065136	2.520578
344.590809	2110.522210	18.064307	-0.065121	2.516045
344.427402	2102.552524	18.069312	-0.065085	2.511485
344.393309	2094.576013	18.074317	-0.065073	2.506923
344.219792	2086.613067	18.079322	-0.065036	2.502350
344.185563	2078.645319	18.084327	-0.065024	2.497776
344.505474	2070.642562	18.089331	-0.065079	2.493199
344.291080	2062.689539	18.094336	-0.065034	2.488604
344.175968	2054.746755	18.099341	-0.065007	2.484012
344.153374	2046.792865	18.104346	-0.064998	2.479413
344.039701	2038.858123	18.109351	-0.064971	2.474810
343.873429	2030.898869	18.114355	-0.064935	2.470180
343.785395	2022.906531	18.119360	-0.064914	2.465528
343.944200	2014.945071	18.124365	-0.064938	2.460903
343.836771	2006.977663	18.129370	-0.064913	2.456247
343.793528	1999.040171	18.134375	-0.064900	2.451603
343.523796	1991.089334	18.139379	-0.064844	2.446926
343.522888	1983.114851	18.144384	-0.064839	2.442247
343.447963	1975.187200	18.149389	-0.064820	2.437580
343.498011	1967.183003	18.154394	-0.064824	2.432869
343.262001	1959.245482	18.159399	-0.064775	2.428166
343.324681	1951.239704	18.164403	-0.064781	2.423437
343.140139	1943.298234	18.169408	-0.064741	2.418717
343.311440	1935.321745	18.174413	-0.064768	2.413995
342.950751	1927.384635	18.179418	-0.064696	2.409245
342.984330	1919.422419	18.184423	-0.064697	2.404503
342.979366	1911.483918	18.189427	-0.064691	2.399761
342.878180	1903.521889	18.194432	-0.064667	2.394989
342.790348	1895.584394	18.199437	-0.064645	2.390223
342.656182	1887.598929	18.204442	-0.064615	2.385415
342.891473	1879.625961	18.209447	-0.064654	2.380635
342.849514	1871.688682	18.214451	-0.064641	2.375844
342.592855	1863.737366	18.219456	-0.064588	2.371017
342.737314	1855.765360	18.224461	-0.064609	2.366200
342.464171	1847.845525	18.229466	-0.064553	2.361372
342.558909	1839.879818	18.234471	-0.064566	2.356535
342.503324	1831.935725	18.239475	-0.064550	2.351690
342.441233	1823.956820	18.244480	-0.064533	2.346812
342.137041	1816.045628	18.249485	-0.064472	2.341946
342.162458	1808.065134	18.254490	-0.064471	2.337055
342.301822	1800.089042	18.259495	-0.064492	2.332165
342.165583	1792.149319	18.264499	-0.064461	2.327265
342.028687	1784.210316	18.269504	-0.064431	2.322355
342.079388	1776.266214	18.274509	-0.064435	2.317446
341.995605	1768.302024	18.279514	-0.064414	2.312504
341.923842	1760.354505	18.284519	-0.064396	2.307562
341.917460	1752.409522	18.289523	-0.064389	2.302617
341.838274	1744.449396	18.294528	-0.064369	2.297646
341.799091	1736.512236	18.299533	-0.064357	2.292681
341.690467	1728.549619	18.304538	-0.064331	2.287684
341.799519	1720.588445	18.309543	-0.064347	2.282696
341.646488	1712.685923	18.314547	-0.064313	2.277711
341.373911	1704.731848	18.319552	-0.064257	2.272671
341.417506	1696.744916	18.324557	-0.064260	2.267628
341.311524	1688.790650	18.329562	-0.064235	2.262581
341.143541	1680.863584	18.334567	-0.064199	2.257534
341.234363	1672.886555	18.339571	-0.064210	2.252467
341.109496	1664.931421	18.344576	-0.064182	2.247384
341.008847	1657.002920	18.349581	-0.064158	2.242308
340.999782	1649.061073	18.354586	-0.064151	2.237220
341.074746	1641.116245	18.359591	-0.064160	2.232126
341.113474	1633.142484	18.364595	-0.064162	2.226999
340.882960	1625.236593	18.369600	-0.064114	2.221879
340.702290	1617.326360	18.374605	-0.064075	2.216749
340.768917	1609.345941	18.379610	-0.064082	2.211584
340.672131	1601.406744	18.384615	-0.064059	2.206419
340.664647	1593.477129	18.389619	-0.064052	2.201257
340.629377	1585.529905	18.394624	-0.064041	2.196068
340.674688	1577.591454	18.399629	-0.064044	2.190880
340.503993	1569.630907	18.404634	-0.064007	2.185645
340.607770	1561.687445	18.409639	-0.064021	2.180434
340.567180	1553.740635	18.414643	-0.064008	2.175195
340.413295	1545.797529	18.419648	-0.063974	2.169936
340.348783	1537.873946	18.424653	-0.063957	2.164684
340.357660	1529.925743	18.429658	-0.063954	2.159411
340.282580	1522.019988	18.434663	-0.063935	2.154145
340.186948	1514.088155	18.439667	-0.063912	2.148847
340.084147	1506.130789	18.444672	-0.063887	2.143517
340.342757	1498.179612	18.449677	-0.063930	2.138214
339.998386	1490.273400	18.454682	-0.063861	2.132869
339.692135	1482.359516	18.459687	-0.063799	2.127509
339.818037	1474.412079	18.464691	-0.063817	2.122155
339.574669	1466.510865	18.469696	-0.063767	2.116783
339.599621	1458.551005	18.474701	-0.063766	2.111383
339.464478	1450.582462	18.479706	-0.063736	2.105948
339.604872	1442.618977	18.484711	-0.063757	2.100530
339.638671	1434.683675	18.489715	-0.063758	2.095106
339.539648	1426.747534	18.494720	-0.063734	2.089654
339.366275	1418.840964	18.499725	-0.063697	2.084201
339.251814	1410.936412	18.504730	-0.063670	2.078741
339.168060	1403.008951	18.509735	-0.063649	2.073254
339.355410	1395.043004	18.514739	-0.063679	2.067753
339.047564	1387.150536	18.519744	-0.063617	2.062238
339.096488	1379.227886	18.524749	-0.063621	2.056724
339.078895	1371.275058	18.529754	-0.063612	2.051167
338.903254	1363.365044	18.534759	-0.063574	2.045608
338.390676	1355.537646	18.539763	-0.063474	2.040057
338.303613	1347.590081	18.544768	-0.063452	2.034451
338.359825	1339.650789	18.549773	-0.063458	2.028850
338.363682	1331.662520	18.554778	-0.063453	2.023193
338.504354	1323.716889	18.559783	-0.063474	2.017565
338.357358	1315.819131	18.564787	-0.063442	2.011926
338.271650	1307.881024	18.569792	-0.063420	2.006247
338.408703	1299.951221	18.574797	-0.063441	2.000583
338.025574	1292.093027	18.579802	-0.063364	1.994898
338.043327	1284.153994	18.584807	-0.063362	1.989182
338.162047	1276.200215	18.589811	-0.063379	1.983449
338.046464	1268.294666	18.594816	-0.063353	1.977709
337.992035	1260.386884	18.599821	-0.063337	1.971958
337.748216	1252.480104	18.604826	-0.063287	1.966170
337.701123	1244.579824	18.609831	-0.063273	1.960391
337.574829	1236.687961	18.614835	-0.063244	1.954592
337.325979	1228.781008	18.619840	-0.063193	1.948751
337.296765	1220.847501	18.624845	-0.063182	1.942898
337.529889	1212.872596	18.629850	-0.063220	1.937026
337.273897	1204.992821	18.634855	-0.063168	1.931151
337.473611	1197.019878	18.639859	-0.063200	1.925240
337.246545	1189.146933	18.644864	-0.063152	1.919338
337.284522	1181.237764	18.649869	-0.063154	1.913421
337.037826	1173.344557	18.654874	-0.063103	1.907464
336.867253	1165.453850	18.659879	-0.063066	1.901499
336.904687	1157.535310	18.664883	-0.063068	1.895519
336.709048	1149.627888	18.669888	-0.063026	1.889501
336.655306	1141.741140	18.674893	-0.063011	1.883496
336.569708	1133.838875	18.679898	-0.062990	1.877456
336.543860	1125.916695	18.684903	-0.062980	1.871389
336.458434	1118.002941	18.689907	-0.062959	1.865301
336.414869	1110.097717	18.694912	-0.062946	1.859204
336.392791	1102.213507	18.699917	-0.062936	1.853107
335.983532	1094.343238	18.704922	-0.062855	1.846954
335.958552	1086.442757	18.709927	-0.062845	1.840802
336.025741	1078.525916	18.714931	-0.062853	1.834629
336.075035	1070.602382	18.719936	-0.062857	1.828427
335.868962	1062.734404	18.724941	-0.062813	1.822217
335.802951	1054.849990	18.729946	-0.062796	1.815989
335.570291	1046.973372	18.734951	-0.062747	1.809726
335.606733	1039.068716	18.739955	-0.062749	1.803452
335.341127	1031.203796	18.744960	-0.062694	1.797150
335.577645	1023.247282	18.749965	-0.062733	1.790815
335.716063	1015.301899	18.754970	-0.062754	1.784455
335.433614	1007.473676	18.759975	-0.062696	1.778113
335.403397	999.579496	18.764979	-0.062685	1.771727
335.228507	991.702181	18.769984	-0.062648	1.765313
335.252267	983.835735	18.774989	-0.062647	1.758910
335.180319	975.948417	18.779994	-0.062628	1.752454
334.987163	968.087539	18.784999	-0.062587	1.745980
334.788840	960.243515	18.790003	-0.062545	1.739496
334.765025	952.331694	18.795008	-0.062536	1.732953
334.977704	944.412119	18.800013	-0.062570	1.726411
334.631837	936.588812	18.805018	-0.062501	1.719850
334.391421	928.757570	18.810023	-0.062451	1.713272
334.506513	920.837305	18.815027	-0.062467	1.706640
334.439215	912.961337	18.820032	-0.062449	1.699996
334.146869	905.146467	18.825037	-0.062390	1.693347
334.079213	897.245255	18.830042	-0.062372	1.686628
334.223126	889.354192	18.835047	-0.062394	1.679920
334.070161	881.529975	18.840051	-0.062360	1.673203
333.796213	873.675678	18.845056	-0.062304	1.666415
333.616421	865.851599	18.850061	-0.062265	1.659639
333.595930	857.963351	18.855066	-0.062256	1.652801
333.325475	850.121479	18.860071	-0.062201	1.645940
333.347738	842.263579	18.865075	-0.062200	1.639078
333.078496	834.419468	18.870080	-0.062145	1.632158
333.119485	826.510863	18.875085	-0.062147	1.625195
332.713037	818.713107	18.880090	-0.062066	1.618237
332.302431	810.905931	18.885095	-0.061985	1.611239
332.168551	803.048224	18.890099	-0.061955	1.604206
331.929799	795.220394	18.895104	-0.061905	1.597153
331.915168	787.356949	18.900109	-0.061897	1.590069
331.902585	779.477188	18.905114	-0.061890	1.582940
331.910151	771.626694	18.910119	-0.061886	1.575807
331.762412	763.799074	18.915123	-0.061854	1.568640
331.891433	755.918667	18.920128	-0.061872	1.561433
331.696310	748.133234	18.925133	-0.061831	1.554231
331.248279	740.344820	18.930138	-0.061743	1.546955
331.160723	732.508088	18.935143	-0.061721	1.539654
331.090481	724.679890	18.940147	-0.061703	1.532329
330.465764	716.915261	18.945152	-0.061582	1.524943
330.560976	709.068652	18.950157	-0.061594	1.517555
330.434017	701.231945	18.955162	-0.061565	1.510106
330.150323	693.437688	18.960167	-0.061507	1.502636
329.916749	685.642516	18.965171	-0.061459	1.495135
329.562240	677.855819	18.970176	-0.061388	1.487585
329.287426	670.076910	18.975181	-0.061332	1.480017
328.495304	662.363735	18.980186	-0.061179	1.472391
328.283523	654.510095	18.985191	-0.061134	1.464681
327.921775	646.733266	18.990195	-0.061062	1.456982
326.920618	639.034710	18.995200	-0.060871	1.449214
325.915248	631.342436	19.000205	-0.060678	1.441410
324.867260	623.648265	19.005210	-0.060478	1.433555
323.836128	615.928819	19.010215	-0.060281	1.425632
322.642924	608.249193	19.015219	-0.060054	1.417678
321.791647	600.476176	19.020224	-0.059890	1.409642
321.258127	592.681271	19.025229	-0.059786	1.401591
320.409663	584.943000	19.030234	-0.059623	1.393497
319.429733	577.197846	19.035239	-0.059435	1.385326
318.886995	569.417042	19.040243	-0.059329	1.377145
317.913300	561.686758	19.045248	-0.059143	1.368892
317.295585	553.920316	19.050253	-0.059023	1.360613
316.426995	546.205992	19.055258	-0.058856	1.352295
315.586540	538.469748	19.060263	-0.058695	1.343906
314.844377	530.734587	19.065267	-0.058551	1.335483
313.996567	523.003946	19.070272	-0.058388	1.326991
313.206445	515.311086	19.075277	-0.058236	1.318497
312.371126	507.529564	19.080282	-0.058076	1.309841
311.524742	499.795760	19.085287	-0.057913	1.301178
310.829985	492.079385	19.090291	-0.057779	1.292505
310.073100	484.358954	19.095296	-0.057633	1.283756
309.237203	476.690075	19.100301	-0.057472	1.274990
308.317757	469.007259	19.105306	-0.057296	1.266131
307.566589	461.322486	19.110311	-0.057151	1.257240
306.951517	453.616678	19.115315	-0.057031	1.248287
306.013974	445.969409	19.120320	-0.056852	1.239274
305.300153	438.303048	19.125325	-0.056714	1.230216
304.126256	430.691056	19.130330	-0.056490	1.221063
303.205339	423.046865	19.135335	-0.056314	1.211853
302.572629	415.365228	19.140339	-0.056191	1.202585
301.580951	407.758089	19.145344	-0.056001	1.193262
300.948578	400.084961	19.150349	-0.055879	1.183859
300.064902	392.474272	19.155354	-0.055709	1.174404
299.349453	384.838826	19.160359	-0.055571	1.164878
298.642713	377.222852	19.165363	-0.055434	1.155298
297.891411	369.576342	19.170368	-0.055290	1.145590
297.223987	361.970105	19.175373	-0.055160	1.135868
296.050885	354.437889	19.180378	-0.054937	1.126045
295.012788	346.904097	19.185383	-0.054739	1.116163
294.346928	339.307626	19.190387	-0.054610	1.106194
293.722133	331.714969	19.195392	-0.054489	1.096148
292.930489	324.164891	19.200397	-0.054336	1.086027
292.157483	316.634214	19.205402	-0.054187	1.075841
291.288758	309.115613	19.210407	-0.054021	1.065551
290.760183	301.554654	19.215411	-0.053917	1.055183
289.801784	294.072784	19.220416	-0.053734	1.044718
289.219420	286.557765	19.225421	-0.053621	1.034191
288.309808	279.096809	19.230426	-0.053446	1.023551
287.681227	271.605265	19.235431	-0.053325	1.012826
286.891835	264.160345	19.240435	-0.053173	1.002011
285.941406	256.744090	19.245440	-0.052991	0.991080
285.468971	249.251435	19.250445	-0.052898	0.980036
284.576718	241.853040	19.255450	-0.052727	0.968897
283.719889	234.476250	19.260455	-0.052563	0.957669
283.237059	227.049330	19.265459	-0.052468	0.946332
282.384137	219.701408	19.270464	-0.052304	0.934878
281.693985	212.345996	19.275469	-0.052171	0.923314
280.900365	205.031093	19.280474	-0.052019	0.911639
280.295455	197.692852	19.285479	-0.051901	0.899827
279.885963	190.345938	19.290483	-0.051820	0.887900
279.220358	183.073047	19.295488	-0.051691	0.875857
278.517906	175.833694	19.300493	-0.051556	0.863691
277.594282	168.648377	19.305498	-0.051379	0.851376
276.813932	161.464206	19.310503	-0.051229	0.838924
276.147419	154.271354	19.315507	-0.051100	0.826305
275.367876	147.126215	19.320512	-0.050951	0.813539
274.873666	139.971564	19.325517	-0.050854	0.800642
274.037486	132.900155	19.330522	-0.050694	0.787575
273.397257	125.832413	19.335527	-0.050570	0.774358
272.881975	118.777496	19.340531	-0.050469	0.760977
272.010267	111.812025	19.345536	-0.050302	0.747407
271.563777	104.810974	19.350541	-0.050215	0.733663
270.861808	97.889948	19.355546	-0.050079	0.719726
270.414763	90.972710	19.360551	-0.049992	0.705613
269.805053	84.130002	19.365555	-0.049874	0.691307
269.163895	77.507525	19.370560	-0.049750	0.677153