Fri Apr 16 18:50:54 2021

Number of Points = 3645
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.549406	0.067582	0.000000	0.000071	0.309546

0.586185	0.061671	0.005005	0.000064	0.309549
0.816564	0.017897	0.010010	0.000021	0.309540
0.728275	0.033440	0.015014	0.000038	0.309538
1.005284	-0.026445	0.020019	-0.000014	0.309493
0.638549	-0.009724	0.025024	0.000055	0.309259
0.449663	0.027071	0.030029	0.000090	0.309271
0.614075	-0.001855	0.035034	0.000059	0.309275
0.608305	-0.003585	0.040038	0.000060	0.309262
0.827198	-0.042260	0.045043	0.000020	0.309267
0.632250	-0.006173	0.050048	0.000056	0.309270
0.821450	-0.042106	0.055053	0.000021	0.309262
1.100644	-0.095306	0.060058	-0.000031	0.309251
0.802112	-0.040041	0.065062	0.000024	0.309255
0.768268	-0.031557	0.070067	0.000031	0.309266
0.802434	-0.039463	0.075072	0.000024	0.309258
0.819554	-0.040982	0.080077	0.000021	0.309265
1.157452	-0.135421	0.085082	-0.000042	0.309110
1.197194	-0.185296	0.090086	-0.000049	0.308911
1.006426	-0.148049	0.095091	-0.000013	0.308922
1.051523	-0.157689	0.100096	-0.000022	0.308916
1.160000	-0.178816	0.105101	-0.000042	0.308909
1.026134	-0.152237	0.110106	-0.000017	0.308919
0.716894	-0.149665	0.115110	0.000041	0.308668
1.215993	-0.254455	0.120115	-0.000052	0.308602
0.434772	-0.108136	0.125120	0.000093	0.308622
0.680630	-0.154172	0.130125	0.000047	0.308615
0.743844	-0.164468	0.135130	0.000036	0.308621
0.423018	-0.156225	0.140134	0.000096	0.308386
0.540530	-0.196755	0.145139	0.000074	0.308296
0.612178	-0.211848	0.150144	0.000060	0.308286
0.613736	-0.211151	0.155149	0.000060	0.308290
0.659884	-0.235047	0.160154	0.000052	0.308217
0.599512	-0.270563	0.165158	0.000063	0.307999
0.071291	-0.168192	0.170163	0.000161	0.308029
0.591217	-0.269054	0.175168	0.000064	0.307999
0.416380	-0.256471	0.180173	0.000097	0.307908
0.798769	-0.377280	0.185178	0.000026	0.307667
0.297831	-0.285279	0.190182	0.000119	0.307671
0.585513	-0.338517	0.195187	0.000066	0.307667
0.568226	-0.391554	0.200192	0.000069	0.307402
1.001964	-0.486112	0.205197	-0.000012	0.307328
1.044207	-0.490783	0.210202	-0.000019	0.307342
0.567989	-0.461211	0.215206	0.000069	0.307074
0.741682	-0.503140	0.220211	0.000037	0.307024
0.526179	-0.464825	0.225216	0.000077	0.307020
0.740450	-0.560249	0.230221	0.000037	0.306754
0.694650	-0.554480	0.235226	0.000046	0.306742
0.556582	-0.545653	0.240230	0.000072	0.306665
0.177933	-0.527289	0.245235	0.000142	0.306427
0.614653	-0.611097	0.250240	0.000061	0.306405
0.770208	-0.676910	0.255245	0.000032	0.306228
0.565608	-0.667724	0.260250	0.000070	0.306096
0.270075	-0.619903	0.265254	0.000125	0.306068
0.755813	-0.769341	0.270259	0.000035	0.305778
0.869344	-0.793361	0.275264	0.000014	0.305762
1.117684	-0.882668	0.280269	-0.000032	0.305553
1.312197	-0.928232	0.285274	-0.000069	0.305504
1.073144	-0.939080	0.290278	-0.000024	0.305247
0.962544	-0.935752	0.295283	-0.000003	0.305167
1.063789	-1.003029	0.300288	-0.000022	0.304935
0.956839	-1.001992	0.305293	-0.000002	0.304848
1.061092	-1.070134	0.310298	-0.000022	0.304614
0.505860	-0.985935	0.315302	0.000082	0.304534
1.154425	-1.150164	0.320307	-0.000039	0.304314
0.775476	-1.098203	0.325312	0.000032	0.304233
0.565395	-1.119363	0.330317	0.000071	0.303951
0.901983	-1.189626	0.335322	0.000008	0.303907
0.535182	-1.187644	0.340326	0.000077	0.303599
0.421972	-1.173987	0.345331	0.000098	0.303566
0.541234	-1.256205	0.350336	0.000076	0.303277
0.326427	-1.231333	0.355341	0.000116	0.303209
0.446324	-1.296438	0.360346	0.000093	0.303003
0.518691	-1.346764	0.365350	0.000080	0.302825
1.032221	-1.478478	0.370355	-0.000016	0.302641
0.548654	-1.444680	0.375360	0.000075	0.302382
0.210609	-1.399038	0.380365	0.000137	0.302307
0.360430	-1.484509	0.385370	0.000110	0.302028
0.403218	-1.523193	0.390374	0.000102	0.301879
0.342758	-1.543200	0.395379	0.000113	0.301731
0.596220	-1.647525	0.400384	0.000066	0.301451
0.370286	-1.634057	0.405389	0.000108	0.301318
0.427694	-1.691858	0.410394	0.000097	0.301091
0.551826	-1.761964	0.415398	0.000074	0.300862
0.650610	-1.807347	0.420403	0.000056	0.300730
0.491770	-1.821934	0.425408	0.000086	0.300521
0.619239	-1.894736	0.430413	0.000062	0.300281
0.826054	-1.968830	0.435418	0.000024	0.300105
0.652652	-1.988599	0.440422	0.000056	0.299858
0.979867	-2.105472	0.445427	-0.000005	0.299580
0.384634	-2.030122	0.450432	0.000106	0.299422
0.426192	-2.074817	0.455437	0.000098	0.299242
0.728526	-2.197662	0.460442	0.000042	0.298913
0.636217	-2.227187	0.465446	0.000059	0.298689
0.735844	-2.287124	0.470451	0.000041	0.298486
0.757870	-2.337060	0.475456	0.000037	0.298263
0.591796	-2.363937	0.480461	0.000068	0.297986
0.856871	-2.462941	0.485466	0.000019	0.297739
0.735120	-2.492039	0.490470	0.000041	0.297490
0.739900	-2.540119	0.495475	0.000040	0.297260
0.647109	-2.574335	0.500480	0.000058	0.297011
0.924641	-2.684162	0.505485	0.000006	0.296722
0.874300	-2.726591	0.510490	0.000016	0.296470
0.441177	-2.698239	0.515494	0.000096	0.296224
0.617986	-2.779412	0.520499	0.000063	0.295984
0.974303	-2.898505	0.525504	-0.000003	0.295718
1.248791	-2.995883	0.530509	-0.000054	0.295486
0.971211	-3.009945	0.535514	-0.000002	0.295169
0.806866	-3.038713	0.540518	0.000029	0.294882
1.227795	-3.172953	0.545523	-0.000050	0.294598
0.931795	-3.173200	0.550528	0.000005	0.294332
1.077160	-3.259883	0.555533	-0.000022	0.294036
1.075027	-3.317905	0.560538	-0.000021	0.293748
0.693036	-3.308174	0.565542	0.000050	0.293454
0.800540	-3.382612	0.570547	0.000030	0.293183
0.715714	-3.424319	0.575552	0.000046	0.292901
0.948828	-3.532851	0.580557	0.000003	0.292573
0.819202	-3.566978	0.585562	0.000027	0.292288
0.637765	-3.596434	0.590566	0.000061	0.291978
0.712257	-3.664340	0.595571	0.000047	0.291709
0.767979	-3.742079	0.600576	0.000037	0.291373
0.634048	-3.777757	0.605581	0.000062	0.291075
0.667389	-3.845693	0.610586	0.000056	0.290767
0.111734	-3.794186	0.615590	0.000159	0.290520
0.420387	-3.916657	0.620595	0.000102	0.290189
-2.661737	-3.419948	0.625600	0.000675	0.289872
-9.453353	-2.199346	0.630605	0.001939	0.289802
-8.837391	-2.365598	0.635610	0.001825	0.289531
-8.804450	-2.375227	0.640614	0.001818	0.289512
-9.627399	-2.264405	0.645619	0.001972	0.289318
-9.586392	-2.286394	0.650624	0.001964	0.289245
-9.691880	-2.276673	0.655629	0.001984	0.289198
-10.245269	-2.232664	0.660634	0.002087	0.288914
-10.491874	-2.187213	0.665638	0.002133	0.288917
-9.969122	-2.305845	0.670643	0.002035	0.288799
-10.516178	-2.246723	0.675648	0.002137	0.288597
-10.413232	-2.266872	0.680653	0.002118	0.288589
-10.357162	-2.318437	0.685658	0.002108	0.288381
-11.186057	-2.189020	0.690662	0.002262	0.288275
-11.066678	-2.209112	0.695667	0.002240	0.288282
-11.113817	-2.249455	0.700672	0.002249	0.288037
-11.154217	-2.253917	0.705677	0.002256	0.287977
-11.210697	-2.250978	0.710682	0.002267	0.287940
-11.571611	-2.243291	0.715686	0.002334	0.287649
-11.072382	-2.336502	0.720691	0.002241	0.287636
-11.300076	-2.327169	0.725696	0.002284	0.287475
-12.047427	-2.220769	0.730701	0.002423	0.287326
-11.846264	-2.255611	0.735706	0.002385	0.287335
-12.498956	-2.185935	0.740710	0.002507	0.287088
-12.552306	-2.190174	0.745715	0.002517	0.287017
-12.395656	-2.218853	0.750720	0.002488	0.287016
-12.390942	-2.272279	0.755725	0.002487	0.286751
-12.619279	-2.234832	0.760730	0.002529	0.286730
-12.863185	-2.200709	0.765734	0.002575	0.286678
-12.940664	-2.243979	0.770739	0.002589	0.286388
-13.474433	-2.145169	0.775744	0.002689	0.286397
-13.337310	-2.186234	0.780749	0.002663	0.286315
-13.132762	-2.269266	0.785754	0.002625	0.286083
-13.230418	-2.255425	0.790758	0.002643	0.286063
-13.087551	-2.313282	0.795763	0.002617	0.285902
-13.310532	-2.301408	0.800768	0.002658	0.285757
-13.588386	-2.251950	0.805773	0.002710	0.285751
-13.459588	-2.321140	0.810778	0.002686	0.285519
-13.903638	-2.245307	0.815782	0.002769	0.285494
-13.736840	-2.293490	0.820787	0.002738	0.285403
-13.815936	-2.329598	0.825792	0.002753	0.285147
-13.894669	-2.315832	0.830797	0.002767	0.285144
-14.160868	-2.308585	0.835802	0.002817	0.284935
-14.403387	-2.285541	0.840806	0.002862	0.284828
-14.186327	-2.331961	0.845811	0.002822	0.284792
-14.564514	-2.320048	0.850816	0.002892	0.284503
-14.723915	-2.292274	0.855821	0.002922	0.284497
-14.869634	-2.290795	0.860826	0.002949	0.284369
-15.185009	-2.264238	0.865830	0.003008	0.284212
-14.729714	-2.346520	0.870835	0.002923	0.284215
-15.206114	-2.318996	0.875840	0.003012	0.283914
-15.868415	-2.204189	0.880845	0.003135	0.283885
-15.203098	-2.337791	0.885850	0.003011	0.283820
-15.593036	-2.316029	0.890854	0.003084	0.283569
-15.789574	-2.278765	0.895859	0.003121	0.283577
-16.055431	-2.266456	0.900864	0.003170	0.283393
-16.541294	-2.203653	0.905869	0.003261	0.283262
-16.507918	-2.208570	0.910874	0.003254	0.283268
-16.508117	-2.254287	0.915878	0.003255	0.283034
-16.954253	-2.185294	0.920883	0.003338	0.282972
-16.889503	-2.198061	0.925888	0.003326	0.282967
-17.100739	-2.220388	0.930893	0.003365	0.282656
-17.295300	-2.188482	0.935898	0.003401	0.282638
-17.363282	-2.179450	0.940902	0.003414	0.282620
-17.478333	-2.218147	0.945907	0.003435	0.282315
-17.474748	-2.218420	0.950912	0.003435	0.282316
-17.532913	-2.222200	0.955917	0.003446	0.282243
-17.831361	-2.217216	0.960922	0.003501	0.281990
-17.832543	-2.219542	0.965926	0.003502	0.281976
-17.595992	-2.284486	0.970931	0.003458	0.281864
-18.275937	-2.192424	0.975936	0.003584	0.281701
-18.408682	-2.168282	0.980941	0.003609	0.281701
-18.119521	-2.256653	0.985946	0.003555	0.281517
-18.673600	-2.184166	0.990950	0.003658	0.281372
-18.578936	-2.201327	0.995955	0.003641	0.281372
-18.567191	-2.249870	1.000960	0.003639	0.281133
-18.997458	-2.186332	1.005965	0.003719	0.281057
-18.692453	-2.241329	1.010970	0.003662	0.281059
-19.088687	-2.232181	1.015974	0.003736	0.280735
-19.036767	-2.239629	1.020979	0.003726	0.280745
-19.438381	-2.175816	1.025984	0.003801	0.280697
-19.339059	-2.232598	1.030989	0.003782	0.280497
-19.830780	-2.137246	1.035994	0.003874	0.280528
-20.266097	-2.077307	1.040998	0.003955	0.280428
-20.344341	-2.111610	1.046003	0.003970	0.280178
-20.149891	-2.146750	1.051008	0.003934	0.280179
-19.937414	-2.212224	1.056013	0.003894	0.280040
-20.886599	-2.071438	1.061018	0.004071	0.279875
-21.127136	-2.027189	1.066022	0.004116	0.279878
-20.766208	-2.112802	1.071027	0.004048	0.279774
-21.204686	-2.075957	1.076032	0.004130	0.279552
-21.372645	-2.046861	1.081037	0.004161	0.279544
-21.251914	-2.077229	1.086042	0.004139	0.279500
-21.259436	-2.126360	1.091046	0.004140	0.279239
-21.069565	-2.161086	1.096051	0.004105	0.279237
-21.390181	-2.119426	1.101056	0.004165	0.279151
-21.427921	-2.161495	1.106061	0.004172	0.278897
-21.388443	-2.166096	1.111066	0.004165	0.278910
-21.527154	-2.173869	1.116070	0.004190	0.278739
-21.532898	-2.203373	1.121075	0.004192	0.278580
-21.873468	-2.137755	1.126080	0.004255	0.278599
-22.071851	-2.149690	1.131085	0.004292	0.278349
-22.634435	-2.059215	1.136090	0.004397	0.278287
-22.164811	-2.148544	1.141094	0.004309	0.278267
-22.193795	-2.188560	1.146099	0.004315	0.278031
-22.391914	-2.163544	1.151104	0.004352	0.277973
-22.369799	-2.173494	1.156109	0.004348	0.277942
-22.485516	-2.209075	1.161114	0.004369	0.277647
-22.910108	-2.135070	1.166118	0.004448	0.277630
-22.783618	-2.178822	1.171123	0.004425	0.277522
-23.038468	-2.169387	1.176128	0.004472	0.277329
-23.323159	-2.118400	1.181133	0.004525	0.277325
-23.341950	-2.147782	1.186138	0.004529	0.277153
-23.373699	-2.172547	1.191142	0.004535	0.276994
-23.431724	-2.160328	1.196147	0.004546	0.277002
-23.585429	-2.176867	1.201152	0.004574	0.276769
-23.839094	-2.142873	1.206157	0.004621	0.276706
-24.148945	-2.081557	1.211162	0.004679	0.276732
-24.323207	-2.117727	1.216166	0.004712	0.276376
-24.336613	-2.113603	1.221171	0.004714	0.276385
-24.294493	-2.128274	1.226176	0.004706	0.276348
-24.767049	-2.094765	1.231181	0.004794	0.276073
-24.802421	-2.085688	1.236186	0.004801	0.276087
-24.618003	-2.136399	1.241190	0.004767	0.275996
-24.723034	-2.163299	1.246195	0.004786	0.275755
-24.905600	-2.130241	1.251200	0.004820	0.275754
-25.130970	-2.113254	1.256205	0.004862	0.275628
-25.055226	-2.147992	1.261210	0.004848	0.275517
-25.188146	-2.126138	1.266214	0.004873	0.275505
-25.527773	-2.111313	1.271219	0.004936	0.275258
-25.698655	-2.094998	1.276224	0.004968	0.275180
-25.939848	-2.052004	1.281229	0.005013	0.275176
-25.748737	-2.141461	1.286234	0.004978	0.274887
-25.896579	-2.120940	1.291238	0.005005	0.274854
-26.300349	-2.052743	1.296243	0.005080	0.274826
-26.980719	-1.979752	1.301248	0.005207	0.274558
-26.931179	-1.990179	1.306253	0.005198	0.274551
-26.605473	-2.050256	1.311258	0.005137	0.274546
-27.176923	-2.001407	1.316262	0.005244	0.274255
-27.497175	-1.940133	1.321267	0.005303	0.274271
-27.612249	-1.917868	1.326272	0.005325	0.274278
-27.661062	-1.966281	1.331277	0.005334	0.273975
-27.731328	-1.961530	1.336282	0.005347	0.273933
-27.776430	-1.955090	1.341286	0.005355	0.273923
-27.790555	-1.992660	1.346291	0.005358	0.273711
-27.732535	-2.021465	1.351296	0.005347	0.273614
-28.109923	-1.953446	1.356301	0.005418	0.273611
-27.807205	-2.047395	1.361306	0.005361	0.273405
-28.300693	-1.978606	1.366310	0.005453	0.273294
-28.558727	-1.929569	1.371315	0.005501	0.273305
-27.742829	-2.119189	1.376320	0.005349	0.273086
-28.355008	-2.026372	1.381325	0.005463	0.272987
-28.517961	-1.994261	1.386330	0.005494	0.273000
-28.026281	-2.146289	1.391334	0.005402	0.272668
-28.382437	-2.084989	1.396339	0.005469	0.272649
-28.560423	-2.065733	1.401344	0.005502	0.272580
-29.326347	-1.969024	1.406349	0.005644	0.272353
-28.686551	-2.086414	1.411354	0.005525	0.272347
-29.820572	-1.897193	1.416358	0.005736	0.272257
-30.069290	-1.891569	1.421363	0.005783	0.272046
-29.330680	-2.027887	1.426368	0.005645	0.272035
-29.502539	-2.018748	1.431373	0.005677	0.271917
-29.955399	-1.969188	1.436378	0.005762	0.271742
-29.652776	-2.026618	1.441382	0.005705	0.271729
-29.458403	-2.095754	1.446387	0.005669	0.271549
-30.103615	-2.007406	1.451392	0.005789	0.271394
-29.798910	-2.066616	1.456397	0.005733	0.271374
-29.669282	-2.134903	1.461402	0.005709	0.271135
-29.987351	-2.089192	1.466406	0.005768	0.271070
-30.208221	-2.061160	1.471411	0.005809	0.271005
-30.397138	-2.069808	1.476416	0.005844	0.270775
-30.386213	-2.074985	1.481421	0.005842	0.270758
-30.764023	-2.030690	1.486426	0.005913	0.270627
-31.425189	-1.929573	1.491430	0.006036	0.270524
-30.651929	-2.072262	1.496435	0.005892	0.270513
-30.757974	-2.103367	1.501440	0.005912	0.270243
-31.495774	-1.982535	1.506445	0.006049	0.270171
-30.781407	-2.121578	1.511450	0.005916	0.270122
-31.032466	-2.128584	1.516454	0.005963	0.269840
-31.142906	-2.109203	1.521459	0.005984	0.269836
-31.508796	-2.075625	1.526464	0.006052	0.269659
-31.449161	-2.114841	1.531469	0.006041	0.269506
-31.587836	-2.088013	1.536474	0.006066	0.269515
-32.220099	-2.024241	1.541478	0.006184	0.269239
-31.839413	-2.094377	1.546483	0.006113	0.269234
-31.720896	-2.141537	1.551488	0.006091	0.269096
-32.445919	-2.046309	1.556493	0.006226	0.268899
-32.165720	-2.095117	1.561498	0.006174	0.268910
-32.484939	-2.087487	1.566502	0.006234	0.268638
-32.849067	-2.031505	1.571507	0.006301	0.268583
-32.337194	-2.136875	1.576512	0.006206	0.268517
-32.959635	-2.070541	1.581517	0.006322	0.268263
-33.156959	-2.033379	1.586522	0.006359	0.268270
-33.257798	-2.045383	1.591526	0.006378	0.268106
-33.290634	-2.064795	1.596531	0.006384	0.267969
-32.830322	-2.148823	1.601536	0.006298	0.267967
-33.326878	-2.122328	1.606541	0.006391	0.267622
-33.167233	-2.149645	1.611546	0.006361	0.267631
-32.948341	-2.225661	1.616550	0.006320	0.267435
-33.699038	-2.113775	1.621555	0.006460	0.267301
-33.651319	-2.125963	1.626560	0.006451	0.267282
-33.927611	-2.131865	1.631565	0.006503	0.266977
-34.148071	-2.088210	1.636570	0.006544	0.266996
-34.487228	-2.055808	1.641574	0.006607	0.266837
-34.523623	-2.072698	1.646579	0.006614	0.266709
-34.434464	-2.087064	1.651584	0.006597	0.266719
-34.739702	-2.091741	1.656589	0.006654	0.266392
-34.822945	-2.078940	1.661594	0.006670	0.266379
-34.887708	-2.085911	1.666598	0.006682	0.266277
-35.177852	-2.072942	1.671603	0.006736	0.266060
-35.404862	-2.029111	1.676608	0.006778	0.266074
-35.189813	-2.110930	1.681613	0.006738	0.265841
-35.479875	-2.074844	1.686618	0.006792	0.265750
-35.510590	-2.076977	1.691622	0.006798	0.265708
-35.519209	-2.117795	1.696627	0.006800	0.265477
-35.234829	-2.169155	1.701632	0.006747	0.265479
-35.700401	-2.128901	1.706637	0.006833	0.265236
-36.059722	-2.080535	1.711642	0.006900	0.265143
-35.855178	-2.127025	1.716646	0.006862	0.265092
-36.382456	-2.080662	1.721651	0.006960	0.264821
-36.028855	-2.146117	1.726656	0.006895	0.264815
-36.117388	-2.171447	1.731661	0.006911	0.264588
-36.574168	-2.105630	1.736666	0.006996	0.264493
-36.459346	-2.137403	1.741670	0.006975	0.264433
-36.791773	-2.119303	1.746675	0.007037	0.264201
-36.440404	-2.181577	1.751680	0.006971	0.264210
-37.082614	-2.110942	1.756685	0.007091	0.263956
-37.191790	-2.106405	1.761690	0.007111	0.263872
-37.086797	-2.138806	1.766694	0.007092	0.263799
-37.226574	-2.158314	1.771699	0.007118	0.263552
-37.269539	-2.148694	1.776704	0.007126	0.263562
-37.303792	-2.189702	1.781709	0.007132	0.263302
-37.663956	-2.134231	1.786714	0.007200	0.263246
-37.977966	-2.095646	1.791718	0.007258	0.263144
-38.401833	-2.052742	1.796723	0.007337	0.262956
-37.996115	-2.126382	1.801728	0.007261	0.262957
-38.784892	-2.029303	1.806733	0.007408	0.262701
-38.732387	-2.054428	1.811738	0.007399	0.262615
-38.285219	-2.144289	1.816742	0.007315	0.262567
-38.464268	-2.161696	1.821747	0.007349	0.262291
-38.510051	-2.153240	1.826752	0.007357	0.262292
-38.688494	-2.164318	1.831757	0.007391	0.262051
-39.117810	-2.100883	1.836762	0.007471	0.261970
-39.239391	-2.089085	1.841766	0.007493	0.261913
-39.344278	-2.112221	1.846771	0.007513	0.261679
-39.171681	-2.142540	1.851776	0.007481	0.261685
-39.645094	-2.100212	1.856781	0.007569	0.261442
-39.409558	-2.161605	1.861786	0.007525	0.261339
-39.329041	-2.189900	1.866790	0.007510	0.261263
-39.884276	-2.129497	1.871795	0.007613	0.261038
-40.099886	-2.088648	1.876800	0.007654	0.261047
-40.304506	-2.094417	1.881805	0.007692	0.260808
-40.365464	-2.097359	1.886810	0.007703	0.260730
-40.378870	-2.104684	1.891814	0.007706	0.260676
-40.537881	-2.111625	1.896819	0.007735	0.260476
-40.594177	-2.099445	1.901824	0.007746	0.260487
-40.964893	-2.073839	1.906829	0.007815	0.260254
-41.224868	-2.046616	1.911834	0.007863	0.260142
-41.194592	-2.054587	1.916838	0.007858	0.260128
-41.031682	-2.140826	1.921843	0.007827	0.259812
-41.204160	-2.108373	1.926848	0.007860	0.259818
-41.438813	-2.098334	1.931853	0.007903	0.259636
-41.342581	-2.142407	1.936858	0.007885	0.259488
-41.424736	-2.133395	1.941862	0.007901	0.259454
-41.904212	-2.091581	1.946867	0.007990	0.259201
-41.689584	-2.128298	1.951872	0.007950	0.259213
-41.710813	-2.164703	1.956877	0.007954	0.258988
-42.272615	-2.084266	1.961882	0.008059	0.258866
-42.050275	-2.132805	1.966886	0.008017	0.258821
-42.237933	-2.145571	1.971891	0.008052	0.258558
-42.426709	-2.110334	1.976896	0.008088	0.258563
-42.811549	-2.082042	1.981901	0.008159	0.258329
-42.562145	-2.144250	1.986906	0.008113	0.258234
-42.845795	-2.102280	1.991910	0.008166	0.258180
-43.163391	-2.087027	1.996915	0.008225	0.257941
-43.272232	-2.082864	2.001920	0.008245	0.257853

-43.651164	-2.056236	2.011917	0.008316	0.257615
-43.697262	-2.092566	2.021914	0.008324	0.257363
-43.682312	-2.113755	2.031910	0.008322	0.257259
-43.979503	-2.112150	2.041907	0.008377	0.256963
-44.062247	-2.101613	2.051904	0.008393	0.256937
-44.342488	-2.095658	2.061901	0.008445	0.256683
-44.233447	-2.116183	2.071898	0.008425	0.256678
-44.361738	-2.125561	2.081894	0.008449	0.256493
-44.621292	-2.103647	2.091891	0.008497	0.256350
-44.695222	-2.089447	2.101888	0.008511	0.256354
-44.894396	-2.052668	2.111885	0.008548	0.256357
-44.345410	-2.171520	2.121882	0.008446	0.256249
-44.890763	-2.109545	2.131878	0.008547	0.256038
-44.660032	-2.152748	2.141875	0.008505	0.256031
-44.574678	-2.167684	2.151872	0.008489	0.256034
-44.802696	-2.124704	2.161869	0.008531	0.256042
-44.816474	-2.122153	2.171866	0.008534	0.256042
-44.899626	-2.107547	2.181862	0.008549	0.256038
-44.885055	-2.110544	2.191859	0.008547	0.256036
-44.754242	-2.134500	2.201856	0.008522	0.256035
-44.881092	-2.089269	2.211853	0.008546	0.256160
-44.634307	-2.100554	2.221850	0.008500	0.256349
-44.875003	-2.057047	2.231846	0.008545	0.256347
-44.516878	-2.122370	2.241843	0.008479	0.256346
-44.541630	-2.117547	2.251840	0.008483	0.256347
-44.641968	-2.063960	2.261837	0.008502	0.256547
-44.259694	-2.109482	2.271834	0.008431	0.256682
-44.414038	-2.081862	2.281830	0.008460	0.256679
-44.269103	-2.091912	2.291827	0.008433	0.256771
-43.863386	-2.130974	2.301824	0.008357	0.256966
-43.950289	-2.114520	2.311821	0.008373	0.256969
-43.935249	-2.088607	2.321818	0.008371	0.257131
-43.896362	-2.064827	2.331814	0.008364	0.257304
-43.842284	-2.070356	2.341811	0.008354	0.257328
-43.464971	-2.088533	2.351808	0.008283	0.257611
-43.493583	-2.082290	2.361805	0.008289	0.257617
-43.259198	-2.071571	2.371802	0.008245	0.257916
-43.122066	-2.090895	2.381798	0.008220	0.257948
-42.956263	-2.080280	2.391795	0.008189	0.258176
-42.827063	-2.093306	2.401792	0.008165	0.258234
-42.636207	-2.083159	2.411789	0.008129	0.258486
-42.393545	-2.113864	2.421786	0.008084	0.258561
-42.418451	-2.061016	2.431782	0.008089	0.258831
-41.947444	-2.139427	2.441779	0.008001	0.258871
-42.122104	-2.046389	2.451776	0.008034	0.259213
-42.123282	-2.029781	2.461773	0.008034	0.259304
-41.663276	-2.077949	2.471770	0.007949	0.259502
-41.570513	-2.057817	2.481766	0.007931	0.259709
-41.381809	-2.069928	2.491763	0.007896	0.259832
-41.387833	-2.012954	2.501760	0.007898	0.260143
-40.988348	-2.057326	2.511757	0.007823	0.260300
-40.660410	-2.083848	2.521754	0.007762	0.260484
-40.743129	-2.030984	2.531750	0.007778	0.260694
-40.378085	-2.071831	2.541747	0.007710	0.260835
-40.011741	-2.102069	2.551744	0.007642	0.261037
-39.662944	-2.122620	2.561741	0.007577	0.261275
-39.860212	-2.059729	2.571738	0.007614	0.261424
-39.187856	-2.136007	2.581734	0.007489	0.261679
-39.323366	-2.075648	2.591731	0.007514	0.261876
-39.179571	-2.074623	2.601728	0.007487	0.262026
-38.737611	-2.106514	2.611725	0.007405	0.262293
-38.326938	-2.143374	2.621722	0.007329	0.262502
-38.232244	-2.133514	2.631718	0.007311	0.262651
-37.887185	-2.143520	2.641715	0.007247	0.262941
-37.923748	-2.104097	2.651712	0.007254	0.263121
-37.587427	-2.134991	2.661709	0.007191	0.263288
-37.320184	-2.134962	2.671706	0.007141	0.263555
-36.978822	-2.158868	2.681702	0.007078	0.263764
-37.256114	-2.076272	2.691699	0.007130	0.263940
-37.003763	-2.073805	2.701696	0.007083	0.264205
-36.518717	-2.117042	2.711693	0.006992	0.264451
-36.408189	-2.102294	2.721690	0.006972	0.264642
-35.860480	-2.171314	2.731686	0.006870	0.264809
-35.920319	-2.102918	2.741683	0.006881	0.265123
-35.474308	-2.145532	2.751680	0.006798	0.265333
-35.259052	-2.151738	2.761677	0.006758	0.265512
-35.061267	-2.147458	2.771674	0.006721	0.265731
-34.800213	-2.151614	2.781670	0.006673	0.265967
-35.057270	-2.067458	2.791667	0.006721	0.266170
-34.585225	-2.114492	2.801664	0.006633	0.266381
-33.971043	-2.168777	2.811661	0.006519	0.266693
-34.223373	-2.087896	2.821658	0.006566	0.266882
-33.743238	-2.137860	2.831654	0.006476	0.267084
-33.669477	-2.110012	2.841651	0.006463	0.267308
-33.460386	-2.091709	2.851648	0.006424	0.267612
-33.092644	-2.116659	2.861645	0.006355	0.267839
-33.121434	-2.069090	2.871642	0.006361	0.268067
-32.518393	-2.145239	2.881638	0.006249	0.268248
-32.289000	-2.128156	2.891635	0.006206	0.268565
-31.940413	-2.156150	2.901632	0.006141	0.268755
-31.839182	-2.134502	2.911629	0.006122	0.268971
-31.641330	-2.125168	2.921626	0.006086	0.269214
-31.387528	-2.122343	2.931622	0.006038	0.269477
-31.190278	-2.117585	2.941619	0.006002	0.269695
-30.829067	-2.144672	2.951616	0.005935	0.269902
-30.705702	-2.121570	2.961613	0.005912	0.270146
-30.378480	-2.120542	2.971610	0.005851	0.270470
-30.177811	-2.124267	2.981606	0.005814	0.270645
-30.067726	-2.107713	2.991603	0.005793	0.270840
-29.471159	-2.176078	3.001600	0.005682	0.271054
-29.321979	-2.148150	3.011597	0.005654	0.271348
-29.118198	-2.146134	3.021594	0.005616	0.271556
-28.924784	-2.138937	3.031590	0.005581	0.271781
-28.982440	-2.089035	3.041587	0.005591	0.271991
-28.255174	-2.161627	3.051584	0.005456	0.272308
-28.242946	-2.124681	3.061581	0.005454	0.272516
-28.041806	-2.118839	3.071578	0.005416	0.272741
-27.548827	-2.166772	3.081574	0.005325	0.272962
-27.573653	-2.106974	3.091571	0.005329	0.273255
-27.361034	-2.099707	3.101568	0.005290	0.273498
-27.269267	-2.073410	3.111565	0.005273	0.273725
-26.761571	-2.123711	3.121562	0.005178	0.273947
-26.620092	-2.097058	3.131558	0.005152	0.274223
-26.369981	-2.092597	3.141555	0.005106	0.274486
-26.102083	-2.097302	3.151552	0.005056	0.274718
-26.063028	-2.058935	3.161549	0.005048	0.274957
-25.712662	-2.077068	3.171546	0.004983	0.275197
-25.351330	-2.085252	3.181542	0.004916	0.275499
-25.461845	-2.024475	3.191539	0.004937	0.275712
-25.082999	-2.048792	3.201536	0.004866	0.275946
-24.613309	-2.092699	3.211533	0.004779	0.276163
-24.279453	-2.110943	3.221530	0.004717	0.276385
-24.165882	-2.072871	3.231526	0.004696	0.276692
-23.593600	-2.134214	3.241523	0.004589	0.276916
-23.690772	-2.071965	3.251520	0.004607	0.277148
-23.432878	-2.074951	3.261517	0.004559	0.277377
-23.009339	-2.104945	3.271514	0.004481	0.277622
-22.851135	-2.074102	3.281510	0.004451	0.277932
-22.589203	-2.080331	3.291507	0.004403	0.278148
-22.315891	-2.088540	3.301504	0.004352	0.278363
-21.854682	-2.132173	3.311501	0.004266	0.278572
-21.328954	-2.169599	3.321498	0.004168	0.278874
-21.556653	-2.083816	3.331494	0.004211	0.279104
-21.218637	-2.103379	3.341491	0.004148	0.279321
-21.114196	-2.080798	3.351488	0.004128	0.279536
-20.391181	-2.155928	3.361485	0.003994	0.279827
-20.171911	-2.152787	3.371482	0.003953	0.280049
-20.247242	-2.096214	3.381478	0.003967	0.280270
-19.641982	-2.164596	3.391475	0.003854	0.280485
-19.516049	-2.143286	3.401472	0.003831	0.280713
-19.485060	-2.107099	3.411469	0.003825	0.280928
-19.066433	-2.141750	3.421466	0.003748	0.281141
-18.698667	-2.169779	3.431462	0.003679	0.281341
-18.292263	-2.182385	3.441459	0.003604	0.281656
-18.189859	-2.166170	3.451456	0.003585	0.281834
-17.950395	-2.172989	3.461453	0.003540	0.282022
-17.639168	-2.177608	3.471450	0.003482	0.282289
-17.476818	-2.157846	3.481446	0.003452	0.282541
-17.360881	-2.136975	3.491443	0.003430	0.282755
-16.968628	-2.165934	3.501440	0.003357	0.282972
-16.756198	-2.153295	3.511437	0.003318	0.283234
-16.271681	-2.195317	3.521434	0.003228	0.283469
-16.121301	-2.187086	3.531430	0.003200	0.283650
-15.777909	-2.209821	3.541427	0.003136	0.283852
-15.478359	-2.202164	3.551424	0.003080	0.284168
-15.161255	-2.227803	3.561421	0.003021	0.284331
-15.083911	-2.206402	3.571418	0.003007	0.284511
-14.887777	-2.183788	3.581414	0.002971	0.284807
-14.520233	-2.207460	3.591411	0.002902	0.285026
-14.474171	-2.177609	3.601408	0.002894	0.285220
-13.966403	-2.221151	3.611405	0.002799	0.285467
-13.860381	-2.196072	3.621402	0.002779	0.285691
-13.721670	-2.183249	3.631398	0.002754	0.285884
-13.522173	-2.180101	3.641395	0.002717	0.286083
-13.350996	-2.159145	3.651392	0.002685	0.286346
-12.859132	-2.193997	3.661389	0.002593	0.286621
-12.716201	-2.182115	3.671386	0.002567	0.286812
-12.476055	-2.191019	3.681382	0.002522	0.286987
-11.857085	-2.243494	3.691379	0.002407	0.287289
-11.852308	-2.204326	3.701376	0.002406	0.287491
-11.489602	-2.232154	3.711373	0.002339	0.287682
-11.161204	-2.239583	3.721370	0.002278	0.287945
-10.899253	-2.240536	3.731366	0.002229	0.288179
-10.654021	-2.251372	3.741363	0.002183	0.288348
-10.303495	-2.273800	3.751360	0.002118	0.288555
-9.996486	-2.273608	3.761357	0.002061	0.288835
-9.961414	-2.244842	3.771354	0.002055	0.289011
-9.327831	-2.322374	3.781350	0.001937	0.289199
-9.296791	-2.274337	3.791347	0.001931	0.289467
-8.990712	-2.296828	3.801344	0.001874	0.289633
-8.680601	-2.316178	3.811341	0.001816	0.289817
-8.514989	-2.284797	3.821338	0.001786	0.290124
-8.450103	-2.260321	3.831334	0.001774	0.290304
-8.227625	-2.262065	3.841331	0.001732	0.290497
-8.002948	-2.255361	3.851328	0.001690	0.290733
-7.673029	-2.272619	3.861325	0.001629	0.290945
-7.450699	-2.277304	3.871322	0.001588	0.291123
-7.044439	-2.303165	3.881318	0.001512	0.291361
-6.838305	-2.289675	3.891315	0.001474	0.291614
-6.675505	-2.285657	3.901312	0.001444	0.291780
-6.451326	-2.285552	3.911309	0.001402	0.291982
-6.078838	-2.294895	3.921306	0.001333	0.292271
-5.970056	-2.279782	3.931302	0.001312	0.292443
-5.663563	-2.298844	3.941299	0.001255	0.292624
-5.332217	-2.291869	3.951296	0.001194	0.292956
-5.185278	-2.285033	3.961293	0.001167	0.293121
-5.122505	-2.259304	3.971290	0.001155	0.293304
-4.732925	-2.276591	3.981286	0.001082	0.293568
-4.464856	-2.278641	3.991283	0.001033	0.293798
-4.500106	-2.231793	4.001280	0.001039	0.293997
-4.309943	-2.221322	4.011277	0.001004	0.294218
-4.121007	-2.197568	4.021274	0.000969	0.294503
-3.880904	-2.194882	4.031270	0.000924	0.294730
-4.053844	-2.116619	4.041267	0.000956	0.294960
-3.582687	-2.154338	4.051264	0.000869	0.295194
-3.442334	-2.120020	4.061261	0.000843	0.295487
-3.460624	-2.069681	4.071258	0.000846	0.295717
-3.279481	-2.052718	4.081254	0.000812	0.295961
-3.110687	-2.030316	4.091251	0.000781	0.296220
-2.902281	-2.014743	4.101248	0.000742	0.296481
-2.673526	-2.000177	4.111245	0.000700	0.296754
-2.725962	-1.938001	4.121242	0.000709	0.297010
-2.497338	-1.917971	4.131238	0.000667	0.297310
-2.277426	-1.895760	4.141235	0.000626	0.297612
-2.239656	-1.839835	4.151232	0.000619	0.297917
-1.993152	-1.827910	4.161229	0.000573	0.298192
-1.980863	-1.769855	4.171226	0.000571	0.298484
-1.808305	-1.738944	4.181222	0.000539	0.298785
-1.788023	-1.675017	4.191219	0.000535	0.299112
-1.589166	-1.648014	4.201216	0.000498	0.299417
-1.585274	-1.582009	4.211213	0.000497	0.299739
-1.325406	-1.560325	4.221210	0.000449	0.300071
-1.152823	-1.518698	4.231206	0.000417	0.300423
-1.073373	-1.476749	4.241203	0.000402	0.300694
-1.164209	-1.387688	4.251200	0.000419	0.301043
-0.985764	-1.344752	4.261197	0.000386	0.301404
-1.002664	-1.265574	4.271194	0.000389	0.301769
-0.734916	-1.242271	4.281190	0.000339	0.302114
-0.916852	-1.131648	4.291187	0.000373	0.302485
-0.791408	-1.072904	4.301184	0.000350	0.302874
-0.754151	-0.991963	4.311181	0.000343	0.303292
-0.667078	-0.925618	4.321178	0.000327	0.303684
-0.426482	-0.885893	4.331174	0.000282	0.304081
-0.352661	-0.816255	4.341171	0.000268	0.304476
-0.411544	-0.710238	4.351168	0.000279	0.304928
-0.312175	-0.640108	4.361165	0.000261	0.305346
-0.355638	-0.544074	4.371162	0.000269	0.305763
-0.239297	-0.473694	4.381158	0.000247	0.306195
-0.079552	-0.409332	4.391155	0.000217	0.306636
0.027296	-0.329883	4.401152	0.000198	0.307102
-0.110590	-0.210662	4.411149	0.000223	0.307545
-0.065333	-0.106298	4.421146	0.000215	0.308074
0.056077	-0.033339	4.431142	0.000192	0.308519
0.039672	0.079777	4.441139	0.000195	0.309035
0.000000	0.175589	4.451136	0.000203	0.309449

-0.067224	0.456378	4.456141	0.000215	0.310702
0.104797	0.983810	4.461146	0.000183	0.313293
0.399586	1.774251	4.466150	0.000127	0.317167
0.544755	2.879536	4.471155	0.000100	0.322288
0.404298	4.328732	4.476160	0.000125	0.328617
0.480424	6.026317	4.481165	0.000110	0.336067
1.107207	7.925888	4.486170	-0.000008	0.344626
1.165343	10.240571	4.491174	-0.000021	0.354253
1.632050	12.777511	4.496179	-0.000109	0.364803
1.984560	15.663971	4.501184	-0.000177	0.376322
2.011109	18.932360	4.506189	-0.000184	0.388703
2.436842	22.459378	4.511194	-0.000265	0.401894
2.707766	26.355737	4.516198	-0.000318	0.415854
2.797159	30.630845	4.521203	-0.000338	0.430525
3.268877	35.173571	4.526208	-0.000428	0.445806
3.787443	40.057312	4.531213	-0.000528	0.461677
4.388810	45.277539	4.536218	-0.000643	0.478084
4.437160	50.938607	4.541222	-0.000656	0.494943
4.872448	56.874028	4.546227	-0.000741	0.512220
5.400461	63.117293	4.551232	-0.000843	0.529820
5.519494	69.749435	4.556237	-0.000870	0.547686
6.199223	76.593397	4.561242	-0.001001	0.565787
6.491150	83.807887	4.566246	-0.001060	0.584072
6.876588	91.283676	4.571251	-0.001136	0.602470
7.395616	99.007061	4.576256	-0.001238	0.620954
7.773234	106.995627	4.581261	-0.001313	0.639447
8.385468	115.185317	4.586266	-0.001433	0.657954
8.561247	123.660515	4.591270	-0.001471	0.676397
8.981702	132.271586	4.596275	-0.001555	0.694725
9.420063	141.063993	4.601280	-0.001642	0.712956
10.203464	149.936689	4.606285	-0.001794	0.731012
11.321471	158.919574	4.611290	-0.002008	0.748960
11.791238	168.121713	4.616294	-0.002101	0.766683
12.282953	177.428667	4.621299	-0.002199	0.784205
15.029375	186.430389	4.626304	-0.002716	0.801515
15.868200	195.862257	4.631309	-0.002878	0.818619
16.650419	205.379383	4.636314	-0.003030	0.835503
17.193935	214.950032	4.641318	-0.003138	0.852072
18.682466	224.389140	4.646323	-0.003421	0.868382
19.883827	233.905900	4.651328	-0.003651	0.884434
20.360624	243.562135	4.656333	-0.003746	0.900219
21.244936	253.141679	4.661338	-0.003917	0.915723
22.325389	262.668621	4.666342	-0.004124	0.930940
22.989097	272.257903	4.671347	-0.004254	0.945896
23.751516	281.805354	4.676352	-0.004402	0.960581
24.152001	291.376171	4.681357	-0.004483	0.974985
25.073653	300.843360	4.686362	-0.004660	0.989161
25.840246	310.272217	4.691366	-0.004809	1.003041
26.264688	319.720086	4.696371	-0.004894	1.016674
27.274566	329.025430	4.701376	-0.005089	1.030069
27.897695	338.337006	4.706381	-0.005211	1.043207
28.559069	347.619772	4.711386	-0.005340	1.056151
29.290188	356.839719	4.716390	-0.005482	1.068869
30.259647	365.967527	4.721395	-0.005668	1.081368
30.713268	375.149424	4.726400	-0.005759	1.093679
31.411924	384.239025	4.731405	-0.005895	1.105786
32.210844	393.271940	4.736410	-0.006049	1.117711
33.261525	402.219811	4.741414	-0.006251	1.129456
33.623310	411.253434	4.746419	-0.006324	1.141038
34.183260	420.232366	4.751424	-0.006434	1.152478
35.089223	429.063887	4.756429	-0.006608	1.163696
35.834705	437.922573	4.761434	-0.006753	1.174805
36.708542	446.707459	4.766438	-0.006921	1.185747
37.414133	455.494222	4.771443	-0.007058	1.196556
37.991627	464.271888	4.776448	-0.007172	1.207231
38.473863	473.028986	4.781453	-0.007267	1.217768
38.970084	481.768951	4.786458	-0.007365	1.228197
39.507887	490.458754	4.791462	-0.007471	1.238488
39.931016	499.121545	4.796467	-0.007555	1.248640
40.855183	507.699502	4.801472	-0.007733	1.258710
41.519617	516.293688	4.806477	-0.007862	1.268668
42.113555	524.884442	4.811482	-0.007978	1.278531
42.882805	533.415717	4.816486	-0.008127	1.288284
43.431368	541.976651	4.821491	-0.008235	1.297955
43.868331	550.562570	4.826496	-0.008322	1.307562
44.543885	559.111910	4.831501	-0.008453	1.317102
45.136499	567.577599	4.836506	-0.008569	1.326466
45.809807	576.020291	4.841510	-0.008700	1.335755
46.156920	584.511193	4.846515	-0.008770	1.344972
46.965068	592.915490	4.851520	-0.008926	1.354116
47.488124	601.331068	4.856525	-0.009029	1.363160
47.606832	609.835793	4.861530	-0.009056	1.372167
48.063222	618.247066	4.866534	-0.009147	1.381077
49.094524	626.554890	4.871539	-0.009344	1.389920
50.413775	634.829831	4.876544	-0.009595	1.398723
50.787336	643.236555	4.881549	-0.009670	1.407445
51.447244	651.609601	4.886554	-0.009798	1.416127
51.836189	660.001610	4.891558	-0.009876	1.424729
52.351029	668.365805	4.896563	-0.009978	1.433272
53.183072	676.660743	4.901568	-0.010138	1.441748
53.542291	685.033300	4.906573	-0.010210	1.450173
53.976193	693.396826	4.911578	-0.010296	1.458553
54.380420	701.732246	4.916582	-0.010377	1.466852
54.992123	710.056711	4.921587	-0.010496	1.475127
55.371655	718.375911	4.926592	-0.010572	1.483313
55.797866	726.670839	4.931597	-0.010657	1.491439
56.474055	734.941709	4.936602	-0.010788	1.499536
56.847417	743.253367	4.941606	-0.010863	1.507581
57.325387	751.513478	4.946611	-0.010958	1.515550
57.885579	759.779647	4.951616	-0.011067	1.523496
58.630971	768.012750	4.956621	-0.011211	1.531398
59.408926	776.252152	4.961626	-0.011362	1.539270
59.723164	784.556652	4.966630	-0.011426	1.547092
60.206905	792.820342	4.971635	-0.011521	1.554862
60.604251	801.089383	4.976640	-0.011600	1.562585
60.769635	809.375856	4.981645	-0.011636	1.570252
61.330634	817.609779	4.986650	-0.011746	1.577891
61.861232	825.828087	4.991654	-0.011850	1.585475
61.999538	834.124423	4.996659	-0.011882	1.593036
62.619404	842.311716	5.001664	-0.012002	1.600533
63.259546	850.512496	5.006669	-0.012127	1.608010
63.817921	858.725235	5.011674	-0.012236	1.615451
64.110577	866.981666	5.016678	-0.012296	1.622858
64.395523	875.240098	5.021683	-0.012354	1.630232
65.238274	883.417246	5.026688	-0.012517	1.637581
65.505045	891.619540	5.031693	-0.012571	1.644837
65.987682	899.831780	5.036698	-0.012667	1.652100
66.486752	908.021634	5.041702	-0.012765	1.659314
66.746504	916.244075	5.046707	-0.012819	1.666491
67.134212	924.463669	5.051712	-0.012896	1.673653
67.737406	932.603127	5.056717	-0.013014	1.680745
68.445623	940.765184	5.061722	-0.013151	1.687840
68.895601	948.970726	5.066726	-0.013240	1.694908
68.992777	957.206757	5.071731	-0.013263	1.701924
69.387474	965.416760	5.076736	-0.013342	1.708930
69.701430	973.594287	5.081741	-0.013406	1.715868
69.933213	981.785475	5.086746	-0.013454	1.722780
70.501861	989.929845	5.091750	-0.013566	1.729668
70.714286	998.133519	5.096755	-0.013610	1.736532
71.024702	1006.321157	5.101760	-0.013674	1.743368
71.516722	1014.470601	5.106765	-0.013770	1.750170
72.106438	1022.619117	5.111770	-0.013886	1.756957
72.406560	1030.797260	5.116774	-0.013947	1.763704
72.819954	1038.947821	5.121779	-0.014029	1.770418
73.108263	1047.166208	5.126784	-0.014088	1.777145
73.451692	1055.308160	5.131789	-0.014157	1.783792
73.809594	1063.499504	5.136794	-0.014229	1.790456
74.269106	1071.655050	5.141798	-0.014320	1.797079
74.750274	1079.748110	5.146803	-0.014415	1.803631
74.813329	1087.974131	5.151808	-0.014432	1.810212
75.410131	1096.066948	5.156813	-0.014548	1.816730
75.972253	1104.191251	5.161818	-0.014658	1.823245
76.336784	1112.352383	5.166822	-0.014731	1.829741
76.775889	1120.477590	5.171827	-0.014818	1.836195
77.464635	1128.598123	5.176832	-0.014952	1.842653
77.559938	1136.804218	5.181837	-0.014975	1.849084
78.061113	1144.933256	5.186842	-0.015073	1.855481
78.537317	1153.050395	5.191846	-0.015167	1.861843
79.049857	1161.175453	5.196851	-0.015268	1.868194
79.305729	1169.361292	5.201856	-0.015321	1.874540
79.797693	1177.440391	5.206861	-0.015418	1.880810
80.224286	1185.581398	5.211866	-0.015503	1.887099
80.705987	1193.714752	5.216870	-0.015598	1.893368
80.949313	1201.866051	5.221875	-0.015648	1.899601
81.317706	1210.006998	5.226880	-0.015722	1.905821
81.731244	1218.140747	5.231885	-0.015804	1.912020
81.787342	1226.328173	5.236890	-0.015820	1.918199
82.398423	1234.388648	5.241894	-0.015939	1.924326
82.760258	1242.517079	5.246899	-0.016012	1.930455
83.198026	1250.663348	5.251904	-0.016098	1.936587
83.534321	1258.777650	5.256909	-0.016166	1.942665
83.909755	1266.929898	5.261914	-0.016242	1.948755
84.450663	1275.005715	5.266918	-0.016347	1.954789
84.870181	1283.083465	5.271923	-0.016431	1.960792
85.406202	1291.200539	5.276928	-0.016536	1.966818
85.864129	1299.316949	5.281933	-0.016626	1.972816
86.368471	1307.424346	5.286938	-0.016726	1.978795
86.453454	1315.579544	5.291942	-0.016747	1.984744
86.813157	1323.695868	5.296947	-0.016819	1.990678
87.113374	1331.840860	5.301952	-0.016880	1.996608
87.039465	1339.997672	5.306957	-0.016872	2.002488
87.490839	1348.075696	5.311962	-0.016961	2.008351
87.704360	1356.231592	5.316966	-0.017006	2.014228
88.108497	1364.293424	5.321971	-0.017086	2.020040
88.409786	1372.425842	5.326976	-0.017148	2.025874
88.674007	1380.548574	5.331981	-0.017202	2.031681
88.758805	1388.672177	5.336986	-0.017223	2.037454
89.605859	1396.664145	5.341990	-0.017386	2.043196
90.109266	1404.743053	5.346995	-0.017485	2.048948
90.311621	1412.910314	5.352000	-0.017528	2.054714
90.509362	1421.014475	5.357005	-0.017570	2.060420
91.121788	1429.076348	5.362010	-0.017689	2.066122
91.539991	1437.196663	5.367014	-0.017773	2.071830
91.465464	1445.355729	5.372019	-0.017764	2.077499
91.601880	1453.471712	5.377024	-0.017795	2.083143
92.076683	1461.523125	5.382029	-0.017888	2.088762
92.322544	1469.648134	5.387034	-0.017939	2.094394
92.496166	1477.764638	5.392038	-0.017977	2.099997
93.249447	1485.779920	5.397043	-0.018122	2.105574
93.551090	1493.936798	5.402048	-0.018184	2.111187
93.739213	1502.045571	5.407053	-0.018224	2.116742
94.250812	1510.087844	5.412058	-0.018324	2.122269
94.605893	1518.186571	5.417062	-0.018396	2.127804
94.954684	1526.278744	5.422067	-0.018466	2.133319
95.373363	1534.373499	5.427072	-0.018549	2.138829
95.539842	1542.462958	5.432077	-0.018585	2.144297
95.976132	1550.559953	5.437082	-0.018672	2.149782
96.589456	1558.593550	5.442086	-0.018791	2.155227
96.843828	1566.693156	5.447091	-0.018844	2.160668
97.116838	1574.804624	5.452096	-0.018900	2.166105
97.405578	1582.910953	5.457101	-0.018959	2.171526
97.688117	1591.015348	5.462106	-0.019017	2.176932
98.023786	1599.100662	5.467110	-0.019085	2.182317
98.069540	1607.219379	5.472115	-0.019098	2.187683
98.491347	1615.301701	5.477120	-0.019182	2.193048
98.775962	1623.366570	5.482125	-0.019240	2.198374
99.265769	1631.399926	5.487130	-0.019337	2.203687
99.851108	1639.483468	5.492134	-0.019451	2.209028
100.149601	1647.576608	5.497139	-0.019512	2.214336
100.631997	1655.657638	5.502144	-0.019607	2.219640
100.848480	1663.740307	5.507149	-0.019652	2.224908
101.249974	1671.840348	5.512154	-0.019732	2.230192
101.658277	1679.924123	5.517158	-0.019814	2.235453
101.971061	1687.974262	5.522163	-0.019877	2.240671
102.312455	1696.063444	5.527168	-0.019946	2.245905
102.651827	1704.153775	5.532173	-0.020014	2.251127
102.659014	1712.286466	5.537178	-0.020021	2.256335
102.857942	1720.379107	5.542182	-0.020063	2.261522
103.255848	1728.430089	5.547187	-0.020143	2.266688
103.837740	1736.520049	5.552192	-0.020256	2.271883
104.084817	1744.589343	5.557197	-0.020307	2.277024
104.461744	1752.638762	5.562202	-0.020383	2.282152
105.093587	1760.673157	5.567206	-0.020506	2.287281
105.667960	1768.710697	5.572211	-0.020618	2.292395
106.045213	1776.812784	5.577216	-0.020693	2.297522
106.173138	1784.914643	5.582221	-0.020722	2.302615
106.489863	1792.989505	5.587226	-0.020787	2.307696
106.834927	1801.083748	5.592230	-0.020856	2.312780
107.165679	1809.129560	5.597235	-0.020923	2.317822
107.818158	1817.164495	5.602240	-0.021050	2.322874
108.007898	1825.251174	5.607245	-0.021090	2.327907
108.151240	1833.381294	5.612250	-0.021122	2.332952
108.701809	1841.427099	5.617254	-0.021230	2.337969
108.950502	1849.493040	5.622259	-0.021281	2.342961
109.269453	1857.596507	5.627264	-0.021346	2.347972
109.807855	1865.641527	5.632269	-0.021451	2.352955
110.310441	1873.678236	5.637274	-0.021550	2.357919
110.611518	1881.748109	5.642278	-0.021612	2.362876
110.778695	1889.834606	5.647283	-0.021648	2.367822
111.206801	1897.915622	5.652288	-0.021733	2.372775
111.426375	1905.998554	5.657293	-0.021779	2.377702
111.872689	1914.030911	5.662298	-0.021867	2.382607
112.561595	1922.081250	5.667302	-0.022001	2.387532
112.807694	1930.182961	5.672307	-0.022052	2.392442
112.935479	1938.285495	5.677312	-0.022081	2.397332
113.256997	1946.312101	5.682317	-0.022146	2.402183
113.525784	1954.398956	5.687322	-0.022201	2.407056
113.770165	1962.484514	5.692326	-0.022252	2.411916
114.174835	1970.532165	5.697331	-0.022333	2.416756
114.608239	1978.592916	5.702336	-0.022418	2.421597
114.680587	1986.684356	5.707341	-0.022437	2.426417
114.681948	1994.816132	5.712346	-0.022443	2.431246
115.319768	2002.836243	5.717350	-0.022567	2.436050
115.451873	2010.890872	5.722355	-0.022596	2.440825
115.845933	2018.934854	5.727360	-0.022675	2.445605
116.187022	2026.993099	5.732365	-0.022744	2.450379
116.607970	2035.040265	5.737370	-0.022827	2.455144
116.825375	2043.123551	5.742374	-0.022873	2.459905
117.009623	2051.162464	5.747379	-0.022913	2.464628
117.550830	2059.225820	5.752384	-0.023019	2.469384
117.783195	2067.286475	5.757389	-0.023067	2.474105
117.968991	2075.362356	5.762394	-0.023107	2.478822
118.454165	2083.386852	5.767398	-0.023202	2.483524
118.628331	2091.458124	5.772403	-0.023240	2.488220
119.041015	2099.523600	5.777408	-0.023322	2.492921
119.214503	2107.605490	5.782413	-0.023360	2.497606
119.734506	2115.638057	5.787418	-0.023462	2.502279
119.768111	2123.752740	5.792422	-0.023473	2.506954
120.216305	2131.784745	5.797427	-0.023562	2.511603
120.653354	2139.835008	5.802432	-0.023648	2.516254
120.871882	2147.892983	5.807437	-0.023694	2.520884
121.269499	2155.918177	5.812442	-0.023774	2.525501
121.547550	2163.998388	5.817446	-0.023831	2.530131
121.892551	2172.041336	5.822451	-0.023900	2.534736
122.278848	2180.108119	5.827456	-0.023977	2.539350
122.516961	2188.154331	5.832461	-0.024027	2.543932
122.884078	2196.229565	5.837466	-0.024100	2.548533
123.138592	2204.298117	5.842470	-0.024153	2.553112
123.287664	2212.342200	5.847475	-0.024186	2.557663
123.962813	2220.359905	5.852480	-0.024317	2.562228
124.226479	2228.433112	5.857485	-0.024371	2.566786
124.297513	2236.527821	5.862490	-0.024390	2.571335
124.685759	2244.587967	5.867494	-0.024467	2.575878
125.030104	2252.616206	5.872499	-0.024536	2.580393
125.305440	2260.678660	5.877504	-0.024593	2.584914
125.486450	2268.759769	5.882509	-0.024632	2.589431
126.070617	2276.880860	5.887514	-0.024746	2.593990
126.414459	2284.906536	5.892518	-0.024815	2.598472
126.683968	2292.904921	5.897523	-0.024870	2.602925
126.924738	2300.970468	5.902528	-0.024921	2.607406
127.117553	2309.020718	5.907533	-0.024962	2.611867
127.395032	2317.081048	5.912538	-0.025019	2.616332
127.618488	2325.130872	5.917542	-0.025065	2.620780
128.271087	2333.109079	5.922547	-0.025192	2.625211
128.481548	2341.207552	5.927552	-0.025236	2.629669
128.734293	2349.253611	5.932557	-0.025289	2.634094
129.233194	2357.252192	5.937562	-0.025387	2.638503
129.452008	2365.333275	5.942566	-0.025433	2.642930
129.474122	2373.400260	5.947571	-0.025442	2.647328
130.164523	2381.435315	5.952576	-0.025576	2.651747
130.579195	2389.482598	5.957581	-0.025658	2.656147
130.721822	2397.541892	5.962586	-0.025690	2.660527
131.126069	2405.592731	5.967590	-0.025771	2.664913
131.268873	2413.664951	5.972595	-0.025802	2.669286
131.464340	2421.750985	5.977600	-0.025844	2.673663
132.109384	2429.732080	5.982605	-0.025969	2.678006
132.577162	2437.737754	5.987610	-0.026062	2.682343
133.194711	2445.782590	5.992614	-0.026182	2.686704
133.423868	2453.846285	5.997619	-0.026230	2.691042
133.936766	2461.899090	6.002624	-0.026330	2.695386
134.275262	2469.940211	6.007629	-0.026399	2.699705
134.750476	2477.958497	6.012634	-0.026492	2.704014
135.058189	2486.055909	6.017638	-0.026555	2.708348
135.258288	2494.128388	6.022643	-0.026597	2.712654
135.192863	2502.247072	6.027648	-0.026590	2.716961
135.494435	2510.261268	6.032653	-0.026652	2.721229
135.857108	2518.281463	6.037658	-0.026724	2.725497
136.134276	2526.351922	6.042662	-0.026781	2.729780
136.183653	2534.414010	6.047667	-0.026796	2.734037
136.517649	2542.449851	6.052672	-0.026863	2.738292
136.878724	2550.473769	6.057677	-0.026936	2.742535
137.054060	2558.540247	6.062682	-0.026973	2.746783
137.383306	2566.630761	6.067686	-0.027040	2.751046
137.462500	2574.699339	6.072691	-0.027060	2.755275
137.949819	2582.691223	6.077696	-0.027156	2.759483
137.910908	2590.723312	6.082701	-0.027154	2.763673
138.477531	2598.714432	6.087706	-0.027264	2.767873
138.847078	2606.813977	6.092710	-0.027339	2.772110
138.995411	2614.844613	6.097715	-0.027371	2.776292
139.351928	2622.887000	6.102720	-0.027443	2.780486
139.672788	2630.892257	6.107725	-0.027508	2.784652
140.048046	2638.961895	6.112730	-0.027583	2.788849
139.966820	2647.099868	6.117734	-0.027573	2.793047
140.135549	2655.104450	6.122739	-0.027610	2.797185
140.658286	2663.096595	6.127744	-0.027712	2.801331
141.004269	2671.117259	6.132749	-0.027782	2.805476
141.267971	2679.176612	6.137754	-0.027836	2.809629
141.535304	2687.246405	6.142758	-0.027891	2.813782
141.706520	2695.311360	6.147763	-0.027928	2.817920
141.759843	2703.379933	6.152768	-0.027943	2.822047
142.275194	2711.390360	6.157773	-0.028045	2.826165
142.496738	2719.439967	6.162778	-0.028091	2.830281
142.838798	2727.458664	6.167782	-0.028160	2.834381
143.317389	2735.443938	6.172787	-0.028254	2.838466
143.922180	2743.473284	6.177792	-0.028372	2.842576
143.921756	2751.572321	6.182797	-0.028377	2.846679
144.066817	2759.636126	6.187802	-0.028409	2.850767
144.539154	2767.682828	6.192806	-0.028503	2.854859
144.693014	2775.706479	6.197811	-0.028536	2.858916
144.900354	2783.768394	6.202816	-0.028580	2.862989
145.084628	2791.841432	6.207821	-0.028620	2.867060
145.758786	2799.812573	6.212826	-0.028750	2.871102
146.126907	2807.885460	6.217830	-0.028824	2.875172
146.344016	2815.869823	6.222835	-0.028870	2.879184
146.994009	2823.896490	6.227840	-0.028996	2.883235
147.219911	2831.973262	6.232845	-0.029043	2.887282
147.480269	2840.033816	6.237850	-0.029097	2.891317
148.051687	2848.088382	6.242854	-0.029209	2.895361
147.980967	2856.140520	6.247859	-0.029201	2.899361
148.291599	2864.159777	6.252864	-0.029264	2.903362
148.462587	2872.233599	6.257869	-0.029301	2.907376
148.766090	2880.310198	6.262874	-0.029363	2.911393
149.111345	2888.377682	6.267878	-0.029432	2.915402
149.290411	2896.347816	6.272883	-0.029471	2.919348
149.809193	2904.343691	6.277888	-0.029572	2.923321
150.049942	2912.385350	6.282893	-0.029622	2.927295
150.080178	2920.459461	6.287898	-0.029633	2.931269
150.441435	2928.509901	6.292902	-0.029706	2.935243
151.046165	2936.466918	6.297907	-0.029823	2.939179
151.209605	2944.545356	6.302912	-0.029859	2.943146
151.224147	2952.619856	6.307917	-0.029867	2.947097
151.668518	2960.644005	6.312922	-0.029955	2.951041
152.014508	2968.692466	6.317926	-0.030025	2.954987
152.091892	2976.709422	6.322931	-0.030044	2.958897
152.262742	2984.766641	6.327936	-0.030081	2.962827
152.442605	2992.786105	6.332941	-0.030120	2.966734
152.793566	3000.821463	6.337946	-0.030191	2.970653
153.232442	3008.877424	6.342950	-0.030277	2.974580
153.616534	3016.881797	6.347955	-0.030354	2.978475
153.937533	3024.914664	6.352960	-0.030419	2.982375
154.090763	3032.987328	6.357965	-0.030453	2.986280
154.565504	3041.013341	6.362970	-0.030546	2.990175
154.643165	3049.093417	6.367974	-0.030566	2.994070
154.702913	3057.108029	6.372979	-0.030582	2.997927
155.327520	3065.108268	6.377984	-0.030704	3.001801
155.557718	3073.155492	6.382989	-0.030752	3.005673
155.621289	3081.189266	6.387994	-0.030769	3.009524
155.934257	3089.263615	6.392998	-0.030833	3.013403
156.290584	3097.289005	6.398003	-0.030904	3.017256
156.797543	3105.294455	6.403008	-0.031004	3.021101
157.087313	3113.338635	6.408013	-0.031063	3.024950
157.451571	3121.366307	6.413018	-0.031136	3.028789
157.789748	3129.438661	6.418022	-0.031204	3.032643
157.730048	3137.512063	6.423027	-0.031198	3.036473
158.118136	3145.509009	6.428032	-0.031276	3.040284
158.784864	3153.469796	6.433037	-0.031405	3.044087
158.721373	3161.586100	6.438042	-0.031398	3.047922
159.053510	3169.640141	6.443046	-0.031465	3.051743
159.262199	3177.665029	6.448051	-0.031509	3.055539
159.491769	3185.704466	6.453056	-0.031557	3.059338
159.559285	3193.726398	6.458061	-0.031575	3.063116
159.689040	3201.780397	6.463066	-0.031605	3.066908
160.090946	3209.848851	6.468070	-0.031685	3.070715
160.063494	3217.907967	6.473075	-0.031685	3.074492
160.584982	3225.890304	6.478080	-0.031787	3.078255
160.824010	3233.925812	6.483085	-0.031837	3.082024
161.272937	3241.902220	6.488090	-0.031925	3.085772
161.785479	3249.906809	6.493094	-0.032026	3.089530
161.680085	3258.014886	6.498099	-0.032012	3.093303
162.022001	3266.044794	6.503104	-0.032081	3.097057
162.507468	3274.041749	6.508109	-0.032176	3.100797
162.672010	3282.059770	6.513114	-0.032212	3.104527
163.077078	3290.130445	6.518118	-0.032293	3.108288
163.293638	3298.174253	6.523123	-0.032338	3.112024
163.650568	3306.199447	6.528128	-0.032410	3.115753
163.974694	3314.199896	6.533133	-0.032475	3.119464
164.208599	3322.232008	6.538138	-0.032524	3.123182
164.386583	3330.309268	6.543142	-0.032562	3.126913
164.777378	3338.333497	6.548147	-0.032640	3.130625
165.083996	3346.373180	6.553152	-0.032703	3.134336
165.352281	3354.418229	6.558157	-0.032758	3.138043
165.539639	3362.440840	6.563162	-0.032798	3.141731
165.827184	3370.495719	6.568166	-0.032857	3.145435
165.911913	3378.528548	6.573171	-0.032878	3.149115
166.581352	3386.519588	6.578176	-0.033008	3.152798
166.867725	3394.565129	6.583181	-0.033066	3.156484
167.156263	3402.556990	6.588186	-0.033125	3.160141
167.365050	3410.610028	6.593190	-0.033169	3.163819
167.213488	3418.731399	6.598195	-0.033146	3.167507
167.302829	3426.793795	6.603200	-0.033168	3.171175
167.525374	3434.793316	6.608205	-0.033215	3.174815
168.051395	3442.771726	6.613210	-0.033318	3.178456
168.141084	3450.839455	6.618214	-0.033340	3.182113
168.271442	3458.860066	6.623219	-0.033369	3.185747
168.495112	3466.908476	6.628224	-0.033416	3.189393
169.103268	3474.897016	6.633229	-0.033534	3.193025
169.293248	3482.934129	6.638234	-0.033575	3.196656
169.382308	3491.002042	6.643238	-0.033597	3.200293
169.441119	3498.977227	6.648243	-0.033613	3.203882
169.953768	3507.022643	6.653248	-0.033714	3.207519
170.414443	3515.044166	6.658253	-0.033805	3.211138
170.611635	3523.082845	6.663258	-0.033846	3.214750
170.930477	3531.132970	6.668262	-0.033911	3.218367
170.776536	3539.219358	6.673267	-0.033888	3.221977
171.362427	3547.188213	6.678272	-0.034002	3.225562
171.883982	3555.211562	6.683277	-0.034104	3.229164
171.936934	3563.255020	6.688282	-0.034119	3.232751
172.028543	3571.339564	6.693286	-0.034142	3.236354
172.616495	3579.254846	6.698291	-0.034256	3.239899
173.062405	3587.258609	6.703296	-0.034344	3.243473
173.312895	3595.316594	6.708301	-0.034396	3.247059
173.739562	3603.346612	6.713306	-0.034481	3.250636
174.058657	3611.399316	6.718310	-0.034545	3.254214
174.079181	3619.471351	6.723315	-0.034555	3.257785
174.095189	3627.561167	6.728320	-0.034563	3.261359
174.335382	3635.544816	6.733325	-0.034613	3.264892
174.645866	3643.557624	6.738330	-0.034676	3.268437
174.989192	3651.633704	6.743334	-0.034745	3.272007
175.108382	3659.630180	6.748339	-0.034772	3.275529
175.573715	3667.604737	6.753344	-0.034864	3.279051
175.920694	3675.617532	6.758349	-0.034934	3.282582
175.855971	3683.707683	6.763354	-0.034927	3.286126
176.656850	3691.694186	6.768358	-0.035081	3.289656
176.817846	3699.744774	6.773363	-0.035116	3.293184
177.070656	3707.783527	6.778368	-0.035169	3.296707
177.342975	3715.839961	6.783373	-0.035225	3.300234
177.533843	3723.828762	6.788378	-0.035265	3.303725
178.106260	3731.863852	6.793382	-0.035377	3.307248
178.210767	3739.930862	6.798387	-0.035402	3.310762
178.572602	3747.913494	6.803392	-0.035474	3.314246
178.732709	3755.974730	6.808397	-0.035509	3.317752
178.583079	3764.049451	6.813402	-0.035487	3.321249
179.081645	3772.023847	6.818406	-0.035585	3.324723
179.312860	3780.061140	6.823411	-0.035633	3.328211
179.722140	3788.099705	6.828416	-0.035714	3.331702
180.234407	3796.104437	6.833421	-0.035815	3.335179
180.520043	3804.113366	6.838426	-0.035873	3.338645
180.663088	3812.180413	6.843430	-0.035905	3.342128
180.974270	3820.196041	6.848435	-0.035968	3.345591
181.460033	3828.220646	6.853440	-0.036064	3.349060
181.619698	3836.288451	6.858445	-0.036099	3.352533
181.899770	3844.296590	6.863450	-0.036156	3.355980
182.344799	3852.308792	6.868454	-0.036244	3.359432
182.334609	3860.342436	6.873459	-0.036248	3.362873
182.667181	3868.343333	6.878464	-0.036315	3.366308
183.220857	3876.366130	6.883469	-0.036423	3.369758
183.688223	3884.396171	6.888474	-0.036515	3.373204
183.889363	3892.496632	6.893478	-0.036558	3.376667
184.044512	3900.511274	6.898483	-0.036592	3.380088
184.535980	3908.488839	6.903488	-0.036689	3.383502
184.821132	3916.572602	6.908493	-0.036747	3.386950
184.829610	3924.598159	6.913498	-0.036754	3.390359
185.504144	3932.656941	6.918502	-0.036885	3.393804
185.652772	3940.663282	6.923507	-0.036918	3.397203
185.765537	3948.725045	6.928512	-0.036944	3.400621
186.082676	3956.663081	6.933517	-0.037008	3.403991
186.225426	3964.720820	6.938522	-0.037040	3.407402
186.498277	3972.789697	6.943526	-0.037096	3.410819
186.662003	3980.779054	6.948531	-0.037131	3.414195
186.972727	3988.835859	6.953536	-0.037194	3.417601
187.215248	3996.861355	6.958541	-0.037245	3.420988
187.386496	4004.853398	6.963546	-0.037282	3.424355
187.885471	4012.868215	6.968550	-0.037380	3.427740
188.102014	4020.954336	6.973555	-0.037426	3.431141
188.241633	4028.937324	6.978560	-0.037457	3.434493
188.185050	4036.981105	6.983565	-0.037451	3.437861
188.740573	4044.988479	6.988570	-0.037560	3.441231
189.179177	4053.013690	6.993574	-0.037647	3.444601
189.179223	4061.079597	6.998579	-0.037652	3.447970
189.470582	4069.100105	7.003584	-0.037712	3.451326
189.700691	4077.157600	7.008589	-0.037760	3.454693
189.699312	4085.181369	7.013594	-0.037765	3.458034
190.014970	4093.224406	7.018598	-0.037829	3.461391
190.155675	4101.196549	7.023603	-0.037860	3.464709
190.761340	4109.208360	7.028608	-0.037978	3.468056
191.022048	4117.266123	7.033613	-0.038032	3.471407
191.445469	4125.220577	7.038618	-0.038116	3.474717
191.675721	4133.267155	7.043622	-0.038164	3.478056
191.940822	4141.290062	7.048627	-0.038218	3.481384
192.317852	4149.279985	7.053632	-0.038294	3.484698
192.729815	4157.356601	7.058637	-0.038376	3.488045
192.361086	4165.439548	7.063642	-0.038312	3.491367
192.696955	4173.486418	7.068646	-0.038380	3.494693
193.005437	4181.476532	7.073651	-0.038443	3.497992
193.224986	4189.501183	7.078656	-0.038489	3.501299
193.498295	4197.510245	7.083661	-0.038545	3.504598
194.147204	4205.498687	7.088666	-0.038671	3.507898
194.512170	4213.566963	7.093670	-0.038744	3.511219
194.973626	4221.534022	7.098675	-0.038835	3.514497
195.374139	4229.577652	7.103680	-0.038915	3.517802
195.926641	4237.602576	7.108685	-0.039023	3.521101
195.716905	4245.641543	7.113690	-0.038989	3.524379
196.164012	4253.700042	7.118694	-0.039077	3.527682
196.512140	4261.728834	7.123699	-0.039147	3.530966
196.865933	4269.748728	7.128704	-0.039218	3.534244
197.069323	4277.797892	7.133709	-0.039262	3.537527
197.094009	4285.848499	7.138714	-0.039271	3.540801
197.614773	4293.820581	7.143718	-0.039374	3.544055
197.677024	4301.834798	7.148723	-0.039390	3.547310
197.977021	4309.909780	7.153728	-0.039451	3.550593
198.267943	4317.973031	7.158733	-0.039511	3.553868
198.402796	4325.955464	7.163738	-0.039541	3.557103
198.611457	4333.980544	7.168742	-0.039585	3.560354
198.781492	4341.971155	7.173747	-0.039622	3.563587
199.300294	4349.961215	7.178752	-0.039724	3.566828
199.292997	4358.036562	7.183757	-0.039728	3.570084
199.684996	4366.020137	7.188762	-0.039806	3.573312
200.187500	4374.059447	7.193766	-0.039905	3.576563
200.466278	4382.055536	7.198771	-0.039962	3.579787
200.777792	4390.058846	7.203776	-0.040025	3.583012
201.020609	4398.157134	7.208781	-0.040075	3.586269
201.165576	4406.150249	7.213786	-0.040107	3.589479
201.284402	4414.209443	7.218790	-0.040135	3.592712
201.804261	4422.226723	7.223795	-0.040237	3.595936
202.223829	4430.166703	7.228800	-0.040320	3.599124
202.212032	4438.273922	7.233805	-0.040323	3.602363
202.722476	4446.253018	7.238810	-0.040423	3.605564
203.144543	4454.287429	7.243814	-0.040507	3.608781
203.028902	4462.377947	7.248819	-0.040491	3.612001
203.296093	4470.391227	7.253824	-0.040546	3.615200
203.872553	4478.404933	7.258829	-0.040658	3.618404
203.900558	4486.443019	7.263834	-0.040669	3.621599
204.184314	4494.435105	7.268838	-0.040727	3.624781
204.588095	4502.491818	7.273843	-0.040807	3.627989
204.947736	4510.562182	7.278848	-0.040879	3.631198
205.283861	4518.543746	7.283853	-0.040947	3.634368
205.418114	4526.536627	7.288858	-0.040977	3.637535
205.739151	4534.610904	7.293862	-0.041042	3.640736
206.092286	4542.530416	7.298867	-0.041113	3.643874
206.307557	4550.602050	7.303872	-0.041158	3.647065
206.596603	4558.651078	7.308877	-0.041217	3.650246
206.747737	4566.671017	7.313882	-0.041251	3.653410
206.855981	4574.729572	7.318886	-0.041276	3.656585
207.363483	4582.699638	7.323891	-0.041376	3.659733
207.742146	4590.683440	7.328896	-0.041451	3.662880
207.983360	4598.768221	7.333901	-0.041502	3.666061
208.122113	4606.774103	7.338906	-0.041533	3.669205
208.665921	4614.809005	7.343910	-0.041639	3.672368
208.876857	4622.831859	7.348915	-0.041684	3.675515
208.979306	4630.861996	7.353920	-0.041708	3.678659
209.081665	4638.899062	7.358925	-0.041732	3.681803
209.301698	4646.897382	7.363930	-0.041778	3.684933
209.562853	4654.928608	7.368934	-0.041832	3.688074
209.966378	4662.934653	7.373939	-0.041912	3.691206
210.101568	4670.966754	7.378944	-0.041943	3.694338
210.318573	4679.025866	7.383949	-0.041988	3.697480
210.629327	4687.014108	7.388954	-0.042051	3.700595
211.221134	4695.025628	7.393958	-0.042167	3.703723
211.250341	4703.068375	7.398963	-0.042177	3.706846
211.494963	4711.107497	7.403968	-0.042228	3.709970
211.822234	4719.197145	7.408973	-0.042294	3.713114
212.008542	4727.242709	7.413978	-0.042334	3.716234
212.112329	4735.197279	7.418982	-0.042359	3.719314
212.337527	4743.202154	7.423987	-0.042406	3.722414
212.420918	4751.232081	7.428992	-0.042427	3.725518
212.799378	4759.266290	7.433997	-0.042502	3.728628
212.780427	4767.276806	7.439002	-0.042504	3.731716
213.293058	4775.297219	7.444006	-0.042605	3.734819
213.885605	4783.273067	7.449011	-0.042720	3.737905
214.075726	4791.337211	7.454016	-0.042761	3.741011
214.357015	4799.319330	7.459021	-0.042818	3.744085
214.261071	4807.407402	7.464026	-0.042806	3.747189
214.543258	4815.436213	7.469030	-0.042863	3.750276
215.166040	4823.404224	7.474035	-0.042985	3.753346
215.568252	4831.448643	7.479040	-0.043065	3.756437
215.532488	4839.472399	7.484045	-0.043063	3.759507
215.626154	4847.478113	7.489050	-0.043086	3.762571
215.904239	4855.511372	7.494054	-0.043143	3.765647
216.430710	4863.492224	7.499059	-0.043246	3.768706
216.674931	4871.567234	7.504064	-0.043297	3.771792
216.868219	4879.621043	7.509069	-0.043338	3.774867
217.086556	4887.598743	7.514074	-0.043384	3.777910
217.276438	4895.682435	7.519078	-0.043424	3.780990
217.478360	4903.611872	7.524083	-0.043467	3.784010
218.023136	4911.632461	7.529088	-0.043574	3.787070
218.130690	4919.727220	7.534093	-0.043599	3.790145
218.482405	4927.666933	7.539098	-0.043670	3.793165
218.854838	4935.750312	7.544102	-0.043744	3.796237
219.030789	4943.704839	7.549107	-0.043782	3.799253
219.301202	4951.744185	7.554112	-0.043838	3.802301
219.575683	4959.766726	7.559117	-0.043894	3.805340
219.848166	4967.761205	7.564122	-0.043950	3.808366
220.298715	4975.861422	7.569126	-0.044039	3.811434
220.471024	4983.860972	7.574131	-0.044076	3.814455
220.813243	4991.886542	7.579136	-0.044145	3.817487
220.957437	4999.962065	7.584141	-0.044177	3.820531
221.074758	5007.938620	7.589146	-0.044204	3.823535
221.549520	5015.955006	7.594150	-0.044298	3.826559
221.747326	5023.990266	7.599155	-0.044340	3.829582
221.873923	5032.026204	7.604160	-0.044369	3.832600
222.161324	5040.069865	7.609165	-0.044427	3.835624
222.369323	5048.037169	7.614170	-0.044471	3.838614
222.643024	5056.080326	7.619174	-0.044527	3.841632
222.642487	5064.091721	7.624179	-0.044532	3.844629
222.915603	5072.100099	7.629184	-0.044589	3.847629
223.225621	5080.178758	7.634189	-0.044651	3.850653
223.241492	5088.188073	7.639194	-0.044660	3.853643
223.634241	5096.215361	7.644198	-0.044738	3.856646
224.038493	5104.212384	7.649203	-0.044818	3.859635
224.127334	5112.204520	7.654208	-0.044840	3.862613
224.351489	5120.279071	7.659213	-0.044887	3.865622
224.711230	5128.290978	7.664218	-0.044959	3.868609
225.062038	5136.347576	7.669222	-0.045030	3.871609
225.053909	5144.492301	7.674227	-0.045034	3.874633
225.511583	5152.398223	7.679232	-0.045124	3.877575
225.903866	5160.401660	7.684237	-0.045202	3.880549
225.908653	5168.314200	7.689242	-0.045208	3.883480
226.254273	5176.393470	7.694246	-0.045278	3.886477
226.451130	5184.400411	7.699251	-0.045320	3.889442
226.630399	5192.432277	7.704256	-0.045358	3.892414
227.016072	5200.445440	7.709261	-0.045435	3.895380
227.163555	5208.434812	7.714266	-0.045468	3.898331
227.333804	5216.513776	7.719270	-0.045505	3.901313
227.489780	5224.464131	7.724275	-0.045539	3.904245
227.782463	5232.555638	7.729280	-0.045599	3.907229
228.317662	5240.550311	7.734285	-0.045703	3.910180
228.303070	5248.595408	7.739290	-0.045706	3.913137
228.470066	5256.601099	7.744294	-0.045742	3.916080
228.683923	5264.571229	7.749299	-0.045787	3.919009
228.901756	5272.603420	7.754304	-0.045833	3.921959
229.190534	5280.627754	7.759309	-0.045892	3.924905
229.462222	5288.647212	7.764314	-0.045948	3.927846
229.891245	5296.730221	7.769318	-0.046033	3.930812
229.996100	5304.742624	7.774323	-0.046058	3.933743
230.120186	5312.754916	7.779328	-0.046086	3.936672
230.508892	5320.747428	7.784333	-0.046163	3.939597
230.440478	5328.795543	7.789338	-0.046156	3.942532
230.737402	5336.790407	7.794342	-0.046216	3.945452
231.112894	5344.845576	7.799347	-0.046291	3.948392
231.188552	5352.899187	7.804352	-0.046311	3.951325
231.403156	5360.940530	7.809357	-0.046356	3.954253
231.760987	5368.906704	7.814362	-0.046428	3.957155
232.156647	5376.918243	7.819366	-0.046507	3.960072
232.305966	5384.899294	7.824371	-0.046540	3.962970
232.398096	5392.984756	7.829376	-0.046562	3.965904
232.821866	5400.996641	7.834381	-0.046646	3.968814
232.890524	5409.006515	7.839386	-0.046664	3.971716
233.191584	5417.062475	7.844390	-0.046725	3.974636
233.323871	5425.059457	7.849395	-0.046755	3.977529
233.883598	5433.052392	7.854400	-0.046864	3.980427
233.953822	5441.079008	7.859405	-0.046883	3.983325
234.266114	5449.091819	7.864410	-0.046946	3.986221
234.478690	5457.136273	7.869414	-0.046991	3.989125
234.894082	5465.168995	7.874419	-0.047073	3.992026
235.131768	5473.165177	7.879424	-0.047123	3.994908
235.316581	5481.177614	7.884429	-0.047162	3.997793
235.597783	5489.180854	7.889434	-0.047220	4.000674
235.864070	5497.171574	7.894438	-0.047275	4.003549
236.101498	5505.271352	7.899443	-0.047324	4.006460
236.356050	5513.231752	7.904448	-0.047377	4.009319
236.613249	5521.296301	7.909453	-0.047430	4.012213
236.793127	5529.304157	7.914458	-0.047469	4.015084
237.260834	5537.307792	7.919462	-0.047561	4.017956
237.454981	5545.370338	7.924467	-0.047602	4.020842
237.584151	5553.329919	7.929472	-0.047631	4.023688
237.874407	5561.425917	7.934477	-0.047691	4.026584
238.060400	5569.385644	7.939482	-0.047731	4.029427
238.185210	5577.490534	7.944486	-0.047759	4.032319
238.301314	5585.537716	7.949491	-0.047786	4.035188
238.351705	5593.482280	7.954496	-0.047800	4.038018
238.632169	5601.486946	7.959501	-0.047858	4.040870
238.836178	5609.434094	7.964506	-0.047901	4.043699
239.428322	5617.521487	7.969510	-0.048016	4.046582
239.558186	5625.522163	7.974515	-0.048046	4.049425
239.729736	5633.566273	7.979520	-0.048083	4.052281
240.061566	5641.595799	7.984525	-0.048150	4.055133
240.248963	5649.611073	7.989530	-0.048190	4.057976
240.400587	5657.667151	7.994534	-0.048223	4.060830
240.570686	5665.601920	7.999539	-0.048260	4.063640
240.737363	5673.653717	8.004544	-0.048296	4.066489
241.152866	5681.699533	8.009549	-0.048379	4.069338
241.401796	5689.701764	8.014554	-0.048431	4.072167
241.708067	5697.728446	8.019558	-0.048493	4.075003
242.084038	5705.736605	8.024563	-0.048568	4.077832
242.014958	5713.795203	8.029568	-0.048560	4.080670
242.437655	5721.769289	8.034573	-0.048644	4.083483
242.626359	5729.807785	8.039578	-0.048685	4.086314
242.888810	5737.839064	8.044582	-0.048739	4.089141
243.043770	5745.900083	8.049587	-0.048773	4.091976
243.381923	5753.889729	8.054592	-0.048841	4.094785
243.519306	5761.912934	8.059597	-0.048872	4.097602
243.572615	5769.906893	8.064602	-0.048887	4.100405
243.887142	5777.925024	8.069606	-0.048950	4.103219
244.236476	5785.968781	8.074611	-0.049021	4.106040
244.335872	5793.939139	8.079616	-0.049044	4.108830
244.601848	5802.026123	8.084621	-0.049099	4.111661
244.917591	5809.988959	8.089626	-0.049163	4.114447
245.204736	5818.030938	8.094630	-0.049222	4.117259
245.402778	5826.065990	8.099635	-0.049264	4.120065
245.790140	5833.970984	8.104640	-0.049341	4.122826
245.839897	5842.074084	8.109645	-0.049356	4.125650
246.086858	5850.047623	8.114650	-0.049407	4.128430
246.506377	5858.143754	8.119654	-0.049490	4.131252
246.621838	5866.120031	8.124659	-0.049517	4.134027
246.775689	5874.146073	8.129664	-0.049551	4.136818
247.106917	5882.168061	8.134669	-0.049618	4.139608
247.368576	5890.171275	8.139674	-0.049671	4.142388
247.578169	5898.162157	8.144678	-0.049716	4.145162
247.737295	5906.230705	8.149683	-0.049750	4.147960
248.036904	5914.244444	8.154688	-0.049811	4.150739
248.344237	5922.237222	8.159693	-0.049874	4.153508
248.491805	5930.292025	8.164698	-0.049907	4.156296
248.804882	5938.237693	8.169702	-0.049970	4.159046
249.097476	5946.309792	8.174707	-0.050030	4.161837
249.152668	5954.274924	8.179712	-0.050045	4.164586
249.763251	5962.363541	8.184717	-0.050164	4.167384
249.954873	5970.361671	8.189722	-0.050205	4.170143
250.177155	5978.387648	8.194726	-0.050251	4.172910
250.310907	5986.414985	8.199731	-0.050282	4.175674
250.559123	5994.381856	8.204736	-0.050333	4.178418
250.729941	6002.500391	8.209741	-0.050370	4.181210
250.764574	6010.411056	8.214746	-0.050382	4.183928
251.001168	6018.517184	8.219750	-0.050431	4.186713
251.306990	6026.529883	8.224755	-0.050493	4.189466
251.575545	6034.561129	8.229760	-0.050548	4.192222
251.938319	6042.627329	8.234765	-0.050621	4.194990
252.073272	6050.573689	8.239770	-0.050651	4.197712
252.127078	6058.612945	8.244774	-0.050667	4.200463
252.470833	6066.573623	8.249779	-0.050736	4.203189
252.647170	6074.590083	8.254784	-0.050774	4.205930
252.786182	6082.664329	8.259789	-0.050805	4.208689
252.768014	6090.697956	8.264794	-0.050807	4.211430
252.999899	6098.659795	8.269798	-0.050855	4.214147
253.364108	6106.704967	8.274803	-0.050928	4.216893
253.603947	6114.707368	8.279808	-0.050978	4.219621
254.069818	6122.748944	8.284813	-0.051070	4.222363
254.076168	6130.753976	8.289818	-0.051076	4.225086
254.323468	6138.787624	8.294822	-0.051127	4.227819
254.568462	6146.806427	8.299827	-0.051178	4.230546
254.719943	6154.798540	8.304832	-0.051212	4.233260
254.913551	6162.858036	8.309837	-0.051253	4.235996
255.203287	6170.825830	8.314842	-0.051312	4.238701
255.315625	6178.893822	8.319846	-0.051338	4.241435
255.640994	6186.875567	8.324851	-0.051404	4.244141
255.525669	6194.890975	8.329856	-0.051388	4.246852
255.823649	6202.920900	8.334861	-0.051448	4.249570
256.000889	6210.933913	8.339866	-0.051486	4.252280
256.347187	6218.969172	8.344870	-0.051556	4.254997
256.569030	6226.985715	8.349875	-0.051603	4.257705
256.639160	6234.994419	8.354880	-0.051621	4.260406
257.092179	6242.972733	8.359885	-0.051710	4.263100
257.202745	6251.030407	8.364890	-0.051736	4.265815
257.394580	6259.042631	8.369894	-0.051777	4.268514
257.658827	6267.107097	8.374899	-0.051832	4.271230
257.741939	6275.074315	8.379904	-0.051852	4.273909
257.884691	6283.105272	8.384909	-0.051884	4.276609
257.930740	6291.092983	8.389914	-0.051898	4.279291
258.332917	6299.121201	8.394918	-0.051978	4.281989
258.606602	6307.094026	8.399923	-0.052034	4.284665
258.725994	6315.160155	8.404928	-0.052061	4.287369
259.143224	6323.146667	8.409933	-0.052144	4.290048
259.341601	6331.191059	8.414938	-0.052186	4.292742
259.295161	6339.233317	8.419942	-0.052183	4.295432
259.947159	6347.211095	8.424947	-0.052310	4.298105
260.167251	6355.256295	8.429952	-0.052356	4.300794
260.410294	6363.256433	8.434957	-0.052406	4.303467
260.410863	6371.303694	8.439962	-0.052411	4.306152
260.676327	6379.289957	8.444966	-0.052466	4.308817
260.990022	6387.373731	8.449971	-0.052530	4.311514
260.968891	6395.288578	8.454976	-0.052531	4.314149
261.173922	6403.377873	8.459981	-0.052574	4.316843
261.409182	6411.303462	8.464986	-0.052623	4.319482
261.514016	6419.366985	8.469990	-0.052648	4.322163
261.732112	6427.376287	8.474995	-0.052694	4.324825
261.928741	6435.380812	8.480000	-0.052736	4.327484
262.290653	6443.386223	8.485005	-0.052808	4.330143
262.178348	6451.451775	8.490010	-0.052792	4.332817
262.691442	6459.437169	8.495014	-0.052893	4.335467
262.946040	6467.451879	8.500019	-0.052946	4.338123
263.044968	6475.481037	8.505024	-0.052969	4.340781
263.371976	6483.481369	8.510029	-0.053035	4.343430
263.713877	6491.485425	8.515034	-0.053104	4.346078
263.702835	6499.534030	8.520038	-0.053107	4.348737
263.834584	6507.640035	8.525043	-0.053137	4.351414
264.179720	6515.588073	8.530048	-0.053207	4.354039
264.342704	6523.676891	8.535053	-0.053242	4.356707
264.603958	6531.563798	8.540058	-0.053296	4.359308
264.973861	6539.591518	8.545062	-0.053370	4.361955
265.065982	6547.582104	8.550067	-0.053392	4.364585
265.219360	6555.608475	8.555072	-0.053426	4.367227
265.409952	6563.698806	8.560077	-0.053467	4.369888
265.595364	6571.645022	8.565082	-0.053507	4.372499
265.938329	6579.674462	8.570087	-0.053576	4.375138
266.179682	6587.692992	8.575091	-0.053626	4.377771
266.277629	6595.710928	8.580096	-0.053649	4.380401
266.436730	6603.771511	8.585101	-0.053684	4.383044
266.660009	6611.759415	8.590106	-0.053731	4.385661
267.049460	6619.778331	8.595111	-0.053808	4.388289
267.316949	6627.852445	8.600115	-0.053863	4.390932
267.236942	6635.822045	8.605120	-0.053854	4.393537
267.603099	6643.902090	8.610125	-0.053927	4.396179
268.032001	6651.809932	8.615130	-0.054012	4.398764
268.242182	6659.864708	8.620135	-0.054057	4.401394
268.352639	6667.848778	8.625139	-0.054082	4.403999
268.884573	6675.870694	8.630144	-0.054186	4.406617
269.073389	6683.944418	8.635149	-0.054227	4.409248
268.986534	6691.954396	8.640154	-0.054216	4.411856
269.211648	6699.971888	8.645159	-0.054263	4.414466
269.500033	6708.048754	8.650163	-0.054322	4.417094
269.726669	6716.005798	8.655168	-0.054369	4.419681
270.080991	6724.069135	8.660173	-0.054440	4.422302
270.286418	6732.090044	8.665178	-0.054484	4.424907
270.435419	6740.132172	8.670183	-0.054517	4.427516
270.738780	6748.136912	8.675187	-0.054579	4.430113
271.142357	6756.191969	8.680192	-0.054659	4.432725
271.319407	6764.206644	8.685197	-0.054697	4.435322
271.569619	6772.171780	8.690202	-0.054749	4.437901
271.634231	6780.267390	8.695207	-0.054766	4.440519
272.087586	6788.247375	8.700211	-0.054856	4.443101
272.172695	6796.235313	8.705216	-0.054877	4.445682
272.351790	6804.301862	8.710221	-0.054915	4.448288
272.583482	6812.311406	8.715226	-0.054964	4.450873
272.908841	6820.296146	8.720231	-0.055029	4.453450
273.097459	6828.381768	8.725235	-0.055070	4.456057
273.158630	6836.345219	8.730240	-0.055086	4.458622
273.579865	6844.399980	8.735245	-0.055170	4.461217
273.634299	6852.349595	8.740250	-0.055185	4.463775
274.037578	6860.437524	8.745255	-0.055265	4.466377
274.297057	6868.419709	8.750259	-0.055319	4.468944
274.325287	6876.445901	8.755264	-0.055329	4.471521
274.745991	6884.420573	8.760269	-0.055413	4.474083
274.837695	6892.507794	8.765274	-0.055435	4.476678
275.052319	6900.446096	8.770279	-0.055480	4.479224
275.205105	6908.537020	8.775283	-0.055514	4.481817
275.428764	6916.468887	8.780288	-0.055561	4.484358
275.749819	6924.545545	8.785293	-0.055626	4.486944
275.872416	6932.533906	8.790298	-0.055654	4.489500
275.875754	6940.545991	8.795303	-0.055660	4.492061
275.998201	6948.592429	8.800307	-0.055688	4.494632
276.112746	6956.598641	8.805312	-0.055714	4.497189
276.555043	6964.601529	8.810317	-0.055802	4.499745
276.577653	6972.624006	8.815322	-0.055811	4.502304
276.752400	6980.608109	8.820327	-0.055849	4.504850
277.083166	6988.687128	8.825331	-0.055916	4.507425
277.147753	6996.632723	8.830336	-0.055933	4.509955
277.350222	7004.660748	8.835341	-0.055976	4.512510
277.637489	7012.645338	8.840346	-0.056034	4.515050
277.827821	7020.660164	8.845351	-0.056075	4.517599
278.192815	7028.735730	8.850355	-0.056148	4.520165
278.412895	7036.657230	8.855360	-0.056194	4.522681
278.598045	7044.752874	8.860365	-0.056234	4.525250
278.737536	7052.765034	8.865370	-0.056265	4.527792
279.199849	7060.752939	8.870375	-0.056356	4.530325
279.371998	7068.768043	8.875379	-0.056394	4.532864
279.477704	7076.807093	8.880384	-0.056419	4.535410
279.889748	7084.808370	8.885389	-0.056500	4.537942
280.020629	7092.832658	8.890394	-0.056530	4.540480
280.120843	7100.853864	8.895399	-0.056554	4.543016
280.404518	7108.891834	8.900403	-0.056612	4.545555
280.487282	7116.898547	8.905408	-0.056632	4.548083
280.557330	7124.960340	8.910413	-0.056651	4.550627
280.986328	7132.915803	8.915418	-0.056736	4.553137
281.174644	7140.945130	8.920423	-0.056776	4.555668
281.359344	7148.922520	8.925427	-0.056816	4.558181
281.471287	7156.938672	8.930432	-0.056842	4.560705
281.867343	7164.964166	8.935437	-0.056921	4.563231
282.007711	7172.965322	8.940442	-0.056952	4.565747
282.298832	7180.949034	8.945447	-0.057011	4.568257
282.384662	7189.038075	8.950451	-0.057033	4.570798
282.633360	7197.024144	8.955456	-0.057084	4.573306
282.988318	7205.062790	8.960461	-0.057155	4.575829
283.040566	7213.053128	8.965466	-0.057170	4.578334
283.148793	7221.105327	8.970471	-0.057196	4.580858
283.381801	7229.120415	8.975475	-0.057244	4.583369
283.565203	7237.139279	8.980480	-0.057283	4.585880
284.015047	7245.119250	8.985485	-0.057372	4.588377
283.989744	7253.178143	8.990490	-0.057373	4.590898
284.239707	7261.132163	8.995495	-0.057425	4.593384
284.556904	7269.188245	9.000499	-0.057489	4.595901
284.723877	7277.125539	9.005504	-0.057525	4.598379
284.983907	7285.234912	9.010509	-0.057579	4.600910
284.988219	7293.155681	9.015514	-0.057585	4.603380
285.318714	7301.237692	9.020519	-0.057651	4.605899
285.476231	7309.226692	9.025523	-0.057686	4.608388
285.753071	7317.293865	9.030528	-0.057743	4.610900
286.038711	7325.264162	9.035533	-0.057801	4.613381
286.284495	7333.319328	9.040538	-0.057852	4.615886
286.366039	7341.293080	9.045543	-0.057872	4.618365
286.705086	7349.378974	9.050547	-0.057941	4.620877
286.795433	7357.285017	9.055552	-0.057963	4.623332
287.113915	7365.423168	9.060557	-0.058027	4.625857
287.073842	7373.390524	9.065562	-0.058025	4.628328
287.490917	7381.406497	9.070567	-0.058108	4.630814
287.639770	7389.386135	9.075571	-0.058141	4.633286
287.608439	7397.453108	9.080576	-0.058140	4.635784
287.934004	7405.423986	9.085581	-0.058206	4.638251
288.272468	7413.451724	9.090586	-0.058274	4.640734
288.436724	7421.409349	9.095591	-0.058310	4.643194
288.735878	7429.515668	9.100595	-0.058371	4.645699
288.836245	7437.508320	9.105600	-0.058395	4.648167
288.803204	7445.592354	9.110605	-0.058394	4.650662
288.984393	7453.524749	9.115610	-0.058433	4.653109
289.220640	7461.595087	9.120615	-0.058482	4.655598
289.564681	7469.571545	9.125619	-0.058551	4.658056
289.652555	7477.570551	9.130624	-0.058573	4.660519
289.767915	7485.613407	9.135629	-0.058599	4.662995
290.096840	7493.612001	9.140634	-0.058666	4.665456
290.343368	7501.611839	9.145639	-0.058717	4.667915
290.529898	7509.695198	9.150643	-0.058757	4.670400
290.850680	7517.692620	9.155648	-0.058822	4.672856
290.899674	7525.729604	9.160653	-0.058836	4.675323
291.016122	7533.700744	9.165658	-0.058863	4.677769
291.189118	7541.676208	9.170663	-0.058900	4.680215
291.441221	7549.699886	9.175667	-0.058952	4.682674
291.395957	7557.683407	9.180672	-0.058949	4.685120
291.844799	7565.732435	9.185677	-0.059038	4.687584
292.232455	7573.770419	9.190682	-0.059115	4.690044
292.246380	7581.789285	9.195687	-0.059123	4.692496
292.507946	7589.803899	9.200691	-0.059177	4.694946
292.560022	7597.843611	9.205696	-0.059192	4.697402
293.088341	7605.805300	9.210701	-0.059295	4.699833
293.175150	7613.869004	9.215706	-0.059317	4.702294
293.313911	7621.827634	9.220711	-0.059348	4.704722
293.651672	7629.906956	9.225715	-0.059416	4.707185
293.747516	7637.844132	9.230720	-0.059439	4.709604
293.818897	7645.937071	9.235725	-0.059457	4.712068
293.933440	7653.928817	9.240730	-0.059484	4.714501
294.144274	7661.916986	9.245735	-0.059528	4.716931
294.148205	7669.939154	9.250739	-0.059534	4.719371
294.488856	7677.971312	9.255744	-0.059603	4.721812
294.821353	7685.922399	9.260749	-0.059670	4.724226
295.012216	7694.047647	9.265754	-0.059711	4.726693
295.399791	7701.988994	9.270759	-0.059788	4.729102
295.524714	7710.098765	9.275763	-0.059817	4.731562
295.456223	7718.041665	9.280768	-0.059809	4.733970
295.820608	7726.089220	9.285773	-0.059882	4.736408
296.141150	7734.072726	9.290778	-0.059947	4.738825
296.177258	7742.123542	9.295783	-0.059959	4.741261
296.281054	7750.094341	9.300787	-0.059983	4.743672
296.504716	7758.182663	9.305792	-0.060030	4.746118
296.817285	7766.191163	9.310797	-0.060094	4.748537
296.781676	7774.252976	9.315802	-0.060092	4.750972
297.102199	7782.174756	9.320807	-0.060157	4.753363
297.497076	7790.237849	9.325811	-0.060236	4.755795
297.316975	7798.189816	9.330816	-0.060207	4.758194
297.727820	7806.279058	9.335821	-0.060289	4.760631
297.869440	7814.199319	9.340826	-0.060321	4.763017
298.011523	7822.204505	9.345831	-0.060352	4.765427
298.285737	7830.303166	9.350835	-0.060409	4.767864
298.345237	7838.339787	9.355840	-0.060425	4.770281
298.631728	7846.381565	9.360845	-0.060483	4.772698
298.805893	7854.404660	9.365850	-0.060521	4.775109
299.012023	7862.389563	9.370855	-0.060565	4.777507
299.201773	7870.421053	9.375859	-0.060605	4.779917
299.318916	7878.388303	9.380864	-0.060632	4.782307
299.707170	7886.397755	9.385869	-0.060710	4.784708
299.913972	7894.482433	9.390874	-0.060753	4.787131
300.241134	7902.416212	9.395879	-0.060819	4.789507
300.298952	7910.536798	9.400883	-0.060835	4.791938
300.445024	7918.442345	9.405888	-0.060868	4.794304
300.933157	7926.538365	9.410893	-0.060964	4.796724
300.904075	7934.479260	9.415898	-0.060964	4.799098
301.082472	7942.550834	9.420903	-0.061002	4.801509
301.428086	7950.482133	9.425907	-0.061071	4.803877
301.526788	7958.553661	9.430912	-0.061095	4.806286
301.752513	7966.576404	9.435917	-0.061142	4.808679
302.005754	7974.619284	9.440922	-0.061195	4.811077
302.191908	7982.607821	9.445927	-0.061234	4.813458
302.256825	7990.107272	9.450931	-0.061251	4.815692
302.570941	7994.836938	9.455936	-0.061313	4.817099

302.722925	7997.273556	9.460941	-0.061343	4.817824
302.864992	7998.643873	9.465946	-0.061370	4.818231
302.858781	7999.062225	9.470951	-0.061369	4.818356
303.248435	8000.204125	9.475955	-0.061442	4.818694
303.401736	8000.213451	9.480960	-0.061471	4.818697
303.330897	8000.256581	9.485965	-0.061458	4.818710
303.613256	8000.264433	9.490970	-0.061510	4.818711
303.705006	8000.164934	9.495975	-0.061527	4.818681
303.757995	8000.293574	9.500979	-0.061537	4.818719
303.822435	8000.189525	9.505984	-0.061549	4.818688
304.028956	8000.180663	9.510989	-0.061588	4.818684
304.259340	8000.240284	9.515994	-0.061630	4.818701
304.170691	8000.229693	9.520999	-0.061614	4.818699
304.289784	8000.259553	9.526003	-0.061636	4.818707
304.385835	8000.188426	9.531008	-0.061654	4.818685
304.561208	8000.284045	9.536013	-0.061687	4.818713
304.433686	8000.286584	9.541018	-0.061663	4.818714
304.625166	8000.218792	9.546023	-0.061698	4.818694
304.677585	8000.263521	9.551027	-0.061708	4.818707
304.745331	8000.232932	9.556032	-0.061721	4.818697
304.905869	8000.285357	9.561037	-0.061751	4.818712
304.703075	8000.274333	9.566042	-0.061713	4.818710
304.762209	8000.226851	9.571047	-0.061724	4.818695
305.065410	8000.290566	9.576051	-0.061780	4.818713
304.940216	8000.294184	9.581056	-0.061757	4.818715
305.056959	8000.276816	9.586061	-0.061779	4.818709
305.178757	8000.297273	9.591066	-0.061801	4.818715
305.268902	8000.259633	9.596071	-0.061818	4.818703
305.382898	8000.300966	9.601075	-0.061839	4.818715
305.275528	8000.272300	9.606080	-0.061819	4.818707
305.219056	8000.267370	9.611085	-0.061809	4.818706
305.369020	8000.287144	9.616090	-0.061836	4.818711
305.440183	8000.253452	9.621095	-0.061850	4.818701
305.637784	8000.278040	9.626099	-0.061886	4.818707
305.558423	8000.263373	9.631104	-0.061872	4.818703
305.589630	8000.260629	9.636109	-0.061877	4.818702
305.787223	8000.265288	9.641114	-0.061914	4.818703
305.840635	8000.228219	9.646119	-0.061924	4.818692
305.877464	8000.303165	9.651123	-0.061931	4.818714
305.612882	8000.288192	9.656128	-0.061882	4.818710
305.870471	8000.307265	9.661133	-0.061930	4.818715
305.694493	8000.314419	9.666138	-0.061897	4.818718
305.775453	8000.280854	9.671143	-0.061912	4.818708
306.119455	8000.304196	9.676147	-0.061976	4.818713
306.004618	8000.268090	9.681152	-0.061954	4.818703
306.076006	8000.237548	9.686157	-0.061968	4.818694
306.020883	8000.303959	9.691162	-0.061957	4.818714
306.089639	8000.261845	9.696167	-0.061970	4.818701
306.092989	8000.298597	9.701171	-0.061971	4.818712
306.018019	8000.242031	9.706176	-0.061957	4.818695
306.181156	8000.255683	9.711181	-0.061987	4.818699
306.407949	8000.293238	9.716186	-0.062029	4.818709
306.222457	8000.234188	9.721191	-0.061995	4.818692
306.461450	8000.319101	9.726195	-0.062039	4.818716
306.572692	8000.249219	9.731200	-0.062060	4.818695
306.567639	8000.254395	9.736205	-0.062059	4.818697
306.260874	8000.315442	9.741210	-0.062002	4.818716
306.437303	8000.273676	9.746215	-0.062035	4.818703
306.344883	8000.337505	9.751219	-0.062017	4.818722
306.348705	8000.321819	9.756224	-0.062018	4.818718
306.669203	8000.264093	9.761229	-0.062078	4.818699
306.605383	8000.330391	9.766234	-0.062066	4.818719
306.483679	8000.302587	9.771239	-0.062043	4.818711
306.553781	8000.354890	9.776243	-0.062056	4.818727
306.628448	8000.285581	9.781248	-0.062070	4.818706
306.764296	8000.273707	9.786253	-0.062095	4.818702
306.728909	8000.307859	9.791258	-0.062089	4.818712
306.650683	8000.313134	9.796263	-0.062074	4.818714
306.937106	8000.357758	9.801267	-0.062127	4.818726
306.540747	8000.320094	9.806272	-0.062053	4.818716
306.716338	8000.270975	9.811277	-0.062086	4.818701
306.807542	8000.304673	9.816282	-0.062103	4.818711
306.870867	8000.204799	9.821287	-0.062115	4.818681
306.873238	8000.252027	9.826291	-0.062115	4.818695
306.927503	8000.323006	9.831296	-0.062125	4.818716
306.859785	8000.298000	9.836301	-0.062113	4.818709
307.061799	8000.274398	9.841306	-0.062150	4.818701
307.082493	8000.266273	9.846311	-0.062154	4.818698
307.020202	8000.314760	9.851315	-0.062142	4.818713
306.923155	8000.263151	9.856320	-0.062124	4.818698
306.909805	8000.273464	9.861325	-0.062122	4.818701
307.095897	8000.323079	9.866330	-0.062156	4.818715
307.139217	8000.257558	9.871335	-0.062164	4.818695
307.152306	8000.303877	9.876339	-0.062167	4.818709
307.183884	8000.254986	9.881344	-0.062173	4.818694
307.259695	8000.218208	9.886349	-0.062187	4.818683
307.259177	8000.267498	9.891354	-0.062187	4.818698
307.226065	8000.197838	9.896359	-0.062180	4.818677
307.408727	8000.336566	9.901363	-0.062214	4.818718
307.358519	8000.315982	9.906368	-0.062205	4.818712
307.306088	8000.332081	9.911373	-0.062195	4.818717
307.385104	8000.322616	9.916378	-0.062210	4.818714
307.283819	8000.299271	9.921383	-0.062191	4.818707
307.228262	8000.317428	9.926387	-0.062181	4.818713
307.325071	8000.269384	9.931392	-0.062199	4.818698
307.495581	8000.347118	9.936397	-0.062230	4.818721
307.625767	8000.328877	9.941402	-0.062255	4.818715
307.416135	8000.265315	9.946407	-0.062215	4.818697
307.445911	8000.356955	9.951411	-0.062221	4.818724
307.391805	8000.342614	9.956416	-0.062211	4.818720
307.331164	8000.331335	9.961421	-0.062200	4.818717
307.565892	8000.324941	9.966426	-0.062243	4.818714
307.463787	8000.243895	9.971431	-0.062224	4.818690
307.640210	8000.316461	9.976435	-0.062257	4.818711
307.747522	8000.306315	9.981440	-0.062277	4.818708
307.712560	8000.323690	9.986445	-0.062270	4.818713
307.660455	8000.351332	9.991450	-0.062261	4.818721
307.501595	8000.303114	9.996455	-0.062231	4.818708
307.722164	8000.330102	10.001459	-0.062272	4.818715
307.631043	8000.299546	10.006464	-0.062255	4.818706
307.518721	8000.315916	10.011469	-0.062234	4.818711
307.703726	8000.301534	10.016474	-0.062269	4.818706
307.693281	8000.208043	10.021479	-0.062266	4.818679
307.742443	8000.299935	10.026483	-0.062276	4.818706
307.386844	8000.323634	10.031488	-0.062209	4.818714
307.593937	8000.256044	10.036493	-0.062248	4.818693
307.605691	8000.362135	10.041498	-0.062250	4.818725
307.388839	8000.333093	10.046503	-0.062210	4.818717
307.533362	8000.365387	10.051507	-0.062237	4.818726
307.615874	8000.315059	10.056512	-0.062252	4.818711
307.692642	8000.319201	10.061517	-0.062266	4.818712
307.737371	8000.330269	10.066522	-0.062274	4.818715
307.784666	8000.266897	10.071527	-0.062283	4.818696
307.775911	8000.311884	10.076531	-0.062282	4.818709
307.623126	8000.294164	10.081536	-0.062253	4.818704
307.730378	8000.271429	10.086541	-0.062273	4.818697
307.798868	8000.335252	10.091546	-0.062286	4.818716
307.664418	8000.266372	10.096551	-0.062261	4.818696
307.822103	8000.295690	10.101555	-0.062290	4.818704
307.935948	8000.305558	10.106560	-0.062311	4.818707
307.844375	8000.344225	10.111565	-0.062294	4.818719
307.955893	8000.315253	10.116570	-0.062315	4.818709
307.801453	8000.269190	10.121575	-0.062286	4.818696
307.815449	8000.340696	10.126579	-0.062289	4.818718
307.812935	8000.316536	10.131584	-0.062288	4.818710
307.997007	8000.269625	10.136589	-0.062322	4.818696
307.826063	8000.335582	10.141594	-0.062291	4.818716
307.619228	8000.341284	10.146599	-0.062252	4.818719
307.759293	8000.314781	10.151603	-0.062278	4.818710
307.867168	8000.308837	10.156608	-0.062298	4.818708
307.898870	8000.336519	10.161613	-0.062304	4.818716
307.797168	8000.342538	10.166618	-0.062285	4.818718
308.082192	8000.285401	10.171623	-0.062338	4.818700
308.168248	8000.345257	10.176627	-0.062354	4.818718
307.918647	8000.331522	10.181632	-0.062307	4.818714
308.094725	8000.292899	10.186637	-0.062340	4.818702
308.260176	8000.326514	10.191642	-0.062371	4.818712
307.990034	8000.275800	10.196647	-0.062321	4.818698
308.108160	8000.335024	10.201651	-0.062343	4.818715
308.285158	8000.340468	10.206656	-0.062376	4.818716
308.093550	8000.329585	10.211661	-0.062340	4.818713
308.111869	8000.348701	10.216666	-0.062343	4.818719
308.366057	8000.269136	10.221671	-0.062390	4.818694
308.288905	8000.371976	10.226675	-0.062376	4.818725
308.164887	8000.324209	10.231680	-0.062353	4.818711
308.430188	8000.287794	10.236685	-0.062402	4.818699
308.319826	8000.283211	10.241690	-0.062382	4.818699
308.262229	8000.292950	10.246695	-0.062371	4.818702
308.297657	8000.341659	10.251699	-0.062378	4.818716
308.410230	8000.310602	10.256704	-0.062399	4.818706
308.238517	8000.296830	10.261709	-0.062366	4.818703
308.436447	8000.369679	10.266714	-0.062403	4.818724
308.367520	8000.293257	10.271719	-0.062390	4.818701
308.386056	8000.362726	10.276723	-0.062394	4.818722
308.314010	8000.331368	10.281728	-0.062380	4.818713
308.539045	8000.310164	10.286733	-0.062422	4.818706
308.729973	8000.332573	10.291738	-0.062458	4.818712
308.566720	8000.341988	10.296743	-0.062427	4.818715
308.485678	8000.328345	10.301747	-0.062412	4.818711
308.491560	8000.330517	10.306752	-0.062413	4.818712
308.447213	8000.244974	10.311757	-0.062405	4.818687
308.520363	8000.331935	10.316762	-0.062419	4.818712
308.571429	8000.351478	10.321767	-0.062428	4.818718
308.675448	8000.398981	10.326771	-0.062447	4.818732
308.476589	8000.349192	10.331776	-0.062410	4.818718
308.467756	8000.296627	10.336781	-0.062409	4.818702
308.716721	8000.361749	10.341786	-0.062455	4.818720
308.575538	8000.285436	10.346791	-0.062429	4.818698
308.680358	8000.373859	10.351795	-0.062448	4.818724
308.623670	8000.325917	10.356800	-0.062438	4.818710
308.702239	8000.294418	10.361805	-0.062452	4.818700
308.802498	8000.353411	10.366810	-0.062471	4.818718
308.697247	8000.340503	10.371815	-0.062451	4.818714
308.669322	8000.308669	10.376819	-0.062446	4.818705
308.707058	8000.341674	10.381824	-0.062453	4.818714
308.556782	8000.333425	10.386829	-0.062425	4.818713
308.869344	8000.312311	10.391834	-0.062483	4.818705
308.642532	8000.262158	10.396839	-0.062441	4.818691
308.549603	8000.321787	10.401843	-0.062423	4.818709
308.689842	8000.327803	10.406848	-0.062450	4.818710
308.555614	8000.322909	10.411853	-0.062425	4.818709
308.601982	8000.329803	10.416858	-0.062433	4.818711
308.688519	8000.244912	10.421863	-0.062449	4.818686
308.738359	8000.292760	10.426867	-0.062458	4.818700
308.620215	8000.333180	10.431872	-0.062436	4.818712
308.709247	8000.329090	10.436877	-0.062453	4.818711
308.698017	8000.369851	10.441882	-0.062451	4.818723
308.687232	8000.350827	10.446887	-0.062449	4.818717
308.706119	8000.350021	10.451891	-0.062452	4.818717
308.693094	8000.349850	10.456896	-0.062450	4.818717
308.734108	8000.269612	10.461901	-0.062457	4.818693
308.691252	8000.371849	10.466906	-0.062449	4.818723
308.624789	8000.324829	10.471911	-0.062437	4.818710
308.910637	8000.293927	10.476915	-0.062490	4.818699
308.812420	8000.314676	10.481920	-0.062472	4.818706
308.868811	8000.272400	10.486925	-0.062482	4.818693
308.972789	8000.316756	10.491930	-0.062502	4.818706
308.891960	8000.287381	10.496935	-0.062487	4.818698
308.872445	8000.330132	10.501939	-0.062483	4.818710
309.037373	8000.318637	10.506944	-0.062514	4.818706
309.253383	8000.293121	10.511949	-0.062554	4.818698
309.108807	8000.333198	10.516954	-0.062527	4.818710
308.786469	8000.344740	10.521959	-0.062467	4.818715
308.776508	8000.375027	10.526963	-0.062465	4.818724
308.665899	8000.335825	10.531968	-0.062444	4.818713
308.723803	8000.355457	10.536973	-0.062455	4.818719
309.008133	8000.353905	10.541978	-0.062508	4.818717
308.885628	8000.263150	10.546983	-0.062485	4.818690
308.881840	8000.318693	10.551987	-0.062484	4.818707
308.861910	8000.322627	10.556992	-0.062481	4.818708
309.086419	8000.279389	10.561997	-0.062522	4.818694
309.199174	8000.345888	10.567002	-0.062543	4.818714
309.081142	8000.324421	10.572007	-0.062521	4.818708
309.047449	8000.286218	10.577011	-0.062515	4.818697
308.869610	8000.278660	10.582016	-0.062482	4.818695
309.023759	8000.262829	10.587021	-0.062511	4.818690
309.109584	8000.336320	10.592026	-0.062527	4.818711
309.111750	8000.284947	10.597031	-0.062527	4.818696
308.969383	8000.352325	10.602035	-0.062500	4.818717
308.770193	8000.389594	10.607040	-0.062463	4.818728
308.854761	8000.350830	10.612045	-0.062479	4.818717
308.952202	8000.361535	10.617050	-0.062497	4.818719
308.662386	8000.363010	10.622055	-0.062443	4.818721
309.128377	8000.383751	10.627059	-0.062530	4.818725
308.993816	8000.331650	10.632064	-0.062505	4.818710
309.009414	8000.297235	10.637069	-0.062508	4.818700
309.032007	8000.367806	10.642074	-0.062512	4.818721
308.942470	8000.348807	10.647079	-0.062495	4.818716
309.079741	8000.387303	10.652083	-0.062521	4.818727
308.987204	8000.334699	10.657088	-0.062503	4.818711
309.155728	8000.328496	10.662093	-0.062535	4.818709
309.111314	8000.366727	10.667098	-0.062526	4.818720
309.191384	8000.280703	10.672103	-0.062541	4.818694
309.293859	8000.335529	10.677107	-0.062560	4.818710
309.210582	8000.309269	10.682112	-0.062545	4.818703
309.104345	8000.263830	10.687117	-0.062525	4.818690
309.278251	8000.374131	10.692122	-0.062557	4.818722
309.170661	8000.303499	10.697127	-0.062537	4.818701
309.273608	8000.373017	10.702131	-0.062556	4.818722
309.314434	8000.331587	10.707136	-0.062564	4.818709
309.179405	8000.330878	10.712141	-0.062539	4.818709
309.224906	8000.353496	10.717146	-0.062547	4.818716
309.084501	8000.324395	10.722151	-0.062521	4.818708
309.109673	8000.346748	10.727155	-0.062526	4.818714
309.059874	8000.336658	10.732160	-0.062516	4.818712
309.134344	8000.293567	10.737165	-0.062530	4.818699
309.296522	8000.341828	10.742170	-0.062560	4.818712
309.041729	8000.321730	10.747175	-0.062513	4.818707
309.218085	8000.293600	10.752179	-0.062546	4.818698
309.236824	8000.320065	10.757184	-0.062549	4.818706
309.241051	8000.308579	10.762189	-0.062550	4.818703
309.452497	8000.352236	10.767194	-0.062589	4.818715
309.467730	8000.332501	10.772199	-0.062592	4.818709
309.400592	8000.321136	10.777203	-0.062579	4.818706
309.367093	8000.332237	10.782208	-0.062573	4.818709
309.417059	8000.314003	10.787213	-0.062582	4.818704
309.451717	8000.373193	10.792218	-0.062589	4.818721
309.513088	8000.307904	10.797223	-0.062600	4.818701
309.544980	8000.378597	10.802227	-0.062606	4.818722
309.328486	8000.374731	10.807232	-0.062566	4.818722
309.236164	8000.395556	10.812237	-0.062549	4.818728
309.454057	8000.371114	10.817242	-0.062589	4.818720
309.372129	8000.296619	10.822247	-0.062574	4.818699
309.442387	8000.334244	10.827251	-0.062587	4.818709
309.656442	8000.335976	10.832256	-0.062627	4.818709
309.514848	8000.264901	10.837261	-0.062600	4.818689
309.413740	8000.355893	10.842266	-0.062581	4.818716
309.553449	8000.318895	10.847271	-0.062607	4.818704
309.570979	8000.286603	10.852275	-0.062611	4.818695
309.186292	8000.297334	10.857280	-0.062539	4.818699
309.311106	8000.256996	10.862285	-0.062562	4.818687
309.528938	8000.317518	10.867290	-0.062603	4.818704
309.392615	8000.282177	10.872295	-0.062577	4.818694
309.405943	8000.365216	10.877299	-0.062580	4.818719
309.591854	8000.346652	10.882304	-0.062614	4.818713
309.689238	8000.336377	10.887309	-0.062632	4.818709
309.677730	8000.366645	10.892314	-0.062630	4.818718
309.439863	8000.309004	10.897319	-0.062586	4.818702
309.590279	8000.326692	10.902323	-0.062614	4.818707
309.512937	8000.341418	10.907328	-0.062600	4.818711
309.523108	8000.285953	10.912333	-0.062601	4.818695
309.676406	8000.363470	10.917338	-0.062630	4.818717
309.528206	8000.338463	10.922343	-0.062602	4.818710
309.604986	8000.301696	10.927347	-0.062617	4.818699
309.567501	8000.358900	10.932352	-0.062610	4.818716
309.433068	8000.367639	10.937357	-0.062584	4.818719
309.749591	8000.360214	10.942362	-0.062643	4.818716
309.528392	8000.300691	10.947367	-0.062602	4.818699
309.778411	8000.341703	10.952371	-0.062649	4.818710
309.598498	8000.327822	10.957376	-0.062615	4.818707
309.589784	8000.323510	10.962381	-0.062613	4.818706
309.894445	8000.389360	10.967386	-0.062670	4.818724
309.612748	8000.316462	10.972391	-0.062618	4.818704
309.608331	8000.319549	10.977395	-0.062617	4.818704
309.737612	8000.312836	10.982400	-0.062641	4.818702
309.631536	8000.266349	10.987405	-0.062621	4.818689
309.772756	8000.329023	10.992410	-0.062647	4.818707
309.740227	8000.302373	10.997415	-0.062641	4.818699
309.789726	8000.283084	11.002419	-0.062650	4.818693
309.737614	8000.320167	11.007424	-0.062641	4.818704
309.637157	8000.262214	11.012429	-0.062622	4.818687
309.874324	8000.292569	11.017434	-0.062666	4.818695
309.727974	8000.285419	11.022439	-0.062639	4.818694
309.742896	8000.317080	11.027443	-0.062642	4.818703
309.759691	8000.322540	11.032448	-0.062645	4.818705
309.862514	8000.322826	11.037453	-0.062664	4.818704
309.941366	8000.330143	11.042458	-0.062678	4.818706
310.007170	8000.353025	11.047463	-0.062691	4.818713
309.945280	8000.294524	11.052467	-0.062679	4.818696
309.882238	8000.317829	11.057472	-0.062667	4.818703
309.809408	8000.248696	11.062477	-0.062654	4.818683
309.923518	8000.362418	11.067482	-0.062675	4.818716
310.034496	8000.315606	11.072487	-0.062696	4.818702
309.984618	8000.357963	11.077491	-0.062686	4.818714
310.009317	8000.365625	11.082496	-0.062691	4.818717
309.989109	8000.351723	11.087501	-0.062687	4.818713
309.955017	8000.382747	11.092506	-0.062681	4.818722
309.824175	8000.368455	11.097511	-0.062656	4.818718
309.860479	8000.368925	11.102515	-0.062663	4.818718
309.766662	8000.307911	11.107520	-0.062645	4.818700
309.801206	8000.242273	11.112525	-0.062652	4.818681
309.966758	8000.336733	11.117530	-0.062683	4.818708
309.921884	8000.319363	11.122535	-0.062674	4.818703
309.944288	8000.309162	11.127539	-0.062678	4.818700
310.070929	8000.330738	11.132544	-0.062702	4.818706
310.060874	8000.267666	11.137549	-0.062700	4.818687
309.940129	8000.347913	11.142554	-0.062678	4.818712
309.745363	8000.296077	11.147559	-0.062641	4.818697
310.056106	8000.315850	11.152563	-0.062699	4.818702
310.155928	8000.334979	11.157568	-0.062718	4.818707
309.936999	8000.300660	11.162573	-0.062677	4.818698
309.969195	8000.314713	11.167578	-0.062683	4.818702
310.036653	8000.291461	11.172583	-0.062695	4.818694
309.932994	8000.295356	11.177587	-0.062676	4.818696
309.930491	8000.327839	11.182592	-0.062675	4.818706
310.024890	8000.227314	11.187597	-0.062693	4.818675
310.030083	8000.329130	11.192602	-0.062694	4.818706
309.786339	8000.266166	11.197607	-0.062648	4.818688
310.115757	8000.287231	11.202611	-0.062710	4.818693
309.979573	8000.316927	11.207616	-0.062684	4.818702
309.923823	8000.240674	11.212621	-0.062674	4.818680
310.185610	8000.355268	11.217626	-0.062723	4.818713
310.126438	8000.313585	11.222631	-0.062712	4.818701
310.166373	8000.384384	11.227635	-0.062719	4.818722
310.094062	8000.354070	11.232640	-0.062706	4.818713
310.185286	8000.352107	11.237645	-0.062723	4.818712
310.160358	8000.376956	11.242650	-0.062718	4.818719
309.753574	8000.353830	11.247655	-0.062642	4.818714
310.091453	8000.307871	11.252659	-0.062705	4.818699
310.113044	8000.342766	11.257664	-0.062709	4.818709
310.078579	8000.345463	11.262669	-0.062702	4.818710
310.076803	8000.402082	11.267674	-0.062702	4.818727
310.024273	8000.348948	11.272679	-0.062692	4.818712
310.032824	8000.404652	11.277683	-0.062694	4.818728
309.932508	8000.381317	11.282688	-0.062675	4.818722
309.929045	8000.373927	11.287693	-0.062675	4.818719
309.991575	8000.418795	11.292698	-0.062686	4.818733
309.841493	8000.340265	11.297703	-0.062658	4.818710
310.047134	8000.320909	11.302707	-0.062696	4.818703
309.970050	8000.381793	11.307712	-0.062682	4.818722
309.943897	8000.337394	11.312717	-0.062677	4.818709
309.870069	8000.403566	11.317722	-0.062663	4.818728
309.970537	8000.350323	11.322727	-0.062682	4.818712
309.902304	8000.352581	11.327731	-0.062669	4.818713
309.897028	8000.324187	11.332736	-0.062668	4.818705
310.120338	8000.323942	11.337741	-0.062710	4.818704
310.214230	8000.360827	11.342746	-0.062727	4.818714
309.945213	8000.347885	11.347751	-0.062677	4.818712
310.277260	8000.351152	11.352755	-0.062739	4.818711
310.214069	8000.365014	11.357760	-0.062727	4.818716
310.109963	8000.301767	11.362765	-0.062708	4.818697
310.137300	8000.341982	11.367770	-0.062713	4.818709
310.205032	8000.330273	11.372775	-0.062725	4.818705
310.163612	8000.321340	11.377779	-0.062718	4.818703
310.133858	8000.362910	11.382784	-0.062712	4.818715
310.132322	8000.313585	11.387789	-0.062712	4.818701
310.221848	8000.363001	11.392794	-0.062728	4.818715
310.134105	8000.317800	11.397799	-0.062712	4.818702
310.225439	8000.389267	11.402803	-0.062729	4.818723
310.412803	8000.322469	11.407808	-0.062764	4.818702
310.133272	8000.289460	11.412813	-0.062712	4.818694
310.203059	8000.267287	11.417818	-0.062725	4.818687
310.169703	8000.244823	11.422823	-0.062718	4.818680
310.356359	8000.290256	11.427827	-0.062753	4.818693
310.136388	8000.291589	11.432832	-0.062712	4.818694
310.079797	8000.335956	11.437837	-0.062702	4.818708
310.284755	8000.339669	11.442842	-0.062740	4.818708
310.209051	8000.342878	11.447847	-0.062726	4.818709
310.294239	8000.336641	11.452851	-0.062741	4.818707
310.259159	8000.335133	11.457856	-0.062735	4.818707
310.163012	8000.355909	11.462861	-0.062717	4.818713
310.317985	8000.396735	11.467866	-0.062746	4.818725
310.201181	8000.331225	11.472871	-0.062724	4.818706
310.330700	8000.353887	11.477875	-0.062748	4.818712
310.303293	8000.353528	11.482880	-0.062743	4.818712
310.377623	8000.350297	11.487885	-0.062757	4.818711
310.456953	8000.378601	11.492890	-0.062771	4.818719
310.111542	8000.373056	11.497895	-0.062707	4.818719
310.237776	8000.361059	11.502899	-0.062731	4.818714
310.398184	8000.361045	11.507904	-0.062760	4.818714
310.252363	8000.322432	11.512909	-0.062733	4.818703
310.294569	8000.380672	11.517914	-0.062741	4.818720
310.230999	8000.330541	11.522919	-0.062729	4.818705
310.322041	8000.343262	11.527923	-0.062746	4.818709
310.181149	8000.356112	11.532928	-0.062720	4.818713
310.241915	8000.328578	11.537933	-0.062731	4.818705
310.329937	8000.395807	11.542938	-0.062747	4.818724
310.261754	8000.316244	11.547943	-0.062735	4.818701
310.175403	8000.307775	11.552947	-0.062719	4.818699
310.366529	8000.318651	11.557952	-0.062754	4.818701
310.408134	8000.286671	11.562957	-0.062762	4.818692
310.324289	8000.377889	11.567962	-0.062746	4.818719
310.252725	8000.328702	11.572967	-0.062733	4.818705
310.477493	8000.293860	11.577971	-0.062775	4.818694
310.329105	8000.367455	11.582976	-0.062747	4.818716
310.176922	8000.327709	11.587981	-0.062719	4.818705
310.272358	8000.402377	11.592986	-0.062736	4.818727
310.241347	8000.353718	11.597991	-0.062731	4.818712
310.241828	8000.342183	11.602995	-0.062731	4.818709
310.347796	8000.364539	11.608000	-0.062750	4.818715
310.493172	8000.347546	11.613005	-0.062777	4.818709
310.489126	8000.364275	11.618010	-0.062777	4.818714
310.325445	8000.361095	11.623015	-0.062746	4.818714
310.417770	8000.306697	11.628019	-0.062763	4.818698
310.229462	8000.333617	11.633024	-0.062728	4.818706
310.135368	8000.276795	11.638029	-0.062711	4.818690
310.444454	8000.260882	11.643034	-0.062768	4.818684
310.560238	8000.278120	11.648039	-0.062790	4.818689
310.453547	8000.339669	11.653043	-0.062770	4.818707
310.467723	8000.345096	11.658048	-0.062772	4.818709
310.452012	8000.303979	11.663053	-0.062769	4.818697
310.481455	8000.348417	11.668058	-0.062775	4.818710
310.269087	8000.318379	11.673063	-0.062735	4.818702
310.467543	8000.315713	11.678067	-0.062772	4.818700
310.423837	8000.361298	11.683072	-0.062764	4.818714
310.495877	8000.353841	11.688077	-0.062777	4.818711
310.674080	8000.359304	11.693082	-0.062811	4.818712
310.531359	8000.325975	11.698087	-0.062784	4.818703
310.367905	8000.362659	11.703091	-0.062753	4.818714
310.556984	8000.374557	11.708096	-0.062789	4.818717
310.472092	8000.308413	11.713101	-0.062773	4.818698
310.366775	8000.366833	11.718106	-0.062753	4.818716
310.543427	8000.351296	11.723111	-0.062786	4.818710
310.729253	8000.356859	11.728115	-0.062821	4.818711
310.517768	8000.374036	11.733120	-0.062781	4.818717
310.359109	8000.320569	11.738125	-0.062752	4.818702
310.382525	8000.328214	11.743130	-0.062756	4.818704
310.541954	8000.300914	11.748135	-0.062786	4.818695
310.599330	8000.336275	11.753139	-0.062796	4.818706
310.494814	8000.345403	11.758144	-0.062777	4.818709
310.560870	8000.341015	11.763149	-0.062789	4.818707
310.448116	8000.331154	11.768154	-0.062768	4.818705
310.408996	8000.346377	11.773159	-0.062761	4.818709
310.670262	8000.340333	11.778163	-0.062809	4.818707
310.566845	8000.334789	11.783168	-0.062790	4.818705
310.352657	8000.293188	11.788173	-0.062750	4.818694
310.615676	8000.302901	11.793178	-0.062799	4.818696
310.552671	8000.308373	11.798183	-0.062787	4.818698
310.757651	8000.372928	11.803187	-0.062825	4.818716
310.672555	8000.387554	11.808192	-0.062810	4.818721
310.575229	8000.348521	11.813197	-0.062791	4.818709
310.669872	8000.380171	11.818202	-0.062809	4.818719
310.574254	8000.362141	11.823207	-0.062791	4.818714
310.553736	8000.347186	11.828211	-0.062787	4.818709
310.634958	8000.373416	11.833216	-0.062802	4.818717
310.511607	8000.329849	11.838221	-0.062779	4.818704
310.546659	8000.358625	11.843226	-0.062786	4.818713
310.662103	8000.323410	11.848231	-0.062807	4.818702
310.588671	8000.328747	11.853235	-0.062794	4.818704
310.497148	8000.375807	11.858240	-0.062777	4.818718
310.509277	8000.344493	11.863245	-0.062779	4.818709
310.612935	8000.353182	11.868250	-0.062798	4.818711
310.414482	8000.336961	11.873255	-0.062761	4.818707
310.483634	8000.346250	11.878259	-0.062774	4.818709
310.547835	8000.355475	11.883264	-0.062786	4.818712
310.626416	8000.328172	11.888269	-0.062800	4.818703
310.635041	8000.339821	11.893274	-0.062802	4.818707
310.523807	8000.337323	11.898279	-0.062781	4.818706
310.610440	8000.284949	11.903283	-0.062797	4.818690
310.728198	8000.344173	11.908288	-0.062819	4.818708
310.559550	8000.323095	11.913293	-0.062788	4.818702
310.606160	8000.373002	11.918298	-0.062796	4.818717
310.446516	8000.346796	11.923303	-0.062767	4.818709
310.606794	8000.323703	11.928307	-0.062796	4.818702
310.786833	8000.358562	11.933312	-0.062830	4.818712
310.636671	8000.325136	11.938317	-0.062802	4.818702
310.734142	8000.327450	11.943322	-0.062820	4.818703
310.666990	8000.320281	11.948327	-0.062807	4.818701
310.574230	8000.286553	11.953331	-0.062790	4.818691
310.609133	8000.373022	11.958336	-0.062797	4.818717
310.764993	8000.324696	11.963341	-0.062826	4.818702
310.790647	8000.336566	11.968346	-0.062830	4.818705
310.662819	8000.329656	11.973351	-0.062807	4.818704
310.582744	8000.279309	11.978355	-0.062792	4.818689
310.802387	8000.331467	11.983360	-0.062832	4.818704
310.511667	8000.314045	11.988365	-0.062778	4.818699
310.670881	8000.310869	11.993370	-0.062808	4.818698
310.792304	8000.318741	11.998375	-0.062830	4.818700
310.792762	8000.306156	12.003379	-0.062831	4.818696
310.858758	8000.348973	12.008384	-0.062843	4.818709
310.735376	8000.306454	12.013389	-0.062820	4.818696
310.775882	8000.341596	12.018394	-0.062827	4.818707
310.811875	8000.333670	12.023399	-0.062834	4.818704
310.805907	8000.375550	12.028403	-0.062833	4.818717
310.890755	8000.383994	12.033408	-0.062849	4.818719
310.656854	8000.315911	12.038413	-0.062805	4.818699
310.767903	8000.323647	12.043418	-0.062826	4.818701
310.751242	8000.306644	12.048423	-0.062823	4.818696
310.909087	8000.312892	12.053427	-0.062852	4.818698
310.935164	8000.331062	12.058432	-0.062857	4.818703
310.748544	8000.249957	12.063437	-0.062822	4.818679
310.929979	8000.349872	12.068442	-0.062856	4.818709
310.591044	8000.358047	12.073447	-0.062793	4.818712
310.654177	8000.350474	12.078451	-0.062804	4.818710
310.713173	8000.372220	12.083456	-0.062815	4.818716
310.774011	8000.286991	12.088461	-0.062826	4.818690
310.846075	8000.362405	12.093466	-0.062840	4.818713
310.779511	8000.359439	12.098471	-0.062827	4.818712
310.939587	8000.334245	12.103475	-0.062857	4.818704
310.814898	8000.380875	12.108480	-0.062834	4.818718
310.872518	8000.309241	12.113485	-0.062845	4.818697
311.038932	8000.359658	12.118490	-0.062876	4.818711
310.884437	8000.329322	12.123495	-0.062847	4.818703
310.704381	8000.311243	12.128499	-0.062813	4.818698
310.748263	8000.347477	12.133504	-0.062821	4.818709
310.697071	8000.278624	12.138509	-0.062812	4.818688
310.786862	8000.326995	12.143514	-0.062829	4.818702
310.917738	8000.328695	12.148519	-0.062853	4.818702
310.775215	8000.358308	12.153523	-0.062826	4.818712
310.635016	8000.390050	12.158528	-0.062800	4.818722
310.846963	8000.313081	12.163533	-0.062840	4.818698
310.929786	8000.368705	12.168538	-0.062855	4.818714
310.850425	8000.346690	12.173543	-0.062840	4.818708
310.783711	8000.303859	12.178547	-0.062828	4.818695
310.763447	8000.336112	12.183552	-0.062824	4.818705
310.901375	8000.306435	12.188557	-0.062850	4.818696
310.844096	8000.367578	12.193562	-0.062839	4.818714
310.822582	8000.345267	12.198567	-0.062835	4.818708
310.880778	8000.378541	12.203571	-0.062846	4.818717
310.960081	8000.354394	12.208576	-0.062860	4.818710
310.957188	8000.318688	12.213581	-0.062860	4.818699
311.011515	8000.364500	12.218586	-0.062870	4.818713
310.924411	8000.346580	12.223591	-0.062854	4.818708
310.961639	8000.292514	12.228595	-0.062860	4.818691
310.904638	8000.371494	12.233600	-0.062850	4.818715
310.861281	8000.310086	12.238605	-0.062842	4.818697
310.977794	8000.335727	12.243610	-0.062863	4.818704
310.780848	8000.353093	12.248615	-0.062827	4.818710
311.003214	8000.330808	12.253619	-0.062868	4.818703
310.942481	8000.338407	12.258624	-0.062857	4.818705
310.716613	8000.310290	12.263629	-0.062815	4.818698
311.038768	8000.340704	12.268634	-0.062875	4.818705
311.026860	8000.365723	12.273639	-0.062872	4.818713
310.839084	8000.352787	12.278643	-0.062837	4.818710
310.969634	8000.357631	12.283648	-0.062862	4.818711
311.027756	8000.337405	12.288653	-0.062872	4.818704
310.923318	8000.346534	12.293658	-0.062853	4.818708
310.856033	8000.317333	12.298663	-0.062840	4.818699
310.984277	8000.300117	12.303667	-0.062864	4.818694
311.187687	8000.386682	12.308672	-0.062902	4.818719
310.858028	8000.319450	12.313677	-0.062841	4.818700
310.996755	8000.368458	12.318682	-0.062866	4.818714
310.989239	8000.373602	12.323687	-0.062865	4.818715
310.961468	8000.357504	12.328691	-0.062860	4.818711
311.144671	8000.364082	12.333696	-0.062894	4.818712
311.030667	8000.366792	12.338701	-0.062873	4.818713
310.997726	8000.375802	12.343706	-0.062866	4.818716
310.943564	8000.332085	12.348711	-0.062856	4.818703
311.080412	8000.311835	12.353715	-0.062882	4.818697
311.153942	8000.365240	12.358720	-0.062895	4.818712
310.753315	8000.304427	12.363725	-0.062821	4.818696
311.070030	8000.316938	12.368730	-0.062880	4.818698
311.150443	8000.320080	12.373735	-0.062895	4.818699
310.962629	8000.295605	12.378739	-0.062860	4.818692
310.992659	8000.374668	12.383744	-0.062865	4.818716
311.052394	8000.260053	12.388749	-0.062876	4.818681
311.068854	8000.338940	12.393754	-0.062879	4.818705
310.858517	8000.357181	12.398759	-0.062840	4.818711
311.044014	8000.247349	12.403763	-0.062875	4.818678
311.222568	8000.354570	12.408768	-0.062908	4.818709
310.997282	8000.340097	12.413773	-0.062866	4.818705
311.001844	8000.360085	12.418778	-0.062867	4.818711
311.075449	8000.362090	12.423783	-0.062880	4.818712
310.968432	8000.344960	12.428787	-0.062860	4.818707
311.034103	8000.345812	12.433792	-0.062873	4.818707
311.156758	8000.263486	12.438797	-0.062895	4.818682
311.115844	8000.312254	12.443802	-0.062888	4.818697
311.139513	8000.307315	12.448807	-0.062892	4.818695
311.044847	8000.309228	12.453811	-0.062874	4.818696
311.142665	8000.302106	12.458816	-0.062893	4.818694
310.804769	8000.297707	12.463821	-0.062830	4.818694
310.984041	8000.334654	12.468826	-0.062863	4.818704
311.160075	8000.361070	12.473831	-0.062896	4.818711
311.033149	8000.313260	12.478835	-0.062872	4.818697
310.993365	8000.360994	12.483840	-0.062865	4.818712
311.097075	8000.309891	12.488845	-0.062884	4.818696
311.083160	8000.317051	12.493850	-0.062881	4.818698
311.105570	8000.290066	12.498855	-0.062885	4.818690
311.219044	8000.241188	12.503859	-0.062907	4.818675
311.208012	8000.322864	12.508864	-0.062905	4.818699
311.029041	8000.301651	12.513869	-0.062871	4.818694
311.052023	8000.313487	12.518874	-0.062875	4.818697
311.161578	8000.366311	12.523879	-0.062896	4.818713
311.157493	8000.244571	12.528883	-0.062895	4.818676
311.069683	8000.360915	12.533888	-0.062879	4.818711
310.971047	8000.329208	12.538893	-0.062860	4.818702
311.179299	8000.342406	12.543898	-0.062899	4.818705
311.064772	8000.345109	12.548903	-0.062878	4.818707
311.156113	8000.302237	12.553907	-0.062895	4.818694
311.251044	8000.326548	12.558912	-0.062912	4.818700
311.095521	8000.320326	12.563917	-0.062883	4.818699
311.050866	8000.382683	12.568922	-0.062875	4.818718
311.146248	8000.382873	12.573927	-0.062893	4.818718
311.067068	8000.324145	12.578931	-0.062878	4.818700
311.136838	8000.396383	12.583936	-0.062891	4.818722
311.155311	8000.304308	12.588941	-0.062894	4.818694
311.224194	8000.375486	12.593946	-0.062907	4.818715
311.046104	8000.364774	12.598951	-0.062874	4.818713
311.149412	8000.353528	12.603955	-0.062893	4.818709
311.324732	8000.396719	12.608960	-0.062926	4.818721
311.166654	8000.349552	12.613965	-0.062896	4.818708
311.197327	8000.371978	12.618970	-0.062902	4.818714
311.239793	8000.386165	12.623975	-0.062910	4.818718
311.166440	8000.391502	12.628979	-0.062896	4.818720
311.178599	8000.404246	12.633984	-0.062898	4.818724
311.286881	8000.349007	12.638989	-0.062918	4.818707
311.391077	8000.353507	12.643994	-0.062938	4.818708
311.344750	8000.324579	12.648999	-0.062929	4.818699
311.219758	8000.322950	12.654003	-0.062906	4.818699
311.311125	8000.325186	12.659008	-0.062923	4.818700
311.181707	8000.330842	12.664013	-0.062899	4.818702
311.351057	8000.358220	12.669018	-0.062930	4.818709
311.420793	8000.372763	12.674023	-0.062943	4.818714
311.464855	8000.312491	12.679027	-0.062951	4.818695
311.222228	8000.327164	12.684032	-0.062906	4.818701
311.189294	8000.274283	12.689037	-0.062900	4.818685
311.289830	8000.336431	12.694042	-0.062919	4.818703
311.225777	8000.349233	12.699047	-0.062907	4.818707
311.154055	8000.285357	12.704051	-0.062893	4.818689
311.230527	8000.389152	12.709056	-0.062907	4.818719
311.184044	8000.337143	12.714061	-0.062899	4.818704
311.156487	8000.379792	12.719066	-0.062894	4.818717
311.063608	8000.364944	12.724071	-0.062876	4.818713
311.230888	8000.272708	12.729075	-0.062907	4.818684
311.253929	8000.327553	12.734080	-0.062912	4.818701
311.320130	8000.311629	12.739085	-0.062924	4.818696
311.245900	8000.298072	12.744090	-0.062910	4.818692
311.227784	8000.337696	12.749095	-0.062907	4.818704
311.010084	8000.326469	12.754099	-0.062866	4.818701
311.157766	8000.414407	12.759104	-0.062894	4.818727
311.322588	8000.343119	12.764109	-0.062924	4.818705
311.036847	8000.392898	12.769114	-0.062871	4.818721
311.150869	8000.374448	12.774119	-0.062892	4.818715
311.087071	8000.374664	12.779123	-0.062880	4.818715
311.157603	8000.378727	12.784128	-0.062893	4.818716
311.107897	8000.349755	12.789133	-0.062884	4.818708
311.254873	8000.414606	12.794138	-0.062911	4.818727
311.316692	8000.393379	12.799143	-0.062923	4.818720
311.141437	8000.411027	12.804147	-0.062890	4.818726
311.262580	8000.379033	12.809152	-0.062913	4.818716
311.134942	8000.377369	12.814157	-0.062889	4.818716
311.241068	8000.354621	12.819162	-0.062909	4.818709
311.351212	8000.373885	12.824167	-0.062929	4.818714
311.329235	8000.371499	12.829171	-0.062925	4.818714
311.378442	8000.413049	12.834176	-0.062934	4.818726
311.076519	8000.362960	12.839181	-0.062878	4.818712
311.403871	8000.390297	12.844186	-0.062939	4.818719
311.458096	8000.360579	12.849191	-0.062949	4.818710
311.257323	8000.348522	12.854195	-0.062911	4.818707
311.408337	8000.412377	12.859200	-0.062940	4.818725
311.359572	8000.361387	12.864205	-0.062930	4.818710
311.269799	8000.387491	12.869210	-0.062914	4.818719
311.347522	8000.358079	12.874215	-0.062928	4.818709
311.207459	8000.343666	12.879219	-0.062902	4.818706
311.150800	8000.392229	12.884224	-0.062891	4.818720
311.071203	8000.370211	12.889229	-0.062877	4.818714
311.321481	8000.307378	12.894234	-0.062923	4.818694
311.410449	8000.358886	12.899239	-0.062940	4.818709
311.176085	8000.318070	12.904243	-0.062896	4.818698
311.400922	8000.360856	12.909248	-0.062938	4.818710
311.262245	8000.369539	12.914253	-0.062912	4.818713
311.263537	8000.343328	12.919258	-0.062912	4.818705
311.120712	8000.339369	12.924263	-0.062886	4.818705
311.292945	8000.381470	12.929267	-0.062918	4.818717
311.440342	8000.415906	12.934272	-0.062945	4.818726
311.366342	8000.374029	12.939277	-0.062931	4.818714
311.400805	8000.429024	12.944282	-0.062938	4.818730
311.351030	8000.389560	12.949287	-0.062928	4.818719
311.440064	8000.369736	12.954291	-0.062945	4.818713
311.406166	8000.404959	12.959296	-0.062938	4.818723
311.500016	8000.378904	12.964301	-0.062956	4.818715
311.403163	8000.369249	12.969306	-0.062938	4.818713
311.259539	8000.384162	12.974311	-0.062911	4.818718
311.515673	8000.302523	12.979315	-0.062959	4.818692
311.482295	8000.338802	12.984320	-0.062952	4.818703
311.439182	8000.349777	12.989325	-0.062944	4.818707
311.551184	8000.354380	12.994330	-0.062965	4.818708
311.523712	8000.380245	12.999335	-0.062960	4.818715
311.462626	8000.323850	13.004339	-0.062949	4.818699
311.364095	8000.351938	13.009344	-0.062930	4.818708
311.254670	8000.319041	13.014349	-0.062910	4.818698
311.464868	8000.337510	13.019354	-0.062949	4.818703
311.412621	8000.368298	13.024359	-0.062939	4.818712
311.343361	8000.304453	13.029363	-0.062926	4.818694
311.450725	8000.324730	13.034368	-0.062946	4.818699
311.270907	8000.276232	13.039373	-0.062913	4.818685
311.438987	8000.337161	13.044378	-0.062944	4.818703
311.424107	8000.365288	13.049383	-0.062941	4.818711
311.335096	8000.323216	13.054387	-0.062925	4.818699
311.221411	8000.384675	13.059392	-0.062903	4.818718
311.373264	8000.343640	13.064397	-0.062932	4.818705
311.376924	8000.306970	13.069402	-0.062932	4.818694
311.086041	8000.351436	13.074407	-0.062878	4.818709
311.138267	8000.316447	13.079411	-0.062888	4.818698
311.373624	8000.377203	13.084416	-0.062932	4.818715
311.403996	8000.366057	13.089421	-0.062937	4.818712
311.405046	8000.363971	13.094426	-0.062937	4.818711
311.338542	8000.366250	13.099431	-0.062925	4.818712
311.220948	8000.354227	13.104435	-0.062903	4.818709
311.444857	8000.407491	13.109440	-0.062945	4.818724
311.358535	8000.323493	13.114445	-0.062929	4.818699
311.410050	8000.356681	13.119450	-0.062938	4.818709
311.275421	8000.339191	13.124455	-0.062913	4.818704
311.389080	8000.259895	13.129459	-0.062934	4.818680
311.491381	8000.364027	13.134464	-0.062953	4.818711
311.411212	8000.348295	13.139469	-0.062938	4.818706
311.420252	8000.279175	13.144474	-0.062940	4.818686
311.540058	8000.344722	13.149479	-0.062962	4.818705
311.582978	8000.281288	13.154483	-0.062970	4.818686
311.443912	8000.348711	13.159488	-0.062944	4.818706
311.365361	8000.357127	13.164493	-0.062929	4.818709
311.387250	8000.359508	13.169498	-0.062934	4.818710
311.317860	8000.362799	13.174503	-0.062921	4.818711
311.357593	8000.326598	13.179507	-0.062928	4.818700
311.470749	8000.391009	13.184512	-0.062949	4.818719
311.352537	8000.368488	13.189517	-0.062927	4.818713
311.404870	8000.415323	13.194522	-0.062937	4.818726
311.438250	8000.390579	13.199527	-0.062943	4.818719
311.261688	8000.347367	13.204531	-0.062910	4.818707
311.532250	8000.394945	13.209536	-0.062960	4.818720
311.383222	8000.352092	13.214541	-0.062932	4.818708
311.493433	8000.374504	13.219546	-0.062953	4.818714
311.536259	8000.405481	13.224551	-0.062961	4.818723
311.287306	8000.460983	13.229555	-0.062915	4.818740
311.322714	8000.433118	13.234560	-0.062921	4.818732
311.144347	8000.374147	13.239565	-0.062888	4.818715
311.348729	8000.385197	13.244570	-0.062926	4.818718
311.291986	8000.405437	13.249575	-0.062915	4.818724
311.355712	8000.415705	13.254579	-0.062927	4.818727
311.362092	8000.425227	13.259584	-0.062928	4.818729
311.327054	8000.359729	13.264589	-0.062922	4.818710
311.359533	8000.412601	13.269594	-0.062928	4.818726
311.262305	8000.397695	13.274599	-0.062910	4.818722
311.333727	8000.372397	13.279603	-0.062923	4.818714
311.400280	8000.345987	13.284608	-0.062935	4.818706
311.384834	8000.363617	13.289613	-0.062932	4.818711
311.459256	8000.379269	13.294618	-0.062946	4.818715
311.438130	8000.343326	13.299623	-0.062942	4.818705
311.503208	8000.311651	13.304627	-0.062954	4.818695
311.380116	8000.403409	13.309632	-0.062931	4.818723
311.259668	8000.338898	13.314637	-0.062909	4.818704
311.716825	8000.345895	13.319642	-0.062994	4.818704
311.536009	8000.372911	13.324647	-0.062960	4.818713
311.356233	8000.327560	13.329651	-0.062927	4.818700
311.556810	8000.355344	13.334656	-0.062964	4.818708
311.595276	8000.344304	13.339661	-0.062971	4.818704
311.423392	8000.342064	13.344666	-0.062939	4.818704
311.555187	8000.380493	13.349671	-0.062964	4.818715
311.404707	8000.340767	13.354675	-0.062936	4.818704
311.415249	8000.351392	13.359680	-0.062937	4.818707
311.280237	8000.330750	13.364685	-0.062912	4.818702
311.370297	8000.317234	13.369690	-0.062929	4.818697
311.419980	8000.365084	13.374695	-0.062938	4.818711
311.255549	8000.344059	13.379699	-0.062908	4.818706
311.422278	8000.409168	13.384704	-0.062939	4.818724
311.381184	8000.344641	13.389709	-0.062931	4.818705
311.371817	8000.317242	13.394714	-0.062929	4.818697
311.367112	8000.372776	13.399719	-0.062928	4.818714
311.556559	8000.301809	13.404723	-0.062963	4.818692
311.506776	8000.354658	13.409728	-0.062954	4.818708
311.279450	8000.339109	13.414733	-0.062912	4.818704
311.496005	8000.330386	13.419738	-0.062952	4.818701
311.574139	8000.340842	13.424743	-0.062967	4.818704
311.454745	8000.326697	13.429747	-0.062944	4.818700
311.573846	8000.414265	13.434752	-0.062967	4.818725
311.586191	8000.358825	13.439757	-0.062969	4.818709
311.441934	8000.314985	13.444762	-0.062942	4.818696
311.413371	8000.390139	13.449767	-0.062937	4.818719
311.515589	8000.353703	13.454771	-0.062956	4.818708
311.575707	8000.361826	13.459776	-0.062967	4.818710
311.266297	8000.385071	13.464781	-0.062909	4.818718
311.423059	8000.393403	13.469786	-0.062938	4.818720
311.591661	8000.417625	13.474791	-0.062970	4.818726
311.290659	8000.373842	13.479795	-0.062913	4.818714
311.270588	8000.388265	13.484800	-0.062910	4.818719
311.352258	8000.279179	13.489805	-0.062925	4.818686
311.451557	8000.312989	13.494810	-0.062943	4.818696
311.441869	8000.347478	13.499815	-0.062942	4.818706
311.501982	8000.282170	13.504819	-0.062953	4.818686
311.474479	8000.361535	13.509824	-0.062948	4.818710
311.488333	8000.369056	13.514829	-0.062950	4.818712
311.491122	8000.349158	13.519834	-0.062951	4.818706
311.508296	8000.373507	13.524839	-0.062954	4.818714
311.005794	8000.384798	13.529843	-0.062860	4.818719
311.257849	8000.427938	13.534848	-0.062907	4.818731
311.175902	8000.411134	13.539853	-0.062892	4.818726
311.036945	8000.365265	13.544858	-0.062866	4.818713
311.115077	8000.353691	13.549863	-0.062880	4.818709
311.340856	8000.276903	13.554867	-0.062922	4.818685
311.574115	8000.353367	13.559872	-0.062966	4.818707
311.409007	8000.331285	13.564877	-0.062935	4.818701
311.634545	8000.285963	13.569882	-0.062977	4.818687
311.593064	8000.361999	13.574887	-0.062969	4.818710
311.592384	8000.345203	13.579891	-0.062969	4.818705
311.521650	8000.395682	13.584896	-0.062956	4.818720
311.434693	8000.395597	13.589901	-0.062940	4.818720
311.534268	8000.403185	13.594906	-0.062958	4.818722
311.480653	8000.412975	13.599911	-0.062948	4.818725
311.337504	8000.381737	13.604915	-0.062921	4.818717
311.458779	8000.409538	13.609920	-0.062944	4.818724
311.429472	8000.382929	13.614925	-0.062938	4.818717
311.465937	8000.434803	13.619930	-0.062945	4.818732
311.470977	8000.438014	13.624935	-0.062946	4.818733
311.540712	8000.370733	13.629939	-0.062959	4.818713
311.615161	8000.401072	13.634944	-0.062973	4.818721
311.526432	8000.375788	13.639949	-0.062956	4.818714
311.496014	8000.404762	13.644954	-0.062951	4.818723
311.660426	8000.398508	13.649959	-0.062981	4.818720
311.511624	8000.283275	13.654963	-0.062953	4.818687
311.802031	8000.312229	13.659968	-0.063007	4.818694
311.493515	8000.334436	13.664973	-0.062950	4.818702
311.653097	8000.413089	13.669978	-0.062980	4.818725
311.810184	8000.396250	13.674983	-0.063009	4.818719
311.613870	8000.352780	13.679987	-0.062972	4.818707
311.504257	8000.366037	13.684992	-0.062952	4.818711
311.396727	8000.307988	13.689997	-0.062932	4.818694
311.576724	8000.325015	13.695002	-0.062965	4.818699
311.387130	8000.382339	13.700007	-0.062930	4.818717
311.262330	8000.385957	13.705011	-0.062907	4.818718
311.532518	8000.383177	13.710016	-0.062957	4.818716
311.627274	8000.352938	13.715021	-0.062975	4.818707
311.618040	8000.362257	13.720026	-0.062973	4.818710
311.628606	8000.395961	13.725031	-0.062975	4.818720
311.499108	8000.274685	13.730035	-0.062951	4.818684
311.635540	8000.372968	13.735040	-0.062976	4.818713
311.529121	8000.349551	13.740045	-0.062956	4.818706
311.620062	8000.413673	13.745050	-0.062973	4.818725
311.448941	8000.410394	13.750055	-0.062941	4.818725
311.542909	8000.365459	13.755059	-0.062959	4.818711
311.602698	8000.437568	13.760064	-0.062970	4.818732
311.616615	8000.382149	13.765069	-0.062972	4.818716
311.437449	8000.394500	13.770074	-0.062939	4.818720
311.489232	8000.396221	13.775079	-0.062949	4.818720
311.329254	8000.315461	13.780083	-0.062919	4.818697
311.285375	8000.403004	13.785088	-0.062911	4.818723
311.549582	8000.387559	13.790093	-0.062960	4.818718
311.487682	8000.406682	13.795098	-0.062948	4.818723
311.497820	8000.420449	13.800103	-0.062950	4.818728
311.510675	8000.391241	13.805107	-0.062952	4.818719
311.518802	8000.440649	13.810112	-0.062954	4.818733
311.352917	8000.393379	13.815117	-0.062923	4.818720
311.196880	8000.414424	13.820122	-0.062894	4.818727
311.219748	8000.451435	13.825127	-0.062898	4.818738
311.289190	8000.385200	13.830131	-0.062911	4.818718
311.433889	8000.412257	13.835136	-0.062938	4.818725
311.587564	8000.419500	13.840141	-0.062966	4.818727
311.664239	8000.435183	13.845146	-0.062981	4.818731
311.522483	8000.402913	13.850151	-0.062954	4.818722
311.239594	8000.401327	13.855155	-0.062902	4.818723
311.552044	8000.434764	13.860160	-0.062960	4.818732
311.644647	8000.405546	13.865165	-0.062977	4.818723
311.328435	8000.448633	13.870170	-0.062918	4.818737
311.498363	8000.393146	13.875175	-0.062950	4.818719
311.596508	8000.404912	13.880179	-0.062968	4.818723
311.438942	8000.451113	13.885184	-0.062938	4.818737
311.309895	8000.417961	13.890189	-0.062914	4.818728
311.543622	8000.435687	13.895194	-0.062958	4.818732
311.407394	8000.418176	13.900199	-0.062932	4.818727
311.381899	8000.410499	13.905203	-0.062928	4.818725
311.563859	8000.412865	13.910208	-0.062962	4.818725
311.696444	8000.390461	13.915213	-0.062986	4.818718
311.490039	8000.393017	13.920218	-0.062948	4.818719
311.534095	8000.409324	13.925223	-0.062956	4.818724
311.717751	8000.361359	13.930227	-0.062990	4.818709
311.502505	8000.397369	13.935232	-0.062950	4.818721
311.361972	8000.345184	13.940237	-0.062924	4.818706
311.448661	8000.351555	13.945242	-0.062940	4.818707
311.546018	8000.393732	13.950247	-0.062958	4.818719
311.589576	8000.297787	13.955251	-0.062966	4.818691
311.752331	8000.413197	13.960256	-0.062996	4.818724
311.911235	8000.385891	13.965261	-0.063026	4.818716
311.757562	8000.449977	13.970266	-0.062997	4.818735
311.473873	8000.452575	13.975271	-0.062944	4.818737
311.639740	8000.389693	13.980275	-0.062975	4.818718
311.699020	8000.405149	13.985280	-0.062986	4.818722
311.462213	8000.373740	13.990285	-0.062942	4.818714
311.521046	8000.412268	13.995290	-0.062953	4.818725
311.710629	8000.414734	14.000295	-0.062988	4.818725
311.443310	8000.373487	14.005299	-0.062938	4.818714
311.648951	8000.413926	14.010304	-0.062977	4.818725
311.710321	8000.341292	14.015309	-0.062988	4.818703
311.617302	8000.299167	14.020314	-0.062971	4.818691
311.497112	8000.355296	14.025319	-0.062948	4.818708
311.463802	8000.289821	14.030323	-0.062942	4.818689
311.491707	8000.377250	14.035328	-0.062947	4.818715
311.625656	8000.331786	14.040333	-0.062972	4.818701
311.636801	8000.357105	14.045338	-0.062974	4.818708
311.512396	8000.390101	14.050343	-0.062951	4.818719
311.681593	8000.318870	14.055347	-0.062982	4.818697
311.688277	8000.391337	14.060352	-0.062984	4.818718
311.689197	8000.351484	14.065357	-0.062984	4.818706
311.375054	8000.387255	14.070362	-0.062925	4.818718
311.678354	8000.370220	14.075367	-0.062982	4.818712
311.772151	8000.336821	14.080371	-0.062999	4.818702
311.821208	8000.368928	14.085376	-0.063008	4.818711
311.738633	8000.359459	14.090381	-0.062993	4.818709
311.717925	8000.361285	14.095386	-0.062989	4.818709
311.727524	8000.379241	14.100391	-0.062991	4.818714
311.571497	8000.277551	14.105395	-0.062962	4.818685
311.679191	8000.323009	14.110400	-0.062982	4.818698
311.674488	8000.355465	14.115405	-0.062981	4.818708
311.720559	8000.402219	14.120410	-0.062989	4.818721
311.737504	8000.402438	14.125415	-0.062992	4.818721
311.726302	8000.360329	14.130419	-0.062990	4.818709
311.809176	8000.401268	14.135424	-0.063006	4.818721
311.573144	8000.358330	14.140429	-0.062962	4.818709
311.652120	8000.367748	14.145434	-0.062976	4.818711
311.767121	8000.376586	14.150439	-0.062998	4.818714
311.659375	8000.327975	14.155443	-0.062978	4.818699
311.804104	8000.361327	14.160448	-0.063005	4.818709
311.879731	8000.324545	14.165453	-0.063019	4.818698
311.860313	8000.362055	14.170458	-0.063015	4.818709
311.676859	8000.394282	14.175463	-0.062981	4.818719
311.775622	8000.311644	14.180467	-0.062999	4.818694
311.783356	8000.353703	14.185472	-0.063001	4.818707
311.609891	8000.383962	14.190477	-0.062968	4.818716
311.679225	8000.371225	14.195482	-0.062981	4.818712
311.735842	8000.413920	14.200487	-0.062992	4.818725
311.519124	8000.376479	14.205491	-0.062951	4.818714
311.586350	8000.404626	14.210496	-0.062964	4.818723
311.673077	8000.362743	14.215501	-0.062980	4.818710
311.646362	8000.359246	14.220506	-0.062975	4.818709
311.605987	8000.351375	14.225511	-0.062967	4.818707
311.512568	8000.311343	14.230515	-0.062950	4.818695
311.656167	8000.360416	14.235520	-0.062977	4.818709
311.718550	8000.372765	14.240525	-0.062988	4.818713
311.610388	8000.323100	14.245530	-0.062968	4.818698
311.727461	8000.368680	14.250535	-0.062990	4.818711
311.555141	8000.333915	14.255539	-0.062958	4.818702
311.617397	8000.367243	14.260544	-0.062969	4.818711
311.663437	8000.340565	14.265549	-0.062978	4.818703
311.489916	8000.259629	14.270554	-0.062945	4.818680
311.571672	8000.372935	14.275559	-0.062961	4.818713
311.539815	8000.378812	14.280563	-0.062955	4.818715
311.777185	8000.366164	14.285568	-0.062999	4.818710
311.519571	8000.396377	14.290573	-0.062951	4.818720
311.532001	8000.376605	14.295578	-0.062953	4.818714
311.579982	8000.386668	14.300583	-0.062962	4.818717
311.458391	8000.311653	14.305587	-0.062939	4.818695
311.471772	8000.349589	14.310592	-0.062942	4.818707
311.654174	8000.360353	14.315597	-0.062976	4.818709
311.582390	8000.374102	14.320602	-0.062962	4.818714
311.559962	8000.395837	14.325607	-0.062958	4.818720
311.583688	8000.344742	14.330611	-0.062962	4.818705
311.642892	8000.351805	14.335616	-0.062973	4.818707
311.547651	8000.368396	14.340621	-0.062956	4.818712
311.558917	8000.351756	14.345626	-0.062958	4.818707
311.695296	8000.382901	14.350631	-0.062983	4.818716
311.588090	8000.344788	14.355635	-0.062963	4.818705
311.506659	8000.382539	14.360640	-0.062948	4.818716
311.496270	8000.340441	14.365645	-0.062946	4.818704
311.463478	8000.351551	14.370650	-0.062940	4.818707
311.598123	8000.361693	14.375655	-0.062965	4.818710
311.458331	8000.322107	14.380659	-0.062939	4.818699
311.811941	8000.250129	14.385664	-0.063004	4.818676
311.877658	8000.260423	14.390669	-0.063017	4.818679
311.763106	8000.240048	14.395674	-0.062995	4.818673
311.914526	8000.322791	14.400679	-0.063024	4.818697
312.013928	8000.327230	14.405683	-0.063042	4.818698
312.056208	8000.371837	14.410688	-0.063050	4.818711
312.110682	8000.368348	14.415693	-0.063060	4.818710
311.977026	8000.357164	14.420698	-0.063035	4.818707
312.009380	8000.385906	14.425703	-0.063041	4.818715
311.889085	8000.389583	14.430707	-0.063019	4.818717
312.098327	8000.374472	14.435712	-0.063058	4.818712
312.044159	8000.392647	14.440717	-0.063047	4.818717
312.087362	8000.360687	14.445722	-0.063055	4.818708
311.865197	8000.404998	14.450727	-0.063014	4.818722
311.948164	8000.381948	14.455731	-0.063029	4.818714
311.856503	7999.285609	14.460736	-0.063012	4.818389

311.992392	7996.185906	14.465741	-0.063035	4.817465
312.072105	7990.677707	14.470746	-0.063046	4.815825
312.200101	7984.024411	14.475751	-0.063066	4.813843
311.980480	7976.784976	14.480755	-0.063020	4.811687
311.925805	7969.230510	14.485760	-0.063005	4.809435
312.028136	7961.421974	14.490765	-0.063019	4.807105
311.704066	7953.507526	14.495770	-0.062953	4.804745
311.784215	7945.569416	14.500775	-0.062963	4.802375
311.873356	7937.554847	14.505779	-0.062974	4.799980
311.827907	7929.632550	14.510784	-0.062961	4.797613
311.787262	7921.557658	14.515789	-0.062948	4.795199
311.688718	7913.617689	14.520794	-0.062924	4.792824
311.538281	7905.616488	14.525799	-0.062891	4.790429
311.503979	7897.563250	14.530803	-0.062879	4.788018
311.690520	7889.572630	14.535808	-0.062909	4.785623
311.730328	7881.565716	14.540813	-0.062911	4.783223
311.408942	7873.558180	14.545818	-0.062846	4.780823
311.690351	7865.588764	14.550823	-0.062893	4.778431
311.708752	7857.597851	14.555827	-0.062891	4.776032
311.560146	7849.544961	14.560832	-0.062858	4.773613
311.460760	7841.561066	14.565837	-0.062834	4.771214
311.603196	7833.529422	14.570842	-0.062856	4.768799
311.528102	7825.596386	14.575847	-0.062837	4.766413
311.404823	7817.522793	14.580851	-0.062808	4.763984
311.416352	7809.646267	14.585856	-0.062805	4.761612
311.542590	7801.534254	14.590861	-0.062823	4.759168
311.179661	7793.599518	14.595866	-0.062751	4.756777
311.194057	7785.584931	14.600871	-0.062748	4.754360
311.036120	7777.578282	14.605875	-0.062713	4.751944
311.206480	7769.509975	14.610880	-0.062740	4.749508
311.039523	7761.505312	14.615885	-0.062704	4.747091
311.004772	7753.475778	14.620890	-0.062692	4.744664
311.079548	7745.560548	14.625895	-0.062701	4.742271
310.752585	7737.507330	14.630899	-0.062634	4.739835
310.967986	7729.519639	14.635904	-0.062669	4.737417
311.188589	7721.527739	14.640909	-0.062705	4.734997
310.926668	7713.514255	14.645914	-0.062651	4.732570
310.903357	7705.539343	14.650919	-0.062641	4.730152
311.049563	7697.493334	14.655923	-0.062663	4.727712
311.063541	7689.501107	14.660928	-0.062661	4.725287
310.877929	7681.541743	14.665933	-0.062621	4.722871
310.918854	7673.500347	14.670938	-0.062623	4.720428
310.927084	7665.593377	14.675943	-0.062620	4.718025
310.814913	7657.534872	14.680947	-0.062594	4.715575
310.801601	7649.577494	14.685952	-0.062586	4.713154
310.817220	7641.550513	14.690957	-0.062583	4.710711
310.718434	7633.507753	14.695962	-0.062560	4.708261
310.810737	7625.525293	14.700967	-0.062572	4.705829
310.809702	7617.510750	14.705971	-0.062566	4.703386
310.770345	7609.576991	14.710976	-0.062554	4.700966
310.561831	7601.566996	14.715981	-0.062510	4.698522
310.596902	7593.521141	14.720986	-0.062511	4.696065
310.618588	7585.504995	14.725991	-0.062510	4.693616
310.555254	7577.520366	14.730995	-0.062493	4.691176
310.606224	7569.483067	14.736000	-0.062497	4.688718
310.630981	7561.532536	14.741005	-0.062496	4.686285
310.612381	7553.484081	14.746010	-0.062488	4.683821
310.485109	7545.593531	14.751015	-0.062459	4.681404
310.491493	7537.480232	14.756019	-0.062455	4.678918
310.490286	7529.590098	14.761024	-0.062449	4.676499
310.432302	7521.506596	14.766029	-0.062433	4.674019
310.453389	7513.496660	14.771034	-0.062432	4.671560
310.469783	7505.472642	14.776039	-0.062430	4.669096
310.316811	7497.454751	14.781043	-0.062396	4.666633
310.346278	7489.415900	14.786048	-0.062396	4.664161
310.465696	7481.545732	14.791053	-0.062413	4.661740
310.265674	7473.459450	14.796058	-0.062371	4.659252
310.310304	7465.534707	14.801063	-0.062374	4.656812
310.273411	7457.458100	14.806067	-0.062361	4.654324
310.360541	7449.516417	14.811072	-0.062372	4.651876
310.245333	7441.442367	14.816077	-0.062346	4.649385
310.114653	7433.484983	14.821082	-0.062316	4.646930
310.195829	7425.462928	14.826087	-0.062326	4.644453
310.086588	7417.540317	14.831091	-0.062301	4.642006
310.105783	7409.472307	14.836096	-0.062299	4.639512
309.974515	7401.495661	14.841101	-0.062269	4.637046
310.077591	7393.391785	14.846106	-0.062283	4.634538
310.158926	7385.519158	14.851111	-0.062293	4.632101
309.996929	7377.392171	14.856115	-0.062257	4.629584
310.113759	7369.475514	14.861120	-0.062274	4.627131
310.071722	7361.409395	14.866125	-0.062261	4.624630
310.053799	7353.489457	14.871130	-0.062252	4.622173
310.208042	7345.452592	14.876135	-0.062276	4.619678
310.018581	7337.455228	14.881139	-0.062235	4.617194
309.896781	7329.400760	14.886144	-0.062207	4.614692
309.995866	7321.434291	14.891149	-0.062221	4.612215
309.903347	7313.382460	14.896154	-0.062198	4.609710
309.932438	7305.450915	14.901159	-0.062198	4.607242
309.778081	7297.341936	14.906163	-0.062164	4.604716
309.947857	7289.455495	14.911168	-0.062191	4.602259
309.811798	7281.455405	14.916173	-0.062160	4.599765
309.643510	7273.441853	14.921178	-0.062123	4.597265
309.778003	7265.426288	14.926183	-0.062143	4.594764
309.645998	7257.398375	14.931187	-0.062113	4.592257
309.686749	7249.398990	14.936192	-0.062116	4.589758
309.608569	7241.419568	14.941197	-0.062096	4.587263
309.730828	7233.336637	14.946202	-0.062113	4.584735
309.581576	7225.423251	14.951207	-0.062080	4.582259
309.496745	7217.390222	14.956211	-0.062059	4.579743
309.525774	7209.401796	14.961216	-0.062060	4.577241
309.425371	7201.386692	14.966221	-0.062036	4.574728
309.320022	7193.355173	14.971226	-0.062011	4.572209
309.351434	7185.352078	14.976231	-0.062011	4.569698
309.227819	7177.314686	14.981235	-0.061983	4.567174
309.373159	7169.366320	14.986240	-0.062005	4.564677
309.309029	7161.459529	14.991245	-0.061988	4.562192
309.214726	7153.355844	14.996250	-0.061965	4.559643
309.166385	7145.428967	15.001255	-0.061951	4.557148
309.154478	7137.339628	15.006259	-0.061943	4.554601
309.201501	7129.382161	15.011264	-0.061947	4.552095
309.176192	7121.334604	15.016269	-0.061937	4.549558
309.097367	7113.367220	15.021274	-0.061917	4.547045
309.112932	7105.333236	15.026279	-0.061914	4.544510
309.223143	7097.398791	15.031283	-0.061930	4.542005
308.981370	7089.317738	15.036288	-0.061879	4.539452
309.151028	7081.397507	15.041293	-0.061906	4.536949
309.227648	7073.299885	15.046298	-0.061915	4.534388
309.175362	7065.355023	15.051303	-0.061900	4.531874
309.030293	7057.279467	15.056307	-0.061868	4.529317
309.113979	7049.341228	15.061312	-0.061878	4.526802
309.075591	7041.257961	15.066317	-0.061865	4.524240
308.918259	7033.362598	15.071322	-0.061831	4.521736
309.031302	7025.352754	15.076327	-0.061847	4.519194
309.076269	7017.354012	15.081331	-0.061850	4.516655
308.823911	7009.317826	15.086336	-0.061798	4.514101
308.720439	7001.356313	15.091341	-0.061773	4.511570
308.940602	6993.295542	15.096346	-0.061809	4.509007
308.894147	6985.309051	15.101351	-0.061795	4.506466
308.642322	6977.240302	15.106355	-0.061743	4.503896
308.587002	6969.301278	15.111360	-0.061727	4.501366
308.773018	6961.265905	15.116365	-0.061757	4.498806
308.616539	6953.284279	15.121370	-0.061722	4.496259
308.629920	6945.290447	15.126375	-0.061720	4.493708
308.515153	6937.277373	15.131379	-0.061693	4.491149
308.478574	6929.238603	15.136384	-0.061681	4.488581
308.384640	6921.298938	15.141389	-0.061658	4.486042
308.400446	6913.233549	15.146394	-0.061656	4.483463
308.268964	6905.340579	15.151399	-0.061626	4.480936
308.250794	6897.251738	15.156403	-0.061617	4.478346
307.936994	6889.314888	15.161408	-0.061554	4.475801
308.209298	6881.267346	15.166413	-0.061599	4.473222
307.985371	6873.229479	15.171418	-0.061552	4.470643
307.937432	6865.255065	15.176423	-0.061538	4.468083
308.076054	6857.212540	15.181427	-0.061559	4.465501
308.059429	6849.266285	15.186432	-0.061550	4.462948
307.934485	6841.271860	15.191437	-0.061522	4.460377
308.069091	6833.231580	15.196442	-0.061542	4.457791
308.123797	6825.249512	15.201447	-0.061547	4.455222
308.012776	6817.236831	15.206451	-0.061521	4.452640
307.877393	6809.193400	15.211456	-0.061490	4.450047
307.991751	6801.249448	15.216461	-0.061506	4.447486
307.941093	6793.176310	15.221466	-0.061492	4.444881
307.965256	6785.238191	15.226471	-0.061491	4.442319
307.908142	6777.205511	15.231475	-0.061475	4.439724
307.987366	6769.292115	15.236480	-0.061484	4.437167
307.742159	6761.211187	15.241485	-0.061434	4.434552
307.641777	6753.182800	15.246490	-0.061410	4.431954
307.724863	6745.183937	15.251495	-0.061420	4.429364
307.526738	6737.207190	15.256499	-0.061378	4.426779
307.438973	6729.159092	15.261504	-0.061356	4.424169
307.646233	6721.214414	15.266509	-0.061389	4.421594
307.838365	6713.153393	15.271514	-0.061420	4.418979
307.816671	6705.240358	15.276519	-0.061411	4.416409
307.679895	6697.108345	15.281523	-0.061380	4.413766
307.824863	6689.214069	15.286528	-0.061402	4.411200
307.638314	6681.185732	15.291533	-0.061362	4.408588
307.751642	6673.176643	15.296538	-0.061378	4.405981
307.736384	6665.176654	15.301543	-0.061369	4.403376
307.494639	6657.251913	15.306547	-0.061319	4.400792
307.460731	6649.190965	15.311552	-0.061308	4.398163
307.397386	6641.277018	15.316557	-0.061291	4.395580
307.310452	6633.216222	15.321562	-0.061269	4.392948
307.500291	6625.226348	15.326567	-0.061299	4.390339
307.390635	6617.205270	15.331571	-0.061274	4.387717
307.295383	6609.215462	15.336576	-0.061251	4.385103
307.235873	6601.253561	15.341581	-0.061234	4.382497
307.001087	6593.249600	15.346586	-0.061185	4.379875
307.092087	6585.295054	15.351591	-0.061197	4.377269
307.063127	6577.272578	15.356595	-0.061186	4.374639
306.853892	6569.303563	15.361600	-0.061142	4.372023
306.833755	6561.275379	15.366605	-0.061133	4.369388
307.013015	6553.283775	15.371610	-0.061161	4.366765
306.938942	6545.283542	15.376615	-0.061142	4.364135
307.078472	6537.326096	15.381619	-0.061163	4.361519
306.890412	6529.302992	15.386624	-0.061123	4.358878
306.928185	6521.338466	15.391629	-0.061125	4.356256
306.804720	6513.258320	15.396634	-0.061096	4.353593
306.911716	6505.254528	15.401639	-0.061111	4.350956
306.889370	6497.258578	15.406643	-0.061102	4.348319
306.621225	6489.219382	15.411648	-0.061046	4.345663
306.888427	6481.282132	15.416653	-0.061091	4.343044
306.780094	6473.242385	15.421658	-0.061066	4.340387
306.755791	6465.318860	15.426663	-0.061056	4.337767
306.664390	6457.239511	15.431667	-0.061033	4.335093
306.872588	6449.273806	15.436672	-0.061067	4.332458
306.759548	6441.268992	15.441677	-0.061041	4.329805
306.727301	6433.235107	15.446682	-0.061029	4.327142
306.730140	6425.258949	15.451687	-0.061025	4.324497
306.643268	6417.270197	15.456691	-0.061003	4.321845
306.739333	6409.215934	15.461696	-0.061016	4.319172
306.722919	6401.291630	15.466701	-0.061008	4.316538
306.728947	6393.212945	15.471706	-0.061004	4.313853
306.700129	6385.284684	15.476711	-0.060993	4.311215
306.512789	6377.242634	15.481715	-0.060953	4.308536
306.746013	6369.230146	15.486720	-0.060991	4.305869
306.743007	6361.240070	15.491725	-0.060985	4.303206
306.330249	6353.252849	15.496730	-0.060903	4.300539
306.529530	6345.252336	15.501735	-0.060935	4.297871
306.471614	6337.179603	15.506739	-0.060919	4.295175
306.348885	6329.240784	15.511744	-0.060891	4.292521
306.493249	6321.181932	15.516749	-0.060912	4.289828
306.454417	6313.218081	15.521754	-0.060900	4.287163
306.282109	6305.200478	15.526759	-0.060863	4.284478
306.281907	6297.232508	15.531763	-0.060857	4.281809
306.514603	6289.198649	15.536768	-0.060895	4.279118
306.328279	6281.308297	15.541773	-0.060856	4.276470
306.222365	6273.168571	15.546778	-0.060830	4.273737
306.043856	6265.290862	15.551783	-0.060792	4.271090
306.064323	6257.181035	15.556787	-0.060791	4.268365
306.134944	6249.173305	15.561792	-0.060798	4.265673
306.064773	6241.225791	15.566797	-0.060780	4.262999
306.194984	6233.183706	15.571802	-0.060799	4.260293
306.206188	6225.242897	15.576807	-0.060796	4.257618
306.018801	6217.229738	15.581811	-0.060756	4.254915
306.010105	6209.188575	15.586816	-0.060749	4.252202
305.928665	6201.204710	15.591821	-0.060729	4.249507
305.848287	6193.201891	15.596826	-0.060708	4.246803
306.089780	6185.139770	15.601831	-0.060748	4.244081
306.116910	6177.229686	15.606835	-0.060748	4.241406
306.039311	6169.151698	15.611840	-0.060728	4.238672
306.066204	6161.219463	15.616845	-0.060728	4.235987
306.017598	6153.241221	15.621850	-0.060714	4.233283
306.053568	6145.215696	15.626855	-0.060715	4.230563
305.827921	6137.182559	15.631859	-0.060668	4.227835
305.793697	6129.159562	15.636864	-0.060656	4.225111
305.897162	6121.184147	15.641869	-0.060670	4.222403
305.685884	6113.147885	15.646874	-0.060626	4.219669
305.726434	6105.213257	15.651879	-0.060628	4.216971
305.510242	6097.181226	15.656883	-0.060582	4.214234
305.561808	6089.168516	15.661888	-0.060587	4.211506
305.425617	6081.183749	15.666893	-0.060556	4.208783
305.379588	6073.187451	15.671898	-0.060542	4.206056
305.313942	6065.219895	15.676903	-0.060525	4.203336
305.157221	6057.224981	15.681907	-0.060490	4.200605
305.375684	6049.200583	15.686912	-0.060526	4.197865
305.392900	6041.196480	15.691917	-0.060524	4.195129
305.287069	6033.145299	15.696922	-0.060499	4.192373
305.045210	6025.163452	15.701927	-0.060449	4.189638
305.314297	6017.114387	15.706931	-0.060493	4.186883
305.142494	6009.116980	15.711936	-0.060456	4.184140
304.945433	6001.240429	15.716941	-0.060414	4.181436
304.694056	5993.208240	15.721946	-0.060362	4.178675
304.973886	5985.196093	15.726951	-0.060409	4.175927
304.977498	5977.149102	15.731955	-0.060405	4.173161
305.217404	5969.136116	15.736960	-0.060444	4.170408
305.187177	5961.176234	15.741965	-0.060433	4.167668
304.994992	5953.171337	15.746970	-0.060392	4.164909
305.081441	5945.199634	15.751975	-0.060403	4.162163
305.061872	5937.173726	15.756979	-0.060394	4.159395
304.982667	5929.225030	15.761984	-0.060374	4.156651
305.105410	5921.190938	15.766989	-0.060392	4.153878
305.125077	5913.227451	15.771994	-0.060390	4.151127
304.946357	5905.245129	15.776999	-0.060352	4.148365
304.821870	5897.165125	15.782003	-0.060323	4.145567
304.843129	5889.173422	15.787008	-0.060322	4.142801
304.971964	5881.180236	15.792013	-0.060341	4.140033
305.008370	5873.224711	15.797018	-0.060342	4.137275
304.836711	5865.208760	15.802023	-0.060305	4.134492
304.884880	5857.238290	15.807027	-0.060309	4.131726
304.876726	5849.214254	15.812032	-0.060302	4.128938
304.875445	5841.240268	15.817037	-0.060296	4.126166
304.757590	5833.173968	15.822042	-0.060269	4.123358
304.621746	5825.247517	15.827047	-0.060239	4.120597
304.616794	5817.237012	15.832051	-0.060232	4.117807
304.535538	5809.230522	15.837056	-0.060212	4.115015
304.558888	5801.247670	15.842061	-0.060211	4.112230
304.573578	5793.164171	15.847066	-0.060209	4.109409
304.418863	5785.232490	15.852071	-0.060175	4.106636
304.598134	5777.125641	15.857075	-0.060203	4.103805
304.347520	5769.249840	15.862080	-0.060151	4.101047
303.980624	5761.280801	15.867085	-0.060077	4.098253
304.038431	5753.221374	15.872090	-0.060083	4.095431
304.080980	5745.209970	15.877095	-0.060085	4.092623
304.043267	5737.158463	15.882099	-0.060073	4.089799
304.359175	5729.152838	15.887104	-0.060127	4.086994
304.269001	5721.164369	15.892109	-0.060105	4.084187
304.141051	5713.205235	15.897114	-0.060076	4.081388
304.274492	5705.205897	15.902119	-0.060095	4.078576
304.293103	5697.185009	15.907123	-0.060093	4.075754
304.313930	5689.181987	15.912128	-0.060092	4.072935
304.315921	5681.201256	15.917133	-0.060087	4.070123
304.278647	5673.173767	15.922138	-0.060075	4.067291
304.294920	5665.192009	15.927143	-0.060073	4.064474
304.139671	5657.248023	15.932147	-0.060039	4.061667
303.761913	5649.231059	15.937152	-0.059963	4.058827
303.907756	5641.236500	15.942157	-0.059985	4.056002
303.758979	5633.217291	15.947162	-0.059952	4.053162
303.720842	5625.182110	15.952167	-0.059940	4.050316
303.852940	5617.214565	15.957171	-0.059959	4.047494
303.855119	5609.165077	15.962176	-0.059954	4.044639
303.721418	5601.254908	15.967181	-0.059924	4.041830
303.784508	5593.198162	15.972186	-0.059931	4.038969
304.030557	5585.301246	15.977191	-0.059971	4.036167
303.860696	5577.205806	15.982195	-0.059934	4.033285
303.700540	5569.151740	15.987200	-0.059899	4.030416
304.055130	5561.149897	15.992205	-0.059960	4.027571
303.794886	5553.166215	15.997210	-0.059906	4.024722
303.691184	5545.293042	16.002215	-0.059882	4.021912
303.633883	5537.223896	16.007219	-0.059866	4.019031
303.594139	5529.258481	16.012224	-0.059853	4.016185
303.794434	5521.222845	16.017229	-0.059885	4.013316
303.597471	5513.198531	16.022234	-0.059843	4.010443
303.516852	5505.249531	16.027239	-0.059823	4.007596
303.591687	5497.235222	16.032243	-0.059832	4.004727
303.543768	5489.277769	16.037248	-0.059818	4.001874
303.629133	5481.263945	16.042253	-0.059828	3.999000
303.231430	5473.324318	16.047258	-0.059749	3.996143
303.679639	5465.251482	16.052263	-0.059827	3.993251
303.574314	5457.272815	16.057267	-0.059802	3.990381
303.777826	5449.238914	16.062272	-0.059835	3.987495
303.671944	5441.217216	16.067277	-0.059810	3.984605
303.238929	5433.284158	16.072282	-0.059724	3.981739
303.572717	5425.267256	16.077287	-0.059781	3.978855
303.500835	5417.284764	16.082291	-0.059762	3.975973
303.441570	5409.275486	16.087296	-0.059746	3.973081
303.274090	5401.248105	16.092301	-0.059710	3.970177
303.378073	5393.251920	16.097306	-0.059724	3.967288
303.222261	5385.244396	16.102311	-0.059689	3.964387
302.925550	5377.357648	16.107315	-0.059629	3.961526
302.930982	5369.254731	16.112320	-0.059625	3.958590
302.919507	5361.296383	16.117325	-0.059617	3.955704
302.897525	5353.248937	16.122330	-0.059608	3.952783
302.905717	5345.248017	16.127335	-0.059604	3.949877
302.947204	5337.247840	16.132339	-0.059607	3.946970
302.871976	5329.218386	16.137344	-0.059588	3.944048
302.977300	5321.310746	16.142349	-0.059602	3.941172
302.959666	5313.255876	16.147354	-0.059593	3.938238
302.889474	5305.291957	16.152359	-0.059575	3.935333
302.758355	5297.265285	16.157363	-0.059545	3.932402
302.707556	5289.247273	16.162368	-0.059531	3.929474
302.736861	5281.277166	16.167373	-0.059531	3.926563
302.650819	5273.223475	16.172378	-0.059510	3.923617
302.669570	5265.297392	16.177383	-0.059508	3.920717
302.971588	5257.300688	16.182387	-0.059559	3.917795
302.949895	5249.267550	16.187392	-0.059550	3.914851
302.715454	5241.299564	16.192397	-0.059501	3.911924
302.618527	5233.294514	16.197402	-0.059477	3.908985
302.721304	5225.313612	16.202407	-0.059491	3.906056
302.612739	5217.339954	16.207411	-0.059466	3.903123
302.702245	5209.318270	16.212416	-0.059477	3.900174
302.814787	5201.376817	16.217421	-0.059493	3.897253
302.699430	5193.300450	16.222426	-0.059466	3.894276
302.759018	5185.353583	16.227431	-0.059472	3.891347
302.661600	5177.316469	16.232435	-0.059449	3.888380
302.421781	5169.328097	16.237440	-0.059399	3.885426
302.280734	5161.428250	16.242445	-0.059367	3.882504
302.438353	5153.317706	16.247450	-0.059391	3.879508
302.622324	5145.402477	16.252455	-0.059420	3.876583
302.256505	5137.335328	16.257459	-0.059347	3.873587
302.365716	5129.222500	16.262464	-0.059362	3.870583
302.418392	5121.236926	16.267469	-0.059367	3.867622
302.163175	5113.269071	16.272474	-0.059314	3.864659
302.059985	5105.369336	16.277479	-0.059290	3.861722
302.263062	5097.332217	16.282483	-0.059322	3.858738
302.078202	5089.360420	16.287488	-0.059282	3.855768
302.082190	5081.378102	16.292493	-0.059278	3.852796
301.825437	5073.355051	16.297498	-0.059225	3.849801
301.788547	5065.390042	16.302503	-0.059213	3.846830
301.994045	5057.290002	16.307507	-0.059246	3.843811
301.841798	5049.394265	16.312512	-0.059212	3.840858
301.867939	5041.377337	16.317517	-0.059212	3.837862
301.575631	5033.392894	16.322522	-0.059152	3.834869
301.498841	5025.397938	16.327527	-0.059133	3.831874
301.555340	5017.360573	16.332531	-0.059138	3.828864
301.877741	5009.326209	16.337536	-0.059193	3.825858
301.797176	5001.339490	16.342541	-0.059172	3.822859
301.613596	4993.383516	16.347546	-0.059133	3.819867
301.719777	4985.380789	16.352551	-0.059147	3.816862
301.536388	4977.385149	16.357555	-0.059108	3.813850
301.590862	4969.387362	16.362560	-0.059113	3.810840
301.704280	4961.360003	16.367565	-0.059129	3.807818
301.503341	4953.356407	16.372570	-0.059086	3.804796
301.699052	4945.410361	16.377575	-0.059117	3.801802
301.519807	4937.368628	16.382579	-0.059079	3.798761
301.515835	4929.430016	16.387584	-0.059073	3.795760
301.319450	4921.472394	16.392589	-0.059031	3.792746
301.369085	4913.382359	16.397594	-0.059035	3.789684
301.643989	4905.385398	16.402599	-0.059081	3.786661
301.399928	4897.403880	16.407603	-0.059030	3.783629
301.399859	4889.412857	16.412608	-0.059025	3.780596
301.513425	4881.448272	16.417613	-0.059041	3.777574
301.559585	4873.408028	16.422618	-0.059044	3.774519
301.361490	4865.474952	16.427623	-0.059002	3.771497
301.346310	4857.437609	16.432627	-0.058994	3.768437
301.333504	4849.432867	16.437632	-0.058986	3.765387
301.237683	4841.508636	16.442637	-0.058963	3.762363
301.233729	4833.459863	16.447642	-0.058957	3.759291
301.330623	4825.528084	16.452647	-0.058970	3.756264
301.360863	4817.470588	16.457651	-0.058971	3.753185
301.090888	4809.467522	16.462656	-0.058915	3.750116
301.112313	4801.525723	16.467661	-0.058914	3.747076
301.091958	4793.432627	16.472666	-0.058905	3.743974
301.191763	4785.522373	16.477671	-0.058918	3.740943
300.940742	4777.493307	16.482675	-0.058866	3.737855
301.127316	4769.448163	16.487680	-0.058896	3.734769
301.129834	4761.511723	16.492685	-0.058891	3.731718
300.983799	4753.457694	16.497690	-0.058858	3.728616
301.167661	4745.476270	16.502695	-0.058887	3.725547
301.152437	4737.503949	16.507699	-0.058879	3.722474
300.885895	4729.500640	16.512704	-0.058824	3.719380
300.802490	4721.599479	16.517709	-0.058804	3.716327
300.643533	4713.502301	16.522714	-0.058769	3.713195
300.619918	4705.479670	16.527719	-0.058759	3.710092
300.693687	4697.485472	16.532723	-0.058768	3.707000
300.666549	4689.451515	16.537728	-0.058757	3.703887
300.768522	4681.542829	16.542733	-0.058771	3.700824
300.523255	4673.516897	16.547738	-0.058720	3.697703
300.454397	4665.523686	16.552743	-0.058702	3.694598
300.257752	4657.557951	16.557747	-0.058660	3.691497
300.224683	4649.504432	16.562752	-0.058649	3.688363
300.379491	4641.515493	16.567757	-0.058672	3.685257
300.351230	4633.555369	16.572762	-0.058662	3.682155
299.945623	4625.620676	16.577767	-0.058581	3.679049
299.563128	4617.669689	16.582771	-0.058505	3.675936
299.953732	4609.595549	16.587776	-0.058572	3.672792
299.847183	4601.622436	16.592781	-0.058547	3.669672
300.062914	4593.525323	16.597786	-0.058582	3.666510
300.074701	4585.590341	16.602791	-0.058579	3.663402
299.919201	4577.650683	16.607795	-0.058545	3.660286
300.000358	4569.604248	16.612800	-0.058555	3.657131
299.991091	4561.613991	16.617805	-0.058548	3.653994
299.901391	4553.617211	16.622810	-0.058526	3.650849
299.988191	4545.605388	16.627815	-0.058537	3.647700
300.101028	4537.601779	16.632819	-0.058552	3.644552
299.941719	4529.672668	16.637824	-0.058518	3.641424
300.003747	4521.672181	16.642829	-0.058524	3.638270
299.683556	4513.690068	16.647834	-0.058459	3.635111
299.762599	4505.693589	16.652839	-0.058468	3.631954
300.014680	4497.607954	16.657843	-0.058510	3.628765
299.887141	4489.636277	16.662848	-0.058481	3.625606
299.911011	4481.677234	16.667853	-0.058480	3.622455
299.768275	4473.653718	16.672858	-0.058448	3.619270
299.862631	4465.675983	16.677863	-0.058461	3.616107
299.691521	4457.667914	16.682867	-0.058424	3.612922
299.697133	4449.655676	16.687872	-0.058419	3.609738
299.789597	4441.694366	16.692877	-0.058431	3.606573
299.518648	4433.692971	16.697882	-0.058376	3.603380
299.789998	4425.693402	16.702887	-0.058421	3.600200
299.895113	4417.725550	16.707891	-0.058435	3.597024
299.684507	4409.721571	16.712896	-0.058391	3.593823
299.740625	4401.733187	16.717901	-0.058396	3.590632
299.622841	4393.728904	16.722906	-0.058369	3.587428
299.464249	4385.714602	16.727911	-0.058334	3.584215
299.481582	4377.781664	16.732915	-0.058332	3.581037
299.330617	4369.766421	16.737920	-0.058299	3.577818
299.396677	4361.759285	16.742925	-0.058306	3.574606
299.510520	4353.723103	16.747930	-0.058322	3.571381
299.579587	4345.754940	16.752935	-0.058329	3.568179
299.537291	4337.740294	16.757939	-0.058316	3.564952
299.410799	4329.813680	16.762944	-0.058288	3.561755
299.606011	4321.793174	16.767949	-0.058319	3.558528
299.525490	4313.816335	16.772954	-0.058298	3.555306
299.389611	4305.802326	16.777959	-0.058268	3.552065
299.300545	4297.774362	16.782963	-0.058246	3.548816
299.175499	4289.786631	16.787968	-0.058218	3.545580
299.576125	4281.798157	16.792973	-0.058287	3.542357
299.332660	4273.781031	16.797978	-0.058236	3.539099
299.359601	4265.865073	16.802983	-0.058236	3.535888
299.439353	4257.823126	16.807987	-0.058246	3.532624
299.267886	4249.827298	16.812992	-0.058209	3.529368
299.161682	4241.875260	16.817997	-0.058184	3.526129
299.061603	4233.842758	16.823002	-0.058160	3.522854
298.995274	4225.905460	16.828007	-0.058142	3.519617
298.868100	4217.926743	16.833011	-0.058113	3.516357
298.924120	4209.883766	16.838016	-0.058118	3.513074
298.759187	4201.892437	16.843021	-0.058082	3.509802
298.728743	4193.889616	16.848026	-0.058071	3.506526
298.740726	4185.853595	16.853031	-0.058068	3.503235
298.856898	4177.885351	16.858035	-0.058085	3.499972
298.722374	4169.903397	16.863040	-0.058055	3.496693
298.571655	4161.922694	16.868045	-0.058021	3.493410
298.622091	4153.910692	16.873050	-0.058025	3.490118
298.572339	4145.960530	16.878055	-0.058011	3.486845
298.559444	4137.951256	16.883059	-0.058003	3.483545
298.443401	4129.966225	16.888064	-0.057976	3.480249
298.641304	4121.955122	16.893069	-0.058008	3.476950
298.551137	4113.927283	16.898074	-0.057986	3.473631
298.170867	4106.022049	16.903079	-0.057910	3.470350
298.236151	4097.989422	16.908083	-0.057917	3.467028
298.290314	4089.938259	16.913088	-0.057922	3.463694
298.506753	4081.990674	16.918093	-0.057957	3.460406
298.370626	4074.010285	16.923098	-0.057926	3.457089
298.357351	4065.982458	16.928103	-0.057918	3.453754
298.173162	4058.020751	16.933107	-0.057879	3.450437
298.091868	4050.025309	16.938112	-0.057858	3.447106
298.402393	4042.008205	16.943117	-0.057911	3.443776
298.488789	4034.051727	16.948122	-0.057922	3.440461
298.168169	4026.124765	16.953127	-0.057857	3.437141
298.109183	4018.088224	16.958131	-0.057841	3.433781
298.123276	4010.100479	16.963136	-0.057838	3.430440
298.022541	4002.127891	16.968141	-0.057814	3.427099
297.921305	3994.066376	16.973146	-0.057790	3.423716
297.731316	3986.152751	16.978151	-0.057749	3.420390
298.138449	3978.086592	16.983155	-0.057820	3.417017
297.983482	3970.092042	16.988160	-0.057786	3.413651
298.008141	3962.116940	16.993165	-0.057785	3.410297
297.896638	3954.107150	16.998170	-0.057759	3.406919
298.004492	3946.112603	17.003175	-0.057774	3.403553
298.092784	3938.146074	17.008179	-0.057785	3.400194
297.856438	3930.190748	17.013184	-0.057736	3.396825
297.920968	3922.179281	17.018189	-0.057743	3.393440
297.900916	3914.118904	17.023194	-0.057734	3.390028
297.846490	3906.141793	17.028199	-0.057718	3.386646
297.695147	3898.167058	17.033203	-0.057685	3.383258
297.765673	3890.186354	17.038208	-0.057693	3.379873
297.818676	3882.212199	17.043213	-0.057698	3.376486
297.702864	3874.190994	17.048218	-0.057671	3.373070
297.743633	3866.209051	17.053223	-0.057673	3.369672
297.715825	3858.231606	17.058227	-0.057663	3.366271
297.520029	3850.240358	17.063232	-0.057621	3.362854
297.575219	3842.262377	17.068237	-0.057626	3.359448
297.239334	3834.318037	17.073242	-0.057558	3.356039
297.387779	3826.298492	17.078247	-0.057581	3.352613
297.242256	3818.307903	17.083251	-0.057548	3.349184
297.477415	3810.266465	17.088256	-0.057587	3.345744
297.411095	3802.311494	17.093261	-0.057569	3.342326
297.330647	3794.306409	17.098266	-0.057549	3.338883
297.382839	3786.331919	17.103271	-0.057554	3.335454
297.382262	3778.358717	17.108275	-0.057548	3.332021
297.398339	3770.320589	17.113280	-0.057546	3.328556
297.377551	3762.358483	17.118285	-0.057537	3.325120
297.198268	3754.395005	17.123290	-0.057498	3.321673
297.197066	3746.405831	17.128295	-0.057493	3.318218
297.266228	3738.410714	17.133299	-0.057500	3.314759
297.073968	3730.412233	17.138304	-0.057459	3.311286
296.985034	3722.421523	17.143309	-0.057438	3.307816
296.949549	3714.392002	17.148314	-0.057426	3.304328
296.953754	3706.467149	17.153319	-0.057421	3.300883
296.952483	3698.430605	17.158323	-0.057416	3.297386
296.985267	3690.394469	17.163328	-0.057417	3.293886
297.005719	3682.438826	17.168333	-0.057415	3.290418
296.946974	3674.438070	17.173338	-0.057399	3.286923
297.110832	3666.446116	17.178343	-0.057424	3.283437
297.048234	3658.490550	17.183347	-0.057407	3.279954
296.867178	3650.532307	17.188352	-0.057368	3.276461
296.798412	3642.565144	17.193357	-0.057350	3.272966
296.788748	3634.523562	17.198362	-0.057343	3.269436
296.727795	3626.570004	17.203367	-0.057327	3.265939
296.425749	3618.605563	17.208371	-0.057265	3.262423
296.459344	3610.577474	17.213376	-0.057266	3.258890
296.627249	3602.604291	17.218381	-0.057292	3.255382
296.565032	3594.577718	17.223386	-0.057275	3.251838
296.647917	3586.568927	17.228391	-0.057286	3.248304
296.665195	3578.591914	17.233395	-0.057284	3.244777
296.378017	3570.653648	17.238400	-0.057225	3.241250
296.727591	3562.640146	17.243405	-0.057285	3.237713
296.492098	3554.665935	17.248410	-0.057236	3.234166
296.301073	3546.696381	17.253415	-0.057195	3.230618
296.203925	3538.672031	17.258419	-0.057172	3.227046
296.326298	3530.646249	17.263424	-0.057189	3.223478
296.813957	3522.642088	17.268429	-0.057275	3.219932
296.095804	3514.730208	17.273434	-0.057136	3.216371
296.345529	3506.718743	17.278439	-0.057177	3.212804
296.311231	3498.686770	17.283443	-0.057165	3.209211
296.120608	3490.729720	17.288448	-0.057125	3.205641
296.231658	3482.742835	17.293453	-0.057140	3.202067
296.228064	3474.748753	17.298458	-0.057134	3.198480
296.294790	3466.775602	17.303463	-0.057141	3.194902
296.165625	3458.804653	17.308467	-0.057112	3.191312
296.292786	3450.758249	17.313472	-0.057130	3.187696
296.107718	3442.815673	17.318477	-0.057091	3.184108
295.769867	3434.879049	17.323482	-0.057023	3.180513
295.900615	3426.885784	17.328487	-0.057042	3.176908
295.889309	3418.856775	17.333491	-0.057034	3.173277
295.644284	3410.873661	17.338496	-0.056984	3.169652
295.849139	3402.882466	17.343501	-0.057016	3.166039
295.817496	3394.885747	17.348506	-0.057005	3.162409
295.660264	3386.939460	17.353511	-0.056971	3.158792
296.088360	3378.886898	17.358515	-0.057045	3.155149
295.815297	3370.935446	17.363520	-0.056989	3.151517
295.958658	3362.916407	17.368525	-0.057011	3.147868
295.782691	3354.918504	17.373530	-0.056973	3.144209
295.647637	3346.990801	17.378535	-0.056942	3.140581
295.812059	3338.979700	17.383539	-0.056968	3.136924
295.660844	3330.983523	17.388544	-0.056934	3.133255
295.680376	3323.013714	17.393549	-0.056933	3.129602
295.604670	3315.023339	17.398554	-0.056913	3.125930
295.666722	3307.038726	17.403559	-0.056920	3.122263
295.646565	3299.068354	17.408563	-0.056911	3.118595
295.518736	3291.082343	17.413568	-0.056882	3.114910
295.792903	3283.093614	17.418573	-0.056927	3.111238
295.618121	3275.086687	17.423578	-0.056890	3.107533
295.488814	3267.103682	17.428583	-0.056860	3.103836
295.294921	3259.182661	17.433587	-0.056819	3.100161
295.511158	3251.135762	17.438592	-0.056854	3.096442
295.551384	3243.166826	17.443597	-0.056856	3.092746
295.374030	3235.168527	17.448602	-0.056818	3.089022
295.359394	3227.200189	17.453607	-0.056810	3.085315
295.170295	3219.249297	17.458611	-0.056770	3.081604
295.164726	3211.250390	17.463616	-0.056763	3.077874
295.243627	3203.257158	17.468621	-0.056773	3.074147
295.096756	3195.217446	17.473626	-0.056740	3.070383
295.142935	3187.224381	17.478631	-0.056744	3.066645
295.231288	3179.210030	17.483635	-0.056755	3.062894
295.320951	3171.225937	17.488640	-0.056766	3.059153
295.214917	3163.307794	17.493645	-0.056741	3.055429
295.102946	3155.304432	17.498650	-0.056715	3.051661
294.988038	3147.331867	17.503655	-0.056689	3.047901
294.998276	3139.337577	17.508659	-0.056685	3.044133
294.758299	3131.424352	17.513664	-0.056635	3.040387
294.785082	3123.448767	17.518669	-0.056635	3.036619
294.459074	3115.459504	17.523674	-0.056569	3.032823
294.532592	3107.454785	17.528679	-0.056578	3.029034
294.668193	3099.421919	17.533683	-0.056598	3.025231
294.677421	3091.432159	17.538688	-0.056594	3.021436
294.764429	3083.480278	17.543693	-0.056605	3.017659
294.705661	3075.486285	17.548698	-0.056589	3.013850
294.501895	3067.556461	17.553703	-0.056546	3.010060
294.351754	3059.575464	17.558707	-0.056512	3.006242
294.099480	3051.590123	17.563712	-0.056460	3.002413
294.176306	3043.613170	17.568717	-0.056469	2.998599
294.404501	3035.578025	17.573722	-0.056507	2.994761
294.430463	3027.582565	17.578727	-0.056506	2.990926
294.329609	3019.606432	17.583731	-0.056482	2.987089
294.577751	3011.575780	17.588736	-0.056523	2.983239
294.536645	3003.640334	17.593741	-0.056510	2.979415
294.253865	2995.673284	17.598746	-0.056452	2.975558
294.314365	2987.682783	17.603751	-0.056458	2.971703
294.398762	2979.676154	17.608755	-0.056469	2.967836
294.260801	2971.687964	17.613760	-0.056438	2.963961
294.424232	2963.743137	17.618765	-0.056463	2.960118
294.151580	2955.823949	17.623770	-0.056407	2.956260
294.368694	2947.780873	17.628775	-0.056442	2.952362
294.011504	2939.845759	17.633779	-0.056371	2.948481
294.111096	2931.786709	17.638784	-0.056384	2.944559
293.898139	2923.908204	17.643789	-0.056339	2.940703
293.796520	2915.896368	17.648794	-0.056315	2.936782
294.008178	2907.884997	17.653799	-0.056349	2.932874
293.822101	2899.908990	17.658803	-0.056309	2.928956
293.684264	2891.915527	17.663808	-0.056278	2.925027
293.789661	2883.971986	17.668813	-0.056293	2.921130
293.537957	2876.025970	17.673818	-0.056241	2.917208
293.419444	2868.027835	17.678823	-0.056213	2.913262
293.040298	2860.010798	17.683827	-0.056137	2.909287
293.018109	2851.999850	17.688832	-0.056128	2.905328
293.168988	2844.018340	17.693837	-0.056151	2.901389
293.376281	2835.982062	17.698842	-0.056184	2.897420
293.438161	2828.016393	17.703847	-0.056191	2.893473
293.395578	2820.038740	17.708851	-0.056177	2.889509
293.444183	2812.033570	17.713856	-0.056181	2.885531
293.473581	2804.111744	17.718861	-0.056181	2.881587
293.076319	2796.188226	17.723866	-0.056102	2.877614
292.802961	2788.231244	17.728871	-0.056046	2.873625
293.230422	2780.180495	17.733875	-0.056120	2.869623
292.851745	2772.246543	17.738880	-0.056045	2.865628
293.079149	2764.235064	17.743885	-0.056082	2.861624
293.095907	2756.234430	17.748890	-0.056080	2.857607
293.282219	2748.234384	17.753895	-0.056109	2.853594
293.103768	2740.295211	17.758899	-0.056071	2.849586
293.000558	2732.296215	17.763904	-0.056046	2.845546
293.261803	2724.324310	17.768909	-0.056090	2.841535
293.258383	2716.355041	17.773914	-0.056084	2.837505
292.767264	2708.458114	17.778919	-0.055987	2.833477
292.910389	2700.446720	17.783923	-0.056009	2.829422
292.840261	2692.427113	17.788928	-0.055990	2.825345
292.868981	2684.489271	17.793933	-0.055990	2.821309
292.836131	2676.478028	17.798938	-0.055979	2.817226
292.687359	2668.524886	17.803943	-0.055946	2.813160
293.164717	2660.462342	17.808947	-0.056030	2.809070
292.926870	2652.524377	17.813952	-0.055980	2.804995
292.918924	2644.568239	17.818957	-0.055974	2.800918
292.895454	2636.609083	17.823962	-0.055964	2.796833
293.029551	2628.624321	17.828967	-0.055984	2.792738
292.930691	2620.647562	17.833971	-0.055960	2.788627
292.684089	2612.673317	17.838976	-0.055909	2.784503
292.446255	2604.769229	17.843981	-0.055859	2.780409
292.671103	2596.731919	17.848986	-0.055896	2.776268
292.393150	2588.785641	17.853991	-0.055839	2.772138
292.545520	2580.789710	17.858995	-0.055862	2.768002
292.451087	2572.798185	17.864000	-0.055839	2.763847
292.356329	2564.876963	17.869005	-0.055816	2.759722
292.394865	2556.881728	17.874010	-0.055818	2.755561
292.448835	2548.848264	17.879015	-0.055823	2.751374
292.248764	2540.873366	17.884019	-0.055781	2.747196
292.173400	2532.897629	17.889024	-0.055761	2.743019
292.267286	2524.941850	17.894029	-0.055774	2.738856
292.162994	2516.945131	17.899034	-0.055749	2.734653
292.335242	2508.943651	17.904039	-0.055776	2.730459
292.315435	2500.993419	17.909043	-0.055767	2.726273
292.234405	2493.019569	17.914048	-0.055747	2.722064
292.172210	2485.091277	17.919053	-0.055730	2.717874
292.147630	2477.112306	17.924058	-0.055720	2.713653
292.327186	2469.096365	17.929063	-0.055748	2.709419
292.107381	2461.168217	17.934067	-0.055702	2.705199
292.155238	2453.167284	17.939072	-0.055706	2.700952
292.476675	2445.183809	17.944077	-0.055760	2.696724
292.350751	2437.207345	17.949082	-0.055732	2.692465
292.427080	2429.237647	17.954087	-0.055741	2.688215
292.179307	2421.291439	17.959091	-0.055689	2.683951
292.060506	2413.353316	17.964096	-0.055662	2.679692
291.968116	2405.414178	17.969101	-0.055640	2.675428
291.954233	2397.417740	17.974106	-0.055632	2.671131
291.951254	2389.420081	17.979111	-0.055626	2.666827
291.933253	2381.440072	17.984115	-0.055617	2.662525
291.968875	2373.439207	17.989120	-0.055619	2.658208
291.627624	2365.545665	17.994125	-0.055550	2.653917
291.594032	2357.536665	17.999130	-0.055539	2.649577
291.656656	2349.538103	18.004135	-0.055545	2.645243
291.938368	2341.564511	18.009139	-0.055592	2.640929
291.909661	2333.589561	18.014144	-0.055582	2.636586
291.902592	2325.629937	18.019149	-0.055575	2.632247
291.857642	2317.647595	18.024154	-0.055561	2.627885
291.880631	2309.700572	18.029159	-0.055561	2.623540
291.430176	2301.809858	18.034163	-0.055472	2.619186
291.537423	2293.801695	18.039168	-0.055486	2.614798
291.654061	2285.805162	18.044173	-0.055503	2.610410
291.356165	2277.860393	18.049178	-0.055442	2.606015
291.383900	2269.882361	18.054183	-0.055442	2.601616
291.524191	2261.916909	18.059187	-0.055463	2.597225
291.480799	2253.900903	18.064192	-0.055450	2.592786
291.518877	2245.856859	18.069197	-0.055451	2.588329
291.204467	2237.922303	18.074202	-0.055388	2.583900
291.342616	2229.954906	18.079207	-0.055408	2.579478
291.291502	2222.004366	18.084211	-0.055393	2.575043
291.221769	2214.036663	18.089216	-0.055375	2.570591
291.359891	2206.062232	18.094221	-0.055396	2.566141
291.241701	2198.121652	18.099226	-0.055368	2.561685
291.102710	2190.188438	18.104231	-0.055337	2.557223
291.129691	2182.208551	18.109235	-0.055337	2.552739
290.855626	2174.288927	18.114240	-0.055281	2.548260
290.945477	2166.280921	18.119245	-0.055292	2.543749
290.797790	2158.332164	18.124250	-0.055260	2.539246
290.921665	2150.341482	18.129255	-0.055277	2.534731
290.910017	2142.372771	18.134259	-0.055270	2.530211
290.729520	2134.411789	18.139264	-0.055231	2.525675
290.773985	2126.481663	18.144269	-0.055234	2.521164
290.786733	2118.511262	18.149274	-0.055231	2.516621
290.348747	2110.613593	18.154279	-0.055145	2.512077
290.576885	2102.572166	18.159283	-0.055182	2.507492
290.422118	2094.602906	18.164288	-0.055148	2.502912
290.779720	2086.601247	18.169293	-0.055209	2.498342
290.569598	2078.661099	18.174298	-0.055165	2.493758
290.465218	2070.704573	18.179303	-0.055140	2.489163
290.488674	2062.736377	18.184307	-0.055139	2.484563
290.295041	2054.823442	18.189312	-0.055098	2.479969
290.328506	2046.869706	18.194317	-0.055099	2.475361
290.115207	2038.909420	18.199322	-0.055054	2.470722
289.955337	2030.953442	18.204327	-0.055019	2.466080
290.322509	2022.911891	18.209331	-0.055082	2.461420
289.949308	2015.015194	18.214336	-0.055008	2.456779
290.348673	2007.005315	18.219341	-0.055077	2.452123
290.234546	1999.041542	18.224346	-0.055050	2.447445
290.240819	1991.080045	18.229351	-0.055046	2.442768
290.276341	1983.167532	18.234355	-0.055048	2.438114
289.881756	1975.242555	18.239360	-0.054969	2.433410
290.119130	1967.189756	18.244365	-0.055008	2.428671
290.106673	1959.212641	18.249370	-0.055000	2.423948
289.851926	1951.297571	18.254375	-0.054948	2.419233
290.060029	1943.321600	18.259379	-0.054981	2.414509
290.017877	1935.348197	18.264384	-0.054968	2.409758
289.990477	1927.403983	18.269389	-0.054958	2.405016
289.801966	1919.494438	18.274394	-0.054918	2.400273
290.099748	1911.495517	18.279399	-0.054968	2.395505
289.818595	1903.595096	18.284403	-0.054910	2.390741
289.809720	1895.597441	18.289408	-0.054903	2.385930
289.879336	1887.652166	18.294413	-0.054911	2.381148
289.625865	1879.724589	18.299418	-0.054859	2.376340
289.742376	1871.726839	18.304423	-0.054875	2.371511
289.633067	1863.793879	18.309427	-0.054850	2.366692
289.342093	1855.884832	18.314432	-0.054790	2.361863
289.296952	1847.956964	18.319437	-0.054777	2.357033
289.219473	1839.971542	18.324442	-0.054757	2.352155
289.411172	1831.951780	18.329447	-0.054787	2.347269
289.331114	1824.029936	18.334451	-0.054767	2.342409
288.941139	1816.112793	18.339456	-0.054689	2.337517
288.936000	1808.155532	18.344461	-0.054683	2.332621
289.300341	1800.114782	18.349466	-0.054746	2.327695
289.295798	1792.159563	18.354471	-0.054740	2.322781
289.005386	1784.284618	18.359475	-0.054681	2.317881
289.125828	1776.294090	18.364480	-0.054698	2.312934
289.137566	1768.358108	18.369485	-0.054695	2.308001
288.706007	1760.450406	18.374490	-0.054609	2.303038
288.706419	1752.486637	18.379495	-0.054604	2.298065
288.724173	1744.538191	18.384499	-0.054602	2.293093
288.650101	1736.560250	18.389504	-0.054583	2.288084
288.961275	1728.567477	18.394509	-0.054636	2.283088
288.954974	1720.642996	18.399514	-0.054629	2.278096
288.492770	1712.748146	18.404519	-0.054538	2.273072
288.424590	1704.778473	18.409523	-0.054520	2.268024
288.768071	1696.732032	18.414528	-0.054579	2.262952
288.968104	1688.786223	18.419533	-0.054611	2.257921
288.758140	1680.860713	18.424538	-0.054567	2.252854
288.527690	1672.957742	18.429543	-0.054519	2.247789
288.552940	1665.000805	18.434547	-0.054518	2.242701
288.587107	1657.048971	18.439552	-0.054519	2.237605
288.641606	1649.126181	18.444557	-0.054524	2.232518
288.594074	1641.162663	18.449562	-0.054510	2.227384
288.486962	1633.215781	18.454567	-0.054485	2.222243
288.389729	1625.305470	18.459571	-0.054462	2.217115
288.495405	1617.327136	18.464576	-0.054476	2.211949
288.275760	1609.443140	18.469581	-0.054430	2.206803
288.378787	1601.465660	18.474586	-0.054444	2.201614
288.368619	1593.523444	18.479591	-0.054437	2.196425
288.248587	1585.607509	18.484595	-0.054409	2.191230
288.373455	1577.602389	18.489600	-0.054427	2.185988
288.285616	1569.695263	18.494605	-0.054406	2.180777
288.320981	1561.745287	18.499610	-0.054407	2.175538
288.160393	1553.822379	18.504615	-0.054372	2.170285
287.996075	1545.894582	18.509619	-0.054336	2.165015
287.868631	1537.978087	18.514624	-0.054307	2.159744
288.006825	1530.027895	18.519629	-0.054328	2.154463
288.012444	1522.066146	18.524634	-0.054324	2.149148
288.093082	1514.107917	18.529639	-0.054334	2.143830
288.071978	1506.198887	18.534643	-0.054324	2.138522
288.063807	1498.247123	18.539648	-0.054318	2.133173
287.782063	1490.358275	18.544653	-0.054260	2.127827
287.776567	1482.405899	18.549658	-0.054254	2.122451
287.969754	1474.455001	18.554663	-0.054285	2.117081
287.963173	1466.513382	18.559667	-0.054278	2.111685
287.925321	1458.531128	18.564672	-0.054266	2.106244
287.903594	1450.605514	18.569677	-0.054257	2.100830
287.916617	1442.683884	18.574682	-0.054254	2.095407
287.685991	1434.786001	18.579687	-0.054206	2.089962
287.795029	1426.835257	18.584691	-0.054221	2.084501
287.650540	1418.930780	18.589696	-0.054189	2.079032
287.691760	1410.999732	18.594701	-0.054191	2.073549
287.777119	1403.039991	18.599706	-0.054202	2.068036
287.690865	1395.121864	18.604711	-0.054181	2.062519
287.568970	1387.229307	18.609715	-0.054153	2.057002
287.494525	1379.297736	18.614720	-0.054134	2.051448
287.459487	1371.365202	18.619725	-0.054122	2.045882
287.356148	1363.455465	18.624730	-0.054097	2.040310
287.276590	1355.540222	18.629735	-0.054077	2.034721
287.351107	1347.601929	18.634739	-0.054086	2.029116
287.455802	1339.634401	18.639744	-0.054100	2.023478
287.238492	1331.756888	18.644749	-0.054055	2.017855
287.237344	1323.827187	18.649754	-0.054049	2.012202
287.218090	1315.883409	18.654759	-0.054041	2.006520
287.334129	1307.945894	18.659763	-0.054057	2.000841
287.045759	1300.078709	18.664768	-0.053998	1.995154
287.213484	1292.127185	18.669773	-0.054024	1.989438
286.954754	1284.234912	18.674778	-0.053971	1.983703
286.852757	1276.345850	18.679783	-0.053947	1.977970
286.824928	1268.411811	18.684787	-0.053936	1.972196
287.013049	1260.441472	18.689792	-0.053966	1.966403
286.787815	1252.574843	18.694797	-0.053919	1.960622
286.617320	1244.690413	18.699802	-0.053882	1.954818
286.683869	1236.745535	18.704807	-0.053889	1.948978
286.687611	1228.811050	18.709811	-0.053885	1.943120
286.622431	1220.889808	18.714816	-0.053867	1.937248
286.652571	1212.973163	18.719821	-0.053868	1.931371
286.514553	1205.061231	18.724826	-0.053837	1.925462
286.455456	1197.168597	18.729831	-0.053821	1.919557
286.638220	1189.231339	18.734835	-0.053850	1.913628
286.649271	1181.296901	18.739840	-0.053846	1.907663
286.514246	1173.428257	18.744845	-0.053816	1.901713
286.383220	1165.524595	18.749850	-0.053786	1.895718
286.264044	1157.618746	18.754855	-0.053759	1.889703
286.241310	1149.726070	18.759859	-0.053750	1.883690
286.090943	1141.839530	18.764864	-0.053717	1.877648
286.253586	1133.917545	18.769869	-0.053742	1.871596
286.047868	1126.021714	18.774874	-0.053698	1.865501
286.023593	1118.112675	18.779879	-0.053688	1.859397
285.944793	1110.228100	18.784883	-0.053669	1.853285
285.618358	1102.345639	18.789888	-0.053603	1.847126
285.809422	1094.417420	18.794893	-0.053633	1.840972
285.869731	1086.511341	18.799898	-0.053639	1.834799
285.812034	1078.615422	18.804903	-0.053623	1.828599
285.555723	1070.765512	18.809907	-0.053570	1.822390
285.545597	1062.848794	18.814912	-0.053563	1.816136
285.596646	1054.946091	18.819917	-0.053568	1.809880
285.507197	1047.064986	18.824922	-0.053546	1.803602
285.565233	1039.172044	18.829927	-0.053551	1.797311
285.511320	1031.272873	18.834931	-0.053536	1.790979
285.422687	1023.353144	18.839936	-0.053514	1.784603
285.412238	1015.476031	18.844941	-0.053507	1.778249
285.259763	1007.607817	18.849946	-0.053474	1.771861
285.396418	999.678378	18.854951	-0.053494	1.765437
285.393534	991.817997	18.859955	-0.053488	1.759028
284.985735	984.000722	18.864960	-0.053407	1.752579
285.322695	976.043174	18.869965	-0.053465	1.746087
285.189494	968.184912	18.874970	-0.053435	1.739592
285.144823	960.309766	18.879975	-0.053421	1.733070
285.026663	952.457818	18.884979	-0.053394	1.726532
285.127899	944.550255	18.889984	-0.053408	1.719953
284.901110	936.753794	18.894989	-0.053360	1.713398
284.989196	928.831138	18.899994	-0.053372	1.706753
284.828036	920.974005	18.904999	-0.053337	1.700104
284.990777	913.084078	18.910003	-0.053362	1.693445
284.706633	905.237189	18.915008	-0.053304	1.686736
284.492685	897.417356	18.920013	-0.053259	1.680033
284.643435	889.532371	18.925018	-0.053282	1.673297
284.539570	881.653178	18.930023	-0.053257	1.666503
284.452676	873.798223	18.935027	-0.053236	1.659705
284.478546	865.933781	18.940032	-0.053235	1.652887
284.794833	858.021868	18.945037	-0.053289	1.646039
284.557941	850.215275	18.950042	-0.053240	1.639177
284.412303	842.369658	18.955047	-0.053208	1.632265
284.437793	834.479248	18.960051	-0.053207	1.625309
284.371185	826.629039	18.965056	-0.053190	1.618344
284.421227	818.767268	18.970061	-0.053194	1.611357
284.367493	810.921655	18.975066	-0.053179	1.604338
284.278215	803.103762	18.980071	-0.053157	1.597308
284.203142	795.269641	18.985075	-0.053138	1.590235
284.365985	787.387944	18.990080	-0.053163	1.583121
284.304261	779.571887	18.995085	-0.053146	1.576002
284.097784	771.758140	19.000090	-0.053103	1.568832
284.165399	763.905493	19.005095	-0.053110	1.561633
284.277045	756.077699	19.010099	-0.053126	1.554431
283.983195	748.279373	19.015104	-0.053066	1.547162
283.964407	740.449473	19.020109	-0.053057	1.539870
284.115317	732.586518	19.025114	-0.053080	1.532539
283.701349	724.817509	19.030119	-0.052998	1.525174
283.727195	717.012359	19.035123	-0.052998	1.517807
283.736058	709.164233	19.040128	-0.052994	1.510361
283.806317	701.342217	19.045133	-0.053002	1.502912
283.826030	693.522559	19.050138	-0.053001	1.495420
283.696028	685.723180	19.055143	-0.052971	1.487887
283.694108	677.924329	19.060147	-0.052966	1.480336
283.364146	670.166417	19.065152	-0.052899	1.472734
283.409736	662.311655	19.070157	-0.052903	1.465058
283.702923	654.465362	19.075162	-0.052952	1.457389
283.593928	646.674527	19.080167	-0.052927	1.449670
283.343465	638.935244	19.085171	-0.052875	1.441938
283.215198	631.164048	19.090176	-0.052846	1.434151
283.407798	623.336010	19.095181	-0.052877	1.426319
283.170580	615.592497	19.100186	-0.052828	1.418457
283.253617	607.787371	19.105191	-0.052838	1.410542
283.235570	600.022634	19.110195	-0.052829	1.402607
283.074864	592.275593	19.115200	-0.052794	1.394620
283.070968	584.494809	19.120205	-0.052789	1.386580
282.990513	576.738533	19.125210	-0.052769	1.378505
282.990293	568.962940	19.130215	-0.052763	1.370375
283.034496	561.204919	19.135219	-0.052767	1.362224
282.826732	553.481982	19.140224	-0.052723	1.354016
282.933140	545.706240	19.145229	-0.052738	1.345758
282.742960	537.996721	19.150234	-0.052697	1.337467
282.596885	530.261096	19.155239	-0.052665	1.329104
282.924549	522.474472	19.160243	-0.052721	1.320718
282.668529	514.758757	19.165248	-0.052668	1.312250
282.594951	506.983765	19.170253	-0.052649	1.303694
282.368684	499.292635	19.175258	-0.052602	1.295147
282.242824	491.582403	19.180263	-0.052573	1.286541
282.181473	483.891927	19.185267	-0.052557	1.277910
282.157128	476.167851	19.190272	-0.052547	1.269191
282.270541	468.448760	19.195277	-0.052563	1.260443
282.035360	460.797118	19.200282	-0.052515	1.251643
282.108574	453.081430	19.205287	-0.052523	1.242768
281.884700	445.447502	19.210291	-0.052477	1.233865
281.780488	437.757480	19.215296	-0.052452	1.224856
281.582860	430.117626	19.220301	-0.052410	1.215820
281.690184	422.416749	19.225306	-0.052425	1.206706
281.813547	414.729289	19.230311	-0.052443	1.197541
281.889655	407.070091	19.235315	-0.052452	1.188331
281.712039	399.446133	19.240320	-0.052414	1.179038
281.198475	391.898996	19.245325	-0.052314	1.169696
281.741870	384.160843	19.250330	-0.052410	1.160266
281.542188	376.561343	19.255335	-0.052368	1.150772
281.424761	368.949166	19.260339	-0.052341	1.141202
281.428903	361.327233	19.265344	-0.052336	1.131564
281.384819	353.733264	19.270349	-0.052323	1.121869
281.559230	346.117112	19.275354	-0.052351	1.112109
281.344977	338.563742	19.280359	-0.052306	1.102258
281.215411	331.021504	19.285363	-0.052277	1.092351
280.983655	323.484073	19.290368	-0.052229	1.082337
280.975210	315.940073	19.295373	-0.052222	1.072272
280.931269	308.387979	19.300378	-0.052209	1.062092
280.886940	300.849302	19.305383	-0.052196	1.051832
281.042857	293.299690	19.310387	-0.052220	1.041504
281.001157	285.803285	19.315392	-0.052207	1.031098
280.551260	278.389417	19.320397	-0.052119	1.020603
280.646328	270.874536	19.325402	-0.052131	1.009990
280.486430	263.427964	19.330407	-0.052097	0.999298
280.459573	255.949659	19.335411	-0.052087	0.988478
280.425342	248.482602	19.340416	-0.052076	0.977554
280.271702	241.074483	19.345421	-0.052042	0.966562
280.358461	233.642983	19.350426	-0.052053	0.955471
280.176951	226.263524	19.355431	-0.052015	0.944259
280.245888	218.863957	19.360435	-0.052023	0.932948
279.958608	211.538684	19.365440	-0.051964	0.921516
279.892498	204.205086	19.370445	-0.051947	0.909989
279.851825	196.864462	19.375450	-0.051935	0.898310
280.153005	189.488926	19.380455	-0.051986	0.886518
279.751049	182.285153	19.385459	-0.051907	0.874646
279.281811	175.082812	19.390464	-0.051814	0.862593
279.476671	167.791599	19.395469	-0.051846	0.850417
279.092218	160.639831	19.400474	-0.051770	0.838127
279.001830	153.423689	19.405479	-0.051748	0.825633
279.188744	146.202100	19.410483	-0.051778	0.813024
279.047673	139.065066	19.415488	-0.051747	0.800264
279.103770	131.928515	19.420493	-0.051753	0.787361
279.281202	124.803574	19.425498	-0.051781	0.774306
279.212826	117.750772	19.430503	-0.051764	0.761080
279.363820	110.701971	19.435507	-0.051788	0.747703
279.088001	103.755109	19.440512	-0.051732	0.734133
279.111219	96.798070	19.445517	-0.051731	0.720393
279.014980	89.898640	19.450522	-0.051709	0.706459
278.772094	83.063521	19.455527	-0.051659	0.692325
278.923142	76.381251	19.460531	-0.051683	0.678369