Fri Apr 16 18:53:45 2021

Number of Points = 3631
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.553717	0.090123	0.000000	0.000064	0.311216

3.437589	0.150789	0.005005	0.000086	0.311400
3.565995	0.124094	0.010010	0.000062	0.311384
3.738457	0.090655	0.015014	0.000030	0.311375
3.651670	0.064116	0.020019	0.000046	0.311178
3.607780	0.049357	0.025024	0.000054	0.311072
3.871111	0.000975	0.030029	0.000005	0.311070
3.608685	0.050576	0.035034	0.000054	0.311078
3.610574	0.049588	0.040038	0.000053	0.311075
3.510965	0.068945	0.045043	0.000072	0.311081
3.558550	0.058997	0.050048	0.000063	0.311075
3.358294	0.098783	0.055053	0.000100	0.311091
3.476400	0.075091	0.060058	0.000078	0.311080
3.612708	0.049338	0.065062	0.000053	0.311076
3.491088	0.073840	0.070067	0.000076	0.311087
3.534838	0.062847	0.075072	0.000068	0.311073
3.426304	0.085147	0.080077	0.000088	0.311084
3.234690	0.120624	0.085082	0.000124	0.311088
3.225084	0.112176	0.090086	0.000125	0.311040
3.388601	0.025955	0.095091	0.000095	0.310777
2.469007	0.197987	0.100096	0.000266	0.310800
2.831610	0.130917	0.105101	0.000199	0.310794
2.939763	0.110208	0.110106	0.000179	0.310789
2.763858	0.142940	0.115110	0.000211	0.310793
3.176239	0.066167	0.120115	0.000135	0.310784
3.160153	0.065897	0.125120	0.000138	0.310769
3.389534	0.009344	0.130125	0.000095	0.310700
3.450451	-0.041049	0.135130	0.000084	0.310517
3.449917	-0.042123	0.140134	0.000084	0.310511
3.463760	-0.043272	0.145139	0.000081	0.310518
3.431866	-0.040340	0.150144	0.000087	0.310504
3.477932	-0.078907	0.155149	0.000079	0.310363
3.257338	-0.079613	0.160154	0.000120	0.310173
3.154240	-0.060675	0.165158	0.000139	0.310174
3.292784	-0.083666	0.170163	0.000113	0.310184
3.467397	-0.132739	0.175168	0.000081	0.310103
3.649216	-0.219713	0.180173	0.000047	0.309851
3.652853	-0.220385	0.185178	0.000046	0.309851
3.742683	-0.237924	0.190182	0.000029	0.309845
3.664343	-0.275386	0.195187	0.000044	0.309604
3.409234	-0.246699	0.200192	0.000092	0.309521
3.514370	-0.264284	0.205197	0.000072	0.309528
3.154398	-0.224849	0.210202	0.000139	0.309407
3.337653	-0.293790	0.215206	0.000105	0.309240
3.049886	-0.238251	0.220211	0.000159	0.309255
3.301203	-0.308351	0.225216	0.000112	0.309141
3.382635	-0.374316	0.230221	0.000097	0.308901
3.390123	-0.376850	0.235226	0.000095	0.308896
3.254780	-0.380126	0.240230	0.000121	0.308765
3.343516	-0.433265	0.245235	0.000104	0.308591
3.122487	-0.392251	0.250240	0.000145	0.308595
3.232348	-0.457393	0.255245	0.000125	0.308383
3.262697	-0.485099	0.260250	0.000119	0.308279
3.421630	-0.522700	0.265254	0.000090	0.308238
3.445390	-0.580418	0.270259	0.000085	0.307987
3.371076	-0.568629	0.275264	0.000099	0.307979
2.785726	-0.508605	0.280269	0.000208	0.307761
3.129542	-0.597384	0.285274	0.000144	0.307638
3.472437	-0.681260	0.290278	0.000080	0.307536
3.508934	-0.732549	0.295283	0.000074	0.307326
3.266394	-0.698293	0.300288	0.000119	0.307280
3.504441	-0.802120	0.305293	0.000075	0.306994
3.334280	-0.771602	0.310298	0.000106	0.306992
3.555323	-0.872917	0.315302	0.000065	0.306704
3.743011	-0.905839	0.320307	0.000030	0.306709
3.603751	-0.951999	0.325312	0.000056	0.306372
3.209810	-0.880148	0.330317	0.000130	0.306373
2.590280	-0.828249	0.335322	0.000245	0.306086
2.572080	-0.825006	0.340326	0.000248	0.306086
2.516629	-0.875005	0.345331	0.000259	0.305802
2.658434	-0.910816	0.350336	0.000232	0.305754
2.747553	-0.974197	0.355341	0.000216	0.305531
2.722687	-0.976941	0.360346	0.000220	0.305496
3.111580	-1.115002	0.365350	0.000148	0.305177
3.433828	-1.188742	0.370355	0.000088	0.305105
3.239264	-1.212608	0.375360	0.000124	0.304824
3.333776	-1.256267	0.380365	0.000107	0.304698
3.069411	-1.247549	0.385370	0.000156	0.304511
2.812891	-1.240541	0.390374	0.000204	0.304323
3.404661	-1.370518	0.395379	0.000094	0.304216
3.020840	-1.371858	0.400384	0.000165	0.303878
2.868768	-1.363190	0.405389	0.000194	0.303788
2.879394	-1.409160	0.410394	0.000192	0.303578
2.708210	-1.425011	0.415398	0.000224	0.303354
2.708995	-1.447301	0.420403	0.000223	0.303248
2.571200	-1.483249	0.425408	0.000249	0.302957
2.415489	-1.479277	0.430413	0.000278	0.302841
2.714657	-1.579433	0.435418	0.000222	0.302622
2.466663	-1.586808	0.440422	0.000269	0.302371
2.520852	-1.622079	0.445427	0.000259	0.302249
2.633544	-1.698698	0.450432	0.000238	0.301980
2.517217	-1.717606	0.455437	0.000259	0.301788
2.460674	-1.738168	0.460442	0.000270	0.301640
2.579327	-1.817143	0.465446	0.000248	0.301365
2.459806	-1.838712	0.470451	0.000270	0.301157
1.920203	-1.772620	0.475456	0.000371	0.301003
2.051854	-1.850522	0.480461	0.000346	0.300743
2.186669	-1.908213	0.485466	0.000321	0.300583
2.091019	-1.923473	0.490470	0.000339	0.300426
1.730168	-1.910043	0.495475	0.000406	0.300175
1.578094	-1.934656	0.500480	0.000435	0.299923
1.783353	-2.004485	0.505485	0.000396	0.299766
2.100461	-2.112365	0.510490	0.000337	0.299523
2.322923	-2.207358	0.515494	0.000296	0.299259
2.667685	-2.313827	0.520499	0.000232	0.299047
2.174018	-2.273084	0.525504	0.000324	0.298810
2.194778	-2.324973	0.530509	0.000320	0.298577
2.190938	-2.384407	0.535514	0.000321	0.298286
1.792979	-2.354689	0.540518	0.000395	0.298079
1.028882	-2.253045	0.545523	0.000537	0.297898
0.615878	-2.234291	0.550528	0.000614	0.297624
0.745091	-2.304628	0.555533	0.000590	0.297396
0.143900	-2.230234	0.560538	0.000702	0.297227
0.110857	-2.273417	0.565542	0.000708	0.296987
0.172644	-2.332906	0.570547	0.000697	0.296752
-0.602927	-2.225821	0.575552	0.000841	0.296586
-0.812995	-2.228604	0.580557	0.000880	0.296386
-0.667213	-2.307751	0.585562	0.000853	0.296129
-0.943981	-2.290549	0.590566	0.000905	0.295967
-1.433329	-2.243139	0.595571	0.000996	0.295764
-1.605082	-2.251611	0.600576	0.001028	0.295570
-1.942823	-2.209180	0.605581	0.001091	0.295477
-2.003789	-2.260995	0.610586	0.001102	0.295169
-2.017303	-2.294249	0.615590	0.001105	0.294994
-2.013529	-2.324741	0.620595	0.001104	0.294847
-2.600163	-2.281320	0.625600	0.001213	0.294537
-2.613646	-2.299163	0.630605	0.001216	0.294437
-2.350568	-2.391209	0.635610	0.001167	0.294220
-2.647923	-2.384598	0.640614	0.001222	0.293986
-3.164497	-2.312988	0.645619	0.001318	0.293876
-3.398522	-2.333304	0.650624	0.001362	0.293567
-3.215778	-2.387112	0.655629	0.001328	0.293465
-3.909048	-2.303889	0.660634	0.001457	0.293254
-4.315727	-2.265895	0.665638	0.001533	0.293076
-4.494751	-2.253653	0.670643	0.001566	0.292976
-4.730903	-2.268786	0.675648	0.001610	0.292689
-4.773648	-2.273665	0.680653	0.001618	0.292627
-5.054025	-2.284421	0.685658	0.001670	0.292321
-5.111198	-2.285937	0.690662	0.001681	0.292262
-5.622173	-2.247710	0.695667	0.001776	0.291991
-5.689849	-2.250152	0.700672	0.001789	0.291918
-5.602108	-2.310750	0.705677	0.001772	0.291697
-5.791201	-2.299895	0.710682	0.001808	0.291580
-6.293584	-2.253840	0.715686	0.001901	0.291355
-6.321594	-2.269870	0.720691	0.001906	0.291250
-6.796556	-2.221402	0.725696	0.001995	0.291062
-6.580812	-2.287176	0.730701	0.001955	0.290930
-6.804983	-2.284027	0.735706	0.001996	0.290742
-7.296047	-2.214274	0.740710	0.002088	0.290645
-7.518559	-2.202314	0.745715	0.002129	0.290503
-7.723768	-2.188066	0.750720	0.002167	0.290388
-7.655713	-2.247835	0.755725	0.002155	0.290152
-7.761350	-2.246309	0.760730	0.002175	0.290064
-8.279335	-2.200265	0.765734	0.002271	0.289823
-7.940309	-2.269543	0.770739	0.002208	0.289785
-8.394877	-2.245028	0.775744	0.002293	0.289495
-8.548454	-2.216490	0.780749	0.002321	0.289498
-8.484553	-2.284876	0.785754	0.002309	0.289214
-8.528196	-2.278465	0.790758	0.002317	0.289206
-8.763270	-2.298329	0.795763	0.002361	0.288893
-9.080959	-2.245688	0.800768	0.002420	0.288867
-9.029505	-2.303979	0.805773	0.002411	0.288622
-9.399851	-2.248032	0.810778	0.002480	0.288564
-9.827670	-2.214556	0.815782	0.002559	0.288342
-9.765859	-2.245240	0.820787	0.002548	0.288244
-9.984137	-2.232295	0.825792	0.002589	0.288110
-10.161289	-2.230851	0.830797	0.002622	0.287955
-9.934889	-2.287197	0.835802	0.002579	0.287879
-10.534376	-2.232072	0.840806	0.002691	0.287608
-10.436406	-2.249570	0.845811	0.002673	0.287609
-10.754872	-2.253664	0.850816	0.002732	0.287297
-10.486291	-2.303035	0.855821	0.002682	0.287295
-11.142337	-2.230195	0.860826	0.002804	0.287060
-11.734364	-2.139228	0.865830	0.002915	0.286976
-11.817210	-2.137530	0.870835	0.002930	0.286909
-12.438041	-2.063997	0.875840	0.003046	0.286710
-12.188936	-2.110186	0.880845	0.002999	0.286706
-12.099023	-2.174176	0.885850	0.002983	0.286465
-12.601569	-2.102348	0.890854	0.003076	0.286366
-12.681329	-2.095222	0.895859	0.003091	0.286329
-12.996098	-2.090699	0.900864	0.003150	0.286062
-12.758150	-2.132652	0.905869	0.003105	0.286069
-13.140974	-2.095090	0.910874	0.003177	0.285907
-13.274003	-2.104349	0.915878	0.003201	0.285737
-12.984251	-2.154551	0.920883	0.003147	0.285750
-13.656883	-2.080909	0.925888	0.003273	0.285503
-13.660022	-2.082595	0.930893	0.003273	0.285492
-13.673410	-2.097240	0.935898	0.003276	0.285405
-13.814472	-2.122561	0.940902	0.003302	0.285146
-14.276289	-2.034979	0.945907	0.003388	0.285165
-14.376272	-2.060191	0.950912	0.003407	0.284944
-14.322038	-2.091391	0.955917	0.003397	0.284836
-14.675898	-2.024269	0.960922	0.003462	0.284850
-15.227080	-1.984761	0.965926	0.003565	0.284541
-14.992988	-2.030752	0.970931	0.003522	0.284524
-15.093542	-2.018247	0.975936	0.003540	0.284494
-15.467681	-2.001325	0.980941	0.003610	0.284234
-15.307864	-2.031613	0.985946	0.003580	0.284228
-15.128022	-2.087082	0.990950	0.003547	0.284111
-15.240812	-2.111606	0.995955	0.003568	0.283882
-15.531433	-2.060269	1.000960	0.003622	0.283874
-15.378135	-2.125486	1.005965	0.003593	0.283684
-15.692547	-2.090246	1.010970	0.003652	0.283572
-16.007705	-2.032744	1.015974	0.003711	0.283573
-16.468338	-2.006496	1.020979	0.003796	0.283279
-16.498302	-2.004841	1.025984	0.003802	0.283259
-16.235143	-2.064116	1.030989	0.003753	0.283201
-16.819819	-2.001889	1.035994	0.003862	0.282975
-16.994991	-1.969442	1.040998	0.003894	0.282978
-16.869482	-2.012423	1.046003	0.003871	0.282875
-17.705922	-1.907820	1.051008	0.004027	0.282632
-16.754347	-2.083701	1.056013	0.003850	0.282617
-16.567463	-2.146818	1.061018	0.003815	0.282468
-17.297636	-2.048180	1.066022	0.003951	0.282293
-17.043736	-2.090982	1.071027	0.003904	0.282310
-17.340367	-2.090791	1.076032	0.003959	0.282034
-18.127160	-1.955072	1.081037	0.004105	0.281997
-18.248462	-1.931474	1.086042	0.004128	0.282005
-17.869349	-2.057963	1.091046	0.004057	0.281709
-17.881334	-2.058349	1.096051	0.004060	0.281696
-18.049374	-2.046323	1.101056	0.004091	0.281600
-17.929831	-2.115579	1.106061	0.004069	0.281356
-17.939285	-2.113095	1.111066	0.004071	0.281360
-18.829418	-1.990066	1.116070	0.004236	0.281160
-18.885889	-1.999241	1.121075	0.004247	0.281060
-18.624763	-2.048397	1.126080	0.004198	0.281051
-18.546976	-2.113105	1.131085	0.004184	0.280790
-19.280251	-1.988859	1.136090	0.004320	0.280743
-18.995905	-2.049609	1.141094	0.004267	0.280697
-19.067153	-2.073537	1.146099	0.004281	0.280506
-19.253826	-2.042703	1.151104	0.004315	0.280490
-19.255759	-2.072610	1.156109	0.004316	0.280334
-19.605241	-2.042091	1.161114	0.004381	0.280163
-19.445386	-2.073799	1.166118	0.004351	0.280150
-19.533339	-2.106121	1.171123	0.004368	0.279900
-19.627564	-2.101641	1.176128	0.004385	0.279834
-19.556147	-2.131961	1.181133	0.004372	0.279744
-20.294885	-2.041079	1.186138	0.004509	0.279519
-20.580453	-1.989074	1.191142	0.004563	0.279520
-20.264596	-2.074111	1.196147	0.004504	0.279377
-20.969620	-1.974962	1.201152	0.004635	0.279226
-20.518116	-2.056080	1.206157	0.004551	0.279231
-20.782625	-2.058894	1.211162	0.004600	0.278967
-21.139559	-2.008192	1.216166	0.004667	0.278893
-21.042361	-2.029532	1.221171	0.004649	0.278874
-20.921313	-2.109722	1.226176	0.004626	0.278572
-20.793055	-2.133436	1.231181	0.004602	0.278570
-21.260171	-2.079142	1.236186	0.004689	0.278410
-21.706034	-2.028728	1.241190	0.004772	0.278251
-20.905231	-2.174587	1.246195	0.004623	0.278249
-21.796383	-2.065422	1.251200	0.004789	0.277974
-21.615330	-2.101871	1.256205	0.004755	0.277956
-21.179036	-2.204926	1.261210	0.004674	0.277832
-22.106453	-2.077096	1.266214	0.004847	0.277619
-22.254651	-2.047136	1.271219	0.004875	0.277635
-22.270406	-2.094964	1.276224	0.004877	0.277370
-22.445781	-2.075570	1.281229	0.004910	0.277305
-22.659169	-2.042874	1.286234	0.004950	0.277273
-22.738827	-2.083652	1.291238	0.004965	0.276984
-22.726756	-2.083895	1.296243	0.004963	0.276994
-23.170238	-2.030710	1.301248	0.005045	0.276851
-23.524071	-1.993987	1.306253	0.005111	0.276706
-23.014722	-2.088037	1.311258	0.005016	0.276699
-23.456745	-2.056712	1.316262	0.005098	0.276442
-24.001268	-1.969695	1.321267	0.005200	0.276379
-23.880228	-1.993312	1.326272	0.005177	0.276370
-23.832442	-2.055409	1.331277	0.005168	0.276090
-24.315483	-1.970594	1.336282	0.005258	0.276074
-24.372015	-1.969895	1.341286	0.005269	0.276024
-23.849568	-2.117900	1.346291	0.005172	0.275746
-23.847619	-2.120905	1.351296	0.005171	0.275732
-24.345779	-2.053996	1.356301	0.005264	0.275608
-24.479267	-2.050156	1.361306	0.005289	0.275500
-24.325915	-2.080246	1.366310	0.005260	0.275488
-24.598580	-2.089834	1.371315	0.005311	0.275177
-24.716851	-2.073645	1.376320	0.005333	0.275149
-24.672647	-2.105668	1.381325	0.005325	0.275023
-25.108094	-2.061537	1.386330	0.005406	0.274838
-25.106186	-2.062266	1.391334	0.005406	0.274836
-24.929126	-2.140684	1.396339	0.005373	0.274592
-25.430099	-2.065364	1.401344	0.005466	0.274509
-25.644809	-2.037068	1.406349	0.005506	0.274452
-25.663195	-2.077842	1.411354	0.005510	0.274219
-25.742800	-2.064400	1.416358	0.005524	0.274214
-25.665105	-2.112663	1.421363	0.005510	0.274034
-26.356022	-2.014982	1.426368	0.005639	0.273886
-25.997116	-2.081147	1.431373	0.005572	0.273881
-26.378296	-2.065902	1.436378	0.005643	0.273595
-26.714598	-2.009981	1.441382	0.005705	0.273567
-25.942351	-2.166817	1.446387	0.005562	0.273480
-26.583730	-2.092775	1.451392	0.005681	0.273254
-26.769462	-2.059366	1.456397	0.005716	0.273252
-26.691663	-2.112849	1.461402	0.005701	0.273044
-26.878246	-2.096654	1.466406	0.005736	0.272950
-26.852921	-2.112857	1.471411	0.005731	0.272888
-27.463555	-2.052329	1.476416	0.005845	0.272620
-27.263387	-2.087878	1.481421	0.005808	0.272624
-27.366833	-2.102484	1.486426	0.005827	0.272447
-27.995491	-2.013613	1.491430	0.005944	0.272311
-27.562711	-2.091606	1.496435	0.005864	0.272315
-27.769242	-2.115098	1.501440	0.005902	0.271990
-28.007701	-2.071650	1.506445	0.005946	0.271990
-28.048013	-2.085061	1.511450	0.005954	0.271880
-28.354850	-2.064115	1.516454	0.006011	0.271694
-28.216475	-2.087122	1.521459	0.005985	0.271706
-28.706950	-2.047191	1.526464	0.006077	0.271443
-28.465429	-2.106808	1.531469	0.006032	0.271359
-28.435616	-2.123471	1.536474	0.006026	0.271299
-29.144061	-2.040620	1.541478	0.006158	0.271053
-28.926890	-2.076110	1.546483	0.006118	0.271075
-28.963533	-2.106898	1.551488	0.006125	0.270874
-29.428132	-2.045987	1.556493	0.006211	0.270748
-29.684292	-1.995644	1.561498	0.006259	0.270768
-29.737029	-2.033440	1.566502	0.006269	0.270515
-29.649264	-2.052195	1.571507	0.006252	0.270500
-30.004667	-2.002959	1.576512	0.006318	0.270417
-30.080901	-2.037756	1.581517	0.006333	0.270156
-29.888207	-2.073087	1.586522	0.006297	0.270155
-30.201887	-2.052316	1.591526	0.006355	0.269960
-30.393153	-2.039733	1.596531	0.006391	0.269841
-30.378235	-2.042934	1.601536	0.006388	0.269838
-30.764982	-2.031844	1.606541	0.006460	0.269520
-30.955097	-1.998109	1.611546	0.006495	0.269515
-30.929550	-2.016057	1.616550	0.006491	0.269444
-31.116386	-2.021256	1.621555	0.006526	0.269233
-31.247623	-1.999752	1.626560	0.006550	0.269220
-31.341093	-2.012901	1.631565	0.006567	0.269058
-31.566580	-2.002162	1.636570	0.006609	0.268895
-31.861817	-1.949692	1.641574	0.006664	0.268888
-31.470691	-2.063453	1.646579	0.006592	0.268659
-31.856532	-2.007874	1.651584	0.006663	0.268580
-31.883905	-2.008950	1.656589	0.006669	0.268547
-32.030986	-2.036309	1.661594	0.006696	0.268255
-32.106668	-2.024803	1.666598	0.006710	0.268243
-32.018303	-2.061753	1.671603	0.006694	0.268130
-32.219176	-2.057081	1.676608	0.006731	0.267958
-32.332382	-2.035747	1.681613	0.006752	0.267962
-32.351831	-2.085401	1.686618	0.006756	0.267674
-32.881451	-2.001083	1.691622	0.006854	0.267609
-32.590443	-2.067567	1.696627	0.006800	0.267536
-33.177263	-2.001407	1.701632	0.006910	0.267316
-33.465611	-1.948217	1.706637	0.006963	0.267320
-33.401722	-1.989064	1.711642	0.006951	0.267161
-33.614223	-1.983629	1.716646	0.006991	0.266981
-33.324521	-2.034499	1.721651	0.006937	0.266991
-33.901039	-1.971566	1.726656	0.007044	0.266763
-34.037109	-1.957947	1.731661	0.007070	0.266703
-33.520545	-2.058662	1.736666	0.006974	0.266666
-34.253443	-1.980205	1.741670	0.007110	0.266368
-34.337706	-1.962987	1.746675	0.007126	0.266378
-34.589646	-1.933941	1.751680	0.007173	0.266287
-34.650648	-1.964091	1.756685	0.007184	0.266062
-34.507837	-1.987970	1.761690	0.007157	0.266074
-34.557345	-2.018042	1.766694	0.007167	0.265861
-34.766237	-2.001427	1.771699	0.007206	0.265744
-34.790868	-1.998322	1.776704	0.007210	0.265737
-35.102177	-1.987109	1.781709	0.007268	0.265489
-34.467486	-2.104175	1.786714	0.007150	0.265480
-35.048718	-2.028728	1.791718	0.007258	0.265315
-35.709715	-1.939139	1.796723	0.007381	0.265147
-35.150698	-2.043253	1.801728	0.007277	0.265134
-35.669103	-1.995136	1.806733	0.007374	0.264882
-35.762431	-1.988766	1.811738	0.007391	0.264824
-35.722313	-2.008069	1.816742	0.007384	0.264758
-35.773075	-2.046603	1.821747	0.007393	0.264496
-36.135611	-1.982154	1.826752	0.007461	0.264488
-36.198319	-2.000477	1.831757	0.007472	0.264325
-36.010625	-2.055389	1.836762	0.007438	0.264211
-36.473875	-1.971884	1.841766	0.007524	0.264207
-36.608108	-2.006154	1.846771	0.007549	0.263885
-36.458078	-2.037474	1.851776	0.007521	0.263863
-36.705925	-2.014188	1.856781	0.007567	0.263743
-36.994425	-1.994323	1.861786	0.007621	0.263564
-37.137693	-1.969572	1.866790	0.007647	0.263557
-36.921293	-2.052559	1.871795	0.007607	0.263317
-37.319983	-1.995298	1.876800	0.007681	0.263233
-37.479770	-1.974016	1.881805	0.007711	0.263190
-37.312607	-2.048400	1.886810	0.007680	0.262948
-37.500926	-2.015266	1.891814	0.007715	0.262941
-37.612178	-2.031752	1.896819	0.007736	0.262739
-37.863409	-2.010842	1.901824	0.007783	0.262602
-37.616311	-2.060101	1.906829	0.007737	0.262578
-38.221555	-1.999348	1.911834	0.007849	0.262306
-38.327412	-1.983901	1.916838	0.007869	0.262285
-37.922464	-2.085051	1.921843	0.007794	0.262133
-38.430171	-2.022488	1.926848	0.007888	0.261968
-38.299407	-2.047391	1.931853	0.007864	0.261962
-38.482148	-2.064299	1.936858	0.007898	0.261684
-38.644484	-2.036742	1.941862	0.007928	0.261673
-38.655212	-2.065040	1.946867	0.007930	0.261506
-38.901970	-2.049649	1.951872	0.007976	0.261342
-38.717984	-2.087464	1.956877	0.007942	0.261318
-39.190328	-2.051737	1.961882	0.008030	0.261040
-39.398275	-2.015033	1.966886	0.008069	0.261033
-39.511306	-2.023148	1.971891	0.008090	0.260874
-39.885500	-1.981277	1.976896	0.008159	0.260729
-39.852527	-1.987806	1.981901	0.008153	0.260726
-39.730651	-2.051728	1.986906	0.008131	0.260494
-39.841017	-2.035468	1.991910	0.008151	0.260472
-39.816356	-2.067968	1.996915	0.008147	0.260316
-40.178872	-2.034795	2.001920	0.008214	0.260134

-40.542798	-2.020534	2.011917	0.008282	0.259844
-40.575017	-2.044397	2.021914	0.008288	0.259678
-40.961525	-2.007198	2.031910	0.008360	0.259493
-41.037053	-2.028035	2.041907	0.008374	0.259300
-41.133493	-2.027899	2.051904	0.008392	0.259203
-41.413474	-2.011897	2.061901	0.008444	0.259007
-41.411865	-2.036392	2.071898	0.008444	0.258872
-41.643409	-1.993084	2.081894	0.008487	0.258878
-41.597242	-2.034384	2.091891	0.008478	0.258694
-41.798104	-2.022384	2.101888	0.008516	0.258556
-42.008003	-1.982115	2.111885	0.008555	0.258568
-42.039736	-1.975260	2.121882	0.008561	0.258574
-42.565400	-1.877143	2.131878	0.008659	0.258588
-42.122065	-1.960800	2.141875	0.008576	0.258571
-42.046125	-1.976011	2.151872	0.008562	0.258563
-41.996699	-1.985184	2.161869	0.008553	0.258561
-41.894405	-2.003371	2.171866	0.008534	0.258564
-41.865733	-2.009393	2.181862	0.008529	0.258559
-42.007782	-1.982625	2.191859	0.008555	0.258564
-42.268756	-1.934292	2.201856	0.008604	0.258569
-42.136906	-1.957842	2.211853	0.008579	0.258571
-42.055171	-1.972105	2.221850	0.008564	0.258574
-41.608272	-2.000601	2.231846	0.008481	0.258870
-41.664767	-1.990340	2.241843	0.008491	0.258869
-41.604332	-2.001027	2.251840	0.008480	0.258871
-41.380790	-2.041656	2.261837	0.008439	0.258871
-41.214276	-2.034905	2.271834	0.008408	0.259078
-41.110188	-2.031482	2.281830	0.008388	0.259203
-41.127596	-2.027046	2.291827	0.008392	0.259210
-41.386576	-1.960111	2.301824	0.008440	0.259320
-41.026041	-1.993675	2.311821	0.008373	0.259499
-40.855782	-2.025268	2.321818	0.008341	0.259495
-40.707648	-2.012403	2.331814	0.008314	0.259717
-40.777789	-1.980702	2.341811	0.008327	0.259823
-40.795825	-1.957259	2.351808	0.008330	0.259935
-40.394020	-1.993538	2.361805	0.008255	0.260140
-40.355356	-1.987877	2.371802	0.008248	0.260210
-39.989766	-2.006021	2.381798	0.008180	0.260479
-39.870162	-2.025112	2.391795	0.008158	0.260494
-39.836036	-1.991031	2.401792	0.008151	0.260718
-39.581462	-2.032845	2.411789	0.008104	0.260743
-39.702657	-1.956178	2.421786	0.008127	0.261046
-39.673266	-1.942860	2.431782	0.008121	0.261149
-39.775846	-1.884236	2.441779	0.008140	0.261370
-39.292337	-1.934141	2.451776	0.008050	0.261581
-39.064427	-1.954516	2.461773	0.008008	0.261698
-39.232633	-1.870292	2.471770	0.008039	0.261994
-39.010858	-1.881256	2.481766	0.007998	0.262156
-38.919641	-1.869312	2.491763	0.007981	0.262314
-38.526923	-1.885565	2.501760	0.007908	0.262618
-38.270406	-1.900715	2.511757	0.007860	0.262792
-38.394247	-1.841924	2.521754	0.007883	0.262991
-38.132246	-1.839714	2.531750	0.007834	0.263266
-38.045786	-1.816472	2.541747	0.007818	0.263480
-37.733652	-1.839678	2.551744	0.007760	0.263664
-37.615798	-1.817666	2.561741	0.007738	0.263902
-37.326347	-1.812975	2.571738	0.007684	0.264217
-37.136751	-1.814880	2.581734	0.007649	0.264395
-37.042971	-1.792034	2.591731	0.007632	0.264613
-36.741723	-1.802112	2.601728	0.007576	0.264858
-35.739152	-1.936172	2.611725	0.007389	0.265122
-35.548299	-1.942891	2.621722	0.007354	0.265274
-35.469567	-1.915303	2.631718	0.007339	0.265503
-35.203991	-1.920712	2.641715	0.007290	0.265737
-35.004293	-1.928063	2.651712	0.007252	0.265894
-35.165628	-1.858390	2.661709	0.007282	0.266114
-35.196234	-1.798789	2.671706	0.007288	0.266408
-34.444381	-1.886831	2.681702	0.007148	0.266672
-34.118633	-1.916222	2.691699	0.007088	0.266834
-34.207251	-1.865084	2.701696	0.007104	0.267024
-33.514665	-1.935323	2.711693	0.006975	0.267326
-33.597866	-1.882391	2.721690	0.006991	0.267530
-33.048091	-1.947647	2.731686	0.006888	0.267718
-32.982934	-1.910635	2.741683	0.006876	0.267982
-32.785741	-1.900084	2.751680	0.006840	0.268233
-32.395742	-1.936895	2.761677	0.006767	0.268417
-32.296521	-1.915542	2.771674	0.006749	0.268629
-32.301654	-1.861239	2.781670	0.006750	0.268916
-31.810761	-1.904427	2.791667	0.006658	0.269164
-31.625747	-1.902144	2.801664	0.006624	0.269357
-31.537506	-1.879335	2.811661	0.006607	0.269566
-31.116111	-1.901890	2.821658	0.006529	0.269856
-30.912048	-1.892498	2.831654	0.006491	0.270106
-30.591314	-1.912529	2.841651	0.006431	0.270311
-29.963556	-1.990590	2.851648	0.006314	0.270504
-30.028114	-1.931681	2.861645	0.006326	0.270756
-30.002802	-1.896781	2.871642	0.006322	0.270967
-29.536545	-1.942793	2.881638	0.006235	0.271174
-29.372094	-1.932745	2.891635	0.006204	0.271387
-29.082386	-1.926701	2.901632	0.006151	0.271700
-28.694849	-1.961795	2.911629	0.006078	0.271889
-28.286611	-2.004536	2.921626	0.006002	0.272056
-28.365237	-1.937660	2.931622	0.006017	0.272336
-27.907704	-1.976603	2.941619	0.005932	0.272571
-27.308564	-2.052149	2.951616	0.005820	0.272748
-27.049477	-2.059382	2.961613	0.005772	0.272960
-26.756538	-2.063764	2.971610	0.005718	0.273219
-26.773187	-2.029054	2.981606	0.005721	0.273386
-26.443244	-2.053425	2.991603	0.005659	0.273575
-26.032291	-2.073718	3.001600	0.005583	0.273863
-26.074109	-2.032488	3.011597	0.005591	0.274040
-25.801928	-2.043869	3.021594	0.005540	0.274241
-25.644302	-2.021485	3.031590	0.005511	0.274511
-25.063143	-2.089764	3.041587	0.005403	0.274708
-25.037326	-2.060422	3.051584	0.005398	0.274887
-24.866450	-2.041707	3.061581	0.005366	0.275149
-24.361379	-2.084900	3.071578	0.005272	0.275405
-24.540957	-2.019480	3.081574	0.005305	0.275577
-24.105362	-2.069710	3.091571	0.005224	0.275729
-24.072457	-2.017921	3.101568	0.005218	0.276032
-23.763111	-2.036835	3.111565	0.005161	0.276227
-23.564150	-2.033358	3.121562	0.005124	0.276435
-23.337512	-2.025590	3.131558	0.005082	0.276691
-23.088500	-2.023023	3.141555	0.005035	0.276941
-22.988386	-1.998935	3.151552	0.005017	0.277162
-22.468366	-2.056104	3.161549	0.004920	0.277357
-22.031114	-2.086301	3.171546	0.004838	0.277614
-21.786146	-2.081749	3.181542	0.004793	0.277870
-21.994966	-2.005908	3.191539	0.004832	0.278067
-21.482080	-2.063458	3.201536	0.004736	0.278253
-21.495574	-1.999703	3.211533	0.004739	0.278572
-20.996568	-2.047175	3.221530	0.004646	0.278796
-20.862861	-2.032378	3.231526	0.004621	0.278999
-20.380146	-2.079356	3.241523	0.004531	0.279211
-20.517822	-1.998784	3.251520	0.004557	0.279498
-20.181580	-2.017706	3.261517	0.004494	0.279717
-19.733802	-2.059260	3.271514	0.004411	0.279923
-19.427677	-2.072485	3.281510	0.004354	0.280142
-19.155601	-2.061070	3.291507	0.004303	0.280456
-19.189394	-2.025205	3.301504	0.004310	0.280609
-18.840475	-2.055081	3.311501	0.004245	0.280782
-18.571196	-2.054367	3.321498	0.004195	0.281038
-18.261344	-2.060517	3.331494	0.004137	0.281297
-17.964652	-2.073088	3.341491	0.004082	0.281509
-17.823913	-2.059865	3.351488	0.004056	0.281709
-17.556280	-2.058884	3.361485	0.004006	0.281963
-17.418417	-2.033656	3.371482	0.003980	0.282221
-17.214604	-2.029534	3.381478	0.003942	0.282432
-16.787054	-2.067422	3.391475	0.003863	0.282636
-16.695243	-2.024489	3.401472	0.003846	0.282941
-16.235894	-2.064146	3.411469	0.003760	0.283166
-16.208180	-2.029829	3.421466	0.003755	0.283366
-15.971309	-2.028413	3.431462	0.003711	0.283593
-15.678469	-2.027846	3.441459	0.003656	0.283868
-15.372225	-2.032901	3.451456	0.003599	0.284126
-15.196618	-2.024236	3.461453	0.003567	0.284332
-15.024173	-2.014380	3.471450	0.003535	0.284542
-14.549786	-2.045558	3.481446	0.003446	0.284822
-14.176243	-2.064187	3.491443	0.003377	0.285072
-13.994468	-2.057401	3.501440	0.003343	0.285274
-13.609611	-2.086366	3.511437	0.003271	0.285482
-13.298565	-2.094003	3.521434	0.003213	0.285729
-13.002164	-2.110406	3.531430	0.003158	0.285919
-12.977407	-2.075371	3.541427	0.003154	0.286119
-12.959250	-2.031122	3.551424	0.003150	0.286359
-12.698183	-2.018454	3.561421	0.003102	0.286663
-12.580253	-1.998635	3.571418	0.003080	0.286871
-12.196701	-2.025987	3.581414	0.003008	0.287085
-11.596728	-2.092236	3.591411	0.002897	0.287300
-11.401619	-2.071784	3.601408	0.002860	0.287582
-10.872737	-2.127880	3.611405	0.002762	0.287783
-10.658953	-2.131334	3.621402	0.002722	0.287961
-10.315990	-2.138571	3.631398	0.002658	0.288238
-10.008828	-2.158472	3.641395	0.002601	0.288418
-9.920185	-2.142642	3.651392	0.002585	0.288578
-9.459185	-2.168503	3.661389	0.002499	0.288868
-9.393703	-2.141131	3.671386	0.002487	0.289065
-9.133685	-2.153055	3.681382	0.002438	0.289242
-8.814975	-2.161439	3.691379	0.002379	0.289489
-8.627739	-2.152375	3.701376	0.002344	0.289705
-8.415865	-2.155433	3.711373	0.002305	0.289882
-8.345354	-2.117157	3.721370	0.002292	0.290136
-8.034152	-2.119414	3.731366	0.002234	0.290407
-8.073760	-2.077333	3.741363	0.002241	0.290581
-7.546672	-2.141888	3.751360	0.002143	0.290736
-7.421685	-2.101474	3.761357	0.002120	0.291050
-7.331328	-2.077074	3.771354	0.002103	0.291253
-7.059490	-2.082994	3.781350	0.002052	0.291469
-7.128697	-2.023146	3.791347	0.002065	0.291703
-6.881449	-2.010205	3.801344	0.002019	0.291990
-6.728122	-1.990708	3.811341	0.001991	0.292225
-6.137184	-2.051721	3.821338	0.001881	0.292454
-5.960232	-2.038422	3.831334	0.001848	0.292679
-5.633181	-2.040407	3.841331	0.001787	0.292963
-5.737570	-1.972607	3.851328	0.001806	0.293204
-5.782684	-1.916048	3.861325	0.001815	0.293442
-5.272141	-1.959241	3.871322	0.001720	0.293687
-5.150705	-1.931959	3.881318	0.001697	0.293930
-4.764092	-1.943950	3.891315	0.001625	0.294216
-4.448457	-1.949085	3.901312	0.001567	0.294473
-4.724864	-1.846934	3.911309	0.001618	0.294728
-4.318119	-1.864925	3.921306	0.001542	0.295002
-4.629185	-1.753368	3.931302	0.001600	0.295272
-4.135160	-1.783763	3.941299	0.001508	0.295563
-3.821040	-1.798014	3.951296	0.001450	0.295772
-3.548420	-1.788848	3.961293	0.001399	0.296059
-2.963461	-1.835448	3.971290	0.001290	0.296351
-3.881776	-1.611197	3.981286	0.001461	0.296630
-2.788486	-1.751461	3.991283	0.001258	0.296915
-2.946484	-1.667284	4.001280	0.001287	0.297185
-3.173002	-1.565105	4.011277	0.001329	0.297482
-3.148875	-1.495114	4.021274	0.001325	0.297843
-2.539999	-1.546570	4.031270	0.001211	0.298131
-2.770874	-1.440605	4.041267	0.001254	0.298441
-3.325790	-1.267566	4.051264	0.001358	0.298791
-2.998057	-1.254272	4.061261	0.001297	0.299143
-2.353343	-1.302549	4.071258	0.001177	0.299476
-2.205060	-1.259075	4.081254	0.001149	0.299816
-1.984241	-1.223605	4.091251	0.001108	0.300181
-2.091921	-1.128014	4.101248	0.001128	0.300547
-2.233148	-1.040006	4.111245	0.001154	0.300847
-2.442353	-0.924280	4.121242	0.001193	0.301220
-1.920196	-0.940288	4.131238	0.001096	0.301599
-1.729681	-0.896352	4.141235	0.001060	0.301975
-1.392333	-0.873345	4.151232	0.000998	0.302379
-1.421530	-0.787078	4.161229	0.001003	0.302766
-1.067111	-0.774306	4.171226	0.000937	0.303134
-1.058417	-0.694632	4.181222	0.000935	0.303522
-0.907680	-0.629933	4.191219	0.000907	0.303960
-0.957841	-0.538948	4.201216	0.000917	0.304350
-0.796644	-0.487499	4.211213	0.000887	0.304733
-0.528282	-0.434475	4.221210	0.000837	0.305216
-0.666164	-0.325982	4.231206	0.000862	0.305611
-0.376239	-0.296323	4.241203	0.000808	0.306000
-0.621165	-0.149153	4.251200	0.000854	0.306485
-0.143338	-0.151282	4.261197	0.000765	0.306885
-0.122848	-0.053349	4.271194	0.000761	0.307364
-0.081000	0.034012	4.281190	0.000753	0.307810
0.041234	0.111401	4.291187	0.000730	0.308278
-0.111583	0.239283	4.301184	0.000759	0.308747
0.000000	0.312003	4.311181	0.000738	0.309183

-0.218608	0.623377	4.316186	0.000779	0.310451
-0.203799	1.176939	4.321190	0.000775	0.313033
0.079883	1.966415	4.326195	0.000722	0.316896
0.646878	2.992572	4.331200	0.000616	0.322011
1.098628	4.336138	4.336205	0.000531	0.328354
2.183296	5.858066	4.341210	0.000328	0.335842
3.608362	7.624187	4.346214	0.000061	0.344455
4.446527	9.818509	4.351219	-0.000096	0.354173
5.504521	12.277006	4.356224	-0.000295	0.364839
7.360821	14.921849	4.361229	-0.000642	0.376475
8.588380	18.019708	4.366234	-0.000873	0.389025
10.434352	21.345419	4.371238	-0.001218	0.402405
13.293451	24.849318	4.376243	-0.001753	0.416610
16.673336	28.633474	4.381248	-0.002385	0.431602
20.248127	32.751453	4.386253	-0.003053	0.447283
23.240043	37.358140	4.391258	-0.003613	0.463627
25.389996	42.492769	4.396262	-0.004017	0.480545
27.235454	48.040732	4.401267	-0.004364	0.497927
30.641751	53.675993	4.406272	-0.005002	0.515755
34.835274	59.530768	4.411277	-0.005787	0.533964
37.746451	65.973928	4.416282	-0.006333	0.552505
40.338034	72.811991	4.421286	-0.006820	0.571295
43.210903	79.926839	4.426291	-0.007359	0.590287
45.760901	87.399952	4.431296	-0.007839	0.609396
48.236612	95.172952	4.436301	-0.008305	0.628582
51.442801	103.077909	4.441306	-0.008907	0.647782
54.375315	111.304703	4.446310	-0.009459	0.667019
56.457519	119.884677	4.451315	-0.009852	0.686137
59.953088	128.420159	4.456320	-0.010508	0.705161
62.858832	137.257893	4.461325	-0.011055	0.724075
64.976270	146.403586	4.466330	-0.011455	0.742832
67.093214	155.686873	4.471334	-0.011856	0.761385
69.272140	165.066244	4.476339	-0.012267	0.779693
71.789281	174.482986	4.481344	-0.012742	0.797755
73.819740	184.081762	4.486349	-0.013126	0.815586
76.106319	193.688655	4.491354	-0.013558	0.833125
77.464046	203.500248	4.496358	-0.013818	0.850370
79.431032	213.213337	4.501363	-0.014190	0.867286
81.995723	222.837654	4.506368	-0.014674	0.883903
85.932470	232.257041	4.511373	-0.015413	0.900270
87.781212	242.059572	4.516378	-0.015764	0.916368
88.658817	251.992240	4.521382	-0.015934	0.932124
91.820105	261.483308	4.526387	-0.016528	0.947554
95.922861	270.830660	4.531392	-0.017298	0.962765
99.296229	280.299627	4.536397	-0.017933	0.977729
102.592310	289.784425	4.541402	-0.018553	0.992468
104.956244	299.359955	4.546406	-0.018999	1.006886
108.609995	308.682517	4.551411	-0.019685	1.021059
111.896766	318.042442	4.556416	-0.020304	1.034998
114.537639	327.473039	4.561421	-0.020801	1.048693
118.526092	336.629461	4.566426	-0.021550	1.062154
121.011105	346.035506	4.571430	-0.022019	1.075430
123.609380	355.321988	4.576435	-0.022509	1.088411
125.948689	364.627477	4.581440	-0.022950	1.101203
129.368659	373.695704	4.586445	-0.023593	1.113780
135.584663	382.272410	4.591450	-0.024756	1.126201
137.889192	391.533453	4.596454	-0.025191	1.138500
140.203723	400.725172	4.601459	-0.025628	1.150580
141.785340	409.951407	4.606464	-0.025929	1.162421
143.100242	419.163465	4.611469	-0.026179	1.174068
144.125572	428.331167	4.616474	-0.026376	1.185486
148.876030	436.824994	4.621478	-0.027266	1.196748
151.433686	445.712321	4.626483	-0.027748	1.207926
154.071660	454.522621	4.631488	-0.028245	1.218926
157.126636	463.261055	4.636493	-0.028820	1.229824
158.696629	472.177946	4.641498	-0.029118	1.240540
160.372448	481.039598	4.646502	-0.029436	1.251120
161.110461	489.990066	4.651507	-0.029579	1.261531
162.033004	498.853957	4.656512	-0.029756	1.271794
163.011989	507.647123	4.661517	-0.029944	1.281905
164.845845	516.263058	4.666522	-0.030292	1.291899
167.073693	524.797552	4.671526	-0.030712	1.301799
169.024269	533.411414	4.676531	-0.031081	1.311659
170.777208	541.986845	4.681536	-0.031413	1.321367
173.293426	550.392965	4.686541	-0.031887	1.330959
175.503911	558.847321	4.691546	-0.032304	1.340477
177.194188	567.395399	4.696550	-0.032624	1.349934
178.230828	575.988726	4.701555	-0.032823	1.359257
179.124213	584.590366	4.706560	-0.032995	1.368500
181.268290	592.968383	4.711565	-0.033399	1.377664
182.616437	601.439623	4.716570	-0.033656	1.386726
183.886186	609.933080	4.721574	-0.033898	1.395739
186.446300	618.163043	4.726579	-0.034380	1.404642
188.910103	626.447017	4.731584	-0.034844	1.413527
190.469904	634.885170	4.736589	-0.035140	1.422359
191.839131	643.317840	4.741594	-0.035400	1.431100
192.866695	651.798446	4.746598	-0.035597	1.439778
194.868115	660.088751	4.751603	-0.035975	1.448374
198.029240	668.215249	4.756608	-0.036569	1.456946
200.662480	676.458391	4.761613	-0.037065	1.465495
201.815909	684.947795	4.766618	-0.037285	1.473997
202.745715	693.413366	4.771622	-0.037464	1.482391
203.608541	701.849866	4.776627	-0.037630	1.490698
204.369087	710.294364	4.781632	-0.037777	1.498951
205.003308	718.715467	4.786637	-0.037900	1.507116
206.245560	726.996314	4.791642	-0.038137	1.515198
208.105729	735.204962	4.796646	-0.038489	1.523264
209.135940	743.539437	4.801651	-0.038686	1.531277
210.760987	751.764460	4.806656	-0.038994	1.539237
212.173708	760.053565	4.811661	-0.039262	1.547182
213.377904	768.350119	4.816666	-0.039492	1.555062
215.206081	776.529893	4.821670	-0.039838	1.562888
216.082578	784.862852	4.826675	-0.040006	1.570672
217.302095	793.130980	4.831680	-0.040239	1.578410
219.552304	801.223764	4.836685	-0.040663	1.586101
221.266671	809.419899	4.841690	-0.040988	1.593770
222.601544	817.693870	4.846694	-0.041242	1.601416
224.530467	825.862547	4.851699	-0.041606	1.609017
225.213862	834.235005	4.856704	-0.041739	1.616584
225.890074	842.586511	4.861709	-0.041870	1.624097
226.827098	850.875924	4.866714	-0.042050	1.631556
228.197866	859.085232	4.871718	-0.042310	1.638972
229.565424	867.246500	4.876723	-0.042570	1.646312
230.943769	875.443162	4.881728	-0.042832	1.653651
233.086413	883.515667	4.886733	-0.043237	1.660955
234.828618	891.684986	4.891738	-0.043566	1.668255
236.102521	899.923597	4.896742	-0.043809	1.675518
236.589964	908.262899	4.901747	-0.043905	1.682728
237.542580	916.498601	4.906752	-0.044088	1.689882
238.636229	924.732299	4.911757	-0.044297	1.697023
239.225140	932.996276	4.916762	-0.044412	1.704092
240.330134	941.199808	4.921766	-0.044623	1.711148
241.277940	949.402799	4.926771	-0.044805	1.718155
242.040644	957.593831	4.931776	-0.044952	1.725098
243.167672	965.774355	4.936781	-0.045167	1.732052
245.038710	973.811860	4.941786	-0.045521	1.738957
246.780825	981.916966	4.946790	-0.045850	1.745872
247.478031	990.198490	4.951795	-0.045986	1.752770
248.310318	998.396749	4.956800	-0.046146	1.759590
248.919859	1006.657340	4.961805	-0.046265	1.766405
249.760647	1014.852219	4.966810	-0.046427	1.773171
250.007111	1023.126143	4.971814	-0.046478	1.779899
250.512998	1031.338123	4.976819	-0.046578	1.786584
251.359335	1039.526901	4.981824	-0.046740	1.793269
252.772512	1047.584620	4.986829	-0.047009	1.799893
253.604754	1055.720988	4.991834	-0.047169	1.806484
253.953642	1063.975778	4.996838	-0.047239	1.813085
254.720132	1072.125695	5.001843	-0.047387	1.819631
255.651198	1080.223595	5.006848	-0.047566	1.826131
256.271313	1088.434470	5.011853	-0.047687	1.832659
257.206863	1096.531189	5.016858	-0.047866	1.839113
258.430823	1104.600250	5.021862	-0.048099	1.845557
259.419088	1112.748195	5.026867	-0.048289	1.852011
260.144823	1120.917593	5.031872	-0.048429	1.858428
260.758145	1129.100972	5.036877	-0.048549	1.864820
261.780232	1137.211638	5.041882	-0.048744	1.871182
262.965283	1145.304150	5.046886	-0.048970	1.877528
263.432613	1153.499159	5.051891	-0.049063	1.883846
263.843657	1161.682690	5.056896	-0.049144	1.890128
264.703070	1169.825563	5.061901	-0.049310	1.896409
265.568445	1177.919504	5.066906	-0.049476	1.902634
266.483662	1186.047076	5.071910	-0.049652	1.908869
267.136492	1194.185094	5.076915	-0.049779	1.915061
267.498240	1202.381017	5.081920	-0.049851	1.921244
268.271447	1210.497685	5.086925	-0.050001	1.927394
269.005316	1218.626141	5.091930	-0.050142	1.933528
269.584881	1226.776139	5.096934	-0.050256	1.939641
270.316456	1234.886364	5.101939	-0.050397	1.945723
271.314201	1242.967940	5.106944	-0.050588	1.951794
272.105084	1251.071999	5.111949	-0.050741	1.957839
272.881353	1259.167532	5.116954	-0.050891	1.963858
273.597183	1267.307708	5.121958	-0.051029	1.969884
274.609210	1275.388115	5.126963	-0.051223	1.975881
275.466793	1283.492505	5.131968	-0.051388	1.981859
276.124252	1291.647898	5.136973	-0.051515	1.987835
276.620187	1299.799216	5.141978	-0.051613	1.993772
277.425468	1307.876640	5.146982	-0.051768	1.999671
277.854839	1316.033426	5.151987	-0.051854	2.005570
278.439228	1324.167331	5.156992	-0.051968	2.011451
279.585568	1332.212185	5.161997	-0.052186	2.017311
280.446963	1340.297671	5.167002	-0.052352	2.023152
281.398315	1348.408284	5.172006	-0.052534	2.029004
282.574086	1356.472608	5.177011	-0.052759	2.034829
283.501078	1364.544295	5.182016	-0.052936	2.040616
284.176423	1372.709210	5.187021	-0.053067	2.046427
284.883871	1380.834092	5.192026	-0.053205	2.052196
286.076692	1388.892344	5.197030	-0.053432	2.057952
287.173499	1396.957286	5.202035	-0.053641	2.063686
287.632986	1405.132644	5.207040	-0.053732	2.069416
288.556962	1413.227915	5.212045	-0.053909	2.075122
288.818103	1421.380442	5.217050	-0.053963	2.080784
289.477048	1429.492824	5.222054	-0.054091	2.086443
290.100130	1437.619815	5.227059	-0.054213	2.092093
290.693465	1445.727570	5.232064	-0.054328	2.097712
291.297533	1453.837703	5.237069	-0.054446	2.103318
291.761519	1461.970128	5.242074	-0.054538	2.108911
293.017690	1470.012708	5.247078	-0.054777	2.114505
293.689153	1478.089399	5.252083	-0.054907	2.120050
294.419209	1486.146965	5.257088	-0.055048	2.125574
295.300681	1494.252627	5.262093	-0.055218	2.131130
295.790435	1502.380632	5.267098	-0.055314	2.136648
296.353867	1510.476602	5.272102	-0.055424	2.142137
297.048345	1518.579155	5.277107	-0.055559	2.147630
297.609786	1526.675056	5.282112	-0.055669	2.153091
298.194754	1534.770752	5.287117	-0.055783	2.158540
298.896259	1542.834465	5.292122	-0.055919	2.163965
300.106801	1550.867190	5.297126	-0.056150	2.169404
300.615127	1559.003505	5.302131	-0.056249	2.174831
300.901462	1567.128672	5.307136	-0.056308	2.180217
302.064012	1575.167738	5.312141	-0.056530	2.185614
302.729699	1583.277942	5.317146	-0.056659	2.190998
303.238873	1591.381401	5.322150	-0.056759	2.196350
303.655233	1599.490890	5.327155	-0.056842	2.201684
303.960206	1607.590310	5.332160	-0.056904	2.206989
304.448958	1615.712579	5.337165	-0.057000	2.212312
304.782704	1623.810128	5.342170	-0.057068	2.217592
305.726897	1631.817754	5.347174	-0.057249	2.222857
306.587989	1639.892616	5.352179	-0.057414	2.228145
307.435342	1647.933391	5.357184	-0.057577	2.233397
308.405860	1655.994449	5.362189	-0.057763	2.238661
308.971310	1664.075373	5.367194	-0.057874	2.243888
309.531652	1672.208069	5.372198	-0.057983	2.249136
310.227360	1680.303760	5.377203	-0.058118	2.254360
310.514023	1688.424976	5.382208	-0.058177	2.259552
311.248824	1696.496728	5.387213	-0.058319	2.264739
311.714985	1704.584189	5.392218	-0.058411	2.269901
312.183357	1712.721021	5.397222	-0.058503	2.275083
312.757582	1720.772062	5.402227	-0.058616	2.280208
313.559951	1728.775729	5.407232	-0.058770	2.285311
314.818903	1736.809656	5.412237	-0.059010	2.290462
316.218616	1744.762246	5.417242	-0.059276	2.295562
317.121989	1752.815760	5.422246	-0.059449	2.300670
317.680680	1760.948599	5.427251	-0.059558	2.305787
318.569452	1769.004491	5.432256	-0.059729	2.310872
319.055816	1777.135556	5.437261	-0.059825	2.315959
319.577919	1785.213057	5.442266	-0.059927	2.321004
320.183374	1793.301139	5.447270	-0.060045	2.326051
321.072931	1801.387125	5.452275	-0.060216	2.331111
322.057352	1809.428300	5.457280	-0.060405	2.336139
323.129875	1817.470386	5.462285	-0.060610	2.341164
324.201226	1825.480650	5.467290	-0.060814	2.346159
324.711702	1833.638959	5.472294	-0.060915	2.351187
325.239931	1841.740158	5.477299	-0.061018	2.356170
325.738436	1849.815657	5.482304	-0.061116	2.361125
326.445011	1857.882875	5.487309	-0.061253	2.366081
326.995837	1865.965086	5.492314	-0.061361	2.371024
327.621606	1874.035305	5.497318	-0.061483	2.375954
327.841414	1882.192982	5.502323	-0.061529	2.380894
328.396782	1890.242406	5.507328	-0.061638	2.385786
329.030221	1898.314366	5.512333	-0.061761	2.390687
329.935849	1906.307386	5.517338	-0.061935	2.395553
330.737249	1914.340901	5.522342	-0.062089	2.400425
331.661522	1922.373534	5.527347	-0.062266	2.405295
332.392989	1930.469814	5.532352	-0.062408	2.410179
333.243202	1938.546418	5.537357	-0.062571	2.415050
334.164472	1946.583842	5.542362	-0.062748	2.419893
334.865836	1954.658008	5.547366	-0.062884	2.424731
335.605542	1962.773024	5.552371	-0.063027	2.429586
336.027859	1970.887004	5.557376	-0.063111	2.434406
336.957183	1978.898737	5.562381	-0.063289	2.439195
337.640813	1986.942036	5.567386	-0.063422	2.443975
338.316966	1995.011052	5.572390	-0.063553	2.448759
338.563841	2003.137404	5.577395	-0.063604	2.453535
339.240191	2011.165190	5.582400	-0.063735	2.458276
340.197104	2019.198586	5.587405	-0.063919	2.463033
340.892148	2027.244646	5.592410	-0.064053	2.467768
341.214596	2035.366201	5.597414	-0.064119	2.472510
341.479452	2043.475247	5.602419	-0.064173	2.477230
341.706216	2051.539020	5.607424	-0.064221	2.481912
342.136260	2059.616015	5.612429	-0.064306	2.486609
342.527029	2067.671660	5.617434	-0.064384	2.491281
343.557054	2075.677486	5.622438	-0.064581	2.495964
344.372141	2083.722570	5.627443	-0.064738	2.500644
345.102962	2091.741288	5.632448	-0.064879	2.505293
345.896231	2099.830120	5.637453	-0.065032	2.509979
346.427082	2107.900631	5.642458	-0.065136	2.514626
346.960448	2115.948806	5.647462	-0.065241	2.519252
347.670829	2123.984092	5.652467	-0.065378	2.523875
348.000270	2132.091283	5.657472	-0.065445	2.528502
348.549687	2140.164333	5.662477	-0.065553	2.533117
349.066518	2148.228470	5.667482	-0.065654	2.537716
349.521738	2156.298305	5.672486	-0.065744	2.542306
350.248068	2164.327562	5.677491	-0.065885	2.546884
350.732888	2172.405895	5.682496	-0.065980	2.551464
351.678787	2180.434997	5.687501	-0.066161	2.556041
351.868131	2188.524093	5.692506	-0.066202	2.560589
352.680141	2196.542712	5.697510	-0.066358	2.565134
353.942906	2204.512724	5.702515	-0.066599	2.569675
355.224274	2212.512085	5.707520	-0.066842	2.574226
355.847498	2220.620874	5.712525	-0.066964	2.578783
356.598303	2228.671206	5.717530	-0.067109	2.583308
357.696696	2236.709490	5.722534	-0.067318	2.587843
359.111458	2244.801199	5.727539	-0.067587	2.592421
360.147425	2252.830746	5.732544	-0.067785	2.596930
361.364052	2260.831552	5.737549	-0.068017	2.601428
362.151409	2268.895349	5.742554	-0.068169	2.605923
363.390640	2276.905106	5.747558	-0.068405	2.610412
364.323488	2285.002981	5.752563	-0.068584	2.614919
365.077491	2293.030188	5.757568	-0.068729	2.619368
365.754931	2301.120464	5.762573	-0.068861	2.623839
366.565825	2309.188629	5.767578	-0.069017	2.628298
366.474268	2317.405622	5.772582	-0.069005	2.632770
368.137384	2325.266686	5.777587	-0.069320	2.637159
368.839251	2333.316837	5.782592	-0.069456	2.641579
369.324229	2341.432174	5.787597	-0.069552	2.646011
369.628291	2349.545052	5.792602	-0.069613	2.650423
370.273358	2357.588036	5.797606	-0.069739	2.654813
371.065595	2365.612450	5.802611	-0.069892	2.659194
371.987654	2373.603907	5.807616	-0.070068	2.663560
372.773928	2381.692491	5.812621	-0.070220	2.667961
373.339552	2389.768346	5.817626	-0.070331	2.672333
374.366431	2397.760061	5.822630	-0.070527	2.676683
375.004405	2405.838499	5.827635	-0.070651	2.681047
375.687387	2413.857741	5.832640	-0.070783	2.685375
376.576940	2421.937299	5.837645	-0.070954	2.689742
377.229335	2429.990043	5.842650	-0.071081	2.694071
377.913526	2438.030536	5.847654	-0.071214	2.698389
378.775091	2446.067584	5.852659	-0.071379	2.702710
379.618794	2454.103064	5.857664	-0.071542	2.707021
380.344945	2462.183746	5.862669	-0.071682	2.711342
380.712192	2470.252899	5.867674	-0.071756	2.715627
381.501470	2478.284328	5.872678	-0.071908	2.719912
381.730348	2486.395499	5.877683	-0.071956	2.724197
381.930470	2494.481416	5.882688	-0.071998	2.728460
382.394109	2502.563490	5.887693	-0.072090	2.732730
383.227453	2510.542219	5.892698	-0.072250	2.736963
383.820220	2518.572602	5.897702	-0.072366	2.741201
384.167020	2526.660569	5.902707	-0.072436	2.745447
384.354005	2534.734711	5.907712	-0.072476	2.749670
384.720721	2542.866076	5.912717	-0.072549	2.753927
384.941297	2550.879107	5.917722	-0.072596	2.758106
385.403659	2558.906554	5.922726	-0.072687	2.762302
386.145147	2566.916572	5.927731	-0.072830	2.766499
386.820274	2574.911986	5.932736	-0.072961	2.770678
387.403839	2582.974161	5.937741	-0.073075	2.774880
388.636078	2590.878309	5.942746	-0.073310	2.779033
388.797861	2599.019860	5.947750	-0.073345	2.783237
389.288298	2607.109873	5.952755	-0.073442	2.787428
389.875550	2615.106759	5.957760	-0.073556	2.791570
390.657368	2623.121208	5.962765	-0.073707	2.795727
390.956092	2631.217066	5.967770	-0.073768	2.799891
391.483292	2639.245450	5.972774	-0.073871	2.804027
391.966731	2647.321668	5.977779	-0.073966	2.808179
392.051921	2655.415165	5.982784	-0.073988	2.812310
392.604373	2663.459248	5.987789	-0.074096	2.816438
392.901409	2671.506197	5.992794	-0.074156	2.820545
393.444409	2679.526254	5.997798	-0.074262	2.824647
393.592325	2687.632686	6.002803	-0.074295	2.828764
394.087405	2695.638936	6.007808	-0.074393	2.832845
394.813562	2703.650318	6.012813	-0.074533	2.836935
395.536016	2711.627043	6.017818	-0.074673	2.841002
395.614967	2719.706457	6.022822	-0.074693	2.845078
396.278777	2727.731453	6.027827	-0.074822	2.849153
396.294514	2735.847670	6.032832	-0.074830	2.853232
396.845945	2743.869195	6.037837	-0.074938	2.857288
397.548010	2751.855414	6.042842	-0.075074	2.861329
398.018597	2759.898260	6.047846	-0.075166	2.865379
398.597667	2767.964885	6.052851	-0.075280	2.869441
399.169805	2776.005849	6.057856	-0.075391	2.873484
399.611135	2784.069431	6.062861	-0.075479	2.877526
399.833170	2792.114613	6.067866	-0.075525	2.881540
399.949626	2800.189912	6.072870	-0.075552	2.885558
400.398647	2808.219122	6.077875	-0.075641	2.889565
401.089712	2816.196713	6.082880	-0.075775	2.893555
401.306167	2824.317005	6.087885	-0.075820	2.897584
401.520111	2832.361090	6.092890	-0.075866	2.901569
401.932577	2840.377806	6.097894	-0.075948	2.905546
402.402404	2848.413322	6.102899	-0.076040	2.909530
403.101885	2856.456249	6.107904	-0.076176	2.913525
403.798640	2864.462573	6.112909	-0.076311	2.917496
403.928192	2872.546029	6.117914	-0.076340	2.921468
404.026524	2880.589802	6.122918	-0.076364	2.925414
404.115498	2888.680010	6.127923	-0.076385	2.929377
404.698557	2896.654683	6.132928	-0.076499	2.933304
405.099924	2904.683985	6.137933	-0.076579	2.937243
405.686648	2912.689249	6.142938	-0.076694	2.941175
405.742177	2920.761675	6.147942	-0.076709	2.945106
405.836239	2928.865150	6.152947	-0.076732	2.949049
406.169815	2936.883921	6.157952	-0.076799	2.952958
406.974920	2944.846778	6.162957	-0.076954	2.956860
407.076575	2952.906599	6.167962	-0.076978	2.960766
407.326415	2960.919711	6.172966	-0.077030	2.964652
407.713290	2968.979791	6.177971	-0.077107	2.968563
408.173671	2977.004548	6.182976	-0.077198	2.972456
408.256204	2985.123605	6.187981	-0.077219	2.976369
408.408556	2993.175069	6.192986	-0.077253	2.980248
408.702406	3001.166625	6.197990	-0.077313	2.984100
408.959276	3009.244291	6.202995	-0.077366	2.987987
409.479982	3017.226783	6.208000	-0.077468	2.991837
409.748931	3025.319211	6.213005	-0.077523	2.995721
410.327995	3033.267610	6.218010	-0.077636	2.999548
410.871132	3041.226362	6.223014	-0.077742	3.003372
411.106738	3049.339005	6.228019	-0.077792	3.007249
411.030312	3057.439506	6.233024	-0.077783	3.011100
411.673453	3065.441376	6.238029	-0.077908	3.014935
412.013426	3073.473936	6.243034	-0.077976	3.018765
412.245010	3081.485464	6.248038	-0.078024	3.022574
412.491164	3089.615896	6.253043	-0.078076	3.026435
413.145924	3097.561989	6.258048	-0.078203	3.030225
413.217822	3105.635680	6.263053	-0.078221	3.034041
413.333586	3113.683860	6.268058	-0.078248	3.037842
413.551404	3121.721588	6.273062	-0.078294	3.041639
414.084671	3129.730637	6.278067	-0.078398	3.045432
414.275632	3137.761619	6.283072	-0.078439	3.049215
414.402248	3145.853297	6.288077	-0.078468	3.053018
414.429369	3153.928119	6.293082	-0.078478	3.056804
415.098657	3161.892512	6.298086	-0.078608	3.060564
415.632226	3169.875048	6.303091	-0.078713	3.064322
415.890334	3177.936184	6.308096	-0.078766	3.068098
415.971572	3186.065770	6.313101	-0.078786	3.071894
416.217859	3194.120781	6.318106	-0.078837	3.075657
416.400125	3202.068792	6.323110	-0.078876	3.079363
416.561884	3210.142198	6.328115	-0.078912	3.083122
417.123568	3218.108676	6.333120	-0.079022	3.086846
417.442024	3226.173192	6.338125	-0.079086	3.090599
418.265343	3234.112017	6.343130	-0.079245	3.094313
418.593209	3242.167824	6.348134	-0.079311	3.098053
419.040287	3250.228237	6.353139	-0.079399	3.101796
419.498954	3258.263590	6.358144	-0.079490	3.105524
420.233367	3266.274250	6.363149	-0.079632	3.109248
420.370314	3274.348250	6.368154	-0.079663	3.112970
420.674684	3282.387980	6.373158	-0.079725	3.116679
421.011407	3290.443054	6.378163	-0.079792	3.120392
421.240917	3298.403481	6.383168	-0.079840	3.124052
421.483667	3306.496197	6.388173	-0.079891	3.127769
422.213432	3314.472270	6.393178	-0.080032	3.131450
422.597634	3322.532827	6.398182	-0.080109	3.135150
422.966699	3330.591605	6.403187	-0.080183	3.138844
423.144222	3338.637241	6.408192	-0.080221	3.142519
423.940292	3346.629166	6.413197	-0.080374	3.146193
423.975601	3354.714856	6.418202	-0.080386	3.149871
424.303589	3362.735798	6.423206	-0.080452	3.153529
424.707285	3370.750519	6.428211	-0.080533	3.157182
424.980108	3378.768960	6.433216	-0.080589	3.160828
424.916653	3386.838699	6.438221	-0.080582	3.164477
425.580547	3394.832145	6.443226	-0.080711	3.168120
425.696499	3402.909322	6.448230	-0.080738	3.171772
426.091926	3410.943741	6.453235	-0.080817	3.175413
426.401489	3418.929357	6.458240	-0.080880	3.179024
426.650857	3426.980033	6.463245	-0.080931	3.182657
427.304745	3435.002998	6.468250	-0.081058	3.186291
427.724125	3443.012867	6.473254	-0.081142	3.189905
428.159382	3451.059766	6.478259	-0.081228	3.193532
428.442471	3459.086732	6.483264	-0.081286	3.197140
428.590401	3467.166602	6.488269	-0.081319	3.200761
428.812500	3475.178700	6.493274	-0.081365	3.204351
429.053245	3483.207917	6.498278	-0.081415	3.207945
429.727530	3491.249062	6.503283	-0.081546	3.211559
430.003125	3499.268813	6.508288	-0.081602	3.215143
430.651612	3507.270671	6.513293	-0.081728	3.218730
431.026153	3515.344300	6.518298	-0.081803	3.222334
431.083772	3523.388165	6.523302	-0.081819	3.225906
431.512059	3531.435592	6.528307	-0.081904	3.229492
432.077146	3539.417936	6.533312	-0.082015	3.233051
432.487604	3547.462024	6.538317	-0.082096	3.236627
432.950751	3555.452312	6.543322	-0.082188	3.240177
433.256921	3563.449305	6.548326	-0.082250	3.243719
433.630160	3571.543160	6.553331	-0.082325	3.247303
434.003646	3579.558889	6.558336	-0.082400	3.250849
434.304781	3587.602360	6.563341	-0.082461	3.254400
434.650695	3595.621472	6.568346	-0.082530	3.257938
434.884083	3603.649227	6.573350	-0.082579	3.261472
434.996541	3611.766083	6.578355	-0.082605	3.265035
435.959594	3619.662246	6.583360	-0.082790	3.268533
436.579519	3627.703153	6.588365	-0.082910	3.272076
436.678864	3635.816612	6.593370	-0.082934	3.275626
436.982302	3643.800743	6.598374	-0.082996	3.279124
437.499307	3651.822733	6.603379	-0.083097	3.282643
437.597765	3659.868115	6.608384	-0.083121	3.286152
438.102836	3667.871496	6.613389	-0.083220	3.289655
438.878816	3675.892107	6.618394	-0.083370	3.293172
438.801411	3683.942924	6.623398	-0.083361	3.296665
439.157592	3691.985356	6.628403	-0.083432	3.300168
439.585951	3699.982420	6.633408	-0.083517	3.303650
439.965337	3708.048836	6.638413	-0.083593	3.307156
439.930770	3716.128692	6.643418	-0.083592	3.310648
440.288658	3724.117519	6.648422	-0.083664	3.314113
440.823499	3732.125840	6.653427	-0.083769	3.317589
441.019497	3740.177424	6.658432	-0.083810	3.321067
441.312269	3748.199910	6.663437	-0.083870	3.324532
441.728678	3756.227917	6.668442	-0.083953	3.328001
441.867152	3764.262257	6.673446	-0.083984	3.331458
442.086603	3772.334967	6.678451	-0.084030	3.334931
442.475717	3780.316718	6.683456	-0.084108	3.338368
442.693486	3788.375951	6.688461	-0.084153	3.341829
442.940329	3796.406781	6.693466	-0.084204	3.345274
443.138102	3804.415242	6.698470	-0.084247	3.348704
443.643637	3812.458489	6.703475	-0.084346	3.352158
443.508985	3820.517844	6.708480	-0.084326	3.355590
443.669443	3828.498841	6.713485	-0.084361	3.358997
444.007500	3836.532024	6.718490	-0.084429	3.362429
444.060440	3844.588028	6.723494	-0.084444	3.365857
444.689027	3852.564229	6.728499	-0.084567	3.369268
444.663060	3860.619318	6.733504	-0.084567	3.372685
445.117732	3868.673589	6.738509	-0.084657	3.376117
445.350421	3876.676438	6.743514	-0.084705	3.379514
445.691535	3884.659703	6.748518	-0.084774	3.382904
446.258695	3892.745622	6.753523	-0.084885	3.386342
446.169643	3900.785815	6.758528	-0.084874	3.389733
446.540729	3908.843717	6.763533	-0.084948	3.393145
446.669871	3916.909714	6.768538	-0.084977	3.396549
446.754007	3924.900122	6.773542	-0.084998	3.399915
447.124086	3932.871342	6.778547	-0.085072	3.403280
447.495746	3940.884703	6.783552	-0.085147	3.406660
447.802272	3948.914666	6.788557	-0.085209	3.410041
447.909308	3956.994089	6.793562	-0.085234	3.413432
447.879994	3965.032623	6.798566	-0.085234	3.416798
448.326747	3973.028830	6.803571	-0.085322	3.420159
448.768909	3980.959527	6.808576	-0.085410	3.423490
448.995575	3989.066435	6.813581	-0.085457	3.426883
449.067553	3997.162138	6.818586	-0.085476	3.430263
449.187106	4005.123278	6.823590	-0.085503	3.433585
449.797825	4013.144637	6.828595	-0.085622	3.436946
449.748822	4021.194724	6.833600	-0.085618	3.440293
450.190282	4029.161193	6.838605	-0.085706	3.443618
450.515013	4037.199325	6.843610	-0.085771	3.446966
450.641640	4045.235284	6.848614	-0.085800	3.450303
450.666961	4053.322791	6.853619	-0.085810	3.453655
451.233900	4061.277476	6.858624	-0.085921	3.456967
451.648958	4069.302252	6.863629	-0.086003	3.460299
451.995395	4077.321627	6.868634	-0.086073	3.463624
452.262091	4085.368946	6.873638	-0.086128	3.466954
452.664552	4093.414699	6.878643	-0.086208	3.470285
452.408813	4101.488733	6.883648	-0.086166	3.473603
452.564165	4109.521437	6.888653	-0.086200	3.476914
453.243829	4117.455321	6.893658	-0.086332	3.480198
453.138278	4125.478752	6.898662	-0.086317	3.483490
453.590233	4133.530769	6.903667	-0.086407	3.486809
453.424756	4141.579563	6.908672	-0.086381	3.490103
453.690857	4149.632177	6.913677	-0.086436	3.493410
453.614323	4157.703622	6.918682	-0.086427	3.496710
454.011898	4165.663504	6.923686	-0.086506	3.499977
454.609130	4173.645891	6.928691	-0.086622	3.503257
454.543072	4181.733280	6.933696	-0.086615	3.506554
455.112581	4189.717189	6.938701	-0.086727	3.509827
455.486649	4197.716419	6.943706	-0.086801	3.513097
455.580858	4205.762744	6.948710	-0.086824	3.516374
456.031057	4213.807398	6.953715	-0.086913	3.519658
456.351340	4221.769101	6.958720	-0.086978	3.522902
456.553092	4229.868325	6.963725	-0.087021	3.526194
457.054902	4237.868085	6.968730	-0.087120	3.529452
457.099060	4245.902975	6.973734	-0.087133	3.532708
457.126403	4253.996773	6.978739	-0.087143	3.535983
457.280939	4261.963183	6.983744	-0.087177	3.539208
457.792628	4269.984688	6.988749	-0.087278	3.542464
457.965553	4278.026453	6.993754	-0.087315	3.545714
458.145421	4286.030990	6.998758	-0.087354	3.548946
458.725334	4294.111101	7.003763	-0.087467	3.552218
458.824401	4302.132028	7.008768	-0.087491	3.555448
459.008500	4310.125146	7.013773	-0.087530	3.558667
459.311130	4318.145454	7.018778	-0.087592	3.561897
459.556706	4326.119088	7.023782	-0.087643	3.565104
460.011467	4334.132681	7.028787	-0.087733	3.568330
459.964979	4342.227782	7.033792	-0.087729	3.571571
460.220767	4350.232803	7.038797	-0.087782	3.574782
460.803664	4358.224000	7.043802	-0.087896	3.577995
460.935330	4366.272465	7.048806	-0.087925	3.581213
461.489302	4374.249328	7.053811	-0.088034	3.584413
461.899241	4382.269248	7.058816	-0.088115	3.587623
462.152632	4390.345674	7.063821	-0.088168	3.590848
462.192286	4398.365085	7.068826	-0.088180	3.594040
462.631120	4406.378213	7.073830	-0.088267	3.597240
462.933971	4414.425094	7.078835	-0.088329	3.600445
462.806936	4422.449138	7.083840	-0.088310	3.603627
463.018198	4430.525812	7.088845	-0.088355	3.606836
463.271441	4438.539745	7.093850	-0.088407	3.610018
463.288720	4446.529745	7.098854	-0.088416	3.613182
464.050629	4454.573550	7.103859	-0.088563	3.616385
464.070219	4462.576860	7.108864	-0.088572	3.619548
464.340885	4470.612756	7.113869	-0.088627	3.622729
464.473674	4478.684672	7.118874	-0.088657	3.625916
464.577560	4486.646148	7.123878	-0.088682	3.629057
464.638957	4494.785738	7.128883	-0.088699	3.632264
464.982941	4502.727613	7.133888	-0.088768	3.635398
464.997640	4510.721163	7.138893	-0.088776	3.638541
465.378386	4518.743626	7.143898	-0.088852	3.641702
465.490037	4526.702157	7.148902	-0.088878	3.644828
465.784899	4534.771081	7.153907	-0.088938	3.648000
466.001405	4542.816749	7.158912	-0.088984	3.651157
466.334099	4550.810338	7.163917	-0.089051	3.654295
466.534191	4558.860080	7.168922	-0.089093	3.657448
466.917086	4566.867459	7.173926	-0.089170	3.660587
467.258465	4574.864749	7.178931	-0.089238	3.663718
467.328534	4582.906904	7.183936	-0.089257	3.666857
467.824283	4590.931628	7.188941	-0.089354	3.669997
467.985570	4598.990320	7.193946	-0.089389	3.673139
468.365175	4606.979296	7.198950	-0.089465	3.676257
468.464416	4615.010349	7.203955	-0.089489	3.679381
468.539187	4623.026615	7.208960	-0.089508	3.682496
468.746139	4631.092296	7.213965	-0.089552	3.685632
468.882134	4639.116553	7.218970	-0.089583	3.688746
469.244443	4647.137299	7.223974	-0.089655	3.691862
469.748378	4655.173264	7.228979	-0.089754	3.694986
469.851430	4663.178409	7.233984	-0.089779	3.698084
469.700158	4671.255752	7.238989	-0.089756	3.701201
470.147562	4679.230531	7.243994	-0.089844	3.704291
470.099744	4687.286244	7.248998	-0.089841	3.707397
470.409596	4695.338875	7.254003	-0.089903	3.710509
470.400214	4703.386158	7.259008	-0.089907	3.713607
470.575072	4711.355021	7.264013	-0.089945	3.716678
470.819310	4719.336583	7.269018	-0.089995	3.719752
471.062043	4727.314392	7.274022	-0.090046	3.722823
471.278944	4735.426719	7.279027	-0.090091	3.725942
471.154156	4743.422301	7.284032	-0.090073	3.729005
471.528554	4751.432095	7.289037	-0.090148	3.732083
471.663591	4759.520388	7.294042	-0.090179	3.735183
471.558909	4767.505121	7.299046	-0.090164	3.738235
471.928079	4775.526470	7.304051	-0.090238	3.741309
471.848199	4783.521097	7.309056	-0.090229	3.744361
472.349560	4791.499140	7.314061	-0.090327	3.747417
472.486623	4799.577490	7.319066	-0.090358	3.750500
472.657589	4807.565306	7.324070	-0.090395	3.753547
472.873024	4815.617611	7.329075	-0.090440	3.756617
473.049016	4823.621600	7.334080	-0.090478	3.759666
472.909732	4831.642064	7.339085	-0.090458	3.762710
473.086460	4839.690356	7.344090	-0.090496	3.765771
473.410635	4847.662831	7.349094	-0.090561	3.768803
473.618690	4855.697695	7.354099	-0.090605	3.771854
473.982980	4863.721250	7.359104	-0.090678	3.774902
474.450521	4871.721156	7.364109	-0.090771	3.777940
474.662706	4879.803709	7.369114	-0.090815	3.781002
474.749721	4887.765026	7.374118	-0.090837	3.784012
475.290937	4895.823274	7.379123	-0.090943	3.787067
475.553858	4903.841472	7.384128	-0.090997	3.790098
476.144278	4911.809045	7.389133	-0.091112	3.793114
476.236808	4919.946035	7.394138	-0.091134	3.796181
476.526393	4927.846218	7.399142	-0.091194	3.799161
476.950792	4935.896629	7.404147	-0.091278	3.802197
476.876594	4943.959439	7.409152	-0.091269	3.805225
477.328834	4951.959768	7.414157	-0.091359	3.808239
477.618345	4960.030445	7.419162	-0.091418	3.811273
477.472663	4968.037683	7.424166	-0.091396	3.814271
477.426820	4976.112808	7.429171	-0.091393	3.817294
478.323409	4984.046135	7.434176	-0.091565	3.820283
478.601657	4992.026574	7.439181	-0.091622	3.823273
478.755623	5000.141036	7.444186	-0.091656	3.826308
478.752080	5008.166637	7.449190	-0.091660	3.829305
478.905813	5016.212824	7.454195	-0.091694	3.832310
479.190323	5024.185762	7.459200	-0.091752	3.835288
479.431856	5032.176734	7.464205	-0.091802	3.838269
479.311958	5040.302258	7.469210	-0.091785	3.841291
479.453346	5048.222616	7.474214	-0.091817	3.844239
479.771391	5056.270139	7.479219	-0.091881	3.847236
479.672700	5064.339421	7.484224	-0.091868	3.850230
479.803336	5072.337946	7.489229	-0.091898	3.853200
480.514488	5080.332597	7.494234	-0.092035	3.856179
480.802737	5088.269913	7.499238	-0.092094	3.859125
480.313203	5096.463869	7.504243	-0.092008	3.862148
480.605568	5104.377890	7.509248	-0.092068	3.865081
480.701873	5112.469564	7.514253	-0.092091	3.868074
481.242078	5120.457444	7.519258	-0.092197	3.871035
481.295906	5128.603906	7.524262	-0.092212	3.874042
482.058188	5136.526166	7.529267	-0.092359	3.876978
482.420692	5144.491181	7.534272	-0.092432	3.879920
482.194355	5152.532870	7.539277	-0.092395	3.882876
482.683860	5160.515162	7.544282	-0.092491	3.885822
482.786606	5168.547729	7.549286	-0.092516	3.888777
482.900453	5176.582454	7.554291	-0.092542	3.891730
482.663558	5184.646552	7.559296	-0.092503	3.894685
483.126239	5192.598098	7.564301	-0.092594	3.897611
483.425489	5200.625957	7.569306	-0.092655	3.900558
483.443990	5208.611069	7.574310	-0.092664	3.903483
484.092509	5216.641171	7.579315	-0.092790	3.906434
484.371162	5224.655409	7.584320	-0.092847	3.909369
484.509652	5232.700307	7.589325	-0.092878	3.912311
484.683549	5240.764005	7.594330	-0.092916	3.915258
484.955972	5248.701980	7.599334	-0.092972	3.918159
485.242191	5256.800319	7.604339	-0.093030	3.921117
485.062028	5264.793726	7.609344	-0.093002	3.924025
485.494054	5272.805836	7.614349	-0.093087	3.926949
485.446947	5280.897835	7.619354	-0.093084	3.929891
485.172648	5288.974932	7.624358	-0.093038	3.932822
485.915420	5296.932649	7.629363	-0.093182	3.935726
486.496891	5304.897068	7.634368	-0.093295	3.938627
486.566287	5312.966903	7.639373	-0.093313	3.941554
486.805890	5320.925536	7.644378	-0.093363	3.944442
486.885140	5328.964633	7.649382	-0.093383	3.947354
487.191082	5337.026783	7.654387	-0.093445	3.950277
486.860830	5345.101890	7.659392	-0.093389	3.953190
487.386892	5353.058787	7.664397	-0.093492	3.956074
487.526302	5361.050476	7.669402	-0.093523	3.958962
487.616856	5369.063473	7.674406	-0.093545	3.961854
487.989022	5377.052008	7.679411	-0.093620	3.964741
488.102776	5385.098253	7.684416	-0.093646	3.967641
488.168423	5393.161474	7.689421	-0.093664	3.970544
488.218635	5401.203599	7.694426	-0.093678	3.973438
488.289646	5409.261032	7.699430	-0.093697	3.976335
488.505690	5417.184315	7.704435	-0.093742	3.979184
488.350448	5425.273114	7.709440	-0.093718	3.982085
488.643049	5433.209533	7.714445	-0.093778	3.984936
488.664831	5441.290205	7.719450	-0.093787	3.987832
488.798103	5449.299076	7.724454	-0.093817	3.990703
488.914536	5457.328538	7.729459	-0.093844	3.993578
488.946680	5465.382672	7.734464	-0.093856	3.996459
488.749542	5473.360776	7.739469	-0.093824	3.999306
489.058040	5481.410897	7.744474	-0.093887	4.002186
489.519113	5489.312797	7.749478	-0.093978	4.005013
490.192939	5497.298189	7.754483	-0.094108	4.007872
490.336414	5505.400877	7.759488	-0.094140	4.010761
490.243014	5513.425649	7.764493	-0.094128	4.013617
490.801736	5521.467461	7.769498	-0.094237	4.016487
491.267811	5529.362263	7.774502	-0.094329	4.019302
491.330451	5537.461345	7.779507	-0.094346	4.022180
491.220460	5545.525694	7.784512	-0.094331	4.025042
491.497303	5553.518448	7.789517	-0.094388	4.027882
491.320342	5561.629828	7.794522	-0.094360	4.030755
491.283951	5569.684228	7.799526	-0.094358	4.033608
491.916710	5577.651041	7.804531	-0.094481	4.036438
492.029350	5585.596433	7.809536	-0.094508	4.039251
491.826474	5593.686775	7.814541	-0.094475	4.042107
492.424228	5601.654794	7.819546	-0.094592	4.044932
492.191464	5609.676435	7.824550	-0.094553	4.047760
492.483805	5617.717047	7.829555	-0.094613	4.050601
492.439483	5625.762069	7.834560	-0.094610	4.053436
492.676092	5633.752728	7.839565	-0.094659	4.056255
492.559191	5641.785516	7.844570	-0.094643	4.059081
492.567008	5649.814092	7.849574	-0.094649	4.061905
493.211421	5657.744790	7.854579	-0.094775	4.064703
493.222517	5665.839616	7.859584	-0.094782	4.067547
493.079276	5673.897692	7.864589	-0.094761	4.070373
493.569526	5681.861744	7.869594	-0.094857	4.073175
493.791384	5689.860513	7.874598	-0.094903	4.075982
494.203355	5697.824011	7.879603	-0.094985	4.078778
494.249797	5705.909972	7.884608	-0.094999	4.081609
494.195837	5713.894115	7.889613	-0.094994	4.084401
494.963940	5721.934898	7.894618	-0.095143	4.087223
494.679045	5730.000361	7.899622	-0.095095	4.090037
494.830890	5738.032076	7.904627	-0.095128	4.092843
495.177828	5746.013153	7.909632	-0.095198	4.095632
495.583419	5753.973279	7.914637	-0.095279	4.098413
495.828429	5762.063740	7.919642	-0.095330	4.101235
496.354753	5769.975555	7.924646	-0.095433	4.103997
496.264255	5778.099579	7.929651	-0.095421	4.106822
496.656177	5786.102363	7.934656	-0.095499	4.109609
496.759596	5794.137344	7.939661	-0.095524	4.112402
496.428995	5802.222655	7.944666	-0.095468	4.115205
497.154837	5810.122017	7.949670	-0.095608	4.117955
497.465821	5818.135768	7.954675	-0.095671	4.120738
497.410802	5826.152911	7.959680	-0.095666	4.123515
497.368001	5834.197526	7.964685	-0.095663	4.126300
497.490952	5842.235845	7.969690	-0.095691	4.129083
497.166330	5850.289357	7.974694	-0.095636	4.131863
497.398253	5858.256717	7.979699	-0.095685	4.134619
497.852515	5866.278149	7.984704	-0.095774	4.137395
498.301077	5874.266459	7.989709	-0.095863	4.140157
498.710598	5882.256312	7.994714	-0.095944	4.142918
498.491843	5890.317425	7.999718	-0.095909	4.145693
499.083177	5898.323318	8.004723	-0.096024	4.148458
498.916914	5906.476778	8.009728	-0.095999	4.151261
498.875938	5914.404122	8.014733	-0.095996	4.153987
499.480983	5922.429666	8.019738	-0.096114	4.156753
499.925361	5930.341094	8.024742	-0.096202	4.159476
500.082829	5938.412813	8.029747	-0.096236	4.162248
500.187035	5946.432692	8.034752	-0.096261	4.165000
500.379993	5954.469371	8.039757	-0.096302	4.167757
501.030572	5962.479897	8.044762	-0.096429	4.170509
501.229887	5970.511742	8.049766	-0.096471	4.173261
501.479425	5978.581015	8.054771	-0.096523	4.176024
501.658720	5986.569552	8.059776	-0.096561	4.178757
501.631795	5994.628983	8.064781	-0.096561	4.181510
502.055004	6002.570420	8.069786	-0.096645	4.184226
501.920816	6010.691722	8.074790	-0.096626	4.186995
501.912027	6018.689549	8.079795	-0.096629	4.189722
502.135411	6026.791128	8.084800	-0.096676	4.192485
502.610756	6034.731995	8.089805	-0.096770	4.195194
502.801616	6042.709654	8.094810	-0.096810	4.197911
502.795604	6050.752319	8.099814	-0.096815	4.200646
503.163075	6058.705289	8.104819	-0.096888	4.203353
503.020129	6066.798788	8.109824	-0.096867	4.206100
503.031534	6074.730580	8.114829	-0.096874	4.208792
503.421074	6082.815512	8.119834	-0.096952	4.211538
504.103064	6090.743590	8.124838	-0.097084	4.214233
504.329291	6098.826123	8.129843	-0.097131	4.216973
504.172398	6106.847691	8.134848	-0.097107	4.219687
504.038769	6114.914257	8.139853	-0.097088	4.222414
504.535490	6122.840695	8.144858	-0.097185	4.225099
504.986581	6130.869936	8.149862	-0.097275	4.227816
504.905217	6138.929259	8.154867	-0.097265	4.230537
504.929856	6146.957179	8.159872	-0.097275	4.233246
504.752750	6154.975092	8.164877	-0.097247	4.235947
505.376686	6162.947905	8.169882	-0.097368	4.238640
505.347274	6170.999452	8.174886	-0.097368	4.241352
505.812886	6178.906829	8.179891	-0.097460	4.244017
505.819384	6187.042831	8.184896	-0.097466	4.246754
505.801559	6195.032425	8.189901	-0.097468	4.249439
506.157246	6203.088672	8.194906	-0.097540	4.252149
506.141942	6211.061439	8.199910	-0.097542	4.254825
506.415078	6219.065350	8.204915	-0.097598	4.257513
506.408812	6227.150445	8.209920	-0.097602	4.260223
506.532814	6235.053360	8.214925	-0.097630	4.262872
506.485279	6243.162896	8.219930	-0.097627	4.265587
506.420554	6251.228604	8.224934	-0.097620	4.268285
506.689892	6259.209772	8.229939	-0.097675	4.270957
506.902802	6267.249947	8.234944	-0.097720	4.273646
507.142808	6275.168302	8.239949	-0.097770	4.276293
507.213166	6283.247872	8.244954	-0.097788	4.278990
507.496004	6291.249111	8.249958	-0.097846	4.281662
508.162545	6299.144909	8.254963	-0.097975	4.284300
508.457115	6307.237644	8.259968	-0.098035	4.286998
508.750708	6315.175230	8.264973	-0.098095	4.289644
509.052852	6323.319419	8.269978	-0.098157	4.292356
509.071376	6331.327901	8.274982	-0.098165	4.295019
508.942592	6339.387476	8.279987	-0.098147	4.297696
509.234754	6347.389484	8.284992	-0.098206	4.300356
509.683651	6355.371871	8.289997	-0.098295	4.303009
509.721333	6363.430991	8.295002	-0.098307	4.305683
509.820530	6371.444605	8.300006	-0.098331	4.308340
510.245799	6379.456026	8.305011	-0.098415	4.310997
510.356851	6387.420914	8.310016	-0.098441	4.313635
510.399927	6395.435819	8.315021	-0.098455	4.316287
510.326291	6403.472687	8.320026	-0.098446	4.318944
510.315414	6411.512966	8.325030	-0.098449	4.321601
510.610951	6419.478984	8.330035	-0.098509	4.324234
510.700752	6427.512594	8.335040	-0.098531	4.326886
510.665941	6435.489732	8.340045	-0.098530	4.329517
510.718898	6443.630719	8.345050	-0.098545	4.332201
510.857020	6451.586163	8.350054	-0.098576	4.334823
511.359378	6459.563723	8.355059	-0.098675	4.337453
511.539013	6467.604946	8.360064	-0.098714	4.340100
511.789893	6475.620107	8.365069	-0.098765	4.342738
512.056666	6483.630391	8.370074	-0.098820	4.345372
512.005740	6491.646049	8.375078	-0.098816	4.348004
512.394894	6499.646399	8.380083	-0.098894	4.350633
512.781232	6507.687992	8.385088	-0.098971	4.353273
512.568645	6515.753295	8.390093	-0.098937	4.355916
512.892407	6523.724231	8.395098	-0.099002	4.358530
512.666628	6531.830979	8.400102	-0.098965	4.361182
512.756600	6539.725977	8.405107	-0.098987	4.363767
512.649351	6547.830345	8.410112	-0.098972	4.366416
512.427194	6555.845466	8.415117	-0.098936	4.369034
513.255021	6563.828543	8.420122	-0.099096	4.371647
513.395211	6571.777091	8.425126	-0.099127	4.374243
513.472791	6579.858993	8.430131	-0.099147	4.376880
513.004983	6587.938443	8.435136	-0.099065	4.379511
513.614930	6595.895950	8.440141	-0.099183	4.382108
513.839892	6603.890859	8.445146	-0.099231	4.384713
513.864629	6611.935742	8.450150	-0.099240	4.387332
514.101754	6619.973714	8.455155	-0.099290	4.389948
514.564105	6627.959492	8.460160	-0.099381	4.392546
515.214017	6635.890932	8.465165	-0.099507	4.395127
515.535336	6643.945917	8.470170	-0.099572	4.397744
515.509216	6651.969846	8.475174	-0.099573	4.400348
515.713608	6659.988573	8.480179	-0.099616	4.402949
515.906917	6668.045094	8.485184	-0.099657	4.405561
515.720033	6676.087182	8.490189	-0.099628	4.408165
516.287007	6684.151626	8.495194	-0.099738	4.410779
516.075349	6692.161210	8.500198	-0.099704	4.413369
516.443440	6700.191573	8.505203	-0.099778	4.415967
516.638349	6708.194961	8.510208	-0.099819	4.418555
517.177667	6716.211868	8.515213	-0.099925	4.421146
517.051665	6724.209871	8.520218	-0.099907	4.423727
517.273904	6732.249410	8.525222	-0.099953	4.426321
517.104580	6740.319459	8.530227	-0.099927	4.428922
517.559230	6748.364854	8.535232	-0.100017	4.431516
517.204151	6756.302794	8.540237	-0.099956	4.434071
517.585364	6764.341440	8.545242	-0.100032	4.436659
517.835806	6772.317036	8.550246	-0.100084	4.439226
517.769471	6780.423609	8.555251	-0.100077	4.441831
518.064615	6788.367160	8.560256	-0.100137	4.444384
517.931534	6796.382040	8.565261	-0.100117	4.446957
517.922362	6804.459080	8.570266	-0.100121	4.449548
517.954513	6812.451617	8.575271	-0.100132	4.452111
518.165203	6820.437476	8.580275	-0.100177	4.454672
518.023733	6828.483651	8.585280	-0.100156	4.457248
518.685501	6836.380914	8.590285	-0.100284	4.459779
519.117336	6844.417838	8.595290	-0.100369	4.462352
518.945900	6852.477439	8.600295	-0.100343	4.464929
519.553644	6860.480519	8.605299	-0.100461	4.467489
519.042588	6868.595901	8.610304	-0.100371	4.470079
519.828365	6876.467282	8.615309	-0.100523	4.472594
520.554296	6884.505697	8.620314	-0.100663	4.475161
520.015513	6892.563769	8.625319	-0.100568	4.477728
520.654271	6900.538342	8.630323	-0.100692	4.480272
520.805081	6908.596152	8.635328	-0.100725	4.482838
520.497194	6916.614040	8.640333	-0.100673	4.485389
520.652208	6924.668291	8.645338	-0.100707	4.487952
521.055653	6932.642835	8.650343	-0.100788	4.490488
521.159369	6940.667695	8.655347	-0.100812	4.493038
521.341992	6948.693339	8.660352	-0.100851	4.495587
521.578473	6956.690561	8.665357	-0.100901	4.498126
521.807723	6964.718079	8.670362	-0.100949	4.500673
521.405283	6972.744055	8.675367	-0.100879	4.503216
521.635830	6980.730449	8.680371	-0.100927	4.505747
521.717159	6988.774224	8.685376	-0.100947	4.508294
522.243079	6996.696810	8.690381	-0.101050	4.510803
522.608202	7004.781588	8.695386	-0.101124	4.513361
523.165383	7012.769498	8.700391	-0.101233	4.515888
523.102145	7020.769860	8.705395	-0.101226	4.518415
522.992623	7028.879948	8.710400	-0.101211	4.520976
523.158554	7036.779371	8.715405	-0.101247	4.523469
523.025288	7044.891792	8.720410	-0.101227	4.526027
523.458912	7052.806767	8.725415	-0.101313	4.528523
523.073995	7060.946234	8.730419	-0.101247	4.531086
523.531059	7068.915692	8.735424	-0.101337	4.533597
523.512133	7076.920330	8.740429	-0.101339	4.536115
523.743810	7084.882794	8.745434	-0.101387	4.538620
524.225182	7092.913441	8.750439	-0.101482	4.541146
524.037466	7100.908944	8.755443	-0.101452	4.543657
524.591586	7108.963170	8.760448	-0.101561	4.546187
524.788093	7116.914135	8.765453	-0.101602	4.548682
525.290063	7125.002905	8.770458	-0.101701	4.551220
525.410495	7132.997279	8.775463	-0.101729	4.553726
524.880942	7141.112902	8.780467	-0.101635	4.556268
525.365072	7149.014141	8.785472	-0.101731	4.558742
525.126352	7157.120796	8.790477	-0.101692	4.561279
525.510343	7165.009596	8.795482	-0.101768	4.563747
525.828066	7173.089020	8.800487	-0.101833	4.566273
526.070921	7181.016515	8.805491	-0.101883	4.568750
526.211703	7189.199990	8.810496	-0.101915	4.571305
526.049529	7197.173466	8.815501	-0.101890	4.573793
526.413153	7205.207771	8.820506	-0.101962	4.576299
526.184791	7213.169220	8.825511	-0.101925	4.578781
526.408939	7221.217103	8.830515	-0.101972	4.581288
527.136466	7229.144002	8.835520	-0.102113	4.583758
526.856973	7237.238079	8.840525	-0.102066	4.586276
527.039937	7245.211233	8.845530	-0.102105	4.588756
527.149898	7253.263384	8.850535	-0.102131	4.591259
527.370515	7261.242205	8.855539	-0.102177	4.593739
527.490616	7269.346438	8.860544	-0.102205	4.596255
527.454458	7277.244337	8.865549	-0.102203	4.598706
527.475540	7285.345620	8.870554	-0.102212	4.601219
527.630477	7293.212255	8.875559	-0.102246	4.603658
527.864712	7301.297607	8.880563	-0.102295	4.606163
528.343753	7309.305223	8.885568	-0.102390	4.608644
528.677541	7317.315632	8.890573	-0.102457	4.611123
528.410211	7325.362919	8.895578	-0.102412	4.613612
528.704138	7333.429668	8.900583	-0.102472	4.616106
528.869095	7341.382853	8.905587	-0.102508	4.618564
528.949021	7349.498199	8.910592	-0.102528	4.621070
528.767326	7357.435158	8.915597	-0.102500	4.623520
529.092933	7365.447672	8.920602	-0.102566	4.625992
529.406447	7373.427142	8.925607	-0.102629	4.628453
529.387345	7381.482094	8.930611	-0.102631	4.630935
529.655934	7389.497679	8.935616	-0.102686	4.633404
529.765139	7397.541004	8.940621	-0.102712	4.635880
529.780076	7405.511535	8.945626	-0.102720	4.638332
529.833827	7413.560440	8.950631	-0.102735	4.640807
529.891393	7421.522228	8.955635	-0.102751	4.643254
530.027549	7429.605206	8.960640	-0.102781	4.645737
530.481916	7437.506700	8.965645	-0.102871	4.648163
530.791228	7445.624036	8.970650	-0.102934	4.650654
530.611773	7453.654622	8.975655	-0.102906	4.653117
530.464355	7461.693522	8.980659	-0.102883	4.655581
531.139912	7469.603422	8.985664	-0.103014	4.658004
530.950693	7477.669112	8.990669	-0.102984	4.660474
530.838167	7485.739169	8.995674	-0.102969	4.662944
530.500899	7493.768050	9.000679	-0.102911	4.665400
530.853419	7501.726090	9.005683	-0.102982	4.667832
531.101290	7509.762760	9.010688	-0.103033	4.670288
531.362243	7517.729154	9.015693	-0.103087	4.672721
531.502417	7525.817103	9.020698	-0.103118	4.675189
531.626850	7533.821306	9.025703	-0.103147	4.677631
531.838843	7541.778835	9.030707	-0.103191	4.680057
532.343902	7549.778522	9.035712	-0.103291	4.682494
532.230492	7557.801775	9.040717	-0.103275	4.684938
532.282196	7565.851380	9.045722	-0.103290	4.687389
532.182489	7573.882014	9.050727	-0.103276	4.689832
532.674467	7581.876259	9.055731	-0.103373	4.692263
532.991021	7589.855554	9.060736	-0.103437	4.694688
532.832840	7597.900581	9.065741	-0.103413	4.697132
533.250909	7605.903229	9.070746	-0.103496	4.699561
533.313786	7613.949522	9.075751	-0.103513	4.702003
533.474613	7621.885241	9.080755	-0.103548	4.704409
533.594803	7630.053552	9.085760	-0.103576	4.706886
533.737459	7637.956318	9.090765	-0.103607	4.709280
533.912378	7646.057220	9.095770	-0.103645	4.711733
534.187236	7654.003116	9.100775	-0.103702	4.714137
534.477432	7662.073020	9.105779	-0.103761	4.716578
534.495987	7670.027718	9.110784	-0.103770	4.718983
534.500881	7678.097995	9.115789	-0.103776	4.721422
534.978500	7686.033047	9.120794	-0.103870	4.723818
534.750620	7694.156604	9.125799	-0.103833	4.726271
534.848981	7702.049683	9.130803	-0.103856	4.728652
534.706025	7710.235941	9.135808	-0.103835	4.731122
534.613978	7718.218585	9.140813	-0.103823	4.733528
534.872058	7726.257775	9.145818	-0.103876	4.735950
535.067948	7734.205275	9.150823	-0.103918	4.738342
535.641207	7742.150659	9.155827	-0.104030	4.740732
535.335527	7750.271396	9.160832	-0.103978	4.743176
535.319080	7758.211759	9.165837	-0.103980	4.745563
535.439525	7766.262290	9.170842	-0.104008	4.747982
535.855278	7774.327972	9.175847	-0.104090	4.750403
535.912825	7782.280198	9.180851	-0.104106	4.752791
536.418543	7790.301049	9.185856	-0.104206	4.755196
536.547741	7798.336072	9.190861	-0.104235	4.757605
536.672852	7806.371018	9.195866	-0.104263	4.760013
536.668474	7814.366053	9.200871	-0.104268	4.762408
536.596237	7822.362339	9.205875	-0.104260	4.764803
537.313157	7830.370851	9.210880	-0.104398	4.767197
537.421757	7838.362600	9.215885	-0.104424	4.769588
537.604496	7846.399944	9.220890	-0.104463	4.771990
537.731976	7854.461710	9.225895	-0.104492	4.774399
537.639016	7862.450899	9.230899	-0.104480	4.776785
537.905900	7870.474310	9.235904	-0.104535	4.779179
538.034812	7878.501301	9.240909	-0.104564	4.781574
538.100158	7886.470890	9.245914	-0.104581	4.783950
537.836953	7894.581973	9.250919	-0.104538	4.786369
537.888884	7902.506988	9.255923	-0.104552	4.788730
538.294687	7910.540995	9.260928	-0.104633	4.791121
538.448776	7918.500470	9.265933	-0.104667	4.793489
538.833374	7926.575017	9.270938	-0.104744	4.795889
538.903182	7934.557259	9.275943	-0.104762	4.798263
539.030969	7942.606249	9.280947	-0.104791	4.800654
539.316283	7950.588869	9.285952	-0.104849	4.803024
539.430272	7958.642652	9.290957	-0.104876	4.805414
539.754431	7966.649714	9.295962	-0.104941	4.807789
539.848457	7974.658711	9.300967	-0.104964	4.810164
539.937684	7982.691658	9.305971	-0.104986	4.812545
540.242934	7990.113039	9.310976	-0.105048	4.814742
540.113003	7994.907352	9.315981	-0.105027	4.816163

540.206208	7997.551948	9.320986	-0.105046	4.816946
540.641496	7998.988149	9.325991	-0.105128	4.817369
540.537879	7999.437989	9.330995	-0.105109	4.817502
540.803927	8000.274991	9.336000	-0.105159	4.817749
540.792016	8000.302237	9.341005	-0.105156	4.817757
541.020871	8000.283422	9.346010	-0.105199	4.817751
540.800540	8000.291812	9.351015	-0.105158	4.817754
540.910900	8000.295528	9.356019	-0.105179	4.817755
541.190142	8000.327016	9.361024	-0.105231	4.817763
540.965041	8000.291041	9.366029	-0.105189	4.817753
541.012897	8000.338141	9.371034	-0.105198	4.817767
541.001915	8000.324270	9.376039	-0.105195	4.817763
540.682544	8000.335436	9.381043	-0.105136	4.817768
540.897008	8000.341723	9.386048	-0.105176	4.817768
541.148362	8000.302144	9.391053	-0.105223	4.817756
541.462771	8000.330981	9.396058	-0.105281	4.817763
541.052268	8000.331326	9.401063	-0.105205	4.817765
541.102057	8000.335214	9.406067	-0.105214	4.817766
541.164883	8000.386751	9.411072	-0.105226	4.817781
541.163016	8000.328717	9.416077	-0.105225	4.817763
541.343513	8000.338729	9.421082	-0.105259	4.817766
541.263444	8000.348107	9.426087	-0.105244	4.817769
541.889213	8000.311876	9.431091	-0.105360	4.817755
541.834904	8000.341668	9.436096	-0.105350	4.817764
541.901411	8000.299396	9.441101	-0.105363	4.817752
542.023168	8000.325426	9.446106	-0.105385	4.817759
541.863528	8000.344191	9.451111	-0.105356	4.817765
542.125758	8000.311099	9.456115	-0.105404	4.817754
542.269011	8000.333225	9.461120	-0.105431	4.817760
542.038773	8000.327758	9.466125	-0.105388	4.817759
541.942899	8000.331633	9.471130	-0.105370	4.817761
542.034517	8000.330858	9.476135	-0.105387	4.817760
541.996576	8000.339796	9.481139	-0.105380	4.817763
542.166141	8000.344376	9.486144	-0.105412	4.817764
542.090853	8000.305309	9.491149	-0.105398	4.817753
542.076435	8000.359940	9.496154	-0.105395	4.817769
542.107601	8000.340355	9.501159	-0.105401	4.817763
542.213847	8000.336629	9.506163	-0.105421	4.817761
542.261152	8000.346810	9.511168	-0.105430	4.817764
542.311538	8000.314849	9.516173	-0.105439	4.817754
542.098970	8000.365537	9.521178	-0.105399	4.817770
542.539474	8000.326607	9.526183	-0.105481	4.817757
542.717209	8000.332361	9.531187	-0.105514	4.817758
542.784239	8000.335447	9.536192	-0.105527	4.817758
542.477586	8000.305662	9.541197	-0.105470	4.817751
542.514835	8000.314642	9.546202	-0.105477	4.817753
542.596921	8000.312673	9.551207	-0.105492	4.817753
542.530772	8000.296942	9.556211	-0.105480	4.817748
542.764627	8000.346756	9.561216	-0.105523	4.817762
542.806028	8000.247165	9.566221	-0.105531	4.817732
542.665793	8000.290470	9.571226	-0.105505	4.817746
542.706126	8000.301604	9.576231	-0.105512	4.817749
542.738864	8000.296806	9.581235	-0.105518	4.817747
542.900337	8000.352948	9.586240	-0.105548	4.817763
542.724883	8000.338787	9.591245	-0.105516	4.817760
542.707204	8000.352239	9.596250	-0.105512	4.817764
542.490296	8000.340638	9.601255	-0.105472	4.817761
542.370860	8000.354716	9.606259	-0.105450	4.817766
542.738954	8000.360082	9.611264	-0.105518	4.817766
542.669887	8000.354855	9.616269	-0.105505	4.817765
542.414142	8000.391202	9.621274	-0.105458	4.817777
542.466418	8000.358214	9.626279	-0.105467	4.817767
542.430662	8000.356636	9.631283	-0.105461	4.817766
542.866722	8000.374595	9.636288	-0.105542	4.817770
542.333543	8000.394241	9.641293	-0.105443	4.817778
542.297158	8000.377889	9.646298	-0.105436	4.817773
542.396638	8000.361409	9.651303	-0.105454	4.817768
542.481915	8000.331011	9.656307	-0.105470	4.817758
543.105613	8000.362253	9.661312	-0.105586	4.817765
543.237742	8000.344140	9.666317	-0.105611	4.817759
543.021966	8000.368414	9.671322	-0.105571	4.817767
543.109425	8000.343321	9.676327	-0.105587	4.817759
543.209137	8000.335282	9.681331	-0.105606	4.817757
543.180275	8000.325368	9.686336	-0.105600	4.817754
543.217959	8000.299549	9.691341	-0.105607	4.817746
543.243924	8000.313637	9.696346	-0.105612	4.817750
543.464971	8000.325298	9.701351	-0.105653	4.817753
543.417407	8000.299290	9.706355	-0.105644	4.817745
543.322908	8000.344317	9.711360	-0.105627	4.817759
543.137758	8000.331069	9.716365	-0.105592	4.817756
543.095258	8000.310409	9.721370	-0.105584	4.817750
543.212441	8000.325828	9.726375	-0.105606	4.817754
543.201961	8000.303525	9.731379	-0.105604	4.817747
543.231536	8000.364073	9.736384	-0.105610	4.817765
543.097622	8000.337861	9.741389	-0.105585	4.817758
543.090820	8000.372565	9.746394	-0.105583	4.817768
543.287125	8000.372263	9.751399	-0.105620	4.817767
543.246940	8000.333707	9.756403	-0.105612	4.817756
543.468328	8000.367521	9.761408	-0.105654	4.817765
543.403616	8000.330716	9.766413	-0.105642	4.817754
543.106607	8000.374899	9.771418	-0.105586	4.817769
543.458031	8000.352601	9.776423	-0.105652	4.817761
543.246683	8000.324205	9.781427	-0.105612	4.817753
543.367913	8000.366050	9.786432	-0.105635	4.817765
543.255299	8000.362297	9.791437	-0.105614	4.817764
543.424905	8000.355278	9.796442	-0.105645	4.817762
543.720903	8000.344829	9.801447	-0.105700	4.817757
543.263848	8000.351872	9.806451	-0.105615	4.817761
543.507541	8000.390230	9.811456	-0.105661	4.817772
543.263616	8000.358194	9.816461	-0.105615	4.817763
543.112187	8000.381297	9.821466	-0.105587	4.817771
543.546295	8000.358096	9.826471	-0.105668	4.817762
543.754162	8000.317885	9.831475	-0.105707	4.817749
543.727790	8000.344921	9.836480	-0.105702	4.817757
543.567182	8000.325702	9.841485	-0.105672	4.817752
543.748557	8000.369480	9.846490	-0.105706	4.817764
543.596161	8000.354599	9.851495	-0.105677	4.817761
543.360960	8000.359605	9.856499	-0.105633	4.817763
543.704952	8000.364622	9.861504	-0.105697	4.817763
543.566924	8000.361552	9.866509	-0.105672	4.817763
543.651570	8000.376497	9.871514	-0.105687	4.817767
543.635547	8000.350949	9.876519	-0.105684	4.817759
543.611760	8000.283101	9.881523	-0.105680	4.817739
543.917312	8000.327635	9.886528	-0.105737	4.817751
543.589769	8000.293325	9.891533	-0.105676	4.817743
543.719893	8000.369051	9.896538	-0.105700	4.817764
543.912245	8000.360254	9.901543	-0.105736	4.817761
543.750828	8000.317819	9.906547	-0.105706	4.817749
543.913392	8000.331791	9.911552	-0.105736	4.817753
543.850087	8000.297116	9.916557	-0.105724	4.817743
543.985549	8000.329678	9.921562	-0.105749	4.817752
543.734183	8000.372416	9.926567	-0.105703	4.817765
543.640681	8000.357340	9.931571	-0.105685	4.817761
543.788631	8000.384810	9.936576	-0.105713	4.817769
543.747601	8000.363116	9.941581	-0.105705	4.817763
543.876991	8000.363948	9.946586	-0.105729	4.817762
543.983809	8000.331755	9.951591	-0.105749	4.817752
543.856970	8000.320411	9.956595	-0.105725	4.817749
543.817916	8000.363083	9.961600	-0.105718	4.817762
544.108366	8000.306146	9.966605	-0.105772	4.817744
544.010340	8000.311043	9.971610	-0.105754	4.817746
544.257260	8000.355779	9.976615	-0.105800	4.817758
543.762073	8000.359099	9.981619	-0.105708	4.817761
543.665661	8000.381950	9.986624	-0.105690	4.817768
543.619646	8000.347527	9.991629	-0.105681	4.817758
543.782192	8000.291889	9.996634	-0.105711	4.817741
544.125024	8000.313764	10.001639	-0.105775	4.817746
543.919146	8000.324471	10.006643	-0.105737	4.817750
544.105285	8000.369374	10.011648	-0.105771	4.817763
543.842950	8000.342341	10.016653	-0.105723	4.817756
543.971558	8000.342107	10.021658	-0.105747	4.817755
543.767463	8000.382371	10.026663	-0.105709	4.817768
543.487337	8000.363518	10.031667	-0.105656	4.817764
543.705458	8000.387793	10.036672	-0.105697	4.817770
543.856466	8000.349916	10.041677	-0.105725	4.817758
543.544824	8000.368572	10.046682	-0.105667	4.817765
543.609671	8000.351587	10.051687	-0.105679	4.817760
543.837363	8000.335923	10.056691	-0.105721	4.817754
543.516407	8000.380810	10.061696	-0.105662	4.817769
543.752121	8000.333622	10.066701	-0.105706	4.817754
543.825816	8000.333641	10.071706	-0.105719	4.817753
543.880967	8000.392454	10.076711	-0.105730	4.817771
543.852627	8000.367781	10.081715	-0.105724	4.817763
543.993729	8000.390933	10.086720	-0.105750	4.817770
543.777558	8000.378285	10.091725	-0.105710	4.817767
543.526901	8000.383065	10.096730	-0.105664	4.817769
543.691149	8000.394952	10.101735	-0.105694	4.817772
543.582598	8000.368054	10.106739	-0.105674	4.817765
543.729750	8000.383911	10.111744	-0.105701	4.817769
543.651191	8000.351123	10.116749	-0.105687	4.817759
543.808946	8000.361861	10.121754	-0.105716	4.817762
543.759248	8000.406487	10.126759	-0.105707	4.817775
543.697498	8000.346521	10.131763	-0.105695	4.817758
543.570525	8000.433263	10.136768	-0.105672	4.817784
543.818364	8000.365158	10.141773	-0.105718	4.817763
543.541870	8000.386436	10.146778	-0.105666	4.817770
543.603789	8000.397885	10.151783	-0.105678	4.817773
543.667892	8000.384053	10.156787	-0.105690	4.817769
543.792495	8000.375323	10.161792	-0.105713	4.817766
543.899100	8000.344181	10.166797	-0.105733	4.817756
544.026370	8000.381897	10.171802	-0.105756	4.817767
543.892910	8000.375730	10.176807	-0.105731	4.817766
543.663308	8000.368160	10.181811	-0.105689	4.817764
543.993094	8000.375080	10.186816	-0.105750	4.817765
543.839107	8000.350683	10.191821	-0.105721	4.817758
543.878711	8000.405050	10.196826	-0.105729	4.817774
543.794520	8000.394328	10.201831	-0.105713	4.817772
543.734064	8000.383952	10.206835	-0.105702	4.817769
543.672571	8000.370398	10.211840	-0.105690	4.817765
543.811384	8000.343945	10.216845	-0.105716	4.817757
543.925980	8000.349834	10.221850	-0.105737	4.817758
544.034332	8000.373563	10.226855	-0.105758	4.817764
543.888967	8000.355620	10.231859	-0.105731	4.817760
544.123727	8000.386467	10.236864	-0.105774	4.817768
544.088130	8000.339539	10.241869	-0.105768	4.817754
543.925824	8000.341389	10.246874	-0.105737	4.817755
544.355287	8000.372967	10.251879	-0.105817	4.817763
544.093733	8000.377587	10.256883	-0.105769	4.817765
544.193903	8000.388540	10.261888	-0.105787	4.817768
544.121921	8000.332643	10.266893	-0.105774	4.817752
544.350150	8000.343355	10.271898	-0.105816	4.817754
544.348781	8000.367593	10.276903	-0.105816	4.817761
544.162132	8000.333227	10.281907	-0.105781	4.817752
544.377027	8000.365893	10.286912	-0.105821	4.817761
544.493839	8000.352831	10.291917	-0.105843	4.817756
544.241733	8000.352315	10.296922	-0.105796	4.817757
544.334056	8000.374755	10.301927	-0.105813	4.817763
544.503155	8000.332924	10.306931	-0.105845	4.817750
544.477083	8000.364184	10.311936	-0.105840	4.817760
544.440057	8000.336219	10.316941	-0.105833	4.817752
544.366223	8000.345688	10.321946	-0.105819	4.817755
544.516844	8000.358432	10.326951	-0.105847	4.817758
544.247895	8000.365053	10.331955	-0.105797	4.817761
544.236848	8000.384931	10.336960	-0.105795	4.817767
544.289345	8000.378313	10.341965	-0.105805	4.817765
544.232516	8000.364826	10.346970	-0.105794	4.817761
543.977335	8000.389578	10.351975	-0.105747	4.817769
544.105965	8000.368250	10.356979	-0.105771	4.817763
544.411436	8000.375871	10.361984	-0.105827	4.817763
544.118876	8000.376874	10.366989	-0.105773	4.817765
544.411502	8000.356885	10.371994	-0.105827	4.817758
544.264014	8000.376880	10.376999	-0.105800	4.817764
544.399028	8000.357755	10.382003	-0.105825	4.817758
544.242764	8000.385006	10.387008	-0.105796	4.817767
544.359754	8000.365617	10.392013	-0.105818	4.817761
544.235832	8000.389121	10.397018	-0.105795	4.817768
544.386617	8000.384992	10.402023	-0.105823	4.817766
544.238815	8000.330098	10.407027	-0.105795	4.817751
544.284964	8000.370850	10.412032	-0.105804	4.817763
544.412576	8000.370601	10.417037	-0.105828	4.817762
544.278482	8000.321181	10.422042	-0.105802	4.817748
544.474848	8000.348304	10.427047	-0.105839	4.817755
544.448845	8000.344759	10.432051	-0.105834	4.817754
544.353194	8000.375004	10.437056	-0.105816	4.817763
544.629072	8000.349497	10.442061	-0.105868	4.817755
544.614353	8000.355609	10.447066	-0.105865	4.817757
544.668124	8000.359557	10.452071	-0.105875	4.817758
544.628562	8000.352650	10.457075	-0.105868	4.817756
544.813292	8000.365892	10.462080	-0.105902	4.817759
544.779964	8000.344310	10.467085	-0.105896	4.817753
544.578651	8000.338207	10.472090	-0.105858	4.817752
544.955500	8000.372184	10.477095	-0.105928	4.817760
544.861922	8000.333901	10.482099	-0.105911	4.817749
544.741836	8000.369062	10.487104	-0.105889	4.817760
544.616670	8000.373563	10.492109	-0.105865	4.817762
544.835490	8000.392577	10.497114	-0.105906	4.817767
544.889028	8000.373317	10.502119	-0.105916	4.817761
544.594111	8000.328932	10.507123	-0.105861	4.817749
544.724129	8000.375127	10.512128	-0.105885	4.817762
544.722173	8000.342400	10.517133	-0.105885	4.817752
544.826273	8000.368178	10.522138	-0.105904	4.817759
544.820102	8000.372305	10.527143	-0.105903	4.817761
544.760858	8000.359837	10.532147	-0.105892	4.817757
544.426953	8000.406644	10.537152	-0.105830	4.817773
544.590836	8000.373174	10.542157	-0.105860	4.817762
544.498345	8000.383425	10.547162	-0.105843	4.817765
544.477188	8000.432688	10.552167	-0.105839	4.817780
544.416781	8000.363248	10.557171	-0.105828	4.817760
544.551150	8000.393685	10.562176	-0.105853	4.817768
544.318131	8000.389229	10.567181	-0.105809	4.817768
544.544216	8000.353502	10.572186	-0.105852	4.817756
544.604698	8000.371259	10.577191	-0.105863	4.817761
544.393430	8000.365011	10.582195	-0.105823	4.817760
544.598628	8000.398591	10.587200	-0.105862	4.817769
544.685444	8000.377708	10.592205	-0.105878	4.817763
544.730330	8000.375198	10.597210	-0.105886	4.817762
544.623664	8000.408446	10.602215	-0.105866	4.817772
544.689899	8000.369332	10.607219	-0.105879	4.817760
544.703867	8000.398012	10.612224	-0.105881	4.817769
544.595477	8000.384827	10.617229	-0.105861	4.817765
544.424457	8000.421355	10.622234	-0.105829	4.817777
544.525670	8000.403846	10.627239	-0.105848	4.817771
544.766085	8000.375712	10.632243	-0.105893	4.817762
544.629719	8000.391651	10.637248	-0.105867	4.817767
544.580619	8000.400425	10.642253	-0.105858	4.817770
544.372720	8000.419539	10.647258	-0.105819	4.817777
544.294763	8000.454261	10.652263	-0.105805	4.817787
543.956348	8000.412406	10.657267	-0.105742	4.817776
544.317739	8000.431390	10.662272	-0.105809	4.817780
544.392149	8000.347042	10.667277	-0.105823	4.817755
544.211671	8000.436168	10.672282	-0.105789	4.817782
544.139121	8000.467804	10.677287	-0.105776	4.817792
544.617733	8000.409396	10.682291	-0.105865	4.817773
544.522252	8000.420658	10.687296	-0.105847	4.817776
544.573586	8000.402421	10.692301	-0.105857	4.817771
544.594506	8000.420655	10.697306	-0.105861	4.817776
544.586323	8000.445848	10.702311	-0.105859	4.817783
544.280961	8000.421351	10.707315	-0.105802	4.817778
544.533927	8000.430315	10.712320	-0.105849	4.817779
544.617946	8000.399898	10.717325	-0.105865	4.817770
544.373465	8000.406876	10.722330	-0.105819	4.817773
544.336495	8000.377858	10.727335	-0.105812	4.817764
544.278131	8000.443453	10.732339	-0.105802	4.817784
544.374003	8000.349926	10.737344	-0.105819	4.817756
544.697855	8000.375745	10.742349	-0.105880	4.817762
544.757494	8000.379779	10.747354	-0.105891	4.817763
544.678114	8000.401823	10.752359	-0.105876	4.817770
544.379896	8000.432275	10.757363	-0.105820	4.817780
544.626516	8000.397904	10.762368	-0.105866	4.817769
544.705398	8000.383233	10.767373	-0.105881	4.817764
543.915280	8000.428656	10.772378	-0.105734	4.817781
544.059219	8000.389621	10.777383	-0.105761	4.817769
544.231739	8000.448038	10.782387	-0.105793	4.817786
544.079587	8000.378314	10.787392	-0.105764	4.817766
544.051347	8000.400050	10.792397	-0.105759	4.817772
544.050782	8000.404260	10.797402	-0.105759	4.817773
543.690076	8000.413761	10.802407	-0.105692	4.817778
543.730626	8000.362671	10.807411	-0.105699	4.817763
543.552070	8000.426512	10.812416	-0.105666	4.817782
543.588689	8000.345833	10.817421	-0.105673	4.817758
543.925302	8000.453049	10.822426	-0.105736	4.817788
544.116073	8000.237507	10.827431	-0.105771	4.817724
544.272352	8000.460221	10.832435	-0.105800	4.817789
544.156110	8000.340395	10.837440	-0.105779	4.817754
544.480588	8000.396810	10.842445	-0.105839	4.817769
544.531016	8000.397545	10.847450	-0.105848	4.817769
544.748511	8000.405992	10.852455	-0.105889	4.817771
544.013671	8000.406869	10.857459	-0.105752	4.817774
544.436144	8000.384555	10.862464	-0.105831	4.817766
544.512199	8000.414142	10.867469	-0.105845	4.817774
544.457824	8000.402800	10.872474	-0.105835	4.817771
544.695438	8000.411540	10.877479	-0.105879	4.817773
544.441336	8000.442636	10.882483	-0.105832	4.817783
544.547414	8000.427308	10.887488	-0.105851	4.817778
544.532664	8000.427091	10.892493	-0.105849	4.817778
544.508767	8000.315995	10.897498	-0.105844	4.817745
544.716135	8000.403399	10.902503	-0.105883	4.817770
544.257379	8000.387210	10.907507	-0.105797	4.817768
544.694939	8000.380938	10.912512	-0.105879	4.817764
544.574467	8000.391835	10.917517	-0.105856	4.817768
544.335412	8000.390454	10.922522	-0.105812	4.817768
544.621568	8000.392520	10.927527	-0.105865	4.817768
545.143051	8000.375872	10.932531	-0.105962	4.817760
545.131094	8000.386244	10.937536	-0.105960	4.817763
544.709293	8000.395907	10.942541	-0.105881	4.817768
544.330302	8000.405140	10.947546	-0.105811	4.817773
544.479619	8000.461109	10.952551	-0.105838	4.817788
544.571369	8000.407602	10.957555	-0.105856	4.817772
544.575617	8000.428757	10.962560	-0.105856	4.817778
544.509697	8000.407754	10.967565	-0.105844	4.817773
544.390480	8000.389137	10.972570	-0.105822	4.817768
544.623652	8000.319763	10.977575	-0.105865	4.817746
544.659042	8000.365632	10.982579	-0.105872	4.817759
544.542472	8000.429322	10.987584	-0.105850	4.817779
544.510207	8000.403537	10.992589	-0.105844	4.817771
544.479680	8000.419966	10.997594	-0.105838	4.817776
544.486403	8000.452759	11.002599	-0.105840	4.817786
543.708929	8000.388677	11.007603	-0.105695	4.817770
544.068276	8000.452983	11.012608	-0.105762	4.817788
544.351334	8000.457113	11.017613	-0.105814	4.817788
544.469036	8000.369178	11.022618	-0.105836	4.817761
544.582069	8000.462588	11.027623	-0.105857	4.817788
544.203600	8000.442297	11.032627	-0.105787	4.817784
543.980870	8000.387364	11.037632	-0.105745	4.817769
543.589379	8000.180205	11.042637	-0.105672	4.817709
543.815190	8000.282638	11.047642	-0.105714	4.817739
543.881422	8000.334229	11.052647	-0.105727	4.817753
544.161967	8000.442738	11.057651	-0.105779	4.817784
543.907719	8000.246015	11.062656	-0.105732	4.817727
544.318603	8000.480882	11.067661	-0.105808	4.817795
544.650986	8000.404519	11.072666	-0.105870	4.817771
544.677477	8000.373262	11.077671	-0.105875	4.817762
544.700390	8000.421058	11.082675	-0.105879	4.817776
544.550490	8000.426252	11.087680	-0.105851	4.817778
544.268346	8000.460103	11.092685	-0.105799	4.817789
544.289352	8000.379195	11.097690	-0.105803	4.817765
544.180888	8000.282687	11.102695	-0.105782	4.817737
544.136055	8000.239844	11.107699	-0.105774	4.817724
544.173353	8000.429180	11.112704	-0.105781	4.817780
544.312679	8000.420665	11.117709	-0.105807	4.817777
544.441325	8000.439417	11.122714	-0.105831	4.817782
544.709623	8000.439113	11.127719	-0.105881	4.817781
544.505751	8000.385509	11.132723	-0.105843	4.817766
544.635376	8000.439082	11.137728	-0.105867	4.817781
544.995097	8000.426401	11.142733	-0.105934	4.817776
544.794248	8000.422414	11.147738	-0.105896	4.817776
544.997108	8000.390567	11.152743	-0.105934	4.817765
544.951610	8000.373026	11.157747	-0.105926	4.817760
544.999726	8000.375837	11.162752	-0.105935	4.817761
544.964003	8000.350001	11.167757	-0.105928	4.817753
545.222140	8000.363261	11.172762	-0.105976	4.817756
544.939277	8000.378115	11.177767	-0.105923	4.817762
545.005393	8000.372751	11.182771	-0.105936	4.817760
545.260805	8000.431325	11.187776	-0.105983	4.817776
545.282457	8000.405272	11.192781	-0.105987	4.817768
544.842677	8000.402014	11.197786	-0.105905	4.817769
544.670640	8000.459622	11.202791	-0.105873	4.817787
544.710954	8000.415910	11.207795	-0.105881	4.817774
544.767554	8000.419900	11.212800	-0.105891	4.817775
544.362459	8000.506802	11.217805	-0.105816	4.817803
544.346729	8000.412700	11.222810	-0.105813	4.817775
544.353624	8000.306273	11.227815	-0.105814	4.817743
544.487509	8000.310335	11.232819	-0.105839	4.817744
544.842064	8000.426255	11.237824	-0.105905	4.817777
544.629970	8000.446362	11.242829	-0.105866	4.817783
544.832732	8000.397639	11.247834	-0.105903	4.817768
544.967300	8000.431244	11.252839	-0.105928	4.817778
544.975303	8000.397608	11.257843	-0.105930	4.817768
544.833311	8000.403972	11.262848	-0.105903	4.817770
544.659402	8000.367681	11.267853	-0.105871	4.817760
544.736556	8000.382518	11.272858	-0.105885	4.817764
544.907229	8000.459894	11.277863	-0.105917	4.817786
545.096271	8000.408861	11.282867	-0.105952	4.817770
545.006454	8000.433917	11.287872	-0.105936	4.817778
544.867338	8000.322193	11.292877	-0.105910	4.817746
544.591038	8000.393045	11.297882	-0.105858	4.817768
544.757600	8000.447157	11.302887	-0.105889	4.817783
545.077314	8000.412798	11.307891	-0.105949	4.817772
544.970874	8000.396476	11.312896	-0.105929	4.817767
544.918427	8000.388326	11.317901	-0.105919	4.817765
544.681756	8000.409130	11.322906	-0.105875	4.817772
544.962517	8000.425884	11.327911	-0.105927	4.817776
544.852601	8000.414785	11.332915	-0.105907	4.817773
545.417201	8000.399823	11.337920	-0.106012	4.817766
545.055402	8000.407196	11.342925	-0.105945	4.817770
544.799236	8000.399237	11.347930	-0.105897	4.817769
545.187831	8000.415456	11.352935	-0.105969	4.817772
545.035590	8000.371042	11.357939	-0.105941	4.817759
544.802862	8000.418271	11.362944	-0.105897	4.817774
545.169910	8000.393041	11.367949	-0.105966	4.817765
545.190261	8000.394392	11.372954	-0.105970	4.817766
545.350380	8000.388290	11.377959	-0.105999	4.817763
545.028874	8000.365665	11.382963	-0.105939	4.817758
544.923205	8000.413694	11.387968	-0.105920	4.817773
544.797609	8000.436118	11.392973	-0.105896	4.817780
544.694496	8000.412463	11.397978	-0.105877	4.817773
545.052287	8000.412411	11.402983	-0.105944	4.817772
545.219866	8000.370557	11.407987	-0.105975	4.817758
544.765503	8000.401894	11.412992	-0.105890	4.817770
545.148495	8000.402210	11.417997	-0.105962	4.817768
544.908918	8000.370233	11.423002	-0.105917	4.817760
545.203830	8000.415672	11.428007	-0.105972	4.817772
545.209073	8000.332423	11.433011	-0.105973	4.817747
545.052893	8000.395536	11.438016	-0.105944	4.817767
545.297584	8000.403326	11.443021	-0.105989	4.817768
545.023024	8000.396152	11.448026	-0.105938	4.817767
544.757494	8000.383837	11.453031	-0.105889	4.817764
544.823154	8000.463899	11.458035	-0.105901	4.817788
544.450630	8000.481664	11.463040	-0.105832	4.817795
544.577628	8000.387537	11.468045	-0.105855	4.817766
544.496233	8000.371582	11.473050	-0.105840	4.817762
544.904788	8000.358558	11.478055	-0.105916	4.817756
544.935018	8000.411735	11.483059	-0.105922	4.817772
544.712215	8000.467547	11.488064	-0.105880	4.817789
544.437619	8000.186147	11.493069	-0.105829	4.817707
544.137015	8000.164885	11.498074	-0.105773	4.817702
544.591022	8000.369794	11.503079	-0.105858	4.817761
544.583339	8000.461442	11.508083	-0.105856	4.817788
544.721714	8000.455023	11.513088	-0.105882	4.817786
545.234547	8000.409772	11.518093	-0.105977	4.817770
545.183223	8000.395310	11.523098	-0.105968	4.817766
544.935948	8000.376932	11.528103	-0.105922	4.817762
544.756729	8000.435490	11.533107	-0.105888	4.817780
545.013421	8000.412867	11.538112	-0.105936	4.817772
545.085459	8000.422356	11.543117	-0.105950	4.817774
545.339665	8000.391259	11.548122	-0.105997	4.817764
544.931339	8000.383188	11.553127	-0.105921	4.817763
544.902837	8000.465040	11.558131	-0.105916	4.817788
544.737469	8000.443639	11.563136	-0.105885	4.817782
544.370144	8000.487849	11.568141	-0.105816	4.817797
544.848413	8000.317634	11.573146	-0.105905	4.817744
544.619949	8000.464070	11.578151	-0.105863	4.817789
544.869334	8000.432903	11.583155	-0.105909	4.817778
544.676932	8000.425874	11.588160	-0.105873	4.817777
545.311694	8000.409826	11.593165	-0.105992	4.817770
545.383465	8000.376066	11.598170	-0.106005	4.817759
545.098635	8000.353976	11.603175	-0.105952	4.817754
545.139040	8000.418904	11.608179	-0.105959	4.817773
545.256396	8000.444876	11.613184	-0.105981	4.817780
545.330004	8000.410088	11.618189	-0.105995	4.817770
544.924964	8000.391517	11.623194	-0.105919	4.817766
545.135525	8000.419903	11.628199	-0.105959	4.817773
545.371752	8000.390654	11.633203	-0.106003	4.817764
545.380708	8000.399221	11.638208	-0.106004	4.817766
545.134355	8000.416718	11.643213	-0.105958	4.817773
545.646407	8000.385168	11.648218	-0.106054	4.817761
545.640618	8000.399849	11.653223	-0.106053	4.817765
545.572380	8000.367209	11.658227	-0.106040	4.817756
545.337578	8000.408079	11.663232	-0.105996	4.817769
545.223539	8000.422234	11.668237	-0.105975	4.817774
545.271080	8000.364916	11.673242	-0.105984	4.817757
545.128890	8000.442999	11.678247	-0.105957	4.817780
545.238361	8000.401352	11.683251	-0.105978	4.817768
545.628961	8000.398616	11.688256	-0.106050	4.817765
545.853745	8000.390295	11.693261	-0.106092	4.817762
545.450262	8000.390730	11.698266	-0.106017	4.817763
545.442049	8000.424361	11.703271	-0.106015	4.817773
545.359257	8000.403111	11.708275	-0.106000	4.817768
545.332046	8000.400603	11.713280	-0.105995	4.817767
545.290217	8000.427415	11.718285	-0.105987	4.817775
545.213765	8000.391491	11.723290	-0.105973	4.817765
545.392885	8000.405707	11.728295	-0.106006	4.817768
545.134097	8000.428296	11.733299	-0.105958	4.817776
545.408476	8000.427027	11.738304	-0.106009	4.817774
545.488997	8000.408162	11.743309	-0.106024	4.817768
545.352154	8000.395615	11.748314	-0.105999	4.817765
545.387775	8000.330740	11.753319	-0.106005	4.817746
545.449953	8000.372782	11.758323	-0.106017	4.817758
545.216890	8000.395746	11.763328	-0.105973	4.817766
545.225125	8000.430672	11.768333	-0.105975	4.817776
545.040255	8000.412151	11.773338	-0.105940	4.817772
545.196992	8000.429204	11.778343	-0.105970	4.817776
545.099797	8000.421455	11.783347	-0.105952	4.817774
545.109785	8000.419491	11.788352	-0.105953	4.817773
544.923681	8000.499042	11.793357	-0.105919	4.817798
545.192671	8000.420699	11.798362	-0.105969	4.817773
545.241480	8000.435122	11.803367	-0.105978	4.817778
544.881572	8000.456235	11.808371	-0.105911	4.817785
544.817014	8000.375131	11.813376	-0.105899	4.817762
545.142590	8000.387266	11.818381	-0.105959	4.817764
544.944114	8000.379094	11.823386	-0.105922	4.817762
544.678845	8000.501788	11.828391	-0.105873	4.817800
544.775838	8000.372416	11.833395	-0.105891	4.817761
544.786140	8000.445342	11.838400	-0.105893	4.817783
544.304049	8000.314902	11.843405	-0.105803	4.817746
544.618771	8000.374339	11.848410	-0.105862	4.817762
544.803366	8000.381251	11.853415	-0.105896	4.817763
544.852097	8000.417822	11.858419	-0.105905	4.817774
544.864755	8000.356831	11.863424	-0.105907	4.817756
544.705908	8000.313378	11.868429	-0.105878	4.817744
544.684304	8000.415370	11.873434	-0.105874	4.817774
545.006727	8000.460155	11.878439	-0.105934	4.817786
545.085221	8000.391687	11.883443	-0.105949	4.817765
544.953048	8000.451986	11.888448	-0.105924	4.817784
545.270670	8000.281535	11.893453	-0.105983	4.817732
545.719897	8000.385129	11.898458	-0.106067	4.817761
545.550821	8000.375276	11.903463	-0.106035	4.817758
545.573124	8000.357670	11.908467	-0.106039	4.817753
545.414316	8000.408087	11.913472	-0.106010	4.817769
545.526043	8000.425539	11.918477	-0.106031	4.817773
545.148562	8000.407369	11.923482	-0.105960	4.817770
545.017328	8000.439204	11.928487	-0.105936	4.817780
544.804590	8000.313748	11.933491	-0.105896	4.817743
544.574179	8000.133193	11.938496	-0.105853	4.817691
545.110198	8000.424735	11.943501	-0.105953	4.817775
544.684316	8000.417462	11.948506	-0.105874	4.817775
544.928709	8000.300789	11.953511	-0.105919	4.817739
545.237574	8000.431865	11.958515	-0.105977	4.817777
545.205967	8000.322764	11.963520	-0.105971	4.817744
545.182867	8000.447940	11.968525	-0.105966	4.817782
544.451754	8000.371873	11.973530	-0.105830	4.817762
544.371794	8000.095426	11.978535	-0.105815	4.817681
544.855243	8000.316586	11.983539	-0.105905	4.817744
544.783350	8000.295495	11.988544	-0.105892	4.817738
544.831101	8000.492371	11.993549	-0.105901	4.817796
545.385735	8000.405541	11.998554	-0.106004	4.817768
545.343702	8000.446061	12.003559	-0.105996	4.817780
545.582104	8000.424227	12.008563	-0.106041	4.817773
545.609299	8000.401419	12.013568	-0.106046	4.817766
545.709386	8000.420810	12.018573	-0.106064	4.817771
545.729720	8000.367313	12.023578	-0.106068	4.817755
545.441259	8000.409509	12.028583	-0.106014	4.817769
545.289343	8000.422056	12.033587	-0.105986	4.817773
545.534013	8000.390821	12.038592	-0.106032	4.817763
545.467473	8000.397232	12.043597	-0.106019	4.817765
545.424007	8000.382884	12.048602	-0.106011	4.817761
545.531151	8000.347531	12.053607	-0.106031	4.817750
545.663065	8000.390591	12.058611	-0.106056	4.817763
545.792684	8000.400921	12.063616	-0.106080	4.817765
545.950461	8000.420100	12.068621	-0.106109	4.817770
545.561097	8000.383825	12.073626	-0.106037	4.817761
545.814486	8000.391743	12.078631	-0.106084	4.817762
545.839092	8000.389992	12.083635	-0.106088	4.817762
545.626174	8000.405867	12.088640	-0.106049	4.817767
545.762874	8000.428957	12.093645	-0.106074	4.817773
545.882461	8000.386403	12.098650	-0.106096	4.817760
545.999228	8000.385997	12.103655	-0.106118	4.817760
545.964868	8000.374947	12.108659	-0.106112	4.817757
545.593638	8000.382182	12.113664	-0.106042	4.817760
545.757811	8000.400399	12.118669	-0.106073	4.817765
545.576164	8000.389308	12.123674	-0.106039	4.817763
545.711751	8000.386013	12.128679	-0.106064	4.817761
545.769934	8000.386861	12.133683	-0.106075	4.817761
545.703061	8000.398540	12.138688	-0.106063	4.817765
545.658096	8000.408430	12.143693	-0.106054	4.817768
545.671895	8000.365386	12.148698	-0.106057	4.817755
545.644207	8000.409280	12.153703	-0.106052	4.817768
545.572783	8000.433550	12.158707	-0.106039	4.817776
545.682742	8000.417224	12.163712	-0.106059	4.817770
545.803054	8000.436910	12.168717	-0.106081	4.817776
545.887428	8000.380130	12.173722	-0.106097	4.817758
545.863687	8000.418808	12.178727	-0.106093	4.817770
545.944881	8000.402062	12.183731	-0.106108	4.817765
545.959304	8000.405435	12.188736	-0.106110	4.817766
546.006650	8000.418783	12.193741	-0.106119	4.817769
545.853434	8000.398613	12.198746	-0.106091	4.817764
546.135418	8000.410114	12.203751	-0.106143	4.817766
546.154282	8000.387183	12.208755	-0.106147	4.817759
545.893828	8000.391816	12.213760	-0.106098	4.817762
545.907421	8000.422602	12.218765	-0.106101	4.817771
546.069975	8000.379620	12.223770	-0.106131	4.817758
546.166638	8000.389469	12.228775	-0.106149	4.817760
546.135990	8000.380582	12.233779	-0.106143	4.817758
546.185027	8000.389735	12.238784	-0.106152	4.817760
546.089737	8000.391506	12.243789	-0.106134	4.817761
545.839858	8000.383637	12.248794	-0.106088	4.817760
545.866004	8000.420934	12.253799	-0.106093	4.817771
545.886894	8000.418074	12.258803	-0.106097	4.817770
545.523789	8000.424372	12.263808	-0.106029	4.817773
545.745516	8000.436047	12.268813	-0.106070	4.817776
545.332529	8000.367785	12.273818	-0.105993	4.817757
545.424751	8000.418704	12.278823	-0.106011	4.817772
545.366722	8000.433677	12.283827	-0.106000	4.817777
545.339660	8000.433280	12.288832	-0.105995	4.817777
545.502480	8000.329127	12.293837	-0.106025	4.817745
545.549776	8000.416306	12.298842	-0.106034	4.817771
545.716670	8000.420851	12.303847	-0.106065	4.817771
545.842369	8000.398426	12.308851	-0.106088	4.817764
545.474455	8000.416257	12.313856	-0.106020	4.817771
545.832826	8000.429928	12.318861	-0.106086	4.817773
545.862891	8000.410325	12.323866	-0.106092	4.817768
545.916292	8000.415323	12.328871	-0.106102	4.817769
545.928350	8000.420772	12.333875	-0.106104	4.817770
546.015237	8000.409382	12.338880	-0.106120	4.817767
545.927594	8000.441854	12.343885	-0.106104	4.817777
545.708233	8000.397513	12.348890	-0.106063	4.817764
545.714813	8000.426087	12.353895	-0.106064	4.817773
545.832772	8000.399330	12.358899	-0.106086	4.817764
545.690189	8000.395137	12.363904	-0.106060	4.817764
545.985895	8000.438480	12.368909	-0.106115	4.817775
545.958104	8000.391664	12.373914	-0.106110	4.817762
545.982349	8000.418386	12.378919	-0.106114	4.817769
545.761594	8000.427818	12.383923	-0.106073	4.817773
545.559122	8000.453338	12.388928	-0.106035	4.817782
545.744942	8000.394875	12.393933	-0.106070	4.817763
545.518583	8000.433758	12.398938	-0.106028	4.817776
545.730759	8000.434746	12.403943	-0.106067	4.817775
545.848435	8000.429080	12.408947	-0.106089	4.817773
545.653799	8000.431510	12.413952	-0.106053	4.817775
545.527574	8000.439159	12.418957	-0.106029	4.817778
545.788176	8000.407102	12.423962	-0.106078	4.817767
545.907418	8000.433101	12.428967	-0.106100	4.817774
546.033839	8000.413851	12.433971	-0.106124	4.817768
546.118868	8000.364464	12.438976	-0.106139	4.817753
546.148442	8000.395482	12.443981	-0.106145	4.817762
545.624009	8000.416301	12.448986	-0.106047	4.817770
545.515591	8000.426319	12.453991	-0.106027	4.817774
545.423220	8000.432352	12.458995	-0.106010	4.817776
545.752690	8000.394972	12.464000	-0.106071	4.817763
545.963042	8000.438124	12.469005	-0.106110	4.817775
545.939698	8000.393482	12.474010	-0.106106	4.817762
546.028139	8000.416922	12.479015	-0.106122	4.817769
545.928419	8000.427067	12.484019	-0.106104	4.817772
545.894067	8000.428674	12.489024	-0.106097	4.817773
545.803813	8000.413643	12.494029	-0.106081	4.817769
545.844137	8000.397354	12.499034	-0.106088	4.817764
545.878881	8000.403134	12.504039	-0.106094	4.817765
545.994556	8000.415370	12.509043	-0.106116	4.817768
546.083845	8000.406125	12.514048	-0.106133	4.817765
545.945192	8000.416756	12.519053	-0.106107	4.817769
545.771562	8000.405781	12.524058	-0.106074	4.817767
546.008303	8000.409238	12.529063	-0.106119	4.817767
545.835883	8000.426759	12.534067	-0.106086	4.817773
545.804468	8000.337699	12.539072	-0.106080	4.817746
545.981335	8000.426771	12.544077	-0.106113	4.817772
545.220643	8000.448359	12.549082	-0.105972	4.817782
545.523912	8000.426417	12.554087	-0.106028	4.817774
545.624834	8000.432109	12.559091	-0.106047	4.817775
545.653833	8000.417765	12.564096	-0.106052	4.817771
545.706037	8000.450169	12.569101	-0.106062	4.817780
545.797193	8000.401925	12.574106	-0.106079	4.817765
545.674564	8000.400133	12.579111	-0.106056	4.817765
546.018313	8000.414645	12.584115	-0.106120	4.817768
545.705906	8000.397424	12.589120	-0.106062	4.817764
545.813131	8000.428522	12.594125	-0.106082	4.817773
545.705725	8000.403748	12.599130	-0.106062	4.817766
545.717420	8000.408137	12.604135	-0.106064	4.817768
545.800367	8000.414621	12.609139	-0.106080	4.817769
545.996375	8000.394277	12.614144	-0.106116	4.817762
545.726267	8000.432522	12.619149	-0.106066	4.817775
545.830937	8000.400297	12.624154	-0.106085	4.817765
545.898822	8000.428711	12.629159	-0.106098	4.817773
545.985633	8000.408883	12.634163	-0.106114	4.817767
545.828293	8000.384434	12.639168	-0.106085	4.817760
545.904445	8000.430899	12.644173	-0.106099	4.817773
545.349578	8000.434398	12.649178	-0.105996	4.817777
545.652482	8000.427217	12.654183	-0.106052	4.817773
545.726159	8000.432511	12.659187	-0.106066	4.817775
545.782380	8000.410126	12.664192	-0.106076	4.817768
546.052965	8000.429899	12.669197	-0.106126	4.817773
545.848374	8000.432183	12.674202	-0.106088	4.817774
546.078828	8000.345893	12.679207	-0.106131	4.817748
545.858298	8000.425997	12.684211	-0.106090	4.817772
545.849984	8000.398451	12.689216	-0.106089	4.817764
546.211120	8000.400560	12.694221	-0.106156	4.817763
545.747643	8000.415940	12.699226	-0.106069	4.817770
545.951753	8000.446343	12.704231	-0.106108	4.817778
546.299928	8000.424004	12.709235	-0.106172	4.817770
545.924568	8000.398480	12.714240	-0.106102	4.817764
545.618962	8000.414056	12.719245	-0.106045	4.817770
545.782535	8000.409060	12.724250	-0.106076	4.817768
545.830854	8000.428750	12.729255	-0.106085	4.817773
545.662424	8000.458987	12.734259	-0.106054	4.817783
545.230759	8000.427369	12.739264	-0.105973	4.817775
545.898322	8000.366447	12.744269	-0.106097	4.817754
545.890173	8000.411681	12.749274	-0.106096	4.817768
545.864837	8000.427131	12.754279	-0.106091	4.817773
545.891558	8000.434904	12.759283	-0.106096	4.817775
545.867997	8000.407135	12.764288	-0.106092	4.817767
546.157258	8000.435618	12.769293	-0.106146	4.817774
545.676546	8000.420158	12.774298	-0.106056	4.817771
545.878902	8000.427331	12.779303	-0.106094	4.817773
546.023221	8000.429438	12.784307	-0.106121	4.817773
545.879227	8000.424169	12.789312	-0.106094	4.817772
546.099110	8000.438982	12.794317	-0.106135	4.817775
545.872731	8000.303830	12.799322	-0.106092	4.817736
545.434417	8000.450368	12.804327	-0.106011	4.817781
545.723669	8000.466193	12.809331	-0.106065	4.817785
545.921880	8000.415294	12.814336	-0.106102	4.817769
546.128735	8000.349754	12.819341	-0.106140	4.817748
545.579089	8000.433490	12.824346	-0.106038	4.817776
545.676692	8000.459174	12.829351	-0.106056	4.817783
545.565755	8000.380556	12.834355	-0.106035	4.817760
545.795489	8000.350157	12.839360	-0.106078	4.817750
545.909338	8000.435144	12.844365	-0.106099	4.817775
545.786214	8000.410140	12.849370	-0.106076	4.817768
545.885258	8000.428462	12.854375	-0.106095	4.817773
545.992555	8000.408932	12.859379	-0.106115	4.817767
545.802032	8000.418806	12.864384	-0.106079	4.817770
545.585214	8000.411419	12.869389	-0.106039	4.817769
545.492894	8000.462808	12.874394	-0.106022	4.817785
545.810634	8000.258606	12.879399	-0.106081	4.817723
545.757718	8000.369635	12.884403	-0.106071	4.817756
545.708852	8000.431151	12.889408	-0.106062	4.817774
545.780949	8000.438532	12.894413	-0.106075	4.817776
545.823971	8000.429666	12.899418	-0.106083	4.817773
545.709491	8000.450143	12.904423	-0.106062	4.817780
545.749387	8000.481312	12.909427	-0.106069	4.817789
545.865836	8000.421836	12.914432	-0.106091	4.817771
545.964350	8000.471793	12.919437	-0.106109	4.817785
545.540758	8000.364349	12.924442	-0.106030	4.817755
545.739723	8000.427374	12.929447	-0.106067	4.817773
545.503240	8000.229847	12.934451	-0.106023	4.817716
545.467828	8000.354843	12.939456	-0.106017	4.817753
545.628977	8000.308676	12.944461	-0.106047	4.817739
545.957952	8000.322971	12.949466	-0.106108	4.817741
545.477461	8000.468893	12.954471	-0.106018	4.817787
545.879361	8000.426242	12.959475	-0.106093	4.817772
545.972688	8000.401235	12.964480	-0.106111	4.817764
546.049892	8000.431895	12.969485	-0.106125	4.817773
545.581766	8000.428221	12.974490	-0.106038	4.817774
545.238011	8000.310344	12.979495	-0.105974	4.817741
545.471844	8000.381260	12.984499	-0.106017	4.817761
545.544275	8000.398137	12.989504	-0.106031	4.817765
546.034600	8000.391585	12.994509	-0.106122	4.817761
545.730902	8000.400860	12.999514	-0.106065	4.817765
545.865748	8000.399664	13.004519	-0.106091	4.817764
545.718211	8000.418603	13.009523	-0.106063	4.817771
545.835161	8000.410817	13.014528	-0.106085	4.817768
545.850452	8000.405766	13.019533	-0.106088	4.817766
545.642791	8000.386911	13.024538	-0.106049	4.817762
545.719482	8000.414398	13.029543	-0.106063	4.817769
546.003173	8000.357364	13.034547	-0.106116	4.817751
545.841671	8000.414071	13.039552	-0.106086	4.817769
545.454451	8000.453770	13.044557	-0.106014	4.817782
545.478351	8000.474158	13.049562	-0.106018	4.817788
545.620208	8000.341220	13.054567	-0.106045	4.817748
545.661317	8000.399830	13.059571	-0.106052	4.817765
545.525860	8000.410508	13.064576	-0.106027	4.817769
545.899400	8000.431783	13.069581	-0.106097	4.817774
545.247462	8000.444412	13.074586	-0.105975	4.817780
545.488136	8000.342450	13.079591	-0.106020	4.817749
546.062750	8000.400413	13.084595	-0.106127	4.817764
545.488352	8000.415229	13.089600	-0.106020	4.817771
545.722989	8000.466118	13.094605	-0.106064	4.817785
545.871675	8000.402893	13.099610	-0.106091	4.817765
545.515829	8000.371327	13.104615	-0.106025	4.817758
545.398807	8000.384384	13.109619	-0.106003	4.817762
545.363574	8000.428167	13.114624	-0.105997	4.817775
545.417785	8000.396261	13.119629	-0.106007	4.817765
545.731404	8000.411387	13.124634	-0.106065	4.817768
545.155278	8000.455710	13.129639	-0.105958	4.817784
545.448140	8000.353456	13.134643	-0.106012	4.817753
545.358144	8000.414371	13.139648	-0.105996	4.817771
544.606513	7999.973075	13.144653	-0.105855	4.817644
544.308838	8000.087913	13.149658	-0.105800	4.817679
544.653350	8000.019108	13.154663	-0.105864	4.817657
545.085135	8000.240568	13.159667	-0.105945	4.817721
544.855644	7999.812171	13.164672	-0.105902	4.817595
544.797456	8000.051793	13.169677	-0.105891	4.817666
545.024043	8000.396828	13.174682	-0.105933	4.817767
545.155651	8000.362887	13.179687	-0.105958	4.817757
545.307313	8000.452644	13.184691	-0.105986	4.817783
545.399609	8000.317928	13.189696	-0.106003	4.817742
545.420072	8000.406824	13.194701	-0.106007	4.817768
545.457228	8000.427406	13.199706	-0.106014	4.817774
545.372766	8000.449376	13.204711	-0.105998	4.817781
544.799476	8000.416746	13.209715	-0.105891	4.817774
545.021967	8000.120450	13.214720	-0.105933	4.817685
545.611983	8000.269340	13.219725	-0.106043	4.817727
545.138356	8000.505015	13.224730	-0.105955	4.817799
544.918046	8000.417418	13.229735	-0.105913	4.817774
545.456439	8000.434770	13.234739	-0.106014	4.817777
545.516854	8000.456746	13.239744	-0.106025	4.817783
545.075142	8000.226692	13.244749	-0.105943	4.817717
545.091950	8000.327135	13.249754	-0.105946	4.817746
544.965610	8000.113290	13.254759	-0.105922	4.817684
544.782420	8000.078975	13.259763	-0.105888	4.817674
544.760594	8000.094476	13.264768	-0.105884	4.817679
545.071832	8000.236130	13.269773	-0.105942	4.817719
545.119554	8000.441444	13.274778	-0.105951	4.817780
545.192678	8000.305394	13.279783	-0.105964	4.817739
545.233506	8000.294387	13.284787	-0.105972	4.817736
545.106212	8000.398002	13.289792	-0.105948	4.817767
545.334464	8000.357034	13.294797	-0.105991	4.817754
545.183231	8000.399124	13.299802	-0.105963	4.817767
545.077578	8000.487233	13.304807	-0.105943	4.817794
545.131132	8000.328748	13.309811	-0.105953	4.817747
545.420006	8000.347730	13.314816	-0.106007	4.817751
545.296590	8000.466168	13.319821	-0.105984	4.817787
545.459032	8000.365174	13.324826	-0.106014	4.817756
545.871165	8000.408107	13.329831	-0.106091	4.817767
545.436539	8000.443949	13.334835	-0.106010	4.817779
544.678827	8000.257802	13.339840	-0.105869	4.817728
545.042860	8000.105959	13.344845	-0.105936	4.817681
545.174564	8000.358906	13.349850	-0.105961	4.817755
545.131051	8000.283383	13.354855	-0.105953	4.817733
544.791197	8000.053767	13.359859	-0.105889	4.817667
544.675143	8000.179693	13.364864	-0.105868	4.817704
544.714175	7999.858577	13.369869	-0.105875	4.817609
544.462737	7999.877058	13.374874	-0.105828	4.817616
544.625890	8000.081938	13.379879	-0.105858	4.817676
544.944377	8000.083419	13.384883	-0.105918	4.817675
544.851955	8000.268755	13.389888	-0.105901	4.817730
544.425985	7999.972494	13.394893	-0.105821	4.817644
545.023883	8000.369351	13.399898	-0.105933	4.817759
544.994996	8000.396352	13.404903	-0.105927	4.817767
545.360932	8000.359503	13.409907	-0.105995	4.817755
545.176471	8000.448572	13.414912	-0.105961	4.817782
545.498356	8000.437449	13.419917	-0.106021	4.817777
545.173841	8000.406341	13.424922	-0.105961	4.817769
544.895186	8000.311565	13.429927	-0.105909	4.817743
544.849175	8000.126317	13.434931	-0.105900	4.817688
545.086293	8000.246850	13.439936	-0.105944	4.817723
545.606366	8000.243892	13.444941	-0.106041	4.817719
544.990697	7999.969116	13.449946	-0.105926	4.817641
545.507157	8000.324712	13.454951	-0.106022	4.817744
545.612651	8000.386371	13.459955	-0.106042	4.817762
545.232964	8000.474699	13.464960	-0.105971	4.817789
545.172040	8000.313488	13.469965	-0.105960	4.817742
545.537094	8000.468590	13.474970	-0.106028	4.817786
545.251054	8000.328350	13.479975	-0.105975	4.817746
545.180838	8000.411703	13.484979	-0.105962	4.817771
545.270580	8000.318086	13.489984	-0.105978	4.817743
545.109767	8000.372693	13.494989	-0.105948	4.817760
545.051088	7999.974205	13.499994	-0.105937	4.817642
545.265393	8000.415043	13.504999	-0.105977	4.817772
545.448220	8000.238405	13.510003	-0.106011	4.817719
545.112981	8000.411761	13.515008	-0.105949	4.817771
544.896753	8000.145976	13.520013	-0.105908	4.817694
545.317063	8000.262855	13.525018	-0.105987	4.817726
545.002264	8000.255095	13.530023	-0.105928	4.817725
545.042648	7999.951925	13.535027	-0.105935	4.817635
545.272618	8000.378224	13.540032	-0.105979	4.817761
545.673083	8000.446301	13.545037	-0.106053	4.817779
545.110908	8000.082647	13.550042	-0.105948	4.817674
545.252299	8000.457030	13.555047	-0.105975	4.817784
545.626354	8000.450889	13.560051	-0.106044	4.817781
545.383222	8000.356629	13.565056	-0.105999	4.817754
545.025212	8000.479025	13.570061	-0.105932	4.817792
545.210930	8000.404739	13.575066	-0.105967	4.817769
544.952369	8000.407292	13.580071	-0.105919	4.817771
545.009030	8000.199281	13.585075	-0.105929	4.817709
544.947145	8000.357641	13.590080	-0.105918	4.817756
545.153921	8000.359603	13.595085	-0.105956	4.817756
545.077174	8000.347934	13.600090	-0.105942	4.817753
545.073270	8000.333110	13.605095	-0.105941	4.817748
545.255243	8000.071028	13.610099	-0.105975	4.817670
545.019913	8000.337602	13.615104	-0.105931	4.817750
544.913044	8000.339206	13.620109	-0.105911	4.817751
545.299677	8000.317425	13.625114	-0.105983	4.817743
545.331427	8000.475044	13.630119	-0.105989	4.817789
544.882196	8000.372503	13.635123	-0.105906	4.817761
544.746823	8000.344158	13.640128	-0.105880	4.817753
545.734424	8000.373341	13.645133	-0.106064	4.817757
545.259584	8000.371680	13.650138	-0.105976	4.817759
545.457481	8000.410430	13.655143	-0.106013	4.817769
545.572873	8000.443756	13.660147	-0.106034	4.817779
545.274811	8000.459443	13.665152	-0.105979	4.817785
545.487609	8000.372896	13.670157	-0.106018	4.817758
545.684065	8000.419008	13.675162	-0.106055	4.817771
545.470627	8000.419054	13.680167	-0.106015	4.817772
545.235081	8000.477844	13.685171	-0.105971	4.817790
545.272913	8000.409837	13.690176	-0.105978	4.817770
545.202443	8000.251651	13.695181	-0.105965	4.817724
545.339200	8000.378105	13.700186	-0.105991	4.817760
545.314803	8000.379857	13.705191	-0.105986	4.817761
545.161373	8000.121317	13.710195	-0.105957	4.817685
545.305643	8000.421911	13.715200	-0.105984	4.817773
545.630796	8000.285321	13.720205	-0.106045	4.817732
545.232512	8000.297437	13.725210	-0.105971	4.817737
545.688979	8000.443326	13.730215	-0.106056	4.817778
545.507933	8000.410094	13.735219	-0.106022	4.817769
545.233073	8000.458817	13.740224	-0.105971	4.817785
545.723349	8000.391087	13.745229	-0.106062	4.817763
545.433109	8000.313016	13.750234	-0.106008	4.817741
545.645198	8000.443736	13.755239	-0.106047	4.817778
545.675878	8000.368241	13.760243	-0.106053	4.817756
545.564929	8000.442562	13.765248	-0.106032	4.817778
545.453093	8000.351274	13.770253	-0.106011	4.817752
545.851360	8000.463618	13.775258	-0.106086	4.817783
545.487255	8000.381303	13.780263	-0.106018	4.817761
545.376270	8000.181391	13.785267	-0.105997	4.817702
545.111310	8000.485505	13.790272	-0.105948	4.817793
545.111613	8000.271397	13.795277	-0.105948	4.817730
545.390145	8000.386209	13.800282	-0.106000	4.817763
545.142942	8000.392092	13.805287	-0.105954	4.817765
545.395372	8000.464335	13.810291	-0.106001	4.817786
545.208913	8000.480596	13.815296	-0.105966	4.817791
545.198746	8000.353878	13.820301	-0.105964	4.817754
545.273458	8000.332818	13.825306	-0.105978	4.817747
545.456302	8000.420920	13.830311	-0.106012	4.817773
545.271016	8000.446692	13.835315	-0.105977	4.817781
545.055436	8000.354945	13.840320	-0.105937	4.817755
545.338903	8000.391779	13.845325	-0.105990	4.817764
545.222623	8000.267731	13.850330	-0.105968	4.817728
545.093971	8000.459924	13.855335	-0.105944	4.817786
544.989426	8000.291748	13.860339	-0.105925	4.817736
545.353843	8000.434183	13.865344	-0.105993	4.817777
545.272348	8000.446703	13.870349	-0.105978	4.817781
545.405066	8000.380082	13.875354	-0.106002	4.817761
545.058824	8000.448857	13.880359	-0.105938	4.817783
544.936990	8000.249843	13.885363	-0.105915	4.817724
544.687302	8000.007833	13.890368	-0.105868	4.817654
545.087415	8000.146563	13.895373	-0.105943	4.817693
544.951860	8000.080247	13.900378	-0.105918	4.817674
545.010596	8000.372206	13.905383	-0.105929	4.817760
544.939710	7999.898657	13.910387	-0.105915	4.817620
545.158076	8000.421820	13.915392	-0.105956	4.817774
545.145655	8000.355189	13.920397	-0.105954	4.817754
545.246491	8000.295485	13.925402	-0.105973	4.817736
545.302537	8000.457678	13.930407	-0.105983	4.817784
545.256499	8000.325162	13.935411	-0.105974	4.817745
545.302651	8000.350093	13.940416	-0.105983	4.817752
544.728622	7999.945142	13.945421	-0.105876	4.817635
545.234869	8000.299529	13.950426	-0.105970	4.817738
544.741390	8000.263848	13.955431	-0.105878	4.817729
545.303034	8000.344821	13.960435	-0.105983	4.817751
545.611935	8000.450586	13.965440	-0.106041	4.817781
545.162735	8000.369139	13.970445	-0.105957	4.817758
545.475829	8000.444377	13.975450	-0.106015	4.817779
545.244504	8000.480024	13.980455	-0.105972	4.817791
545.251105	8000.158424	13.985459	-0.105973	4.817696
545.193146	8000.482436	13.990464	-0.105963	4.817792
545.383289	8000.371298	13.995469	-0.105998	4.817758
545.540268	8000.453750	14.000474	-0.106027	4.817782
545.365978	8000.346784	14.005479	-0.105995	4.817751
545.248514	8000.501170	14.010483	-0.105973	4.817797
545.209687	8000.359267	14.015488	-0.105965	4.817755
545.094908	8000.315401	14.020493	-0.105944	4.817743
545.426598	8000.466851	14.025498	-0.106006	4.817786
545.301394	8000.377478	14.030503	-0.105983	4.817760
545.227227	8000.392215	14.035507	-0.105969	4.817765
545.113154	8000.386330	14.040512	-0.105947	4.817764
545.501489	8000.297071	14.045517	-0.106020	4.817736
545.720451	8000.380428	14.050522	-0.106060	4.817759
545.656565	8000.421684	14.055527	-0.106049	4.817772
545.799257	8000.439588	14.060531	-0.106075	4.817777
545.623673	8000.447570	14.065536	-0.106042	4.817780
545.813605	8000.367017	14.070541	-0.106078	4.817755
545.108168	8000.125731	14.075546	-0.105946	4.817687
545.397223	8000.392577	14.080551	-0.106000	4.817764
545.650236	8000.298179	14.085555	-0.106047	4.817735
545.082500	8000.490290	14.090560	-0.105942	4.817795
545.256421	8000.103631	14.095565	-0.105974	4.817679
545.752515	8000.454717	14.100570	-0.106066	4.817781
545.323292	8000.458996	14.105575	-0.105986	4.817784
545.765035	8000.440131	14.110579	-0.106069	4.817777
546.025707	8000.313147	14.115584	-0.106117	4.817738
546.013463	8000.420553	14.120589	-0.106115	4.817770
545.876491	8000.444920	14.125594	-0.106089	4.817778
545.304351	8000.413359	14.130599	-0.105983	4.817771
545.519278	8000.346883	14.135603	-0.106023	4.817750
545.745203	8000.476751	14.140608	-0.106065	4.817788
545.664503	8000.292045	14.145613	-0.106050	4.817734
545.755152	8000.298641	14.150618	-0.106067	4.817735
546.113230	8000.440987	14.155623	-0.106133	4.817776
545.909306	8000.312492	14.160627	-0.106095	4.817739
545.718768	8000.401472	14.165632	-0.106060	4.817766
545.956286	8000.437637	14.170637	-0.106104	4.817775
545.417189	8000.262059	14.175642	-0.106004	4.817726
545.420574	8000.320118	14.180647	-0.106004	4.817743
545.302294	8000.153852	14.185651	-0.105982	4.817694
545.317756	8000.294356	14.190656	-0.105985	4.817736
545.554480	8000.377971	14.195661	-0.106029	4.817759
545.531087	8000.407161	14.200666	-0.106025	4.817768
545.409414	8000.446519	14.205671	-0.106002	4.817780
545.244933	8000.411419	14.210675	-0.105971	4.817771
545.557091	8000.469768	14.215680	-0.106030	4.817787
545.523430	8000.378567	14.220685	-0.106023	4.817760
545.553805	8000.345257	14.225690	-0.106029	4.817750
544.927423	8000.392013	14.230695	-0.105912	4.817766
545.404943	8000.061468	14.235699	-0.106001	4.817666
545.277705	8000.463573	14.240704	-0.105978	4.817786
545.573096	8000.432024	14.245709	-0.106033	4.817775
545.523469	8000.381725	14.250714	-0.106023	4.817761
545.669318	8000.380689	14.255719	-0.106050	4.817760
545.986282	8000.443328	14.260723	-0.106109	4.817777
545.771176	8000.410652	14.265728	-0.106069	4.817768
546.092029	8000.410063	14.270733	-0.106129	4.817767
545.536117	8000.472612	14.275738	-0.106026	4.817788
545.516346	8000.335205	14.280743	-0.106022	4.817747
545.945390	8000.441671	14.285747	-0.106102	4.817777
545.769401	8000.430661	14.290752	-0.106069	4.817774
545.625853	8000.447549	14.295757	-0.106042	4.817780
545.644928	8000.364501	14.300762	-0.106046	4.817755
545.933699	8000.413017	14.305767	-0.106099	4.817768
546.096918	8000.434385	14.310771	-0.106130	4.817774
546.095594	8000.385846	14.315776	-0.106130	4.817759
545.975207	7999.459089	14.320781	-0.106107	4.817486

546.227076	7996.173470	14.325786	-0.106151	4.816512
545.961383	7990.638734	14.330791	-0.106098	4.814874
546.468959	7984.011587	14.335795	-0.106188	4.812909
546.057923	7976.768473	14.340800	-0.106107	4.810764
546.014941	7969.115901	14.345805	-0.106094	4.808495
546.304432	7961.353657	14.350810	-0.106143	4.806191
545.998733	7953.416641	14.355815	-0.106081	4.803837
545.830014	7945.594782	14.360819	-0.106044	4.801515
545.913563	7937.524766	14.365824	-0.106055	4.799118
545.785231	7929.571545	14.370829	-0.106025	4.796754
545.340565	7921.562657	14.375834	-0.105937	4.794374
545.505685	7913.525678	14.380839	-0.105963	4.791983
545.345441	7905.498093	14.385843	-0.105928	4.789594
545.598774	7897.527800	14.390848	-0.105970	4.787219
545.211312	7889.507649	14.395853	-0.105892	4.784831
545.593609	7881.562452	14.400858	-0.105958	4.782461
545.612856	7873.525829	14.405863	-0.105957	4.780064
545.792408	7865.497147	14.410867	-0.105985	4.777667
545.592474	7857.506888	14.415872	-0.105942	4.775282
545.496310	7849.494674	14.420877	-0.105919	4.772889
545.347236	7841.524596	14.425882	-0.105886	4.770508
545.697848	7833.410392	14.430887	-0.105946	4.768081
545.707644	7825.499068	14.435891	-0.105943	4.765714
545.724067	7817.445755	14.440896	-0.105941	4.763303
545.561789	7809.505219	14.445901	-0.105905	4.760926
545.393924	7801.559289	14.450906	-0.105869	4.758546
545.551842	7793.514326	14.455911	-0.105893	4.756134
545.326349	7785.476036	14.460915	-0.105846	4.753723
545.146204	7777.505786	14.465920	-0.105807	4.751332
545.150487	7769.477867	14.470925	-0.105803	4.748922
545.002523	7761.504646	14.475930	-0.105770	4.746527
545.233261	7753.358062	14.480935	-0.105808	4.744079
544.959893	7745.554954	14.485939	-0.105752	4.741733
545.305741	7737.424754	14.490944	-0.105811	4.739286
545.291286	7729.465801	14.495949	-0.105803	4.736891
545.055352	7721.491534	14.500954	-0.105754	4.734490
544.961582	7713.484167	14.505959	-0.105731	4.732078
544.743714	7705.423059	14.510963	-0.105685	4.729648
544.569902	7697.514489	14.515968	-0.105648	4.727263
544.717187	7689.408487	14.520973	-0.105670	4.724817
544.514289	7681.531668	14.525978	-0.105627	4.722439
544.545977	7673.413515	14.530983	-0.105627	4.719987
544.344295	7665.503580	14.535987	-0.105585	4.717597
544.328275	7657.467816	14.540992	-0.105576	4.715167
544.582806	7649.364606	14.545997	-0.105618	4.712715
544.618756	7641.420969	14.551002	-0.105620	4.710310
544.618244	7633.430676	14.556007	-0.105615	4.707890
544.861550	7625.375795	14.561011	-0.105655	4.705449
544.681164	7617.414391	14.566016	-0.105616	4.703036
545.047994	7609.397179	14.571021	-0.105679	4.700603
544.929067	7601.451531	14.576026	-0.105652	4.698192
544.626515	7593.483450	14.581031	-0.105590	4.695773
544.857196	7585.442905	14.586035	-0.105628	4.693330
544.920903	7577.458114	14.591040	-0.105634	4.690903
544.827391	7569.436759	14.596045	-0.105612	4.688464
544.315662	7561.546199	14.601050	-0.105511	4.686064
544.699481	7553.405904	14.606055	-0.105577	4.683585
544.423306	7545.521564	14.611059	-0.105521	4.681184
544.042883	7537.481258	14.616064	-0.105445	4.678734
544.047553	7529.492604	14.621069	-0.105440	4.676299
543.990179	7521.490541	14.626074	-0.105425	4.673858
543.882099	7513.409719	14.631079	-0.105399	4.671391
544.057937	7505.364611	14.636083	-0.105427	4.668934
544.125940	7497.394926	14.641088	-0.105434	4.666499
543.848424	7489.294878	14.646093	-0.105377	4.664023
543.624702	7481.499361	14.651098	-0.105330	4.661639
543.622977	7473.406437	14.656103	-0.105325	4.659162
543.933894	7465.405994	14.661107	-0.105377	4.656712
543.565915	7457.388310	14.666112	-0.105304	4.654256
543.113877	7449.479789	14.671117	-0.105214	4.651832
543.564005	7441.406539	14.676122	-0.105293	4.649356
543.418989	7433.369478	14.681127	-0.105261	4.646890
543.488353	7425.355185	14.686131	-0.105268	4.644430
543.341314	7417.477119	14.691136	-0.105236	4.642010
543.235951	7409.428557	14.696141	-0.105211	4.639536
543.330426	7401.470626	14.701146	-0.105223	4.637089
542.815151	7393.410430	14.706151	-0.105122	4.634609
543.024373	7385.452869	14.711155	-0.105156	4.632160
543.181363	7377.358608	14.716160	-0.105180	4.629667
543.102958	7369.377200	14.721165	-0.105160	4.627207
543.033797	7361.374758	14.726170	-0.105142	4.624740
543.252343	7353.358091	14.731175	-0.105177	4.622267
543.326632	7345.358971	14.736179	-0.105186	4.619798
543.566933	7337.384074	14.741184	-0.105225	4.617336
542.992271	7329.360175	14.746189	-0.105113	4.614856
543.108459	7321.426345	14.751194	-0.105130	4.612403
543.306264	7313.287651	14.756199	-0.105161	4.609886
543.343955	7305.370529	14.761203	-0.105163	4.607436
543.600599	7297.337123	14.766208	-0.105206	4.604949
543.152306	7289.406555	14.771213	-0.105117	4.602491
543.179888	7281.413599	14.776218	-0.105117	4.600014
542.840256	7273.380781	14.781223	-0.105048	4.597522
542.955560	7265.339918	14.786227	-0.105064	4.595027
543.103178	7257.348513	14.791232	-0.105087	4.592546
543.329737	7249.317887	14.796237	-0.105124	4.590051
543.250133	7241.334893	14.801242	-0.105104	4.587570
542.803170	7233.293504	14.806247	-0.105015	4.585069
543.137530	7225.361724	14.811251	-0.105072	4.582601
542.852092	7217.339582	14.816256	-0.105014	4.580103
543.088031	7209.323544	14.821261	-0.105053	4.577607
543.057465	7201.342115	14.826266	-0.105042	4.575119
542.732144	7193.322481	14.831271	-0.104976	4.572618
542.853339	7185.305054	14.836275	-0.104993	4.570116
542.892486	7177.301418	14.841280	-0.104995	4.567618
543.502169	7169.196052	14.846285	-0.105103	4.565087
542.904436	7161.341600	14.851290	-0.104987	4.562631
542.776433	7153.324125	14.856295	-0.104958	4.560124
543.009572	7145.359770	14.861299	-0.104996	4.557633
543.094221	7137.304915	14.866304	-0.105007	4.555111
543.028756	7129.309287	14.871309	-0.104989	4.552607
542.675265	7121.373815	14.876314	-0.104918	4.550119
542.846621	7113.291874	14.881319	-0.104945	4.547585
542.869626	7105.274130	14.886323	-0.104944	4.545070
542.945049	7097.250497	14.891328	-0.104953	4.542551
543.395087	7089.187735	14.896333	-0.105031	4.540020
543.380140	7081.309673	14.901338	-0.105023	4.537544
542.821576	7073.282390	14.906343	-0.104914	4.535019
543.199466	7065.279011	14.911347	-0.104979	4.532502
543.015695	7057.281619	14.916352	-0.104940	4.529984
542.895565	7049.260467	14.921357	-0.104912	4.527457
542.796176	7041.286257	14.926362	-0.104888	4.524944
543.148315	7033.260054	14.931367	-0.104949	4.522415
542.694936	7025.345437	14.936371	-0.104859	4.519916
542.818316	7017.302490	14.941376	-0.104877	4.517378
542.698194	7009.293996	14.946381	-0.104849	4.514848
542.882063	7001.334520	14.951386	-0.104878	4.512333
542.748832	6993.194005	14.956391	-0.104848	4.509759
543.062511	6985.197744	14.961395	-0.104901	4.507230
543.151374	6977.181536	14.966400	-0.104913	4.504693
543.226382	6969.201495	14.971405	-0.104921	4.502166
543.293546	6961.231907	14.976410	-0.104929	4.499640
543.083091	6953.283557	14.981415	-0.104884	4.497119
542.730378	6945.260653	14.986419	-0.104813	4.494572
542.719308	6937.277944	14.991424	-0.104806	4.492038
543.108148	6929.139937	14.996429	-0.104873	4.489455
542.867974	6921.254370	15.001434	-0.104823	4.486948
542.579455	6913.184449	15.006439	-0.104764	4.484381
542.792808	6905.274135	15.011443	-0.104799	4.481865
542.538854	6897.238580	15.016448	-0.104746	4.479306
542.516695	6889.220537	15.021453	-0.104737	4.476751
542.646047	6881.163074	15.026458	-0.104756	4.474184
542.979942	6873.199584	15.031463	-0.104813	4.471646
542.454313	6865.208584	15.036467	-0.104710	4.469094
542.584870	6857.196142	15.041472	-0.104729	4.466536
542.288360	6849.163655	15.046477	-0.104668	4.463969
542.428854	6841.246200	15.051482	-0.104689	4.461439
542.631428	6833.137153	15.056487	-0.104722	4.458846
542.815907	6825.197837	15.061491	-0.104751	4.456307
542.506536	6817.187096	15.066496	-0.104688	4.453740
542.413888	6809.203331	15.071501	-0.104666	4.451182
541.843314	6801.238923	15.076506	-0.104554	4.448627
542.013758	6793.177935	15.081511	-0.104581	4.446042
542.279735	6785.127933	15.086515	-0.104625	4.443460
541.955154	6777.241106	15.091520	-0.104559	4.440926
541.941862	6769.204564	15.096525	-0.104552	4.438343
542.239795	6761.186341	15.101530	-0.104602	4.435767
541.811753	6753.173371	15.106535	-0.104517	4.433187
541.876345	6745.160335	15.111539	-0.104524	4.430609
541.761443	6737.172276	15.116544	-0.104497	4.428035
541.415062	6729.136500	15.121549	-0.104427	4.425444
541.466873	6721.182273	15.126554	-0.104432	4.422880
541.209687	6713.172005	15.131559	-0.104379	4.420294
541.861795	6705.086442	15.136563	-0.104495	4.417688
541.526970	6697.132369	15.141568	-0.104427	4.415117
542.019498	6689.055827	15.146573	-0.104514	4.412509
542.121551	6681.103597	15.151578	-0.104527	4.409938
541.764112	6673.098474	15.156583	-0.104456	4.407346
541.675307	6665.094390	15.161587	-0.104434	4.404754
541.675668	6657.184021	15.166592	-0.104429	4.402191
541.920021	6649.099542	15.171597	-0.104469	4.399572
541.669225	6641.179979	15.176602	-0.104417	4.397002
541.927302	6633.111433	15.181607	-0.104460	4.394386
541.948272	6625.121256	15.186611	-0.104459	4.391791
541.609832	6617.122447	15.191616	-0.104390	4.389190
542.012504	6609.059594	15.196621	-0.104460	4.386571
542.070272	6601.080042	15.201626	-0.104466	4.383976
542.164237	6593.117917	15.206631	-0.104478	4.381385
542.102477	6585.111798	15.211635	-0.104461	4.378777
542.131577	6577.193909	15.216640	-0.104461	4.376197
542.129287	6569.112853	15.221645	-0.104456	4.373562
542.177245	6561.121749	15.226650	-0.104459	4.370956
542.198498	6553.125433	15.231655	-0.104458	4.368345
542.355330	6545.106245	15.236659	-0.104482	4.365727
542.200410	6537.159446	15.241664	-0.104448	4.363128
542.188260	6529.185808	15.246669	-0.104441	4.360521
542.395574	6521.204649	15.251674	-0.104474	4.357910
541.957053	6513.236357	15.256679	-0.104387	4.355298
542.168805	6505.199867	15.261683	-0.104421	4.352667
541.931888	6497.177025	15.266688	-0.104372	4.350035
542.113776	6489.214595	15.271693	-0.104401	4.347424
541.991847	6481.153346	15.276698	-0.104373	4.344777
541.870344	6473.210143	15.281703	-0.104345	4.342168
541.735976	6465.199885	15.286707	-0.104314	4.339534
541.864431	6457.234103	15.291712	-0.104333	4.336916
541.592802	6449.203578	15.296717	-0.104277	4.334271
541.339178	6441.253492	15.301722	-0.104225	4.331652
541.708431	6433.127932	15.306727	-0.104288	4.328978
541.591614	6425.208101	15.311731	-0.104261	4.326366
541.793006	6417.182385	15.316736	-0.104294	4.323721
541.482934	6409.237151	15.321741	-0.104231	4.321096
541.736199	6401.181169	15.326746	-0.104273	4.318438
541.782962	6393.187042	15.331751	-0.104276	4.315797
541.815626	6385.194368	15.336755	-0.104277	4.313154
541.846837	6377.227377	15.341760	-0.104278	4.310519
541.011402	6369.202059	15.346765	-0.104117	4.307855
541.415982	6361.163074	15.351770	-0.104187	4.305195
541.467949	6353.149148	15.356775	-0.104191	4.302539
541.480889	6345.162798	15.361779	-0.104189	4.299891
541.333997	6337.212763	15.366784	-0.104156	4.297251
541.329769	6329.116420	15.371789	-0.104150	4.294562
540.880188	6321.179572	15.376794	-0.104061	4.291921
541.233984	6313.098972	15.381799	-0.104122	4.289237
541.387457	6305.141182	15.386803	-0.104145	4.286591
540.912313	6297.172245	15.391808	-0.104051	4.283934
540.774055	6289.225614	15.396813	-0.104020	4.281286
541.030311	6281.198356	15.401818	-0.104063	4.278612
541.283213	6273.141488	15.406823	-0.104105	4.275927
540.877912	6265.158193	15.411827	-0.104024	4.273259
541.006963	6257.156840	15.416832	-0.104043	4.270588
540.968065	6249.100689	15.421837	-0.104030	4.267896
541.427724	6241.088843	15.426842	-0.104111	4.265221
541.229647	6233.136829	15.431847	-0.104069	4.262559
540.986729	6225.166911	15.436851	-0.104018	4.259888
541.347305	6217.110260	15.441856	-0.104080	4.257193
540.942862	6209.136522	15.446861	-0.103999	4.254516
541.182068	6201.190209	15.451866	-0.104039	4.251853
541.076068	6193.113823	15.456871	-0.104014	4.249141
541.104451	6185.131614	15.461875	-0.104014	4.246461
541.111857	6177.079839	15.466880	-0.104010	4.243755
540.911756	6169.197175	15.471885	-0.103968	4.241102
540.924629	6161.199976	15.476890	-0.103965	4.238411
540.816545	6153.165169	15.481895	-0.103939	4.235705
541.173638	6145.130661	15.486899	-0.104001	4.233001
541.156395	6137.130198	15.491904	-0.103992	4.230304
540.368138	6129.158609	15.496909	-0.103840	4.227607
540.713919	6121.107348	15.501914	-0.103899	4.224892
540.638944	6113.209155	15.506919	-0.103880	4.222224
540.641632	6105.127957	15.511923	-0.103875	4.219492
540.253996	6097.217508	15.516928	-0.103798	4.216813
539.965109	6089.162490	15.521933	-0.103739	4.214083
540.226782	6081.159719	15.526938	-0.103783	4.211376
539.974019	6073.113157	15.531943	-0.103730	4.208646
539.992275	6065.134944	15.536947	-0.103728	4.205941
539.937052	6057.162417	15.541952	-0.103713	4.203235
539.600154	6049.186816	15.546957	-0.103645	4.200524
540.246983	6041.112447	15.551962	-0.103760	4.197787
540.382746	6033.064614	15.556967	-0.103780	4.195053
540.605040	6025.054874	15.561971	-0.103816	4.192330
540.629281	6017.028474	15.566976	-0.103816	4.189598
540.331320	6009.096051	15.571981	-0.103755	4.186893
540.267224	6001.068476	15.576986	-0.103738	4.184156
540.096812	5993.191640	15.581991	-0.103701	4.181467
540.459162	5985.092270	15.586995	-0.103763	4.178707
540.580758	5977.095055	15.592000	-0.103780	4.175977
540.307749	5969.084756	15.597005	-0.103724	4.173236
540.472171	5961.097432	15.602010	-0.103750	4.170507
540.553670	5953.074409	15.607015	-0.103760	4.167762
540.217547	5945.086872	15.612019	-0.103692	4.165023
540.470310	5937.159444	15.617024	-0.103734	4.162310
539.960336	5929.156886	15.622029	-0.103634	4.159559
540.551261	5921.171301	15.627034	-0.103738	4.156827
540.216008	5913.115040	15.632039	-0.103671	4.154057
540.127927	5905.188875	15.637043	-0.103649	4.151332
540.263746	5897.110011	15.642048	-0.103669	4.148557
540.176479	5889.070986	15.647053	-0.103648	4.145790
540.209190	5881.124518	15.652058	-0.103649	4.143055
539.905977	5873.165831	15.657063	-0.103587	4.140309
540.166731	5865.140865	15.662067	-0.103630	4.137546
539.737281	5857.185886	15.667072	-0.103545	4.134797
540.035736	5849.123114	15.672077	-0.103595	4.132017
540.059663	5841.156445	15.677082	-0.103595	4.129266
539.776808	5833.159786	15.682087	-0.103537	4.126498
539.793838	5825.097609	15.687091	-0.103535	4.123710
540.241703	5817.176743	15.692096	-0.103613	4.120975
539.692220	5809.159755	15.697101	-0.103505	4.118191
539.930345	5801.162915	15.702106	-0.103544	4.115422
540.095282	5793.163417	15.707111	-0.103570	4.112650
539.601544	5785.207633	15.712115	-0.103473	4.109883
539.485875	5777.199406	15.717120	-0.103446	4.107100
539.860750	5769.054225	15.722125	-0.103510	4.104275
540.065582	5761.138449	15.727130	-0.103543	4.101525
539.962555	5753.111050	15.732135	-0.103519	4.098730
539.848388	5745.167597	15.737139	-0.103492	4.095962
540.046297	5737.133689	15.742144	-0.103524	4.093166
539.960105	5729.131924	15.747149	-0.103503	4.090374
539.774644	5721.168326	15.752154	-0.103463	4.087593
539.869531	5713.152288	15.757159	-0.103475	4.084795
539.897308	5705.193594	15.762163	-0.103475	4.082015
539.492551	5697.204623	15.767168	-0.103395	4.079216
539.784404	5689.156733	15.772173	-0.103444	4.076404
540.053688	5681.134832	15.777178	-0.103489	4.073599
539.961478	5673.130817	15.782183	-0.103466	4.070793
539.324938	5665.181077	15.787187	-0.103343	4.067997
539.811765	5657.116662	15.792192	-0.103428	4.065174
539.700923	5649.136360	15.797197	-0.103402	4.062371
539.500258	5641.175222	15.802202	-0.103360	4.059571
539.278560	5633.235659	15.807207	-0.103313	4.056776
539.520166	5625.127383	15.812211	-0.103353	4.053927
539.530258	5617.146411	15.817216	-0.103350	4.051117
539.143305	5609.145703	15.822221	-0.103272	4.048292
539.640314	5601.136088	15.827226	-0.103360	4.045476
539.426780	5593.184213	15.832231	-0.103315	4.042667
539.121901	5585.162426	15.837235	-0.103253	4.039830
539.154614	5577.245435	15.842240	-0.103254	4.037033
538.843068	5569.212389	15.847245	-0.103190	4.034188
539.080643	5561.133316	15.852250	-0.103229	4.031333
538.827987	5553.131192	15.857255	-0.103177	4.028496
538.957254	5545.098260	15.862259	-0.103196	4.025652
539.003685	5537.153919	15.867264	-0.103199	4.022836
538.835696	5529.138657	15.872269	-0.103163	4.019989
538.793321	5521.192865	15.877274	-0.103150	4.017167
538.711495	5513.156112	15.882279	-0.103129	4.014310
538.466053	5505.203736	15.887283	-0.103078	4.011479
538.501330	5497.197645	15.892288	-0.103080	4.008631
538.295407	5489.211920	15.897293	-0.103036	4.005784
538.392459	5481.206481	15.902298	-0.103049	4.002933
538.265328	5473.224190	15.907303	-0.103020	4.000084
538.355970	5465.208565	15.912307	-0.103032	3.997225
538.204804	5457.207415	15.917312	-0.102998	3.994366
538.064668	5449.213291	15.922317	-0.102967	3.991506
538.299613	5441.181835	15.927322	-0.103005	3.988638
538.485417	5433.163640	15.932327	-0.103035	3.985772
538.225203	5425.195160	15.937331	-0.102981	3.982914
538.380275	5417.259572	15.942336	-0.103005	3.980072
537.650630	5409.323575	15.947341	-0.102864	3.977214
537.966228	5401.213369	15.952346	-0.102917	3.974308
538.234067	5393.185148	15.957351	-0.102962	3.971429
538.301655	5385.139433	15.962355	-0.102969	3.968539
537.560728	5377.283254	15.967360	-0.102826	3.965700
537.847259	5369.169126	15.972365	-0.102874	3.962784
538.514738	5361.152917	15.977370	-0.102993	3.959909
538.177937	5353.254443	15.982375	-0.102925	3.957055
537.797224	5345.252401	15.987379	-0.102849	3.954162
538.398767	5337.182174	15.992384	-0.102956	3.951259
537.923464	5329.214039	15.997389	-0.102862	3.948372
538.096322	5321.196820	16.002394	-0.102889	3.945477
537.461326	5313.284961	16.007399	-0.102766	3.942603
537.962610	5305.206780	16.012403	-0.102854	3.939687
537.895049	5297.226259	16.017408	-0.102836	3.936794
537.874319	5289.188994	16.022413	-0.102827	3.933880
538.406376	5281.180900	16.027418	-0.102921	3.930984
538.193229	5273.208330	16.032423	-0.102876	3.928084
538.234564	5265.163301	16.037427	-0.102878	3.925162
538.234913	5257.241375	16.042432	-0.102873	3.922281
538.175261	5249.201494	16.047437	-0.102857	3.919353
538.286626	5241.298369	16.052442	-0.102872	3.916477
538.262465	5233.253151	16.057447	-0.102863	3.913544
538.352931	5225.213069	16.062451	-0.102874	3.910613
538.310397	5217.222786	16.067456	-0.102861	3.907696
537.805607	5209.251095	16.072461	-0.102762	3.904774
538.185203	5201.269166	16.077466	-0.102827	3.901863
537.725712	5193.289322	16.082471	-0.102737	3.898935
537.721690	5185.298883	16.087475	-0.102731	3.896009
538.262605	5177.215238	16.092480	-0.102826	3.893058
537.998355	5169.202333	16.097485	-0.102772	3.890115
538.242032	5161.236073	16.102490	-0.102812	3.887196
538.022745	5153.236337	16.107495	-0.102766	3.884254
538.249705	5145.300732	16.112499	-0.102803	3.881342
538.188028	5137.315554	16.117504	-0.102786	3.878404
537.860708	5129.328195	16.122509	-0.102720	3.875457
538.242538	5121.201965	16.127514	-0.102786	3.872472
537.938552	5113.164747	16.132519	-0.102724	3.869503
537.654167	5105.186038	16.137523	-0.102666	3.866554
537.776421	5097.225493	16.142528	-0.102683	3.863617
537.886534	5089.245451	16.147533	-0.102699	3.860671
537.574605	5081.307008	16.152538	-0.102635	3.857729
537.756031	5073.281986	16.157543	-0.102664	3.854763
537.550026	5065.319556	16.162547	-0.102620	3.851810
537.883272	5057.256907	16.167552	-0.102677	3.848829
537.475842	5049.298124	16.172557	-0.102596	3.845868
537.577539	5041.282900	16.177562	-0.102610	3.842895
537.349426	5033.394421	16.182567	-0.102562	3.839960
537.312312	5025.352498	16.187571	-0.102550	3.836969
537.181110	5017.350824	16.192576	-0.102520	3.833989
537.087457	5009.354933	16.197581	-0.102498	3.831010
537.126855	5001.339145	16.202586	-0.102500	3.828024
537.055924	4993.318468	16.207591	-0.102481	3.825031
536.835340	4985.374746	16.212595	-0.102435	3.822061
536.876312	4977.358433	16.217600	-0.102437	3.819068
536.822443	4969.343132	16.222605	-0.102422	3.816070
537.190136	4961.289204	16.227610	-0.102485	3.813065
537.167923	4953.286281	16.232615	-0.102476	3.810069
537.188945	4945.296259	16.237619	-0.102475	3.807075
537.302800	4937.295322	16.242624	-0.102491	3.804078
536.868501	4929.423303	16.247629	-0.102405	3.801114
537.065288	4921.365964	16.252634	-0.102436	3.798092
536.991544	4913.340406	16.257639	-0.102417	3.795073
537.258041	4905.336359	16.262643	-0.102461	3.792068
537.259356	4897.333090	16.267648	-0.102456	3.789055
537.168241	4889.315316	16.272653	-0.102434	3.786032
536.854037	4881.383000	16.277658	-0.102370	3.783034
536.929913	4873.364576	16.282663	-0.102379	3.780010
536.739466	4865.418491	16.287667	-0.102339	3.777004
536.773746	4857.398088	16.292672	-0.102340	3.773973
536.865268	4849.385528	16.297677	-0.102352	3.770944
536.885852	4841.326074	16.302682	-0.102350	3.767894
536.604229	4833.411382	16.307687	-0.102293	3.764888
536.472448	4825.440290	16.312691	-0.102263	3.761862
537.153172	4817.337621	16.317696	-0.102384	3.758803
536.642924	4809.458225	16.322701	-0.102284	3.755798
536.607026	4801.428220	16.327706	-0.102272	3.752745
536.783202	4793.406130	16.332711	-0.102300	3.749697
536.878484	4785.397261	16.337715	-0.102312	3.746650
536.578906	4777.447831	16.342720	-0.102251	3.743614
536.942317	4769.404593	16.347725	-0.102314	3.740555
536.892562	4761.456358	16.352730	-0.102299	3.737520
537.010024	4753.442603	16.357735	-0.102316	3.734462
536.691730	4745.481378	16.362739	-0.102251	3.731410
536.811030	4737.436569	16.367744	-0.102268	3.728335
536.650186	4729.415680	16.372749	-0.102233	3.725260
536.907200	4721.456589	16.377754	-0.102276	3.722216
536.931644	4713.431999	16.382759	-0.102275	3.719138
537.000252	4705.498957	16.387763	-0.102283	3.716095
536.489054	4697.531601	16.392768	-0.102182	3.713021
536.076823	4689.492341	16.397773	-0.102100	3.709919
536.194092	4681.489142	16.402778	-0.102117	3.706842
535.834794	4673.476255	16.407783	-0.102045	3.703747
536.148413	4665.452318	16.412787	-0.102098	3.700662
536.264965	4657.489299	16.417792	-0.102114	3.697592
536.248377	4649.451211	16.422797	-0.102106	3.694488
536.226341	4641.472745	16.427802	-0.102097	3.691404
536.271157	4633.435964	16.432807	-0.102100	3.688297
536.414252	4625.449311	16.437811	-0.102121	3.685209
536.176698	4617.533644	16.442816	-0.102072	3.682136
536.161675	4609.497770	16.447821	-0.102064	3.679019
535.811502	4601.602432	16.452826	-0.101993	3.675946
535.751736	4593.550276	16.457831	-0.101977	3.672817
535.802075	4585.492684	16.462835	-0.101981	3.669686
536.295652	4577.475776	16.467840	-0.102068	3.666580
536.075068	4569.532102	16.472845	-0.102022	3.663481
535.773948	4561.559163	16.477850	-0.101960	3.660365
535.933594	4553.574143	16.482855	-0.101985	3.657255
535.677409	4545.562291	16.487859	-0.101932	3.654120
535.400028	4537.633180	16.492864	-0.101875	3.651014
535.393081	4529.565243	16.497869	-0.101868	3.647859
535.759957	4521.505305	16.502874	-0.101932	3.644714
535.753030	4513.596229	16.507879	-0.101925	3.641615
535.977169	4505.553511	16.512883	-0.101962	3.638468
535.865024	4497.616080	16.517888	-0.101935	3.635350
535.948318	4489.589088	16.522893	-0.101946	3.632200
535.710002	4481.591791	16.527898	-0.101896	3.629049
535.720764	4473.598945	16.532903	-0.101893	3.625905
535.839058	4465.602210	16.537907	-0.101910	3.622759
536.171289	4457.589982	16.542912	-0.101966	3.619611
535.881348	4449.626726	16.547917	-0.101907	3.616461
535.759411	4441.657700	16.552922	-0.101879	3.613311
535.798103	4433.619372	16.557927	-0.101881	3.610136
535.678458	4425.608994	16.562931	-0.101854	3.606964
535.667824	4417.621486	16.567936	-0.101846	3.603802
535.743203	4409.685170	16.572941	-0.101855	3.600660
535.519167	4401.694898	16.577946	-0.101808	3.597485
535.578627	4393.665958	16.582951	-0.101814	3.594300
535.195882	4385.720431	16.587955	-0.101738	3.591132
535.623561	4377.638712	16.592960	-0.101812	3.587931
535.509199	4369.646197	16.597965	-0.101786	3.584747
535.511665	4361.688271	16.602970	-0.101781	3.581577
535.580506	4353.673784	16.607975	-0.101788	3.578384
535.566166	4345.652254	16.612979	-0.101781	3.575183
535.610190	4337.692187	16.617984	-0.101784	3.572005
535.637645	4329.675630	16.622989	-0.101783	3.568801
535.503156	4321.729830	16.627994	-0.101753	3.565618
535.542019	4313.717437	16.632999	-0.101755	3.562410
535.341382	4305.718543	16.638003	-0.101713	3.559198
535.484326	4297.789790	16.643008	-0.101734	3.556021
535.261636	4289.744101	16.648013	-0.101687	3.552784
535.196331	4281.687741	16.653018	-0.101670	3.549544
535.416915	4273.687684	16.658023	-0.101706	3.546332
535.274827	4265.697548	16.663027	-0.101674	3.543111
535.050871	4257.789126	16.668032	-0.101627	3.539916
534.985946	4249.773685	16.673037	-0.101610	3.536681
534.989771	4241.771941	16.678042	-0.101605	3.533450
534.733505	4233.843049	16.683047	-0.101552	3.530238
534.684084	4225.784453	16.688051	-0.101538	3.526977
534.893951	4217.762655	16.693056	-0.101572	3.523736
534.604377	4209.859174	16.698061	-0.101513	3.520524
535.035453	4201.794822	16.703066	-0.101588	3.517266
534.935084	4193.831340	16.708071	-0.101564	3.514030
534.716125	4185.857613	16.713075	-0.101518	3.510783
534.735128	4177.860497	16.718080	-0.101516	3.507531
534.594267	4169.834264	16.723085	-0.101485	3.504259
534.466483	4161.888851	16.728090	-0.101456	3.501017
534.651511	4153.852789	16.733095	-0.101485	3.497745
534.790782	4145.805611	16.738099	-0.101506	3.494464
534.591864	4137.899594	16.743104	-0.101463	3.491227
534.385315	4129.868104	16.748109	-0.101420	3.487935
534.547497	4121.862236	16.753114	-0.101445	3.484662
534.369338	4113.938154	16.758119	-0.101406	3.481409
534.439564	4105.902064	16.763123	-0.101414	3.478115
534.882898	4097.868761	16.768128	-0.101491	3.474831
534.444755	4089.927281	16.773133	-0.101405	3.471553
534.118972	4081.964746	16.778138	-0.101339	3.468267
534.033264	4073.944317	16.783143	-0.101318	3.464962
534.391846	4065.873704	16.788147	-0.101379	3.461648
534.432757	4057.919614	16.793152	-0.101381	3.458368
534.292917	4049.915949	16.798157	-0.101350	3.455058
534.311182	4041.965280	16.803162	-0.101348	3.451772
534.668603	4033.926608	16.808167	-0.101410	3.448459
534.362336	4025.942274	16.813171	-0.101347	3.445142
534.349792	4018.006427	16.818176	-0.101340	3.441852
534.387637	4010.000331	16.823181	-0.101342	3.438531
534.466506	4002.024873	16.828186	-0.101351	3.435222
534.328870	3994.050182	16.833191	-0.101320	3.431902
534.423889	3985.996523	16.838195	-0.101333	3.428554
534.382757	3978.039903	16.843200	-0.101320	3.425238
533.923701	3970.100330	16.848205	-0.101229	3.421912
534.193327	3962.055600	16.853210	-0.101274	3.418564
534.360328	3954.065302	16.858215	-0.101300	3.415232
533.928485	3946.075431	16.863219	-0.101214	3.411876
533.817468	3938.130060	16.868224	-0.101189	3.408546
533.785646	3930.088280	16.873229	-0.101177	3.405176
533.974536	3922.101340	16.878234	-0.101207	3.401832
533.898897	3914.108110	16.883239	-0.101188	3.398474
534.033897	3906.099032	16.888243	-0.101208	3.395113
534.148024	3898.095147	16.893248	-0.101224	3.391751
533.875141	3890.093557	16.898253	-0.101168	3.388372
533.618066	3882.096513	16.903258	-0.101115	3.384992
533.809956	3874.135755	16.908263	-0.101145	3.381640
534.104630	3866.090503	16.913267	-0.101195	3.378253
533.823976	3858.153535	16.918272	-0.101138	3.374887
533.776977	3850.151413	16.923277	-0.101124	3.371499
533.525601	3842.172787	16.928282	-0.101072	3.368110
533.780496	3834.145286	16.933287	-0.101114	3.364716
533.789646	3826.163978	16.938291	-0.101110	3.361329
533.908426	3818.192943	16.943296	-0.101127	3.357946
533.508553	3810.245694	16.948301	-0.101047	3.354551
533.680998	3802.226698	16.953306	-0.101074	3.351144
533.673877	3794.223430	16.958311	-0.101068	3.347733
533.652520	3786.215676	16.963315	-0.101059	3.344315
533.526637	3778.266221	16.968320	-0.101030	3.340916
533.503096	3770.268467	16.973325	-0.101020	3.337496
533.515371	3762.262640	16.978330	-0.101017	3.334071
533.533232	3754.307523	16.983335	-0.101016	3.330664
533.447361	3746.273679	16.988339	-0.100994	3.327215
533.395246	3738.341166	16.993344	-0.100979	3.323808
533.113784	3730.380584	16.998349	-0.100922	3.320377
532.972287	3722.415887	17.003354	-0.100890	3.316946
533.153772	3714.374109	17.008359	-0.100919	3.313490
533.333494	3706.311839	17.013363	-0.100947	3.310022
533.381161	3698.329090	17.018368	-0.100951	3.306579
533.382606	3690.333511	17.023373	-0.100946	3.303125
533.303405	3682.355011	17.028378	-0.100926	3.299672
533.045547	3674.432046	17.033383	-0.100873	3.296233
532.852901	3666.395632	17.038387	-0.100831	3.292743
533.023183	3658.380942	17.043392	-0.100858	3.289273
533.002550	3650.405645	17.048397	-0.100849	3.285809
532.812286	3642.452077	17.053402	-0.100808	3.282345
533.057229	3634.438575	17.058407	-0.100849	3.278867
532.852375	3626.491814	17.063411	-0.100805	3.275398
532.644157	3618.518108	17.068416	-0.100761	3.271912
532.608489	3610.482106	17.073421	-0.100749	3.268403
532.939976	3602.443076	17.078426	-0.100806	3.264903
532.814895	3594.503862	17.083431	-0.100777	3.261425
532.407925	3586.563628	17.088435	-0.100696	3.257931
532.628112	3578.541960	17.093440	-0.100732	3.254423
532.616948	3570.526151	17.098445	-0.100725	3.250905
532.721309	3562.528164	17.103450	-0.100739	3.247395
532.828510	3554.527160	17.108455	-0.100754	3.243880
532.769394	3546.573708	17.113459	-0.100738	3.240376
532.576551	3538.653449	17.118464	-0.100696	3.236876
532.629781	3530.592894	17.123469	-0.100701	3.233322
532.640658	3522.597433	17.128474	-0.100698	3.229790
532.678609	3514.606047	17.133479	-0.100700	3.226258
532.542465	3506.594026	17.138483	-0.100669	3.222705
532.613863	3498.642379	17.143488	-0.100677	3.219183
532.553562	3490.668286	17.148493	-0.100661	3.215643
532.433897	3482.648939	17.153498	-0.100633	3.212076
532.434879	3474.650936	17.158503	-0.100628	3.208519
532.328679	3466.646795	17.163507	-0.100603	3.204951
532.375391	3458.697217	17.168512	-0.100607	3.201410
532.009620	3450.752562	17.173517	-0.100533	3.197850
532.013759	3442.750702	17.178522	-0.100529	3.194276
532.156338	3434.746579	17.183527	-0.100550	3.190703
532.000118	3426.752268	17.188531	-0.100516	3.187117
532.280206	3418.712375	17.193536	-0.100563	3.183526
531.992734	3410.777358	17.198541	-0.100504	3.179953
532.073309	3402.793497	17.203546	-0.100514	3.176370
532.122648	3394.782092	17.208551	-0.100518	3.172770
531.898815	3386.778626	17.213555	-0.100471	3.169156
531.830256	3378.858561	17.218560	-0.100453	3.165584
531.723201	3370.859269	17.223565	-0.100428	3.161969
531.731449	3362.866179	17.228570	-0.100424	3.158359
532.018641	3354.862452	17.233575	-0.100472	3.154752
531.840905	3346.877606	17.238579	-0.100434	3.151128
531.713199	3338.895044	17.243584	-0.100405	3.147504
531.763080	3330.848530	17.248589	-0.100409	3.143854
531.715593	3322.910924	17.253594	-0.100395	3.140245
531.930361	3314.925622	17.258599	-0.100430	3.136623
531.869472	3306.880199	17.263603	-0.100413	3.132956
531.994156	3298.914051	17.268608	-0.100431	3.129329
531.907947	3290.946650	17.273613	-0.100410	3.125688
531.919160	3282.959735	17.278618	-0.100407	3.122039
531.856900	3275.036560	17.283623	-0.100390	3.118411
531.820974	3267.014423	17.288627	-0.100378	3.114734
531.694428	3259.059864	17.293632	-0.100349	3.111080
531.745076	3251.048641	17.298637	-0.100354	3.107404
531.545630	3243.068694	17.303642	-0.100311	3.103726
531.496182	3235.122477	17.308647	-0.100297	3.100067
531.367915	3227.105623	17.313651	-0.100268	3.096367
531.556973	3219.085858	17.318656	-0.100298	3.092676
531.459254	3211.098627	17.323661	-0.100274	3.088982
531.450054	3203.135607	17.328666	-0.100267	3.085299
531.506644	3195.163264	17.333671	-0.100273	3.081610
531.428569	3187.162372	17.338675	-0.100253	3.077897
531.494585	3179.176594	17.343680	-0.100260	3.074194
531.411178	3171.157317	17.348685	-0.100239	3.070463
531.347173	3163.178698	17.353690	-0.100222	3.066748
531.335133	3155.218498	17.358695	-0.100215	3.063040
531.303792	3147.188990	17.363699	-0.100204	3.059293
531.131690	3139.286111	17.368704	-0.100166	3.055595
530.965500	3131.295511	17.373709	-0.100130	3.051851
531.127515	3123.247438	17.378714	-0.100155	3.048091
531.238208	3115.251825	17.383719	-0.100171	3.044349
530.855271	3107.345967	17.388723	-0.100094	3.040620
530.863277	3099.377356	17.393728	-0.100090	3.036877
531.060078	3091.345781	17.398733	-0.100122	3.033108
530.686183	3083.386480	17.403738	-0.100047	3.029341
530.622261	3075.414029	17.408743	-0.100030	3.025578
530.735611	3067.392598	17.413747	-0.100046	3.021796
530.844357	3059.429153	17.418752	-0.100061	3.018037
530.681265	3051.437014	17.423757	-0.100025	3.014245
530.690697	3043.434814	17.428762	-0.100022	3.010453
530.940987	3035.435609	17.433767	-0.100063	3.006669
530.668327	3027.505080	17.438771	-0.100007	3.002887
530.629174	3019.521844	17.443776	-0.099995	2.999087
530.581152	3011.557552	17.448781	-0.099980	2.995291
530.630371	3003.535452	17.453786	-0.099984	2.991467
530.653895	2995.549195	17.458791	-0.099984	2.987654
530.408707	2987.554247	17.463795	-0.099933	2.983818
530.548407	2979.594262	17.468800	-0.099953	2.980014
530.504808	2971.608738	17.473805	-0.099940	2.976184
530.434705	2963.620773	17.478810	-0.099922	2.972345
530.511840	2955.631838	17.483815	-0.099931	2.968509
530.471034	2947.627029	17.488819	-0.099918	2.964655
530.193467	2939.706172	17.493824	-0.099861	2.960823
530.311378	2931.714068	17.498829	-0.099878	2.956973
530.368499	2923.709853	17.503834	-0.099883	2.953108
530.248599	2915.742430	17.508839	-0.099856	2.949247
529.725333	2907.824941	17.513843	-0.099753	2.945384
530.376376	2899.759086	17.518848	-0.099869	2.941506
530.042190	2891.817019	17.523853	-0.099802	2.937631
529.981775	2883.815854	17.528858	-0.099785	2.933736
529.969505	2875.846331	17.533863	-0.099778	2.929854
529.794236	2867.875222	17.538867	-0.099740	2.925957
529.769135	2859.904043	17.543872	-0.099730	2.922064
529.765868	2851.922590	17.548877	-0.099724	2.918161
529.719064	2843.939423	17.553882	-0.099710	2.914250
529.670884	2835.915607	17.558887	-0.099696	2.910313
529.533345	2827.913218	17.563891	-0.099665	2.906377
529.683648	2819.917695	17.568896	-0.099688	2.902454
529.541603	2811.990147	17.573901	-0.099656	2.898544
529.369651	2803.984301	17.578906	-0.099619	2.894588
529.547957	2796.027495	17.583911	-0.099647	2.890670
529.320533	2788.032082	17.588915	-0.099600	2.886706
529.172900	2780.069092	17.593920	-0.099567	2.882756
529.266364	2772.085629	17.598925	-0.099579	2.878804
529.074021	2764.142068	17.603930	-0.099538	2.874851
529.314168	2756.136350	17.608935	-0.099578	2.870885
529.335227	2748.106103	17.613939	-0.099576	2.866890
529.534038	2740.128923	17.618944	-0.099608	2.862925
529.305227	2732.185462	17.623949	-0.099560	2.858948
528.990628	2724.261035	17.628954	-0.099497	2.854969
529.242899	2716.249775	17.633959	-0.099538	2.850974
528.738544	2708.288387	17.638963	-0.099439	2.846955
528.898516	2700.300098	17.643968	-0.099464	2.842955
528.733132	2692.334039	17.648973	-0.099428	2.838942
528.349006	2684.423565	17.653978	-0.099351	2.834938
528.251477	2676.456983	17.658983	-0.099328	2.830917
528.306794	2668.369275	17.663987	-0.099333	2.826838
528.585767	2660.348969	17.668992	-0.099379	2.822800
528.624945	2652.381152	17.673997	-0.099381	2.818768
528.599175	2644.391585	17.679002	-0.099371	2.814717
528.425120	2636.462620	17.684007	-0.099334	2.810681
528.481132	2628.460834	17.689011	-0.099339	2.806616
528.494397	2620.486593	17.694016	-0.099336	2.802557
528.502905	2612.523837	17.699021	-0.099333	2.798498
528.258342	2604.559904	17.704026	-0.099282	2.794417
528.544981	2596.564773	17.709031	-0.099330	2.790345
528.340629	2588.609200	17.714035	-0.099287	2.786259
528.079863	2580.678696	17.719040	-0.099233	2.782176
527.741049	2572.741782	17.724045	-0.099165	2.778079
527.918630	2564.692530	17.729050	-0.099193	2.773949
528.577961	2556.608874	17.734055	-0.099310	2.769825
528.349825	2548.667299	17.739059	-0.099262	2.765713
528.233732	2540.720229	17.744064	-0.099236	2.761600
527.886610	2532.836447	17.749069	-0.099166	2.757499
528.061015	2524.781327	17.754074	-0.099193	2.753336
528.192699	2516.761383	17.759079	-0.099212	2.749181
528.224448	2508.760538	17.764083	-0.099213	2.745024
527.994089	2500.855069	17.769088	-0.099165	2.740894
527.999542	2492.897081	17.774093	-0.099161	2.736746
527.860088	2484.902712	17.779098	-0.099130	2.732562
527.712408	2476.968171	17.784103	-0.099097	2.728404
527.905992	2468.927574	17.789107	-0.099128	2.724204
528.023887	2460.985041	17.794112	-0.099144	2.720045
527.622319	2453.072968	17.799117	-0.099065	2.715863
527.595262	2445.061908	17.804122	-0.099054	2.711646
527.739300	2437.075288	17.809127	-0.099076	2.707446
527.293609	2429.149609	17.814131	-0.098988	2.703234
527.663881	2421.107331	17.819136	-0.099051	2.699006
527.908625	2413.135629	17.824141	-0.099092	2.694800
527.886683	2405.130295	17.829146	-0.099082	2.690553
527.350677	2397.274565	17.834151	-0.098977	2.686346
527.467529	2389.240705	17.839155	-0.098994	2.682080
527.229242	2381.340059	17.844160	-0.098944	2.677854
527.230558	2373.336302	17.849165	-0.098939	2.673583
526.635809	2365.422778	17.854170	-0.098824	2.669314
527.112482	2357.355110	17.859175	-0.098907	2.665025
527.205864	2349.350002	17.864179	-0.098919	2.660739
527.275607	2341.377479	17.869184	-0.098927	2.656461
527.150323	2333.436498	17.874189	-0.098898	2.652180
527.273383	2325.410407	17.879194	-0.098916	2.647863
527.443209	2317.450803	17.884199	-0.098943	2.643578
527.409809	2309.485814	17.889203	-0.098931	2.639270
526.874909	2301.643377	17.894208	-0.098826	2.634987
526.940672	2293.625171	17.899213	-0.098833	2.630643
527.191684	2285.584274	17.904218	-0.098875	2.626291
527.340579	2277.601910	17.909223	-0.098897	2.621957
527.002359	2269.704987	17.914227	-0.098829	2.617629
526.885499	2261.752316	17.919232	-0.098802	2.613279
526.813516	2253.777694	17.924237	-0.098784	2.608913
527.024936	2245.730931	17.929242	-0.098818	2.604519
526.887310	2237.843063	17.934247	-0.098787	2.600181
526.665632	2229.897539	17.939251	-0.098741	2.595798
526.357558	2221.890585	17.944256	-0.098678	2.591368
526.807019	2213.783286	17.949261	-0.098756	2.586927
526.411122	2205.882776	17.954266	-0.098677	2.582535
526.280855	2197.958202	17.959271	-0.098648	2.578140
525.929813	2190.026723	17.964275	-0.098577	2.573718
525.902526	2182.051543	17.969280	-0.098567	2.569287
526.633435	2173.936853	17.974285	-0.098698	2.564824
526.497857	2166.017743	17.979290	-0.098668	2.560401
526.420171	2158.085757	17.984295	-0.098648	2.555967
526.242492	2150.144328	17.989299	-0.098610	2.551514
526.405667	2142.153919	17.994304	-0.098635	2.547049
526.458422	2134.169561	17.999309	-0.098639	2.542572
526.187503	2126.250609	18.004314	-0.098584	2.538101
526.541400	2118.260759	18.009319	-0.098644	2.533627
526.270189	2110.305551	18.014323	-0.098589	2.529119
526.462353	2102.311503	18.019328	-0.098619	2.524615
526.659586	2094.365929	18.024333	-0.098651	2.520131
526.335861	2086.444305	18.029338	-0.098585	2.515614
526.449545	2078.462265	18.034343	-0.098601	2.511087
526.392439	2070.473602	18.039347	-0.098585	2.506535
526.312232	2062.542944	18.044352	-0.098565	2.502006
526.306436	2054.565449	18.049357	-0.098559	2.497448
526.186599	2046.610235	18.054362	-0.098532	2.492886
526.472838	2038.609514	18.059367	-0.098580	2.488320
526.035402	2030.690644	18.064371	-0.098493	2.483738
525.639329	2022.810525	18.069376	-0.098414	2.479173
525.916384	2014.798833	18.074381	-0.098460	2.474574
525.827799	2006.807018	18.079386	-0.098439	2.469951
525.909655	1998.831604	18.084391	-0.098449	2.465341
525.941323	1990.853693	18.089395	-0.098449	2.460717
525.778262	1982.942369	18.094400	-0.098414	2.456109
525.788124	1974.967239	18.099405	-0.098411	2.451468
525.763111	1966.971141	18.104410	-0.098401	2.446803
525.872794	1959.024312	18.109415	-0.098416	2.442169
525.736434	1951.104220	18.114419	-0.098385	2.437522
525.596497	1943.143144	18.119424	-0.098354	2.432842
525.661354	1935.129192	18.124429	-0.098361	2.428138
525.740206	1927.128597	18.129434	-0.098370	2.423434
525.669767	1919.206940	18.134439	-0.098352	2.418756
525.773437	1911.226549	18.139443	-0.098366	2.414047
525.561322	1903.303218	18.144448	-0.098321	2.409338
525.533471	1895.339632	18.149453	-0.098311	2.404611
525.462744	1887.395088	18.154458	-0.098293	2.399882
525.397282	1879.473387	18.159463	-0.098275	2.395157
525.181356	1871.516196	18.164467	-0.098230	2.390391
525.359724	1863.511642	18.169472	-0.098258	2.385618
525.154458	1855.607610	18.174477	-0.098215	2.380864
524.634685	1847.724955	18.179482	-0.098113	2.376089
525.028829	1839.688598	18.184487	-0.098181	2.371285
524.962740	1831.706605	18.189491	-0.098163	2.366468
524.801614	1823.781370	18.194496	-0.098128	2.361666
524.731168	1815.846416	18.199501	-0.098110	2.356857
524.626913	1807.870327	18.204506	-0.098085	2.352010
524.444690	1799.939797	18.209511	-0.098046	2.347174
524.478092	1791.945710	18.214515	-0.098047	2.342307
524.296930	1784.026292	18.219520	-0.098008	2.337458
523.876776	1776.139950	18.224525	-0.097925	2.332599
524.094303	1768.100032	18.229530	-0.097960	2.327689
523.942289	1760.161478	18.234535	-0.097926	2.322800
523.743584	1752.224338	18.239539	-0.097884	2.317898
524.207488	1744.182140	18.244544	-0.097965	2.312976
524.383802	1736.210359	18.249549	-0.097993	2.308063
523.766461	1728.344189	18.254554	-0.097873	2.303138
523.907772	1720.388001	18.259559	-0.097894	2.298210
523.750320	1712.461151	18.264563	-0.097860	2.293265
523.951994	1704.444623	18.269568	-0.097892	2.288284
523.821901	1696.530213	18.274573	-0.097862	2.283327
523.748864	1688.602006	18.279578	-0.097844	2.278356
523.856513	1680.622599	18.284583	-0.097859	2.273358
523.791456	1672.630350	18.289587	-0.097841	2.268325
523.715000	1664.676006	18.294592	-0.097822	2.263304
523.950274	1656.715188	18.299597	-0.097860	2.258295
523.764956	1648.785693	18.304602	-0.097821	2.253258
523.666465	1640.854548	18.309607	-0.097797	2.248216
523.626255	1632.918634	18.314611	-0.097784	2.243165
523.603623	1624.975889	18.319616	-0.097775	2.238100
523.678374	1617.024291	18.324621	-0.097784	2.233026
523.510381	1609.085098	18.329626	-0.097747	2.227927
523.438410	1601.166714	18.334631	-0.097729	2.222838
523.438713	1593.197911	18.339635	-0.097724	2.217712
523.572277	1585.224618	18.344640	-0.097743	2.212582
523.424466	1577.312809	18.349645	-0.097711	2.207455
523.268232	1569.366988	18.354650	-0.097676	2.202294
523.321040	1561.457359	18.359655	-0.097681	2.197163
523.599183	1553.449403	18.364659	-0.097727	2.191976
523.426239	1545.532349	18.369664	-0.097690	2.186795
522.820340	1537.690468	18.374669	-0.097572	2.181610
523.058087	1529.652178	18.379674	-0.097611	2.176363
523.277273	1521.692199	18.384679	-0.097647	2.171153
522.989560	1513.780897	18.389683	-0.097588	2.165915
522.875178	1505.853998	18.394688	-0.097562	2.160670
523.292469	1497.851002	18.399693	-0.097634	2.155413
523.028252	1489.963233	18.404698	-0.097580	2.150154
522.598404	1482.091984	18.409703	-0.097495	2.144878
522.530067	1474.153615	18.414707	-0.097477	2.139578
522.713403	1466.166545	18.419712	-0.097506	2.134257
522.519618	1458.261021	18.424717	-0.097464	2.128940
522.225661	1450.337142	18.429722	-0.097404	2.123588
522.276722	1442.417620	18.434727	-0.097409	2.118260
522.584295	1434.399354	18.439731	-0.097461	2.112876
522.486741	1426.425180	18.444736	-0.097437	2.107468
522.355698	1418.512908	18.449741	-0.097408	2.102086
522.177340	1410.600815	18.454746	-0.097369	2.096685
521.938328	1402.712330	18.459751	-0.097320	2.091280
521.967185	1394.744531	18.464755	-0.097320	2.085833
521.955069	1386.820980	18.469760	-0.097312	2.080398
521.911956	1378.906320	18.474765	-0.097299	2.074953
521.682292	1370.996980	18.479770	-0.097251	2.069477
521.599072	1363.073981	18.484775	-0.097231	2.063993
520.937615	1355.237049	18.489779	-0.097102	2.058494
520.934463	1347.267488	18.494784	-0.097097	2.052956
521.050962	1339.304735	18.499789	-0.097113	2.047420
521.023230	1331.351830	18.504794	-0.097103	2.041861
521.038704	1323.434908	18.509799	-0.097100	2.036316
520.778736	1315.515799	18.514803	-0.097047	2.030726
520.803019	1307.552337	18.519808	-0.097046	2.025119
520.862293	1299.621377	18.524813	-0.097052	2.019523
520.429089	1291.750945	18.529818	-0.096966	2.013902
520.560006	1283.785557	18.534823	-0.096985	2.008258
519.907298	1275.964060	18.539827	-0.096859	2.002618
519.631813	1268.062303	18.544832	-0.096802	1.996944
519.115550	1260.209694	18.549837	-0.096701	1.991263
519.386113	1252.166680	18.554842	-0.096746	1.985513
519.301883	1244.247918	18.559847	-0.096725	1.979799
518.919692	1236.383656	18.564851	-0.096649	1.974074
518.880473	1228.419321	18.569856	-0.096636	1.968298
518.317730	1220.582770	18.574861	-0.096527	1.962541
518.128564	1212.644747	18.579866	-0.096486	1.956733
517.729757	1204.782379	18.584871	-0.096407	1.950940
517.954045	1196.741960	18.589875	-0.096443	1.945068
518.122206	1188.764143	18.594880	-0.096469	1.939218
517.888471	1180.880347	18.599885	-0.096421	1.933375
517.564143	1172.981155	18.604890	-0.096355	1.927493
517.031670	1165.149127	18.609895	-0.096251	1.921620
516.420975	1157.285279	18.614899	-0.096132	1.915695
516.387373	1149.332887	18.619904	-0.096121	1.909751
515.938589	1141.452665	18.624909	-0.096032	1.903796
515.477329	1133.574258	18.629914	-0.095941	1.897821
515.451416	1125.625424	18.634919	-0.095931	1.891825
514.973316	1117.737916	18.639923	-0.095837	1.885803
514.586329	1109.866598	18.644928	-0.095759	1.879785
513.906129	1102.040395	18.649933	-0.095628	1.873748
513.546627	1094.100941	18.654938	-0.095556	1.867642
512.917311	1086.242878	18.659943	-0.095433	1.861547
512.561263	1078.319509	18.664947	-0.095362	1.855413
512.616440	1070.331606	18.669952	-0.095367	1.849258
512.319107	1062.444529	18.674957	-0.095306	1.843118
511.695858	1054.589567	18.679962	-0.095185	1.836944
511.322318	1046.708855	18.684967	-0.095110	1.830759
511.093964	1038.769485	18.689971	-0.095063	1.824524
510.381504	1030.953658	18.694976	-0.094925	1.818306
510.290425	1023.000766	18.699981	-0.094903	1.812034
510.113305	1015.064311	18.704986	-0.094865	1.805743
509.465972	1007.263929	18.709991	-0.094739	1.799480
509.020934	999.376402	18.714995	-0.094651	1.793151
508.715750	991.441873	18.720000	-0.094589	1.786778
507.960730	983.630018	18.725005	-0.094443	1.780425
507.186548	975.784000	18.730010	-0.094294	1.774019
506.973964	967.859879	18.735015	-0.094249	1.767598
506.488516	959.975978	18.740019	-0.094154	1.761151
505.811804	952.141309	18.745024	-0.094023	1.754695
505.813743	944.184339	18.750029	-0.094018	1.748203
505.344078	936.296959	18.755034	-0.093925	1.741683
504.509426	928.511980	18.760039	-0.093765	1.735175
504.097766	920.608910	18.765043	-0.093683	1.728600
504.077283	912.665668	18.770048	-0.093674	1.722018
503.388806	904.869262	18.775053	-0.093540	1.715444
502.363005	897.085843	18.780058	-0.093344	1.708812
501.881999	889.205166	18.785063	-0.093250	1.702144
501.079288	881.381303	18.790067	-0.093095	1.695455
500.735510	873.455166	18.795072	-0.093026	1.688713
500.688674	865.511502	18.800077	-0.093012	1.681970
499.841929	857.723538	18.805082	-0.092849	1.675224
499.640036	849.813883	18.810087	-0.092806	1.668434
499.473610	841.890823	18.815091	-0.092770	1.661610
498.784653	834.096855	18.820096	-0.092637	1.654797
498.518948	826.215215	18.825101	-0.092582	1.647938
497.889507	818.377911	18.830106	-0.092460	1.641039
497.188797	810.588412	18.835111	-0.092324	1.634141
496.974135	802.644142	18.840115	-0.092279	1.627147
496.381139	794.813576	18.845120	-0.092164	1.620170
495.803082	787.011212	18.850125	-0.092051	1.613189
495.671778	779.068620	18.855130	-0.092021	1.606116
495.256092	771.253094	18.860135	-0.091939	1.599085
494.940705	763.389238	18.865139	-0.091875	1.591994
494.647953	755.525542	18.870144	-0.091815	1.584874
493.758504	747.812522	18.875149	-0.091645	1.577772
493.232673	739.954268	18.880154	-0.091542	1.570558
492.906562	732.115334	18.885159	-0.091476	1.563358
492.609602	724.271372	18.890163	-0.091415	1.556124
492.148510	716.434438	18.895168	-0.091324	1.548839
491.608232	708.616876	18.900173	-0.091219	1.541525
491.388603	700.744789	18.905178	-0.091173	1.534173
491.008042	692.923455	18.910183	-0.091097	1.526809
490.408571	685.146515	18.915187	-0.090980	1.519417
490.038309	677.332006	18.920192	-0.090906	1.511989
489.505562	669.533336	18.925197	-0.090802	1.504514
489.319372	661.673490	18.930202	-0.090762	1.496997
489.130232	653.832751	18.935207	-0.090721	1.489460
488.426466	646.092878	18.940211	-0.090585	1.481900
487.804888	638.344677	18.945216	-0.090465	1.474307
487.832568	630.428390	18.950221	-0.090465	1.466614
486.883450	622.727217	18.955226	-0.090283	1.458933
486.351144	614.952454	18.960231	-0.090179	1.451207
485.416894	607.240060	18.965235	-0.090000	1.443435
485.318842	599.378030	18.970240	-0.089976	1.435610
485.699413	591.446902	18.975245	-0.090042	1.427751
485.197934	583.681804	18.980250	-0.089943	1.419870
484.659326	575.956018	18.985255	-0.089838	1.411977
484.100910	568.200654	18.990259	-0.089729	1.404007
483.640638	560.459016	18.995264	-0.089638	1.396022
483.374439	552.658537	19.000269	-0.089584	1.387963
482.649484	544.939845	19.005274	-0.089444	1.379863
482.263872	537.184594	19.010279	-0.089367	1.371735
481.381361	529.510330	19.015283	-0.089197	1.363557
481.106308	521.724660	19.020288	-0.089141	1.355318
480.244738	514.055480	19.025293	-0.088976	1.347049
479.820352	506.285388	19.030298	-0.088892	1.338698
479.866707	498.452844	19.035303	-0.088895	1.330313
478.996571	490.805845	19.040307	-0.088728	1.321909
478.332269	483.093300	19.045312	-0.088599	1.313417
478.227433	475.223539	19.050317	-0.088575	1.304800
477.854376	467.488865	19.055322	-0.088500	1.296225
477.683909	459.732556	19.060327	-0.088463	1.287606
476.943585	452.093163	19.065331	-0.088320	1.278953
476.720141	444.338109	19.070336	-0.088274	1.270209
476.331706	436.655758	19.075341	-0.088196	1.261454
475.811999	428.979020	19.080346	-0.088095	1.252619
474.940159	421.384676	19.085351	-0.087927	1.243748
474.725912	413.666520	19.090355	-0.087882	1.234798
474.351214	405.966748	19.095360	-0.087808	1.225772
473.834273	398.322696	19.100365	-0.087706	1.216717
473.662726	390.590626	19.105370	-0.087669	1.207558
473.019218	382.999759	19.110375	-0.087545	1.198402
472.793731	375.319184	19.115379	-0.087498	1.189153
472.013070	367.737594	19.120384	-0.087347	1.179836
472.011190	360.033246	19.125389	-0.087342	1.170458
471.369010	352.437416	19.130394	-0.087217	1.161002
470.373307	344.932213	19.135399	-0.087027	1.151506
469.988183	337.277202	19.140403	-0.086950	1.141874
469.886121	329.602907	19.145408	-0.086926	1.132197
469.139985	322.067130	19.150413	-0.086782	1.122472
468.842654	314.448733	19.155418	-0.086722	1.112655
468.333031	306.884929	19.160423	-0.086622	1.102773
467.980078	299.304677	19.165427	-0.086552	1.092816
467.249783	291.794185	19.170432	-0.086411	1.082773
467.048357	284.215178	19.175437	-0.086368	1.072666
466.006155	276.776431	19.180442	-0.086169	1.062456
465.389682	269.276162	19.185447	-0.086050	1.052163
464.741225	261.782183	19.190451	-0.085924	1.041768
463.853109	254.347200	19.195456	-0.085754	1.031293
462.852989	246.936253	19.200461	-0.085563	1.020717
462.730513	239.360695	19.205466	-0.085535	1.010012
462.039520	231.923511	19.210471	-0.085401	0.999248
461.031429	224.529689	19.215475	-0.085209	0.988350
459.939350	217.164535	19.220480	-0.085001	0.977351
458.950067	209.801093	19.225485	-0.084812	0.966254
457.869611	202.453474	19.230490	-0.084606	0.955029
455.768999	195.298377	19.235495	-0.084210	0.943690
453.870498	188.093552	19.240499	-0.083852	0.932190
450.896777	181.087507	19.245504	-0.083293	0.920561
447.124436	174.198154	19.250509	-0.082586	0.908745
443.210102	167.278650	19.255514	-0.081853	0.896683
437.897815	160.601183	19.260519	-0.080860	0.884448
430.596887	154.239557	19.265523	-0.079496	0.871982
422.954151	147.854818	19.270528	-0.078069	0.859191
414.724891	141.528901	19.275533	-0.076532	0.846127
405.387786	135.328939	19.280538	-0.074790	0.832732
396.768179	128.955578	19.285543	-0.073181	0.819031
389.799977	122.269966	19.290547	-0.071879	0.805055
382.481006	115.674170	19.295552	-0.070512	0.790878
374.529869	109.190300	19.300557	-0.069027	0.776436
366.683838	102.692207	19.305562	-0.067562	0.761723
360.115694	95.996447	19.310567	-0.066334	0.746771
353.186166	89.399230	19.315571	-0.065040	0.731576
346.190671	83.026231	19.320576	-0.063733	0.716479