Fri Apr 16 18:56:36 2021

Number of Points = 3642
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.884271	-0.059465	0.000000	-0.000062	0.311070

0.849794	-0.095352	0.005005	-0.000055	0.310874
0.574222	-0.067827	0.010010	-0.000004	0.310769
0.534361	-0.062396	0.015014	0.000003	0.310760
0.650227	-0.082499	0.020019	-0.000018	0.310765
0.582866	-0.071716	0.025024	-0.000006	0.310758
0.352463	-0.028532	0.030029	0.000037	0.310764
0.712370	-0.094402	0.035034	-0.000030	0.310762
0.410293	-0.039445	0.040038	0.000026	0.310762
0.774062	-0.106532	0.045043	-0.000041	0.310758
0.893277	-0.128946	0.050048	-0.000064	0.310754
0.642018	-0.081155	0.055053	-0.000017	0.310764
0.861748	-0.120188	0.060058	-0.000058	0.310768
0.712871	-0.096682	0.065062	-0.000030	0.310752
0.465697	-0.048292	0.070067	0.000016	0.310768
0.678963	-0.132377	0.075072	-0.000024	0.310557
0.593558	-0.127243	0.080077	-0.000008	0.310508
0.893664	-0.181076	0.085082	-0.000064	0.310512
0.714676	-0.149190	0.090086	-0.000030	0.310509
0.864885	-0.175873	0.095091	-0.000058	0.310511
0.991151	-0.201309	0.100096	-0.000082	0.310500
0.964080	-0.249730	0.105101	-0.000077	0.310251
0.542694	-0.190379	0.110106	0.000002	0.310171
0.633774	-0.209562	0.115110	-0.000015	0.310159
0.821295	-0.243548	0.120115	-0.000050	0.310159
0.610897	-0.204502	0.125120	-0.000011	0.310163
0.652392	-0.265573	0.130125	-0.000019	0.309913
0.893710	-0.323313	0.135130	-0.000063	0.309848
1.162071	-0.375698	0.140134	-0.000113	0.309831
0.805514	-0.309053	0.145139	-0.000047	0.309840
0.813329	-0.365790	0.150144	-0.000048	0.309582
0.882377	-0.394734	0.155149	-0.000061	0.309505
0.952618	-0.407007	0.160154	-0.000074	0.309507
0.985671	-0.430831	0.165158	-0.000081	0.309424
0.823141	-0.443370	0.170163	-0.000050	0.309227
0.558249	-0.394942	0.175168	-0.000001	0.309229
0.058821	-0.300611	0.180173	0.000092	0.309245
0.225813	-0.384499	0.185178	0.000061	0.308995
0.316978	-0.420522	0.190182	0.000044	0.308904
0.270383	-0.411019	0.195187	0.000053	0.308908
0.582011	-0.498899	0.200192	-0.000005	0.308762
0.598247	-0.540161	0.205197	-0.000008	0.308582
0.593835	-0.539014	0.210202	-0.000008	0.308584
0.498801	-0.560113	0.215206	0.000010	0.308404
0.507792	-0.591454	0.220211	0.000009	0.308265
0.550260	-0.599499	0.225216	0.000001	0.308263
0.490608	-0.637589	0.230221	0.000012	0.308033
0.333135	-0.618577	0.235226	0.000041	0.307988
0.466331	-0.657182	0.240230	0.000016	0.307921
0.303687	-0.685882	0.245235	0.000047	0.307647
0.616413	-0.746857	0.250240	-0.000012	0.307627
0.662851	-0.800063	0.255245	-0.000020	0.307417
0.556930	-0.801661	0.260250	-0.000000	0.307319
0.464437	-0.809429	0.265254	0.000017	0.307203
0.826073	-0.920180	0.270259	-0.000051	0.306991
0.488667	-0.866910	0.275264	0.000012	0.306953
0.288581	-0.883183	0.280269	0.000050	0.306705
0.266878	-0.876588	0.285274	0.000054	0.306717
0.464801	-0.980031	0.290278	0.000017	0.306399
-0.119730	-0.875130	0.295283	0.000126	0.306393
0.205497	-0.984172	0.300288	0.000065	0.306157
0.327469	-1.027105	0.305293	0.000042	0.306058
0.227934	-1.049566	0.310298	0.000061	0.305867
0.436253	-1.116021	0.315302	0.000022	0.305731
0.530718	-1.166910	0.320307	0.000005	0.305572
0.451171	-1.172000	0.325312	0.000019	0.305479
0.469956	-1.230635	0.330317	0.000016	0.305218
0.409181	-1.236076	0.335322	0.000027	0.305139
0.311095	-1.279403	0.340326	0.000046	0.304849
0.110882	-1.251746	0.345331	0.000083	0.304808
0.208901	-1.335671	0.350336	0.000065	0.304494
0.282726	-1.365227	0.355341	0.000051	0.304417
0.111354	-1.376086	0.360346	0.000083	0.304218
0.231698	-1.436707	0.365350	0.000060	0.304033
0.300897	-1.482560	0.370355	0.000048	0.303875
0.192119	-1.515816	0.375360	0.000068	0.303622
0.047852	-1.510391	0.380365	0.000095	0.303523
0.022667	-1.564423	0.385370	0.000100	0.303244
0.134915	-1.613500	0.390374	0.000079	0.303107
-0.055195	-1.609548	0.395379	0.000114	0.302961
-0.172484	-1.645743	0.400384	0.000136	0.302686
-0.027858	-1.699472	0.405389	0.000109	0.302555
-0.027269	-1.752020	0.410394	0.000109	0.302304
-0.063649	-1.790473	0.415398	0.000116	0.302088
-0.224365	-1.786151	0.420403	0.000146	0.301969
-0.298626	-1.830749	0.425408	0.000159	0.301691
-0.321822	-1.863679	0.430413	0.000164	0.301512
-0.420451	-1.879038	0.435418	0.000182	0.301353
-0.313874	-1.962340	0.440422	0.000162	0.301045
-0.329165	-1.991194	0.445427	0.000165	0.300893
-0.441449	-2.006899	0.450432	0.000186	0.300720
-0.695164	-2.009922	0.455437	0.000233	0.300483
-0.594767	-2.061875	0.460442	0.000215	0.300321
-0.777369	-2.067767	0.465446	0.000249	0.300133
-0.838750	-2.119102	0.470451	0.000260	0.299831
-1.091720	-2.110141	0.475456	0.000307	0.299653
-1.597107	-2.050122	0.480461	0.000401	0.299499
-1.903391	-2.050455	0.485466	0.000458	0.299228
-2.012658	-2.065542	0.490470	0.000479	0.299059
-2.303686	-2.047874	0.495475	0.000533	0.298889
-2.447898	-2.076898	0.500480	0.000560	0.298621
-2.668205	-2.064516	0.505485	0.000601	0.298487
-2.609094	-2.124960	0.510490	0.000590	0.298246
-2.634621	-2.161562	0.515494	0.000595	0.298046
-2.919011	-2.133682	0.520499	0.000648	0.297930
-3.525507	-2.087540	0.525504	0.000761	0.297619
-3.365439	-2.144657	0.530509	0.000731	0.297483
-3.349868	-2.183149	0.535514	0.000728	0.297309
-3.857545	-2.146043	0.540518	0.000822	0.297041
-4.060938	-2.128778	0.545523	0.000860	0.296945
-4.302918	-2.136577	0.550528	0.000905	0.296692
-4.356643	-2.157832	0.555533	0.000915	0.296541
-4.811109	-2.112087	0.560538	0.001000	0.296361
-4.906653	-2.140879	0.565542	0.001018	0.296136
-5.173822	-2.109657	0.570547	0.001067	0.296051
-5.350723	-2.138678	0.575552	0.001100	0.295752
-5.348257	-2.151114	0.580557	0.001100	0.295693
-5.571569	-2.152000	0.585562	0.001142	0.295490
-6.034379	-2.093222	0.590566	0.001228	0.295366
-6.191787	-2.109702	0.595571	0.001257	0.295145
-6.098824	-2.158195	0.600576	0.001240	0.294990
-6.704486	-2.080875	0.605581	0.001352	0.294829
-6.729361	-2.116665	0.610586	0.001357	0.294631
-6.885895	-2.115438	0.615590	0.001386	0.294498
-6.845035	-2.163468	0.620595	0.001379	0.294298
-7.293448	-2.099350	0.625600	0.001462	0.294213
-7.650816	-2.089259	0.630605	0.001529	0.293943
-7.626843	-2.106711	0.635610	0.001524	0.293878
-7.647060	-2.156133	0.640614	0.001528	0.293617
-8.020813	-2.098082	0.645619	0.001598	0.293568
-7.993684	-2.158363	0.650624	0.001593	0.293295
-8.349972	-2.105085	0.655629	0.001659	0.293238
-8.471816	-2.130632	0.660634	0.001682	0.293003
-8.693698	-2.102302	0.665638	0.001723	0.292943
-8.629208	-2.166943	0.670643	0.001711	0.292682
-9.109011	-2.094234	0.675648	0.001800	0.292610
-9.120132	-2.139409	0.680653	0.001802	0.292377
-9.180735	-2.143365	0.685658	0.001814	0.292303
-9.687187	-2.097109	0.690662	0.001908	0.292076
-9.736247	-2.107367	0.695667	0.001917	0.291981
-9.735649	-2.140112	0.700672	0.001917	0.291819
-10.167901	-2.088042	0.705677	0.001997	0.291687
-10.161745	-2.114193	0.710682	0.001996	0.291563
-10.637641	-2.070430	0.715686	0.002085	0.291351
-10.229770	-2.157370	0.720691	0.002009	0.291287
-10.933495	-2.077716	0.725696	0.002140	0.291047
-11.019427	-2.062508	0.730701	0.002156	0.291045
-10.990872	-2.125925	0.735706	0.002151	0.290756
-11.304391	-2.074500	0.740710	0.002209	0.290728
-11.595423	-2.055802	0.745715	0.002263	0.290558
-11.446637	-2.098584	0.750720	0.002235	0.290479
-11.594448	-2.102623	0.755725	0.002263	0.290325
-12.105883	-2.045424	0.760730	0.002358	0.290147
-12.294846	-2.017383	0.765734	0.002393	0.290115
-12.325665	-2.069010	0.770739	0.002399	0.289830
-12.667950	-2.006233	0.775744	0.002463	0.289833
-12.654636	-2.054722	0.780749	0.002460	0.289603
-12.604835	-2.084463	0.785754	0.002451	0.289499
-12.786011	-2.071052	0.790758	0.002485	0.289401
-12.798040	-2.107602	0.795763	0.002487	0.289208
-12.804473	-2.107474	0.800768	0.002488	0.289202
-13.439284	-2.059266	0.805773	0.002606	0.288866
-13.322843	-2.078884	0.810778	0.002585	0.288874
-13.796846	-2.029492	0.815782	0.002673	0.288689
-13.735576	-2.064738	0.820787	0.002662	0.288569
-13.997115	-2.025308	0.825792	0.002710	0.288528
-14.419106	-2.006388	0.830797	0.002789	0.288238
-13.825676	-2.113077	0.835802	0.002678	0.288244
-14.239336	-2.078954	0.840806	0.002755	0.288038
-14.615581	-2.027383	0.845811	0.002825	0.287953
-14.514121	-2.059736	0.850816	0.002807	0.287883
-14.752727	-2.071492	0.855821	0.002851	0.287606
-14.885749	-2.045471	0.860826	0.002876	0.287615
-15.349011	-2.005590	0.865830	0.002962	0.287392
-15.695905	-1.958301	0.870835	0.003027	0.287312
-15.553289	-1.988334	0.875840	0.003000	0.287292
-16.202350	-1.931185	0.880845	0.003121	0.286985
-15.791086	-2.005125	0.885850	0.003044	0.286989
-16.012483	-1.987946	0.890854	0.003086	0.286873
-16.262478	-1.977749	0.895859	0.003132	0.286695
-16.061477	-2.015614	0.900864	0.003095	0.286688
-16.195606	-2.038184	0.905869	0.003120	0.286451
-16.513193	-1.997891	0.910874	0.003179	0.286363
-16.835584	-1.945499	0.915878	0.003239	0.286331
-16.780174	-2.009496	0.920883	0.003228	0.286059
-17.289900	-1.914644	0.925888	0.003323	0.286070
-17.345937	-1.926476	0.930893	0.003334	0.285958
-17.014655	-2.030821	0.935898	0.003272	0.285735
-16.996986	-2.035967	0.940902	0.003269	0.285725
-17.103221	-2.052795	0.945907	0.003289	0.285542
-17.565863	-1.980270	0.950912	0.003375	0.285483
-17.326545	-2.033685	0.955917	0.003330	0.285433
-17.627504	-2.036058	0.960922	0.003386	0.285143
-18.047439	-1.962778	0.965926	0.003464	0.285128
-17.811309	-2.037338	0.970931	0.003420	0.284967
-18.327980	-1.970019	0.975936	0.003517	0.284832
-18.452623	-1.949972	0.980941	0.003540	0.284819
-18.558476	-1.980716	0.985946	0.003560	0.284565
-18.510124	-2.004024	0.990950	0.003551	0.284491
-18.246381	-2.065336	0.995955	0.003502	0.284423
-18.829248	-2.002103	1.000960	0.003610	0.284205
-18.565694	-2.050664	1.005965	0.003561	0.284202
-18.785475	-2.053583	1.010970	0.003602	0.283983
-19.594990	-1.928518	1.015974	0.003753	0.283871
-19.015149	-2.033547	1.020979	0.003645	0.283873
-19.585452	-1.989247	1.025984	0.003751	0.283570
-20.025667	-1.909672	1.030989	0.003833	0.283567
-19.501990	-2.019722	1.035994	0.003735	0.283492
-19.973703	-1.982829	1.040998	0.003823	0.283242
-19.850312	-2.004760	1.046003	0.003800	0.283244
-19.905249	-2.027720	1.051008	0.003810	0.283076
-20.309560	-1.977745	1.056013	0.003886	0.282956
-20.029025	-2.027500	1.061018	0.003833	0.282962
-20.561846	-1.997780	1.066022	0.003933	0.282618
-20.462147	-2.017203	1.071027	0.003914	0.282612
-20.264607	-2.074762	1.076032	0.003877	0.282501
-21.172377	-1.950172	1.081037	0.004046	0.282293
-20.614216	-2.051239	1.086042	0.003942	0.282296
-20.727571	-2.077099	1.091046	0.003964	0.282057
-21.125272	-2.021994	1.096051	0.004038	0.281969
-21.130938	-2.029660	1.101056	0.004039	0.281924
-21.449203	-2.019996	1.106061	0.004098	0.281677
-21.312450	-2.042181	1.111066	0.004072	0.281690
-21.871868	-1.975463	1.116070	0.004177	0.281510
-22.320262	-1.924043	1.121075	0.004260	0.281356
-21.573033	-2.060971	1.126080	0.004121	0.281350
-22.027474	-2.028134	1.131085	0.004206	0.281094
-22.279898	-1.991784	1.136090	0.004252	0.281045
-22.016497	-2.052734	1.141094	0.004203	0.280977
-22.067581	-2.092914	1.146099	0.004213	0.280722
-22.623426	-1.991607	1.151104	0.004316	0.280724
-22.843715	-1.977024	1.156109	0.004357	0.280592
-22.602820	-2.039132	1.161114	0.004313	0.280498
-22.721872	-2.020650	1.166118	0.004335	0.280481
-22.859297	-2.057709	1.171123	0.004360	0.280161
-23.016410	-2.031336	1.176128	0.004390	0.280150
-23.352470	-1.993905	1.181133	0.004452	0.280027
-23.372227	-2.028550	1.186138	0.004456	0.279830
-23.435913	-2.018098	1.191142	0.004468	0.279824
-23.483828	-2.054556	1.196147	0.004477	0.279590
-24.141856	-1.950349	1.201152	0.004599	0.279510
-24.113483	-1.958161	1.206157	0.004594	0.279496
-23.762986	-2.075231	1.211162	0.004529	0.279220
-24.132840	-2.010071	1.216166	0.004598	0.279209
-23.977846	-2.067816	1.221171	0.004569	0.279056
-24.430887	-2.019481	1.226176	0.004653	0.278879
-24.494358	-2.008571	1.231181	0.004665	0.278876
-24.824499	-1.996808	1.236186	0.004726	0.278625
-25.118736	-1.954758	1.241190	0.004781	0.278566
-24.736828	-2.032392	1.246195	0.004710	0.278523
-25.047759	-2.029896	1.251200	0.004768	0.278242
-25.078617	-2.025605	1.256205	0.004774	0.278235
-24.857328	-2.092689	1.261210	0.004732	0.278095
-25.437041	-2.015367	1.266214	0.004840	0.277949
-25.412021	-2.019468	1.271219	0.004836	0.277952
-25.562896	-2.053665	1.276224	0.004864	0.277630
-25.738028	-2.026900	1.281229	0.004896	0.277604
-25.771743	-2.038955	1.286234	0.004903	0.277509
-25.977672	-2.043791	1.291238	0.004941	0.277288
-25.794841	-2.075621	1.296243	0.004907	0.277296
-26.132369	-2.062009	1.301248	0.004970	0.277046
-26.482058	-2.013634	1.306253	0.005035	0.276967
-26.143352	-2.085070	1.311258	0.004972	0.276915
-26.628853	-2.042372	1.316262	0.005062	0.276677
-26.695587	-2.029331	1.321267	0.005075	0.276682
-26.741825	-2.058111	1.326272	0.005083	0.276487
-27.039796	-2.030854	1.331277	0.005139	0.276346
-26.954921	-2.045853	1.336282	0.005123	0.276348
-27.475626	-2.010511	1.341286	0.005220	0.276037
-27.237277	-2.052817	1.346291	0.005176	0.276042
-27.248792	-2.073342	1.351296	0.005178	0.275924
-27.967412	-1.979906	1.356301	0.005311	0.275728
-27.685321	-2.028852	1.361306	0.005259	0.275741
-27.803869	-2.043943	1.366310	0.005281	0.275548
-27.909770	-2.036423	1.371315	0.005301	0.275487
-27.697511	-2.087285	1.376320	0.005261	0.275422
-28.120946	-2.063627	1.381325	0.005340	0.275142
-28.285400	-2.031970	1.386330	0.005371	0.275151
-28.617936	-2.009523	1.391334	0.005433	0.274951
-28.459320	-2.061460	1.396339	0.005403	0.274829
-28.453394	-2.065001	1.401344	0.005402	0.274816
-28.969672	-2.031409	1.406349	0.005498	0.274498
-28.809769	-2.058214	1.411354	0.005468	0.274510
-29.195554	-2.013156	1.416358	0.005540	0.274378
-29.462305	-1.994729	1.421363	0.005590	0.274219
-29.282309	-2.026864	1.426368	0.005556	0.274222
-29.274004	-2.081371	1.431373	0.005555	0.273942
-29.820582	-1.992838	1.436378	0.005657	0.273885
-29.987031	-1.971215	1.441382	0.005688	0.273839
-30.157270	-1.989538	1.446387	0.005719	0.273578
-30.076273	-2.004202	1.451392	0.005704	0.273579
-30.281375	-1.994454	1.456397	0.005742	0.273433
-30.142299	-2.051598	1.461402	0.005717	0.273264
-30.358461	-2.014411	1.466406	0.005757	0.273253
-30.599957	-2.014679	1.471411	0.005802	0.273019
-30.653675	-2.015516	1.476416	0.005812	0.272962
-30.689434	-2.019941	1.481421	0.005818	0.272904
-30.972737	-2.019677	1.486426	0.005871	0.272632
-31.139855	-1.992230	1.491430	0.005902	0.272617
-30.908899	-2.064873	1.496435	0.005859	0.272454
-31.399336	-2.002101	1.501440	0.005951	0.272313
-31.456896	-1.992396	1.506445	0.005961	0.272309
-31.361319	-2.063212	1.511450	0.005943	0.272025
-31.655856	-2.017930	1.516454	0.005998	0.271981
-31.694959	-2.026972	1.521459	0.006006	0.271895
-32.000193	-2.009326	1.526464	0.006062	0.271693
-31.997192	-2.011526	1.531469	0.006062	0.271684
-31.890515	-2.069065	1.536474	0.006042	0.271481
-32.464101	-1.988850	1.541478	0.006149	0.271353
-32.164122	-2.045650	1.546483	0.006093	0.271341
-32.336750	-2.068230	1.551488	0.006125	0.271052
-32.724500	-1.998662	1.556493	0.006197	0.271047
-32.302904	-2.101625	1.561498	0.006119	0.270907
-32.908052	-2.023414	1.566502	0.006231	0.270737
-32.869022	-2.029593	1.571507	0.006224	0.270741
-33.155934	-2.022009	1.576512	0.006278	0.270503
-33.079959	-2.040734	1.581517	0.006263	0.270477
-33.117988	-2.055376	1.586522	0.006271	0.270361
-33.933101	-1.949655	1.591526	0.006422	0.270133
-33.520552	-2.023739	1.596531	0.006346	0.270138
-33.561087	-2.056056	1.601536	0.006353	0.269926
-34.223865	-1.955251	1.606541	0.006476	0.269820
-33.904078	-2.016468	1.611546	0.006417	0.269803
-34.149820	-2.031081	1.616550	0.006463	0.269485
-34.366368	-1.990359	1.621555	0.006503	0.269492
-34.391924	-2.007546	1.626560	0.006508	0.269375
-34.647955	-1.992492	1.631565	0.006555	0.269205
-34.518527	-2.013816	1.636570	0.006531	0.269217
-34.922525	-1.991314	1.641574	0.006607	0.268943
-34.888942	-2.011130	1.646579	0.006600	0.268869
-34.719892	-2.052239	1.651584	0.006569	0.268813
-35.469554	-1.963636	1.656589	0.006708	0.268556
-35.205810	-2.010112	1.661594	0.006659	0.268564
-35.193141	-2.044767	1.666598	0.006657	0.268389
-35.491594	-2.018302	1.671603	0.006713	0.268239
-35.522588	-2.012549	1.676608	0.006718	0.268240
-35.958596	-1.984029	1.681613	0.006799	0.267966
-35.765356	-2.019913	1.686618	0.006763	0.267962
-35.927643	-2.012218	1.691622	0.006794	0.267844
-36.083673	-2.025904	1.696627	0.006823	0.267616
-36.210750	-2.003021	1.701632	0.006846	0.267615
-36.380381	-2.015255	1.706637	0.006878	0.267382
-36.579346	-1.992651	1.711642	0.006915	0.267308
-36.610518	-1.993867	1.716646	0.006921	0.267271
-36.770848	-2.019391	1.721651	0.006951	0.266974
-37.080200	-1.962982	1.726656	0.007008	0.266975
-37.050158	-1.991073	1.731661	0.007003	0.266852
-37.157595	-1.999289	1.736666	0.007023	0.266702
-37.400373	-1.957063	1.741670	0.007068	0.266691
-37.551472	-1.977731	1.746675	0.007096	0.266430
-37.653635	-1.971751	1.751680	0.007115	0.266361
-37.722292	-1.966886	1.756685	0.007128	0.266320
-37.992405	-1.966676	1.761690	0.007178	0.266053
-37.850256	-1.993866	1.766694	0.007152	0.266046
-37.768883	-2.035540	1.771699	0.007137	0.265900
-38.275554	-1.975305	1.776704	0.007231	0.265726
-38.113497	-2.005703	1.781709	0.007201	0.265721
-38.228755	-2.023191	1.786714	0.007222	0.265511
-38.655467	-1.954036	1.791718	0.007302	0.265465
-38.570968	-1.985136	1.796723	0.007286	0.265379
-38.621928	-2.021579	1.801728	0.007295	0.265130
-38.910182	-1.971028	1.806733	0.007349	0.265119
-39.155763	-1.960556	1.811738	0.007395	0.264933
-39.499301	-1.919940	1.816742	0.007459	0.264813
-39.217080	-1.970599	1.821747	0.007406	0.264817
-39.801609	-1.920648	1.826752	0.007515	0.264508
-39.877276	-1.911606	1.831757	0.007529	0.264482
-39.254811	-2.036824	1.836762	0.007413	0.264417
-39.800880	-1.977852	1.841766	0.007515	0.264196
-39.671779	-2.001079	1.846771	0.007491	0.264197
-39.612687	-2.054210	1.851776	0.007480	0.263965
-40.014348	-2.001831	1.856781	0.007555	0.263851
-40.251009	-1.965094	1.861786	0.007599	0.263816
-40.728873	-1.925900	1.866790	0.007688	0.263554
-40.243285	-2.014540	1.871795	0.007597	0.263553
-40.436801	-2.010595	1.876800	0.007633	0.263381
-40.917393	-1.951826	1.881805	0.007723	0.263223
-40.374517	-2.049558	1.886810	0.007622	0.263229
-40.801161	-2.025886	1.891814	0.007701	0.262932
-40.999912	-1.989480	1.896819	0.007738	0.262933
-40.932570	-2.028789	1.901824	0.007726	0.262784
-41.076480	-2.037755	1.906829	0.007752	0.262590
-41.197972	-2.014218	1.911834	0.007775	0.262598
-41.481270	-2.019386	1.916838	0.007828	0.262285
-41.365773	-2.040622	1.921843	0.007806	0.262284
-41.575364	-2.030426	1.926848	0.007845	0.262130
-42.312588	-1.928637	1.931853	0.007983	0.261951
-41.743186	-2.030140	1.936858	0.007877	0.261963
-41.951162	-2.041510	1.941862	0.007915	0.261691
-42.406674	-1.962411	1.946867	0.008000	0.261670
-42.184991	-2.024398	1.951872	0.007959	0.261550
-42.492768	-2.007880	1.956877	0.008016	0.261331
-42.760651	-1.956169	1.961882	0.008066	0.261348
-42.977213	-1.963865	1.966886	0.008106	0.261087
-43.110992	-1.948054	1.971891	0.008131	0.261039
-42.984547	-1.981508	1.976896	0.008108	0.260981
-43.260341	-1.980410	1.981901	0.008159	0.260709
-42.895120	-2.045333	1.986906	0.008091	0.260717
-43.083420	-2.041705	1.991910	0.008126	0.260547
-43.418934	-1.993665	1.996915	0.008189	0.260475
-43.295469	-2.053714	2.001920	0.008166	0.260266

-43.540802	-2.048831	2.011917	0.008211	0.260044
-43.779157	-2.047430	2.021914	0.008256	0.259811
-44.351096	-1.985605	2.031910	0.008362	0.259575
-44.230712	-2.023302	2.041907	0.008340	0.259487
-44.442082	-2.029094	2.051904	0.008379	0.259240
-44.730545	-1.983367	2.061901	0.008433	0.259202
-44.684814	-2.020067	2.071898	0.008424	0.259044
-45.118254	-1.972386	2.081894	0.008505	0.258869
-45.068064	-1.980937	2.091891	0.008496	0.258872
-44.909996	-2.011542	2.101888	0.008466	0.258862
-45.639198	-1.925204	2.111885	0.008602	0.258603
-45.317187	-1.991747	2.121882	0.008542	0.258558
-45.487956	-1.962364	2.131878	0.008574	0.258549
-45.414068	-1.975688	2.141875	0.008560	0.258549
-45.388676	-1.979523	2.151872	0.008555	0.258554
-45.371667	-1.982998	2.161869	0.008552	0.258552
-45.039766	-2.044082	2.171866	0.008490	0.258548
-45.387483	-1.980620	2.181862	0.008555	0.258549
-45.169779	-2.020139	2.191859	0.008515	0.258549
-45.385023	-1.981717	2.201856	0.008555	0.258545
-45.167569	-2.000459	2.211853	0.008514	0.258662
-44.983155	-1.998246	2.221850	0.008480	0.258862
-45.257118	-1.948701	2.231846	0.008531	0.258860
-45.076102	-1.981713	2.241843	0.008497	0.258860
-45.077529	-1.981143	2.251840	0.008497	0.258862
-44.862524	-1.978131	2.261837	0.008457	0.259097
-44.629645	-2.002726	2.271834	0.008414	0.259197
-44.715651	-1.986827	2.281830	0.008430	0.259198
-44.547519	-2.001699	2.291827	0.008399	0.259286
-44.237592	-2.023972	2.301824	0.008341	0.259476
-44.328088	-2.006791	2.311821	0.008358	0.259480
-44.264730	-1.990748	2.321818	0.008346	0.259634
-44.004849	-2.006691	2.331814	0.008298	0.259809
-43.952823	-2.016917	2.341811	0.008288	0.259805
-43.781574	-1.995744	2.351808	0.008256	0.260096
-43.525834	-2.037175	2.361805	0.008208	0.260125
-43.404035	-2.023888	2.371802	0.008186	0.260322
-43.201168	-2.034463	2.381798	0.008148	0.260468
-43.268539	-2.007380	2.391795	0.008161	0.260551
-43.001956	-2.027750	2.401792	0.008111	0.260707
-42.927117	-2.024358	2.411789	0.008097	0.260801
-42.665941	-2.030823	2.421786	0.008048	0.261029
-42.630927	-2.017505	2.431782	0.008042	0.261139
-42.300439	-2.042787	2.441779	0.007980	0.261332
-42.534135	-1.968580	2.451776	0.008024	0.261507
-41.924835	-2.050079	2.461773	0.007910	0.261670
-41.925422	-2.013122	2.471770	0.007910	0.261874
-41.773201	-2.026716	2.481766	0.007882	0.261952
-41.504911	-2.016926	2.491763	0.007832	0.262275
-41.495145	-2.002565	2.501760	0.007830	0.262364
-41.100050	-2.033083	2.511757	0.007757	0.262593
-41.033375	-2.004349	2.521754	0.007744	0.262818
-40.774959	-2.028944	2.531750	0.007696	0.262941
-40.889941	-1.956007	2.541747	0.007718	0.263228
-40.495902	-1.999439	2.551744	0.007644	0.263383
-40.246190	-2.015075	2.561741	0.007598	0.263547
-40.109708	-1.985749	2.571738	0.007572	0.263844
-39.658778	-2.037988	2.581734	0.007488	0.264008
-39.588054	-2.017564	2.591731	0.007475	0.264190
-39.461822	-1.994037	2.601728	0.007452	0.264445
-39.220928	-2.007343	2.611725	0.007407	0.264612
-39.195496	-1.975207	2.621722	0.007402	0.264813
-38.958670	-1.960799	2.631718	0.007358	0.265127
-38.885940	-1.935616	2.641715	0.007344	0.265337
-38.372151	-1.997464	2.651712	0.007249	0.265509
-38.373449	-1.955705	2.661709	0.007249	0.265736
-38.107481	-1.957945	2.671706	0.007200	0.265987
-37.921410	-1.955163	2.681702	0.007165	0.266186
-37.739253	-1.950645	2.691699	0.007131	0.266391
-37.343281	-1.966527	2.701696	0.007057	0.266696
-36.820233	-2.027233	2.711693	0.006960	0.266883
-36.815264	-1.995258	2.721690	0.006959	0.267061
-36.637936	-1.982592	2.731686	0.006926	0.267305
-36.334411	-1.987428	2.741683	0.006869	0.267578
-36.248383	-1.961866	2.751680	0.006853	0.267801
-36.016503	-1.965098	2.761677	0.006810	0.268011
-35.563804	-2.004409	2.771674	0.006726	0.268243
-35.160424	-2.031086	2.781670	0.006651	0.268495
-35.406687	-1.948481	2.791667	0.006697	0.268699
-34.881522	-2.005857	2.801664	0.006599	0.268905
-34.577715	-2.004187	2.811661	0.006542	0.269211
-34.289497	-2.018374	2.821658	0.006489	0.269417
-34.315866	-1.973968	2.831654	0.006494	0.269629
-34.128045	-1.967854	2.841651	0.006459	0.269846
-33.772267	-1.976332	2.851648	0.006392	0.270147
-33.479058	-1.983911	2.861645	0.006338	0.270392
-33.298000	-1.981038	2.871642	0.006304	0.270584
-33.003484	-2.002442	2.881638	0.006249	0.270756
-32.707739	-2.000087	2.891635	0.006194	0.271056
-32.484064	-2.000212	2.901632	0.006152	0.271273
-32.477480	-1.960220	2.911629	0.006151	0.271492
-31.939536	-2.017832	2.921626	0.006051	0.271707
-31.839201	-1.983070	2.931622	0.006032	0.271989
-31.644834	-1.974565	2.941619	0.005996	0.272223
-31.470147	-1.964387	2.951616	0.005964	0.272446
-31.527832	-1.906538	2.961613	0.005974	0.272697
-30.827486	-1.982903	2.971610	0.005844	0.272968
-30.832892	-1.932240	2.981606	0.005845	0.273231
-30.560257	-1.938441	2.991603	0.005794	0.273461
-30.110821	-1.979525	3.001600	0.005711	0.273676
-30.032439	-1.950183	3.011597	0.005696	0.273907
-29.500439	-1.987483	3.021594	0.005597	0.274221
-29.394685	-1.965531	3.031590	0.005577	0.274438
-29.429287	-1.916540	3.041587	0.005584	0.274663
-28.880513	-1.972179	3.051584	0.005481	0.274896
-28.675654	-1.960819	3.061581	0.005443	0.275152
-28.031250	-2.022440	3.071578	0.005323	0.275444
-28.050785	-1.985870	3.081574	0.005327	0.275618
-28.216744	-1.918803	3.091571	0.005358	0.275811
-27.918192	-1.924094	3.101568	0.005302	0.276068
-27.441964	-1.954888	3.111565	0.005214	0.276361
-27.233397	-1.945963	3.121562	0.005175	0.276606
-27.009952	-1.945146	3.131558	0.005133	0.276823
-26.817614	-1.938522	3.141555	0.005097	0.277041
-26.457011	-1.952218	3.151552	0.005030	0.277312
-26.380771	-1.913295	3.161549	0.005016	0.277587
-25.791215	-1.974119	3.171546	0.004906	0.277829
-25.496970	-1.989037	3.181542	0.004851	0.278030
-25.040549	-2.031298	3.191539	0.004767	0.278242
-25.099751	-1.964274	3.201536	0.004777	0.278534
-24.648343	-2.007024	3.211533	0.004693	0.278739
-24.301480	-2.031392	3.221530	0.004629	0.278940
-24.184187	-2.000031	3.231526	0.004607	0.279213
-23.624892	-2.056315	3.241523	0.004503	0.279448
-23.837528	-1.979821	3.251520	0.004542	0.279644
-23.395083	-2.018906	3.261517	0.004460	0.279858
-23.355722	-1.969677	3.271514	0.004453	0.280150
-23.267156	-1.932783	3.281510	0.004436	0.280424
-23.133134	-1.917391	3.291507	0.004411	0.280629
-23.141296	-1.876393	3.301504	0.004413	0.280832
-22.449806	-1.956808	3.311501	0.004284	0.281066
-21.701308	-2.037990	3.321498	0.004145	0.281349
-22.028155	-1.933240	3.331494	0.004206	0.281582
-21.695051	-1.949186	3.341491	0.004144	0.281811
-21.536538	-1.937473	3.351488	0.004114	0.282019
-21.160770	-1.950621	3.361485	0.004044	0.282302
-20.850778	-1.955902	3.371482	0.003986	0.282564
-20.558076	-1.965573	3.381478	0.003932	0.282787
-20.244311	-1.978932	3.391475	0.003873	0.283011
-20.050544	-1.970567	3.401472	0.003837	0.283233
-19.619428	-1.993778	3.411469	0.003757	0.283515
-19.690470	-1.939942	3.421466	0.003770	0.283724
-19.457995	-1.936055	3.431462	0.003727	0.283959
-18.837520	-2.001088	3.441459	0.003611	0.284203
-18.646244	-1.985266	3.451456	0.003576	0.284461
-18.382669	-1.992587	3.461453	0.003527	0.284667
-18.180869	-1.986756	3.471450	0.003489	0.284883
-17.991722	-1.970863	3.481446	0.003454	0.285139
-17.538039	-1.997375	3.491443	0.003370	0.285422
-17.444737	-1.980281	3.501440	0.003352	0.285595
-16.856162	-2.056002	3.511437	0.003243	0.285754
-17.067902	-1.959017	3.521434	0.003282	0.286050
-16.736880	-1.972179	3.531430	0.003220	0.286288
-16.554389	-1.959965	3.541427	0.003186	0.286517
-16.193445	-1.985801	3.551424	0.003119	0.286718
-15.807001	-2.004620	3.561421	0.003047	0.286977
-15.551086	-2.004058	3.571418	0.003000	0.287215
-15.194103	-2.030797	3.581414	0.002933	0.287407
-15.135158	-1.999876	3.591411	0.002922	0.287617
-14.949830	-1.966590	3.601408	0.002888	0.287953
-14.628768	-1.986617	3.611405	0.002828	0.288146
-14.563369	-1.959868	3.621402	0.002816	0.288340
-14.133597	-1.992692	3.631398	0.002736	0.288567
-13.673156	-2.018916	3.641395	0.002650	0.288856
-13.522373	-2.006051	3.651392	0.002622	0.289057
-13.061000	-2.051361	3.661389	0.002536	0.289250
-13.183694	-1.978554	3.671386	0.002559	0.289503
-12.880187	-1.979202	3.681382	0.002502	0.289775
-12.870771	-1.938004	3.691379	0.002500	0.289990
-12.270386	-2.009397	3.701376	0.002389	0.290178
-11.957190	-2.004219	3.711373	0.002330	0.290487
-11.641921	-2.026510	3.721370	0.002272	0.290662
-11.381414	-2.039619	3.731366	0.002223	0.290832
-11.124972	-2.040841	3.741363	0.002175	0.291058
-10.856604	-2.034485	3.751360	0.002125	0.291332
-10.642027	-2.035810	3.761357	0.002085	0.291519
-10.168871	-2.085375	3.771354	0.001997	0.291700
-9.975577	-2.063597	3.781350	0.001961	0.291982
-9.897374	-2.040321	3.791347	0.001947	0.292168
-9.419225	-2.092620	3.801344	0.001858	0.292340
-9.413637	-2.037932	3.811341	0.001857	0.292615
-9.102284	-2.044136	3.821338	0.001799	0.292864
-9.005325	-2.023509	3.831334	0.001781	0.293053
-8.844753	-2.011779	3.841331	0.001751	0.293255
-8.374865	-2.037577	3.851328	0.001663	0.293549
-8.690659	-1.938944	3.861325	0.001722	0.293752
-8.289104	-1.964167	3.871322	0.001647	0.293988
-7.750483	-2.014495	3.881318	0.001547	0.294222
-7.752476	-1.959789	3.891315	0.001547	0.294489
-7.236974	-2.011701	3.901312	0.001451	0.294694
-7.230099	-1.970561	3.911309	0.001450	0.294902
-6.805066	-1.996681	3.921306	0.001371	0.295153
-6.283053	-2.033083	3.931302	0.001274	0.295440
-6.210741	-2.014949	3.941299	0.001260	0.295593
-6.101356	-2.000781	3.951296	0.001240	0.295759
-5.771650	-2.001436	3.961293	0.001179	0.296049
-5.324575	-2.039856	3.971290	0.001095	0.296258
-5.210316	-2.022242	3.981286	0.001074	0.296446
-5.009740	-2.006788	3.991283	0.001037	0.296699
-4.613165	-2.028319	4.001280	0.000963	0.296946
-4.656121	-1.980600	4.011277	0.000971	0.297140
-4.205491	-2.020922	4.021274	0.000887	0.297342
-4.141875	-1.974683	4.031270	0.000875	0.297624
-4.028481	-1.942246	4.041267	0.000854	0.297881
-3.853000	-1.929521	4.051264	0.000821	0.298098
-3.670513	-1.919212	4.061261	0.000787	0.298309
-3.724451	-1.852504	4.071258	0.000797	0.298585
-3.636792	-1.807405	4.081254	0.000781	0.298880
-3.507861	-1.775575	4.091251	0.000757	0.299148
-3.207078	-1.779969	4.101248	0.000701	0.299391
-2.897807	-1.784307	4.111245	0.000643	0.299641
-2.644024	-1.778042	4.121242	0.000596	0.299894
-2.555910	-1.738593	4.131238	0.000580	0.300162
-2.656499	-1.650929	4.141235	0.000598	0.300496
-2.544677	-1.624798	4.151232	0.000577	0.300720
-2.522589	-1.569173	4.161229	0.000573	0.301006
-2.414784	-1.528048	4.171226	0.000553	0.301298
-2.050871	-1.528835	4.181222	0.000485	0.301612
-1.993798	-1.479317	4.191219	0.000475	0.301899
-1.924465	-1.425869	4.201216	0.000462	0.302215
-2.003783	-1.344088	4.211213	0.000477	0.302538
-1.829825	-1.301644	4.221210	0.000444	0.302892
-1.975017	-1.206960	4.231206	0.000471	0.303218
-2.014482	-1.118651	4.241203	0.000478	0.303605
-1.611368	-1.117828	4.251200	0.000403	0.303957
-1.839121	-0.997925	4.261197	0.000446	0.304331
-1.505286	-0.986354	4.271194	0.000384	0.304674
-1.118517	-0.979315	4.281190	0.000312	0.305041
-1.103261	-0.901549	4.291187	0.000309	0.305423
-1.169586	-0.810914	4.301184	0.000321	0.305795
-0.886667	-0.782651	4.311181	0.000268	0.306172
-0.883793	-0.700958	4.321178	0.000268	0.306560
-0.709740	-0.654859	4.331174	0.000235	0.306926
-0.718822	-0.556318	4.341171	0.000237	0.307383
-0.630079	-0.486647	4.351168	0.000220	0.307786
-0.639784	-0.401963	4.361165	0.000222	0.308176
-0.603000	-0.304872	4.371162	0.000215	0.308663
-0.499979	-0.233923	4.381158	0.000196	0.309083
-0.356366	-0.166820	4.391155	0.000169	0.309519
-0.218747	-0.093247	4.401152	0.000143	0.309979
-0.274793	0.015638	4.411149	0.000154	0.310440
0.000000	0.055057	4.421146	0.000103	0.310856

-0.196682	0.359256	4.426150	0.000139	0.312103
-0.139203	0.913180	4.431155	0.000128	0.314708
0.510901	1.644953	4.436160	0.000006	0.318591
1.021456	2.692165	4.441165	-0.000089	0.323726
1.737050	4.001782	4.446170	-0.000223	0.330097
2.679543	5.563875	4.451174	-0.000400	0.337608
3.769102	7.407722	4.456179	-0.000604	0.346246
4.935155	9.556426	4.461184	-0.000823	0.355971
6.646973	11.914332	4.466189	-0.001143	0.366654
8.554069	14.578386	4.471194	-0.001500	0.378342
10.703244	17.534452	4.476198	-0.001902	0.390924
12.700717	20.868709	4.481203	-0.002276	0.404368
15.374887	24.442421	4.486208	-0.002776	0.418631
17.940782	28.402666	4.491213	-0.003256	0.433647
20.407647	32.746530	4.496218	-0.003719	0.449336
23.813557	37.292726	4.501222	-0.004356	0.465651
28.502233	41.991670	4.506227	-0.005232	0.482564
34.335587	46.888321	4.511232	-0.006321	0.500070
42.434034	51.782074	4.516237	-0.007832	0.518111
49.023046	57.367505	4.521242	-0.009063	0.536670
53.226999	63.750823	4.526246	-0.009850	0.555562
58.644656	70.276301	4.531251	-0.010863	0.574735
62.968072	77.356120	4.536256	-0.011672	0.594155
67.117469	84.767956	4.541261	-0.012450	0.613665
70.413500	92.655660	4.546266	-0.013069	0.633306
75.694920	100.441924	4.551270	-0.014057	0.652915
81.595721	108.415382	4.556275	-0.015161	0.672587
87.531318	116.628955	4.561280	-0.016272	0.692208
90.104181	125.670028	4.566285	-0.016757	0.711746
91.831289	135.027624	4.571290	-0.017084	0.731087
92.945489	144.623879	4.576294	-0.017298	0.750177
93.684924	154.380697	4.581299	-0.017442	0.768968
94.787764	164.155874	4.586304	-0.017654	0.787463
95.622549	174.026538	4.591309	-0.017816	0.805618
96.169922	184.010096	4.596314	-0.017924	0.823481
96.969050	193.957903	4.601318	-0.018079	0.840979
97.599643	203.933677	4.606323	-0.018203	0.858116
98.382235	213.880977	4.611328	-0.018356	0.874915
98.958811	223.846313	4.616333	-0.018469	0.891367
101.386269	233.487381	4.621338	-0.018928	0.907522
102.394837	243.349834	4.626342	-0.019122	0.923349
103.139689	253.222356	4.631347	-0.019267	0.938853
103.962812	263.045317	4.636352	-0.019427	0.954050
104.299871	272.888828	4.641357	-0.019496	0.968913
104.796420	282.662955	4.646362	-0.019595	0.983490
105.592300	292.320326	4.651366	-0.019749	0.997760
106.624241	301.846366	4.656371	-0.019948	1.011700
107.319178	311.397256	4.661376	-0.020083	1.025402
108.234953	320.832522	4.666381	-0.020260	1.038815
109.406073	330.182502	4.671386	-0.020484	1.052001
110.116016	339.557488	4.676390	-0.020622	1.064948
110.909762	348.858852	4.681395	-0.020776	1.077660
111.411327	358.155871	4.686400	-0.020876	1.090151
111.992198	367.375296	4.691405	-0.020990	1.102417
112.818446	376.511301	4.696410	-0.021150	1.114493
113.615808	385.575013	4.701414	-0.021304	1.126341
114.467285	394.598724	4.706419	-0.021468	1.138027
115.004967	403.651670	4.711424	-0.021574	1.149562
115.477377	412.638999	4.716429	-0.021668	1.160886
116.602376	421.462874	4.721434	-0.021883	1.172038
116.831206	430.418400	4.726438	-0.021932	1.183057
117.445447	439.256227	4.731443	-0.022052	1.193912
117.726872	448.102744	4.736448	-0.022110	1.204611
118.541297	456.825491	4.741453	-0.022268	1.215177
119.486073	465.514237	4.746458	-0.022449	1.225637
120.165278	474.200466	4.751462	-0.022581	1.235952
120.951962	482.834254	4.756467	-0.022733	1.246143
121.343246	491.532273	4.761472	-0.022812	1.256247
121.704311	500.196591	4.766477	-0.022885	1.266226
122.688532	508.732474	4.771482	-0.023074	1.276100
123.283937	517.304205	4.776486	-0.023190	1.285865
123.491216	525.939057	4.781491	-0.023234	1.295554
123.869349	534.509413	4.786496	-0.023310	1.305131
124.655326	543.049665	4.791501	-0.023462	1.314680
125.092256	551.554350	4.796506	-0.023549	1.324057
125.746498	560.000212	4.801510	-0.023676	1.333344
126.241349	568.468397	4.806515	-0.023774	1.342562
126.869543	576.901212	4.811520	-0.023896	1.351703
127.215439	585.337017	4.816525	-0.023966	1.360735
128.007307	593.724756	4.821530	-0.024119	1.369735
128.507713	602.143992	4.826534	-0.024218	1.378659
128.937130	610.564837	4.831539	-0.024303	1.387514
129.155293	619.012781	4.836544	-0.024350	1.396304
129.720042	627.346005	4.841549	-0.024460	1.404981
130.282568	635.715519	4.846554	-0.024570	1.413641
130.574389	644.099429	4.851558	-0.024630	1.422217
131.239239	652.414854	4.856563	-0.024759	1.430734
131.853501	660.733609	4.861568	-0.024879	1.439196
132.115338	669.095233	4.866573	-0.024933	1.447593
132.577563	677.438807	4.871578	-0.025025	1.455956
132.755054	685.796629	4.876582	-0.025063	1.464239
133.122235	694.150372	4.881587	-0.025137	1.472502
133.677405	702.428594	4.886592	-0.025246	1.480676
133.983718	710.728909	4.891597	-0.025308	1.488786
134.668119	718.986155	4.896602	-0.025441	1.496870
134.927355	727.286054	4.901606	-0.025495	1.504884
135.357283	735.568175	4.906611	-0.025580	1.512866
136.031893	743.793493	4.911616	-0.025711	1.520790
136.393228	752.065860	4.916621	-0.025784	1.528668
137.151537	760.296362	4.921626	-0.025931	1.536528
137.279510	768.613967	4.926630	-0.025960	1.544332
137.986516	776.838702	4.931635	-0.026097	1.552099
138.432117	785.077703	4.936640	-0.026185	1.559800
138.881924	793.320355	4.941645	-0.026274	1.567468
139.570796	801.531369	4.946650	-0.026408	1.575104
139.914007	809.791323	4.951654	-0.026477	1.582697
140.020500	818.093107	4.956659	-0.026502	1.590257
140.575989	826.302546	4.961664	-0.026611	1.597763
141.187191	834.470202	4.966669	-0.026730	1.605205
141.210628	842.804008	4.971674	-0.026740	1.612675
141.837308	850.973218	4.976678	-0.026862	1.620051
142.554509	859.155693	4.981683	-0.027001	1.627418
143.154240	867.382005	4.986688	-0.027118	1.634774
143.333060	875.622208	4.991693	-0.027157	1.642050
143.832450	883.807818	4.996698	-0.027255	1.649290
144.384905	891.993555	5.001702	-0.027363	1.656506
145.119377	900.132954	5.006707	-0.027505	1.663675
145.447102	908.378660	5.011712	-0.027572	1.670850
145.555580	916.614749	5.016717	-0.027597	1.677955
146.104386	924.772585	5.021722	-0.027705	1.685023
146.474464	932.994929	5.026726	-0.027779	1.692093
146.981097	941.169573	5.031731	-0.027879	1.699110
147.543779	949.330008	5.036736	-0.027989	1.706094
147.739481	957.559480	5.041741	-0.028031	1.713059
148.432861	965.680291	5.046746	-0.028165	1.719970
148.867399	973.854176	5.051750	-0.028251	1.726864
149.302779	982.045686	5.056755	-0.028338	1.733745
149.812966	990.204370	5.061760	-0.028438	1.740581
149.820290	998.448692	5.066765	-0.028445	1.747395
150.612492	1006.565161	5.071770	-0.028597	1.754179
150.877735	1014.742990	5.076774	-0.028652	1.760920
151.071757	1022.947513	5.081779	-0.028694	1.767647
151.517763	1031.112080	5.086784	-0.028782	1.774348
151.757581	1039.278810	5.091789	-0.028832	1.781000
152.247735	1047.446062	5.096794	-0.028929	1.787658
152.741566	1055.603095	5.101798	-0.029026	1.794284
152.854566	1063.789892	5.106803	-0.029052	1.800862
153.393019	1071.900420	5.111808	-0.029158	1.807408
153.910084	1080.024766	5.116813	-0.029259	1.813938
154.477177	1088.148894	5.121818	-0.029370	1.820451
154.857377	1096.304666	5.126822	-0.029446	1.826942
155.169196	1104.483913	5.131827	-0.029510	1.833421
155.623190	1112.596960	5.136832	-0.029600	1.839842
155.897083	1120.758538	5.141837	-0.029656	1.846256
156.260151	1128.932869	5.146842	-0.029729	1.852669
156.645037	1137.056018	5.151846	-0.029806	1.859023
156.863401	1145.214499	5.156851	-0.029852	1.865362
157.124535	1153.406375	5.161856	-0.029906	1.871711
156.953692	1161.607186	5.166861	-0.029879	1.877994
157.436741	1169.686028	5.171866	-0.029974	1.884239
157.807365	1177.800900	5.176870	-0.030049	1.890478
158.590175	1185.853823	5.181875	-0.030200	1.896697
158.823918	1194.015829	5.186880	-0.030249	1.902915
159.234831	1202.128202	5.191885	-0.030330	1.909095
159.749963	1210.243757	5.196890	-0.030432	1.915270
159.719338	1218.428347	5.201894	-0.030431	1.921414
159.712318	1226.613010	5.206899	-0.030435	1.927542
160.305407	1234.686068	5.211904	-0.030551	1.933634
160.908986	1242.745091	5.216909	-0.030669	1.939698
161.343797	1250.870935	5.221914	-0.030755	1.945773
161.868495	1258.977745	5.226918	-0.030858	1.951826
162.401199	1267.057873	5.231923	-0.030962	1.957840
162.859479	1275.166213	5.236928	-0.031053	1.963849
163.298872	1283.266569	5.241933	-0.031140	1.969831
163.986305	1291.361205	5.246938	-0.031273	1.975818
164.449194	1299.470156	5.251942	-0.031365	1.981773
164.491317	1307.659898	5.256947	-0.031378	1.987722
164.687548	1315.835686	5.261952	-0.031420	1.993661
165.366319	1323.856445	5.266957	-0.031551	1.999521
165.660871	1331.991541	5.271962	-0.031612	2.005406
166.109007	1340.093973	5.276966	-0.031700	2.011266
166.477508	1348.216517	5.281971	-0.031774	2.017115
166.777060	1356.360252	5.286976	-0.031835	2.022955
167.014488	1364.476314	5.291981	-0.031885	2.028751
167.632001	1372.569967	5.296986	-0.032005	2.034555
168.117343	1380.637355	5.301990	-0.032101	2.040310
168.548805	1388.724572	5.306995	-0.032186	2.046057
169.154243	1396.824841	5.312000	-0.032304	2.051815
169.493207	1404.920899	5.317005	-0.032373	2.057526
169.804558	1413.054309	5.322010	-0.032436	2.063245
169.975866	1421.206209	5.327014	-0.032473	2.068946
170.357841	1429.296614	5.332019	-0.032550	2.074611
170.961593	1437.354693	5.337024	-0.032667	2.080259
171.005454	1445.478311	5.342029	-0.032681	2.085881
171.807663	1453.546358	5.347034	-0.032835	2.091526
171.943304	1461.683058	5.352038	-0.032866	2.097136
172.070169	1469.811729	5.357043	-0.032895	2.102725
172.597151	1477.895099	5.362048	-0.032998	2.108307
173.099348	1486.004835	5.367053	-0.033097	2.113890
173.287498	1494.116694	5.372058	-0.033137	2.119429
173.592205	1502.175958	5.377062	-0.033199	2.124929
174.046700	1510.250409	5.382067	-0.033289	2.130440
174.321689	1518.364862	5.387072	-0.033346	2.135946
174.358277	1526.489350	5.392077	-0.033358	2.141421
174.596663	1534.586089	5.397082	-0.033407	2.146883
175.406129	1542.597777	5.402086	-0.033563	2.152329
175.578972	1550.715444	5.407091	-0.033601	2.157771
175.987068	1558.782991	5.412096	-0.033682	2.163188
176.165201	1566.890133	5.417101	-0.033721	2.168596
176.472228	1575.001360	5.422106	-0.033783	2.174006
176.815991	1583.081260	5.427110	-0.033852	2.179385
176.797250	1591.201335	5.432115	-0.033854	2.184742
177.437188	1599.265151	5.437120	-0.033978	2.190112
177.651023	1607.347949	5.442125	-0.034024	2.195441
178.166978	1615.385488	5.447130	-0.034125	2.200755
178.394755	1623.477962	5.452134	-0.034173	2.206065
178.672146	1631.572309	5.457139	-0.034229	2.211369
178.924325	1639.680260	5.462144	-0.034282	2.216666
179.073322	1647.762163	5.467149	-0.034315	2.221924
179.700186	1655.833869	5.472154	-0.034437	2.227207
179.753794	1663.953159	5.477158	-0.034452	2.232456
180.057791	1672.017118	5.482163	-0.034514	2.237679
180.342303	1680.093892	5.487168	-0.034572	2.242897
180.303174	1688.219468	5.492173	-0.034570	2.248105
180.824790	1696.271451	5.497178	-0.034672	2.253303
181.417033	1704.301697	5.502182	-0.034788	2.258482
181.887810	1712.354029	5.507187	-0.034881	2.263653
182.187740	1720.468365	5.512192	-0.034942	2.268835
182.395230	1728.597343	5.517197	-0.034986	2.274007
182.487956	1736.696951	5.522202	-0.035008	2.279139
182.609117	1744.745080	5.527206	-0.035036	2.284229
182.560876	1752.869236	5.532211	-0.035033	2.289340
183.250322	1760.879074	5.537216	-0.035166	2.294433
183.647864	1768.907917	5.542221	-0.035245	2.299501
184.308934	1776.922384	5.547226	-0.035374	2.304571
184.481022	1785.068694	5.552230	-0.035411	2.309670
184.942085	1793.108049	5.557235	-0.035502	2.314716
185.264630	1801.175766	5.562240	-0.035568	2.319757
185.393529	1809.247266	5.567245	-0.035597	2.324773
185.945897	1817.322971	5.572250	-0.035705	2.329816
186.144071	1825.411631	5.577254	-0.035747	2.334826
186.387048	1833.476685	5.582259	-0.035798	2.339815
186.591718	1841.587999	5.587264	-0.035841	2.344819
186.873146	1849.658948	5.592269	-0.035899	2.349793
186.885890	1857.788101	5.597274	-0.035906	2.354770
187.052686	1865.837050	5.602278	-0.035943	2.359700
187.451989	1873.842186	5.607283	-0.036022	2.364613
187.705038	1881.944949	5.612288	-0.036075	2.369562
188.009144	1889.996145	5.617293	-0.036136	2.374474
188.518136	1898.047129	5.622298	-0.036236	2.379392
188.726088	1906.119024	5.627302	-0.036280	2.384289
188.958788	1914.200962	5.632307	-0.036329	2.389183
189.631477	1922.222811	5.637312	-0.036460	2.394066
189.609979	1930.337303	5.642317	-0.036461	2.398940
190.033689	1938.360111	5.647322	-0.036545	2.403784
190.117001	1946.477098	5.652326	-0.036566	2.408647
190.132971	1954.575338	5.657331	-0.036574	2.413484
190.459221	1962.636094	5.662336	-0.036640	2.418314
190.483444	1970.715623	5.667341	-0.036650	2.423121
190.794349	1978.774111	5.672346	-0.036713	2.427928
191.384025	1986.823337	5.677350	-0.036828	2.432743
191.847949	1994.857232	5.682355	-0.036920	2.437529
192.318662	2002.883025	5.687360	-0.037012	2.442301
192.520561	2010.936529	5.692365	-0.037055	2.447060
193.068919	2018.982665	5.697370	-0.037163	2.451831
193.368889	2027.051778	5.702374	-0.037224	2.456587
193.680236	2035.118955	5.707379	-0.037287	2.461334
193.901871	2043.211045	5.712384	-0.037334	2.466080
194.110901	2051.289453	5.717389	-0.037378	2.470807
194.535988	2059.337957	5.722394	-0.037462	2.475524
194.811236	2067.396977	5.727398	-0.037519	2.480227
195.127204	2075.427351	5.732403	-0.037583	2.484907
195.607711	2083.484260	5.737408	-0.037677	2.489606
195.741991	2091.564252	5.742413	-0.037708	2.494284
196.097448	2099.626107	5.747418	-0.037779	2.498959
196.204986	2107.711629	5.752422	-0.037804	2.503620
196.244989	2115.818616	5.757427	-0.037817	2.508280
196.705505	2123.879403	5.762432	-0.037908	2.512935
196.771575	2131.922666	5.767437	-0.037926	2.517543
197.163711	2139.947066	5.772442	-0.038004	2.522156
197.287894	2148.022625	5.777446	-0.038032	2.526770
197.688050	2156.034382	5.782451	-0.038112	2.531359
197.786060	2164.144079	5.787456	-0.038136	2.535973
198.022353	2172.176192	5.792461	-0.038185	2.540545
198.074765	2180.270800	5.797466	-0.038200	2.545131
198.530445	2188.294958	5.802470	-0.038290	2.549698
198.769787	2196.335412	5.807475	-0.038340	2.554250
198.887295	2204.435613	5.812480	-0.038367	2.558819
198.997760	2212.470928	5.817485	-0.038393	2.563343
199.642251	2220.476510	5.822490	-0.038518	2.567880
199.436823	2228.637287	5.827494	-0.038485	2.572436
199.312851	2236.706497	5.832499	-0.038467	2.576938
199.673690	2244.742620	5.837504	-0.038540	2.581448
200.300835	2252.715315	5.842509	-0.038662	2.585933
200.506479	2260.836666	5.847514	-0.038705	2.590464
200.802588	2268.946049	5.852518	-0.038766	2.594986
201.241225	2276.910577	5.857523	-0.038852	2.599430
201.786446	2284.902443	5.862528	-0.038959	2.603889
201.938657	2292.971812	5.867533	-0.038993	2.608356
202.292111	2301.037269	5.872538	-0.039064	2.612827
202.902726	2309.035766	5.877542	-0.039183	2.617271
203.167032	2317.069594	5.882547	-0.039237	2.621703
203.514695	2325.157778	5.887552	-0.039307	2.626163
203.773261	2333.215099	5.892557	-0.039361	2.630592
203.930694	2341.326747	5.897562	-0.039395	2.635037
203.694080	2349.411779	5.902566	-0.039356	2.639433
203.672809	2357.476302	5.907571	-0.039358	2.643825
204.006209	2365.518965	5.912576	-0.039425	2.648222
204.026972	2373.565198	5.917581	-0.039434	2.652592
204.692621	2381.543739	5.922586	-0.039563	2.656962
205.124919	2389.560514	5.927590	-0.039649	2.661329
205.432313	2397.611863	5.932595	-0.039711	2.665699
205.736647	2405.699004	5.937600	-0.039773	2.670082
205.867213	2413.762316	5.942605	-0.039803	2.674433
206.618191	2421.718179	5.947610	-0.039948	2.678759
206.689426	2429.797757	5.952614	-0.039967	2.683101
206.665058	2437.878811	5.957619	-0.039967	2.687430
207.195020	2445.907721	5.962624	-0.040071	2.691760
207.331119	2453.973198	5.967629	-0.040102	2.696077
207.918918	2462.000964	5.972634	-0.040216	2.700396
208.109419	2470.051353	5.977638	-0.040257	2.704695
208.198951	2478.131588	5.982643	-0.040279	2.708996
208.289136	2486.249961	5.987648	-0.040301	2.713311
208.577709	2494.240645	5.992653	-0.040360	2.717564
208.972731	2502.256008	5.997658	-0.040439	2.721830
209.052093	2510.341648	6.002662	-0.040459	2.726106
209.395833	2518.368024	6.007667	-0.040528	2.730361
209.771121	2526.437762	6.012672	-0.040603	2.734634
210.095245	2534.447430	6.017677	-0.040669	2.738865
210.405916	2542.486762	6.022682	-0.040732	2.743105
210.656230	2550.588836	6.027686	-0.040784	2.747367
210.799710	2558.652478	6.032691	-0.040816	2.751596
211.342929	2566.688884	6.037696	-0.040922	2.755829
211.439172	2574.719131	6.042701	-0.040945	2.760024
211.638459	2582.740456	6.047706	-0.040988	2.764215
211.740918	2590.806551	6.052710	-0.041012	2.768416
212.298050	2598.804816	6.057715	-0.041121	2.772604
212.608517	2606.861444	6.062720	-0.041184	2.776801
212.900148	2614.872919	6.067725	-0.041244	2.780967
213.062179	2622.958340	6.072730	-0.041279	2.785156
213.192357	2631.012561	6.077734	-0.041308	2.789322
213.335400	2639.081641	6.082739	-0.041340	2.793489
213.484955	2647.146313	6.087744	-0.041373	2.797649
213.763042	2655.135124	6.092749	-0.041430	2.801771
214.358205	2663.139720	6.097754	-0.041547	2.805914
214.289830	2671.241587	6.102758	-0.041539	2.810061
214.316811	2679.311343	6.107763	-0.041549	2.814191
214.546803	2687.381066	6.112768	-0.041597	2.818327
214.887644	2695.356244	6.117773	-0.041666	2.822415
215.050347	2703.429392	6.122778	-0.041702	2.826537
215.676390	2711.447475	6.127782	-0.041823	2.830651
215.880939	2719.492274	6.132787	-0.041867	2.834749
216.133088	2727.534124	6.137792	-0.041919	2.838842
216.276212	2735.538541	6.142797	-0.041951	2.842904
216.564367	2743.618817	6.147802	-0.042010	2.847006
216.781722	2751.668896	6.152806	-0.042055	2.851084
216.881747	2759.730388	6.157811	-0.042079	2.855154
217.523705	2767.718731	6.162816	-0.042204	2.859213
217.753298	2775.737737	6.167821	-0.042252	2.863258
217.988030	2783.823016	6.172826	-0.042301	2.867331
218.345171	2791.868038	6.177830	-0.042373	2.871384
218.363176	2799.938676	6.182835	-0.042381	2.875426
218.473143	2807.985299	6.187840	-0.042407	2.879455
218.256152	2816.066369	6.192845	-0.042372	2.883477
218.472521	2824.098538	6.197850	-0.042417	2.887493
219.087734	2832.078362	6.202854	-0.042537	2.891500
219.036762	2840.155658	6.207859	-0.042533	2.895513
219.821354	2848.114680	6.212864	-0.042684	2.899508
219.407400	2856.241810	6.217869	-0.042613	2.903514
219.908491	2864.259513	6.222874	-0.042711	2.907511
219.965230	2872.367740	6.227878	-0.042727	2.911523
220.425645	2880.382809	6.232883	-0.042818	2.915505
220.948430	2888.340070	6.237888	-0.042920	2.919457
221.062820	2896.361916	6.242893	-0.042947	2.923413
221.365363	2904.399295	6.247898	-0.043008	2.927381
221.552370	2912.497414	6.252902	-0.043049	2.931368
221.561797	2920.552338	6.257907	-0.043056	2.935318
222.385008	2928.484546	6.262912	-0.043214	2.939247
222.677559	2936.532749	6.267917	-0.043274	2.943198
222.947774	2944.592464	6.272922	-0.043329	2.947149
223.017690	2952.701086	6.277926	-0.043348	2.951107
223.328738	2960.703851	6.282931	-0.043411	2.955022
223.507039	2968.744084	6.287936	-0.043449	2.958942
223.484445	2976.793803	6.292941	-0.043450	2.962851
224.186508	2984.750275	6.297946	-0.043586	2.966748
224.351052	2992.851350	6.302950	-0.043622	2.970681
224.149567	3000.940910	6.307955	-0.043590	2.974585
224.736902	3008.944089	6.312960	-0.043704	2.978483
224.880347	3016.972951	6.317965	-0.043736	2.982365
225.002443	3025.030863	6.322970	-0.043764	2.986254
224.970198	3033.113351	6.327974	-0.043764	2.990143
225.631674	3041.071459	6.332979	-0.043892	2.994002
225.919467	3049.116665	6.337984	-0.043951	2.997879
225.861065	3057.157334	6.342989	-0.043945	3.001731
226.146689	3065.185942	6.347994	-0.044004	3.005590
226.833237	3073.196687	6.352998	-0.044137	3.009455
226.930014	3081.257923	6.358003	-0.044160	3.013310
227.481973	3089.285810	6.363008	-0.044268	3.017167
227.755669	3097.346535	6.368013	-0.044324	3.021021
227.987714	3105.353815	6.373018	-0.044373	3.024842
228.024604	3113.414303	6.378022	-0.044385	3.028673
228.144812	3121.472956	6.383027	-0.044412	3.032503
228.507074	3129.521684	6.388032	-0.044485	3.036336
228.540687	3137.553237	6.393037	-0.044496	3.040139
228.953210	3145.545920	6.398042	-0.044578	3.043938
229.264052	3153.555473	6.403046	-0.044642	3.047735
229.171714	3161.658346	6.408051	-0.044630	3.051551
229.637807	3169.697880	6.413056	-0.044722	3.055360
229.846981	3177.690070	6.418061	-0.044766	3.059130
230.168916	3185.711116	6.423066	-0.044831	3.062914
230.305163	3193.798113	6.428070	-0.044862	3.066715
230.389938	3201.867880	6.433075	-0.044883	3.070501
230.856565	3209.934275	6.438080	-0.044975	3.074298
231.439948	3217.861201	6.443085	-0.045089	3.078032
231.825978	3225.885930	6.448090	-0.045166	3.081797
232.216190	3233.920920	6.453094	-0.045244	3.085563
232.139128	3241.970870	6.458099	-0.045235	3.089308
232.267683	3250.077363	6.463104	-0.045264	3.093085
232.794467	3258.044949	6.468109	-0.045367	3.096812
233.185576	3266.070560	6.473114	-0.045445	3.100555
233.118253	3274.114932	6.478118	-0.045438	3.104280
233.768765	3282.092062	6.483123	-0.045564	3.108003
234.198027	3290.167716	6.488128	-0.045649	3.111757
234.109142	3298.219803	6.493133	-0.045638	3.115471
234.522916	3306.192155	6.498138	-0.045720	3.119168
234.879329	3314.243017	6.503142	-0.045792	3.122893
235.137069	3322.296625	6.508147	-0.045845	3.126611
235.426849	3330.365581	6.513152	-0.045904	3.130332
235.669523	3338.382319	6.518157	-0.045955	3.134024
236.064286	3346.404346	6.523162	-0.046033	3.137720
236.358162	3354.448146	6.528166	-0.046093	3.141417
236.456221	3362.472572	6.533171	-0.046117	3.145092
236.834353	3370.553157	6.538176	-0.046193	3.148801
236.833472	3378.596832	6.543181	-0.046198	3.152471
237.082765	3386.623771	6.548186	-0.046249	3.156141
237.303907	3394.639637	6.553190	-0.046296	3.159800
237.309609	3402.666218	6.558195	-0.046302	3.163451
237.734221	3410.693212	6.563200	-0.046386	3.167116
237.792796	3418.748432	6.568205	-0.046402	3.170773
237.682596	3426.850200	6.573210	-0.046387	3.174439
238.319480	3434.798544	6.578214	-0.046511	3.178065
238.595880	3442.820476	6.583219	-0.046568	3.181704
239.176417	3450.826971	6.588224	-0.046681	3.185345
239.561506	3458.821056	6.593229	-0.046758	3.188968
239.852201	3466.890436	6.598234	-0.046817	3.192616
240.145358	3474.967574	6.603238	-0.046877	3.196264
240.351055	3482.957607	6.608243	-0.046921	3.199865
240.838436	3490.955343	6.613248	-0.047017	3.203477
240.708283	3499.039162	6.618253	-0.046998	3.207097
241.269564	3507.060809	6.623258	-0.047107	3.210715
241.083714	3515.166849	6.628262	-0.047078	3.214334
241.338984	3523.155209	6.633267	-0.047131	3.217916
241.551698	3531.236421	6.638272	-0.047176	3.221533
241.819225	3539.210943	6.643277	-0.047231	3.225101
242.019593	3547.263924	6.648282	-0.047273	3.228696
242.198557	3555.339250	6.653286	-0.047312	3.232297
242.496272	3563.304214	6.658291	-0.047372	3.235850
242.728692	3571.316615	6.663296	-0.047421	3.239417
242.893395	3579.319698	6.668301	-0.047457	3.242974
243.004472	3587.419899	6.673306	-0.047483	3.246567
243.152196	3595.453697	6.678310	-0.047516	3.250128
243.531747	3603.435810	6.683315	-0.047591	3.253672
243.995060	3611.468513	6.688320	-0.047683	3.257238
243.886952	3619.548669	6.693325	-0.047668	3.260798
244.183524	3627.533303	6.698330	-0.047728	3.264328
244.883612	3635.522620	6.703334	-0.047864	3.267872
244.494012	3643.660311	6.708339	-0.047797	3.271434
245.164254	3651.643949	6.713344	-0.047927	3.274967
245.252639	3659.655344	6.718349	-0.047948	3.278485
245.579791	3667.705447	6.723354	-0.048015	3.282026
245.535819	3675.754979	6.728358	-0.048012	3.285547
246.169426	3683.681708	6.733363	-0.048135	3.289039
246.713872	3691.737614	6.738368	-0.048241	3.292579
247.104324	3699.786456	6.743373	-0.048319	3.296106
247.089398	3707.815827	6.748378	-0.048322	3.299605
247.392966	3715.874990	6.753382	-0.048384	3.303126
247.613432	3723.904477	6.758387	-0.048430	3.306626
248.034508	3731.938809	6.763392	-0.048514	3.310133
248.591398	3739.919942	6.768397	-0.048622	3.313619
248.972561	3747.935680	6.773402	-0.048699	3.317108
249.081272	3756.000422	6.778406	-0.048724	3.320605
249.268783	3763.984337	6.783411	-0.048764	3.324066
249.856655	3772.043464	6.788416	-0.048879	3.327572
249.829343	3780.101221	6.793421	-0.048879	3.331049
249.812027	3788.177367	6.798426	-0.048881	3.334531
249.802535	3796.240953	6.803430	-0.048885	3.338004
250.091336	3804.215328	6.808435	-0.048944	3.341447
250.635602	3812.225584	6.813440	-0.049050	3.344911
250.821677	3820.245517	6.818445	-0.049090	3.348362
251.301210	3828.277071	6.823450	-0.049185	3.351825
251.397566	3836.346509	6.828454	-0.049208	3.355287
251.562563	3844.303022	6.833459	-0.049244	3.358699
252.011025	3852.334915	6.838464	-0.049332	3.362151
252.237429	3860.366906	6.843469	-0.049380	3.365591
252.096886	3868.469968	6.848474	-0.049359	3.369044
252.301879	3876.511656	6.853478	-0.049402	3.372480
252.561987	3884.502594	6.858483	-0.049456	3.375893
252.926676	3892.531601	6.863488	-0.049529	3.379323
253.225235	3900.517339	6.868493	-0.049590	3.382728
253.587186	3908.572751	6.873498	-0.049663	3.386161
254.114814	3916.598703	6.878502	-0.049766	3.389585
254.026654	3924.675561	6.883507	-0.049755	3.393004
253.969495	3932.757876	6.888512	-0.049750	3.396423
254.447943	3940.688064	6.893517	-0.049844	3.399794
254.300054	3948.756644	6.898522	-0.049822	3.403197
254.597316	3956.768732	6.903526	-0.049882	3.406589
255.228870	3964.727989	6.908531	-0.050005	3.409968
255.612791	3972.763874	6.913536	-0.050082	3.413366
255.816805	3980.823152	6.918541	-0.050125	3.416764
256.154690	3988.853268	6.923546	-0.050193	3.420152
256.436104	3996.827083	6.928550	-0.050251	3.423510
256.241591	4004.923245	6.933555	-0.050220	3.426900
256.837234	4012.925439	6.938560	-0.050336	3.430274
256.934020	4020.961784	6.943565	-0.050359	3.433642
257.017549	4029.020618	6.948570	-0.050380	3.437016
257.396926	4037.000041	6.953574	-0.050456	3.440363
257.789378	4044.971371	6.958579	-0.050534	3.443704
257.869574	4053.084315	6.963584	-0.050554	3.447091
258.032309	4061.103255	6.968589	-0.050590	3.450437
258.148164	4069.140677	6.973594	-0.050617	3.453786
258.512847	4077.156514	6.978598	-0.050690	3.457132
258.728294	4085.190264	6.983603	-0.050735	3.460476
258.944010	4093.207036	6.988608	-0.050780	3.463811
259.184106	4101.256773	6.993613	-0.050830	3.467156
259.674875	4109.266868	6.998618	-0.050927	3.470491
259.839804	4117.280395	7.003622	-0.050963	3.473812
259.910844	4125.329676	7.008627	-0.050981	3.477142
260.151110	4133.368510	7.013632	-0.051031	3.480470
260.252338	4141.333246	7.018637	-0.051055	3.483760
260.714949	4149.356840	7.023642	-0.051147	3.487082
260.846654	4157.423941	7.028646	-0.051177	3.490409
260.618536	4165.488106	7.033651	-0.051139	3.493719
261.199180	4173.464139	7.038656	-0.051253	3.497017
261.007874	4181.549728	7.043661	-0.051222	3.500331
261.294898	4189.515083	7.048666	-0.051281	3.503608
261.625913	4197.576761	7.053670	-0.051348	3.506923
261.747829	4205.604013	7.058675	-0.051376	3.510214
262.144484	4213.639352	7.063680	-0.051455	3.513514
262.224718	4221.666807	7.068685	-0.051475	3.516797
262.480532	4229.664325	7.073690	-0.051528	3.520071
262.585884	4237.723295	7.078694	-0.051553	3.523362
263.041967	4245.673588	7.083699	-0.051643	3.526616
263.412361	4253.749343	7.088704	-0.051717	3.529916
263.633491	4261.723872	7.093709	-0.051763	3.533167
263.967298	4269.796272	7.098714	-0.051831	3.536459
264.079884	4277.831900	7.103718	-0.051857	3.539725
264.122172	4285.817287	7.108723	-0.051870	3.542965
264.619726	4293.879835	7.113728	-0.051968	3.546249
264.519669	4301.928021	7.118733	-0.051955	3.549504
264.879538	4309.986996	7.123738	-0.052027	3.552775
265.124632	4318.038367	7.128742	-0.052078	3.556037
265.355314	4325.925846	7.133747	-0.052126	3.559229
265.543466	4333.988657	7.138752	-0.052166	3.562487
265.663590	4342.011396	7.143757	-0.052194	3.565724
266.028665	4349.974905	7.148762	-0.052267	3.568942
265.972987	4358.090805	7.153766	-0.052262	3.572206
266.081467	4366.109308	7.158771	-0.052287	3.575432
266.043402	4374.177977	7.163776	-0.052285	3.578671
266.186090	4382.175826	7.168781	-0.052317	3.581884
266.421099	4390.152233	7.173786	-0.052366	3.585089
266.911489	4398.180860	7.178790	-0.052463	3.588319
267.345918	4406.187536	7.183795	-0.052549	3.591535
267.283272	4414.243032	7.188800	-0.052542	3.594754
267.900540	4422.182082	7.193805	-0.052662	3.597943
268.292832	4430.236587	7.198810	-0.052741	3.601169
268.155839	4438.291098	7.203814	-0.052721	3.604376
268.338737	4446.327759	7.208819	-0.052760	3.607582
268.671846	4454.397590	7.213824	-0.052827	3.610804
268.757251	4462.369481	7.218829	-0.052848	3.613976
268.991723	4470.446890	7.223834	-0.052897	3.617192
269.311468	4478.464836	7.228838	-0.052962	3.620383
269.578670	4486.427642	7.233843	-0.053017	3.623549
269.951787	4494.496337	7.238848	-0.053092	3.626756
270.049327	4502.541637	7.243853	-0.053115	3.629944
270.255446	4510.576021	7.248858	-0.053159	3.633127
270.619925	4518.597552	7.253862	-0.053232	3.636307
270.748875	4526.553651	7.258867	-0.053261	3.639452
271.052605	4534.589009	7.263872	-0.053323	3.642630
271.152736	4542.657832	7.268877	-0.053347	3.645813
271.233636	4550.666903	7.273882	-0.053367	3.648969
271.307856	4558.735817	7.278886	-0.053386	3.652146
271.500958	4566.723992	7.283891	-0.053427	3.655291
271.694638	4574.756479	7.288896	-0.053468	3.658451
272.039500	4582.701873	7.293901	-0.053538	3.661579
272.256446	4590.734028	7.298906	-0.053583	3.664734
272.110681	4598.824711	7.303910	-0.053562	3.667899
271.951496	4606.887343	7.308915	-0.053537	3.671051
272.361738	4614.865602	7.313920	-0.053619	3.674182
272.544433	4622.885711	7.318925	-0.053658	3.677320
272.744003	4630.874799	7.323930	-0.053700	3.680444
272.762041	4638.924841	7.328934	-0.053709	3.683585
273.215920	4646.898314	7.333939	-0.053799	3.686704
273.335617	4654.945618	7.338944	-0.053826	3.689841
273.603472	4662.953646	7.343949	-0.053881	3.692964
273.656143	4671.049031	7.348954	-0.053896	3.696112
273.968159	4679.037344	7.353958	-0.053960	3.699223
274.161991	4687.056578	7.358963	-0.054001	3.702340
274.712857	4695.097371	7.363968	-0.054109	3.705472
274.987190	4703.125831	7.368973	-0.054165	3.708589
275.296031	4711.160487	7.373978	-0.054228	3.711707
275.215248	4719.270764	7.378982	-0.054218	3.714841
275.406107	4727.225972	7.383987	-0.054259	3.717920
275.445228	4735.307918	7.388992	-0.054271	3.721042
275.575537	4743.205257	7.393997	-0.054301	3.724092
275.987592	4751.219449	7.399002	-0.054383	3.727191
276.246461	4759.272440	7.404006	-0.054436	3.730299
276.236441	4767.314939	7.409011	-0.054440	3.733394
276.637890	4775.350302	7.414016	-0.054520	3.736493
276.466471	4783.375264	7.419021	-0.054493	3.739572
276.707165	4791.389030	7.424026	-0.054543	3.742654
276.992257	4799.405020	7.429030	-0.054601	3.745735
277.362991	4807.398595	7.434035	-0.054675	3.748807
277.534429	4815.438608	7.439040	-0.054713	3.751890
277.674951	4823.471783	7.444045	-0.054744	3.754967
277.526030	4831.521092	7.449050	-0.054722	3.758040
277.743901	4839.573230	7.454054	-0.054767	3.761121
277.519745	4847.523428	7.459059	-0.054731	3.764150
278.350082	4855.492733	7.464064	-0.054891	3.767209
278.504041	4863.549216	7.469069	-0.054925	3.770282
278.678679	4871.573311	7.474074	-0.054962	3.773341
279.064194	4879.617891	7.479078	-0.055039	3.776410
279.514990	4887.551717	7.484083	-0.055128	3.779436
279.284935	4895.682510	7.489088	-0.055091	3.782519
279.895705	4903.644218	7.494093	-0.055210	3.785554
280.385268	4911.647271	7.499098	-0.055306	3.788600
280.314664	4919.760770	7.504102	-0.055298	3.791672
280.595380	4927.717321	7.509107	-0.055356	3.794690
280.835962	4935.770325	7.514112	-0.055406	3.797742
281.229721	4943.780071	7.519117	-0.055484	3.800778
281.237340	4951.745465	7.524122	-0.055491	3.803786
281.263349	4959.868365	7.529126	-0.055501	3.806851
281.731311	4967.830273	7.534131	-0.055593	3.809864
281.961300	4975.878536	7.539136	-0.055641	3.812901
282.224542	4983.917221	7.544141	-0.055696	3.815933
282.103772	4991.894904	7.549146	-0.055678	3.818930
282.081895	5000.001722	7.554150	-0.055680	3.821977
282.650524	5007.915188	7.559155	-0.055791	3.824961
282.641359	5016.042491	7.564160	-0.055794	3.828010
283.008165	5024.088243	7.569165	-0.055868	3.831035
283.339841	5032.005862	7.574170	-0.055935	3.834008
282.873581	5040.166866	7.579174	-0.055853	3.837053
283.140773	5048.102516	7.584179	-0.055908	3.840027
283.649490	5056.097207	7.589184	-0.056008	3.843026
283.379465	5064.187969	7.594189	-0.055963	3.846041
283.905861	5072.131690	7.599194	-0.056066	3.849017
283.913540	5080.222317	7.604198	-0.056073	3.852034
284.085796	5088.185757	7.609203	-0.056110	3.855004
284.480904	5096.229051	7.614208	-0.056189	3.858007
284.724555	5104.243788	7.619213	-0.056240	3.860994
284.765253	5112.241954	7.624218	-0.056252	3.863967
285.093654	5120.264450	7.629222	-0.056319	3.866954
285.323464	5128.296351	7.634227	-0.056367	3.869939
285.470135	5136.474008	7.639232	-0.056399	3.872975
285.522710	5144.514244	7.644237	-0.056414	3.875955
285.896041	5152.372345	7.649242	-0.056489	3.878872
286.370651	5160.373544	7.654246	-0.056583	3.881842
285.905513	5168.386022	7.659251	-0.056501	3.884795
286.379370	5176.400568	7.664256	-0.056595	3.887765
286.750131	5184.431379	7.669261	-0.056669	3.890737
287.069322	5192.428148	7.674266	-0.056734	3.893693
286.952357	5200.523691	7.679270	-0.056717	3.896674
286.615094	5208.528869	7.684275	-0.056660	3.899615
287.044757	5216.542343	7.689280	-0.056745	3.902573
287.464006	5224.462426	7.694285	-0.056828	3.905493
287.727764	5232.495629	7.699290	-0.056882	3.908450
288.069666	5240.605688	7.704294	-0.056951	3.911434
288.197853	5248.562446	7.709299	-0.056980	3.914356
288.535333	5256.603479	7.714304	-0.057048	3.917310
288.720243	5264.611967	7.719309	-0.057088	3.920248
288.825321	5272.644436	7.724314	-0.057113	3.923190
289.010887	5280.727404	7.729318	-0.057153	3.926150
289.490307	5288.686572	7.734323	-0.057247	3.929068
289.998084	5296.747874	7.739328	-0.057347	3.932022
290.080558	5304.756393	7.744333	-0.057368	3.934946
290.179898	5312.788875	7.749338	-0.057391	3.937877
290.243825	5320.842087	7.754342	-0.057408	3.940812
290.205925	5328.848274	7.759347	-0.057407	3.943727
290.216889	5336.935973	7.764352	-0.057414	3.946669
290.160290	5344.948142	7.769357	-0.057409	3.949581
290.546112	5352.957347	7.774362	-0.057486	3.952498
290.991165	5360.930051	7.779366	-0.057574	3.955401
290.985401	5368.909290	7.784371	-0.057578	3.958295
291.419610	5377.023783	7.789376	-0.057664	3.961244
291.540794	5384.945575	7.794381	-0.057692	3.964116
291.802936	5392.954114	7.799386	-0.057746	3.967020
292.262147	5401.006291	7.804390	-0.057837	3.969940
292.637586	5408.995315	7.809395	-0.057912	3.972834
293.321788	5417.017409	7.814400	-0.058044	3.975744
293.248646	5425.055362	7.819405	-0.058036	3.978643
293.659816	5433.083140	7.824410	-0.058118	3.981545
293.763398	5441.093885	7.829414	-0.058142	3.984434
293.698862	5449.120427	7.834419	-0.058135	3.987323
293.888172	5457.189046	7.839424	-0.058176	3.990229
293.942541	5465.188516	7.844429	-0.058191	3.993107
294.264460	5473.221748	7.849434	-0.058256	3.995999
294.448756	5481.211007	7.854438	-0.058296	3.998870
294.847480	5489.194104	7.859443	-0.058375	4.001741
294.535946	5497.250892	7.864448	-0.058323	4.004624
295.184099	5505.235612	7.869453	-0.058449	4.007496
295.216790	5513.268484	7.874458	-0.058460	4.010372
295.708776	5521.297772	7.879462	-0.058557	4.013253
295.921936	5529.311154	7.884467	-0.058602	4.016121
295.941667	5537.334134	7.889472	-0.058611	4.018987
296.381429	5545.359104	7.894477	-0.058698	4.021859
296.471271	5553.365907	7.899482	-0.058720	4.024717
296.767123	5561.436427	7.904486	-0.058780	4.027599
296.747158	5569.430888	7.909491	-0.058781	4.030446
297.023880	5577.540298	7.914496	-0.058838	4.033337
297.219202	5585.538179	7.919501	-0.058880	4.036185
297.475141	5593.462610	7.924506	-0.058933	4.039005
297.669374	5601.531767	7.929510	-0.058974	4.041875
297.928546	5609.468324	7.934515	-0.059027	4.044696
298.501007	5617.499566	7.939520	-0.059139	4.047553
298.678434	5625.564878	7.944525	-0.059178	4.050415
298.654130	5633.571717	7.949530	-0.059178	4.053250
298.929807	5641.650354	7.954534	-0.059235	4.056113
298.997958	5649.589397	7.959539	-0.059253	4.058922
299.349768	5657.690362	7.964544	-0.059324	4.061791
299.450790	5665.639217	7.969549	-0.059348	4.064600
299.733087	5673.690189	7.974554	-0.059405	4.067445
300.079407	5681.735310	7.979558	-0.059475	4.070288
299.858914	5689.783949	7.984563	-0.059439	4.073121
300.325301	5697.829159	7.989568	-0.059531	4.075962
300.557022	5705.779237	7.994573	-0.059580	4.078763
300.513579	5713.805141	7.999578	-0.059577	4.081585
300.673844	5721.773799	8.004582	-0.059612	4.084388
300.911433	5729.836355	8.009587	-0.059661	4.087223
301.388755	5737.863463	8.014592	-0.059755	4.090047
301.328560	5745.915098	8.019597	-0.059749	4.092870
301.510796	5753.908782	8.024602	-0.059789	4.095674
301.626449	5761.958921	8.029606	-0.059815	4.098495
301.807098	5769.987014	8.034611	-0.059854	4.101308
302.229583	5777.895648	8.039616	-0.059938	4.104080
302.380183	5785.961135	8.044621	-0.059971	4.106901
302.212868	5794.026298	8.049626	-0.059945	4.109715
302.968246	5802.012423	8.054630	-0.060091	4.112513
303.240393	5810.006621	8.059635	-0.060147	4.115305
303.308904	5818.044938	8.064640	-0.060165	4.118108
303.427125	5826.072451	8.069645	-0.060192	4.120905
303.797948	5834.025535	8.074650	-0.060267	4.123679
304.164101	5842.070514	8.079654	-0.060340	4.126482
304.366717	5850.050233	8.084659	-0.060383	4.129258
304.695354	5858.140214	8.089664	-0.060450	4.132073
304.784679	5866.174920	8.094669	-0.060471	4.134863
304.910861	5874.150656	8.099674	-0.060500	4.137631
305.173934	5882.207645	8.104678	-0.060554	4.140427
305.277695	5890.159957	8.109683	-0.060579	4.143184
305.644341	5898.221338	8.114688	-0.060652	4.145979
305.651983	5906.254891	8.119693	-0.060659	4.148758
305.799990	5914.297618	8.124698	-0.060692	4.151541
306.174970	5922.275882	8.129702	-0.060767	4.154302
306.335790	5930.295596	8.134707	-0.060802	4.157072
306.657730	5938.293069	8.139712	-0.060867	4.159836
306.860136	5946.317595	8.144717	-0.060910	4.162605
306.881786	5954.368651	8.149722	-0.060919	4.165379
307.274350	5962.352678	8.154726	-0.060998	4.168133
307.441021	5970.377534	8.159731	-0.061034	4.170896
307.582268	5978.413243	8.164736	-0.061065	4.173661
307.699253	5986.464301	8.169741	-0.061092	4.176429
307.905215	5994.438474	8.174746	-0.061136	4.179170
308.329065	6002.511298	8.179750	-0.061220	4.181945
308.495986	6010.442053	8.184755	-0.061256	4.184667
308.555269	6018.549480	8.189760	-0.061273	4.187446
308.589317	6026.591162	8.194765	-0.061284	4.190201
308.745156	6034.619354	8.199770	-0.061319	4.192950
308.871689	6042.682198	8.204774	-0.061347	4.195710
309.090207	6050.594684	8.209779	-0.061393	4.198417
309.625386	6058.648825	8.214784	-0.061498	4.201174
309.612029	6066.581529	8.219789	-0.061501	4.203882
309.952466	6074.631069	8.224794	-0.061569	4.206632
310.320813	6082.625547	8.229798	-0.061643	4.209361
310.322746	6090.710858	8.234803	-0.061649	4.212116
310.718001	6098.712370	8.239808	-0.061728	4.214844
310.718313	6106.774402	8.244813	-0.061733	4.217587
310.982717	6114.743075	8.249818	-0.061787	4.220300
311.270479	6122.804467	8.254822	-0.061846	4.223042
311.180875	6130.777604	8.259827	-0.061835	4.225749
311.706070	6138.787693	8.264832	-0.061938	4.228473
311.822353	6146.897210	8.269837	-0.061965	4.231224
311.983831	6154.826334	8.274842	-0.062000	4.233913
312.080363	6162.927664	8.279846	-0.062023	4.236658
312.486512	6170.825333	8.284851	-0.062104	4.239335
312.560954	6178.905567	8.289856	-0.062123	4.242069
312.722983	6186.879336	8.294861	-0.062159	4.244766
312.910431	6194.896298	8.299866	-0.062199	4.247477
313.328922	6202.935487	8.304870	-0.062282	4.250195
313.583935	6210.945141	8.309875	-0.062335	4.252900
313.839810	6218.984989	8.314880	-0.062387	4.255613
313.827501	6226.977837	8.319885	-0.062390	4.258306
313.981638	6235.020895	8.324890	-0.062424	4.261016
314.221678	6243.004435	8.329894	-0.062474	4.263705
314.333302	6251.037737	8.334899	-0.062500	4.266408
314.607693	6259.094687	8.339904	-0.062557	4.269118
314.922778	6267.119439	8.344909	-0.062620	4.271817
315.240803	6275.082328	8.349914	-0.062685	4.274493
315.336596	6283.118117	8.354918	-0.062708	4.277189
315.422590	6291.101541	8.359923	-0.062729	4.279866
315.760747	6299.121144	8.364928	-0.062797	4.282556
315.752697	6307.177044	8.369933	-0.062801	4.285253
315.888701	6315.153765	8.374938	-0.062832	4.287923
316.258396	6323.204744	8.379942	-0.062906	4.290619
316.615630	6331.200540	8.384947	-0.062977	4.293294
316.842068	6339.245231	8.389952	-0.063025	4.295983
316.989431	6347.232626	8.394957	-0.063057	4.298650
317.101683	6355.296210	8.399962	-0.063084	4.301340
317.268645	6363.230405	8.404966	-0.063120	4.303987
317.364866	6371.300793	8.409971	-0.063143	4.306676
317.571005	6379.344319	8.414976	-0.063187	4.309356
317.791615	6387.362531	8.419981	-0.063233	4.312025
317.985071	6395.309490	8.424986	-0.063274	4.314669
318.208452	6403.374363	8.429990	-0.063321	4.317351
318.570854	6411.330795	8.434995	-0.063394	4.319996
318.571790	6419.356872	8.440000	-0.063399	4.322660
318.753552	6427.358911	8.445005	-0.063438	4.325316
319.058789	6435.412826	8.450010	-0.063500	4.327988
319.302048	6443.434720	8.455014	-0.063551	4.330647
319.427766	6451.483383	8.460019	-0.063579	4.333313
319.888498	6459.467604	8.465024	-0.063670	4.335958
320.055873	6467.493211	8.470029	-0.063707	4.338613
320.255114	6475.508875	8.475034	-0.063749	4.341263
320.489484	6483.495597	8.480038	-0.063798	4.343902
320.841018	6491.570647	8.485043	-0.063869	4.346570
320.876151	6499.549263	8.490048	-0.063880	4.349202
320.971901	6507.642187	8.495053	-0.063904	4.351870
321.269519	6515.612278	8.500058	-0.063964	4.354498
321.406695	6523.658290	8.505062	-0.063995	4.357148
321.608225	6531.566394	8.510067	-0.064038	4.359752
321.822866	6539.650924	8.515072	-0.064083	4.362412
322.004811	6547.608158	8.520077	-0.064122	4.365028
322.229264	6555.658702	8.525082	-0.064169	4.367673
322.377679	6563.667346	8.530086	-0.064202	4.370303
322.531202	6571.683628	8.535091	-0.064236	4.372934
322.703050	6579.726327	8.540096	-0.064273	4.375571
322.854019	6587.716250	8.545101	-0.064306	4.378190
323.226066	6595.738841	8.550106	-0.064381	4.380820
323.518575	6603.769007	8.555110	-0.064440	4.383449
323.551721	6611.798927	8.560115	-0.064452	4.386075
323.809316	6619.804285	8.565120	-0.064505	4.388694
323.753591	6627.836125	8.570125	-0.064500	4.391317
323.923875	6635.816597	8.575130	-0.064537	4.393923
324.273854	6643.901726	8.580135	-0.064607	4.396563
324.569395	6651.836800	8.585139	-0.064667	4.399152
324.652588	6659.909198	8.590144	-0.064688	4.401783
324.692123	6667.902911	8.595149	-0.064701	4.404386
324.941201	6675.946351	8.600154	-0.064752	4.407006
325.174573	6683.970975	8.605159	-0.064801	4.409617
325.340611	6692.004587	8.610163	-0.064837	4.412230
325.625241	6700.085079	8.615168	-0.064895	4.414857
325.736736	6708.088041	8.620173	-0.064921	4.417456
325.814065	6716.106968	8.625178	-0.064941	4.420058
326.127083	6724.145738	8.630183	-0.065004	4.422667
326.376357	6732.118238	8.635187	-0.065056	4.425252
326.538560	6740.147154	8.640192	-0.065092	4.427854
326.602323	6748.247188	8.645197	-0.065109	4.430476
326.877874	6756.204636	8.650202	-0.065165	4.433052
327.125657	6764.281266	8.655207	-0.065217	4.435665
327.222095	6772.192283	8.660211	-0.065240	4.438222
327.610773	6780.306189	8.665216	-0.065317	4.440844
327.734601	6788.221314	8.670221	-0.065346	4.443400
327.969522	6796.282558	8.675226	-0.065395	4.446001
328.048976	6804.322988	8.680231	-0.065415	4.448594
328.410804	6812.346298	8.685235	-0.065487	4.451181
328.824298	6820.330959	8.690240	-0.065569	4.453754
328.948159	6828.371393	8.695245	-0.065598	4.456342
329.232124	6836.327739	8.700250	-0.065656	4.458902
329.519201	6844.427662	8.705255	-0.065715	4.461507
329.628134	6852.331874	8.710259	-0.065740	4.464047
329.810644	6860.472045	8.715264	-0.065779	4.466661
329.915343	6868.425471	8.720269	-0.065804	4.469214
330.274217	6876.514312	8.725274	-0.065876	4.471810
330.457925	6884.454526	8.730279	-0.065915	4.474355
330.559435	6892.488208	8.735283	-0.065940	4.476929
330.919109	6900.460657	8.740288	-0.066012	4.479483
331.190765	6908.513154	8.745293	-0.066068	4.482060
331.260501	6916.478305	8.750298	-0.066086	4.484608
331.668966	6924.567767	8.755303	-0.066167	4.487195
331.974408	6932.525508	8.760307	-0.066229	4.489737
332.086318	6940.582264	8.765312	-0.066255	4.492310
332.404056	6948.582431	8.770317	-0.066320	4.494863
332.505435	6956.616339	8.775322	-0.066344	4.497425
332.731996	6964.625948	8.780327	-0.066391	4.499978
332.902291	6972.618307	8.785331	-0.066428	4.502524
333.090957	6980.646450	8.790336	-0.066468	4.505080
333.209915	6988.702602	8.795341	-0.066496	4.507643
333.278033	6996.733508	8.800346	-0.066514	4.510197
333.604237	7004.747512	8.805351	-0.066580	4.512744
333.784202	7012.679243	8.810355	-0.066618	4.515264
333.936160	7020.693508	8.815360	-0.066652	4.517808
334.048276	7028.713754	8.820365	-0.066678	4.520352
334.183948	7036.665437	8.825370	-0.066708	4.522874
334.398388	7044.754880	8.830375	-0.066754	4.525438
334.510712	7052.730670	8.835379	-0.066780	4.527964
334.806762	7060.834528	8.840384	-0.066840	4.530529
335.076472	7068.828825	8.845389	-0.066896	4.533059
334.981472	7076.861661	8.850394	-0.066883	4.535598
335.389889	7084.845041	8.855399	-0.066964	4.538121
335.394853	7092.873158	8.860403	-0.066970	4.540656
335.512295	7100.838511	8.865408	-0.066998	4.543171
335.586093	7108.915623	8.870413	-0.067017	4.545718
335.779146	7116.880424	8.875418	-0.067058	4.548230
336.008228	7124.993146	8.880423	-0.067106	4.550786
336.172382	7132.913676	8.885427	-0.067141	4.553281
336.424499	7140.979852	8.890432	-0.067194	4.555820
336.524523	7148.936589	8.895437	-0.067217	4.558323
336.924140	7156.949232	8.900442	-0.067297	4.560843
337.094454	7164.936271	8.905447	-0.067334	4.563352
337.136689	7173.034072	8.910451	-0.067347	4.565895
337.340925	7181.014937	8.915456	-0.067390	4.568400
337.413212	7189.089728	8.920461	-0.067409	4.570933
337.553272	7197.074972	8.925466	-0.067440	4.573437
337.902291	7205.105256	8.930471	-0.067510	4.575953
338.019854	7213.058682	8.935475	-0.067538	4.578444
338.350662	7221.127047	8.940480	-0.067604	4.580970
338.637199	7229.104399	8.945485	-0.067663	4.583466
338.786046	7237.131894	8.950490	-0.067696	4.585975
339.001712	7245.170511	8.955495	-0.067741	4.588487
339.180341	7253.176804	8.960499	-0.067780	4.590988
339.343559	7261.192614	8.965504	-0.067815	4.593490
339.493365	7269.237955	8.970509	-0.067849	4.595999
339.631713	7277.173616	8.975514	-0.067879	4.598474
339.678677	7285.260312	8.980519	-0.067893	4.600993
339.895703	7293.187352	8.985523	-0.067939	4.603462
340.163942	7301.227914	8.990528	-0.067994	4.605965
340.326480	7309.258274	8.995533	-0.068030	4.608463
340.423594	7317.268167	9.000538	-0.068053	4.610954
340.841093	7325.291493	9.005543	-0.068136	4.613447
340.889965	7333.349563	9.010547	-0.068150	4.615950
340.932886	7341.348665	9.015552	-0.068164	4.618433
340.926939	7349.402552	9.020557	-0.068168	4.620932
341.198843	7357.324189	9.025562	-0.068224	4.623388
341.441508	7365.403387	9.030567	-0.068274	4.625892
341.477013	7373.380590	9.035571	-0.068286	4.628362
341.844929	7381.431106	9.040576	-0.068360	4.630855
341.955806	7389.415853	9.045581	-0.068385	4.633325
342.227205	7397.459231	9.050586	-0.068441	4.635813
342.544833	7405.431205	9.055591	-0.068505	4.638276
342.798305	7413.469282	9.060595	-0.068558	4.640759
343.093222	7421.439919	9.065600	-0.068618	4.643220
343.088116	7429.508190	9.070605	-0.068622	4.645710
343.421011	7437.474341	9.075610	-0.068690	4.648166
343.577524	7445.601919	9.080615	-0.068724	4.650671
343.774679	7453.525121	9.085619	-0.068766	4.653112
344.103274	7461.611835	9.090624	-0.068832	4.655602
344.175377	7469.566923	9.095629	-0.068851	4.658050
344.276521	7477.615601	9.100634	-0.068875	4.660525
344.612496	7485.592600	9.105639	-0.068943	4.662977
344.659117	7493.649882	9.110643	-0.068957	4.665453
344.883455	7501.665916	9.115648	-0.069004	4.667914
345.171164	7509.712821	9.120653	-0.069062	4.670384
345.282322	7517.722084	9.125658	-0.069088	4.672840
345.517801	7525.773522	9.130663	-0.069137	4.675309
345.401720	7533.699189	9.135667	-0.069121	4.677737
345.976830	7541.706911	9.140672	-0.069233	4.680189
346.349092	7549.698181	9.145677	-0.069308	4.682635
346.337452	7557.701985	9.150682	-0.069311	4.685084
346.627335	7565.786387	9.155687	-0.069370	4.687555
346.797582	7573.784901	9.160691	-0.069407	4.690000
347.254475	7581.795720	9.165696	-0.069497	4.692446
347.204028	7589.816369	9.170701	-0.069493	4.694895
347.427124	7597.820669	9.175706	-0.069540	4.697337
347.691806	7605.851911	9.180711	-0.069594	4.699785
347.909627	7613.858582	9.185715	-0.069640	4.702226
348.165055	7621.831730	9.190720	-0.069693	4.704654
348.395637	7629.935150	9.195725	-0.069741	4.707121
348.392815	7637.897176	9.200730	-0.069746	4.709544
348.599377	7646.036780	9.205735	-0.069790	4.712020
348.778213	7653.939214	9.210739	-0.069828	4.714422
349.005700	7662.013531	9.215744	-0.069876	4.716875
349.066496	7669.943186	9.220749	-0.069892	4.719283
349.186271	7677.983217	9.225754	-0.069920	4.721723
349.617363	7685.977762	9.230759	-0.070005	4.724147
349.461560	7694.054501	9.235763	-0.069981	4.726597
349.683904	7701.996502	9.240768	-0.070028	4.729003
350.046047	7710.079609	9.245773	-0.070101	4.731451
350.227424	7718.049318	9.250778	-0.070140	4.733863
350.184389	7726.198158	9.255783	-0.070137	4.736329
350.449421	7734.092101	9.260787	-0.070192	4.738716
350.582578	7742.200993	9.265792	-0.070222	4.741166
350.702018	7750.186901	9.270797	-0.070249	4.743579
350.828888	7758.205940	9.275802	-0.070278	4.746000
351.043875	7766.228770	9.280807	-0.070323	4.748421
351.039816	7774.237505	9.285811	-0.070328	4.750836
351.391539	7782.228319	9.290816	-0.070398	4.753245
351.583052	7790.266573	9.295821	-0.070439	4.755667
351.667409	7798.208567	9.300826	-0.070460	4.758058
351.658193	7806.290726	9.305831	-0.070464	4.760491
351.809295	7814.235204	9.310835	-0.070497	4.762881
352.028920	7822.332850	9.315840	-0.070543	4.765316
352.097803	7830.339837	9.320845	-0.070561	4.767722
352.317886	7838.313862	9.325850	-0.070607	4.770117
352.505605	7846.402960	9.330855	-0.070648	4.772545
352.715960	7854.349760	9.335859	-0.070692	4.774930
352.839972	7862.339320	9.340864	-0.070720	4.777326
353.103925	7870.429158	9.345869	-0.070775	4.779750
353.247616	7878.455268	9.350874	-0.070807	4.782155
353.457657	7886.401725	9.355879	-0.070851	4.784534
353.725129	7894.451948	9.360883	-0.070906	4.786943
354.097230	7902.474084	9.365888	-0.070980	4.789342
354.251250	7910.490651	9.370893	-0.071014	4.791739
354.336044	7918.532455	9.375898	-0.071035	4.794142
354.609000	7926.595141	9.380903	-0.071091	4.796550
354.423025	7934.504957	9.385907	-0.071062	4.798912
354.899813	7942.549984	9.390912	-0.071156	4.801311
355.204245	7950.474648	9.395917	-0.071218	4.803674
355.372410	7958.544110	9.400922	-0.071254	4.806079
355.549181	7966.587404	9.405927	-0.071293	4.808476
355.828118	7974.640279	9.410931	-0.071350	4.810873
356.068666	7982.650634	9.415936	-0.071400	4.813257
355.908294	7990.139243	9.420941	-0.071375	4.815485
355.848536	7994.682402	9.425946	-0.071367	4.816837

356.321315	7997.286084	9.430951	-0.071456	4.817609
356.751762	7998.451026	9.435955	-0.071537	4.817954
356.694677	7998.952206	9.440960	-0.071527	4.818103
356.798652	7999.889256	9.445965	-0.071547	4.818381
357.034268	7999.892396	9.450970	-0.071591	4.818381
357.261125	7999.920625	9.455975	-0.071633	4.818389
357.220976	7999.871782	9.460979	-0.071626	4.818374
357.559234	7999.898346	9.465984	-0.071689	4.818381
357.697759	7999.886541	9.470989	-0.071714	4.818377
357.679432	7999.897849	9.475994	-0.071711	4.818380
358.017502	7999.910759	9.480999	-0.071774	4.818383
357.938585	7999.860348	9.486003	-0.071759	4.818368
357.850613	7999.904332	9.491008	-0.071743	4.818382
357.972576	7999.916461	9.496013	-0.071766	4.818385
357.993389	7999.883132	9.501018	-0.071769	4.818375
358.160819	7999.906370	9.506023	-0.071801	4.818381
358.305398	7999.886244	9.511027	-0.071828	4.818374
358.429610	7999.899453	9.516032	-0.071851	4.818378
358.421032	7999.902490	9.521037	-0.071849	4.818379
358.206866	7999.900683	9.526042	-0.071809	4.818379
358.644361	7999.912821	9.531047	-0.071891	4.818381
358.702798	7999.893647	9.536051	-0.071902	4.818375
358.562353	7999.922229	9.541056	-0.071875	4.818384
358.740177	7999.909899	9.546061	-0.071908	4.818380
358.763064	7999.897601	9.551066	-0.071913	4.818376
358.770240	7999.928153	9.556071	-0.071914	4.818385
358.877158	7999.889672	9.561075	-0.071934	4.818373
359.020906	7999.919946	9.566080	-0.071961	4.818382
358.977881	7999.899418	9.571085	-0.071953	4.818376
358.838236	7999.909107	9.576090	-0.071927	4.818379
359.072951	7999.922741	9.581095	-0.071970	4.818382
359.145943	7999.921615	9.586099	-0.071984	4.818382
359.309057	7999.927993	9.591104	-0.072014	4.818383
359.199320	7999.932830	9.596109	-0.071994	4.818385
359.187636	7999.932674	9.601114	-0.071992	4.818385
359.301976	7999.959405	9.606119	-0.072013	4.818392
359.143494	7999.908980	9.611123	-0.071984	4.818378
359.027095	7999.953636	9.616128	-0.071962	4.818392
359.366256	7999.999122	9.621133	-0.072025	4.818404
359.190010	7999.949509	9.626138	-0.071992	4.818390
359.605952	7999.959262	9.631143	-0.072070	4.818391
359.639660	7999.909301	9.636147	-0.072076	4.818376
359.509364	7999.934868	9.641152	-0.072052	4.818384
359.514236	7999.927581	9.646157	-0.072053	4.818382
359.449610	7999.918317	9.651162	-0.072041	4.818379
359.643217	7999.925102	9.656167	-0.072077	4.818381
359.369887	7999.910951	9.661171	-0.072026	4.818378
359.623845	7999.920643	9.666176	-0.072073	4.818379
359.783815	7999.926979	9.671181	-0.072103	4.818381
359.591292	7999.924409	9.676186	-0.072067	4.818381
359.673870	7999.953868	9.681191	-0.072082	4.818389
359.736187	7999.933695	9.686195	-0.072094	4.818383
359.759172	7999.976011	9.691200	-0.072098	4.818395
359.819384	7999.935856	9.696205	-0.072109	4.818383
359.897809	7999.924300	9.701210	-0.072124	4.818379
360.135955	7999.923279	9.706215	-0.072168	4.818378
359.977123	7999.950565	9.711219	-0.072139	4.818387
359.968147	7999.932591	9.716224	-0.072137	4.818382
360.018758	7999.918564	9.721229	-0.072147	4.818377
360.004952	7999.918379	9.726234	-0.072144	4.818377
360.330132	7999.923772	9.731239	-0.072205	4.818378
360.141669	7999.921255	9.736243	-0.072169	4.818378
360.061161	7999.913879	9.741248	-0.072154	4.818376
360.109991	7999.914531	9.746253	-0.072164	4.818376
360.334815	7999.924885	9.751258	-0.072205	4.818378
360.347569	7999.933457	9.756263	-0.072208	4.818380
360.318697	7999.911016	9.761267	-0.072202	4.818374
360.346019	7999.941838	9.766272	-0.072208	4.818383
360.382720	7999.942329	9.771277	-0.072214	4.818383
360.309134	7999.925592	9.776282	-0.072201	4.818378
360.373358	7999.922249	9.781287	-0.072213	4.818377
360.393359	7999.896260	9.786291	-0.072216	4.818369
360.196051	7999.928283	9.791296	-0.072180	4.818379
360.318746	7999.925720	9.796301	-0.072202	4.818378
360.416378	7999.920723	9.801306	-0.072221	4.818376
360.590794	7999.931454	9.806311	-0.072253	4.818379
360.423827	7999.910320	9.811315	-0.072222	4.818373
360.524618	7999.923219	9.816320	-0.072241	4.818377
360.600799	7999.924236	9.821325	-0.072255	4.818377
360.560644	7999.899544	9.826330	-0.072247	4.818369
360.399456	7999.948854	9.831335	-0.072217	4.818385
360.517925	7999.933632	9.836339	-0.072240	4.818380
360.671189	7999.947232	9.841344	-0.072268	4.818383
360.564558	7999.940556	9.846349	-0.072248	4.818382
360.505276	7999.924011	9.851354	-0.072237	4.818377
360.620802	7999.941308	9.856359	-0.072259	4.818382
360.476442	7999.898420	9.861363	-0.072232	4.818369
360.659222	7999.907162	9.866368	-0.072266	4.818371
360.543846	7999.906672	9.871373	-0.072244	4.818372
360.652197	7999.915470	9.876378	-0.072265	4.818374
360.739351	7999.932389	9.881383	-0.072281	4.818379
360.751494	7999.913646	9.886387	-0.072283	4.818373
360.904666	7999.946150	9.891392	-0.072312	4.818382
360.733651	7999.951217	9.896397	-0.072280	4.818384
360.857966	7999.949727	9.901402	-0.072303	4.818383
360.813026	7999.952277	9.906407	-0.072294	4.818384
360.760363	7999.908513	9.911411	-0.072285	4.818371
360.556679	7999.943602	9.916416	-0.072247	4.818383
360.756051	7999.920009	9.921421	-0.072284	4.818375
360.770866	7999.901302	9.926426	-0.072287	4.818369
360.797273	7999.931062	9.931431	-0.072292	4.818378
360.810639	7999.899733	9.936435	-0.072294	4.818369
360.902734	7999.934571	9.941440	-0.072311	4.818379
360.860978	7999.910908	9.946445	-0.072303	4.818372
360.742388	7999.930329	9.951450	-0.072281	4.818378
360.857417	7999.969675	9.956455	-0.072303	4.818389
360.856874	7999.915054	9.961459	-0.072303	4.818373
360.900389	7999.945043	9.966464	-0.072311	4.818382
361.016077	7999.923482	9.971469	-0.072332	4.818375
360.857659	7999.937120	9.976474	-0.072303	4.818379
360.782519	7999.960272	9.981479	-0.072289	4.818387
360.904490	7999.917790	9.986483	-0.072312	4.818374
360.964975	7999.934352	9.991488	-0.072323	4.818378
361.074658	7999.929516	9.996493	-0.072343	4.818376
360.894014	7999.946008	10.001498	-0.072310	4.818382
361.045234	7999.944877	10.006503	-0.072338	4.818381
360.971528	7999.917636	10.011507	-0.072324	4.818373
361.018174	7999.921410	10.016512	-0.072333	4.818374
361.180348	7999.926727	10.021517	-0.072363	4.818375
361.137070	7999.933501	10.026522	-0.072355	4.818377
361.147850	7999.959902	10.031527	-0.072357	4.818385
361.082260	7999.911763	10.036531	-0.072345	4.818371
361.268668	7999.946812	10.041536	-0.072379	4.818381
361.234425	7999.954757	10.046541	-0.072373	4.818383
360.972743	7999.928155	10.051546	-0.072324	4.818376
361.279000	7999.965855	10.056551	-0.072381	4.818386
361.240966	7999.926487	10.061555	-0.072374	4.818375
361.096138	7999.949758	10.066560	-0.072347	4.818382
361.241422	7999.938046	10.071565	-0.072374	4.818378
361.359114	7999.942769	10.076570	-0.072396	4.818379
361.291499	7999.949218	10.081575	-0.072384	4.818381
361.153116	7999.912710	10.086579	-0.072358	4.818371
361.236970	7999.936936	10.091584	-0.072373	4.818378
361.295965	7999.937725	10.096589	-0.072384	4.818378
361.204495	7999.933352	10.101594	-0.072367	4.818377
361.425038	7999.961505	10.106599	-0.072408	4.818384
361.379764	7999.939895	10.111603	-0.072400	4.818378
361.291636	7999.938717	10.116608	-0.072384	4.818378
361.227453	7999.945211	10.121613	-0.072372	4.818380
361.352819	7999.935333	10.126618	-0.072395	4.818377
361.361861	7999.949108	10.131623	-0.072397	4.818381
361.266222	7999.931026	10.136627	-0.072379	4.818376
361.314672	7999.950578	10.141632	-0.072388	4.818382
361.431347	7999.923780	10.146637	-0.072410	4.818373
361.138339	7999.917764	10.151642	-0.072355	4.818373
361.416872	7999.949843	10.156647	-0.072407	4.818381
361.386648	7999.909529	10.161651	-0.072401	4.818369
361.264390	7999.921549	10.166656	-0.072379	4.818373
361.336790	7999.909913	10.171661	-0.072392	4.818369
361.418200	7999.921503	10.176666	-0.072407	4.818373
361.369196	7999.925050	10.181671	-0.072398	4.818374
361.267404	7999.927891	10.186675	-0.072379	4.818375
361.475468	7999.921218	10.191680	-0.072418	4.818372
361.688716	7999.937722	10.196685	-0.072458	4.818376
361.513019	7999.925921	10.201690	-0.072425	4.818374
361.628160	7999.955818	10.206695	-0.072446	4.818382
361.405157	7999.933932	10.211699	-0.072405	4.818376
361.503200	7999.976203	10.216704	-0.072423	4.818389
361.616480	7999.938857	10.221709	-0.072444	4.818377
361.459101	7999.917849	10.226714	-0.072415	4.818371
361.553745	7999.957974	10.231719	-0.072432	4.818383
361.491143	7999.924579	10.236723	-0.072421	4.818373
361.521172	7999.937583	10.241728	-0.072426	4.818377
361.608602	7999.935601	10.246733	-0.072443	4.818376
361.447680	7999.923998	10.251738	-0.072413	4.818373
361.664992	7999.939505	10.256743	-0.072453	4.818377
361.599075	7999.924971	10.261747	-0.072441	4.818373
361.579395	7999.956216	10.266752	-0.072437	4.818382
361.606189	7999.942921	10.271757	-0.072442	4.818378
361.452325	7999.928261	10.276762	-0.072414	4.818374
361.608951	7999.961863	10.281767	-0.072443	4.818384
361.421539	7999.936252	10.286771	-0.072408	4.818377
361.418367	7999.974020	10.291776	-0.072407	4.818388
361.684375	7999.976524	10.296781	-0.072457	4.818388
361.445447	7999.938672	10.301786	-0.072412	4.818378
361.411242	7999.958170	10.306791	-0.072406	4.818384
361.551986	7999.941146	10.311795	-0.072432	4.818378
361.425802	7999.952063	10.316800	-0.072409	4.818382
361.438707	7999.977442	10.321805	-0.072411	4.818389
361.442705	7999.950189	10.326810	-0.072412	4.818381
361.618010	7999.931526	10.331815	-0.072444	4.818375
361.570757	7999.928794	10.336819	-0.072436	4.818374
361.597524	7999.960660	10.341824	-0.072441	4.818384
361.851069	7999.946194	10.346829	-0.072488	4.818378
361.665836	7999.934265	10.351834	-0.072453	4.818375
361.766194	7999.951361	10.356839	-0.072472	4.818380
361.863461	7999.930605	10.361843	-0.072490	4.818374
361.833073	7999.944903	10.366848	-0.072484	4.818378
361.624219	7999.959966	10.371853	-0.072446	4.818383
361.730584	7999.937231	10.376858	-0.072465	4.818376
361.761941	7999.982813	10.381863	-0.072471	4.818389
361.794527	7999.946488	10.386867	-0.072477	4.818379
361.671128	7999.962694	10.391872	-0.072454	4.818384
361.809402	7999.955089	10.396877	-0.072480	4.818381
361.714323	7999.926511	10.401882	-0.072462	4.818373
361.826893	7999.957424	10.406887	-0.072483	4.818382
361.769987	7999.928305	10.411891	-0.072473	4.818373
361.768499	7999.963995	10.416896	-0.072472	4.818384
361.690285	7999.959799	10.421901	-0.072458	4.818383
361.710758	7999.948520	10.426906	-0.072462	4.818379
361.846320	7999.952432	10.431911	-0.072487	4.818380
361.699881	7999.942072	10.436915	-0.072460	4.818378
361.708937	7999.944294	10.441920	-0.072461	4.818378
361.659903	7999.948890	10.446925	-0.072452	4.818380
361.760273	7999.917673	10.451930	-0.072471	4.818370
361.653110	7999.958252	10.456935	-0.072451	4.818383
361.843610	7999.947144	10.461939	-0.072486	4.818379
361.736670	7999.968821	10.466944	-0.072467	4.818385
361.833923	7999.952266	10.471949	-0.072485	4.818380
361.778392	7999.949424	10.476954	-0.072474	4.818379
361.884312	7999.979197	10.481959	-0.072494	4.818388
361.930422	7999.926249	10.486963	-0.072503	4.818372
361.735338	7999.966703	10.491968	-0.072466	4.818385
361.784993	7999.978920	10.496973	-0.072476	4.818388
361.859196	7999.953654	10.501978	-0.072489	4.818380
361.846119	7999.961882	10.506983	-0.072487	4.818383
361.814382	7999.949905	10.511987	-0.072481	4.818379
362.072814	7999.923951	10.516992	-0.072529	4.818371
361.905099	7999.921709	10.521997	-0.072498	4.818371
361.823593	7999.937424	10.527002	-0.072483	4.818376
361.867732	7999.961121	10.532007	-0.072491	4.818383
361.876136	7999.940227	10.537011	-0.072492	4.818376
361.787354	7999.961097	10.542016	-0.072476	4.818383
361.789525	7999.969528	10.547021	-0.072476	4.818385
361.946764	7999.932769	10.552026	-0.072506	4.818374
361.783418	7999.947390	10.557031	-0.072475	4.818379
361.884847	7999.920388	10.562035	-0.072494	4.818370
361.938043	7999.946306	10.567040	-0.072504	4.818378
362.021993	7999.943227	10.572045	-0.072520	4.818377
361.838296	7999.904012	10.577050	-0.072485	4.818366
361.949396	7999.958011	10.582055	-0.072506	4.818381
361.999569	7999.934525	10.587059	-0.072515	4.818374
361.838894	7999.934478	10.592064	-0.072486	4.818375
361.810388	7999.942499	10.597069	-0.072480	4.818377
361.988739	7999.914425	10.602074	-0.072513	4.818368
361.832276	7999.938591	10.607079	-0.072484	4.818376
361.858513	7999.927388	10.612083	-0.072489	4.818373
361.942951	7999.964227	10.617088	-0.072505	4.818383
361.971288	7999.952002	10.622093	-0.072510	4.818379
362.023005	7999.913833	10.627098	-0.072520	4.818368
362.087649	7999.939904	10.632103	-0.072532	4.818375
361.935435	7999.932618	10.637107	-0.072503	4.818374
361.876630	7999.944435	10.642112	-0.072493	4.818378
361.921903	7999.958694	10.647117	-0.072501	4.818382
361.969542	7999.940426	10.652122	-0.072510	4.818376
362.041483	7999.947689	10.657127	-0.072523	4.818378
361.916210	7999.922908	10.662131	-0.072500	4.818371
362.243877	7999.951445	10.667136	-0.072561	4.818378
362.184802	7999.958007	10.672141	-0.072550	4.818380
361.982043	7999.953196	10.677146	-0.072512	4.818380
362.153208	7999.972289	10.682151	-0.072544	4.818385
362.146378	7999.924934	10.687155	-0.072543	4.818371
361.966357	7999.965590	10.692160	-0.072509	4.818384
362.246009	7999.947272	10.697165	-0.072561	4.818377
362.190800	7999.942333	10.702170	-0.072551	4.818376
362.241424	7999.954563	10.707175	-0.072560	4.818379
362.301358	7999.941710	10.712179	-0.072572	4.818375
362.263083	7999.948551	10.717184	-0.072565	4.818377
362.120723	7999.932994	10.722189	-0.072538	4.818373
362.083534	7999.944050	10.727194	-0.072531	4.818377
362.167698	7999.954628	10.732199	-0.072547	4.818379
362.091274	7999.917896	10.737203	-0.072533	4.818369
362.204601	7999.949870	10.742208	-0.072554	4.818378
362.160491	7999.939827	10.747213	-0.072545	4.818375
362.050031	7999.919445	10.752218	-0.072525	4.818369
362.200958	7999.957173	10.757223	-0.072553	4.818380
361.914771	7999.926040	10.762227	-0.072500	4.818372
362.017020	7999.964167	10.767232	-0.072519	4.818383
362.228047	7999.956485	10.772237	-0.072558	4.818380
362.095678	7999.930559	10.777242	-0.072533	4.818373
362.193430	7999.981229	10.782247	-0.072552	4.818387
362.287111	7999.944671	10.787251	-0.072569	4.818376
362.216160	7999.923767	10.792256	-0.072556	4.818370
362.223129	7999.945916	10.797261	-0.072557	4.818377
362.035273	7999.942355	10.802266	-0.072522	4.818376
362.196801	7999.960268	10.807271	-0.072552	4.818381
362.095771	7999.932660	10.812275	-0.072533	4.818373
362.259257	7999.960053	10.817280	-0.072564	4.818381
362.345402	7999.943350	10.822285	-0.072580	4.818375
362.350471	7999.917160	10.827290	-0.072581	4.818368
362.216545	7999.946879	10.832295	-0.072556	4.818377
362.192132	7999.938150	10.837299	-0.072551	4.818374
362.159947	7999.956625	10.842304	-0.072545	4.818380
362.182697	7999.961130	10.847309	-0.072550	4.818381
362.124516	7999.951950	10.852314	-0.072539	4.818379
362.306323	7999.954381	10.857319	-0.072573	4.818379
362.250977	7999.921081	10.862323	-0.072562	4.818369
362.031447	7999.954907	10.867328	-0.072521	4.818380
362.318655	7999.940892	10.872333	-0.072575	4.818375
362.314719	7999.957644	10.877338	-0.072574	4.818380
362.172045	7999.964139	10.882343	-0.072548	4.818382
362.321553	7999.928327	10.887347	-0.072575	4.818371
362.320312	7999.968222	10.892352	-0.072575	4.818383
362.126410	7999.933070	10.897357	-0.072539	4.818373
362.205040	7999.915216	10.902362	-0.072554	4.818368
362.180085	7999.919084	10.907367	-0.072549	4.818369
362.123133	7999.940378	10.912371	-0.072538	4.818375
362.076538	7999.974415	10.917376	-0.072530	4.818386
362.212446	7999.954176	10.922381	-0.072555	4.818379
362.126676	7999.945677	10.927386	-0.072539	4.818377
362.373347	7999.948975	10.932391	-0.072585	4.818377
362.426671	7999.930782	10.937395	-0.072595	4.818371
362.320076	7999.958766	10.942400	-0.072575	4.818380
362.299095	7999.942731	10.947405	-0.072571	4.818375
362.128050	7999.948847	10.952410	-0.072539	4.818378
362.089186	7999.981937	10.957415	-0.072532	4.818388
362.175575	7999.970488	10.962419	-0.072548	4.818384
362.045323	7999.976099	10.967424	-0.072524	4.818386
362.508631	7999.956035	10.972429	-0.072610	4.818379
362.137021	7999.952117	10.977434	-0.072541	4.818379
362.275185	7999.968669	10.982439	-0.072567	4.818383
362.242148	7999.946171	10.987443	-0.072561	4.818377
362.109783	7999.979061	10.992448	-0.072536	4.818387
362.397269	7999.975552	10.997453	-0.072590	4.818385
362.399538	7999.948275	11.002458	-0.072590	4.818377
362.352089	7999.979150	11.007463	-0.072581	4.818386
362.186865	7999.939130	11.012467	-0.072550	4.818375
362.110669	7999.964369	11.017472	-0.072536	4.818383
362.483214	7999.963048	11.022477	-0.072606	4.818381
362.387559	7999.949165	11.027482	-0.072588	4.818377
362.399867	7999.943028	11.032487	-0.072590	4.818375
362.581403	7999.925499	11.037491	-0.072624	4.818369
362.387428	7999.978572	11.042496	-0.072588	4.818386
362.476896	7999.955611	11.047501	-0.072604	4.818379
362.324522	7999.956725	11.052506	-0.072576	4.818379
362.334189	7999.971558	11.057511	-0.072578	4.818384
362.401180	7999.940945	11.062515	-0.072590	4.818374
362.389863	7999.962850	11.067520	-0.072588	4.818381
362.532913	7999.945857	11.072525	-0.072615	4.818375
362.504331	7999.952827	11.077530	-0.072609	4.818378
362.496929	7999.971634	11.082535	-0.072608	4.818383
362.531859	7999.946893	11.087539	-0.072615	4.818376
362.209043	7999.954131	11.092544	-0.072554	4.818379
362.468604	7999.964953	11.097549	-0.072603	4.818381
362.225280	7999.948046	11.102554	-0.072557	4.818377
362.346860	7999.949671	11.107559	-0.072580	4.818377
362.533984	7999.937469	11.112563	-0.072615	4.818373
362.516616	7999.951941	11.117568	-0.072612	4.818377
362.415466	7999.973695	11.122573	-0.072593	4.818384
362.560793	7999.934677	11.127578	-0.072620	4.818372
362.512876	7999.971847	11.132583	-0.072611	4.818383
362.365586	7999.942570	11.137587	-0.072584	4.818375
362.421702	7999.972728	11.142592	-0.072594	4.818384
362.534247	7999.965831	11.147597	-0.072615	4.818381
362.369960	7999.957332	11.152602	-0.072584	4.818379
362.596619	7999.989772	11.157607	-0.072627	4.818388
362.536291	7999.942751	11.162611	-0.072615	4.818374
362.543769	7999.969109	11.167616	-0.072617	4.818382
362.236198	7999.947142	11.172621	-0.072560	4.818377
362.342862	7999.966423	11.177626	-0.072579	4.818382
362.630068	7999.968162	11.182631	-0.072633	4.818382
362.405246	7999.942050	11.187635	-0.072591	4.818375
362.658871	7999.964346	11.192640	-0.072638	4.818380
362.606777	7999.982555	11.197645	-0.072629	4.818386
362.518593	7999.975074	11.202650	-0.072612	4.818384
362.544233	7999.999574	11.207655	-0.072617	4.818391
362.455362	7999.963726	11.212659	-0.072600	4.818381
362.322010	7999.949339	11.217664	-0.072576	4.818377
362.405199	7999.998766	11.222669	-0.072591	4.818392
362.678832	7999.963563	11.227674	-0.072642	4.818380
362.828500	7999.971866	11.232679	-0.072670	4.818382
362.441881	7999.951992	11.237683	-0.072598	4.818378
362.502258	7999.962252	11.242688	-0.072609	4.818380
362.599800	7999.953054	11.247693	-0.072627	4.818377
362.652532	7999.924350	11.252698	-0.072637	4.818369
362.537751	7999.985834	11.257703	-0.072616	4.818387
362.700859	7999.956505	11.262707	-0.072646	4.818378
362.650298	7999.955829	11.267712	-0.072637	4.818378
362.573630	7999.959005	11.272717	-0.072622	4.818379
362.711103	7999.948240	11.277722	-0.072648	4.818375
362.795231	7999.976673	11.282727	-0.072664	4.818384
362.495028	7999.945351	11.287731	-0.072608	4.818375
362.662205	7999.988548	11.292736	-0.072639	4.818388
362.794734	7999.968264	11.297741	-0.072664	4.818381
362.626125	7999.959707	11.302746	-0.072632	4.818379
362.546800	7999.973351	11.307751	-0.072617	4.818384
362.693793	7999.952210	11.312755	-0.072645	4.818377
362.640075	7999.970397	11.317760	-0.072635	4.818382
362.654166	7999.986340	11.322765	-0.072637	4.818387
362.667950	7999.947663	11.327770	-0.072640	4.818375
362.756953	7999.975111	11.332775	-0.072657	4.818383
362.561118	7999.975643	11.337779	-0.072620	4.818384
362.675467	7999.962468	11.342784	-0.072641	4.818380
362.732752	7999.957982	11.347789	-0.072652	4.818378
362.696478	7999.939642	11.352794	-0.072645	4.818373
362.702595	7999.980686	11.357799	-0.072646	4.818385
362.878387	7999.972534	11.362803	-0.072679	4.818382
362.681171	7999.970947	11.367808	-0.072642	4.818382
362.752604	7999.988707	11.372813	-0.072656	4.818387
362.559582	7999.971422	11.377818	-0.072620	4.818383
362.869406	7999.970313	11.382823	-0.072677	4.818381
362.797115	7999.935736	11.387827	-0.072664	4.818371
362.861325	7999.973356	11.392832	-0.072676	4.818382
362.852458	7999.961684	11.397837	-0.072674	4.818379
362.660659	7999.931811	11.402842	-0.072639	4.818371
362.763448	7999.987802	11.407847	-0.072658	4.818387
362.736632	7999.969588	11.412851	-0.072653	4.818382
362.724887	7999.971531	11.417856	-0.072651	4.818382
362.664210	7999.971770	11.422861	-0.072639	4.818383
362.605455	7999.939475	11.427866	-0.072628	4.818373
362.808362	7999.998906	11.432871	-0.072666	4.818390
362.709495	7999.959772	11.437875	-0.072648	4.818379
362.752158	7999.956141	11.442880	-0.072656	4.818378
362.875613	7999.960943	11.447885	-0.072679	4.818379
362.744334	7999.945534	11.452890	-0.072654	4.818374
362.768148	7999.975261	11.457895	-0.072659	4.818383
362.887729	7999.956904	11.462899	-0.072681	4.818377
362.850529	7999.971111	11.467904	-0.072674	4.818382
362.856349	7999.984843	11.472909	-0.072675	4.818386
362.906029	7999.982356	11.477914	-0.072684	4.818385
362.878300	7999.985137	11.482919	-0.072679	4.818386
362.752575	7999.969801	11.487923	-0.072656	4.818382
362.764503	7999.982564	11.492928	-0.072658	4.818385
362.838085	7999.969894	11.497933	-0.072672	4.818381
362.702791	7999.963884	11.502938	-0.072646	4.818380
362.876433	7999.978810	11.507943	-0.072679	4.818384
362.716804	7999.949367	11.512947	-0.072649	4.818376
362.917570	7999.946800	11.517952	-0.072686	4.818374
362.839555	7999.960461	11.522957	-0.072672	4.818379
362.654501	7999.942232	11.527962	-0.072637	4.818374
362.945720	7999.972384	11.532967	-0.072692	4.818382
362.815156	7999.954883	11.537971	-0.072667	4.818377
362.830177	7999.951933	11.542976	-0.072670	4.818376
362.784815	7999.955528	11.547981	-0.072662	4.818377
362.869590	7999.926203	11.552986	-0.072677	4.818368
362.794075	7999.936746	11.557991	-0.072663	4.818372
362.789951	7999.961899	11.562995	-0.072663	4.818379
362.876519	7999.989314	11.568000	-0.072679	4.818387
362.764520	7999.959458	11.573005	-0.072658	4.818379
362.924433	7999.944791	11.578010	-0.072688	4.818374
363.190910	7999.963060	11.583015	-0.072737	4.818378
362.887004	7999.956895	11.588019	-0.072681	4.818377
362.682149	7999.952055	11.593024	-0.072643	4.818377
362.968502	7999.965337	11.598029	-0.072696	4.818379
362.813100	7999.963259	11.603034	-0.072667	4.818379
362.997196	7999.993029	11.608039	-0.072701	4.818388
362.877699	7999.934714	11.613043	-0.072679	4.818371
362.895199	7999.942300	11.618048	-0.072682	4.818373
363.025145	7999.971346	11.623053	-0.072706	4.818381
362.736709	7999.953835	11.628058	-0.072653	4.818377
363.035543	7999.964133	11.633063	-0.072708	4.818379
362.970573	7999.948559	11.638067	-0.072696	4.818374
362.799550	7999.948373	11.643072	-0.072664	4.818375
362.941572	7999.955524	11.648077	-0.072691	4.818377
362.950795	7999.939892	11.653082	-0.072693	4.818372
362.855082	7999.950166	11.658087	-0.072675	4.818375
362.910020	7999.942498	11.663091	-0.072685	4.818373
363.122504	7999.945340	11.668096	-0.072725	4.818373
363.016099	7999.956521	11.673101	-0.072705	4.818377
362.946174	7999.949284	11.678106	-0.072692	4.818375
363.108979	7999.984021	11.683111	-0.072722	4.818384
363.060665	7999.955016	11.688115	-0.072713	4.818376
362.954077	7999.958842	11.693120	-0.072693	4.818378
362.923481	7999.957383	11.698125	-0.072688	4.818377
363.060872	7999.940314	11.703130	-0.072713	4.818372
363.008029	7999.962715	11.708135	-0.072703	4.818379
363.041949	7999.942162	11.713139	-0.072710	4.818372
363.014955	7999.952304	11.718144	-0.072705	4.818375
363.224404	7999.961407	11.723149	-0.072744	4.818377
363.062481	7999.936135	11.728154	-0.072713	4.818370
363.074652	7999.954153	11.733159	-0.072716	4.818376
363.204510	7999.948537	11.738163	-0.072740	4.818374
363.013045	7999.935474	11.743168	-0.072704	4.818370
363.304189	7999.949871	11.748173	-0.072758	4.818374
363.251333	7999.946013	11.753178	-0.072749	4.818373
363.086022	7999.960607	11.758183	-0.072718	4.818378
363.119980	7999.958960	11.763187	-0.072724	4.818377
363.163894	7999.972152	11.768192	-0.072732	4.818381
363.124542	7999.965323	11.773197	-0.072725	4.818379
362.944929	7999.949267	11.778202	-0.072692	4.818375
363.057801	7999.961280	11.783207	-0.072713	4.818378
363.186699	7999.930444	11.788211	-0.072737	4.818368
363.083035	7999.959517	11.793216	-0.072717	4.818377
362.986948	7999.979238	11.798221	-0.072699	4.818384
363.071063	7999.928897	11.803226	-0.072715	4.818368
362.871105	7999.954582	11.808231	-0.072678	4.818377
363.087656	7999.933320	11.813235	-0.072718	4.818369
363.124056	7999.960065	11.818240	-0.072725	4.818377
363.275498	7999.977846	11.823245	-0.072753	4.818382
363.022712	7999.947156	11.828250	-0.072706	4.818374
363.035980	7999.966240	11.833255	-0.072708	4.818379
363.205839	7999.931750	11.838259	-0.072740	4.818369
362.918068	7999.948908	11.843264	-0.072687	4.818375
363.013945	7999.951240	11.848269	-0.072704	4.818375
363.333855	7999.950268	11.853274	-0.072764	4.818374
363.101813	7999.966070	11.858279	-0.072721	4.818379
362.945015	7999.951369	11.863283	-0.072692	4.818375
362.980075	7999.979146	11.868288	-0.072698	4.818384
363.045912	7999.993681	11.873293	-0.072710	4.818388
362.973422	7999.955950	11.878298	-0.072697	4.818377
363.074858	7999.986716	11.883303	-0.072716	4.818385
362.960019	7999.967324	11.888307	-0.072694	4.818380
362.973548	7999.971707	11.893312	-0.072697	4.818381
362.892753	7999.993733	11.898317	-0.072682	4.818388
363.006978	7999.971103	11.903322	-0.072703	4.818381
363.073569	8000.009806	11.908327	-0.072715	4.818392
362.987661	7999.965594	11.913331	-0.072699	4.818379
362.871859	7999.981900	11.918336	-0.072678	4.818385
362.906964	8000.011779	11.923341	-0.072684	4.818393
362.986172	7999.941416	11.928346	-0.072699	4.818372
363.087740	7999.979536	11.933351	-0.072718	4.818383
363.316026	7999.958432	11.938355	-0.072761	4.818376
363.139869	7999.965529	11.943360	-0.072728	4.818379
363.057838	7999.966532	11.948365	-0.072713	4.818379
363.180413	7999.960819	11.953370	-0.072735	4.818377
363.037652	7999.992520	11.958375	-0.072709	4.818387
363.040332	7999.952644	11.963379	-0.072709	4.818375
363.044460	7999.970555	11.968384	-0.072710	4.818381
363.283902	7999.981109	11.973389	-0.072755	4.818383
363.081527	7999.956346	11.978394	-0.072717	4.818376
363.205412	7999.958003	11.983399	-0.072740	4.818376
363.081850	7999.938495	11.988403	-0.072717	4.818371
363.044905	7999.954806	11.993408	-0.072710	4.818376
363.184074	7999.953516	11.998413	-0.072736	4.818375
363.134700	7999.965460	12.003418	-0.072727	4.818379
363.220840	7999.972914	12.008423	-0.072743	4.818381
363.173728	7999.944975	12.013427	-0.072734	4.818373
363.078796	7999.948957	12.018432	-0.072716	4.818374
363.184339	7999.996583	12.023437	-0.072736	4.818388
363.241019	7999.955328	12.028442	-0.072747	4.818375
363.158140	7999.981528	12.033447	-0.072731	4.818384
363.138980	7999.953963	12.038451	-0.072728	4.818375
363.179630	7999.963960	12.043456	-0.072735	4.818378
363.384607	7999.963551	12.048461	-0.072773	4.818377
363.242197	7999.939589	12.053466	-0.072747	4.818371
363.125583	8000.023106	12.058471	-0.072725	4.818396
363.178821	7999.999660	12.063475	-0.072735	4.818389
363.134161	7999.989610	12.068480	-0.072727	4.818386
363.350755	8000.000910	12.073485	-0.072767	4.818389
363.352811	7999.974679	12.078490	-0.072767	4.818381
363.368603	7999.968588	12.083495	-0.072770	4.818379
363.335239	7999.979696	12.088499	-0.072764	4.818382
363.290718	7999.974899	12.093504	-0.072756	4.818381
363.043937	7999.972648	12.098509	-0.072710	4.818381
363.063045	7999.962401	12.103514	-0.072714	4.818378
363.161052	7999.970014	12.108519	-0.072732	4.818380
363.074582	7999.966756	12.113523	-0.072716	4.818379
363.095254	7999.958630	12.118528	-0.072720	4.818377
363.232109	7999.997222	12.123533	-0.072745	4.818388
363.156962	7999.969959	12.128538	-0.072731	4.818380
363.228338	7999.981417	12.133543	-0.072744	4.818383
363.274181	7999.967325	12.138547	-0.072753	4.818379
363.289004	7999.961222	12.143552	-0.072756	4.818377
363.499594	7999.966139	12.148557	-0.072795	4.818378
363.241679	7999.956388	12.153562	-0.072747	4.818376
363.291324	7999.986461	12.158567	-0.072756	4.818384
363.489275	7999.979656	12.163571	-0.072793	4.818382
363.388648	7999.979360	12.168576	-0.072774	4.818382
363.273973	8000.003034	12.173581	-0.072753	4.818389
363.311237	7999.969922	12.178586	-0.072760	4.818379
363.243108	8000.011024	12.183591	-0.072747	4.818392
363.189990	7999.932589	12.188595	-0.072737	4.818369
363.316391	7999.948984	12.193600	-0.072761	4.818373
363.354013	7999.948437	12.198605	-0.072768	4.818373
363.331804	7999.938687	12.203610	-0.072764	4.818370
363.477728	7999.998407	12.208615	-0.072791	4.818387
363.426624	7999.980918	12.213619	-0.072781	4.818382
363.110503	7999.976690	12.218624	-0.072722	4.818382
363.267818	7999.963039	12.223629	-0.072752	4.818378
363.041313	7999.953708	12.228634	-0.072709	4.818376
363.072970	7999.958333	12.233639	-0.072715	4.818377
362.918939	7999.968876	12.238643	-0.072687	4.818381
363.141555	7999.988659	12.243648	-0.072728	4.818386
363.036088	8000.038714	12.248653	-0.072709	4.818401
362.689014	8000.000462	12.253658	-0.072644	4.818391
363.155411	7999.988844	12.258663	-0.072731	4.818386
362.985142	8000.020177	12.263667	-0.072699	4.818396
362.517594	8000.068541	12.268672	-0.072612	4.818412
362.696037	8000.066726	12.273677	-0.072645	4.818411
363.112767	7999.993525	12.278682	-0.072723	4.818387
362.864601	8000.042722	12.283687	-0.072677	4.818403
362.854212	8000.001621	12.288691	-0.072675	4.818391
362.923635	8000.024606	12.293696	-0.072688	4.818397
363.116955	8000.046098	12.298701	-0.072724	4.818403
362.917495	8000.011920	12.303706	-0.072686	4.818393
362.850596	8000.030982	12.308711	-0.072674	4.818399
362.924689	7999.984708	12.313715	-0.072688	4.818385
362.879376	8000.004058	12.318720	-0.072679	4.818391
363.081688	8000.008865	12.323725	-0.072717	4.818392
363.181866	7999.957688	12.328730	-0.072736	4.818376
363.165348	7999.998430	12.333735	-0.072733	4.818389
363.380162	7999.964542	12.338739	-0.072773	4.818378
363.381719	7999.983469	12.343744	-0.072773	4.818383
363.473146	7999.977340	12.348749	-0.072790	4.818381
363.408359	7999.961768	12.353754	-0.072778	4.818377
363.305078	7999.970890	12.358759	-0.072759	4.818380
363.431906	7999.977838	12.363763	-0.072782	4.818381
363.169571	7999.973279	12.368768	-0.072733	4.818381
363.197631	7999.972604	12.373773	-0.072739	4.818381
363.179501	7999.957657	12.378778	-0.072735	4.818376
362.971172	7999.994783	12.383783	-0.072696	4.818388
363.167689	7999.971153	12.388787	-0.072733	4.818380
363.079511	7999.992031	12.393792	-0.072717	4.818387
363.198550	8000.008327	12.398797	-0.072739	4.818391
363.126053	7999.972697	12.403802	-0.072725	4.818381
363.199567	8000.016744	12.408807	-0.072739	4.818394
363.354716	7999.993611	12.413811	-0.072768	4.818386
363.254845	8000.001728	12.418816	-0.072749	4.818389
363.152508	8000.018215	12.423821	-0.072730	4.818394
363.293396	7999.974935	12.428826	-0.072756	4.818381
363.099782	7999.992302	12.433831	-0.072720	4.818387
363.207989	7999.974843	12.438835	-0.072741	4.818381
363.085330	7999.981605	12.443840	-0.072718	4.818384
363.302983	8000.004473	12.448845	-0.072758	4.818390
362.996953	8000.014034	12.453850	-0.072701	4.818394
363.507925	7999.991459	12.458855	-0.072796	4.818385
363.452269	7999.971809	12.463859	-0.072786	4.818379
363.322571	7999.976376	12.468864	-0.072762	4.818381
363.326607	8000.013191	12.473869	-0.072763	4.818392
363.436450	7999.947440	12.478874	-0.072783	4.818372
363.541236	7999.986653	12.483879	-0.072803	4.818384
363.444440	7999.969604	12.488883	-0.072785	4.818379
363.354674	7999.979956	12.493888	-0.072768	4.818382
363.376606	7999.956092	12.498893	-0.072772	4.818375
363.313683	7999.939496	12.503898	-0.072760	4.818370
363.328945	7999.964908	12.508903	-0.072763	4.818378
363.511343	7999.948442	12.513907	-0.072797	4.818372
363.459334	7999.957199	12.518912	-0.072787	4.818375
363.382044	8000.010782	12.523917	-0.072773	4.818391
363.358150	7999.988406	12.528922	-0.072768	4.818385
363.488927	8000.012212	12.533927	-0.072793	4.818391
363.549405	7999.971008	12.538931	-0.072804	4.818379
363.371757	7999.962329	12.543936	-0.072771	4.818377
363.351579	7999.986217	12.548941	-0.072767	4.818384
363.392739	7999.947906	12.553946	-0.072775	4.818373
363.568930	7999.968118	12.558951	-0.072808	4.818378
363.592874	7999.975791	12.563955	-0.072812	4.818380
363.357340	7999.993646	12.568960	-0.072768	4.818386
363.267188	8000.001893	12.573965	-0.072752	4.818389
363.329208	7999.954408	12.578970	-0.072763	4.818375
363.587790	7999.997780	12.583975	-0.072811	4.818387
363.558765	7999.959579	12.588979	-0.072806	4.818375
363.429093	7999.971499	12.593984	-0.072782	4.818379
363.544215	7999.991945	12.598989	-0.072803	4.818385
363.491896	7999.954484	12.603994	-0.072793	4.818374
363.235984	8000.016181	12.608999	-0.072746	4.818393
363.300277	7999.992883	12.614003	-0.072758	4.818386
363.468379	8000.003535	12.619008	-0.072789	4.818389
363.572436	7999.981819	12.624013	-0.072808	4.818382
363.450923	7999.990697	12.629018	-0.072786	4.818385
363.762701	8000.000120	12.634023	-0.072844	4.818387
363.660929	7999.997708	12.639027	-0.072825	4.818386
363.625456	7999.982529	12.644032	-0.072818	4.818382
363.600771	7999.991652	12.649037	-0.072814	4.818385
363.553164	7999.947951	12.654042	-0.072805	4.818372
363.600738	7999.970644	12.659047	-0.072814	4.818379
363.702221	7999.958348	12.664051	-0.072833	4.818374
363.684792	7999.967568	12.669056	-0.072829	4.818377
363.600071	7999.981139	12.674061	-0.072814	4.818382
363.581757	7999.966189	12.679066	-0.072810	4.818377
363.669443	7999.981017	12.684071	-0.072826	4.818381
363.706577	7999.955255	12.689075	-0.072833	4.818374
363.596163	7999.951677	12.694080	-0.072813	4.818373
363.758987	7999.995869	12.699085	-0.072843	4.818385
363.477946	7999.961650	12.704090	-0.072791	4.818376
363.571338	7999.962899	12.709095	-0.072808	4.818376
363.471908	8000.024589	12.714099	-0.072790	4.818395
363.600252	7999.994796	12.719104	-0.072814	4.818386
363.580238	8000.069102	12.724109	-0.072810	4.818408
363.355836	7999.990476	12.729114	-0.072768	4.818385
363.492997	8000.016468	12.734119	-0.072794	4.818393
363.467679	8000.019280	12.739123	-0.072789	4.818393
362.760872	8000.057091	12.744128	-0.072657	4.818408
363.032469	8000.072277	12.749133	-0.072708	4.818411
363.223073	7999.993951	12.754138	-0.072743	4.818387
363.342665	8000.032313	12.759143	-0.072766	4.818398
363.406574	7999.983802	12.764147	-0.072778	4.818383
363.200733	8000.006257	12.769152	-0.072739	4.818391
363.388844	8000.033981	12.774157	-0.072774	4.818398
363.249550	7999.973299	12.779162	-0.072748	4.818381
363.377172	8000.067435	12.784167	-0.072772	4.818408
362.876069	8000.166815	12.789171	-0.072679	4.818440
362.778480	8000.106691	12.794176	-0.072661	4.818422
362.974927	8000.103017	12.799181	-0.072697	4.818420
362.958728	8000.075492	12.804186	-0.072694	4.818412
363.275215	8000.034561	12.809191	-0.072753	4.818399
363.315067	8000.018289	12.814195	-0.072760	4.818394
363.389634	8000.016136	12.819200	-0.072774	4.818393
363.382007	8000.031789	12.824205	-0.072773	4.818398
363.402257	7999.979543	12.829210	-0.072777	4.818382
363.440651	7999.990560	12.834215	-0.072784	4.818385
363.544730	7999.969895	12.839219	-0.072803	4.818379
363.623515	7999.960446	12.844224	-0.072818	4.818375
363.400193	7999.992120	12.849229	-0.072776	4.818386
363.430405	7999.983071	12.854234	-0.072782	4.818383
363.517858	7999.996845	12.859239	-0.072798	4.818387
363.489136	7999.961800	12.864243	-0.072793	4.818376
363.583405	7999.989319	12.869248	-0.072810	4.818384
363.721264	7999.980660	12.874253	-0.072836	4.818381
363.417294	7999.962939	12.879258	-0.072779	4.818377
363.454047	8000.008595	12.884263	-0.072786	4.818390
363.248053	8000.037349	12.889267	-0.072748	4.818400
363.350995	7999.967304	12.894272	-0.072767	4.818379
363.244149	7999.999485	12.899277	-0.072747	4.818389
363.306365	7999.963556	12.904282	-0.072759	4.818378
363.646056	7999.992258	12.909287	-0.072822	4.818385
363.580502	7999.978777	12.914291	-0.072810	4.818381
363.510812	7999.964190	12.919296	-0.072797	4.818377
363.419725	7999.985029	12.924301	-0.072780	4.818384
363.344791	7999.942013	12.929306	-0.072766	4.818371
363.237458	8000.023553	12.934311	-0.072746	4.818396
363.645930	7999.959696	12.939315	-0.072822	4.818375
363.466915	7999.989861	12.944320	-0.072789	4.818385
363.869508	7999.996298	12.949325	-0.072864	4.818385
363.801802	7999.983838	12.954330	-0.072851	4.818382
363.622904	7999.973042	12.959335	-0.072818	4.818379
363.686661	7999.983348	12.964339	-0.072830	4.818382
363.791903	7999.959548	12.969344	-0.072849	4.818374
363.954190	7999.970122	12.974349	-0.072879	4.818377
363.498978	7999.974535	12.979354	-0.072795	4.818380
363.717960	7999.992170	12.984359	-0.072836	4.818384
363.840005	8000.010608	12.989363	-0.072858	4.818389
363.810569	7999.992358	12.994368	-0.072853	4.818384
363.808001	7999.992324	12.999373	-0.072852	4.818384
363.884371	7999.961836	13.004378	-0.072866	4.818375
363.817908	7999.968299	13.009383	-0.072854	4.818377
363.728287	7999.959747	13.014387	-0.072837	4.818375
363.746309	7999.945284	13.019392	-0.072841	4.818370
363.825518	8000.016716	13.024397	-0.072856	4.818391
363.809842	7999.996550	13.029402	-0.072853	4.818385
363.438080	8000.020986	13.034407	-0.072783	4.818394
363.725527	7999.991221	13.039411	-0.072837	4.818384
363.384980	7999.997168	13.044416	-0.072774	4.818387
363.545299	8000.016118	13.049421	-0.072803	4.818392
363.693087	7999.955075	13.054426	-0.072831	4.818374
363.789561	7999.988926	13.059431	-0.072849	4.818383
363.624398	7999.976213	13.064435	-0.072818	4.818380
363.716660	7999.978498	13.069440	-0.072835	4.818380
363.785473	8000.003577	13.074445	-0.072848	4.818388
363.819273	7999.987223	13.079450	-0.072854	4.818383
363.676860	8000.016828	13.084455	-0.072828	4.818392
363.774791	8000.016038	13.089459	-0.072846	4.818391
363.609609	7999.993871	13.094464	-0.072815	4.818385
363.675065	8000.019955	13.099469	-0.072828	4.818393
363.607724	7999.978091	13.104474	-0.072815	4.818381
363.757673	7999.995852	13.109479	-0.072843	4.818385
363.827604	8000.000989	13.114483	-0.072856	4.818387
363.878588	7999.962809	13.119488	-0.072865	4.818375
364.048168	8000.015495	13.124493	-0.072897	4.818390
363.846380	7999.980234	13.129498	-0.072859	4.818380
363.730926	8000.001796	13.134503	-0.072838	4.818387
363.879607	7999.977527	13.139507	-0.072866	4.818379
363.788889	7999.967911	13.144512	-0.072849	4.818377
363.535150	8000.007580	13.149517	-0.072801	4.818390
363.522939	7999.963303	13.154522	-0.072799	4.818377
363.676858	7999.984268	13.159527	-0.072828	4.818382
363.721643	7999.980666	13.164531	-0.072836	4.818381
363.551234	7999.977335	13.169536	-0.072804	4.818381
363.756598	8000.008442	13.174541	-0.072843	4.818389
363.712277	7999.968987	13.179546	-0.072834	4.818378
363.721514	7999.994318	13.184551	-0.072836	4.818385
363.710152	7999.999418	13.189555	-0.072834	4.818387
363.787286	7999.989947	13.194560	-0.072848	4.818384
363.629985	8000.028805	13.199565	-0.072819	4.818396
363.636797	7999.983732	13.204570	-0.072820	4.818382
363.764335	7999.996992	13.209575	-0.072844	4.818386
363.775768	8000.001346	13.214579	-0.072846	4.818387
363.661237	7999.984059	13.219584	-0.072825	4.818382
363.738464	8000.037609	13.224589	-0.072839	4.818398
363.786071	7999.976276	13.229594	-0.072848	4.818379
363.766936	7999.986523	13.234599	-0.072845	4.818383
363.830907	7999.965322	13.239603	-0.072857	4.818376
363.947656	7999.970035	13.244608	-0.072878	4.818377
363.742572	8000.008255	13.249613	-0.072840	4.818389
363.617034	7999.991870	13.254618	-0.072817	4.818385
363.796166	8000.010022	13.259623	-0.072850	4.818389
363.884587	7999.994400	13.264627	-0.072867	4.818384
363.836790	7999.967502	13.269632	-0.072858	4.818377
363.875448	8000.015284	13.274637	-0.072865	4.818391
363.693390	7999.979237	13.279642	-0.072831	4.818381
363.681204	7999.980125	13.284647	-0.072829	4.818381
363.524862	8000.014795	13.289651	-0.072800	4.818392
363.659914	7999.999796	13.294656	-0.072825	4.818387
363.956423	8000.000613	13.299661	-0.072880	4.818386
363.544791	8000.001407	13.304666	-0.072803	4.818388
363.751044	8000.003116	13.309671	-0.072842	4.818388
364.067818	8000.000003	13.314675	-0.072901	4.818385
363.774008	7999.976115	13.319680	-0.072846	4.818379
363.667638	8000.014604	13.324685	-0.072826	4.818391
363.638467	7999.980603	13.329690	-0.072821	4.818381
363.645859	8000.001709	13.334695	-0.072822	4.818388
363.794485	7999.993194	13.339699	-0.072850	4.818384
363.761776	8000.004310	13.344704	-0.072844	4.818388
363.885655	8000.022773	13.349709	-0.072867	4.818393
363.906860	7999.982094	13.354714	-0.072871	4.818381
363.969696	8000.000790	13.359719	-0.072882	4.818386
364.120647	8000.009113	13.364723	-0.072911	4.818388
363.719209	7999.994288	13.369728	-0.072836	4.818385
363.851309	7999.991854	13.374733	-0.072860	4.818384
363.728563	7999.978658	13.379738	-0.072837	4.818380
363.871621	7999.988975	13.384743	-0.072864	4.818383
363.779579	7999.990894	13.389747	-0.072847	4.818384
363.881824	7999.970205	13.394752	-0.072866	4.818377
364.000701	8000.003306	13.399757	-0.072888	4.818387
363.702223	8000.078088	13.404762	-0.072833	4.818410
363.777856	8000.070697	13.409767	-0.072847	4.818408
363.727995	8000.004909	13.414771	-0.072837	4.818388
363.697964	7999.991903	13.419776	-0.072832	4.818384
363.933948	8000.009765	13.424781	-0.072876	4.818389
363.844390	7999.998063	13.429786	-0.072859	4.818386
363.833094	7999.998963	13.434791	-0.072857	4.818386
363.736200	7999.979811	13.439795	-0.072839	4.818381
363.646740	7999.970211	13.444800	-0.072822	4.818378
363.597412	7999.998960	13.449805	-0.072813	4.818387
363.648010	7999.958674	13.454810	-0.072822	4.818375
363.699451	7999.984571	13.459815	-0.072832	4.818382
363.846047	8000.009639	13.464819	-0.072859	4.818389
363.949198	7999.984761	13.469824	-0.072879	4.818381
364.030026	7999.982692	13.474829	-0.072894	4.818380
364.019848	7999.956297	13.479834	-0.072892	4.818373
364.052868	7999.968293	13.484839	-0.072898	4.818376
363.967445	7999.957696	13.489843	-0.072882	4.818373
364.055433	7999.953622	13.494848	-0.072898	4.818372
363.942692	7999.971020	13.499853	-0.072877	4.818377
363.840500	7999.961250	13.504858	-0.072858	4.818375
363.896042	7999.983000	13.509863	-0.072869	4.818381
363.991843	7999.962224	13.514867	-0.072886	4.818374
363.969928	7999.988190	13.519872	-0.072882	4.818382
363.978547	8000.010362	13.524877	-0.072884	4.818389
363.899334	7999.954685	13.529882	-0.072869	4.818373
364.014644	7999.981436	13.534887	-0.072891	4.818380
364.012007	7999.963545	13.539891	-0.072890	4.818375
363.883680	7999.935569	13.544896	-0.072866	4.818367
363.953113	7999.993216	13.549901	-0.072879	4.818384
363.821186	7999.975696	13.554906	-0.072855	4.818379
363.896425	7999.991408	13.559911	-0.072869	4.818384
364.094547	7999.965699	13.564915	-0.072906	4.818375
363.774161	7999.989772	13.569920	-0.072846	4.818384
363.850001	7999.983434	13.574925	-0.072860	4.818381
363.953882	7999.966968	13.579930	-0.072879	4.818376
363.821551	8000.005111	13.584935	-0.072855	4.818388
363.887115	7999.970276	13.589939	-0.072867	4.818377
363.910625	7999.974792	13.594944	-0.072871	4.818379
363.829890	7999.994719	13.599949	-0.072856	4.818385
363.972335	7999.948309	13.604954	-0.072883	4.818370
364.004027	7999.980243	13.609959	-0.072889	4.818380
363.954953	7999.996392	13.614963	-0.072880	4.818385
363.966294	7999.967134	13.619968	-0.072882	4.818376
364.091703	7999.975115	13.624973	-0.072905	4.818378
364.030849	7999.965898	13.629978	-0.072894	4.818375
363.814394	7999.981907	13.634983	-0.072853	4.818381
363.812814	7999.969282	13.639987	-0.072853	4.818377
363.820309	7999.968332	13.644992	-0.072855	4.818377
363.795625	8000.006864	13.649997	-0.072850	4.818389
363.816116	7999.968276	13.655002	-0.072854	4.818377
363.566077	7999.991189	13.660007	-0.072807	4.818385
363.832945	7999.980055	13.665011	-0.072857	4.818380
363.909941	7999.972682	13.670016	-0.072871	4.818378
363.831754	7999.990542	13.675021	-0.072857	4.818384
363.757315	7999.970640	13.680026	-0.072843	4.818378
363.709109	7999.985751	13.685031	-0.072834	4.818383
363.701358	7999.991949	13.690035	-0.072832	4.818384
363.776940	7999.991910	13.695040	-0.072847	4.818384
363.880477	7999.991194	13.700045	-0.072866	4.818384
363.545633	7999.991966	13.705050	-0.072803	4.818385
363.602545	8000.011634	13.710055	-0.072814	4.818391
363.909397	7999.991581	13.715059	-0.072871	4.818384
363.852248	7999.979263	13.720064	-0.072861	4.818380
364.025449	7999.993134	13.725069	-0.072893	4.818384
363.833301	7999.950650	13.730074	-0.072857	4.818372
363.936076	7999.965680	13.735079	-0.072876	4.818376
363.950563	7999.973226	13.740083	-0.072879	4.818378
363.956519	7999.948098	13.745088	-0.072880	4.818370
364.052610	8000.023958	13.750093	-0.072898	4.818393
363.923314	7999.995969	13.755098	-0.072874	4.818385
363.969892	8000.003945	13.760103	-0.072882	4.818387
363.965238	7999.986027	13.765107	-0.072882	4.818382
363.980049	7999.968369	13.770112	-0.072884	4.818376
363.816670	7999.999794	13.775117	-0.072854	4.818386
363.887482	7999.962929	13.780122	-0.072867	4.818375
364.020536	8000.017227	13.785127	-0.072892	4.818391
363.902320	7999.974681	13.790131	-0.072870	4.818379
363.865126	7999.972083	13.795136	-0.072863	4.818378
364.067642	7999.993699	13.800141	-0.072901	4.818384
364.101700	7999.971047	13.805146	-0.072907	4.818377
363.911082	7999.977950	13.810151	-0.072871	4.818379
364.024307	8000.001522	13.815155	-0.072893	4.818386
364.121727	7999.974466	13.820160	-0.072911	4.818378
364.035888	8000.000627	13.825165	-0.072895	4.818386
364.127097	7999.989243	13.830170	-0.072912	4.818382
364.080268	8000.000170	13.835175	-0.072903	4.818385
364.092325	7999.983526	13.840179	-0.072905	4.818380
364.061386	7999.990464	13.845184	-0.072899	4.818383
364.061921	8000.009378	13.850189	-0.072900	4.818388
363.951135	7999.977435	13.855194	-0.072879	4.818379
363.939134	8000.000382	13.860199	-0.072877	4.818386
363.961876	7999.999636	13.865203	-0.072881	4.818386
363.922349	7999.974950	13.870208	-0.072874	4.818379
363.974411	7999.988250	13.875213	-0.072883	4.818382
363.672583	7999.994715	13.880218	-0.072827	4.818385
363.852677	8000.022333	13.885223	-0.072861	4.818393
363.971441	7999.997664	13.890227	-0.072883	4.818385
363.782574	7999.990935	13.895232	-0.072848	4.818384
364.091626	8000.016078	13.900237	-0.072905	4.818390
363.961514	7999.989128	13.905242	-0.072881	4.818383
363.890384	7999.989227	13.910247	-0.072868	4.818383
363.953287	8000.003723	13.915251	-0.072879	4.818387
363.898101	7999.999833	13.920256	-0.072869	4.818386
363.739414	8000.022918	13.925261	-0.072840	4.818393
363.479837	8000.001590	13.930266	-0.072791	4.818388
364.072633	7999.976961	13.935271	-0.072902	4.818379
364.088853	7999.990832	13.940275	-0.072905	4.818383
363.853178	7999.966672	13.945280	-0.072861	4.818376
364.040763	8000.010145	13.950285	-0.072896	4.818389
364.055078	7999.976726	13.955290	-0.072898	4.818379
364.164138	8000.000242	13.960295	-0.072919	4.818385
364.093033	7999.985636	13.965299	-0.072905	4.818381
364.146725	7999.974801	13.970304	-0.072915	4.818378
364.406690	7999.997187	13.975309	-0.072964	4.818383
364.148565	7999.987430	13.980314	-0.072916	4.818381
364.278424	7999.989168	13.985319	-0.072940	4.818381
364.238277	8000.029594	13.990323	-0.072932	4.818393
364.145968	8000.010503	13.995328	-0.072915	4.818388
364.103581	8000.024641	14.000333	-0.072907	4.818393
364.264828	7999.980583	14.005338	-0.072937	4.818379
364.341796	8000.011023	14.010343	-0.072952	4.818388
364.313134	7999.988582	14.015347	-0.072946	4.818381
364.081745	7999.974982	14.020352	-0.072903	4.818378
364.315327	7999.998065	14.025357	-0.072947	4.818384
364.154022	7999.975949	14.030362	-0.072917	4.818378
364.100485	8000.024599	14.035367	-0.072907	4.818393
364.290558	8000.008237	14.040371	-0.072942	4.818387
364.103309	8000.018335	14.045376	-0.072907	4.818391
363.801452	8000.047906	14.050381	-0.072851	4.818401
364.095077	8000.011923	14.055386	-0.072906	4.818389
363.812787	8000.050159	14.060391	-0.072853	4.818401
363.789038	8000.016230	14.065395	-0.072849	4.818391
363.677284	8000.013685	14.070400	-0.072828	4.818391
364.212306	8000.013492	14.075405	-0.072928	4.818389
363.979875	7999.975720	14.080410	-0.072884	4.818379
364.130273	7999.985085	14.085415	-0.072912	4.818381
364.334676	7999.976266	14.090419	-0.072950	4.818377
364.144283	7999.978970	14.095424	-0.072915	4.818379
364.226621	8000.009482	14.100429	-0.072930	4.818388
364.096848	8000.012997	14.105434	-0.072906	4.818389
364.156996	8000.013802	14.110439	-0.072917	4.818389
363.924662	8000.030649	14.115443	-0.072874	4.818395
363.996453	7999.983294	14.120448	-0.072887	4.818381
363.797713	8000.035252	14.125453	-0.072850	4.818397
363.958290	7999.988035	14.130458	-0.072880	4.818382
363.802397	8000.021661	14.135463	-0.072851	4.818393
364.118680	8000.009088	14.140467	-0.072910	4.818388
363.658176	8000.006077	14.145472	-0.072824	4.818389
363.767624	8000.030649	14.150477	-0.072845	4.818396
363.993790	8000.024222	14.155482	-0.072887	4.818393
363.582277	8000.073333	14.160487	-0.072810	4.818409
363.550660	8000.064507	14.165491	-0.072804	4.818407
364.004986	7999.976056	14.170496	-0.072889	4.818379
364.194178	8000.001695	14.175501	-0.072924	4.818385
363.893683	8000.009228	14.180506	-0.072868	4.818389
363.791087	8000.017308	14.185511	-0.072849	4.818392
364.167272	8000.008688	14.190515	-0.072919	4.818388
364.015952	7999.978303	14.195520	-0.072891	4.818379
363.997413	8000.005364	14.200525	-0.072888	4.818387
364.216108	7999.985183	14.205530	-0.072928	4.818380
364.216845	7999.991495	14.210535	-0.072928	4.818382
364.188509	7999.973260	14.215539	-0.072923	4.818377
364.210960	7999.995618	14.220544	-0.072927	4.818384
364.285317	7999.978757	14.225549	-0.072941	4.818378
364.248373	7999.957256	14.230554	-0.072934	4.818372
364.234078	7999.984373	14.235559	-0.072932	4.818380
364.229757	8000.006373	14.240563	-0.072931	4.818387
364.257268	7999.967878	14.245568	-0.072936	4.818375
364.295282	8000.012502	14.250573	-0.072943	4.818388
364.181714	7999.966867	14.255578	-0.072922	4.818375
364.262746	7999.988958	14.260583	-0.072937	4.818381
364.177696	8000.006727	14.265587	-0.072921	4.818387
364.209545	7999.978793	14.270592	-0.072927	4.818379
364.390702	7999.987520	14.275597	-0.072961	4.818380
364.141584	7999.964229	14.280602	-0.072914	4.818374
364.299628	7999.989452	14.285607	-0.072944	4.818381
364.188007	8000.008965	14.290611	-0.072923	4.818388
363.944614	8000.026715	14.295616	-0.072878	4.818394
364.300708	8000.002071	14.300621	-0.072944	4.818385
363.996752	7999.972795	14.305626	-0.072887	4.818378
364.218141	8000.006218	14.310631	-0.072929	4.818387
364.105007	8000.001553	14.315635	-0.072908	4.818386
364.045392	7999.990251	14.320640	-0.072897	4.818383
364.217632	8000.031419	14.325645	-0.072929	4.818394
364.166534	8000.056994	14.330650	-0.072919	4.818402
364.063487	8000.036709	14.335655	-0.072900	4.818396
364.022342	8000.085525	14.340659	-0.072892	4.818411
364.101436	8000.009908	14.345664	-0.072907	4.818388
364.120338	7999.998607	14.350669	-0.072910	4.818385
363.880113	7999.986989	14.355674	-0.072866	4.818382
364.265963	8000.001606	14.360679	-0.072938	4.818385
364.295690	7999.973644	14.365683	-0.072943	4.818377
364.141292	7999.976830	14.370688	-0.072914	4.818378
364.533347	8000.007285	14.375693	-0.072987	4.818386
364.476845	7999.975018	14.380698	-0.072977	4.818376
364.316920	8000.000187	14.385703	-0.072947	4.818384
364.400647	7999.970848	14.390707	-0.072963	4.818375
364.408845	7999.948900	14.395712	-0.072964	4.818369
364.418026	7999.982634	14.400717	-0.072966	4.818379
364.266023	7999.982701	14.405722	-0.072938	4.818379
364.201036	8000.009140	14.410727	-0.072925	4.818388
364.320067	7999.998129	14.415731	-0.072948	4.818384
364.328022	7999.985631	14.420736	-0.072949	4.818380
364.130478	8000.017649	14.425741	-0.072912	4.818390
364.313396	7999.118918	14.430746	-0.072946	4.818123

364.217815	7996.037426	14.435751	-0.072926	4.817207
364.293483	7990.646045	14.440755	-0.072937	4.815603
364.110040	7983.977063	14.445760	-0.072898	4.813620
364.009185	7976.841018	14.450765	-0.072875	4.811497
363.857216	7969.136166	14.455770	-0.072841	4.809204
364.096707	7961.385438	14.460775	-0.072881	4.806894
364.039025	7953.463998	14.465779	-0.072865	4.804533
363.725465	7945.609344	14.470784	-0.072801	4.802192
363.772944	7937.582971	14.475789	-0.072805	4.799798
363.577297	7929.595403	14.480794	-0.072763	4.797415
363.546311	7921.554200	14.485799	-0.072752	4.795013
363.667542	7913.593983	14.490803	-0.072770	4.792635
363.423509	7905.598125	14.495808	-0.072719	4.790246
363.139105	7897.662276	14.500813	-0.072661	4.787873
362.579734	7889.610705	14.505818	-0.072552	4.785466
362.990462	7881.551707	14.510823	-0.072623	4.783052
363.042604	7873.607559	14.515827	-0.072627	4.780672
362.652756	7865.618095	14.520832	-0.072550	4.778279
362.931871	7857.571765	14.525837	-0.072596	4.775866
362.887070	7849.592844	14.530842	-0.072583	4.773473
362.934654	7841.588672	14.535847	-0.072586	4.771070
362.843864	7833.515506	14.540851	-0.072564	4.768646
363.108333	7825.499608	14.545856	-0.072608	4.766237
362.692196	7817.565684	14.550861	-0.072526	4.763854
362.551975	7809.625862	14.555866	-0.072494	4.761466
362.854984	7801.459443	14.560871	-0.072545	4.759008
363.224400	7793.594220	14.565875	-0.072609	4.756640
362.669795	7785.521070	14.570880	-0.072501	4.754209
362.732347	7777.574240	14.575885	-0.072507	4.751815
362.677940	7769.540425	14.580890	-0.072492	4.749393
362.707792	7761.505169	14.585895	-0.072492	4.746969
363.048756	7753.445293	14.590899	-0.072550	4.744535
363.038545	7745.471657	14.595904	-0.072543	4.742128
363.027262	7737.459717	14.600909	-0.072536	4.739707
363.147314	7729.492018	14.605914	-0.072553	4.737299
362.962378	7721.505668	14.610919	-0.072513	4.734884
362.992375	7713.541362	14.615923	-0.072514	4.732474
362.980210	7705.451970	14.620928	-0.072506	4.730025
363.099236	7697.470622	14.625933	-0.072523	4.727607
363.280810	7689.455578	14.630938	-0.072552	4.725178
363.148867	7681.463407	14.635943	-0.072522	4.722755
363.165592	7673.541030	14.640947	-0.072520	4.720352
363.226777	7665.535514	14.645952	-0.072526	4.717922
363.204442	7657.515181	14.650957	-0.072517	4.715486
363.332408	7649.524400	14.655962	-0.072535	4.713058
363.061929	7641.494752	14.660967	-0.072480	4.710618
363.330921	7633.548777	14.665971	-0.072525	4.708201
363.313874	7625.477340	14.670976	-0.072516	4.705745
362.814148	7617.533216	14.675981	-0.072418	4.703327
362.916429	7609.522991	14.680986	-0.072432	4.700887
363.003290	7601.532198	14.685991	-0.072443	4.698451
362.837355	7593.566124	14.690995	-0.072407	4.696022
362.621864	7585.477223	14.696000	-0.072361	4.693555
363.094002	7577.500148	14.701005	-0.072444	4.691119
362.814073	7569.475767	14.706010	-0.072387	4.688669
362.794613	7561.509531	14.711015	-0.072378	4.686234
362.607329	7553.498016	14.716019	-0.072338	4.683785
362.319224	7545.563999	14.721024	-0.072279	4.681358
362.503117	7537.462894	14.726029	-0.072308	4.678879
362.812979	7529.546684	14.731034	-0.072360	4.676455
362.574929	7521.458260	14.736039	-0.072311	4.673977
362.501252	7513.510929	14.741043	-0.072292	4.671541
362.419843	7505.444631	14.746048	-0.072272	4.669067
362.341793	7497.496572	14.751053	-0.072252	4.666628
362.540067	7489.403546	14.756058	-0.072283	4.664143
362.580271	7481.479236	14.761063	-0.072286	4.661709
362.579035	7473.456464	14.766067	-0.072280	4.659243
362.454336	7465.475450	14.771072	-0.072252	4.656789
362.368307	7457.426682	14.776077	-0.072231	4.654313
362.340000	7449.495801	14.781082	-0.072220	4.651871
362.269272	7441.417103	14.786087	-0.072202	4.649383
362.282095	7433.508840	14.791091	-0.072199	4.646946
362.165572	7425.400316	14.796096	-0.072172	4.644446
362.153139	7417.529849	14.801101	-0.072165	4.642018
362.280652	7409.391367	14.806106	-0.072183	4.639506
362.333075	7401.449363	14.811111	-0.072188	4.637053
362.322890	7393.393444	14.816115	-0.072180	4.634564
362.209372	7385.443990	14.821120	-0.072154	4.632106
362.531366	7377.385054	14.826125	-0.072209	4.629614
362.115635	7369.432589	14.831130	-0.072126	4.627152
362.177382	7361.341405	14.836135	-0.072132	4.624647
362.346188	7353.479002	14.841139	-0.072159	4.622211
362.240552	7345.410924	14.846144	-0.072134	4.619710
362.253559	7337.457646	14.851149	-0.072131	4.617243
362.129565	7329.380272	14.856154	-0.072103	4.614737
361.983762	7321.410950	14.861159	-0.072070	4.612262
362.103877	7313.387838	14.866163	-0.072088	4.609770
362.164522	7305.394335	14.871168	-0.072094	4.607286
362.174092	7297.405315	14.876173	-0.072090	4.604801
362.039197	7289.463294	14.881178	-0.072060	4.602330
362.014526	7281.376780	14.886183	-0.072050	4.599812
362.051626	7273.433728	14.891187	-0.072052	4.597338
362.001132	7265.382168	14.896192	-0.072037	4.594828
361.990087	7257.399912	14.901197	-0.072030	4.592339
361.811820	7249.386786	14.906202	-0.071991	4.589839
361.656776	7241.347996	14.911207	-0.071957	4.587329
361.793509	7233.360123	14.916211	-0.071978	4.584834
361.625497	7225.366209	14.921216	-0.071941	4.582336
361.805549	7217.366803	14.926221	-0.071969	4.579835
361.585362	7209.377007	14.931226	-0.071923	4.577335
361.728802	7201.351613	14.936231	-0.071945	4.574823
361.642095	7193.361893	14.941235	-0.071923	4.572320
361.461405	7185.322408	14.946240	-0.071884	4.569800
361.668051	7177.367520	14.951245	-0.071918	4.567306
361.570019	7169.342353	14.956250	-0.071894	4.564789
361.385153	7161.395841	14.961255	-0.071855	4.562294
361.321147	7153.372401	14.966259	-0.071838	4.559774
361.358558	7145.370565	14.971264	-0.071839	4.557259
361.474597	7137.336812	14.976269	-0.071856	4.554733
361.473422	7129.393704	14.981274	-0.071850	4.552235
361.357707	7121.301186	14.986279	-0.071823	4.549687
361.412370	7113.385302	14.991283	-0.071828	4.547194
361.233724	7105.308292	14.996288	-0.071790	4.544648
361.341638	7097.373032	15.001293	-0.071805	4.542147
361.229348	7089.342115	15.006298	-0.071779	4.539613
361.231538	7081.358227	15.011303	-0.071774	4.537093
361.303519	7073.314901	15.016307	-0.071782	4.534553
361.190233	7065.314323	15.021312	-0.071756	4.532024
361.235141	7057.243718	15.026317	-0.071759	4.529473
361.042462	7049.291428	15.031322	-0.071718	4.526956
361.056517	7041.241033	15.036327	-0.071715	4.524408
361.281946	7033.331023	15.041331	-0.071752	4.521904
361.186348	7025.276918	15.046336	-0.071729	4.519351
361.084116	7017.336744	15.051341	-0.071705	4.516833
361.188028	7009.294573	15.056346	-0.071719	4.514282
360.997499	7001.326959	15.061351	-0.071678	4.511753
361.030625	6993.291664	15.066355	-0.071679	4.509201
360.850044	6985.266253	15.071360	-0.071640	4.506650
360.904152	6977.291871	15.076365	-0.071645	4.504114
360.911332	6969.297003	15.081370	-0.071641	4.501571
360.756273	6961.239937	15.086375	-0.071607	4.499005
360.822800	6953.310312	15.091379	-0.071614	4.496480
360.892224	6945.226431	15.096384	-0.071622	4.493904
360.837294	6937.267139	15.101389	-0.071607	4.491366
360.730997	6929.230847	15.106394	-0.071582	4.488801
360.555082	6921.234305	15.111399	-0.071544	4.486248
360.658422	6913.243665	15.116403	-0.071558	4.483696
360.565996	6905.256206	15.121408	-0.071535	4.481143
360.511692	6897.260149	15.126413	-0.071520	4.478586
360.086188	6889.315652	15.131418	-0.071435	4.476042
359.750843	6881.255676	15.136423	-0.071368	4.473460
359.807770	6873.344106	15.141427	-0.071373	4.470926
359.995444	6865.218015	15.146432	-0.071403	4.468322
359.947077	6857.209940	15.151437	-0.071389	4.465754
360.169677	6849.224942	15.156442	-0.071425	4.463192
360.483128	6841.174096	15.161447	-0.071478	4.460609
360.185773	6833.210724	15.166451	-0.071417	4.458049
359.983239	6825.192365	15.171456	-0.071375	4.455471
360.318398	6817.204489	15.176461	-0.071432	4.452903
360.153901	6809.179360	15.181466	-0.071396	4.450320
360.163825	6801.186282	15.186471	-0.071393	4.447746
360.333851	6793.214670	15.191475	-0.071419	4.445178
360.107823	6785.217170	15.196480	-0.071372	4.442599
359.963670	6777.210505	15.201485	-0.071340	4.440015
360.042092	6769.228116	15.206490	-0.071349	4.437440
359.820340	6761.183813	15.211495	-0.071302	4.434840
359.531761	6753.250726	15.216499	-0.071244	4.432275
359.636676	6745.168933	15.221504	-0.071258	4.429663
359.784610	6737.199183	15.226509	-0.071280	4.427085
359.647244	6729.109791	15.231514	-0.071249	4.424466
359.404945	6721.210182	15.236519	-0.071199	4.421906
359.691367	6713.142129	15.241523	-0.071247	4.419293
359.633339	6705.169635	15.246528	-0.071231	4.416707
359.566043	6697.143332	15.251533	-0.071213	4.414103
359.834305	6689.158897	15.256538	-0.071258	4.411512
359.579611	6681.117666	15.261543	-0.071205	4.408898
359.302374	6673.207522	15.266547	-0.071149	4.406325
359.134720	6665.156094	15.271552	-0.071112	4.403706
359.388309	6657.239571	15.276557	-0.071154	4.401131
359.450478	6649.170262	15.281562	-0.071161	4.398504
359.592011	6641.165514	15.286567	-0.071182	4.395897
359.555388	6633.192916	15.291571	-0.071170	4.393297
359.471006	6625.137985	15.296576	-0.071149	4.390669
359.527150	6617.135772	15.301581	-0.071154	4.388058
359.437181	6609.149877	15.306586	-0.071132	4.385449
359.467939	6601.170122	15.311591	-0.071133	4.382841
358.910499	6593.285554	15.316595	-0.071024	4.380259
359.130874	6585.217909	15.321600	-0.071059	4.377621
359.497173	6577.210126	15.326605	-0.071122	4.375002
359.478059	6569.279989	15.331610	-0.071114	4.372404
359.223852	6561.219651	15.336615	-0.071061	4.369761
359.429007	6553.263789	15.341619	-0.071094	4.367153
359.208902	6545.242961	15.346624	-0.071048	4.364519
359.316314	6537.286383	15.351629	-0.071063	4.361907
359.313747	6529.254339	15.356634	-0.071057	4.359268
359.243235	6521.308437	15.361639	-0.071039	4.356656
359.207362	6513.293499	15.366643	-0.071027	4.354019
359.093927	6505.200820	15.371648	-0.071000	4.351354
359.003925	6497.216849	15.376653	-0.070978	4.348724
359.045161	6489.237548	15.381658	-0.070981	4.346094
358.906666	6481.208593	15.386663	-0.070950	4.343446
359.076577	6473.262450	15.391667	-0.070976	4.340825
359.206708	6465.236914	15.396672	-0.070995	4.338176
359.075739	6457.265956	15.401677	-0.070966	4.335542
359.034867	6449.272232	15.406682	-0.070953	4.332899
359.218732	6441.216599	15.411687	-0.070982	4.330236
359.065632	6433.221284	15.416691	-0.070948	4.327589
358.989712	6425.196036	15.421696	-0.070929	4.324930
359.299787	6417.241475	15.426701	-0.070981	4.322297
359.074217	6409.247698	15.431706	-0.070934	4.319644
358.752619	6401.316864	15.436711	-0.070869	4.317010
358.966916	6393.226907	15.441715	-0.070904	4.314326
358.776320	6385.293251	15.446720	-0.070863	4.311689
358.748067	6377.234507	15.451725	-0.070853	4.309010
358.646765	6369.200530	15.456730	-0.070829	4.306337
358.785530	6361.148395	15.461735	-0.070849	4.303659
358.754113	6353.252873	15.466739	-0.070838	4.301029
358.544265	6345.190882	15.471744	-0.070794	4.298341
358.908111	6337.150423	15.476749	-0.070856	4.295663
358.744115	6329.176844	15.481754	-0.070821	4.293001
358.482661	6321.143634	15.486759	-0.070767	4.290317
358.644470	6313.191756	15.491763	-0.070792	4.287662
358.907269	6305.151385	15.496768	-0.070835	4.284977
358.989669	6297.252549	15.501773	-0.070845	4.282335
358.620753	6289.240668	15.506778	-0.070772	4.279650
358.387232	6281.265562	15.511783	-0.070723	4.276977
358.381057	6273.231334	15.516787	-0.070717	4.274285
358.081283	6265.210587	15.521792	-0.070655	4.271592
357.958937	6257.208514	15.526797	-0.070627	4.268906
358.366175	6249.203599	15.531802	-0.070698	4.266223
358.343227	6241.103727	15.536807	-0.070689	4.263501
358.101342	6233.242941	15.541811	-0.070638	4.260856
358.306831	6225.139158	15.546816	-0.070671	4.258132
358.035540	6217.214176	15.551821	-0.070616	4.255462
357.971344	6209.177804	15.556826	-0.070598	4.252755
358.160228	6201.117644	15.561831	-0.070628	4.250040
358.206005	6193.180743	15.566835	-0.070632	4.247364
358.002639	6185.145468	15.571840	-0.070589	4.244650
358.114457	6177.217561	15.576845	-0.070604	4.241974
357.960245	6169.203096	15.581850	-0.070570	4.239265
357.884608	6161.186763	15.586855	-0.070551	4.236554
357.681643	6153.209112	15.591859	-0.070508	4.233852
357.467145	6145.225943	15.596864	-0.070463	4.231148
357.899335	6137.142689	15.601869	-0.070538	4.228414
357.576386	6129.118990	15.606874	-0.070473	4.225691
357.743137	6121.147439	15.611879	-0.070499	4.222989
357.792556	6113.165413	15.616883	-0.070503	4.220280
357.581147	6105.160221	15.621888	-0.070458	4.217559
357.817454	6097.151155	15.626893	-0.070497	4.214839
357.939120	6089.149106	15.631898	-0.070514	4.212120
357.521642	6081.126920	15.636903	-0.070431	4.209385
357.490925	6073.218237	15.641907	-0.070420	4.206692
357.679140	6065.139686	15.646912	-0.070450	4.203941
357.571752	6057.198051	15.651917	-0.070425	4.201232
357.480437	6049.140296	15.656922	-0.070403	4.198482
357.544722	6041.147471	15.661927	-0.070410	4.195754
357.857064	6033.151328	15.666931	-0.070462	4.193026
357.516347	6025.076861	15.671936	-0.070394	4.190262
357.674545	6017.086384	15.676941	-0.070418	4.187530
357.626325	6009.103697	15.681946	-0.070404	4.184797
357.781018	6001.156502	15.686951	-0.070427	4.182077
357.574440	5993.170690	15.691955	-0.070384	4.179338
357.158855	5985.183960	15.696960	-0.070301	4.176593
357.557406	5977.100913	15.701965	-0.070370	4.173824
357.409427	5969.154423	15.706970	-0.070337	4.171093
357.371879	5961.139301	15.711975	-0.070325	4.168338
357.420164	5953.174495	15.716979	-0.070329	4.165600
357.226887	5945.138447	15.721984	-0.070288	4.162833
357.056167	5937.192206	15.726989	-0.070251	4.160094
357.330407	5929.184187	15.731994	-0.070297	4.157338
357.534500	5921.142328	15.736999	-0.070329	4.154568
357.396959	5913.215241	15.742003	-0.070299	4.151832
357.127765	5905.140167	15.747008	-0.070243	4.149040
357.149206	5897.195237	15.752013	-0.070242	4.146296
356.960738	5889.155158	15.757018	-0.070202	4.143514
357.206083	5881.153725	15.762023	-0.070242	4.140749
357.143524	5873.203541	15.767027	-0.070225	4.137996
356.847187	5865.203674	15.772032	-0.070165	4.135221
356.950478	5857.234429	15.777037	-0.070179	4.132459
356.922790	5849.163979	15.782042	-0.070169	4.129660
356.900274	5841.187832	15.787047	-0.070159	4.126891
356.909578	5833.169987	15.792051	-0.070156	4.124106
356.901452	5825.206733	15.797056	-0.070149	4.121338
356.949825	5817.201743	15.802061	-0.070153	4.118554
356.767680	5809.248961	15.807066	-0.070114	4.115784
356.524103	5801.212665	15.812071	-0.070063	4.112982
356.724592	5793.190130	15.817075	-0.070095	4.110188
356.755378	5785.135063	15.822080	-0.070096	4.107380
356.509978	5777.133338	15.827085	-0.070045	4.104583
356.582867	5769.182323	15.832090	-0.070053	4.101808
356.686423	5761.122000	15.837095	-0.070067	4.098992
356.613389	5753.230599	15.842099	-0.070048	4.096231
356.570034	5745.167644	15.847104	-0.070035	4.093409
356.837739	5737.155319	15.852109	-0.070080	4.090607
356.577814	5729.164103	15.857114	-0.070026	4.087803
356.466610	5721.137560	15.862119	-0.070000	4.084987
356.545614	5713.198441	15.867123	-0.070010	4.082202
356.348407	5705.162609	15.872128	-0.069968	4.079377
356.316966	5697.236423	15.877133	-0.069957	4.076591
356.380560	5689.171399	15.882138	-0.069963	4.073756
356.520759	5681.136188	15.887143	-0.069984	4.070931
356.566258	5673.181476	15.892147	-0.069988	4.068130
356.482902	5665.147453	15.897152	-0.069967	4.065298
356.415164	5657.217520	15.902157	-0.069949	4.062501
356.326757	5649.159550	15.907162	-0.069927	4.059656
356.257081	5641.199254	15.912167	-0.069909	4.056844
356.289093	5633.160556	15.917171	-0.069910	4.054004
356.191439	5625.177338	15.922176	-0.069886	4.051179
356.292342	5617.156537	15.927181	-0.069900	4.048343
356.279360	5609.158732	15.932186	-0.069892	4.045510
355.883534	5601.215365	15.937191	-0.069814	4.042689
355.805798	5593.244949	15.942195	-0.069794	4.039862
355.699323	5585.229559	15.947200	-0.069769	4.037016
356.024942	5577.167782	15.952205	-0.069824	4.034158
355.828783	5569.161672	15.957210	-0.069782	4.031310
355.760718	5561.137906	15.962215	-0.069765	4.028456
355.973996	5553.151681	15.967219	-0.069799	4.025617
356.038847	5545.154183	15.972224	-0.069806	4.022770
355.968049	5537.170354	15.977229	-0.069788	4.019924
355.888884	5529.218859	15.982234	-0.069768	4.017087
355.795772	5521.187970	15.987239	-0.069745	4.014219
355.796269	5513.253734	15.992243	-0.069740	4.011386
355.531978	5505.207450	15.997248	-0.069685	4.008506
355.405528	5497.247820	16.002253	-0.069657	4.005657
355.480222	5489.259957	16.007258	-0.069665	4.002799
355.338671	5481.258445	16.012263	-0.069634	3.999931
355.625845	5473.252688	16.017267	-0.069682	3.997067
355.380952	5465.203269	16.022272	-0.069631	3.994175
355.509666	5457.238294	16.027277	-0.069650	3.991319
355.314492	5449.227746	16.032282	-0.069609	3.988438
355.146292	5441.227842	16.037287	-0.069572	3.985560
355.322011	5433.246517	16.042291	-0.069600	3.982692
355.043503	5425.220293	16.047296	-0.069542	3.979798
355.364014	5417.232956	16.052301	-0.069597	3.976926
355.523009	5409.202095	16.057306	-0.069621	3.974034
355.325184	5401.215465	16.062311	-0.069579	3.971149
355.483054	5393.198879	16.067315	-0.069603	3.968258
355.491685	5385.186028	16.072320	-0.069600	3.965363
355.376957	5377.268083	16.077325	-0.069573	3.962498
355.266407	5369.264277	16.082330	-0.069547	3.959600
355.336768	5361.271896	16.087335	-0.069555	3.956708
355.229436	5353.269371	16.092339	-0.069530	3.953806
354.917037	5345.270303	16.097344	-0.069467	3.950900
355.190303	5337.203468	16.102349	-0.069512	3.947978
355.256220	5329.193525	16.107354	-0.069519	3.945070
355.225877	5321.208164	16.112359	-0.069509	3.942168
355.208533	5313.198854	16.117363	-0.069500	3.939255
355.236072	5305.248036	16.122368	-0.069500	3.936362
355.285530	5297.202520	16.127373	-0.069504	3.933432
355.184306	5289.221376	16.132378	-0.069480	3.930521
355.025981	5281.221812	16.137383	-0.069445	3.927600
355.159961	5273.241950	16.142387	-0.069465	3.924690
355.021772	5265.267817	16.147392	-0.069434	3.921774
354.917697	5257.285065	16.152397	-0.069410	3.918854
354.925321	5249.335637	16.157402	-0.069406	3.915946
354.736077	5241.255172	16.162407	-0.069365	3.912984
354.896754	5233.289912	16.167411	-0.069390	3.910068
354.823050	5225.282715	16.172416	-0.069371	3.907131
354.911812	5217.235383	16.177421	-0.069382	3.904180
354.886241	5209.331176	16.182426	-0.069372	3.901276
354.899468	5201.270261	16.187431	-0.069370	3.898314
355.124007	5193.285400	16.192435	-0.069406	3.895382
354.692920	5185.341530	16.197440	-0.069321	3.892450
354.949465	5177.254196	16.202445	-0.069363	3.889476
354.906144	5169.316480	16.207450	-0.069350	3.886549
354.798059	5161.289374	16.212455	-0.069325	3.883586
354.676623	5153.379083	16.217459	-0.069297	3.880663
354.415256	5145.350840	16.222464	-0.069243	3.877691
354.352177	5137.384456	16.227469	-0.069226	3.874744
354.277222	5129.233384	16.232474	-0.069207	3.871727
354.317925	5121.189217	16.237479	-0.069209	3.868749
354.545078	5113.235849	16.242483	-0.069246	3.865806
354.412432	5105.234807	16.247488	-0.069216	3.862836
354.321165	5097.290599	16.252493	-0.069194	3.859885
354.389603	5089.301382	16.257498	-0.069202	3.856919
354.365499	5081.284975	16.262503	-0.069192	3.853938
354.374172	5073.334977	16.267507	-0.069188	3.850981
354.204581	5065.320905	16.272512	-0.069152	3.847993
354.349049	5057.308359	16.277517	-0.069173	3.845011
354.166194	5049.371197	16.282522	-0.069134	3.842047
354.076165	5041.320270	16.287527	-0.069112	3.839041
354.332848	5033.343164	16.292531	-0.069155	3.836067
354.306059	5025.307776	16.297536	-0.069144	3.833063
354.242662	5017.335089	16.302541	-0.069127	3.830079
354.213534	5009.339114	16.307546	-0.069117	3.827085
354.174222	5001.281716	16.312551	-0.069104	3.824066
353.911394	4993.393806	16.317555	-0.069050	3.821102
354.157614	4985.329589	16.322560	-0.069091	3.818082
354.204108	4977.345095	16.327565	-0.069094	3.815084
354.068664	4969.387744	16.332570	-0.069064	3.812090
353.726425	4961.328853	16.337575	-0.068995	3.809052
353.905536	4953.358639	16.342579	-0.069023	3.806055
353.904238	4945.360827	16.347584	-0.069018	3.803042
353.992818	4937.350654	16.352589	-0.069029	3.800024
353.821744	4929.423022	16.357594	-0.068992	3.797029
353.905815	4921.376206	16.362599	-0.069002	3.793992
353.927595	4913.401556	16.367603	-0.069001	3.790979
353.883305	4905.366353	16.372608	-0.068988	3.787939
353.778043	4897.371071	16.377613	-0.068963	3.784910
353.642812	4889.412929	16.382618	-0.068932	3.781892
353.682448	4881.344160	16.387623	-0.068935	3.778833
353.805070	4873.420665	16.392627	-0.068952	3.775830
353.504897	4865.416458	16.397632	-0.068891	3.772783
353.632777	4857.390365	16.402637	-0.068910	3.769736
353.599147	4849.423537	16.407642	-0.068898	3.766704
353.441703	4841.411932	16.412647	-0.068864	3.763651
353.423522	4833.461980	16.417651	-0.068855	3.760621
353.169706	4825.469570	16.422656	-0.068803	3.757568
353.515272	4817.442330	16.427661	-0.068862	3.754513
353.470818	4809.483980	16.432666	-0.068848	3.751472
353.395783	4801.415682	16.437671	-0.068829	3.748387
353.516708	4793.430394	16.442675	-0.068846	3.745335
353.409228	4785.440206	16.447680	-0.068821	3.742273
353.333136	4777.471685	16.452685	-0.068802	3.739218
353.249834	4769.534597	16.457690	-0.068781	3.736172
353.155476	4761.447814	16.462695	-0.068758	3.733066
353.326524	4753.446361	16.467699	-0.068785	3.729997
353.189717	4745.466698	16.472704	-0.068754	3.726926
353.205725	4737.449584	16.477709	-0.068752	3.723841
352.976654	4729.542767	16.482714	-0.068704	3.720791
352.855462	4721.518006	16.487719	-0.068676	3.717695
352.656822	4713.547189	16.492723	-0.068634	3.714616
352.913554	4705.436431	16.497728	-0.068677	3.711491
352.987780	4697.402704	16.502733	-0.068685	3.708389
353.005933	4689.416541	16.507738	-0.068684	3.705301
352.883858	4681.456908	16.512743	-0.068656	3.702218
352.797001	4673.465345	16.517747	-0.068634	3.699120
352.617060	4665.526236	16.522752	-0.068596	3.696038
352.489816	4657.531560	16.527757	-0.068567	3.692933
352.680612	4649.493993	16.532762	-0.068597	3.689817
352.435929	4641.496743	16.537767	-0.068546	3.686702
352.771898	4633.457171	16.542771	-0.068603	3.683584
352.769036	4625.501927	16.547776	-0.068598	3.680487
352.572678	4617.560239	16.552781	-0.068556	3.677387
352.598664	4609.551641	16.557786	-0.068556	3.674265
352.446796	4601.586089	16.562791	-0.068522	3.671152
352.706317	4593.539019	16.567795	-0.068565	3.668016
352.316782	4585.534922	16.572800	-0.068487	3.664876
352.347090	4577.594023	16.577805	-0.068488	3.661769
352.526100	4569.555464	16.582810	-0.068516	3.658626
352.423928	4561.583196	16.587815	-0.068492	3.655499
352.239658	4553.623556	16.592819	-0.068452	3.652371
352.316966	4545.547529	16.597824	-0.068461	3.649202
352.294068	4537.613399	16.602829	-0.068452	3.646084
352.198126	4529.619826	16.607834	-0.068429	3.642937
352.329226	4521.602061	16.612839	-0.068448	3.639784
352.463252	4513.646426	16.617843	-0.068468	3.636654
352.243287	4505.638127	16.622848	-0.068422	3.633489
352.236491	4497.639077	16.627853	-0.068415	3.630332
352.175353	4489.612178	16.632858	-0.068399	3.627160
352.037097	4481.574984	16.637863	-0.068368	3.623978
351.774443	4473.697398	16.642867	-0.068314	3.620853
352.272727	4465.607909	16.647872	-0.068401	3.617663
352.269041	4457.626229	16.652877	-0.068395	3.614499
352.037474	4449.661794	16.657882	-0.068347	3.611333
352.000521	4441.618780	16.662887	-0.068335	3.608138
352.079249	4433.668686	16.667891	-0.068344	3.604980
351.908372	4425.684958	16.672896	-0.068307	3.601799
351.898087	4417.672289	16.677901	-0.068300	3.598608
351.935163	4409.691442	16.682906	-0.068302	3.595429
351.603462	4401.720588	16.687911	-0.068235	3.592240
351.746326	4393.687484	16.692915	-0.068256	3.589037
351.677553	4385.716230	16.697920	-0.068238	3.585850
351.756343	4377.695876	16.702925	-0.068248	3.582644
351.759461	4369.678954	16.707930	-0.068243	3.579435
351.823953	4361.716824	16.712935	-0.068250	3.576247
351.918188	4353.707406	16.717939	-0.068262	3.573038
351.562925	4345.709362	16.722944	-0.068191	3.569817
351.842303	4337.700432	16.727949	-0.068238	3.566608
351.685184	4329.745511	16.732954	-0.068203	3.563404
351.612677	4321.778235	16.737959	-0.068185	3.560195
351.261485	4313.837002	16.742963	-0.068114	3.556986
350.929982	4305.817244	16.747968	-0.068047	3.553742
351.060709	4297.741103	16.752973	-0.068066	3.550487
350.855080	4289.753656	16.757978	-0.068023	3.547254
350.924083	4281.715489	16.762983	-0.068030	3.544006
351.373867	4273.762588	16.767987	-0.068109	3.540802
351.143422	4265.792050	16.772992	-0.068061	3.537566
351.090148	4257.771358	16.777997	-0.068045	3.534312
350.999488	4249.833262	16.783002	-0.068023	3.531088
351.109167	4241.767826	16.788007	-0.068039	3.527816
350.934400	4233.832517	16.793011	-0.068001	3.524584
351.128254	4225.812164	16.798016	-0.068032	3.521327
351.070486	4217.840279	16.803021	-0.068016	3.518078
350.693730	4209.860228	16.808026	-0.067940	3.514813
350.676028	4201.863377	16.813031	-0.067932	3.511549
350.834538	4193.828766	16.818035	-0.067956	3.508272
350.682399	4185.820785	16.823040	-0.067923	3.504994
350.458895	4177.895418	16.828045	-0.067876	3.501743
350.901286	4169.854577	16.833050	-0.067953	3.498464
350.634685	4161.891942	16.838055	-0.067898	3.495191
350.954045	4153.844538	16.843059	-0.067952	3.491899
350.786296	4145.835163	16.848064	-0.067916	3.488604
350.755942	4137.867969	16.853069	-0.067905	3.485328
350.883346	4129.888031	16.858074	-0.067924	3.482048
350.716890	4121.876340	16.863079	-0.067887	3.478742
350.870089	4113.951749	16.868083	-0.067911	3.475480
350.500728	4105.984561	16.873088	-0.067837	3.472180
350.510684	4097.937705	16.878093	-0.067833	3.468856
350.376630	4089.979701	16.883098	-0.067803	3.465561
350.227191	4081.934078	16.888103	-0.067770	3.462226
350.494241	4073.929300	16.893107	-0.067815	3.458919
350.116445	4066.014205	16.898112	-0.067739	3.455624
350.293915	4057.966541	16.903117	-0.067767	3.452290
350.032578	4050.004732	16.908122	-0.067713	3.448973
349.804085	4042.029993	16.913127	-0.067665	3.445649
350.147072	4034.021075	16.918131	-0.067724	3.442327
349.575147	4026.068568	16.923136	-0.067612	3.438993
349.933319	4018.047558	16.928141	-0.067674	3.435660
350.250562	4010.021133	16.933146	-0.067728	3.432320
350.035560	4002.009443	16.938151	-0.067682	3.428965
350.161348	3994.019726	16.943155	-0.067701	3.425627
349.964342	3986.046164	16.948160	-0.067659	3.422282
350.002096	3978.043651	16.953165	-0.067661	3.418929
350.043961	3970.086562	16.958170	-0.067663	3.415592
349.927022	3962.074100	16.963175	-0.067636	3.412223
350.278826	3954.068564	16.968179	-0.067697	3.408870
349.902719	3946.097598	16.973184	-0.067621	3.405503
349.897288	3938.098016	16.978189	-0.067615	3.402133
349.853901	3930.104417	16.983194	-0.067602	3.398762
349.790464	3922.187772	16.988199	-0.067585	3.395418
349.671479	3914.138934	16.993203	-0.067557	3.392014
349.694014	3906.083152	16.998208	-0.067556	3.388608
349.892467	3898.066048	17.003213	-0.067588	3.385222
349.919806	3890.120221	17.008218	-0.067588	3.381856
349.485125	3882.162588	17.013223	-0.067502	3.378465
349.888180	3874.132591	17.018227	-0.067572	3.375070
349.801823	3866.147784	17.023232	-0.067550	3.371673
349.791681	3858.161512	17.028237	-0.067543	3.368275
349.849959	3850.163427	17.033242	-0.067549	3.364871
349.807922	3842.203396	17.038247	-0.067536	3.361477
349.767024	3834.246943	17.043251	-0.067523	3.358080
349.430157	3826.255117	17.048256	-0.067455	3.354653
349.559998	3818.245205	17.053261	-0.067474	3.351233
349.601602	3810.250455	17.058266	-0.067477	3.347813
349.347878	3802.261522	17.063271	-0.067424	3.344380
349.511154	3794.309509	17.068275	-0.067449	3.340976
348.880711	3786.377018	17.073280	-0.067327	3.337546
348.963689	3778.305391	17.078285	-0.067337	3.334080
349.339674	3770.292187	17.083290	-0.067402	3.330646
349.230895	3762.283954	17.088295	-0.067376	3.327193
349.449675	3754.275066	17.093299	-0.067412	3.323749
349.161003	3746.345882	17.098304	-0.067353	3.320315
349.160373	3738.359450	17.103309	-0.067348	3.316865
349.167330	3730.353233	17.108314	-0.067344	3.313403
349.010414	3722.362958	17.113319	-0.067309	3.309937
349.027340	3714.375497	17.118323	-0.067307	3.306476
349.094846	3706.345783	17.123328	-0.067315	3.302995
349.080565	3698.352047	17.128333	-0.067307	3.299523
348.995032	3690.416281	17.133338	-0.067286	3.296069
349.057908	3682.384295	17.138343	-0.067292	3.292576
348.640385	3674.464851	17.143347	-0.067209	3.289109
348.442693	3666.500213	17.148352	-0.067167	3.285627
348.544337	3658.447333	17.153357	-0.067181	3.282116
349.104337	3650.405152	17.158362	-0.067280	3.278623
348.685155	3642.487866	17.163367	-0.067197	3.275142
348.724266	3634.501989	17.168371	-0.067199	3.271646
348.722517	3626.475753	17.173376	-0.067193	3.268126
348.609028	3618.495539	17.178381	-0.067167	3.264619
348.361991	3610.579682	17.183386	-0.067116	3.261130
348.151514	3602.585315	17.188391	-0.067071	3.257605
348.359569	3594.564209	17.193395	-0.067105	3.254081
348.178655	3586.559035	17.198400	-0.067066	3.250544
348.328770	3578.550038	17.203405	-0.067089	3.247016
348.646280	3570.507129	17.208410	-0.067143	3.243475
348.341169	3562.581500	17.213415	-0.067081	3.239957
348.549889	3554.602814	17.218419	-0.067114	3.236433
348.492526	3546.605054	17.223424	-0.067098	3.232886
348.130288	3538.646364	17.228429	-0.067026	3.229339
347.980419	3530.693316	17.233434	-0.066993	3.225799
347.771780	3522.690112	17.238439	-0.066949	3.222231
348.075971	3514.635134	17.243443	-0.067000	3.218658
348.091014	3506.624243	17.248448	-0.066998	3.215088
348.249789	3498.611302	17.253453	-0.067022	3.211519
348.094687	3490.663804	17.258458	-0.066988	3.207962
347.922043	3482.653624	17.263463	-0.066950	3.204372
347.922529	3474.729942	17.268467	-0.066945	3.200825
348.032907	3466.711867	17.273472	-0.066961	3.197236
347.784802	3458.749185	17.278477	-0.066909	3.193652
348.379708	3450.696629	17.283482	-0.067015	3.190060
347.892967	3442.770211	17.288487	-0.066919	3.186475
347.861601	3434.785158	17.293491	-0.066908	3.182878
347.748060	3426.774922	17.298496	-0.066882	3.179262
347.209095	3418.911463	17.303501	-0.066776	3.175690
347.517368	3410.843095	17.308506	-0.066828	3.172059
347.360978	3402.844496	17.313511	-0.066794	3.168434
347.646415	3394.788350	17.318515	-0.066842	3.164799
347.737976	3386.839535	17.323520	-0.066854	3.161199
347.634810	3378.866661	17.328525	-0.066829	3.157576
347.547194	3370.874676	17.333530	-0.066808	3.153941
347.448795	3362.872441	17.338535	-0.066784	3.150296
347.653888	3354.889184	17.343539	-0.066817	3.146670
347.528202	3346.883543	17.348544	-0.066789	3.143014
347.681663	3338.869085	17.353549	-0.066812	3.139363
347.463998	3330.959580	17.358554	-0.066766	3.135738
347.440070	3322.952697	17.363559	-0.066757	3.132073
347.476056	3314.961467	17.368563	-0.066758	3.128414
347.031307	3307.013472	17.373568	-0.066670	3.124749
347.115237	3299.036883	17.378573	-0.066681	3.121090
347.385731	3290.991104	17.383578	-0.066726	3.117404
347.351451	3283.000350	17.388583	-0.066714	3.113725
347.484114	3275.044857	17.393587	-0.066734	3.110065
347.152201	3267.074666	17.398592	-0.066667	3.106373
346.969087	3259.091603	17.403597	-0.066627	3.102677
346.821088	3251.158436	17.408602	-0.066595	3.099001
346.849459	3243.142002	17.413607	-0.066595	3.095291
347.078281	3235.116072	17.418611	-0.066632	3.091582
347.286595	3227.073519	17.423616	-0.066666	3.087859
347.090376	3219.137034	17.428621	-0.066624	3.084162
347.187167	3211.183470	17.433626	-0.066637	3.080466
347.017366	3203.191770	17.438631	-0.066600	3.076736
347.113495	3195.187828	17.443635	-0.066613	3.073008
347.151854	3187.162088	17.448640	-0.066614	3.069262
346.883800	3179.217836	17.453645	-0.066559	3.065536
346.971744	3171.224530	17.458650	-0.066571	3.061799
346.843776	3163.242028	17.463655	-0.066542	3.058052
346.701366	3155.268884	17.468659	-0.066510	3.054304
346.830883	3147.254047	17.473664	-0.066529	3.050545
346.980185	3139.230377	17.478669	-0.066551	3.046778
346.938073	3131.291545	17.483674	-0.066538	3.043037
346.744292	3123.347275	17.488679	-0.066497	3.039282
346.743868	3115.406526	17.493683	-0.066492	3.035533
346.666661	3107.412369	17.498688	-0.066472	3.031750
346.200032	3099.465926	17.503693	-0.066380	3.027966
346.746778	3091.362879	17.508698	-0.066477	3.024153
346.335022	3083.449943	17.513703	-0.066395	3.020378
346.220526	3075.488069	17.518707	-0.066368	3.016590
345.811760	3067.521546	17.523712	-0.066287	3.012780
346.191604	3059.454027	17.528717	-0.066352	3.008957
346.263406	3051.469257	17.533722	-0.066361	3.005153
345.793299	3043.558220	17.538727	-0.066268	3.001351
346.419273	3035.506444	17.543731	-0.066379	2.997534
346.233271	3027.510424	17.548736	-0.066339	2.993696
346.066333	3019.553955	17.553741	-0.066303	2.989874
345.712111	3011.640213	17.558746	-0.066232	2.986058
346.032602	3003.561605	17.563751	-0.066286	2.982192
346.184845	2995.565905	17.568755	-0.066310	2.978353
346.140849	2987.581549	17.573760	-0.066296	2.974504
346.038021	2979.646899	17.578765	-0.066272	2.970670
345.977771	2971.665614	17.583770	-0.066255	2.966812
345.943452	2963.663548	17.588775	-0.066244	2.962940
345.944766	2955.697721	17.593779	-0.066239	2.959082
345.984137	2947.727200	17.598784	-0.066241	2.955219
345.908691	2939.768687	17.603789	-0.066222	2.951350
346.127545	2931.708909	17.608794	-0.066257	2.947443
346.000305	2923.757843	17.613799	-0.066228	2.943565
345.681689	2915.843437	17.618803	-0.066164	2.939690
345.552634	2907.872147	17.623808	-0.066135	2.935792
345.659044	2899.849849	17.628813	-0.066149	2.931876
345.633708	2891.863577	17.633818	-0.066139	2.927966
345.389168	2883.877830	17.638823	-0.066089	2.924039
345.664485	2875.898810	17.643827	-0.066135	2.920138
345.509240	2867.947566	17.648832	-0.066101	2.916222
345.407357	2859.914935	17.653837	-0.066076	2.912263
345.441596	2851.913592	17.658842	-0.066078	2.908322
345.033514	2843.946448	17.663847	-0.065996	2.904369
345.464474	2835.937744	17.668851	-0.066071	2.900435
345.302349	2827.968797	17.673856	-0.066036	2.896484
344.949072	2820.061821	17.678861	-0.065965	2.892546
345.310183	2812.002000	17.683866	-0.066027	2.888568
345.263004	2803.998984	17.688871	-0.066013	2.884589
345.267020	2796.092201	17.693875	-0.066009	2.880656
345.415457	2788.075969	17.698880	-0.066031	2.876670
345.225655	2780.132745	17.703885	-0.065991	2.872697
345.378005	2772.121297	17.708890	-0.066014	2.868703
344.875806	2764.195130	17.713895	-0.065915	2.864710
345.049856	2756.226532	17.718899	-0.065942	2.860728
344.951675	2748.229009	17.723904	-0.065919	2.856710
345.115618	2740.221613	17.728909	-0.065944	2.852697
344.640201	2732.323183	17.733914	-0.065850	2.848696
344.441357	2724.313453	17.738919	-0.065808	2.844649
344.644592	2716.322359	17.743923	-0.065841	2.840629
344.813160	2708.303217	17.748928	-0.065867	2.836587
345.016057	2700.311198	17.753933	-0.065900	2.832556
344.914331	2692.353813	17.758938	-0.065875	2.828518
344.796440	2684.351297	17.763943	-0.065848	2.824450
345.195273	2676.374984	17.768947	-0.065917	2.820421
345.027522	2668.426350	17.773952	-0.065881	2.816366
344.929272	2660.463446	17.778957	-0.065857	2.812303
344.906481	2652.468500	17.783962	-0.065848	2.808221
344.216085	2644.568915	17.788967	-0.065714	2.804143
344.764358	2636.531461	17.793971	-0.065811	2.800062
344.984807	2628.524793	17.798976	-0.065847	2.795971
344.816822	2620.560521	17.803981	-0.065810	2.791873
344.717265	2612.589709	17.808986	-0.065787	2.787769
344.650843	2604.597718	17.813991	-0.065769	2.783651
344.641126	2596.655102	17.818995	-0.065762	2.779555
344.694053	2588.681182	17.824000	-0.065767	2.775441
344.634638	2580.700920	17.829005	-0.065751	2.771311
344.786900	2572.699777	17.834010	-0.065774	2.767176
344.660559	2564.731406	17.839015	-0.065745	2.763035
344.545879	2556.807300	17.844019	-0.065718	2.758912
344.648968	2548.805715	17.849024	-0.065732	2.754756
344.519846	2540.801215	17.854029	-0.065703	2.750577
344.086155	2532.890023	17.859034	-0.065617	2.746422
343.678660	2524.919875	17.864039	-0.065536	2.742232
344.289362	2516.860280	17.869043	-0.065645	2.738051
344.096230	2508.909933	17.874048	-0.065604	2.733872
344.188906	2500.889499	17.879053	-0.065616	2.729666
344.091503	2492.969426	17.884058	-0.065592	2.725496
343.568482	2485.078893	17.889063	-0.065490	2.721307
343.808246	2477.062893	17.894067	-0.065529	2.717094
343.772533	2469.069944	17.899072	-0.065517	2.712870
344.103085	2461.035820	17.904077	-0.065574	2.708640
344.160312	2453.053573	17.909082	-0.065579	2.704414
343.821452	2445.137020	17.914087	-0.065511	2.700190
343.857911	2437.197502	17.919091	-0.065512	2.695972
343.386884	2429.257622	17.924096	-0.065420	2.691714
343.759438	2421.177042	17.929101	-0.065484	2.687430
343.780054	2413.227946	17.934106	-0.065482	2.683185
343.847795	2405.258254	17.939111	-0.065490	2.678926
343.468302	2397.364018	17.944115	-0.065414	2.674671
343.440256	2389.351175	17.949120	-0.065403	2.670369
343.689653	2381.322458	17.954125	-0.065445	2.666070
343.422950	2373.404118	17.959130	-0.065390	2.661789
343.127901	2365.462820	17.964135	-0.065330	2.657487
343.130003	2357.496783	17.969139	-0.065325	2.653184
343.356060	2349.437324	17.974144	-0.065362	2.648839
342.998696	2341.530412	17.979149	-0.065290	2.644530
343.274815	2333.539496	17.984154	-0.065336	2.640211
342.947237	2325.617978	17.989159	-0.065270	2.635882
342.789325	2317.650217	17.994163	-0.065236	2.631532
342.968245	2309.615228	17.999168	-0.065264	2.627161
343.078891	2301.632548	18.004173	-0.065279	2.622807
343.212499	2293.661616	18.009178	-0.065299	2.618454
342.993856	2285.709747	18.014183	-0.065253	2.614079
343.024506	2277.731028	18.019187	-0.065253	2.609700
342.829094	2269.811026	18.024192	-0.065212	2.605330
342.427457	2261.888699	18.029197	-0.065132	2.600937
342.532346	2253.926769	18.034202	-0.065146	2.596550
342.584769	2245.842372	18.039207	-0.065151	2.592084
342.665332	2237.794794	18.044211	-0.065160	2.587632
342.551295	2229.844064	18.049216	-0.065134	2.583213
342.395542	2221.925469	18.054221	-0.065100	2.578802
342.332383	2213.974603	18.059226	-0.065083	2.574371
342.402334	2205.972182	18.064231	-0.065091	2.569914
342.507818	2197.997511	18.069235	-0.065105	2.565466
342.211327	2190.101691	18.074240	-0.065045	2.561027
342.504185	2182.088419	18.079245	-0.065094	2.556556
342.356045	2174.173047	18.084250	-0.065061	2.552100
342.092995	2166.221395	18.089255	-0.065007	2.547608
342.289637	2158.220362	18.094259	-0.065039	2.543114
341.860576	2150.318828	18.099264	-0.064954	2.538622
342.382085	2142.225626	18.104269	-0.065045	2.534083
342.125561	2134.333103	18.109274	-0.064992	2.529593
342.177034	2126.325764	18.114279	-0.064997	2.525052
342.511895	2118.355484	18.119283	-0.065054	2.520545
342.237691	2110.461776	18.124288	-0.064998	2.516029
342.181366	2102.489439	18.129293	-0.064982	2.511476
342.191498	2094.504426	18.134298	-0.064979	2.506912
342.149194	2086.530669	18.139303	-0.064966	2.502342
342.405059	2078.547698	18.144307	-0.065008	2.497781
342.093144	2070.627535	18.149312	-0.064945	2.493205
342.171384	2062.629537	18.154317	-0.064954	2.488605
341.704026	2054.741821	18.159322	-0.064862	2.484020
341.440582	2046.797777	18.164327	-0.064808	2.479408
341.667668	2038.818725	18.169331	-0.064845	2.474805
341.598081	2030.840577	18.174336	-0.064827	2.470171
341.467311	2022.865079	18.179341	-0.064797	2.465525
341.687404	2014.885331	18.184346	-0.064833	2.460895
341.756987	2006.905792	18.189351	-0.064841	2.456245
341.681604	1998.966835	18.194355	-0.064822	2.451599
341.730028	1990.977088	18.199360	-0.064825	2.446923
341.549560	1983.053844	18.204365	-0.064787	2.442260
341.736650	1975.094765	18.209370	-0.064816	2.437595
341.595045	1967.108614	18.214375	-0.064785	2.432880
341.535527	1959.142978	18.219379	-0.064768	2.428174
341.381321	1951.194070	18.224384	-0.064735	2.423462
341.448557	1943.226473	18.229389	-0.064742	2.418747
341.629065	1935.246639	18.234394	-0.064770	2.414024
341.521039	1927.292531	18.239399	-0.064745	2.409284
341.588468	1919.336940	18.244403	-0.064752	2.404548
341.428243	1911.416245	18.249408	-0.064717	2.399806
341.331192	1903.470246	18.254413	-0.064694	2.395043
341.577763	1895.493147	18.259418	-0.064735	2.390281
341.256875	1887.554147	18.264423	-0.064670	2.385486
341.097764	1879.629457	18.269427	-0.064635	2.380703
341.260856	1871.625592	18.274432	-0.064660	2.375888
341.390551	1863.657311	18.279437	-0.064679	2.371083
341.322720	1855.701181	18.284442	-0.064661	2.366259
341.226276	1847.761589	18.289447	-0.064638	2.361433
341.327036	1839.819207	18.294451	-0.064652	2.356612
341.162673	1831.875551	18.299456	-0.064616	2.351758
341.066572	1823.912541	18.304461	-0.064593	2.346888
341.225361	1815.940291	18.309466	-0.064617	2.342023
341.058551	1807.999938	18.314471	-0.064581	2.337141
341.057243	1800.057209	18.319475	-0.064576	2.332260
340.990651	1792.084060	18.324480	-0.064558	2.327346
340.953833	1784.137099	18.329485	-0.064546	2.322439
340.944639	1776.202144	18.334490	-0.064539	2.317532
340.883619	1768.246321	18.339495	-0.064523	2.312597
340.686157	1760.328299	18.344499	-0.064481	2.307663
340.552864	1752.370125	18.349504	-0.064451	2.302699
340.792695	1744.379935	18.354509	-0.064490	2.297737
340.657654	1736.456901	18.359514	-0.064460	2.292773
340.650096	1728.473710	18.364519	-0.064453	2.287772
340.668874	1720.533380	18.369523	-0.064452	2.282790
340.641541	1712.601145	18.374528	-0.064441	2.277797
340.818527	1704.624766	18.379533	-0.064469	2.272784
340.601289	1696.667915	18.384538	-0.064423	2.267737
340.487651	1688.715460	18.389543	-0.064397	2.262691
340.532376	1680.779833	18.394547	-0.064400	2.257658
340.373444	1672.841297	18.399552	-0.064365	2.252594
340.299836	1664.896785	18.404557	-0.064347	2.247522
340.397141	1656.938479	18.409562	-0.064360	2.242445
340.135073	1649.028098	18.414567	-0.064306	2.237356
339.898272	1641.121891	18.419571	-0.064256	2.232259
340.155157	1633.101891	18.424576	-0.064299	2.227122
340.035141	1625.167818	18.429581	-0.064271	2.221995
339.935940	1617.259804	18.434586	-0.064248	2.216874
339.898664	1609.286519	18.439591	-0.064236	2.211705
340.073843	1601.324631	18.444595	-0.064263	2.206551
340.132712	1593.359839	18.449600	-0.064269	2.201372
339.879492	1585.481431	18.454605	-0.064217	2.196208
339.780637	1577.556871	18.459610	-0.064193	2.191017
339.477101	1569.622948	18.464615	-0.064131	2.185787
339.607442	1561.657319	18.469619	-0.064150	2.180565
339.550036	1553.701701	18.474624	-0.064135	2.175319
339.594560	1545.741057	18.479629	-0.064138	2.170067
339.300011	1537.851666	18.484634	-0.064078	2.164817
338.968413	1529.956135	18.489639	-0.064011	2.159547
338.865233	1522.054844	18.494643	-0.063986	2.154282
339.151778	1514.033948	18.499648	-0.064035	2.148961
338.691322	1506.127747	18.504653	-0.063944	2.143632
338.933071	1498.165772	18.509658	-0.063983	2.138320
339.246344	1490.135786	18.514663	-0.064037	2.132956
339.060986	1482.254919	18.519667	-0.063997	2.127631
339.128983	1474.294463	18.524672	-0.064004	2.122263
339.197378	1466.369911	18.529677	-0.064012	2.116906
339.019924	1458.453885	18.534682	-0.063974	2.111517
338.548341	1450.545646	18.539687	-0.063881	2.106090
338.941302	1442.547786	18.544691	-0.063949	2.100674
338.585134	1434.673557	18.549696	-0.063877	2.095254
338.709342	1426.701061	18.554701	-0.063895	2.089800
339.031415	1418.709276	18.559706	-0.063950	2.084339
338.532447	1410.892962	18.564711	-0.063852	2.078902
338.135226	1403.018725	18.569715	-0.063773	2.073420
338.364469	1395.014874	18.574720	-0.063810	2.067898
338.278884	1387.078830	18.579725	-0.063789	2.062376
338.609584	1379.114580	18.584730	-0.063846	2.056862
338.371902	1371.205669	18.589735	-0.063796	2.051314
338.568858	1363.242071	18.594739	-0.063828	2.045757
338.277235	1355.385070	18.599744	-0.063768	2.040209
338.120992	1347.479404	18.604749	-0.063734	2.034626
338.420417	1339.498591	18.609754	-0.063785	2.029021
338.316667	1331.558076	18.614759	-0.063760	2.023388
338.449561	1323.633854	18.619763	-0.063780	2.017776
338.357199	1315.717909	18.624768	-0.063757	2.012129
338.365664	1307.782613	18.629773	-0.063754	2.006464
338.200889	1299.911798	18.634778	-0.063718	2.000811
337.807974	1292.042402	18.639783	-0.063640	1.995118
338.016939	1284.083246	18.644787	-0.063673	1.989408
338.248685	1276.105136	18.649792	-0.063711	1.983671
338.209530	1268.197289	18.654797	-0.063699	1.977939
338.002274	1260.330460	18.659802	-0.063655	1.972202
338.006587	1252.383695	18.664807	-0.063651	1.966413
337.642497	1244.542270	18.669811	-0.063578	1.960644
337.809932	1236.569857	18.674816	-0.063604	1.954819
337.793244	1228.665287	18.679821	-0.063596	1.949007
337.849324	1220.718554	18.684826	-0.063601	1.943155
337.626904	1212.827802	18.689831	-0.063554	1.937295
337.552486	1204.920015	18.694835	-0.063535	1.931421
337.547408	1196.984343	18.699840	-0.063529	1.925516
337.433546	1189.095728	18.704845	-0.063503	1.919616
337.384104	1181.215203	18.709850	-0.063488	1.913712
337.433083	1173.253981	18.714855	-0.063492	1.907739
337.405674	1165.343505	18.719859	-0.063482	1.901777
337.434067	1157.418182	18.724864	-0.063482	1.895792
337.474891	1149.496605	18.729869	-0.063485	1.889792
337.553974	1141.602474	18.734874	-0.063494	1.883798
337.118330	1133.770340	18.739879	-0.063408	1.877773
337.013543	1125.878856	18.744883	-0.063383	1.871721
337.064357	1117.932483	18.749888	-0.063388	1.865625
336.915624	1110.051706	18.754893	-0.063355	1.859537
336.947373	1102.147941	18.759898	-0.063356	1.853432
337.063552	1094.194060	18.764903	-0.063372	1.847278
337.001153	1086.325280	18.769907	-0.063355	1.841149
336.563856	1078.493991	18.774912	-0.063269	1.834983
336.787312	1070.533876	18.779917	-0.063305	1.828775
336.458091	1062.692890	18.784922	-0.063239	1.822573
336.153496	1054.836901	18.789927	-0.063177	1.816341
336.651296	1046.826113	18.794931	-0.063264	1.810062
337.027030	1038.877248	18.799936	-0.063329	1.803797
336.793707	1031.047651	18.804941	-0.063281	1.797529
336.573737	1023.182850	18.809946	-0.063235	1.791213
336.498749	1015.258328	18.814951	-0.063215	1.784844
336.474390	1007.397175	18.819955	-0.063206	1.778510
336.218480	999.531309	18.824960	-0.063153	1.772121
336.318512	991.617068	18.829965	-0.063167	1.765714
336.254358	983.755944	18.834970	-0.063149	1.759306
336.297898	975.866749	18.839975	-0.063152	1.752865
336.220868	967.986605	18.844979	-0.063133	1.746393
336.072622	960.131167	18.849984	-0.063100	1.739907
336.026962	952.248062	18.854989	-0.063087	1.733388
336.252349	944.320382	18.859994	-0.063123	1.726843
336.194861	936.455644	18.864999	-0.063108	1.720288
336.290592	928.595219	18.870003	-0.063120	1.713732
336.343022	920.696162	18.875008	-0.063125	1.707112
336.100087	912.865651	18.880013	-0.063075	1.700485
336.214541	904.985488	18.885018	-0.063091	1.693838
336.067925	897.113599	18.890023	-0.063058	1.687137
335.941036	889.279448	18.895027	-0.063030	1.680443
335.847139	881.427817	18.900032	-0.063007	1.673713
335.732997	873.574392	18.905037	-0.062981	1.666951
335.589448	865.731926	18.910042	-0.062949	1.660166
335.752105	857.822405	18.915047	-0.062974	1.653339
335.805697	849.957902	18.920051	-0.062979	1.646506
334.974741	842.254658	18.925056	-0.062819	1.639663
335.197251	834.325359	18.930061	-0.062855	1.632740
335.138928	826.444849	18.935066	-0.062839	1.625792
335.163437	818.566418	18.940071	-0.062839	1.618826
335.407148	810.672559	18.945075	-0.062879	1.611849
335.138891	802.846517	18.950080	-0.062824	1.604828
335.002092	795.036728	18.955085	-0.062793	1.597810
334.875924	787.206140	18.960090	-0.062765	1.590744
334.643793	779.387539	18.965095	-0.062716	1.583641
334.781013	771.529939	18.970099	-0.062737	1.576525
334.843951	763.652505	18.975104	-0.062743	1.569348
334.775528	755.820674	18.980109	-0.062726	1.562160
334.786488	748.003385	18.985114	-0.062722	1.554965
334.705030	740.168326	18.990119	-0.062702	1.547705
334.860760	732.306519	18.995123	-0.062726	1.540422
334.804185	724.495321	19.000128	-0.062710	1.533120
334.704994	716.666846	19.005133	-0.062687	1.525760
334.568569	708.892483	19.010138	-0.062656	1.518409
334.562496	701.053679	19.015143	-0.062650	1.510982
334.299895	693.288229	19.020147	-0.062596	1.503548
334.368278	685.441973	19.025152	-0.062604	1.496052
334.568620	677.588794	19.030157	-0.062636	1.488531
334.173086	669.868833	19.035162	-0.062557	1.481008
334.092860	662.063452	19.040167	-0.062537	1.473412
333.999689	654.228848	19.045171	-0.062515	1.465747
333.983055	646.428664	19.050176	-0.062507	1.458088
333.748744	638.649239	19.055181	-0.062458	1.450373
333.790550	630.836333	19.060186	-0.062461	1.442629
333.524781	623.092755	19.065191	-0.062406	1.434861
333.569627	615.294331	19.070195	-0.062409	1.427048
333.700810	607.469963	19.075200	-0.062429	1.419180
333.687623	599.672860	19.080205	-0.062421	1.411272
333.758354	591.889252	19.085210	-0.062429	1.403346
333.309838	584.209381	19.090215	-0.062341	1.395394
333.534026	576.376924	19.095219	-0.062377	1.387354
333.256713	568.645619	19.100224	-0.062321	1.379286
333.712971	560.781748	19.105229	-0.062401	1.371159
333.743607	553.023931	19.110234	-0.062401	1.363021
333.399407	545.345694	19.115239	-0.062332	1.354852
333.647914	537.548918	19.120243	-0.062373	1.346613
333.569641	529.821755	19.125248	-0.062354	1.338339
333.258075	522.131234	19.130253	-0.062291	1.330010
333.396700	514.373453	19.135258	-0.062311	1.321639
333.175509	506.655773	19.140263	-0.062265	1.313191
333.287839	498.835889	19.145267	-0.062281	1.304638
333.103865	491.143405	19.150272	-0.062242	1.296115
333.095746	483.417857	19.155277	-0.062235	1.287531
332.940881	475.739559	19.160282	-0.062201	1.278915
332.744726	468.054403	19.165287	-0.062160	1.270224
332.581279	460.380474	19.170291	-0.062124	1.261493
332.841191	452.626140	19.175296	-0.062168	1.252691
332.939293	444.896643	19.180301	-0.062181	1.243823
332.836718	437.249038	19.185306	-0.062157	1.234948
332.442147	429.628283	19.190311	-0.062078	1.225981
332.434367	421.955449	19.195315	-0.062072	1.216965
332.395943	414.272755	19.200320	-0.062060	1.207863
331.990141	406.679834	19.205325	-0.061979	1.198725
332.086919	398.999301	19.210330	-0.061992	1.189514
332.067536	391.333187	19.215335	-0.061984	1.180224
332.169498	383.668650	19.220339	-0.061998	1.170888
332.003582	376.071493	19.225344	-0.061962	1.161504
331.609627	368.499211	19.230349	-0.061884	1.152026
331.774974	360.824110	19.235354	-0.061909	1.142460
331.942375	353.168314	19.240359	-0.061936	1.132838
331.782841	345.596635	19.245363	-0.061901	1.123170
331.340894	338.083341	19.250368	-0.061814	1.113430
331.470450	330.454035	19.255373	-0.061833	1.103581
331.374605	322.897180	19.260378	-0.061810	1.093688
331.168725	315.340747	19.265383	-0.061767	1.083680
331.379480	307.753360	19.270387	-0.061801	1.073633
331.394402	300.196252	19.275392	-0.061799	1.063486
331.075841	292.707735	19.280397	-0.061735	1.053256
331.001186	285.189515	19.285402	-0.061716	1.042944
331.259719	277.626862	19.290407	-0.061759	1.032547
330.946080	270.184190	19.295411	-0.061696	1.022073
330.570852	262.748308	19.300416	-0.061621	1.011484
331.019439	255.182523	19.305421	-0.061700	1.000803
330.827772	247.749480	19.310426	-0.061659	0.990038
330.706658	240.293526	19.315431	-0.061632	0.979139
330.730606	232.852472	19.320435	-0.061632	0.968176
330.229629	225.520165	19.325440	-0.061534	0.957114
330.171676	218.110150	19.330445	-0.061518	0.945921
329.703375	210.806146	19.335450	-0.061426	0.934647
329.887405	203.369319	19.340455	-0.061455	0.923207
329.941669	196.009120	19.345459	-0.061461	0.911707
329.640052	188.709628	19.350464	-0.061400	0.900058
329.713513	181.366189	19.355469	-0.061409	0.888291
329.944785	174.024740	19.360474	-0.061447	0.876416
329.455788	166.832940	19.365479	-0.061351	0.864415
329.778909	159.514676	19.370483	-0.061407	0.852272
329.688276	152.302453	19.375488	-0.061385	0.840011
329.259131	145.158382	19.380493	-0.061300	0.827583
329.623665	137.894637	19.385498	-0.061364	0.815002
329.147164	130.815113	19.390503	-0.061270	0.802286
329.136917	123.697379	19.395507	-0.061264	0.789446
328.701118	116.665635	19.400512	-0.061178	0.776413
328.962737	109.538717	19.405517	-0.061222	0.763212
328.808487	102.538147	19.410522	-0.061189	0.749878
328.110392	95.648178	19.415527	-0.061054	0.736330
328.618665	88.574739	19.420531	-0.061144	0.722590
328.561443	81.659361	19.425536	-0.061129	0.708699
328.584308	74.939412	19.430541	-0.061129	0.694964