Fri Apr 16 18:59:29 2021

Number of Points = 3641
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.603923	0.125550	0.000000	0.000123	0.312655

1.169584	0.020061	0.005005	0.000017	0.312643
1.440343	-0.030858	0.010010	-0.000033	0.312635
1.193638	0.014053	0.015014	0.000013	0.312636
1.341978	-0.010489	0.020019	-0.000015	0.312647
1.189826	0.014807	0.025024	0.000014	0.312637
1.297696	-0.003905	0.030029	-0.000007	0.312641
1.221442	0.009576	0.035034	0.000008	0.312639
1.310191	-0.008484	0.040038	-0.000009	0.312631
1.131976	0.026615	0.045043	0.000024	0.312643
1.262416	0.000370	0.050048	-0.000000	0.312632
1.313556	-0.007964	0.055053	-0.000010	0.312636
1.328966	-0.017591	0.060058	-0.000013	0.312605
1.147688	-0.046513	0.065062	0.000021	0.312319
1.485205	-0.106324	0.070067	-0.000042	0.312326
1.281688	-0.070843	0.075072	-0.000004	0.312319
1.479316	-0.105260	0.080077	-0.000041	0.312326
1.412447	-0.093505	0.085082	-0.000028	0.312325
1.322959	-0.078815	0.090086	-0.000012	0.312318
1.182028	-0.050273	0.095091	0.000014	0.312331
0.906532	-0.061686	0.100096	0.000066	0.312047
1.194086	-0.124567	0.105101	0.000012	0.311998
1.141634	-0.113057	0.110106	0.000022	0.312007
1.274520	-0.140230	0.115110	-0.000003	0.311993
1.411754	-0.163396	0.120115	-0.000029	0.312002
1.185171	-0.143409	0.125120	0.000014	0.311904
1.311580	-0.208161	0.130125	-0.000010	0.311710
1.225626	-0.192546	0.135130	0.000006	0.311710
1.332208	-0.213967	0.140134	-0.000014	0.311701
1.290899	-0.203096	0.145139	-0.000006	0.311717
0.962140	-0.212309	0.150144	0.000055	0.311397
1.312515	-0.279930	0.155149	-0.000010	0.311378
1.131945	-0.245576	0.160154	0.000023	0.311386
1.061163	-0.236363	0.165158	0.000036	0.311369
1.241236	-0.330227	0.170163	0.000003	0.311085
1.054542	-0.299545	0.175168	0.000038	0.311070
0.782415	-0.248223	0.180173	0.000088	0.311079
0.901688	-0.291434	0.185178	0.000066	0.310979
0.543510	-0.271226	0.190182	0.000133	0.310771
0.664939	-0.292219	0.195187	0.000110	0.310776
0.668346	-0.295107	0.200192	0.000109	0.310765
0.724325	-0.348030	0.205197	0.000099	0.310567
1.295549	-0.465035	0.210202	-0.000007	0.310505
0.862241	-0.385039	0.215206	0.000073	0.310511
0.881968	-0.441661	0.220211	0.000069	0.310264
0.750468	-0.437486	0.225216	0.000094	0.310172
0.673703	-0.421984	0.230221	0.000108	0.310180
0.667494	-0.473135	0.235226	0.000109	0.309936
0.967767	-0.546943	0.240230	0.000053	0.309847
1.221091	-0.601348	0.245235	0.000006	0.309808
0.906000	-0.606712	0.250240	0.000065	0.309515
1.186249	-0.657264	0.255245	0.000013	0.309517
1.074123	-0.675560	0.260250	0.000033	0.309337
0.806536	-0.648911	0.265254	0.000083	0.309234
0.955506	-0.690504	0.270259	0.000055	0.309166
0.878471	-0.732778	0.275264	0.000070	0.308903
0.766283	-0.710846	0.280269	0.000091	0.308910
0.866724	-0.789132	0.285274	0.000072	0.308629
0.858797	-0.796434	0.290278	0.000073	0.308589
1.052043	-0.877639	0.295283	0.000037	0.308373
1.034999	-0.898325	0.300288	0.000041	0.308261
0.974299	-0.921777	0.305293	0.000052	0.308100
1.024354	-0.956815	0.310298	0.000042	0.307978
0.682254	-0.930696	0.315302	0.000106	0.307809
1.091003	-1.040651	0.320307	0.000030	0.307641
0.794871	-1.024449	0.325312	0.000085	0.307465
0.908216	-1.075020	0.330317	0.000064	0.307324
0.910911	-1.115925	0.335322	0.000063	0.307134
1.022137	-1.167111	0.340326	0.000043	0.306988
1.071694	-1.219238	0.345331	0.000034	0.306785
0.803544	-1.186822	0.350336	0.000083	0.306708
0.877218	-1.263694	0.355341	0.000070	0.306409
1.312920	-1.362752	0.360346	-0.000011	0.306315
0.937986	-1.347293	0.365350	0.000058	0.306066
1.038030	-1.396464	0.370355	0.000040	0.305920
1.146995	-1.452944	0.375360	0.000019	0.305747
1.056424	-1.480627	0.380365	0.000036	0.305538
1.302682	-1.550665	0.385370	-0.000010	0.305418
1.185779	-1.588592	0.390374	0.000012	0.305138
0.912122	-1.579274	0.395379	0.000063	0.304947
1.026552	-1.629018	0.400384	0.000042	0.304810
1.230656	-1.732382	0.405389	0.000004	0.304495
1.161528	-1.750708	0.410394	0.000017	0.304348
1.012324	-1.755497	0.415398	0.000044	0.304197
1.042367	-1.825574	0.420403	0.000039	0.303890
0.965912	-1.849958	0.425408	0.000053	0.303708
0.940098	-1.879947	0.430413	0.000058	0.303543
0.420840	-1.842860	0.435418	0.000154	0.303270
0.603924	-1.915456	0.440422	0.000120	0.303082
0.695666	-1.963524	0.445427	0.000103	0.302933
0.698489	-2.027725	0.450432	0.000103	0.302628
0.512480	-2.041140	0.455437	0.000137	0.302403
0.644321	-2.102952	0.460442	0.000113	0.302222
0.468686	-2.120058	0.465446	0.000145	0.301987
0.544244	-2.184643	0.470451	0.000131	0.301744
0.665706	-2.252750	0.475456	0.000109	0.301523
0.718248	-2.307755	0.480461	0.000099	0.301305
0.749283	-2.365421	0.485466	0.000093	0.301056
0.479649	-2.373337	0.490470	0.000143	0.300782
0.578922	-2.424608	0.495475	0.000125	0.300622
0.415879	-2.437093	0.500480	0.000155	0.300420
0.615242	-2.527785	0.505485	0.000118	0.300158
0.457359	-2.558447	0.510490	0.000147	0.299872
0.564617	-2.630829	0.515494	0.000127	0.299617
0.766181	-2.715873	0.520499	0.000090	0.299383
0.747753	-2.763936	0.525504	0.000093	0.299135
0.359685	-2.744318	0.530509	0.000165	0.298889
0.281412	-2.793711	0.535514	0.000180	0.298581
-0.007634	-2.792573	0.540518	0.000234	0.298332
-0.179844	-2.803906	0.545523	0.000266	0.298125
-0.477176	-2.798756	0.550528	0.000321	0.297888
-2.342130	-2.511117	0.555533	0.000668	0.297639
-5.086453	-2.064132	0.560538	0.001179	0.297387
-4.879569	-2.117587	0.565542	0.001140	0.297310
-4.749564	-2.199339	0.570547	0.001116	0.297028
-4.940730	-2.176661	0.575552	0.001152	0.296969
-5.527998	-2.122880	0.580557	0.001261	0.296711
-5.446810	-2.141968	0.585562	0.001246	0.296690
-5.978717	-2.108430	0.590566	0.001345	0.296382
-6.422602	-2.028431	0.595571	0.001427	0.296379
-6.512554	-2.073998	0.600576	0.001444	0.296077
-6.613891	-2.055388	0.605581	0.001463	0.296078
-6.677827	-2.106665	0.610586	0.001475	0.295771
-6.650633	-2.116680	0.615590	0.001470	0.295746
-6.649384	-2.161505	0.620595	0.001469	0.295528
-7.360028	-2.036380	0.625600	0.001602	0.295508
-7.747036	-2.022122	0.630605	0.001674	0.295234
-7.453566	-2.087206	0.635610	0.001619	0.295177
-7.921109	-2.046323	0.640614	0.001706	0.294961
-8.251205	-2.006669	0.645619	0.001767	0.294861
-7.968605	-2.088979	0.650624	0.001715	0.294709
-8.031863	-2.117204	0.655629	0.001726	0.294514
-8.209330	-2.100997	0.660634	0.001759	0.294436
-8.332568	-2.123797	0.665638	0.001782	0.294214
-8.262162	-2.144449	0.670643	0.001769	0.294175
-8.805051	-2.105499	0.675648	0.001870	0.293882
-8.613914	-2.139920	0.680653	0.001835	0.293883
-9.191876	-2.093486	0.685658	0.001942	0.293595
-9.457136	-2.048687	0.690662	0.001991	0.293578
-9.653994	-2.055776	0.695667	0.002028	0.293367
-9.842785	-2.043509	0.700672	0.002063	0.293258
-9.488215	-2.130620	0.705677	0.001997	0.293147
-10.080720	-2.059105	0.710682	0.002107	0.292968
-10.224581	-2.037383	0.715686	0.002134	0.292947
-10.544859	-2.038789	0.720691	0.002194	0.292652
-10.701958	-2.013046	0.725696	0.002223	0.292638
-10.781119	-2.038934	0.730701	0.002238	0.292439
-10.611804	-2.094473	0.735706	0.002206	0.292317
-11.040802	-2.031318	0.740710	0.002286	0.292244
-11.592049	-1.979024	0.745715	0.002388	0.292007
-11.574975	-1.983242	0.750720	0.002385	0.292001
-11.260450	-2.081382	0.755725	0.002327	0.291799
-11.626429	-2.032928	0.760730	0.002395	0.291709
-11.535508	-2.070644	0.765734	0.002378	0.291604
-11.695570	-2.089037	0.770739	0.002408	0.291369
-11.983216	-2.036894	0.775744	0.002461	0.291368
-12.321100	-2.026991	0.780749	0.002524	0.291112
-12.319127	-2.037307	0.785754	0.002524	0.291063
-12.356668	-2.053134	0.790758	0.002530	0.290951
-12.648878	-2.040580	0.795763	0.002585	0.290749
-12.667235	-2.037847	0.800768	0.002588	0.290746
-12.701762	-2.074790	0.805773	0.002595	0.290531
-12.843859	-2.057338	0.810778	0.002621	0.290490
-13.293934	-1.999659	0.815782	0.002705	0.290370
-13.249320	-2.052161	0.820787	0.002696	0.290149
-13.546027	-1.997203	0.825792	0.002752	0.290154
-13.623039	-2.034852	0.830797	0.002766	0.289896
-13.652337	-2.042286	0.835802	0.002771	0.289833
-13.797575	-2.035103	0.840806	0.002798	0.289737
-14.027246	-2.040276	0.845811	0.002841	0.289503
-14.237675	-2.002426	0.850816	0.002880	0.289501
-14.326575	-2.022760	0.855821	0.002897	0.289319
-14.699559	-1.973263	0.860826	0.002966	0.289227
-15.070221	-1.906182	0.865830	0.003035	0.289226
-14.898738	-1.998985	0.870835	0.003003	0.288918
-15.283133	-1.936067	0.875840	0.003075	0.288883
-15.153705	-1.972677	0.880845	0.003050	0.288818
-14.996110	-2.051501	0.885850	0.003021	0.288566
-15.271018	-2.002712	0.890854	0.003072	0.288561
-15.732725	-1.950596	0.895859	0.003158	0.288401
-15.698254	-1.988905	0.900864	0.003152	0.288241
-15.564959	-2.013239	0.905869	0.003127	0.288240
-15.531023	-2.068710	0.910874	0.003120	0.287993
-16.320468	-1.931569	0.915878	0.003267	0.287961
-16.003538	-2.001984	0.920883	0.003208	0.287897
-16.385289	-1.987045	0.925888	0.003279	0.287623
-16.805009	-1.910184	0.930893	0.003357	0.287626
-16.652306	-1.962989	0.935898	0.003329	0.287501
-16.752095	-1.984072	0.940902	0.003348	0.287303
-16.805866	-1.971934	0.945907	0.003357	0.287315
-17.001937	-1.981239	0.950912	0.003394	0.287089
-16.926756	-2.016907	0.955917	0.003380	0.286978
-17.018637	-2.001333	0.960922	0.003397	0.286973
-17.475440	-1.975231	0.965926	0.003482	0.286686
-17.055653	-2.051785	0.970931	0.003404	0.286685
-17.126668	-2.066302	0.975936	0.003417	0.286546
-17.619464	-2.016654	0.980941	0.003509	0.286345
-17.403190	-2.054684	0.985946	0.003468	0.286352
-17.571565	-2.076308	0.990950	0.003500	0.286088
-18.003111	-2.005550	0.995955	0.003580	0.286049
-18.172335	-1.986963	1.000960	0.003611	0.285988
-18.272753	-2.019210	1.005965	0.003630	0.285732
-18.254717	-2.021246	1.010970	0.003627	0.285739
-18.894929	-1.931191	1.015974	0.003746	0.285605
-18.940264	-1.947093	1.020979	0.003754	0.285483
-18.669087	-1.997531	1.025984	0.003704	0.285478
-19.242734	-1.941479	1.030989	0.003810	0.285233
-19.329371	-1.944244	1.035994	0.003827	0.285139
-19.052917	-1.997923	1.040998	0.003775	0.285122
-18.968759	-2.070283	1.046003	0.003759	0.284833
-19.371529	-2.000639	1.051008	0.003834	0.284815
-19.306542	-2.035580	1.056013	0.003822	0.284697
-19.268254	-2.082807	1.061018	0.003815	0.284493
-19.825705	-1.983363	1.066022	0.003919	0.284483
-19.744877	-2.037903	1.071027	0.003904	0.284281
-20.135455	-1.980660	1.076032	0.003976	0.284211
-20.190527	-1.976483	1.081037	0.003987	0.284181
-20.387479	-2.001482	1.086042	0.004023	0.283872
-20.554379	-1.971069	1.091046	0.004054	0.283872
-20.403421	-2.019506	1.096051	0.004026	0.283765
-21.128861	-1.927793	1.101056	0.004161	0.283561
-20.774410	-1.992250	1.106061	0.004095	0.283561
-21.010681	-1.981187	1.111066	0.004139	0.283398
-21.898082	-1.849619	1.116070	0.004304	0.283246
-21.816107	-1.861638	1.121075	0.004289	0.283261
-21.260684	-1.998311	1.126080	0.004185	0.283079
-22.019059	-1.884984	1.131085	0.004326	0.282954
-21.826093	-1.917995	1.136090	0.004291	0.282964
-21.911452	-1.952754	1.141094	0.004306	0.282707
-21.863150	-1.979328	1.146099	0.004297	0.282616
-21.897605	-1.975095	1.151104	0.004304	0.282606
-22.118685	-1.996583	1.156109	0.004345	0.282290
-22.005829	-2.015791	1.161114	0.004324	0.282297
-22.532060	-1.940269	1.166118	0.004422	0.282194
-22.465849	-1.995475	1.171123	0.004409	0.281973
-22.245754	-2.036019	1.176128	0.004368	0.281970
-22.860103	-1.960422	1.181133	0.004483	0.281785
-23.097267	-1.935853	1.186138	0.004527	0.281690
-22.857861	-1.980884	1.191142	0.004482	0.281682
-22.919583	-2.024980	1.196147	0.004494	0.281398
-23.432009	-1.941284	1.201152	0.004589	0.281350
-23.308735	-1.973226	1.206157	0.004566	0.281301
-23.157292	-2.051406	1.211162	0.004538	0.281040
-23.504277	-1.989885	1.216166	0.004602	0.281033
-23.662465	-1.991685	1.221171	0.004632	0.280875
-23.965057	-1.965721	1.226176	0.004688	0.280726
-24.105460	-1.938445	1.231181	0.004714	0.280735
-24.064476	-1.979143	1.236186	0.004706	0.280564
-24.374221	-1.938002	1.241190	0.004764	0.280486
-23.919139	-2.025757	1.246195	0.004679	0.280460
-24.329016	-2.012049	1.251200	0.004756	0.280146
-24.673022	-1.950199	1.256205	0.004820	0.280143
-24.262448	-2.050078	1.261210	0.004743	0.280013
-24.834864	-1.982779	1.266214	0.004850	0.279823
-24.775797	-1.991575	1.271219	0.004839	0.279833
-24.921438	-2.015128	1.276224	0.004866	0.279574
-25.189257	-1.980350	1.281229	0.004916	0.279502
-25.307110	-1.964117	1.286234	0.004937	0.279476
-25.902239	-1.906248	1.291238	0.005048	0.279215
-25.620148	-1.955670	1.296243	0.004996	0.279225
-25.607618	-1.980746	1.301248	0.004993	0.279107
-26.381541	-1.882728	1.306253	0.005137	0.278885
-25.944093	-1.960511	1.311258	0.005056	0.278895
-26.095275	-1.967265	1.316262	0.005084	0.278717
-26.929312	-1.840718	1.321267	0.005239	0.278587
-26.490872	-1.920964	1.326272	0.005157	0.278584
-26.515520	-1.960462	1.331277	0.005162	0.278356
-27.075711	-1.876979	1.336282	0.005266	0.278261
-26.866049	-1.917949	1.341286	0.005227	0.278246
-26.741347	-1.987242	1.346291	0.005204	0.278004
-27.086973	-1.932349	1.351296	0.005268	0.277962
-27.094535	-1.941087	1.356301	0.005270	0.277910
-27.163429	-1.983225	1.361306	0.005282	0.277625
-27.337032	-1.951947	1.366310	0.005315	0.277624
-27.331498	-1.980541	1.371315	0.005314	0.277480
-27.591023	-1.966625	1.376320	0.005362	0.277307
-27.674580	-1.951148	1.381325	0.005377	0.277309
-28.072073	-1.922222	1.386330	0.005451	0.277082
-28.510828	-1.861570	1.391334	0.005533	0.276983
-28.203004	-1.916321	1.396339	0.005476	0.276989
-28.150497	-1.974687	1.401344	0.005466	0.276734
-28.846468	-1.855677	1.406349	0.005595	0.276695
-28.519203	-1.920416	1.411354	0.005534	0.276668
-28.686120	-1.948971	1.416358	0.005565	0.276360
-28.811218	-1.924839	1.421363	0.005589	0.276367
-29.162881	-1.875960	1.426368	0.005654	0.276288
-29.199675	-1.912594	1.431373	0.005661	0.276061
-29.179206	-1.915511	1.436378	0.005657	0.276066
-29.549323	-1.880485	1.441382	0.005726	0.275897
-29.588436	-1.901969	1.446387	0.005733	0.275747
-29.453816	-1.926969	1.451392	0.005708	0.275744
-29.678665	-1.921324	1.456397	0.005750	0.275560
-29.964276	-1.879762	1.461402	0.005803	0.275505
-29.614358	-1.945819	1.466406	0.005738	0.275493
-29.824769	-1.970988	1.471411	0.005777	0.275159
-30.058399	-1.930481	1.476416	0.005820	0.275149
-30.282603	-1.907070	1.481421	0.005862	0.275058
-30.504028	-1.906729	1.486426	0.005903	0.274848
-30.650834	-1.882105	1.491430	0.005931	0.274837
-30.535037	-1.936902	1.496435	0.005909	0.274660
-30.788100	-1.918783	1.501440	0.005956	0.274513
-30.889375	-1.901037	1.506445	0.005975	0.274510
-30.936529	-1.936190	1.511450	0.005984	0.274279
-31.405518	-1.861958	1.516454	0.006071	0.274221
-31.157385	-1.911982	1.521459	0.006025	0.274195
-31.354304	-1.935032	1.526464	0.006061	0.273885
-31.411939	-1.924838	1.531469	0.006072	0.273883
-31.361013	-1.957978	1.536474	0.006062	0.273757
-31.820479	-1.910026	1.541478	0.006148	0.273569
-31.318857	-2.001255	1.546483	0.006055	0.273569
-31.554266	-2.006489	1.551488	0.006098	0.273315
-32.422577	-1.860990	1.556493	0.006260	0.273250
-32.018080	-1.940643	1.561498	0.006185	0.273218
-32.282946	-1.940799	1.566502	0.006234	0.272962
-32.259477	-1.945595	1.571507	0.006229	0.272959
-32.411846	-1.948363	1.576512	0.006258	0.272798
-32.682939	-1.932386	1.581517	0.006308	0.272621
-32.554174	-1.953621	1.586522	0.006284	0.272633
-32.874684	-1.948475	1.591526	0.006344	0.272350
-33.082378	-1.917439	1.596531	0.006382	0.272315
-32.962126	-1.951997	1.601536	0.006360	0.272248
-33.335525	-1.933711	1.606541	0.006429	0.271984
-33.141864	-1.966962	1.611546	0.006393	0.271995
-33.563166	-1.924623	1.616550	0.006472	0.271812
-33.742492	-1.914263	1.621555	0.006505	0.271694
-33.779433	-1.906987	1.626560	0.006512	0.271697
-34.034543	-1.916012	1.631565	0.006559	0.271402
-34.037792	-1.919973	1.636570	0.006560	0.271378
-34.377226	-1.869557	1.641574	0.006623	0.271318
-34.554201	-1.883706	1.646579	0.006656	0.271070
-34.324461	-1.927465	1.651584	0.006613	0.271060
-34.595873	-1.904446	1.656589	0.006664	0.270920
-34.752515	-1.908184	1.661594	0.006693	0.270748
-34.761681	-1.907756	1.666598	0.006694	0.270741
-35.031571	-1.892964	1.671603	0.006745	0.270558
-35.154324	-1.882275	1.676608	0.006767	0.270496
-35.025595	-1.910035	1.681613	0.006743	0.270473
-34.818047	-2.009307	1.686618	0.006705	0.270143
-35.418269	-1.901610	1.691622	0.006816	0.270136
-35.306953	-1.948830	1.696627	0.006796	0.269991
-35.473963	-1.948952	1.701632	0.006827	0.269828
-35.441800	-1.956209	1.706637	0.006821	0.269821
-35.731916	-1.958043	1.711642	0.006875	0.269528
-35.831398	-1.947343	1.716646	0.006893	0.269488
-35.837297	-1.963698	1.721651	0.006894	0.269395
-36.285353	-1.915810	1.726656	0.006978	0.269214
-36.276204	-1.918159	1.731661	0.006976	0.269211
-35.974470	-2.018126	1.736666	0.006920	0.268969
-36.917072	-1.863667	1.741670	0.007095	0.268877
-37.128441	-1.826570	1.746675	0.007134	0.268870
-36.957263	-1.912593	1.751680	0.007103	0.268575
-37.111846	-1.885258	1.756685	0.007131	0.268571
-37.188154	-1.891731	1.761690	0.007145	0.268461
-37.314278	-1.909569	1.766694	0.007169	0.268241
-37.052585	-1.956506	1.771699	0.007120	0.268245
-37.525442	-1.909201	1.776704	0.007208	0.268036
-38.000120	-1.837853	1.781709	0.007296	0.267956
-37.170975	-1.993801	1.786714	0.007142	0.267928
-38.081619	-1.886774	1.791718	0.007311	0.267611
-38.158088	-1.871552	1.796723	0.007326	0.267619
-37.948105	-1.931367	1.801728	0.007287	0.267502
-38.486465	-1.870687	1.806733	0.007387	0.267301
-38.241496	-1.914758	1.811738	0.007341	0.267303
-38.368027	-1.937894	1.816742	0.007365	0.267054
-38.696096	-1.891634	1.821747	0.007426	0.266981
-39.133517	-1.813435	1.826752	0.007507	0.266974
-39.388814	-1.817773	1.831757	0.007554	0.266699
-38.851480	-1.915327	1.836762	0.007454	0.266700
-39.130374	-1.886256	1.841766	0.007506	0.266582
-39.240619	-1.908597	1.846771	0.007527	0.266352
-39.255765	-1.904323	1.851776	0.007530	0.266361
-39.411078	-1.917186	1.856781	0.007558	0.266137
-39.842723	-1.853878	1.861786	0.007639	0.266055
-39.758086	-1.872184	1.866790	0.007623	0.266039
-39.791150	-1.922833	1.871795	0.007629	0.265731
-39.688500	-1.941766	1.876800	0.007610	0.265730
-39.884080	-1.930210	1.881805	0.007646	0.265599
-39.763400	-1.975096	1.886810	0.007624	0.265474
-40.004666	-1.932853	1.891814	0.007669	0.265465
-40.429061	-1.916247	1.896819	0.007748	0.265135
-40.485085	-1.907532	1.901824	0.007758	0.265127
-40.452117	-1.937526	1.906829	0.007752	0.264996
-40.773502	-1.912617	1.911834	0.007812	0.264813
-40.822514	-1.905511	1.916838	0.007821	0.264803
-40.579569	-1.998107	1.921843	0.007776	0.264539
-41.085124	-1.916614	1.926848	0.007870	0.264482
-41.345328	-1.886420	1.931853	0.007918	0.264388
-41.313623	-1.926075	1.936858	0.007912	0.264203
-41.384745	-1.913551	1.941862	0.007925	0.264201
-41.494358	-1.938619	1.946867	0.007946	0.263954
-41.856783	-1.889500	1.951872	0.008013	0.263862
-41.688240	-1.930167	1.956877	0.007982	0.263807
-41.875636	-1.942143	1.961882	0.008016	0.263555
-42.273180	-1.872186	1.966886	0.008090	0.263542
-42.080520	-1.939574	1.971891	0.008055	0.263364
-42.212226	-1.939945	1.976896	0.008079	0.263231
-42.574612	-1.875642	1.981901	0.008146	0.263222
-42.462637	-1.946512	1.986906	0.008126	0.262944
-42.689891	-1.906795	1.991910	0.008168	0.262936
-42.834260	-1.908367	1.996915	0.008195	0.262782
-43.053641	-1.902308	2.001920	0.008235	0.262596

-43.479042	-1.871886	2.011917	0.008315	0.262337
-43.266539	-1.934911	2.021914	0.008275	0.262203
-43.994945	-1.845173	2.031910	0.008410	0.261967
-43.900469	-1.880176	2.041907	0.008393	0.261869
-44.187360	-1.861427	2.051904	0.008446	0.261685
-44.192264	-1.860723	2.061901	0.008447	0.261684
-44.382965	-1.878931	2.071898	0.008482	0.261392
-44.524039	-1.861280	2.081894	0.008508	0.261348
-44.578359	-1.851682	2.091891	0.008519	0.261347
-44.391327	-1.886057	2.101888	0.008484	0.261345
-44.630331	-1.898430	2.111885	0.008528	0.261036
-44.528110	-1.917426	2.121882	0.008509	0.261034
-44.855331	-1.857045	2.131878	0.008570	0.261040
-45.017619	-1.825612	2.141875	0.008600	0.261051
-44.989650	-1.830948	2.151872	0.008595	0.261050
-44.674336	-1.890023	2.161869	0.008536	0.261041
-44.675172	-1.890784	2.171866	0.008536	0.261036
-44.716422	-1.883018	2.181862	0.008543	0.261038
-44.887693	-1.851331	2.191859	0.008575	0.261042
-44.861906	-1.836469	2.201856	0.008570	0.261151
-44.511765	-1.863829	2.211853	0.008505	0.261352
-44.443445	-1.876675	2.221850	0.008492	0.261351
-44.541505	-1.859124	2.231846	0.008510	0.261350
-44.484223	-1.870495	2.241843	0.008500	0.261345
-44.606629	-1.814728	2.251840	0.008522	0.261531
-44.106963	-1.877715	2.261837	0.008429	0.261686
-44.257875	-1.850546	2.271834	0.008457	0.261685
-44.361367	-1.818301	2.281830	0.008476	0.261759
-43.991095	-1.848837	2.291827	0.008407	0.261964
-43.903981	-1.864877	2.301824	0.008391	0.261963
-43.695890	-1.877038	2.311821	0.008352	0.262105
-43.599990	-1.859877	2.321818	0.008334	0.262297
-43.791246	-1.823647	2.331814	0.008370	0.262305
-43.571495	-1.807519	2.341811	0.008329	0.262616
-43.378019	-1.843874	2.351808	0.008293	0.262610
-43.157087	-1.830579	2.361805	0.008251	0.262905
-43.122147	-1.827476	2.371802	0.008245	0.262957
-42.781403	-1.851365	2.381798	0.008181	0.263168
-42.490861	-1.892810	2.391795	0.008127	0.263231
-42.362378	-1.875612	2.401792	0.008103	0.263454
-42.157816	-1.893866	2.411789	0.008065	0.263559
-42.133113	-1.859013	2.421786	0.008060	0.263776
-41.939057	-1.877340	2.431782	0.008024	0.263869
-42.291563	-1.758444	2.441779	0.008090	0.264170
-41.565698	-1.879067	2.451776	0.007954	0.264233
-40.991237	-1.937806	2.461773	0.007847	0.264484
-41.340573	-1.856389	2.471770	0.007912	0.264583
-41.390747	-1.802231	2.481766	0.007921	0.264830
-41.280079	-1.782241	2.491763	0.007901	0.265049
-40.963143	-1.817459	2.501760	0.007842	0.265172
-40.576519	-1.830885	2.511757	0.007770	0.265483
-40.710795	-1.779820	2.521754	0.007795	0.265629
-40.395355	-1.814014	2.531750	0.007736	0.265756
-40.037050	-1.824175	2.541747	0.007669	0.266056
-39.781903	-1.846347	2.551744	0.007621	0.266188
-39.319190	-1.898679	2.561741	0.007535	0.266362
-39.305440	-1.846483	2.571738	0.007532	0.266660
-39.104054	-1.856779	2.581734	0.007495	0.266803
-39.158454	-1.813165	2.591731	0.007505	0.266987
-38.535633	-1.873215	2.601728	0.007389	0.267276
-38.584753	-1.834467	2.611725	0.007398	0.267438
-38.472595	-1.818270	2.621722	0.007377	0.267636
-38.206316	-1.806750	2.631718	0.007327	0.267961
-38.212017	-1.773279	2.641715	0.007328	0.268137
-37.640417	-1.847401	2.651712	0.007222	0.268298
-37.428974	-1.833487	2.661709	0.007182	0.268581
-37.196233	-1.835970	2.671706	0.007139	0.268796
-36.816133	-1.873254	2.681702	0.007068	0.268968
-36.751704	-1.837648	2.691699	0.007056	0.269223
-36.462622	-1.846122	2.701696	0.007002	0.269461
-36.379083	-1.826360	2.711693	0.006986	0.269649
-36.061615	-1.845858	2.721690	0.006927	0.269855
-35.905982	-1.818300	2.731686	0.006898	0.270155
-35.594222	-1.830536	2.741683	0.006840	0.270394
-35.207893	-1.869690	2.751680	0.006768	0.270561
-35.044885	-1.863897	2.761677	0.006737	0.270751
-34.783049	-1.860590	2.771674	0.006689	0.271023
-34.663045	-1.846428	2.781670	0.006666	0.271216
-34.405026	-1.859246	2.791667	0.006618	0.271399
-34.123184	-1.854245	2.801664	0.006565	0.271699
-34.021164	-1.831937	2.811661	0.006546	0.271917
-33.557906	-1.880540	2.821658	0.006460	0.272107
-33.497730	-1.851519	2.831654	0.006449	0.272320
-33.504428	-1.790784	2.841651	0.006450	0.272637
-32.844689	-1.867595	2.851648	0.006327	0.272867
-32.787917	-1.842197	2.861645	0.006316	0.273057
-32.487797	-1.858365	2.871642	0.006260	0.273261
-32.219109	-1.848177	2.881638	0.006210	0.273574
-32.202135	-1.813206	2.891635	0.006207	0.273776
-31.817376	-1.841798	2.901632	0.006135	0.273995
-31.366987	-1.882417	2.911629	0.006051	0.274214
-31.153099	-1.867140	2.921626	0.006011	0.274500
-30.843643	-1.885466	2.931622	0.005954	0.274700
-30.735870	-1.867324	2.941619	0.005934	0.274900
-30.379156	-1.884831	2.951616	0.005867	0.275150
-30.252274	-1.852400	2.961613	0.005843	0.275442
-30.036171	-1.857608	2.971610	0.005803	0.275622
-29.840014	-1.859813	2.981606	0.005766	0.275798
-29.505730	-1.872217	2.991603	0.005704	0.276052
-29.167454	-1.884219	3.001600	0.005641	0.276312
-29.283949	-1.821394	3.011597	0.005663	0.276531
-28.727128	-1.881268	3.021594	0.005559	0.276748
-28.549454	-1.867841	3.031590	0.005526	0.276987
-28.364639	-1.849309	3.041587	0.005491	0.277260
-28.090911	-1.858240	3.051584	0.005440	0.277474
-27.996259	-1.831124	3.061581	0.005422	0.277705
-27.313973	-1.906404	3.071578	0.005295	0.277960
-27.149128	-1.889585	3.081574	0.005264	0.278204
-27.086874	-1.861231	3.091571	0.005253	0.278411
-26.750548	-1.880993	3.101568	0.005190	0.278627
-26.613808	-1.857136	3.111565	0.005164	0.278880
-26.288948	-1.860332	3.121562	0.005104	0.279170
-25.994308	-1.877017	3.131558	0.005049	0.279362
-25.640637	-1.906052	3.141555	0.004983	0.279545
-25.461260	-1.884316	3.151552	0.004950	0.279827
-24.920672	-1.935112	3.161549	0.004849	0.280073
-24.710556	-1.935572	3.171546	0.004810	0.280269
-24.671704	-1.900693	3.181542	0.004802	0.280486
-24.542118	-1.879120	3.191539	0.004778	0.280719
-24.266779	-1.889243	3.201536	0.004727	0.280925
-24.044723	-1.889982	3.211533	0.004685	0.281130
-23.693761	-1.911245	3.221530	0.004620	0.281349
-23.751016	-1.837021	3.231526	0.004630	0.281678
-23.095782	-1.917578	3.241523	0.004508	0.281876
-23.135630	-1.873081	3.251520	0.004516	0.282068
-22.714789	-1.905631	3.261517	0.004437	0.282294
-22.606240	-1.864821	3.271514	0.004417	0.282605
-22.483844	-1.841542	3.281510	0.004394	0.282838
-22.285565	-1.832572	3.291507	0.004357	0.283069
-22.114018	-1.822195	3.301504	0.004325	0.283282
-21.500081	-1.879155	3.311501	0.004211	0.283562
-21.250161	-1.877121	3.321498	0.004164	0.283804
-20.998240	-1.881489	3.331494	0.004117	0.284016
-20.613244	-1.911525	3.341491	0.004045	0.284220
-20.611477	-1.859757	3.351488	0.004045	0.284486
-20.072814	-1.907932	3.361485	0.003944	0.284739
-19.932001	-1.893611	3.371482	0.003918	0.284943
-19.408661	-1.951933	3.381478	0.003821	0.285130
-19.249890	-1.915257	3.391475	0.003791	0.285463
-19.441183	-1.848320	3.401472	0.003826	0.285626
-18.853629	-1.919271	3.411469	0.003717	0.285809
-18.975424	-1.849746	3.421466	0.003739	0.286049
-18.391221	-1.898261	3.431462	0.003631	0.286341
-18.044159	-1.919854	3.441459	0.003566	0.286551
-18.061256	-1.877659	3.451456	0.003569	0.286749
-17.607523	-1.915839	3.461453	0.003484	0.286973
-17.300761	-1.915849	3.471450	0.003427	0.287255
-17.128939	-1.908018	3.481446	0.003395	0.287452
-16.682646	-1.951215	3.491443	0.003312	0.287643
-16.495168	-1.925541	3.501440	0.003277	0.287944
-16.390312	-1.902041	3.511437	0.003257	0.288158
-16.308523	-1.877991	3.521434	0.003242	0.288354
-15.719274	-1.944007	3.531430	0.003132	0.288561
-15.640194	-1.898294	3.541427	0.003117	0.288863
-15.335696	-1.911882	3.551424	0.003061	0.289072
-14.996591	-1.933749	3.561421	0.002997	0.289272
-14.990102	-1.890481	3.571418	0.002996	0.289494
-14.582869	-1.907233	3.581414	0.002920	0.289781
-14.534412	-1.874510	3.591411	0.002911	0.289989
-14.196758	-1.894214	3.601408	0.002848	0.290197
-13.691883	-1.928719	3.611405	0.002754	0.290483
-13.399730	-1.943207	3.621402	0.002700	0.290676
-13.526361	-1.883163	3.631398	0.002723	0.290861
-13.328667	-1.874795	3.641395	0.002686	0.291081
-12.924938	-1.891680	3.651392	0.002611	0.291363
-12.382662	-1.942528	3.661389	0.002510	0.291600
-12.279759	-1.925067	3.671386	0.002491	0.291780
-11.860811	-1.960185	3.681382	0.002413	0.291984
-11.855842	-1.904292	3.691379	0.002411	0.292266
-11.463159	-1.937479	3.701376	0.002338	0.292455
-10.944686	-1.995355	3.711373	0.002242	0.292635
-10.830204	-1.951172	3.721370	0.002220	0.292957
-10.447763	-1.984522	3.731366	0.002149	0.293136
-10.316544	-1.978228	3.741363	0.002124	0.293285
-10.048473	-1.969911	3.751360	0.002074	0.293567
-9.647906	-2.000537	3.761357	0.002000	0.293775
-9.531611	-1.988931	3.771354	0.001978	0.293937
-9.062378	-2.018924	3.781350	0.001891	0.294209
-8.957794	-1.994854	3.791347	0.001871	0.294422
-8.874077	-1.978081	3.801344	0.001855	0.294579
-8.310208	-2.030064	3.811341	0.001750	0.294828
-8.140114	-2.011068	3.821338	0.001719	0.295073
-7.922997	-2.014567	3.831334	0.001678	0.295250
-7.608658	-2.023608	3.841331	0.001619	0.295486
-7.447400	-2.013202	3.851328	0.001589	0.295681
-7.277691	-2.011964	3.861325	0.001558	0.295838
-6.772460	-2.059904	3.871322	0.001463	0.296053
-6.492415	-2.059989	3.881318	0.001411	0.296302
-6.497563	-2.026965	3.891315	0.001412	0.296459
-5.944207	-2.080657	3.901312	0.001309	0.296688
-5.943020	-2.033557	3.911309	0.001309	0.296919
-5.616267	-2.059481	3.921306	0.001248	0.297082
-5.420721	-2.050260	3.931302	0.001211	0.297301
-5.222474	-2.032935	3.941299	0.001174	0.297561
-4.892722	-2.057557	3.951296	0.001113	0.297733
-4.840184	-2.021577	3.961293	0.001103	0.297954
-4.360523	-2.054606	3.971290	0.001013	0.298218
-4.310340	-2.028741	3.981286	0.001004	0.298388
-4.218508	-2.008176	3.991283	0.000987	0.298569
-3.905123	-2.002260	4.001280	0.000928	0.298874
-3.741049	-1.989868	4.011277	0.000898	0.299078
-3.696719	-1.955483	4.021274	0.000889	0.299284
-3.342393	-1.975614	4.031270	0.000823	0.299498
-3.264530	-1.930733	4.041267	0.000809	0.299784
-2.927210	-1.946755	4.051264	0.000746	0.300003
-2.669419	-1.950507	4.061261	0.000698	0.300211
-2.587856	-1.907722	4.071258	0.000682	0.300489
-2.368680	-1.904463	4.081254	0.000641	0.300697
-2.602638	-1.814636	4.091251	0.000685	0.300925
-2.329393	-1.813780	4.101248	0.000634	0.301168
-2.078296	-1.806875	4.111245	0.000587	0.301421
-1.954233	-1.772036	4.121242	0.000564	0.301696
-1.622541	-1.773526	4.131238	0.000502	0.301979
-1.655874	-1.711936	4.141235	0.000508	0.302245
-1.477111	-1.689135	4.151232	0.000475	0.302510
-1.327557	-1.656299	4.161229	0.000447	0.302797
-1.349609	-1.592205	4.171226	0.000451	0.303085
-1.436623	-1.515277	4.181222	0.000467	0.303377
-1.103409	-1.512345	4.191219	0.000405	0.303680
-1.198720	-1.428861	4.201216	0.000422	0.303995
-1.171169	-1.365114	4.211213	0.000417	0.304322
-0.895293	-1.351727	4.221210	0.000366	0.304625
-0.873009	-1.283038	4.231206	0.000361	0.304970
-1.015579	-1.182839	4.241203	0.000388	0.305323
-0.949147	-1.126549	4.251200	0.000375	0.305647
-0.724669	-1.095871	4.261197	0.000333	0.305986
-0.843974	-0.995888	4.271194	0.000355	0.306356
-0.742224	-0.927297	4.281190	0.000336	0.306767
-0.722134	-0.856963	4.291187	0.000332	0.307117
-0.786714	-0.761044	4.301184	0.000344	0.307513
-0.796440	-0.669017	4.311181	0.000346	0.307938
-0.574043	-0.620227	4.321178	0.000304	0.308357
-0.514043	-0.546324	4.331174	0.000293	0.308755
-0.482929	-0.458946	4.341171	0.000287	0.309191
-0.214595	-0.416121	4.351168	0.000237	0.309620
-0.132578	-0.343032	4.361165	0.000222	0.310031
-0.003588	-0.261671	4.371162	0.000197	0.310520
-0.049858	-0.169774	4.381158	0.000206	0.310909
-0.180479	-0.049933	4.391155	0.000230	0.311357
-0.094348	0.038573	4.401152	0.000214	0.311841
0.000000	0.111611	4.411149	0.000196	0.312259

-0.170615	0.424811	4.416154	0.000228	0.313564
0.252930	0.913627	4.421158	0.000149	0.316164
0.178766	1.782358	4.426163	0.000162	0.320054
0.425310	2.880736	4.431168	0.000115	0.325180
0.634858	4.283583	4.436173	0.000075	0.331529
0.717313	5.996307	4.441178	0.000059	0.338985
1.074254	7.967492	4.446182	-0.000009	0.347565
1.429831	10.244492	4.451187	-0.000077	0.357179
1.613034	12.856566	4.456192	-0.000113	0.367737
1.838669	15.786175	4.461197	-0.000157	0.379244
2.237368	19.009836	4.466202	-0.000233	0.391615
2.546122	22.583348	4.471206	-0.000293	0.404800
3.034091	26.464146	4.476211	-0.000386	0.418745
3.387741	30.715733	4.481216	-0.000455	0.433398
3.871229	35.287172	4.486221	-0.000548	0.448679
4.250771	40.221423	4.491226	-0.000622	0.464529
4.747961	45.483436	4.496230	-0.000718	0.480906
5.033198	51.129610	4.501235	-0.000775	0.497750
5.656727	57.054808	4.506240	-0.000895	0.514998
6.003485	63.355885	4.511245	-0.000964	0.532572
6.653885	69.912415	4.516250	-0.001089	0.550400
7.139055	76.816029	4.521254	-0.001184	0.568476
8.008695	83.954750	4.526259	-0.001351	0.586744
8.671634	91.402829	4.531264	-0.001479	0.605111
9.495686	99.103626	4.536269	-0.001638	0.623590
9.956023	107.108513	4.541274	-0.001728	0.642074
10.163818	115.400887	4.546278	-0.001773	0.660571
11.046763	123.770001	4.551283	-0.001943	0.678985
11.837682	132.348024	4.556288	-0.002095	0.697311
12.974177	141.047693	4.561293	-0.002313	0.715537
15.032796	149.748674	4.566298	-0.002702	0.733635
16.117670	158.786376	4.571302	-0.002910	0.751611
16.921289	167.976109	4.576307	-0.003065	0.769358
17.575705	177.305593	4.581312	-0.003193	0.786912
18.373845	186.687401	4.586317	-0.003348	0.804222
19.280344	196.119003	4.591322	-0.003523	0.821288
20.597786	205.555400	4.596326	-0.003775	0.838139
21.537239	215.075908	4.601331	-0.003956	0.854687
22.542680	224.614889	4.606336	-0.004149	0.870969
23.493738	234.186288	4.611341	-0.004333	0.886989
24.230362	243.804449	4.616346	-0.004476	0.902739
25.214414	253.374631	4.621350	-0.004666	0.918211
26.389948	262.894667	4.626355	-0.004891	0.933400
26.935544	272.508278	4.631360	-0.004999	0.948319
27.937562	282.014686	4.636365	-0.005191	0.962966
29.087210	291.464405	4.641370	-0.005412	0.977347
29.919692	300.968836	4.646374	-0.005573	0.991517
30.532949	310.438898	4.651379	-0.005693	1.005383
31.054552	319.867812	4.656384	-0.005797	1.018979
31.826515	329.226583	4.661389	-0.005947	1.032359
32.560236	338.521638	4.666394	-0.006089	1.045469
33.371817	347.783126	4.671398	-0.006246	1.058389
34.367374	356.968675	4.676403	-0.006438	1.071093
35.469022	366.082948	4.681408	-0.006649	1.083577
36.091395	375.255596	4.686413	-0.006771	1.095886
36.525459	384.391618	4.691418	-0.006858	1.107968
37.063396	393.468785	4.696422	-0.006964	1.119866
37.537762	402.512380	4.701427	-0.007058	1.131582
38.216826	411.478312	4.706432	-0.007190	1.143124
38.885310	420.435411	4.711437	-0.007321	1.154537
39.469808	429.310578	4.716442	-0.007435	1.165719
40.140939	438.168158	4.721446	-0.007566	1.176790
40.782466	446.979086	4.726451	-0.007691	1.187695
40.998543	455.831733	4.731456	-0.007738	1.198463
41.786352	464.551827	4.736461	-0.007890	1.209093
42.486023	473.254987	4.741466	-0.008026	1.219592
43.018937	481.978365	4.746470	-0.008131	1.229992
43.736810	490.621509	4.751475	-0.008270	1.240248
44.456550	499.240110	4.756480	-0.008410	1.250390
44.971308	507.884851	4.761485	-0.008511	1.260441
45.602905	516.475337	4.766490	-0.008635	1.270373
46.087274	525.069257	4.771494	-0.008731	1.280204
46.686984	533.628811	4.776499	-0.008848	1.289943
47.010527	542.200741	4.781504	-0.008914	1.299570
47.542370	550.771516	4.786509	-0.009018	1.309164
47.803957	559.355609	4.791514	-0.009073	1.318652
48.684903	567.753011	4.796518	-0.009242	1.327983
49.260008	576.212889	4.801523	-0.009355	1.337260
49.737412	584.650453	4.806528	-0.009449	1.346432
50.316252	593.100709	4.811533	-0.009563	1.355573
50.336494	601.587021	4.816538	-0.009572	1.364592
51.184596	609.946622	4.821542	-0.009735	1.373563
51.802489	618.335513	4.826547	-0.009856	1.382467
52.219011	626.748095	4.831552	-0.009939	1.391303
52.940308	635.082874	4.836557	-0.010079	1.400055
53.590191	643.430011	4.841562	-0.010205	1.408753
53.818159	651.854850	4.846566	-0.010253	1.417405
54.001509	660.258258	4.851571	-0.010293	1.425975
54.678548	668.567416	4.856576	-0.010425	1.434482
55.559817	676.833506	4.861581	-0.010594	1.442928
56.175135	685.149776	4.866586	-0.010714	1.451332
56.557547	693.504029	4.871590	-0.010791	1.459686
57.610589	701.748359	4.876595	-0.010992	1.467993
57.894202	710.130486	4.881600	-0.011051	1.476264
58.251648	718.447238	4.886605	-0.011123	1.484437
58.423288	726.803425	4.891610	-0.011160	1.492573
59.056539	735.057623	4.896614	-0.011283	1.500641
59.262796	743.388812	4.901619	-0.011327	1.508671
59.468188	751.688505	4.906624	-0.011371	1.516629
60.156701	759.909997	4.911629	-0.011505	1.524546
60.917413	768.134423	4.916634	-0.011652	1.532435
61.242637	776.426345	4.921638	-0.011718	1.540281
61.905226	784.670561	4.926643	-0.011846	1.548093
62.516044	792.896941	4.931648	-0.011966	1.555842
63.187998	801.119242	4.936653	-0.012096	1.563557
63.591404	809.381176	4.941658	-0.012177	1.571230
64.309170	817.603867	4.946662	-0.012316	1.578877
64.472233	825.897434	4.951667	-0.012351	1.586470
64.925778	834.140029	4.956672	-0.012441	1.594022
65.019240	842.433242	4.961677	-0.012464	1.601532
65.148893	850.697300	4.966682	-0.012494	1.608987
65.730852	858.897853	4.971686	-0.012608	1.616414
66.316324	867.082934	4.976691	-0.012722	1.623795
66.356943	875.383977	4.981696	-0.012735	1.631167
67.047533	883.550961	4.986701	-0.012869	1.638479
67.337760	891.734962	4.991706	-0.012928	1.645718
67.818340	899.938905	4.996710	-0.013023	1.652969
67.970390	908.167975	5.001715	-0.013057	1.660164
68.247530	916.367078	5.006720	-0.013114	1.667319
68.738599	924.562650	5.011725	-0.013211	1.674470
69.180555	932.716211	5.016730	-0.013298	1.681548
69.393853	940.940757	5.021734	-0.013343	1.688625
69.574952	949.173112	5.026739	-0.013383	1.695675
69.978866	957.325366	5.031744	-0.013463	1.702658
70.384104	965.530014	5.036749	-0.013544	1.709657
70.846234	973.685172	5.041754	-0.013635	1.716592
71.463382	981.815107	5.046758	-0.013756	1.723500
71.814544	989.997976	5.051763	-0.013826	1.730388
72.422399	998.152252	5.056768	-0.013945	1.737259
73.188012	1006.273396	5.061773	-0.014093	1.744096
73.617222	1014.455220	5.066778	-0.014178	1.750912
74.333868	1022.593570	5.071782	-0.014317	1.757703
74.802255	1030.757616	5.076787	-0.014410	1.764457
75.110527	1038.960099	5.081792	-0.014472	1.771196
75.506797	1047.151789	5.086797	-0.014551	1.777911
75.886958	1055.305428	5.091802	-0.014628	1.784569
76.202027	1063.521365	5.096806	-0.014692	1.791243
76.554379	1071.686105	5.101811	-0.014763	1.797856
76.945934	1079.804768	5.106816	-0.014841	1.804413
77.557073	1087.946917	5.111821	-0.014960	1.810992
77.680072	1096.145212	5.116826	-0.014988	1.817531
77.928790	1104.311725	5.121830	-0.015040	1.824037
78.474582	1112.437610	5.126835	-0.015147	1.830525
78.830808	1120.577042	5.131840	-0.015219	1.836976
79.031200	1128.748152	5.136845	-0.015261	1.843411
79.328552	1136.885704	5.141850	-0.015322	1.849809
79.839232	1145.011512	5.146854	-0.015422	1.856201
80.070799	1153.182917	5.151859	-0.015471	1.862573
80.418795	1161.313973	5.156864	-0.015541	1.868906
81.424302	1169.355627	5.161869	-0.015734	1.875226
81.534550	1177.523849	5.166874	-0.015760	1.881517
81.907070	1185.661713	5.171878	-0.015834	1.887794
82.190659	1193.835272	5.176883	-0.015892	1.894067
82.424630	1201.978635	5.181888	-0.015941	1.900291
82.767533	1210.099783	5.186893	-0.016011	1.906490
83.040796	1218.240700	5.191898	-0.016067	1.912675
83.123213	1226.416873	5.196902	-0.016087	1.918846
83.520657	1234.508847	5.201907	-0.016167	1.924969
83.968706	1242.594869	5.206912	-0.016256	1.931074
84.231357	1250.773893	5.211917	-0.016310	1.937208
84.680772	1258.847294	5.216922	-0.016399	1.943265
85.279533	1266.944437	5.221926	-0.016516	1.949337
85.594948	1275.068808	5.226931	-0.016580	1.955379
85.440647	1283.236432	5.231936	-0.016556	1.961382
85.826142	1291.346192	5.236941	-0.016633	1.967384
85.808000	1299.498721	5.241946	-0.016635	1.973354
86.302036	1307.576532	5.246950	-0.016733	1.979308
86.168052	1315.758680	5.251955	-0.016713	1.985251
86.858474	1323.781140	5.256960	-0.016847	1.991150
87.365230	1331.879157	5.261965	-0.016947	1.997067
87.608775	1339.989087	5.266970	-0.016997	2.002946
87.746200	1348.147120	5.271974	-0.017028	2.008831
88.285600	1356.212816	5.276979	-0.017134	2.014675
88.379153	1364.360275	5.281984	-0.017157	2.020514
88.883144	1372.447547	5.286989	-0.017256	2.026336
89.026325	1380.592586	5.291994	-0.017288	2.032144
89.574238	1388.653181	5.296998	-0.017395	2.037918
90.146103	1396.702624	5.302003	-0.017507	2.043671
90.508034	1404.802637	5.307008	-0.017580	2.049421
90.472515	1413.009800	5.312013	-0.017579	2.055189
90.679686	1421.108027	5.317018	-0.017622	2.060889
91.222609	1429.161002	5.322022	-0.017729	2.066576
91.515003	1437.281651	5.327027	-0.017789	2.072270
91.232748	1445.475787	5.332032	-0.017741	2.077940
92.083557	1453.451099	5.337037	-0.017905	2.083558
92.428801	1461.543038	5.342042	-0.017975	2.089190
92.999910	1469.613960	5.347046	-0.018086	2.094815
93.340080	1477.731827	5.352051	-0.018155	2.100435
93.345786	1485.876637	5.357056	-0.018161	2.106024
93.934857	1493.982110	5.362061	-0.018276	2.111629
94.158858	1502.086531	5.367066	-0.018323	2.117183
94.334464	1510.176038	5.372070	-0.018361	2.122707
94.361275	1518.314517	5.377075	-0.018372	2.128235
94.428327	1526.423141	5.382080	-0.018390	2.133733
94.880999	1534.490392	5.387085	-0.018479	2.139226
94.730207	1542.607937	5.392090	-0.018456	2.144680
95.047977	1550.693969	5.397094	-0.018521	2.150145
95.513133	1558.744439	5.402099	-0.018613	2.155586
95.811929	1566.800454	5.407104	-0.018674	2.161001
96.208682	1574.882329	5.412109	-0.018753	2.166429
96.626615	1582.951685	5.417114	-0.018836	2.171837
97.022017	1591.026567	5.422118	-0.018915	2.177233
97.296909	1599.119633	5.427123	-0.018972	2.182616
97.487108	1607.222012	5.432128	-0.019012	2.187984
98.047824	1615.296216	5.437133	-0.019122	2.193355
98.089102	1623.397639	5.442138	-0.019135	2.198682
98.255478	1631.493130	5.447142	-0.019171	2.204004
98.461639	1639.597428	5.452147	-0.019215	2.209322
98.537163	1647.706851	5.457152	-0.019234	2.214619
98.917829	1655.768610	5.462157	-0.019311	2.219900
98.926236	1663.867744	5.467162	-0.019317	2.225159
99.151970	1671.972796	5.472166	-0.019365	2.230429
99.888234	1679.970424	5.477171	-0.019507	2.235664
100.218907	1688.028359	5.482176	-0.019574	2.240888
100.550955	1696.120224	5.487181	-0.019641	2.246122
100.763202	1704.210745	5.492186	-0.019686	2.251333
101.267610	1712.277811	5.497190	-0.019785	2.256542
101.752208	1720.349779	5.502195	-0.019881	2.261740
101.982910	1728.431728	5.507200	-0.019929	2.266910
102.213090	1736.570728	5.512205	-0.019977	2.272105
102.422187	1744.640796	5.517210	-0.020021	2.277242
102.811717	1752.679225	5.522214	-0.020099	2.282363
102.898333	1760.782004	5.527219	-0.020121	2.287487
102.999914	1768.872177	5.532224	-0.020145	2.292593
103.440065	1776.918191	5.537229	-0.020232	2.297689
103.664853	1784.986993	5.542234	-0.020279	2.302769
103.760333	1793.100121	5.547238	-0.020303	2.307855
104.106018	1801.165457	5.552243	-0.020372	2.312921
104.411317	1809.205129	5.557248	-0.020434	2.317956
104.526781	1817.310465	5.562253	-0.020461	2.323005
104.802516	1825.355611	5.567258	-0.020518	2.328020
105.011038	1833.451246	5.572262	-0.020562	2.333049
105.289849	1841.517444	5.577267	-0.020619	2.338055
105.621750	1849.548241	5.582272	-0.020686	2.343033
106.205551	1857.619403	5.587277	-0.020800	2.348046
106.214017	1865.722205	5.592282	-0.020807	2.353020
106.173590	1873.828921	5.597286	-0.020805	2.357981
106.513663	1881.873381	5.602291	-0.020874	2.362926
106.668716	1889.942614	5.607296	-0.020908	2.367860
107.160353	1897.987044	5.612301	-0.021005	2.372796
107.524866	1906.028460	5.617306	-0.021078	2.377710
107.927863	1914.081826	5.622310	-0.021158	2.382624
108.083158	1922.190165	5.627315	-0.021192	2.387540
108.442362	1930.247738	5.632320	-0.021264	2.392433
108.806668	1938.310994	5.637325	-0.021338	2.397319
108.811541	1946.398157	5.642330	-0.021344	2.402181
109.091808	1954.456187	5.647334	-0.021401	2.407037
109.427068	1962.539768	5.652339	-0.021469	2.411903
109.790059	1970.561662	5.657344	-0.021542	2.416725
110.158822	1978.640724	5.662349	-0.021616	2.421572
110.570456	1986.675893	5.667354	-0.021698	2.426386
110.805899	1994.798907	5.672358	-0.021747	2.431229
111.111865	2002.876181	5.677363	-0.021809	2.436040
111.537073	2010.884071	5.682368	-0.021894	2.440810
111.846540	2018.949194	5.687373	-0.021957	2.445596
112.132771	2027.017224	5.692378	-0.022015	2.450372
112.183222	2035.132618	5.697382	-0.022030	2.455148
112.533987	2043.168854	5.702387	-0.022101	2.459892
113.067651	2051.161264	5.707392	-0.022205	2.464615
113.195166	2059.291213	5.712397	-0.022234	2.469378
113.343971	2067.341506	5.717402	-0.022267	2.474087
113.792951	2075.370817	5.722406	-0.022356	2.478797
114.100955	2083.434434	5.727411	-0.022419	2.483508
113.961872	2091.539455	5.732416	-0.022398	2.488200
114.397281	2099.583864	5.737421	-0.022485	2.492891
114.923240	2107.607039	5.742426	-0.022588	2.497569
115.089417	2115.693794	5.747430	-0.022624	2.502246
115.223436	2123.795638	5.752435	-0.022654	2.506922
115.660123	2131.823123	5.757440	-0.022741	2.511568
115.887945	2139.883570	5.762445	-0.022789	2.516209
116.064747	2147.932641	5.767450	-0.022827	2.520832
116.272763	2155.993394	5.772454	-0.022871	2.525454
116.709251	2164.055188	5.777459	-0.022957	2.530086
116.803125	2172.114446	5.782464	-0.022980	2.534683
116.850872	2180.220173	5.787469	-0.022994	2.539294
116.585799	2188.325782	5.792474	-0.022950	2.543874
116.736531	2196.371830	5.797478	-0.022984	2.548442
117.253624	2204.375834	5.802483	-0.023085	2.553005
117.559663	2212.379668	5.807488	-0.023147	2.557544
117.578027	2220.493440	5.812493	-0.023156	2.562116
117.926804	2228.502375	5.817498	-0.023226	2.566645
118.496707	2236.522864	5.822502	-0.023338	2.571188
118.480524	2244.649106	5.827507	-0.023340	2.575741
118.698266	2252.674297	5.832512	-0.023386	2.580246
118.874856	2260.750205	5.837517	-0.023424	2.584768
119.269037	2268.788466	5.842522	-0.023503	2.589276
119.363908	2276.963584	5.847526	-0.023526	2.593832
119.724581	2284.957051	5.852531	-0.023598	2.598297
120.124690	2292.929666	5.857536	-0.023678	2.602746
120.410101	2300.989015	5.862541	-0.023736	2.607227
120.380540	2309.071410	5.867546	-0.023736	2.611691
120.878028	2317.100162	5.872550	-0.023834	2.616155
121.298252	2325.134164	5.877555	-0.023918	2.620608
121.220229	2333.181535	5.882560	-0.023908	2.625027
121.372078	2341.264141	5.887565	-0.023942	2.629474
121.669696	2349.308728	5.892570	-0.024003	2.633902
121.788079	2357.371619	5.897574	-0.024030	2.638320
121.818659	2365.442127	5.902579	-0.024041	2.642729
122.224290	2373.438960	5.907584	-0.024122	2.647117
122.313105	2381.543917	5.912589	-0.024144	2.651534
122.698309	2389.553661	5.917594	-0.024221	2.655912
122.721968	2397.636436	5.922598	-0.024230	2.660298
123.027638	2405.659759	5.927603	-0.024293	2.664663
123.146611	2413.715343	5.932608	-0.024320	2.669027
123.617642	2421.754277	5.937613	-0.024413	2.673397
123.646623	2429.813878	5.942618	-0.024424	2.677742
123.931264	2437.838464	5.947622	-0.024482	2.682078
124.256663	2445.879957	5.952627	-0.024548	2.686419
124.561797	2453.917903	5.957632	-0.024610	2.690750
125.208991	2461.951832	5.962637	-0.024736	2.695093
125.116280	2470.018947	5.967642	-0.024724	2.699400
125.165892	2478.082203	5.972646	-0.024738	2.703706
125.640368	2486.136171	5.977651	-0.024832	2.708028
125.745818	2494.196856	5.982656	-0.024857	2.712323
125.631422	2502.310480	5.987661	-0.024841	2.716625
125.642363	2510.340480	5.992666	-0.024848	2.720884
126.114557	2518.316902	5.997670	-0.024941	2.725138
126.408584	2526.358225	6.002675	-0.025002	2.729407
126.549874	2534.433614	6.007680	-0.025033	2.733679
126.794180	2542.492775	6.012685	-0.025084	2.737941
127.046174	2550.518594	6.017690	-0.025136	2.742180
127.368294	2558.553960	6.022694	-0.025201	2.746421
127.915781	2566.609017	6.027699	-0.025309	2.750681
127.965785	2574.709868	6.032704	-0.025323	2.754926
127.996605	2582.730530	6.037709	-0.025334	2.759122
128.328476	2590.734280	6.042714	-0.025401	2.763322
128.472526	2598.784644	6.047718	-0.025433	2.767527
128.747923	2606.867822	6.052723	-0.025490	2.771752
129.083419	2614.861415	6.057728	-0.025558	2.775927
129.496326	2622.916517	6.062733	-0.025640	2.780132
129.567602	2630.942866	6.067738	-0.025658	2.784295
129.405903	2639.049719	6.072742	-0.025634	2.788480
129.865707	2647.089100	6.077747	-0.025725	2.792661
129.777320	2655.140798	6.082752	-0.025713	2.796809
129.780917	2663.206998	6.087757	-0.025719	2.800963
129.827416	2671.261343	6.092762	-0.025733	2.805108
130.219102	2679.249080	6.097766	-0.025812	2.809234
130.477343	2687.327679	6.102771	-0.025865	2.813392
130.628859	2695.329485	6.107776	-0.025898	2.817498
131.018242	2703.364974	6.112781	-0.025976	2.821629
131.015376	2711.440124	6.117786	-0.025981	2.825751
131.030875	2719.526788	6.122790	-0.025989	2.829875
131.240669	2727.573387	6.127795	-0.026033	2.833983
131.568363	2735.557970	6.132800	-0.026100	2.838061
131.533758	2743.603270	6.137805	-0.026099	2.842142
131.979134	2751.610576	6.142810	-0.026187	2.846226
131.846256	2759.705161	6.147814	-0.026167	2.850315
132.189224	2767.727195	6.152819	-0.026236	2.854389
132.071374	2775.787511	6.157824	-0.026220	2.858450
131.999849	2783.871930	6.162829	-0.026212	2.862520
132.135599	2791.894564	6.167834	-0.026242	2.866564
132.072164	2799.961812	6.172838	-0.026236	2.870615
132.318902	2807.992171	6.177843	-0.026287	2.874658
132.713009	2815.969285	6.182848	-0.026366	2.878678
132.932904	2823.996819	6.187853	-0.026412	2.882707
133.457715	2832.003807	6.192858	-0.026515	2.886738
133.435198	2840.094579	6.197862	-0.026516	2.890773
133.903917	2848.109437	6.202867	-0.026609	2.894793
133.480614	2856.231438	6.207872	-0.026535	2.898811
133.576242	2864.283698	6.212877	-0.026558	2.902817
133.976265	2872.277204	6.217882	-0.026638	2.906806
134.262680	2880.341256	6.222886	-0.026697	2.910818
134.371714	2888.433214	6.227891	-0.026722	2.914828
134.615913	2896.373403	6.232896	-0.026773	2.918765
135.218883	2904.362465	6.237901	-0.026890	2.922741
135.052657	2912.445500	6.242906	-0.026865	2.926715
135.423307	2920.447634	6.247910	-0.026939	2.930674
135.539979	2928.513016	6.252915	-0.026966	2.934644
135.703826	2936.543448	6.257920	-0.027002	2.938594
136.149365	2944.563963	6.262925	-0.027090	2.942549
136.298333	2952.631307	6.267930	-0.027123	2.946506
136.330833	2960.703188	6.272934	-0.027134	2.950454
136.568299	2968.744256	6.277939	-0.027184	2.954392
137.009610	2976.734171	6.282944	-0.027271	2.958310
136.840274	2984.833651	6.287949	-0.027245	2.962245
136.865761	2992.854485	6.292954	-0.027255	2.966146
137.344159	3000.836002	6.297958	-0.027350	2.970047
137.804344	3008.886301	6.302963	-0.027441	2.973975
137.993239	3016.923350	6.307968	-0.027481	2.977877
138.331458	3024.954899	6.312973	-0.027549	2.981779
138.464928	3033.011501	6.317978	-0.027579	2.985678
138.525373	3041.067153	6.322982	-0.027596	2.989567
138.345002	3049.198149	6.327987	-0.027568	2.993475
138.479441	3057.179910	6.332992	-0.027598	2.997322
138.591759	3065.231588	6.337997	-0.027624	3.001197
139.249653	3073.165059	6.343002	-0.027752	3.005038
139.354218	3081.216363	6.348006	-0.027777	3.008902
139.346199	3089.319452	6.353011	-0.027780	3.012780
139.082470	3097.373933	6.358016	-0.027737	3.016617
139.838289	3105.345949	6.363021	-0.027883	3.020461
140.094407	3113.346126	6.368026	-0.027936	3.024289
140.086657	3121.424520	6.373030	-0.027939	3.028136
140.185162	3129.511818	6.378035	-0.027963	3.031987
140.333457	3137.535810	6.383040	-0.027996	3.035806
140.625630	3145.552872	6.388045	-0.028056	3.039624
140.923284	3153.527511	6.393050	-0.028116	3.043417
140.738490	3161.653289	6.398054	-0.028087	3.047253
141.228775	3169.659076	6.403059	-0.028184	3.051061
141.267399	3177.687893	6.408064	-0.028196	3.054852
141.332870	3185.741143	6.413069	-0.028214	3.058652
142.027276	3193.680607	6.418074	-0.028348	3.062425
142.078297	3201.764155	6.423078	-0.028363	3.066228
142.471984	3209.816261	6.428083	-0.028442	3.070029
142.735917	3217.859354	6.433088	-0.028496	3.073815
143.254735	3225.849507	6.438093	-0.028598	3.077584
142.989362	3233.943260	6.443098	-0.028554	3.081358
143.046341	3241.993584	6.448102	-0.028570	3.085123
143.530492	3249.967075	6.453107	-0.028665	3.088869
143.453318	3258.052265	6.458112	-0.028656	3.092634
143.640069	3266.099477	6.463117	-0.028696	3.096390
143.442253	3274.188448	6.468122	-0.028665	3.100143
143.743051	3282.132738	6.473126	-0.028726	3.103848
144.044972	3290.194294	6.478131	-0.028787	3.107602
144.201844	3298.233975	6.483136	-0.028822	3.111335
144.483230	3306.241759	6.488141	-0.028880	3.115055
144.800395	3314.229291	6.493146	-0.028944	3.118762
145.113581	3322.238399	6.498150	-0.029007	3.122475
145.362613	3330.309732	6.503155	-0.029059	3.126209
145.370426	3338.354072	6.508160	-0.029066	3.129914
145.724395	3346.391545	6.513165	-0.029137	3.133629
145.829657	3354.453460	6.518170	-0.029162	3.137338
146.331051	3362.417992	6.523174	-0.029261	3.141017
146.616573	3370.464088	6.528179	-0.029319	3.144719
146.831909	3378.525441	6.533184	-0.029364	3.148420
147.156495	3386.578709	6.538189	-0.029430	3.152118
147.247285	3394.636078	6.543194	-0.029452	3.155803
147.443929	3402.610968	6.548198	-0.029494	3.159450
147.419780	3410.704044	6.553203	-0.029495	3.163138
147.767071	3418.651215	6.558208	-0.029565	3.166771
147.819829	3426.736298	6.563213	-0.029580	3.170450
148.307073	3434.742731	6.568218	-0.029676	3.174108
148.427072	3442.793279	6.573222	-0.029704	3.177765
148.449925	3450.859225	6.578227	-0.029713	3.181421
148.416472	3458.886132	6.583232	-0.029712	3.185053
148.828181	3466.931325	6.588237	-0.029794	3.188708
149.033329	3474.939641	6.593242	-0.029838	3.192333
149.440914	3482.931981	6.598246	-0.029919	3.195956
149.886314	3490.936178	6.603251	-0.030007	3.199582
149.954690	3498.963917	6.608256	-0.030025	3.203197
150.131490	3507.028529	6.613261	-0.030063	3.206830
150.575510	3515.075262	6.618266	-0.030151	3.210462
150.316278	3523.147365	6.623270	-0.030108	3.214071
150.408125	3531.187085	6.628275	-0.030131	3.217677
150.893155	3539.178704	6.633280	-0.030226	3.221274
151.099686	3547.203304	6.638285	-0.030270	3.224869
151.356154	3555.249701	6.643290	-0.030323	3.228473
151.414928	3563.281299	6.648294	-0.030339	3.232057
151.590309	3571.369684	6.653299	-0.030377	3.235668
152.019373	3579.288026	6.658304	-0.030462	3.239209
152.212227	3587.328238	6.663309	-0.030503	3.242791
152.396427	3595.359262	6.668314	-0.030543	3.246365
152.254088	3603.447581	6.673318	-0.030522	3.249946
152.709164	3611.445624	6.678323	-0.030612	3.253508
152.873519	3619.472860	6.683328	-0.030648	3.257067
152.769538	3627.563747	6.688333	-0.030634	3.260639
153.004472	3635.549760	6.693338	-0.030683	3.264175
152.997064	3643.590503	6.698342	-0.030687	3.267722
153.612513	3651.614691	6.703347	-0.030806	3.271282
153.526052	3659.666206	6.708352	-0.030796	3.274822
153.113719	3667.756568	6.713357	-0.030724	3.278362
153.584116	3675.733385	6.718362	-0.030817	3.281884
153.595834	3683.739933	6.723366	-0.030824	3.285397
153.816003	3691.782932	6.728371	-0.030871	3.288931
153.989728	3699.790435	6.733376	-0.030908	3.292443
154.457784	3707.837480	6.738381	-0.031001	3.295981
154.708525	3715.824596	6.743386	-0.031053	3.299479
154.347569	3723.899025	6.748390	-0.030991	3.302988
154.874103	3731.900373	6.753395	-0.031094	3.306497
154.927437	3739.974267	6.758400	-0.031109	3.310014
155.377004	3747.974190	6.763405	-0.031198	3.313512
155.478855	3756.011361	6.768410	-0.031223	3.317008
155.901359	3764.011578	6.773414	-0.031306	3.320496
156.032900	3772.024288	6.778419	-0.031336	3.323976
155.931221	3780.116183	6.783424	-0.031323	3.327476
156.247542	3788.150200	6.788429	-0.031387	3.330965
156.659375	3796.122822	6.793434	-0.031469	3.334426
156.465208	3804.186972	6.798438	-0.031438	3.337900
156.709048	3812.240700	6.803443	-0.031489	3.341383
156.531998	3820.272215	6.808448	-0.031461	3.344837
157.102745	3828.249987	6.813453	-0.031572	3.348292
157.113675	3836.339583	6.818458	-0.031580	3.351771
157.423727	3844.312275	6.823462	-0.031643	3.355207
157.491348	3852.364888	6.828467	-0.031661	3.358665
157.670836	3860.357703	6.833472	-0.031699	3.362097
157.785066	3868.417029	6.838477	-0.031726	3.365552
158.039030	3876.422811	6.843482	-0.031778	3.368986
158.335135	3884.454409	6.848486	-0.031839	3.372429
158.850621	3892.483299	6.853491	-0.031940	3.375876
159.092173	3900.460954	6.858496	-0.031990	3.379286
159.232095	3908.530400	6.863501	-0.032022	3.382729
159.436108	3916.585712	6.868506	-0.032065	3.386164
159.254180	3924.659856	6.873510	-0.032036	3.389590
159.671011	3932.701537	6.878515	-0.032119	3.393021
159.289072	3940.790774	6.883520	-0.032053	3.396439
160.191374	3948.655501	6.888525	-0.032227	3.399805
160.646838	3956.624972	6.893530	-0.032317	3.403196
160.601256	3964.700039	6.898534	-0.032313	3.406609
160.571572	3972.795144	6.903539	-0.032313	3.410029
160.628979	3980.820671	6.908544	-0.032329	3.413419
161.023225	3988.840462	6.913549	-0.032408	3.416815
161.100972	3996.885562	6.918554	-0.032428	3.420207
161.289191	4004.849957	6.923558	-0.032468	3.423566
161.723759	4012.895129	6.928563	-0.032554	3.426964
161.829068	4020.932286	6.933568	-0.032579	3.430343
161.934410	4028.971469	6.938573	-0.032604	3.433720
162.417157	4036.975140	6.943578	-0.032699	3.437092
162.470541	4045.008556	6.948582	-0.032714	3.440459
162.577214	4053.023039	6.953587	-0.032739	3.443815
162.512029	4061.100026	6.958592	-0.032733	3.447189
162.987130	4069.136400	6.963597	-0.032826	3.450561
162.753286	4077.174317	6.968602	-0.032788	3.453906
162.933568	4085.179780	6.973606	-0.032827	3.457248
163.074434	4093.248841	6.978611	-0.032858	3.460613
163.294951	4101.181112	6.983616	-0.032905	3.463919
163.333722	4109.257727	6.988621	-0.032917	3.467277
163.488272	4117.331987	6.993626	-0.032951	3.470634
163.668064	4125.297608	6.998630	-0.032990	3.473944
163.795530	4133.340756	7.003635	-0.033019	3.477280
164.059804	4141.345891	7.008640	-0.033074	3.480603
164.158015	4149.356377	7.013645	-0.033097	3.483919
163.854323	4157.425131	7.018650	-0.033046	3.487242
164.543703	4165.393490	7.023654	-0.033179	3.490554
164.459387	4173.483398	7.028659	-0.033169	3.493887
164.683774	4181.503947	7.033664	-0.033216	3.497198
165.068526	4189.492829	7.038669	-0.033293	3.500499
165.562549	4197.445019	7.043674	-0.033390	3.503785
165.669963	4205.509419	7.048678	-0.033416	3.507101
165.851788	4213.579410	7.053683	-0.033455	3.510419
165.917387	4221.614523	7.058688	-0.033472	3.513715
165.896644	4229.677761	7.063693	-0.033474	3.517018
165.772829	4237.739139	7.068698	-0.033456	3.520312
165.622309	4245.732193	7.073702	-0.033433	3.523576
166.448061	4253.708842	7.078707	-0.033592	3.526860
166.534454	4261.705195	7.083712	-0.033613	3.530126
166.975169	4269.730400	7.088717	-0.033701	3.533412
166.833685	4277.847683	7.093722	-0.033680	3.536714
167.111604	4285.827888	7.098726	-0.033737	3.539970
167.639071	4293.764762	7.103731	-0.033840	3.543214
167.793988	4301.846346	7.108736	-0.033874	3.546501
168.269111	4309.883910	7.113741	-0.033968	3.549778
168.408524	4317.994205	7.118746	-0.033999	3.553070
168.384607	4326.005854	7.123750	-0.034000	3.556314
168.797032	4333.936669	7.128755	-0.034082	3.559537
168.859635	4341.963335	7.133760	-0.034099	3.562784
168.597359	4350.036752	7.138765	-0.034056	3.566037
168.624415	4358.069947	7.143770	-0.034066	3.569280
168.918452	4366.070903	7.148774	-0.034126	3.572515
169.110622	4374.115628	7.153779	-0.034167	3.575761
169.394224	4382.077840	7.158784	-0.034225	3.578975
169.664218	4390.110506	7.163789	-0.034281	3.582213
169.663033	4398.135887	7.168794	-0.034286	3.585437
169.631204	4406.192576	7.173798	-0.034285	3.588670
169.742720	4414.294136	7.178803	-0.034311	3.591922
169.712904	4422.291982	7.183808	-0.034311	3.595125
170.130231	4430.229493	7.188813	-0.034394	3.598315
170.509326	4438.273909	7.193818	-0.034470	3.601544
170.352919	4446.305784	7.198822	-0.034446	3.604748
170.576751	4454.323833	7.203827	-0.034493	3.607956
170.680418	4462.354803	7.208832	-0.034517	3.611162
170.816007	4470.374956	7.213837	-0.034548	3.614362
171.284752	4478.404662	7.218842	-0.034640	3.617573
171.480077	4486.416068	7.223846	-0.034682	3.620765
171.739940	4494.416599	7.228851	-0.034736	3.623953
171.936169	4502.476882	7.233856	-0.034777	3.627159
172.166278	4510.497862	7.238861	-0.034826	3.630348
172.640728	4518.506850	7.243866	-0.034919	3.633536
172.396351	4526.597544	7.248870	-0.034879	3.636733
172.528420	4534.620165	7.253875	-0.034909	3.639911
172.555290	4542.624191	7.258880	-0.034919	3.643076
172.986735	4550.622218	7.263885	-0.035005	3.646248
172.922847	4558.687891	7.268890	-0.034998	3.649429
172.816277	4566.713699	7.273894	-0.034984	3.652591
173.172211	4574.758963	7.278899	-0.035055	3.655770
173.248099	4582.713674	7.283904	-0.035074	3.658903
173.672170	4590.730221	7.288909	-0.035159	3.662068
173.844769	4598.767529	7.293914	-0.035196	3.665231
174.131931	4606.768066	7.298918	-0.035255	3.668380
174.135202	4614.863855	7.303923	-0.035261	3.671555
174.167938	4622.861014	7.308928	-0.035272	3.674691
174.344184	4630.863065	7.313933	-0.035310	3.677829
174.458096	4638.960962	7.318938	-0.035337	3.681000
174.035827	4646.933423	7.323942	-0.035263	3.684105
175.232756	4654.858056	7.328947	-0.035491	3.687233
174.947762	4662.996243	7.333952	-0.035444	3.690401
175.014925	4671.000314	7.338957	-0.035461	3.693523
175.194038	4679.047671	7.343962	-0.035500	3.696663
175.617251	4686.987498	7.348966	-0.035584	3.699765
175.778669	4695.030601	7.353971	-0.035619	3.702897
175.534616	4703.122421	7.358976	-0.035579	3.706035
175.890106	4711.133197	7.363981	-0.035651	3.709155
176.067101	4719.232100	7.368986	-0.035689	3.712301
176.228448	4727.220550	7.373990	-0.035724	3.715401
176.728730	4735.147176	7.378995	-0.035823	3.718484
176.459189	4743.234314	7.384000	-0.035778	3.721606
176.894556	4751.152133	7.389005	-0.035864	3.724679
177.252006	4759.198269	7.394010	-0.035936	3.727796
177.064179	4767.277539	7.399014	-0.035906	3.730910
177.436157	4775.312112	7.404019	-0.035981	3.734018
177.329358	4783.350882	7.409024	-0.035966	3.737112
177.849840	4791.333388	7.414029	-0.036068	3.740199
178.149377	4799.338742	7.419034	-0.036129	3.743286
177.871119	4807.412747	7.424038	-0.036083	3.746382
178.086452	4815.452410	7.429043	-0.036128	3.749475
178.354913	4823.436780	7.434048	-0.036184	3.752546
178.765872	4831.426790	7.439053	-0.036265	3.755619
179.026376	4839.420144	7.444058	-0.036319	3.758688
179.341437	4847.447669	7.449062	-0.036383	3.761768
179.249145	4855.544648	7.454067	-0.036371	3.764863
179.509915	4863.503212	7.459072	-0.036425	3.767911
179.832927	4871.568278	7.464077	-0.036490	3.770998
179.799049	4879.607807	7.469082	-0.036489	3.774064
179.946623	4887.579350	7.474086	-0.036522	3.777107
180.210244	4895.614060	7.479091	-0.036576	3.780174
180.371662	4903.642123	7.484096	-0.036612	3.783233
180.290008	4911.705073	7.489101	-0.036602	3.786297
180.569571	4919.739723	7.494106	-0.036659	3.789357
180.821915	4927.729213	7.499110	-0.036711	3.792396
180.995848	4935.793473	7.504115	-0.036749	3.795459
181.195611	4943.719368	7.509120	-0.036792	3.798468
181.501810	4951.756427	7.514125	-0.036854	3.801519
181.517123	4959.802220	7.519130	-0.036862	3.804565
181.615384	4967.794895	7.524134	-0.036886	3.807589
182.260933	4975.830933	7.529139	-0.037011	3.810640
182.165322	4983.850824	7.534144	-0.036999	3.813666
182.111930	4991.941560	7.539149	-0.036994	3.816717
182.059844	4999.969900	7.544154	-0.036989	3.819742
182.175257	5007.949746	7.549158	-0.037016	3.822750
182.581966	5015.979073	7.554163	-0.037097	3.825780
183.214595	5023.885186	7.559168	-0.037220	3.828768
183.498625	5031.949832	7.564173	-0.037278	3.831804
183.842953	5039.987482	7.569178	-0.037348	3.834829
183.822776	5047.989905	7.574182	-0.037349	3.837831
183.971192	5056.106145	7.579187	-0.037382	3.840876
184.394622	5064.032630	7.584192	-0.037466	3.843854
184.663192	5072.105540	7.589197	-0.037522	3.846881
184.522281	5080.208815	7.594202	-0.037501	3.849909
184.691117	5088.175865	7.599206	-0.037537	3.852889
185.029180	5096.263165	7.604211	-0.037606	3.855916
185.398737	5104.173487	7.609216	-0.037680	3.858875
185.530333	5112.230254	7.614221	-0.037709	3.861881
185.594906	5120.277921	7.619226	-0.037727	3.864880
185.509530	5128.322822	7.624230	-0.037716	3.867873
185.950115	5136.359082	7.629235	-0.037803	3.870871
186.331788	5144.426967	7.634240	-0.037880	3.873877
186.405204	5152.395928	7.639245	-0.037899	3.876837
186.639304	5160.388055	7.644250	-0.037948	3.879808
186.720750	5168.383197	7.649254	-0.037968	3.882774
186.569245	5176.459079	7.654259	-0.037945	3.885762
186.456413	5184.466406	7.659264	-0.037929	3.888724
187.029948	5192.429813	7.664269	-0.038041	3.891682
187.302727	5200.467740	7.669274	-0.038097	3.894658
187.354302	5208.437899	7.674278	-0.038112	3.897603
187.224054	5216.529903	7.679283	-0.038093	3.900586
187.489159	5224.462402	7.684288	-0.038148	3.903517
187.828991	5232.512171	7.689293	-0.038217	3.906490
188.096157	5240.540797	7.694298	-0.038272	3.909452
187.853293	5248.629611	7.699302	-0.038232	3.912423
188.160385	5256.639537	7.704307	-0.038294	3.915374
188.649141	5264.565948	7.709312	-0.038390	3.918295
188.802928	5272.637277	7.714317	-0.038424	3.921261
189.183587	5280.586866	7.719322	-0.038500	3.924185
189.379691	5288.618845	7.724326	-0.038542	3.927133
189.025840	5296.729627	7.729331	-0.038482	3.930096
189.939788	5304.680360	7.734336	-0.038657	3.933024
189.870795	5312.782286	7.739341	-0.038649	3.935985
189.895666	5320.751181	7.744346	-0.038659	3.938898
190.189755	5328.770931	7.749350	-0.038719	3.941832
190.504062	5336.785466	7.754355	-0.038783	3.944762
190.447521	5344.833057	7.759360	-0.038778	3.947695
190.665002	5352.869020	7.764365	-0.038824	3.950627
190.762906	5360.922359	7.769370	-0.038847	3.953561
190.947906	5368.942061	7.774374	-0.038887	3.956482
190.991073	5376.960422	7.779379	-0.038900	3.959398
190.992628	5384.973941	7.784384	-0.038906	3.962308
191.045649	5392.953752	7.789389	-0.038921	3.965206
191.216613	5400.986853	7.794394	-0.038958	3.968123
191.636325	5408.991019	7.799398	-0.039041	3.971032
191.609650	5417.046046	7.804403	-0.039042	3.973949
191.671595	5425.088754	7.809408	-0.039059	3.976860
191.886219	5433.072795	7.814413	-0.039104	3.979752
192.606689	5441.039397	7.819418	-0.039243	3.982644
192.715962	5449.074278	7.824422	-0.039269	3.985547
192.825655	5457.153998	7.829427	-0.039295	3.988465
192.695941	5465.216770	7.834432	-0.039276	3.991370
193.183989	5473.113081	7.839437	-0.039372	3.994223
193.300008	5481.192929	7.844442	-0.039399	3.997135
193.550642	5489.195824	7.849446	-0.039451	4.000019
193.961555	5497.154318	7.854451	-0.039532	4.002887
194.250180	5505.178467	7.859456	-0.039591	4.005775
194.228934	5513.224223	7.864461	-0.039593	4.008663
194.197166	5521.349407	7.869466	-0.039592	4.011577
194.146221	5529.317621	7.874470	-0.039588	4.014433
194.471295	5537.354813	7.879475	-0.039654	4.017318
194.732926	5545.318029	7.884480	-0.039708	4.020173
194.585661	5553.357687	7.889485	-0.039685	4.023046
194.929887	5561.398460	7.894490	-0.039755	4.025926
194.867514	5569.390588	7.899494	-0.039748	4.028780
195.247083	5577.449291	7.904499	-0.039824	4.031663
195.330607	5585.479409	7.909504	-0.039845	4.034529
195.709348	5593.460558	7.914509	-0.039921	4.037380
195.843138	5601.507804	7.919514	-0.039951	4.040248
195.740609	5609.505772	7.924518	-0.039937	4.043093
195.932243	5617.557481	7.929523	-0.039978	4.045960
195.874962	5625.520771	7.934528	-0.039973	4.048790
196.216370	5633.554369	7.939533	-0.040042	4.051649
196.356284	5641.573762	7.944538	-0.040073	4.054497
196.693025	5649.555759	7.949542	-0.040141	4.057333
196.514737	5657.634162	7.954547	-0.040113	4.060194
197.017659	5665.584971	7.959552	-0.040212	4.063018
197.124880	5673.592442	7.964557	-0.040237	4.065853
197.354459	5681.678795	7.969562	-0.040285	4.068717
197.811853	5689.695641	7.974566	-0.040376	4.071557
198.016496	5697.683255	7.979571	-0.040419	4.074382
198.515231	5705.696559	7.984576	-0.040517	4.077217
198.654889	5713.714253	7.989581	-0.040549	4.080047
198.824299	5721.753144	7.994586	-0.040585	4.082883
198.629940	5729.793675	7.999590	-0.040554	4.085712
198.956534	5737.822959	8.004595	-0.040621	4.088542
199.070534	5745.918422	8.009600	-0.040647	4.091391
199.173272	5753.877875	8.014605	-0.040671	4.094190
199.330818	5761.957025	8.019610	-0.040706	4.097030
199.898053	5769.856634	8.024614	-0.040817	4.099811
199.728380	5777.928591	8.029619	-0.040791	4.102639
199.559551	5785.995327	8.034624	-0.040764	4.105464
199.954158	5793.960636	8.039629	-0.040843	4.108259
200.144258	5802.035365	8.044634	-0.040884	4.111088
200.049591	5809.998724	8.049638	-0.040872	4.113872
200.458818	5818.031072	8.054643	-0.040953	4.116685
200.572525	5826.022859	8.059648	-0.040979	4.119478
200.439191	5834.072067	8.064653	-0.040960	4.122286
200.750373	5842.062448	8.069658	-0.041023	4.125077
200.959340	5850.053470	8.074662	-0.041067	4.127865
201.402803	5858.094536	8.079667	-0.041155	4.130672
201.598117	5866.075637	8.084672	-0.041197	4.133453
201.663561	5874.136406	8.089677	-0.041214	4.136258
201.810623	5882.164469	8.094682	-0.041247	4.139051
201.924432	5890.160651	8.099686	-0.041273	4.141830
202.081365	5898.186688	8.104691	-0.041308	4.144618
202.341072	5906.220571	8.109696	-0.041361	4.147409
202.538942	5914.223597	8.114701	-0.041404	4.150186
202.748488	5922.236138	8.119706	-0.041448	4.152964
202.874461	5930.252778	8.124710	-0.041477	4.155741
203.170076	5938.252231	8.129715	-0.041537	4.158513
203.368012	5946.318606	8.134720	-0.041579	4.161304
203.663928	5954.213299	8.139725	-0.041639	4.164035
203.859168	5962.331391	8.144730	-0.041681	4.166841
204.031781	5970.357214	8.149734	-0.041718	4.169612
203.937153	5978.448032	8.154739	-0.041706	4.172401
204.067356	5986.420051	8.159744	-0.041736	4.175149
204.280685	5994.429752	8.164749	-0.041781	4.177910
204.515045	6002.448629	8.169754	-0.041829	4.180673
204.751508	6010.402002	8.174758	-0.041879	4.183411
204.884665	6018.484318	8.179763	-0.041909	4.186190
205.120443	6026.483869	8.184768	-0.041958	4.188940
205.257714	6034.528644	8.189773	-0.041989	4.191703
205.640177	6042.621211	8.194778	-0.042065	4.194483
205.793569	6050.558708	8.199782	-0.042099	4.197205
205.686744	6058.612544	8.204787	-0.042085	4.199963
205.978933	6066.584016	8.209792	-0.042144	4.202695
206.132915	6074.581048	8.214797	-0.042178	4.205432
206.244137	6082.624098	8.219802	-0.042204	4.208183
206.326527	6090.641442	8.224806	-0.042225	4.210923
206.607325	6098.671105	8.229811	-0.042282	4.213667
206.687453	6106.773244	8.234816	-0.042303	4.216432
206.872221	6114.675753	8.239821	-0.042342	4.219129
207.177086	6122.727001	8.244826	-0.042404	4.221876
206.873956	6130.747634	8.249830	-0.042353	4.224603
207.455174	6138.746315	8.254835	-0.042466	4.227332
207.794265	6146.775711	8.259840	-0.042535	4.230066
207.962559	6154.792981	8.264845	-0.042572	4.232792
208.311963	6162.840040	8.269850	-0.042642	4.235529
208.193389	6170.826384	8.274854	-0.042625	4.238238
208.418405	6178.895313	8.279859	-0.042672	4.240978
208.326105	6186.852395	8.284864	-0.042660	4.243674
208.484778	6194.916371	8.289869	-0.042695	4.246407
208.676672	6202.927386	8.294874	-0.042736	4.249121
208.950352	6210.947546	8.299878	-0.042792	4.251837
208.807311	6218.993128	8.304883	-0.042771	4.254556
208.972303	6226.995594	8.309888	-0.042807	4.257261
209.296962	6234.956768	8.314893	-0.042873	4.259953
209.822912	6242.997577	8.319898	-0.042976	4.262671
209.955320	6250.990682	8.324902	-0.043006	4.265368
209.796075	6259.069853	8.329907	-0.042981	4.268089
210.069420	6267.088502	8.334912	-0.043038	4.270793
210.340448	6275.035404	8.339917	-0.043093	4.273470
210.678232	6283.131233	8.344922	-0.043162	4.276197
210.947412	6291.029965	8.349926	-0.043217	4.278854
210.972313	6299.124813	8.354931	-0.043227	4.281574
211.234255	6307.047827	8.359936	-0.043281	4.284236
211.640261	6315.120732	8.364941	-0.043362	4.286949
211.729073	6323.151966	8.369946	-0.043383	4.289642
211.809368	6331.206238	8.374950	-0.043404	4.292342
212.011538	6339.200687	8.379955	-0.043447	4.295021
212.023224	6347.268924	8.384960	-0.043454	4.297721
211.995884	6355.244336	8.389965	-0.043454	4.300388
212.273675	6363.242565	8.394970	-0.043511	4.303064
212.560668	6371.239100	8.399974	-0.043570	4.305738
212.631817	6379.271770	8.404979	-0.043588	4.308420
212.629010	6387.386338	8.409984	-0.043593	4.311127
212.876661	6395.275530	8.414989	-0.043645	4.313760
213.268975	6403.360812	8.419994	-0.043723	4.316457
213.101035	6411.282067	8.424998	-0.043697	4.319093
213.308169	6419.370154	8.430003	-0.043741	4.321786
213.669062	6427.315767	8.435008	-0.043813	4.324432
213.609274	6435.400184	8.440013	-0.043807	4.327119
213.889537	6443.433079	8.445018	-0.043865	4.329789
214.250738	6451.410699	8.450022	-0.043937	4.332440
214.467429	6459.455315	8.455027	-0.043983	4.335111
214.621687	6467.470730	8.460032	-0.044017	4.337770
214.860819	6475.451357	8.465037	-0.044067	4.340416
214.913869	6483.482968	8.470042	-0.044082	4.343076
214.913888	6491.500990	8.475046	-0.044087	4.345729
215.233425	6499.518183	8.480051	-0.044152	4.348383
215.451690	6507.622177	8.485056	-0.044198	4.351063
215.681354	6515.568380	8.490061	-0.044246	4.353690
215.945938	6523.627461	8.495066	-0.044300	4.356352
216.079241	6531.566825	8.500070	-0.044330	4.358973
215.945861	6539.651631	8.505075	-0.044311	4.361637
216.385348	6547.530252	8.510080	-0.044398	4.364237
216.296538	6555.642809	8.515085	-0.044387	4.366908
216.424675	6563.666267	8.520090	-0.044416	4.369549
216.597739	6571.668009	8.525094	-0.044453	4.372182
216.871633	6579.626839	8.530099	-0.044510	4.374800
217.117099	6587.713805	8.535104	-0.044561	4.377459
217.023943	6595.683717	8.540109	-0.044549	4.380075
217.012339	6603.796538	8.545114	-0.044552	4.382736
217.270315	6611.752406	8.550118	-0.044605	4.385347
217.424227	6619.761999	8.555123	-0.044639	4.387973
217.474062	6627.813900	8.560128	-0.044653	4.390610
217.685022	6635.796754	8.565133	-0.044698	4.393225
218.054132	6643.849972	8.570138	-0.044772	4.395862
217.678881	6651.854416	8.575143	-0.044707	4.398476
217.912114	6659.888602	8.580147	-0.044756	4.401103
218.521018	6667.776799	8.585152	-0.044875	4.403682
218.685538	6675.847001	8.590157	-0.044911	4.406317
218.741977	6683.898349	8.595162	-0.044926	4.408943
218.888177	6691.940349	8.600167	-0.044959	4.411565
218.921338	6699.943332	8.605171	-0.044970	4.414172
218.891558	6708.039543	8.610176	-0.044970	4.416808
219.165063	6715.990006	8.615181	-0.045026	4.419397
219.752134	6724.030712	8.620186	-0.045141	4.422015
219.782994	6732.017369	8.625191	-0.045152	4.424610
219.636142	6740.118671	8.630195	-0.045130	4.427241
220.252089	6748.105306	8.635200	-0.045250	4.429837
220.226787	6756.157285	8.640205	-0.045250	4.432448
220.581237	6764.169822	8.645210	-0.045322	4.435048
220.665301	6772.180306	8.650215	-0.045343	4.437644
220.883023	6780.199993	8.655219	-0.045388	4.440242
220.877105	6788.200257	8.660224	-0.045392	4.442831
220.977215	6796.199565	8.665229	-0.045416	4.445419
220.996118	6804.271580	8.670234	-0.045425	4.448028
221.121600	6812.305049	8.675239	-0.045454	4.450624
221.068202	6820.315190	8.680243	-0.045449	4.453210
221.536681	6828.353623	8.685248	-0.045542	4.455807
221.461156	6836.330908	8.690253	-0.045533	4.458379
221.911945	6844.333690	8.695258	-0.045622	4.460960
221.819433	6852.299194	8.700263	-0.045610	4.463526
222.022453	6860.424847	8.705267	-0.045653	4.466143
222.458375	6868.393670	8.710272	-0.045740	4.468709
222.536472	6876.424963	8.715277	-0.045759	4.471291
222.410184	6884.466821	8.720282	-0.045741	4.473875
222.506629	6892.517875	8.725287	-0.045764	4.476461
222.590466	6900.443441	8.730291	-0.045785	4.479006
222.950122	6908.503072	8.735296	-0.045858	4.481593
222.891102	6916.420345	8.740301	-0.045852	4.484131
223.596862	6924.517870	8.745306	-0.045989	4.486729
223.892802	6932.458124	8.750311	-0.046049	4.489273
224.212051	6940.490513	8.755315	-0.046114	4.491845
224.330491	6948.559533	8.760320	-0.046141	4.494427
224.527977	6956.515016	8.765325	-0.046183	4.496971
224.582903	6964.624471	8.770330	-0.046198	4.499562
224.673388	6972.604208	8.775335	-0.046221	4.502111
225.125353	6980.547900	8.780339	-0.046310	4.504648
225.246102	6988.668631	8.785344	-0.046338	4.507238
225.289301	6996.662751	8.790349	-0.046351	4.509787
225.629559	7004.725607	8.795354	-0.046420	4.512357
225.661554	7012.657447	8.800359	-0.046431	4.514883
226.058813	7020.654423	8.805363	-0.046510	4.517429
226.255119	7028.670071	8.810368	-0.046552	4.519979
225.940104	7036.665406	8.815373	-0.046499	4.522519
226.619855	7044.679127	8.820378	-0.046630	4.525068
226.406484	7052.728595	8.825383	-0.046596	4.527623
226.557107	7060.771918	8.830387	-0.046629	4.530176
227.057456	7068.776949	8.835392	-0.046728	4.532716
227.141788	7076.763184	8.840397	-0.046749	4.535248
227.240942	7084.833628	8.845402	-0.046772	4.537804
227.115427	7092.826956	8.850407	-0.046754	4.540335
227.496306	7100.788431	8.855411	-0.046830	4.542855
227.669640	7108.840300	8.860416	-0.046868	4.545402
227.693645	7116.846709	8.865421	-0.046878	4.547933
228.014077	7124.930155	8.870426	-0.046943	4.550487
228.401466	7132.888133	8.875431	-0.047020	4.553001
228.381364	7140.921344	8.880435	-0.047022	4.555536
228.425147	7148.906029	8.885440	-0.047035	4.558054
228.726270	7156.862408	8.890445	-0.047096	4.560562
229.024659	7164.888742	8.895450	-0.047157	4.563091
228.961783	7172.927327	8.900455	-0.047151	4.565622
229.039921	7180.999098	8.905459	-0.047171	4.568162
229.321441	7189.032246	8.910464	-0.047228	4.570689
229.330184	7197.028130	8.915469	-0.047235	4.573202
229.723095	7205.077532	8.920474	-0.047314	4.575732
229.762553	7213.070202	8.925479	-0.047326	4.578241
229.805807	7221.086165	8.930483	-0.047340	4.580757
229.835661	7229.090709	8.935488	-0.047350	4.583267
229.708259	7237.151409	8.940493	-0.047332	4.585793
229.889447	7245.144955	8.945498	-0.047371	4.588298
230.071119	7253.105042	8.950503	-0.047410	4.590790
230.571140	7261.098762	8.955507	-0.047508	4.593293
230.525468	7269.199720	8.960512	-0.047505	4.595826
230.557065	7277.162886	8.965517	-0.047516	4.598315
230.877181	7285.186983	8.970522	-0.047581	4.600823
231.026787	7293.109357	8.975527	-0.047614	4.603297
231.460474	7301.162899	8.980531	-0.047700	4.605810
231.249756	7309.262775	8.985536	-0.047666	4.608336
231.353791	7317.248548	8.990541	-0.047691	4.610826
231.670444	7325.258925	8.995546	-0.047755	4.613322
231.529912	7333.343622	9.000551	-0.047734	4.615839
231.235669	7341.324840	9.005555	-0.047685	4.618323
231.849650	7349.334422	9.010560	-0.047804	4.620815
231.709963	7357.267487	9.015565	-0.047784	4.623281
232.185647	7365.365814	9.020570	-0.047877	4.625797
231.965955	7373.387117	9.025575	-0.047842	4.628288
232.305647	7381.372053	9.030579	-0.047910	4.630767
232.497698	7389.375833	9.035584	-0.047951	4.633250
232.589768	7397.404341	9.040589	-0.047974	4.635739
232.833037	7405.385528	9.045594	-0.048024	4.638212
233.243781	7413.422223	9.050599	-0.048106	4.640701
233.439615	7421.377963	9.055603	-0.048148	4.643164
233.859106	7429.467942	9.060608	-0.048231	4.645667
233.686302	7437.454018	9.065613	-0.048204	4.648136
233.607558	7445.587694	9.070618	-0.048195	4.650650
233.831561	7453.519277	9.075623	-0.048242	4.653099
234.244798	7461.524841	9.080627	-0.048324	4.655571
234.070574	7469.557275	9.085632	-0.048297	4.658049
234.504874	7477.533096	9.090637	-0.048383	4.660509
234.791765	7485.543693	9.095642	-0.048442	4.662977
234.655824	7493.604157	9.100647	-0.048422	4.665460
235.100952	7501.562641	9.105651	-0.048510	4.667910
235.333138	7509.693813	9.110656	-0.048558	4.670412
235.265305	7517.689057	9.115661	-0.048551	4.672871
235.103953	7525.711762	9.120666	-0.048526	4.675337
235.580657	7533.653045	9.125671	-0.048620	4.677777
235.570345	7541.681358	9.130675	-0.048624	4.680242
236.037352	7549.631250	9.135680	-0.048716	4.682682
236.278623	7557.614587	9.140685	-0.048766	4.685130
235.844436	7565.765851	9.145690	-0.048690	4.687629
235.927723	7573.773655	9.150695	-0.048711	4.690083
236.013933	7581.777542	9.155699	-0.048733	4.692534
236.516145	7589.766336	9.160704	-0.048831	4.694979
236.720173	7597.768867	9.165709	-0.048875	4.697427
236.775156	7605.772149	9.170714	-0.048890	4.699874
237.186461	7613.798141	9.175719	-0.048972	4.702326
237.201869	7621.753535	9.180723	-0.048980	4.704756
237.164277	7629.918476	9.185728	-0.048978	4.707249
237.449934	7637.869935	9.190733	-0.049037	4.709674
237.583595	7645.946866	9.195738	-0.049067	4.712137
237.353299	7653.906690	9.200743	-0.049029	4.714564
237.118446	7662.000701	9.205747	-0.048991	4.717030
237.631423	7669.885867	9.210752	-0.049092	4.719430
237.410239	7677.966732	9.215757	-0.049056	4.721890
237.443176	7685.898988	9.220762	-0.049067	4.724302
238.314346	7693.931049	9.225767	-0.049235	4.726743
238.324007	7701.918816	9.230771	-0.049242	4.729170
238.659858	7709.960832	9.235776	-0.049309	4.731611
238.582016	7717.986251	9.240781	-0.049300	4.734048
238.783476	7726.093610	9.245786	-0.049343	4.736507
238.665966	7734.052952	9.250791	-0.049326	4.738920
238.965599	7742.128171	9.255795	-0.049388	4.741367
239.284632	7750.117088	9.260800	-0.049452	4.743786
239.447805	7758.108137	9.265805	-0.049488	4.746205
239.737044	7766.128972	9.270810	-0.049547	4.748632
239.944680	7774.171004	9.275815	-0.049591	4.751063
240.304073	7782.140868	9.280819	-0.049663	4.753472
240.393069	7790.231764	9.285824	-0.049685	4.755916
240.178806	7798.139422	9.290829	-0.049650	4.758304
240.126983	7806.268505	9.295834	-0.049646	4.760758
240.578688	7814.166696	9.300839	-0.049735	4.763139
240.501345	7822.229333	9.305843	-0.049726	4.765570
241.191370	7830.204108	9.310848	-0.049860	4.767972
241.023456	7838.312614	9.315853	-0.049834	4.770415
241.053919	7846.337763	9.320858	-0.049845	4.772830
241.227639	7854.331967	9.325863	-0.049882	4.775235
241.389571	7862.347820	9.330867	-0.049918	4.777645
241.386631	7870.388053	9.335872	-0.049923	4.780062
241.376106	7878.357450	9.340877	-0.049926	4.782456
241.376906	7886.399593	9.345882	-0.049931	4.784871
241.709428	7894.441844	9.350887	-0.049999	4.787284
241.868044	7902.439667	9.355891	-0.050033	4.789683
242.101018	7910.495461	9.360896	-0.050082	4.792097
242.328753	7918.393837	9.365901	-0.050130	4.794463
242.360503	7926.538065	9.370906	-0.050141	4.796903
242.578641	7934.416247	9.375911	-0.050187	4.799260
242.725300	7942.521980	9.380915	-0.050219	4.801685
243.017067	7950.464368	9.385920	-0.050279	4.804059
243.003472	7958.554575	9.390925	-0.050282	4.806478
243.452881	7966.555010	9.395930	-0.050371	4.808866
243.289297	7974.646390	9.400935	-0.050345	4.811283
243.290252	7982.554404	9.405939	-0.050351	4.813643
243.518809	7990.015856	9.410944	-0.050398	4.815868
243.372328	7994.732563	9.415949	-0.050374	4.817276

243.924180	7997.146891	9.420954	-0.050478	4.817993
243.601021	7998.823768	9.425959	-0.050419	4.818494
243.863045	7999.574892	9.430963	-0.050469	4.818717
244.341118	7999.767346	9.435968	-0.050558	4.818773
244.161106	8000.456403	9.440973	-0.050525	4.818979
244.338870	8000.505781	9.445978	-0.050558	4.818993
244.610259	8000.452638	9.450983	-0.050609	4.818976
244.528924	8000.471519	9.455987	-0.050594	4.818982
244.695035	8000.481994	9.460992	-0.050625	4.818984
244.626842	8000.488471	9.465997	-0.050612	4.818987
244.853943	8000.431627	9.471002	-0.050654	4.818969
244.454726	8000.432887	9.476007	-0.050580	4.818971
244.710944	8000.395265	9.481011	-0.050628	4.818959
244.924587	8000.485948	9.486016	-0.050667	4.818985
244.861135	8000.485152	9.491021	-0.050656	4.818985
244.930165	8000.417937	9.496026	-0.050669	4.818965
244.863554	8000.459001	9.501031	-0.050656	4.818977
244.647082	8000.419615	9.506035	-0.050616	4.818966
244.620141	8000.406709	9.511040	-0.050611	4.818962
244.707415	8000.433999	9.516045	-0.050627	4.818970
245.168494	8000.489042	9.521050	-0.050713	4.818985
245.350253	8000.452577	9.526055	-0.050747	4.818973
245.392752	8000.473018	9.531059	-0.050755	4.818979
245.501270	8000.485911	9.536064	-0.050775	4.818983
245.253632	8000.406326	9.541069	-0.050729	4.818960
245.465364	8000.526318	9.546074	-0.050769	4.818995
245.583388	8000.480670	9.551079	-0.050791	4.818981
245.452196	8000.507303	9.556083	-0.050766	4.818989
245.543381	8000.487504	9.561088	-0.050783	4.818983
245.637701	8000.388135	9.566093	-0.050801	4.818953
245.556266	8000.480340	9.571098	-0.050786	4.818981
245.687672	8000.480952	9.576103	-0.050810	4.818980
245.647098	8000.471016	9.581107	-0.050803	4.818978
245.776586	8000.495696	9.586112	-0.050827	4.818984
245.758102	8000.461945	9.591117	-0.050824	4.818975
245.811273	8000.479379	9.596122	-0.050834	4.818979
245.977398	8000.463668	9.601127	-0.050865	4.818974
245.981311	8000.467910	9.606131	-0.050865	4.818975
245.835052	8000.495400	9.611136	-0.050838	4.818984
245.736651	8000.464833	9.616141	-0.050820	4.818975
245.871361	8000.502149	9.621146	-0.050845	4.818986
245.892871	8000.456332	9.626151	-0.050849	4.818972
245.905906	8000.436597	9.631155	-0.050851	4.818966
245.947816	8000.490551	9.636160	-0.050859	4.818982
245.745895	8000.500580	9.641165	-0.050822	4.818986
245.855937	8000.422358	9.646170	-0.050842	4.818962
245.993164	8000.481704	9.651175	-0.050868	4.818979
245.965975	8000.502315	9.656179	-0.050863	4.818986
246.229040	8000.492016	9.661184	-0.050912	4.818982
245.736144	8000.409338	9.666189	-0.050820	4.818959
245.725401	8000.207038	9.671194	-0.050818	4.818899
245.701782	8000.382723	9.676199	-0.050814	4.818951
245.703358	8000.365986	9.681203	-0.050814	4.818946
246.177814	8000.386633	9.686208	-0.050903	4.818950
245.970019	8000.480389	9.691213	-0.050864	4.818979
245.924726	8000.374022	9.696218	-0.050856	4.818948
245.930276	8000.456849	9.701223	-0.050857	4.818972
245.921361	8000.376081	9.706227	-0.050855	4.818948
245.646896	8000.229118	9.711232	-0.050804	4.818906
245.879235	8000.412219	9.716237	-0.050847	4.818959
245.991082	8000.447152	9.721242	-0.050868	4.818969
245.762197	8000.421225	9.726247	-0.050826	4.818962
245.628871	8000.324225	9.731251	-0.050801	4.818934
245.869896	8000.360785	9.736256	-0.050846	4.818944
245.932842	8000.407672	9.741261	-0.050857	4.818958
245.871219	8000.445656	9.746266	-0.050846	4.818969
245.989821	8000.519433	9.751271	-0.050868	4.818991
246.131025	8000.355707	9.756275	-0.050894	4.818941
246.080357	8000.347739	9.761280	-0.050885	4.818939
245.868229	8000.406872	9.766285	-0.050846	4.818958
245.849327	8000.342739	9.771290	-0.050842	4.818939
245.873327	8000.214201	9.776295	-0.050847	4.818900
245.922073	8000.141494	9.781299	-0.050856	4.818878
245.989306	8000.071114	9.786304	-0.050868	4.818857
245.568390	8000.269029	9.791309	-0.050790	4.818918
245.548636	7999.871787	9.796314	-0.050786	4.818799
246.152196	8000.050129	9.801319	-0.050899	4.818850
246.043022	8000.185980	9.806323	-0.050878	4.818891
246.214975	8000.353656	9.811328	-0.050911	4.818940
246.306205	8000.485749	9.816333	-0.050928	4.818979
246.278139	8000.442450	9.821338	-0.050922	4.818967
246.051485	8000.160958	9.826343	-0.050880	4.818884
245.761345	7999.903815	9.831347	-0.050826	4.818808
245.984899	8000.111940	9.836352	-0.050868	4.818869
245.834356	7999.851319	9.841357	-0.050840	4.818792
246.371271	8000.140906	9.846362	-0.050940	4.818876
246.024811	8000.181587	9.851367	-0.050875	4.818890
246.205673	7999.967036	9.856371	-0.050909	4.818825
246.230976	7999.938028	9.861376	-0.050914	4.818817
246.227884	8000.221865	9.866381	-0.050913	4.818901
246.266126	8000.066271	9.871386	-0.050920	4.818855
246.099417	8000.120739	9.876391	-0.050889	4.818871
246.388857	8000.344367	9.881395	-0.050944	4.818937
246.128481	8000.026837	9.886400	-0.050895	4.818843
246.485922	8000.305790	9.891405	-0.050962	4.818925
246.583196	8000.335302	9.896410	-0.050980	4.818934
246.538791	8000.401787	9.901415	-0.050972	4.818954
246.249977	8000.409673	9.906419	-0.050918	4.818957
246.007662	8000.044185	9.911424	-0.050873	4.818849
246.397924	8000.519439	9.916429	-0.050946	4.818989
246.488058	8000.156040	9.921434	-0.050962	4.818881
246.325876	8000.354075	9.926439	-0.050932	4.818940
246.409184	8000.339415	9.931443	-0.050948	4.818935
246.713193	8000.300302	9.936448	-0.051004	4.818923
246.569889	8000.299546	9.941453	-0.050978	4.818923
246.692365	8000.029785	9.946458	-0.051000	4.818842
246.676152	8000.402502	9.951463	-0.050998	4.818953
246.475505	8000.347599	9.956467	-0.050960	4.818938
246.795347	8000.335921	9.961472	-0.051020	4.818933
246.593788	8000.489465	9.966477	-0.050983	4.818979
246.820597	8000.433666	9.971482	-0.051025	4.818962
246.715781	8000.349592	9.976487	-0.051005	4.818937
246.453719	8000.409143	9.981491	-0.050957	4.818956
246.455343	8000.288701	9.986496	-0.050957	4.818920
246.217395	8000.277326	9.991501	-0.050913	4.818918
246.180706	7999.973091	9.996506	-0.050906	4.818827
246.499661	8000.424400	10.001511	-0.050965	4.818960
246.742099	8000.326896	10.006515	-0.051010	4.818930
246.849508	8000.364917	10.011520	-0.051030	4.818941
246.608107	8000.359781	10.016525	-0.050986	4.818941
246.930837	8000.286336	10.021530	-0.051046	4.818918
247.012064	8000.424590	10.026535	-0.051061	4.818959
246.951633	8000.384024	10.031539	-0.051050	4.818947
246.780052	8000.086462	10.036544	-0.051018	4.818859
246.983443	8000.276535	10.041549	-0.051056	4.818915
247.117415	8000.509734	10.046554	-0.051081	4.818984
247.146794	8000.491252	10.051559	-0.051086	4.818978
247.246769	8000.355287	10.056563	-0.051105	4.818937
247.213053	8000.219733	10.061568	-0.051099	4.818897
246.734445	8000.395973	10.066573	-0.051010	4.818951
246.976081	8000.183230	10.071578	-0.051054	4.818887
247.284372	8000.455290	10.076583	-0.051112	4.818967
247.243314	8000.381447	10.081587	-0.051104	4.818945
247.002114	8000.221279	10.086592	-0.051059	4.818898
247.036440	8000.451125	10.091597	-0.051066	4.818966
247.076307	8000.160416	10.096602	-0.051073	4.818880
247.365383	8000.413378	10.101607	-0.051127	4.818954
247.347694	8000.511627	10.106611	-0.051124	4.818983
247.187384	8000.257150	10.111616	-0.051094	4.818908
247.328574	8000.523963	10.116621	-0.051121	4.818987
247.515273	8000.445659	10.121626	-0.051155	4.818963
247.448817	8000.352639	10.126631	-0.051143	4.818935
247.344429	8000.475984	10.131635	-0.051124	4.818973
247.402362	8000.248353	10.136640	-0.051134	4.818905
247.257522	8000.439277	10.141645	-0.051108	4.818962
247.293200	8000.380020	10.146650	-0.051114	4.818944
247.187945	8000.428978	10.151655	-0.051095	4.818959
247.303827	8000.516342	10.156659	-0.051116	4.818985
247.466481	8000.339265	10.161664	-0.051147	4.818931
247.311719	8000.513305	10.166669	-0.051118	4.818984
247.263181	8000.308424	10.171674	-0.051109	4.818923
247.150336	8000.452612	10.176679	-0.051088	4.818966
247.179564	8000.424700	10.181683	-0.051093	4.818958
247.236573	8000.199153	10.186688	-0.051104	4.818891
247.112055	8000.287675	10.191693	-0.051081	4.818917
247.235515	8000.365705	10.196698	-0.051104	4.818940
247.085325	8000.318770	10.201703	-0.051076	4.818927
247.212482	8000.507887	10.206707	-0.051100	4.818983
247.359715	8000.335853	10.211712	-0.051127	4.818931
247.368733	8000.400918	10.216717	-0.051129	4.818950
247.375953	8000.388442	10.221722	-0.051130	4.818946
247.289801	8000.413547	10.226727	-0.051114	4.818954
247.335381	8000.347082	10.231731	-0.051123	4.818934
247.380188	8000.351840	10.236736	-0.051131	4.818935
247.680590	8000.422675	10.241741	-0.051187	4.818955
247.643459	8000.529061	10.246746	-0.051181	4.818987
247.641433	8000.531134	10.251751	-0.051180	4.818988
247.700265	8000.525593	10.256755	-0.051191	4.818986
248.014565	8000.525372	10.261760	-0.051250	4.818985
248.028868	8000.435464	10.266765	-0.051252	4.818958
247.833436	8000.447668	10.271770	-0.051216	4.818962
247.802684	8000.527945	10.276775	-0.051210	4.818986
247.965973	8000.528961	10.281779	-0.051241	4.818986
247.791255	8000.528855	10.286784	-0.051208	4.818987
247.788518	8000.494253	10.291789	-0.051208	4.818976
247.909253	8000.512541	10.296794	-0.051230	4.818981
247.737981	8000.515621	10.301799	-0.051199	4.818983
247.605336	8000.425955	10.306803	-0.051174	4.818957
247.905943	8000.535555	10.311808	-0.051230	4.818988
247.851238	8000.483537	10.316813	-0.051220	4.818973
247.908331	8000.533496	10.321818	-0.051230	4.818988
247.867006	8000.355939	10.326823	-0.051223	4.818935
247.723093	8000.521736	10.331827	-0.051196	4.818985
247.565266	8000.388803	10.336832	-0.051167	4.818946
247.472892	8000.425353	10.341837	-0.051150	4.818957
247.676353	8000.445731	10.346842	-0.051187	4.818962
247.767491	8000.446884	10.351847	-0.051204	4.818962
247.619938	8000.529878	10.356851	-0.051177	4.818988
247.561728	8000.453722	10.361856	-0.051166	4.818965
247.599055	8000.491908	10.366861	-0.051173	4.818976
247.210062	8000.319397	10.371866	-0.051101	4.818926
247.095474	8000.325288	10.376871	-0.051079	4.818929
247.079621	8000.303093	10.381875	-0.051077	4.818922
247.635372	8000.450476	10.386880	-0.051180	4.818964
247.440105	8000.520297	10.391885	-0.051144	4.818985
247.470500	8000.316411	10.396890	-0.051149	4.818925
247.524528	8000.426040	10.401895	-0.051160	4.818957
247.473011	8000.428536	10.406899	-0.051150	4.818958
247.579461	8000.448738	10.411904	-0.051170	4.818964
247.345924	8000.367229	10.416909	-0.051127	4.818940
247.294774	8000.219931	10.421914	-0.051117	4.818896
247.523898	8000.445951	10.426919	-0.051160	4.818963
247.384273	8000.352008	10.431923	-0.051134	4.818935
247.418612	8000.203693	10.436928	-0.051140	4.818891
247.307228	8000.319616	10.441933	-0.051119	4.818926
247.289409	8000.073224	10.446938	-0.051116	4.818853
247.007308	8000.012058	10.451943	-0.051064	4.818836
247.219822	8000.342617	10.456947	-0.051103	4.818933
247.517575	8000.264666	10.461952	-0.051159	4.818909
247.502845	8000.453042	10.466957	-0.051156	4.818965
247.758998	8000.336855	10.471962	-0.051204	4.818930
247.876477	8000.514331	10.476967	-0.051226	4.818982
247.203985	8000.081596	10.481971	-0.051100	4.818856
247.773097	8000.378944	10.486976	-0.051207	4.818942
247.647951	8000.429746	10.491981	-0.051183	4.818958
247.845358	8000.465762	10.496986	-0.051220	4.818968
248.022060	8000.519325	10.501991	-0.051253	4.818983
247.785533	8000.438824	10.506995	-0.051209	4.818960
247.753987	8000.199586	10.512000	-0.051203	4.818889
247.849897	8000.521352	10.517005	-0.051221	4.818984
247.827738	8000.444603	10.522010	-0.051217	4.818961
247.869250	8000.529983	10.527015	-0.051225	4.818987
248.080582	8000.449894	10.532019	-0.051264	4.818962
247.690442	8000.477450	10.537024	-0.051192	4.818972
247.745602	8000.503290	10.542029	-0.051202	4.818979
247.893606	8000.238032	10.547034	-0.051230	4.818900
247.582600	8000.208972	10.552039	-0.051172	4.818892
247.309457	8000.283050	10.557043	-0.051121	4.818915
247.646993	8000.470631	10.562048	-0.051184	4.818970
247.552184	8000.424393	10.567053	-0.051166	4.818956
247.711002	8000.452588	10.572058	-0.051196	4.818964
247.813575	8000.525120	10.577063	-0.051215	4.818985
247.725212	8000.508295	10.582067	-0.051199	4.818981
246.883786	7999.875454	10.587072	-0.051042	4.818795
247.055073	7999.986556	10.592077	-0.051074	4.818828
247.329374	8000.134574	10.597082	-0.051125	4.818871
247.596260	8000.334880	10.602087	-0.051175	4.818930
247.346494	8000.429156	10.607091	-0.051128	4.818959
247.383360	7999.985467	10.612096	-0.051135	4.818826
247.538833	8000.378162	10.617101	-0.051164	4.818943
247.245483	8000.177528	10.622106	-0.051109	4.818884
247.142802	8000.262135	10.627111	-0.051090	4.818910
247.257458	8000.273011	10.632115	-0.051112	4.818912
247.259489	8000.186094	10.637120	-0.051112	4.818886
247.332720	8000.288632	10.642125	-0.051126	4.818917
247.535621	8000.424232	10.647130	-0.051164	4.818956
247.484070	8000.219313	10.652135	-0.051154	4.818896
247.502645	8000.420680	10.657139	-0.051158	4.818955
247.869051	8000.256648	10.662144	-0.051226	4.818905
247.905675	8000.391200	10.667149	-0.051233	4.818945
247.357427	8000.254392	10.672154	-0.051131	4.818906
247.656780	8000.407970	10.677159	-0.051187	4.818951
247.768969	8000.405198	10.682163	-0.051208	4.818950
247.686861	8000.450258	10.687168	-0.051192	4.818964
247.882627	8000.513490	10.692173	-0.051229	4.818982
247.891361	8000.525126	10.697178	-0.051231	4.818985
247.848134	8000.329737	10.702183	-0.051223	4.818927
247.599418	8000.355934	10.707187	-0.051176	4.818936
247.626002	8000.185522	10.712192	-0.051181	4.818885
247.656365	8000.229905	10.717197	-0.051187	4.818898
247.622099	8000.311185	10.722202	-0.051181	4.818922
247.433768	8000.233389	10.727207	-0.051146	4.818900
247.717097	8000.414002	10.732211	-0.051198	4.818953
247.703785	8000.436883	10.737216	-0.051196	4.818960
247.417342	8000.366229	10.742221	-0.051143	4.818940
247.385798	8000.208703	10.747226	-0.051137	4.818893
247.610758	8000.404292	10.752231	-0.051179	4.818950
247.662787	8000.501327	10.757235	-0.051189	4.818979
247.759527	8000.443887	10.762240	-0.051207	4.818961
247.522096	8000.449275	10.767245	-0.051162	4.818964
247.760979	8000.356963	10.772250	-0.051207	4.818935
247.470321	8000.375299	10.777255	-0.051153	4.818942
247.313110	8000.320942	10.782259	-0.051124	4.818926
247.214291	8000.207612	10.787264	-0.051105	4.818893
247.424680	8000.269978	10.792269	-0.051144	4.818911
247.192843	8000.151829	10.797274	-0.051101	4.818876
247.498846	8000.209114	10.802279	-0.051158	4.818892
247.560826	8000.202566	10.807283	-0.051170	4.818890
247.738509	8000.207952	10.812288	-0.051203	4.818891
247.908643	8000.266668	10.817293	-0.051235	4.818908
247.527960	8000.279678	10.822298	-0.051164	4.818913
247.574918	8000.021531	10.827303	-0.051173	4.818836
247.606239	8000.218866	10.832307	-0.051179	4.818895
247.856889	8000.125656	10.837312	-0.051225	4.818866
247.620153	8000.321707	10.842317	-0.051181	4.818925
247.555139	8000.295749	10.847322	-0.051169	4.818918
247.639879	8000.320915	10.852327	-0.051185	4.818925
247.487686	8000.262431	10.857331	-0.051157	4.818908
247.595364	8000.029143	10.862336	-0.051177	4.818838
247.362419	8000.107917	10.867341	-0.051133	4.818863
247.881085	8000.034846	10.872346	-0.051230	4.818839
247.745431	8000.243695	10.877351	-0.051205	4.818902
247.814734	8000.442560	10.882355	-0.051218	4.818961
247.626090	7999.870321	10.887360	-0.051183	4.818791
247.787806	8000.425465	10.892365	-0.051213	4.818956
247.781630	8000.385583	10.897370	-0.051212	4.818944
247.796347	8000.386819	10.902375	-0.051215	4.818944
247.941952	8000.380279	10.907379	-0.051242	4.818942
247.827356	8000.388264	10.912384	-0.051221	4.818945
248.019409	8000.434688	10.917389	-0.051256	4.818958
248.080694	8000.446987	10.922394	-0.051268	4.818961
247.961886	8000.371114	10.927399	-0.051246	4.818939
247.804057	8000.253895	10.932403	-0.051216	4.818905
248.195801	8000.335311	10.937408	-0.051289	4.818927
248.007053	8000.241795	10.942413	-0.051254	4.818900
247.883698	8000.267479	10.947418	-0.051231	4.818908
247.864053	8000.378275	10.952423	-0.051228	4.818941
248.153248	8000.522302	10.957427	-0.051282	4.818983
247.737553	8000.164033	10.962432	-0.051204	4.818878
248.035074	8000.444343	10.967437	-0.051260	4.818960
247.735180	8000.010020	10.972442	-0.051204	4.818832
247.699009	7999.977094	10.977447	-0.051197	4.818822
247.430832	8000.256551	10.982451	-0.051147	4.818907
247.507056	7999.952683	10.987456	-0.051161	4.818816
247.780451	8000.262014	10.992461	-0.051212	4.818907
247.743671	8000.200795	10.997466	-0.051206	4.818889
247.779109	8000.277716	11.002471	-0.051212	4.818912
247.695909	8000.140489	11.007475	-0.051197	4.818871
248.137359	8000.137678	11.012480	-0.051279	4.818869
247.663252	8000.293025	11.017485	-0.051191	4.818917
247.761733	8000.097331	11.022490	-0.051209	4.818858
247.922080	8000.347625	11.027495	-0.051239	4.818932
248.046357	8000.498999	11.032499	-0.051262	4.818977
248.128638	8000.470708	11.037504	-0.051278	4.818968
247.909296	8000.233289	11.042509	-0.051237	4.818898
247.907349	8000.302407	11.047514	-0.051237	4.818919
248.199733	8000.291432	11.052519	-0.051291	4.818914
248.078368	8000.466943	11.057523	-0.051269	4.818967
247.779512	8000.035774	11.062528	-0.051213	4.818840
248.280880	8000.421316	11.067533	-0.051306	4.818953
247.885485	8000.273862	11.072538	-0.051233	4.818910
248.099742	8000.173907	11.077543	-0.051273	4.818880
247.674069	8000.061693	11.082547	-0.051193	4.818848
248.157638	8000.083506	11.087552	-0.051283	4.818852
247.801404	8000.087397	11.092557	-0.051217	4.818855
248.245446	8000.324510	11.097562	-0.051300	4.818924
248.041328	8000.026528	11.102567	-0.051262	4.818836
247.671658	8000.036537	11.107571	-0.051193	4.818840
247.806223	7999.726073	11.112576	-0.051218	4.818747
247.720477	7999.815082	11.117581	-0.051202	4.818774
247.674684	7999.941258	11.122586	-0.051194	4.818812
247.837103	7999.928643	11.127591	-0.051224	4.818807
247.999728	8000.216676	11.132595	-0.051254	4.818893
247.724525	7999.913612	11.137600	-0.051203	4.818803
248.135245	8000.412190	11.142605	-0.051280	4.818950
248.256565	8000.248208	11.147610	-0.051302	4.818901
248.060127	8000.218497	11.152615	-0.051266	4.818893
247.992103	8000.438677	11.157619	-0.051253	4.818959
247.698088	7999.844157	11.162624	-0.051198	4.818783
247.861554	8000.333328	11.167629	-0.051229	4.818928
247.880514	8000.267574	11.172634	-0.051233	4.818908
247.991218	8000.060510	11.177639	-0.051253	4.818846
247.589113	8000.175911	11.182643	-0.051178	4.818882
248.189897	8000.121684	11.187648	-0.051290	4.818864
248.091984	8000.004175	11.192653	-0.051272	4.818829
247.825205	8000.056334	11.197658	-0.051222	4.818846
248.244065	8000.152756	11.202663	-0.051301	4.818873
248.332678	8000.216730	11.207667	-0.051317	4.818891
248.247030	7999.910815	11.212672	-0.051301	4.818801
247.891697	7999.963954	11.217677	-0.051235	4.818818
247.374735	7999.855832	11.222682	-0.051139	4.818787
247.424332	7999.861697	11.227687	-0.051148	4.818789
247.464283	7999.891534	11.232691	-0.051155	4.818798
247.411319	7999.753645	11.237696	-0.051146	4.818757
246.891720	7999.867567	11.242701	-0.051049	4.818793
247.580454	7999.947478	11.247706	-0.051177	4.818814
247.983489	8000.171498	11.252711	-0.051252	4.818879
247.760998	8000.160315	11.257715	-0.051211	4.818877
247.901268	8000.023811	11.262720	-0.051237	4.818836
247.940714	7999.965649	11.267725	-0.051245	4.818818
248.529980	8000.335538	11.272730	-0.051355	4.818926
248.633728	8000.297043	11.277735	-0.051374	4.818914
248.518430	8000.213880	11.282739	-0.051352	4.818890
248.498529	8000.210490	11.287744	-0.051349	4.818889
248.098786	8000.130026	11.292749	-0.051274	4.818866
248.372945	8000.041302	11.297754	-0.051325	4.818839
248.618834	7999.990981	11.302759	-0.051371	4.818823
248.413307	8000.349801	11.307763	-0.051333	4.818931
248.664575	8000.109938	11.312768	-0.051380	4.818858
248.143112	8000.120125	11.317773	-0.051283	4.818863
248.409267	8000.192623	11.322778	-0.051332	4.818884
248.716870	8000.421736	11.327783	-0.051390	4.818951
248.599572	8000.535493	11.332787	-0.051368	4.818985
248.381487	8000.343132	11.337792	-0.051327	4.818929
248.607619	8000.540839	11.342797	-0.051370	4.818987
248.622720	8000.424750	11.347802	-0.051373	4.818952
248.567043	8000.343387	11.352807	-0.051362	4.818928
248.471437	8000.457417	11.357811	-0.051344	4.818963
248.440018	8000.159513	11.362816	-0.051338	4.818874
248.382746	8000.219553	11.367821	-0.051328	4.818892
248.195859	8000.043304	11.372826	-0.051293	4.818840
248.716063	8000.324331	11.377831	-0.051390	4.818922
248.510733	8000.447452	11.382835	-0.051352	4.818960
248.649642	8000.430352	11.387840	-0.051378	4.818954
248.484781	8000.316184	11.392845	-0.051347	4.818920
248.537487	8000.212095	11.397850	-0.051357	4.818889
248.534690	7999.903033	11.402855	-0.051356	4.818797
248.511876	8000.447482	11.407859	-0.051352	4.818960
248.457065	7999.983769	11.412864	-0.051342	4.818822
248.371880	7999.867468	11.417869	-0.051326	4.818787
248.371048	8000.082208	11.422874	-0.051326	4.818851
248.566758	7999.982018	11.427879	-0.051363	4.818821
248.299641	8000.011127	11.432883	-0.051313	4.818830
248.501695	8000.186525	11.437888	-0.051351	4.818882
248.259220	8000.188708	11.442893	-0.051306	4.818883
248.329799	7999.963329	11.447898	-0.051319	4.818816
248.396651	8000.061598	11.452903	-0.051331	4.818845
248.316274	8000.233434	11.457907	-0.051316	4.818896
248.162231	8000.052362	11.462912	-0.051288	4.818843
248.112739	8000.105166	11.467917	-0.051278	4.818859
247.939827	7999.985664	11.472922	-0.051246	4.818824
248.011042	7999.915332	11.477927	-0.051259	4.818803
248.262383	8000.268386	11.482931	-0.051307	4.818907
248.494123	8000.046087	11.487936	-0.051350	4.818840
248.367631	8000.167059	11.492941	-0.051326	4.818876
248.317661	8000.288996	11.497946	-0.051317	4.818913
248.482196	8000.233459	11.502951	-0.051348	4.818896
248.210903	8000.280323	11.507955	-0.051297	4.818911
248.652534	8000.405322	11.512960	-0.051380	4.818946
248.643127	8000.450252	11.517965	-0.051378	4.818960
248.523965	8000.348183	11.522970	-0.051356	4.818930
248.475632	8000.376909	11.527975	-0.051347	4.818939
248.392474	8000.302532	11.532979	-0.051331	4.818917
248.443055	8000.034997	11.537984	-0.051340	4.818837
248.620264	8000.168180	11.542989	-0.051374	4.818876
248.662174	8000.281850	11.547994	-0.051382	4.818910
248.445702	7999.935522	11.552999	-0.051341	4.818807
248.139391	8000.339162	11.558003	-0.051284	4.818929
248.610123	7999.994169	11.563008	-0.051372	4.818824
248.240897	7999.982184	11.568013	-0.051303	4.818822
248.653806	8000.222048	11.573018	-0.051380	4.818892
248.748550	8000.345813	11.578023	-0.051398	4.818928
248.815789	8000.408472	11.583027	-0.051411	4.818947
248.514228	8000.046400	11.588032	-0.051354	4.818840
248.564336	8000.340354	11.593037	-0.051364	4.818927
248.513625	8000.307242	11.598042	-0.051354	4.818918
248.455112	8000.085471	11.603047	-0.051343	4.818852
248.050932	8000.224939	11.608051	-0.051268	4.818895
248.363982	8000.177560	11.613056	-0.051327	4.818880
247.898338	7999.935994	11.618061	-0.051240	4.818809
247.692632	7999.874743	11.623066	-0.051201	4.818792
247.944988	7999.832882	11.628071	-0.051248	4.818778
247.787115	7999.840323	11.633075	-0.051219	4.818781
247.489320	7999.809338	11.638080	-0.051164	4.818773
247.671157	7999.877626	11.643085	-0.051198	4.818793
247.972974	7999.851055	11.648090	-0.051254	4.818784
248.030272	7999.782643	11.653095	-0.051264	4.818763
247.678836	7999.800216	11.658099	-0.051199	4.818770
248.179664	7999.906046	11.663104	-0.051292	4.818799
248.219872	7999.877225	11.668109	-0.051300	4.818791
248.030618	7999.823513	11.673114	-0.051265	4.818775
248.374882	7999.997557	11.678119	-0.051329	4.818826
248.164303	8000.250508	11.683123	-0.051290	4.818902
248.022398	7999.834941	11.688128	-0.051263	4.818779
247.698156	7999.860189	11.693133	-0.051203	4.818787
248.059679	8000.020831	11.698138	-0.051271	4.818834
248.697978	8000.183923	11.703143	-0.051390	4.818880
248.075317	8000.110076	11.708147	-0.051274	4.818861
248.231907	7999.966444	11.713152	-0.051303	4.818817
248.390996	8000.157013	11.718157	-0.051332	4.818873
248.427807	8000.148052	11.723162	-0.051339	4.818871
248.022658	7999.987909	11.728167	-0.051264	4.818824
247.436978	7999.789881	11.733171	-0.051155	4.818768
247.836020	7999.800149	11.738176	-0.051229	4.818769
247.966891	7999.856273	11.743181	-0.051254	4.818785
248.077435	7999.971851	11.748186	-0.051274	4.818819
248.298316	7999.820650	11.753191	-0.051315	4.818773
248.069085	7999.975941	11.758195	-0.051273	4.818821
248.170347	8000.033789	11.763200	-0.051292	4.818837
248.148784	7999.816679	11.768205	-0.051288	4.818773
248.072381	7999.990658	11.773210	-0.051274	4.818825
247.955890	7999.761878	11.778215	-0.051252	4.818757
248.307259	8000.173804	11.783219	-0.051317	4.818879
248.694305	8000.018412	11.788224	-0.051389	4.818831
248.327239	8000.070354	11.793229	-0.051321	4.818848
248.332016	8000.119652	11.798234	-0.051322	4.818862
248.468280	7999.907673	11.803239	-0.051347	4.818799
248.661501	8000.368947	11.808243	-0.051384	4.818935
248.785373	7999.999672	11.813248	-0.051407	4.818825
248.504523	8000.060034	11.818253	-0.051354	4.818844
248.459836	8000.266891	11.823258	-0.051346	4.818906
248.604825	8000.122064	11.828263	-0.051373	4.818862
248.621744	8000.340175	11.833267	-0.051377	4.818927
248.709888	8000.036447	11.838272	-0.051393	4.818836
248.635123	8000.041793	11.843277	-0.051379	4.818838
248.604466	8000.184925	11.848282	-0.051373	4.818881
248.846306	7999.898852	11.853287	-0.051418	4.818795
248.512160	8000.156530	11.858291	-0.051356	4.818873
248.505435	7999.929129	11.863296	-0.051355	4.818805
248.847058	8000.385991	11.868301	-0.051419	4.818940
248.605827	8000.047727	11.873306	-0.051374	4.818840
248.199450	8000.193453	11.878311	-0.051298	4.818885
248.156564	8000.005403	11.883315	-0.051290	4.818829
248.268423	8000.037195	11.888320	-0.051311	4.818838
248.413451	8000.120737	11.893325	-0.051338	4.818862
248.428826	8000.113601	11.898330	-0.051341	4.818860
248.663693	7999.813823	11.903335	-0.051385	4.818770
248.574023	8000.035823	11.908339	-0.051368	4.818837
248.612070	7999.980786	11.913344	-0.051375	4.818820
248.290140	7999.839501	11.918349	-0.051315	4.818779
247.830989	7999.965706	11.923354	-0.051230	4.818818
248.043370	7999.788210	11.928359	-0.051269	4.818765
247.792044	7999.893989	11.933363	-0.051223	4.818797
248.234107	7999.783288	11.938368	-0.051305	4.818763
248.455484	8000.074157	11.943373	-0.051346	4.818848
248.087928	7999.959532	11.948378	-0.051278	4.818816
248.258099	7999.865307	11.953383	-0.051310	4.818787
248.209953	7999.840610	11.958387	-0.051301	4.818780
248.706993	8000.100387	11.963392	-0.051393	4.818855
248.598050	8000.020449	11.968397	-0.051373	4.818832
248.572541	8000.144790	11.973402	-0.051369	4.818869
248.905855	8000.071478	11.978407	-0.051431	4.818846
248.801979	8000.295399	11.983411	-0.051411	4.818913
248.879945	8000.122488	11.988416	-0.051426	4.818861
248.987366	8000.172035	11.993421	-0.051446	4.818876
248.405167	8000.229642	11.998426	-0.051338	4.818895
249.163182	8000.268542	12.003431	-0.051479	4.818904
248.722018	8000.345736	12.008435	-0.051397	4.818928
248.917352	8000.075834	12.013440	-0.051433	4.818847
248.430217	8000.113690	12.018445	-0.051342	4.818860
248.220702	7999.913064	12.023450	-0.051303	4.818801
248.253376	7999.828628	12.028455	-0.051309	4.818776
248.201201	8000.191473	12.033459	-0.051300	4.818884
248.517325	7999.999569	12.038464	-0.051359	4.818826
248.923673	8000.182784	12.043469	-0.051435	4.818879
248.238947	7999.809603	12.048474	-0.051307	4.818770
248.399396	8000.030565	12.053479	-0.051337	4.818836
248.394516	8000.114311	12.058483	-0.051336	4.818861
248.649395	8000.339615	12.063488	-0.051384	4.818927
248.619866	7999.988310	12.068493	-0.051378	4.818822
248.782863	8000.297307	12.073498	-0.051409	4.818914
248.623239	7999.906649	12.078503	-0.051379	4.818798
249.111865	8000.407272	12.083507	-0.051470	4.818945
248.986081	8000.176266	12.088512	-0.051447	4.818877
249.039726	8000.155994	12.093517	-0.051457	4.818871
248.823889	8000.152226	12.098522	-0.051416	4.818870
248.741477	7999.924916	12.103527	-0.051401	4.818803
248.664365	8000.024512	12.108531	-0.051387	4.818833
248.452854	7999.914997	12.113536	-0.051347	4.818801
248.575515	8000.123963	12.118541	-0.051370	4.818863
248.958706	8000.388601	12.123546	-0.051442	4.818940
248.997729	8000.309479	12.128551	-0.051449	4.818916
248.801184	8000.355191	12.133555	-0.051413	4.818931
248.662043	8000.018215	12.138560	-0.051387	4.818831
248.898336	8000.381565	12.143565	-0.051431	4.818938
248.980447	8000.536601	12.148570	-0.051446	4.818984
249.182574	8000.324399	12.153575	-0.051484	4.818920
249.210347	8000.510177	12.158579	-0.051489	4.818975
249.100966	8000.218616	12.163584	-0.051469	4.818889
248.779948	8000.168475	12.168589	-0.051409	4.818875
248.937330	8000.269984	12.173594	-0.051438	4.818905
248.986003	8000.075752	12.178599	-0.051447	4.818847
248.716080	8000.068159	12.183603	-0.051397	4.818846
248.551499	7999.896383	12.188608	-0.051366	4.818795
248.957075	8000.015684	12.193613	-0.051442	4.818829
248.710550	8000.171808	12.198618	-0.051396	4.818876
248.764526	7999.974502	12.203623	-0.051406	4.818817
248.574735	8000.051726	12.208627	-0.051371	4.818841
248.840393	8000.183931	12.213632	-0.051421	4.818880
248.809202	8000.142685	12.218637	-0.051415	4.818867
248.875808	8000.289141	12.223642	-0.051427	4.818911
248.708342	7999.871148	12.228647	-0.051396	4.818787
248.796946	8000.236821	12.233651	-0.051413	4.818896
248.848619	7999.919015	12.238656	-0.051422	4.818801
248.831386	7999.999463	12.243661	-0.051419	4.818825
248.871308	8000.306908	12.248666	-0.051427	4.818916
249.191641	8000.057439	12.253671	-0.051486	4.818841
249.040703	8000.224198	12.258675	-0.051458	4.818891
249.157083	8000.259192	12.263680	-0.051480	4.818901
249.059566	8000.080924	12.268685	-0.051462	4.818848
248.929583	8000.263660	12.273690	-0.051438	4.818903
248.995244	8000.081166	12.278695	-0.051450	4.818848
248.853006	8000.382125	12.283699	-0.051424	4.818939
248.542638	8000.111080	12.288704	-0.051366	4.818859
248.612535	8000.080538	12.293709	-0.051379	4.818850
248.946159	8000.255504	12.298714	-0.051441	4.818901
248.986147	8000.334580	12.303719	-0.051449	4.818924
248.831765	8000.287589	12.308723	-0.051420	4.818911
249.070449	8000.439362	12.313728	-0.051464	4.818955
249.052582	8000.206575	12.318733	-0.051461	4.818886
248.650140	8000.261212	12.323738	-0.051386	4.818903
248.896897	8000.015006	12.328743	-0.051432	4.818829
248.984581	8000.434100	12.333747	-0.051449	4.818954
248.730308	8000.259090	12.338752	-0.051401	4.818902
248.891509	8000.220271	12.343757	-0.051431	4.818890
249.020904	8000.398949	12.348762	-0.051456	4.818943
249.128086	8000.194978	12.353767	-0.051475	4.818882
248.756230	8000.350568	12.358771	-0.051406	4.818930
248.935202	8000.069984	12.363776	-0.051439	4.818845
248.859546	7999.970561	12.368781	-0.051425	4.818816
248.682059	8000.132793	12.373786	-0.051392	4.818865
248.918890	8000.387204	12.378791	-0.051437	4.818940
248.450800	8000.215782	12.383795	-0.051350	4.818891
248.358526	7999.931781	12.388800	-0.051332	4.818806
248.487348	8000.004642	12.393805	-0.051356	4.818827
248.438906	7999.982036	12.398810	-0.051347	4.818821
248.672090	8000.163065	12.403815	-0.051391	4.818874
248.477648	8000.042241	12.408819	-0.051355	4.818839
248.701084	8000.179150	12.413824	-0.051396	4.818879
248.757245	8000.180909	12.418829	-0.051407	4.818879
248.743975	8000.319025	12.423834	-0.051405	4.818920
248.774571	8000.221989	12.428839	-0.051410	4.818891
248.821841	8000.331537	12.433843	-0.051419	4.818924
248.687906	8000.153857	12.438848	-0.051394	4.818871
249.068291	8000.374462	12.443853	-0.051465	4.818935
248.935175	8000.292121	12.448858	-0.051440	4.818911
248.681336	8000.008172	12.453863	-0.051393	4.818828
248.718733	8000.333394	12.458867	-0.051400	4.818925
248.766423	8000.098294	12.463872	-0.051409	4.818854
249.099056	8000.286868	12.468877	-0.051471	4.818909
248.932102	8000.269050	12.473882	-0.051440	4.818905
248.915290	8000.333791	12.478887	-0.051437	4.818924
248.993337	8000.280305	12.483891	-0.051451	4.818908
249.081587	8000.208091	12.488896	-0.051468	4.818886
248.902400	7999.987938	12.493901	-0.051434	4.818821
248.840664	8000.163154	12.498906	-0.051423	4.818873
248.989598	8000.088563	12.503911	-0.051451	4.818851
249.145305	8000.406901	12.508915	-0.051480	4.818945
248.878634	7999.979270	12.513920	-0.051430	4.818818
248.615401	8000.215845	12.518925	-0.051381	4.818890
248.865303	8000.246238	12.523930	-0.051428	4.818898
248.833254	8000.083463	12.528935	-0.051422	4.818850
249.049239	8000.178377	12.533939	-0.051462	4.818877
248.939034	8000.182228	12.538944	-0.051442	4.818879
248.474063	7999.980471	12.543949	-0.051355	4.818820
248.861648	7999.835561	12.548954	-0.051427	4.818776
248.319745	7999.862254	12.553959	-0.051326	4.818786
248.418852	7999.981879	12.558963	-0.051345	4.818821
248.834484	8000.049977	12.563968	-0.051422	4.818840
248.743025	8000.169297	12.568973	-0.051406	4.818876
248.584011	7999.926355	12.573978	-0.051376	4.818804
248.878953	8000.052642	12.578983	-0.051431	4.818840
248.305425	7999.863139	12.583987	-0.051324	4.818786
248.384573	7999.981464	12.588992	-0.051339	4.818821
249.039125	8000.014864	12.593997	-0.051461	4.818828
248.915607	8000.274155	12.599002	-0.051438	4.818906
248.656522	7999.909479	12.604007	-0.051390	4.818798
248.517417	8000.116191	12.609011	-0.051364	4.818861
248.944999	8000.288153	12.614016	-0.051444	4.818910
248.641739	8000.037103	12.619021	-0.051387	4.818837
248.612271	8000.326911	12.624026	-0.051382	4.818923
248.987406	8000.341077	12.629031	-0.051452	4.818926
248.792889	8000.226534	12.634035	-0.051415	4.818892
249.015630	8000.382295	12.639040	-0.051457	4.818938
249.043944	8000.293611	12.644045	-0.051462	4.818911
248.895414	8000.423735	12.649050	-0.051435	4.818951
249.060419	8000.360870	12.654055	-0.051466	4.818931
249.073433	8000.295039	12.659059	-0.051468	4.818912
249.205309	8000.266327	12.664064	-0.051493	4.818903
249.155748	7999.987048	12.669069	-0.051483	4.818820
249.048232	8000.442441	12.674074	-0.051463	4.818956
249.206035	8000.356438	12.679079	-0.051493	4.818930
248.835851	8000.131777	12.684083	-0.051424	4.818864
248.812497	8000.194339	12.689088	-0.051420	4.818883
249.123646	8000.091416	12.694093	-0.051477	4.818851
249.144049	8000.212148	12.699098	-0.051481	4.818887
249.168334	7999.837426	12.704103	-0.051486	4.818775
248.829912	8000.373708	12.709107	-0.051423	4.818936
249.321328	8000.241632	12.714112	-0.051515	4.818895
248.999687	8000.115008	12.719117	-0.051455	4.818858
248.780128	8000.074529	12.724122	-0.051414	4.818847
249.083772	8000.012366	12.729127	-0.051470	4.818827
249.162893	8000.468019	12.734131	-0.051485	4.818963
248.685079	8000.133050	12.739136	-0.051396	4.818865
248.724190	7999.886322	12.744141	-0.051403	4.818791
249.058214	8000.321091	12.749146	-0.051466	4.818920
248.944466	8000.236899	12.754151	-0.051445	4.818895
248.819814	8000.296089	12.759155	-0.051422	4.818913
249.122651	8000.397340	12.764160	-0.051478	4.818942
249.355516	8000.407616	12.769165	-0.051522	4.818944
249.139451	8000.192231	12.774170	-0.051481	4.818881
249.058970	8000.183885	12.779175	-0.051466	4.818879
249.021162	8000.079701	12.784179	-0.051459	4.818848
248.607401	7999.910018	12.789184	-0.051382	4.818799
248.922781	7999.930759	12.794189	-0.051441	4.818804
249.114516	8000.292499	12.799194	-0.051477	4.818911
249.180091	8000.119431	12.804199	-0.051489	4.818859
248.844802	8000.306910	12.809203	-0.051427	4.818916
248.876415	8000.241314	12.814208	-0.051433	4.818896
249.286863	8000.300972	12.819213	-0.051509	4.818913
248.664374	8000.177886	12.824218	-0.051393	4.818878
248.871462	8000.052698	12.829223	-0.051432	4.818840
248.917119	8000.009279	12.834227	-0.051440	4.818827
248.799027	7999.953319	12.839232	-0.051418	4.818811
248.721828	7999.875877	12.844237	-0.051404	4.818788
248.729088	8000.218525	12.849242	-0.051405	4.818890
248.874701	7999.910285	12.854247	-0.051432	4.818798
248.757971	8000.453554	12.859251	-0.051411	4.818960
248.875585	8000.337712	12.864256	-0.051433	4.818925
249.127020	8000.282223	12.869261	-0.051480	4.818908
248.806718	8000.199615	12.874266	-0.051420	4.818884
248.485105	7999.945194	12.879271	-0.051360	4.818810
248.817868	8000.021675	12.884275	-0.051422	4.818831
248.737097	7999.819529	12.889280	-0.051407	4.818771
248.296192	7999.755312	12.894285	-0.051325	4.818754
248.422242	8000.051264	12.899290	-0.051349	4.818842
248.363219	7999.803302	12.904295	-0.051338	4.818768
248.540454	7999.943815	12.909299	-0.051371	4.818809
248.762055	8000.163458	12.914304	-0.051412	4.818874
249.157695	8000.082552	12.919309	-0.051486	4.818848
248.935334	8000.213839	12.924314	-0.051445	4.818888
248.939156	8000.161512	12.929319	-0.051445	4.818872
248.660991	8000.285809	12.934323	-0.051394	4.818911
248.685281	8000.186599	12.939328	-0.051398	4.818881
249.001887	8000.343544	12.944333	-0.051457	4.818926
248.502062	8000.144486	12.949338	-0.051364	4.818869
248.318062	7999.884471	12.954343	-0.051330	4.818792
248.245246	7999.864700	12.959347	-0.051316	4.818787
248.314542	7999.848816	12.964352	-0.051329	4.818782
248.793963	7999.910383	12.969357	-0.051418	4.818798
248.100060	7999.779076	12.974362	-0.051289	4.818762
248.443184	7999.777119	12.979367	-0.051353	4.818760
248.415611	7999.922382	12.984371	-0.051348	4.818803
248.518071	7999.839874	12.989376	-0.051367	4.818778
248.336488	7999.772640	12.994381	-0.051333	4.818759
249.002878	8000.188547	12.999386	-0.051458	4.818880
248.989100	7999.768303	13.004391	-0.051455	4.818755
248.434241	8000.015864	13.009395	-0.051352	4.818831
248.460161	7999.780496	13.014400	-0.051357	4.818761
248.758381	7999.748642	13.019405	-0.051412	4.818750
248.889302	8000.015327	13.024410	-0.051437	4.818829
248.475554	7999.819458	13.029415	-0.051360	4.818772
248.494974	7999.854275	13.034419	-0.051363	4.818783
248.840199	8000.127854	13.039424	-0.051428	4.818863
248.964412	8000.005811	13.044429	-0.051451	4.818826
248.874577	8000.379713	13.049434	-0.051434	4.818938
248.964985	7999.915734	13.054439	-0.051451	4.818799
248.891154	8000.103367	13.059443	-0.051437	4.818855
248.112118	7999.871465	13.064448	-0.051292	4.818789
248.474799	7999.850899	13.069453	-0.051360	4.818782
248.589860	7999.820926	13.074458	-0.051381	4.818772
248.689741	7999.779239	13.079463	-0.051400	4.818759
249.012189	8000.048341	13.084467	-0.051460	4.818838
248.713131	7999.989050	13.089472	-0.051404	4.818822
248.800033	7999.995387	13.094477	-0.051421	4.818823
248.470221	7999.852954	13.099482	-0.051359	4.818782
248.878939	7999.905251	13.104487	-0.051435	4.818796
248.804329	8000.121158	13.109491	-0.051422	4.818861
248.824576	8000.001994	13.114496	-0.051425	4.818825
248.910179	7999.960127	13.119501	-0.051441	4.818812
249.275015	8000.237103	13.124506	-0.051510	4.818894
249.154089	7999.950639	13.129511	-0.051487	4.818809
249.175946	8000.314428	13.134515	-0.051491	4.818917
249.025587	8000.151205	13.139520	-0.051463	4.818869
248.962684	8000.076036	13.144525	-0.051451	4.818847
249.113506	8000.180605	13.149530	-0.051480	4.818877
249.420305	8000.265145	13.154535	-0.051537	4.818901
249.271470	8000.265364	13.159539	-0.051509	4.818902
249.308037	8000.184117	13.164544	-0.051516	4.818878
249.513157	7999.857768	13.169549	-0.051554	4.818780
249.462917	8000.386168	13.174554	-0.051545	4.818937
249.439727	8000.132361	13.179559	-0.051541	4.818862
249.279187	8000.055959	13.184563	-0.051511	4.818840
249.429881	8000.287286	13.189568	-0.051539	4.818908
249.201687	7999.988990	13.194573	-0.051496	4.818820
248.884626	8000.050991	13.199578	-0.051437	4.818840
249.167933	7999.983333	13.204583	-0.051490	4.818818
249.156788	7999.903580	13.209587	-0.051488	4.818795
249.208099	8000.063461	13.214592	-0.051498	4.818842
249.018867	7999.846326	13.219597	-0.051462	4.818778
249.087663	8000.122707	13.224602	-0.051476	4.818860
249.358158	8000.010889	13.229607	-0.051526	4.818826
248.856163	7999.922850	13.234611	-0.051432	4.818802
248.997562	7999.875401	13.239616	-0.051459	4.818787
248.888234	7999.950497	13.244621	-0.051438	4.818810
248.907821	8000.027219	13.249626	-0.051442	4.818832
249.142341	7999.939042	13.254631	-0.051486	4.818805
248.958985	7999.936732	13.259635	-0.051452	4.818805
249.094877	7999.958353	13.264640	-0.051477	4.818811
249.238164	7999.992638	13.269645	-0.051504	4.818821
248.904475	7999.895199	13.274650	-0.051442	4.818793
248.662479	7999.857581	13.279655	-0.051397	4.818783
248.914689	7999.819910	13.284659	-0.051444	4.818771
249.038362	8000.001653	13.289664	-0.051467	4.818824
248.754672	7999.855610	13.294669	-0.051414	4.818782
248.446333	7999.745924	13.299674	-0.051357	4.818750
249.090737	7999.818999	13.304679	-0.051477	4.818770
248.921199	8000.082945	13.309683	-0.051445	4.818849
249.114917	8000.125200	13.314688	-0.051481	4.818861
249.235500	8000.119392	13.319693	-0.051504	4.818859
249.271229	8000.105179	13.324698	-0.051511	4.818854
249.391663	8000.202032	13.329703	-0.051533	4.818883
248.960516	7999.745094	13.334707	-0.051453	4.818748
248.951426	7999.879069	13.339712	-0.051451	4.818788
248.952018	7999.821464	13.344717	-0.051451	4.818771
249.223020	8000.103538	13.349722	-0.051502	4.818854
249.464921	7999.979837	13.354727	-0.051547	4.818816
249.440675	7999.773162	13.359731	-0.051542	4.818755
248.873468	7999.836199	13.364736	-0.051437	4.818776
249.325140	7999.847136	13.369741	-0.051521	4.818777
249.227940	7999.922385	13.374746	-0.051503	4.818800
249.299603	7999.829011	13.379751	-0.051516	4.818772
249.053302	7999.868858	13.384755	-0.051470	4.818785
248.974157	7999.950620	13.389760	-0.051456	4.818809
249.301865	7999.734768	13.394765	-0.051517	4.818744
249.237353	8000.171842	13.399770	-0.051505	4.818874
248.668975	7999.835740	13.404775	-0.051399	4.818776
248.647122	7999.843848	13.409779	-0.051395	4.818779
248.631195	7999.835269	13.414784	-0.051392	4.818776
248.872658	7999.761846	13.419789	-0.051437	4.818753
248.574758	7999.880656	13.424794	-0.051382	4.818790
248.265091	7999.835901	13.429799	-0.051324	4.818778
248.431207	7999.814952	13.434803	-0.051355	4.818771
248.581383	7999.827323	13.439808	-0.051383	4.818774
249.171152	7999.903902	13.444813	-0.051493	4.818795
248.808595	7999.985233	13.449818	-0.051425	4.818820
248.845953	7999.767815	13.454823	-0.051432	4.818755
249.069104	7999.843961	13.459827	-0.051474	4.818777
249.200424	7999.944091	13.464832	-0.051499	4.818807
248.870131	7999.781747	13.469837	-0.051437	4.818759
248.963497	7999.954727	13.474842	-0.051454	4.818811
249.415322	8000.116519	13.479847	-0.051539	4.818857
249.185540	8000.054958	13.484851	-0.051496	4.818840
249.066266	8000.157166	13.489856	-0.051474	4.818871
249.089901	7999.900812	13.494861	-0.051478	4.818794
249.237548	7999.924677	13.499866	-0.051506	4.818801
249.499939	7999.904943	13.504871	-0.051555	4.818794
249.252646	7999.831640	13.509875	-0.051509	4.818773
249.332994	7999.988744	13.514880	-0.051524	4.818819
249.275632	8000.044592	13.519885	-0.051513	4.818836
249.318714	8000.160373	13.524890	-0.051521	4.818871
249.331290	7999.949971	13.529895	-0.051523	4.818808
248.572768	7999.852413	13.534899	-0.051382	4.818782
248.793371	7999.878244	13.539904	-0.051423	4.818788
249.147969	7999.869100	13.544909	-0.051489	4.818784
248.821587	7999.757089	13.549914	-0.051429	4.818752
249.110484	7999.971295	13.554919	-0.051483	4.818815
248.833273	7999.949993	13.559923	-0.051431	4.818810
248.630792	7999.768311	13.564928	-0.051393	4.818756
248.618327	7999.863484	13.569933	-0.051391	4.818785
249.049496	7999.916064	13.574938	-0.051471	4.818799
249.134600	7999.904570	13.579943	-0.051487	4.818795
248.778232	7999.871794	13.584947	-0.051421	4.818787
249.030651	8000.126397	13.589952	-0.051468	4.818861
249.237318	8000.016917	13.594957	-0.051507	4.818828
248.751029	7999.865175	13.599962	-0.051416	4.818785
249.078795	7999.767698	13.604967	-0.051477	4.818754
249.033301	7999.831029	13.609971	-0.051469	4.818773
248.793272	7999.920190	13.614976	-0.051424	4.818801
248.900215	7999.829356	13.619981	-0.051444	4.818773
248.750446	8000.021269	13.624986	-0.051416	4.818831
249.121712	7999.995576	13.629991	-0.051485	4.818822
249.096664	7999.816129	13.634995	-0.051481	4.818769
249.427802	8000.184866	13.640000	-0.051543	4.818877
249.004847	7999.932304	13.645005	-0.051464	4.818804
249.033640	7999.984001	13.650010	-0.051469	4.818819
249.173120	8000.155471	13.655015	-0.051495	4.818870
248.894597	7999.992729	13.660019	-0.051443	4.818822
249.054004	8000.039788	13.665024	-0.051473	4.818836
249.270497	8000.116901	13.670029	-0.051513	4.818858
248.906182	7999.749851	13.675034	-0.051445	4.818750
249.077293	8000.023330	13.680039	-0.051478	4.818831
249.129138	7999.903516	13.685043	-0.051487	4.818795
249.066487	8000.205478	13.690048	-0.051476	4.818885
249.201985	7999.912822	13.695053	-0.051501	4.818797
249.054539	8000.032483	13.700058	-0.051473	4.818833
248.980615	7999.752902	13.705063	-0.051460	4.818750
249.120259	7999.817519	13.710067	-0.051486	4.818769
248.740963	7999.756172	13.715072	-0.051415	4.818752
248.596878	7999.926156	13.720077	-0.051388	4.818803
248.675334	7999.748018	13.725082	-0.051403	4.818750
249.006940	7999.810865	13.730087	-0.051465	4.818768
249.001227	7999.863173	13.735091	-0.051464	4.818783
249.382474	8000.039787	13.740096	-0.051535	4.818834
249.238958	7999.859892	13.745101	-0.051508	4.818781
249.012648	7999.831900	13.750106	-0.051466	4.818774
249.157367	7999.838965	13.755111	-0.051493	4.818775
248.975625	7999.847152	13.760115	-0.051459	4.818778
249.668972	8000.256079	13.765120	-0.051589	4.818898
249.842298	8000.270842	13.770125	-0.051621	4.818901
249.821879	8000.445538	13.775130	-0.051617	4.818954
249.546836	8000.126740	13.780135	-0.051566	4.818860
249.924063	8000.291788	13.785139	-0.051636	4.818907
249.776326	8000.486876	13.790144	-0.051609	4.818966
249.841926	8000.336851	13.795149	-0.051621	4.818921
249.965341	8000.465174	13.800154	-0.051644	4.818959
249.702039	8000.362328	13.805159	-0.051595	4.818929
249.615245	8000.256475	13.810163	-0.051579	4.818898
249.630841	8000.448387	13.815168	-0.051582	4.818955
249.393431	7999.909026	13.820173	-0.051538	4.818795
249.490287	8000.162718	13.825178	-0.051556	4.818871
249.666584	8000.114662	13.830183	-0.051589	4.818856
249.799083	8000.050339	13.835187	-0.051613	4.818836
249.694814	8000.281593	13.840192	-0.051594	4.818905
249.843282	8000.422803	13.845197	-0.051622	4.818947
250.060882	8000.542888	13.850202	-0.051663	4.818982
250.108664	8000.446066	13.855207	-0.051671	4.818953
250.136958	8000.550141	13.860211	-0.051677	4.818984
249.844807	8000.471024	13.865216	-0.051622	4.818961
249.876491	8000.138288	13.870221	-0.051628	4.818862
249.774424	8000.376904	13.875226	-0.051609	4.818933
249.854015	8000.413531	13.880231	-0.051624	4.818944
250.092484	8000.439593	13.885235	-0.051669	4.818951
249.933053	8000.540250	13.890240	-0.051639	4.818981
250.281193	8000.549890	13.895245	-0.051704	4.818983
249.850445	8000.435498	13.900250	-0.051624	4.818950
249.892268	8000.476886	13.905255	-0.051632	4.818963
250.008872	8000.148364	13.910259	-0.051653	4.818864
249.965407	8000.066105	13.915264	-0.051645	4.818840
249.832801	8000.107386	13.920269	-0.051620	4.818853
249.394972	8000.182527	13.925274	-0.051539	4.818877
249.730489	8000.100863	13.930279	-0.051601	4.818851
249.988393	8000.337737	13.935283	-0.051650	4.818921
249.900283	8000.338723	13.940288	-0.051633	4.818921
249.910433	8000.177523	13.945293	-0.051635	4.818873
249.886540	8000.446460	13.950298	-0.051631	4.818954
249.760263	8000.169347	13.955303	-0.051607	4.818871
249.637287	8000.371032	13.960307	-0.051585	4.818932
249.792802	8000.414904	13.965312	-0.051614	4.818945
249.941775	8000.299456	13.970317	-0.051641	4.818910
249.950617	8000.407475	13.975322	-0.051643	4.818942
249.775486	8000.240791	13.980327	-0.051610	4.818893
249.672868	8000.165119	13.985331	-0.051591	4.818871
249.634647	8000.358446	13.990336	-0.051584	4.818928
249.669715	8000.301273	13.995341	-0.051591	4.818911
249.603055	8000.393672	14.000346	-0.051579	4.818939
249.446038	7999.864755	14.005351	-0.051549	4.818782
249.460528	8000.043029	14.010355	-0.051552	4.818835
249.647538	8000.063201	14.015360	-0.051587	4.818840
249.787767	7999.983262	14.020365	-0.051613	4.818816
249.602368	8000.093017	14.025370	-0.051578	4.818849
249.636704	8000.260021	14.030375	-0.051585	4.818899
249.732612	7999.931243	14.035379	-0.051603	4.818801
249.614745	7999.878428	14.040384	-0.051581	4.818785
249.628921	8000.109078	14.045389	-0.051584	4.818854
249.654892	7999.911415	14.050394	-0.051588	4.818795
249.856008	8000.347661	14.055399	-0.051626	4.818924
249.942322	8000.454564	14.060403	-0.051642	4.818956
249.942868	8000.484955	14.065408	-0.051642	4.818965
249.967982	8000.128039	14.070413	-0.051647	4.818858
249.573924	8000.414301	14.075418	-0.051574	4.818945
249.733605	8000.203656	14.080423	-0.051603	4.818882
249.813292	8000.167999	14.085427	-0.051618	4.818871
249.880873	8000.350092	14.090432	-0.051631	4.818925
249.920700	8000.370502	14.095437	-0.051638	4.818931
250.069441	8000.523242	14.100442	-0.051666	4.818976
250.300160	8000.450730	14.105447	-0.051709	4.818953
250.138337	8000.441356	14.110451	-0.051679	4.818951
250.054922	8000.530401	14.115456	-0.051664	4.818978
250.085646	8000.322315	14.120461	-0.051669	4.818916
249.866421	8000.403358	14.125466	-0.051629	4.818941
249.712845	8000.320756	14.130471	-0.051600	4.818917
249.977628	8000.366007	14.135475	-0.051649	4.818929
249.650978	8000.008845	14.140480	-0.051588	4.818824
249.944639	8000.014649	14.145485	-0.051643	4.818825
250.105748	8000.466111	14.150490	-0.051673	4.818959
250.054543	8000.267467	14.155495	-0.051664	4.818900
249.993601	8000.350510	14.160499	-0.051653	4.818925
249.957314	8000.537578	14.165504	-0.051646	4.818980
250.247494	8000.273056	14.170509	-0.051700	4.818901
250.129181	8000.370041	14.175514	-0.051678	4.818930
249.950210	8000.043026	14.180519	-0.051645	4.818833
249.960479	8000.274678	14.185523	-0.051647	4.818902
250.069986	8000.551589	14.190528	-0.051667	4.818984
250.101345	8000.386463	14.195533	-0.051673	4.818935
250.044854	8000.530324	14.200538	-0.051663	4.818978
250.075352	8000.259379	14.205543	-0.051668	4.818897
249.984889	8000.438430	14.210547	-0.051651	4.818951
249.897197	8000.529516	14.215552	-0.051635	4.818978
249.866111	8000.181318	14.220557	-0.051629	4.818875
249.893362	8000.448806	14.225562	-0.051635	4.818954
249.960830	8000.363757	14.230567	-0.051647	4.818929
250.013857	8000.347668	14.235571	-0.051657	4.818924
250.006632	8000.390532	14.240576	-0.051656	4.818936
250.151413	8000.536936	14.245581	-0.051683	4.818979
249.902442	8000.441603	14.250586	-0.051636	4.818952
249.837777	8000.285742	14.255591	-0.051624	4.818906
250.189549	8000.163426	14.260595	-0.051690	4.818868
249.943679	8000.364609	14.265600	-0.051644	4.818929
250.101183	8000.483935	14.270605	-0.051674	4.818964
250.120076	8000.422367	14.275610	-0.051677	4.818945
250.126085	8000.336541	14.280615	-0.051678	4.818920
249.734861	8000.112654	14.285619	-0.051605	4.818855
249.695559	8000.405490	14.290624	-0.051598	4.818942
249.719021	8000.183697	14.295629	-0.051603	4.818876
249.646402	8000.257163	14.300634	-0.051589	4.818898
249.917995	8000.228119	14.305639	-0.051640	4.818888
250.093457	8000.433575	14.310643	-0.051673	4.818949
249.977002	8000.441536	14.315648	-0.051651	4.818952
250.052445	8000.458206	14.320653	-0.051665	4.818956
250.158531	8000.365263	14.325658	-0.051685	4.818928
250.012677	8000.396948	14.330663	-0.051658	4.818938
249.734788	8000.262490	14.335667	-0.051606	4.818899
249.742400	8000.340112	14.340672	-0.051607	4.818922
249.950546	8000.301887	14.345677	-0.051646	4.818910
249.849361	8000.363469	14.350682	-0.051627	4.818929
250.069498	8000.537015	14.355687	-0.051669	4.818980
250.141939	8000.438408	14.360691	-0.051682	4.818950
250.077188	8000.531880	14.365696	-0.051670	4.818978
250.148858	8000.541169	14.370701	-0.051684	4.818981
250.123113	8000.448656	14.375706	-0.051679	4.818953
250.144447	8000.355690	14.380711	-0.051683	4.818925
250.131044	8000.157525	14.385715	-0.051680	4.818866
250.062361	8000.416469	14.390720	-0.051667	4.818944
250.061378	8000.150366	14.395725	-0.051667	4.818865
249.777742	8000.250500	14.400730	-0.051614	4.818896
250.083961	8000.171609	14.405735	-0.051671	4.818871
250.148312	8000.348423	14.410739	-0.051684	4.818923
249.867650	8000.317644	14.415744	-0.051631	4.818915
249.939478	7999.570576	14.420749	-0.051644	4.818692

250.135856	7996.322777	14.425754	-0.051679	4.817724
250.049363	7990.764339	14.430759	-0.051659	4.816067
249.866280	7984.066919	14.435763	-0.051621	4.814070
249.961581	7976.838006	14.440768	-0.051634	4.811913
250.054450	7969.188810	14.445773	-0.051646	4.809629
249.888571	7961.408515	14.450778	-0.051610	4.807306
249.769859	7953.490532	14.455783	-0.051583	4.804940
249.903295	7945.590837	14.460787	-0.051603	4.802578
249.975137	7937.541946	14.465792	-0.051611	4.800170
249.988431	7929.611166	14.470797	-0.051608	4.797797
250.021442	7921.608424	14.475802	-0.051609	4.795401
249.813695	7913.619645	14.480807	-0.051565	4.793008
249.787763	7905.660776	14.485811	-0.051555	4.790623
249.380466	7897.618747	14.490816	-0.051474	4.788213
249.745846	7889.543883	14.495821	-0.051537	4.785789
249.610229	7881.560638	14.500826	-0.051507	4.783394
249.596374	7873.609640	14.505831	-0.051499	4.781006
249.865157	7865.558278	14.510835	-0.051544	4.778586
249.637188	7857.606018	14.515840	-0.051496	4.776196
249.824606	7849.552600	14.520845	-0.051526	4.773774
249.726310	7841.595084	14.525850	-0.051503	4.771379
249.734522	7833.522265	14.530855	-0.051499	4.768949
249.665773	7825.595914	14.535859	-0.051481	4.766561
249.469195	7817.529598	14.540864	-0.051439	4.764131
249.423866	7809.648808	14.545869	-0.051426	4.761755
249.206180	7801.543014	14.550874	-0.051380	4.759310
249.217889	7793.615918	14.555879	-0.051377	4.756917
249.606628	7785.536449	14.560883	-0.051444	4.754476
249.396567	7777.572353	14.565888	-0.051400	4.752071
249.403228	7769.515817	14.570893	-0.051396	4.749635
248.989124	7761.577150	14.575898	-0.051314	4.747235
249.334497	7753.484754	14.580903	-0.051373	4.744785
249.021258	7745.628233	14.585907	-0.051309	4.742407
248.779656	7737.588700	14.590912	-0.051259	4.739973
249.046247	7729.587383	14.595917	-0.051304	4.737547
249.095032	7721.523941	14.600922	-0.051307	4.735102
249.077536	7713.505429	14.605927	-0.051299	4.732669
249.053726	7705.539348	14.610931	-0.051289	4.730251
248.860913	7697.542546	14.615936	-0.051248	4.727823
248.988320	7689.546436	14.620941	-0.051267	4.725393
248.997641	7681.515830	14.625946	-0.051264	4.722952
248.802082	7673.577689	14.630951	-0.051222	4.720537
248.678372	7665.613248	14.635955	-0.051194	4.718114
248.686692	7657.554096	14.640960	-0.051190	4.715660
248.067552	7649.685062	14.645965	-0.051070	4.713263
248.748996	7641.511038	14.650970	-0.051191	4.710771
248.551691	7633.525082	14.655975	-0.051149	4.708336
248.673037	7625.546523	14.660979	-0.051167	4.705901
248.554952	7617.494567	14.665984	-0.051140	4.703444
248.666451	7609.560009	14.670989	-0.051155	4.701020
248.767849	7601.472191	14.675994	-0.051169	4.698548
249.056212	7593.522845	14.680999	-0.051218	4.696117
248.924954	7585.529491	14.686003	-0.051188	4.693672
248.767119	7577.539277	14.691008	-0.051153	4.691227
248.816258	7569.539488	14.696013	-0.051157	4.688777
248.837740	7561.522420	14.701018	-0.051156	4.686321
248.951375	7553.463907	14.706023	-0.051172	4.683850
249.107628	7545.639662	14.711027	-0.051196	4.681450
248.817998	7537.519711	14.716032	-0.051137	4.678959
248.875008	7529.554069	14.721037	-0.051142	4.676513
248.996325	7521.516446	14.726042	-0.051160	4.674044
248.819904	7513.529490	14.731047	-0.051122	4.671589
248.734875	7505.509316	14.736051	-0.051101	4.669122
248.581836	7497.481217	14.741056	-0.051067	4.666652
248.575762	7489.440241	14.746061	-0.051061	4.664177
248.632401	7481.528187	14.751066	-0.051066	4.661740
248.407718	7473.497743	14.756071	-0.051019	4.659265
248.606697	7465.591987	14.761075	-0.051051	4.656827
248.592737	7457.468844	14.766080	-0.051043	4.654321
248.541739	7449.493700	14.771085	-0.051029	4.651860
248.558941	7441.441896	14.776090	-0.051027	4.649373
248.520822	7433.462136	14.781095	-0.051014	4.646907
248.361787	7425.455494	14.786099	-0.050980	4.644432
248.299050	7417.525697	14.791104	-0.050963	4.641979
248.632277	7409.453238	14.796109	-0.051020	4.639481
248.382755	7401.528205	14.801114	-0.050968	4.637026
248.257891	7393.436968	14.806119	-0.050940	4.634519
248.388917	7385.514715	14.811123	-0.050959	4.632064
248.611700	7377.402179	14.816128	-0.050995	4.629548
248.447440	7369.511233	14.821133	-0.050959	4.627099
248.014518	7361.477525	14.826138	-0.050874	4.624604
248.077160	7353.497068	14.831143	-0.050880	4.622125
248.157916	7345.468604	14.836147	-0.050890	4.619629
247.997412	7337.425204	14.841152	-0.050855	4.617128
248.051064	7329.393488	14.846157	-0.050860	4.614628
248.099502	7321.444325	14.851162	-0.050864	4.612154
247.860115	7313.393356	14.856167	-0.050814	4.609645
247.848213	7305.468092	14.861171	-0.050806	4.607175
247.963442	7297.403411	14.866176	-0.050823	4.604661
248.069975	7289.458175	14.871181	-0.050837	4.602182
247.651176	7281.453702	14.876186	-0.050754	4.599682
247.650223	7273.416709	14.881191	-0.050749	4.597172
247.958187	7265.458423	14.886195	-0.050801	4.594685
247.788444	7257.420048	14.891200	-0.050764	4.592171
248.172685	7249.383082	14.896205	-0.050831	4.589657
248.159225	7241.416468	14.901210	-0.050823	4.587164
247.924404	7233.370806	14.906215	-0.050774	4.584643
248.013517	7225.432265	14.911219	-0.050786	4.582156
248.002512	7217.363262	14.916224	-0.050778	4.579626
247.995390	7209.412121	14.921229	-0.050772	4.577131
247.738635	7201.360604	14.926234	-0.050719	4.574603
247.867308	7193.369623	14.931239	-0.050738	4.572094
247.778697	7185.384526	14.936243	-0.050716	4.569584
247.595774	7177.421421	14.941248	-0.050677	4.567080
247.251229	7169.407419	14.946253	-0.050607	4.564558
247.444501	7161.440471	14.951258	-0.050638	4.562051
247.548371	7153.342767	14.956263	-0.050652	4.559501
247.704107	7145.411581	14.961267	-0.050676	4.557002
247.620888	7137.338174	14.966272	-0.050656	4.554456
247.585607	7129.408419	14.971277	-0.050644	4.551955
247.273452	7121.339088	14.976282	-0.050580	4.549407
246.970428	7113.415651	14.981287	-0.050519	4.546904
247.334189	7105.369199	14.986291	-0.050581	4.544362
247.195719	7097.370242	14.991296	-0.050551	4.541832
246.922872	7089.410612	14.996301	-0.050495	4.539314
246.884938	7081.407901	15.001306	-0.050482	4.536780
247.135469	7073.309293	15.006311	-0.050524	4.534216
247.431677	7065.356552	15.011315	-0.050574	4.531697
247.005878	7057.278645	15.016320	-0.050489	4.529135
247.020910	7049.345536	15.021325	-0.050487	4.526618
247.092883	7041.304143	15.026330	-0.050495	4.524066
246.953302	7033.353078	15.031335	-0.050464	4.521540
247.080788	7025.326982	15.036339	-0.050483	4.518990
246.652958	7017.417581	15.041344	-0.050398	4.516474
246.684999	7009.332918	15.046349	-0.050399	4.513902
246.835996	7001.363263	15.051354	-0.050422	4.511365
246.848914	6993.300683	15.056359	-0.050419	4.508798
246.840177	6985.309557	15.061363	-0.050412	4.506251
246.837216	6977.270032	15.066368	-0.050406	4.503687
246.824263	6969.360437	15.071373	-0.050399	4.501164
246.751146	6961.320139	15.076378	-0.050380	4.498597
246.562039	6953.289848	15.081383	-0.050339	4.496031
246.666728	6945.279968	15.086387	-0.050354	4.493472
246.965027	6937.238899	15.091392	-0.050404	4.490902
246.916951	6929.259600	15.096397	-0.050390	4.488349
246.918054	6921.271532	15.101402	-0.050385	4.485792
246.577320	6913.283928	15.106407	-0.050316	4.483232
246.602026	6905.281357	15.111411	-0.050316	4.480667
246.674816	6897.275878	15.116416	-0.050324	4.478100
246.682292	6889.285626	15.121421	-0.050320	4.475536
246.581536	6881.297632	15.126426	-0.050297	4.472971
246.562760	6873.247972	15.131431	-0.050288	4.470385
246.778452	6865.275249	15.136435	-0.050323	4.467823
246.678832	6857.202095	15.141440	-0.050299	4.465227
246.735340	6849.260306	15.146445	-0.050304	4.462671
246.679382	6841.272439	15.151450	-0.050289	4.460099
246.521187	6833.257868	15.156455	-0.050254	4.457516
246.393284	6825.286262	15.161459	-0.050225	4.454946
246.027463	6817.280543	15.166464	-0.050152	4.452362
246.127761	6809.222761	15.171469	-0.050165	4.449762
246.107624	6801.262481	15.176474	-0.050157	4.447191
245.896845	6793.189236	15.181479	-0.050112	4.444581
246.063470	6785.275716	15.186483	-0.050138	4.442024
245.861964	6777.225319	15.191488	-0.050095	4.439419
246.111176	6769.279039	15.196493	-0.050137	4.436848
246.390388	6761.197016	15.201498	-0.050183	4.434232
246.046389	6753.236534	15.206503	-0.050114	4.431650
245.931849	6745.204574	15.211507	-0.050088	4.429045
245.882717	6737.242598	15.216512	-0.050073	4.426462
246.339287	6729.169416	15.221517	-0.050153	4.423844
246.308250	6721.217387	15.226522	-0.050142	4.421261
246.243444	6713.160214	15.231527	-0.050125	4.418642
246.277661	6705.284512	15.236531	-0.050126	4.416081
245.962428	6697.196486	15.241536	-0.050062	4.413447
245.815348	6689.247292	15.246541	-0.050030	4.410858
246.019100	6681.183020	15.251546	-0.050063	4.408232
246.133491	6673.185541	15.256551	-0.050079	4.405626
246.197039	6665.223420	15.261555	-0.050085	4.403029
246.159394	6657.235472	15.266560	-0.050073	4.400422
246.149445	6649.224009	15.271565	-0.050066	4.397806
245.825787	6641.304868	15.276570	-0.050001	4.395216
245.638930	6633.313273	15.281575	-0.049961	4.392602
245.878459	6625.333941	15.286579	-0.050000	4.389993
245.985023	6617.260011	15.291584	-0.050015	4.387351
245.685018	6609.237571	15.296589	-0.049954	4.384721
245.728898	6601.348009	15.301594	-0.049957	4.382136
245.579287	6593.291157	15.306599	-0.049924	4.379493
245.760099	6585.313903	15.311603	-0.049952	4.376877
245.705353	6577.286598	15.316608	-0.049937	4.374241
246.045163	6569.286839	15.321613	-0.049995	4.371615
246.073970	6561.250232	15.326618	-0.049995	4.368974
245.857121	6553.301787	15.331623	-0.049950	4.366358
245.941468	6545.303039	15.336627	-0.049960	4.363726
245.872258	6537.343861	15.341632	-0.049942	4.361104
245.854998	6529.340006	15.346637	-0.049934	4.358467
245.773327	6521.370900	15.351642	-0.049913	4.355839
245.550586	6513.302087	15.356647	-0.049867	4.353175
245.572178	6505.276053	15.361651	-0.049866	4.350526
245.401969	6497.235835	15.366656	-0.049829	4.347869
245.578317	6489.276362	15.371661	-0.049856	4.345239
245.188566	6481.348505	15.376666	-0.049779	4.342614
245.290854	6473.283492	15.381671	-0.049793	4.339946
245.307957	6465.319749	15.386675	-0.049791	4.337309
245.191039	6457.301047	15.391680	-0.049764	4.334652
244.883949	6449.326881	15.396685	-0.049701	4.332005
244.867362	6441.258234	15.401690	-0.049693	4.329329
244.918625	6433.280317	15.406695	-0.049697	4.326681
244.848072	6425.248357	15.411699	-0.049679	4.324012
244.747998	6417.342351	15.416704	-0.049655	4.321384
245.006239	6409.278961	15.421709	-0.049698	4.318705
245.253802	6401.264840	15.426714	-0.049739	4.316040
244.967197	6393.268657	15.431719	-0.049681	4.313375
245.323358	6385.230570	15.436723	-0.049742	4.310700
245.271297	6377.244718	15.441728	-0.049727	4.308038
245.311576	6369.179022	15.446733	-0.049729	4.305347
245.487404	6361.218485	15.451738	-0.049757	4.302692
245.268224	6353.247382	15.456743	-0.049711	4.300027
245.337544	6345.290220	15.461747	-0.049719	4.297369
245.033284	6337.240943	15.466752	-0.049657	4.294674
245.190191	6329.274506	15.471757	-0.049681	4.292010
245.144717	6321.203040	15.476762	-0.049667	4.289307
245.265687	6313.189753	15.481767	-0.049684	4.286623
245.210996	6305.251592	15.486771	-0.049669	4.283961
245.178247	6297.272180	15.491776	-0.049658	4.281284
245.049504	6289.248473	15.496781	-0.049629	4.278590
244.663253	6281.346050	15.501786	-0.049552	4.275931
244.535989	6273.236866	15.506791	-0.049523	4.273205
244.657890	6265.294503	15.511795	-0.049540	4.270535
244.294866	6257.223000	15.516800	-0.049468	4.267815
244.508556	6249.193409	15.521805	-0.049502	4.265113
244.938583	6241.204036	15.526810	-0.049577	4.262425
244.799673	6233.188533	15.531815	-0.049546	4.259721
244.489771	6225.291598	15.536819	-0.049483	4.257054
244.819080	6217.148206	15.541824	-0.049539	4.254308
244.656037	6209.216301	15.546829	-0.049504	4.251627
244.624100	6201.199556	15.551834	-0.049493	4.248917
244.981595	6193.176767	15.556839	-0.049554	4.246207
245.053109	6185.206634	15.561843	-0.049562	4.243510
244.955780	6177.227506	15.566848	-0.049539	4.240807
244.926544	6169.224650	15.571853	-0.049528	4.238094
244.868283	6161.236145	15.576858	-0.049512	4.235385
244.481450	6153.253194	15.581863	-0.049435	4.232672
244.511555	6145.219804	15.586867	-0.049435	4.229944
244.478814	6137.163316	15.591872	-0.049424	4.227207
244.707111	6129.159548	15.596877	-0.049462	4.224488
244.605615	6121.270749	15.601882	-0.049438	4.221803
244.559430	6113.140405	15.606887	-0.049424	4.219035
244.918496	6105.222771	15.611891	-0.049485	4.216342
244.843322	6097.193626	15.616896	-0.049466	4.213604
244.736654	6089.195502	15.621901	-0.049441	4.210875
244.686226	6081.207114	15.626906	-0.049427	4.208148
244.776298	6073.181693	15.631911	-0.049438	4.205408
244.698352	6065.248491	15.636915	-0.049419	4.202696
244.579469	6057.222379	15.641920	-0.049391	4.199950
244.864303	6049.233223	15.646925	-0.049439	4.197219
244.791162	6041.199617	15.651930	-0.049420	4.194467
244.285011	6033.242014	15.656935	-0.049321	4.191735
244.404440	6025.174989	15.661939	-0.049338	4.188970
244.304259	6017.194688	15.666944	-0.049314	4.186231
243.982419	6009.205716	15.671949	-0.049249	4.183484
244.336892	6001.170720	15.676954	-0.049310	4.180728
243.888648	5993.240524	15.681959	-0.049221	4.177996
243.829971	5985.243576	15.686963	-0.049205	4.175245
243.449780	5977.249097	15.691968	-0.049129	4.172488
243.662436	5969.193128	15.696973	-0.049164	4.169716
243.632121	5961.229217	15.701978	-0.049153	4.166970
243.561295	5953.148108	15.706983	-0.049134	4.164182
243.680462	5945.267950	15.711987	-0.049152	4.161464
243.489967	5937.222809	15.716992	-0.049111	4.158682
243.417763	5929.280747	15.721997	-0.049092	4.155937
243.464799	5921.245627	15.727002	-0.049096	4.153158
243.182294	5913.260812	15.732007	-0.049038	4.150391
243.612994	5905.213757	15.737011	-0.049113	4.147610
243.558314	5897.175179	15.742016	-0.049098	4.144824
243.583173	5889.255980	15.747021	-0.049097	4.142078
243.753544	5881.200599	15.752026	-0.049124	4.139285
243.406666	5873.261448	15.757031	-0.049054	4.136524
243.562458	5865.224608	15.762035	-0.049078	4.133733
243.305946	5857.275722	15.767040	-0.049025	4.130966
243.424183	5849.212565	15.772045	-0.049042	4.128162
243.534364	5841.227771	15.777050	-0.049057	4.125383
243.356507	5833.254401	15.782055	-0.049019	4.122603
243.419984	5825.275054	15.787059	-0.049026	4.119822
243.237588	5817.251017	15.792064	-0.048986	4.117020
242.815469	5809.252036	15.797069	-0.048903	4.114221
243.273762	5801.263172	15.802074	-0.048983	4.111437
243.437739	5793.178156	15.807079	-0.049008	4.108613
243.575887	5785.196935	15.812083	-0.049029	4.105823
243.411310	5777.209472	15.817088	-0.048993	4.103024
243.355428	5769.237296	15.822093	-0.048977	4.100230
243.426910	5761.253722	15.827098	-0.048985	4.097433
243.369608	5753.200879	15.832103	-0.048970	4.094607
243.115582	5745.260556	15.837107	-0.048917	4.091816
242.968574	5737.193322	15.842112	-0.048885	4.088980
243.127209	5729.242233	15.847117	-0.048909	4.086187
243.238893	5721.224877	15.852122	-0.048925	4.083369
243.187604	5713.243025	15.857127	-0.048910	4.080558
243.305531	5705.253243	15.862131	-0.048927	4.077746
242.812578	5697.274879	15.867136	-0.048830	4.074926
242.619145	5689.268057	15.872141	-0.048789	4.072099
242.482370	5681.256465	15.877146	-0.048758	4.069269
242.669295	5673.216942	15.882151	-0.048787	4.066432
242.777466	5665.207602	15.887155	-0.048802	4.063602
242.741952	5657.232188	15.892160	-0.048791	4.060780
242.594891	5649.239940	15.897165	-0.048758	4.057949
242.611854	5641.271604	15.902170	-0.048756	4.055127
242.702937	5633.249159	15.907175	-0.048768	4.052285
242.482349	5625.276192	15.912179	-0.048722	4.049453
242.486673	5617.266249	15.917184	-0.048717	4.046610
242.698006	5609.213926	15.922189	-0.048751	4.043753
242.606376	5601.305636	15.927194	-0.048729	4.040940
242.436738	5593.252039	15.932199	-0.048692	4.038073
242.307985	5585.298809	15.937203	-0.048663	4.035239
242.573597	5577.210441	15.942208	-0.048708	4.032362
242.451848	5569.209534	15.947213	-0.048680	4.029508
242.268551	5561.278447	15.952218	-0.048641	4.026676
242.106969	5553.243608	15.957223	-0.048605	4.023805
242.234100	5545.281454	15.962227	-0.048624	4.020963
241.900970	5537.299347	15.967232	-0.048557	4.018104
242.001646	5529.275578	15.972237	-0.048570	4.015235
242.106617	5521.259920	15.977242	-0.048585	4.012367
241.874427	5513.233746	15.982247	-0.048536	4.009488
242.391540	5505.250813	15.987251	-0.048627	4.006634
242.085696	5497.242320	15.992256	-0.048565	4.003756
241.839152	5489.372473	15.997261	-0.048514	4.000926
241.953096	5481.300666	16.002266	-0.048530	3.998028
241.707913	5473.273784	16.007271	-0.048479	3.995138
241.975469	5465.288575	16.012275	-0.048524	3.992269
242.221567	5457.221642	16.017280	-0.048565	3.989369
241.984195	5449.276008	16.022285	-0.048515	3.986501
241.823706	5441.302983	16.027290	-0.048480	3.983624
242.180201	5433.259203	16.032295	-0.048541	3.980727
242.024856	5425.306174	16.037299	-0.048507	3.977853
241.966333	5417.310099	16.042304	-0.048491	3.974962
241.981057	5409.307577	16.047309	-0.048489	3.972068
242.419230	5401.243916	16.052314	-0.048565	3.969158
242.079509	5393.295871	16.057319	-0.048497	3.966273
241.896970	5385.335470	16.062323	-0.048458	3.963385
242.087335	5377.278548	16.067328	-0.048488	3.960466
241.965458	5369.321658	16.072333	-0.048460	3.957576
241.744979	5361.355067	16.077338	-0.048414	3.954678
241.578255	5353.299789	16.082343	-0.048378	3.951746
242.025266	5345.278105	16.087347	-0.048456	3.948837
242.009192	5337.280125	16.092352	-0.048447	3.945925
241.847232	5329.270800	16.097357	-0.048412	3.943004
241.954785	5321.310782	16.102362	-0.048427	3.940104
241.551939	5313.329416	16.107367	-0.048347	3.937184
241.709690	5305.301615	16.112371	-0.048371	3.934256
241.441616	5297.325247	16.117376	-0.048316	3.931336
241.698537	5289.324577	16.122381	-0.048359	3.928416
241.763861	5281.304114	16.127386	-0.048366	3.925482
241.322918	5273.383942	16.132391	-0.048278	3.922573
241.884060	5265.321695	16.137395	-0.048378	3.919629
241.432366	5257.381782	16.142400	-0.048288	3.916708
241.513307	5249.345310	16.147405	-0.048298	3.913760
241.505957	5241.362123	16.152410	-0.048292	3.910828
240.935901	5233.391708	16.157415	-0.048181	3.907886
241.539000	5225.295765	16.162419	-0.048288	3.904920
241.466564	5217.345226	16.167424	-0.048269	3.901992
241.612891	5209.325162	16.172429	-0.048291	3.899040
241.505290	5201.369110	16.177434	-0.048266	3.896104
241.349319	5193.377798	16.182439	-0.048232	3.893152
241.156097	5185.392996	16.187443	-0.048191	3.890200
241.556885	5177.351739	16.192448	-0.048260	3.887236
241.550990	5169.304556	16.197453	-0.048254	3.884260
241.942472	5161.377045	16.202458	-0.048321	3.881334
241.703602	5153.380408	16.207463	-0.048272	3.878367
241.612473	5145.426288	16.212467	-0.048250	3.875417
241.504462	5137.310129	16.217472	-0.048224	3.872404
241.433383	5129.278943	16.222477	-0.048206	3.869421
241.339603	5121.348518	16.227482	-0.048183	3.866473
241.565707	5113.305176	16.232487	-0.048220	3.863487
241.660979	5105.350951	16.237491	-0.048233	3.860529
241.181482	5097.390622	16.242496	-0.048138	3.857554
241.385260	5089.348609	16.247501	-0.048171	3.854562
241.808635	5081.358606	16.252506	-0.048245	3.851591
241.476791	5073.338243	16.257511	-0.048178	3.848590
241.713713	5065.340392	16.262515	-0.048217	3.845607
241.267456	5057.463771	16.267520	-0.048129	3.842653
241.381196	5049.412875	16.272525	-0.048145	3.839643
241.416113	5041.427070	16.277530	-0.048146	3.836654
240.993552	5033.427053	16.282535	-0.048062	3.833647
241.164216	5025.429941	16.287539	-0.048089	3.830652
241.273009	5017.385323	16.292544	-0.048104	3.827635
240.908146	5009.420149	16.297549	-0.048031	3.824635
240.791740	5001.464774	16.302554	-0.048004	3.821642
241.049667	4993.386184	16.307559	-0.048047	3.818609
241.046976	4985.411677	16.312563	-0.048041	3.815606
241.051151	4977.376780	16.317568	-0.048037	3.812579
241.193425	4969.384582	16.322573	-0.048058	3.809568
241.065658	4961.426657	16.327578	-0.048029	3.806562
240.687444	4953.428399	16.332583	-0.047953	3.803532
240.897606	4945.493945	16.337587	-0.047987	3.800538
240.792614	4937.495925	16.342592	-0.047963	3.797510
240.856026	4929.452743	16.347597	-0.047969	3.794466
240.867280	4921.468636	16.352602	-0.047966	3.791442
240.691238	4913.440794	16.357607	-0.047928	3.788393
240.846813	4905.428470	16.362611	-0.047952	3.785356
240.631586	4897.517959	16.367616	-0.047907	3.782347
240.709332	4889.473999	16.372621	-0.047916	3.779291
240.813913	4881.487333	16.377626	-0.047930	3.776255
240.723966	4873.434876	16.382631	-0.047908	3.773187
240.726172	4865.460997	16.387635	-0.047904	3.770149
240.873081	4857.477017	16.392640	-0.047926	3.767107
240.562683	4849.459808	16.397645	-0.047863	3.764040
240.363845	4841.590042	16.402650	-0.047821	3.761029
240.499995	4833.498714	16.407655	-0.047841	3.757939
240.658645	4825.528369	16.412659	-0.047865	3.754894
240.464288	4817.561057	16.417664	-0.047824	3.751838
240.458094	4809.494536	16.422669	-0.047818	3.748747
240.651928	4801.516932	16.427674	-0.047849	3.745692
240.434758	4793.510647	16.432679	-0.047803	3.742613
240.585557	4785.522838	16.437683	-0.047826	3.739549
240.312306	4777.565960	16.442688	-0.047770	3.736482
240.148028	4769.538047	16.447693	-0.047734	3.733389
240.283690	4761.533628	16.452698	-0.047754	3.730310
240.270125	4753.514828	16.457703	-0.047746	3.727219
240.059053	4745.540012	16.462707	-0.047702	3.724137
240.189067	4737.577585	16.467712	-0.047721	3.721066
239.712751	4729.598980	16.472717	-0.047627	3.717971
239.864474	4721.624108	16.477722	-0.047650	3.714891
239.582646	4713.558185	16.482727	-0.047593	3.711762
239.605647	4705.526289	16.487731	-0.047592	3.708651
239.750267	4697.507440	16.492736	-0.047613	3.705546
240.003959	4689.486290	16.497741	-0.047656	3.702440
240.168700	4681.489833	16.502746	-0.047681	3.699339
239.897518	4673.570525	16.507751	-0.047625	3.696254
239.385000	4665.620618	16.512755	-0.047525	3.693148
239.699022	4657.541106	16.517760	-0.047578	3.690010
239.253623	4649.613974	16.522765	-0.047490	3.686910
239.549631	4641.538838	16.527770	-0.047540	3.683768
239.373191	4633.602098	16.532775	-0.047502	3.680666
239.341660	4625.619003	16.537779	-0.047491	3.677546
239.746149	4617.583011	16.542784	-0.047561	3.674415
239.503756	4609.627272	16.547789	-0.047511	3.671295
239.855588	4601.568555	16.552794	-0.047571	3.668149
239.807595	4593.573148	16.557799	-0.047557	3.665013
239.974068	4585.635632	16.562803	-0.047583	3.661904
239.575160	4577.666554	16.567808	-0.047503	3.658764
239.590001	4569.705579	16.572813	-0.047501	3.655635
239.705535	4561.673707	16.577818	-0.047517	3.652479
239.626373	4553.653778	16.582823	-0.047497	3.649320
239.720927	4545.710095	16.587827	-0.047510	3.646193
239.749903	4537.655198	16.592832	-0.047510	3.643017
239.724091	4529.654708	16.597837	-0.047500	3.639858
239.591698	4521.753323	16.602842	-0.047470	3.636733
239.396509	4513.754376	16.607847	-0.047429	3.633565
239.287186	4505.743711	16.612851	-0.047403	3.630392
239.519986	4497.688663	16.617856	-0.047441	3.627208
239.255083	4489.682061	16.622861	-0.047387	3.624026
239.413654	4481.749459	16.627866	-0.047411	3.620883
239.177579	4473.710116	16.632871	-0.047362	3.617684
239.153981	4465.713554	16.637875	-0.047353	3.614505
239.302301	4457.715409	16.642880	-0.047375	3.611327
239.154300	4449.722429	16.647885	-0.047342	3.608140
239.198151	4441.721715	16.652890	-0.047345	3.604953
239.069586	4433.759529	16.657895	-0.047316	3.601773
238.802288	4425.793574	16.662899	-0.047261	3.598585
238.867717	4417.780507	16.667904	-0.047268	3.595385
238.947440	4409.770369	16.672909	-0.047278	3.592184
239.014520	4401.764383	16.677914	-0.047285	3.588981
238.630511	4393.782805	16.682919	-0.047209	3.585772
238.917294	4385.791079	16.687923	-0.047257	3.582575
238.952866	4377.767660	16.692928	-0.047258	3.579356
239.220424	4369.737121	16.697933	-0.047303	3.576138
238.695640	4361.840914	16.702938	-0.047200	3.572947
238.786580	4353.792289	16.707943	-0.047212	3.569710
238.692492	4345.852476	16.712947	-0.047189	3.566509
238.514482	4337.848043	16.717952	-0.047151	3.563276
237.970852	4329.939879	16.722957	-0.047045	3.560068
238.550957	4321.893851	16.727962	-0.047147	3.556836
239.086790	4313.734770	16.732967	-0.047242	3.553553
238.797526	4305.779680	16.737971	-0.047183	3.550325
238.910409	4297.794105	16.742976	-0.047199	3.547094
238.913211	4289.769595	16.747981	-0.047194	3.543841
238.768474	4281.884597	16.752986	-0.047162	3.540637
238.820035	4273.844080	16.757991	-0.047167	3.537373
239.147867	4265.830961	16.762995	-0.047222	3.534126
238.764120	4257.954088	16.768000	-0.047146	3.530909
238.728034	4249.857458	16.773005	-0.047134	3.527610
238.701830	4241.901611	16.778010	-0.047124	3.524366
238.680211	4233.916037	16.783015	-0.047115	3.521107
238.730948	4225.923778	16.788019	-0.047119	3.517844
238.400991	4217.948311	16.793024	-0.047052	3.514573
238.313621	4209.960495	16.798029	-0.047031	3.511302
238.365638	4201.947030	16.803034	-0.047035	3.508022
238.374788	4193.875176	16.808039	-0.047032	3.504713
238.754065	4185.909248	16.813043	-0.047097	3.501457
238.550359	4177.948449	16.818048	-0.047054	3.498181
238.055447	4170.020777	16.823053	-0.046957	3.494905
238.226638	4161.992761	16.828058	-0.046984	3.491608
238.518439	4153.884526	16.833063	-0.047033	3.488278
238.273314	4145.961133	16.838067	-0.046982	3.485003
238.583834	4137.961112	16.843072	-0.047035	3.481712
238.273458	4130.005177	16.848077	-0.046972	3.478416
237.957403	4122.077018	16.853082	-0.046908	3.475127
238.030981	4114.041124	16.858087	-0.046916	3.471804
237.945944	4106.052946	16.863091	-0.046895	3.468492
237.978343	4098.045535	16.868096	-0.046896	3.465173
238.173674	4090.044469	16.873101	-0.046927	3.461859
238.294810	4082.028526	16.878106	-0.046945	3.458533
238.307338	4074.017174	16.883111	-0.046942	3.455202
238.260205	4066.045457	16.888115	-0.046928	3.451883
238.367422	4058.031973	16.893120	-0.046943	3.448548
238.072232	4050.108183	16.898125	-0.046883	3.445233
238.165870	4042.119493	16.903130	-0.046895	3.441902
238.132667	4034.112466	16.908135	-0.046884	3.438555
238.151886	4026.158122	16.913139	-0.046882	3.435229
237.880854	4018.181345	16.918144	-0.046826	3.431880
237.871014	4010.138463	16.923149	-0.046819	3.428509
237.763315	4002.142967	16.928154	-0.046794	3.425151
238.081358	3994.119506	16.933159	-0.046848	3.421794
237.658228	3986.192334	16.938163	-0.046764	3.418447
237.659368	3978.178633	16.943168	-0.046759	3.415075
237.620677	3970.190306	16.948173	-0.046747	3.411710
237.917594	3962.139903	16.953178	-0.046797	3.408327
237.708713	3954.153021	16.958183	-0.046753	3.404949
237.694893	3946.207009	16.963187	-0.046745	3.401592
237.725667	3938.184588	16.968192	-0.046746	3.398202
237.486009	3930.263405	16.973197	-0.046696	3.394840
237.300649	3922.210726	16.978202	-0.046656	3.391422
237.166625	3914.214077	16.983207	-0.046626	3.388026
237.371885	3906.190333	16.988211	-0.046659	3.384627
237.098652	3898.258562	16.993216	-0.046603	3.381247
237.416902	3890.198451	16.998221	-0.046657	3.377830
237.421350	3882.242518	17.003226	-0.046653	3.374443
236.715859	3874.343987	17.008231	-0.046517	3.371050
236.976623	3866.293306	17.013235	-0.046560	3.367625
237.196521	3858.249159	17.018240	-0.046596	3.364198
236.833704	3850.335747	17.023245	-0.046523	3.360801
237.010492	3842.325476	17.028250	-0.046551	3.357380
236.834838	3834.328846	17.033255	-0.046513	3.353947
236.534489	3826.404617	17.038259	-0.046452	3.350538
236.370205	3818.408233	17.043264	-0.046416	3.347099
236.323739	3810.350884	17.048269	-0.046402	3.343635
236.772725	3802.363789	17.053274	-0.046481	3.340216
236.710153	3794.357031	17.058279	-0.046464	3.336766
236.286099	3786.446593	17.063283	-0.046380	3.333340
236.436414	3778.387537	17.068288	-0.046403	3.329868
236.285468	3770.420171	17.073293	-0.046369	3.326421
236.516420	3762.406626	17.078298	-0.046407	3.322965
236.380240	3754.412016	17.083303	-0.046377	3.319499
236.568872	3746.453410	17.088307	-0.046407	3.316058
236.357392	3738.460741	17.093312	-0.046362	3.312583
236.142492	3730.471844	17.098317	-0.046317	3.309106
236.226990	3722.482213	17.103322	-0.046327	3.305636
235.996610	3714.485124	17.108327	-0.046279	3.302147
236.022102	3706.504789	17.113331	-0.046279	3.298672
236.571232	3698.424180	17.118336	-0.046376	3.295170
236.669185	3690.422522	17.123341	-0.046389	3.291682
236.389845	3682.498916	17.128346	-0.046332	3.288208
236.288246	3674.489724	17.133351	-0.046308	3.284701
236.029177	3666.612674	17.138355	-0.046254	3.281241
235.885334	3658.614547	17.143360	-0.046223	3.277729
236.213775	3650.539411	17.148365	-0.046278	3.274198
236.448075	3642.549744	17.153370	-0.046317	3.270698
236.319705	3634.517079	17.158375	-0.046288	3.267160
236.469691	3626.559398	17.163379	-0.046311	3.263663
236.477352	3618.621334	17.168384	-0.046307	3.260165
236.117147	3610.680216	17.173389	-0.046235	3.256646
236.189560	3602.655047	17.178394	-0.046243	3.253105
236.302681	3594.593834	17.183399	-0.046259	3.249545
236.435644	3586.649503	17.188403	-0.046279	3.246034
235.760142	3578.775837	17.193408	-0.046148	3.242517
235.804132	3570.705219	17.198413	-0.046151	3.238938
235.840806	3562.748882	17.203418	-0.046152	3.235406
236.369350	3554.651394	17.208423	-0.046245	3.231828
235.973425	3546.713577	17.213427	-0.046167	3.228279
235.939305	3538.721520	17.218432	-0.046155	3.224716
235.876255	3530.731282	17.223437	-0.046138	3.221149
235.632688	3522.804223	17.228442	-0.046088	3.217599
235.324661	3514.813345	17.233447	-0.046025	3.214013
235.826245	3506.753807	17.238451	-0.046113	3.210428
235.889337	3498.757052	17.243456	-0.046120	3.206847
235.715031	3490.757304	17.248461	-0.046082	3.203252
235.491807	3482.856122	17.253466	-0.046036	3.199694
235.862136	3474.812005	17.258471	-0.046099	3.196093
235.875524	3466.824558	17.263475	-0.046097	3.192499
235.856450	3458.815325	17.268480	-0.046088	3.188889
235.498275	3450.870323	17.273485	-0.046016	3.185290
235.315124	3442.957481	17.278490	-0.045977	3.181708
235.440253	3434.886173	17.283495	-0.045995	3.178064
235.350789	3426.920217	17.288499	-0.045973	3.174455
235.395655	3418.913693	17.293504	-0.045976	3.170829
235.568018	3410.872824	17.298509	-0.046003	3.167188
235.250049	3402.975294	17.303514	-0.045939	3.163587
235.479800	3394.930610	17.308519	-0.045977	3.159939
235.798889	3386.945211	17.313523	-0.046031	3.156318
235.723928	3378.944883	17.318528	-0.046012	3.152669
235.723944	3370.930688	17.323533	-0.046007	3.149012
235.477840	3363.009712	17.328538	-0.045956	3.145382
235.176938	3355.048889	17.333543	-0.045894	3.141728
235.440088	3347.042514	17.338547	-0.045938	3.138074
235.358666	3339.047143	17.343552	-0.045918	3.134405
235.240606	3331.055332	17.348557	-0.045891	3.130731
235.626581	3323.024371	17.353562	-0.045958	3.127059
235.404526	3315.081479	17.358567	-0.045911	3.123395
235.700299	3307.073453	17.363571	-0.045961	3.119720
235.796738	3299.122595	17.368576	-0.045974	3.116058
235.513221	3291.135014	17.373581	-0.045916	3.112358
235.487280	3283.164036	17.378586	-0.045906	3.108672
235.586493	3275.139242	17.383591	-0.045919	3.104963
235.390420	3267.235532	17.388595	-0.045877	3.101292
235.418848	3259.232289	17.393600	-0.045878	3.097581
235.134293	3251.241718	17.398605	-0.045819	3.093856
235.314038	3243.247606	17.403610	-0.045848	3.090148
235.286179	3235.240731	17.408615	-0.045837	3.086419
234.827329	3227.346744	17.413619	-0.045747	3.082717
234.870583	3219.321859	17.418624	-0.045750	3.078974
234.896188	3211.339249	17.423629	-0.045749	3.075246
235.021800	3203.287280	17.428634	-0.045768	3.071485
235.031694	3195.242435	17.433639	-0.045764	3.067717
235.088523	3187.261149	17.438643	-0.045770	3.063977
234.893600	3179.350963	17.443648	-0.045728	3.060254
234.860407	3171.356015	17.448653	-0.045717	3.056493
234.751626	3163.422559	17.453658	-0.045691	3.052754
234.649359	3155.409485	17.458663	-0.045667	3.048972
234.848377	3147.372880	17.463667	-0.045699	3.045190
234.657394	3139.437255	17.468672	-0.045658	3.041432
234.769175	3131.436853	17.473677	-0.045674	3.037653
234.544919	3123.501488	17.478682	-0.045627	3.033883
234.562723	3115.472279	17.483687	-0.045625	3.030077
234.643421	3107.490534	17.488691	-0.045635	3.026291
235.011634	3099.452207	17.493696	-0.045699	3.022488
234.844444	3091.492380	17.498701	-0.045662	3.018691
234.921335	3083.527857	17.503706	-0.045671	3.014899
234.694284	3075.582778	17.508711	-0.045624	3.011096
234.696561	3067.580962	17.513715	-0.045619	3.007272
234.345947	3059.631579	17.518720	-0.045549	3.003451
234.374738	3051.651899	17.523725	-0.045549	2.999630
234.275040	3043.720864	17.528730	-0.045525	2.995821
233.974557	3035.737727	17.533735	-0.045464	2.991972
234.279640	3027.659647	17.538739	-0.045516	2.988103
234.496664	3019.635703	17.543744	-0.045551	2.984251
234.311465	3011.701674	17.548749	-0.045511	2.980416
234.186644	3003.770131	17.553754	-0.045483	2.976581
234.662466	2995.668257	17.558759	-0.045566	2.972689
234.451288	2987.731246	17.563763	-0.045522	2.968837
234.012732	2979.810061	17.568768	-0.045435	2.964975
234.122112	2971.822381	17.573773	-0.045450	2.961105
234.005909	2963.861356	17.578778	-0.045424	2.957230
233.902879	2955.871553	17.583783	-0.045399	2.953337
233.616572	2947.917534	17.588787	-0.045341	2.949447
233.465615	2939.938208	17.593792	-0.045308	2.945546
234.027924	2931.827275	17.598797	-0.045407	2.941615
234.068018	2923.874317	17.603802	-0.045409	2.937727
233.467285	2916.000627	17.608807	-0.045292	2.933838
233.582756	2907.956787	17.613811	-0.045309	2.929899
233.478919	2899.995621	17.618816	-0.045284	2.925984
233.335253	2892.021666	17.623821	-0.045252	2.922055
233.480897	2884.032087	17.628826	-0.045274	2.918129
233.360871	2876.063123	17.633831	-0.045247	2.914193
233.055682	2868.069388	17.638835	-0.045185	2.910229
233.068450	2860.072036	17.643840	-0.045182	2.906276
232.468118	2852.166094	17.648845	-0.045065	2.902328
232.526427	2844.143960	17.653850	-0.045071	2.898354
232.629418	2836.110187	17.658855	-0.045085	2.894371
232.674181	2828.155462	17.663859	-0.045088	2.890419
233.002824	2820.097530	17.668864	-0.045144	2.886426
232.775460	2812.137066	17.673869	-0.045097	2.882445
233.090039	2804.160239	17.678874	-0.045150	2.878481
232.375471	2796.317573	17.683879	-0.045012	2.874520
232.760265	2788.227473	17.688883	-0.045078	2.870492
233.040725	2780.215756	17.693888	-0.045125	2.866492
232.620433	2772.308457	17.698893	-0.045042	2.862498
232.964675	2764.284963	17.703898	-0.045101	2.858485
233.107587	2756.297390	17.708903	-0.045122	2.854472
233.111193	2748.320188	17.713907	-0.045118	2.850451
233.011312	2740.374125	17.718912	-0.045094	2.846434
233.168116	2732.362369	17.723917	-0.045118	2.842393
233.462889	2724.378111	17.728922	-0.045168	2.838368
233.150998	2716.435460	17.733927	-0.045105	2.834323
232.921178	2708.502845	17.738931	-0.045057	2.830282
233.088715	2700.478727	17.743936	-0.045083	2.826212
232.774111	2692.540231	17.748941	-0.045019	2.822152
233.072542	2684.528837	17.753946	-0.045069	2.818084
233.391604	2676.476351	17.758951	-0.045124	2.813991
233.234399	2668.545679	17.763955	-0.045089	2.809927
233.345645	2660.563630	17.768960	-0.045105	2.805846
233.057585	2652.631191	17.773965	-0.045046	2.801760
233.088060	2644.672049	17.778970	-0.045047	2.797674
232.914681	2636.699247	17.783975	-0.045009	2.793563
233.138359	2628.675381	17.788979	-0.045046	2.789443
233.063135	2620.727970	17.793984	-0.045026	2.785338
232.519200	2612.824492	17.798989	-0.044920	2.781222
232.582555	2604.850023	17.803994	-0.044927	2.777100
232.512588	2596.830244	17.808999	-0.044908	2.772940
232.546225	2588.828326	17.814003	-0.044910	2.768789
232.392910	2580.879124	17.819008	-0.044876	2.764648
232.540630	2572.895436	17.824013	-0.044898	2.760501
232.544767	2564.946097	17.829018	-0.044894	2.756357
232.516451	2556.912783	17.834023	-0.044883	2.752161
232.659334	2548.873722	17.839027	-0.044905	2.747967
232.212905	2540.986283	17.844032	-0.044817	2.743808
232.016438	2533.030616	17.849037	-0.044775	2.739623
232.388051	2525.001385	17.854042	-0.044839	2.735429
232.472109	2516.995020	17.859047	-0.044849	2.731222
232.351231	2509.052198	17.864051	-0.044822	2.727029
232.259658	2501.112812	17.869056	-0.044800	2.722833
232.100509	2493.153722	17.874061	-0.044765	2.718616
232.450253	2485.137401	17.879066	-0.044825	2.714395
232.501576	2477.150004	17.884071	-0.044829	2.710164
232.276829	2469.220224	17.889075	-0.044782	2.705938
232.287274	2461.257425	17.894080	-0.044779	2.701704
232.269101	2453.260214	17.899085	-0.044770	2.697443
232.210283	2445.310996	17.904090	-0.044754	2.693198
232.237283	2437.311931	17.909095	-0.044754	2.688925
232.153040	2429.343799	17.914099	-0.044733	2.684655
232.069907	2421.425497	17.919104	-0.044713	2.680404
231.614973	2413.520580	17.924109	-0.044623	2.676130
231.774406	2405.483619	17.929114	-0.044647	2.671818
231.745065	2397.473452	17.934119	-0.044637	2.667501
231.746072	2389.490455	17.939123	-0.044632	2.663194
231.757676	2381.533494	17.944128	-0.044629	2.658895
231.935415	2373.528553	17.949133	-0.044657	2.654574
231.877456	2365.558473	17.954138	-0.044641	2.650249
232.013285	2357.566249	17.959143	-0.044661	2.645918
231.927741	2349.618196	17.964147	-0.044640	2.641589
231.806488	2341.707977	17.969152	-0.044612	2.637271
231.237845	2333.797821	17.974157	-0.044501	2.632915
231.664683	2325.746295	17.979162	-0.044575	2.628543
231.826230	2317.711661	17.984167	-0.044600	2.624154
231.400387	2309.848487	17.989171	-0.044516	2.619812
231.411566	2301.878339	17.994176	-0.044513	2.615434
231.392691	2293.894397	17.999181	-0.044504	2.611039
231.487209	2285.893830	18.004186	-0.044517	2.606636
231.345385	2277.947445	18.009191	-0.044485	2.602238
231.240255	2270.011363	18.014195	-0.044460	2.597841
231.954326	2261.894285	18.019200	-0.044588	2.593394
231.568054	2253.892826	18.024205	-0.044511	2.588926
231.613383	2245.948730	18.029210	-0.044514	2.584512
231.404596	2238.032434	18.034215	-0.044470	2.580089
231.349005	2230.074616	18.039219	-0.044455	2.575645
231.330576	2222.128070	18.044224	-0.044446	2.571203
231.275650	2214.159788	18.049229	-0.044431	2.566739
231.374675	2206.181052	18.054234	-0.044444	2.562271
231.381791	2198.211514	18.059239	-0.044440	2.557795
231.494159	2190.238309	18.064243	-0.044456	2.553316
231.279300	2182.327546	18.069248	-0.044411	2.548841
231.084279	2174.340435	18.074253	-0.044370	2.544316
231.284095	2166.390285	18.079258	-0.044402	2.539833
231.147772	2158.429016	18.084263	-0.044371	2.535311
230.829436	2150.494205	18.089267	-0.044307	2.530783
231.189338	2142.472607	18.094272	-0.044368	2.526247
231.085231	2134.528676	18.099277	-0.044344	2.521713
231.279221	2126.536215	18.104282	-0.044375	2.517165
231.066371	2118.605593	18.109287	-0.044330	2.512614
231.102745	2110.607588	18.114291	-0.044332	2.508034
230.912188	2102.669948	18.119296	-0.044291	2.503464
231.167209	2094.665881	18.124301	-0.044333	2.498881
230.990474	2086.746132	18.129306	-0.044295	2.494306
230.961407	2078.784995	18.134311	-0.044285	2.489709
230.605626	2070.852140	18.139315	-0.044214	2.485095
230.904640	2062.861452	18.144320	-0.044264	2.480489
230.879466	2054.895657	18.149325	-0.044254	2.475865
231.170020	2046.896871	18.154330	-0.044303	2.471236
230.909479	2038.961502	18.159335	-0.044249	2.466594
230.723754	2031.035387	18.164339	-0.044210	2.461954
230.912443	2023.060556	18.169344	-0.044240	2.457305
230.956244	2015.074031	18.174349	-0.044243	2.452630
230.549094	2007.191822	18.179354	-0.044162	2.447972
230.286692	1999.241788	18.184359	-0.044108	2.443276
230.048070	1991.316482	18.189363	-0.044058	2.438588
229.914526	1983.362491	18.194368	-0.044028	2.433882
229.816934	1975.338503	18.199373	-0.044005	2.429128
230.061491	1967.299965	18.204378	-0.044045	2.424383
229.605041	1959.431431	18.209383	-0.043955	2.419674
229.851811	1951.419559	18.214387	-0.043996	2.414927
229.639863	1943.500593	18.219392	-0.043951	2.410189
229.276879	1935.544722	18.224397	-0.043879	2.405408
229.975909	1927.488472	18.229402	-0.044004	2.400642
229.965377	1919.553488	18.234407	-0.043997	2.395883
230.164920	1911.568894	18.239411	-0.044029	2.391101
229.991798	1903.642572	18.244416	-0.043991	2.386314
229.941068	1895.702819	18.249421	-0.043977	2.381520
229.832390	1887.770140	18.254426	-0.043951	2.376716
229.565654	1879.845603	18.259431	-0.043896	2.371893
229.871726	1871.821965	18.264435	-0.043948	2.367048
230.038446	1863.873703	18.269440	-0.043974	2.362228
229.932126	1855.948200	18.274445	-0.043949	2.357388
229.716637	1848.022992	18.279450	-0.043904	2.352530
229.691763	1840.053914	18.284455	-0.043894	2.347651
230.218024	1832.009927	18.289459	-0.043987	2.342762
229.803505	1824.159901	18.294464	-0.043905	2.337903
229.299151	1816.257727	18.299469	-0.043806	2.332994
229.304504	1808.282955	18.304474	-0.043802	2.328072
229.350218	1800.288732	18.309479	-0.043805	2.323132
229.320052	1792.349573	18.314483	-0.043794	2.318209
229.662012	1784.356746	18.319488	-0.043853	2.313274
229.224568	1776.462334	18.324493	-0.043766	2.308323
228.867988	1768.555736	18.329498	-0.043695	2.303360
229.164689	1760.544452	18.334503	-0.043745	2.298378
229.682853	1752.493543	18.339507	-0.043836	2.293379
229.317152	1744.632964	18.344512	-0.043763	2.288412
229.331475	1736.655175	18.349517	-0.043760	2.283394
229.187997	1728.777409	18.354522	-0.043729	2.278413
228.501394	1720.923938	18.359527	-0.043596	2.273390
228.536525	1712.876940	18.364531	-0.043597	2.268296
228.628946	1704.891565	18.369536	-0.043609	2.263235
228.966492	1696.864725	18.374541	-0.043667	2.258158
228.841925	1688.958002	18.379546	-0.043638	2.253105
228.670682	1681.026346	18.384551	-0.043601	2.248020
228.234835	1673.154489	18.389555	-0.043515	2.242939
228.653358	1665.135797	18.394560	-0.043588	2.237828
228.538979	1657.185128	18.399565	-0.043561	2.232702
228.719746	1649.220632	18.404570	-0.043590	2.227581
228.906594	1641.240404	18.409575	-0.043620	2.222440
228.411451	1633.393845	18.414579	-0.043522	2.217310
228.410718	1625.458631	18.419584	-0.043517	2.212157
228.459312	1617.464968	18.424589	-0.043521	2.206957
228.460672	1609.538128	18.429594	-0.043516	2.201785
228.058900	1601.669036	18.434599	-0.043436	2.196601
228.468183	1593.633049	18.439603	-0.043507	2.191371
228.722290	1585.643015	18.444608	-0.043549	2.186144
228.574926	1577.737661	18.449613	-0.043517	2.180922
229.061341	1569.715492	18.454618	-0.043602	2.175671
228.853375	1561.841522	18.459623	-0.043558	2.170439
228.606083	1553.938256	18.464627	-0.043507	2.165172
228.579697	1546.034433	18.469632	-0.043497	2.159912
228.381951	1538.122321	18.474637	-0.043455	2.154618
228.510798	1530.149012	18.479642	-0.043474	2.149301
228.736988	1522.163391	18.484647	-0.043511	2.143972
228.256672	1514.309715	18.489651	-0.043417	2.138650
228.264349	1506.381880	18.494656	-0.043413	2.133312
228.432753	1498.379276	18.499661	-0.043439	2.127925
228.101404	1490.524390	18.504666	-0.043372	2.122577
228.436634	1482.515972	18.509671	-0.043430	2.117176
228.365705	1474.583897	18.514675	-0.043411	2.111773
228.682550	1466.573298	18.519680	-0.043465	2.106341
228.749188	1458.626570	18.524685	-0.043472	2.100914
228.402829	1450.778656	18.529690	-0.043403	2.095499
228.149936	1442.896354	18.534695	-0.043351	2.090056
228.097735	1434.935542	18.539699	-0.043336	2.084565
228.419655	1426.986812	18.544704	-0.043390	2.079105
227.879877	1419.123216	18.549709	-0.043285	2.073603
228.253649	1411.135938	18.554714	-0.043349	2.068093
228.242065	1403.202260	18.559719	-0.043342	2.062566
227.776380	1395.359938	18.564723	-0.043250	2.057041
227.713697	1387.422038	18.569728	-0.043233	2.051477
227.800262	1379.440631	18.574733	-0.043244	2.045882
227.514834	1371.594760	18.579738	-0.043186	2.040328
227.780077	1363.611791	18.584743	-0.043230	2.034720
227.686139	1355.681724	18.589747	-0.043208	2.029096
227.675917	1347.747893	18.594752	-0.043201	2.023463
227.423548	1339.858264	18.599757	-0.043149	2.017819
227.281383	1331.949182	18.604762	-0.043117	2.012158
227.297163	1323.996930	18.609767	-0.043115	2.006467
227.068972	1316.107876	18.614771	-0.043067	2.000778
227.213077	1308.169012	18.619776	-0.043089	1.995078
227.208006	1300.223372	18.624781	-0.043083	1.989340
227.300155	1292.285665	18.629786	-0.043095	1.983602
227.035352	1284.430264	18.634791	-0.043041	1.977868
226.884830	1276.513930	18.639795	-0.043007	1.972086
226.892078	1268.604060	18.644800	-0.043004	1.966309
227.119758	1260.604286	18.649805	-0.043041	1.960472
227.021524	1252.733994	18.654810	-0.043018	1.954678
226.862422	1244.843811	18.659815	-0.042983	1.948845
226.378025	1236.980876	18.664819	-0.042888	1.942978
227.158617	1228.915070	18.669824	-0.043028	1.937085
227.071601	1220.998451	18.674829	-0.043006	1.931187
227.316420	1213.042234	18.679834	-0.043047	1.925279
227.237233	1205.164106	18.684839	-0.043027	1.919375
227.138413	1197.296622	18.689843	-0.043004	1.913458
227.065015	1189.411366	18.694848	-0.042985	1.907512
226.843119	1181.520083	18.699853	-0.042938	1.901527
226.295268	1173.725064	18.704858	-0.042831	1.895557
226.611871	1165.731305	18.709863	-0.042885	1.889517
226.682595	1157.784610	18.714867	-0.042893	1.883466
226.390279	1149.952898	18.719872	-0.042834	1.877440
226.921640	1141.933914	18.724877	-0.042927	1.871348
226.884703	1134.043048	18.729882	-0.042915	1.865268
226.582334	1126.209572	18.734887	-0.042854	1.859181
226.622173	1118.277195	18.739891	-0.042856	1.853038
226.967453	1110.316226	18.744896	-0.042915	1.846889
226.192729	1102.557187	18.749901	-0.042766	1.840742
226.387997	1094.618939	18.754906	-0.042797	1.834551
226.576118	1086.686549	18.759911	-0.042827	1.828343
226.548280	1078.786012	18.764915	-0.042817	1.822113
226.394027	1070.932644	18.769920	-0.042783	1.815883
226.450050	1063.002051	18.774925	-0.042789	1.809596
226.689452	1055.096482	18.779930	-0.042828	1.803330
226.467420	1047.259223	18.784935	-0.042782	1.797040
226.575406	1039.317770	18.789939	-0.042797	1.790685
226.813592	1031.377880	18.794944	-0.042836	1.784325
226.433344	1023.564425	18.799949	-0.042760	1.777966
226.402989	1015.671721	18.804954	-0.042749	1.771565
226.330303	1007.792692	18.809959	-0.042731	1.765146
226.175654	999.947541	18.814963	-0.042697	1.758720
226.141839	992.070576	18.819968	-0.042685	1.752261
226.279120	984.134979	18.824973	-0.042706	1.745751
226.300105	976.282549	18.829978	-0.042705	1.739271
226.252451	968.407310	18.834983	-0.042691	1.732739
226.333574	960.490906	18.839987	-0.042701	1.726164
226.357149	952.654279	18.844992	-0.042700	1.719624
226.153929	944.824086	18.849997	-0.042657	1.713034
225.989043	936.954785	18.855002	-0.042621	1.706390
225.693884	929.119518	18.860007	-0.042561	1.699732
225.594748	921.259877	18.865011	-0.042538	1.693054
225.741272	913.340900	18.870016	-0.042560	1.686331
225.522890	905.508700	18.875021	-0.042514	1.679606
225.598467	897.634962	18.880026	-0.042523	1.672859
225.250889	889.813764	18.885031	-0.042453	1.666071
225.505944	881.882219	18.890035	-0.042496	1.659243
225.667222	874.006923	18.895040	-0.042521	1.652423
225.252477	866.206310	18.900045	-0.042438	1.645560
224.892123	858.427595	18.905050	-0.042366	1.638694
225.008669	850.518119	18.910055	-0.042383	1.631752
225.109402	842.594226	18.915059	-0.042397	1.624765
224.812282	834.799180	18.920064	-0.042336	1.617806
225.122659	826.855162	18.925069	-0.042389	1.610770
225.029002	819.028208	18.930074	-0.042366	1.603751
225.210288	811.173753	18.935079	-0.042395	1.596715
224.864227	803.375579	18.940083	-0.042326	1.589623
225.348207	795.450476	18.945088	-0.042411	1.582505
225.030068	787.676258	18.950093	-0.042346	1.575375
224.661278	779.908616	18.955098	-0.042273	1.568210
225.062015	771.982821	18.960103	-0.042342	1.560982
224.928774	764.188942	18.965107	-0.042312	1.553762
225.134593	756.327618	18.970112	-0.042345	1.546497
224.799119	748.550862	18.975117	-0.042278	1.539194
225.004637	740.693145	18.980122	-0.042311	1.531863
224.852316	732.886549	18.985127	-0.042278	1.524490
224.815950	725.072215	18.990131	-0.042266	1.517092
224.474816	717.329853	18.995136	-0.042197	1.509678
224.586741	709.471695	19.000141	-0.042213	1.502188
224.376395	701.701379	19.005146	-0.042169	1.494695
224.685919	693.821380	19.010151	-0.042222	1.487139
224.743284	686.001469	19.015155	-0.042227	1.479564
224.722232	678.212919	19.020160	-0.042218	1.471967
224.477945	670.420512	19.025165	-0.042168	1.464292
224.587432	662.600302	19.030170	-0.042183	1.456606
224.672272	654.782428	19.035175	-0.042194	1.448877
224.650089	646.995260	19.040179	-0.042185	1.441120
224.407885	639.281162	19.045184	-0.042135	1.433358
224.678385	631.409143	19.050189	-0.042180	1.425479
224.521944	623.679501	19.055194	-0.042146	1.417630
224.194618	615.951494	19.060199	-0.042080	1.409709
223.975887	608.207674	19.065203	-0.042034	1.401746
224.263465	600.393019	19.070208	-0.042083	1.393752
224.163545	592.615153	19.075213	-0.042059	1.385682
224.326496	584.830585	19.080218	-0.042084	1.377604
224.154073	577.093611	19.085223	-0.042047	1.369469
223.918326	569.364979	19.090227	-0.041998	1.361284
223.753992	561.652142	19.095232	-0.041963	1.353078
223.764187	553.873368	19.100237	-0.041960	1.344783
223.667908	546.155402	19.105242	-0.041937	1.336482
223.736483	538.388844	19.110247	-0.041944	1.328107
223.398432	530.712226	19.115251	-0.041876	1.319703
223.180809	522.977676	19.120256	-0.041831	1.311203
223.338592	515.142571	19.125261	-0.041855	1.302606
223.491737	507.397818	19.130266	-0.041879	1.294052
223.468570	499.674686	19.135271	-0.041869	1.285432
223.179651	492.017884	19.140275	-0.041811	1.276778
223.191626	484.317823	19.145280	-0.041808	1.268073
223.073932	476.621871	19.150285	-0.041781	1.259288
223.030637	468.938319	19.155290	-0.041768	1.250469
222.665712	461.305386	19.160295	-0.041695	1.241584
222.720592	453.596632	19.165299	-0.041700	1.232629
223.045866	445.849927	19.170304	-0.041756	1.223618
222.843241	438.205276	19.175309	-0.041713	1.214554
222.856931	430.524531	19.180314	-0.041711	1.205423
222.672018	422.916514	19.185319	-0.041672	1.196270
222.367633	415.310960	19.190323	-0.041610	1.187024
222.525437	407.630904	19.195328	-0.041634	1.177710
222.059601	400.067432	19.200333	-0.041543	1.168335
222.059693	392.439369	19.205338	-0.041538	1.158902
222.158123	384.769381	19.210343	-0.041551	1.149361
221.957833	377.161159	19.215347	-0.041509	1.139753
222.266765	369.491387	19.220352	-0.041562	1.130096
222.113296	361.911808	19.225357	-0.041528	1.120370
222.092981	354.332103	19.230362	-0.041519	1.110588
221.853089	346.795790	19.235367	-0.041470	1.100727
221.714788	339.235023	19.240371	-0.041439	1.090767
221.439294	331.732069	19.245376	-0.041383	1.080760
221.316318	324.186606	19.250381	-0.041355	1.070638
221.354982	316.619999	19.255386	-0.041358	1.060429
221.618042	309.028615	19.260391	-0.041402	1.050140
221.100158	301.601256	19.265395	-0.041301	1.039789
221.199151	294.073624	19.270400	-0.041314	1.029343
221.411791	286.519873	19.275405	-0.041349	1.018781
221.185859	279.082256	19.280410	-0.041302	1.008165
221.113187	271.629267	19.285415	-0.041284	0.997452
221.292533	264.104509	19.290419	-0.041312	0.986583
221.152245	256.685087	19.295424	-0.041281	0.975665
220.926188	249.290334	19.300429	-0.041234	0.964638
220.926546	241.878097	19.305434	-0.041230	0.953518
221.190043	234.423822	19.310439	-0.041274	0.942271
220.463471	227.174077	19.315443	-0.041134	0.930938
220.502106	219.802693	19.320448	-0.041136	0.919483
220.812585	212.383446	19.325453	-0.041189	0.907884
220.762852	205.064801	19.330458	-0.041175	0.896195
220.211754	197.860546	19.335463	-0.041068	0.884395
220.392246	190.528413	19.340467	-0.041097	0.872435
220.589451	183.226869	19.345472	-0.041129	0.860366
220.545961	175.988361	19.350477	-0.041116	0.848160
220.174843	168.844544	19.355482	-0.041043	0.835839
219.970256	161.663253	19.360487	-0.041000	0.823319
220.037039	154.464534	19.365491	-0.041008	0.810660
220.477240	147.243448	19.370496	-0.041085	0.797880
220.184607	140.183713	19.375501	-0.041026	0.784949
219.903150	133.156863	19.380506	-0.040969	0.771866
220.090157	126.066822	19.385511	-0.040999	0.758596
219.754984	119.102351	19.390515	-0.040932	0.745152
219.859541	112.095798	19.395520	-0.040947	0.731533
219.659941	105.184787	19.400525	-0.040906	0.717738
219.672262	98.273246	19.405530	-0.040903	0.703748
219.409619	91.454991	19.410535	-0.040850	0.689567
219.465860	84.618570	19.415539	-0.040856	0.675171
219.569230	77.988625	19.420544	-0.040871	0.660929