Fri Apr 16 19:02:20 2021

Number of Points = 3639
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.145938	-0.140531	0.000000	-0.000148	0.312045

1.679695	-0.242593	0.005005	-0.000247	0.312022
2.043806	-0.369136	0.010010	-0.000315	0.311742
1.696836	-0.309060	0.015014	-0.000251	0.311728
1.699909	-0.312452	0.020019	-0.000251	0.311715
1.878407	-0.342480	0.025024	-0.000284	0.311727
1.316303	-0.239266	0.030029	-0.000180	0.311732
1.028190	-0.183341	0.035034	-0.000126	0.311749
1.079541	-0.192964	0.040038	-0.000136	0.311748
1.049805	-0.188331	0.045043	-0.000130	0.311744
0.855004	-0.205621	0.050048	-0.000094	0.311500
0.576789	-0.172736	0.055053	-0.000042	0.311418
1.584132	-0.358393	0.060058	-0.000230	0.311406
1.201050	-0.285775	0.065062	-0.000159	0.311420
1.177207	-0.282716	0.070067	-0.000154	0.311414
1.423025	-0.326674	0.075072	-0.000200	0.311418
0.937405	-0.264086	0.080077	-0.000110	0.311299
1.040465	-0.323910	0.085082	-0.000129	0.311108
1.011624	-0.318695	0.090086	-0.000124	0.311108
1.184449	-0.352171	0.095091	-0.000156	0.311098
1.555469	-0.418662	0.100096	-0.000225	0.311103
1.003742	-0.359345	0.105101	-0.000122	0.310913
1.443588	-0.467732	0.110106	-0.000204	0.310780
0.899912	-0.365700	0.115110	-0.000103	0.310796
1.170280	-0.419875	0.120115	-0.000153	0.310772
1.321093	-0.470459	0.125120	-0.000181	0.310665
1.100676	-0.459419	0.130125	-0.000140	0.310530
0.847025	-0.410391	0.135130	-0.000093	0.310544
1.496479	-0.530709	0.140134	-0.000214	0.310533
1.326974	-0.565211	0.145139	-0.000183	0.310229
1.600684	-0.623622	0.150144	-0.000233	0.310188
1.627021	-0.630879	0.155149	-0.000238	0.310177
1.289966	-0.620775	0.160154	-0.000176	0.309939
1.312626	-0.638481	0.165158	-0.000180	0.309875
0.767058	-0.540429	0.170163	-0.000078	0.309871
1.031106	-0.635680	0.175168	-0.000128	0.309650
1.062255	-0.666527	0.180173	-0.000133	0.309532
0.775037	-0.612089	0.185178	-0.000080	0.309543
0.743326	-0.649486	0.190182	-0.000074	0.309341
1.241886	-0.760923	0.195187	-0.000167	0.309244
1.225270	-0.758642	0.200192	-0.000164	0.309241
0.757105	-0.742707	0.205197	-0.000077	0.308917
1.143386	-0.813337	0.210202	-0.000149	0.308916
1.190624	-0.850875	0.215206	-0.000157	0.308780
0.950845	-0.844897	0.220211	-0.000113	0.308604
0.946649	-0.841409	0.225216	-0.000112	0.308617
0.714623	-0.866707	0.230221	-0.000069	0.308301
1.088994	-0.940088	0.235226	-0.000139	0.308276
0.945813	-0.950594	0.240230	-0.000112	0.308105
0.679392	-0.926492	0.245235	-0.000062	0.307991
0.621237	-0.934949	0.250240	-0.000052	0.307901
0.390371	-0.943770	0.255245	-0.000009	0.307663
0.573077	-0.978412	0.260250	-0.000043	0.307656
0.726108	-1.069703	0.265254	-0.000071	0.307358
0.505639	-1.032538	0.270259	-0.000030	0.307344
0.392980	-1.063917	0.275264	-0.000009	0.307100
0.071996	-1.019755	0.280269	0.000050	0.307034
0.432270	-1.124127	0.285274	-0.000017	0.306851
0.009967	-1.069682	0.290278	0.000062	0.306746
0.036177	-1.105912	0.295283	0.000057	0.306597
0.014326	-1.138710	0.300288	0.000061	0.306424
-0.775684	-1.009085	0.305293	0.000208	0.306359
-0.769223	-1.060025	0.310298	0.000207	0.306124
-0.381890	-1.131533	0.315302	0.000135	0.306118
-0.696094	-1.142007	0.320307	0.000193	0.305799
-0.468202	-1.184407	0.325312	0.000151	0.305795
-0.622108	-1.205131	0.330317	0.000179	0.305564
-0.629757	-1.208428	0.335322	0.000181	0.305542
-0.657831	-1.261458	0.340326	0.000186	0.305267
-0.828628	-1.245029	0.345331	0.000218	0.305198
-0.019175	-1.449236	0.350336	0.000067	0.304927
-0.177461	-1.436832	0.355341	0.000097	0.304850
-0.546429	-1.435205	0.360346	0.000165	0.304540
-0.553217	-1.439525	0.365350	0.000166	0.304513
-1.022639	-1.408767	0.370355	0.000254	0.304254
-0.894787	-1.446841	0.375360	0.000230	0.304184
-0.759720	-1.529168	0.380365	0.000205	0.303909
-0.836261	-1.540852	0.385370	0.000219	0.303787
-0.707667	-1.603717	0.390374	0.000195	0.303599
-0.956463	-1.603958	0.395379	0.000241	0.303383
-0.957820	-1.623713	0.400384	0.000242	0.303288
-1.459554	-1.584752	0.405389	0.000335	0.303039
-1.167093	-1.654188	0.410394	0.000281	0.302961
-1.366678	-1.678045	0.415398	0.000318	0.302674
-1.481690	-1.682588	0.420403	0.000339	0.302553
-1.247663	-1.769330	0.425408	0.000295	0.302341
-1.596070	-1.749318	0.430413	0.000360	0.302134
-1.364065	-1.819598	0.435418	0.000317	0.302000
-1.436576	-1.862165	0.440422	0.000331	0.301733
-1.890028	-1.803950	0.445427	0.000415	0.301617
-2.046820	-1.821801	0.450432	0.000444	0.301395
-2.210489	-1.828090	0.455437	0.000475	0.301222
-2.425006	-1.818520	0.460442	0.000514	0.301081
-2.660484	-1.825356	0.465446	0.000558	0.300842
-2.731960	-1.832188	0.470451	0.000572	0.300747
-2.410612	-1.934228	0.475456	0.000512	0.300537
-2.635177	-1.920820	0.480461	0.000554	0.300405
-2.916368	-1.915211	0.485466	0.000606	0.300186
-3.009055	-1.941671	0.490470	0.000623	0.299978
-3.073935	-1.954174	0.495475	0.000635	0.299861
-3.102275	-2.011626	0.500480	0.000640	0.299559
-3.332144	-1.988974	0.505485	0.000683	0.299467
-3.536356	-1.997155	0.510490	0.000721	0.299248
-3.628241	-2.018764	0.515494	0.000738	0.299063
-3.961592	-1.989092	0.520499	0.000800	0.298913
-3.518075	-2.122980	0.525504	0.000718	0.298655
-3.990128	-2.059112	0.530509	0.000806	0.298549
-4.315831	-2.055186	0.535514	0.000866	0.298282
-4.246716	-2.091413	0.540518	0.000853	0.298167
-4.309313	-2.116249	0.545523	0.000865	0.297991
-4.846275	-2.064856	0.550528	0.000965	0.297767
-4.742650	-2.106484	0.555533	0.000945	0.297657
-5.355120	-2.055805	0.560538	0.001059	0.297362
-5.357494	-2.067516	0.565542	0.001060	0.297303
-5.857442	-2.033513	0.570547	0.001153	0.297026
-6.164681	-1.990474	0.575552	0.001210	0.296964
-6.477679	-1.978695	0.580557	0.001268	0.296744
-6.414605	-2.014002	0.585562	0.001257	0.296628
-7.003059	-1.948041	0.590566	0.001366	0.296428
-6.871872	-1.995758	0.595571	0.001342	0.296312
-7.343263	-1.947088	0.600576	0.001429	0.296132
-7.536776	-1.929912	0.605581	0.001465	0.296044
-7.469548	-1.993829	0.610586	0.001453	0.295791
-7.017818	-2.090301	0.615590	0.001369	0.295721
-7.488167	-2.045730	0.620595	0.001456	0.295521
-7.734758	-2.018949	0.625600	0.001502	0.295433
-8.160827	-1.988743	0.630605	0.001581	0.295202
-7.919294	-2.052924	0.635610	0.001536	0.295102
-8.197021	-2.049209	0.640614	0.001588	0.294873
-8.268002	-2.053229	0.645619	0.001601	0.294790
-8.461201	-2.067847	0.650624	0.001637	0.294546
-8.056362	-2.159741	0.655629	0.001562	0.294456
-8.929330	-2.043139	0.660634	0.001724	0.294250
-8.867312	-2.066823	0.665638	0.001713	0.294189
-9.642474	-1.980277	0.670643	0.001857	0.293922
-9.655793	-1.974981	0.675648	0.001859	0.293936
-9.877643	-1.998194	0.680653	0.001901	0.293623
-10.103776	-1.955715	0.685658	0.001943	0.293630
-10.245098	-1.979021	0.690662	0.001969	0.293389
-10.592058	-1.934848	0.695667	0.002033	0.293296
-9.912922	-2.088585	0.700672	0.001907	0.293146
-10.218096	-2.064623	0.705677	0.001964	0.292991
-10.613550	-2.014602	0.710682	0.002037	0.292883
-10.777467	-2.028621	0.715686	0.002068	0.292667
-10.830113	-2.026164	0.720691	0.002078	0.292632
-11.118058	-2.031334	0.725696	0.002131	0.292347
-10.985525	-2.055940	0.730701	0.002107	0.292345
-11.370727	-2.043639	0.735706	0.002178	0.292059
-11.571649	-2.013112	0.740710	0.002216	0.292030
-11.728672	-2.020738	0.745715	0.002245	0.291851
-11.458111	-2.094350	0.750720	0.002194	0.291730
-11.834039	-2.050389	0.755725	0.002264	0.291609
-12.156330	-2.036883	0.760730	0.002324	0.291386
-12.095610	-2.047420	0.765734	0.002313	0.291388
-12.303990	-2.071465	0.770739	0.002352	0.291081
-12.329220	-2.066822	0.775744	0.002356	0.291081
-12.151928	-2.152620	0.780749	0.002323	0.290815
-12.506299	-2.099900	0.785754	0.002389	0.290757
-12.652059	-2.101598	0.790758	0.002416	0.290617
-13.035478	-2.052497	0.795763	0.002488	0.290514
-13.069685	-2.063318	0.800768	0.002494	0.290430
-13.762567	-1.985707	0.805773	0.002623	0.290189
-13.415979	-2.051714	0.810778	0.002558	0.290174
-13.689586	-2.057215	0.815782	0.002609	0.289899
-13.886445	-2.029053	0.820787	0.002646	0.289861
-14.377007	-1.967412	0.825792	0.002737	0.289723
-14.861223	-1.912876	0.830797	0.002827	0.289556
-14.082809	-2.059003	0.835802	0.002682	0.289533
-14.376223	-2.058556	0.840806	0.002737	0.289269
-15.017443	-1.944867	0.845811	0.002856	0.289255
-14.678224	-2.038938	0.850816	0.002793	0.289093
-15.618511	-1.900776	0.855821	0.002968	0.288929
-15.664209	-1.892366	0.860826	0.002977	0.288930
-15.549190	-1.961475	0.865830	0.002955	0.288688
-15.694737	-1.951075	0.870835	0.002982	0.288608
-15.496335	-2.001642	0.875840	0.002945	0.288535
-16.067784	-1.945409	0.880845	0.003052	0.288296
-15.902005	-1.975502	0.885850	0.003021	0.288297
-16.124457	-1.968711	0.890854	0.003062	0.288128
-16.968379	-1.838546	0.895859	0.003219	0.288011
-16.594105	-1.904718	0.900864	0.003149	0.288021
-16.658333	-1.950337	0.905869	0.003161	0.287733
-17.159565	-1.873169	0.910874	0.003255	0.287663
-16.765748	-1.950374	0.915878	0.003181	0.287635
-17.394409	-1.890282	0.920883	0.003298	0.287362
-17.217839	-1.923133	0.925888	0.003265	0.287359
-17.601475	-1.869993	0.930893	0.003337	0.287275
-17.038693	-2.025362	0.935898	0.003232	0.287008
-16.758575	-2.077123	0.940902	0.003180	0.287004
-17.708419	-1.949820	0.945907	0.003357	0.286775
-17.581572	-1.981513	0.950912	0.003333	0.286732
-17.522137	-2.008272	0.955917	0.003322	0.286652
-17.912481	-1.990252	0.960922	0.003394	0.286384
-17.722520	-2.022558	0.965926	0.003359	0.286396
-18.306711	-1.956105	0.970931	0.003468	0.286195
-18.477739	-1.944726	0.975936	0.003500	0.286095
-18.416921	-1.957040	0.980941	0.003488	0.286089
-18.507619	-2.003158	0.985946	0.003505	0.285773
-18.634365	-1.978758	0.990950	0.003529	0.285780
-19.623797	-1.811689	0.995955	0.003713	0.285715
-19.191386	-1.925682	1.000960	0.003632	0.285536
-18.753575	-2.008584	1.005965	0.003551	0.285519
-19.480252	-1.916185	1.010970	0.003686	0.285318
-19.983495	-1.846618	1.015974	0.003780	0.285207
-19.361033	-1.964642	1.020979	0.003664	0.285183
-20.261256	-1.845497	1.025984	0.003831	0.284957
-20.130233	-1.885657	1.030989	0.003807	0.284874
-20.198133	-1.871806	1.035994	0.003819	0.284882
-20.040311	-1.960243	1.040998	0.003790	0.284578
-20.242534	-1.932111	1.046003	0.003828	0.284534
-20.950493	-1.805785	1.051008	0.003959	0.284522
-20.731603	-1.893953	1.056013	0.003919	0.284276
-20.742852	-1.896015	1.061018	0.003921	0.284256
-20.312497	-2.000830	1.066022	0.003841	0.284121
-20.798142	-1.953343	1.071027	0.003931	0.283913
-21.056511	-1.901950	1.076032	0.003979	0.283936
-21.518488	-1.859534	1.081037	0.004065	0.283724
-21.736114	-1.837671	1.086042	0.004105	0.283634
-21.539427	-1.873443	1.091046	0.004069	0.283634
-22.100389	-1.825170	1.096051	0.004173	0.283360
-21.934601	-1.867091	1.101056	0.004142	0.283300
-21.969312	-1.859711	1.106061	0.004149	0.283305
-22.030967	-1.902928	1.111066	0.004160	0.283027
-22.098984	-1.894887	1.116070	0.004173	0.283005
-21.961770	-1.931961	1.121075	0.004147	0.282943
-22.146839	-1.952701	1.126080	0.004182	0.282665
-22.737321	-1.844059	1.131085	0.004291	0.282672
-22.777094	-1.861082	1.136090	0.004299	0.282548
-22.893862	-1.874891	1.141094	0.004321	0.282369
-23.207110	-1.819690	1.146099	0.004379	0.282360
-22.961744	-1.899282	1.151104	0.004333	0.282181
-23.372597	-1.852788	1.156109	0.004410	0.282036
-23.654392	-1.801817	1.161114	0.004462	0.282035
-23.114580	-1.936634	1.166118	0.004362	0.281847
-23.270515	-1.933433	1.171123	0.004391	0.281718
-23.436478	-1.900249	1.176128	0.004421	0.281733
-24.336880	-1.797304	1.181133	0.004589	0.281421
-23.681283	-1.923013	1.186138	0.004467	0.281388
-23.368189	-1.990963	1.191142	0.004409	0.281331
-23.794785	-1.961650	1.196147	0.004488	0.281083
-23.844464	-1.953548	1.201152	0.004497	0.281079
-23.719349	-2.014366	1.206157	0.004474	0.280883
-23.593975	-2.064608	1.211162	0.004451	0.280741
-23.497536	-2.092973	1.216166	0.004433	0.280686
-24.078363	-2.020476	1.221171	0.004541	0.280515
-24.204957	-1.994478	1.226176	0.004564	0.280531
-24.616682	-1.971938	1.231181	0.004641	0.280261
-24.971536	-1.921420	1.236186	0.004707	0.280189
-24.808679	-1.958615	1.241190	0.004676	0.280150
-25.029663	-1.974681	1.246195	0.004718	0.279859
-24.560811	-2.060337	1.251200	0.004630	0.279857
-24.745551	-2.068412	1.256205	0.004665	0.279642
-25.433446	-1.963273	1.261210	0.004793	0.279539
-25.440108	-1.970019	1.266214	0.004794	0.279498
-25.776395	-1.956596	1.271219	0.004856	0.279251
-25.287946	-2.046054	1.276224	0.004765	0.279247
-25.690316	-2.010928	1.281229	0.004840	0.279050
-27.024077	-1.790314	1.286234	0.005088	0.278937
-26.141408	-1.950936	1.291238	0.004924	0.278936
-26.456230	-1.947614	1.296243	0.004983	0.278657
-26.353349	-1.977018	1.301248	0.004964	0.278601
-26.503573	-1.962599	1.306253	0.004991	0.278534
-26.716973	-1.971092	1.311258	0.005031	0.278289
-26.840414	-1.947761	1.316262	0.005054	0.278293
-27.393802	-1.877597	1.321267	0.005157	0.278135
-27.265431	-1.925512	1.326272	0.005133	0.278007
-27.550655	-1.871912	1.331277	0.005186	0.278017
-27.882458	-1.865302	1.336282	0.005248	0.277737
-27.925044	-1.868275	1.341286	0.005256	0.277681
-27.986224	-1.858198	1.346291	0.005267	0.277676
-28.248352	-1.866801	1.351296	0.005316	0.277383
-28.009273	-1.914680	1.356301	0.005271	0.277360
-28.373039	-1.857533	1.361306	0.005339	0.277313
-28.720273	-1.845171	1.366310	0.005404	0.277048
-28.525442	-1.884275	1.371315	0.005367	0.277029
-27.923737	-2.016916	1.376320	0.005255	0.276908
-28.639618	-1.919546	1.381325	0.005389	0.276736
-29.049898	-1.843633	1.386330	0.005465	0.276743
-28.620042	-1.962957	1.391334	0.005385	0.276528
-28.862748	-1.944267	1.396339	0.005430	0.276395
-29.151721	-1.887750	1.401344	0.005484	0.276416
-29.453882	-1.892284	1.406349	0.005540	0.276105
-29.370016	-1.909935	1.411354	0.005524	0.276092
-29.412163	-1.914829	1.416358	0.005532	0.276027
-30.056446	-1.843118	1.421363	0.005652	0.275788
-29.159243	-2.009592	1.426368	0.005485	0.275771
-29.708229	-1.934004	1.431373	0.005587	0.275644
-30.636357	-1.783745	1.436378	0.005760	0.275547
-29.890399	-1.917989	1.441382	0.005621	0.275555
-30.560161	-1.851501	1.446387	0.005746	0.275264
-31.127363	-1.756811	1.451392	0.005851	0.275220
-30.444784	-1.883909	1.456397	0.005724	0.275204
-30.889223	-1.859766	1.461402	0.005807	0.274906
-31.122913	-1.817613	1.466406	0.005850	0.274904
-30.522217	-1.944550	1.471411	0.005738	0.274811
-30.017408	-2.089963	1.476416	0.005645	0.274529
-30.310021	-2.034020	1.481421	0.005699	0.274544
-31.537419	-1.853856	1.486426	0.005927	0.274317
-30.868207	-1.986626	1.491430	0.005803	0.274259
-31.400340	-1.898495	1.496435	0.005902	0.274213
-31.318252	-1.969655	1.501440	0.005886	0.273916
-31.483323	-1.938558	1.506445	0.005917	0.273922
-31.721407	-1.928622	1.511450	0.005961	0.273746
-32.261683	-1.851108	1.516454	0.006062	0.273636
-32.080176	-1.887481	1.521459	0.006028	0.273619
-32.097616	-1.935965	1.526464	0.006031	0.273346
-32.223395	-1.922024	1.531469	0.006055	0.273298
-32.562859	-1.873001	1.536474	0.006118	0.273231
-32.330889	-1.955954	1.541478	0.006075	0.273015
-32.818390	-1.866586	1.546483	0.006165	0.273019
-33.165961	-1.836711	1.551488	0.006230	0.272843
-33.194660	-1.862660	1.556493	0.006235	0.272677
-32.622172	-1.969287	1.561498	0.006129	0.272664
-33.335458	-1.885429	1.566502	0.006262	0.272421
-33.798111	-1.812811	1.571507	0.006348	0.272360
-33.112047	-1.945512	1.576512	0.006220	0.272318
-33.185334	-1.985187	1.581517	0.006234	0.272036
-33.468486	-1.937665	1.586522	0.006286	0.272015
-33.578105	-1.946700	1.591526	0.006307	0.271861
-33.867251	-1.917794	1.596531	0.006360	0.271735
-33.667053	-1.953740	1.601536	0.006323	0.271738
-34.154494	-1.924643	1.606541	0.006414	0.271420
-34.561673	-1.851632	1.611546	0.006489	0.271415
-34.286258	-1.919716	1.616550	0.006438	0.271319
-34.724844	-1.879975	1.621555	0.006520	0.271106
-34.428138	-1.934582	1.626560	0.006465	0.271103
-34.335775	-1.990633	1.631565	0.006447	0.270893
-35.179586	-1.858397	1.636570	0.006604	0.270780
-34.755149	-1.937724	1.641574	0.006525	0.270769
-34.614699	-2.010216	1.646579	0.006499	0.270518
-34.883496	-1.960465	1.651584	0.006549	0.270522
-35.444524	-1.893301	1.656589	0.006654	0.270336
-35.358095	-1.939785	1.661594	0.006637	0.270171
-34.900325	-2.025126	1.666598	0.006552	0.270160
-35.673082	-1.940840	1.671603	0.006696	0.269859
-35.800320	-1.916307	1.676608	0.006720	0.269866
-35.542045	-1.994083	1.681613	0.006672	0.269701
-36.159598	-1.913097	1.686618	0.006786	0.269533
-36.239916	-1.895421	1.691622	0.006801	0.269550
-36.199083	-1.953853	1.696627	0.006794	0.269276
-36.895504	-1.828713	1.701632	0.006923	0.269268
-37.081750	-1.803235	1.706637	0.006958	0.269223
-36.891344	-1.895010	1.711642	0.006922	0.268916
-36.620840	-1.941211	1.716646	0.006872	0.268932
-37.149757	-1.873737	1.721651	0.006971	0.268778
-36.906755	-1.951525	1.726656	0.006925	0.268597
-36.473133	-2.031366	1.731661	0.006845	0.268592
-37.814155	-1.841492	1.736666	0.007094	0.268300
-37.851341	-1.834057	1.741670	0.007101	0.268304
-37.664583	-1.883224	1.746675	0.007066	0.268222
-37.806848	-1.897105	1.751680	0.007093	0.268008
-38.278974	-1.808836	1.756685	0.007180	0.268021
-38.742351	-1.753810	1.761690	0.007267	0.267863
-38.828667	-1.768432	1.766694	0.007283	0.267699
-39.126597	-1.714803	1.771699	0.007338	0.267696
-38.994064	-1.765167	1.776704	0.007313	0.267555
-38.535466	-1.885173	1.781709	0.007228	0.267357
-38.344368	-1.924181	1.786714	0.007192	0.267334
-38.610764	-1.920505	1.791718	0.007242	0.267091
-38.834923	-1.893822	1.796723	0.007284	0.267015
-38.282061	-2.010778	1.801728	0.007181	0.266927
-38.926160	-1.929527	1.806733	0.007301	0.266732
-39.211472	-1.877079	1.811738	0.007354	0.266735
-38.622695	-2.030335	1.816742	0.007244	0.266485
-39.304342	-1.921539	1.821747	0.007371	0.266402
-39.582580	-1.885987	1.826752	0.007423	0.266321
-39.593679	-1.925188	1.831757	0.007425	0.266096
-40.149921	-1.822040	1.836762	0.007528	0.266107
-40.058036	-1.872445	1.841766	0.007511	0.265924
-39.919597	-1.926235	1.846771	0.007485	0.265769
-39.714753	-1.966591	1.851776	0.007447	0.265752
-40.196629	-1.921785	1.856781	0.007537	0.265519
-40.280422	-1.908892	1.861786	0.007552	0.265506
-40.360610	-1.922812	1.866790	0.007567	0.265351
-40.668733	-1.900366	1.871795	0.007625	0.265167
-40.891563	-1.858807	1.876800	0.007666	0.265173
-41.032078	-1.884312	1.881805	0.007692	0.264894
-40.764556	-1.941099	1.886810	0.007642	0.264850
-41.005896	-1.917712	1.891814	0.007687	0.264738
-40.988528	-1.963545	1.896819	0.007684	0.264505
-40.708504	-2.014363	1.901824	0.007632	0.264506
-40.775444	-2.052090	1.906829	0.007644	0.264233
-41.476979	-1.925570	1.911834	0.007775	0.264227
-41.030846	-2.041225	1.916838	0.007692	0.264038
-41.528053	-1.978539	1.921843	0.007784	0.263886
-42.094843	-1.878084	1.926848	0.007890	0.263871
-41.792160	-1.984208	1.931853	0.007833	0.263591
-41.899021	-1.965706	1.936858	0.007853	0.263586
-42.304559	-1.927336	1.941862	0.007929	0.263392
-42.395718	-1.933658	1.946867	0.007946	0.263266
-42.339760	-1.951441	1.951872	0.007935	0.263225
-42.322094	-1.999970	1.956877	0.007932	0.262975
-42.835460	-1.906927	1.961882	0.008027	0.262974
-42.603231	-1.988717	1.966886	0.007984	0.262756
-42.972288	-1.944904	1.971891	0.008053	0.262628
-42.783643	-1.993952	1.976896	0.008018	0.262547
-42.650650	-2.061859	1.981901	0.007993	0.262306
-42.383727	-2.112228	1.986906	0.007943	0.262296
-42.641615	-2.121535	1.991910	0.007991	0.261985
-43.242232	-2.013950	1.996915	0.008103	0.261976
-43.364404	-2.032894	2.001920	0.008126	0.261749

-43.812833	-1.992555	2.011917	0.008209	0.261521
-43.986125	-1.990844	2.021914	0.008241	0.261356
-44.220324	-2.001235	2.031910	0.008285	0.261063
-44.065386	-2.052164	2.041907	0.008256	0.260937
-44.241985	-2.056447	2.051904	0.008289	0.260735
-45.032250	-1.922820	2.061901	0.008436	0.260679
-45.120777	-1.937873	2.071898	0.008452	0.260507
-45.152373	-1.932907	2.081894	0.008458	0.260503
-44.632023	-2.052631	2.091891	0.008361	0.260364
-45.050650	-2.015000	2.101888	0.008439	0.260150
-45.232708	-1.980874	2.111885	0.008473	0.260156
-45.105795	-2.004725	2.121882	0.008449	0.260152
-45.080547	-2.008998	2.131878	0.008444	0.260154
-45.085543	-2.039728	2.141875	0.008445	0.259978
-45.407461	-2.006315	2.151872	0.008505	0.259839
-45.774927	-1.938355	2.161869	0.008573	0.259845
-45.199202	-2.045748	2.171866	0.008466	0.259831
-45.383736	-2.012613	2.181862	0.008500	0.259829
-45.102961	-2.038051	2.191859	0.008448	0.259972
-44.972702	-2.030261	2.201856	0.008424	0.260148
-45.218505	-1.984696	2.211853	0.008469	0.260153
-45.094211	-2.007910	2.221850	0.008446	0.260150
-45.191468	-1.988899	2.231846	0.008464	0.260158
-45.478936	-1.936860	2.241843	0.008517	0.260157
-45.007021	-2.013367	2.251840	0.008430	0.260209
-44.767624	-2.005829	2.261837	0.008385	0.260494
-44.875879	-1.984893	2.271834	0.008405	0.260501
-45.152821	-1.933048	2.281830	0.008456	0.260510
-44.756036	-1.980749	2.291827	0.008382	0.260646
-44.484798	-2.012387	2.301824	0.008332	0.260745
-45.011938	-1.915152	2.311821	0.008430	0.260753
-44.177810	-2.020403	2.321818	0.008275	0.261011
-44.341559	-1.981587	2.331814	0.008305	0.261062
-44.399769	-1.953683	2.341811	0.008316	0.261158
-44.199195	-1.950842	2.351808	0.008278	0.261377
-43.709759	-2.042387	2.361805	0.008187	0.261363
-43.543672	-2.011922	2.371802	0.008156	0.261700
-43.740387	-1.976049	2.381798	0.008193	0.261701
-43.323334	-2.009121	2.391795	0.008115	0.261938
-43.321962	-2.000622	2.401792	0.008115	0.261987
-42.909331	-2.031015	2.411789	0.008038	0.262234
-43.264313	-1.950179	2.421786	0.008104	0.262324
-43.084446	-1.933202	2.431782	0.008070	0.262599
-42.840330	-1.964197	2.441779	0.008025	0.262673
-42.451228	-1.980898	2.451776	0.007952	0.262972
-42.311742	-1.993013	2.461773	0.007926	0.263045
-42.266473	-1.962154	2.471770	0.007918	0.263261
-41.802322	-2.015405	2.481766	0.007831	0.263432
-41.806963	-1.987331	2.491763	0.007832	0.263582
-41.870779	-1.925818	2.501760	0.007844	0.263857
-41.668814	-1.938181	2.511757	0.007806	0.263991
-41.863177	-1.855988	2.521754	0.007842	0.264248
-40.848124	-2.003425	2.531750	0.007653	0.264453
-41.281705	-1.895028	2.541747	0.007734	0.264615
-40.566374	-1.983840	2.551744	0.007600	0.264841
-40.366876	-1.980778	2.561741	0.007563	0.265056
-40.256183	-1.974089	2.571738	0.007542	0.265203
-39.762862	-2.011206	2.581734	0.007451	0.265491
-39.501729	-2.031669	2.591731	0.007402	0.265639
-39.847090	-1.942594	2.601728	0.007466	0.265782
-39.293137	-1.987327	2.611725	0.007363	0.266088
-39.096710	-1.995248	2.621722	0.007326	0.266240
-39.193647	-1.943896	2.631718	0.007344	0.266423
-39.095258	-1.903098	2.641715	0.007326	0.266743
-38.551524	-1.966217	2.651712	0.007224	0.266937
-38.066931	-2.027874	2.661709	0.007134	0.267081
-38.210338	-1.955972	2.671706	0.007161	0.267330
-37.534713	-2.031523	2.681702	0.007035	0.267587
-37.560393	-1.993748	2.691699	0.007040	0.267766
-37.107798	-2.035343	2.701696	0.006955	0.267987
-36.852744	-2.036212	2.711693	0.006908	0.268233
-37.216587	-1.937182	2.721690	0.006975	0.268411
-36.819498	-1.970655	2.731686	0.006901	0.268620
-36.826778	-1.912875	2.741683	0.006903	0.268925
-36.414144	-1.943245	2.751680	0.006826	0.269165
-36.315339	-1.919156	2.761677	0.006807	0.269392
-35.632459	-2.017464	2.771674	0.006680	0.269532
-35.297883	-2.018389	2.781670	0.006618	0.269854
-35.281241	-1.983551	2.791667	0.006614	0.270057
-35.450839	-1.908364	2.801664	0.006646	0.270295
-34.612037	-2.019760	2.811661	0.006490	0.270516
-34.467532	-2.004178	2.821658	0.006463	0.270740
-34.482303	-1.965472	2.831654	0.006465	0.270933
-34.131148	-1.989967	2.841651	0.006400	0.271144
-33.989540	-1.967629	2.851648	0.006373	0.271401
-33.353359	-2.034025	2.861645	0.006255	0.271665
-33.996250	-1.876245	2.871642	0.006374	0.271883
-33.031752	-2.014673	2.881638	0.006195	0.272080
-32.720192	-2.022602	2.891635	0.006137	0.272340
-32.415454	-2.031444	2.901632	0.006080	0.272588
-32.317748	-2.011767	2.911629	0.006062	0.272787
-31.925084	-2.046505	2.921626	0.005989	0.272982
-31.551945	-2.059193	2.931622	0.005919	0.273275
-31.676627	-1.999180	2.941619	0.005942	0.273473
-31.070663	-2.074934	2.951616	0.005829	0.273655
-31.266656	-1.990420	2.961613	0.005866	0.273914
-30.946700	-1.995266	2.971610	0.005806	0.274196
-30.523386	-2.037106	2.981606	0.005727	0.274382
-30.497731	-2.002076	2.991603	0.005722	0.274592
-29.922142	-2.056429	3.001600	0.005615	0.274858
-29.836643	-2.026900	3.011597	0.005599	0.275095
-29.726830	-2.005748	3.021594	0.005578	0.275312
-29.084116	-2.083935	3.031590	0.005459	0.275516
-29.317627	-1.994044	3.041587	0.005502	0.275766
-28.922363	-2.023006	3.051584	0.005428	0.275991
-29.143540	-1.939261	3.061581	0.005469	0.276220
-28.772429	-1.964576	3.071578	0.005400	0.276441
-28.465125	-1.965187	3.081574	0.005343	0.276731
-27.902138	-2.021592	3.091571	0.005238	0.276972
-27.681320	-2.022249	3.101568	0.005197	0.277178
-27.587947	-1.996737	3.111565	0.005179	0.277401
-27.433137	-1.976420	3.121562	0.005151	0.277654
-27.134159	-1.969367	3.131558	0.005095	0.277974
-27.362799	-1.885341	3.141555	0.005137	0.278196
-27.196560	-1.863674	3.151552	0.005106	0.278466
-26.679072	-1.913308	3.161549	0.005010	0.278697
-25.785794	-2.036751	3.171546	0.004843	0.278900
-25.431138	-2.042911	3.181542	0.004777	0.279203
-26.160262	-1.865818	3.191539	0.004913	0.279434
-25.806102	-1.881054	3.201536	0.004847	0.279689
-25.468405	-1.896875	3.211533	0.004784	0.279926
-25.203644	-1.892481	3.221530	0.004735	0.280197
-25.203450	-1.828217	3.231526	0.004734	0.280530
-24.525507	-1.914877	3.241523	0.004608	0.280719
-24.319152	-1.913064	3.251520	0.004570	0.280922
-24.207598	-1.884214	3.261517	0.004549	0.281176
-23.719017	-1.930458	3.271514	0.004458	0.281395
-23.041919	-1.993671	3.281510	0.004332	0.281704
-22.847348	-1.992276	3.291507	0.004295	0.281893
-22.676122	-1.983478	3.301504	0.004263	0.282098
-22.079769	-2.049696	3.311501	0.004152	0.282315
-21.978635	-2.013719	3.321498	0.004133	0.282594
-21.934444	-1.980299	3.331494	0.004125	0.282807
-21.403990	-2.036779	3.341491	0.004026	0.283012
-21.184180	-2.027027	3.351488	0.003985	0.283266
-21.371800	-1.945051	3.361485	0.004020	0.283511
-21.013932	-1.964876	3.371482	0.003953	0.283742
-21.073916	-1.908693	3.381478	0.003964	0.283974
-20.208912	-2.014433	3.391475	0.003803	0.284237
-19.855670	-2.034482	3.401472	0.003737	0.284462
-19.825448	-2.003037	3.411469	0.003732	0.284650
-19.717034	-1.978547	3.421466	0.003711	0.284875
-19.759133	-1.911373	3.431462	0.003719	0.285178
-19.375416	-1.925857	3.441459	0.003648	0.285459
-19.011324	-1.954426	3.451456	0.003580	0.285650
-18.438359	-2.030256	3.461453	0.003473	0.285794
-18.523472	-1.957734	3.471450	0.003489	0.286083
-18.112354	-1.984955	3.481446	0.003412	0.286323
-18.175174	-1.926805	3.491443	0.003424	0.286560
-18.098960	-1.889913	3.501440	0.003410	0.286817
-17.445513	-1.970435	3.511437	0.003288	0.287010
-17.282775	-1.939593	3.521434	0.003257	0.287315
-17.038934	-1.941467	3.531430	0.003212	0.287529
-16.514748	-1.993664	3.541427	0.003114	0.287746
-15.969181	-2.047386	3.551424	0.003013	0.287975
-15.710375	-2.045663	3.561421	0.002964	0.288221
-15.645865	-2.020744	3.571418	0.002952	0.288405
-15.247793	-2.057656	3.581414	0.002878	0.288583
-14.743540	-2.088438	3.591411	0.002784	0.288889
-14.973179	-2.010456	3.601408	0.002827	0.289071
-14.601868	-2.037784	3.611405	0.002758	0.289272
-14.448589	-2.015607	3.621402	0.002729	0.289523
-13.914336	-2.067801	3.631398	0.002629	0.289748
-13.769219	-2.057801	3.641395	0.002602	0.289930
-13.551306	-2.048304	3.651392	0.002562	0.290175
-13.185054	-2.058606	3.661389	0.002493	0.290456
-12.966515	-2.069741	3.671386	0.002453	0.290599
-12.381059	-2.145122	3.681382	0.002344	0.290754
-12.479029	-2.069560	3.691379	0.002362	0.291041
-12.483691	-2.032691	3.701376	0.002363	0.291221
-11.871767	-2.109817	3.711373	0.002249	0.291391
-12.026292	-2.014730	3.721370	0.002277	0.291724
-12.022396	-1.975119	3.731366	0.002276	0.291924
-11.322122	-2.063878	3.741363	0.002146	0.292115
-11.161693	-2.047780	3.751360	0.002116	0.292340
-10.764496	-2.063485	3.761357	0.002042	0.292620
-10.938533	-1.990231	3.771354	0.002074	0.292826
-10.442485	-2.039529	3.781350	0.001982	0.293028
-10.265666	-2.020030	3.791347	0.001949	0.293283
-9.812322	-2.055457	3.801344	0.001864	0.293515
-9.632789	-2.047057	3.811341	0.001831	0.293718
-9.381857	-2.054558	3.821338	0.001784	0.293906
-8.927986	-2.075537	3.831334	0.001699	0.294209
-8.883223	-2.047542	3.841331	0.001691	0.294387
-8.520372	-2.081184	3.851328	0.001623	0.294546
-8.274593	-2.064478	3.861325	0.001578	0.294848
-8.150383	-2.043064	3.871322	0.001554	0.295064
-8.062118	-2.019617	3.881318	0.001538	0.295258
-7.787495	-2.017572	3.891315	0.001487	0.295513
-8.095006	-1.911720	3.901312	0.001544	0.295758
-7.978123	-1.883159	3.911309	0.001522	0.296002
-7.511284	-1.921218	3.921306	0.001435	0.296231
-7.530930	-1.865920	3.931302	0.001438	0.296484
-7.309640	-1.851503	3.941299	0.001397	0.296751
-6.698395	-1.910130	3.951296	0.001283	0.297007
-6.713556	-1.852640	3.961293	0.001286	0.297274
-6.323872	-1.874507	3.971290	0.001213	0.297512
-5.992256	-1.885104	3.981286	0.001152	0.297754
-5.849749	-1.858903	3.991283	0.001125	0.298008
-5.496627	-1.867409	4.001280	0.001059	0.298278
-5.431090	-1.825599	4.011277	0.001047	0.298539
-5.278244	-1.799550	4.021274	0.001018	0.298800
-5.236050	-1.755059	4.031270	0.001010	0.299053
-5.139428	-1.716160	4.041267	0.000992	0.299326
-4.827373	-1.720557	4.051264	0.000934	0.299580
-4.893889	-1.649119	4.061261	0.000946	0.299866
-4.677054	-1.625898	4.071258	0.000906	0.300169
-4.421093	-1.605743	4.081254	0.000858	0.300490
-4.381486	-1.564896	4.091251	0.000851	0.300722
-4.120586	-1.552432	4.101248	0.000802	0.301010
-4.379582	-1.443677	4.111245	0.000850	0.301307
-4.238621	-1.401130	4.121242	0.000824	0.301635
-3.834366	-1.412525	4.131238	0.000748	0.301933
-3.844471	-1.342036	4.141235	0.000750	0.302262
-3.515181	-1.333557	4.151232	0.000689	0.302589
-3.448721	-1.273404	4.161229	0.000676	0.302935
-2.927224	-1.304968	4.171226	0.000579	0.303237
-2.731581	-1.273262	4.181222	0.000542	0.303558
-2.986375	-1.155504	4.191219	0.000590	0.303898
-3.519741	-0.970427	4.201216	0.000689	0.304318
-3.752006	-0.849732	4.211213	0.000732	0.304692
-3.421258	-0.832124	4.221210	0.000670	0.305061
-2.537021	-0.912103	4.231206	0.000506	0.305443
-2.547944	-0.841247	4.241203	0.000508	0.305770
-1.955216	-0.868610	4.251200	0.000397	0.306150
-2.116289	-0.762373	4.261197	0.000427	0.306514
-1.325125	-0.833297	4.271194	0.000280	0.306858
-1.207126	-0.782637	4.281190	0.000258	0.307198
-1.504751	-0.647790	4.291187	0.000313	0.307579
-1.182256	-0.614508	4.301184	0.000253	0.308011
-1.550987	-0.465962	4.311181	0.000321	0.308394
-1.188931	-0.448730	4.321178	0.000254	0.308784
-0.943941	-0.410890	4.331174	0.000208	0.309170
-0.311621	-0.435995	4.341171	0.000090	0.309590
-0.523863	-0.311831	4.351168	0.000129	0.309990
0.010247	-0.323307	4.361165	0.000030	0.310389
-0.215511	-0.206668	4.371162	0.000072	0.310742
-0.099387	-0.131687	4.381158	0.000050	0.311189
0.000000	-0.064286	4.391155	0.000031	0.311587

0.054714	0.196687	4.396160	0.000021	0.312842
1.111868	0.573903	4.401165	-0.000176	0.315464
2.557193	1.176292	4.406170	-0.000446	0.319406
3.829777	2.104902	4.411174	-0.000683	0.324616
5.896029	3.199537	4.416179	-0.001069	0.331102
8.681393	4.464139	4.421184	-0.001588	0.338747
11.755282	6.005169	4.426189	-0.002162	0.347594
16.030856	7.660083	4.431194	-0.002959	0.357565
21.150889	9.505294	4.436198	-0.003913	0.368613
27.958265	11.416270	4.441203	-0.005182	0.380750
36.842927	13.343598	4.446208	-0.006838	0.393953
52.024325	14.565725	4.451213	-0.009665	0.408264
98.696218	10.675018	4.456218	-0.018353	0.424083
118.111349	12.464974	4.461222	-0.021970	0.441757
123.278041	17.304445	4.466227	-0.022935	0.460224
128.377503	22.557221	4.471232	-0.023888	0.479183
133.987931	28.140918	4.476237	-0.024936	0.498641
138.834864	34.270406	4.481242	-0.025843	0.518498
143.608116	40.777211	4.486246	-0.026736	0.538594
148.469985	47.654288	4.491251	-0.027646	0.558959
153.276166	54.895119	4.496256	-0.028545	0.579483
157.869107	62.514061	4.501261	-0.029405	0.600118
163.732248	70.222313	4.506266	-0.030502	0.620797
170.582735	78.081629	4.511270	-0.031783	0.641541
177.108366	86.314154	4.516275	-0.033003	0.662314
182.625444	94.968497	4.521280	-0.034036	0.682959
187.874492	103.909361	4.526285	-0.035020	0.703481
195.198231	112.695190	4.531290	-0.036389	0.723844
202.659500	121.686459	4.536294	-0.037784	0.744086
208.990454	131.048495	4.541299	-0.038969	0.764106
214.628474	140.680254	4.546304	-0.040025	0.783878
219.770591	150.505320	4.551309	-0.040989	0.803348
224.542055	160.479760	4.556314	-0.041884	0.822498
229.193662	170.528639	4.561318	-0.042757	0.841300
233.733011	180.622208	4.566323	-0.043609	0.859728
238.537629	190.675242	4.571328	-0.044510	0.877775
243.614762	200.698301	4.576333	-0.045462	0.895483
247.091183	210.996578	4.581338	-0.046116	0.912835
249.250369	221.439401	4.586342	-0.046525	0.929726
251.121333	231.886727	4.591347	-0.046880	0.946245
252.419947	242.309760	4.596352	-0.047129	0.962293
254.420029	252.521125	4.601357	-0.047508	0.977945
255.728231	262.794992	4.606362	-0.047758	0.993266
257.533753	272.822381	4.611366	-0.048101	1.008124
259.597720	282.723087	4.616371	-0.048492	1.022650
260.894248	292.664442	4.621376	-0.048740	1.036844
262.635085	302.430216	4.626381	-0.049070	1.050709
264.583282	312.076499	4.631386	-0.049439	1.064280
266.181395	321.698921	4.636390	-0.049743	1.077567
267.658471	331.261424	4.641395	-0.050024	1.090584
269.348218	340.683889	4.646400	-0.050345	1.103312
270.542127	350.138887	4.651405	-0.050574	1.115825
271.875282	359.465847	4.656410	-0.050828	1.128067
273.089098	368.734584	4.661414	-0.051060	1.140077
274.305366	377.961693	4.666419	-0.051293	1.151910
275.559685	387.073001	4.671424	-0.051532	1.163487
276.977013	396.108684	4.676429	-0.051802	1.174890
278.141190	405.136008	4.681434	-0.052025	1.186121
279.696283	414.018010	4.686438	-0.052320	1.197151
280.644136	422.986645	4.691443	-0.052503	1.208060
282.023861	431.815214	4.696448	-0.052765	1.218792
283.348914	440.620241	4.701453	-0.053018	1.229392
284.684309	449.382136	4.706458	-0.053272	1.239852
285.524861	458.176690	4.711462	-0.053434	1.250165
286.860105	466.869335	4.716467	-0.053689	1.260372
287.848290	475.579831	4.721472	-0.053878	1.270451
288.745997	484.257221	4.726477	-0.054051	1.280396
290.117639	492.827741	4.731482	-0.054312	1.290233
291.125426	501.446935	4.736486	-0.054506	1.299982
292.268037	510.056483	4.741491	-0.054724	1.309672
293.076802	518.688505	4.746496	-0.054880	1.319253
294.221788	527.173486	4.751501	-0.055099	1.328667
295.145422	535.696358	4.756506	-0.055277	1.338015
295.869010	544.202934	4.761510	-0.055417	1.347245
297.120654	552.626467	4.766515	-0.055656	1.356417
297.666591	561.140602	4.771520	-0.055763	1.365499
298.859420	569.526789	4.776525	-0.055990	1.374499
299.709701	577.966735	4.781530	-0.056154	1.383436
300.533781	586.407396	4.786534	-0.056313	1.392313
301.560667	594.771681	4.791539	-0.056510	1.401088
302.645261	603.123303	4.796544	-0.056717	1.409806
303.563168	611.500857	4.801549	-0.056894	1.418468
304.521450	619.870231	4.806554	-0.057078	1.427075
305.427009	628.220253	4.811558	-0.057252	1.435602
306.355281	636.570927	4.816563	-0.057430	1.444083
306.792636	644.999906	4.821568	-0.057517	1.452512
307.315304	653.380656	4.826573	-0.057620	1.460858
308.148638	661.714688	4.831578	-0.057781	1.469160
308.727508	670.086165	4.836582	-0.057894	1.477412
309.725131	678.308262	4.841587	-0.058085	1.485539
310.339979	686.640264	4.846592	-0.058205	1.493667
311.184401	694.920264	4.851597	-0.058368	1.501737
311.832494	703.237336	4.856602	-0.058494	1.509769
312.318018	711.549062	4.861606	-0.058590	1.517727
313.022965	719.820266	4.866611	-0.058726	1.525640
313.546167	728.130764	4.871616	-0.058829	1.533520
314.002054	736.437356	4.876621	-0.058919	1.541346
314.827974	744.674025	4.881626	-0.059079	1.549123
315.501793	752.901478	4.886630	-0.059210	1.556829
316.511730	761.078402	4.891635	-0.059403	1.564501
316.846089	769.397953	4.896640	-0.059471	1.572166
317.287196	777.668325	4.901645	-0.059558	1.579764
317.879011	785.919067	4.906650	-0.059674	1.587330
318.769988	794.086649	4.911654	-0.059845	1.594829
319.578996	802.290057	4.916659	-0.060001	1.602312
320.010185	810.564467	4.921664	-0.060087	1.609770
320.710404	818.786617	4.926669	-0.060223	1.617184
320.865415	827.089701	4.931674	-0.060257	1.624559
321.189428	835.371218	4.936678	-0.060323	1.631906
321.664745	843.590344	4.941683	-0.060417	1.639186
322.367209	851.725091	4.946688	-0.060553	1.646391
323.347907	859.865060	4.951693	-0.060741	1.653608
323.761450	868.106230	4.956698	-0.060823	1.660803
324.103476	876.338783	4.961702	-0.060892	1.667949
324.555544	884.553511	4.966707	-0.060982	1.675064
325.628482	892.619747	4.971712	-0.061187	1.682107
326.206096	900.826302	4.976717	-0.061300	1.689172
327.014961	908.995489	4.981722	-0.061456	1.696207
327.230708	917.243978	4.986726	-0.061501	1.703200
328.194976	925.377404	4.991731	-0.061686	1.710168
328.650738	933.577419	4.996736	-0.061776	1.717095
329.332474	941.721100	5.001741	-0.061909	1.723977
329.660074	949.965628	5.006746	-0.061975	1.730869
329.961845	958.179785	5.011750	-0.062037	1.737705
330.611453	966.318368	5.016755	-0.062163	1.744497
331.381038	974.452853	5.021760	-0.062312	1.751275
332.039829	982.617689	5.026765	-0.062440	1.758036
332.178429	990.848919	5.031770	-0.062471	1.764760
332.597813	999.038025	5.036774	-0.062554	1.771459
333.158249	1007.204488	5.041779	-0.062664	1.778132
333.781119	1015.332700	5.046784	-0.062785	1.784758
334.185535	1023.546775	5.051789	-0.062866	1.791400
334.977416	1031.666076	5.056794	-0.063019	1.797989
335.421699	1039.792326	5.061798	-0.063107	1.804517
336.131954	1047.931705	5.066803	-0.063245	1.811065
336.575568	1056.091679	5.071808	-0.063332	1.817572
336.571365	1064.321759	5.076813	-0.063337	1.824057
337.786166	1072.358434	5.081818	-0.063569	1.830515
337.815997	1080.572875	5.086822	-0.063580	1.836945
338.736047	1088.652699	5.091827	-0.063756	1.843355
339.599498	1096.735421	5.096832	-0.063922	1.849738
340.533081	1104.826036	5.101837	-0.064101	1.856114
341.139013	1112.988091	5.106842	-0.064220	1.862483
341.979119	1121.109076	5.111846	-0.064381	1.868827
342.058381	1129.347438	5.116851	-0.064401	1.875149
342.458080	1137.487193	5.121856	-0.064481	1.881413
343.141929	1145.603330	5.126861	-0.064614	1.887671
343.867750	1153.726643	5.131866	-0.064754	1.893918
344.548020	1161.817393	5.136870	-0.064886	1.900114
344.683910	1170.052106	5.141875	-0.064917	1.906336
345.511193	1178.123874	5.146880	-0.065076	1.912494
345.797855	1186.298474	5.151885	-0.065135	1.918648
346.118042	1194.445515	5.156890	-0.065200	1.924766
346.525177	1202.578959	5.161894	-0.065281	1.930863
346.996344	1210.726305	5.166899	-0.065374	1.936959
347.761567	1218.774666	5.171904	-0.065522	1.942995
348.121621	1226.953628	5.176909	-0.065595	1.949064
348.786406	1235.037720	5.181914	-0.065724	1.955077
349.020927	1243.176452	5.186918	-0.065773	1.961065
349.711577	1251.258422	5.191923	-0.065907	1.967042
350.154574	1259.392788	5.196928	-0.065994	1.973013
350.698645	1267.481944	5.201933	-0.066101	1.978943
351.335323	1275.587209	5.206938	-0.066225	1.984878
352.131930	1283.651193	5.211942	-0.066378	1.990781
352.500926	1291.812610	5.216947	-0.066453	1.996692
352.815912	1299.926145	5.221952	-0.066516	2.002545
353.374986	1308.048000	5.226957	-0.066626	2.008412
354.196877	1316.140864	5.231962	-0.066784	2.014270
354.531161	1324.257429	5.236966	-0.066852	2.020075
354.956966	1332.393366	5.241971	-0.066936	2.025887
355.888629	1340.433642	5.246976	-0.067115	2.031668
356.257776	1348.567276	5.251981	-0.067189	2.037439
356.748659	1356.657876	5.256986	-0.067286	2.043177
357.175420	1364.790213	5.261990	-0.067371	2.048920
357.660756	1372.908950	5.266995	-0.067467	2.054645
358.063648	1381.019548	5.272000	-0.067547	2.060338
358.611546	1389.093219	5.277005	-0.067654	2.066006
358.996937	1397.256146	5.282010	-0.067731	2.071703
359.252135	1405.355738	5.287014	-0.067784	2.077327
359.754469	1413.438489	5.292019	-0.067883	2.082949
360.546720	1421.489191	5.297024	-0.068036	2.088563
360.717393	1429.666343	5.302029	-0.068073	2.094186
361.447744	1437.707702	5.307034	-0.068214	2.099757
361.730582	1445.844671	5.312038	-0.068272	2.105334
362.589136	1453.904381	5.317043	-0.068437	2.110901
363.031250	1462.006467	5.322048	-0.068525	2.116440
363.619584	1470.069269	5.327053	-0.068640	2.121953
363.672726	1478.247904	5.332058	-0.068655	2.127477
364.179417	1486.305607	5.337062	-0.068755	2.132949
364.550641	1494.407170	5.342067	-0.068829	2.138424
364.959557	1502.510604	5.347072	-0.068911	2.143889
365.983658	1510.495480	5.352077	-0.069107	2.149320
366.199990	1518.651639	5.357082	-0.069152	2.154774
366.462464	1526.745594	5.362086	-0.069206	2.160178
367.032278	1534.815383	5.367091	-0.069318	2.165581
367.131272	1542.977481	5.372096	-0.069342	2.170987
367.528709	1551.059642	5.377101	-0.069421	2.176355
368.159784	1559.104337	5.382106	-0.069544	2.181706
368.582219	1567.177501	5.387110	-0.069628	2.187044
368.611904	1575.366348	5.392115	-0.069639	2.192408
369.432159	1583.357900	5.397120	-0.069797	2.197703
369.869262	1591.402243	5.402125	-0.069883	2.202984
370.423131	1599.491559	5.407130	-0.069992	2.208292
370.633604	1607.614776	5.412134	-0.070036	2.213578
371.200376	1615.685356	5.417139	-0.070147	2.218850
371.521766	1623.758034	5.422144	-0.070212	2.224088
371.599389	1631.910971	5.427149	-0.070232	2.229344
372.420302	1639.938951	5.432154	-0.070390	2.234574
372.714166	1648.024385	5.437158	-0.070450	2.239781
373.392537	1656.059136	5.442163	-0.070582	2.244977
374.176909	1664.115586	5.447168	-0.070733	2.250185
374.542859	1672.226852	5.452173	-0.070806	2.255378
374.915553	1680.334977	5.457178	-0.070881	2.260558
375.039540	1688.444785	5.462182	-0.070910	2.265705
375.528867	1696.553263	5.467187	-0.071006	2.270872
375.832783	1704.655988	5.472192	-0.071068	2.276007
376.433189	1712.652913	5.477197	-0.071185	2.281089
377.022013	1720.718017	5.482202	-0.071300	2.286202
377.118108	1728.825293	5.487206	-0.071323	2.291287
377.383204	1736.933584	5.492211	-0.071378	2.296377
377.771429	1744.990701	5.497216	-0.071455	2.301433
378.241352	1753.029455	5.502221	-0.071548	2.306474
378.400430	1761.165867	5.507226	-0.071583	2.311537
379.015703	1769.166798	5.512230	-0.071703	2.316545
379.628759	1777.209553	5.517235	-0.071822	2.321567
379.933230	1785.295918	5.522240	-0.071884	2.326579
380.390310	1793.373755	5.527245	-0.071975	2.331588
380.770278	1801.469632	5.532250	-0.072051	2.336591
381.389251	1809.483485	5.537254	-0.072171	2.341552
381.453152	1817.634513	5.542259	-0.072189	2.346541
381.938928	1825.687480	5.547264	-0.072284	2.351494
382.525966	1833.723753	5.552269	-0.072399	2.356434
382.966980	1841.788338	5.557274	-0.072486	2.361370
383.691881	1849.770356	5.562278	-0.072627	2.366268
384.392833	1857.842908	5.567283	-0.072762	2.371209
384.700942	1865.952896	5.572288	-0.072825	2.376130
384.908073	1874.050456	5.577293	-0.072869	2.381025
385.325044	1882.142850	5.582298	-0.072952	2.385923
385.702457	1890.205127	5.587302	-0.073027	2.390791
385.980736	1898.297130	5.592307	-0.073085	2.395658
386.514556	1906.313776	5.597312	-0.073189	2.400491
387.051506	1914.356482	5.602317	-0.073295	2.405329
387.679957	1922.432157	5.607322	-0.073417	2.410185
388.119030	1930.497432	5.612326	-0.073504	2.415009
388.567269	1938.608763	5.617331	-0.073593	2.419852
389.082403	1946.656964	5.622336	-0.073694	2.424653
389.269792	1954.751460	5.627341	-0.073734	2.429446
389.847603	1962.833946	5.632346	-0.073847	2.434253
390.255188	1970.868690	5.637350	-0.073928	2.439009
390.616034	1978.926101	5.642355	-0.074001	2.443766
391.090001	1986.984800	5.647360	-0.074094	2.448522
391.409304	1995.062486	5.652365	-0.074159	2.453269
391.845039	2003.116080	5.657370	-0.074245	2.458001
391.861530	2011.204587	5.662374	-0.074254	2.462712
392.631374	2019.212505	5.667379	-0.074402	2.467424
393.138299	2027.278477	5.672384	-0.074502	2.472142
393.299130	2035.363336	5.677389	-0.074537	2.476835
393.758597	2043.425200	5.682394	-0.074628	2.481528
393.927672	2051.490091	5.687398	-0.074665	2.486192
394.235120	2059.571508	5.692403	-0.074727	2.490867
394.706446	2067.606228	5.697408	-0.074820	2.495519
395.230968	2075.651800	5.702413	-0.074923	2.500172
395.697311	2083.703047	5.707418	-0.075016	2.504815
395.966807	2091.796917	5.712422	-0.075071	2.509460
396.309807	2099.878113	5.717427	-0.075140	2.514094
396.626271	2107.906506	5.722432	-0.075204	2.518687
397.121546	2115.924812	5.727437	-0.075302	2.523279
397.437070	2124.012012	5.732442	-0.075366	2.527889
397.915012	2132.057454	5.737446	-0.075460	2.532479
398.077251	2140.174303	5.742451	-0.075496	2.537077
398.717056	2148.164544	5.747456	-0.075620	2.541631
398.847786	2156.263987	5.752461	-0.075650	2.546200
399.178929	2164.350001	5.757466	-0.075717	2.550769
399.544435	2172.363360	5.762470	-0.075790	2.555291
399.933846	2180.418238	5.767475	-0.075868	2.559830
400.226234	2188.439059	5.772480	-0.075928	2.564334
400.427121	2196.546530	5.777485	-0.075970	2.568873
400.874499	2204.604451	5.782490	-0.076059	2.573393
401.152922	2212.640305	5.787494	-0.076116	2.577881
401.688741	2220.684313	5.792499	-0.076221	2.582384
401.944712	2228.750335	5.797504	-0.076274	2.586872
402.310745	2236.867802	5.802509	-0.076348	2.591388
402.787668	2244.964798	5.807514	-0.076442	2.595892
403.025927	2252.971466	5.812518	-0.076491	2.600322
403.421813	2260.987817	5.817523	-0.076570	2.604761
403.589968	2269.038602	5.822528	-0.076607	2.609195
404.112221	2277.066396	5.827533	-0.076709	2.613634
404.205507	2285.182745	5.832538	-0.076732	2.618083
404.486322	2293.201304	5.837542	-0.076790	2.622485
405.090370	2301.198219	5.842547	-0.076907	2.626890
405.666060	2309.228221	5.847552	-0.077020	2.631302
406.066686	2317.282536	5.852557	-0.077100	2.635709
406.450970	2325.342817	5.857562	-0.077177	2.640111
406.685815	2333.389117	5.862566	-0.077226	2.644487
407.077266	2341.459909	5.867571	-0.077304	2.648880
407.440454	2349.507041	5.872576	-0.077377	2.653251
407.764475	2357.554229	5.877581	-0.077442	2.657613
408.202702	2365.614175	5.882586	-0.077529	2.661981
408.355681	2373.681874	5.887590	-0.077563	2.666327
408.796100	2381.744575	5.892595	-0.077650	2.670683
409.289095	2389.778130	5.897600	-0.077747	2.675019
409.491691	2397.824197	5.902605	-0.077790	2.679336
409.778266	2405.873734	5.907610	-0.077849	2.683653
409.912067	2413.926841	5.912614	-0.077879	2.687955
410.263074	2421.966002	5.917619	-0.077950	2.692257
410.843244	2430.011062	5.922624	-0.078063	2.696570
410.982332	2438.080281	5.927629	-0.078094	2.700860
411.621415	2446.097347	5.932634	-0.078219	2.705148
411.884095	2454.147473	5.937638	-0.078273	2.709422
412.272111	2462.211962	5.942643	-0.078350	2.713705
412.517784	2470.270965	5.947648	-0.078401	2.717969
412.946533	2478.276897	5.952653	-0.078486	2.722211
413.537021	2486.315444	5.957658	-0.078602	2.726472
413.633013	2494.429601	5.962662	-0.078625	2.730736
414.144030	2502.434220	5.967667	-0.078725	2.734962
414.773946	2510.450496	5.972672	-0.078848	2.739194
414.888614	2518.513309	5.977677	-0.078874	2.743412
415.185356	2526.622108	5.982682	-0.078935	2.747659
415.666722	2534.655136	5.987686	-0.079030	2.751871
415.940254	2542.740981	5.992691	-0.079086	2.756092
416.001333	2550.792857	5.997696	-0.079103	2.760275
416.293743	2558.784490	6.002701	-0.079162	2.764435
417.064767	2566.792348	6.007706	-0.079311	2.768626
417.235175	2574.842886	6.012710	-0.079348	2.772796
417.547743	2582.891387	6.017715	-0.079412	2.776967
418.018827	2590.942698	6.022720	-0.079505	2.781143
418.423111	2598.962571	6.027725	-0.079585	2.785292
418.844924	2607.011452	6.032730	-0.079669	2.789452
418.856407	2615.108856	6.037734	-0.079677	2.793605
419.304595	2623.122346	6.042739	-0.079765	2.797735
419.422370	2631.195495	6.047744	-0.079793	2.801870
419.629402	2639.209095	6.052749	-0.079836	2.805973
420.117476	2647.279226	6.057754	-0.079933	2.810116
420.780412	2655.240063	6.062758	-0.080061	2.814208
420.974690	2663.319813	6.067763	-0.080103	2.818326
421.352533	2671.363880	6.072768	-0.080178	2.822431
421.383948	2679.462803	6.077773	-0.080190	2.826537
421.383542	2687.580888	6.082778	-0.080195	2.830645
421.783267	2695.570935	6.087782	-0.080274	2.834706
422.143284	2703.588357	6.092787	-0.080347	2.838772
422.709789	2711.577774	6.097792	-0.080457	2.842831
423.156534	2719.591966	6.102797	-0.080546	2.846889
423.616127	2727.663024	6.107802	-0.080637	2.850970
424.184690	2735.663160	6.112806	-0.080748	2.855016
424.193141	2743.758465	6.117811	-0.080755	2.859072
424.605291	2751.776469	6.122816	-0.080837	2.863107
424.720031	2759.863406	6.127821	-0.080863	2.867153
425.194055	2767.920666	6.132826	-0.080957	2.871199
425.668921	2775.931767	6.137830	-0.081051	2.875217
425.871778	2783.978024	6.142835	-0.081094	2.879231
425.834363	2792.063861	6.147840	-0.081092	2.883245
426.441156	2800.002475	6.152845	-0.081210	2.887217
426.714184	2808.120249	6.157850	-0.081266	2.891254
426.897856	2816.168560	6.162854	-0.081306	2.895245
427.556919	2824.143467	6.167859	-0.081434	2.899221
428.122042	2832.168640	6.172864	-0.081544	2.903211
427.982240	2840.285382	6.177869	-0.081524	2.907202
428.418346	2848.344900	6.182874	-0.081610	2.911190
428.761611	2856.395469	6.187878	-0.081679	2.915164
428.892581	2864.426547	6.192883	-0.081709	2.919111
429.295361	2872.419462	6.197888	-0.081789	2.923049
429.496416	2880.464110	6.202893	-0.081832	2.926996
430.096036	2888.505977	6.207898	-0.081949	2.930957
430.388784	2896.521015	6.212902	-0.082009	2.934884
430.527820	2904.590073	6.217907	-0.082040	2.938823
431.060857	2912.583311	6.222912	-0.082144	2.942741
431.530610	2920.595688	6.227917	-0.082237	2.946660
431.881236	2928.676385	6.232922	-0.082308	2.950600
432.214587	2936.715169	6.237926	-0.082375	2.954514
432.657335	2944.718717	6.242931	-0.082463	2.958411
432.854445	2952.790052	6.247936	-0.082505	2.962323
432.699581	2960.883700	6.252941	-0.082481	2.966222
433.036641	2968.955556	6.257946	-0.082549	2.970131
433.520879	2976.908825	6.262950	-0.082645	2.973986
433.828104	2984.964482	6.267955	-0.082707	2.977875
434.194860	2992.995175	6.272960	-0.082781	2.981750
434.352514	3001.029614	6.277965	-0.082815	2.985612
434.884535	3009.065808	6.282970	-0.082920	2.989488
435.034516	3017.129349	6.287974	-0.082953	2.993353
435.230573	3025.187370	6.292979	-0.082995	2.997212
435.933755	3033.169201	6.297984	-0.083131	3.001056
436.150349	3041.168073	6.302989	-0.083176	3.004878
436.650414	3049.210228	6.307994	-0.083275	3.008730
436.873617	3057.281735	6.312998	-0.083322	3.012578
436.950404	3065.344263	6.318003	-0.083341	3.016408
437.349346	3073.385769	6.323008	-0.083421	3.020240
437.651476	3081.377285	6.328013	-0.083482	3.024039
437.998218	3089.467488	6.333018	-0.083552	3.027881
438.258470	3097.507763	6.338022	-0.083606	3.031691
438.971285	3105.484455	6.343027	-0.083744	3.035489
439.357736	3113.487024	6.348032	-0.083821	3.039277
439.596058	3121.520539	6.353037	-0.083871	3.043068
439.772109	3129.620546	6.358042	-0.083909	3.046883
440.150725	3137.645863	6.363046	-0.083985	3.050667
440.532872	3145.665655	6.368051	-0.084061	3.054444
440.868196	3153.724448	6.373056	-0.084129	3.058233
441.306152	3161.742061	6.378061	-0.084216	3.062002
441.193205	3169.866029	6.383066	-0.084200	3.065790
441.480744	3177.879761	6.388070	-0.084259	3.069541
441.467531	3185.996697	6.393075	-0.084262	3.073322
442.271595	3193.921036	6.398080	-0.084417	3.077046
442.516363	3201.954277	6.403085	-0.084467	3.080791
442.818666	3209.971357	6.408090	-0.084529	3.084526
442.738407	3218.037288	6.413094	-0.084519	3.088260
443.014520	3226.082115	6.418099	-0.084576	3.091998
442.583345	3234.227515	6.423104	-0.084501	3.095744
443.465103	3242.094691	6.428109	-0.084670	3.099418
443.588103	3250.172293	6.433114	-0.084699	3.103150
443.930866	3258.186663	6.438118	-0.084768	3.106858
444.215336	3266.268934	6.443123	-0.084826	3.110591
444.200911	3274.283035	6.448128	-0.084829	3.114274
444.455322	3282.270811	6.453133	-0.084881	3.117952
444.901185	3290.304856	6.458138	-0.084969	3.121656
445.395970	3298.313779	6.463142	-0.085067	3.125347
445.450902	3306.362631	6.468147	-0.085082	3.129031
445.683279	3314.447786	6.473152	-0.085131	3.132736
446.110903	3322.453423	6.478157	-0.085216	3.136409
446.757527	3330.464092	6.483162	-0.085341	3.140089
446.865544	3338.495926	6.488166	-0.085367	3.143751
447.131258	3346.547720	6.493171	-0.085422	3.147424
447.337696	3354.648605	6.498176	-0.085465	3.151113
447.669110	3362.626991	6.503181	-0.085532	3.154747
448.345869	3370.620840	6.508186	-0.085664	3.158399
448.650788	3378.624135	6.513190	-0.085726	3.162035
448.764101	3386.699755	6.518195	-0.085752	3.165691
449.001898	3394.748419	6.523200	-0.085802	3.169336
449.053444	3402.806602	6.528205	-0.085816	3.172973
449.601350	3410.818206	6.533210	-0.085924	3.176606
449.784060	3418.871903	6.538214	-0.085963	3.180238
449.617083	3426.923574	6.543219	-0.085937	3.183850
450.219195	3434.942038	6.548224	-0.086055	3.187476
450.707396	3442.930769	6.553229	-0.086151	3.191080
450.972046	3450.971904	6.558234	-0.086205	3.194694
451.418572	3458.966425	6.563238	-0.086294	3.198290
451.568715	3467.043299	6.568243	-0.086327	3.201906
451.861880	3475.081426	6.573248	-0.086387	3.205507
451.988446	3483.113117	6.578253	-0.086416	3.209094
452.674001	3491.123787	6.583258	-0.086549	3.212691
452.957261	3499.147604	6.588262	-0.086607	3.216273
452.873560	3507.253965	6.593267	-0.086596	3.219872
453.214410	3515.260936	6.598272	-0.086665	3.223441
453.607991	3523.247320	6.603277	-0.086744	3.226998
454.019149	3531.316526	6.608282	-0.086825	3.230590
454.186360	3539.337372	6.613286	-0.086862	3.234145
454.669563	3547.331830	6.618291	-0.086957	3.237698
454.670424	3555.425060	6.623296	-0.086963	3.241271
455.012635	3563.387658	6.628301	-0.087031	3.244797
455.239405	3571.413113	6.633306	-0.087079	3.248341
455.442346	3579.480197	6.638310	-0.087122	3.251899
455.580508	3587.537364	6.643315	-0.087153	3.255446
456.193173	3595.489699	6.648320	-0.087272	3.258962
456.495232	3603.546604	6.653325	-0.087334	3.262508
456.751765	3611.616631	6.658330	-0.087387	3.266053
457.033276	3619.631158	6.663334	-0.087445	3.269572
457.122365	3627.696439	6.668339	-0.087467	3.273101
457.618221	3635.683822	6.673344	-0.087564	3.276609
457.655274	3643.691193	6.678349	-0.087576	3.280103
457.876195	3651.741243	6.683354	-0.087623	3.283619
457.838917	3659.802744	6.688358	-0.087621	3.287126
457.952701	3667.863424	6.693363	-0.087648	3.290635
458.357116	3675.853187	6.698368	-0.087728	3.294121
458.662175	3683.861331	6.703373	-0.087790	3.297608
458.922644	3691.914566	6.708378	-0.087844	3.301108
458.656274	3699.995099	6.713382	-0.087800	3.304596
459.134357	3708.000492	6.718387	-0.087894	3.308077
459.455603	3716.039474	6.723392	-0.087959	3.311562
459.988565	3723.994306	6.728397	-0.088063	3.315016
460.275092	3732.027534	6.733402	-0.088122	3.318490
460.619988	3740.031484	6.738406	-0.088192	3.321950
460.701977	3748.104367	6.743411	-0.088212	3.325426
461.054703	3756.146453	6.748416	-0.088283	3.328896
461.093647	3764.167411	6.753421	-0.088296	3.332340
461.539017	3772.192833	6.758426	-0.088384	3.335799
461.888639	3780.223581	6.763430	-0.088454	3.339253
462.039121	3788.263549	6.768435	-0.088487	3.342699
462.678571	3796.258019	6.773440	-0.088612	3.346141
462.455247	3804.345364	6.778445	-0.088575	3.349586
462.764222	3812.372463	6.783450	-0.088638	3.353022
463.070786	3820.384707	6.788454	-0.088701	3.356448
463.300017	3828.395878	6.793459	-0.088749	3.359867
463.728173	3836.384108	6.798464	-0.088834	3.363281
464.044070	3844.409501	6.803469	-0.088898	3.366702
464.435766	3852.485240	6.808474	-0.088976	3.370144
464.209851	3860.564469	6.813478	-0.088939	3.373561
464.789916	3868.534538	6.818483	-0.089052	3.376959
465.327186	3876.560881	6.823488	-0.089158	3.380374
465.415680	3884.541658	6.828493	-0.089179	3.383751
465.641281	3892.646712	6.833498	-0.089227	3.387182
465.833129	3900.694854	6.838502	-0.089268	3.390584
466.162982	3908.729809	6.843507	-0.089334	3.393982
466.526665	3916.740434	6.848512	-0.089407	3.397367
466.337194	3924.796389	6.853517	-0.089377	3.400749
466.748898	3932.754505	6.858522	-0.089459	3.404107
466.901303	3940.799081	6.863526	-0.089493	3.407489
466.939057	3948.875518	6.868531	-0.089505	3.410877
467.462435	3956.858894	6.873536	-0.089608	3.414240
467.864563	3964.843372	6.878541	-0.089688	3.417595
468.258632	3972.915016	6.883546	-0.089767	3.420984
468.413956	3980.904049	6.888550	-0.089801	3.424326
469.043653	3988.930436	6.893555	-0.089923	3.427697
469.113395	3997.029416	6.898560	-0.089942	3.431075
469.016954	4005.033144	6.903565	-0.089929	3.434405
469.427457	4013.035074	6.908570	-0.090011	3.437748
469.762758	4021.055691	6.913574	-0.090078	3.441093
470.261794	4029.017423	6.918579	-0.090177	3.444415
470.255052	4037.142211	6.923584	-0.090181	3.447785
470.628463	4045.127816	6.928589	-0.090255	3.451107
470.853360	4053.179425	6.933594	-0.090303	3.454448
470.590450	4061.304279	6.938598	-0.090259	3.457799
471.182493	4069.265503	6.943603	-0.090374	3.461109
471.162708	4077.299268	6.948608	-0.090376	3.464424
471.254477	4085.332480	6.953613	-0.090398	3.467740
471.939451	4093.329456	6.958618	-0.090531	3.471058
471.744527	4101.416472	6.963622	-0.090500	3.474380
472.109269	4109.378944	6.968627	-0.090573	3.477666
472.807821	4117.388591	6.973632	-0.090709	3.480979
472.776263	4125.357872	6.978637	-0.090708	3.484249
473.366833	4133.350657	6.983642	-0.090823	3.487545
473.578202	4141.450002	6.988646	-0.090868	3.490870
473.300164	4149.525693	6.993651	-0.090821	3.494166
473.664593	4157.592539	6.998656	-0.090895	3.497476
473.857370	4165.599667	7.003661	-0.090936	3.500753
474.188304	4173.565269	7.008666	-0.091003	3.504014
474.295798	4181.641769	7.013670	-0.091028	3.507310
474.571138	4189.682896	7.018675	-0.091084	3.510594
474.726846	4197.681914	7.023680	-0.091119	3.513854
474.986218	4205.674229	7.028685	-0.091172	3.517112
475.612544	4213.660991	7.033690	-0.091294	3.520376
475.571745	4221.725564	7.038694	-0.091292	3.523647
475.941883	4229.762816	7.043699	-0.091366	3.526917
475.950429	4237.830920	7.048704	-0.091373	3.530185
476.195369	4245.815029	7.053709	-0.091424	3.533423
476.639243	4253.818382	7.058714	-0.091512	3.536673
476.843881	4261.849908	7.063718	-0.091555	3.539923
477.227058	4269.829643	7.068723	-0.091632	3.543155
477.502821	4277.929603	7.073728	-0.091688	3.546429
477.503838	4285.978142	7.078733	-0.091694	3.549671
477.654679	4294.080153	7.083738	-0.091727	3.552936
477.904882	4302.087418	7.088742	-0.091779	3.556163
478.435851	4309.997753	7.093747	-0.091883	3.559356
478.159033	4318.084242	7.098752	-0.091837	3.562593
478.680302	4326.011508	7.103757	-0.091939	3.565787
478.817328	4334.063698	7.108762	-0.091970	3.569017
479.271253	4342.084829	7.113766	-0.092060	3.572241
479.401369	4350.135123	7.118771	-0.092089	3.575464
479.678885	4358.183395	7.123776	-0.092146	3.578687
479.958143	4366.182586	7.128781	-0.092203	3.581888
480.103902	4374.224749	7.133786	-0.092236	3.585099
480.006795	4382.299097	7.138790	-0.092223	3.588313
480.418418	4390.310412	7.143795	-0.092305	3.591514
480.683565	4398.344487	7.148800	-0.092360	3.594717
480.675290	4406.308312	7.153805	-0.092363	3.597881
481.042696	4414.362774	7.158810	-0.092437	3.601090
480.629240	4422.430808	7.163814	-0.092365	3.604278
480.542024	4430.448325	7.168819	-0.092354	3.607453
481.556190	4438.390296	7.173824	-0.092548	3.610626
481.879506	4446.391774	7.178829	-0.092614	3.613801
482.107521	4454.465755	7.183834	-0.092662	3.616998
482.399491	4462.471231	7.188838	-0.092721	3.620168
482.653824	4470.465962	7.193843	-0.092774	3.623329
482.615312	4478.595598	7.198848	-0.092772	3.626532
482.602078	4486.614038	7.203853	-0.092775	3.629690
483.052399	4494.601908	7.208858	-0.092864	3.632846
483.202263	4502.653880	7.213862	-0.092897	3.636015
483.165668	4510.625087	7.218867	-0.092895	3.639146
483.828499	4518.631275	7.223872	-0.093024	3.642306
483.569168	4526.676579	7.228877	-0.092981	3.645454
483.743394	4534.699277	7.233882	-0.093019	3.648602
484.047523	4542.733517	7.238886	-0.093081	3.651755
484.108940	4550.786093	7.243891	-0.093097	3.654906
484.166462	4558.828338	7.248896	-0.093113	3.658050
484.379690	4566.830796	7.253901	-0.093158	3.661180
484.639353	4574.829804	7.258906	-0.093212	3.664307
484.712745	4582.874190	7.263910	-0.093231	3.667445
485.100600	4590.864696	7.268915	-0.093308	3.670567
485.570040	4598.854214	7.273920	-0.093401	3.673688
485.688873	4606.894673	7.278925	-0.093428	3.676817
485.423299	4615.017158	7.283930	-0.093384	3.679965
485.404166	4623.029223	7.288934	-0.093386	3.683073
485.915666	4630.963147	7.293939	-0.093487	3.686163
486.367992	4639.007100	7.298944	-0.093576	3.689292
486.366595	4647.071559	7.303949	-0.093581	3.692413
486.510564	4655.116175	7.308954	-0.093613	3.695528
486.358564	4663.155044	7.313958	-0.093590	3.698631
486.276824	4671.195125	7.318963	-0.093580	3.701733
486.229102	4679.231573	7.323968	-0.093577	3.704833
486.420117	4687.233039	7.328973	-0.093617	3.707922
487.035206	4695.211720	7.333978	-0.093737	3.711010
487.303347	4703.243647	7.338982	-0.093792	3.714108
487.778640	4711.222544	7.343987	-0.093886	3.717188
487.825582	4719.293957	7.348992	-0.093900	3.720290
487.990595	4727.239146	7.353997	-0.093936	3.723344
487.890818	4735.372615	7.359002	-0.093923	3.726461
488.330535	4743.291321	7.364006	-0.094010	3.729506
488.487171	4751.324682	7.369011	-0.094044	3.732586
489.132061	4759.321935	7.374016	-0.094170	3.735662
489.607706	4767.305054	7.379021	-0.094263	3.738725
489.570943	4775.429082	7.384026	-0.094262	3.741827
489.357925	4783.476133	7.389030	-0.094228	3.744893
489.712076	4791.440432	7.394035	-0.094299	3.747938
490.402611	4799.465493	7.399040	-0.094433	3.751013
490.225032	4807.507119	7.404045	-0.094405	3.754070
490.497990	4815.540018	7.409050	-0.094461	3.757132
490.911190	4823.519851	7.414054	-0.094543	3.760174
490.911490	4831.533801	7.419059	-0.094548	3.763218
490.947261	4839.608006	7.424064	-0.094560	3.766282
491.542269	4847.560148	7.429069	-0.094676	3.769311
491.399504	4855.655346	7.434074	-0.094655	3.772375
491.839464	4863.654252	7.439078	-0.094742	3.775413
491.663250	4871.710115	7.444083	-0.094715	3.778455
492.199979	4879.711301	7.449088	-0.094820	3.781491
492.031277	4887.731703	7.454093	-0.094794	3.784516
492.277973	4895.767896	7.459098	-0.094845	3.787554
492.543073	4903.815338	7.464102	-0.094900	3.790594
492.944980	4911.773187	7.469107	-0.094980	3.793600
493.378150	4919.811158	7.474112	-0.095066	3.796636
493.585942	4927.809529	7.479117	-0.095110	3.799648
493.677595	4935.846247	7.484122	-0.095132	3.802670
494.340735	4943.793682	7.489126	-0.095261	3.805669
494.535352	4951.843868	7.494131	-0.095302	3.808694
494.718254	4959.947898	7.499136	-0.095342	3.811736
494.615011	4967.963701	7.504141	-0.095328	3.814736
494.797245	4976.018998	7.509146	-0.095367	3.817755
494.954766	4984.068850	7.514150	-0.095401	3.820769
494.761839	4992.034518	7.519155	-0.095371	3.823742
495.149570	5000.075264	7.524160	-0.095448	3.826753
495.273896	5008.088469	7.529165	-0.095477	3.829745
495.316955	5016.146229	7.534170	-0.095490	3.832750
495.474489	5024.147543	7.539174	-0.095524	3.835734
495.606843	5032.127248	7.544179	-0.095554	3.838707
496.255301	5040.138138	7.549184	-0.095680	3.841701
496.576280	5048.103721	7.554189	-0.095745	3.844668
496.815425	5056.201385	7.559194	-0.095795	3.847680
496.749864	5064.274854	7.564198	-0.095788	3.850674
497.070821	5072.246763	7.569203	-0.095853	3.853637
496.871142	5080.330223	7.574208	-0.095821	3.856627
497.011289	5088.313857	7.579213	-0.095853	3.859586
497.371867	5096.313276	7.584218	-0.095925	3.862552
497.923678	5104.316771	7.589222	-0.096033	3.865522
498.208578	5112.321236	7.594227	-0.096091	3.868484
498.262052	5120.457366	7.599232	-0.096107	3.871488
498.369499	5128.517247	7.604237	-0.096132	3.874462
498.378819	5136.498936	7.609242	-0.096139	3.877403
498.262166	5144.513971	7.614246	-0.096123	3.880352
498.754459	5152.396482	7.619251	-0.096219	3.883262
498.680538	5160.507987	7.624256	-0.096211	3.886242
498.462667	5168.504285	7.629261	-0.096176	3.889176
498.729144	5176.547533	7.634266	-0.096231	3.892133
499.254748	5184.538769	7.639270	-0.096334	3.895075
499.233980	5192.553710	7.644275	-0.096335	3.898012
499.540898	5200.629637	7.649280	-0.096398	3.900976
499.377700	5208.604642	7.654285	-0.096372	3.903891
500.431176	5216.557605	7.659290	-0.096574	3.906820
500.266110	5224.631950	7.664294	-0.096548	3.909767
500.105148	5232.686447	7.669299	-0.096524	3.912705
500.081443	5240.777385	7.674304	-0.096525	3.915656
499.731446	5248.783575	7.679309	-0.096465	3.918569
500.607291	5256.708474	7.684314	-0.096633	3.921472
500.571443	5264.705892	7.689318	-0.096631	3.924383
500.872706	5272.735569	7.694323	-0.096693	3.927310
501.701140	5280.718403	7.699328	-0.096852	3.930227
501.752730	5288.793885	7.704333	-0.096867	3.933161
502.197912	5296.827742	7.709338	-0.096955	3.936085
502.503202	5304.799984	7.714342	-0.097017	3.938982
502.408022	5312.892514	7.719347	-0.097005	3.941913
502.342971	5320.924825	7.724352	-0.096998	3.944820
502.949270	5328.899853	7.729357	-0.097116	3.947717
503.537532	5336.923372	7.734362	-0.097231	3.950629
503.640617	5344.972151	7.739366	-0.097256	3.953539
503.532247	5353.030526	7.744371	-0.097241	3.956447
503.924281	5361.024943	7.749376	-0.097319	3.959338
503.712295	5369.046572	7.754381	-0.097285	3.962226
503.974401	5377.021153	7.759386	-0.097339	3.965104
504.223916	5385.060390	7.764390	-0.097391	3.968002
504.515780	5393.095736	7.769395	-0.097450	3.970898
504.796862	5401.128048	7.774400	-0.097508	3.973790
504.572239	5409.167366	7.779405	-0.097471	3.976674
505.567497	5417.062200	7.784410	-0.097662	3.979525
505.389204	5425.143175	7.789414	-0.097634	3.982420
505.396634	5433.155719	7.794419	-0.097641	3.985292
506.204862	5441.148086	7.799424	-0.097796	3.988168
506.174154	5449.218692	7.804429	-0.097796	3.991056
506.454542	5457.209692	7.809434	-0.097853	3.993919
506.866543	5465.247547	7.814438	-0.097935	3.996798
507.212189	5473.216657	7.819443	-0.098005	3.999650
507.345961	5481.285518	7.824448	-0.098035	4.002531
507.437623	5489.289523	7.829453	-0.098057	4.005387
507.929310	5497.285148	7.834458	-0.098154	4.008244
507.879235	5505.380084	7.839462	-0.098150	4.011126
507.783071	5513.364451	7.844467	-0.098138	4.013965
508.094055	5521.446497	7.849472	-0.098201	4.016844
508.166654	5529.417881	7.854477	-0.098219	4.019678
508.369900	5537.487520	7.859482	-0.098263	4.022546
508.367042	5545.460525	7.864486	-0.098267	4.025375
508.590979	5553.517039	7.869491	-0.098314	4.028235
508.782676	5561.563194	7.874496	-0.098355	4.031089
508.915151	5569.598371	7.879501	-0.098385	4.033936
509.521012	5577.578573	7.884506	-0.098503	4.036769
509.419398	5585.608244	7.889510	-0.098490	4.039606
509.302311	5593.597354	7.894515	-0.098473	4.042427
509.632722	5601.607804	7.899520	-0.098540	4.045260
509.836177	5609.602991	7.904525	-0.098583	4.048084
510.035369	5617.678449	7.909530	-0.098625	4.050934
510.263119	5625.663601	7.914534	-0.098673	4.053751
510.543273	5633.721350	7.919539	-0.098730	4.056592
510.936255	5641.699265	7.924544	-0.098809	4.059404
510.984564	5649.724212	7.929549	-0.098823	4.062226
511.341184	5657.701695	7.934554	-0.098895	4.065034
511.664909	5665.751179	7.939558	-0.098960	4.067865
511.561315	5673.807447	7.944563	-0.098946	4.070690
511.969366	5681.821161	7.949568	-0.099028	4.073505
512.063925	5689.850966	7.954573	-0.099050	4.076320
511.939768	5697.839226	7.959578	-0.099033	4.079114
512.525633	5705.843825	7.964582	-0.099147	4.081923
512.672039	5713.850778	7.969587	-0.099179	4.084725
512.816625	5721.928628	7.974592	-0.099212	4.087549
513.060727	5729.912373	7.979597	-0.099262	4.090340
513.146504	5737.966267	7.984602	-0.099284	4.093151
513.198367	5746.023522	7.989606	-0.099299	4.095960
513.463819	5753.940637	7.994611	-0.099353	4.098723
514.215938	5761.960429	7.999616	-0.099499	4.101525
514.362374	5769.958880	8.004621	-0.099531	4.104310
514.736996	5778.017605	8.009626	-0.099606	4.107117
514.298409	5786.124720	8.014630	-0.099530	4.109928
514.912132	5794.029695	8.019635	-0.099649	4.112681
515.141555	5802.105484	8.024640	-0.099697	4.115486
514.961699	5810.109040	8.029645	-0.099669	4.118258
515.005077	5818.180536	8.034650	-0.099682	4.121056
515.639840	5826.077063	8.039654	-0.099806	4.123798
516.139049	5834.094392	8.044659	-0.099904	4.126579
516.099744	5842.181101	8.049664	-0.099902	4.129375
516.060442	5850.237131	8.054669	-0.099900	4.132158
516.572649	5858.223638	8.059674	-0.100001	4.134923
516.656319	5866.235316	8.064678	-0.100021	4.137689
516.643987	5874.250526	8.069683	-0.100024	4.140452
516.788088	5882.302475	8.074688	-0.100056	4.143229
516.782900	5890.297361	8.079693	-0.100061	4.145982
517.508540	5898.262709	8.084698	-0.100201	4.148733
518.337880	5906.270748	8.089702	-0.100361	4.151497
518.285693	5914.295425	8.094707	-0.100356	4.154255
518.437427	5922.367194	8.099712	-0.100390	4.157029
518.773551	5930.332288	8.104717	-0.100458	4.159767
518.894475	5938.374160	8.109722	-0.100486	4.162527
519.120779	5946.383080	8.114726	-0.100533	4.165275
519.009393	5954.464874	8.119731	-0.100517	4.168042
519.110355	5962.536367	8.124736	-0.100542	4.170806
519.610999	5970.487995	8.129741	-0.100640	4.173532
519.542031	5978.591704	8.134746	-0.100632	4.176302
520.074217	5986.513738	8.139750	-0.100737	4.179014
519.511830	5994.677048	8.144755	-0.100637	4.181795
519.825439	6002.577813	8.149760	-0.100701	4.184494
520.170092	6010.576193	8.154765	-0.100770	4.187225
520.391750	6018.639984	8.159770	-0.100817	4.189976
520.529957	6026.744061	8.164774	-0.100848	4.192737
520.469264	6034.728906	8.169779	-0.100842	4.195453
520.580429	6042.744462	8.174784	-0.100868	4.198180
520.916388	6050.726664	8.179789	-0.100936	4.200897
521.034586	6058.664267	8.184794	-0.100963	4.203594
521.467371	6066.707245	8.189798	-0.101049	4.206328
521.437301	6074.700577	8.194803	-0.101048	4.209039
521.751267	6082.798604	8.199808	-0.101112	4.211787
521.889431	6090.795172	8.204813	-0.101143	4.214498
522.368877	6098.785235	8.209818	-0.101238	4.217208
522.600494	6106.803203	8.214822	-0.101286	4.219922
522.749894	6114.778198	8.219827	-0.101319	4.222620
522.898374	6122.821246	8.224832	-0.101352	4.225339
523.407259	6130.843627	8.229837	-0.101452	4.228053
523.437538	6138.885124	8.234842	-0.101463	4.230767
523.750423	6146.902822	8.239846	-0.101527	4.233473
523.617591	6154.989319	8.244851	-0.101507	4.236197
523.824503	6162.940003	8.249856	-0.101551	4.238877
523.704858	6170.986294	8.254861	-0.101534	4.241583
524.504666	6178.884117	8.259866	-0.101688	4.244248
524.453015	6187.025111	8.264870	-0.101684	4.246984
524.479817	6194.982165	8.269875	-0.101694	4.249657
524.837670	6203.056491	8.274880	-0.101766	4.252371
525.483621	6210.975133	8.279885	-0.101891	4.255033
525.977386	6219.005842	8.284890	-0.101989	4.257730
526.244796	6227.081861	8.289894	-0.102044	4.260439
526.084529	6235.087563	8.294899	-0.102019	4.263118
526.346119	6243.164785	8.299904	-0.102073	4.265823
526.282521	6251.156397	8.304909	-0.102067	4.268495
527.014331	6259.140298	8.309914	-0.102208	4.271170
527.246223	6267.139527	8.314918	-0.102256	4.273843
527.239300	6275.196240	8.319923	-0.102260	4.276532
527.302996	6283.196193	8.324928	-0.102278	4.279201
527.589732	6291.184860	8.329933	-0.102336	4.281867
527.444150	6299.201439	8.334938	-0.102314	4.284536
527.942317	6307.217134	8.339942	-0.102412	4.287209
527.785224	6315.289098	8.344947	-0.102388	4.289894
527.957847	6323.320809	8.349952	-0.102426	4.292566
528.100790	6331.314202	8.354957	-0.102458	4.295223
528.158641	6339.337373	8.359962	-0.102474	4.297888
528.854369	6347.390651	8.364966	-0.102609	4.300567
528.785606	6355.301035	8.369971	-0.102601	4.303190
529.529686	6363.387020	8.374976	-0.102745	4.305876
529.406965	6371.368973	8.379981	-0.102727	4.308520
530.140833	6379.378895	8.384986	-0.102869	4.311177
530.195888	6387.347511	8.389990	-0.102885	4.313814
530.314230	6395.438497	8.394995	-0.102912	4.316490
530.817262	6403.381598	8.400000	-0.103011	4.319119
530.732144	6411.488554	8.405005	-0.103000	4.321796
530.878648	6419.407633	8.410010	-0.103033	4.324410
530.842958	6427.539445	8.415014	-0.103031	4.327092
530.937142	6435.451554	8.420019	-0.103054	4.329701
530.874352	6443.601544	8.425024	-0.103048	4.332385
531.349215	6451.568702	8.430029	-0.103141	4.335012
531.789702	6459.536930	8.435034	-0.103229	4.337637
531.803341	6467.572067	8.440038	-0.103237	4.340279
531.887944	6475.542096	8.445043	-0.103258	4.342898
532.020639	6483.649040	8.450048	-0.103288	4.345562
532.110706	6491.629698	8.455053	-0.103310	4.348182
532.808361	6499.656208	8.460058	-0.103445	4.350820
532.970719	6507.761394	8.465062	-0.103480	4.353478
532.864323	6515.764887	8.470067	-0.103466	4.356099
533.062359	6523.751433	8.475072	-0.103508	4.358715
532.719593	6531.787661	8.480077	-0.103449	4.361342
533.522099	6539.648082	8.485082	-0.103604	4.363918
533.838750	6547.742348	8.490086	-0.103668	4.366566
533.515991	6555.810773	8.495091	-0.103613	4.369199
534.013061	6563.840526	8.500096	-0.103711	4.371823
534.317892	6571.793973	8.505101	-0.103773	4.374420
534.196927	6579.858450	8.510106	-0.103756	4.377048
535.050867	6587.799266	8.515110	-0.103920	4.379641
535.491099	6595.795404	8.520115	-0.104007	4.382248
535.396394	6603.872069	8.525120	-0.103995	4.384875
535.864500	6611.883262	8.530125	-0.104087	4.387484
535.966783	6619.921709	8.535130	-0.104112	4.390097
536.221889	6628.010203	8.540134	-0.104165	4.392726
536.509817	6635.957792	8.545139	-0.104223	4.395308
536.646051	6643.996696	8.550144	-0.104254	4.397917
536.587030	6652.072867	8.555149	-0.104248	4.400536
536.926267	6659.986723	8.560154	-0.104317	4.403102
537.354691	6668.003074	8.565159	-0.104402	4.405701
537.558724	6676.072656	8.570163	-0.104445	4.408314
537.674970	6684.148638	8.575168	-0.104472	4.410927
537.312406	6692.152668	8.580173	-0.104410	4.413513
537.537047	6700.232489	8.585178	-0.104457	4.416125
537.548408	6708.199877	8.590183	-0.104464	4.418698
537.271530	6716.273463	8.595187	-0.104418	4.421302
537.381585	6724.232087	8.600192	-0.104444	4.423869
537.791886	6732.276754	8.605197	-0.104525	4.426464
538.059788	6740.242315	8.610202	-0.104581	4.429032
538.177678	6748.357564	8.615207	-0.104608	4.431645
538.795434	6756.202971	8.620211	-0.104728	4.434173
539.142167	6764.280631	8.625216	-0.104798	4.436772
539.581296	6772.262660	8.630221	-0.104885	4.439340
539.473842	6780.358804	8.635226	-0.104870	4.441940
539.581052	6788.292074	8.640231	-0.104895	4.444487
539.679669	6796.344928	8.645235	-0.104919	4.447071
540.071574	6804.375886	8.650240	-0.104997	4.449648
540.125614	6812.425238	8.655245	-0.105013	4.452228
540.211061	6820.423267	8.660250	-0.105034	4.454790
540.558774	6828.445733	8.665255	-0.105104	4.457359
540.605896	6836.420449	8.670259	-0.105118	4.459910
540.564018	6844.493748	8.675264	-0.105115	4.462491
541.004515	6852.444135	8.680269	-0.105202	4.465034
541.097172	6860.508409	8.685274	-0.105225	4.467609
540.755527	6868.613295	8.690279	-0.105167	4.470195
541.248790	6876.487980	8.695283	-0.105264	4.472708
541.800525	6884.528203	8.700288	-0.105372	4.475274
541.654255	6892.531837	8.705293	-0.105350	4.477823
542.074607	6900.519415	8.710298	-0.105433	4.480368
542.448885	6908.541695	8.715303	-0.105508	4.482923
542.458293	6916.558239	8.720307	-0.105515	4.485472
543.102339	6924.586809	8.725312	-0.105640	4.488027
542.783608	6932.701853	8.730317	-0.105586	4.490604
542.971186	6940.667309	8.735322	-0.105627	4.493134
543.193232	6948.740295	8.740327	-0.105673	4.495696
543.544237	6956.645267	8.745331	-0.105744	4.498204
543.627904	6964.732978	8.750336	-0.105765	4.500768
543.959225	6972.677876	8.755341	-0.105832	4.503286
544.226138	6980.731579	8.760346	-0.105887	4.505837
544.545434	6988.758845	8.765351	-0.105951	4.508378
544.677236	6996.791609	8.770355	-0.105981	4.510918
544.784445	7004.784732	8.775360	-0.106006	4.513445
544.771875	7012.808217	8.780365	-0.106009	4.515979
545.266469	7020.706945	8.785370	-0.106107	4.518475
545.609549	7028.825379	8.790375	-0.106176	4.521037
545.348406	7036.789452	8.795379	-0.106132	4.523548
545.625798	7044.888010	8.800384	-0.106189	4.526101
545.760364	7052.879429	8.805389	-0.106220	4.528619
546.007641	7060.869477	8.810394	-0.106271	4.531135
546.235068	7068.887058	8.815399	-0.106319	4.533658
546.203332	7076.966826	8.820403	-0.106318	4.536198
546.330055	7084.938634	8.825408	-0.106347	4.538704
546.468421	7092.967510	8.830413	-0.106378	4.541226
546.527557	7100.922896	8.835418	-0.106394	4.543724
546.802063	7108.977732	8.840423	-0.106450	4.546252
546.718660	7116.953950	8.845427	-0.106440	4.548753
547.047666	7125.006547	8.850432	-0.106507	4.551277
547.749291	7132.961674	8.855437	-0.106643	4.553771
547.451528	7141.074274	8.860442	-0.106592	4.556310
547.265248	7149.071848	8.865447	-0.106563	4.558812
547.398723	7157.090868	8.870451	-0.106593	4.561320
547.718173	7164.999411	8.875456	-0.106658	4.563792
547.946364	7173.082825	8.880461	-0.106706	4.566317
548.217888	7181.061552	8.885466	-0.106761	4.568809
548.172682	7189.217487	8.890471	-0.106758	4.571353
548.473937	7197.114916	8.895475	-0.106820	4.573817
548.657440	7205.226682	8.900480	-0.106859	4.576345
548.800902	7213.146699	8.905485	-0.106891	4.578813
549.082868	7221.180801	8.910490	-0.106949	4.581314
549.317518	7229.200536	8.915495	-0.106998	4.583810
549.189153	7237.253251	8.920499	-0.106979	4.586314
549.453822	7245.184305	8.925504	-0.107034	4.588780
549.505325	7253.314488	8.930509	-0.107049	4.591305
550.250903	7261.182380	8.935514	-0.107193	4.593749
550.811097	7269.275725	8.940519	-0.107302	4.596261
550.899018	7277.195848	8.945523	-0.107324	4.598717
551.167474	7285.362566	8.950528	-0.107379	4.601249
551.374010	7293.255832	8.955533	-0.107423	4.603694
551.540969	7301.303750	8.960538	-0.107459	4.606186
551.777620	7309.335773	8.965543	-0.107508	4.608672
551.876365	7317.396725	8.970547	-0.107532	4.611165
552.437162	7325.333005	8.975552	-0.107642	4.613619
552.502285	7333.449345	8.980557	-0.107659	4.616126
552.938019	7341.368393	8.985562	-0.107746	4.618572
552.897691	7349.507873	8.990567	-0.107743	4.621084
553.092697	7357.431863	8.995571	-0.107785	4.623528
553.211515	7365.476675	9.000576	-0.107812	4.626008
553.503855	7373.465970	9.005581	-0.107872	4.628470
553.637069	7381.514453	9.010586	-0.107902	4.630948
554.138796	7389.486091	9.015591	-0.108001	4.633402
554.123411	7397.535215	9.020595	-0.108003	4.635878
554.687544	7405.491289	9.025600	-0.108113	4.638324
554.666714	7413.554163	9.030605	-0.108115	4.640802
554.757369	7421.516688	9.035610	-0.108137	4.643247
554.941679	7429.592390	9.040615	-0.108177	4.645726
554.841196	7437.568362	9.045619	-0.108163	4.648173
555.370965	7445.641965	9.050624	-0.108267	4.650649
555.679256	7453.609718	9.055629	-0.108330	4.653090
555.621883	7461.679059	9.060634	-0.108324	4.655562
555.707252	7469.729474	9.065639	-0.108345	4.658027
555.854238	7477.705732	9.070643	-0.108378	4.660467
555.900187	7485.701329	9.075648	-0.108392	4.662912
555.975318	7493.727782	9.080653	-0.108411	4.665365
556.009155	7501.770656	9.085658	-0.108423	4.667822
556.156587	7509.843678	9.090663	-0.108455	4.670287
556.750177	7517.782176	9.095667	-0.108571	4.672709
556.913922	7525.835256	9.100672	-0.108607	4.675165
556.884817	7533.852037	9.105677	-0.108607	4.677609
557.000062	7541.809979	9.110682	-0.108633	4.680034
557.317307	7549.794399	9.115687	-0.108698	4.682465
557.096115	7557.841491	9.120691	-0.108662	4.684914
557.636863	7565.832252	9.125696	-0.108768	4.687345
558.006584	7573.809171	9.130701	-0.108842	4.689769
558.184127	7581.887116	9.135706	-0.108880	4.692224
558.596735	7589.931418	9.140711	-0.108962	4.694667
557.459970	7598.051603	9.145715	-0.108756	4.697133
557.871756	7606.031278	9.150720	-0.108838	4.699554
558.280591	7614.030665	9.155725	-0.108919	4.701979
558.176280	7621.962473	9.160730	-0.108905	4.704383
558.598461	7629.996164	9.165735	-0.108989	4.706816
558.930230	7637.977952	9.170739	-0.109056	4.709232
558.974645	7646.127323	9.175744	-0.109070	4.711698
559.234211	7654.034557	9.180749	-0.109123	4.714090
559.198702	7662.114434	9.185754	-0.109122	4.716532
559.518540	7670.046884	9.190759	-0.109187	4.718928
559.844860	7678.103494	9.195763	-0.109253	4.721361
559.624813	7686.077740	9.200768	-0.109217	4.723768
559.688951	7694.176058	9.205773	-0.109234	4.726211
559.876785	7702.128319	9.210778	-0.109274	4.728608
559.940218	7710.278545	9.215783	-0.109292	4.731065
560.540076	7718.162535	9.220787	-0.109408	4.733438
561.030427	7726.180531	9.225792	-0.109505	4.735851
561.401611	7734.173806	9.230797	-0.109579	4.738255
561.067861	7742.253574	9.235802	-0.109522	4.740686
561.216667	7750.308310	9.240807	-0.109555	4.743106
561.298118	7758.265806	9.245811	-0.109576	4.745497
561.568215	7766.367377	9.250816	-0.109631	4.747929
561.666194	7774.377976	9.255821	-0.109655	4.750333
562.257879	7782.306781	9.260826	-0.109770	4.752710
561.981038	7790.369930	9.265831	-0.109724	4.755128
561.993389	7798.338853	9.270835	-0.109732	4.757516
562.200898	7806.358584	9.275840	-0.109776	4.759917
562.921958	7814.344943	9.280845	-0.109915	4.762306
563.031845	7822.336525	9.285850	-0.109941	4.764697
563.169394	7830.433753	9.290855	-0.109972	4.767118
563.333384	7838.432017	9.295859	-0.110007	4.769508
563.846979	7846.455987	9.300864	-0.110108	4.771904
563.862247	7854.414810	9.305869	-0.110116	4.774280
563.959327	7862.472716	9.310874	-0.110140	4.776685
564.594545	7870.448853	9.315879	-0.110263	4.779062
564.590451	7878.505455	9.320883	-0.110268	4.781464
564.600006	7886.495020	9.325888	-0.110275	4.783845
565.060069	7894.573756	9.330893	-0.110366	4.786249
564.754472	7902.559134	9.335898	-0.110314	4.788628
564.944802	7910.681607	9.340903	-0.110355	4.791044
564.618624	7918.618952	9.345907	-0.110299	4.793406
564.807588	7926.622460	9.350912	-0.110340	4.795784
564.808893	7934.633855	9.355917	-0.110345	4.798164
565.810185	7942.571118	9.360922	-0.110537	4.800517
565.689404	7950.642638	9.365927	-0.110520	4.802913
565.745915	7958.599535	9.370931	-0.110536	4.805274
565.949576	7966.685650	9.375936	-0.110579	4.807670
566.280337	7974.686013	9.380941	-0.110646	4.810040
566.271482	7982.725643	9.385946	-0.110649	4.812421
566.607354	7990.073921	9.390951	-0.110717	4.814596
566.393454	7994.675329	9.395955	-0.110680	4.815958

566.803887	7997.128143	9.400960	-0.110758	4.816682
567.160058	7998.467211	9.405965	-0.110825	4.817077
567.145058	7998.891223	9.410970	-0.110823	4.817202
567.005126	8000.069042	9.415975	-0.110797	4.817551
566.909860	8000.057083	9.420979	-0.110780	4.817548
567.274716	8000.082530	9.425984	-0.110848	4.817554
567.674645	8000.012455	9.430989	-0.110922	4.817532
567.411754	8000.032847	9.435994	-0.110873	4.817539
567.886559	8000.007150	9.440999	-0.110962	4.817529
567.541034	8000.073813	9.446003	-0.110897	4.817551
567.298095	8000.112442	9.451008	-0.110852	4.817563
567.456347	8000.153834	9.456013	-0.110882	4.817575
567.635660	8000.076276	9.461018	-0.110915	4.817551
567.600926	8000.195027	9.466023	-0.110909	4.817586
567.430285	8000.101743	9.471027	-0.110877	4.817559
567.780504	8000.132252	9.476032	-0.110942	4.817567
568.145418	8000.051106	9.481037	-0.111010	4.817541
567.650739	8000.127174	9.486042	-0.110918	4.817566
567.908600	8000.167929	9.491047	-0.110966	4.817577
567.574006	8000.150320	9.496051	-0.110904	4.817573
567.905457	8000.108785	9.501056	-0.110966	4.817559
567.602760	8000.169749	9.506061	-0.110909	4.817579
567.923220	8000.124885	9.511066	-0.110969	4.817564
568.187929	8000.155187	9.516071	-0.111018	4.817572
568.072309	8000.090156	9.521075	-0.110997	4.817553
568.160678	8000.112574	9.526080	-0.111013	4.817559
568.469127	8000.101306	9.531085	-0.111071	4.817555
568.152287	8000.175781	9.536090	-0.111012	4.817578
568.433082	8000.146162	9.541095	-0.111064	4.817568
568.592259	8000.117912	9.546099	-0.111094	4.817559
568.407753	8000.138406	9.551104	-0.111060	4.817566
568.452713	8000.138018	9.556109	-0.111068	4.817566
568.859038	8000.066984	9.561114	-0.111144	4.817543
568.675213	8000.102264	9.566119	-0.111110	4.817554
568.612220	8000.121389	9.571123	-0.111098	4.817560
568.454780	8000.163392	9.576128	-0.111069	4.817573
568.763223	8000.108852	9.581133	-0.111126	4.817556
568.935439	8000.082905	9.586138	-0.111158	4.817547
569.122747	8000.116286	9.591143	-0.111193	4.817556
568.967489	8000.073886	9.596147	-0.111164	4.817544
568.653704	8000.158961	9.601152	-0.111106	4.817571
568.671953	8000.215172	9.606157	-0.111109	4.817587
569.091746	8000.128505	9.611162	-0.111187	4.817560
569.429535	8000.132450	9.616167	-0.111250	4.817560
569.242893	8000.179298	9.621171	-0.111216	4.817574
569.612622	8000.129887	9.626176	-0.111285	4.817558
569.478515	8000.152182	9.631181	-0.111260	4.817565
568.780051	8000.247397	9.636186	-0.111130	4.817596
569.250290	8000.194196	9.641191	-0.111217	4.817579
569.264158	8000.199681	9.646195	-0.111220	4.817580
569.234134	8000.200296	9.651200	-0.111214	4.817581
568.925385	8000.253781	9.656205	-0.111157	4.817598
569.280263	8000.195707	9.661210	-0.111223	4.817579
569.511705	8000.209689	9.666215	-0.111266	4.817582
568.800232	8000.308933	9.671219	-0.111134	4.817615
569.138957	8000.225289	9.676224	-0.111197	4.817588
569.676988	8000.219532	9.681229	-0.111297	4.817584
569.378835	8000.134909	9.686234	-0.111242	4.817561
569.769666	8000.149138	9.691239	-0.111314	4.817563
569.529561	8000.216304	9.696243	-0.111270	4.817584
569.556538	8000.204041	9.701248	-0.111275	4.817580
569.585601	8000.239304	9.706253	-0.111280	4.817591
569.411952	8000.181854	9.711258	-0.111248	4.817574
569.803206	8000.195035	9.716263	-0.111321	4.817576
569.414985	8000.214624	9.721267	-0.111249	4.817584
569.794677	8000.178027	9.726272	-0.111319	4.817571
569.946230	8000.142276	9.731277	-0.111348	4.817560
569.620935	8000.177574	9.736282	-0.111287	4.817572
569.886714	8000.201563	9.741287	-0.111337	4.817578
570.286166	8000.102987	9.746291	-0.111411	4.817547
570.187871	8000.118422	9.751296	-0.111393	4.817552
570.318249	8000.069692	9.756301	-0.111417	4.817537
569.895187	8000.103543	9.761306	-0.111338	4.817549
569.932487	8000.210700	9.766311	-0.111345	4.817581
569.829548	8000.175405	9.771315	-0.111326	4.817571
570.107860	8000.121476	9.776320	-0.111378	4.817553
570.235210	8000.129696	9.781325	-0.111402	4.817555
570.657250	8000.089505	9.786330	-0.111480	4.817542
570.200382	8000.186182	9.791335	-0.111395	4.817572
570.057087	8000.109126	9.796339	-0.111369	4.817550
570.076050	8000.155851	9.801344	-0.111372	4.817564
570.246232	8000.097155	9.806349	-0.111404	4.817546
570.455996	8000.077042	9.811354	-0.111443	4.817539
570.835716	8000.092165	9.816359	-0.111514	4.817542
570.603828	8000.117233	9.821363	-0.111471	4.817550
570.253355	8000.175378	9.826368	-0.111405	4.817569
570.582206	8000.158083	9.831373	-0.111467	4.817562
570.109095	8000.164805	9.836378	-0.111379	4.817566
570.515118	8000.120155	9.841383	-0.111454	4.817551
570.136196	8000.192654	9.846387	-0.111384	4.817574
570.290624	8000.173834	9.851392	-0.111413	4.817568
570.632385	8000.106067	9.856397	-0.111476	4.817547
570.452099	8000.103402	9.861402	-0.111443	4.817547
570.689224	8000.170244	9.866407	-0.111487	4.817565
570.618841	8000.144929	9.871411	-0.111474	4.817558
570.846362	8000.111358	9.876416	-0.111516	4.817547
570.870967	8000.118058	9.881421	-0.111521	4.817549
570.588450	8000.117046	9.886426	-0.111468	4.817550
570.649735	8000.138010	9.891431	-0.111480	4.817556
570.587767	8000.163483	9.896435	-0.111468	4.817564
570.256424	8000.190246	9.901440	-0.111407	4.817573
570.326875	8000.227178	9.906445	-0.111420	4.817584
570.483673	8000.145064	9.911450	-0.111449	4.817559
570.434392	8000.228776	9.916455	-0.111440	4.817584
570.204740	8000.228546	9.921459	-0.111397	4.817585
570.375529	8000.176192	9.926464	-0.111429	4.817568
570.715548	8000.246668	9.931469	-0.111492	4.817588
570.425541	8000.214936	9.936474	-0.111438	4.817580
570.697746	8000.169360	9.941479	-0.111489	4.817565
570.986991	8000.075485	9.946483	-0.111543	4.817536
571.160326	8000.119219	9.951488	-0.111575	4.817548
570.720809	8000.168656	9.956493	-0.111494	4.817565
570.706314	8000.118836	9.961498	-0.111491	4.817550
571.223114	8000.101159	9.966503	-0.111587	4.817542
570.938878	8000.157116	9.971507	-0.111534	4.817560
570.717048	8000.167557	9.976512	-0.111493	4.817564
571.029482	8000.155297	9.981517	-0.111551	4.817559
571.030523	8000.127873	9.986522	-0.111551	4.817551
571.051832	8000.148246	9.991527	-0.111555	4.817557
571.207151	8000.054499	9.996531	-0.111584	4.817529
570.940310	8000.110715	10.001536	-0.111535	4.817547
571.090994	8000.143558	10.006541	-0.111563	4.817556
570.765312	8000.139795	10.011546	-0.111502	4.817556
571.071743	8000.135890	10.016551	-0.111559	4.817553
571.254639	8000.082660	10.021555	-0.111593	4.817537
571.660667	8000.066510	10.026560	-0.111669	4.817530
571.723725	8000.074835	10.031565	-0.111681	4.817532
571.140789	8000.082039	10.036570	-0.111572	4.817537
571.020251	8000.164697	10.041575	-0.111550	4.817562
570.857322	8000.128512	10.046579	-0.111520	4.817552
571.252743	8000.103760	10.051584	-0.111593	4.817543
571.318782	8000.143795	10.056589	-0.111606	4.817555
571.120000	8000.111301	10.061594	-0.111569	4.817546
570.553907	8000.246469	10.066599	-0.111463	4.817588
570.578713	8000.225730	10.071603	-0.111468	4.817582
571.039980	8000.160789	10.076608	-0.111554	4.817561
570.681914	8000.217764	10.081613	-0.111487	4.817579
571.005413	8000.098009	10.086618	-0.111547	4.817542
571.080177	8000.175115	10.091623	-0.111561	4.817565
570.497080	8000.198150	10.096627	-0.111453	4.817574
570.658982	8000.169940	10.101632	-0.111483	4.817565
571.120820	8000.136672	10.106637	-0.111569	4.817553
571.136075	8000.105236	10.111642	-0.111572	4.817544
571.342266	8000.117792	10.116647	-0.111610	4.817547
571.522816	8000.090914	10.121651	-0.111644	4.817538
571.063403	8000.181221	10.126656	-0.111559	4.817567
571.008260	8000.173019	10.131661	-0.111548	4.817565
570.828532	8000.175638	10.136666	-0.111515	4.817566
570.948317	8000.234412	10.141671	-0.111537	4.817583
570.783281	8000.230916	10.146675	-0.111507	4.817583
570.583426	8000.220571	10.151680	-0.111469	4.817581
571.092879	8000.191175	10.156685	-0.111564	4.817570
571.586217	8000.080267	10.161690	-0.111656	4.817535
571.611601	8000.103867	10.166695	-0.111661	4.817542
571.684742	8000.106009	10.171699	-0.111675	4.817542
571.377981	8000.115191	10.176704	-0.111618	4.817546
571.714550	8000.093790	10.181709	-0.111680	4.817538
571.458951	8000.156505	10.186714	-0.111633	4.817558
571.671636	8000.110049	10.191719	-0.111672	4.817543
570.988298	8000.105212	10.196723	-0.111545	4.817545
571.219036	8000.125519	10.201728	-0.111588	4.817550
571.323691	8000.120739	10.206733	-0.111608	4.817548
571.472546	8000.077559	10.211738	-0.111635	4.817534
571.496302	8000.087414	10.216743	-0.111640	4.817537
571.151912	8000.113982	10.221747	-0.111576	4.817547
571.390789	8000.099579	10.226752	-0.111620	4.817541
571.540622	8000.091246	10.231757	-0.111648	4.817538
571.828429	8000.049068	10.236762	-0.111702	4.817524
571.668958	8000.117429	10.241767	-0.111672	4.817545
572.186840	8000.015329	10.246771	-0.111769	4.817513
572.019666	8000.068798	10.251776	-0.111738	4.817529
572.121080	8000.061859	10.256781	-0.111756	4.817527
571.645480	8000.061152	10.261786	-0.111668	4.817529
571.837478	8000.116773	10.266791	-0.111704	4.817544
571.825499	8000.066990	10.271795	-0.111702	4.817530
571.985921	8000.087313	10.276800	-0.111731	4.817535
571.880091	8000.099470	10.281805	-0.111712	4.817539
571.904690	8000.048117	10.286810	-0.111716	4.817524
572.081526	8000.079238	10.291815	-0.111749	4.817532
572.087110	8000.041326	10.296819	-0.111750	4.817521
572.353952	8000.075891	10.301824	-0.111800	4.817530
571.873582	8000.180663	10.306829	-0.111711	4.817563
571.992917	8000.068439	10.311834	-0.111733	4.817529
572.460590	8000.059536	10.316839	-0.111820	4.817525
572.050480	8000.075630	10.321843	-0.111744	4.817531
572.379534	8000.060452	10.326848	-0.111805	4.817525
571.968190	8000.129304	10.331853	-0.111729	4.817547
571.522841	8000.138544	10.336858	-0.111646	4.817552
571.875248	8000.142711	10.341863	-0.111711	4.817552
572.112532	8000.089231	10.346867	-0.111756	4.817535
572.162881	8000.076258	10.351872	-0.111765	4.817531
571.838054	8000.127392	10.356877	-0.111705	4.817547
572.118107	8000.085101	10.361882	-0.111757	4.817534
571.445600	8000.174362	10.366887	-0.111632	4.817563
571.213237	8000.230032	10.371891	-0.111588	4.817581
571.302766	8000.160642	10.376896	-0.111605	4.817560
571.341271	8000.178103	10.381901	-0.111612	4.817565
571.283326	8000.192025	10.386906	-0.111602	4.817569
571.727335	8000.162717	10.391911	-0.111684	4.817558
571.335660	8000.181196	10.396915	-0.111611	4.817566
571.597061	8000.078464	10.401920	-0.111660	4.817534
571.904767	8000.114689	10.406925	-0.111717	4.817543
571.603156	8000.119725	10.411930	-0.111661	4.817546
571.976842	8000.107319	10.416935	-0.111731	4.817541
572.058162	8000.077917	10.421939	-0.111746	4.817532
571.902791	8000.112562	10.426944	-0.111717	4.817543
571.688939	8000.179061	10.431949	-0.111677	4.817563
571.889567	8000.134538	10.436954	-0.111715	4.817549
572.384500	8000.121817	10.441959	-0.111807	4.817543
572.210445	8000.105520	10.446963	-0.111775	4.817539
572.182424	8000.117774	10.451968	-0.111769	4.817543
572.138374	8000.113958	10.456973	-0.111761	4.817542
572.473719	8000.022876	10.461978	-0.111824	4.817514
572.332591	8000.105231	10.466983	-0.111798	4.817539
572.239619	8000.081691	10.471987	-0.111780	4.817532
572.312041	8000.094377	10.476992	-0.111794	4.817536
571.922738	8000.108669	10.481997	-0.111721	4.817542
571.942058	8000.098403	10.487002	-0.111725	4.817538
572.301968	8000.084737	10.492007	-0.111792	4.817533
572.029406	8000.083870	10.497011	-0.111741	4.817534
572.188628	8000.072510	10.502016	-0.111771	4.817530
572.489068	8000.073796	10.507021	-0.111827	4.817529
572.348208	8000.049547	10.512026	-0.111801	4.817522
572.639743	8000.095034	10.517031	-0.111855	4.817534
572.506300	8000.047673	10.522035	-0.111830	4.817521
572.503866	8000.069806	10.527040	-0.111830	4.817527
572.244501	8000.100799	10.532045	-0.111782	4.817538
571.967639	8000.100923	10.537050	-0.111730	4.817539
572.256811	8000.117876	10.542055	-0.111784	4.817543
572.875753	8000.034162	10.547059	-0.111899	4.817515
572.714345	8000.042329	10.552064	-0.111869	4.817518
572.524833	8000.085968	10.557069	-0.111834	4.817532
572.605149	8000.043884	10.562074	-0.111849	4.817519
572.704027	8000.058018	10.567079	-0.111867	4.817523
572.576609	8000.040301	10.572083	-0.111844	4.817518
573.126489	8000.032618	10.577088	-0.111946	4.817514
572.881098	8000.068040	10.582093	-0.111901	4.817525
572.982087	8000.003040	10.587098	-0.111919	4.817506
573.036185	8000.071399	10.592103	-0.111929	4.817526
572.791462	8000.065665	10.597107	-0.111884	4.817525
572.863490	8000.056180	10.602112	-0.111897	4.817522
572.953104	8000.052233	10.607117	-0.111914	4.817520
573.145635	8000.045589	10.612122	-0.111950	4.817517
572.848788	8000.051750	10.617127	-0.111895	4.817521
573.049368	8000.020947	10.622131	-0.111932	4.817511
572.694070	8000.065296	10.627136	-0.111866	4.817525
572.704158	8000.072838	10.632141	-0.111868	4.817527
572.632505	8000.096056	10.637146	-0.111855	4.817535
572.630997	8000.138258	10.642151	-0.111854	4.817547
572.339199	8000.153993	10.647155	-0.111800	4.817553
572.455224	8000.164159	10.652160	-0.111822	4.817556
572.868342	8000.113285	10.657165	-0.111899	4.817539
572.766865	8000.109673	10.662170	-0.111880	4.817538
572.613152	8000.149620	10.667175	-0.111851	4.817551
572.334369	8000.114883	10.672179	-0.111799	4.817542
572.532899	8000.115716	10.677184	-0.111836	4.817541
572.376181	8000.160896	10.682189	-0.111807	4.817555
572.295198	8000.095312	10.687194	-0.111792	4.817536
572.117264	8000.199287	10.692199	-0.111759	4.817567
572.453914	8000.094503	10.697203	-0.111822	4.817535
572.060074	8000.162558	10.702208	-0.111749	4.817557
572.712367	8000.101505	10.707213	-0.111870	4.817536
572.366314	8000.094270	10.712218	-0.111806	4.817535
572.371615	8000.181960	10.717223	-0.111807	4.817561
572.645837	8000.114250	10.722227	-0.111858	4.817540
573.087702	8000.098634	10.727232	-0.111940	4.817533
572.828122	8000.176067	10.732237	-0.111892	4.817557
572.762579	8000.100156	10.737242	-0.111880	4.817535
572.780968	8000.101487	10.742247	-0.111883	4.817536
572.786786	8000.116354	10.747251	-0.111884	4.817540
572.657825	8000.120779	10.752256	-0.111860	4.817542
572.536386	8000.146427	10.757261	-0.111838	4.817550
572.446307	8000.119763	10.762266	-0.111821	4.817542
572.747489	8000.148505	10.767271	-0.111877	4.817550
572.291280	8000.176582	10.772275	-0.111792	4.817560
572.677010	8000.106302	10.777280	-0.111864	4.817537
572.811738	8000.147356	10.782285	-0.111889	4.817549
572.799103	8000.104950	10.787290	-0.111887	4.817537
572.944105	8000.099713	10.792295	-0.111914	4.817534
572.744835	8000.116819	10.797299	-0.111877	4.817540
573.052489	8000.092881	10.802304	-0.111934	4.817532
572.832579	8000.093847	10.807309	-0.111893	4.817533
572.829433	8000.080082	10.812314	-0.111893	4.817529
573.165258	8000.076617	10.817319	-0.111955	4.817527
572.875554	8000.062827	10.822323	-0.111901	4.817524
572.764452	8000.084406	10.827328	-0.111881	4.817531
572.719436	8000.147074	10.832333	-0.111872	4.817549
573.156373	8000.057498	10.837338	-0.111954	4.817521
572.979102	8000.106595	10.842343	-0.111921	4.817536
573.106445	8000.056764	10.847347	-0.111945	4.817521
572.710830	8000.093127	10.852352	-0.111871	4.817533
572.335516	8000.182567	10.857357	-0.111801	4.817561
572.333556	8000.159319	10.862362	-0.111801	4.817555
572.458998	8000.188625	10.867367	-0.111824	4.817563
572.440109	8000.211570	10.872371	-0.111821	4.817570
572.575610	8000.151304	10.877376	-0.111846	4.817551
573.123187	8000.112977	10.882381	-0.111948	4.817537
572.713875	8000.080527	10.887386	-0.111872	4.817530
572.720009	8000.124953	10.892391	-0.111873	4.817543
573.174114	8000.070464	10.897395	-0.111958	4.817525
572.611625	8000.133909	10.902400	-0.111853	4.817546
572.907282	8000.124571	10.907405	-0.111908	4.817542
573.174747	8000.040928	10.912410	-0.111958	4.817516
573.200298	8000.106753	10.917415	-0.111963	4.817535
572.751641	8000.132829	10.922419	-0.111879	4.817545
572.992664	8000.088905	10.927424	-0.111924	4.817531
573.027884	8000.131651	10.932429	-0.111931	4.817543
572.605668	8000.178175	10.937434	-0.111852	4.817559
572.764712	8000.173146	10.942439	-0.111882	4.817557
573.122684	8000.084510	10.947443	-0.111948	4.817529
572.803025	8000.126220	10.952448	-0.111889	4.817543
572.950004	8000.140012	10.957453	-0.111916	4.817546
572.928789	8000.109090	10.962458	-0.111912	4.817537
572.848533	8000.164903	10.967463	-0.111897	4.817554
572.800606	8000.175807	10.972467	-0.111889	4.817557
572.839931	8000.123616	10.977472	-0.111896	4.817542
573.050460	8000.124628	10.982477	-0.111935	4.817541
572.861143	8000.112326	10.987482	-0.111900	4.817538
572.565968	8000.164954	10.992487	-0.111845	4.817555
572.378540	8000.211790	10.997491	-0.111810	4.817570
572.680478	8000.159268	11.002496	-0.111866	4.817553
572.938587	8000.144096	11.007501	-0.111915	4.817547
572.321962	8000.165573	11.012506	-0.111800	4.817556
573.049721	8000.115138	11.017511	-0.111935	4.817538
573.167007	8000.109491	11.022515	-0.111957	4.817536
573.149426	8000.088122	11.027520	-0.111954	4.817530
572.939062	8000.161007	11.032525	-0.111915	4.817552
573.072433	8000.095432	11.037530	-0.111940	4.817532
572.854930	8000.097490	11.042535	-0.111899	4.817534
573.329208	8000.072855	11.047539	-0.111988	4.817525
573.367960	8000.094543	11.052544	-0.111995	4.817531
573.217312	8000.127146	11.057549	-0.111967	4.817541
573.276303	8000.069969	11.062554	-0.111978	4.817524
573.506386	8000.082882	11.067559	-0.112021	4.817527
573.387200	8000.093785	11.072563	-0.111999	4.817531
573.297276	8000.097733	11.077568	-0.111982	4.817532
573.373095	8000.097804	11.082573	-0.111996	4.817532
573.677440	8000.046374	11.087578	-0.112053	4.817515
573.616423	8000.069750	11.092583	-0.112041	4.817522
573.510253	8000.089291	11.097587	-0.112022	4.817529
573.748586	8000.050604	11.102592	-0.112066	4.817516
573.773259	8000.082640	11.107597	-0.112071	4.817526
573.513157	8000.039732	11.112602	-0.112022	4.817514
573.980780	8000.060388	11.117607	-0.112109	4.817518
573.914945	8000.053082	11.122611	-0.112097	4.817516
573.712553	8000.049030	11.127616	-0.112060	4.817516
573.804615	8000.064120	11.132621	-0.112077	4.817520
573.552003	8000.051934	11.137626	-0.112030	4.817517
573.371978	8000.094658	11.142631	-0.111996	4.817531
573.222193	8000.090330	11.147635	-0.111968	4.817530
573.141684	8000.098640	11.152640	-0.111953	4.817533
572.970289	8000.130936	11.157645	-0.111922	4.817543
572.980450	8000.102590	11.162650	-0.111924	4.817535
573.183927	8000.172108	11.167655	-0.111961	4.817555
573.396903	8000.102435	11.172659	-0.112001	4.817533
573.011139	8000.153720	11.177664	-0.111929	4.817550
573.058310	8000.135422	11.182669	-0.111938	4.817544
573.082442	8000.112561	11.187674	-0.111943	4.817537
572.853488	8000.152449	11.192679	-0.111900	4.817550
572.700031	8000.134345	11.197683	-0.111872	4.817546
572.876678	8000.114799	11.202688	-0.111905	4.817539
573.095871	8000.140217	11.207693	-0.111945	4.817546
572.938927	8000.130505	11.212698	-0.111916	4.817543
572.627311	8000.179723	11.217703	-0.111858	4.817559
572.939084	8000.116792	11.222707	-0.111916	4.817539
573.123931	8000.119534	11.227712	-0.111951	4.817539
573.473580	8000.103608	11.232717	-0.112016	4.817533
573.268164	8000.095289	11.237722	-0.111978	4.817532
573.082700	8000.134765	11.242727	-0.111943	4.817544
572.842416	8000.118541	11.247731	-0.111898	4.817540
572.698744	8000.163915	11.252736	-0.111872	4.817554
573.157326	8000.132714	11.257741	-0.111957	4.817543
572.624337	8000.136430	11.262746	-0.111858	4.817547
572.641735	8000.181023	11.267751	-0.111861	4.817560
573.218844	8000.073469	11.272755	-0.111969	4.817525
572.840076	8000.086859	11.277760	-0.111898	4.817531
572.380140	8000.206711	11.282765	-0.111813	4.817568
572.577620	8000.163197	11.287770	-0.111850	4.817555
572.369525	8000.261448	11.292775	-0.111811	4.817585
572.116389	8000.324198	11.297779	-0.111764	4.817604
572.253503	8000.177404	11.302784	-0.111789	4.817560
572.419903	8000.241093	11.307789	-0.111820	4.817578
572.570538	8000.153608	11.312794	-0.111848	4.817552
573.231132	8000.115900	11.317799	-0.111971	4.817538
573.202189	8000.107030	11.322803	-0.111966	4.817535
572.773626	8000.155570	11.327808	-0.111886	4.817551
573.228170	8000.125365	11.332813	-0.111971	4.817541
573.166015	8000.144503	11.337818	-0.111959	4.817547
572.739594	8000.224741	11.342823	-0.111880	4.817572
573.187077	8000.131099	11.347827	-0.111963	4.817542
572.636703	8000.206334	11.352832	-0.111861	4.817567
573.144798	8000.175867	11.357837	-0.111956	4.817556
572.726402	8000.208725	11.362842	-0.111878	4.817567
573.109297	8000.170069	11.367847	-0.111949	4.817554
573.144830	8000.168488	11.372851	-0.111956	4.817554
572.870209	8000.171810	11.377856	-0.111905	4.817556
572.520976	8000.250025	11.382861	-0.111840	4.817581
573.275382	8000.085988	11.387866	-0.111980	4.817529
573.257139	8000.149054	11.392871	-0.111977	4.817547
573.527681	8000.144622	11.397875	-0.112027	4.817545
573.338963	8000.125995	11.402880	-0.111992	4.817540
573.730755	8000.120194	11.407885	-0.112065	4.817537
573.615320	8000.077320	11.412890	-0.112044	4.817525
573.482864	8000.107026	11.417895	-0.112019	4.817534
573.873786	8000.065324	11.422899	-0.112092	4.817520
573.739630	8000.057005	11.427904	-0.112067	4.817518
573.397307	8000.106823	11.432909	-0.112003	4.817534
573.081694	8000.145426	11.437914	-0.111945	4.817547
573.311282	8000.224831	11.442919	-0.111987	4.817570
572.880004	8000.225831	11.447923	-0.111907	4.817572
573.337931	8000.112288	11.452928	-0.111992	4.817536
573.709197	8000.132572	11.457933	-0.112062	4.817541
573.499245	8000.117852	11.462938	-0.112022	4.817537
573.310421	8000.159389	11.467943	-0.111987	4.817550
573.481195	8000.111257	11.472947	-0.112019	4.817535
573.460586	8000.161621	11.477952	-0.112015	4.817550
573.185604	8000.208215	11.482957	-0.111964	4.817565
573.299066	8000.142345	11.487962	-0.111985	4.817545
573.477344	8000.180879	11.492967	-0.112019	4.817556
573.352892	8000.199093	11.497971	-0.111996	4.817562
573.861721	8000.093694	11.502976	-0.112090	4.817528
573.854409	8000.147422	11.507981	-0.112089	4.817544
573.905960	8000.104912	11.512986	-0.112099	4.817532
574.251144	8000.092087	11.517991	-0.112163	4.817526
573.935160	8000.116962	11.522995	-0.112104	4.817535
573.739725	8000.116179	11.528000	-0.112068	4.817536
574.057202	8000.070221	11.533005	-0.112127	4.817521
573.889405	8000.062459	11.538010	-0.112096	4.817519
573.785986	8000.089429	11.543015	-0.112076	4.817527
573.839658	8000.084950	11.548019	-0.112086	4.817526
573.814428	8000.078246	11.553024	-0.112082	4.817524
574.078361	8000.075828	11.558029	-0.112131	4.817522
573.598222	8000.099325	11.563034	-0.112042	4.817531
573.985717	8000.078683	11.568039	-0.112114	4.817523
574.008350	8000.080077	11.573043	-0.112118	4.817524
573.829158	8000.094313	11.578048	-0.112085	4.817529
573.719209	8000.130686	11.583053	-0.112064	4.817540
573.532502	8000.061422	11.588058	-0.112030	4.817520
573.773286	8000.100883	11.593063	-0.112074	4.817531
574.016499	8000.074936	11.598067	-0.112120	4.817522
573.804557	8000.074964	11.603072	-0.112080	4.817523
573.689911	8000.105990	11.608077	-0.112059	4.817533
573.608307	8000.053061	11.613082	-0.112044	4.817517
573.488603	8000.122012	11.618087	-0.112022	4.817538
573.578916	8000.083243	11.623091	-0.112038	4.817527
573.614876	8000.094334	11.628096	-0.112045	4.817530
574.177219	8000.043562	11.633101	-0.112150	4.817512
573.828475	8000.026784	11.638106	-0.112085	4.817509
573.513009	8000.083334	11.643111	-0.112026	4.817527
573.875580	8000.072877	11.648115	-0.112094	4.817522
573.754623	8000.080588	11.653120	-0.112071	4.817525
573.445773	8000.133013	11.658125	-0.112014	4.817542
573.314897	8000.100465	11.663130	-0.111990	4.817533
573.575930	8000.103281	11.668135	-0.112038	4.817532
573.596080	8000.095139	11.673139	-0.112042	4.817530
573.915418	8000.071375	11.678144	-0.112102	4.817522
573.966640	8000.093249	11.683149	-0.112111	4.817528
573.610873	8000.092201	11.688154	-0.112045	4.817529
574.001324	8000.065269	11.693159	-0.112118	4.817519
573.305442	8000.171068	11.698163	-0.111988	4.817554
573.262614	8000.132437	11.703168	-0.111980	4.817542
573.809414	8000.121545	11.708173	-0.112082	4.817537
573.764609	8000.078661	11.713178	-0.112074	4.817524
573.828956	8000.108118	11.718183	-0.112086	4.817533
573.846175	8000.069321	11.723187	-0.112089	4.817521
573.527361	8000.079376	11.728192	-0.112030	4.817526
573.914162	8000.092502	11.733197	-0.112102	4.817528
574.026393	8000.048779	11.738202	-0.112123	4.817514
573.507259	8000.090699	11.743207	-0.112026	4.817529
573.506106	8000.121296	11.748211	-0.112026	4.817538
573.330913	8000.100758	11.753216	-0.111993	4.817533
573.672505	8000.096324	11.758221	-0.112057	4.817530
573.436927	8000.127668	11.763226	-0.112013	4.817540
573.400625	8000.155633	11.768231	-0.112006	4.817549
573.513443	8000.108753	11.773235	-0.112027	4.817534
573.601986	8000.081569	11.778240	-0.112044	4.817526
573.718765	8000.116025	11.783245	-0.112066	4.817536
573.351474	8000.113751	11.788250	-0.111997	4.817537
573.784460	8000.120172	11.793255	-0.112078	4.817537
573.900907	8000.114512	11.798259	-0.112100	4.817534
573.859517	8000.099124	11.803264	-0.112092	4.817530
573.705811	8000.122182	11.808269	-0.112064	4.817537
573.849374	8000.078924	11.813274	-0.112090	4.817524
573.850424	8000.078943	11.818279	-0.112091	4.817524
573.634801	8000.112694	11.823283	-0.112050	4.817535
573.780842	8000.080028	11.828288	-0.112078	4.817525
574.190598	8000.091384	11.833293	-0.112154	4.817526
574.274970	8000.028248	11.838298	-0.112170	4.817507
574.181727	8000.052202	11.843303	-0.112152	4.817515
573.970987	8000.068081	11.848307	-0.112113	4.817520
574.087043	8000.039194	11.853312	-0.112135	4.817511
574.383368	8000.063646	11.858317	-0.112190	4.817517
573.996739	8000.047361	11.863322	-0.112118	4.817514
573.929141	8000.094918	11.868327	-0.112106	4.817528
574.021112	8000.076229	11.873331	-0.112123	4.817522
573.836588	8000.041830	11.878336	-0.112088	4.817513
573.575509	8000.143519	11.883341	-0.112040	4.817544
573.622553	8000.146330	11.888346	-0.112049	4.817545
573.730115	8000.119428	11.893351	-0.112069	4.817537
573.914678	8000.113722	11.898355	-0.112103	4.817534
573.730619	8000.096219	11.903360	-0.112069	4.817530
573.455686	8000.143869	11.908365	-0.112018	4.817545
573.536740	8000.100740	11.913370	-0.112033	4.817532
573.312636	8000.132255	11.918375	-0.111991	4.817542
573.959114	8000.115452	11.923379	-0.112112	4.817534
573.825135	8000.071246	11.928384	-0.112087	4.817522
573.901425	8000.116714	11.933389	-0.112101	4.817535
573.819515	8000.091225	11.938394	-0.112086	4.817528
573.850877	8000.053693	11.943399	-0.112092	4.817517
573.992527	8000.063185	11.948403	-0.112118	4.817519
573.752487	8000.081796	11.953408	-0.112073	4.817525
573.821025	8000.111315	11.958413	-0.112086	4.817534
573.593417	8000.111111	11.963418	-0.112044	4.817535
573.845139	8000.139123	11.968423	-0.112091	4.817542
573.647346	8000.123528	11.973427	-0.112054	4.817538
573.577693	8000.114054	11.978432	-0.112041	4.817536
573.843521	8000.139109	11.983437	-0.112091	4.817542
574.036501	8000.063861	11.988442	-0.112127	4.817519
573.405151	8000.190672	11.993447	-0.112009	4.817559
573.175423	8000.242159	11.998451	-0.111966	4.817575
573.459343	8000.142926	12.003456	-0.112019	4.817545
573.563021	8000.207799	12.008461	-0.112039	4.817563
573.492470	8000.185645	12.013466	-0.112025	4.817557
573.682298	8000.172629	12.018471	-0.112061	4.817552
573.597340	8000.179817	12.023475	-0.112045	4.817555
573.667263	8000.128079	12.028480	-0.112058	4.817539
573.667929	8000.177703	12.033485	-0.112058	4.817554
573.912465	8000.103220	12.038490	-0.112104	4.817531
574.105198	8000.098691	12.043495	-0.112140	4.817529
574.056454	8000.073694	12.048499	-0.112131	4.817522
574.018679	8000.058359	12.053504	-0.112124	4.817517
573.914845	8000.159212	12.058509	-0.112104	4.817547
574.174746	8000.065957	12.063514	-0.112153	4.817519
574.200048	8000.083224	12.068519	-0.112158	4.817524
574.258862	8000.091488	12.073523	-0.112169	4.817526
573.863563	8000.067686	12.078528	-0.112095	4.817521
573.882154	8000.085909	12.083533	-0.112099	4.817526
574.150947	8000.071953	12.088538	-0.112149	4.817521
574.291471	8000.088817	12.093543	-0.112175	4.817525
573.850608	8000.103395	12.098547	-0.112093	4.817531
573.760836	8000.078846	12.103552	-0.112076	4.817524
573.918686	8000.160356	12.108557	-0.112106	4.817548
573.596416	8000.139748	12.113562	-0.112046	4.817543
574.038089	8000.104076	12.118567	-0.112128	4.817531
573.884035	8000.107073	12.123571	-0.112099	4.817532
573.464307	8000.146243	12.128576	-0.112021	4.817546
574.136783	8000.097104	12.133581	-0.112146	4.817528
573.962742	8000.076582	12.138586	-0.112114	4.817523
573.844118	8000.091716	12.143591	-0.112092	4.817528
573.729576	8000.093188	12.148595	-0.112071	4.817529
573.442068	8000.140651	12.153600	-0.112017	4.817544
573.624274	8000.149688	12.158605	-0.112051	4.817546
573.825656	8000.069288	12.163610	-0.112089	4.817521
573.325464	8000.148432	12.168615	-0.111996	4.817547
573.714168	8000.126752	12.173619	-0.112068	4.817539
573.575772	8000.132093	12.178624	-0.112042	4.817541
573.562049	8000.176226	12.183629	-0.112040	4.817554
573.284558	8000.176338	12.188634	-0.111988	4.817555
573.310289	8000.175667	12.193639	-0.111993	4.817555
573.342386	8000.182479	12.198643	-0.111999	4.817557
573.643353	8000.153166	12.203648	-0.112055	4.817547
573.713323	8000.162650	12.208653	-0.112068	4.817549
573.653939	8000.138551	12.213658	-0.112057	4.817542
574.053114	8000.104360	12.218663	-0.112131	4.817531
573.561439	8000.160408	12.223667	-0.112040	4.817549
573.595047	8000.125021	12.228672	-0.112046	4.817539
573.199069	8000.264821	12.233677	-0.111973	4.817582
573.305296	8000.170343	12.238682	-0.111992	4.817553
573.425751	8000.172131	12.243687	-0.112015	4.817553
573.782426	8000.109866	12.248691	-0.112081	4.817533
573.857401	8000.066647	12.253696	-0.112095	4.817520
573.834188	8000.127528	12.258701	-0.112091	4.817538
573.500719	8000.147922	12.263706	-0.112029	4.817546
573.824345	8000.111555	12.268711	-0.112089	4.817534
574.107393	8000.096754	12.273715	-0.112142	4.817528
574.083210	8000.045732	12.278720	-0.112137	4.817513
573.399888	8000.155939	12.283725	-0.112010	4.817549
573.799290	8000.116474	12.288730	-0.112085	4.817535
573.827567	8000.136952	12.293735	-0.112090	4.817541
573.951883	8000.098687	12.298739	-0.112113	4.817529
573.733628	8000.120788	12.303744	-0.112073	4.817537
573.696769	8000.158244	12.308749	-0.112066	4.817548
573.756267	8000.121129	12.313754	-0.112077	4.817537
574.087853	8000.085937	12.318759	-0.112139	4.817525
574.038324	8000.090483	12.323763	-0.112129	4.817527
573.639270	8000.121515	12.328768	-0.112055	4.817537
573.564694	8000.156302	12.333773	-0.112041	4.817548
574.061579	8000.109837	12.338778	-0.112134	4.817532
573.259736	8000.160232	12.343783	-0.111985	4.817551
573.377643	8000.156705	12.348787	-0.112007	4.817549
573.461066	8000.125223	12.353792	-0.112022	4.817539
573.432023	8000.219795	12.358797	-0.112017	4.817567
573.754583	8000.098968	12.363802	-0.112077	4.817530
573.851107	8000.126791	12.368807	-0.112095	4.817538
574.074726	8000.130110	12.373811	-0.112137	4.817538
573.754162	8000.101083	12.378816	-0.112077	4.817531
573.718504	8000.139613	12.383821	-0.112070	4.817542
573.810727	8000.138872	12.388826	-0.112088	4.817542
574.166239	8000.094534	12.393831	-0.112154	4.817527
574.016020	8000.094421	12.398835	-0.112126	4.817528
573.451565	8000.135668	12.403840	-0.112021	4.817542
573.786739	8000.153306	12.408845	-0.112083	4.817546
573.186033	8000.207738	12.413850	-0.111972	4.817565
573.761111	8000.141321	12.418855	-0.112079	4.817543
574.056431	8000.123536	12.423859	-0.112134	4.817536
574.105596	8000.029267	12.428864	-0.112143	4.817508
573.966549	8000.115876	12.433869	-0.112117	4.817534
573.920462	8000.095140	12.438874	-0.112108	4.817528
573.924570	8000.104704	12.443879	-0.112109	4.817531
573.941231	8000.135566	12.448883	-0.112112	4.817540
573.643619	8000.105823	12.453888	-0.112057	4.817533
574.029256	8000.122099	12.458893	-0.112129	4.817536
573.787714	8000.120632	12.463898	-0.112084	4.817537
573.719570	8000.114347	12.468903	-0.112071	4.817535
573.551742	8000.175196	12.473907	-0.112040	4.817554
573.784907	8000.131155	12.478912	-0.112083	4.817540
574.161606	8000.126188	12.483917	-0.112154	4.817537
574.047728	8000.102335	12.488922	-0.112132	4.817530
574.379479	8000.065034	12.493927	-0.112194	4.817517
573.762571	8000.107614	12.498931	-0.112079	4.817533
573.762228	8000.086501	12.503936	-0.112079	4.817527
573.872889	8000.147256	12.508941	-0.112100	4.817544
573.873191	8000.076541	12.513946	-0.112100	4.817523
573.916095	8000.064513	12.518951	-0.112108	4.817519
574.133460	8000.058239	12.523955	-0.112149	4.817517
574.104504	8000.068368	12.528960	-0.112143	4.817520
573.523488	8000.155814	12.533965	-0.112035	4.817548
573.908688	8000.117194	12.538970	-0.112107	4.817535
574.099124	8000.140076	12.543975	-0.112143	4.817541
574.055267	8000.110929	12.548979	-0.112134	4.817532
573.997541	8000.077353	12.553984	-0.112124	4.817523
573.971519	8000.177250	12.558989	-0.112119	4.817552
573.766724	8000.156272	12.563994	-0.112081	4.817547
573.896723	8000.081146	12.568999	-0.112105	4.817524
573.791109	8000.061639	12.574003	-0.112085	4.817519
573.391060	8000.122212	12.579008	-0.112011	4.817539
574.073140	8000.098548	12.584013	-0.112138	4.817529
574.402947	8000.032718	12.589018	-0.112199	4.817508
573.902722	8000.106584	12.594023	-0.112106	4.817532
573.749324	8000.146535	12.599027	-0.112078	4.817544
573.922150	8000.125878	12.604032	-0.112110	4.817537
574.276722	8000.095249	12.609037	-0.112176	4.817527
574.481710	8000.062402	12.614042	-0.112214	4.817516
574.076050	8000.079613	12.619047	-0.112139	4.817523
574.238245	8000.087299	12.624051	-0.112169	4.817525
573.977504	8000.077103	12.629056	-0.112120	4.817523
573.722614	8000.161994	12.634061	-0.112073	4.817549
574.077742	8000.092317	12.639066	-0.112139	4.817527
574.310302	8000.086268	12.644071	-0.112183	4.817524
574.283362	8000.074260	12.649075	-0.112178	4.817521
574.153808	8000.068121	12.654080	-0.112153	4.817519
574.412873	8000.094132	12.659085	-0.112202	4.817526
573.948404	8000.116804	12.664090	-0.112115	4.817535
574.011102	8000.108237	12.669095	-0.112127	4.817532
574.419233	8000.090013	12.674099	-0.112203	4.817525
574.366512	8000.093457	12.679104	-0.112193	4.817526
574.174641	8000.107504	12.684109	-0.112158	4.817531
574.194331	8000.096188	12.689114	-0.112161	4.817527
574.345239	8000.095261	12.694119	-0.112189	4.817527
574.305875	8000.114737	12.699123	-0.112182	4.817532
574.207480	8000.083725	12.704128	-0.112164	4.817524
574.256191	8000.119284	12.709133	-0.112173	4.817534
574.219410	8000.134575	12.714138	-0.112166	4.817539
574.474169	8000.118300	12.719143	-0.112214	4.817533
574.412776	8000.114226	12.724147	-0.112202	4.817532
574.499119	8000.087009	12.729152	-0.112218	4.817523
574.543987	8000.127789	12.734157	-0.112227	4.817535
574.233879	8000.105249	12.739162	-0.112169	4.817530
574.455029	8000.110643	12.744167	-0.112210	4.817531
574.443714	8000.110478	12.749171	-0.112208	4.817531
574.046383	8000.113034	12.754176	-0.112134	4.817533
574.098120	8000.107471	12.759181	-0.112144	4.817531
574.046963	8000.113049	12.764186	-0.112134	4.817533
574.252684	8000.065435	12.769191	-0.112173	4.817518
573.918767	8000.123821	12.774195	-0.112111	4.817537
573.684905	8000.114024	12.779200	-0.112067	4.817535
573.415354	8000.180754	12.784205	-0.112017	4.817556
573.402523	8000.164734	12.789210	-0.112015	4.817551
573.294402	8000.157856	12.794215	-0.111995	4.817550
573.752146	8000.126645	12.799219	-0.112080	4.817538
573.827171	8000.099260	12.804224	-0.112094	4.817530
573.907292	8000.113117	12.809229	-0.112109	4.817534
573.775729	8000.127003	12.814234	-0.112084	4.817538
573.997691	8000.050074	12.819239	-0.112126	4.817515
573.828520	8000.120403	12.824243	-0.112094	4.817536
573.661300	8000.142205	12.829248	-0.112063	4.817543
573.733213	8000.150663	12.834253	-0.112077	4.817546
573.195794	8000.192311	12.839258	-0.111977	4.817560
573.676517	8000.182551	12.844263	-0.112066	4.817555
574.223628	8000.097776	12.849267	-0.112168	4.817528
573.850264	8000.123911	12.854272	-0.112099	4.817537
573.951322	8000.099023	12.859277	-0.112117	4.817529
574.183235	8000.113020	12.864282	-0.112161	4.817532
574.330937	8000.069823	12.869287	-0.112188	4.817519
574.367516	8000.113647	12.874291	-0.112195	4.817532
574.204224	8000.091173	12.879296	-0.112165	4.817526
574.021611	8000.109580	12.884301	-0.112131	4.817532
573.947413	8000.126428	12.889306	-0.112117	4.817537
574.232340	8000.113766	12.894311	-0.112170	4.817532
574.117771	8000.107849	12.899315	-0.112149	4.817531
573.470696	8000.161593	12.904320	-0.112028	4.817550
573.990138	8000.137629	12.909325	-0.112125	4.817541
573.895849	8000.130957	12.914330	-0.112108	4.817539
573.761330	8000.151132	12.919335	-0.112083	4.817546
574.094908	8000.115970	12.924339	-0.112145	4.817534
574.182220	8000.096156	12.929344	-0.112161	4.817527
574.729041	8000.078933	12.934349	-0.112263	4.817520
574.646079	8000.039705	12.939354	-0.112247	4.817509
574.636150	8000.062784	12.944359	-0.112246	4.817516
574.822101	8000.034933	12.949363	-0.112280	4.817507
574.773630	8000.021550	12.954368	-0.112271	4.817503
575.029300	8000.044345	12.959373	-0.112319	4.817508
574.668769	8000.056946	12.964378	-0.112252	4.817514
574.823398	8000.085632	12.969383	-0.112281	4.817522
574.473096	8000.109997	12.974387	-0.112215	4.817530
574.606316	8000.087697	12.979392	-0.112240	4.817523
574.796296	8000.121129	12.984397	-0.112276	4.817532
574.667458	8000.060109	12.989402	-0.112252	4.817515
574.143389	8000.105120	12.994407	-0.112154	4.817530
574.583457	8000.078926	12.999411	-0.112236	4.817521
574.465157	8000.076119	13.004416	-0.112214	4.817520
574.667487	8000.099178	13.009421	-0.112252	4.817526
575.041509	8000.065672	13.014426	-0.112322	4.817515
574.690671	8000.078417	13.019431	-0.112256	4.817520
574.804705	8000.088556	13.024435	-0.112278	4.817522
574.370525	8000.065231	13.029440	-0.112197	4.817517
574.289655	8000.102036	13.034445	-0.112182	4.817529
573.984454	8000.084847	13.039450	-0.112125	4.817525
573.949735	8000.124447	13.044455	-0.112119	4.817537
574.439080	8000.091594	13.049459	-0.112210	4.817525
574.613009	8000.040341	13.054464	-0.112242	4.817509
574.799032	8000.051548	13.059469	-0.112277	4.817512
574.885275	8000.052830	13.064474	-0.112293	4.817512
574.720170	8000.084163	13.069479	-0.112262	4.817522
574.798283	8000.057879	13.074483	-0.112277	4.817513
574.398535	8000.092066	13.079488	-0.112202	4.817525
574.281477	8000.153668	13.084493	-0.112181	4.817544
574.663219	8000.100220	13.089498	-0.112252	4.817527
574.459907	8000.119375	13.094503	-0.112214	4.817533
574.453231	8000.171003	13.099507	-0.112213	4.817548
574.447332	8000.105472	13.104512	-0.112212	4.817529
574.529465	8000.083471	13.109517	-0.112227	4.817522
574.579707	8000.055718	13.114522	-0.112236	4.817514
574.560279	8000.053322	13.119527	-0.112233	4.817513
574.548334	8000.113316	13.124531	-0.112231	4.817531
574.659147	8000.070628	13.129536	-0.112251	4.817518
575.006187	8000.066277	13.134541	-0.112316	4.817515
575.120466	8000.021530	13.139546	-0.112337	4.817501
575.137814	8000.020734	13.144551	-0.112340	4.817501
575.116119	8000.066862	13.149555	-0.112336	4.817515
574.626236	8000.090211	13.154560	-0.112245	4.817524
574.633277	8000.085041	13.159565	-0.112247	4.817522
574.757581	8000.110110	13.164570	-0.112270	4.817529
574.834465	8000.060585	13.169575	-0.112284	4.817514
575.018872	8000.084435	13.174579	-0.112319	4.817520
574.307439	8000.067555	13.179584	-0.112186	4.817518
574.958608	8000.072992	13.184589	-0.112307	4.817517
575.070182	8000.067260	13.189594	-0.112328	4.817515
574.831005	8000.048938	13.194599	-0.112284	4.817511
574.579684	8000.102216	13.199603	-0.112237	4.817527
574.607177	8000.092070	13.204608	-0.112242	4.817524
575.097240	8000.063452	13.209613	-0.112333	4.817514
574.796311	8000.068492	13.214618	-0.112277	4.817517
574.590190	8000.111884	13.219623	-0.112239	4.817530
574.673797	8000.102571	13.224627	-0.112255	4.817527
574.695747	8000.074399	13.229632	-0.112259	4.817519
575.004229	8000.068421	13.234637	-0.112316	4.817516
574.780434	8000.071439	13.239642	-0.112275	4.817517
574.189722	8000.099628	13.244647	-0.112165	4.817528
574.536876	8000.107945	13.249651	-0.112229	4.817529
574.593473	8000.076064	13.254656	-0.112240	4.817520
574.233349	8000.152007	13.259661	-0.112173	4.817544
574.703159	8000.071364	13.264666	-0.112260	4.817518
575.171821	8000.064595	13.269671	-0.112348	4.817514
575.256106	8000.071126	13.274675	-0.112364	4.817515
574.811524	8000.070869	13.279680	-0.112281	4.817517
574.843546	8000.084014	13.284685	-0.112287	4.817521
574.906507	8000.090229	13.289690	-0.112299	4.817522
574.602044	8000.071994	13.294695	-0.112242	4.817518
574.671615	8000.090973	13.299699	-0.112255	4.817524
574.683898	8000.070047	13.304704	-0.112257	4.817517
575.051543	8000.047002	13.309709	-0.112326	4.817509
575.124607	8000.011143	13.314714	-0.112339	4.817498
574.915925	8000.037607	13.319719	-0.112301	4.817507
575.160099	8000.051788	13.324723	-0.112346	4.817510
575.032452	7999.995007	13.329728	-0.112322	4.817494
575.037972	8000.035204	13.334733	-0.112323	4.817506
575.095626	8000.045563	13.339738	-0.112334	4.817508
574.326762	8000.104888	13.344743	-0.112191	4.817529
575.063440	8000.095760	13.349747	-0.112328	4.817523
575.057430	8000.061895	13.354752	-0.112327	4.817513
574.862667	8000.093844	13.359757	-0.112291	4.817524
574.732381	8000.102470	13.364762	-0.112267	4.817527
574.914241	8000.075614	13.369767	-0.112301	4.817518
575.125611	8000.075586	13.374771	-0.112340	4.817517
575.093273	8000.033941	13.379776	-0.112334	4.817505
575.204618	8000.078875	13.384781	-0.112355	4.817518
575.224754	8000.074954	13.389786	-0.112359	4.817517
575.153821	8000.057016	13.394791	-0.112345	4.817512
575.096573	8000.081504	13.399795	-0.112335	4.817519
574.981104	8000.033348	13.404800	-0.112313	4.817505
575.041454	8000.081748	13.409805	-0.112325	4.817519
575.124249	8000.065034	13.414810	-0.112340	4.817514
575.267830	8000.001720	13.419815	-0.112367	4.817495
575.211178	8000.065274	13.424819	-0.112356	4.817514
575.090365	8000.017039	13.429824	-0.112334	4.817500
574.961294	8000.067907	13.434829	-0.112310	4.817516
575.195915	8000.056612	13.439834	-0.112354	4.817511
574.948689	8000.062449	13.444839	-0.112308	4.817514
575.161115	8000.075103	13.449843	-0.112347	4.817517
575.210305	8000.018834	13.454848	-0.112356	4.817500
575.224196	8000.032765	13.459853	-0.112359	4.817504
575.231132	8000.027593	13.464858	-0.112360	4.817502
575.426021	7999.946040	13.469863	-0.112397	4.817478
575.528112	8000.015115	13.474867	-0.112416	4.817497
575.082734	8000.062347	13.479872	-0.112333	4.817513
575.272267	8000.058828	13.484877	-0.112368	4.817512
575.188877	8000.052316	13.489882	-0.112353	4.817510
575.196055	8000.022869	13.494887	-0.112354	4.817501
575.549592	8000.018616	13.499891	-0.112420	4.817498
575.249189	7999.993051	13.504896	-0.112364	4.817492
575.303361	8000.040304	13.509901	-0.112374	4.817506
575.052570	8000.076700	13.514906	-0.112327	4.817518
575.197810	8000.048245	13.519911	-0.112355	4.817509
575.330718	8000.070276	13.524915	-0.112379	4.817515
575.249036	8000.024732	13.529920	-0.112364	4.817502
574.830311	8000.061804	13.534925	-0.112286	4.817514
575.154193	8000.042332	13.539930	-0.112347	4.817507
575.084886	8000.053974	13.544935	-0.112334	4.817511
575.358991	8000.064377	13.549939	-0.112385	4.817513
574.969392	8000.073379	13.554944	-0.112312	4.817517
574.918086	8000.091622	13.559949	-0.112303	4.817523
574.919540	8000.095869	13.564954	-0.112303	4.817524
575.112088	8000.054393	13.569959	-0.112339	4.817511
575.022303	8000.078399	13.574963	-0.112322	4.817518
575.184022	8000.057578	13.579968	-0.112352	4.817512
575.025854	8000.053123	13.584973	-0.112323	4.817511
574.921391	8000.079023	13.589978	-0.112304	4.817519
575.185315	8000.049161	13.594983	-0.112353	4.817509
574.943352	8000.078299	13.599987	-0.112308	4.817519
574.831905	8000.018592	13.604992	-0.112287	4.817502
575.223580	8000.061350	13.609997	-0.112360	4.817512
575.268995	8000.035636	13.615002	-0.112369	4.817505
575.085932	8000.018146	13.620007	-0.112334	4.817500
575.232348	8000.087879	13.625011	-0.112362	4.817520
574.900691	8000.039683	13.630016	-0.112300	4.817507
574.626797	8000.059903	13.635021	-0.112249	4.817515
574.849331	8000.058984	13.640026	-0.112291	4.817513
574.606813	8000.067002	13.645031	-0.112245	4.817517
574.709250	8000.082247	13.650035	-0.112265	4.817521
575.283577	8000.035877	13.655040	-0.112372	4.817505
575.421834	8000.026320	13.660045	-0.112397	4.817501
574.765160	8000.083085	13.665050	-0.112275	4.817521
574.793165	8000.046558	13.670055	-0.112280	4.817510
575.189928	8000.072502	13.675059	-0.112354	4.817516
575.097255	8000.038407	13.680064	-0.112337	4.817506
575.050194	8000.071491	13.685069	-0.112328	4.817516
574.707173	8000.066407	13.690074	-0.112265	4.817516
574.761271	8000.059823	13.695079	-0.112275	4.817514
574.761960	8000.088337	13.700083	-0.112275	4.817522
574.717860	8000.068686	13.705088	-0.112267	4.817517
574.952165	8000.087998	13.710093	-0.112310	4.817522
574.731835	8000.088955	13.715098	-0.112269	4.817523
574.480494	8000.132732	13.720103	-0.112223	4.817537
574.843168	8000.077946	13.725107	-0.112290	4.817519
575.078682	8000.021273	13.730112	-0.112334	4.817501
574.824131	8000.069225	13.735117	-0.112287	4.817517
575.156931	8000.061497	13.740122	-0.112349	4.817513
574.879101	8000.023600	13.745127	-0.112297	4.817503
574.569582	8000.087626	13.750131	-0.112239	4.817523
574.547057	8000.071462	13.755136	-0.112235	4.817518
575.167495	8000.024720	13.760141	-0.112351	4.817502
575.371762	8000.033031	13.765146	-0.112389	4.817503
574.984663	8000.031515	13.770151	-0.112317	4.817505
575.160226	8000.037288	13.775155	-0.112350	4.817506
575.262173	7999.982857	13.780160	-0.112369	4.817489
575.445880	7999.997197	13.785165	-0.112403	4.817492
575.498901	8000.013820	13.790170	-0.112413	4.817497
575.617725	8000.017697	13.795175	-0.112435	4.817498
575.553181	8000.075856	13.800179	-0.112423	4.817515
575.555591	8000.031560	13.805184	-0.112423	4.817502
575.743872	7999.996354	13.810189	-0.112458	4.817491
575.601079	8000.015351	13.815194	-0.112432	4.817497
575.491225	7999.979946	13.820199	-0.112411	4.817487
575.199937	8000.089632	13.825203	-0.112357	4.817521
575.075112	8000.049783	13.830208	-0.112334	4.817510
575.289323	8000.046629	13.835213	-0.112374	4.817508
575.516044	8000.032050	13.840218	-0.112416	4.817502
575.527424	7999.984720	13.845223	-0.112418	4.817488
575.590818	8000.032110	13.850227	-0.112430	4.817502
575.455377	8000.016381	13.855232	-0.112405	4.817498
575.472436	8000.008193	13.860237	-0.112408	4.817496
575.475364	7999.995572	13.865242	-0.112409	4.817492
575.405486	8000.035707	13.870247	-0.112396	4.817504
575.379430	8000.040601	13.875251	-0.112391	4.817506
575.388345	8000.023847	13.880256	-0.112393	4.817501
575.555919	8000.051670	13.885261	-0.112424	4.817508
575.280218	8000.064473	13.890266	-0.112373	4.817513
575.408083	7999.985092	13.895271	-0.112397	4.817489
575.573275	8000.049826	13.900275	-0.112427	4.817507
575.351878	8000.026488	13.905280	-0.112386	4.817502
575.501701	8000.036103	13.910285	-0.112414	4.817504
575.721658	8000.067871	13.915290	-0.112455	4.817512
575.701288	8000.020069	13.920295	-0.112451	4.817498
575.334314	8000.076909	13.925299	-0.112383	4.817517
575.348846	8000.042293	13.930304	-0.112386	4.817506
575.727846	8000.008861	13.935309	-0.112456	4.817495
575.612018	7999.973367	13.940314	-0.112435	4.817485
575.542393	7999.986060	13.945319	-0.112422	4.817489
575.616351	8000.024106	13.950323	-0.112436	4.817500
575.426618	7999.995960	13.955328	-0.112400	4.817492
575.289821	8000.038269	13.960333	-0.112375	4.817505
575.572673	8000.064635	13.965338	-0.112428	4.817512
575.375092	8000.018428	13.970343	-0.112391	4.817499
575.315326	8000.073491	13.975347	-0.112380	4.817516
575.498696	8000.004434	13.980352	-0.112414	4.817494
575.738352	8000.006936	13.985357	-0.112459	4.817494
575.652732	8000.023614	13.990362	-0.112443	4.817499
575.612352	8000.004018	13.995367	-0.112435	4.817494
575.792471	8000.040472	14.000371	-0.112469	4.817504
575.318713	8000.052448	14.005376	-0.112381	4.817509
575.193584	8000.069596	14.010381	-0.112358	4.817515
575.162428	8000.094471	14.015386	-0.112352	4.817522
574.823320	8000.064110	14.020391	-0.112289	4.817515
574.897218	8000.104266	14.025395	-0.112303	4.817527
575.052273	8000.041122	14.030400	-0.112331	4.817507
574.821853	8000.095765	14.035405	-0.112289	4.817524
574.975837	8000.099108	14.040410	-0.112317	4.817525
574.786299	8000.060410	14.045415	-0.112282	4.817514
575.106234	8000.075714	14.050419	-0.112342	4.817517
574.716845	8000.099498	14.055424	-0.112269	4.817526
574.716331	8000.112161	14.060429	-0.112269	4.817530
574.964480	8000.068343	14.065434	-0.112315	4.817516
575.145420	8000.049918	14.070439	-0.112349	4.817509
575.146147	8000.112211	14.075443	-0.112349	4.817528
574.670599	8000.111495	14.080448	-0.112261	4.817530
575.119434	8000.110766	14.085453	-0.112344	4.817527
575.385371	8000.074601	14.090458	-0.112394	4.817516
575.134126	8000.105712	14.095463	-0.112347	4.817526
575.427475	8000.112178	14.100467	-0.112402	4.817527
575.475295	8000.057999	14.105472	-0.112411	4.817510
575.319137	8000.063075	14.110477	-0.112382	4.817512
575.483768	8000.063409	14.115482	-0.112412	4.817512
575.768285	7999.988463	14.120487	-0.112465	4.817488
575.471138	8000.065339	14.125491	-0.112410	4.817512
575.402398	8000.049544	14.130496	-0.112397	4.817508
575.313669	8000.086232	14.135501	-0.112381	4.817519
575.297665	8000.078609	14.140506	-0.112378	4.817517
574.788833	8000.111177	14.145511	-0.112283	4.817529
575.222669	8000.129227	14.150515	-0.112364	4.817532
575.002432	8000.103795	14.155520	-0.112323	4.817526
575.366038	8000.052190	14.160525	-0.112391	4.817509
575.474140	8000.065408	14.165530	-0.112411	4.817512
574.995057	8000.072028	14.170535	-0.112322	4.817517
575.014374	8000.077595	14.175539	-0.112325	4.817518
575.066058	8000.072031	14.180544	-0.112335	4.817516
575.315036	8000.075727	14.185549	-0.112382	4.817516
575.337990	8000.075015	14.190554	-0.112386	4.817516
574.932812	8000.074286	14.195559	-0.112310	4.817517
575.390600	8000.120137	14.200563	-0.112396	4.817529
575.487484	8000.089910	14.205568	-0.112414	4.817520
575.345178	8000.104691	14.210573	-0.112387	4.817525
575.216320	8000.079559	14.215578	-0.112363	4.817518
575.300768	8000.054425	14.220583	-0.112379	4.817510
575.262383	8000.108750	14.225587	-0.112372	4.817526
574.948241	8000.086148	14.230592	-0.112314	4.817521
575.438500	8000.076534	14.235597	-0.112405	4.817516
575.094775	8000.137941	14.240602	-0.112341	4.817536
574.894317	8000.134970	14.245607	-0.112304	4.817536
575.621857	8000.117265	14.250611	-0.112439	4.817527
575.306483	8000.072477	14.255616	-0.112380	4.817515
575.297856	8000.097686	14.260621	-0.112379	4.817523
575.411472	8000.062429	14.265626	-0.112400	4.817512
574.968731	8000.074865	14.270631	-0.112318	4.817517
574.542561	8000.158273	14.275635	-0.112238	4.817544
575.033358	8000.114887	14.280640	-0.112330	4.817529
574.563894	8000.172318	14.285645	-0.112243	4.817548
574.192626	8000.183704	14.290650	-0.112173	4.817553
574.022849	8000.187523	14.295655	-0.112142	4.817555
574.061707	8000.223992	14.300659	-0.112149	4.817566
574.346991	8000.169113	14.305664	-0.112202	4.817548
574.376674	8000.162168	14.310669	-0.112208	4.817546
574.890430	8000.115955	14.315674	-0.112304	4.817530
574.990774	8000.115336	14.320679	-0.112322	4.817529
574.995238	8000.142850	14.325683	-0.112323	4.817537
574.585688	8000.133612	14.330688	-0.112247	4.817537
574.746169	8000.151829	14.335693	-0.112277	4.817541
574.662159	8000.187532	14.340698	-0.112261	4.817552
574.741112	8000.130649	14.345703	-0.112276	4.817535
574.512668	8000.189543	14.350707	-0.112233	4.817553
574.558731	8000.158562	14.355712	-0.112242	4.817544
574.781617	8000.161871	14.360717	-0.112284	4.817544
574.644038	8000.203112	14.365722	-0.112258	4.817557
574.574727	8000.140863	14.370727	-0.112245	4.817539
574.573350	8000.175680	14.375731	-0.112245	4.817549
574.588106	8000.122067	14.380736	-0.112248	4.817533
574.434255	8000.156734	14.385741	-0.112219	4.817544
574.658030	8000.205446	14.390746	-0.112261	4.817557
574.191951	8000.223871	14.395751	-0.112174	4.817565
574.847369	7999.119980	14.400755	-0.112296	4.817236

574.161108	7996.028039	14.405760	-0.112166	4.816324
574.625678	7990.513349	14.410765	-0.112249	4.814690
574.712977	7984.030026	14.415770	-0.112261	4.812771
574.281743	7976.757626	14.420775	-0.112176	4.810619
574.299686	7969.116732	14.425779	-0.112174	4.808355
574.330562	7961.358516	14.430784	-0.112175	4.806056
574.830851	7953.363092	14.435789	-0.112263	4.803683
574.783060	7945.595483	14.440794	-0.112249	4.801378
574.149123	7937.524144	14.445799	-0.112126	4.798985
574.192070	7929.640423	14.450803	-0.112129	4.796643
574.222057	7921.552386	14.455808	-0.112129	4.794240
574.060974	7913.593011	14.460813	-0.112094	4.791875
574.481043	7905.523188	14.465818	-0.112167	4.789473
574.262354	7897.510215	14.470823	-0.112121	4.787089
573.904207	7889.551002	14.475827	-0.112049	4.784721
574.275499	7881.524956	14.480832	-0.112113	4.782329
574.140070	7873.511498	14.485837	-0.112083	4.779941
574.451710	7865.552285	14.490842	-0.112135	4.777567
574.491907	7857.466188	14.495847	-0.112138	4.775154
574.565955	7849.559188	14.500851	-0.112146	4.772794
574.071146	7841.543220	14.505856	-0.112049	4.770402
573.916227	7833.544539	14.510861	-0.112015	4.768013
574.005972	7825.494053	14.515866	-0.112027	4.765606
573.737879	7817.524249	14.520871	-0.111971	4.763223
574.063706	7809.493670	14.525875	-0.112027	4.760819
573.746418	7801.507513	14.530880	-0.111963	4.758430
574.168280	7793.494194	14.535885	-0.112036	4.756028
574.232066	7785.450080	14.540890	-0.112043	4.753617
573.513241	7777.515085	14.545895	-0.111904	4.751240
573.771326	7769.467462	14.550899	-0.111947	4.748825
573.880894	7761.486977	14.555904	-0.111962	4.746430
573.668391	7753.443198	14.560909	-0.111917	4.744015
573.906315	7745.526970	14.565914	-0.111956	4.741636
573.531908	7737.438128	14.570919	-0.111881	4.739205
573.505911	7729.521478	14.575923	-0.111871	4.736825
573.422892	7721.444475	14.580928	-0.111851	4.734394
573.448724	7713.465824	14.585933	-0.111850	4.731992
573.621785	7705.443649	14.590938	-0.111877	4.729576
573.392140	7697.447362	14.595943	-0.111829	4.727166
573.055954	7689.471036	14.600947	-0.111762	4.724762
573.703541	7681.442769	14.605952	-0.111877	4.722339
573.921673	7673.373022	14.610957	-0.111912	4.719903
573.300757	7665.533265	14.615962	-0.111792	4.717537
573.306348	7657.409411	14.620967	-0.111788	4.715082
573.936377	7649.442418	14.625971	-0.111900	4.712672
573.428134	7641.447532	14.630976	-0.111800	4.710255
573.566017	7633.371046	14.635981	-0.111820	4.707811
573.473357	7625.443779	14.640986	-0.111798	4.705411
573.285900	7617.414976	14.645991	-0.111758	4.702980
573.782824	7609.363166	14.650995	-0.111845	4.700539
573.798979	7601.409638	14.656000	-0.111843	4.698127
573.493526	7593.515186	14.661005	-0.111781	4.695732
573.409800	7585.460392	14.666010	-0.111760	4.693287
573.353761	7577.429489	14.671015	-0.111745	4.690848
573.881146	7569.372473	14.676019	-0.111838	4.688400
573.866770	7561.399342	14.681024	-0.111830	4.685976
573.759731	7553.373543	14.686029	-0.111805	4.683535
573.802324	7545.501257	14.691034	-0.111808	4.681139
573.657580	7537.409880	14.696039	-0.111775	4.678675
573.737520	7529.466003	14.701043	-0.111785	4.676255
574.119671	7521.361299	14.706048	-0.111851	4.673784
573.991354	7513.411696	14.711053	-0.111822	4.671360
573.714301	7505.352315	14.716058	-0.111765	4.668901
573.282231	7497.465581	14.721063	-0.111680	4.666494
573.060566	7489.404782	14.726067	-0.111633	4.664032
573.318875	7481.428045	14.731072	-0.111676	4.661594
573.349817	7473.336518	14.736077	-0.111677	4.659120
573.275303	7465.464356	14.741082	-0.111658	4.656711
573.324531	7457.357903	14.746087	-0.111662	4.654230
573.700580	7449.394841	14.751091	-0.111726	4.651791
573.522738	7441.343443	14.756096	-0.111688	4.649324
573.475942	7433.396307	14.761101	-0.111674	4.646888
573.043977	7425.434713	14.766106	-0.111589	4.644445
573.102130	7417.427983	14.771111	-0.111594	4.641988
573.507194	7409.363644	14.776115	-0.111665	4.639512
573.221552	7401.407899	14.781120	-0.111606	4.637068
573.354223	7393.338726	14.786125	-0.111626	4.634587
573.237878	7385.411869	14.791130	-0.111599	4.632149
573.858867	7377.288197	14.796135	-0.111709	4.629649
573.606247	7369.373879	14.801139	-0.111657	4.627213
573.267417	7361.374731	14.806144	-0.111589	4.624748
573.233733	7353.468835	14.811149	-0.111577	4.622312
573.430794	7345.416077	14.816154	-0.111609	4.619828
572.844771	7337.397904	14.821159	-0.111495	4.617354
573.314166	7329.306901	14.826163	-0.111577	4.614857
573.270690	7321.369492	14.831168	-0.111564	4.612405
572.796017	7313.349258	14.836173	-0.111470	4.609926
572.667467	7305.391371	14.841178	-0.111441	4.607465
572.596820	7297.312568	14.846183	-0.111423	4.604966
572.580451	7289.355017	14.851187	-0.111414	4.602503
572.919922	7281.333287	14.856192	-0.111472	4.600018
573.033431	7273.349642	14.861197	-0.111488	4.597545
573.119982	7265.358259	14.866202	-0.111499	4.595067
572.754096	7257.379653	14.871207	-0.111426	4.592592
572.791540	7249.346812	14.876211	-0.111428	4.590098
572.651832	7241.373237	14.881216	-0.111397	4.587622
572.750080	7233.273551	14.886221	-0.111410	4.585105
572.509605	7225.362346	14.891226	-0.111360	4.582645
572.938559	7217.238972	14.896231	-0.111434	4.580119
573.202659	7209.314191	14.901235	-0.111478	4.577653
573.055859	7201.316278	14.906240	-0.111446	4.575162
573.020412	7193.300218	14.911245	-0.111434	4.572665
573.036754	7185.293309	14.916250	-0.111432	4.570169
572.536181	7177.292437	14.921255	-0.111334	4.567672
572.493768	7169.305697	14.926259	-0.111321	4.565180
572.293141	7161.342212	14.931264	-0.111278	4.562693
572.325972	7153.294904	14.936269	-0.111279	4.560179
572.686186	7145.290027	14.941274	-0.111341	4.557677
572.792280	7137.209140	14.946279	-0.111355	4.555150
572.811976	7129.276868	14.951283	-0.111354	4.552667
572.657793	7121.262336	14.956288	-0.111320	4.550158
572.709655	7113.286779	14.961293	-0.111324	4.547659
572.795343	7105.302415	14.966298	-0.111335	4.545156
572.587954	7097.279720	14.971303	-0.111291	4.542640
572.540227	7089.284267	14.976307	-0.111277	4.540131
572.308529	7081.335394	14.981312	-0.111229	4.537634
572.168591	7073.263123	14.986317	-0.111198	4.535098
572.479702	7065.275287	14.991322	-0.111251	4.532588
572.393496	7057.240386	14.996327	-0.111229	4.530061
572.508835	7049.257937	15.001331	-0.111246	4.527549
572.358898	7041.197865	15.006336	-0.111213	4.525011
572.620449	7033.237897	15.011341	-0.111256	4.522504
572.467798	7025.279968	15.016346	-0.111223	4.519995
572.478085	7017.296355	15.021351	-0.111219	4.517477
572.260883	7009.292591	15.026355	-0.111174	4.514951
572.376253	7001.301141	15.031360	-0.111190	4.512428
572.470813	6993.237263	15.036365	-0.111202	4.509881
572.546687	6985.212654	15.041370	-0.111211	4.507344
572.620251	6977.144208	15.046375	-0.111220	4.504793
572.532307	6969.217081	15.051379	-0.111198	4.502284
572.402612	6961.197261	15.056384	-0.111169	4.499744
572.288303	6953.197629	15.061389	-0.111142	4.497209
572.583366	6945.199131	15.066394	-0.111192	4.494675
572.463081	6937.170233	15.071399	-0.111165	4.492128
572.496990	6929.204214	15.076403	-0.111166	4.489600
572.386762	6921.176493	15.081408	-0.111140	4.487051
572.504997	6913.144850	15.086413	-0.111157	4.484499
572.439926	6905.254404	15.091418	-0.111140	4.481991
572.042382	6897.188884	15.096423	-0.111060	4.479424
572.202630	6889.204739	15.101427	-0.111085	4.476884
571.952450	6881.177207	15.106432	-0.111033	4.474326
571.860044	6873.267005	15.111437	-0.111011	4.471806
572.103123	6865.195500	15.116442	-0.111051	4.469233
571.884774	6857.145278	15.121447	-0.111005	4.466665
571.776995	6849.136470	15.126451	-0.110980	4.464108
572.039822	6841.171347	15.131456	-0.111024	4.461565
571.787432	6833.146323	15.136461	-0.110972	4.459000
571.587143	6825.235622	15.141466	-0.110929	4.456470
571.548398	6817.129201	15.146471	-0.110917	4.453877
571.503765	6809.222623	15.151475	-0.110903	4.451346
571.479496	6801.141940	15.156480	-0.110894	4.448757
571.069207	6793.169935	15.161485	-0.110812	4.446201
571.456153	6785.147187	15.166490	-0.110879	4.443630
571.157037	6777.193612	15.171495	-0.110818	4.441077
571.194815	6769.110355	15.176499	-0.110820	4.438482
571.254115	6761.180157	15.181504	-0.110826	4.435935
571.326274	6753.094064	15.186509	-0.110834	4.433337
571.337997	6745.149513	15.191514	-0.110831	4.430782
571.164330	6737.102876	15.196519	-0.110793	4.428192
571.460962	6729.030217	15.201523	-0.110843	4.425595
571.325509	6721.113558	15.206528	-0.110813	4.423044
571.127021	6713.137688	15.211533	-0.110771	4.420472
571.416384	6705.150699	15.216538	-0.110820	4.417897
571.138932	6697.130395	15.221543	-0.110763	4.415308
571.225395	6689.089396	15.226547	-0.110774	4.412712
570.928760	6681.115720	15.231552	-0.110713	4.410134
571.018988	6673.091831	15.236557	-0.110725	4.407540
571.196953	6665.075918	15.241562	-0.110753	4.404949
570.985436	6657.124623	15.246567	-0.110708	4.402374
571.282234	6649.049431	15.251571	-0.110758	4.399760
571.417133	6641.107081	15.256576	-0.110778	4.397188
571.289711	6633.081739	15.261581	-0.110749	4.394585
570.964099	6625.153395	15.266586	-0.110684	4.392011
570.933417	6617.093548	15.271591	-0.110673	4.389394
570.901281	6609.134644	15.276595	-0.110662	4.386809
571.247858	6601.013791	15.281600	-0.110721	4.384172
571.232826	6593.078399	15.286605	-0.110713	4.381591
571.369911	6585.080460	15.291610	-0.110733	4.378989
571.043039	6577.107880	15.296615	-0.110667	4.376392
571.068305	6569.111124	15.301619	-0.110667	4.373787
571.005980	6561.124722	15.306624	-0.110650	4.371183
570.449897	6553.085199	15.311629	-0.110541	4.368557
571.141460	6545.082543	15.316634	-0.110665	4.365950
570.886472	6537.096339	15.321639	-0.110612	4.363340
570.842303	6529.117306	15.326643	-0.110599	4.360733
571.005111	6521.150163	15.331648	-0.110624	4.358129
570.801655	6513.156402	15.336653	-0.110581	4.355512
570.614210	6505.169096	15.341658	-0.110541	4.352896
570.455477	6497.122211	15.346663	-0.110506	4.350259
570.375942	6489.157586	15.351667	-0.110486	4.347649
570.443272	6481.104133	15.356672	-0.110494	4.345008
570.496602	6473.128155	15.361677	-0.110498	4.342391
570.294886	6465.131326	15.366682	-0.110456	4.339764
570.409039	6457.173128	15.371687	-0.110472	4.337150
570.395135	6449.124824	15.376691	-0.110464	4.334504
570.463500	6441.164948	15.381696	-0.110471	4.331886
570.413301	6433.112102	15.386701	-0.110457	4.329236
570.365073	6425.139984	15.391706	-0.110443	4.326610
570.205252	6417.134643	15.396711	-0.110408	4.323970
570.410618	6409.224007	15.401715	-0.110441	4.321363
570.433308	6401.139887	15.406720	-0.110440	4.318696
569.998381	6393.171091	15.411725	-0.110354	4.316062
570.453793	6385.123279	15.416730	-0.110433	4.313407
570.458831	6377.157409	15.421735	-0.110429	4.310774
570.266664	6369.141848	15.426739	-0.110388	4.308121
570.107348	6361.126719	15.431744	-0.110353	4.305467
569.992855	6353.090030	15.436749	-0.110327	4.302805
569.746208	6345.205824	15.441754	-0.110276	4.300190
569.655696	6337.143690	15.446759	-0.110254	4.297516
569.702439	6329.103779	15.451763	-0.110257	4.294849
569.694188	6321.117282	15.456768	-0.110251	4.292197
569.862032	6313.013691	15.461773	-0.110277	4.289507
569.997450	6305.072778	15.466778	-0.110297	4.286868
569.877634	6297.029936	15.471783	-0.110269	4.284192
569.996517	6289.127401	15.476787	-0.110286	4.281563
569.779058	6281.122519	15.481792	-0.110241	4.278895
569.501063	6273.167449	15.486797	-0.110184	4.276242
569.594707	6265.110884	15.491802	-0.110196	4.273557
569.422925	6257.139612	15.496807	-0.110159	4.270895
569.089075	6249.124589	15.501811	-0.110091	4.268216
569.498491	6241.089345	15.506816	-0.110162	4.265536
569.485240	6233.049387	15.511821	-0.110155	4.262848
569.439738	6225.121794	15.516826	-0.110141	4.260196
569.494731	6217.104920	15.521831	-0.110146	4.257513
569.175861	6209.121505	15.526835	-0.110082	4.254836
569.029268	6201.124311	15.531840	-0.110049	4.252155
569.104217	6193.049476	15.536845	-0.110058	4.249448
569.237645	6185.123151	15.541850	-0.110078	4.246789
569.222794	6177.031356	15.546855	-0.110070	4.244072
568.936263	6169.134878	15.551859	-0.110011	4.241416
569.024161	6161.132969	15.556864	-0.110022	4.238727
569.044134	6153.106605	15.561869	-0.110021	4.236027
568.929564	6145.121874	15.566874	-0.109994	4.233338
569.462310	6137.029931	15.571879	-0.110088	4.230618
569.206878	6129.095812	15.576883	-0.110036	4.227941
569.313871	6121.072384	15.581888	-0.110050	4.225236
569.063618	6113.095647	15.586893	-0.109999	4.222542
569.218796	6105.107771	15.591898	-0.110022	4.219846
569.260547	6097.086942	15.596903	-0.110025	4.217136
569.356210	6089.037250	15.601907	-0.110038	4.214415
569.361337	6081.090611	15.606912	-0.110033	4.211727
569.004844	6073.048146	15.611917	-0.109962	4.209000
569.147145	6065.116610	15.616922	-0.109983	4.206314
568.820891	6057.087405	15.621927	-0.109917	4.203589
569.089703	6049.118705	15.626931	-0.109962	4.200888
568.919912	6041.087555	15.631936	-0.109925	4.198160
568.812684	6033.055967	15.636941	-0.109900	4.195431
568.850660	6025.095551	15.641946	-0.109902	4.192726
568.912903	6016.983457	15.646951	-0.109908	4.189968
568.888792	6009.007050	15.651955	-0.109899	4.187253
568.766468	6001.007068	15.656960	-0.109871	4.184527
568.660067	5993.113475	15.661965	-0.109846	4.181836
568.932795	5985.029037	15.666970	-0.109891	4.179082
568.626671	5977.086748	15.671975	-0.109829	4.176369
568.910230	5969.021560	15.676979	-0.109877	4.173618
568.802952	5961.049123	15.681984	-0.109852	4.170893
568.940968	5952.994888	15.686989	-0.109872	4.168141
569.009710	5945.016772	15.691994	-0.109880	4.165412
569.057001	5937.044620	15.696999	-0.109883	4.162684
568.901681	5929.085777	15.702003	-0.109849	4.159955
569.015846	5921.108963	15.707008	-0.109866	4.157222
568.959257	5913.040662	15.712013	-0.109850	4.154454
568.900165	5905.118793	15.717018	-0.109834	4.151734
568.686638	5897.053273	15.722023	-0.109789	4.148961
568.736818	5889.078978	15.727027	-0.109793	4.146221
568.813394	5881.033659	15.732032	-0.109802	4.143455
568.484364	5873.093861	15.737037	-0.109736	4.140718
568.675511	5865.084018	15.742042	-0.109766	4.137962
568.802736	5857.073669	15.747047	-0.109784	4.135203
568.743881	5849.083724	15.752051	-0.109768	4.132447
568.711162	5841.052034	15.757056	-0.109757	4.129675
568.219272	5833.145236	15.762061	-0.109660	4.126938
568.119365	5825.117914	15.767066	-0.109637	4.124163
568.317543	5817.135209	15.772071	-0.109668	4.121405
568.568869	5809.027654	15.777075	-0.109710	4.118603
568.569845	5801.114544	15.782080	-0.109705	4.115864
568.614006	5793.063617	15.787085	-0.109708	4.113075
568.553408	5785.078028	15.792090	-0.109691	4.110305
568.373864	5777.063831	15.797095	-0.109653	4.107522
568.297321	5769.037611	15.802099	-0.109633	4.104735
568.258352	5761.144754	15.807104	-0.109621	4.101992
568.393697	5753.059961	15.812109	-0.109641	4.099183
568.422237	5745.115899	15.817114	-0.109641	4.096420
568.240255	5737.079852	15.822119	-0.109602	4.093620
568.211735	5729.090682	15.827123	-0.109592	4.090836
568.062747	5721.119011	15.832128	-0.109559	4.088055
567.880526	5713.061143	15.837133	-0.109520	4.085241
567.957967	5705.127925	15.842138	-0.109529	4.082473
567.838520	5697.114343	15.847143	-0.109501	4.079672
568.100094	5689.087915	15.852147	-0.109545	4.076870
567.913028	5681.097109	15.857152	-0.109505	4.074072
567.914558	5673.085296	15.862157	-0.109500	4.071268
567.995169	5665.084609	15.867162	-0.109510	4.068466
567.908484	5657.051926	15.872167	-0.109489	4.065649
567.761676	5649.086115	15.877171	-0.109456	4.062853
567.683039	5641.134521	15.882176	-0.109436	4.060061
567.443697	5633.124211	15.887181	-0.109386	4.057243
567.772185	5625.051744	15.892186	-0.109442	4.054411
567.830048	5617.068301	15.897191	-0.109448	4.051603
567.845809	5609.017716	15.902195	-0.109446	4.048770
567.770056	5601.065342	15.907200	-0.109427	4.045968
568.099847	5593.054790	15.912205	-0.109483	4.043149
567.735515	5585.156189	15.917210	-0.109410	4.040357
567.782480	5577.127516	15.922215	-0.109413	4.037524
567.838803	5569.074896	15.927219	-0.109419	4.034681
567.750469	5561.064377	15.932224	-0.109397	4.031848
567.600524	5553.006694	15.937229	-0.109364	4.028995
567.934324	5545.033639	15.942234	-0.109421	4.026178
567.851895	5537.027479	15.947239	-0.109400	4.023341
567.559941	5529.093700	15.952243	-0.109341	4.020524
567.609897	5521.108752	15.957248	-0.109345	4.017692
567.506634	5513.081889	15.962253	-0.109321	4.014841
567.438183	5505.124199	15.967258	-0.109303	4.012013
567.208760	5497.109315	15.972263	-0.109255	4.009160
567.478109	5489.077230	15.977267	-0.109300	4.006307
567.320915	5481.084548	15.982272	-0.109265	4.003460
566.871001	5473.146287	15.987277	-0.109176	4.000624
566.979971	5465.171983	15.992282	-0.109192	3.997783
567.001874	5457.147906	15.997287	-0.109190	3.994921
567.005002	5449.128714	16.002291	-0.109186	3.992058
566.935483	5441.102120	16.007296	-0.109168	3.989189
567.073046	5433.102052	16.012301	-0.109188	3.986331
567.030442	5425.110156	16.017306	-0.109175	3.983471
566.851631	5417.155825	16.022311	-0.109137	3.980620
566.804971	5409.139950	16.027315	-0.109123	3.977747
566.944285	5401.148768	16.032320	-0.109143	3.974885
566.736411	5393.114885	16.037325	-0.109100	3.971998
566.528505	5385.179936	16.042330	-0.109056	3.969145
566.881861	5377.143465	16.047335	-0.109116	3.966264
566.759985	5369.120378	16.052339	-0.109088	3.963377
566.939053	5361.133475	16.057344	-0.109117	3.960506
566.830687	5353.127505	16.062349	-0.109091	3.957620
567.000169	5345.169926	16.067354	-0.109118	3.954756
566.132646	5337.218658	16.072359	-0.108951	3.951873
566.551802	5329.080370	16.077363	-0.109024	3.948943
566.929872	5321.123692	16.082368	-0.109089	3.946076
566.752489	5313.105661	16.087373	-0.109051	3.943175
566.952558	5305.136638	16.092378	-0.109083	3.940296
567.105127	5297.130940	16.097383	-0.109106	3.937401
566.742098	5289.144437	16.102387	-0.109033	3.934501
566.847943	5281.134820	16.107392	-0.109048	3.931600
566.684362	5273.095885	16.112397	-0.109012	3.928680
566.612293	5265.153701	16.117402	-0.108994	3.925795
566.583023	5257.139586	16.122407	-0.108983	3.922883
566.543397	5249.150004	16.127411	-0.108970	3.919978
566.670864	5241.190250	16.132416	-0.108989	3.917084
566.487460	5233.141182	16.137421	-0.108950	3.914149
566.501474	5225.185497	16.142426	-0.108947	3.911251
566.486375	5217.134550	16.147431	-0.108939	3.908314
566.379041	5209.133030	16.152435	-0.108914	3.905392
566.559678	5201.176943	16.157440	-0.108942	3.902490
566.274593	5193.137116	16.162445	-0.108884	3.899546
566.530722	5185.169237	16.167450	-0.108927	3.896637
566.368442	5177.147827	16.172455	-0.108891	3.893697
565.891573	5169.186141	16.177459	-0.108797	3.890771
565.808639	5161.219562	16.182464	-0.108777	3.887849
565.912832	5153.157836	16.187469	-0.108791	3.884893
566.197047	5145.204599	16.192474	-0.108839	3.881979
566.080430	5137.190802	16.197479	-0.108812	3.879032
566.110967	5129.230244	16.202483	-0.108812	3.876106
566.095622	5121.204435	16.207488	-0.108804	3.873152
565.938255	5113.051940	16.212493	-0.108770	3.870146
566.228270	5105.073257	16.217498	-0.108819	3.867212
566.028706	5097.120141	16.222503	-0.108776	3.864274
565.846147	5089.189126	16.227507	-0.108737	3.861343
565.664831	5081.232044	16.232512	-0.108698	3.858400
565.565253	5073.200546	16.237517	-0.108675	3.855429
565.749572	5065.180359	16.242522	-0.108704	3.852465
565.250982	5057.226850	16.247527	-0.108606	3.849510
565.443484	5049.204192	16.252531	-0.108636	3.846541
565.344485	5041.216892	16.257536	-0.108613	3.843577
565.416128	5033.218473	16.262541	-0.108621	3.840610
565.500333	5025.223810	16.267546	-0.108631	3.837643
565.196400	5017.254294	16.272551	-0.108570	3.834674
565.085625	5009.248045	16.277555	-0.108544	3.831694
565.883208	5001.164401	16.282560	-0.108687	3.828701
565.271273	4993.213962	16.287565	-0.108568	3.825726
565.174954	4985.269180	16.292570	-0.108545	3.822762
565.091408	4977.252918	16.297575	-0.108524	3.819769
565.195397	4969.219428	16.302579	-0.108538	3.816771
565.566757	4961.173945	16.307584	-0.108602	3.813772
565.462322	4953.182799	16.312589	-0.108578	3.810781
565.406000	4945.202627	16.317594	-0.108562	3.807793
565.432828	4937.208807	16.322599	-0.108562	3.804799
565.309183	4929.271880	16.327603	-0.108534	3.801820
565.588397	4921.205641	16.332608	-0.108581	3.798800
565.307633	4913.278261	16.337613	-0.108523	3.795817
565.480983	4905.263422	16.342618	-0.108550	3.792809
565.501641	4897.220962	16.347623	-0.108549	3.789785
565.589091	4889.242219	16.352627	-0.108560	3.786784
565.342838	4881.260263	16.357632	-0.108509	3.783771
564.983344	4873.296661	16.362637	-0.108437	3.780761
564.685631	4865.346533	16.367642	-0.108376	3.777754
564.853334	4857.253599	16.372647	-0.108402	3.774702
565.036546	4849.250417	16.377651	-0.108431	3.771682
565.207227	4841.249396	16.382656	-0.108458	3.768660
564.661486	4833.294232	16.387661	-0.108351	3.765636
564.727578	4825.339749	16.392666	-0.108358	3.762624
564.996868	4817.249692	16.397671	-0.108403	3.759563
564.521473	4809.360797	16.402675	-0.108310	3.756558
564.091383	4801.417234	16.407680	-0.108224	3.753532
564.085769	4793.350880	16.412685	-0.108218	3.750466
564.558479	4785.301095	16.417690	-0.108301	3.747415
564.801015	4777.219792	16.422695	-0.108341	3.744345
564.047860	4769.407395	16.427699	-0.108195	3.741350
564.052353	4761.417386	16.432704	-0.108191	3.738304
564.059387	4753.360133	16.437709	-0.108187	3.735229
563.812403	4745.407532	16.442714	-0.108136	3.732186
563.533406	4737.379501	16.447719	-0.108079	3.729110
563.461612	4729.388892	16.452723	-0.108060	3.726052
563.988099	4721.318856	16.457728	-0.108153	3.722975
564.329906	4713.318571	16.462733	-0.108212	3.719918
564.487199	4705.355458	16.467738	-0.108236	3.716868
564.568728	4697.316768	16.472743	-0.108246	3.713785
564.533944	4689.276100	16.477747	-0.108234	3.710695
564.362998	4681.335521	16.482752	-0.108197	3.707638
564.093590	4673.352101	16.487757	-0.108142	3.704560
564.106129	4665.398939	16.492762	-0.108139	3.701497
563.775913	4657.408695	16.497767	-0.108072	3.698409
563.696101	4649.388396	16.502771	-0.108052	3.695314
564.173735	4641.323930	16.507776	-0.108136	3.692212
564.002254	4633.326423	16.512781	-0.108099	3.689118
563.570486	4625.458081	16.517786	-0.108013	3.686064
563.866330	4617.386233	16.522791	-0.108063	3.682948
563.677767	4609.403730	16.527795	-0.108023	3.679851
564.123859	4601.414062	16.532800	-0.108101	3.676765
564.034029	4593.366750	16.537805	-0.108079	3.673640
563.921087	4585.410674	16.542810	-0.108053	3.670547
563.955605	4577.360565	16.547815	-0.108054	3.667419
563.818536	4569.366765	16.552819	-0.108023	3.664306
564.321335	4561.417657	16.557824	-0.108112	3.661225
564.281731	4553.377016	16.562829	-0.108099	3.658091
563.952743	4545.484896	16.567834	-0.108033	3.655004
563.951066	4537.446616	16.572839	-0.108027	3.651866
563.762113	4529.441034	16.577843	-0.107987	3.648734
563.864245	4521.474031	16.582848	-0.108001	3.645621
563.566370	4513.495465	16.587853	-0.107940	3.642491
563.588890	4505.504654	16.592858	-0.107939	3.639362
563.475893	4497.564456	16.597863	-0.107913	3.636246
563.201358	4489.534321	16.602867	-0.107857	3.633088
563.705587	4481.461093	16.607872	-0.107945	3.629931
563.729814	4473.446904	16.612877	-0.107945	3.626782
563.148899	4465.526253	16.617882	-0.107832	3.623650
563.463531	4457.490327	16.622887	-0.107885	3.620495
563.609146	4449.465412	16.627891	-0.107907	3.617337
563.862223	4441.471406	16.632896	-0.107949	3.614191
563.696172	4433.479541	16.637901	-0.107913	3.611032
563.534661	4425.522858	16.642906	-0.107877	3.607883
563.677759	4417.498351	16.647911	-0.107899	3.604714
563.514580	4409.554246	16.652915	-0.107863	3.601565
563.908447	4401.530289	16.657920	-0.107932	3.598398
563.389523	4393.592983	16.662925	-0.107830	3.595236
563.330849	4385.596313	16.667930	-0.107814	3.592061
563.294394	4377.568980	16.672935	-0.107802	3.588872
563.480513	4369.513651	16.677939	-0.107831	3.585675
563.128318	4361.605379	16.682944	-0.107760	3.582518
563.236542	4353.559828	16.687949	-0.107775	3.579317
563.574560	4345.563952	16.692954	-0.107833	3.576140
562.887341	4337.640814	16.697959	-0.107700	3.572958
563.063698	4329.560099	16.702963	-0.107728	3.569737
563.312495	4321.576464	16.707968	-0.107769	3.566553
563.161071	4313.582146	16.712973	-0.107736	3.563351
562.961689	4305.622060	16.717978	-0.107693	3.560157
563.179654	4297.644899	16.722983	-0.107729	3.556967
563.041538	4289.605903	16.727987	-0.107698	3.553738
563.121581	4281.572592	16.732992	-0.107707	3.550515
563.067848	4273.556662	16.737997	-0.107692	3.547293
562.692955	4265.606537	16.743002	-0.107617	3.544083
562.809782	4257.677567	16.748007	-0.107634	3.540895
562.618960	4249.652130	16.753011	-0.107593	3.537655
562.679641	4241.642001	16.758016	-0.107599	3.534426
563.006343	4233.615700	16.763021	-0.107655	3.531196
562.697621	4225.652347	16.768026	-0.107592	3.527969
562.606125	4217.661956	16.773031	-0.107570	3.524735
562.786173	4209.679572	16.778035	-0.107598	3.521509
562.877265	4201.678191	16.783040	-0.107610	3.518270
562.823370	4193.678460	16.788045	-0.107595	3.515024
562.662269	4185.754449	16.793050	-0.107560	3.511803
562.710753	4177.710849	16.798055	-0.107564	3.508536
562.053523	4169.767477	16.803059	-0.107436	3.505285
562.487166	4161.741715	16.808064	-0.107512	3.502032
562.222808	4153.752764	16.813069	-0.107457	3.498768
562.117285	4145.787964	16.818074	-0.107433	3.495517
561.980668	4137.769633	16.823079	-0.107402	3.492239
562.340884	4129.674525	16.828083	-0.107464	3.488943
562.345813	4121.739459	16.833088	-0.107460	3.485698
561.946598	4113.792081	16.838093	-0.107380	3.482432
562.120508	4105.767065	16.843098	-0.107407	3.479149
561.946026	4097.833688	16.848103	-0.107370	3.475890
561.852380	4089.798743	16.853107	-0.107347	3.472589
561.829375	4081.806065	16.858112	-0.107338	3.469304
561.598759	4073.787608	16.863117	-0.107289	3.465998
561.684362	4065.797637	16.868122	-0.107300	3.462712
561.638669	4057.819778	16.873127	-0.107287	3.459422
561.552546	4049.836165	16.878131	-0.107265	3.456127
562.172277	4041.757508	16.883136	-0.107376	3.452812
561.918904	4033.774052	16.888141	-0.107323	3.449504
561.923823	4025.827077	16.893146	-0.107319	3.446217
561.917812	4017.829043	16.898151	-0.107313	3.442905
561.687623	4009.853338	16.903155	-0.107265	3.439592
561.959577	4001.885511	16.908160	-0.107310	3.436296
562.256332	3993.822467	16.913165	-0.107360	3.432958
562.114931	3985.883658	16.918170	-0.107329	3.429653
562.083720	3977.869945	16.923175	-0.107318	3.426318
562.133988	3969.855793	16.928179	-0.107322	3.422982
562.249246	3961.911398	16.933184	-0.107338	3.419674
562.069263	3953.932702	16.938189	-0.107300	3.416339
562.017086	3945.951206	16.943194	-0.107285	3.413003
562.067189	3937.924192	16.948199	-0.107289	3.409649
561.759859	3929.952220	16.953203	-0.107226	3.406302
561.647621	3921.989690	16.958208	-0.107200	3.402962
561.745177	3913.983106	16.963213	-0.107213	3.399608
561.418870	3906.073746	16.968218	-0.107148	3.396277
561.703895	3897.948939	16.973223	-0.107195	3.392873
561.660075	3889.914988	16.978227	-0.107182	3.389492
561.340139	3882.026729	16.983232	-0.107117	3.386160
561.129206	3873.998623	16.988237	-0.107073	3.382769
561.402787	3865.969782	16.993242	-0.107119	3.379392
561.245913	3858.020469	16.998247	-0.107084	3.376030
561.279917	3849.967525	17.003251	-0.107085	3.372627
561.460153	3841.991228	17.008256	-0.107114	3.369259
561.631573	3834.003696	17.013261	-0.107140	3.365882
561.359358	3826.044072	17.018266	-0.107085	3.362497
561.106050	3818.071840	17.023271	-0.107032	3.359105
561.232771	3810.115904	17.028275	-0.107051	3.355730
561.137052	3802.134452	17.033280	-0.107028	3.352332
561.145930	3794.044259	17.038285	-0.107024	3.348888
561.439158	3786.045894	17.043290	-0.107074	3.345491
561.411647	3778.112895	17.048295	-0.107063	3.342106
561.360250	3770.103083	17.053299	-0.107049	3.338684
561.212552	3762.166934	17.058304	-0.107016	3.335286
560.959210	3754.174609	17.063309	-0.106964	3.331857
560.641715	3746.187569	17.068314	-0.106899	3.328424
560.693649	3738.191468	17.073319	-0.106904	3.324998
560.663609	3730.187605	17.078323	-0.106893	3.321561
560.608129	3722.236432	17.083328	-0.106878	3.318143
560.437551	3714.205805	17.088333	-0.106841	3.314683
560.701018	3706.177461	17.093338	-0.106885	3.311236
560.932294	3698.154445	17.098343	-0.106922	3.307787
560.936909	3690.144852	17.103347	-0.106918	3.304332
560.584985	3682.263865	17.108352	-0.106847	3.300915
560.577292	3674.252631	17.113357	-0.106841	3.297451
560.096968	3666.319932	17.118362	-0.106746	3.293999
559.923764	3658.335560	17.123367	-0.106709	3.290533
560.229762	3650.221949	17.128371	-0.106761	3.287026
560.423374	3642.241346	17.133376	-0.106791	3.283568
560.098422	3634.304117	17.138381	-0.106726	3.280106
560.208073	3626.299876	17.143386	-0.106741	3.276628
560.192770	3618.321970	17.148391	-0.106733	3.273152
559.654571	3610.367592	17.153395	-0.106628	3.269662
559.705198	3602.385718	17.158400	-0.106632	3.266180
559.998302	3594.302879	17.163405	-0.106681	3.262660
559.708163	3586.374482	17.168410	-0.106622	3.259181
559.671564	3578.433381	17.173415	-0.106610	3.255702
559.362607	3570.447026	17.178419	-0.106548	3.252188
559.276334	3562.461569	17.183424	-0.106526	3.248680
559.149678	3554.426750	17.188429	-0.106498	3.245145
559.261762	3546.430983	17.193434	-0.106513	3.241633
559.275590	3538.468607	17.198439	-0.106511	3.238128
559.093885	3530.472987	17.203443	-0.106472	3.234597
559.622712	3522.423038	17.208448	-0.106565	3.231067
559.719877	3514.393268	17.213453	-0.106578	3.227524
559.573085	3506.422782	17.218458	-0.106545	3.223993
559.411640	3498.492090	17.223463	-0.106510	3.220476
559.459281	3490.479950	17.228467	-0.106514	3.216927
559.963623	3482.404489	17.233472	-0.106602	3.213365
559.718682	3474.437035	17.238477	-0.106552	3.209816
559.574982	3466.526419	17.243482	-0.106520	3.206293
559.323982	3458.568218	17.248487	-0.106468	3.202740
558.804869	3450.625004	17.253491	-0.106366	3.199178
559.679123	3442.507058	17.258496	-0.106524	3.195593
559.794984	3434.495042	17.263501	-0.106540	3.192020
559.559381	3426.554359	17.268506	-0.106491	3.188459
559.558662	3418.541476	17.273511	-0.106486	3.184872
559.072996	3410.668007	17.278515	-0.106390	3.181323
558.979008	3402.671082	17.283520	-0.106368	3.177731
559.145615	3394.636446	17.288525	-0.106393	3.174129
559.133819	3386.644836	17.293530	-0.106386	3.170535
559.564539	3378.615753	17.298535	-0.106461	3.166940
559.278827	3370.664765	17.303539	-0.106403	3.163344
559.003777	3362.766871	17.308544	-0.106346	3.159768
559.247879	3354.702192	17.313549	-0.106387	3.156136
559.211286	3346.729416	17.318554	-0.106375	3.152529
559.085755	3338.717329	17.323559	-0.106346	3.148896
558.849825	3330.750211	17.328563	-0.106297	3.145274
559.181355	3322.737069	17.333568	-0.106354	3.141653
559.170201	3314.726374	17.338573	-0.106346	3.138013
558.839948	3306.806677	17.343578	-0.106280	3.134395
558.660783	3298.834012	17.348583	-0.106241	3.130757
558.969922	3290.750959	17.353587	-0.106293	3.127086
558.836515	3282.833460	17.358592	-0.106264	3.123466
558.594907	3274.871832	17.363597	-0.106213	3.119816
558.680731	3266.878699	17.368602	-0.106224	3.116163
558.821048	3258.855376	17.373607	-0.106245	3.112495
558.501788	3250.878762	17.378611	-0.106181	3.108822
558.804740	3242.841643	17.383616	-0.106232	3.105146
558.914487	3234.855094	17.388621	-0.106247	3.101480
558.387718	3226.973425	17.393626	-0.106144	3.097828
558.564269	3218.956997	17.398631	-0.106172	3.094142
558.645699	3210.946828	17.403635	-0.106181	3.090451
558.730067	3202.950621	17.408640	-0.106192	3.086761
558.226549	3195.027829	17.413645	-0.106093	3.083074
558.526990	3187.004470	17.418650	-0.106144	3.079374
558.344564	3179.080334	17.423655	-0.106105	3.075692
558.144123	3171.048629	17.428659	-0.106062	3.071955
558.425945	3162.970620	17.433664	-0.106110	3.068215
558.249515	3154.995017	17.438669	-0.106072	3.064496
557.891562	3147.100126	17.443674	-0.106000	3.060801
558.025999	3139.109967	17.448679	-0.106020	3.057081
558.066607	3131.056306	17.453683	-0.106022	3.053323
557.912129	3123.126177	17.458688	-0.105988	3.049608
558.093751	3115.098269	17.463693	-0.106017	3.045859
557.991255	3107.136978	17.468698	-0.105992	3.042123
557.828364	3099.185161	17.473703	-0.105957	3.038384
557.914420	3091.170761	17.478707	-0.105968	3.034622
558.092856	3083.169865	17.483712	-0.105996	3.030868
558.211113	3075.146671	17.488717	-0.106013	3.027095
557.990267	3067.211338	17.493722	-0.105966	3.023342
557.623079	3059.305318	17.498727	-0.105893	3.019591
557.868828	3051.264262	17.503731	-0.105934	3.015801
557.289826	3043.380822	17.508736	-0.105821	3.012041
557.665237	3035.270400	17.513741	-0.105885	3.008216
557.680093	3027.283881	17.518746	-0.105883	3.004427
557.826123	3019.334888	17.523751	-0.105905	3.000657
557.225183	3011.416810	17.528755	-0.105788	2.996860
557.613448	3003.346798	17.533760	-0.105855	2.993036
557.853332	2995.304685	17.538765	-0.105894	2.989212
557.308217	2987.425203	17.543770	-0.105788	2.985421
557.257561	2979.443064	17.548775	-0.105773	2.981602
557.764252	2971.355378	17.553779	-0.105862	2.977756
557.611203	2963.420984	17.558784	-0.105829	2.973944
557.658345	2955.401854	17.563789	-0.105832	2.970097
557.859589	2947.411530	17.568794	-0.105865	2.966267
557.956523	2939.462784	17.573799	-0.105878	2.962446
557.577291	2931.509718	17.578803	-0.105802	2.958594
557.746573	2923.549144	17.583808	-0.105828	2.954762
557.954850	2915.510626	17.588813	-0.105862	2.950889
557.400518	2907.599682	17.593818	-0.105753	2.947033
557.355116	2899.628474	17.598823	-0.105740	2.943169
557.011984	2891.675816	17.603827	-0.105671	2.939293
557.347789	2883.653806	17.608832	-0.105728	2.935415
557.329270	2875.636770	17.613837	-0.105719	2.931515
557.173267	2867.678175	17.618842	-0.105685	2.927631
556.847873	2859.747567	17.623847	-0.105620	2.923746
556.668816	2851.773860	17.628851	-0.105581	2.919843
556.718735	2843.784374	17.633856	-0.105585	2.915939
556.633704	2835.743371	17.638861	-0.105564	2.911998
557.062513	2827.661504	17.643866	-0.105639	2.908059
556.760583	2819.748295	17.648871	-0.105577	2.904157
556.482603	2811.819103	17.653875	-0.105521	2.900244
556.474187	2803.849848	17.658880	-0.105514	2.896321
556.523423	2795.815980	17.663885	-0.105518	2.892363
556.880109	2787.756217	17.668890	-0.105579	2.888405
556.956515	2779.789162	17.673895	-0.105588	2.884471
556.964572	2771.858873	17.678899	-0.105584	2.880546
556.356797	2764.007259	17.683904	-0.105466	2.876621
556.763140	2755.936990	17.688909	-0.105537	2.872638
556.533492	2747.986369	17.693914	-0.105489	2.868674
556.524279	2739.990019	17.698919	-0.105482	2.864694
556.424979	2732.028742	17.703923	-0.105458	2.860720
556.905121	2723.966089	17.708928	-0.105542	2.856724
556.714151	2716.013046	17.713933	-0.105502	2.852738
556.354631	2708.071670	17.718938	-0.105430	2.848743
556.520246	2700.066304	17.723943	-0.105455	2.844740
556.273077	2692.136576	17.728947	-0.105404	2.840746
556.487315	2684.146203	17.733952	-0.105439	2.836743
556.487879	2676.156102	17.738957	-0.105434	2.832721
556.286497	2668.198629	17.743962	-0.105391	2.828699
556.401670	2660.173604	17.748967	-0.105407	2.824655
556.271349	2652.227732	17.753971	-0.105378	2.820631
556.422521	2644.231886	17.758976	-0.105401	2.816592
555.736996	2636.333477	17.763981	-0.105268	2.812548
555.661610	2628.336362	17.768986	-0.105249	2.808484
555.376366	2620.401539	17.773991	-0.105191	2.804433
555.385679	2612.381689	17.778995	-0.105187	2.800351
555.628077	2604.385006	17.784000	-0.105227	2.796288
555.364663	2596.440929	17.789005	-0.105173	2.792216
555.750853	2588.379821	17.794010	-0.105240	2.788117
555.893455	2580.347206	17.799015	-0.105261	2.784012
555.779776	2572.407412	17.804019	-0.105235	2.779933
555.966971	2564.433778	17.809024	-0.105265	2.775848
555.591865	2556.514677	17.814029	-0.105190	2.771752
555.800286	2548.494729	17.819034	-0.105223	2.767633
555.678230	2540.552701	17.824039	-0.105195	2.763529
555.450375	2532.598783	17.829043	-0.105148	2.759405
555.600100	2524.627376	17.834048	-0.105170	2.755289
555.716295	2516.564607	17.839053	-0.105187	2.751118
555.437844	2508.620249	17.844058	-0.105130	2.746978
555.604511	2500.598605	17.849063	-0.105156	2.742818
555.790719	2492.607684	17.854067	-0.105185	2.738670
555.657749	2484.700262	17.859072	-0.105155	2.734539
555.080433	2476.799290	17.864077	-0.105043	2.730377
555.087344	2468.792011	17.869082	-0.105039	2.726190
555.054889	2460.819604	17.874087	-0.105028	2.722012
554.887508	2452.848262	17.879091	-0.104991	2.717820
555.011824	2444.890530	17.884096	-0.105009	2.713647
554.800156	2436.907686	17.889101	-0.104965	2.709432
555.108341	2428.857634	17.894106	-0.105017	2.705209
555.083166	2420.931086	17.899111	-0.105007	2.701024
554.705960	2412.997985	17.904115	-0.104932	2.696806
554.621243	2405.046842	17.909120	-0.104911	2.692590
554.761821	2396.993847	17.914125	-0.104932	2.688328
554.776721	2388.994629	17.919130	-0.104929	2.684080
554.925777	2381.064465	17.924135	-0.104952	2.679871
554.896943	2373.075245	17.929139	-0.104941	2.675612
554.535916	2365.175502	17.934144	-0.104869	2.671372
554.716077	2357.130796	17.939149	-0.104897	2.667083
555.045355	2349.102239	17.944154	-0.104954	2.662806
555.191457	2341.147800	17.949159	-0.104976	2.658550
554.657863	2333.240047	17.954163	-0.104871	2.654267
555.036787	2325.203941	17.959168	-0.104937	2.649968
554.921451	2317.258274	17.964173	-0.104910	2.645679
554.646221	2309.336889	17.969178	-0.104854	2.641385
554.844128	2301.356563	17.974183	-0.104885	2.637084
554.306503	2293.462818	17.979187	-0.104780	2.632773
554.644436	2285.416645	17.984192	-0.104838	2.628431
554.541624	2277.425895	17.989197	-0.104813	2.624083
554.871114	2269.426548	17.994202	-0.104870	2.619752
554.693441	2261.506489	17.999207	-0.104831	2.615422
554.587079	2253.511920	18.004211	-0.104806	2.611050
554.618559	2245.551237	18.009216	-0.104807	2.606698
554.599165	2237.604492	18.014221	-0.104798	2.602343
554.758496	2229.612868	18.019226	-0.104823	2.597968
554.763530	2221.647996	18.024231	-0.104819	2.593590
554.624972	2213.570712	18.029235	-0.104788	2.589133
554.372654	2205.659994	18.034240	-0.104736	2.584752
554.183652	2197.728041	18.039245	-0.104695	2.580356
554.194965	2189.735969	18.044250	-0.104692	2.575933
554.269148	2181.775264	18.049255	-0.104701	2.571525
554.342140	2173.765687	18.054259	-0.104709	2.567082
553.774335	2165.931614	18.059264	-0.104598	2.562683
553.928725	2157.914416	18.064269	-0.104622	2.558226
553.796001	2149.951787	18.069274	-0.104592	2.553771
553.442983	2142.054048	18.074279	-0.104521	2.549329
553.430818	2134.032997	18.079283	-0.104514	2.544835
553.600320	2126.054602	18.084288	-0.104540	2.540369
553.519595	2118.085795	18.089293	-0.104520	2.535883
553.272878	2110.146584	18.094298	-0.104469	2.531394
553.420463	2102.142539	18.099303	-0.104491	2.526889
553.216918	2094.204139	18.104307	-0.104448	2.522387
553.558528	2086.185359	18.109312	-0.104507	2.517871
553.145473	2078.284886	18.114317	-0.104425	2.513359
552.932160	2070.322844	18.119322	-0.104380	2.508819
553.336945	2062.263385	18.124327	-0.104450	2.504260
553.270559	2054.314619	18.129331	-0.104432	2.499722
553.053859	2046.407182	18.134336	-0.104387	2.495188
552.930830	2038.428795	18.139341	-0.104359	2.490611
553.214520	2030.401099	18.144346	-0.104407	2.486029
553.070969	2022.507725	18.149351	-0.104375	2.481483
552.876690	2014.556940	18.154355	-0.104333	2.476892
552.986343	2006.581851	18.159360	-0.104349	2.472301
553.484419	1998.515349	18.164365	-0.104436	2.467678
553.096155	1990.627719	18.169370	-0.104359	2.463084
552.868014	1982.740760	18.174375	-0.104311	2.458492
552.925981	1974.727465	18.179379	-0.104317	2.453841
552.853873	1966.781531	18.184384	-0.104298	2.449210
552.975851	1958.773210	18.189389	-0.104316	2.444549
553.081257	1950.829238	18.194394	-0.104330	2.439915
553.153143	1942.881003	18.199399	-0.104339	2.435268
552.700594	1934.931957	18.204403	-0.104249	2.430570
553.135844	1926.896003	18.209408	-0.104325	2.425881
552.727477	1919.003442	18.214413	-0.104244	2.421202
552.795079	1911.021881	18.219418	-0.104251	2.416499
552.521854	1903.111208	18.224423	-0.104195	2.411801
552.615875	1895.096587	18.229427	-0.104208	2.407061
552.838431	1887.110213	18.234432	-0.104244	2.402339
552.738911	1879.196616	18.239437	-0.104220	2.397626
552.738614	1871.213107	18.244442	-0.104215	2.392870
552.457832	1863.335842	18.249447	-0.104158	2.388145
552.615661	1855.294212	18.254451	-0.104182	2.383347
552.474020	1847.409102	18.259456	-0.104150	2.378609
552.458463	1839.429067	18.264461	-0.104142	2.373816
552.425662	1831.450375	18.269466	-0.104131	2.369011
552.354970	1823.519375	18.274471	-0.104113	2.364223
552.261056	1815.575874	18.279475	-0.104090	2.359416
552.198990	1807.650225	18.284480	-0.104073	2.354612
551.752073	1799.738750	18.289485	-0.103985	2.349775
551.976374	1791.702918	18.294490	-0.104022	2.344908
552.330739	1783.707381	18.299495	-0.104082	2.340066
552.101318	1775.781869	18.304499	-0.104035	2.335209
552.073371	1767.823586	18.309504	-0.104024	2.330338
552.089017	1759.850813	18.314509	-0.104022	2.325452
552.114654	1751.897723	18.319514	-0.104022	2.320568
552.141800	1743.962660	18.324519	-0.104022	2.315685
552.330160	1735.970877	18.329523	-0.104051	2.310771
552.240675	1728.049512	18.334528	-0.104030	2.305866
552.288334	1720.092206	18.339533	-0.104033	2.300939
552.073856	1712.178464	18.344538	-0.103988	2.296007
552.122948	1704.215929	18.349543	-0.103992	2.291057
552.352927	1696.204561	18.354547	-0.104030	2.286081
551.783020	1688.387239	18.359552	-0.103919	2.281146
551.723318	1680.444828	18.364557	-0.103903	2.276167
551.571070	1672.461367	18.369562	-0.103869	2.271142
551.507183	1664.501980	18.374567	-0.103852	2.266130
551.562135	1656.511800	18.379571	-0.103857	2.261097
551.579568	1648.552479	18.384576	-0.103855	2.256069
551.422790	1640.620651	18.389581	-0.103821	2.251032
551.364531	1632.655078	18.394586	-0.103805	2.245971
551.224160	1624.766277	18.399591	-0.103774	2.240940
551.642339	1616.712612	18.404595	-0.103846	2.235842
551.653038	1608.775883	18.409600	-0.103843	2.230772
551.380338	1600.864851	18.414605	-0.103787	2.225680
551.453582	1592.918098	18.419610	-0.103796	2.220585
551.761842	1584.936544	18.424615	-0.103848	2.215477
551.298956	1577.066450	18.429619	-0.103757	2.210360
551.571724	1569.075303	18.434624	-0.103802	2.205219
551.543874	1561.149424	18.439629	-0.103792	2.200081
551.319396	1553.248544	18.444634	-0.103745	2.194929
551.429159	1545.287345	18.449639	-0.103760	2.189756
551.400609	1537.306679	18.454643	-0.103750	2.184546
551.177089	1529.416638	18.459648	-0.103703	2.179364
551.198632	1521.465669	18.464653	-0.103702	2.174153
551.454541	1513.470899	18.469658	-0.103744	2.168923
551.286815	1505.568470	18.474663	-0.103708	2.163701
550.360685	1497.789633	18.479667	-0.103531	2.158476
550.653877	1489.771662	18.484672	-0.103580	2.153196
550.846634	1481.795979	18.489677	-0.103611	2.147921
550.333887	1473.905141	18.494682	-0.103510	2.142622
550.409934	1465.950956	18.499687	-0.103519	2.137325
550.715085	1457.929345	18.504691	-0.103571	2.131991
550.831744	1449.973798	18.509696	-0.103587	2.126669
550.793472	1442.046262	18.514701	-0.103575	2.121339
550.698981	1434.148173	18.519706	-0.103552	2.116009
550.632144	1426.193547	18.524711	-0.103535	2.110630
550.411877	1418.242315	18.529715	-0.103489	2.105225
550.340592	1410.345612	18.534720	-0.103470	2.099858
550.648576	1402.353102	18.539725	-0.103523	2.094448
550.455355	1394.444067	18.544730	-0.103481	2.089033
550.145118	1386.569064	18.549735	-0.103419	2.083615
550.141930	1378.632929	18.554739	-0.103413	2.078171
549.873316	1370.752251	18.559744	-0.103358	2.072724
549.824661	1362.797452	18.564749	-0.103344	2.067234
550.022170	1354.811292	18.569754	-0.103375	2.061733
550.248564	1346.851031	18.574759	-0.103412	2.056238
549.989517	1338.946559	18.579763	-0.103359	2.050718
550.037358	1331.012173	18.584768	-0.103363	2.045193
550.001533	1323.104118	18.589773	-0.103351	2.039663
549.682711	1315.226967	18.594778	-0.103286	2.034110
549.530256	1307.317490	18.599783	-0.103253	2.028537
549.493610	1299.359635	18.604787	-0.103241	2.022926
549.870450	1291.365106	18.609792	-0.103306	2.017317
549.724448	1283.468409	18.614797	-0.103274	2.011707
549.465206	1275.574867	18.619802	-0.103220	2.006071
549.328276	1267.690989	18.624807	-0.103190	2.000439
549.372800	1259.745903	18.629811	-0.103193	1.994767
549.481231	1251.790994	18.634816	-0.103208	1.989078
549.447601	1243.869714	18.639821	-0.103196	1.983382
549.483205	1235.943115	18.644826	-0.103198	1.977674
549.333177	1228.058902	18.649831	-0.103165	1.971959
549.303504	1220.114896	18.654835	-0.103154	1.966197
549.508204	1212.170189	18.659840	-0.103187	1.960444
549.452530	1204.289606	18.664845	-0.103172	1.954692
549.035508	1196.444759	18.669850	-0.103089	1.948909
549.325407	1188.454247	18.674855	-0.103138	1.943080
548.943817	1180.576099	18.679859	-0.103062	1.937242
549.322562	1172.591241	18.684864	-0.103127	1.931392
549.116616	1164.710111	18.689869	-0.103084	1.925535
549.018820	1156.798114	18.694874	-0.103060	1.919651
548.840019	1148.945926	18.699879	-0.103022	1.913783
548.777262	1141.008121	18.704883	-0.103005	1.907846
549.007200	1133.053314	18.709888	-0.103043	1.901912
549.144446	1125.113970	18.714893	-0.103063	1.895960
549.075772	1117.204905	18.719898	-0.103045	1.889988
549.077545	1109.318573	18.724903	-0.103040	1.884023
548.891712	1101.454585	18.729907	-0.103001	1.878034
548.817077	1093.556850	18.734912	-0.102982	1.872013
548.757609	1085.637542	18.739917	-0.102966	1.865958
548.965613	1077.692009	18.744922	-0.102999	1.859894
548.769326	1069.850375	18.749927	-0.102958	1.853843
548.821150	1061.915761	18.754931	-0.102962	1.847730
548.808833	1053.997845	18.759936	-0.102955	1.841601
548.530364	1046.163478	18.764941	-0.102898	1.835486
548.350326	1038.275445	18.769946	-0.102859	1.829319
548.544874	1030.341977	18.774951	-0.102890	1.823142
548.593196	1022.434720	18.779955	-0.102894	1.816946
548.307237	1014.584468	18.784960	-0.102836	1.810734
548.270138	1006.681198	18.789965	-0.102824	1.804488
548.193580	998.809037	18.794970	-0.102804	1.798241
548.067925	990.922498	18.799975	-0.102776	1.791954
547.960610	983.005594	18.804979	-0.102751	1.785623
548.005654	975.106729	18.809984	-0.102754	1.779303
547.845375	967.231964	18.814989	-0.102719	1.772954
547.806350	959.325057	18.819994	-0.102707	1.766572
547.875238	951.440250	18.824999	-0.102714	1.760197
547.835014	943.561445	18.830003	-0.102702	1.753791
547.795571	935.669256	18.835008	-0.102689	1.747351
547.662835	927.814876	18.840013	-0.102660	1.740905
547.544566	919.943575	18.845018	-0.102633	1.734424
547.671844	912.038036	18.850023	-0.102651	1.727922
547.804030	904.122151	18.855027	-0.102671	1.721387
547.616483	896.298701	18.860032	-0.102631	1.714863
547.072290	888.515080	18.865037	-0.102524	1.708299
547.375861	880.540696	18.870042	-0.102576	1.701663
547.617058	872.647515	18.875047	-0.102615	1.695061
547.567438	864.773775	18.880051	-0.102601	1.688410
547.320642	856.947036	18.885056	-0.102550	1.681747
547.166166	849.121102	18.890061	-0.102516	1.675070
546.930916	841.273988	18.895066	-0.102467	1.668337
546.854539	833.410018	18.900071	-0.102448	1.661584
546.801895	825.546928	18.905075	-0.102433	1.654808
546.736406	817.686007	18.910080	-0.102416	1.648003
546.224704	809.900971	18.915085	-0.102316	1.641175
546.561076	801.956423	18.920090	-0.102373	1.634297
546.625188	794.058746	18.925095	-0.102380	1.627393
546.413928	786.213581	18.930099	-0.102336	1.620467
546.507173	778.345856	18.935104	-0.102348	1.613534
546.529208	770.478763	18.940109	-0.102347	1.606562
546.316652	762.659831	18.945114	-0.102302	1.599568
546.274607	754.837352	18.950119	-0.102289	1.592566
546.110404	746.991092	18.955123	-0.102254	1.585493
546.037037	739.165463	18.960128	-0.102235	1.578420
545.818355	731.345294	18.965133	-0.102189	1.571300
545.936224	723.463204	18.970138	-0.102206	1.564139
546.036756	715.639038	18.975143	-0.102220	1.556997
545.544750	707.870210	18.980147	-0.102123	1.549784
545.607399	700.001278	18.985152	-0.102130	1.542528
545.249096	692.221501	18.990157	-0.102058	1.535257
545.441642	684.335992	18.995162	-0.102089	1.527936
545.125168	676.566380	19.000167	-0.102025	1.520611
545.103935	668.741004	19.005171	-0.102016	1.513243
544.874109	660.930920	19.010176	-0.101968	1.505821
544.973718	653.101085	19.015181	-0.101981	1.498395
544.465427	645.344280	19.020186	-0.101882	1.490906
544.647451	637.485968	19.025191	-0.101910	1.483391
544.444716	629.705413	19.030195	-0.101868	1.475852
544.343626	621.866354	19.035200	-0.101844	1.468233
544.304543	614.036089	19.040205	-0.101831	1.460593
543.945748	606.291727	19.045210	-0.101760	1.452945
544.209479	598.427590	19.050215	-0.101804	1.445240
543.505967	590.758061	19.055219	-0.101668	1.437529
543.565693	582.931094	19.060224	-0.101674	1.429744
543.393832	575.146917	19.065229	-0.101637	1.421921
543.552001	567.307604	19.070234	-0.101661	1.414055
543.064301	559.596019	19.075239	-0.101565	1.406165
542.491432	551.906582	19.080243	-0.101454	1.398239
542.015310	544.180551	19.085248	-0.101360	1.390246
541.601252	536.432009	19.090253	-0.101278	1.382195
541.396750	528.647131	19.095258	-0.101235	1.374094
540.554007	520.981517	19.100263	-0.101073	1.365959
539.995121	513.263859	19.105267	-0.100964	1.357770
539.652431	505.499440	19.110272	-0.100895	1.349519
539.210612	497.762972	19.115277	-0.100808	1.341230
538.458734	490.079719	19.120282	-0.100663	1.332891
538.166566	482.326856	19.125287	-0.100603	1.324506
536.899084	474.754414	19.130291	-0.100362	1.316087
535.993725	466.999390	19.135296	-0.100189	1.307479
535.647248	459.223908	19.140301	-0.100119	1.298895
535.570796	451.411471	19.145306	-0.100100	1.290264
534.949106	443.732998	19.150311	-0.099979	1.281621
534.246959	436.077870	19.155315	-0.099844	1.272929
533.696797	428.367737	19.160320	-0.099736	1.264145
532.913418	420.732294	19.165325	-0.099585	1.255339
532.196058	413.052329	19.170330	-0.099447	1.246433
531.682267	405.385097	19.175335	-0.099346	1.237516
530.997654	397.720142	19.180339	-0.099214	1.228503
530.369379	390.051909	19.185344	-0.099092	1.219431
529.781026	382.385088	19.190349	-0.098977	1.210300
529.473308	374.673757	19.195354	-0.098915	1.201104
528.607547	367.102360	19.200359	-0.098749	1.191890
528.114743	359.426735	19.205363	-0.098652	1.182555
527.275902	351.844054	19.210368	-0.098491	1.173186
527.078464	344.151838	19.215373	-0.098449	1.163742
526.098510	336.601302	19.220378	-0.098262	1.154230
525.852869	328.908639	19.225383	-0.098211	1.144618
525.274187	321.307818	19.230387	-0.098099	1.134969
524.411867	313.756321	19.235392	-0.097933	1.125237
523.960144	306.155330	19.240397	-0.097844	1.115447
523.644866	298.523101	19.245402	-0.097781	1.105559
523.068965	290.980994	19.250407	-0.097668	1.095642
522.235699	283.467001	19.255411	-0.097508	1.085612
521.552137	275.951002	19.260416	-0.097376	1.075520
520.774885	268.451397	19.265421	-0.097227	1.065332
520.567673	260.842108	19.270426	-0.097183	1.055030
519.952618	253.333953	19.275431	-0.097064	1.044669
519.277603	245.861012	19.280435	-0.096933	1.034237
519.115607	238.282590	19.285440	-0.096898	1.023676
518.493064	230.833123	19.290445	-0.096778	1.013074
518.194547	223.322249	19.295450	-0.096717	1.002352
517.576128	215.891876	19.300455	-0.096597	0.991550
517.071722	208.417514	19.305459	-0.096498	0.980593
516.757117	200.952350	19.310464	-0.096435	0.969575
516.437262	193.519844	19.315469	-0.096371	0.958477
515.831298	186.138887	19.320474	-0.096253	0.947251
515.314702	178.779075	19.325479	-0.096152	0.935946
514.654617	171.441824	19.330483	-0.096024	0.924499
513.941155	164.145102	19.335488	-0.095887	0.912956
513.562368	156.783317	19.340493	-0.095812	0.901255
512.884932	149.508233	19.345498	-0.095681	0.889456
512.386914	142.229526	19.350503	-0.095583	0.877542
511.470111	135.034742	19.355507	-0.095408	0.865481
511.019804	127.777572	19.360512	-0.095319	0.853283
510.520694	120.556471	19.365517	-0.095222	0.840953
509.861106	113.376381	19.370522	-0.095094	0.828462
509.267912	106.209532	19.375527	-0.094979	0.815823
508.650455	99.073318	19.380531	-0.094860	0.803031
507.591180	92.059684	19.385536	-0.094658	0.790113
507.161419	84.950164	19.390541	-0.094573	0.777007
506.568405	77.896443	19.395546	-0.094458	0.763727
506.230723	71.036358	19.400551	-0.094391	0.750666