Fri Apr 16 19:05:11 2021

Number of Points = 3637
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.920455	0.121488	0.000000	0.000060	0.311065

1.869435	0.132703	0.005005	0.000069	0.311074
1.784847	0.147796	0.010010	0.000085	0.311073
1.985876	0.109510	0.015014	0.000048	0.311065
2.053308	0.099162	0.020019	0.000035	0.311074
1.649608	0.171523	0.025024	0.000110	0.311070
1.782164	0.102690	0.030029	0.000085	0.310862
1.548414	0.123866	0.035034	0.000129	0.310763
1.751974	0.084983	0.040038	0.000091	0.310754
2.008132	0.039037	0.045043	0.000043	0.310757
1.886525	0.060078	0.050048	0.000066	0.310752
1.906973	0.058058	0.055053	0.000062	0.310760
1.767164	0.083156	0.060058	0.000088	0.310759
1.819637	0.074447	0.065062	0.000078	0.310763
1.700294	0.097816	0.070067	0.000100	0.310771
1.752664	0.085006	0.075072	0.000091	0.310756
1.673486	0.101887	0.080077	0.000105	0.310767
1.888592	0.061418	0.085082	0.000065	0.310761
1.479205	0.136046	0.090086	0.000141	0.310762
1.554218	0.117248	0.095091	0.000128	0.310739
1.712039	0.040078	0.100096	0.000098	0.310513
1.412739	0.097302	0.105101	0.000154	0.310526
1.654146	0.049990	0.110106	0.000109	0.310510
1.854970	0.012447	0.115110	0.000071	0.310505
1.944770	-0.002169	0.120115	0.000055	0.310514
1.730438	0.036401	0.125120	0.000095	0.310512
1.871957	-0.033177	0.130125	0.000068	0.310308
1.713595	-0.033223	0.135130	0.000098	0.310173
1.682390	-0.028546	0.140134	0.000103	0.310169
1.529333	0.001239	0.145139	0.000132	0.310178
1.495384	0.005899	0.150144	0.000138	0.310171
1.545323	-0.038577	0.155149	0.000129	0.310006
1.208912	-0.006980	0.160154	0.000191	0.309869
1.477247	-0.058789	0.165158	0.000142	0.309855
1.578018	-0.075344	0.170163	0.000123	0.309863
1.663648	-0.097878	0.175168	0.000107	0.309830
1.938554	-0.213844	0.180173	0.000056	0.309522
1.958864	-0.217473	0.185178	0.000052	0.309523
1.781001	-0.186855	0.190182	0.000085	0.309515
1.824222	-0.225917	0.195187	0.000077	0.309369
1.394599	-0.174496	0.200192	0.000157	0.309245
1.531002	-0.197233	0.205197	0.000131	0.309254
1.597976	-0.217165	0.210202	0.000119	0.309218
1.893348	-0.340198	0.215206	0.000064	0.308894
1.789068	-0.318312	0.220211	0.000083	0.308907
1.601538	-0.291428	0.225216	0.000118	0.308874
1.310009	-0.296779	0.230221	0.000172	0.308601
1.279688	-0.290269	0.235226	0.000178	0.308606
1.156719	-0.269497	0.240230	0.000201	0.308598
1.139710	-0.333053	0.245235	0.000204	0.308286
1.322692	-0.370130	0.250240	0.000170	0.308268
1.177608	-0.344694	0.255245	0.000197	0.308264
1.020204	-0.373202	0.260250	0.000226	0.307996
1.420043	-0.449799	0.265254	0.000152	0.307977
1.879720	-0.562394	0.270259	0.000066	0.307841
1.373124	-0.513783	0.275264	0.000160	0.307637
1.468736	-0.530821	0.280269	0.000143	0.307639
1.573625	-0.614234	0.285274	0.000123	0.307336
1.407141	-0.587786	0.290278	0.000154	0.307318
1.160624	-0.579302	0.295283	0.000200	0.307147
1.377198	-0.651872	0.300288	0.000160	0.306991
1.646768	-0.717849	0.305293	0.000109	0.306911
1.364190	-0.707562	0.310298	0.000162	0.306718
1.554598	-0.753953	0.315302	0.000127	0.306662
1.626422	-0.825221	0.320307	0.000113	0.306387
1.173846	-0.746463	0.325312	0.000197	0.306371
1.180102	-0.808667	0.330317	0.000196	0.306083
1.380610	-0.847380	0.335322	0.000159	0.306072
1.000773	-0.839699	0.340326	0.000230	0.305782
1.154799	-0.869475	0.345331	0.000201	0.305774
1.218497	-0.935800	0.350336	0.000189	0.305515
1.367636	-0.965242	0.355341	0.000161	0.305504
1.014134	-0.970282	0.360346	0.000227	0.305176
0.896462	-0.952763	0.365350	0.000249	0.305158
1.158883	-1.064520	0.370355	0.000200	0.304854
1.099517	-1.068139	0.375360	0.000211	0.304786
0.756689	-1.059633	0.380365	0.000275	0.304530
1.332664	-1.187904	0.385370	0.000168	0.304418
1.365915	-1.236295	0.390374	0.000162	0.304217
1.151204	-1.237300	0.395379	0.000202	0.304027
0.967941	-1.231749	0.400384	0.000236	0.303895
1.010953	-1.297260	0.405389	0.000228	0.303620
1.097344	-1.331454	0.410394	0.000212	0.303532
1.003523	-1.373168	0.415398	0.000229	0.303252
0.807534	-1.363790	0.420403	0.000265	0.303127
0.528743	-1.344576	0.425408	0.000317	0.302977
0.590688	-1.413344	0.430413	0.000306	0.302703
0.759644	-1.468453	0.435418	0.000274	0.302586
0.492875	-1.474444	0.440422	0.000324	0.302326
0.489757	-1.507907	0.445427	0.000325	0.302163
0.231613	-1.493436	0.450432	0.000373	0.302008
0.245171	-1.549361	0.455437	0.000370	0.301752
0.618016	-1.647674	0.460442	0.000301	0.301605
0.354126	-1.647231	0.465446	0.000350	0.301377
0.092649	-1.644168	0.470451	0.000398	0.301164
0.309667	-1.716337	0.475456	0.000358	0.301007
0.698018	-1.841458	0.480461	0.000286	0.300745
0.534607	-1.847198	0.485466	0.000316	0.300574
0.393237	-1.855364	0.490470	0.000342	0.300411
0.297239	-1.887057	0.495475	0.000360	0.300175
-0.084068	-1.871075	0.500480	0.000431	0.299918
0.320961	-1.982124	0.505485	0.000356	0.299737
0.064730	-1.978798	0.510490	0.000404	0.299529
-0.622254	-1.906202	0.515494	0.000531	0.299276
-0.312569	-1.996214	0.520499	0.000474	0.299113
-0.256804	-2.050813	0.525504	0.000463	0.298898
-0.589098	-2.050471	0.530509	0.000525	0.298608
-0.853277	-2.036951	0.535514	0.000574	0.298441
-1.079509	-2.028373	0.540518	0.000616	0.298283
-1.231221	-2.057161	0.545523	0.000645	0.298010
-1.906074	-1.969835	0.550528	0.000770	0.297838
-1.631749	-2.058515	0.555533	0.000719	0.297650
-1.895079	-2.070228	0.560538	0.000768	0.297360
-2.038433	-2.078609	0.565542	0.000795	0.297193
-2.332934	-2.061875	0.570547	0.000850	0.297014
-2.460363	-2.089684	0.575552	0.000873	0.296765
-2.590081	-2.094301	0.580557	0.000898	0.296628
-3.137832	-2.040928	0.585562	0.000999	0.296403
-3.315778	-2.050120	0.590566	0.001033	0.296200
-3.435584	-2.049793	0.595571	0.001055	0.296095
-3.627934	-2.080976	0.600576	0.001091	0.295772
-4.136986	-2.002413	0.605581	0.001185	0.295704
-4.446500	-1.981718	0.610586	0.001243	0.295530
-4.165304	-2.073987	0.615590	0.001191	0.295329
-4.345698	-2.070724	0.620595	0.001224	0.295184
-5.388742	-1.934787	0.625600	0.001418	0.294921
-4.896005	-2.037318	0.630605	0.001327	0.294858
-5.360155	-2.014433	0.635610	0.001413	0.294556
-5.519267	-2.000460	0.640614	0.001443	0.294483
-6.147474	-1.930124	0.645619	0.001559	0.294267
-5.472028	-2.079899	0.650624	0.001434	0.294135
-5.447735	-2.134025	0.655629	0.001429	0.293890
-5.748558	-2.111495	0.660634	0.001485	0.293732
-6.257497	-2.046507	0.665638	0.001580	0.293596
-6.100696	-2.120592	0.670643	0.001551	0.293372
-7.013518	-1.970716	0.675648	0.001721	0.293293
-7.062017	-2.010203	0.680653	0.001730	0.293055
-6.806419	-2.070210	0.685658	0.001682	0.292988
-7.202716	-2.062112	0.690662	0.001756	0.292672
-7.249338	-2.057614	0.695667	0.001764	0.292652
-7.437179	-2.087826	0.700672	0.001799	0.292334
-7.252034	-2.129216	0.705677	0.001765	0.292296
-7.758026	-2.096360	0.710682	0.001859	0.292003
-7.690257	-2.116997	0.715686	0.001846	0.291962
-7.854481	-2.135569	0.720691	0.001877	0.291722
-8.643660	-2.002470	0.725696	0.002024	0.291671
-9.172335	-1.959558	0.730701	0.002122	0.291407
-8.372943	-2.113764	0.735706	0.001973	0.291363
-9.329376	-1.994630	0.740710	0.002151	0.291091
-9.602755	-1.942042	0.745715	0.002202	0.291106
-9.279626	-2.061515	0.750720	0.002142	0.290804
-9.218294	-2.080470	0.755725	0.002131	0.290765
-9.483573	-2.074603	0.760730	0.002180	0.290555
-9.776933	-2.032055	0.765734	0.002235	0.290501
-9.921992	-2.050840	0.770739	0.002262	0.290276
-9.881933	-2.083251	0.775744	0.002254	0.290151
-9.927704	-2.114057	0.780749	0.002263	0.289956
-10.550838	-2.020457	0.785754	0.002378	0.289858
-10.276998	-2.105223	0.790758	0.002328	0.289683
-10.631196	-2.074140	0.795763	0.002393	0.289517
-10.382642	-2.142482	0.800768	0.002347	0.289401
-10.655746	-2.129544	0.805773	0.002398	0.289218
-11.203481	-2.043213	0.810778	0.002500	0.289152
-11.446046	-2.050343	0.815782	0.002545	0.288895
-10.985835	-2.137682	0.820787	0.002459	0.288877
-11.708291	-2.065348	0.825792	0.002594	0.288582
-11.855496	-2.038097	0.830797	0.002621	0.288584
-11.360596	-2.182087	0.835802	0.002529	0.288313
-11.456468	-2.178452	0.840806	0.002547	0.288244
-12.010466	-2.118013	0.845811	0.002650	0.288042
-12.402273	-2.062471	0.850816	0.002723	0.287963
-11.991605	-2.173533	0.855821	0.002646	0.287781
-12.279524	-2.152958	0.860826	0.002700	0.287621
-12.575246	-2.122493	0.865830	0.002755	0.287504
-12.800814	-2.120334	0.870835	0.002797	0.287308
-12.867028	-2.115230	0.875840	0.002809	0.287274
-13.149512	-2.120767	0.880845	0.002862	0.286987
-12.960835	-2.155289	0.885850	0.002827	0.286986
-13.714719	-2.068656	0.890854	0.002967	0.286732
-13.540637	-2.106334	0.895859	0.002935	0.286701
-13.645940	-2.125176	0.900864	0.002954	0.286510
-13.722577	-2.140009	0.905869	0.002968	0.286365
-13.658246	-2.172008	0.910874	0.002956	0.286262
-14.362337	-2.086492	0.915878	0.003087	0.286047
-13.599254	-2.227965	0.920883	0.002945	0.286034
-14.328137	-2.154793	0.925888	0.003081	0.285733
-14.507860	-2.124261	0.930893	0.003114	0.285723
-14.443078	-2.172581	0.935898	0.003102	0.285538
-14.663338	-2.145342	0.940902	0.003143	0.285473
-14.842591	-2.144118	0.945907	0.003177	0.285314
-15.311952	-2.093964	0.950912	0.003264	0.285136
-14.897356	-2.179953	0.955917	0.003187	0.285082
-15.152177	-2.184663	0.960922	0.003234	0.284823
-15.510194	-2.121899	0.965926	0.003301	0.284811
-15.667012	-2.145635	0.970931	0.003330	0.284546
-16.006415	-2.094112	0.975936	0.003393	0.284494
-15.920984	-2.134556	0.980941	0.003377	0.284367
-16.354495	-2.085613	0.985946	0.003458	0.284215
-16.200083	-2.115140	0.990950	0.003429	0.284208
-16.319464	-2.159376	0.995955	0.003451	0.283872
-16.473233	-2.133856	1.000960	0.003480	0.283860
-16.452452	-2.172638	1.005965	0.003476	0.283682
-17.079672	-2.081177	1.010970	0.003593	0.283567
-17.442074	-2.023016	1.015974	0.003660	0.283527
-17.115953	-2.136317	1.020979	0.003600	0.283252
-17.517418	-2.062836	1.025984	0.003674	0.283254
-17.889749	-2.030788	1.030989	0.003743	0.283072
-18.112691	-2.011729	1.035994	0.003785	0.282963
-18.189762	-1.995927	1.040998	0.003799	0.282972
-17.985967	-2.090757	1.046003	0.003761	0.282676
-18.391057	-2.029376	1.051008	0.003837	0.282614
-17.904531	-2.138714	1.056013	0.003746	0.282507
-18.748312	-2.021216	1.061018	0.003903	0.282323
-18.935262	-1.989661	1.066022	0.003938	0.282311
-19.043703	-2.006549	1.071027	0.003958	0.282123
-19.337432	-1.978514	1.076032	0.004013	0.281993
-19.357873	-1.972818	1.081037	0.004016	0.282003
-19.082303	-2.072714	1.086042	0.003965	0.281748
-19.361999	-2.032488	1.091046	0.004017	0.281693
-19.625456	-1.994955	1.096051	0.004066	0.281640
-19.787640	-2.018461	1.101056	0.004096	0.281368
-19.650751	-2.043310	1.106061	0.004071	0.281368
-19.651918	-2.072917	1.111066	0.004071	0.281215
-20.449457	-1.957682	1.116070	0.004219	0.281062
-19.941732	-2.049883	1.121075	0.004125	0.281062
-20.273329	-2.042578	1.126080	0.004187	0.280790
-20.424325	-2.025149	1.131085	0.004215	0.280738
-20.477510	-2.022688	1.136090	0.004225	0.280701
-20.935805	-1.975498	1.141094	0.004310	0.280515
-20.825516	-1.994240	1.146099	0.004289	0.280522
-21.331902	-1.927179	1.151104	0.004384	0.280393
-21.027397	-2.026708	1.156109	0.004327	0.280165
-20.982524	-2.032754	1.161114	0.004319	0.280176
-21.609295	-1.962766	1.166118	0.004435	0.279949
-21.546302	-1.992417	1.171123	0.004423	0.279855
-21.317296	-2.035292	1.176128	0.004381	0.279848
-21.645854	-2.037615	1.181133	0.004442	0.279527
-21.622424	-2.043590	1.186138	0.004438	0.279519
-21.480080	-2.092765	1.191142	0.004411	0.279398
-22.135385	-2.002877	1.196147	0.004533	0.279247
-22.151806	-2.002485	1.201152	0.004536	0.279233
-22.277289	-2.024882	1.206157	0.004559	0.278999
-22.205287	-2.057264	1.211162	0.004546	0.278899
-22.476758	-2.016753	1.216166	0.004596	0.278853
-22.311568	-2.099894	1.221171	0.004566	0.278578
-22.321077	-2.100268	1.226176	0.004567	0.278567
-22.524927	-2.099861	1.231181	0.004605	0.278376
-22.851212	-2.062941	1.236186	0.004666	0.278260
-22.862512	-2.064135	1.241190	0.004668	0.278243
-22.722477	-2.142196	1.246195	0.004642	0.277970
-23.612159	-1.979378	1.251200	0.004808	0.277975
-23.520695	-2.025676	1.256205	0.004791	0.277821
-23.084293	-2.142545	1.261210	0.004709	0.277625
-23.452594	-2.077392	1.266214	0.004778	0.277616
-24.141627	-2.001379	1.271219	0.004906	0.277359
-24.258093	-1.986052	1.276224	0.004928	0.277329
-23.790894	-2.088206	1.281229	0.004841	0.277239
-24.560779	-1.994043	1.286234	0.004984	0.277000
-24.178026	-2.067514	1.291238	0.004913	0.276980
-23.973566	-2.135337	1.296243	0.004875	0.276820
-24.660852	-2.034241	1.301248	0.005003	0.276695
-24.728754	-2.020470	1.306253	0.005015	0.276703
-24.521794	-2.119349	1.311258	0.004977	0.276382
-25.112090	-2.015875	1.316262	0.005086	0.276362
-25.223467	-2.011685	1.321267	0.005107	0.276278
-25.005039	-2.093847	1.326272	0.005066	0.276056
-25.012130	-2.092529	1.331277	0.005068	0.276056
-25.698625	-2.009747	1.336282	0.005196	0.275836
-25.861574	-1.996136	1.341286	0.005226	0.275752
-25.391184	-2.087324	1.346291	0.005138	0.275722
-26.290047	-1.962304	1.351296	0.005306	0.275520
-26.640127	-1.897235	1.356301	0.005371	0.275528
-25.936759	-2.043502	1.361306	0.005240	0.275432
-26.132628	-2.059339	1.366310	0.005276	0.275161
-26.497998	-1.989443	1.371315	0.005344	0.275179
-27.040479	-1.926183	1.376320	0.005445	0.274993
-27.175294	-1.926452	1.381325	0.005470	0.274863
-26.949934	-1.968047	1.386330	0.005428	0.274860
-27.277640	-1.955703	1.391334	0.005489	0.274611
-27.400848	-1.945003	1.396339	0.005512	0.274549
-27.975877	-1.839591	1.401344	0.005619	0.274554
-27.918304	-1.896224	1.406349	0.005608	0.274311
-27.593458	-1.967152	1.411354	0.005548	0.274248
-27.486849	-1.991871	1.416358	0.005528	0.274220
-28.063813	-1.943677	1.421363	0.005635	0.273921
-28.355978	-1.888980	1.426368	0.005690	0.273929
-28.162584	-1.935012	1.431373	0.005654	0.273872
-28.458588	-1.930650	1.436378	0.005709	0.273610
-28.731988	-1.881587	1.441382	0.005760	0.273607
-28.413308	-1.953720	1.446387	0.005700	0.273532
-28.982069	-1.894859	1.451392	0.005806	0.273296
-28.758590	-1.938000	1.456397	0.005764	0.273283
-28.890438	-1.932785	1.461402	0.005789	0.273184
-29.181163	-1.915330	1.466406	0.005843	0.272996
-28.975132	-1.952819	1.471411	0.005805	0.272997
-29.743381	-1.849149	1.476416	0.005948	0.272805
-29.447538	-1.930818	1.481421	0.005893	0.272658
-29.585726	-1.903101	1.486426	0.005918	0.272672
-30.191500	-1.838423	1.491430	0.006031	0.272430
-30.077713	-1.872484	1.496435	0.006010	0.272359
-29.859340	-1.914373	1.501440	0.005969	0.272348
-30.021637	-1.935486	1.506445	0.005999	0.272079
-29.734429	-1.999608	1.511450	0.005946	0.272016
-29.982063	-1.965459	1.516454	0.005992	0.271958
-30.052038	-1.997339	1.521459	0.006005	0.271720
-29.974785	-2.012636	1.526464	0.005991	0.271714
-29.901955	-2.064559	1.531469	0.005977	0.271508
-30.302691	-2.013886	1.536474	0.006052	0.271390
-30.708402	-1.943531	1.541478	0.006127	0.271371
-30.540812	-2.027242	1.546483	0.006096	0.271087
-30.461809	-2.042741	1.551488	0.006081	0.271081
-30.995127	-1.975726	1.556493	0.006180	0.270921
-31.156642	-1.974895	1.561498	0.006210	0.270769
-30.650608	-2.070408	1.566502	0.006116	0.270751
-31.027503	-2.044231	1.571507	0.006186	0.270524
-31.341286	-1.992136	1.576512	0.006245	0.270498
-31.172231	-2.049017	1.581517	0.006213	0.270358
-31.226075	-2.077146	1.586522	0.006223	0.270155
-31.486888	-2.031532	1.591526	0.006272	0.270145
-31.543392	-2.076205	1.596531	0.006282	0.269851
-31.871589	-2.018755	1.601536	0.006343	0.269839
-31.960976	-2.030462	1.606541	0.006360	0.269689
-32.154776	-2.028915	1.611546	0.006396	0.269508
-31.934669	-2.070446	1.616550	0.006355	0.269500
-31.991406	-2.110203	1.621555	0.006365	0.269231
-32.620389	-1.995906	1.626560	0.006483	0.269231
-32.478199	-2.053346	1.631565	0.006456	0.269061
-32.687779	-2.047669	1.636570	0.006495	0.268887
-33.307695	-1.934125	1.641574	0.006610	0.268891
-33.239142	-1.995266	1.646579	0.006598	0.268629
-33.411508	-1.970795	1.651584	0.006630	0.268592
-33.817631	-1.907880	1.656589	0.006705	0.268533
-33.713562	-1.976006	1.661594	0.006686	0.268268
-33.887688	-1.944452	1.666598	0.006718	0.268267
-34.024848	-1.944610	1.671603	0.006744	0.268132
-34.077687	-1.964211	1.676608	0.006754	0.267974
-34.187016	-1.944483	1.681613	0.006774	0.267974
-34.210513	-1.988095	1.686618	0.006778	0.267715
-34.692340	-1.915015	1.691622	0.006868	0.267636
-34.127377	-2.027810	1.696627	0.006763	0.267582
-34.330280	-2.041893	1.701632	0.006800	0.267306
-34.731760	-1.967565	1.706637	0.006875	0.267314
-34.646135	-2.016856	1.711642	0.006859	0.267131
-34.712798	-2.033082	1.716646	0.006872	0.266977
-35.131038	-1.953488	1.721651	0.006949	0.266997
-35.363709	-1.963584	1.726656	0.006993	0.266712
-35.351715	-1.965897	1.731661	0.006990	0.266712
-35.505703	-1.958181	1.736666	0.007019	0.266602
-36.904466	-1.738704	1.741670	0.007279	0.266412
-36.599260	-1.793475	1.746675	0.007222	0.266416
-36.029147	-1.918180	1.751680	0.007116	0.266302
-37.144353	-1.750774	1.756685	0.007324	0.266110
-36.383958	-1.893417	1.761690	0.007182	0.266086
-36.323886	-1.928788	1.766694	0.007171	0.265953
-36.643168	-1.905222	1.771699	0.007231	0.265766
-36.961785	-1.845317	1.776704	0.007290	0.265776
-36.868043	-1.895123	1.781709	0.007272	0.265598
-36.599070	-1.961026	1.786714	0.007222	0.265506
-36.632748	-1.958916	1.791718	0.007229	0.265484
-37.011572	-1.950498	1.796723	0.007299	0.265154
-36.880897	-1.974338	1.801728	0.007275	0.265154
-37.073007	-1.967351	1.806733	0.007310	0.265001
-37.574154	-1.903948	1.811738	0.007404	0.264850
-37.206496	-1.974018	1.816742	0.007335	0.264832
-37.432347	-1.980823	1.821747	0.007377	0.264570
-37.662849	-1.950195	1.826752	0.007420	0.264509
-37.753638	-1.946601	1.831757	0.007437	0.264438
-37.845899	-1.967851	1.836762	0.007454	0.264230
-38.162590	-1.910139	1.841766	0.007513	0.264231
-38.221906	-1.939032	1.846771	0.007524	0.264013
-38.276757	-1.952610	1.851776	0.007534	0.263884
-38.523082	-1.907168	1.856781	0.007580	0.263888
-38.747021	-1.921400	1.861786	0.007622	0.263586
-38.533783	-1.963324	1.866790	0.007582	0.263569
-38.931467	-1.907198	1.871795	0.007656	0.263480
-38.725601	-1.987261	1.876800	0.007618	0.263246
-39.159054	-1.906348	1.881805	0.007698	0.263258
-39.159127	-1.943456	1.886810	0.007698	0.263053
-39.600953	-1.878366	1.891814	0.007781	0.262969
-39.281053	-1.943569	1.896819	0.007721	0.262931
-39.452907	-1.967765	1.901824	0.007753	0.262626
-39.708077	-1.921448	1.906829	0.007800	0.262625
-39.701729	-1.951806	1.911834	0.007799	0.262464
-39.985142	-1.929340	1.916838	0.007852	0.262304
-39.848298	-1.952522	1.921843	0.007826	0.262313
-39.985816	-1.987174	1.926848	0.007852	0.261984
-40.315493	-1.928100	1.931853	0.007913	0.261979
-40.070656	-1.993505	1.936858	0.007868	0.261864
-40.712098	-1.906859	1.941862	0.007987	0.261698
-40.710243	-1.907277	1.946867	0.007987	0.261698
-40.290678	-2.033776	1.951872	0.007909	0.261420
-40.649245	-1.980470	1.956877	0.007975	0.261354
-40.893271	-1.953616	1.961882	0.008021	0.261257
-41.055125	-1.962558	1.966886	0.008051	0.261044
-40.462658	-2.070520	1.971891	0.007941	0.261044
-40.757359	-2.069932	1.976896	0.007995	0.260749
-41.224554	-1.989060	1.981901	0.008082	0.260727
-41.244680	-2.004332	1.986906	0.008086	0.260622
-41.533082	-1.976865	1.991910	0.008140	0.260483
-41.610635	-1.963676	1.996915	0.008154	0.260478
-42.157304	-1.921806	2.001920	0.008256	0.260158

-42.119618	-1.965639	2.011917	0.008249	0.259952
-42.149927	-1.988158	2.021914	0.008254	0.259796
-42.484697	-1.980462	2.031910	0.008317	0.259500
-42.566723	-1.984241	2.041907	0.008332	0.259396
-42.447033	-2.040195	2.051904	0.008310	0.259205
-42.658796	-2.019089	2.061901	0.008349	0.259108
-43.006143	-1.996898	2.071898	0.008414	0.258879
-43.095058	-1.980794	2.081894	0.008430	0.258879
-43.267221	-1.977575	2.091891	0.008462	0.258722
-43.377051	-1.985539	2.101888	0.008482	0.258566
-43.201154	-2.018414	2.111885	0.008450	0.258562
-43.343124	-1.990886	2.121882	0.008476	0.258571
-43.700918	-1.925468	2.131878	0.008542	0.258574
-43.284715	-2.002365	2.141875	0.008465	0.258567
-43.415315	-1.978095	2.151872	0.008489	0.258571
-43.795408	-1.934667	2.161869	0.008560	0.258427
-43.464239	-1.967249	2.171866	0.008498	0.258582
-43.366893	-1.987403	2.181862	0.008480	0.258569
-43.309492	-1.997754	2.191859	0.008469	0.258570
-43.489318	-1.965586	2.201856	0.008503	0.258567
-43.251076	-2.009329	2.211853	0.008458	0.258565
-43.395845	-1.982017	2.221850	0.008485	0.258571
-43.628627	-1.938477	2.231846	0.008528	0.258578
-43.338401	-1.993163	2.241843	0.008474	0.258568
-43.579481	-1.896351	2.251840	0.008519	0.258864
-43.569474	-1.892195	2.261837	0.008517	0.258898
-43.202477	-1.960958	2.271834	0.008449	0.258887
-43.097265	-1.940616	2.281830	0.008429	0.259109
-42.415538	-2.046984	2.291827	0.008302	0.259208
-42.699468	-1.995098	2.301824	0.008355	0.259209
-42.684872	-1.975386	2.311821	0.008352	0.259334
-42.151225	-2.043703	2.321818	0.008253	0.259495
-42.524271	-1.975290	2.331814	0.008322	0.259499
-41.952150	-2.032166	2.341811	0.008216	0.259763
-42.553536	-1.909712	2.351808	0.008327	0.259836
-42.241779	-1.936542	2.361805	0.008269	0.260002
-42.307699	-1.895264	2.371802	0.008282	0.260166
-41.760350	-1.968132	2.381798	0.008180	0.260315
-41.404680	-2.002958	2.391795	0.008113	0.260481
-41.755210	-1.917988	2.401792	0.008178	0.260600
-41.360832	-1.964835	2.411789	0.008105	0.260738
-41.346980	-1.934902	2.421786	0.008102	0.260919
-41.133165	-1.949004	2.431782	0.008062	0.261057
-40.836677	-1.960621	2.441779	0.008007	0.261292
-40.923863	-1.930749	2.451776	0.008023	0.261370
-40.547430	-1.939265	2.461773	0.007953	0.261702
-40.640053	-1.903642	2.471770	0.007970	0.261806
-40.392580	-1.915081	2.481766	0.007924	0.261992
-40.247560	-1.896779	2.491763	0.007897	0.262240
-40.145336	-1.890135	2.501760	0.007878	0.262379
-39.733669	-1.918760	2.511757	0.007801	0.262635
-39.600330	-1.902219	2.521754	0.007776	0.262860
-39.360628	-1.919232	2.531750	0.007732	0.263007
-39.329836	-1.878193	2.541747	0.007726	0.263264
-39.050743	-1.890441	2.551744	0.007674	0.263476
-38.959599	-1.875292	2.561741	0.007657	0.263651
-38.517442	-1.910185	2.571738	0.007575	0.263901
-38.081047	-1.947746	2.581734	0.007493	0.264131
-37.872995	-1.960400	2.591731	0.007454	0.264269
-37.676839	-1.952559	2.601728	0.007418	0.264508
-37.180992	-2.004300	2.611725	0.007325	0.264719
-37.245865	-1.964189	2.621722	0.007337	0.264874
-36.798953	-1.995350	2.631718	0.007254	0.265148
-37.004913	-1.914175	2.641715	0.007292	0.265387
-36.794452	-1.921936	2.651712	0.007253	0.265554
-36.339845	-1.966978	2.661709	0.007169	0.265760
-36.429370	-1.904348	2.671706	0.007185	0.266012
-36.127013	-1.923027	2.681702	0.007129	0.266210
-35.820437	-1.946075	2.691699	0.007072	0.266389
-35.567592	-1.929595	2.701696	0.007024	0.266728
-35.285270	-1.950068	2.711693	0.006972	0.266896
-35.219552	-1.927495	2.721690	0.006960	0.267084
-34.820930	-1.953859	2.731686	0.006885	0.267334
-34.963659	-1.878094	2.741683	0.006912	0.267604
-34.331205	-1.955317	2.751680	0.006794	0.267809
-33.786843	-2.019988	2.761677	0.006693	0.267995
-34.242865	-1.882548	2.771674	0.006777	0.268290
-33.704490	-1.937868	2.781670	0.006677	0.268520
-33.796772	-1.881650	2.791667	0.006694	0.268733
-33.068188	-1.980530	2.801664	0.006558	0.268914
-32.526092	-2.019695	2.811661	0.006457	0.269234
-32.538558	-1.985908	2.821658	0.006460	0.269404
-32.379667	-1.980935	2.831654	0.006430	0.269587
-32.234311	-1.957740	2.841651	0.006403	0.269853
-32.193323	-1.914291	2.851648	0.006395	0.270127
-31.622253	-1.976365	2.861645	0.006289	0.270351
-31.548151	-1.952379	2.871642	0.006275	0.270552
-31.275259	-1.960096	2.881638	0.006224	0.270776
-31.572358	-1.855652	2.891635	0.006279	0.271046
-31.193268	-1.879454	2.901632	0.006209	0.271288
-30.933665	-1.884382	2.911629	0.006160	0.271513
-30.512277	-1.917330	2.921626	0.006082	0.271747
-30.123986	-1.935680	2.931622	0.006009	0.272025
-29.844280	-1.943221	2.941619	0.005957	0.272256
-29.692923	-1.929596	2.951616	0.005929	0.272475
-30.006841	-1.823790	2.961613	0.005987	0.272734
-29.415648	-1.879261	2.971610	0.005877	0.273011
-29.019957	-1.901899	2.981606	0.005803	0.273273
-28.807217	-1.897525	2.991603	0.005764	0.273501
-28.262326	-1.957727	3.001600	0.005662	0.273707
-27.745368	-2.015280	3.011597	0.005566	0.273900
-27.337105	-2.030709	3.021594	0.005490	0.274211
-27.169591	-2.029724	3.031590	0.005459	0.274378
-26.850318	-2.058756	3.041587	0.005399	0.274531
-27.160885	-1.939840	3.051584	0.005457	0.274861
-26.704650	-1.981427	3.061581	0.005372	0.275079
-26.229986	-2.029400	3.071578	0.005284	0.275281
-26.268057	-1.977535	3.081574	0.005290	0.275517
-25.983216	-1.985207	3.091571	0.005237	0.275750
-25.341478	-2.067648	3.101568	0.005118	0.275930
-25.477675	-2.005029	3.111565	0.005143	0.276129
-25.085784	-2.029062	3.121562	0.005070	0.276376
-24.769736	-2.035996	3.131558	0.005011	0.276641
-24.934597	-1.967996	3.141555	0.005042	0.276841
-24.662004	-1.978268	3.151552	0.004991	0.277046
-24.125073	-2.023598	3.161549	0.004891	0.277320
-23.737032	-2.049203	3.171546	0.004819	0.277555
-24.134435	-1.931908	3.181542	0.004893	0.277790
-23.548322	-1.997156	3.191539	0.004783	0.278005
-23.859538	-1.885892	3.201536	0.004841	0.278290
-23.576448	-1.884182	3.211533	0.004788	0.278567
-23.498884	-1.848885	3.221530	0.004774	0.278824
-23.184175	-1.857439	3.231526	0.004715	0.279077
-22.482426	-1.941501	3.241523	0.004585	0.279303
-22.203897	-1.948220	3.251520	0.004533	0.279531
-22.139670	-1.902280	3.261517	0.004521	0.279830
-21.703480	-1.935485	3.271514	0.004439	0.280068
-22.129934	-1.806853	3.281510	0.004519	0.280333
-21.251665	-1.922338	3.291507	0.004355	0.280561
-20.607130	-2.005644	3.301504	0.004235	0.280736
-20.157390	-2.041118	3.311501	0.004151	0.280975
-19.844446	-2.062703	3.321498	0.004093	0.281157
-19.853095	-2.021173	3.331494	0.004094	0.281363
-19.809559	-1.967444	3.341491	0.004086	0.281681
-19.977221	-1.893648	3.351488	0.004117	0.281903
-19.098685	-2.018306	3.361485	0.003954	0.282084
-18.631253	-2.058877	3.371482	0.003867	0.282312
-18.836409	-1.965560	3.381478	0.003905	0.282599
-18.445584	-1.992376	3.391475	0.003832	0.282826
-18.413628	-1.954135	3.401472	0.003826	0.283052
-17.903359	-2.005983	3.411469	0.003731	0.283261
-18.095841	-1.912287	3.421466	0.003767	0.283562
-17.687725	-1.943540	3.431462	0.003691	0.283781
-16.953065	-2.039638	3.441459	0.003554	0.283972
-16.470255	-2.080387	3.451456	0.003464	0.284212
-16.505798	-2.027798	3.461453	0.003470	0.284448
-16.096698	-2.064860	3.471450	0.003394	0.284638
-15.756128	-2.091082	3.481446	0.003331	0.284819
-15.393976	-2.100369	3.491443	0.003263	0.285107
-15.820204	-1.984053	3.501440	0.003342	0.285304
-15.233034	-2.048368	3.511437	0.003233	0.285520
-15.721999	-1.911568	3.521434	0.003324	0.285763
-15.056413	-1.980554	3.531430	0.003200	0.286027
-14.558294	-2.033105	3.541427	0.003107	0.286219
-14.702851	-1.965090	3.551424	0.003134	0.286430
-13.923605	-2.052512	3.561421	0.002989	0.286705
-14.141148	-1.967935	3.571418	0.003029	0.286932
-13.644227	-2.018191	3.581414	0.002937	0.287135
-13.293310	-2.042139	3.591411	0.002871	0.287336
-13.164254	-2.006554	3.601408	0.002847	0.287633
-12.714243	-2.041817	3.611405	0.002763	0.287868
-12.461443	-2.053353	3.621402	0.002716	0.288041
-11.637622	-2.162314	3.631398	0.002563	0.288246
-11.868216	-2.070307	3.641395	0.002606	0.288498
-11.762798	-2.055379	3.651392	0.002586	0.288669
-11.137237	-2.127761	3.661389	0.002470	0.288877
-11.333341	-2.032551	3.671386	0.002506	0.289175
-11.122361	-2.032212	3.681382	0.002467	0.289369
-10.863163	-2.043243	3.691379	0.002418	0.289550
-10.496631	-2.052250	3.701376	0.002350	0.289838
-10.335747	-2.032314	3.711373	0.002320	0.290084
-10.370142	-1.984334	3.721370	0.002326	0.290292
-9.634016	-2.074902	3.731366	0.002189	0.290508
-9.776851	-1.999954	3.741363	0.002216	0.290752
-9.103050	-2.083521	3.751360	0.002090	0.290946
-8.858601	-2.092538	3.761357	0.002045	0.291123
-8.353104	-2.134835	3.771354	0.001950	0.291370
-8.270578	-2.102738	3.781350	0.001935	0.291604
-8.167507	-2.086034	3.791347	0.001916	0.291780
-7.580455	-2.150894	3.801344	0.001806	0.291988
-7.736664	-2.069493	3.811341	0.001835	0.292251
-7.416546	-2.092613	3.821338	0.001776	0.292424
-7.311686	-2.068247	3.831334	0.001756	0.292640
-7.022983	-2.055964	3.841331	0.001702	0.292960
-6.985563	-2.025592	3.851328	0.001695	0.293144
-6.607108	-2.054589	3.861325	0.001625	0.293340
-6.611979	-2.003026	3.871322	0.001626	0.293591
-6.053750	-2.048976	3.881318	0.001522	0.293864
-6.176643	-1.983787	3.891315	0.001544	0.294076
-5.965297	-1.977456	3.901312	0.001505	0.294296
-5.617883	-1.994583	3.911309	0.001440	0.294523
-5.478710	-1.957453	3.921306	0.001414	0.294829
-5.318087	-1.940556	3.931302	0.001384	0.295056
-5.223642	-1.907468	3.941299	0.001367	0.295303
-4.900781	-1.917977	3.951296	0.001306	0.295539
-4.540434	-1.941793	3.961293	0.001239	0.295743
-4.629035	-1.863727	3.971290	0.001256	0.296046
-4.526623	-1.831441	3.981286	0.001236	0.296295
-4.339133	-1.810410	3.991283	0.001201	0.296565
-4.006219	-1.819027	4.001280	0.001139	0.296818
-3.424293	-1.880805	4.011277	0.001031	0.297033
-3.573289	-1.793619	4.021274	0.001059	0.297326
-3.816096	-1.683914	4.031270	0.001104	0.297645
-3.688027	-1.643692	4.041267	0.001080	0.297954
-3.304565	-1.659377	4.051264	0.001008	0.298216
-3.182017	-1.621302	4.061261	0.000985	0.298509
-3.286979	-1.540779	4.071258	0.001005	0.298807
-2.849564	-1.554028	4.081254	0.000923	0.299128
-2.525058	-1.554861	4.091251	0.000863	0.299410
-2.478641	-1.503718	4.101248	0.000854	0.299698
-2.421854	-1.445499	4.111245	0.000843	0.300029
-2.664267	-1.330473	4.121242	0.000888	0.300371
-2.086946	-1.375780	4.131238	0.000781	0.300658
-2.045064	-1.322787	4.141235	0.000773	0.300950
-1.996192	-1.262155	4.151232	0.000764	0.301285
-1.782385	-1.228091	4.161229	0.000724	0.301635
-1.726976	-1.171659	4.171226	0.000714	0.301954
-1.472887	-1.145176	4.181222	0.000666	0.302302
-1.255369	-1.108918	4.191219	0.000626	0.302665
-0.894183	-1.101008	4.201216	0.000558	0.303017
-0.692738	-1.068751	4.211213	0.000521	0.303346
-0.887422	-0.958277	4.221210	0.000557	0.303704
-0.470237	-0.958723	4.231206	0.000479	0.304063
-0.773662	-0.829668	4.241203	0.000535	0.304415
-0.958575	-0.711033	4.251200	0.000570	0.304819
-0.869444	-0.634004	4.261197	0.000553	0.305262
-0.861511	-0.555400	4.271194	0.000551	0.305641
-0.762611	-0.492681	4.281190	0.000533	0.306023
-0.687343	-0.408497	4.291187	0.000519	0.306486
-0.721310	-0.316248	4.301184	0.000525	0.306892
-0.637218	-0.237975	4.311181	0.000509	0.307333
-0.835683	-0.098498	4.321178	0.000546	0.307820
-0.324069	-0.101753	4.331174	0.000451	0.308242
-0.431443	0.020374	4.341171	0.000470	0.308723
-0.423026	0.120288	4.351168	0.000469	0.309198
-0.364330	0.212861	4.361165	0.000458	0.309681
0.000000	0.241749	4.371162	0.000390	0.310126

-0.196407	0.548116	4.376166	0.000426	0.311386
0.027814	1.071482	4.381171	0.000384	0.313996
-0.009961	1.927820	4.386176	0.000390	0.317887
0.514567	2.963200	4.391181	0.000292	0.322992
1.307381	4.252633	4.396186	0.000144	0.329350
2.123559	5.829847	4.401190	-0.000009	0.336845
2.776178	7.742735	4.406195	-0.000132	0.345460
4.461847	9.785608	4.411200	-0.000447	0.355160
6.109781	12.145447	4.416205	-0.000756	0.365830
19.075843	12.812843	4.421210	-0.003171	0.377576
27.241594	14.804068	4.426214	-0.004692	0.390644
28.828261	18.347307	4.431219	-0.004990	0.404575
30.981983	22.156412	4.436224	-0.005394	0.419312
34.046993	26.160715	4.441229	-0.005967	0.434747
37.732195	30.427415	4.446234	-0.006656	0.450852
41.329152	35.102485	4.451238	-0.007329	0.467614
46.067911	39.953738	4.456243	-0.008214	0.484933
50.979378	45.178273	4.461248	-0.009132	0.502814
54.728224	50.986268	4.466253	-0.009834	0.521115
58.977183	57.073372	4.471258	-0.010629	0.539780
63.215403	63.522654	4.476262	-0.011423	0.558750
67.245937	70.363439	4.481267	-0.012178	0.577979
73.276721	77.188212	4.486272	-0.013305	0.597414
78.216572	84.535561	4.491277	-0.014230	0.616997
82.819782	92.262440	4.496282	-0.015092	0.636698
87.482424	100.262503	4.501286	-0.015965	0.656427
93.439920	108.299422	4.506291	-0.017080	0.676149
98.523983	116.731119	4.511296	-0.018032	0.695802
103.124435	125.478174	4.516301	-0.018895	0.715373
107.500595	134.466883	4.521306	-0.019715	0.734814
113.604567	143.319472	4.526310	-0.020858	0.754078
119.635603	152.362551	4.531315	-0.021987	0.773187
123.268965	161.968078	4.536320	-0.022669	0.792080
127.924600	171.468302	4.541325	-0.023542	0.810665
133.191823	180.987200	4.546330	-0.024529	0.829049
137.532662	190.729817	4.551334	-0.025344	0.847133
141.535737	200.547967	4.556339	-0.026096	0.864861
146.151260	210.303635	4.561344	-0.026962	0.882304
151.701288	219.921293	4.566349	-0.028001	0.899446
156.189982	229.759872	4.571354	-0.028844	0.916319
160.334594	239.626758	4.576358	-0.029622	0.932833
164.712917	249.427041	4.581363	-0.030443	0.949017
168.147189	259.375711	4.586368	-0.031089	0.964902
171.429712	269.274052	4.591373	-0.031707	0.980414
175.290870	279.077433	4.596378	-0.032433	0.995691
179.003151	288.788870	4.601382	-0.033130	1.010566
182.972766	298.428482	4.606387	-0.033876	1.025184
186.281256	308.101353	4.611392	-0.034498	1.039481
188.380700	317.917939	4.616397	-0.034895	1.053493
190.519995	327.639861	4.621402	-0.035300	1.067200
192.803999	337.230453	4.626406	-0.035732	1.080591
194.498404	346.852123	4.631411	-0.036053	1.093723
195.654847	356.479362	4.636416	-0.036275	1.106585
196.468277	366.042494	4.641421	-0.036433	1.119140
198.030109	375.401399	4.646426	-0.036730	1.131459
200.469666	384.527667	4.651430	-0.037190	1.143541
202.384738	393.712192	4.656435	-0.037552	1.155456
203.755548	402.894172	4.661440	-0.037814	1.167130
204.219366	412.160268	4.666445	-0.037906	1.178601
205.392972	421.228758	4.671450	-0.038131	1.189869
206.266056	430.264179	4.676454	-0.038299	1.200929
207.648519	439.152159	4.681459	-0.038562	1.211816
208.472403	448.115949	4.686464	-0.038722	1.222583
209.423150	456.994740	4.691469	-0.038904	1.233181
211.118473	465.684281	4.696474	-0.039226	1.243616
212.888311	474.338388	4.701478	-0.039561	1.253936
213.860079	483.101865	4.706483	-0.039748	1.264143
214.768871	491.841467	4.711488	-0.039923	1.274228
215.299499	500.582349	4.716493	-0.040027	1.284163
216.350057	509.230294	4.721498	-0.040229	1.294016
217.621653	517.780065	4.726502	-0.040471	1.303726
218.441379	526.457520	4.731507	-0.040629	1.313421
219.115547	535.060258	4.736512	-0.040760	1.322937
219.610975	543.644523	4.741517	-0.040858	1.332332
220.268548	552.175661	4.746522	-0.040986	1.341633
221.390427	560.596449	4.751526	-0.041201	1.350835
222.237547	569.048086	4.756531	-0.041364	1.359958
222.938039	577.524908	4.761536	-0.041500	1.369021
223.305301	586.050637	4.766541	-0.041574	1.378017
224.425899	594.414459	4.771546	-0.041788	1.386917
225.189326	602.829397	4.776550	-0.041936	1.395751
225.883174	611.206067	4.781555	-0.042070	1.404478
226.884545	619.561844	4.786560	-0.042262	1.413181
227.207507	628.001084	4.791565	-0.042328	1.421802
227.920187	636.364056	4.796570	-0.042466	1.430358
228.531136	644.731635	4.801574	-0.042585	1.438851
229.264274	653.061623	4.806579	-0.042727	1.447277
230.104374	661.400904	4.811584	-0.042889	1.455680
230.761707	669.730893	4.816589	-0.043017	1.463996
231.875821	678.019798	4.821594	-0.043230	1.472298
232.347165	686.374366	4.826598	-0.043323	1.480514
233.166408	694.643441	4.831603	-0.043481	1.488657
234.015610	702.930825	4.836608	-0.043645	1.496778
235.020599	711.162352	4.841613	-0.043837	1.504825
235.989531	719.426330	4.846618	-0.044023	1.512855
236.488741	727.730944	4.851622	-0.044122	1.520808
237.237237	736.010766	4.856627	-0.044266	1.528734
238.215073	744.260750	4.861632	-0.044454	1.536626
238.774266	752.553743	4.866637	-0.044563	1.544454
239.217655	760.886132	4.871642	-0.044651	1.552261
239.665648	769.160794	4.876646	-0.044740	1.559977
240.235992	777.411633	4.881651	-0.044852	1.567651
240.779145	785.691467	4.886656	-0.044958	1.575309
241.361245	793.921843	4.891661	-0.045072	1.582891
241.877021	802.194155	4.896666	-0.045174	1.590465
242.589352	810.394784	4.901670	-0.045312	1.597967
243.247100	818.598840	4.906675	-0.045440	1.605429
243.642343	826.891939	4.911680	-0.045519	1.612898
243.939845	835.139083	4.916685	-0.045579	1.620277
244.173486	843.427744	4.921690	-0.045628	1.627651
245.436825	851.537145	4.926694	-0.045869	1.634978
245.832200	859.762726	4.931699	-0.045948	1.642253
246.416751	867.959081	4.936704	-0.046062	1.649496
247.221520	876.111910	4.941709	-0.046217	1.656700
247.715443	884.332787	4.946714	-0.046315	1.663889
248.023553	892.572745	4.951718	-0.046377	1.671037
248.918930	900.714091	4.956723	-0.046549	1.678150
249.848444	908.840393	4.961728	-0.046728	1.685225
250.140639	917.098835	4.966733	-0.046788	1.692296
250.993848	925.244361	4.971738	-0.046952	1.699318
251.497875	933.452858	4.976742	-0.047051	1.706317
251.875337	941.676553	4.981747	-0.047127	1.713283
252.444359	949.841022	4.986752	-0.047238	1.720196
252.774965	958.045947	4.991757	-0.047305	1.727084
253.452867	966.210572	4.996762	-0.047437	1.733956
253.625424	974.428918	5.001766	-0.047474	1.740780
254.100933	982.603939	5.006771	-0.047568	1.747580
254.490806	990.799599	5.011776	-0.047646	1.754360
254.957695	998.952440	5.016781	-0.047738	1.761089
255.526490	1007.107033	5.021786	-0.047850	1.767806
256.040461	1015.273673	5.026790	-0.047951	1.774500
256.441769	1023.435883	5.031795	-0.048031	1.781152
257.000893	1031.599035	5.036800	-0.048140	1.787798
257.410623	1039.795140	5.041805	-0.048222	1.794428
257.883389	1047.930465	5.046810	-0.048315	1.800993
258.478835	1056.045343	5.051814	-0.048431	1.807533
259.106164	1064.182717	5.056819	-0.048553	1.814070
259.744203	1072.306912	5.061824	-0.048678	1.820575
259.984729	1080.499788	5.066829	-0.048728	1.827062
260.405828	1088.681247	5.071834	-0.048812	1.833539
260.855638	1096.795934	5.076838	-0.048901	1.839944
260.986799	1104.977556	5.081843	-0.048930	1.846341
261.459226	1113.135062	5.086848	-0.049024	1.852737
261.742424	1121.276990	5.091853	-0.049082	1.859077
262.262926	1129.404148	5.096858	-0.049184	1.865412
262.670971	1137.557957	5.101862	-0.049265	1.871733
263.168357	1145.672640	5.106867	-0.049363	1.878013
263.618716	1153.787769	5.111872	-0.049452	1.884266
264.163035	1161.899132	5.116877	-0.049559	1.890507
264.794793	1170.021205	5.121882	-0.049682	1.896745
265.311251	1178.143511	5.126886	-0.049784	1.902950
265.691990	1186.284195	5.131891	-0.049860	1.909132
265.857784	1194.481329	5.136896	-0.049896	1.915313
266.410996	1202.559403	5.141901	-0.050004	1.921428
267.147248	1210.639800	5.146906	-0.050147	1.927546
267.651283	1218.771130	5.151910	-0.050246	1.933656
267.734520	1226.955066	5.156915	-0.050267	1.939739
268.446805	1235.041674	5.161920	-0.050405	1.945801
268.840564	1243.189785	5.166925	-0.050483	1.951854
269.241181	1251.295114	5.171930	-0.050563	1.957857
269.827531	1259.373918	5.176934	-0.050678	1.963843
270.370286	1267.468172	5.181939	-0.050784	1.969817
270.914800	1275.583787	5.186944	-0.050891	1.975788
271.182185	1283.715290	5.191949	-0.050946	1.981723
271.657029	1291.840658	5.196954	-0.051040	1.987658
271.948038	1300.004073	5.201958	-0.051099	1.993583
272.339528	1308.089768	5.206963	-0.051177	1.999445
272.934107	1316.175436	5.211968	-0.051293	2.005311
273.046367	1324.338146	5.216973	-0.051320	2.011164
273.628371	1332.423525	5.221978	-0.051433	2.016994
273.950050	1340.551807	5.226982	-0.051499	2.022811
274.529856	1348.644211	5.231987	-0.051612	2.028612
274.816274	1356.786825	5.236992	-0.051671	2.034402
275.212947	1364.851297	5.241997	-0.051750	2.040132
275.678061	1372.942477	5.247002	-0.051842	2.045871
275.926713	1381.089070	5.252006	-0.051893	2.051610
276.190950	1389.199192	5.257011	-0.051948	2.057310
276.683400	1397.279722	5.262016	-0.052045	2.062996
276.968790	1405.394203	5.267021	-0.052103	2.068669
277.405113	1413.492667	5.272026	-0.052190	2.074331
278.252469	1421.506323	5.277030	-0.052353	2.079960
278.401019	1429.637574	5.282035	-0.052386	2.085585
278.598581	1437.815348	5.287040	-0.052428	2.091231
278.815874	1445.917076	5.292045	-0.052474	2.096812
279.396408	1453.981150	5.297050	-0.052587	2.102388
279.635605	1462.119635	5.302054	-0.052637	2.107966
280.127161	1470.215972	5.307059	-0.052734	2.113526
280.880288	1478.250345	5.312064	-0.052879	2.119054
281.206496	1486.297386	5.317069	-0.052945	2.124535
281.557999	1494.422689	5.322074	-0.053016	2.130057
281.724421	1502.552427	5.327078	-0.053052	2.135549
281.965662	1510.661064	5.332083	-0.053103	2.141021
282.312797	1518.761891	5.337088	-0.053173	2.146483
282.303295	1526.892289	5.342093	-0.053176	2.151917
282.776162	1534.961422	5.347098	-0.053269	2.157343
283.351827	1542.994458	5.352102	-0.053382	2.162741
283.559801	1551.093994	5.357107	-0.053426	2.168134
284.386554	1559.133539	5.362112	-0.053585	2.173532
284.463425	1567.264892	5.367117	-0.053605	2.178907
284.794552	1575.328448	5.372122	-0.053672	2.184248
284.893822	1583.482330	5.377126	-0.053696	2.189614
285.546144	1591.500245	5.382131	-0.053822	2.194929
285.938757	1599.586877	5.387136	-0.053901	2.200251
285.652734	1607.746602	5.392141	-0.053853	2.205546
286.434729	1615.744428	5.397146	-0.054004	2.210821
286.427043	1623.909829	5.402150	-0.054008	2.216119
287.048163	1631.905200	5.407155	-0.054128	2.221352
287.703999	1639.974283	5.412160	-0.054256	2.226624
287.977511	1648.069455	5.417165	-0.054312	2.231865
288.368741	1656.146915	5.422170	-0.054390	2.237093
288.960010	1664.190171	5.427174	-0.054506	2.242305
289.210935	1672.286321	5.432179	-0.054558	2.247507
289.780404	1680.367897	5.437184	-0.054669	2.252717
290.064244	1688.461134	5.442189	-0.054727	2.257897
290.712559	1696.508573	5.447194	-0.054853	2.263068
291.114120	1704.620842	5.452198	-0.054933	2.268246
291.137513	1712.776618	5.457203	-0.054943	2.273407
291.397079	1720.866653	5.462208	-0.054997	2.278535
291.493894	1728.921237	5.467213	-0.055020	2.283615
292.035142	1736.966872	5.472218	-0.055126	2.288717
292.700011	1745.007777	5.477222	-0.055255	2.293815
292.810080	1753.085438	5.482227	-0.055281	2.298877
293.241894	1761.139635	5.487232	-0.055366	2.303940
293.251693	1769.279506	5.492237	-0.055374	2.309010
293.678614	1777.339444	5.497242	-0.055458	2.314054
293.794759	1785.447593	5.502246	-0.055485	2.319091
294.098601	1793.462603	5.507251	-0.055547	2.324075
294.629863	1801.524409	5.512256	-0.055651	2.329097
294.847183	1809.611136	5.517261	-0.055697	2.334096
295.528837	1817.631641	5.522266	-0.055829	2.339083
295.515579	1825.757583	5.527270	-0.055832	2.344066
295.887423	1833.834615	5.532275	-0.055907	2.349040
296.613693	1841.862696	5.537280	-0.056047	2.354003
296.978285	1849.908594	5.542285	-0.056120	2.358937
297.454051	1857.942910	5.547290	-0.056214	2.363862
297.982592	1866.011379	5.552294	-0.056318	2.368802
298.132910	1874.124171	5.557299	-0.056351	2.373727
298.569884	1882.208527	5.562304	-0.056438	2.378649
299.212674	1890.202657	5.567309	-0.056563	2.383522
299.556493	1898.315346	5.572314	-0.056632	2.388433
299.941180	1906.390831	5.577318	-0.056709	2.393314
300.139519	1914.466357	5.582323	-0.056751	2.398170
300.597130	1922.530458	5.587328	-0.056842	2.403031
301.055447	1930.557447	5.592333	-0.056932	2.407859
301.175440	1938.703749	5.597338	-0.056960	2.412722
301.726569	1946.741013	5.602342	-0.057068	2.417544
302.278394	1954.758792	5.607347	-0.057176	2.422345
302.543700	1962.870264	5.612352	-0.057231	2.427169
302.897203	1970.963085	5.617357	-0.057302	2.431980
303.427718	1978.999167	5.622362	-0.057406	2.436761
303.613014	1987.088328	5.627366	-0.057446	2.441537
303.692116	1995.158561	5.632371	-0.057466	2.446285
304.194467	2003.209724	5.637376	-0.057565	2.451044
304.117094	2011.315359	5.642381	-0.057555	2.455782
304.249462	2019.376640	5.647386	-0.057585	2.460501
305.170534	2027.347452	5.652390	-0.057762	2.465218
305.354171	2035.446726	5.657395	-0.057802	2.469945
305.664747	2043.513536	5.662400	-0.057865	2.474653
305.950560	2051.559531	5.667405	-0.057923	2.479338
306.728116	2059.545642	5.672410	-0.058073	2.484017
307.097191	2067.620611	5.677414	-0.058147	2.488708
306.978686	2075.748794	5.682419	-0.058131	2.493383
307.664881	2083.774509	5.687424	-0.058264	2.498052
307.948688	2091.839893	5.692429	-0.058322	2.502704
308.283406	2099.910603	5.697434	-0.058389	2.507354
308.636340	2107.993614	5.702438	-0.058460	2.512004
308.771862	2116.059731	5.707443	-0.058491	2.516619
309.007316	2124.130050	5.712448	-0.058540	2.521236
308.953740	2132.210536	5.717453	-0.058535	2.525829
309.520817	2140.212106	5.722458	-0.058646	2.530414
309.941815	2148.257517	5.727462	-0.058730	2.535005
310.103784	2156.334990	5.732467	-0.058765	2.539587
310.498296	2164.373037	5.737472	-0.058844	2.544155
310.794363	2172.445857	5.742477	-0.058904	2.548728
311.245130	2180.481967	5.747482	-0.058994	2.553282
311.357621	2188.571105	5.752486	-0.059020	2.557834
311.810246	2196.577665	5.757491	-0.059109	2.562356
312.177614	2204.646337	5.762496	-0.059183	2.566898
312.455013	2212.708796	5.767501	-0.059240	2.571422
312.885963	2220.755258	5.772506	-0.059326	2.575941
313.063085	2228.852156	5.777510	-0.059364	2.580461
313.286857	2236.869211	5.782515	-0.059411	2.584933
313.222363	2245.015208	5.787520	-0.059404	2.589448
313.850402	2253.106824	5.792525	-0.059526	2.593973
314.113069	2261.111666	5.797530	-0.059580	2.598417
314.528146	2269.120027	5.802534	-0.059663	2.602866
314.407345	2277.208083	5.807539	-0.059646	2.607314
314.885928	2285.245973	5.812544	-0.059740	2.611768
315.082400	2293.300973	5.817549	-0.059782	2.616205
315.681964	2301.272189	5.822554	-0.059899	2.620615
316.075319	2309.318853	5.827558	-0.059977	2.625046
316.102238	2317.402896	5.832563	-0.059988	2.629464
316.368164	2325.479772	5.837568	-0.060043	2.633887
316.632498	2333.494841	5.842573	-0.060097	2.638269
316.905912	2341.528026	5.847578	-0.060153	2.642654
317.242931	2349.577231	5.852582	-0.060221	2.647045
317.470270	2357.660750	5.857587	-0.060269	2.651439
317.526503	2365.760411	5.862592	-0.060285	2.655824
317.576149	2373.818179	5.867597	-0.060299	2.660178
317.787625	2381.838022	5.872602	-0.060344	2.664515
318.538109	2389.826482	5.877606	-0.060489	2.668864
318.634746	2397.909601	5.882611	-0.060512	2.673214
319.045899	2405.953546	5.887616	-0.060594	2.677556
319.519634	2413.969328	5.892621	-0.060687	2.681880
319.622509	2422.028891	5.897626	-0.060712	2.686196
320.103242	2430.073686	5.902630	-0.060807	2.690522
320.385892	2438.132903	5.907635	-0.060865	2.694836
320.494643	2446.212778	5.912640	-0.060890	2.699142
320.726083	2454.239618	5.917645	-0.060938	2.703421
321.014442	2462.284225	5.922650	-0.060997	2.707707
321.538705	2470.325103	5.927654	-0.061100	2.711999
321.574795	2478.378720	5.932659	-0.061112	2.716259
321.920064	2486.436253	5.937664	-0.061182	2.720535
321.973107	2494.496692	5.942669	-0.061197	2.724787
321.974639	2502.573558	5.947674	-0.061203	2.729037
322.354479	2510.611823	5.952678	-0.061279	2.733285
322.885704	2518.586969	5.957683	-0.061383	2.737502
323.229844	2526.645350	5.962688	-0.061452	2.741745
323.221253	2534.732721	5.967693	-0.061456	2.745974
323.617832	2542.779025	5.972698	-0.061535	2.750200
324.158962	2550.843564	5.977702	-0.061641	2.754438
324.159681	2558.890627	5.982707	-0.061646	2.758627
324.483802	2566.905073	5.987712	-0.061712	2.762813
324.755352	2574.939277	5.992717	-0.061768	2.766999
325.070984	2582.998704	5.997722	-0.061832	2.771195
325.375465	2591.033199	6.002726	-0.061894	2.775370
325.615822	2599.057271	6.007731	-0.061944	2.779530
325.340856	2607.201793	6.012736	-0.061898	2.783715
325.979285	2615.154426	6.017741	-0.062022	2.787850
326.496114	2623.178402	6.022746	-0.062124	2.792008
326.986783	2631.221343	6.027750	-0.062220	2.796168
326.955832	2639.267244	6.032755	-0.062220	2.800292
327.134952	2647.332295	6.037760	-0.062258	2.804432
327.646607	2655.359764	6.042765	-0.062359	2.808566
327.574401	2663.456016	6.047770	-0.062351	2.812695
328.002664	2671.499480	6.052774	-0.062436	2.816820
328.093913	2679.549721	6.057779	-0.062458	2.820923
328.150832	2687.625535	6.062784	-0.062474	2.825031
328.293648	2695.636155	6.067789	-0.062506	2.829105
328.649556	2703.648096	6.072794	-0.062577	2.833186
328.968886	2711.676610	6.077798	-0.062642	2.837268
329.110068	2719.727383	6.082803	-0.062674	2.841344
329.655499	2727.715718	6.087808	-0.062780	2.845406
329.880692	2735.775896	6.092813	-0.062828	2.849481
330.197523	2743.844752	6.097818	-0.062892	2.853558
330.106709	2751.950564	6.102822	-0.062880	2.857626
330.152828	2759.983211	6.107827	-0.062894	2.861659
330.504095	2768.011336	6.112832	-0.062965	2.865701
330.465506	2776.098865	6.117837	-0.062963	2.869745
331.049603	2784.050520	6.122842	-0.063077	2.873750
331.289876	2792.091201	6.127846	-0.063127	2.877775
331.005580	2800.191677	6.132851	-0.063079	2.881795
331.418595	2808.197939	6.137856	-0.063161	2.885801
332.129590	2816.181500	6.142861	-0.063299	2.889807
331.933451	2824.289469	6.147866	-0.063268	2.893818
332.081015	2832.343045	6.152870	-0.063301	2.897816
332.472772	2840.330058	6.157875	-0.063379	2.901789
333.236769	2848.320281	6.162880	-0.063526	2.905779
333.124194	2856.430798	6.167885	-0.063511	2.909774
333.250640	2864.544895	6.172890	-0.063540	2.913778
333.556252	2872.548144	6.177894	-0.063602	2.917733
333.835902	2880.543676	6.182899	-0.063659	2.921677
333.897565	2888.618812	6.187904	-0.063676	2.925642
334.310909	2896.605608	6.192909	-0.063758	2.929578
334.369478	2904.696682	6.197914	-0.063774	2.933540
334.996170	2912.671759	6.202918	-0.063896	2.937471
334.913882	2920.759291	6.207923	-0.063886	2.941414
335.560064	2928.734952	6.212928	-0.064012	2.945335
335.684740	2936.778578	6.217933	-0.064040	2.949257
335.963045	2944.821370	6.222938	-0.064097	2.953181
336.136654	2952.888990	6.227942	-0.064135	2.957106
336.165770	2960.951555	6.232947	-0.064146	2.961016
336.748643	2968.893745	6.237952	-0.064259	2.964892
336.741428	2976.999711	6.242957	-0.064263	2.968811
336.666501	2985.087477	6.247962	-0.064255	2.972712
337.058593	2993.113421	6.252966	-0.064333	2.976603
336.970137	3001.166805	6.257971	-0.064322	2.980476
337.281548	3009.159710	6.262976	-0.064385	2.984337
337.455469	3017.227970	6.267981	-0.064423	2.988221
337.653524	3025.257355	6.272986	-0.064465	2.992083
338.163195	3033.282819	6.277990	-0.064565	2.995954
338.379514	3041.281035	6.282995	-0.064610	2.999792
338.361638	3049.334178	6.288000	-0.064612	3.003639
338.757266	3057.345164	6.293005	-0.064691	3.007482
339.035026	3065.416485	6.298010	-0.064748	3.011343
339.148114	3073.500013	6.303014	-0.064775	3.015197
339.294885	3081.480646	6.308019	-0.064807	3.018998
339.754608	3089.480499	6.313024	-0.064898	3.022819
339.954118	3097.543173	6.318029	-0.064940	3.026653
339.926458	3105.636771	6.323034	-0.064941	3.030484
340.475106	3113.596894	6.328038	-0.065048	3.034277
340.419788	3121.651045	6.333043	-0.065043	3.038079
340.708317	3129.684605	6.338048	-0.065102	3.041883
340.891544	3137.728763	6.343053	-0.065141	3.045682
341.479548	3145.717002	6.348058	-0.065256	3.049471
341.568696	3153.821197	6.353062	-0.065278	3.053284
341.673351	3161.851451	6.358067	-0.065303	3.057059
341.874985	3169.913628	6.363072	-0.065346	3.060849
342.288507	3177.894619	6.368077	-0.065428	3.064606
342.305258	3185.964648	6.373082	-0.065436	3.068381
342.841265	3194.003181	6.378086	-0.065541	3.072162
342.814565	3202.099711	6.383091	-0.065542	3.075938
343.173344	3210.084836	6.388096	-0.065614	3.079676
343.033763	3218.141638	6.393101	-0.065593	3.083419
343.177860	3226.145563	6.398106	-0.065625	3.087146
343.581011	3234.192695	6.403110	-0.065705	3.090902
343.709273	3242.192265	6.408115	-0.065735	3.094617
344.135804	3250.191439	6.413120	-0.065819	3.098342
344.366299	3258.226431	6.418125	-0.065867	3.102070
344.574874	3266.259233	6.423130	-0.065911	3.105791
344.701025	3274.337868	6.428134	-0.065940	3.109525
344.763750	3282.394050	6.433139	-0.065957	3.113241
345.129033	3290.407047	6.438144	-0.066031	3.116947
345.618180	3298.375888	6.443149	-0.066127	3.120633
345.820540	3306.395409	6.448154	-0.066170	3.124326
346.194746	3314.448871	6.453158	-0.066245	3.128037
346.091785	3322.537256	6.458163	-0.066231	3.131738
346.500203	3330.569169	6.463168	-0.066312	3.135433
346.320124	3338.639934	6.468173	-0.066284	3.139113
346.107800	3346.716447	6.473178	-0.066250	3.142791
346.914670	3354.643088	6.478182	-0.066405	3.146442
347.530695	3362.619488	6.483187	-0.066525	3.150103
347.433526	3370.759656	6.488192	-0.066512	3.153802
347.134983	3378.843933	6.493197	-0.066462	3.157462
347.696449	3386.786821	6.498202	-0.066572	3.161093
348.397044	3394.762685	6.503206	-0.066707	3.164740
348.274254	3402.842540	6.508211	-0.066690	3.168393
348.380288	3410.927949	6.513216	-0.066715	3.172055
349.006769	3418.895942	6.518221	-0.066837	3.175682
349.081961	3426.938105	6.523226	-0.066856	3.179315
349.279855	3434.968582	6.528230	-0.066898	3.182943
349.165487	3443.044847	6.533235	-0.066882	3.186574
349.600483	3451.050725	6.538240	-0.066968	3.190194
349.377357	3459.174669	6.543245	-0.066932	3.193833
349.855799	3467.132955	6.548250	-0.067027	3.197425
350.030041	3475.191721	6.553254	-0.067064	3.201044
350.085505	3483.159459	6.558259	-0.067080	3.204614
350.192159	3491.239486	6.563264	-0.067105	3.208231
350.511121	3499.268539	6.568269	-0.067170	3.211831
350.828886	3507.287276	6.573274	-0.067234	3.215423
351.140535	3515.302408	6.578278	-0.067297	3.219008
351.446606	3523.316642	6.583283	-0.067360	3.222589
351.779989	3531.349302	6.588288	-0.067427	3.226175
351.521847	3539.462507	6.593293	-0.067384	3.229767
351.823239	3547.466320	6.598298	-0.067446	3.233331
352.560977	3555.391489	6.603302	-0.067588	3.236874
353.018424	3563.375352	6.608307	-0.067678	3.240428
353.068786	3571.438194	6.613312	-0.067693	3.243995
353.528155	3579.486500	6.618317	-0.067784	3.247569
353.276584	3587.601129	6.623322	-0.067742	3.251139
353.136605	3595.689351	6.628326	-0.067722	3.254698
353.280657	3603.653510	6.633331	-0.067754	3.258211
353.567559	3611.680552	6.638336	-0.067812	3.261753
353.484510	3619.738658	6.643341	-0.067802	3.265289
353.656435	3627.763384	6.648346	-0.067839	3.268818
353.806729	3635.815257	6.653350	-0.067873	3.272353
354.405177	3643.761180	6.658355	-0.067989	3.275857
354.149759	3651.852205	6.663360	-0.067947	3.279386
354.817836	3659.792094	6.668365	-0.068077	3.282882
355.060130	3667.816948	6.673370	-0.068127	3.286394
355.658489	3675.818006	6.678374	-0.068244	3.289906
355.815156	3683.898274	6.683379	-0.068278	3.293432
356.128666	3691.912715	6.688384	-0.068342	3.296931
356.152776	3700.005925	6.693389	-0.068352	3.300449
356.601162	3707.936276	6.698394	-0.068440	3.303909
356.847624	3716.057628	6.703398	-0.068492	3.307441
356.817287	3724.115389	6.708403	-0.068491	3.310930
356.546314	3732.174408	6.713408	-0.068446	3.314407
357.354690	3740.112403	6.718413	-0.068602	3.317870
357.376084	3748.158482	6.723418	-0.068611	3.321346
357.565317	3756.185703	6.728422	-0.068652	3.324816
357.779985	3764.214067	6.733427	-0.068697	3.328284
358.135259	3772.272514	6.738432	-0.068768	3.331766
358.346937	3780.316723	6.743437	-0.068813	3.335234
358.398846	3788.326843	6.748442	-0.068828	3.338677
358.802877	3796.354913	6.753446	-0.068908	3.342137
358.740349	3804.388191	6.758451	-0.068902	3.345578
359.215319	3812.372952	6.763456	-0.068996	3.349016
359.253423	3820.442465	6.768461	-0.069008	3.352469
359.700492	3828.434806	6.773466	-0.069096	3.355902
359.808013	3836.484246	6.778470	-0.069122	3.359342
359.835315	3844.518960	6.783475	-0.069132	3.362770
360.487072	3852.481176	6.788480	-0.069259	3.366186
360.635093	3860.538824	6.793485	-0.069292	3.369621
360.570549	3868.609221	6.798490	-0.069285	3.373050
360.785075	3876.685756	6.803494	-0.069330	3.376488
360.480154	3884.735909	6.808499	-0.069279	3.379893
360.660935	3892.715417	6.813504	-0.069317	3.383282
361.102040	3900.719772	6.818509	-0.069405	3.386687
360.952282	3908.810315	6.823514	-0.069382	3.390104
360.933102	3916.921455	6.828518	-0.069384	3.393531
361.667053	3924.798284	6.833523	-0.069526	3.396883
362.077832	3932.807011	6.838528	-0.069608	3.400275
362.200918	3940.788297	6.843533	-0.069636	3.403642
362.308239	3948.850129	6.848538	-0.069661	3.407039
362.332596	3956.962729	6.853542	-0.069671	3.410451
362.824808	3964.886407	6.858547	-0.069768	3.413797
362.509244	3973.005842	6.863552	-0.069714	3.417193
362.535527	3981.069522	6.868557	-0.069724	3.420575
362.638572	3989.035586	6.873562	-0.069749	3.423915
363.063073	3997.061034	6.878566	-0.069833	3.427287
363.323346	4005.091086	6.883571	-0.069887	3.430653
363.483225	4013.114306	6.888576	-0.069922	3.434009
363.277506	4021.197478	6.893581	-0.069889	3.437374
363.175698	4029.203440	6.898586	-0.069875	3.440707
363.406930	4037.155135	6.903590	-0.069923	3.444025
363.842809	4045.178121	6.908595	-0.070010	3.447377
364.177131	4053.212206	6.913600	-0.070077	3.450727
364.430976	4061.245055	6.918605	-0.070130	3.454071
364.336465	4069.329346	6.923610	-0.070118	3.457420
364.803985	4077.324353	6.928614	-0.070210	3.460749
365.134989	4085.273491	6.933619	-0.070277	3.464050
365.733049	4093.322761	6.938624	-0.070393	3.467399
365.632425	4101.424557	6.943629	-0.070380	3.470743
365.604947	4109.406375	6.948634	-0.070380	3.474036
365.913720	4117.449729	6.953638	-0.070443	3.477363
366.332022	4125.449674	6.958643	-0.070526	3.480672
366.624297	4133.423517	6.963648	-0.070586	3.483963
366.656902	4141.514693	6.968653	-0.070597	3.487291
366.665758	4149.579775	6.973658	-0.070604	3.490604
367.077770	4157.573257	6.978662	-0.070686	3.493898
367.039636	4165.635356	6.983667	-0.070684	3.497202
367.736069	4173.610296	6.988672	-0.070819	3.500491
368.106272	4181.624944	6.993677	-0.070893	3.503782
368.081424	4189.671559	6.998682	-0.070894	3.507071
368.197256	4197.756728	7.003686	-0.070921	3.510377
368.747795	4205.715217	7.008691	-0.071028	3.513642
369.023326	4213.727398	7.013696	-0.071085	3.516917
369.219661	4221.784037	7.018701	-0.071127	3.520204
369.313148	4229.786453	7.023706	-0.071149	3.523464
369.230469	4237.866093	7.028710	-0.071139	3.526745
369.438305	4245.877668	7.033715	-0.071183	3.530006
369.496999	4253.910581	7.038720	-0.071200	3.533267
369.443710	4262.021217	7.043725	-0.071195	3.536553
369.790055	4269.921265	7.048730	-0.071265	3.539763
370.032161	4277.947024	7.053734	-0.071315	3.543018
370.544119	4285.948062	7.058739	-0.071416	3.546269
370.742177	4294.013875	7.063744	-0.071458	3.549533
370.953720	4302.089281	7.068749	-0.071502	3.552798
371.080810	4310.116645	7.073754	-0.071531	3.556038
371.484685	4318.054452	7.078758	-0.071612	3.559247
371.389734	4326.137395	7.083763	-0.071599	3.562497
371.558228	4334.154243	7.088768	-0.071636	3.565725
371.715778	4342.169153	7.093773	-0.071671	3.568949
371.487617	4350.279428	7.098778	-0.071633	3.572197
372.173189	4358.183836	7.103782	-0.071766	3.575386
372.210386	4366.190710	7.108787	-0.071778	3.578595
372.626126	4374.241441	7.113792	-0.071861	3.581829
372.825889	4382.246913	7.118797	-0.071904	3.585036
373.374493	4390.226830	7.123802	-0.072011	3.588240
373.268351	4398.378223	7.128806	-0.071996	3.591491
373.790912	4406.313717	7.133811	-0.072099	3.594670
373.356361	4414.423877	7.138816	-0.072023	3.597889
373.431215	4422.480313	7.143821	-0.072043	3.601098
373.601375	4430.380739	7.148826	-0.072079	3.604245
374.127474	4438.428117	7.153830	-0.072183	3.607458
374.426442	4446.458483	7.158835	-0.072244	3.610654
374.233679	4454.574998	7.163840	-0.072213	3.613868
374.347489	4462.586685	7.168845	-0.072240	3.617046
374.330696	4470.599888	7.173850	-0.072242	3.620219
374.801551	4478.585121	7.178854	-0.072335	3.623391
374.832354	4486.607487	7.183859	-0.072346	3.626563
375.423577	4494.588986	7.188864	-0.072461	3.629731
375.828392	4502.625044	7.193869	-0.072542	3.632913
376.291823	4510.657839	7.198874	-0.072633	3.636093
376.457911	4518.673727	7.203878	-0.072669	3.639254
376.534447	4526.691084	7.208883	-0.072689	3.642411
376.809787	4534.720509	7.213888	-0.072745	3.645576
376.997249	4542.744923	7.218893	-0.072785	3.648733
377.315131	4550.737804	7.223898	-0.072850	3.651879
377.589231	4558.799725	7.228902	-0.072906	3.655047
377.527914	4566.838712	7.233907	-0.072900	3.658195
377.856536	4574.847160	7.238912	-0.072967	3.661339
378.169864	4582.816588	7.243917	-0.073030	3.664465
378.280438	4590.899680	7.248922	-0.073056	3.667626
378.302635	4598.985488	7.253926	-0.073065	3.670784
378.602953	4606.959103	7.258931	-0.073127	3.673903
378.872088	4614.987445	7.263936	-0.073182	3.677039
378.960338	4623.003836	7.268941	-0.073204	3.680163
378.922204	4631.014015	7.273946	-0.073202	3.683279
379.348174	4639.046067	7.278950	-0.073286	3.686413
379.307838	4647.078914	7.283955	-0.073284	3.689532
379.384363	4655.121930	7.288960	-0.073304	3.692655
379.778580	4663.177004	7.293965	-0.073382	3.695789
379.663044	4671.183007	7.298970	-0.073366	3.698888
379.833675	4679.203164	7.303974	-0.073403	3.701997
380.179072	4687.164389	7.308979	-0.073473	3.705086
380.047209	4695.276489	7.313984	-0.073453	3.708217
380.258751	4703.359685	7.318989	-0.073498	3.711344
380.171735	4711.361058	7.323994	-0.073487	3.714429
380.525612	4719.324597	7.328998	-0.073558	3.717508
380.757089	4727.311055	7.334003	-0.073607	3.720590
380.833830	4735.337108	7.339008	-0.073626	3.723681
380.834037	4743.433351	7.344013	-0.073631	3.726794
381.141076	4751.380630	7.349018	-0.073694	3.729855
381.783012	4759.364088	7.354022	-0.073819	3.732936
382.088652	4767.419364	7.359027	-0.073881	3.736033
382.200446	4775.423078	7.364032	-0.073907	3.739103
382.526441	4783.433509	7.369037	-0.073973	3.742179
382.537197	4791.472538	7.374042	-0.073980	3.745255
382.678085	4799.517218	7.379046	-0.074012	3.748334
383.107369	4807.560822	7.384051	-0.074097	3.751417
383.071470	4815.583529	7.389056	-0.074095	3.754478
383.614130	4823.532701	7.394061	-0.074202	3.757523
383.849597	4831.591583	7.399066	-0.074251	3.760599
384.222153	4839.585374	7.404070	-0.074325	3.763651
384.178702	4847.647249	7.409075	-0.074323	3.766717
384.421754	4855.664881	7.414080	-0.074373	3.769770
384.946432	4863.639482	7.419085	-0.074476	3.772812
384.957052	4871.716927	7.424090	-0.074483	3.775877
385.146962	4879.730526	7.429094	-0.074524	3.778920
385.387026	4887.733559	7.434099	-0.074574	3.781958
385.357948	4895.783650	7.439104	-0.074574	3.785005
385.591834	4903.800124	7.444109	-0.074622	3.788042
385.785776	4911.866908	7.449114	-0.074664	3.791096
386.117639	4919.847512	7.454118	-0.074731	3.794117
386.250377	4927.893095	7.459123	-0.074761	3.797156
386.320275	4935.905925	7.464128	-0.074779	3.800179
386.226716	4943.905207	7.469133	-0.074767	3.803190
386.283328	4951.956508	7.474138	-0.074783	3.806222
387.133754	4959.909293	7.479142	-0.074946	3.809233
387.039214	4967.994289	7.484147	-0.074934	3.812269
387.269378	4976.033889	7.489152	-0.074982	3.815294
387.241439	4984.080342	7.494157	-0.074982	3.818312
387.327810	4992.094728	7.499162	-0.075004	3.821319
387.837344	5000.039618	7.504166	-0.075104	3.824307
387.509340	5008.135380	7.509171	-0.075048	3.827330
388.168146	5016.104344	7.514176	-0.075176	3.830325
388.041683	5024.170898	7.519181	-0.075158	3.833338
388.146798	5032.181743	7.524186	-0.075182	3.836332
388.240845	5040.218792	7.529190	-0.075205	3.839333
388.839804	5048.175981	7.534195	-0.075322	3.842313
389.291603	5056.148946	7.539200	-0.075411	3.845293
389.681718	5064.223293	7.544205	-0.075489	3.848307
390.223053	5072.221596	7.549210	-0.075595	3.851294
390.478302	5080.309915	7.554214	-0.075648	3.854306
390.461582	5088.347000	7.559219	-0.075650	3.857291
390.824691	5096.337623	7.564224	-0.075723	3.860264
390.939708	5104.356178	7.569229	-0.075750	3.863240
391.158003	5112.388640	7.574234	-0.075796	3.866220
391.710701	5120.389226	7.579238	-0.075904	3.869194
392.157466	5128.483187	7.584243	-0.075992	3.872198
392.380074	5136.518403	7.589248	-0.076039	3.875173
392.581237	5144.475692	7.594253	-0.076082	3.878116
392.725064	5152.504063	7.599258	-0.076114	3.881082
392.885287	5160.458988	7.604262	-0.076149	3.884020
392.818435	5168.507917	7.609267	-0.076142	3.886985
392.897255	5176.546510	7.614272	-0.076162	3.889946
393.434316	5184.508543	7.619277	-0.076267	3.892887
393.354002	5192.586010	7.624282	-0.076257	3.895855
393.493414	5200.565896	7.629286	-0.076288	3.898790
394.047532	5208.557542	7.634291	-0.076397	3.901735
393.678154	5216.677523	7.639296	-0.076333	3.904707
394.096491	5224.659923	7.644301	-0.076416	3.907641
394.566593	5232.613344	7.649306	-0.076509	3.910563
394.780546	5240.681271	7.654310	-0.076554	3.913521
394.989569	5248.728335	7.659315	-0.076599	3.916468
394.967595	5256.724539	7.664320	-0.076600	3.919390
395.404200	5264.727374	7.669325	-0.076686	3.922321
395.670996	5272.712771	7.674330	-0.076741	3.925240
395.743153	5280.806048	7.679334	-0.076760	3.928192
395.555906	5288.903524	7.684339	-0.076730	3.931139
396.112594	5296.826894	7.689344	-0.076839	3.934034
396.194216	5304.895916	7.694349	-0.076860	3.936972
396.312648	5312.866881	7.699354	-0.076887	3.939872
396.946759	5320.870644	7.704358	-0.077010	3.942791
396.965512	5328.930111	7.709363	-0.077019	3.945717
397.022501	5336.985881	7.714368	-0.077035	3.948640
397.579605	5345.052468	7.719373	-0.077144	3.951574
397.776241	5352.985691	7.724378	-0.077186	3.954451
398.029197	5360.995299	7.729382	-0.077238	3.957354
397.747148	5369.060155	7.734387	-0.077191	3.960266
397.882567	5377.043461	7.739392	-0.077221	3.963154
398.104819	5385.113092	7.744397	-0.077268	3.966072
398.248473	5393.108708	7.749402	-0.077300	3.968960
398.527136	5401.161589	7.754406	-0.077357	3.971868
398.904979	5409.134153	7.759411	-0.077433	3.974748
398.905865	5417.111157	7.764416	-0.077438	3.977620
399.249517	5425.189207	7.769421	-0.077507	3.980533
399.284955	5433.159724	7.774426	-0.077519	3.983399
399.389731	5441.230013	7.779430	-0.077544	3.986300
399.465151	5449.237182	7.784435	-0.077563	3.989176
399.815460	5457.254401	7.789440	-0.077634	3.992058
399.953731	5465.291179	7.794445	-0.077665	3.994942
399.724172	5473.321681	7.799450	-0.077627	3.997815
400.059863	5481.353782	7.804454	-0.077695	4.000696
400.279426	5489.278561	7.809459	-0.077741	4.003534
400.373994	5497.316284	7.814464	-0.077764	4.006409
400.769477	5505.309031	7.819469	-0.077843	4.009271
400.663374	5513.419398	7.824474	-0.077829	4.012164
400.810108	5521.425787	7.829478	-0.077861	4.015022
400.793661	5529.459508	7.834483	-0.077863	4.017885
401.398663	5537.426533	7.839488	-0.077981	4.020733
401.628564	5545.466666	7.844493	-0.078029	4.023598
401.525242	5553.523440	7.849498	-0.078015	4.026462
401.865918	5561.508634	7.854502	-0.078084	4.029305
402.394689	5569.541240	7.859507	-0.078188	4.032167
402.812075	5577.555758	7.864512	-0.078271	4.035018
403.091578	5585.540917	7.869517	-0.078328	4.037854
403.290354	5593.596226	7.874522	-0.078370	4.040712
403.652832	5601.542466	7.879526	-0.078443	4.043532
403.663396	5609.621174	7.884531	-0.078450	4.046391
403.920863	5617.607305	7.889536	-0.078503	4.049219
404.054536	5625.684984	7.894541	-0.078534	4.052076
404.287487	5633.669465	7.899546	-0.078582	4.054899
404.242555	5641.750456	7.904550	-0.078579	4.057750
404.091595	5649.824878	7.909555	-0.078556	4.060595
404.405877	5657.738642	7.914560	-0.078620	4.063389
404.855030	5665.794108	7.919565	-0.078709	4.066232
405.036259	5673.750579	7.924570	-0.078748	4.069035
405.268982	5681.852530	7.929574	-0.078797	4.071887
405.392689	5689.836011	7.934579	-0.078825	4.074695
405.515869	5697.895337	7.939584	-0.078853	4.077527
405.980506	5705.897963	7.944589	-0.078945	4.080342
405.894138	5713.849138	7.949594	-0.078934	4.083129
406.346385	5721.881397	7.954598	-0.079023	4.085950
406.319534	5729.931167	7.959603	-0.079024	4.088769
406.131281	5738.031498	7.964608	-0.078994	4.091601
406.444434	5745.990933	7.969613	-0.079057	4.094389
407.123015	5753.961606	7.974618	-0.079189	4.097184
407.067142	5761.994604	7.979622	-0.079184	4.099988
407.436939	5769.975648	7.984627	-0.079258	4.102779
407.593937	5777.998590	7.989632	-0.079292	4.105579
408.076973	5786.051699	7.994637	-0.079388	4.108392
407.793447	5794.164318	7.999642	-0.079340	4.111213
408.335909	5802.080129	8.004646	-0.079446	4.113976
408.456109	5810.137542	8.009651	-0.079474	4.116780
408.454530	5818.122602	8.014656	-0.079479	4.119555
408.473747	5826.161700	8.019661	-0.079488	4.122347
408.658220	5834.126972	8.024666	-0.079527	4.125114
408.982640	5842.138200	8.029670	-0.079593	4.127897
409.309258	5850.172913	8.034675	-0.079659	4.130686
409.955753	5858.171234	8.039680	-0.079785	4.133465
411.217508	5866.269148	8.044685	-0.080025	4.136285
411.708977	5874.188234	8.049690	-0.080122	4.139030
412.452932	5882.223470	8.054694	-0.080266	4.141817
412.610502	5890.262851	8.059699	-0.080300	4.144596
412.762532	5898.327812	8.064704	-0.080334	4.147382
412.715294	5906.416503	8.069709	-0.080330	4.150171
412.675985	5914.365372	8.074714	-0.080328	4.152911
413.451906	5922.362168	8.079718	-0.080478	4.155675
412.902531	5930.426479	8.084723	-0.080381	4.158445
413.152897	5938.465168	8.089728	-0.080433	4.161213
413.498785	5946.405954	8.094733	-0.080502	4.163947
413.407295	5954.450500	8.099738	-0.080491	4.166710
413.682075	5962.460016	8.104742	-0.080547	4.169463
413.461745	5970.533452	8.109747	-0.080511	4.172231
413.871241	5978.497064	8.114752	-0.080593	4.174966
414.078998	5986.531477	8.119757	-0.080637	4.177722
414.488917	5994.501312	8.124762	-0.080718	4.180456
414.750481	6002.514536	8.129766	-0.080772	4.183201
414.899606	6010.586331	8.134771	-0.080805	4.185963
414.899358	6018.610157	8.139776	-0.080810	4.188705
414.962978	6026.710229	8.144781	-0.080828	4.191472
415.307527	6034.681723	8.149786	-0.080897	4.194196
415.365479	6042.679189	8.154790	-0.080913	4.196925
415.548422	6050.692366	8.159795	-0.080952	4.199658
415.356991	6058.735227	8.164800	-0.080922	4.202395
415.618085	6066.710486	8.169805	-0.080976	4.205113
416.210414	6074.623200	8.174810	-0.081091	4.207812
416.101664	6082.808537	8.179814	-0.081076	4.210593
416.210383	6090.792697	8.184819	-0.081102	4.213307
416.953548	6098.746839	8.189824	-0.081246	4.216015
417.473808	6106.741181	8.194829	-0.081348	4.218733
417.026307	6114.868504	8.199834	-0.081270	4.221484
416.905937	6122.810849	8.204838	-0.081252	4.224174
417.247202	6130.867240	8.209843	-0.081321	4.226906
417.522447	6138.848925	8.214848	-0.081378	4.229610
417.560986	6146.943866	8.219853	-0.081390	4.232348
417.718226	6154.920271	8.224858	-0.081425	4.235045
417.996662	6162.925847	8.229862	-0.081482	4.237752
418.125615	6170.930127	8.234867	-0.081511	4.240455
418.562840	6178.882996	8.239872	-0.081598	4.243142
418.684413	6186.989581	8.244877	-0.081626	4.245876
418.064269	6195.048588	8.249882	-0.081515	4.248585
418.701321	6203.012907	8.254886	-0.081639	4.251272
419.158154	6211.007358	8.259891	-0.081730	4.253967
419.335496	6219.048721	8.264896	-0.081768	4.256672
419.257435	6227.073924	8.269901	-0.081759	4.259368
419.032494	6235.154946	8.274906	-0.081722	4.262079
419.456016	6243.078112	8.279910	-0.081806	4.264743
419.734455	6251.135338	8.284915	-0.081863	4.267447
420.061548	6259.108829	8.289920	-0.081929	4.270123
420.144574	6267.203435	8.294925	-0.081950	4.272835
420.340711	6275.129323	8.299930	-0.081992	4.275490
420.847810	6283.088915	8.304934	-0.082091	4.278157
420.828195	6291.219571	8.309939	-0.082093	4.280875
420.758095	6299.163290	8.314944	-0.082085	4.283529
420.835283	6307.279063	8.319949	-0.082105	4.286239
421.040541	6315.218727	8.324954	-0.082148	4.288891
421.285768	6323.296239	8.329958	-0.082199	4.291586
421.583952	6331.288504	8.334963	-0.082260	4.294253
421.678194	6339.292198	8.339968	-0.082283	4.296919
421.927631	6347.334363	8.344973	-0.082335	4.299598
422.074845	6355.315783	8.349978	-0.082367	4.302254
422.284626	6363.295885	8.354982	-0.082412	4.304909
422.205852	6371.397458	8.359987	-0.082402	4.307600
422.624979	6379.423662	8.364992	-0.082486	4.310268
422.843432	6387.388560	8.369997	-0.082531	4.312913
422.407731	6395.460558	8.375002	-0.082456	4.315586
422.831788	6403.425520	8.380006	-0.082540	4.318229
423.006600	6411.471476	8.385011	-0.082578	4.320895
423.157873	6419.371148	8.390016	-0.082611	4.323511
423.479187	6427.483964	8.395021	-0.082676	4.326197
423.864451	6435.417145	8.400026	-0.082753	4.328823
424.062047	6443.510095	8.405030	-0.082795	4.331498
424.291602	6451.469281	8.410035	-0.082843	4.334128
424.590674	6459.544394	8.415040	-0.082904	4.336795
424.084728	6467.603613	8.420045	-0.082815	4.339448
424.239702	6475.621005	8.425050	-0.082849	4.342092
424.997369	6483.511000	8.430054	-0.082996	4.344696
424.746341	6491.650053	8.435059	-0.082954	4.347373
425.291414	6499.598544	8.440064	-0.083061	4.349992
425.468090	6507.710380	8.445069	-0.083099	4.352660
425.624734	6515.722207	8.450074	-0.083133	4.355293
425.326979	6523.746082	8.455078	-0.083083	4.357926
425.653912	6531.735401	8.460083	-0.083149	4.360550
425.968689	6539.649943	8.465088	-0.083213	4.363148
426.146691	6547.727573	8.470093	-0.083252	4.365796
426.682194	6555.692970	8.475098	-0.083357	4.368409
426.774168	6563.738495	8.480102	-0.083379	4.371044
426.965885	6571.782072	8.485107	-0.083420	4.373676
426.689356	6579.856464	8.490112	-0.083374	4.376314
427.359421	6587.790152	8.495117	-0.083504	4.378911
427.067021	6595.863035	8.500122	-0.083455	4.381546
426.927561	6603.825651	8.505126	-0.083434	4.384144
427.689407	6611.876565	8.510131	-0.083581	4.386774
427.967920	6619.830023	8.515136	-0.083638	4.389369
428.286991	6627.902551	8.520141	-0.083703	4.392001
428.209573	6635.931091	8.525146	-0.083694	4.394614
428.111745	6644.005085	8.530150	-0.083681	4.397241
428.514860	6651.980323	8.535155	-0.083761	4.399837
428.558892	6659.980588	8.540160	-0.083774	4.402437
428.843040	6668.015791	8.545165	-0.083833	4.405048
429.111545	6676.029233	8.550170	-0.083888	4.407651
429.205388	6684.079561	8.555174	-0.083911	4.410263
429.461938	6692.140469	8.560179	-0.083964	4.412878
429.761920	6700.142855	8.565184	-0.084025	4.415473
430.184694	6708.182649	8.570189	-0.084109	4.418079
430.123372	6716.193272	8.575194	-0.084103	4.420671
430.404671	6724.159280	8.580199	-0.084160	4.423249
430.670563	6732.260737	8.585203	-0.084215	4.425870
430.573519	6740.207869	8.590208	-0.084202	4.428437
431.204845	6748.258796	8.595213	-0.084325	4.431039
430.729681	6756.318236	8.600218	-0.084242	4.433638
430.612507	6764.388076	8.605223	-0.084225	4.436239
431.639215	6772.200244	8.610227	-0.084422	4.438763
431.610154	6780.275269	8.615232	-0.084421	4.441364
431.757346	6788.263041	8.620237	-0.084454	4.443936
431.397830	6796.379750	8.625242	-0.084392	4.446545
432.058027	6804.310845	8.630247	-0.084521	4.449099
432.375349	6812.388909	8.635251	-0.084585	4.451696
432.482560	6820.347544	8.640256	-0.084610	4.454253
432.791177	6828.457702	8.645261	-0.084673	4.456858
433.097552	6836.340104	8.650266	-0.084735	4.459388
432.959499	6844.476913	8.655271	-0.084715	4.461996
432.773841	6852.502145	8.660275	-0.084685	4.464567
432.940668	6860.493930	8.665280	-0.084722	4.467127
433.295808	6868.530751	8.670285	-0.084793	4.469700
433.132693	6876.522658	8.675290	-0.084768	4.472256
433.676270	6884.449200	8.680295	-0.084874	4.474792
434.387085	6892.514156	8.685299	-0.085012	4.477372
434.207940	6900.520126	8.690304	-0.084984	4.479928
434.291285	6908.560570	8.695309	-0.085005	4.482494
434.601308	6916.523544	8.700314	-0.085068	4.485035
434.426046	6924.617587	8.705319	-0.085040	4.487614
434.738674	6932.644691	8.710323	-0.085104	4.490173
435.179152	6940.611242	8.715328	-0.085191	4.492711
435.309813	6948.666552	8.720333	-0.085221	4.495275
435.427767	6956.624543	8.725338	-0.085248	4.497806
435.854436	6964.659259	8.730343	-0.085333	4.500362
435.986697	6972.676406	8.735347	-0.085362	4.502909
436.276961	6980.670866	8.740352	-0.085422	4.505448
436.116483	6988.747584	8.745357	-0.085397	4.508010
436.210368	6996.785811	8.750362	-0.085420	4.510560
436.108150	7004.789257	8.755367	-0.085406	4.513096
436.525568	7012.757442	8.760371	-0.085489	4.515621
436.791177	7020.714989	8.765376	-0.085544	4.518141
437.324669	7028.738656	8.770381	-0.085648	4.520682
437.509351	7036.719005	8.775386	-0.085688	4.523206
437.346518	7044.809877	8.780391	-0.085663	4.525763
437.770758	7052.805027	8.785395	-0.085747	4.528289
437.804741	7060.846864	8.790400	-0.085759	4.530828
438.101576	7068.880062	8.795405	-0.085819	4.533363
438.097230	7076.899642	8.800410	-0.085824	4.535892
438.337633	7084.828529	8.805415	-0.085874	4.538392
438.143406	7092.966674	8.810419	-0.085843	4.540955
438.045207	7100.869516	8.815424	-0.085830	4.543442
438.546417	7108.954664	8.820429	-0.085928	4.545987
438.647085	7116.926400	8.825434	-0.085952	4.548494
438.723593	7125.004111	8.830439	-0.085972	4.551033
438.964157	7133.021573	8.835443	-0.086022	4.553552
439.044985	7141.002902	8.840448	-0.086042	4.556058
439.164681	7148.987407	8.845453	-0.086070	4.558563
439.270109	7157.051144	8.850458	-0.086095	4.561092
439.893054	7164.966656	8.855463	-0.086216	4.563574
439.696038	7173.093165	8.860467	-0.086185	4.566119
439.781301	7181.064844	8.865472	-0.086206	4.568615
440.141459	7189.135158	8.870477	-0.086278	4.571140
440.239277	7197.097698	8.875482	-0.086301	4.573630
440.530668	7205.129531	8.880487	-0.086361	4.576141
440.566974	7213.151221	8.885491	-0.086373	4.578647
441.104784	7221.138821	8.890496	-0.086478	4.581141
441.337160	7229.130451	8.895501	-0.086527	4.583635
441.057525	7237.224016	8.900506	-0.086480	4.586159
441.325591	7245.228352	8.905511	-0.086535	4.588654
441.764917	7253.254485	8.910515	-0.086622	4.591154
441.641876	7261.219215	8.915520	-0.086605	4.593634
441.424480	7269.360185	8.920525	-0.086569	4.596167
441.634161	7277.233906	8.925530	-0.086614	4.598616
441.811260	7285.284833	8.930535	-0.086652	4.601118
442.331088	7293.200391	8.935539	-0.086754	4.603578
442.418829	7301.287658	8.940544	-0.086776	4.606089
442.749731	7309.288121	8.945549	-0.086842	4.608572
442.687751	7317.322264	8.950554	-0.086836	4.611063
443.110996	7325.302127	8.955559	-0.086920	4.613537
443.331775	7333.373590	8.960563	-0.086967	4.616038
443.423182	7341.296489	8.965568	-0.086989	4.618491
443.213161	7349.441158	8.970573	-0.086955	4.621012
443.485141	7357.345066	8.975578	-0.087011	4.623457
443.517786	7365.469800	8.980583	-0.087022	4.625968
443.520917	7373.509053	8.985587	-0.087028	4.628452
443.882464	7381.436963	8.990592	-0.087101	4.630900
444.172465	7389.476533	8.995597	-0.087160	4.633382
443.652253	7397.532223	9.000602	-0.087068	4.635867
444.012496	7405.488293	9.005607	-0.087141	4.638319
444.683388	7413.492210	9.010611	-0.087271	4.640786
444.550275	7421.460174	9.015616	-0.087251	4.643240
444.870069	7429.535835	9.020621	-0.087316	4.645726
445.273167	7437.508379	9.025626	-0.087396	4.648178
445.451469	7445.605035	9.030631	-0.087435	4.650668
446.006570	7453.637266	9.035635	-0.087544	4.653136
445.899816	7461.604263	9.040640	-0.087529	4.655583
446.010252	7469.629568	9.045645	-0.087555	4.658046
445.907753	7477.668062	9.050650	-0.087541	4.660513
446.483943	7485.633363	9.055655	-0.087653	4.662955
446.685732	7493.696190	9.060659	-0.087696	4.665426
446.685399	7501.662077	9.065664	-0.087701	4.667866
447.097263	7509.734985	9.070669	-0.087783	4.670338
447.499396	7517.743941	9.075674	-0.087864	4.672788
447.531221	7525.773717	9.080679	-0.087875	4.675244
447.571519	7533.807758	9.085683	-0.087887	4.677700
447.519379	7541.799785	9.090688	-0.087883	4.680142
448.314322	7549.736157	9.095693	-0.088036	4.682564
448.095960	7557.763730	9.100698	-0.088001	4.685014
448.096159	7565.802318	9.105703	-0.088006	4.687466
448.394825	7573.851325	9.110707	-0.088067	4.689920
448.791752	7581.805636	9.115712	-0.088146	4.692343
448.805154	7589.874450	9.120717	-0.088154	4.694801
449.164794	7597.867911	9.125722	-0.088226	4.697233
449.098029	7605.831968	9.130727	-0.088219	4.699656
449.035050	7613.941860	9.135731	-0.088213	4.702122
449.349394	7621.837906	9.140736	-0.088276	4.704522
449.981047	7629.900073	9.145741	-0.088399	4.706970
449.962187	7637.949948	9.150746	-0.088401	4.709413
450.318625	7646.004995	9.155751	-0.088473	4.711857
450.615684	7653.974455	9.160755	-0.088533	4.714273
450.311239	7662.045619	9.165760	-0.088482	4.716720
450.366621	7670.006535	9.170765	-0.088497	4.719132
450.358411	7678.112447	9.175770	-0.088501	4.721587
450.979131	7685.944887	9.180775	-0.088622	4.723956
451.071933	7694.098082	9.185779	-0.088644	4.726422
451.440882	7702.051893	9.190784	-0.088718	4.728826
451.721630	7710.130202	9.195789	-0.088776	4.731267
451.611022	7718.105575	9.200794	-0.088760	4.733675
451.676160	7726.183507	9.205799	-0.088778	4.736114
451.708682	7734.238479	9.210803	-0.088789	4.738544
451.969080	7742.203057	9.215808	-0.088843	4.740945
452.165284	7750.184742	9.220813	-0.088885	4.743350
451.970829	7758.253434	9.225818	-0.088854	4.745781
451.901696	7766.295085	9.230823	-0.088846	4.748203
452.326440	7774.266156	9.235827	-0.088930	4.750600
452.870109	7782.241420	9.240832	-0.089037	4.752998
453.276801	7790.279960	9.245837	-0.089118	4.755413
453.247811	7798.289692	9.250842	-0.089118	4.757820
453.334300	7806.300389	9.255847	-0.089139	4.760226
453.686130	7814.294806	9.260851	-0.089210	4.762624
453.640634	7822.274981	9.265856	-0.089207	4.765018
453.800629	7830.392407	9.270861	-0.089242	4.767452
454.243150	7838.343929	9.275866	-0.089329	4.769834
454.670617	7846.390146	9.280871	-0.089414	4.772243
454.667781	7854.427758	9.285875	-0.089419	4.774649
455.061920	7862.384958	9.290880	-0.089498	4.777029
455.270724	7870.449727	9.295885	-0.089542	4.779441
455.177363	7878.467268	9.300890	-0.089530	4.781838
454.922470	7886.468177	9.305895	-0.089487	4.784229
455.418513	7894.547462	9.310899	-0.089585	4.786640
455.067626	7902.489350	9.315904	-0.089525	4.789012
455.402896	7910.559346	9.320909	-0.089593	4.791418
456.051904	7918.468700	9.325914	-0.089719	4.793775
456.011002	7926.558183	9.330919	-0.089716	4.796186
456.264125	7934.550548	9.335923	-0.089769	4.798566
456.246004	7942.583422	9.340928	-0.089771	4.800957
456.666536	7950.530426	9.345933	-0.089854	4.803321
456.612101	7958.639122	9.350938	-0.089849	4.805733
456.695312	7966.583528	9.355943	-0.089870	4.808094
457.006619	7974.688370	9.360947	-0.089933	4.810501
457.429568	7982.603342	9.365952	-0.090017	4.812850
457.532462	7990.163426	9.370957	-0.090041	4.815094
457.849285	7994.821323	9.375962	-0.090103	4.816475

458.156209	7997.501756	9.380967	-0.090162	4.817269
458.301938	7998.826785	9.385971	-0.090190	4.817661
457.926917	7999.217302	9.390976	-0.090121	4.817779
458.357195	8000.307509	9.395981	-0.090202	4.818100
458.258649	8000.330340	9.400986	-0.090183	4.818108
458.295718	8000.289809	9.405991	-0.090190	4.818095
458.440331	8000.406577	9.410995	-0.090217	4.818129
458.882443	8000.301198	9.416000	-0.090300	4.818096
458.784936	8000.356676	9.421005	-0.090282	4.818113
458.696101	8000.374381	9.426010	-0.090265	4.818119
458.998474	8000.253357	9.431015	-0.090321	4.818082
459.031428	8000.325402	9.436019	-0.090328	4.818103
459.050129	8000.278297	9.441024	-0.090331	4.818089
459.544992	8000.266291	9.446029	-0.090423	4.818083
459.577767	8000.269911	9.451034	-0.090429	4.818084
459.532139	8000.158744	9.456039	-0.090421	4.818051
459.570052	8000.281387	9.461043	-0.090428	4.818088
459.617282	8000.256788	9.466048	-0.090437	4.818080
459.603568	8000.249229	9.471053	-0.090434	4.818078
459.772861	8000.215816	9.476058	-0.090466	4.818067
459.815275	8000.190096	9.481063	-0.090474	4.818059
459.840849	8000.319936	9.486067	-0.090479	4.818098
459.621561	8000.288440	9.491072	-0.090438	4.818089
459.844528	8000.309466	9.496077	-0.090479	4.818095
459.760730	8000.325135	9.501082	-0.090464	4.818100
459.788415	8000.256050	9.506087	-0.090469	4.818079
460.010628	8000.327593	9.511091	-0.090510	4.818099
460.296898	8000.286347	9.516096	-0.090564	4.818086
460.096448	8000.291958	9.521101	-0.090526	4.818088
460.035088	8000.319522	9.526106	-0.090515	4.818097
460.296796	8000.274773	9.531111	-0.090564	4.818083
459.982563	8000.318790	9.536115	-0.090505	4.818097
460.223966	8000.296915	9.541120	-0.090550	4.818089
460.428395	8000.299786	9.546125	-0.090588	4.818089
460.131901	8000.320892	9.551130	-0.090533	4.818097
460.145413	8000.318979	9.556135	-0.090536	4.818096
460.371647	8000.289522	9.561139	-0.090578	4.818087
460.370771	8000.176875	9.566144	-0.090578	4.818053
460.457984	8000.256000	9.571149	-0.090594	4.818076
460.628126	8000.219440	9.576154	-0.090626	4.818065
460.537985	8000.221336	9.581159	-0.090609	4.818066
460.761819	8000.233953	9.586163	-0.090651	4.818068
460.376036	8000.226437	9.591168	-0.090579	4.818068
460.128625	8000.355607	9.596173	-0.090533	4.818107
460.493838	8000.319679	9.601178	-0.090601	4.818095
460.093630	8000.346699	9.606183	-0.090526	4.818105
460.291537	8000.356847	9.611187	-0.090563	4.818107
460.158731	8000.362355	9.616192	-0.090539	4.818109
460.141496	8000.432646	9.621197	-0.090535	4.818130
460.275907	8000.350319	9.626202	-0.090560	4.818105
460.326372	8000.344713	9.631207	-0.090570	4.818103
460.361361	8000.389420	9.636211	-0.090576	4.818116
460.693114	8000.302493	9.641216	-0.090638	4.818089
460.531559	8000.303386	9.646221	-0.090608	4.818090
460.548504	8000.323628	9.651226	-0.090611	4.818096
460.611969	8000.286624	9.656231	-0.090623	4.818085
460.576478	8000.362975	9.661235	-0.090617	4.818108
460.564052	8000.361750	9.666240	-0.090614	4.818107
460.871853	8000.351335	9.671245	-0.090672	4.818103
460.495180	8000.360789	9.676250	-0.090602	4.818107
460.567489	8000.341804	9.681255	-0.090615	4.818101
460.431535	8000.393586	9.686259	-0.090590	4.818117
460.666304	8000.321089	9.691264	-0.090634	4.818095
460.831376	8000.370780	9.696269	-0.090664	4.818109
460.666016	8000.381094	9.701274	-0.090634	4.818113
460.508428	8000.371516	9.706279	-0.090604	4.818110
460.475391	8000.435269	9.711283	-0.090598	4.818129
460.853879	8000.334261	9.716288	-0.090669	4.818098
460.826210	8000.406512	9.721293	-0.090664	4.818119
460.854061	8000.424801	9.726298	-0.090669	4.818125
460.611406	8000.407712	9.731303	-0.090624	4.818121
461.221120	8000.381534	9.736307	-0.090737	4.818110
461.137259	8000.325618	9.741312	-0.090722	4.818094
461.305578	8000.345880	9.746317	-0.090753	4.818099
461.514944	8000.360401	9.751322	-0.090792	4.818103
461.099453	8000.397732	9.756327	-0.090715	4.818116
460.996375	8000.427868	9.761331	-0.090696	4.818125
461.072494	8000.353144	9.766336	-0.090710	4.818103
461.347085	8000.340158	9.771341	-0.090761	4.818098
461.368210	8000.348879	9.776346	-0.090765	4.818100
461.309151	8000.317523	9.781351	-0.090754	4.818091
461.393141	8000.374499	9.786355	-0.090770	4.818108
461.205314	8000.381338	9.791360	-0.090735	4.818110
461.454281	8000.369046	9.796365	-0.090781	4.818106
461.514796	8000.396216	9.801370	-0.090792	4.818113
461.241345	8000.375535	9.806375	-0.090741	4.818108
461.223405	8000.347915	9.811379	-0.090738	4.818100
461.606229	8000.295393	9.816384	-0.090809	4.818083
461.260012	8000.375804	9.821389	-0.090745	4.818108
460.909342	8000.396149	9.826394	-0.090680	4.818116
460.839782	8000.370963	9.831399	-0.090667	4.818109
460.937258	8000.407073	9.836403	-0.090685	4.818119
460.623620	8000.431096	9.841408	-0.090627	4.818128
460.706741	8000.361733	9.846413	-0.090642	4.818107
460.913364	8000.441484	9.851418	-0.090681	4.818129
460.987288	8000.395152	9.856423	-0.090694	4.818115
461.226559	8000.398514	9.861427	-0.090739	4.818115
460.923504	8000.422685	9.866432	-0.090683	4.818124
461.375018	8000.400603	9.871437	-0.090767	4.818115
461.069110	8000.401574	9.876442	-0.090710	4.818117
461.032276	8000.412639	9.881447	-0.090703	4.818120
461.352109	8000.378181	9.886451	-0.090763	4.818109
461.400230	8000.353594	9.891456	-0.090772	4.818101
461.176900	8000.384148	9.896461	-0.090730	4.818111
461.551051	8000.354664	9.901466	-0.090800	4.818101
461.771220	8000.351441	9.906471	-0.090841	4.818099
461.578437	8000.397162	9.911475	-0.090805	4.818113
461.133859	8000.361446	9.916480	-0.090722	4.818105
461.538577	8000.386080	9.921485	-0.090797	4.818110
461.689127	8000.348193	9.926490	-0.090826	4.818098
461.266704	8000.374898	9.931495	-0.090747	4.818108
461.600265	8000.370109	9.936499	-0.090809	4.818105
461.539674	8000.372419	9.941504	-0.090798	4.818106
461.537350	8000.343965	9.946509	-0.090797	4.818098
461.877218	8000.348740	9.951514	-0.090861	4.818098
461.570708	8000.357071	9.956519	-0.090804	4.818102
461.789148	8000.353825	9.961523	-0.090844	4.818100
461.871458	8000.291819	9.966528	-0.090860	4.818081
461.944469	8000.311796	9.971533	-0.090873	4.818087
461.716223	8000.354913	9.976538	-0.090831	4.818100
461.650062	8000.286612	9.981543	-0.090819	4.818080
461.994787	8000.340934	9.986547	-0.090883	4.818095
461.916413	8000.229299	9.991552	-0.090868	4.818062
461.811657	8000.304679	9.996557	-0.090849	4.818085
462.217894	8000.254592	10.001562	-0.090924	4.818068
462.029177	8000.261418	10.006567	-0.090889	4.818071
462.114238	8000.281564	10.011571	-0.090905	4.818077
461.965383	8000.246842	10.016576	-0.090877	4.818067
462.249946	8000.259262	10.021581	-0.090930	4.818070
462.399681	8000.229785	10.026586	-0.090958	4.818060
462.327376	8000.240352	10.031591	-0.090945	4.818064
462.223481	8000.309429	10.036595	-0.090926	4.818085
461.923489	8000.282058	10.041600	-0.090870	4.818078
462.100717	8000.346661	10.046605	-0.090903	4.818096
462.157739	8000.339042	10.051610	-0.090914	4.818094
462.124519	8000.260676	10.056615	-0.090907	4.818071
462.316551	8000.287588	10.061619	-0.090943	4.818078
461.935378	8000.280132	10.066624	-0.090872	4.818077
461.823835	8000.378577	10.071629	-0.090852	4.818107
462.014386	8000.364412	10.076634	-0.090887	4.818102
461.909954	8000.332418	10.081639	-0.090868	4.818093
462.258203	8000.293097	10.086643	-0.090932	4.818080
462.323212	8000.248744	10.091648	-0.090945	4.818066
461.833092	8000.335557	10.096653	-0.090853	4.818094
462.074474	8000.289471	10.101658	-0.090898	4.818079
461.930116	8000.362190	10.106663	-0.090872	4.818102
462.059006	8000.390321	10.111667	-0.090896	4.818109
461.969104	8000.338529	10.116672	-0.090879	4.818094
462.044183	8000.396434	10.121677	-0.090893	4.818111
461.701641	8000.400047	10.126682	-0.090829	4.818114
461.823121	8000.314379	10.131687	-0.090852	4.818088
461.853156	8000.367440	10.136691	-0.090857	4.818103
461.762539	8000.370381	10.141696	-0.090841	4.818105
461.702609	8000.423231	10.146701	-0.090829	4.818121
461.941413	8000.380267	10.151706	-0.090874	4.818107
462.223382	8000.325276	10.156711	-0.090926	4.818089
462.107673	8000.401556	10.161715	-0.090905	4.818113
462.235146	8000.325446	10.166720	-0.090929	4.818089
462.345173	8000.353312	10.171725	-0.090949	4.818097
462.010376	8000.389669	10.176730	-0.090887	4.818109
461.930428	8000.383285	10.181735	-0.090872	4.818108
462.355560	8000.338727	10.186739	-0.090951	4.818093
462.739200	8000.277795	10.191744	-0.091023	4.818073
462.362956	8000.329361	10.196749	-0.090953	4.818090
462.325785	8000.331999	10.201754	-0.090946	4.818091
462.142102	8000.352582	10.206759	-0.090912	4.818098
462.497113	8000.387048	10.211763	-0.090978	4.818107
461.941454	8000.396089	10.216768	-0.090874	4.818112
461.880297	8000.455239	10.221773	-0.090863	4.818129
462.048550	8000.419706	10.226778	-0.090894	4.818118
462.315297	8000.207643	10.231783	-0.090944	4.818054
461.974303	8000.397613	10.236787	-0.090881	4.818112
462.264256	8000.366947	10.241792	-0.090935	4.818102
462.331377	8000.333152	10.246797	-0.090947	4.818091
461.971287	8000.410210	10.251802	-0.090880	4.818116
462.233728	8000.350735	10.256807	-0.090929	4.818097
462.453395	8000.401196	10.261811	-0.090970	4.818111
462.142816	8000.404205	10.266816	-0.090912	4.818113
462.244439	8000.378264	10.271821	-0.090931	4.818105
462.092953	8000.406668	10.276826	-0.090903	4.818114
461.878992	8000.380505	10.281831	-0.090863	4.818107
462.067731	8000.420004	10.286835	-0.090898	4.818118
462.041714	8000.394375	10.291840	-0.090894	4.818111
461.698913	8000.456938	10.296845	-0.090830	4.818131
461.485950	8000.429737	10.301850	-0.090790	4.818123
461.372348	8000.442882	10.306855	-0.090769	4.818128
461.782519	8000.481279	10.311859	-0.090845	4.818137
462.209975	8000.416752	10.316864	-0.090925	4.818117
462.588175	8000.337848	10.321869	-0.090995	4.818092
462.511601	8000.355724	10.326874	-0.090981	4.818097
462.471059	8000.303572	10.331879	-0.090974	4.818082
462.427566	8000.360865	10.336883	-0.090966	4.818099
462.557205	8000.339528	10.341888	-0.090990	4.818092
462.528597	8000.365447	10.346893	-0.090984	4.818100
462.691049	8000.325622	10.351898	-0.091015	4.818088
462.915967	8000.252986	10.356903	-0.091057	4.818065
462.941313	8000.313351	10.361907	-0.091061	4.818083
462.519137	8000.344269	10.366912	-0.090983	4.818094
462.376834	8000.353852	10.371917	-0.090956	4.818097
462.735844	8000.353635	10.376922	-0.091023	4.818096
462.301698	8000.361224	10.381927	-0.090942	4.818100
462.002972	8000.435986	10.386931	-0.090887	4.818123
462.225441	8000.404373	10.391936	-0.090928	4.818113
462.545137	8000.394128	10.396941	-0.090988	4.818108
462.403756	8000.379511	10.401946	-0.090962	4.818105
462.210717	8000.378907	10.406951	-0.090926	4.818105
462.290958	8000.413724	10.411955	-0.090941	4.818115
462.552606	8000.296337	10.416960	-0.090989	4.818079
462.323645	8000.259435	10.421965	-0.090947	4.818069
462.798267	8000.356641	10.426970	-0.091035	4.818096
462.624529	8000.320514	10.431975	-0.091003	4.818086
462.710092	8000.346985	10.436979	-0.091019	4.818094
462.793507	8000.298680	10.441984	-0.091034	4.818079
462.777088	8000.375302	10.446989	-0.091031	4.818102
462.740100	8000.385313	10.451994	-0.091025	4.818105
462.224978	8000.354918	10.456999	-0.090929	4.818098
462.442778	8000.414828	10.462003	-0.090969	4.818115
462.666772	8000.351654	10.467008	-0.091011	4.818095
462.381401	8000.383441	10.472013	-0.090958	4.818106
462.592414	8000.406410	10.477018	-0.090997	4.818112
462.499085	8000.360886	10.482023	-0.090980	4.818099
462.464933	8000.414099	10.487027	-0.090974	4.818115
462.779760	8000.357465	10.492032	-0.091032	4.818097
462.724786	8000.356695	10.497037	-0.091022	4.818097
462.582268	8000.412596	10.502042	-0.090996	4.818114
462.129995	8000.434669	10.507047	-0.090911	4.818122
462.793745	8000.389253	10.512051	-0.091035	4.818106
463.043166	8000.336964	10.517056	-0.091081	4.818089
462.603893	8000.402382	10.522061	-0.091000	4.818111
462.456862	8000.400319	10.527066	-0.090972	4.818111
462.333943	8000.440704	10.532071	-0.090949	4.818123
462.816783	8000.375903	10.537075	-0.091039	4.818102
462.916401	8000.368883	10.542080	-0.091058	4.818099
462.983066	8000.360348	10.547085	-0.091070	4.818097
462.757619	8000.337180	10.552090	-0.091028	4.818091
462.892959	8000.259075	10.557095	-0.091054	4.818067
463.139366	8000.379395	10.562099	-0.091100	4.818102
463.264421	8000.305356	10.567104	-0.091123	4.818079
463.129348	8000.240295	10.572109	-0.091098	4.818060
463.031390	8000.349460	10.577114	-0.091080	4.818093
462.905705	8000.326642	10.582119	-0.091056	4.818087
462.994795	8000.378428	10.587123	-0.091073	4.818102
462.484418	8000.414423	10.592128	-0.090978	4.818115
462.314854	8000.413096	10.597133	-0.090946	4.818115
462.219821	8000.480192	10.602138	-0.090929	4.818135
462.010848	8000.450940	10.607143	-0.090890	4.818128
462.022937	8000.361629	10.612147	-0.090892	4.818101
462.420061	8000.445113	10.617152	-0.090966	4.818124
462.404419	8000.434368	10.622157	-0.090963	4.818121
462.877598	8000.405225	10.627162	-0.091051	4.818110
462.466537	8000.434193	10.632167	-0.090975	4.818121
462.495534	8000.469344	10.637171	-0.090980	4.818131
462.317730	8000.412105	10.642176	-0.090947	4.818115
462.617122	8000.394206	10.647181	-0.091003	4.818108
462.494514	8000.390380	10.652186	-0.090980	4.818108
462.845768	8000.285831	10.657191	-0.091045	4.818075
463.127613	8000.356117	10.662195	-0.091098	4.818095
463.129880	8000.363521	10.667200	-0.091098	4.818097
462.933264	8000.336547	10.672205	-0.091062	4.818090
463.059763	8000.374120	10.677210	-0.091085	4.818100
463.208423	8000.322521	10.682215	-0.091113	4.818084
462.848561	8000.409057	10.687219	-0.091046	4.818112
462.755989	8000.371965	10.692224	-0.091029	4.818101
462.938348	8000.362949	10.697229	-0.091063	4.818098
462.824278	8000.375035	10.702234	-0.091042	4.818102
462.944966	8000.306198	10.707239	-0.091064	4.818081
462.583369	8000.409554	10.712243	-0.090997	4.818113
462.703820	8000.393352	10.717248	-0.091019	4.818108
462.720255	8000.379899	10.722253	-0.091023	4.818103
462.970096	8000.417100	10.727258	-0.091069	4.818113
462.626700	8000.410172	10.732263	-0.091005	4.818113
462.654263	8000.435828	10.737267	-0.091010	4.818120
462.546470	8000.405891	10.742272	-0.090990	4.818112
462.641339	8000.393541	10.747277	-0.091008	4.818108
463.039950	8000.366509	10.752282	-0.091082	4.818098
462.589552	8000.391765	10.757287	-0.090998	4.818108
462.956165	8000.434818	10.762291	-0.091067	4.818119
462.642891	8000.414627	10.767296	-0.091008	4.818114
462.663943	8000.384396	10.772301	-0.091012	4.818105
462.642119	8000.448309	10.777306	-0.091008	4.818124
462.617590	8000.386907	10.782311	-0.091004	4.818106
463.067443	8000.375334	10.787315	-0.091088	4.818101
462.524864	8000.389820	10.792320	-0.090987	4.818107
462.701061	8000.344924	10.797325	-0.091019	4.818093
463.038869	8000.309668	10.802330	-0.091082	4.818081
463.042571	8000.281298	10.807335	-0.091083	4.818073
463.434249	8000.288910	10.812339	-0.091156	4.818073
463.715270	8000.280228	10.817344	-0.091208	4.818070
463.289659	8000.259511	10.822349	-0.091129	4.818065
463.236926	8000.321938	10.827354	-0.091119	4.818084
463.319401	8000.272567	10.832359	-0.091135	4.818069
463.322480	8000.407366	10.837363	-0.091135	4.818109
463.072822	8000.355433	10.842368	-0.091089	4.818095
462.656424	8000.382220	10.847373	-0.091011	4.818104
463.003151	8000.388147	10.852378	-0.091076	4.818105
462.495694	8000.383125	10.857383	-0.090982	4.818105
462.998280	8000.335445	10.862387	-0.091075	4.818089
463.176461	8000.352690	10.867392	-0.091108	4.818093
463.382030	8000.269255	10.872397	-0.091147	4.818068
463.274403	8000.326699	10.877402	-0.091127	4.818085
463.466376	8000.235703	10.882407	-0.091162	4.818058
463.544615	8000.258913	10.887411	-0.091177	4.818064
463.271382	8000.250865	10.892416	-0.091126	4.818063
463.190378	8000.291840	10.897421	-0.091111	4.818075
463.396367	8000.357903	10.902426	-0.091150	4.818094
463.464839	8000.192531	10.907431	-0.091162	4.818045
463.587871	8000.217422	10.912435	-0.091185	4.818052
463.595107	8000.272270	10.917440	-0.091187	4.818068
463.373001	8000.297576	10.922445	-0.091145	4.818076
463.176492	8000.374827	10.927450	-0.091109	4.818100
463.229973	8000.286096	10.932455	-0.091119	4.818073
463.119556	8000.377190	10.937459	-0.091098	4.818101
463.214945	8000.365900	10.942464	-0.091116	4.818097
463.138691	8000.366936	10.947469	-0.091102	4.818098
462.868020	8000.330500	10.952474	-0.091052	4.818088
462.929777	8000.407169	10.957479	-0.091063	4.818111
462.995491	8000.385987	10.962483	-0.091075	4.818104
463.068251	8000.342795	10.967488	-0.091089	4.818091
462.928747	8000.346101	10.972493	-0.091063	4.818093
462.801887	8000.389590	10.977498	-0.091039	4.818106
463.042333	8000.326647	10.982503	-0.091084	4.818086
463.365165	8000.333291	10.987507	-0.091144	4.818087
463.172272	8000.350586	10.992512	-0.091108	4.818093
463.298823	8000.373422	10.997517	-0.091132	4.818099
463.337714	8000.396079	11.002522	-0.091139	4.818106
463.339795	8000.306625	11.007527	-0.091140	4.818079
463.340481	8000.346642	11.012531	-0.091140	4.818091
463.375569	8000.362929	11.017536	-0.091146	4.818096
463.555058	8000.350716	11.022541	-0.091180	4.818091
463.435258	8000.353245	11.027546	-0.091158	4.818093
463.485439	8000.293945	11.032551	-0.091167	4.818075
463.206995	8000.397417	11.037555	-0.091115	4.818107
463.667857	8000.369155	11.042560	-0.091201	4.818096
463.727478	8000.322620	11.047565	-0.091212	4.818082
463.547966	8000.379055	11.052570	-0.091179	4.818100
463.367160	8000.311245	11.057575	-0.091145	4.818080
463.267882	8000.363543	11.062579	-0.091127	4.818096
463.624999	8000.305398	11.067584	-0.091193	4.818078
463.695998	8000.346404	11.072589	-0.091206	4.818089
463.686646	8000.379964	11.077594	-0.091205	4.818099
463.281208	8000.374267	11.082599	-0.091129	4.818099
463.330805	8000.451819	11.087603	-0.091139	4.818122
463.314551	8000.406324	11.092608	-0.091136	4.818109
463.364706	8000.414401	11.097613	-0.091145	4.818111
463.026728	8000.446500	11.102618	-0.091082	4.818122
463.183676	8000.377120	11.107623	-0.091111	4.818101
463.315600	8000.391609	11.112627	-0.091136	4.818104
463.023655	8000.385404	11.117632	-0.091082	4.818104
463.615282	8000.302129	11.122637	-0.091192	4.818077
463.877878	8000.333195	11.127642	-0.091241	4.818085
463.674723	8000.348239	11.132647	-0.091203	4.818090
463.716436	8000.313033	11.137651	-0.091211	4.818079
463.722722	8000.309966	11.142656	-0.091212	4.818078
463.556159	8000.304469	11.147661	-0.091181	4.818078
463.604399	8000.395688	11.152666	-0.091190	4.818104
463.381979	8000.360981	11.157671	-0.091149	4.818095
463.540282	8000.413741	11.162675	-0.091178	4.818110
463.849251	8000.339128	11.167680	-0.091236	4.818087
464.019342	8000.242560	11.172685	-0.091267	4.818057
463.809836	8000.320682	11.177690	-0.091228	4.818081
463.790356	8000.283563	11.182695	-0.091225	4.818070
463.899348	8000.322998	11.187699	-0.091245	4.818082
463.675709	8000.367231	11.192704	-0.091203	4.818096
462.997862	8000.420873	11.197709	-0.091077	4.818114
462.738754	8000.508825	11.202714	-0.091029	4.818142
463.367190	8000.373430	11.207719	-0.091146	4.818099
463.460340	8000.417905	11.212723	-0.091163	4.818112
463.293747	8000.406091	11.217728	-0.091133	4.818109
463.751492	8000.310408	11.222733	-0.091218	4.818078
463.825179	8000.376719	11.227738	-0.091231	4.818098
463.734253	8000.333332	11.232743	-0.091215	4.818085
463.590923	8000.396592	11.237747	-0.091188	4.818105
463.633285	8000.385609	11.242752	-0.091196	4.818101
463.224575	8000.416714	11.247757	-0.091120	4.818112
463.061462	8000.473379	11.252762	-0.091090	4.818130
463.486707	8000.351973	11.257767	-0.091169	4.818092
463.692101	8000.348545	11.262771	-0.091207	4.818090
462.973579	8000.421618	11.267776	-0.091073	4.818115
463.025238	8000.419188	11.272781	-0.091083	4.818114
463.716508	8000.340473	11.277786	-0.091212	4.818088
463.603156	8000.282033	11.282791	-0.091190	4.818071
463.589210	8000.280786	11.287795	-0.091188	4.818070
463.716615	8000.328901	11.292800	-0.091212	4.818084
463.906677	8000.274725	11.297805	-0.091247	4.818067
463.655447	8000.417533	11.302810	-0.091200	4.818111
463.569264	8000.336313	11.307815	-0.091184	4.818087
463.561729	8000.404639	11.312819	-0.091183	4.818107
463.328410	8000.415048	11.317824	-0.091140	4.818111
463.293341	8000.415611	11.322829	-0.091133	4.818112
463.395602	8000.417050	11.327834	-0.091152	4.818112
463.021203	8000.405474	11.332839	-0.091082	4.818110
463.089081	8000.380111	11.337843	-0.091095	4.818102
462.833982	8000.415481	11.342848	-0.091048	4.818113
462.577526	8000.404511	11.347853	-0.091000	4.818111
462.701058	8000.466256	11.352858	-0.091023	4.818129
462.925904	8000.369406	11.357863	-0.091065	4.818099
463.005305	8000.494750	11.362867	-0.091080	4.818136
462.904732	8000.468073	11.367872	-0.091061	4.818129
463.394147	8000.410735	11.372877	-0.091152	4.818110
463.390971	8000.461226	11.377882	-0.091152	4.818125
463.120749	8000.431111	11.382887	-0.091101	4.818117
463.397593	8000.403421	11.387891	-0.091153	4.818108
462.884065	8000.381468	11.392896	-0.091057	4.818103
463.121755	8000.417446	11.397901	-0.091102	4.818113
462.883550	8000.461475	11.402906	-0.091057	4.818127
462.967665	8000.422655	11.407911	-0.091073	4.818115
462.866912	8000.477038	11.412915	-0.091054	4.818132
463.373569	8000.418889	11.417920	-0.091149	4.818112
463.155580	8000.435830	11.422925	-0.091108	4.818118
463.298619	8000.463110	11.427930	-0.091135	4.818126
463.321449	8000.373947	11.432935	-0.091139	4.818099
463.516154	8000.430378	11.437939	-0.091175	4.818115
463.120590	8000.447981	11.442944	-0.091102	4.818122
463.465512	8000.415985	11.447949	-0.091166	4.818111
463.550722	8000.423502	11.452954	-0.091182	4.818113
463.723802	8000.385931	11.457959	-0.091214	4.818101
463.705131	8000.402516	11.462963	-0.091211	4.818106
463.601116	8000.401056	11.467968	-0.091191	4.818106
463.691268	8000.373901	11.472973	-0.091208	4.818098
463.603649	8000.373724	11.477978	-0.091192	4.818098
463.449101	8000.333655	11.482983	-0.091163	4.818087
463.450584	8000.370525	11.487987	-0.091163	4.818098
463.518883	8000.389384	11.492992	-0.091176	4.818103
463.689739	8000.343361	11.497997	-0.091208	4.818088
463.433513	8000.431353	11.503002	-0.091160	4.818116
463.711962	8000.274194	11.508007	-0.091212	4.818068
463.722681	8000.381731	11.513011	-0.091214	4.818100
463.370308	8000.394677	11.518016	-0.091149	4.818105
463.331880	8000.397298	11.523021	-0.091142	4.818106
463.643032	8000.417466	11.528026	-0.091200	4.818111
463.801633	8000.370217	11.533031	-0.091229	4.818096
463.531193	8000.387473	11.538035	-0.091179	4.818102
463.670624	8000.412597	11.543040	-0.091205	4.818109
463.555608	8000.365713	11.548045	-0.091183	4.818096
463.402050	8000.417248	11.553050	-0.091155	4.818112
463.424726	8000.401778	11.558055	-0.091159	4.818107
463.672229	8000.373676	11.563059	-0.091205	4.818098
463.552641	8000.360417	11.568064	-0.091183	4.818094
463.221770	8000.412619	11.573069	-0.091121	4.818111
463.803129	8000.403948	11.578074	-0.091230	4.818106
463.928725	8000.369922	11.583079	-0.091253	4.818095
463.790613	8000.364824	11.588083	-0.091227	4.818094
463.809638	8000.359830	11.593088	-0.091231	4.818093
463.905547	8000.364339	11.598093	-0.091249	4.818094
464.104380	8000.409248	11.603098	-0.091286	4.818106
463.797535	8000.378617	11.608103	-0.091229	4.818098
463.840931	8000.386599	11.613107	-0.091237	4.818101
463.886035	8000.340913	11.618112	-0.091245	4.818087
463.689472	8000.388686	11.623117	-0.091209	4.818102
463.918323	8000.435070	11.628122	-0.091251	4.818115
463.671540	8000.400019	11.633127	-0.091205	4.818105
463.865014	8000.329047	11.638131	-0.091241	4.818083
463.412073	8000.392166	11.643136	-0.091157	4.818104
463.591095	8000.333623	11.648141	-0.091191	4.818086
463.848368	8000.343559	11.653146	-0.091238	4.818088
463.401203	8000.373070	11.658151	-0.091155	4.818098
463.685189	8000.370748	11.663155	-0.091208	4.818097
463.403426	8000.419428	11.668160	-0.091156	4.818112
462.834893	8000.424074	11.673165	-0.091050	4.818116
463.211269	8000.432524	11.678170	-0.091120	4.818117
463.591533	8000.317855	11.683175	-0.091191	4.818081
463.476293	8000.364665	11.688179	-0.091169	4.818096
463.529779	8000.379105	11.693184	-0.091179	4.818100
463.672079	8000.348472	11.698189	-0.091206	4.818090
463.697584	8000.393049	11.703194	-0.091211	4.818103
463.687945	8000.373966	11.708199	-0.091209	4.818098
463.583028	8000.375652	11.713203	-0.091189	4.818098
463.584956	8000.345151	11.718208	-0.091190	4.818089
463.432327	8000.340903	11.723213	-0.091161	4.818089
463.802059	8000.271355	11.728218	-0.091230	4.818067
464.095369	8000.314433	11.733223	-0.091285	4.818078
463.916784	8000.345614	11.738227	-0.091252	4.818088
463.789370	8000.382778	11.743232	-0.091228	4.818100
463.945181	8000.383918	11.748237	-0.091257	4.818099
463.981751	8000.396015	11.753242	-0.091264	4.818103
463.413191	8000.378550	11.758247	-0.091158	4.818100
463.584715	8000.366225	11.763251	-0.091190	4.818096
464.205437	8000.233880	11.768256	-0.091306	4.818054
464.286778	8000.239237	11.773261	-0.091321	4.818055
463.954369	8000.356689	11.778266	-0.091259	4.818091
463.910653	8000.298174	11.783271	-0.091251	4.818074
463.973206	8000.296950	11.788275	-0.091263	4.818073
464.102781	8000.338780	11.793280	-0.091287	4.818085
464.204512	8000.237039	11.798285	-0.091306	4.818055
464.266275	8000.296866	11.803290	-0.091317	4.818072
463.873475	8000.302927	11.808295	-0.091244	4.818076
464.044870	8000.312708	11.813299	-0.091276	4.818078
464.130741	8000.356029	11.818304	-0.091292	4.818090
463.565627	8000.327032	11.823309	-0.091187	4.818084
463.877262	8000.389318	11.828314	-0.091245	4.818101
463.887381	8000.338929	11.833319	-0.091247	4.818086
463.880227	8000.268295	11.838323	-0.091246	4.818065
463.866168	8000.314422	11.843328	-0.091243	4.818079
463.803174	8000.254583	11.848333	-0.091231	4.818062
464.018513	8000.329202	11.853338	-0.091271	4.818083
463.896205	8000.344329	11.858343	-0.091249	4.818088
463.801458	8000.359844	11.863347	-0.091231	4.818093
463.945118	8000.389238	11.868352	-0.091258	4.818101
463.916287	8000.359358	11.873357	-0.091253	4.818092
463.935553	8000.375423	11.878362	-0.091256	4.818097
463.889690	8000.271608	11.883367	-0.091248	4.818066
463.526596	8000.383365	11.888371	-0.091180	4.818101
463.778332	8000.358481	11.893376	-0.091227	4.818093
464.042701	8000.316930	11.898381	-0.091276	4.818079
463.751940	8000.406542	11.903386	-0.091222	4.818107
463.500436	8000.417748	11.908391	-0.091175	4.818111
463.879311	8000.355699	11.913395	-0.091246	4.818091
463.763159	8000.423552	11.918400	-0.091224	4.818112
463.812804	8000.397932	11.923405	-0.091234	4.818104
463.940435	8000.411310	11.928410	-0.091257	4.818108
463.736328	8000.398968	11.933415	-0.091219	4.818105
464.024558	8000.336697	11.938419	-0.091273	4.818085
464.075550	8000.330046	11.943424	-0.091283	4.818083
464.074953	8000.317407	11.948429	-0.091283	4.818079
464.084475	8000.377552	11.953434	-0.091284	4.818097
463.740668	8000.308502	11.958439	-0.091220	4.818078
464.222787	8000.270011	11.963443	-0.091310	4.818064
464.009196	8000.377554	11.968448	-0.091270	4.818097
464.024077	8000.358815	11.973453	-0.091273	4.818092
463.894722	8000.366474	11.978458	-0.091249	4.818094
464.002616	8000.255345	11.983463	-0.091269	4.818061
464.153095	8000.342739	11.988467	-0.091297	4.818086
463.959259	8000.360019	11.993472	-0.091261	4.818092
463.495529	8000.361925	11.998477	-0.091175	4.818095
463.548522	8000.457422	12.003482	-0.091185	4.818123
463.682769	8000.391934	12.008487	-0.091210	4.818103
463.878761	8000.365214	12.013491	-0.091246	4.818094
463.931705	8000.384910	12.018496	-0.091256	4.818100
464.038774	8000.314829	12.023501	-0.091276	4.818078
464.184054	8000.315821	12.028506	-0.091303	4.818078
463.968154	8000.364374	12.033511	-0.091263	4.818093
463.822145	8000.414963	12.038515	-0.091236	4.818109
463.820404	8000.429680	12.043520	-0.091236	4.818113
463.733780	8000.354770	12.048525	-0.091220	4.818092
464.198437	8000.334985	12.053530	-0.091306	4.818084
464.371967	8000.303738	12.058535	-0.091339	4.818074
464.326967	8000.237835	12.063539	-0.091330	4.818054
464.303441	8000.263826	12.068544	-0.091326	4.818062
464.286941	8000.228854	12.073549	-0.091323	4.818052
464.645895	8000.229692	12.078554	-0.091390	4.818051
464.604936	8000.281758	12.083559	-0.091382	4.818066
464.456290	8000.307043	12.088563	-0.091354	4.818074
464.434032	8000.300416	12.093568	-0.091350	4.818073
464.212032	8000.280453	12.098573	-0.091309	4.818068
464.157728	8000.357598	12.103578	-0.091299	4.818091
464.221912	8000.339552	12.108583	-0.091311	4.818085
464.153484	8000.275426	12.113587	-0.091298	4.818066
464.452830	8000.300692	12.118592	-0.091354	4.818073
464.436923	8000.290996	12.123597	-0.091351	4.818070
464.218205	8000.336351	12.128602	-0.091310	4.818084
464.149479	8000.297487	12.133607	-0.091298	4.818073
464.274123	8000.296084	12.138611	-0.091321	4.818072
464.364720	8000.261565	12.143616	-0.091338	4.818061
464.246174	8000.279904	12.148621	-0.091316	4.818067
464.211311	8000.401540	12.153626	-0.091309	4.818103
464.605657	8000.260748	12.158631	-0.091383	4.818060
464.503932	8000.248793	12.163635	-0.091364	4.818057
464.656207	8000.346741	12.168640	-0.091392	4.818085
464.606378	8000.253396	12.173645	-0.091383	4.818058
464.679319	8000.308117	12.178650	-0.091397	4.818074
464.705559	8000.232687	12.183655	-0.091401	4.818051
464.499987	8000.309811	12.188659	-0.091363	4.818075
464.452491	8000.328096	12.193664	-0.091354	4.818081
464.542428	8000.272512	12.198669	-0.091371	4.818064
464.714960	8000.331791	12.203674	-0.091403	4.818081
464.457908	8000.311335	12.208679	-0.091355	4.818076
464.173688	8000.313658	12.213683	-0.091303	4.818078
464.113576	8000.388616	12.218688	-0.091291	4.818100
463.844584	8000.411156	12.223693	-0.091241	4.818108
464.042333	8000.406569	12.228698	-0.091278	4.818106
464.075557	8000.341766	12.233703	-0.091284	4.818086
464.220119	8000.353276	12.238707	-0.091311	4.818089
464.320415	8000.302049	12.243712	-0.091330	4.818073
464.286740	8000.308947	12.248717	-0.091324	4.818076
464.179730	8000.369560	12.253722	-0.091304	4.818094
464.159254	8000.362957	12.258727	-0.091300	4.818092
464.073514	8000.379652	12.263731	-0.091284	4.818098
464.114684	8000.394972	12.268736	-0.091292	4.818102
464.551508	8000.288467	12.273741	-0.091373	4.818068
464.292292	8000.317462	12.278746	-0.091325	4.818078
464.436224	8000.299485	12.283751	-0.091352	4.818072
464.365928	8000.304816	12.288755	-0.091339	4.818074
464.372954	8000.359662	12.293760	-0.091340	4.818090
464.194017	8000.311879	12.298765	-0.091307	4.818077
464.214492	8000.401656	12.303770	-0.091311	4.818103
464.109108	8000.357012	12.308775	-0.091291	4.818091
464.101418	8000.260050	12.313779	-0.091290	4.818062
464.051656	8000.372001	12.318784	-0.091281	4.818095
463.993234	8000.413294	12.323789	-0.091270	4.818108
464.433519	8000.425804	12.328794	-0.091352	4.818110
463.981993	8000.368923	12.333799	-0.091268	4.818095
464.511309	8000.274247	12.338803	-0.091366	4.818064
464.520215	8000.360704	12.343808	-0.091368	4.818090
464.397681	8000.321083	12.348813	-0.091345	4.818079
464.209119	8000.358440	12.353818	-0.091310	4.818091
464.070818	8000.392293	12.358823	-0.091284	4.818101
464.342843	8000.334005	12.363827	-0.091335	4.818083
464.507761	8000.367910	12.368832	-0.091366	4.818092
463.960339	8000.373902	12.373837	-0.091264	4.818096
463.858817	8000.453542	12.378842	-0.091245	4.818120
463.758609	8000.397390	12.383847	-0.091226	4.818104
463.787850	8000.377801	12.388851	-0.091232	4.818098
463.778655	8000.411363	12.393856	-0.091230	4.818108
464.022537	8000.340046	12.398861	-0.091276	4.818086
464.046924	8000.404612	12.403866	-0.091280	4.818105
464.603903	8000.370334	12.408871	-0.091384	4.818093
464.321964	8000.349527	12.413875	-0.091331	4.818088
464.252841	8000.364350	12.418880	-0.091319	4.818092
463.941845	8000.396827	12.423885	-0.091261	4.818103
464.860820	8000.321317	12.428890	-0.091432	4.818077
464.310228	8000.379903	12.433895	-0.091329	4.818097
464.351803	8000.354170	12.438899	-0.091337	4.818089
464.280512	8000.419496	12.443904	-0.091324	4.818108
463.913669	8000.404865	12.448909	-0.091256	4.818106
463.908402	8000.469014	12.453914	-0.091255	4.818125
464.012096	8000.405201	12.458919	-0.091274	4.818105
463.696490	8000.452353	12.463923	-0.091215	4.818121
463.454033	8000.348933	12.468928	-0.091170	4.818091
464.059686	8000.390085	12.473933	-0.091283	4.818101
464.329908	8000.398099	12.478938	-0.091333	4.818102
464.261245	8000.356076	12.483943	-0.091321	4.818090
464.355061	8000.330025	12.488947	-0.091338	4.818082
464.350225	8000.405761	12.493952	-0.091337	4.818104
464.014730	8000.356829	12.498957	-0.091275	4.818091
464.189583	8000.351920	12.503962	-0.091307	4.818089
464.175638	8000.380152	12.508967	-0.091305	4.818097
464.398733	8000.349602	12.513971	-0.091346	4.818087
463.948803	8000.450663	12.518976	-0.091263	4.818119
463.990768	8000.358610	12.523981	-0.091271	4.818092
464.336735	8000.357159	12.528986	-0.091335	4.818090
464.016722	8000.361085	12.533991	-0.091275	4.818092
464.024784	8000.404365	12.538995	-0.091277	4.818105
464.415663	8000.430920	12.544000	-0.091350	4.818111
464.499890	8000.389994	12.549005	-0.091365	4.818099
464.409522	8000.366617	12.554010	-0.091349	4.818092
464.362454	8000.337532	12.559015	-0.091340	4.818084
464.464416	8000.274748	12.564019	-0.091359	4.818065
464.245875	8000.404329	12.569024	-0.091318	4.818104
463.853910	8000.411454	12.574029	-0.091245	4.818108
463.950820	8000.429664	12.579034	-0.091263	4.818113
463.968665	8000.417284	12.584039	-0.091267	4.818109
463.906804	8000.407994	12.589043	-0.091255	4.818107
464.066004	8000.443924	12.594048	-0.091285	4.818117
464.065305	8000.415491	12.599053	-0.091285	4.818108
464.318394	8000.363254	12.604058	-0.091332	4.818092
464.251639	8000.374951	12.609063	-0.091320	4.818095
464.693350	8000.309575	12.614067	-0.091402	4.818074
464.303342	8000.386211	12.619072	-0.091329	4.818098
463.796009	8000.390661	12.624077	-0.091235	4.818102
464.261617	8000.428794	12.629082	-0.091322	4.818111
464.125446	8000.407931	12.634087	-0.091296	4.818106
464.125151	8000.383715	12.639091	-0.091296	4.818098
464.391307	8000.430625	12.644096	-0.091346	4.818111
464.481013	8000.321345	12.649101	-0.091363	4.818078
463.932995	8000.452610	12.654106	-0.091261	4.818120
463.790540	8000.415868	12.659111	-0.091234	4.818109
463.975699	8000.415315	12.664115	-0.091269	4.818108
464.332653	8000.388753	12.669120	-0.091335	4.818099
463.995782	8000.358752	12.674125	-0.091272	4.818092
464.144431	8000.445067	12.679130	-0.091300	4.818117
464.310172	8000.393708	12.684135	-0.091331	4.818101
463.811124	8000.456178	12.689139	-0.091238	4.818121
463.973171	8000.486884	12.694144	-0.091268	4.818130
463.791301	8000.453798	12.699149	-0.091235	4.818121
464.176573	8000.405525	12.704154	-0.091306	4.818105
464.461260	8000.382158	12.709159	-0.091359	4.818097
464.572749	8000.306874	12.714163	-0.091380	4.818074
464.738737	8000.334478	12.719168	-0.091411	4.818081
464.122697	8000.379510	12.724173	-0.091296	4.818097
464.519421	8000.412464	12.729178	-0.091370	4.818105
464.804086	8000.380674	12.734183	-0.091423	4.818095
464.572184	8000.375310	12.739187	-0.091380	4.818094
464.559119	8000.391973	12.744192	-0.091378	4.818099
464.827705	8000.268364	12.749197	-0.091428	4.818061
464.772214	8000.340229	12.754202	-0.091417	4.818083
464.594182	8000.348256	12.759207	-0.091384	4.818086
464.225035	8000.348332	12.764211	-0.091316	4.818088
464.296714	8000.389348	12.769216	-0.091329	4.818099
464.092389	8000.364369	12.774221	-0.091291	4.818093
464.382790	8000.310551	12.779226	-0.091345	4.818076
464.616201	8000.251720	12.784231	-0.091389	4.818057
464.556002	8000.306674	12.789235	-0.091377	4.818074
464.419979	8000.393199	12.794240	-0.091352	4.818100
463.958330	8000.399344	12.799245	-0.091266	4.818104
464.339340	8000.431023	12.804250	-0.091337	4.818112
464.171301	8000.398132	12.809255	-0.091306	4.818103
463.608935	8000.377595	12.814259	-0.091201	4.818099
463.891684	8000.488956	12.819264	-0.091254	4.818131
463.640294	8000.467527	12.824269	-0.091207	4.818125
463.682670	8000.422855	12.829274	-0.091215	4.818112
463.389168	8000.427154	12.834279	-0.091161	4.818114
463.768053	8000.481963	12.839283	-0.091231	4.818129
463.799781	8000.500309	12.844288	-0.091237	4.818134
464.021273	8000.448681	12.849293	-0.091278	4.818118
463.740876	8000.421580	12.854298	-0.091226	4.818111
463.536578	8000.478719	12.859303	-0.091188	4.818129
463.844653	8000.405146	12.864307	-0.091245	4.818106
463.948036	8000.475033	12.869312	-0.091265	4.818126
463.829382	8000.419675	12.874317	-0.091243	4.818110
464.154368	8000.394769	12.879322	-0.091303	4.818102
464.176311	8000.454036	12.884327	-0.091307	4.818119
464.370348	8000.387282	12.889331	-0.091344	4.818098
463.868281	8000.473924	12.894336	-0.091250	4.818126
464.334698	8000.385733	12.899341	-0.091337	4.818098
463.744051	8000.391117	12.904346	-0.091227	4.818102
464.235195	8000.393814	12.909351	-0.091318	4.818101
464.370431	8000.345184	12.914355	-0.091344	4.818086
464.469862	8000.331845	12.919360	-0.091362	4.818082
463.949270	8000.411909	12.924365	-0.091265	4.818108
464.133974	8000.376608	12.929370	-0.091300	4.818096
464.494387	8000.364834	12.934375	-0.091367	4.818091
464.070590	8000.394672	12.939379	-0.091288	4.818102
464.420215	8000.411171	12.944384	-0.091353	4.818105
464.571158	8000.365921	12.949389	-0.091381	4.818091
464.437759	8000.391420	12.954394	-0.091356	4.818099
464.248616	8000.400343	12.959399	-0.091321	4.818103
464.232210	8000.383270	12.964403	-0.091318	4.818098
464.495311	8000.419609	12.969408	-0.091367	4.818108
464.381233	8000.359051	12.974413	-0.091346	4.818090
464.425446	8000.313352	12.979418	-0.091354	4.818076
464.199949	8000.394407	12.984423	-0.091312	4.818101
464.250413	8000.374063	12.989427	-0.091322	4.818095
464.398955	8000.430900	12.994432	-0.091350	4.818111
464.630933	8000.377313	12.999437	-0.091393	4.818094
464.525726	8000.402156	13.004442	-0.091373	4.818102
464.278967	8000.405005	13.009447	-0.091327	4.818104
464.419134	8000.324860	13.014451	-0.091353	4.818080
464.376414	8000.415855	13.019456	-0.091345	4.818107
464.126524	8000.370232	13.024461	-0.091299	4.818094
464.163688	8000.422344	13.029466	-0.091306	4.818110
464.516522	8000.405199	13.034471	-0.091372	4.818103
464.608685	8000.342277	13.039475	-0.091389	4.818084
464.573014	8000.335461	13.044480	-0.091382	4.818082
464.507592	8000.280851	13.049485	-0.091370	4.818066
464.509765	8000.345104	13.054490	-0.091370	4.818085
464.320526	8000.396138	13.059495	-0.091335	4.818101
464.103972	8000.392043	13.064499	-0.091295	4.818101
464.023039	8000.427755	13.069504	-0.091280	4.818112
464.372239	8000.415823	13.074509	-0.091345	4.818107
464.036957	8000.485859	13.079514	-0.091283	4.818129
464.360303	8000.435663	13.084519	-0.091343	4.818113
464.783395	8000.300540	13.089523	-0.091422	4.818071
464.696880	8000.388814	13.094528	-0.091406	4.818098
464.417700	8000.373309	13.099533	-0.091354	4.818094
464.242062	8000.430851	13.104538	-0.091321	4.818112
464.284585	8000.418818	13.109543	-0.091329	4.818108
464.495170	8000.354403	13.114547	-0.091368	4.818088
464.521208	8000.411623	13.119552	-0.091373	4.818105
464.314685	8000.356081	13.124557	-0.091335	4.818089
464.462762	8000.381327	13.129562	-0.091362	4.818096
464.826592	8000.321172	13.134567	-0.091430	4.818077
464.790972	8000.344888	13.139571	-0.091423	4.818084
464.794279	8000.354412	13.144576	-0.091424	4.818087
464.862748	8000.339586	13.149581	-0.091437	4.818082
464.765135	8000.380327	13.154586	-0.091419	4.818095
464.653977	8000.398770	13.159591	-0.091398	4.818101
464.681328	8000.320196	13.164595	-0.091403	4.818077
464.917625	8000.335103	13.169600	-0.091447	4.818081
464.909629	8000.265508	13.174605	-0.091446	4.818060
464.858733	8000.312170	13.179610	-0.091436	4.818074
465.060948	8000.333967	13.184615	-0.091474	4.818080
464.851533	8000.311021	13.189619	-0.091435	4.818074
464.663652	8000.333649	13.194624	-0.091400	4.818081
464.678487	8000.298064	13.199629	-0.091403	4.818071
464.767468	8000.336166	13.204634	-0.091419	4.818082
464.529736	8000.334931	13.209639	-0.091375	4.818082
464.319467	8000.361455	13.214643	-0.091336	4.818091
464.578187	8000.421947	13.219648	-0.091384	4.818108
464.363943	8000.431570	13.224653	-0.091344	4.818112
464.217441	8000.443199	13.229658	-0.091317	4.818116
464.231677	8000.399184	13.234663	-0.091320	4.818103
464.607394	8000.356041	13.239667	-0.091390	4.818088
464.281341	8000.424101	13.244672	-0.091329	4.818110
463.963449	8000.405947	13.249677	-0.091270	4.818106
463.970463	8000.449213	13.254682	-0.091271	4.818118
464.160893	8000.409781	13.259687	-0.091307	4.818106
464.285126	8000.360996	13.264691	-0.091330	4.818091
464.562637	8000.412277	13.269696	-0.091382	4.818105
464.117848	8000.436556	13.274701	-0.091299	4.818114
464.251604	8000.421594	13.279706	-0.091324	4.818109
464.171596	8000.327826	13.284711	-0.091309	4.818082
464.221349	8000.390642	13.289715	-0.091318	4.818100
463.916078	8000.464259	13.294720	-0.091262	4.818123
464.321699	8000.380477	13.299725	-0.091337	4.818097
464.070661	8000.408534	13.304730	-0.091290	4.818106
464.339444	8000.393365	13.309735	-0.091340	4.818100
464.135382	8000.397868	13.314739	-0.091302	4.818103
464.254949	8000.424819	13.319744	-0.091325	4.818110
464.413389	8000.378620	13.324749	-0.091354	4.818096
463.924092	8000.484392	13.329754	-0.091263	4.818129
464.226246	8000.456006	13.334759	-0.091320	4.818119
463.963708	8000.371252	13.339763	-0.091271	4.818095
463.846295	8000.500149	13.344768	-0.091249	4.818134
463.935167	8000.464554	13.349773	-0.091265	4.818123
464.299543	8000.383351	13.354778	-0.091333	4.818098
464.407593	8000.392242	13.359783	-0.091353	4.818100
464.979104	8000.292896	13.364787	-0.091460	4.818068
464.214501	8000.432696	13.369792	-0.091318	4.818113
464.162841	8000.398283	13.374797	-0.091308	4.818103
463.792057	8000.446764	13.379802	-0.091239	4.818118
464.138774	8000.455853	13.384807	-0.091304	4.818120
464.248690	8000.365808	13.389811	-0.091324	4.818093
464.528675	8000.428704	13.394816	-0.091376	4.818110
464.055558	8000.417842	13.399821	-0.091288	4.818109
464.478411	8000.425896	13.404826	-0.091367	4.818109
463.874200	8000.474253	13.409831	-0.091254	4.818126
464.204248	8000.425204	13.414835	-0.091316	4.818110
464.848013	8000.431102	13.419840	-0.091436	4.818109
464.594911	8000.374904	13.424845	-0.091389	4.818094
464.295891	8000.399127	13.429850	-0.091333	4.818102
464.314279	8000.456239	13.434855	-0.091337	4.818119
464.432507	8000.356835	13.439859	-0.091359	4.818089
464.079152	8000.425565	13.444864	-0.091293	4.818111
464.455856	8000.355063	13.449869	-0.091363	4.818088
464.397093	8000.254224	13.454874	-0.091352	4.818059
465.048631	8000.404464	13.459879	-0.091473	4.818101
464.286041	8000.388477	13.464883	-0.091331	4.818099
464.249712	8000.464823	13.469888	-0.091325	4.818122
463.917583	8000.442258	13.474893	-0.091263	4.818117
464.188597	8000.433437	13.479898	-0.091313	4.818113
464.364433	8000.431701	13.484903	-0.091346	4.818112
464.157098	8000.443527	13.489907	-0.091308	4.818116
464.380160	8000.437191	13.494912	-0.091349	4.818113
464.305303	8000.383501	13.499917	-0.091335	4.818098
464.572441	8000.389365	13.504922	-0.091385	4.818098
464.713506	8000.381877	13.509927	-0.091411	4.818095
464.527951	8000.323471	13.514931	-0.091377	4.818079
464.775238	8000.386961	13.519936	-0.091423	4.818097
464.728499	8000.338930	13.524941	-0.091414	4.818083
464.536864	8000.430989	13.529946	-0.091379	4.818111
464.621684	8000.430079	13.534951	-0.091394	4.818110
464.335039	8000.436578	13.539955	-0.091341	4.818113
464.279282	8000.494753	13.544960	-0.091331	4.818131
464.583587	8000.315848	13.549965	-0.091387	4.818076
464.559943	8000.300778	13.554970	-0.091383	4.818072
464.509668	8000.394826	13.559975	-0.091374	4.818100
464.723009	8000.366244	13.564979	-0.091413	4.818091
464.355444	8000.423193	13.569984	-0.091345	4.818109
464.425051	8000.412593	13.574989	-0.091358	4.818106
464.754456	8000.367747	13.579994	-0.091419	4.818091
464.815173	8000.322279	13.584999	-0.091431	4.818077
464.692858	8000.264763	13.590003	-0.091408	4.818061
464.881832	8000.356912	13.595008	-0.091443	4.818087
464.806315	8000.342165	13.600013	-0.091429	4.818083
464.677203	8000.340352	13.605018	-0.091405	4.818083
464.507462	8000.314806	13.610023	-0.091374	4.818076
463.879014	8000.476524	13.615027	-0.091257	4.818127
464.307720	8000.474133	13.620032	-0.091337	4.818124
464.296372	8000.419230	13.625037	-0.091334	4.818108
463.975491	8000.431565	13.630042	-0.091275	4.818113
463.931716	8000.464641	13.635047	-0.091267	4.818123
463.846159	8000.459230	13.640051	-0.091251	4.818122
464.571349	8000.434688	13.645056	-0.091386	4.818112
464.249532	8000.430164	13.650061	-0.091326	4.818112
463.725431	8000.390161	13.655066	-0.091228	4.818102
464.297837	8000.439271	13.660071	-0.091335	4.818114
464.710935	8000.345066	13.665075	-0.091412	4.818084
464.426206	8000.432658	13.670080	-0.091359	4.818112
464.214196	8000.432838	13.675085	-0.091319	4.818113
464.600406	8000.370892	13.680090	-0.091391	4.818093
464.543499	8000.323771	13.685095	-0.091381	4.818079
464.327203	8000.380741	13.690099	-0.091341	4.818097
464.588265	8000.430738	13.695104	-0.091389	4.818110
464.406531	8000.373439	13.700109	-0.091355	4.818094
464.603647	8000.295148	13.705114	-0.091392	4.818070
464.802859	8000.366384	13.710119	-0.091429	4.818090
464.958136	8000.325405	13.715123	-0.091458	4.818078
464.554289	8000.403952	13.720128	-0.091383	4.818103
464.515640	8000.334979	13.725133	-0.091376	4.818082
465.028873	8000.284295	13.730138	-0.091471	4.818065
465.118727	8000.282402	13.735143	-0.091488	4.818064
464.971857	8000.279286	13.740147	-0.091461	4.818064
464.943308	8000.408383	13.745152	-0.091456	4.818102
464.674097	8000.388807	13.750157	-0.091406	4.818098
464.609754	8000.430016	13.755162	-0.091394	4.818110
464.898119	8000.374064	13.760167	-0.091447	4.818092
464.926190	8000.374462	13.765171	-0.091453	4.818092
465.286587	8000.352160	13.770176	-0.091520	4.818084
464.902311	8000.318332	13.775181	-0.091448	4.818076
465.297245	8000.263879	13.780186	-0.091522	4.818058
465.192253	8000.391900	13.785191	-0.091502	4.818096
464.841830	8000.356442	13.790195	-0.091437	4.818087
464.831898	8000.391048	13.795200	-0.091435	4.818098
464.957075	8000.342276	13.800205	-0.091458	4.818083
465.006501	8000.364029	13.805210	-0.091468	4.818089
465.063082	8000.377462	13.810215	-0.091478	4.818093
465.037433	8000.306565	13.815219	-0.091474	4.818072
464.829952	8000.389979	13.820224	-0.091435	4.818097
464.709223	8000.373544	13.825229	-0.091413	4.818093
464.721887	8000.404256	13.830234	-0.091415	4.818102
464.814385	8000.425563	13.835239	-0.091432	4.818108
464.642013	8000.403138	13.840243	-0.091400	4.818102
464.893141	8000.342451	13.845248	-0.091447	4.818083
465.104862	8000.312794	13.850253	-0.091486	4.818073
464.204920	8000.422265	13.855258	-0.091319	4.818109
464.370734	8000.424599	13.860263	-0.091350	4.818109
464.805888	8000.286487	13.865267	-0.091431	4.818067
464.517711	8000.341394	13.870272	-0.091377	4.818084
464.887504	8000.299221	13.875277	-0.091446	4.818070
465.079848	8000.281925	13.880282	-0.091482	4.818064
465.123114	8000.372025	13.885287	-0.091490	4.818091
464.628175	8000.353485	13.890291	-0.091398	4.818087
464.541374	8000.403854	13.895296	-0.091382	4.818103
465.063627	8000.365931	13.900301	-0.091479	4.818089
464.990749	8000.300687	13.905306	-0.091465	4.818070
464.939909	8000.346298	13.910311	-0.091456	4.818084
464.785468	8000.395716	13.915315	-0.091427	4.818099
464.796209	8000.436929	13.920320	-0.091429	4.818111
464.950106	8000.341185	13.925325	-0.091458	4.818082
464.808509	8000.328667	13.930330	-0.091432	4.818079
464.950757	8000.387522	13.935335	-0.091458	4.818096
464.734277	8000.377110	13.940339	-0.091418	4.818094
465.071424	8000.366062	13.945344	-0.091481	4.818089
465.035695	8000.330819	13.950349	-0.091474	4.818079
465.056946	8000.318487	13.955354	-0.091478	4.818075
465.048624	8000.372066	13.960359	-0.091477	4.818091
465.102645	8000.233857	13.965363	-0.091487	4.818050
464.713697	8000.382099	13.970368	-0.091414	4.818095
464.358342	8000.423427	13.975373	-0.091348	4.818109
464.235365	8000.435387	13.980378	-0.091325	4.818113
464.667558	8000.424622	13.985383	-0.091406	4.818108
464.615337	8000.400729	13.990387	-0.091396	4.818101
464.579713	8000.440237	13.995392	-0.091390	4.818113
464.518801	8000.399376	14.000397	-0.091378	4.818101
464.936659	8000.367354	14.005402	-0.091456	4.818090
464.792030	8000.412699	14.010407	-0.091429	4.818104
464.504623	8000.382339	14.015411	-0.091376	4.818096
464.632464	8000.395720	14.020416	-0.091399	4.818100
464.296971	8000.436274	14.025421	-0.091337	4.818113
464.622197	8000.357679	14.030426	-0.091398	4.818088
464.429173	8000.442350	14.035431	-0.091362	4.818114
464.201680	8000.434942	14.040435	-0.091319	4.818113
464.337791	8000.375796	14.045440	-0.091345	4.818095
464.747694	8000.371035	14.050445	-0.091421	4.818092
464.312688	8000.444932	14.055450	-0.091340	4.818116
464.076573	8000.460565	14.060455	-0.091296	4.818121
464.693551	8000.350277	14.065459	-0.091411	4.818086
464.876413	8000.437076	14.070464	-0.091445	4.818111
464.637765	8000.397926	14.075469	-0.091401	4.818100
464.506855	8000.416091	14.080474	-0.091376	4.818106
464.648199	8000.448613	14.085479	-0.091403	4.818115
464.293528	8000.459419	14.090483	-0.091337	4.818120
464.027464	8000.498844	14.095488	-0.091287	4.818133
464.183082	8000.450501	14.100493	-0.091316	4.818118
464.656384	8000.430839	14.105498	-0.091404	4.818110
464.655677	8000.449782	14.110503	-0.091404	4.818116
464.329404	8000.415718	14.115507	-0.091344	4.818107
463.638931	8000.334423	14.120512	-0.091215	4.818086
463.237645	8000.504598	14.125517	-0.091141	4.818138
464.011830	8000.389151	14.130522	-0.091285	4.818100
463.831618	8000.496109	14.135527	-0.091251	4.818133
463.992609	8000.499428	14.140531	-0.091281	4.818133
464.258624	8000.376836	14.145536	-0.091331	4.818096
464.165709	8000.452386	14.150541	-0.091313	4.818118
464.313886	8000.463947	14.155546	-0.091341	4.818121
463.849782	8000.467951	14.160551	-0.091255	4.818124
463.862056	8000.400748	14.165555	-0.091257	4.818104
464.398503	8000.424085	14.170560	-0.091357	4.818109
464.508020	8000.418258	14.175565	-0.091377	4.818107
464.300896	8000.459565	14.180570	-0.091339	4.818120
464.336485	8000.452699	14.185575	-0.091345	4.818118
464.366137	8000.435220	14.190579	-0.091351	4.818113
464.524659	8000.455350	14.195584	-0.091381	4.818118
464.599435	8000.390077	14.200589	-0.091394	4.818098
464.794280	8000.331757	14.205594	-0.091431	4.818080
464.937774	8000.393788	14.210599	-0.091458	4.818098
464.956410	8000.320356	14.215603	-0.091461	4.818076
464.812686	8000.436251	14.220608	-0.091434	4.818111
464.756552	8000.437570	14.225613	-0.091424	4.818112
464.544677	8000.444067	14.230618	-0.091384	4.818114
464.876403	8000.424521	14.235623	-0.091446	4.818107
464.366472	8000.407876	14.240627	-0.091351	4.818104
464.961487	8000.404666	14.245632	-0.091462	4.818101
464.608688	8000.434449	14.250637	-0.091397	4.818111
464.477530	8000.448399	14.255642	-0.091372	4.818116
464.716592	8000.451764	14.260647	-0.091417	4.818116
464.511264	8000.414136	14.265651	-0.091378	4.818106
464.543524	8000.459862	14.270656	-0.091385	4.818119
464.826558	8000.444895	14.275661	-0.091437	4.818113
464.772842	8000.384132	14.280666	-0.091427	4.818096
464.723450	8000.420288	14.285671	-0.091418	4.818107
464.338925	8000.427516	14.290675	-0.091347	4.818110
464.429119	8000.403519	14.295680	-0.091363	4.818103
465.148730	8000.386270	14.300685	-0.091497	4.818095
465.141367	8000.315630	14.305690	-0.091496	4.818074
465.069780	8000.390429	14.310695	-0.091483	4.818096
464.573072	8000.383445	14.315699	-0.091390	4.818096
464.772534	8000.443104	14.320704	-0.091427	4.818113
464.894031	8000.382700	14.325709	-0.091450	4.818095
464.797724	8000.349763	14.330714	-0.091432	4.818085
465.068572	8000.403057	14.335719	-0.091483	4.818100
464.763458	8000.401926	14.340723	-0.091426	4.818101
464.426438	8000.459304	14.345728	-0.091363	4.818119
465.149734	8000.407365	14.350733	-0.091498	4.818101
465.300617	8000.289468	14.355738	-0.091526	4.818065
465.362319	8000.336663	14.360743	-0.091537	4.818079
464.936907	8000.379110	14.365747	-0.091458	4.818093
465.286331	8000.348232	14.370752	-0.091523	4.818083
465.420789	8000.312225	14.375757	-0.091548	4.818072
465.022614	7999.339123	14.380762	-0.091474	4.817785

465.031188	7996.257096	14.385767	-0.091473	4.816871
465.249636	7990.607878	14.390771	-0.091510	4.815194
465.315175	7984.049734	14.395776	-0.091518	4.813247
465.045739	7976.759046	14.400781	-0.091463	4.811084
464.909098	7969.087868	14.405786	-0.091433	4.808806
464.974389	7961.417782	14.410791	-0.091440	4.806526
464.854771	7953.433996	14.415795	-0.091413	4.804152
465.049549	7945.565237	14.420800	-0.091444	4.801811
464.901552	7937.560665	14.425805	-0.091411	4.799429
464.653713	7929.593489	14.430810	-0.091360	4.797058
465.051283	7921.510384	14.435815	-0.091429	4.794648
464.814453	7913.556600	14.440819	-0.091379	4.792278
465.126326	7905.526436	14.445824	-0.091432	4.789882
464.888063	7897.562855	14.450829	-0.091383	4.787507
464.796992	7889.506715	14.455834	-0.091361	4.785103
465.006810	7881.562540	14.460839	-0.091395	4.782729
464.783912	7873.565254	14.465843	-0.091348	4.780340
464.751043	7865.572022	14.470848	-0.091337	4.777951
464.828033	7857.508845	14.475853	-0.091346	4.775539
464.957413	7849.477383	14.480858	-0.091365	4.773135
464.863588	7841.564399	14.485863	-0.091342	4.770766
464.879409	7833.462692	14.490867	-0.091340	4.768339
464.852292	7825.487574	14.495872	-0.091329	4.765949
464.682505	7817.510938	14.500877	-0.091293	4.763557
464.436267	7809.535579	14.505882	-0.091242	4.761165
464.299751	7801.559106	14.510887	-0.091211	4.758771
463.790561	7793.620750	14.515891	-0.091111	4.756388
464.368496	7785.458328	14.520896	-0.091213	4.753934
464.572789	7777.520926	14.525901	-0.091246	4.751547
464.084018	7769.467429	14.530906	-0.091150	4.749126
464.151170	7761.490248	14.535911	-0.091157	4.746725
464.489940	7753.410435	14.540915	-0.091215	4.744292
464.146265	7745.518871	14.545920	-0.091146	4.741915
464.312052	7737.444776	14.550925	-0.091172	4.739481
464.196110	7729.428553	14.555930	-0.091145	4.737064
464.227139	7721.487895	14.560935	-0.091146	4.734669
463.955535	7713.513946	14.565939	-0.091090	4.732262
464.348351	7705.426812	14.570944	-0.091158	4.729819
464.166955	7697.488596	14.575949	-0.091119	4.727421
463.491792	7689.469707	14.580954	-0.090988	4.724998
463.655765	7681.539963	14.585959	-0.091013	4.722599
463.309472	7673.483180	14.590963	-0.090944	4.720161
463.925315	7665.433323	14.595968	-0.091053	4.717722
463.881095	7657.419666	14.600973	-0.091040	4.715295
463.608602	7649.460380	14.605978	-0.090984	4.712883
463.816306	7641.491389	14.610983	-0.091017	4.710466
463.855606	7633.462798	14.615987	-0.091019	4.708029
463.807726	7625.447175	14.620992	-0.091005	4.705596
463.835080	7617.448417	14.625997	-0.091005	4.703167
463.809150	7609.493601	14.631002	-0.090995	4.700749
463.808378	7601.461909	14.636007	-0.090990	4.698307
463.784422	7593.496890	14.641011	-0.090980	4.695884
464.007573	7585.455978	14.646016	-0.091017	4.693437
463.865487	7577.469037	14.651021	-0.090985	4.691005
463.562333	7569.437573	14.656026	-0.090923	4.688558
463.685144	7561.486627	14.661031	-0.090941	4.686134
463.884968	7553.358873	14.666035	-0.090973	4.683655
463.764588	7545.517698	14.671040	-0.090946	4.681262
463.511657	7537.463488	14.676045	-0.090893	4.678803
463.476848	7529.530673	14.681050	-0.090882	4.676380
463.220924	7521.493202	14.686055	-0.090829	4.673923
463.596427	7513.352280	14.691059	-0.090893	4.671434
463.945554	7505.352201	14.696064	-0.090953	4.668986
464.022994	7497.414820	14.701069	-0.090963	4.666556
463.781804	7489.344465	14.706074	-0.090912	4.664084
463.740030	7481.470264	14.711079	-0.090899	4.661671
463.638720	7473.390386	14.716083	-0.090875	4.659194
463.490071	7465.467415	14.721088	-0.090843	4.656763
463.428881	7457.436866	14.726093	-0.090826	4.654299
463.436971	7449.492977	14.731098	-0.090822	4.651859
463.200891	7441.444444	14.736103	-0.090773	4.649386
463.164188	7433.438936	14.741107	-0.090761	4.646925
463.102746	7425.375790	14.746112	-0.090744	4.644445
462.956630	7417.492444	14.751117	-0.090712	4.642019
462.801798	7409.404475	14.756122	-0.090678	4.639528
462.621244	7401.495182	14.761127	-0.090639	4.637092
462.592625	7393.455354	14.766131	-0.090629	4.634613
462.564314	7385.447171	14.771136	-0.090618	4.632144
462.865620	7377.382244	14.776141	-0.090669	4.629655
462.793882	7369.371543	14.781146	-0.090651	4.627182
462.797476	7361.349898	14.786151	-0.090646	4.624704
462.860508	7353.412241	14.791155	-0.090653	4.622251
462.699275	7345.416613	14.796160	-0.090618	4.619778
462.579319	7337.454507	14.801165	-0.090590	4.617314
463.072187	7329.299756	14.806170	-0.090677	4.614790
462.819819	7321.398963	14.811175	-0.090624	4.612343
462.185982	7313.399725	14.816179	-0.090501	4.609863
462.553417	7305.408290	14.821184	-0.090565	4.607386
461.801866	7297.462590	14.826189	-0.090419	4.604920
462.378975	7289.386505	14.831194	-0.090522	4.602414
462.836420	7281.367266	14.836199	-0.090602	4.599924
462.773098	7273.362092	14.841203	-0.090585	4.597436
462.529234	7265.366982	14.846208	-0.090534	4.594950
462.636467	7257.345817	14.851213	-0.090549	4.592455
462.494475	7249.332018	14.856218	-0.090517	4.589960
462.558847	7241.400919	14.861223	-0.090524	4.587490
462.551334	7233.289089	14.866227	-0.090517	4.584963
462.465378	7225.373330	14.871232	-0.090496	4.582495
462.634158	7217.327544	14.876237	-0.090522	4.579985
462.710713	7209.358586	14.881242	-0.090532	4.577499
462.577673	7201.362067	14.886247	-0.090502	4.575001
462.420054	7193.352128	14.891251	-0.090467	4.572498
462.545723	7185.333049	14.896256	-0.090485	4.569992
462.501999	7177.327311	14.901261	-0.090472	4.567487
462.296417	7169.308026	14.906266	-0.090428	4.564977
462.863122	7161.360154	14.911271	-0.090529	4.562490
462.594492	7153.315219	14.916275	-0.090474	4.559969
462.365627	7145.406008	14.921280	-0.090426	4.557489
462.355531	7137.298685	14.926285	-0.090419	4.554946
462.099852	7129.311015	14.931290	-0.090366	4.552439
462.376912	7121.302121	14.936295	-0.090412	4.549925
462.449115	7113.304047	14.941299	-0.090421	4.547412
462.387806	7105.292528	14.946304	-0.090404	4.544894
462.462763	7097.331055	14.951309	-0.090413	4.542390
462.470361	7089.288205	14.956314	-0.090409	4.539859
462.272968	7081.399227	14.961319	-0.090367	4.537374
461.794152	7073.301052	14.966323	-0.090273	4.534822
462.128458	7065.283802	14.971328	-0.090330	4.532295
462.280483	7057.264587	14.976333	-0.090353	4.529767
461.937110	7049.286896	14.981338	-0.090284	4.527248
462.115320	7041.271430	14.986343	-0.090312	4.524718
461.948057	7033.307097	14.991347	-0.090276	4.522201
462.228021	7025.276833	14.996352	-0.090322	4.519663
462.054747	7017.338300	15.001357	-0.090285	4.517152
461.834880	7009.268619	15.006362	-0.090239	4.514598
461.681893	7001.387246	15.011367	-0.090205	4.512102
461.318270	6993.296737	15.016371	-0.090132	4.509537
461.874634	6985.264285	15.021376	-0.090231	4.506993
461.724044	6977.222108	15.026381	-0.090197	4.504441
461.766685	6969.271937	15.031386	-0.090200	4.501919
462.073898	6961.225958	15.036391	-0.090252	4.499365
461.635678	6953.250839	15.041395	-0.090166	4.496829
461.839571	6945.218019	15.046400	-0.090198	4.494277
461.965875	6937.286762	15.051405	-0.090217	4.491754
461.230176	6929.258387	15.056410	-0.090074	4.489196
461.000292	6921.311094	15.061415	-0.090027	4.486665
461.389710	6913.176609	15.066419	-0.090094	4.484074
461.346979	6905.306619	15.071424	-0.090081	4.481565
461.065910	6897.237632	15.076429	-0.090023	4.478990
461.342788	6889.235646	15.081434	-0.090070	4.476437
461.280659	6881.174144	15.086439	-0.090053	4.473863
461.400691	6873.208668	15.091443	-0.090070	4.471318
461.339919	6865.238407	15.096448	-0.090053	4.468769
461.484510	6857.247480	15.101453	-0.090075	4.466214
461.482922	6849.134391	15.106458	-0.090070	4.463617
461.489397	6841.262728	15.111463	-0.090066	4.461096
461.612366	6833.176666	15.116467	-0.090083	4.458505
461.639100	6825.220274	15.121472	-0.090083	4.455954
461.425767	6817.199957	15.126477	-0.090038	4.453380
461.605210	6809.176604	15.131482	-0.090067	4.450805
461.551074	6801.151620	15.136487	-0.090051	4.448228
461.560218	6793.176000	15.141491	-0.090048	4.445664
461.449321	6785.185480	15.146496	-0.090022	4.443094
461.546545	6777.254591	15.151501	-0.090035	4.440543
461.263768	6769.194627	15.156506	-0.089977	4.437947
461.290347	6761.192688	15.161511	-0.089977	4.435369
461.355816	6753.142479	15.166515	-0.089984	4.432775
461.427788	6745.165570	15.171520	-0.089992	4.430203
461.257377	6737.187617	15.176525	-0.089955	4.427627
461.057983	6729.092106	15.181530	-0.089913	4.425012
461.470489	6721.172711	15.186535	-0.089984	4.422456
461.105495	6713.174523	15.191539	-0.089911	4.419869
461.014927	6705.214044	15.196544	-0.089889	4.417293
461.321512	6697.152922	15.201549	-0.089941	4.414686
461.245702	6689.137924	15.206554	-0.089922	4.412090
461.323087	6681.111451	15.211559	-0.089931	4.409490
460.797734	6673.135267	15.216563	-0.089828	4.406901
461.286015	6665.093471	15.221568	-0.089914	4.404295
460.854314	6657.231926	15.226573	-0.089828	4.401740
460.902114	6649.095167	15.231578	-0.089832	4.399098
460.986973	6641.223809	15.236583	-0.089843	4.396540
460.874006	6633.165937	15.241587	-0.089816	4.393919
460.926079	6625.200873	15.246592	-0.089821	4.391328
460.883627	6617.205908	15.251597	-0.089808	4.388725
460.956333	6609.154044	15.256602	-0.089816	4.386103
460.550753	6601.224677	15.261607	-0.089735	4.383515
460.761001	6593.187327	15.266611	-0.089769	4.380895
460.845340	6585.180213	15.271616	-0.089780	4.378283
460.922349	6577.171311	15.276621	-0.089789	4.375668
460.678501	6569.171885	15.281626	-0.089738	4.373053
460.769469	6561.246749	15.286631	-0.089750	4.370463
460.456043	6553.230789	15.291635	-0.089687	4.367838
460.554836	6545.240591	15.296640	-0.089700	4.365224
459.898733	6537.330398	15.301645	-0.089573	4.362628
459.739229	6529.304929	15.306650	-0.089538	4.359997
460.221050	6521.267537	15.311655	-0.089622	4.357365
460.075227	6513.210575	15.316659	-0.089590	4.354720
460.138030	6505.278478	15.321664	-0.089596	4.352116
460.139595	6497.192870	15.326669	-0.089592	4.349460
460.030695	6489.170723	15.331674	-0.089566	4.346822
459.911140	6481.213521	15.336679	-0.089539	4.344204
460.176134	6473.223888	15.341683	-0.089583	4.341577
460.112114	6465.193540	15.346688	-0.089566	4.338932
460.029677	6457.245274	15.351693	-0.089545	4.336312
459.947070	6449.226128	15.356698	-0.089525	4.333668
460.001266	6441.237997	15.361703	-0.089530	4.331033
460.048404	6433.185864	15.366707	-0.089533	4.328375
460.339047	6425.173419	15.371712	-0.089582	4.325731
460.042398	6417.244263	15.376717	-0.089522	4.323107
459.934382	6409.238980	15.381722	-0.089496	4.320459
460.081133	6401.244621	15.386727	-0.089518	4.317815
460.248333	6393.231036	15.391731	-0.089544	4.315163
460.050080	6385.243736	15.396736	-0.089502	4.312514
460.059023	6377.250541	15.401741	-0.089499	4.309865
460.351380	6369.182600	15.406746	-0.089548	4.307191
460.188299	6361.146300	15.411751	-0.089512	4.304522
459.841675	6353.243839	15.416755	-0.089443	4.301894
459.961069	6345.176443	15.421760	-0.089460	4.299213
460.201281	6337.200958	15.426765	-0.089499	4.296563
459.766845	6329.162806	15.431770	-0.089413	4.293885
460.022439	6321.178949	15.436775	-0.089456	4.291228
460.039848	6313.132332	15.441779	-0.089454	4.288547
460.128342	6305.150611	15.446784	-0.089465	4.285887
460.029135	6297.188285	15.451789	-0.089441	4.283230
459.976762	6289.213769	15.456794	-0.089426	4.280568
460.001647	6281.246781	15.461799	-0.089426	4.277907
460.007247	6273.205910	15.466803	-0.089422	4.275219
459.911166	6265.203745	15.471808	-0.089399	4.272542
459.920674	6257.213924	15.476813	-0.089395	4.269869
459.670034	6249.178711	15.481818	-0.089343	4.267175
459.589634	6241.157786	15.486823	-0.089323	4.264487
459.802019	6233.183796	15.491827	-0.089358	4.261816
459.699147	6225.115953	15.496832	-0.089333	4.259108
459.909992	6217.207762	15.501837	-0.089367	4.256455
459.843534	6209.170413	15.506842	-0.089350	4.253755
459.649889	6201.198603	15.511847	-0.089309	4.251073
459.727179	6193.124559	15.516851	-0.089318	4.248358
459.731207	6185.113486	15.521856	-0.089313	4.245662
459.558535	6177.242579	15.526861	-0.089276	4.243010
459.678410	6169.172376	15.531866	-0.089293	4.240291
459.703042	6161.202772	15.536871	-0.089293	4.237604
459.464888	6153.223170	15.541875	-0.089243	4.234909
459.108056	6145.243177	15.546880	-0.089171	4.232211
459.664232	6137.144870	15.551885	-0.089270	4.229481
459.349013	6129.161941	15.556890	-0.089206	4.226779
459.495849	6121.113419	15.561895	-0.089228	4.224058
458.898272	6113.263273	15.566899	-0.089112	4.221394
459.046222	6105.180792	15.571904	-0.089134	4.218658
459.026686	6097.180698	15.576909	-0.089125	4.215946
458.947616	6089.138917	15.581914	-0.089105	4.213218
458.870761	6081.167606	15.586919	-0.089086	4.210512
458.901231	6073.162111	15.591923	-0.089086	4.207793
458.724534	6065.123589	15.596928	-0.089048	4.205060
458.870855	6057.207275	15.601933	-0.089070	4.202370
458.856631	6049.156392	15.606938	-0.089062	4.199630
458.730573	6041.230929	15.611943	-0.089034	4.196930
458.202852	6033.183066	15.616947	-0.088930	4.194182
458.090631	6025.136715	15.621952	-0.088904	4.191438
458.367532	6017.128187	15.626957	-0.088951	4.188709
458.265602	6009.075569	15.631962	-0.088926	4.185958
458.367900	6001.117196	15.636967	-0.088940	4.183241
458.563667	5993.100464	15.641971	-0.088972	4.180503
458.461714	5985.129383	15.646976	-0.088947	4.177775
458.261229	5977.136003	15.651981	-0.088905	4.175037
458.063224	5969.182497	15.656986	-0.088863	4.172311
457.975595	5961.175734	15.661991	-0.088841	4.169565
457.613709	5953.217718	15.666995	-0.088769	4.166832
458.200274	5945.044716	15.672000	-0.088873	4.164034
458.401263	5937.138043	15.677005	-0.088905	4.161321
458.266350	5929.137791	15.682010	-0.088875	4.158571
458.131934	5921.190074	15.687015	-0.088845	4.155836
458.336969	5913.145449	15.692019	-0.088878	4.153071
457.877570	5905.173120	15.697024	-0.088787	4.150320
457.952385	5897.177483	15.702029	-0.088796	4.147566
458.119224	5889.072375	15.707034	-0.088821	4.144774
458.136713	5881.182684	15.712039	-0.088820	4.142052
458.058096	5873.176125	15.717043	-0.088800	4.139287
457.714702	5865.219272	15.722048	-0.088731	4.136533
458.151595	5857.158842	15.727053	-0.088807	4.133753
457.729157	5849.210382	15.732058	-0.088723	4.130997
458.126102	5841.126036	15.737063	-0.088792	4.128204
458.016063	5833.144903	15.742067	-0.088766	4.125438
458.118026	5825.177182	15.747072	-0.088780	4.122678
457.874627	5817.274076	15.752077	-0.088729	4.119933
457.727365	5809.208940	15.757082	-0.088697	4.117132
457.881996	5801.178843	15.762087	-0.088720	4.114345
457.562141	5793.248278	15.767091	-0.088656	4.111584
457.514927	5785.176873	15.772096	-0.088642	4.108776
457.917161	5777.168428	15.777101	-0.088711	4.105994
457.431177	5769.201710	15.782106	-0.088616	4.103213
457.448918	5761.180039	15.787111	-0.088614	4.100417
457.437570	5753.190966	15.792115	-0.088606	4.097631
457.684979	5745.150326	15.797120	-0.088647	4.094828
457.691427	5737.151740	15.802125	-0.088643	4.092035
457.404130	5729.155485	15.807130	-0.088585	4.089237
457.752904	5721.166288	15.812135	-0.088644	4.086448
457.745541	5713.146316	15.817139	-0.088638	4.083641
457.247248	5705.223582	15.822144	-0.088540	4.080859
457.625432	5697.170096	15.827149	-0.088605	4.078043
457.592484	5689.184671	15.832154	-0.088594	4.075242
457.343532	5681.220980	15.837159	-0.088542	4.072444
457.578741	5673.148156	15.842163	-0.088581	4.069612
457.133619	5665.213723	15.847168	-0.088493	4.066818
457.349053	5657.191908	15.852173	-0.088528	4.064000
457.259819	5649.194867	15.857178	-0.088506	4.061184
457.077774	5641.217169	15.862183	-0.088467	4.058372
456.889034	5633.221460	15.867187	-0.088427	4.055552
456.853013	5625.185810	15.872192	-0.088415	4.052718
457.015545	5617.173655	15.877197	-0.088440	4.049893
456.842436	5609.172931	15.882202	-0.088402	4.047065
456.790517	5601.173417	15.887207	-0.088388	4.044238
456.747813	5593.235602	15.892211	-0.088374	4.041430
456.663730	5585.203745	15.897216	-0.088354	4.038586
456.771941	5577.247432	15.902221	-0.088369	4.035771
456.873650	5569.142801	15.907226	-0.088382	4.032900
456.602136	5561.188341	15.912231	-0.088327	4.030075
456.184903	5553.234744	15.917235	-0.088244	4.027246
456.138696	5545.160195	15.922240	-0.088230	4.024378
456.130522	5537.252159	15.927245	-0.088223	4.021568
456.077906	5529.197244	15.932250	-0.088208	4.018702
456.297783	5521.208342	15.937255	-0.088244	4.015863
455.671908	5513.239581	15.942259	-0.088122	4.013014
456.166553	5505.145895	15.947264	-0.088209	4.010138
456.362084	5497.196902	15.952269	-0.088240	4.007307
456.290686	5489.163639	15.957274	-0.088222	4.004438
456.534986	5481.233177	15.962279	-0.088262	4.001610
456.992051	5473.127901	15.967283	-0.088342	3.998721
456.177354	5465.289285	15.972288	-0.088185	3.995904
456.329011	5457.240512	15.977293	-0.088208	3.993026
456.553962	5449.164356	15.982298	-0.088245	3.990137
456.447353	5441.236126	15.987303	-0.088220	3.987293
456.041827	5433.231426	15.992307	-0.088139	3.984415
456.113145	5425.276568	15.997312	-0.088147	3.981561
455.940896	5417.269715	16.002317	-0.088110	3.978682
455.921471	5409.237844	16.007322	-0.088101	3.975794
456.337651	5401.212185	16.012327	-0.088174	3.972915
456.035887	5393.247405	16.017331	-0.088112	3.970042
456.297902	5385.195731	16.022336	-0.088156	3.967146
456.285919	5377.163406	16.027341	-0.088148	3.964250
456.561879	5369.229043	16.032346	-0.088195	3.961392
456.853880	5361.232934	16.037351	-0.088244	3.958511
456.713622	5353.292700	16.042355	-0.088213	3.955640
456.517067	5345.254098	16.047360	-0.088171	3.952730
456.374980	5337.282582	16.052365	-0.088139	3.949843
456.343926	5329.189806	16.057370	-0.088128	3.946912
456.373218	5321.221426	16.062375	-0.088129	3.944025
456.508418	5313.233669	16.067379	-0.088149	3.941131
456.465892	5305.259984	16.072384	-0.088135	3.938236
456.436444	5297.292371	16.077389	-0.088125	3.935342
455.951784	5289.276876	16.082394	-0.088029	3.932420
455.992253	5281.273782	16.087399	-0.088032	3.929510
456.199225	5273.229353	16.092403	-0.088065	3.926586
456.275323	5265.211383	16.097408	-0.088074	3.923667
456.180135	5257.283679	16.102413	-0.088051	3.920775
455.712006	5249.320759	16.107418	-0.087959	3.917861
455.455343	5241.359637	16.112423	-0.087906	3.914950
455.556328	5233.342021	16.117427	-0.087919	3.912023
455.580072	5225.267048	16.122432	-0.087919	3.909071
455.465954	5217.298505	16.127437	-0.087892	3.906153
455.864833	5209.215570	16.132442	-0.087961	3.903201
455.739626	5201.271537	16.137447	-0.087933	3.900288
455.586292	5193.279702	16.142451	-0.087899	3.897354
455.730407	5185.259980	16.147456	-0.087921	3.894414
455.760488	5177.290700	16.152461	-0.087921	3.891488
454.969939	5169.349271	16.157466	-0.087769	3.888553
455.101085	5161.367092	16.162471	-0.087788	3.885620
454.950549	5153.384333	16.167475	-0.087755	3.882678
455.020328	5145.330310	16.172480	-0.087763	3.879712
455.799552	5137.293096	16.177485	-0.087903	3.876765
455.622038	5129.293663	16.182490	-0.087864	3.873810
455.434487	5121.182646	16.187495	-0.087824	3.870812
455.648777	5113.188121	16.192499	-0.087859	3.867862
455.541295	5105.210075	16.197504	-0.087834	3.864909
455.623947	5097.280595	16.202509	-0.087844	3.861977
455.644643	5089.267922	16.207514	-0.087843	3.859010
455.492742	5081.330978	16.212519	-0.087809	3.856065
455.505854	5073.314217	16.217523	-0.087806	3.853091
455.277765	5065.318258	16.222528	-0.087759	3.850118
455.369190	5057.352277	16.227533	-0.087771	3.847161
455.276550	5049.280420	16.232538	-0.087748	3.844158
455.662536	5041.348347	16.237543	-0.087815	3.841214
455.395890	5033.350171	16.242547	-0.087760	3.838230
455.512608	5025.343615	16.247552	-0.087777	3.835249
455.463643	5017.398078	16.252557	-0.087762	3.832285
455.326545	5009.348483	16.257562	-0.087732	3.829277
455.407837	5001.343433	16.262567	-0.087742	3.826289
455.338320	4993.341795	16.267571	-0.087723	3.823296
455.174119	4985.356219	16.272576	-0.087688	3.820305
455.186595	4977.416521	16.277581	-0.087685	3.817333
455.251874	4969.345781	16.282586	-0.087692	3.814310
455.283686	4961.375786	16.287591	-0.087693	3.811322
454.997656	4953.391960	16.292595	-0.087634	3.808319
455.028774	4945.335710	16.297600	-0.087635	3.805294
455.281247	4937.405369	16.302605	-0.087677	3.802319
455.101863	4929.356230	16.307610	-0.087638	3.799287
455.252510	4921.401365	16.312615	-0.087661	3.796295
455.162827	4913.367928	16.317619	-0.087639	3.793266
455.113461	4905.357529	16.322624	-0.087625	3.790244
454.907979	4897.399479	16.327629	-0.087581	3.787236
454.971802	4889.340435	16.332634	-0.087588	3.784194
454.948261	4881.466604	16.337639	-0.087578	3.781217
454.774739	4873.404489	16.342643	-0.087541	3.778163
454.751198	4865.380899	16.347648	-0.087531	3.775125
454.799755	4857.477081	16.352653	-0.087535	3.772131
454.793998	4849.342607	16.357658	-0.087529	3.769046
455.064952	4841.386624	16.362663	-0.087574	3.766033
455.003192	4833.429005	16.367667	-0.087557	3.763009
454.523219	4825.496737	16.372672	-0.087463	3.759982
454.590135	4817.497188	16.377677	-0.087470	3.756941
454.898766	4809.390440	16.382682	-0.087522	3.753861
454.912778	4801.475987	16.387687	-0.087520	3.750846
454.896487	4793.461813	16.392691	-0.087512	3.747789
454.758029	4785.441554	16.397696	-0.087481	3.744725
454.712370	4777.539623	16.402701	-0.087467	3.741705
454.735308	4769.455207	16.407706	-0.087466	3.738615
454.489321	4761.513070	16.412711	-0.087415	3.735570
454.452512	4753.507767	16.417715	-0.087403	3.732503
454.595377	4745.455886	16.422720	-0.087425	3.729421
454.332407	4737.545210	16.427725	-0.087370	3.726380
454.520466	4729.455607	16.432730	-0.087400	3.723279
454.519537	4721.513368	16.437735	-0.087395	3.720228
454.251469	4713.547297	16.442739	-0.087340	3.717158
453.895945	4705.523139	16.447744	-0.087268	3.714061
454.716478	4697.420103	16.452749	-0.087416	3.710961
454.402056	4689.434241	16.457754	-0.087352	3.707875
454.079507	4681.509907	16.462759	-0.087287	3.704809
453.947453	4673.531103	16.467763	-0.087257	3.701725
453.809915	4665.517388	16.472768	-0.087226	3.698624
454.038931	4657.522216	16.477773	-0.087264	3.695538
454.197514	4649.470641	16.482778	-0.087288	3.692425
454.163849	4641.465323	16.487783	-0.087277	3.689323
454.118099	4633.529547	16.492787	-0.087263	3.686245
454.129141	4625.475957	16.497792	-0.087260	3.683120
454.178525	4617.530244	16.502797	-0.087264	3.680035
454.157214	4609.558264	16.507802	-0.087255	3.676935
454.126658	4601.547934	16.512807	-0.087244	3.673818
453.840491	4593.633264	16.517811	-0.087186	3.670728
453.866036	4585.582257	16.522816	-0.087185	3.667591
453.929426	4577.527524	16.527821	-0.087192	3.664451
453.425400	4569.626003	16.532826	-0.087093	3.661353
453.283996	4561.668730	16.537831	-0.087061	3.658240
453.569890	4553.635935	16.542835	-0.087109	3.655107
453.113488	4545.645693	16.547840	-0.087019	3.651967
453.223884	4537.618938	16.552845	-0.087035	3.648825
452.971009	4529.623714	16.557850	-0.086982	3.645684
453.109563	4521.635827	16.562855	-0.087003	3.642553
452.724403	4513.695630	16.567859	-0.086926	3.639424
453.038634	4505.650303	16.572864	-0.086979	3.636270
453.104638	4497.657171	16.577869	-0.086986	3.633127
453.328266	4489.584445	16.582874	-0.087023	3.629954
453.051585	4481.654093	16.587879	-0.086966	3.626821
453.240194	4473.616791	16.592883	-0.086996	3.623656
453.464260	4465.583893	16.597888	-0.087033	3.620491
453.471424	4457.665112	16.602893	-0.087029	3.617362
453.566508	4449.596934	16.607898	-0.087041	3.614174
453.435743	4441.668822	16.612903	-0.087012	3.611032
453.352281	4433.669422	16.617907	-0.086991	3.607860
452.837164	4425.702927	16.622912	-0.086890	3.604686
452.827057	4417.748599	16.627917	-0.086883	3.601529
453.147603	4409.650646	16.632922	-0.086937	3.598322
453.125124	4401.712811	16.637927	-0.086928	3.595165
453.151855	4393.727380	16.642931	-0.086928	3.591988
452.743670	4385.733993	16.647936	-0.086847	3.588792
453.118630	4377.703459	16.652941	-0.086911	3.585602
453.119922	4369.710671	16.657946	-0.086906	3.582413
453.120127	4361.714146	16.662951	-0.086901	3.579219
452.665746	4353.820232	16.667955	-0.086812	3.576051
452.794321	4345.719257	16.672960	-0.086830	3.572813
452.956811	4337.704083	16.677965	-0.086855	3.569609
452.887292	4329.718092	16.682970	-0.086837	3.566406
452.818151	4321.713613	16.687975	-0.086819	3.563193
453.269612	4313.742470	16.692979	-0.086898	3.560006
452.813182	4305.820411	16.697984	-0.086808	3.556808
452.684540	4297.839760	16.702989	-0.086779	3.553594
452.723382	4289.747498	16.707994	-0.086781	3.550337
452.116756	4281.848047	16.712999	-0.086663	3.547135
452.353388	4273.757845	16.718003	-0.086702	3.543879
452.483936	4265.796711	16.723008	-0.086721	3.540669
452.429440	4257.829901	16.728013	-0.086705	3.537448
451.962245	4249.839602	16.733018	-0.086613	3.534202
452.354832	4241.802947	16.738023	-0.086681	3.530961
452.536685	4233.794396	16.743027	-0.086710	3.527721
452.418349	4225.788672	16.748032	-0.086683	3.524471
452.412549	4217.890813	16.753037	-0.086676	3.521264
452.164068	4209.867745	16.758042	-0.086625	3.517997
452.424911	4201.836300	16.763047	-0.086668	3.514738
452.554015	4193.883817	16.768051	-0.086687	3.511505
452.364816	4185.839490	16.773056	-0.086647	3.508222
452.565783	4177.834098	16.778061	-0.086679	3.504963
452.256174	4169.895404	16.783066	-0.086616	3.501713
452.351596	4161.880303	16.788071	-0.086629	3.498441
452.310270	4153.923166	16.793075	-0.086616	3.495185
452.204039	4145.916872	16.798080	-0.086591	3.491904
452.210861	4137.916016	16.803085	-0.086587	3.488626
452.182444	4129.878320	16.808090	-0.086576	3.485329
452.128465	4121.958233	16.813095	-0.086561	3.482075
452.168408	4113.940842	16.818099	-0.086564	3.478782
451.916050	4105.977275	16.823104	-0.086511	3.475499
451.926325	4098.007784	16.828109	-0.086508	3.472218
452.171733	4089.910224	16.833114	-0.086549	3.468889
451.866103	4081.972348	16.838119	-0.086487	3.465605
451.867178	4073.981741	16.843123	-0.086482	3.462306
452.002325	4065.949342	16.848128	-0.086502	3.458991
452.004147	4058.014662	16.853133	-0.086497	3.455709
451.365606	4050.072012	16.858138	-0.086373	3.452399
451.376525	4042.038168	16.863143	-0.086370	3.449069
451.238872	4034.057374	16.868147	-0.086339	3.445754
451.029869	4026.087194	16.873152	-0.086295	3.442437
450.922477	4018.083386	16.878157	-0.086269	3.439106
451.197234	4010.058794	16.883162	-0.086315	3.435777
451.075767	4002.064199	16.888167	-0.086288	3.432443
451.388060	3994.033921	16.893171	-0.086341	3.429107
451.700868	3985.991083	16.898176	-0.086394	3.425761
451.597053	3978.087846	16.903181	-0.086369	3.422457
451.520040	3970.057201	16.908186	-0.086350	3.419097
451.590600	3962.079533	16.913191	-0.086358	3.415760
451.525344	3954.118063	16.918195	-0.086340	3.412423
451.451289	3946.065439	16.923200	-0.086321	3.409044
451.393697	3938.174828	16.928205	-0.086305	3.405730
451.417349	3930.140969	16.933210	-0.086305	3.402355
451.510868	3922.130666	16.938215	-0.086317	3.398990
451.379401	3914.223726	16.943219	-0.086287	3.395656
450.902333	3906.194850	16.948224	-0.086193	3.392256
451.186748	3898.105541	16.953229	-0.086241	3.388854
450.911998	3890.162233	16.958234	-0.086185	3.385490
451.247483	3882.152469	16.963239	-0.086242	3.382116
451.150788	3874.161141	16.968243	-0.086219	3.378732
451.024891	3866.189964	16.973248	-0.086190	3.375351
451.238033	3858.179161	16.978253	-0.086225	3.371963
451.316709	3850.143096	16.983258	-0.086234	3.368556
451.104367	3842.199136	16.988263	-0.086189	3.365173
451.198188	3834.252064	16.993267	-0.086202	3.361797
450.983882	3826.255473	16.998272	-0.086157	3.358386
451.149524	3818.252980	17.003277	-0.086182	3.354982
450.412369	3810.355825	17.008282	-0.086040	3.351586
450.597311	3802.318191	17.013287	-0.086069	3.348161
451.117992	3794.226332	17.018291	-0.086161	3.344723
451.056161	3786.274092	17.023296	-0.086144	3.341318
450.951552	3778.343240	17.028301	-0.086120	3.337918
450.295746	3770.408149	17.033306	-0.085992	3.334491
450.547392	3762.354537	17.038311	-0.086034	3.331044
450.571881	3754.351119	17.043315	-0.086033	3.327607
450.538743	3746.300146	17.048320	-0.086022	3.324143
450.547011	3738.380011	17.053325	-0.086018	3.320734
450.481931	3730.368127	17.058330	-0.086001	3.317279
450.765868	3722.340575	17.063335	-0.086049	3.313827
450.847534	3714.378445	17.068339	-0.086059	3.310392
450.522540	3706.388969	17.073344	-0.085993	3.306925
450.616762	3698.387516	17.078349	-0.086005	3.303467
450.455290	3690.430486	17.083354	-0.085970	3.300013
450.414494	3682.456541	17.088359	-0.085957	3.296554
450.539468	3674.426341	17.093363	-0.085976	3.293073
450.632080	3666.391005	17.098368	-0.085988	3.289585
450.597542	3658.455364	17.103373	-0.085976	3.286131
450.430246	3650.455667	17.108378	-0.085940	3.282641
450.346865	3642.492666	17.113383	-0.085919	3.279166
450.486028	3634.510579	17.118387	-0.085940	3.275688
450.251803	3626.531244	17.123392	-0.085891	3.272193
450.422936	3618.531760	17.128397	-0.085918	3.268701
450.600531	3610.482417	17.133402	-0.085946	3.265184
450.243497	3602.560197	17.138407	-0.085874	3.261697
450.374077	3594.560159	17.143411	-0.085893	3.258193
450.542360	3586.536749	17.148416	-0.085919	3.254675
450.212878	3578.632153	17.153421	-0.085853	3.251186
449.872291	3570.636582	17.158426	-0.085784	3.247653
449.968996	3562.569341	17.163431	-0.085797	3.244102
450.019698	3554.681420	17.168435	-0.085801	3.240624
449.745275	3546.674909	17.173440	-0.085745	3.237077
449.668334	3538.683433	17.178445	-0.085725	3.233541
449.746495	3530.660033	17.183450	-0.085735	3.229993
449.814115	3522.623873	17.188455	-0.085742	3.226435
449.870302	3514.651093	17.193459	-0.085747	3.222901
449.819485	3506.650808	17.198464	-0.085733	3.219346
449.854418	3498.702474	17.203469	-0.085734	3.215814
449.491980	3490.752331	17.208474	-0.085662	3.212261
449.725144	3482.680084	17.213479	-0.085700	3.208674
449.780888	3474.698777	17.218483	-0.085705	3.205117
449.333008	3466.773871	17.223488	-0.085616	3.201559
449.599854	3458.748884	17.228493	-0.085661	3.197983
449.534075	3450.787059	17.233498	-0.085643	3.194417
449.283731	3442.817132	17.238503	-0.085592	3.190835
449.463019	3434.793212	17.243507	-0.085620	3.187244
449.341092	3426.750427	17.248512	-0.085592	3.183627
449.456786	3418.811791	17.253517	-0.085608	3.180063
449.436719	3410.828638	17.258522	-0.085599	3.176470
448.989999	3402.901618	17.263527	-0.085511	3.172879
449.449089	3394.816561	17.268531	-0.085591	3.169252
449.324984	3386.872169	17.273536	-0.085563	3.165659
449.351964	3378.890315	17.278541	-0.085563	3.162051
448.945689	3370.964909	17.283546	-0.085482	3.158446
448.554528	3363.017663	17.288551	-0.085404	3.154827
448.595536	3354.980064	17.293555	-0.085407	3.151182
448.620683	3346.953312	17.298560	-0.085406	3.147538
448.975880	3338.880553	17.303565	-0.085467	3.143883
448.872068	3330.946804	17.308570	-0.085443	3.140266
448.363037	3323.052909	17.313575	-0.085343	3.136645
448.476645	3314.991554	17.318579	-0.085359	3.132972
448.739711	3306.954066	17.323584	-0.085402	3.129312
448.747396	3298.990929	17.328589	-0.085399	3.125670
448.673739	3291.019320	17.333594	-0.085380	3.122017
448.401804	3283.080369	17.338599	-0.085324	3.118365
448.360362	3275.096429	17.343603	-0.085311	3.114698
448.145750	3267.127124	17.348608	-0.085266	3.111026
448.531496	3259.038969	17.353613	-0.085333	3.107323
448.379780	3251.078926	17.358618	-0.085299	3.103649
448.346451	3243.127226	17.363623	-0.085288	3.099980
448.181756	3235.222611	17.368627	-0.085252	3.096323
448.149457	3227.171549	17.373632	-0.085241	3.092600
448.334302	3219.131685	17.378637	-0.085270	3.088887
448.350008	3211.137504	17.383642	-0.085268	3.085184
448.184932	3203.207039	17.388647	-0.085232	3.081497
448.158742	3195.251777	17.393651	-0.085222	3.077800
447.521831	3187.337217	17.398656	-0.085098	3.074089
448.105790	3179.205187	17.403661	-0.085202	3.070330
448.066550	3171.220620	17.408666	-0.085189	3.066606
447.825452	3163.243876	17.413671	-0.085139	3.062871
447.759834	3155.280878	17.418675	-0.085122	3.059147
448.108714	3147.231338	17.423680	-0.085181	3.055397
448.101261	3139.267105	17.428685	-0.085175	3.051666
447.791850	3131.346670	17.433690	-0.085112	3.047936
447.599732	3123.372719	17.438695	-0.085071	3.044181
447.586126	3115.429891	17.443699	-0.085064	3.040446
447.506055	3107.419615	17.448704	-0.085043	3.036671
447.322446	3099.469901	17.453709	-0.085004	3.032914
447.191375	3091.434715	17.458714	-0.084975	3.029116
447.336293	3083.440087	17.463719	-0.084996	3.025345
447.024369	3075.504124	17.468723	-0.084933	3.021574
447.539644	3067.414560	17.473728	-0.085024	3.017768
447.157336	3059.527816	17.478733	-0.084948	3.014008
447.101565	3051.535732	17.483738	-0.084932	3.010209
447.256009	3043.484227	17.488743	-0.084955	3.006388
447.415636	3035.523581	17.493747	-0.084980	3.002606
447.370070	3027.520125	17.498752	-0.084966	2.998788
447.497909	3019.584864	17.503757	-0.084985	2.995006
446.971250	3011.652467	17.508762	-0.084882	2.991188
446.814635	3003.655006	17.513767	-0.084848	2.987353
447.082267	2995.645189	17.518771	-0.084892	2.983528
446.913041	2987.657974	17.523776	-0.084855	2.979687
447.149572	2979.626436	17.528781	-0.084894	2.975841
447.324328	2971.624791	17.533786	-0.084922	2.972001
446.847737	2963.699220	17.538791	-0.084828	2.968159
446.791738	2955.727653	17.543795	-0.084812	2.964311
446.771118	2947.767800	17.548800	-0.084803	2.960466
446.983571	2939.759437	17.553805	-0.084838	2.956605
447.167945	2931.734193	17.558810	-0.084867	2.952729
447.052392	2923.756582	17.563815	-0.084840	2.948855
446.895975	2915.807474	17.568819	-0.084806	2.944988
446.955363	2907.833094	17.573824	-0.084812	2.941115
446.946742	2899.858049	17.578829	-0.084805	2.937233
446.699279	2891.888402	17.583834	-0.084754	2.933335
446.977268	2883.838462	17.588839	-0.084800	2.929421
447.424434	2875.821998	17.593843	-0.084878	2.925528
447.117896	2867.918893	17.598848	-0.084816	2.921644
447.014782	2859.995062	17.603853	-0.084792	2.917756
446.557781	2852.071433	17.608858	-0.084701	2.913843
446.809136	2843.921370	17.613863	-0.084743	2.909853
446.570135	2836.004249	17.618867	-0.084693	2.905945
445.948747	2828.100571	17.623872	-0.084573	2.902017
446.567342	2819.983030	17.628877	-0.084682	2.898046
446.403221	2812.019280	17.633882	-0.084647	2.894103
446.776028	2803.989999	17.638887	-0.084711	2.890152
446.687120	2796.034583	17.643891	-0.084689	2.886207
446.686905	2788.068185	17.648896	-0.084684	2.882255
446.956924	2780.079809	17.653901	-0.084729	2.878302
446.752495	2772.165118	17.658906	-0.084686	2.874354
446.401498	2764.254776	17.663911	-0.084616	2.870395
446.124520	2756.289624	17.668915	-0.084559	2.866406
445.893957	2748.311714	17.673920	-0.084511	2.862408
446.169924	2740.255809	17.678925	-0.084557	2.858395
445.962981	2732.295835	17.683930	-0.084513	2.854396
445.824527	2724.319428	17.688935	-0.084482	2.850387
446.047561	2716.311862	17.693939	-0.084519	2.846378
446.039204	2708.306528	17.698944	-0.084512	2.842351
446.190893	2700.338209	17.703949	-0.084535	2.838346
446.320117	2692.351466	17.708954	-0.084554	2.834325
446.330810	2684.367356	17.713959	-0.084551	2.830293
446.001436	2676.446669	17.718963	-0.084484	2.826267
445.876144	2668.467139	17.723968	-0.084456	2.822217
445.869649	2660.483581	17.728973	-0.084449	2.818167
446.031072	2652.458940	17.733978	-0.084474	2.814099
445.739723	2644.557697	17.738983	-0.084415	2.810062
445.659967	2636.577307	17.743987	-0.084395	2.805992
445.666632	2628.561209	17.748992	-0.084391	2.801902
445.773163	2620.590982	17.753997	-0.084405	2.797835
446.024124	2612.568511	17.759002	-0.084447	2.793745
446.183570	2604.554937	17.764007	-0.084471	2.789648
446.017085	2596.622758	17.769011	-0.084435	2.785567
445.866662	2588.667639	17.774016	-0.084402	2.781469
446.107478	2580.684498	17.779021	-0.084442	2.777374
445.561200	2572.803649	17.784026	-0.084335	2.773278
445.848390	2564.729713	17.789031	-0.084383	2.769127
445.848544	2556.807743	17.794035	-0.084378	2.765031
445.655545	2548.831151	17.799040	-0.084337	2.760889
445.719963	2540.856649	17.804045	-0.084344	2.756757
445.535825	2532.878456	17.809050	-0.084304	2.752602
445.495300	2524.841998	17.814055	-0.084292	2.748419
445.271115	2516.898305	17.819059	-0.084245	2.744267
445.359911	2508.919939	17.824064	-0.084256	2.740110
445.204156	2500.961293	17.829069	-0.084222	2.735941
445.558702	2492.909813	17.834074	-0.084283	2.731749
445.311378	2484.990091	17.839079	-0.084232	2.727583
444.784712	2477.104784	17.844083	-0.084128	2.723410
444.696680	2469.108617	17.849088	-0.084107	2.719201
445.091398	2461.076930	17.854093	-0.084175	2.714996
445.354864	2453.074439	17.859098	-0.084219	2.710792
445.215785	2445.096721	17.864103	-0.084188	2.706570
445.241587	2437.152304	17.869107	-0.084188	2.702368
444.654809	2429.270774	17.874112	-0.084073	2.698155
444.930926	2421.246794	17.879117	-0.084120	2.693914
444.868528	2413.247020	17.884122	-0.084103	2.689658
444.788782	2405.278458	17.889127	-0.084083	2.685410
444.672099	2397.369164	17.894131	-0.084056	2.681185
444.214672	2389.447361	17.899136	-0.083966	2.676925
444.271542	2381.428972	17.904141	-0.083971	2.672639
444.272559	2373.425000	17.909146	-0.083966	2.668351
443.946946	2365.447749	17.914151	-0.083900	2.664048
444.039946	2357.480956	17.919155	-0.083912	2.659772
443.826331	2349.511293	17.924160	-0.083867	2.655467
444.039948	2341.499774	17.929165	-0.083902	2.651161
444.399955	2333.444979	17.934170	-0.083964	2.646834
443.908608	2325.588405	17.939175	-0.083867	2.642551
444.000925	2317.637272	17.944179	-0.083879	2.638248
444.194740	2309.609470	17.949184	-0.083910	2.633904
444.263798	2301.611993	17.954189	-0.083918	2.629560
443.998378	2293.697596	17.959194	-0.083863	2.625232
443.641004	2285.782970	17.964199	-0.083792	2.620891
443.536355	2277.833612	17.969203	-0.083767	2.616540
443.285084	2269.859127	17.974208	-0.083715	2.612158
443.501659	2261.840531	17.979213	-0.083750	2.607777
443.792138	2253.800179	17.984218	-0.083799	2.603381
443.338691	2245.938821	17.989223	-0.083709	2.599026
443.780053	2237.918796	17.994227	-0.083786	2.594637
444.171947	2229.750727	17.999232	-0.083854	2.590156
443.932434	2221.829835	18.004237	-0.083804	2.585760
443.861249	2213.915676	18.009242	-0.083786	2.581372
443.715648	2205.974936	18.014247	-0.083754	2.576956
443.929055	2197.993473	18.019251	-0.083788	2.572536
443.648665	2190.029912	18.024256	-0.083731	2.568083
443.949347	2182.038445	18.029261	-0.083782	2.563647
443.886693	2174.126918	18.034266	-0.083765	2.559223
443.588502	2166.204189	18.039271	-0.083704	2.554768
443.805289	2158.215037	18.044275	-0.083740	2.550305
443.660515	2150.247583	18.049280	-0.083707	2.545821
444.087609	2142.217499	18.054285	-0.083782	2.541334
443.749115	2134.327632	18.059290	-0.083714	2.536863
443.820426	2126.329957	18.064295	-0.083722	2.532354
443.972265	2118.333925	18.069299	-0.083745	2.527842
443.733227	2110.434574	18.074304	-0.083695	2.523350
443.336515	2102.546395	18.079309	-0.083616	2.518843
443.348906	2094.571220	18.084314	-0.083613	2.514310
443.807924	2086.469452	18.089319	-0.083694	2.509728
443.743529	2078.531384	18.094323	-0.083676	2.505194
442.978854	2070.690053	18.099328	-0.083529	2.500654
443.485095	2062.636875	18.104333	-0.083618	2.496079
443.254593	2054.708888	18.109338	-0.083570	2.491513
443.031214	2046.759375	18.114343	-0.083523	2.486927
443.127330	2038.785430	18.119347	-0.083536	2.482341
443.007492	2030.834624	18.124352	-0.083508	2.477745
443.215985	2022.834650	18.129357	-0.083542	2.473136
443.332513	2014.859881	18.134362	-0.083559	2.468527
443.150066	2006.885124	18.139367	-0.083520	2.463886
443.559919	1998.885510	18.144371	-0.083591	2.459267
443.401586	1990.944623	18.149376	-0.083556	2.454630
443.505615	1982.978116	18.154381	-0.083570	2.449989
443.352424	1975.057636	18.159386	-0.083537	2.445347
443.170051	1967.136441	18.164391	-0.083498	2.440693
443.010458	1959.226383	18.169395	-0.083463	2.436039
442.890216	1951.211213	18.174400	-0.083435	2.431316
442.785621	1943.231312	18.179405	-0.083410	2.426607
442.651853	1935.300694	18.184410	-0.083380	2.421915
442.721249	1927.311276	18.189415	-0.083388	2.417196
442.543433	1919.390628	18.194419	-0.083350	2.412488
442.705575	1911.370034	18.199424	-0.083375	2.407739
442.659575	1903.423386	18.204429	-0.083361	2.403007
441.946780	1895.602612	18.209434	-0.083223	2.398289
441.966902	1887.596805	18.214439	-0.083222	2.393508
442.258161	1879.610428	18.219443	-0.083271	2.388752
441.910652	1871.639053	18.224448	-0.083201	2.383944
442.164647	1863.655404	18.229453	-0.083243	2.379167
441.363489	1855.841039	18.234458	-0.083089	2.374397
441.557023	1847.781135	18.239463	-0.083120	2.369550
441.945343	1839.758445	18.244467	-0.083187	2.364732
442.070018	1831.791406	18.249472	-0.083205	2.359916
442.122152	1823.846009	18.254477	-0.083210	2.355097
442.548654	1815.820349	18.259482	-0.083284	2.350251
442.112054	1807.943687	18.264487	-0.083197	2.345414
442.081249	1800.019349	18.269491	-0.083187	2.340571
442.140459	1792.028313	18.274496	-0.083192	2.335685
442.024348	1784.090351	18.279501	-0.083166	2.330807
442.346739	1776.086771	18.284506	-0.083220	2.325915
441.968422	1768.219827	18.289511	-0.083145	2.321038
441.352693	1760.398688	18.294515	-0.083025	2.316159
441.666712	1752.339162	18.299520	-0.083078	2.311200
442.535296	1744.212879	18.304525	-0.083235	2.306237
442.262560	1736.353068	18.309530	-0.083179	2.301332
442.010766	1728.445428	18.314535	-0.083127	2.296387
441.944333	1720.520625	18.319539	-0.083110	2.291438
441.961375	1712.534093	18.324544	-0.083108	2.286446
441.884958	1704.617490	18.329549	-0.083088	2.281479
441.604635	1696.739495	18.334554	-0.083031	2.276508
441.673433	1688.711468	18.339559	-0.083038	2.271462
441.911069	1680.693805	18.344563	-0.083078	2.266425
441.788451	1672.758512	18.349568	-0.083050	2.261399
441.913874	1664.802157	18.354573	-0.083068	2.256369
441.940903	1656.851397	18.359578	-0.083068	2.251323
441.280705	1649.010866	18.364583	-0.082940	2.246275
440.898800	1641.136233	18.369587	-0.082863	2.241218
440.389079	1633.237304	18.374592	-0.082763	2.236123
440.787666	1625.178063	18.379597	-0.082832	2.230995
441.286235	1617.123479	18.384602	-0.082920	2.225867
441.290650	1609.166604	18.389607	-0.082916	2.220746
441.468185	1601.239421	18.394611	-0.082944	2.215647
441.323597	1593.316272	18.399616	-0.082912	2.210511
441.123957	1585.410510	18.404621	-0.082869	2.205368
441.132542	1577.467433	18.409626	-0.082866	2.200208
441.066914	1569.529786	18.414631	-0.082848	2.195033
441.111629	1561.578265	18.419635	-0.082852	2.189847
441.235834	1553.580854	18.424640	-0.082869	2.184626
440.783109	1545.745202	18.429645	-0.082780	2.179444
440.263783	1537.888660	18.434650	-0.082678	2.174230
440.176480	1529.901177	18.439655	-0.082657	2.168958
440.274233	1521.923702	18.444659	-0.082670	2.163697
440.758337	1513.877754	18.449664	-0.082755	2.158414
440.758952	1505.951187	18.454669	-0.082750	2.153152
440.862537	1497.999215	18.459674	-0.082764	2.147870
440.893787	1490.062380	18.464679	-0.082765	2.142578
440.948445	1482.167153	18.469683	-0.082770	2.137303
440.766140	1474.256436	18.474688	-0.082731	2.131982
440.070034	1466.420230	18.479693	-0.082596	2.126648
440.742742	1458.351367	18.484698	-0.082716	2.121276
440.307640	1450.495676	18.489703	-0.082630	2.115927
440.190323	1442.565322	18.494707	-0.082603	2.110544
440.176211	1434.572562	18.499712	-0.082595	2.105116
440.121550	1426.652786	18.504717	-0.082580	2.099719
439.840371	1418.772401	18.509722	-0.082522	2.094313
439.605715	1410.841076	18.514727	-0.082473	2.088863
439.702001	1402.878717	18.519731	-0.082486	2.083410
440.140886	1394.870314	18.524736	-0.082563	2.077945
439.974009	1386.975476	18.529741	-0.082527	2.072483
439.950138	1379.053566	18.534746	-0.082517	2.067003
440.139217	1371.076477	18.539751	-0.082547	2.061491
439.456028	1363.300155	18.544755	-0.082415	2.056016
439.553085	1355.312077	18.549760	-0.082428	2.050457
439.470457	1347.373561	18.554765	-0.082407	2.044900
439.788208	1339.400560	18.559770	-0.082461	2.039345
439.346891	1331.554129	18.564775	-0.082374	2.033785
439.350249	1323.622416	18.569779	-0.082369	2.028196
439.519674	1315.631941	18.574784	-0.082396	2.022567
439.003946	1307.802650	18.579789	-0.082295	2.016965
439.667965	1299.738482	18.584794	-0.082413	2.011305
439.207184	1291.884056	18.589799	-0.082322	2.005659
439.155297	1283.987796	18.594803	-0.082307	2.000010
439.353596	1276.018533	18.599808	-0.082339	1.994320
439.409527	1268.096302	18.604813	-0.082345	1.988633
439.122953	1260.230487	18.609818	-0.082286	1.982933
439.212910	1252.264799	18.614823	-0.082298	1.977184
439.324251	1244.349934	18.619827	-0.082313	1.971459
439.086307	1236.444893	18.624832	-0.082264	1.965685
439.204466	1228.535464	18.629837	-0.082281	1.959931
438.669223	1220.735575	18.634842	-0.082176	1.954167
438.427677	1212.811658	18.639847	-0.082126	1.948328
438.663394	1204.810761	18.644851	-0.082165	1.942468
438.176222	1196.966660	18.649856	-0.082069	1.936625
438.641199	1188.936298	18.654861	-0.082150	1.930733
438.673188	1181.020467	18.659866	-0.082151	1.924859
438.344725	1173.161536	18.664871	-0.082085	1.918969
438.281149	1165.273894	18.669875	-0.082068	1.913070
438.694017	1157.235964	18.674880	-0.082139	1.907094
439.130646	1149.273344	18.679885	-0.082216	1.901158
438.738313	1141.459031	18.684890	-0.082138	1.895221
438.576620	1133.572353	18.689895	-0.082102	1.889237
438.782740	1125.644397	18.694899	-0.082136	1.883245
438.066341	1117.872719	18.699904	-0.081997	1.877245
437.989629	1109.965600	18.704909	-0.081978	1.871197
437.954299	1102.039293	18.709914	-0.081966	1.865120
438.478977	1094.010391	18.714919	-0.082058	1.859010
438.153021	1086.190883	18.719923	-0.081993	1.852941
438.244815	1078.239589	18.724928	-0.082005	1.846800
438.357613	1070.334877	18.729933	-0.082021	1.840677
438.421999	1062.444578	18.734938	-0.082027	1.834539
438.540996	1054.520320	18.739943	-0.082044	1.828360
438.560814	1046.631259	18.744947	-0.082043	1.822176
438.683549	1038.716763	18.749952	-0.082061	1.815963
438.471735	1030.861254	18.754957	-0.082016	1.809735
438.799348	1022.937519	18.759962	-0.082072	1.803497
438.532916	1015.102864	18.764967	-0.082017	1.797236
438.319315	1007.241410	18.769971	-0.081973	1.790937
438.449249	999.291450	18.774976	-0.081992	1.784588
438.451567	991.417030	18.779981	-0.081987	1.778262
438.396215	983.552525	18.784986	-0.081972	1.771913
438.047555	975.693082	18.789991	-0.081902	1.765508
437.847077	967.869580	18.794995	-0.081859	1.759129
437.630187	959.997273	18.800000	-0.081814	1.752684
437.633308	952.088365	18.805005	-0.081809	1.746213
438.038246	944.138076	18.810010	-0.081879	1.739736
437.865388	936.282966	18.815015	-0.081842	1.733239
437.935788	928.380745	18.820019	-0.081850	1.726709
437.779981	920.526658	18.825024	-0.081816	1.720166
437.973414	912.638142	18.830029	-0.081847	1.713615
437.664008	904.813322	18.835034	-0.081784	1.707025
437.473632	896.940628	18.840039	-0.081744	1.700385
437.830242	889.018163	18.845043	-0.081805	1.693751
437.145460	881.262811	18.850048	-0.081672	1.687092
437.248370	873.346498	18.855053	-0.081686	1.680375
437.197061	865.509159	18.860058	-0.081672	1.673679
436.951371	857.661738	18.865063	-0.081621	1.666920
436.806945	849.811926	18.870067	-0.081589	1.660146
437.087709	841.890045	18.875072	-0.081636	1.653340
437.331665	833.960335	18.880077	-0.081676	1.646494
437.121095	826.168450	18.885082	-0.081632	1.639676
437.104107	818.308714	18.890087	-0.081624	1.632798
436.932199	810.451541	18.895091	-0.081587	1.625871
436.381281	802.676380	18.900096	-0.081479	1.618933
436.649345	794.744876	18.905101	-0.081524	1.611943
436.993530	786.832030	18.910106	-0.081583	1.604950
436.857938	779.018232	18.915111	-0.081553	1.597946
436.719202	771.212034	18.920115	-0.081522	1.590917
436.735516	763.343376	18.925120	-0.081520	1.583824
436.848242	755.489317	18.930125	-0.081536	1.576726
436.718074	747.682819	18.935130	-0.081506	1.569603
436.463678	739.875020	18.940135	-0.081454	1.562429
436.656648	732.021462	18.945139	-0.081485	1.555245
436.645839	724.177529	18.950144	-0.081478	1.548007
436.533931	716.348491	18.955149	-0.081452	1.540733
436.667332	708.515569	18.960154	-0.081471	1.533459
436.092686	700.768286	18.965159	-0.081359	1.526122
436.608319	692.860910	18.970163	-0.081450	1.518766
436.612518	685.047914	18.975168	-0.081446	1.511384
436.584652	677.227221	18.980173	-0.081436	1.503955
436.494135	669.446873	18.985178	-0.081414	1.496517
436.553042	661.602647	18.990183	-0.081420	1.489003
436.459195	653.837907	18.995187	-0.081397	1.481505
436.232814	646.064972	19.000192	-0.081350	1.473939
436.211471	638.214481	19.005197	-0.081341	1.466291
435.883787	630.484690	19.010202	-0.081275	1.458672
436.175235	622.601365	19.015207	-0.081324	1.450962
436.175090	614.809749	19.020211	-0.081319	1.443255
436.034327	607.043566	19.025216	-0.081288	1.435508
435.978239	599.262096	19.030221	-0.081272	1.427717
435.963331	591.481710	19.035226	-0.081265	1.419892
435.759321	583.724319	19.040231	-0.081222	1.412015
435.811324	575.936207	19.045235	-0.081226	1.404106
435.655310	568.193588	19.050240	-0.081192	1.396163
435.459155	560.430334	19.055245	-0.081151	1.388147
435.231545	552.709011	19.060250	-0.081103	1.380121
434.852797	544.987631	19.065255	-0.081028	1.372023
434.948833	537.178902	19.070259	-0.081041	1.363868
434.938237	529.416669	19.075264	-0.081034	1.355694
435.595304	521.527223	19.080269	-0.081151	1.347453
435.046637	513.894769	19.085274	-0.081044	1.339222
435.169008	506.107106	19.090279	-0.081061	1.330893
435.172912	498.378501	19.095283	-0.081057	1.322554
435.040364	490.660629	19.100288	-0.081027	1.314149
434.707057	482.890588	19.105293	-0.080960	1.305596
434.796255	475.156834	19.110298	-0.080972	1.297104
434.449828	467.482529	19.115303	-0.080902	1.288542
434.670894	459.723050	19.120307	-0.080939	1.279933
434.384156	452.061352	19.125312	-0.080880	1.271280
434.380504	444.350739	19.130317	-0.080875	1.262566
434.531850	436.622790	19.135322	-0.080898	1.253802
434.291871	428.947403	19.140327	-0.080848	1.244961
434.376014	421.258411	19.145331	-0.080859	1.236104
434.108333	413.608252	19.150336	-0.080804	1.227158
433.949368	405.952916	19.155341	-0.080769	1.218163
433.944671	398.279011	19.160346	-0.080764	1.209109
433.920854	390.596279	19.165351	-0.080754	1.199973
433.924946	382.948867	19.170355	-0.080750	1.190815
433.806876	375.301084	19.175360	-0.080723	1.181560
434.165977	367.587481	19.180365	-0.080785	1.172252
433.957374	359.997285	19.185370	-0.080741	1.162901
434.059407	352.338899	19.190375	-0.080755	1.153456
434.313675	344.659137	19.195379	-0.080798	1.143938
434.443899	337.030327	19.200384	-0.080817	1.134379
434.189445	329.470999	19.205389	-0.080765	1.124742
433.806834	321.962811	19.210394	-0.080689	1.115060
433.604340	314.400967	19.215399	-0.080646	1.105263
433.200818	306.894134	19.220403	-0.080566	1.095405
433.448266	299.254078	19.225408	-0.080607	1.085430
433.241421	291.737870	19.230413	-0.080564	1.075423
433.394515	284.154482	19.235418	-0.080587	1.065315
433.141914	276.649586	19.240423	-0.080535	1.055121
432.977178	269.138517	19.245427	-0.080500	1.044840
432.810688	261.649534	19.250432	-0.080464	1.034487
432.275011	254.220423	19.255437	-0.080359	1.024024
432.185215	246.735677	19.260442	-0.080338	1.013483
432.891683	239.096111	19.265447	-0.080464	1.002808
432.892069	231.631669	19.270451	-0.080460	0.992093
432.349887	224.249735	19.275456	-0.080354	0.981244
432.689904	216.734137	19.280461	-0.080412	0.970304
432.513835	209.339742	19.285466	-0.080375	0.959285
432.476478	201.925171	19.290471	-0.080363	0.948144
432.293265	194.573352	19.295475	-0.080324	0.936928
432.198730	187.207450	19.300480	-0.080302	0.925577
432.526532	179.775952	19.305485	-0.080358	0.914099
432.245963	172.492417	19.310490	-0.080301	0.902541
431.714797	165.256408	19.315495	-0.080198	0.890838
431.376950	158.012799	19.320499	-0.080130	0.879022
431.383747	150.707575	19.325504	-0.080126	0.867043
431.721557	143.373510	19.330509	-0.080185	0.854945
431.720610	136.132740	19.335514	-0.080180	0.842732
431.538920	128.937154	19.340519	-0.080141	0.830361
431.158314	121.806472	19.345523	-0.080066	0.817855
431.026594	114.653092	19.350528	-0.080037	0.805193
431.548200	107.411839	19.355533	-0.080129	0.792379
431.300514	100.351765	19.360538	-0.080078	0.779436
431.105058	93.301742	19.365543	-0.080037	0.766311
431.255734	86.236913	19.370547	-0.080061	0.753046
430.762263	79.309109	19.375552	-0.079965	0.739586
430.741471	72.506029	19.380557	-0.079956	0.726289