Fri Apr 16 19:08:02 2021

Number of Points = 3638
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.489049	-0.040057	0.000000	-0.000048	0.311403

1.923481	-0.120819	0.005005	-0.000129	0.311394
2.298014	-0.191577	0.010010	-0.000199	0.311382
2.167700	-0.169149	0.015014	-0.000175	0.311376
2.385005	-0.206659	0.020019	-0.000215	0.311386
1.984548	-0.132062	0.025024	-0.000141	0.311395
1.868167	-0.114026	0.030029	-0.000119	0.311380
2.332760	-0.198684	0.035034	-0.000206	0.311379
2.395535	-0.211992	0.040038	-0.000217	0.311371
2.183723	-0.170676	0.045043	-0.000178	0.311384
2.059429	-0.200735	0.050048	-0.000155	0.311140
2.237394	-0.248374	0.055053	-0.000188	0.311069
2.146309	-0.229079	0.060058	-0.000171	0.311082
1.861830	-0.179963	0.065062	-0.000118	0.311070
2.236915	-0.247600	0.070067	-0.000188	0.311072
2.319286	-0.262633	0.075072	-0.000203	0.311072
2.061725	-0.269643	0.080077	-0.000155	0.310822
2.140434	-0.297801	0.085082	-0.000170	0.310758
1.872271	-0.249253	0.090086	-0.000120	0.310757
1.903633	-0.252868	0.095091	-0.000126	0.310767
2.026250	-0.276893	0.100096	-0.000149	0.310759
1.755311	-0.269737	0.105101	-0.000099	0.310563
1.830263	-0.292686	0.110106	-0.000113	0.310520
1.681450	-0.267547	0.115110	-0.000085	0.310512
2.081671	-0.340390	0.120115	-0.000159	0.310511
1.901641	-0.340859	0.125120	-0.000126	0.310357
1.879754	-0.377934	0.130125	-0.000122	0.310166
1.803276	-0.362739	0.135130	-0.000108	0.310172
1.764390	-0.355917	0.140134	-0.000100	0.310171
1.497035	-0.347157	0.145139	-0.000051	0.309985
1.628115	-0.397996	0.150144	-0.000075	0.309859
2.111438	-0.489524	0.155149	-0.000165	0.309842
2.138953	-0.509336	0.160154	-0.000170	0.309773
1.836442	-0.510854	0.165158	-0.000114	0.309510
2.200847	-0.575071	0.170163	-0.000182	0.309519
2.451022	-0.638027	0.175168	-0.000228	0.309437
2.194774	-0.636783	0.180173	-0.000181	0.309226
2.178821	-0.632684	0.185178	-0.000178	0.309231
2.246088	-0.684841	0.190182	-0.000190	0.309045
1.963977	-0.665252	0.195187	-0.000138	0.308897
1.954221	-0.665242	0.200192	-0.000136	0.308889
1.812500	-0.695765	0.205197	-0.000110	0.308625
2.170702	-0.769369	0.210202	-0.000176	0.308585
1.942572	-0.753312	0.215206	-0.000134	0.308467
1.820546	-0.774573	0.220211	-0.000111	0.308263
2.099266	-0.826800	0.225216	-0.000163	0.308256
1.987017	-0.862853	0.230221	-0.000142	0.307991
1.933824	-0.857152	0.235226	-0.000133	0.307972
2.102731	-0.933011	0.240230	-0.000164	0.307760
2.156934	-0.971175	0.245235	-0.000174	0.307627
1.788174	-0.931232	0.250240	-0.000105	0.307500
1.800218	-0.971495	0.255245	-0.000108	0.307321
2.177703	-1.058485	0.260250	-0.000178	0.307235
1.683185	-1.020599	0.265254	-0.000086	0.306990
1.772386	-1.044849	0.270259	-0.000103	0.306953
1.952576	-1.129290	0.275264	-0.000136	0.306709
1.854442	-1.124249	0.280269	-0.000118	0.306649
1.718234	-1.158162	0.285274	-0.000093	0.306372
1.745897	-1.175287	0.290278	-0.000098	0.306315
1.859270	-1.249264	0.295283	-0.000119	0.306063
1.570595	-1.212202	0.300288	-0.000065	0.305991
1.618798	-1.274504	0.305293	-0.000074	0.305738
1.919046	-1.347294	0.310298	-0.000130	0.305652
1.515032	-1.310030	0.315302	-0.000055	0.305481
1.282063	-1.303393	0.320307	-0.000012	0.305312
1.446064	-1.367869	0.325312	-0.000042	0.305148
1.631423	-1.449361	0.330317	-0.000077	0.304921
1.582809	-1.458695	0.335322	-0.000068	0.304835
1.600391	-1.529989	0.340326	-0.000071	0.304512
1.811990	-1.587551	0.345331	-0.000110	0.304421
1.698694	-1.612597	0.350336	-0.000089	0.304204
1.381071	-1.596479	0.355341	-0.000030	0.304007
1.733159	-1.687819	0.360346	-0.000096	0.303877
1.446125	-1.700531	0.365350	-0.000042	0.303568
1.193630	-1.676522	0.370355	0.000005	0.303464
1.413810	-1.762729	0.375360	-0.000036	0.303244
1.397773	-1.803739	0.380365	-0.000033	0.303034
0.944974	-1.744868	0.385370	0.000051	0.302923
0.656001	-1.753703	0.390374	0.000105	0.302630
1.372432	-1.918964	0.395379	-0.000029	0.302462
1.231543	-1.927297	0.400384	-0.000003	0.302300
0.988983	-1.949948	0.405389	0.000043	0.301981
0.872414	-1.951036	0.410394	0.000064	0.301874
1.022992	-2.016604	0.415398	0.000036	0.301691
0.791493	-2.039064	0.420403	0.000079	0.301382
0.772892	-2.066061	0.425408	0.000083	0.301236
1.011889	-2.150301	0.430413	0.000038	0.301040
1.010984	-2.212653	0.435418	0.000038	0.300740
0.745496	-2.192955	0.440422	0.000088	0.300603
1.168107	-2.302249	0.445427	0.000009	0.300447
0.782989	-2.293326	0.450432	0.000081	0.300153
0.623916	-2.313964	0.455437	0.000110	0.299914
0.980371	-2.418128	0.460442	0.000044	0.299724
0.413438	-2.360848	0.465446	0.000150	0.299503
0.040761	-2.345144	0.470451	0.000219	0.299252
-0.208450	-2.338761	0.475456	0.000265	0.299064
-0.068361	-2.405313	0.480461	0.000239	0.298866
-0.445936	-2.393774	0.485466	0.000309	0.298589
-1.119914	-2.312656	0.490470	0.000435	0.298389
-1.352977	-2.299742	0.495475	0.000478	0.298246
-1.760490	-2.282818	0.500480	0.000554	0.297969
-2.166173	-2.242059	0.505485	0.000629	0.297809
-2.343040	-2.246236	0.510490	0.000662	0.297633
-2.509514	-2.266872	0.515494	0.000693	0.297386
-2.932269	-2.210077	0.520499	0.000772	0.297288
-3.137667	-2.234573	0.525504	0.000810	0.296987
-3.404199	-2.206660	0.530509	0.000860	0.296888
-3.541340	-2.217271	0.535514	0.000885	0.296715
-3.744465	-2.223138	0.540518	0.000923	0.296506
-4.031981	-2.199182	0.545523	0.000976	0.296368
-4.083640	-2.238802	0.550528	0.000986	0.296129
-4.199468	-2.232746	0.555533	0.001008	0.296056
-4.172737	-2.299808	0.560538	0.001003	0.295752
-4.888729	-2.179692	0.565542	0.001136	0.295703
-4.905010	-2.216650	0.570547	0.001139	0.295508
-4.920650	-2.234807	0.575552	0.001142	0.295405
-5.154011	-2.243369	0.580557	0.001185	0.295156
-5.325897	-2.237379	0.585562	0.001217	0.295032
-5.630568	-2.220309	0.590566	0.001274	0.294844
-5.573395	-2.264914	0.595571	0.001263	0.294677
-6.097908	-2.199721	0.600576	0.001361	0.294529
-6.189883	-2.219494	0.605581	0.001378	0.294350
-7.078855	-2.075467	0.610586	0.001543	0.294264
-6.974977	-2.129358	0.615590	0.001524	0.294092
-7.447384	-2.076561	0.620595	0.001612	0.293929
-7.100896	-2.162309	0.625600	0.001547	0.293817
-6.960664	-2.234245	0.630605	0.001521	0.293588
-7.161268	-2.217370	0.635610	0.001558	0.293492
-7.222742	-2.252151	0.640614	0.001570	0.293266
-7.152900	-2.285998	0.645619	0.001557	0.293161
-7.460553	-2.268664	0.650624	0.001614	0.292971
-7.603744	-2.264805	0.655629	0.001641	0.292862
-7.876456	-2.260159	0.660634	0.001691	0.292640
-7.984711	-2.262041	0.665638	0.001711	0.292534
-7.954711	-2.312373	0.670643	0.001706	0.292312
-7.889527	-2.344079	0.675648	0.001694	0.292214
-8.928926	-2.197425	0.680653	0.001887	0.292004
-8.654494	-2.257777	0.685658	0.001836	0.291953
-8.755569	-2.289971	0.690662	0.001855	0.291702
-8.797270	-2.289221	0.695667	0.001863	0.291668
-9.292014	-2.257888	0.700672	0.001955	0.291378
-9.316335	-2.254507	0.705677	0.001959	0.291373
-9.221849	-2.330847	0.710682	0.001941	0.291079
-9.451227	-2.295064	0.715686	0.001984	0.291050
-9.662232	-2.309862	0.720691	0.002023	0.290786
-9.434967	-2.359897	0.725696	0.001981	0.290742
-9.887549	-2.319901	0.730701	0.002065	0.290532
-9.774672	-2.349397	0.735706	0.002044	0.290488
-10.006720	-2.357323	0.740710	0.002087	0.290238
-10.232459	-2.335495	0.745715	0.002129	0.290143
-10.277309	-2.367019	0.750720	0.002138	0.289945
-10.593827	-2.335355	0.755725	0.002197	0.289816
-10.656351	-2.352683	0.760730	0.002208	0.289673
-11.154545	-2.297449	0.765734	0.002301	0.289496
-11.021952	-2.340695	0.770739	0.002276	0.289401
-11.109468	-2.362119	0.775744	0.002292	0.289214
-11.458334	-2.308126	0.780749	0.002357	0.289167
-11.707696	-2.320706	0.785754	0.002404	0.288878
-11.691571	-2.325389	0.790758	0.002401	0.288869
-11.614845	-2.394826	0.795763	0.002386	0.288591
-12.226757	-2.289858	0.800768	0.002500	0.288560
-12.271430	-2.323218	0.805773	0.002508	0.288352
-12.074431	-2.380615	0.810778	0.002472	0.288244
-12.315344	-2.364921	0.815782	0.002517	0.288103
-12.670155	-2.332137	0.820787	0.002583	0.287944
-12.595057	-2.355874	0.825792	0.002569	0.287893
-12.994973	-2.340395	0.830797	0.002643	0.287606
-12.737818	-2.386039	0.835802	0.002595	0.287611
-13.246330	-2.354646	0.840806	0.002690	0.287304
-13.220772	-2.361472	0.845811	0.002685	0.287294
-13.459319	-2.359392	0.850816	0.002729	0.287086
-13.933743	-2.297393	0.855821	0.002818	0.286964
-13.577714	-2.378756	0.860826	0.002751	0.286880
-14.168541	-2.311840	0.865830	0.002861	0.286676
-14.399651	-2.267556	0.870835	0.002904	0.286687
-14.291235	-2.347406	0.875840	0.002884	0.286384
-14.435357	-2.328370	0.880845	0.002911	0.286348
-14.855097	-2.281434	0.885850	0.002989	0.286200
-14.904648	-2.304145	0.890854	0.002998	0.286039
-14.781644	-2.330175	0.895859	0.002975	0.286021
-15.110949	-2.327855	0.900864	0.003036	0.285730
-15.483062	-2.260284	0.905869	0.003106	0.285730
-15.394424	-2.303200	0.910874	0.003089	0.285594
-15.739952	-2.263362	0.915878	0.003153	0.285478
-15.767762	-2.264379	0.920883	0.003158	0.285447
-15.937568	-2.293123	0.925888	0.003190	0.285145
-15.692503	-2.340499	0.930893	0.003144	0.285131
-16.029148	-2.316619	0.935898	0.003207	0.284942
-16.509233	-2.253869	0.940902	0.003296	0.284817
-15.806908	-2.393176	0.945907	0.003166	0.284758
-16.509967	-2.315429	0.950912	0.003296	0.284504
-16.962000	-2.234080	0.955917	0.003381	0.284500
-16.629196	-2.330495	0.960922	0.003319	0.284317
-16.903743	-2.303143	0.965926	0.003370	0.284203
-16.886568	-2.317763	0.970931	0.003366	0.284144
-17.036960	-2.344784	0.975936	0.003394	0.283867
-17.193013	-2.317165	0.980941	0.003423	0.283864
-17.226965	-2.352062	0.985946	0.003430	0.283655
-17.719671	-2.281742	0.990950	0.003521	0.283556
-17.585384	-2.316864	0.995955	0.003496	0.283502
-17.968651	-2.297698	1.000960	0.003568	0.283244
-18.153609	-2.265623	1.005965	0.003602	0.283236
-18.146853	-2.297699	1.010970	0.003601	0.283079
-18.589434	-2.240721	1.015974	0.003683	0.282959
-18.763183	-2.209481	1.020979	0.003715	0.282957
-18.614773	-2.297573	1.025984	0.003688	0.282645
-18.789483	-2.272308	1.030989	0.003720	0.282612
-18.947640	-2.260903	1.035994	0.003750	0.282523
-19.724545	-2.162673	1.040998	0.003894	0.282303
-19.491571	-2.202761	1.046003	0.003851	0.282315
-19.305594	-2.269721	1.051008	0.003816	0.282145
-19.443032	-2.279690	1.056013	0.003842	0.281966
-19.510193	-2.265393	1.061018	0.003854	0.281977
-19.922193	-2.240482	1.066022	0.003931	0.281720
-20.081518	-2.217202	1.071027	0.003960	0.281691
-20.344901	-2.173869	1.076032	0.004009	0.281668
-20.757907	-2.157474	1.081037	0.004086	0.281366
-20.866700	-2.136745	1.086042	0.004106	0.281371
-21.247511	-2.072571	1.091046	0.004177	0.281346
-21.283701	-2.119367	1.096051	0.004184	0.281071
-21.200849	-2.133478	1.101056	0.004168	0.281076
-21.490839	-2.087653	1.106061	0.004222	0.281041
-20.972828	-2.241507	1.111066	0.004126	0.280734
-20.671337	-2.298871	1.116070	0.004070	0.280721
-20.953111	-2.266554	1.121075	0.004122	0.280623
-21.220400	-2.243284	1.126080	0.004172	0.280493
-21.012128	-2.282214	1.131085	0.004133	0.280488
-21.304718	-2.284870	1.136090	0.004188	0.280199
-21.899683	-2.186484	1.141094	0.004298	0.280149
-21.470833	-2.278286	1.146099	0.004218	0.280078
-21.709543	-2.281838	1.151104	0.004263	0.279835
-21.883346	-2.251998	1.156109	0.004295	0.279826
-21.987620	-2.272237	1.161114	0.004315	0.279624
-22.249324	-2.248456	1.166118	0.004363	0.279501
-22.232556	-2.251754	1.171123	0.004360	0.279500
-22.390553	-2.276531	1.176128	0.004389	0.279222
-22.695510	-2.222823	1.181133	0.004446	0.279214
-22.308209	-2.320671	1.186138	0.004374	0.279072
-22.994725	-2.233232	1.191142	0.004502	0.278878
-22.838821	-2.261416	1.196147	0.004473	0.278879
-22.868428	-2.302863	1.201152	0.004478	0.278636
-23.438252	-2.213169	1.206157	0.004584	0.278564
-23.513293	-2.205824	1.211162	0.004598	0.278531
-23.591354	-2.245268	1.216166	0.004613	0.278253
-23.479515	-2.266360	1.221171	0.004592	0.278249
-23.645281	-2.263088	1.226176	0.004623	0.278109
-24.115906	-2.206546	1.231181	0.004710	0.277958
-23.878828	-2.247706	1.236186	0.004666	0.277969
-24.258740	-2.234580	1.241190	0.004737	0.277677
-24.541056	-2.193622	1.246195	0.004789	0.277623
-24.307366	-2.241791	1.251200	0.004746	0.277594
-24.833327	-2.200666	1.256205	0.004844	0.277310
-24.672524	-2.229034	1.261210	0.004814	0.277315
-24.634799	-2.261792	1.266214	0.004807	0.277180
-24.799406	-2.269338	1.271219	0.004837	0.276984
-25.015938	-2.228534	1.276224	0.004877	0.276992
-25.231014	-2.235087	1.281229	0.004917	0.276753
-24.861746	-2.313559	1.286234	0.004849	0.276694
-25.239150	-2.257191	1.291238	0.004919	0.276630
-25.937219	-2.179149	1.296243	0.005049	0.276374
-25.523782	-2.255369	1.301248	0.004972	0.276369
-25.580962	-2.278311	1.306253	0.004982	0.276195
-25.882128	-2.250513	1.311258	0.005038	0.276054
-25.592745	-2.304620	1.316262	0.004984	0.276046
-25.743264	-2.332750	1.321267	0.005012	0.275755
-26.221478	-2.248999	1.326272	0.005101	0.275738
-26.343150	-2.244160	1.331277	0.005124	0.275648
-26.230685	-2.292656	1.336282	0.005103	0.275501
-26.319163	-2.278855	1.341286	0.005120	0.275489
-26.459407	-2.304842	1.346291	0.005146	0.275218
-26.638148	-2.284415	1.351296	0.005179	0.275155
-26.788952	-2.274056	1.356301	0.005207	0.275065
-27.136277	-2.252711	1.361306	0.005271	0.274846
-27.314038	-2.222016	1.366310	0.005305	0.274837
-27.491198	-2.224974	1.371315	0.005337	0.274652
-27.913382	-2.172313	1.376320	0.005416	0.274525
-27.693939	-2.214394	1.381325	0.005375	0.274514
-27.507293	-2.294732	1.386330	0.005340	0.274269
-28.404820	-2.139103	1.391334	0.005507	0.274229
-28.048417	-2.215194	1.396339	0.005441	0.274170
-28.168466	-2.245672	1.401344	0.005463	0.273894
-28.833673	-2.123399	1.406349	0.005587	0.273901
-28.691003	-2.171473	1.411354	0.005560	0.273784
-28.690151	-2.211856	1.416358	0.005560	0.273572
-28.328954	-2.276878	1.421363	0.005493	0.273575
-28.900606	-2.212896	1.426368	0.005599	0.273364
-29.317801	-2.157907	1.431373	0.005677	0.273254
-28.707747	-2.267312	1.436378	0.005563	0.273262
-29.437484	-2.189218	1.441382	0.005699	0.272973
-29.796698	-2.122207	1.446387	0.005766	0.272982
-29.243490	-2.236608	1.451392	0.005663	0.272909
-29.658680	-2.213758	1.456397	0.005740	0.272630
-29.561555	-2.230042	1.461402	0.005722	0.272637
-29.411458	-2.293037	1.466406	0.005694	0.272448
-29.712931	-2.263239	1.471411	0.005750	0.272315
-30.039546	-2.202446	1.476416	0.005811	0.272323
-30.393628	-2.200283	1.481421	0.005877	0.271992
-30.269571	-2.218500	1.486426	0.005854	0.272015
-30.187839	-2.254910	1.491430	0.005839	0.271901
-30.513370	-2.232595	1.496435	0.005899	0.271704
-30.586329	-2.217665	1.501440	0.005913	0.271713
-31.166505	-2.154858	1.506445	0.006021	0.271486
-31.256526	-2.156679	1.511450	0.006037	0.271389
-31.138955	-2.180079	1.516454	0.006015	0.271379
-31.653485	-2.131956	1.521459	0.006111	0.271136
-31.691056	-2.134248	1.526464	0.006118	0.271088
-32.010643	-2.077226	1.531469	0.006177	0.271082
-31.389692	-2.246041	1.536474	0.006062	0.270784
-31.506530	-2.230409	1.541478	0.006084	0.270754
-32.033967	-2.149135	1.546483	0.006182	0.270676
-31.787341	-2.227350	1.551488	0.006136	0.270497
-31.643882	-2.255628	1.556493	0.006109	0.270486
-31.931152	-2.247769	1.561498	0.006163	0.270248
-32.303820	-2.199097	1.566502	0.006232	0.270146
-32.094962	-2.244563	1.571507	0.006193	0.270106
-32.520472	-2.214672	1.576512	0.006272	0.269852
-33.002036	-2.128055	1.581517	0.006362	0.269847
-32.490597	-2.249427	1.586522	0.006266	0.269695
-32.914298	-2.206689	1.591526	0.006345	0.269511
-32.923909	-2.205241	1.596531	0.006347	0.269509
-32.912235	-2.251707	1.601536	0.006345	0.269271
-33.178375	-2.212182	1.606541	0.006394	0.269224
-33.082310	-2.245894	1.611546	0.006376	0.269137
-33.448041	-2.227601	1.616550	0.006444	0.268877
-33.264392	-2.259807	1.621555	0.006410	0.268884
-33.565339	-2.245815	1.626560	0.006466	0.268665
-34.191791	-2.148564	1.631565	0.006583	0.268575
-33.860565	-2.211467	1.636570	0.006521	0.268561
-34.013518	-2.240263	1.641574	0.006550	0.268256
-34.572350	-2.137787	1.646579	0.006654	0.268260
-34.904748	-2.092096	1.651584	0.006715	0.268181
-34.789956	-2.150352	1.656589	0.006694	0.267979
-34.372190	-2.226435	1.661594	0.006616	0.267979
-34.924307	-2.165663	1.666598	0.006719	0.267765
-34.802903	-2.213796	1.671603	0.006696	0.267624
-34.871684	-2.200718	1.676608	0.006709	0.267627
-35.389124	-2.165237	1.681613	0.006805	0.267310
-35.262017	-2.186731	1.686618	0.006782	0.267319
-34.914646	-2.273953	1.691622	0.006717	0.267189
-35.626175	-2.182843	1.696627	0.006849	0.266982
-35.507231	-2.203484	1.701632	0.006827	0.266987
-35.786426	-2.191633	1.706637	0.006879	0.266776
-35.774143	-2.206468	1.711642	0.006877	0.266708
-36.078517	-2.160275	1.716646	0.006933	0.266659
-35.932806	-2.240553	1.721651	0.006906	0.266367
-35.666365	-2.289433	1.726656	0.006857	0.266365
-36.248532	-2.221036	1.731661	0.006965	0.266161
-36.293898	-2.232244	1.736666	0.006973	0.266055
-36.181472	-2.258371	1.741670	0.006952	0.266025
-36.565187	-2.242207	1.746675	0.007024	0.265733
-36.794641	-2.199337	1.751680	0.007066	0.265739
-36.821682	-2.221692	1.756685	0.007071	0.265591
-37.198694	-2.170657	1.761690	0.007142	0.265495
-37.210775	-2.170842	1.766694	0.007144	0.265482
-37.230570	-2.225537	1.771699	0.007147	0.265165
-37.203216	-2.236675	1.776704	0.007142	0.265131
-37.492109	-2.206544	1.781709	0.007196	0.265009
-37.370768	-2.264761	1.786714	0.007173	0.264812
-37.460530	-2.249093	1.791718	0.007190	0.264808
-37.639602	-2.268828	1.796723	0.007223	0.264522
-38.225396	-2.167043	1.801728	0.007332	0.264496
-38.026597	-2.220415	1.806733	0.007295	0.264402
-38.071914	-2.247507	1.811738	0.007304	0.264209
-38.304265	-2.205882	1.816742	0.007347	0.264206
-38.605766	-2.198461	1.821747	0.007403	0.263946
-38.353933	-2.257975	1.826752	0.007356	0.263871
-38.559779	-2.234678	1.831757	0.007394	0.263793
-38.905507	-2.214834	1.836762	0.007459	0.263557
-38.818441	-2.231325	1.841766	0.007443	0.263554
-38.792687	-2.277579	1.846771	0.007438	0.263326
-39.202205	-2.219317	1.851776	0.007514	0.263237
-39.109622	-2.247610	1.856781	0.007497	0.263174
-38.788830	-2.347942	1.861786	0.007437	0.262943
-39.085426	-2.295203	1.866790	0.007492	0.262936
-39.688085	-2.236580	1.871795	0.007604	0.262656
-39.622443	-2.257013	1.876800	0.007592	0.262609
-39.674711	-2.268614	1.881805	0.007602	0.262493
-40.011627	-2.243683	1.886810	0.007664	0.262292
-39.608902	-2.318993	1.891814	0.007589	0.262281
-40.013895	-2.297571	1.896819	0.007665	0.261993
-40.291334	-2.250476	1.901824	0.007716	0.261974
-40.524533	-2.232406	1.906829	0.007760	0.261840
-40.565587	-2.253773	1.911834	0.007767	0.261681
-40.738027	-2.223969	1.916838	0.007799	0.261672
-40.762557	-2.275031	1.921843	0.007804	0.261365
-40.796164	-2.272122	1.926848	0.007810	0.261348
-41.060401	-2.250318	1.931853	0.007859	0.261202
-41.216190	-2.251203	1.936858	0.007888	0.261040
-41.119369	-2.270550	1.941862	0.007870	0.261031
-41.308899	-2.290731	1.946867	0.007905	0.260728
-41.437198	-2.269689	1.951872	0.007929	0.260715
-41.800762	-2.226710	1.956877	0.007997	0.260587
-41.631431	-2.277565	1.961882	0.007965	0.260476
-41.572840	-2.293200	1.966886	0.007954	0.260448
-41.708164	-2.326975	1.971891	0.007980	0.260123
-41.954323	-2.281381	1.976896	0.008025	0.260128
-42.407504	-2.236867	1.981901	0.008110	0.259917
-42.455666	-2.246477	1.986906	0.008119	0.259815
-42.298372	-2.286719	1.991910	0.008089	0.259750
-42.753167	-2.252471	1.996915	0.008174	0.259480
-42.812230	-2.256642	2.001920	0.008185	0.259397

-43.015633	-2.255230	2.011917	0.008223	0.259199
-43.415094	-2.236601	2.021914	0.008297	0.258897
-43.228346	-2.293621	2.031910	0.008262	0.258769
-43.659836	-2.255419	2.041907	0.008342	0.258543
-43.748037	-2.260055	2.051904	0.008359	0.258428
-44.017183	-2.246631	2.061901	0.008409	0.258229
-43.914334	-2.265319	2.071898	0.008389	0.258230
-44.050759	-2.286107	2.081894	0.008415	0.257974
-44.273413	-2.252758	2.091891	0.008456	0.257935
-44.452872	-2.218934	2.101888	0.008489	0.257942
-44.163329	-2.275520	2.111885	0.008435	0.257920
-44.588401	-2.255534	2.121882	0.008514	0.257599
-44.570952	-2.258414	2.131878	0.008511	0.257601
-44.538511	-2.265363	2.141875	0.008505	0.257595
-44.453734	-2.280760	2.151872	0.008489	0.257596
-44.586286	-2.255743	2.161869	0.008514	0.257601
-44.411447	-2.288369	2.171866	0.008481	0.257597
-44.606561	-2.252331	2.181862	0.008517	0.257601
-44.594726	-2.255281	2.191859	0.008515	0.257597
-44.673526	-2.240327	2.201856	0.008530	0.257601
-44.656249	-2.220403	2.211853	0.008526	0.257731
-44.716678	-2.170629	2.221850	0.008537	0.257949
-44.236596	-2.258306	2.231846	0.008448	0.257948
-44.582423	-2.196372	2.241843	0.008512	0.257943
-44.300136	-2.248436	2.251840	0.008460	0.257939
-43.966255	-2.267658	2.261837	0.008397	0.258173
-44.384674	-2.179189	2.271834	0.008475	0.258243
-44.187064	-2.216144	2.281830	0.008438	0.258237
-44.006327	-2.215698	2.291827	0.008405	0.258425
-43.805219	-2.229192	2.301824	0.008367	0.258555
-43.746542	-2.239136	2.311821	0.008356	0.258559
-44.000781	-2.149072	2.321818	0.008403	0.258805
-43.487359	-2.230966	2.331814	0.008308	0.258870
-43.693231	-2.164101	2.341811	0.008346	0.259035
-43.363966	-2.192726	2.351808	0.008284	0.259210
-43.606357	-2.128425	2.361805	0.008329	0.259323
-43.145169	-2.180335	2.371802	0.008244	0.259502
-43.238089	-2.135063	2.381798	0.008261	0.259661
-42.983045	-2.152243	2.391795	0.008213	0.259825
-42.527749	-2.205087	2.401792	0.008128	0.259992
-42.955682	-2.097651	2.411789	0.008208	0.260157
-42.430492	-2.147509	2.421786	0.008110	0.260412
-42.300400	-2.157185	2.431782	0.008086	0.260490
-42.203600	-2.132073	2.441779	0.008068	0.260728
-41.805785	-2.186853	2.451776	0.007993	0.260826
-41.627220	-2.180289	2.461773	0.007960	0.261044
-41.312975	-2.204587	2.471770	0.007902	0.261226
-41.806294	-2.086725	2.481766	0.007993	0.261383
-41.422904	-2.100109	2.491763	0.007922	0.261695
-41.391016	-2.077308	2.501760	0.007916	0.261854
-41.503095	-2.021107	2.511757	0.007936	0.262052
-40.763127	-2.108777	2.521754	0.007799	0.262312
-40.630751	-2.094630	2.531750	0.007774	0.262524
-40.576539	-2.073138	2.541747	0.007764	0.262697
-39.984917	-2.133338	2.551744	0.007654	0.262959
-39.893775	-2.108662	2.561741	0.007636	0.263186
-39.733836	-2.105626	2.571738	0.007607	0.263363
-39.282527	-2.151171	2.581734	0.007522	0.263565
-39.029796	-2.148080	2.591731	0.007475	0.263835
-39.074255	-2.107067	2.601728	0.007483	0.264016
-38.700926	-2.138684	2.611725	0.007414	0.264215
-38.319136	-2.156838	2.621722	0.007343	0.264497
-38.113110	-2.161755	2.631718	0.007304	0.264675
-37.861503	-2.177616	2.641715	0.007257	0.264840
-37.531786	-2.183481	2.651712	0.007196	0.265136
-37.514104	-2.149340	2.661709	0.007192	0.265340
-37.157868	-2.178217	2.671706	0.007126	0.265537
-36.993662	-2.170865	2.681702	0.007095	0.265740
-36.287248	-2.258801	2.691699	0.006964	0.265961
-36.315950	-2.225452	2.701696	0.006969	0.266115
-36.050161	-2.228384	2.711693	0.006920	0.266362
-35.561126	-2.273352	2.721690	0.006828	0.266602
-35.861937	-2.186099	2.731686	0.006884	0.266779
-35.059515	-2.296886	2.741683	0.006735	0.266970
-35.150800	-2.232724	2.751680	0.006752	0.267228
-35.172260	-2.195456	2.761677	0.006756	0.267410
-34.601321	-2.260489	2.771674	0.006649	0.267620
-34.555767	-2.211282	2.781670	0.006641	0.267932
-34.276868	-2.229512	2.791667	0.006589	0.268108
-33.997229	-2.249179	2.801664	0.006537	0.268276
-33.779468	-2.234062	2.811661	0.006496	0.268572
-33.436984	-2.256651	2.821658	0.006432	0.268787
-33.604212	-2.190115	2.831654	0.006463	0.268982
-33.013435	-2.254185	2.841651	0.006353	0.269215
-32.736684	-2.257439	2.851648	0.006301	0.269469
-32.651727	-2.238051	2.861645	0.006285	0.269657
-32.355468	-2.251876	2.871642	0.006230	0.269872
-32.249656	-2.219568	2.881638	0.006210	0.270149
-31.640400	-2.284405	2.891635	0.006097	0.270396
-31.836096	-2.215826	2.901632	0.006133	0.270573
-31.255499	-2.288970	2.911629	0.006025	0.270747
-31.343734	-2.215404	2.921626	0.006041	0.271055
-31.265362	-2.191122	2.931622	0.006027	0.271261
-30.780996	-2.240876	2.941619	0.005936	0.271466
-30.462168	-2.254581	2.951616	0.005877	0.271702
-30.223419	-2.245748	2.961613	0.005832	0.271981
-29.844444	-2.276727	2.971610	0.005762	0.272183
-29.702306	-2.267309	2.981606	0.005735	0.272371
-29.364765	-2.280922	2.991603	0.005672	0.272626
-29.284885	-2.243351	3.001600	0.005657	0.272903
-29.074836	-2.242349	3.011597	0.005618	0.273111
-28.877449	-2.239955	3.021594	0.005581	0.273314
-28.742827	-2.214477	3.031590	0.005556	0.273579
-28.371671	-2.232622	3.041587	0.005487	0.273841
-28.500155	-2.164769	3.051584	0.005511	0.274076
-27.879850	-2.233933	3.061581	0.005395	0.274307
-27.693135	-2.228135	3.071578	0.005360	0.274518
-27.405183	-2.221000	3.081574	0.005307	0.274832
-27.236865	-2.209934	3.091571	0.005275	0.275052
-27.015165	-2.208282	3.101568	0.005234	0.275273
-26.278776	-2.300134	3.111565	0.005097	0.275494
-26.086170	-2.290119	3.121562	0.005061	0.275731
-26.045322	-2.260445	3.131558	0.005053	0.275927
-25.828678	-2.259850	3.141555	0.005013	0.276137
-25.729638	-2.234990	3.151552	0.004994	0.276362
-25.249121	-2.261395	3.161549	0.004904	0.276682
-25.376517	-2.200145	3.171546	0.004928	0.276881
-24.884626	-2.246898	3.181542	0.004836	0.277105
-24.703274	-2.239578	3.191539	0.004803	0.277316
-24.516330	-2.213951	3.201536	0.004768	0.277627
-23.955866	-2.268116	3.211533	0.004663	0.277876
-23.980170	-2.225031	3.221530	0.004668	0.278078
-23.653344	-2.245256	3.231526	0.004607	0.278283
-23.420450	-2.232361	3.241523	0.004563	0.278570
-23.144882	-2.235564	3.251520	0.004512	0.278814
-22.833498	-2.249012	3.261517	0.004454	0.279039
-22.632300	-2.243085	3.271514	0.004416	0.279260
-22.187591	-2.276613	3.281510	0.004333	0.279506
-22.219998	-2.221824	3.291507	0.004339	0.279759
-21.909840	-2.234473	3.301504	0.004281	0.279986
-21.601154	-2.248342	3.311501	0.004224	0.280205
-21.258390	-2.255155	3.321498	0.004160	0.280492
-21.100206	-2.247222	3.331494	0.004130	0.280682
-21.316167	-2.163484	3.341491	0.004171	0.280911
-20.850155	-2.206334	3.351488	0.004084	0.281127
-20.462712	-2.232794	3.361485	0.004012	0.281354
-20.096480	-2.236047	3.371482	0.003943	0.281680
-19.897350	-2.233229	3.381478	0.003906	0.281881
-19.616380	-2.244665	3.391475	0.003854	0.282085
-19.292904	-2.262310	3.401472	0.003793	0.282297
-18.879722	-2.277291	3.411469	0.003716	0.282605
-18.821983	-2.244317	3.421466	0.003706	0.282828
-18.475329	-2.265504	3.431462	0.003641	0.283043
-18.576518	-2.206407	3.441459	0.003660	0.283251
-18.032578	-2.245586	3.451456	0.003558	0.283557
-17.923605	-2.222580	3.461453	0.003538	0.283776
-17.646131	-2.230840	3.471450	0.003486	0.283991
-17.046965	-2.298333	3.481446	0.003375	0.284203
-17.198268	-2.214437	3.491443	0.003403	0.284490
-16.741076	-2.250890	3.501440	0.003317	0.284728
-16.681895	-2.221271	3.511437	0.003306	0.284934
-16.203580	-2.266925	3.521434	0.003217	0.285144
-15.880754	-2.260094	3.531430	0.003157	0.285477
-15.836487	-2.235959	3.541427	0.003149	0.285640
-15.513897	-2.258173	3.551424	0.003088	0.285825
-15.703489	-2.173516	3.561421	0.003124	0.286080
-15.109366	-2.225865	3.571418	0.003013	0.286362
-15.142865	-2.167506	3.581414	0.003019	0.286626
-15.166090	-2.117589	3.591411	0.003023	0.286857
-14.621651	-2.172681	3.601408	0.002922	0.287079
-14.095986	-2.223346	3.611405	0.002824	0.287306
-14.055780	-2.166873	3.621402	0.002816	0.287627
-13.544829	-2.213366	3.631398	0.002721	0.287861
-13.447769	-2.190429	3.641395	0.002703	0.288065
-12.683788	-2.294406	3.651392	0.002561	0.288241
-12.726082	-2.222514	3.661389	0.002568	0.288564
-12.001171	-2.316200	3.671386	0.002433	0.288755
-12.201899	-2.239496	3.681382	0.002471	0.288957
-11.895017	-2.242709	3.691379	0.002413	0.289221
-11.938648	-2.184347	3.701376	0.002421	0.289473
-11.953393	-2.134555	3.711373	0.002424	0.289709
-11.001625	-2.266701	3.721370	0.002247	0.289914
-10.903221	-2.237707	3.731366	0.002228	0.290148
-10.509394	-2.249176	3.741363	0.002155	0.290448
-10.155490	-2.282848	3.751360	0.002089	0.290601
-9.953373	-2.289484	3.761357	0.002051	0.290752
-9.694428	-2.273403	3.771354	0.002003	0.291066
-9.624229	-2.246710	3.781350	0.001990	0.291263
-9.041371	-2.319422	3.791347	0.001881	0.291428
-8.927061	-2.285695	3.801344	0.001860	0.291699
-8.652214	-2.290129	3.811341	0.001809	0.291925
-8.335590	-2.312932	3.821338	0.001750	0.292098
-8.160440	-2.302503	3.831334	0.001717	0.292308
-8.053882	-2.263176	3.841331	0.001697	0.292599
-7.842214	-2.260201	3.851328	0.001657	0.292804
-7.433227	-2.295398	3.861325	0.001581	0.292998
-7.099718	-2.304666	3.871322	0.001519	0.293252
-7.082135	-2.261743	3.881318	0.001516	0.293480
-6.826806	-2.269429	3.891315	0.001468	0.293671
-6.695719	-2.250502	3.901312	0.001443	0.293882
-6.493534	-2.221862	3.911309	0.001406	0.294204
-6.356668	-2.207103	3.921306	0.001380	0.294399
-6.350465	-2.161722	3.931302	0.001379	0.294628
-6.176331	-2.144038	3.941299	0.001346	0.294871
-6.015361	-2.115213	3.951296	0.001316	0.295156
-6.002501	-2.056020	3.961293	0.001314	0.295458
-6.064813	-1.999116	3.971290	0.001325	0.295682
-5.679891	-2.019238	3.981286	0.001253	0.295926
-5.841327	-1.931501	3.991283	0.001283	0.296212
-5.196134	-1.994150	4.001280	0.001163	0.296479
-5.223594	-1.928798	4.011277	0.001168	0.296774
-4.531583	-2.006792	4.021274	0.001039	0.297007
-4.340718	-1.979077	4.031270	0.001004	0.297311
-4.532937	-1.886624	4.041267	0.001039	0.297591
-4.156658	-1.892777	4.051264	0.000969	0.297894
-4.149410	-1.838520	4.061261	0.000968	0.298165
-3.794363	-1.844494	4.071258	0.000901	0.298449
-3.991422	-1.747504	4.081254	0.000938	0.298746
-4.091249	-1.661515	4.091251	0.000956	0.299075
-4.124623	-1.586348	4.101248	0.000963	0.299409
-3.662656	-1.605136	4.111245	0.000876	0.299724
-3.210870	-1.620018	4.121242	0.000792	0.300049
-3.331365	-1.528621	4.131238	0.000815	0.300384
-3.015403	-1.527038	4.141235	0.000756	0.300669
-3.101160	-1.446744	4.151232	0.000771	0.300981
-2.785411	-1.435215	4.161229	0.000713	0.301312
-2.618070	-1.390460	4.171226	0.000681	0.301673
-2.436576	-1.355491	4.181222	0.000647	0.301999
-2.283416	-1.308052	4.191219	0.000619	0.302360
-2.004875	-1.285603	4.201216	0.000567	0.302710
-1.884735	-1.233438	4.211213	0.000544	0.303064
-1.599355	-1.213470	4.221210	0.000491	0.303407
-1.666926	-1.127072	4.231206	0.000503	0.303761
-1.786980	-1.022542	4.241203	0.000526	0.304155
-1.907080	-0.920261	4.251200	0.000548	0.304538
-1.674943	-0.875341	4.261197	0.000505	0.304952
-1.450323	-0.833071	4.271194	0.000463	0.305346
-1.669059	-0.717126	4.281190	0.000503	0.305707
-1.225294	-0.704073	4.291187	0.000420	0.306151
-1.239209	-0.617102	4.301184	0.000423	0.306550
-0.782427	-0.619541	4.311181	0.000338	0.306930
-0.946824	-0.490701	4.321178	0.000368	0.307397
-0.933902	-0.402379	4.331174	0.000366	0.307824
-0.588836	-0.378368	4.341171	0.000301	0.308231
-0.609668	-0.274000	4.351168	0.000305	0.308704
-0.427968	-0.217206	4.361165	0.000271	0.309125
-0.551227	-0.090923	4.371162	0.000294	0.309611
0.000000	-0.100219	4.381158	0.000191	0.310035

-0.047730	0.182219	4.386163	0.000200	0.311311
0.560200	0.636647	4.391168	0.000086	0.313925
0.967965	1.419290	4.396173	0.000010	0.317849
1.088668	2.540765	4.401178	-0.000013	0.323012
1.909949	3.830441	4.406182	-0.000167	0.329393
3.400248	5.296286	4.411187	-0.000446	0.336933
4.726857	7.096075	4.416192	-0.000694	0.345584
7.190551	9.021879	4.421197	-0.001154	0.355378
13.028927	10.652772	4.426202	-0.002242	0.366163
22.521271	12.013969	4.431206	-0.004011	0.378142
29.036284	14.313348	4.436211	-0.005225	0.391223
36.771856	16.781271	4.441216	-0.006667	0.405269
42.856685	19.965908	4.446221	-0.007802	0.420279
48.693759	23.591313	4.451226	-0.008892	0.436080
52.552041	27.970692	4.456230	-0.009613	0.452592
55.867787	32.844402	4.461235	-0.010234	0.469739
57.841093	38.325824	4.466240	-0.010605	0.487364
59.806433	44.180211	4.471245	-0.010974	0.505435
62.099661	50.321977	4.476250	-0.011406	0.523837
64.088887	56.864845	4.481254	-0.011780	0.542535
65.839676	63.787506	4.486259	-0.012111	0.561475
68.124696	70.925119	4.491264	-0.012541	0.580569
70.064958	78.441067	4.496269	-0.012907	0.599816
72.401704	86.159567	4.501274	-0.013347	0.619100
74.455354	94.214006	4.506278	-0.013735	0.638446
76.958937	102.439748	4.511283	-0.014207	0.657773
80.131547	110.770228	4.516288	-0.014803	0.677025
84.957216	119.037886	4.521293	-0.015707	0.696223
89.530071	127.580772	4.526298	-0.016564	0.715366
94.132762	136.314090	4.531302	-0.017427	0.734391
97.904729	145.380507	4.536307	-0.018135	0.753286
103.031565	154.344947	4.541312	-0.019095	0.771974
107.069872	163.654270	4.546317	-0.019853	0.790494
110.518873	173.162319	4.551322	-0.020502	0.808754
116.156917	182.383484	4.556326	-0.021558	0.826783
121.398632	191.778562	4.561331	-0.022540	0.844600
125.161306	201.490544	4.566336	-0.023247	0.862138
129.499731	211.130248	4.571341	-0.024061	0.879371
132.843307	220.970038	4.576346	-0.024690	0.896310
135.774591	230.883798	4.581350	-0.025242	0.912935
139.266580	240.671346	4.586355	-0.025899	0.929216
141.909247	250.589851	4.591360	-0.026398	0.945187
145.298588	260.340956	4.596365	-0.027035	0.960836
148.603990	270.073133	4.601370	-0.027657	0.976181
151.548997	279.830988	4.606374	-0.028212	0.991233
153.121610	289.763064	4.611379	-0.028511	1.005965
155.896562	299.360647	4.616384	-0.029034	1.020306
158.467778	308.970355	4.621389	-0.029519	1.034413
160.758157	318.562844	4.626394	-0.029952	1.048239
162.895319	328.120228	4.631398	-0.030356	1.061799
164.750011	337.662655	4.636403	-0.030708	1.075102
166.151161	347.166854	4.641408	-0.030975	1.088086
167.803030	356.588081	4.646413	-0.031289	1.100864
169.351578	365.929369	4.651418	-0.031583	1.113369
170.253705	375.305569	4.656422	-0.031757	1.125635
171.661926	384.536980	4.661427	-0.032025	1.137696
172.822805	393.750856	4.666432	-0.032248	1.149554
173.907144	402.905232	4.671437	-0.032456	1.161201
175.507286	411.892109	4.676442	-0.032759	1.172634
177.055414	420.836986	4.681446	-0.033054	1.183893
178.379196	429.784380	4.686451	-0.033306	1.195003
179.083923	438.777504	4.691456	-0.033443	1.205938
179.959429	447.701559	4.696461	-0.033612	1.216727
181.742658	456.400250	4.701466	-0.033950	1.227338
183.027629	465.182668	4.706470	-0.034195	1.237855
184.331777	473.905069	4.711475	-0.034443	1.248218
184.810930	482.731395	4.716480	-0.034538	1.258454
185.563521	491.477497	4.721485	-0.034684	1.268568
186.724250	500.082846	4.726490	-0.034906	1.278522
187.870331	508.663040	4.731494	-0.035125	1.288366
188.656489	517.324707	4.736499	-0.035277	1.298159
189.668371	525.911933	4.741504	-0.035471	1.307838
190.925882	534.485910	4.746509	-0.035711	1.317476
191.352737	543.085828	4.751514	-0.035796	1.326920
191.532773	551.709121	4.756518	-0.035835	1.336278
192.159240	560.213519	4.761523	-0.035957	1.345524
192.738817	568.697566	4.766528	-0.036071	1.354676
193.679800	577.088048	4.771533	-0.036252	1.363731
194.170729	585.577571	4.776538	-0.036349	1.372752
194.445866	594.073767	4.781542	-0.036405	1.381683
194.863545	602.548108	4.786547	-0.036489	1.390558
196.335686	610.758989	4.791552	-0.036768	1.399286
197.044023	619.154523	4.796557	-0.036906	1.408018
197.529602	627.570803	4.801562	-0.037002	1.416680
197.716162	636.007138	4.806566	-0.037042	1.425259
198.579598	644.348926	4.811571	-0.037208	1.433804
199.475216	652.624362	4.816576	-0.037380	1.442238
200.249130	660.948091	4.821581	-0.037530	1.450650
200.709913	669.322867	4.826586	-0.037621	1.459012
201.017361	677.711813	4.831590	-0.037684	1.467316
201.513260	686.076240	4.836595	-0.037782	1.475579
202.122964	694.336266	4.841600	-0.037901	1.483713
202.769876	702.642720	4.846605	-0.038027	1.491853
202.978086	710.997653	4.851610	-0.038071	1.499927
203.204860	719.329026	4.856614	-0.038119	1.507937
203.935544	727.560023	4.861619	-0.038260	1.515887
204.177626	735.855578	4.866624	-0.038311	1.523782
205.287598	744.030127	4.871629	-0.038523	1.531655
205.736328	752.319508	4.876634	-0.038612	1.539494
206.142762	760.597229	4.881638	-0.038693	1.547276
206.973802	768.812224	4.886643	-0.038853	1.555024
207.403938	777.066106	4.891648	-0.038938	1.562710
207.823068	785.342896	4.896653	-0.039022	1.570378
208.594134	793.541020	4.901658	-0.039171	1.577988
208.940810	801.799888	4.906662	-0.039241	1.585554
209.319887	810.083090	4.911667	-0.039317	1.593111
210.218349	818.208273	4.916672	-0.039489	1.600565
210.412572	826.528594	4.921677	-0.039531	1.608057
210.706816	834.786263	4.926682	-0.039591	1.615473
211.559134	842.932728	4.931686	-0.039755	1.622836
212.158032	851.181157	4.936691	-0.039872	1.630220
212.643717	859.409815	4.941696	-0.039968	1.637536
213.678333	867.508401	4.946701	-0.040166	1.644783
214.149114	875.747522	4.951706	-0.040259	1.652042
214.551345	883.961313	4.956710	-0.040339	1.659238
215.177395	892.142900	4.961715	-0.040461	1.666405
215.502772	900.387017	4.966720	-0.040527	1.673554
215.496938	908.664153	4.971725	-0.040532	1.680655
215.781415	916.879218	4.976730	-0.040590	1.687713
216.553695	925.000090	4.981734	-0.040739	1.694728
217.278979	933.145923	4.986739	-0.040880	1.701728
217.295582	941.416035	4.991744	-0.040888	1.708709
218.205611	949.522270	4.996749	-0.041063	1.715642
218.748169	957.677230	5.001754	-0.041169	1.722540
218.998764	965.894748	5.006758	-0.041221	1.729424
219.595253	974.067947	5.011763	-0.041338	1.736289
219.848739	982.275246	5.016768	-0.041390	1.743110
220.915451	990.354051	5.021773	-0.041594	1.749904
222.200033	998.401898	5.026778	-0.041839	1.756674
223.197920	1006.518741	5.031782	-0.042030	1.763437
223.671443	1014.764298	5.036787	-0.042124	1.770212
223.984946	1022.964937	5.041792	-0.042187	1.776904
224.645000	1031.120976	5.046797	-0.042316	1.783579
225.329353	1039.292043	5.051802	-0.042448	1.790243
225.508755	1047.531417	5.056806	-0.042487	1.796875
226.096336	1055.671160	5.061811	-0.042602	1.803453
226.540669	1063.816889	5.066816	-0.042690	1.809994
227.516564	1071.907293	5.071821	-0.042877	1.816533
227.836645	1080.092627	5.076826	-0.042942	1.823043
228.402727	1088.240586	5.081830	-0.043053	1.829530
228.946149	1096.403202	5.086835	-0.043159	1.836003
228.915270	1104.605457	5.091840	-0.043159	1.842415
229.511905	1112.736951	5.096845	-0.043275	1.848825
229.622055	1120.945418	5.101850	-0.043301	1.855214
230.102743	1129.067487	5.106854	-0.043396	1.861558
230.331083	1137.265933	5.111859	-0.043444	1.867910
230.757838	1145.392807	5.116864	-0.043529	1.874208
232.010180	1153.355345	5.121869	-0.043767	1.880456
232.586155	1161.483780	5.126874	-0.043880	1.886730
233.106181	1169.631714	5.131878	-0.043982	1.892992
233.661774	1177.782544	5.136883	-0.044091	1.899240
233.692535	1185.978501	5.141888	-0.044102	1.905440
234.219390	1194.106589	5.146893	-0.044205	1.911626
234.286889	1202.300357	5.151898	-0.044223	1.917789
234.858844	1210.372137	5.156902	-0.044335	1.923899
235.436111	1218.498414	5.161907	-0.044448	1.930029
236.409123	1226.514168	5.166912	-0.044634	1.936103
236.529182	1234.721104	5.171917	-0.044662	1.942204
237.056875	1242.856616	5.176922	-0.044766	1.948278
237.624290	1250.938208	5.181926	-0.044877	1.954297
238.146888	1259.047498	5.186931	-0.044979	1.960314
238.502547	1267.157498	5.191936	-0.045051	1.966294
238.454879	1275.380787	5.196941	-0.045047	1.972294
238.948405	1283.472739	5.201946	-0.045145	1.978240
239.413104	1291.552220	5.206950	-0.045237	1.984155
239.800337	1299.705592	5.211955	-0.045314	1.990098
240.030517	1307.827586	5.216960	-0.045362	1.995983
240.836417	1315.856333	5.221965	-0.045517	2.001846
241.438449	1323.950299	5.226970	-0.045635	2.007716
241.477097	1332.131145	5.231974	-0.045647	2.013571
241.989049	1340.235426	5.236979	-0.045748	2.019405
242.432912	1348.317392	5.241984	-0.045836	2.025199
243.245694	1356.378250	5.246989	-0.045993	2.031000
243.707108	1364.497930	5.251994	-0.046084	2.036789
243.792464	1372.634933	5.256998	-0.046105	2.042534
244.419968	1380.726869	5.262003	-0.046227	2.048288
244.771174	1388.836795	5.267008	-0.046298	2.054010
245.118511	1396.959027	5.272013	-0.046368	2.059724
245.152960	1405.119519	5.277018	-0.046380	2.065417
245.338166	1413.253731	5.282022	-0.046420	2.071091
245.699000	1421.352483	5.287027	-0.046492	2.076742
245.996475	1429.424535	5.292032	-0.046553	2.082354
246.343385	1437.526588	5.297037	-0.046623	2.087976
247.170739	1445.555989	5.302042	-0.046782	2.093581
247.081545	1453.727503	5.307046	-0.046771	2.099176
247.859924	1461.759963	5.312051	-0.046921	2.104748
247.822021	1469.925463	5.317056	-0.046919	2.110315
248.134960	1478.055236	5.322061	-0.046983	2.115878
248.015757	1486.192972	5.327066	-0.046966	2.121389
248.224746	1494.261412	5.332070	-0.047010	2.126871
248.601477	1502.346544	5.337075	-0.047086	2.132366
249.109698	1510.371681	5.342080	-0.047186	2.137820
249.307259	1518.494080	5.347085	-0.047228	2.143295
249.747988	1526.580763	5.352090	-0.047315	2.148755
250.126759	1534.644404	5.357094	-0.047391	2.154180
250.762109	1542.687907	5.362099	-0.047515	2.159602
250.630461	1550.825485	5.367104	-0.047496	2.165000
251.277153	1558.876969	5.372109	-0.047621	2.170402
251.315551	1567.031601	5.377114	-0.047634	2.175800
251.854567	1575.045876	5.382118	-0.047739	2.181140
252.532079	1583.094201	5.387123	-0.047871	2.186502
252.187197	1591.308396	5.392128	-0.047812	2.191864
252.647957	1599.375598	5.397133	-0.047903	2.197191
252.586270	1607.502609	5.402138	-0.047897	2.202497
253.452327	1615.454785	5.407142	-0.048063	2.207761
254.109522	1623.514513	5.412147	-0.048191	2.213063
254.283907	1631.634293	5.417152	-0.048229	2.218348
255.019026	1639.653470	5.422157	-0.048371	2.223605
255.413153	1647.761243	5.427162	-0.048450	2.228876
255.480455	1655.898799	5.432166	-0.048468	2.234125
255.658138	1664.012091	5.437171	-0.048506	2.239355
256.414797	1671.985078	5.442176	-0.048652	2.244535
256.857676	1680.085959	5.447181	-0.048740	2.249757
256.814663	1688.251887	5.452186	-0.048737	2.254964
257.354212	1696.278520	5.457190	-0.048843	2.260123
257.445463	1704.437559	5.462195	-0.048865	2.265314
257.674289	1712.519805	5.467200	-0.048913	2.270457
257.912353	1720.634590	5.472205	-0.048963	2.275610
258.282894	1728.669555	5.477210	-0.049037	2.280712
258.646263	1736.680092	5.482214	-0.049110	2.285787
258.884860	1744.784934	5.487219	-0.049160	2.290898
259.038987	1752.876599	5.492224	-0.049194	2.295983
259.933172	1760.838932	5.497229	-0.049366	2.301039
260.193893	1768.932782	5.502234	-0.049420	2.306112
260.508652	1777.021647	5.507238	-0.049483	2.311175
260.430441	1785.184006	5.512243	-0.049474	2.316239
260.549912	1793.244531	5.517248	-0.049502	2.321245
261.081938	1801.264997	5.522253	-0.049606	2.326251
261.491887	1809.343121	5.527258	-0.049688	2.331272
261.682637	1817.427804	5.532262	-0.049729	2.336267
262.061650	1825.497375	5.537267	-0.049804	2.341258
262.619356	1833.508610	5.542272	-0.049914	2.346217
262.731917	1841.649603	5.547277	-0.049940	2.351208
263.165794	1849.702647	5.552282	-0.050026	2.356161
263.588367	1857.714469	5.557286	-0.050110	2.361078
264.179136	1865.770356	5.562291	-0.050225	2.366025
263.961287	1873.933085	5.567296	-0.050190	2.370960
264.511381	1881.978491	5.572301	-0.050298	2.375877
265.038384	1890.004235	5.577306	-0.050401	2.380770
265.141150	1898.084564	5.582310	-0.050426	2.385651
265.175996	1906.236099	5.587315	-0.050437	2.390559
265.728625	1914.215710	5.592320	-0.050546	2.395396
266.188386	1922.268865	5.597325	-0.050636	2.400259
265.973705	1930.424550	5.602330	-0.050602	2.405120
265.786328	1938.556302	5.607334	-0.050572	2.409959
265.809774	1946.664070	5.612339	-0.050582	2.414791
266.534762	1954.598898	5.617344	-0.050722	2.419566
266.943092	1962.637866	5.622349	-0.050804	2.424368
267.114269	1970.753605	5.627354	-0.050841	2.429187
267.444863	1978.846710	5.632358	-0.050908	2.433996
267.653646	1986.914175	5.637363	-0.050952	2.438770
267.526226	1994.981840	5.642368	-0.050933	2.443510
268.532906	2002.899260	5.647373	-0.051126	2.448239
268.614452	2011.016822	5.652378	-0.051147	2.453006
268.664321	2019.105284	5.657382	-0.051161	2.457743
269.546434	2027.073684	5.662387	-0.051331	2.462465
269.119656	2035.250547	5.667392	-0.051257	2.467200
269.194760	2043.344792	5.672397	-0.051276	2.471915
270.141775	2051.288155	5.677402	-0.051457	2.476600
270.441279	2059.319191	5.682406	-0.051518	2.481278
270.526397	2067.441653	5.687411	-0.051540	2.485984
270.998553	2075.463893	5.692416	-0.051633	2.490652
270.832996	2083.626540	5.697421	-0.051607	2.495344
271.243810	2091.659456	5.702426	-0.051689	2.499996
271.315375	2099.732050	5.707430	-0.051708	2.504637
272.105264	2107.724389	5.712435	-0.051860	2.509276
272.094702	2115.832887	5.717440	-0.051863	2.513914
272.121175	2123.899314	5.722445	-0.051874	2.518522
272.689642	2131.890055	5.727450	-0.051985	2.523118
272.809693	2139.964484	5.732454	-0.052012	2.527721
273.387079	2148.004244	5.737459	-0.052125	2.532329
273.577733	2156.078921	5.742464	-0.052166	2.536920
273.829862	2164.142522	5.747469	-0.052218	2.541501
274.020451	2172.220973	5.752474	-0.052259	2.546077
273.850783	2180.338251	5.757478	-0.052233	2.550642
274.730931	2188.314035	5.762483	-0.052402	2.555194
274.646244	2196.410322	5.767488	-0.052391	2.559736
274.820404	2204.437301	5.772493	-0.052429	2.564250
275.073529	2212.515675	5.777498	-0.052482	2.568790
275.542937	2220.529622	5.782502	-0.052574	2.573301
275.726666	2228.614285	5.787507	-0.052614	2.577824
275.801513	2236.677375	5.792512	-0.052633	2.582319
276.032671	2244.751696	5.797517	-0.052681	2.586823
276.423757	2252.829932	5.802522	-0.052760	2.591333
276.415331	2260.964604	5.807526	-0.052763	2.595839
276.874181	2268.948445	5.812531	-0.052854	2.600285
277.158713	2276.931039	5.817536	-0.052912	2.604711
276.963242	2285.039701	5.822541	-0.052881	2.609166
277.374161	2293.072904	5.827546	-0.052963	2.613614
277.436489	2301.127176	5.832550	-0.052980	2.618042
277.850799	2309.142114	5.837555	-0.053062	2.622464
277.863700	2317.216257	5.842560	-0.053070	2.626884
278.567972	2325.208913	5.847565	-0.053206	2.631300
278.798092	2333.295474	5.852570	-0.053254	2.635726
279.100755	2341.314779	5.857574	-0.053316	2.640114
279.520075	2349.327718	5.862579	-0.053399	2.644498
279.711271	2357.420105	5.867584	-0.053440	2.648903
279.956943	2365.479578	5.872589	-0.053491	2.653287
279.770068	2373.617643	5.877594	-0.053462	2.657677
280.278532	2381.588105	5.882598	-0.053562	2.662015
280.925504	2389.597180	5.887603	-0.053688	2.666376
281.098456	2397.662183	5.892608	-0.053725	2.670729
281.454637	2405.727919	5.897613	-0.053797	2.675087
282.133756	2413.698855	5.902618	-0.053928	2.679408
282.510010	2421.718259	5.907622	-0.054004	2.683728
282.998987	2429.784997	5.912627	-0.054100	2.688074
283.386115	2437.841186	5.917632	-0.054177	2.692400
283.731304	2445.903939	5.922637	-0.054247	2.696721
283.696070	2454.025347	5.927642	-0.054246	2.701041
284.525220	2461.953433	5.932646	-0.054405	2.705306
284.690951	2470.083033	5.937651	-0.054442	2.709630
284.578455	2478.197924	5.942656	-0.054426	2.713921
284.945176	2486.216499	5.947661	-0.054500	2.718184
285.312787	2494.227659	5.952666	-0.054573	2.722437
285.196942	2502.333888	5.957670	-0.054557	2.726703
285.436797	2510.401231	5.962675	-0.054607	2.730965
286.092694	2518.375071	5.967680	-0.054734	2.735196
286.376398	2526.429319	5.972685	-0.054792	2.739440
286.946516	2534.442399	5.977690	-0.054904	2.743673
286.455541	2542.614804	5.982694	-0.054818	2.747917
286.924668	2550.671716	5.987699	-0.054910	2.752154
287.026253	2558.722611	5.992704	-0.054935	2.756359
287.120562	2566.778927	5.997709	-0.054958	2.760559
287.458959	2574.776039	6.002714	-0.055026	2.764737
287.637578	2582.786255	6.007718	-0.055064	2.768906
288.264769	2590.795570	6.012723	-0.055186	2.773095
288.531888	2598.820487	6.017728	-0.055241	2.777265
288.685458	2606.891519	6.022733	-0.055275	2.781444
288.978587	2614.940253	6.027738	-0.055335	2.785615
289.294536	2622.980964	6.032742	-0.055399	2.789776
289.539839	2631.071281	6.037747	-0.055450	2.793952
289.439858	2639.121069	6.042752	-0.055437	2.798081
289.351312	2647.204515	6.047757	-0.055426	2.802221
289.722448	2655.211641	6.052762	-0.055500	2.806344
290.206627	2663.189527	6.057766	-0.055596	2.810452
290.085230	2671.332774	6.062771	-0.055578	2.814603
290.205681	2679.352757	6.067776	-0.055606	2.818699
290.776255	2687.317757	6.072781	-0.055717	2.822787
291.805425	2695.262028	6.077786	-0.055914	2.826886
292.262784	2703.297782	6.082790	-0.056005	2.830992
292.667509	2711.416236	6.087795	-0.056085	2.835131
292.842937	2719.447784	6.092800	-0.056123	2.839206
292.813524	2727.545347	6.097805	-0.056123	2.843296
292.738199	2735.661669	6.102810	-0.056115	2.847388
292.748440	2743.724690	6.107814	-0.056122	2.851452
292.649381	2751.817890	6.112819	-0.056109	2.855519
293.672040	2759.676234	6.117824	-0.056304	2.859527
294.157032	2767.668864	6.122829	-0.056400	2.863565
294.152401	2775.804623	6.127834	-0.056404	2.867641
294.083419	2783.897432	6.132838	-0.056397	2.871687
294.735154	2791.877686	6.137843	-0.056523	2.875711
294.868935	2799.929149	6.142848	-0.056553	2.879736
295.266288	2807.923409	6.147853	-0.056633	2.883741
295.400430	2816.028915	6.152858	-0.056663	2.887782
295.213548	2824.116476	6.157862	-0.056634	2.891790
295.880978	2832.103746	6.162867	-0.056763	2.895790
295.883378	2840.169214	6.167872	-0.056769	2.899787
296.183758	2848.174680	6.172877	-0.056830	2.903764
296.677359	2856.200116	6.177882	-0.056927	2.907757
296.597053	2864.324744	6.182886	-0.056918	2.911762
296.966482	2872.392841	6.187891	-0.056992	2.915758
297.241621	2880.341721	6.192896	-0.057048	2.919684
297.455698	2888.348898	6.197901	-0.057093	2.923631
297.848304	2896.404598	6.202906	-0.057172	2.927605
298.028545	2904.438139	6.207910	-0.057210	2.931552
298.266956	2912.528555	6.212915	-0.057260	2.935524
298.707530	2920.517095	6.217920	-0.057347	2.939453
299.070701	2928.502009	6.222925	-0.057420	2.943369
299.489800	2936.578165	6.227930	-0.057504	2.947328
299.296886	2944.697622	6.232934	-0.057473	2.951271
299.775400	2952.714771	6.237939	-0.057567	2.955193
300.101931	2960.688597	6.242944	-0.057634	2.959082
300.604740	2968.673267	6.247949	-0.057732	2.962980
300.903883	2976.747598	6.252954	-0.057793	2.966905
300.920884	2984.832975	6.257958	-0.057802	2.970816
300.867027	2992.938620	6.262963	-0.057797	2.974727
301.047015	3000.969444	6.267968	-0.057836	2.978610
300.860806	3009.029529	6.272973	-0.057807	2.982482
301.244370	3017.033555	6.277978	-0.057883	2.986352
301.561457	3025.048804	6.282982	-0.057948	2.990219
302.156038	3033.055953	6.287987	-0.058064	2.994091
302.203534	3041.096419	6.292992	-0.058078	2.997946
301.950900	3049.189741	6.297997	-0.058036	3.001806
302.576199	3057.178266	6.303002	-0.058158	3.005656
303.072379	3065.162955	6.308006	-0.058255	3.009493
303.344900	3073.223780	6.313011	-0.058311	3.013349
303.519828	3081.270642	6.318016	-0.058349	3.017189
303.587942	3089.363459	6.323021	-0.058367	3.021040
303.794060	3097.369190	6.328026	-0.058411	3.024852
303.661178	3105.432703	6.333030	-0.058391	3.028669
304.098732	3113.483280	6.338035	-0.058478	3.032505
304.180545	3121.494454	6.343040	-0.058499	3.036298
303.951197	3129.574081	6.348045	-0.058461	3.040104
304.436296	3137.551279	6.353050	-0.058557	3.043893
304.379838	3145.613757	6.358054	-0.058552	3.047690
304.744720	3153.633746	6.363059	-0.058625	3.051483
304.954532	3161.676713	6.368064	-0.058669	3.055274
305.019448	3169.717546	6.373069	-0.058687	3.059052
305.795498	3177.682038	6.378074	-0.058836	3.062825
306.029600	3185.716129	6.383078	-0.058885	3.066599
306.204686	3193.837794	6.388083	-0.058923	3.070407
306.599200	3201.864794	6.393088	-0.059002	3.074176
306.801665	3209.858670	6.398093	-0.059045	3.077916
307.257726	3217.875905	6.403098	-0.059135	3.081674
307.536449	3225.886434	6.408102	-0.059192	3.085416
307.549113	3233.960913	6.413107	-0.059200	3.089171
307.469339	3242.045914	6.418112	-0.059190	3.092921
307.299001	3250.144529	6.423117	-0.059164	3.096669
307.994314	3258.077224	6.428122	-0.059298	3.100377
308.386658	3266.043084	6.433126	-0.059377	3.104080
308.299514	3274.190245	6.438131	-0.059366	3.107841
308.504074	3282.214207	6.443136	-0.059409	3.111554
308.693817	3290.250036	6.448141	-0.059450	3.115268
308.931557	3298.255447	6.453146	-0.059499	3.118965
308.809019	3306.312794	6.458150	-0.059482	3.122665
309.199479	3314.322762	6.463155	-0.059560	3.126362
309.343564	3322.341883	6.468160	-0.059592	3.130048
309.657448	3330.359030	6.473165	-0.059656	3.133736
310.318661	3338.363451	6.478170	-0.059784	3.137430
310.061223	3346.474511	6.483174	-0.059741	3.141126
310.223363	3354.499981	6.488179	-0.059777	3.144799
310.601595	3362.523095	6.493184	-0.059853	3.148475
311.152976	3370.492718	6.498189	-0.059961	3.152131
311.526640	3378.548461	6.503194	-0.060035	3.155813
311.682278	3386.560370	6.508198	-0.060070	3.159461
312.136657	3394.579090	6.513203	-0.060159	3.163122
311.711296	3402.732926	6.518208	-0.060086	3.166800
311.926392	3410.733309	6.523213	-0.060131	3.170433
312.262726	3418.765660	6.528218	-0.060199	3.174082
312.394191	3426.767960	6.533222	-0.060229	3.177704
312.778418	3434.792232	6.538227	-0.060305	3.181343
313.049776	3442.803597	6.543232	-0.060361	3.184966
312.945339	3450.898815	6.548237	-0.060347	3.188607
313.145604	3458.959870	6.553242	-0.060390	3.192242
313.434294	3466.936859	6.558246	-0.060449	3.195838
313.622623	3474.979987	6.563251	-0.060489	3.199456
313.747621	3482.995904	6.568256	-0.060518	3.203055
314.005781	3491.013008	6.573261	-0.060571	3.206656
314.451496	3499.059708	6.578266	-0.060659	3.210274
313.976531	3507.163864	6.583270	-0.060576	3.213874
314.205138	3515.188765	6.588275	-0.060624	3.217465
314.636154	3523.198579	6.593280	-0.060709	3.221054
315.072573	3531.146878	6.598285	-0.060796	3.224611
315.358218	3539.237869	6.603290	-0.060854	3.228222
315.626143	3547.219508	6.608294	-0.060910	3.231779
316.056274	3555.265158	6.613299	-0.060995	3.235368
316.136074	3563.282498	6.618304	-0.061015	3.238925
316.338739	3571.323955	6.623309	-0.061058	3.242494
316.233558	3579.422332	6.628314	-0.061044	3.246071
316.162547	3587.413982	6.633318	-0.061036	3.249599
316.407546	3595.485975	6.638323	-0.061087	3.253172
316.585025	3603.515163	6.643328	-0.061125	3.256719
316.678678	3611.526949	6.648333	-0.061148	3.260251
317.050706	3619.503874	6.653338	-0.061222	3.263775
317.174931	3627.545984	6.658342	-0.061251	3.267313
317.903469	3635.551680	6.663347	-0.061392	3.270857
318.232080	3643.552738	6.668352	-0.061458	3.274378
317.953049	3651.665596	6.673357	-0.061411	3.277920
318.270036	3659.701639	6.678362	-0.061476	3.281449
318.297214	3667.693724	6.683366	-0.061486	3.284942
318.681109	3675.708212	6.688371	-0.061563	3.288457
318.751861	3683.795870	6.693376	-0.061581	3.291986
319.112019	3691.810673	6.698381	-0.061654	3.295492
319.316044	3699.845514	6.703386	-0.061697	3.298996
319.496372	3707.846601	6.708390	-0.061736	3.302482
319.814406	3715.905636	6.713395	-0.061800	3.305994
319.674424	3723.976601	6.718400	-0.061779	3.309489
319.959545	3731.985288	6.723405	-0.061838	3.312970
320.176113	3740.036854	6.728410	-0.061883	3.316464
320.416760	3747.967715	6.733414	-0.061933	3.319902
320.685798	3756.005623	6.738419	-0.061989	3.323385
321.236674	3763.999411	6.743424	-0.062097	3.326855
321.649378	3772.031529	6.748429	-0.062179	3.330333
321.963905	3780.096944	6.753434	-0.062243	3.333818
321.726179	3788.174944	6.758438	-0.062204	3.337283
321.913412	3796.224328	6.763443	-0.062244	3.340749
322.155249	3804.182009	6.768448	-0.062294	3.344174
322.027387	3812.270899	6.773453	-0.062276	3.347637
322.574756	3820.278811	6.778458	-0.062383	3.351088
322.968999	3828.263429	6.783462	-0.062461	3.354519
323.231533	3836.288415	6.788467	-0.062516	3.357960
323.173483	3844.371723	6.793472	-0.062510	3.361409
323.478603	3852.340117	6.798477	-0.062572	3.364820
323.678539	3860.420456	6.803482	-0.062615	3.368270
323.694207	3868.459874	6.808486	-0.062623	3.371693
323.881728	3876.516833	6.813491	-0.062663	3.375127
324.330631	3884.460982	6.818496	-0.062752	3.378518
323.999633	3892.585821	6.823501	-0.062696	3.381954
324.599535	3900.554707	6.828506	-0.062813	3.385355
324.198429	3908.679759	6.833510	-0.062743	3.388781
324.637311	3916.695152	6.838515	-0.062830	3.392189
324.927603	3924.715997	6.843520	-0.062890	3.395589
324.531815	3932.728798	6.848525	-0.062821	3.398959
324.768975	3940.757737	6.853530	-0.062871	3.402354
325.527689	3948.667548	6.858534	-0.063017	3.405715
325.128916	3956.814849	6.863539	-0.062948	3.409130
325.338865	3964.796183	6.868544	-0.062992	3.412495
325.459256	3972.825756	6.873549	-0.063020	3.415873
326.269860	3980.760665	6.878554	-0.063176	3.419232
326.680836	3988.784961	6.883558	-0.063258	3.422611
326.691744	3996.912009	6.888563	-0.063265	3.426016
326.708485	4004.944413	6.893568	-0.063274	3.429378
326.944796	4012.946255	6.898573	-0.063323	3.432732
327.426038	4020.970089	6.903578	-0.063418	3.436100
327.472767	4028.967683	6.908582	-0.063432	3.439439
327.675802	4037.008107	6.913587	-0.063475	3.442797
328.111741	4045.033518	6.918592	-0.063561	3.446154
328.202657	4053.056326	6.923597	-0.063584	3.449495
328.891107	4061.055930	6.928602	-0.063717	3.452843
328.899146	4069.134416	6.933606	-0.063724	3.456198
329.026563	4077.170344	6.938611	-0.063753	3.459536
328.833776	4085.208549	6.943616	-0.063722	3.462860
329.232460	4093.234203	6.948621	-0.063802	3.466197
329.382581	4101.265296	6.953626	-0.063835	3.469523
329.269669	4109.334538	6.958630	-0.063819	3.472854
329.393243	4117.360605	6.963635	-0.063848	3.476171
329.381783	4125.343937	6.968640	-0.063851	3.479464
329.892503	4133.291350	6.973645	-0.063951	3.482755
329.816745	4141.426333	6.978650	-0.063942	3.486101
330.136069	4149.371172	6.983654	-0.064007	3.489379
330.298816	4157.447884	6.988659	-0.064043	3.492703
330.501839	4165.491879	6.993664	-0.064086	3.496011
330.419859	4173.518236	6.998669	-0.064076	3.499300
331.103237	4181.462529	7.003674	-0.064208	3.502577
330.981868	4189.537683	7.008678	-0.064191	3.505878
331.388977	4197.558894	7.013683	-0.064272	3.509171
332.066695	4205.526042	7.018688	-0.064403	3.512448
331.905260	4213.611136	7.023693	-0.064379	3.515742
331.981075	4221.674466	7.028698	-0.064398	3.519032
332.311987	4229.631941	7.033702	-0.064465	3.522285
332.174072	4237.756208	7.038707	-0.064445	3.525587
332.357206	4245.734060	7.043712	-0.064484	3.528836
332.795963	4253.740313	7.048717	-0.064571	3.532103
332.797385	4261.837991	7.053722	-0.064576	3.535389
332.606718	4269.839385	7.058726	-0.064546	3.538628
332.882592	4277.885419	7.063731	-0.064603	3.541896
333.533611	4285.800675	7.068736	-0.064729	3.545120
333.392367	4293.888300	7.073741	-0.064708	3.548386
333.565379	4301.980999	7.078746	-0.064746	3.551660
333.478633	4310.022079	7.083750	-0.064735	3.554903
333.843494	4317.988179	7.088755	-0.064808	3.558126
333.668380	4326.036656	7.093760	-0.064781	3.561364
334.210576	4333.935804	7.098765	-0.064887	3.564560
334.226896	4342.051209	7.103770	-0.064895	3.567824
334.444733	4350.046982	7.108774	-0.064941	3.571043
334.667267	4358.062951	7.113779	-0.064988	3.574267
335.378586	4366.025609	7.118784	-0.065125	3.577482
335.620505	4374.072052	7.123789	-0.065176	3.580713
335.698718	4382.086552	7.128794	-0.065196	3.583924
336.089059	4390.130441	7.133798	-0.065274	3.587153
336.077092	4398.251368	7.138803	-0.065277	3.590397
336.215709	4406.230847	7.143808	-0.065308	3.593587
336.297686	4414.285077	7.148813	-0.065328	3.596802
336.494265	4422.298965	7.153818	-0.065370	3.600002
336.480515	4430.308008	7.158822	-0.065373	3.603190
336.958268	4438.310275	7.163827	-0.065467	3.606387
337.174847	4446.358516	7.168832	-0.065513	3.609592
337.102636	4454.416093	7.173837	-0.065505	3.612790
337.571823	4462.440818	7.178842	-0.065597	3.615987
337.864804	4470.374480	7.183846	-0.065657	3.619140
338.161378	4478.411945	7.188851	-0.065717	3.622332
338.088724	4486.476040	7.193856	-0.065709	3.625521
337.813118	4494.545937	7.198861	-0.065663	3.628703
338.236757	4502.582370	7.203866	-0.065747	3.631890
338.466022	4510.546509	7.208870	-0.065795	3.635039
338.784135	4518.560469	7.213875	-0.065860	3.638208
338.990433	4526.589484	7.218880	-0.065904	3.641377
339.121636	4534.569001	7.223885	-0.065933	3.644521
339.320857	4542.651550	7.228890	-0.065976	3.647705
339.259363	4550.700744	7.233894	-0.065969	3.650867
339.346264	4558.732977	7.238899	-0.065991	3.654022
339.717411	4566.744388	7.243904	-0.066065	3.657175
339.807919	4574.711498	7.248909	-0.066087	3.660300
340.526790	4582.702452	7.253914	-0.066226	3.663448
340.548240	4590.721760	7.258918	-0.066236	3.666586
340.936731	4598.777744	7.263923	-0.066313	3.669746
341.223996	4606.810236	7.268928	-0.066372	3.672890
340.904307	4614.907429	7.273933	-0.066318	3.676041
341.280324	4622.874880	7.278938	-0.066393	3.679158
341.157361	4630.911389	7.283942	-0.066376	3.682285
341.497061	4638.910347	7.288947	-0.066444	3.685407
342.002586	4646.882503	7.293952	-0.066543	3.688521
342.107852	4654.952223	7.298957	-0.066568	3.691659
342.456628	4663.000363	7.303962	-0.066639	3.694793
342.631412	4670.983464	7.308966	-0.066676	3.697894
342.648668	4679.100776	7.313971	-0.066685	3.701040
342.452007	4687.100590	7.318976	-0.066654	3.704133
342.716581	4695.148894	7.323981	-0.066708	3.707254
342.915131	4703.153557	7.328986	-0.066750	3.710353
343.118038	4711.215663	7.333990	-0.066793	3.713472
343.392515	4719.256444	7.338995	-0.066850	3.716582
343.397498	4727.265157	7.344000	-0.066856	3.719671
343.089240	4735.277616	7.349005	-0.066804	3.722750
343.424315	4743.273077	7.354010	-0.066871	3.725836
343.625366	4751.206941	7.359014	-0.066914	3.728893
343.994173	4759.273011	7.364019	-0.066988	3.732002
344.352466	4767.274273	7.369024	-0.067060	3.735084
344.551762	4775.282836	7.374029	-0.067102	3.738161
344.672216	4783.361846	7.379034	-0.067130	3.741262
344.858094	4791.326804	7.384038	-0.067170	3.744317
345.053960	4799.394828	7.389043	-0.067212	3.747410
345.532816	4807.411487	7.394048	-0.067306	3.750487
345.077350	4815.498629	7.399053	-0.067227	3.753566
344.951795	4823.572057	7.404058	-0.067209	3.756645
345.113750	4831.530672	7.409062	-0.067244	3.759685
345.472329	4839.472726	7.414067	-0.067316	3.762721
345.685916	4847.522345	7.419072	-0.067361	3.765792
345.877894	4855.511049	7.424077	-0.067402	3.768836
346.189080	4863.572769	7.429082	-0.067465	3.771909
346.204540	4871.619384	7.434086	-0.067473	3.774966
346.471264	4879.622345	7.439091	-0.067528	3.778011
346.774351	4887.640334	7.444096	-0.067590	3.781059
346.972590	4895.591480	7.449101	-0.067632	3.784077
346.938322	4903.736601	7.454106	-0.067631	3.787161
347.278131	4911.726693	7.459110	-0.067700	3.790192
347.488587	4919.735390	7.464115	-0.067744	3.793225
347.751944	4927.779612	7.469120	-0.067799	3.796269
348.095091	4935.722128	7.474125	-0.067868	3.799275
348.228492	4943.799750	7.479130	-0.067898	3.802325
347.994948	4951.835665	7.484134	-0.067860	3.805348
348.161705	4959.874484	7.489139	-0.067896	3.808379
348.422996	4967.909957	7.494144	-0.067950	3.811408
347.974619	4975.955397	7.499149	-0.067872	3.814423
347.812491	4984.051451	7.504154	-0.067847	3.817460
348.099209	4992.015689	7.509158	-0.067905	3.820456
348.268555	4999.950802	7.514163	-0.067942	3.823436
348.532436	5007.994937	7.519168	-0.067997	3.826457
348.882043	5015.955428	7.524173	-0.068067	3.829445
349.182619	5024.077092	7.529178	-0.068128	3.832491
348.903350	5032.085582	7.534182	-0.068081	3.835479
349.533110	5040.012067	7.539187	-0.068204	3.838454
349.920350	5048.066177	7.544192	-0.068281	3.841469
349.946764	5056.037165	7.549197	-0.068291	3.844443
349.598599	5064.216141	7.554202	-0.068232	3.847483
350.107539	5072.125684	7.559206	-0.068332	3.850440
350.410432	5080.169174	7.564211	-0.068394	3.853440
350.637053	5088.237709	7.569216	-0.068441	3.856444
350.582271	5096.247973	7.574221	-0.068436	3.859419
350.870338	5104.268494	7.579226	-0.068495	3.862403
350.691723	5112.269552	7.584230	-0.068467	3.865367
350.677104	5120.369386	7.589235	-0.068470	3.868370
350.860401	5128.420547	7.594240	-0.068509	3.871355
351.073001	5136.460336	7.599245	-0.068554	3.874335
351.297514	5144.450011	7.604250	-0.068601	3.877295
351.159332	5152.411123	7.609254	-0.068581	3.880234
351.426004	5160.383699	7.614259	-0.068635	3.883183
351.857617	5168.372821	7.619264	-0.068721	3.886140
351.664378	5176.405138	7.624269	-0.068690	3.889097
351.877688	5184.459355	7.629274	-0.068735	3.892069
351.804575	5192.504931	7.634278	-0.068727	3.895029
352.443369	5200.417664	7.639283	-0.068851	3.897952
352.967575	5208.486435	7.644288	-0.068954	3.900929
352.551210	5216.495080	7.649293	-0.068882	3.903862
353.102518	5224.560443	7.654298	-0.068990	3.906833
352.859745	5232.605809	7.659302	-0.068950	3.909778
353.142073	5240.596688	7.664307	-0.069008	3.912712
353.018244	5248.686120	7.669312	-0.068990	3.915672
353.237038	5256.602971	7.674317	-0.069036	3.918573
354.216814	5264.594896	7.679322	-0.069224	3.921514
354.296434	5272.551757	7.684326	-0.069244	3.924422
354.345551	5280.653045	7.689331	-0.069258	3.927380
354.675565	5288.679860	7.694336	-0.069325	3.930315
354.755823	5296.738684	7.699341	-0.069345	3.933254
354.692067	5304.820483	7.704346	-0.069339	3.936196
354.868227	5312.777489	7.709350	-0.069377	3.939096
355.100060	5320.831175	7.714355	-0.069425	3.942029
354.985259	5328.878673	7.719360	-0.069409	3.944952
355.178810	5336.881936	7.724365	-0.069450	3.947862
355.824295	5344.896584	7.729370	-0.069576	3.950782
355.789568	5352.910605	7.734374	-0.069574	3.953687
356.005649	5360.929046	7.739379	-0.069620	3.956597
355.738777	5368.995911	7.744384	-0.069576	3.959513
356.089766	5376.935779	7.749389	-0.069646	3.962392
356.577765	5384.952482	7.754394	-0.069742	3.965299
357.220868	5392.891493	7.759398	-0.069867	3.968179
357.136574	5401.017936	7.764403	-0.069857	3.971111
357.092149	5409.078263	7.769408	-0.069854	3.974018
357.368466	5417.049869	7.774413	-0.069911	3.976896
357.474504	5425.108545	7.779418	-0.069936	3.979801
357.448442	5433.079822	7.784422	-0.069936	3.982670
357.433360	5441.139665	7.789427	-0.069939	3.985569
357.797743	5449.160080	7.794432	-0.070012	3.988458
357.919234	5457.182526	7.799437	-0.070040	3.991341
358.021752	5465.146479	7.804442	-0.070064	3.994201
358.071278	5473.183163	7.809446	-0.070078	3.997084
358.588959	5481.207750	7.814451	-0.070180	3.999969
358.670828	5489.218030	7.819456	-0.070201	4.002839
358.665233	5497.232122	7.824461	-0.070205	4.005707
358.963800	5505.254255	7.829466	-0.070266	4.008581
358.974006	5513.327243	7.834470	-0.070273	4.011466
358.884031	5521.347755	7.839475	-0.070261	4.014329
358.900814	5529.383007	7.844480	-0.070270	4.017196
358.951681	5537.411053	7.849485	-0.070285	4.020060
359.087907	5545.422516	7.854490	-0.070315	4.022917
358.722360	5553.470640	7.859494	-0.070252	4.025776
359.357323	5561.422485	7.864499	-0.070376	4.028616
359.535743	5569.474752	7.869504	-0.070414	4.031482
359.758350	5577.477215	7.874509	-0.070461	4.034329
360.249225	5585.488294	7.879514	-0.070558	4.037181
360.055992	5593.519228	7.884518	-0.070527	4.040028
360.308604	5601.497073	7.889523	-0.070579	4.042860
360.378340	5609.538124	7.894528	-0.070598	4.045710
360.938099	5617.479379	7.899533	-0.070707	4.048531
361.284064	5625.604444	7.904538	-0.070777	4.051411
361.023944	5633.583613	7.909542	-0.070734	4.054228
361.339273	5641.666835	7.914547	-0.070798	4.057088
361.728607	5649.639453	7.919552	-0.070875	4.059909
361.717733	5657.620073	7.924557	-0.070879	4.062725
362.011760	5665.651550	7.929562	-0.070939	4.065561
362.118281	5673.714543	7.934566	-0.070964	4.068403
362.174863	5681.786249	7.939571	-0.070980	4.071245
362.513332	5689.732684	7.944576	-0.071048	4.074046
362.529803	5697.789867	7.949581	-0.071056	4.076879
362.610329	5705.779742	7.954586	-0.071076	4.079687
362.541948	5713.820551	7.959590	-0.071069	4.082509
362.440125	5721.835363	7.964595	-0.071055	4.085320
362.634846	5729.848677	7.969600	-0.071097	4.088132
363.000833	5737.859623	7.974605	-0.071170	4.090944
363.067342	5745.917116	7.979610	-0.071188	4.093766
362.725627	5753.967475	7.984614	-0.071130	4.096578
363.282632	5761.894571	7.989619	-0.071238	4.099357
363.329507	5769.955257	7.994624	-0.071252	4.102174
362.971767	5778.018176	7.999629	-0.071191	4.104984
363.642762	5785.982466	8.004634	-0.071321	4.107773
364.086474	5793.965131	8.009638	-0.071409	4.110562
363.944400	5802.034990	8.014643	-0.071388	4.113372
364.183581	5810.085347	8.019648	-0.071438	4.116178
364.095170	5817.988172	8.024653	-0.071427	4.118927
364.514998	5826.043366	8.029658	-0.071510	4.121734
364.570968	5834.020468	8.034662	-0.071526	4.124506
364.848551	5842.131969	8.039667	-0.071583	4.127327
364.735159	5850.166147	8.044672	-0.071567	4.130113
364.954278	5858.117278	8.049677	-0.071613	4.132873
364.806828	5866.233840	8.054682	-0.071591	4.135684
364.747611	5874.186577	8.059686	-0.071585	4.138437
365.161919	5882.216906	8.064691	-0.071667	4.141222
365.470613	5890.167397	8.069696	-0.071730	4.143975
365.158433	5898.252303	8.074701	-0.071677	4.146765
365.687976	5906.255996	8.079706	-0.071781	4.149537
365.988671	5914.253845	8.084710	-0.071842	4.152301
365.619177	5922.321718	8.089715	-0.071779	4.155079
365.822898	5930.315823	8.094720	-0.071822	4.157837
365.904273	5938.325233	8.099725	-0.071843	4.160597
366.245053	5946.322419	8.104730	-0.071911	4.163354
366.110594	5954.417570	8.109734	-0.071892	4.166137
366.385812	5962.358921	8.114739	-0.071948	4.168870
366.343623	5970.461490	8.119744	-0.071945	4.171653
366.727189	5978.367844	8.124749	-0.072022	4.174372
367.015549	5986.409414	8.129754	-0.072081	4.177134
366.848587	5994.494294	8.134758	-0.072055	4.179904
366.765625	6002.516822	8.139763	-0.072045	4.182652
367.160713	6010.507011	8.144768	-0.072124	4.185392
367.298167	6018.519722	8.149773	-0.072155	4.188135
367.568087	6026.589827	8.154778	-0.072210	4.190898
367.333398	6034.683527	8.159782	-0.072172	4.193661
367.711845	6042.652821	8.164787	-0.072248	4.196387
367.863352	6050.594857	8.169792	-0.072281	4.199099
367.991864	6058.647263	8.174797	-0.072310	4.201847
367.477138	6066.719141	8.179802	-0.072220	4.204592
368.018844	6074.616157	8.184806	-0.072326	4.207288
367.853564	6082.706945	8.189811	-0.072300	4.210040
368.372221	6090.714431	8.194816	-0.072402	4.212769
368.593813	6098.700267	8.199821	-0.072449	4.215486
368.624854	6106.756366	8.204826	-0.072460	4.218223
368.488680	6114.824944	8.209830	-0.072440	4.220961
368.411275	6122.764276	8.214835	-0.072431	4.223654
369.083434	6130.777828	8.219840	-0.072561	4.226378
369.299897	6138.746726	8.224845	-0.072606	4.229080
369.537321	6146.864962	8.229850	-0.072656	4.231832
369.337118	6154.888739	8.234854	-0.072624	4.234545
369.583098	6162.875108	8.239859	-0.072675	4.237248
369.826068	6170.883411	8.244864	-0.072726	4.239957
370.101742	6178.858953	8.249869	-0.072782	4.242654
370.016419	6186.927484	8.254874	-0.072772	4.245376
370.269551	6194.921482	8.259878	-0.072824	4.248075
370.473078	6202.956446	8.264883	-0.072867	4.250786
370.556460	6210.983531	8.269888	-0.072888	4.253490
370.490789	6219.035962	8.274893	-0.072881	4.256201
370.781653	6227.005948	8.279898	-0.072940	4.258885
370.659166	6235.093511	8.284902	-0.072923	4.261603
371.239175	6242.982657	8.289907	-0.073036	4.264260
371.206230	6251.056504	8.294912	-0.073035	4.266970
371.228347	6259.109703	8.299917	-0.073045	4.269673
371.787291	6267.111744	8.304922	-0.073154	4.272362
371.469270	6275.128983	8.309926	-0.073100	4.275046
371.486123	6283.144519	8.314931	-0.073108	4.277731
371.739506	6291.149171	8.319936	-0.073161	4.280413
372.079198	6299.045465	8.324941	-0.073229	4.283057
372.466708	6307.135100	8.329946	-0.073307	4.285765
372.882344	6315.107732	8.334950	-0.073389	4.288433
372.473472	6323.273441	8.339955	-0.073319	4.291156
372.783549	6331.255397	8.344960	-0.073382	4.293822
372.937543	6339.287831	8.349965	-0.073416	4.296502
373.888312	6347.139258	8.354970	-0.073598	4.299127
373.457128	6355.294863	8.359974	-0.073523	4.301839
373.340174	6363.253938	8.364979	-0.073506	4.304487
373.746390	6371.335726	8.369984	-0.073587	4.307179
373.584255	6379.403573	8.374989	-0.073562	4.309860
373.882917	6387.346152	8.379994	-0.073623	4.312501
374.363252	6395.322037	8.384998	-0.073718	4.315153
374.507896	6403.331253	8.390003	-0.073750	4.317812
374.871749	6411.353178	8.395008	-0.073823	4.320475
374.444202	6419.375335	8.400013	-0.073749	4.323130
374.862611	6427.446503	8.405018	-0.073832	4.325806
374.478060	6435.437719	8.410022	-0.073766	4.328448
374.883801	6443.415471	8.415027	-0.073846	4.331090
375.240607	6451.467461	8.420032	-0.073918	4.333755
375.151121	6459.527631	8.425037	-0.073907	4.336417
375.217541	6467.505805	8.430042	-0.073924	4.339051
375.380409	6475.525406	8.435046	-0.073960	4.341699
375.326419	6483.511453	8.440051	-0.073955	4.344332
375.676586	6491.596303	8.445056	-0.074026	4.346999
375.631695	6499.557810	8.450061	-0.074023	4.349621
375.809427	6507.679407	8.455066	-0.074061	4.352296
376.345336	6515.623351	8.460070	-0.074166	4.354913
376.266033	6523.633495	8.465075	-0.074156	4.357546
376.327123	6531.667222	8.470080	-0.074173	4.360186
376.716365	6539.598805	8.475085	-0.074251	4.362793
376.452405	6547.709342	8.480090	-0.074207	4.365452
376.209553	6555.725240	8.485094	-0.074167	4.368080
376.275772	6563.723093	8.490099	-0.074185	4.370701
376.756888	6571.685564	8.495104	-0.074279	4.373313
376.885825	6579.713782	8.500109	-0.074309	4.375942
377.255223	6587.700861	8.505114	-0.074383	4.378558
377.047512	6595.788764	8.510118	-0.074349	4.381201
376.898239	6603.767517	8.515123	-0.074327	4.383807
377.360790	6611.891651	8.520128	-0.074418	4.386463
377.510311	6619.802285	8.525133	-0.074451	4.389046
377.864725	6627.871575	8.530138	-0.074523	4.391680
378.005862	6635.827405	8.535142	-0.074554	4.394275
378.144460	6643.902119	8.540147	-0.074585	4.396906
378.347906	6651.945004	8.545152	-0.074628	4.399526
378.703726	6659.896791	8.550157	-0.074700	4.402116
378.615651	6667.935682	8.555162	-0.074689	4.404730
378.328424	6676.077183	8.560167	-0.074641	4.407374
378.498532	6684.064117	8.565171	-0.074678	4.409969
378.929368	6692.095345	8.570176	-0.074763	4.412579
378.846814	6700.113787	8.575181	-0.074753	4.415180
378.978998	6708.135039	8.580186	-0.074783	4.417782
379.285244	6716.096338	8.585191	-0.074845	4.420363
379.546532	6724.080561	8.590195	-0.074899	4.422950
379.716516	6732.132893	8.595200	-0.074936	4.425557
379.373965	6740.182355	8.600205	-0.074877	4.428159
379.895919	6748.228648	8.605210	-0.074980	4.430763
379.927796	6756.232941	8.610215	-0.074991	4.433350
380.366205	6764.248792	8.615219	-0.075078	4.435940
380.409067	6772.228511	8.620224	-0.075091	4.438516
380.719785	6780.266693	8.625229	-0.075154	4.441110
380.785306	6788.232206	8.630234	-0.075172	4.443678
380.274490	6796.324798	8.635239	-0.075082	4.446282
380.861446	6804.257541	8.640243	-0.075197	4.448839
380.912999	6812.396397	8.645248	-0.075212	4.451458
380.751240	6820.342264	8.650253	-0.075187	4.454012
381.296726	6828.371517	8.655258	-0.075293	4.456596
381.178255	6836.382337	8.660263	-0.075277	4.459168
381.323817	6844.421160	8.665267	-0.075309	4.461749
381.120475	6852.443406	8.670272	-0.075276	4.464322
381.268656	6860.407793	8.675277	-0.075309	4.466877
381.708049	6868.411739	8.680282	-0.075396	4.469443
381.560013	6876.486044	8.685287	-0.075374	4.472029
381.707898	6884.497559	8.690291	-0.075407	4.474594
382.169323	6892.479303	8.695296	-0.075498	4.477149
382.058174	6900.471352	8.700301	-0.075483	4.479704
382.308862	6908.542416	8.705306	-0.075535	4.482284
382.565149	6916.450947	8.710311	-0.075588	4.484811
382.555643	6924.557196	8.715315	-0.075591	4.487398
382.674755	6932.570597	8.720320	-0.075619	4.489954
383.148727	6940.552967	8.725325	-0.075712	4.492501
383.302728	6948.613474	8.730330	-0.075746	4.495070
383.306124	6956.603933	8.735335	-0.075752	4.497614
383.567104	6964.608708	8.740339	-0.075806	4.500163
383.785799	6972.651012	8.745344	-0.075852	4.502722
383.974965	6980.657055	8.750349	-0.075892	4.505267
383.887412	6988.718907	8.755354	-0.075881	4.507828
383.942331	6996.749360	8.760359	-0.075897	4.510378
384.024973	7004.703400	8.765363	-0.075917	4.512903
384.572264	7012.696495	8.770368	-0.076024	4.515440
384.783699	7020.657337	8.775373	-0.076069	4.517964
384.861724	7028.763046	8.780378	-0.076089	4.520532
384.437647	7036.804349	8.785383	-0.076015	4.523077
384.883496	7044.752850	8.790387	-0.076103	4.525593
385.101551	7052.791045	8.795392	-0.076149	4.528136
385.120991	7060.778380	8.800397	-0.076158	4.530661
385.315728	7068.846698	8.805402	-0.076200	4.533210
385.453332	7076.853879	8.810407	-0.076231	4.535739
385.904887	7084.796574	8.815411	-0.076320	4.538247
385.836673	7092.924487	8.820416	-0.076313	4.540810
385.736933	7100.867998	8.825421	-0.076299	4.543313
385.987133	7108.958766	8.830426	-0.076351	4.545863
386.534371	7116.854470	8.835431	-0.076458	4.548350
386.453464	7124.941139	8.840435	-0.076449	4.550894
386.984366	7132.953274	8.845440	-0.076553	4.553415
386.542607	7141.008921	8.850445	-0.076476	4.555946
386.878457	7148.992807	8.855450	-0.076543	4.558455
386.997215	7157.032455	8.860455	-0.076571	4.560980
387.315361	7164.902116	8.865459	-0.076635	4.563450
386.946391	7173.112210	8.870464	-0.076572	4.566024
387.113579	7181.012582	8.875469	-0.076608	4.568501
387.561848	7189.093040	8.880474	-0.076697	4.571033
387.502050	7197.024567	8.885479	-0.076691	4.573516
387.706916	7205.103582	8.890483	-0.076735	4.576045
388.537130	7213.071878	8.895488	-0.076894	4.578538
388.253776	7221.124696	8.900493	-0.076847	4.581055
388.715535	7229.086063	8.905498	-0.076938	4.583543
388.804806	7237.144792	8.910503	-0.076960	4.586059
388.999832	7245.190478	8.915507	-0.077002	4.588570
389.033125	7253.254405	8.920512	-0.077013	4.591085
389.100136	7261.183376	8.925517	-0.077031	4.593557
389.354489	7269.255204	8.930522	-0.077084	4.596072
389.367874	7277.221188	8.935527	-0.077091	4.598552
389.541967	7285.267146	8.940531	-0.077129	4.601057
389.556392	7293.227770	8.945536	-0.077137	4.603533
389.524728	7301.302345	8.950541	-0.077136	4.606043
390.091244	7309.236701	8.955546	-0.077247	4.608508
390.103420	7317.338088	8.960551	-0.077255	4.611024
389.870690	7325.313784	8.965555	-0.077216	4.613499
389.741591	7333.434358	8.970560	-0.077198	4.616018
390.164842	7341.312226	8.975565	-0.077282	4.618461
390.460049	7349.403339	8.980570	-0.077342	4.620968
390.400039	7357.313128	8.985575	-0.077336	4.623418
390.336551	7365.378441	8.990579	-0.077330	4.625914
390.551433	7373.417362	8.995584	-0.077375	4.628401
390.142315	7381.511072	9.000589	-0.077304	4.630903
390.269775	7389.459801	9.005594	-0.077333	4.633360
390.615778	7397.446959	9.010599	-0.077403	4.635827
390.958546	7405.415248	9.015603	-0.077472	4.638286
390.852582	7413.512694	9.020608	-0.077457	4.640785
390.856905	7421.455422	9.025613	-0.077463	4.643234
391.224312	7429.524868	9.030618	-0.077537	4.645721
391.501592	7437.520731	9.035623	-0.077594	4.648184
391.422907	7445.593934	9.040627	-0.077585	4.650669
391.710921	7453.599499	9.045632	-0.077643	4.653132
391.162460	7461.661783	9.050637	-0.077547	4.655612
391.608727	7469.618141	9.055642	-0.077635	4.658057
391.207102	7477.659401	9.060647	-0.077565	4.660528
391.561140	7485.603917	9.065651	-0.077637	4.662967
392.021986	7493.608846	9.070656	-0.077728	4.665423
391.906868	7501.634622	9.075661	-0.077711	4.667885
392.302132	7509.686859	9.080666	-0.077790	4.670353
392.836608	7517.695878	9.085671	-0.077895	4.672807
392.939327	7525.714537	9.090675	-0.077920	4.675262
393.386337	7533.750492	9.095680	-0.078008	4.677722
393.117175	7541.753348	9.100685	-0.077963	4.680170
392.896843	7549.786985	9.105690	-0.077927	4.682626
393.117526	7557.755517	9.110695	-0.077974	4.685061
393.417209	7565.742843	9.115699	-0.078035	4.687500
393.309786	7573.823151	9.120704	-0.078020	4.689967
393.713395	7581.826539	9.125709	-0.078101	4.692409
393.646582	7589.838686	9.130714	-0.078093	4.694852
393.375402	7597.901335	9.135719	-0.078048	4.697309
393.511277	7605.855963	9.140723	-0.078079	4.699732
393.851789	7613.922294	9.145728	-0.078147	4.702188
393.859066	7621.904276	9.150733	-0.078154	4.704617
394.047996	7629.917929	9.155738	-0.078194	4.707054
394.373870	7637.885111	9.160743	-0.078260	4.709475
394.457576	7645.999211	9.165747	-0.078281	4.711940
394.608118	7653.969862	9.170752	-0.078315	4.714361
394.722430	7661.947566	9.175757	-0.078341	4.716782
395.017050	7669.952049	9.180762	-0.078401	4.719209
395.090606	7678.047042	9.185767	-0.078420	4.721664
395.025592	7686.016639	9.190771	-0.078413	4.724079
395.128080	7694.138773	9.195776	-0.078438	4.726539
394.889903	7702.106212	9.200781	-0.078399	4.728951
394.927769	7710.166147	9.205786	-0.078411	4.731390
394.928868	7718.139142	9.210791	-0.078416	4.733801
395.430215	7726.107295	9.215795	-0.078515	4.736208
395.509402	7734.172816	9.220800	-0.078535	4.738644
395.562607	7742.198897	9.225805	-0.078550	4.741068
396.095403	7750.118909	9.230810	-0.078655	4.743457
396.319915	7758.220882	9.235815	-0.078702	4.745900
396.043586	7766.197812	9.240819	-0.078656	4.748305
396.189933	7774.304418	9.245824	-0.078688	4.750748
396.520007	7782.209410	9.250829	-0.078755	4.753128
396.640100	7790.294109	9.255834	-0.078782	4.755561
396.464303	7798.261057	9.260839	-0.078755	4.757958
396.885689	7806.290249	9.265843	-0.078839	4.760372
397.075809	7814.345478	9.270848	-0.078879	4.762792
397.041053	7822.315470	9.275853	-0.078878	4.765186
396.899343	7830.378937	9.280858	-0.078857	4.767608
396.969743	7838.447472	9.285863	-0.078875	4.770029
397.293805	7846.408125	9.290867	-0.078941	4.772416
397.558939	7854.408759	9.295872	-0.078996	4.774813
397.529888	7862.448020	9.300877	-0.078996	4.777222
398.058435	7870.384561	9.305882	-0.079099	4.779598
398.132982	7878.458127	9.310887	-0.079118	4.782014
398.193591	7886.374919	9.315891	-0.079135	4.784382
398.341120	7894.518019	9.320896	-0.079168	4.786817
398.439347	7902.450582	9.325901	-0.079191	4.789187
398.587270	7910.563311	9.330906	-0.079224	4.791610
398.613494	7918.513542	9.335911	-0.079234	4.793984
398.622509	7926.575309	9.340915	-0.079241	4.796390
398.321658	7934.574590	9.345920	-0.079190	4.798777
398.120493	7942.618770	9.350925	-0.079158	4.801176
398.691259	7950.514054	9.355930	-0.079270	4.803527
398.813477	7958.575534	9.360935	-0.079298	4.805927
398.738035	7966.575625	9.365939	-0.079289	4.808309
398.856989	7974.723880	9.370944	-0.079316	4.810733
398.852872	7982.622654	9.375949	-0.079321	4.813082
399.175426	7990.146204	9.380954	-0.079386	4.815317
399.494524	7994.907151	9.385959	-0.079448	4.816730

399.703316	7997.515349	9.390963	-0.079489	4.817504
399.895247	7998.825537	9.395968	-0.079526	4.817892
400.005909	7999.312687	9.400973	-0.079547	4.818037
400.116947	8000.306555	9.405978	-0.079568	4.818331
400.241151	8000.397609	9.410983	-0.079591	4.818358
400.112422	8000.403216	9.415987	-0.079567	4.818360
399.999837	8000.444785	9.420992	-0.079546	4.818373
399.613054	8000.435309	9.425997	-0.079474	4.818372
399.830424	8000.465609	9.431002	-0.079515	4.818380
399.659642	8000.494821	9.436007	-0.079483	4.818389
399.676414	8000.471925	9.441011	-0.079486	4.818382
400.071695	8000.442627	9.446016	-0.079560	4.818372
399.986374	8000.448826	9.451021	-0.079544	4.818374
400.477873	8000.467096	9.456026	-0.079636	4.818378
400.173159	8000.468200	9.461031	-0.079579	4.818379
400.490429	8000.444146	9.466035	-0.079638	4.818371
400.343286	8000.486296	9.471040	-0.079611	4.818384
400.272754	8000.466414	9.476045	-0.079598	4.818378
400.470498	8000.370295	9.481050	-0.079635	4.818349
400.334795	8000.481984	9.486055	-0.079609	4.818383
400.470819	8000.444946	9.491059	-0.079635	4.818371
400.561463	8000.438826	9.496064	-0.079652	4.818369
400.472653	8000.423952	9.501069	-0.079635	4.818365
400.539496	8000.488994	9.506074	-0.079648	4.818384
400.932347	8000.428127	9.511079	-0.079721	4.818364
401.046673	8000.422331	9.516083	-0.079742	4.818362
401.031017	8000.472582	9.521088	-0.079739	4.818377
401.262365	8000.386382	9.526093	-0.079782	4.818350
400.940022	8000.469244	9.531098	-0.079722	4.818376
400.587443	8000.418181	9.536103	-0.079657	4.818363
400.585961	8000.430779	9.541107	-0.079657	4.818366
400.489638	8000.444186	9.546112	-0.079639	4.818371
400.661504	8000.436021	9.551117	-0.079671	4.818368
400.801107	8000.484185	9.556122	-0.079697	4.818381
400.630953	8000.498687	9.561127	-0.079665	4.818386
400.371904	8000.424721	9.566131	-0.079617	4.818365
400.329852	8000.464099	9.571136	-0.079609	4.818377
400.398002	8000.417725	9.576141	-0.079622	4.818363
401.063937	8000.463608	9.581146	-0.079746	4.818374
400.851953	8000.468077	9.586151	-0.079707	4.818376
400.865456	8000.488239	9.591155	-0.079709	4.818382
401.060427	8000.398390	9.596160	-0.079745	4.818355
400.987697	8000.482555	9.601165	-0.079732	4.818380
400.829135	8000.508779	9.606170	-0.079703	4.818389
400.938589	8000.510276	9.611175	-0.079723	4.818389
401.148132	8000.463727	9.616179	-0.079762	4.818374
401.322181	8000.400926	9.621184	-0.079794	4.818354
401.453338	8000.406924	9.626189	-0.079819	4.818356
401.188830	8000.485318	9.631194	-0.079770	4.818380
401.450155	8000.464708	9.636199	-0.079818	4.818373
401.069531	8000.492107	9.641203	-0.079748	4.818383
401.132250	8000.492966	9.646208	-0.079759	4.818383
400.668410	8000.410948	9.651213	-0.079673	4.818360
400.971971	8000.434016	9.656218	-0.079729	4.818366
400.660343	8000.464460	9.661223	-0.079672	4.818376
400.807350	8000.485391	9.666227	-0.079699	4.818382
401.024289	8000.518842	9.671232	-0.079739	4.818391
401.121270	8000.394014	9.676237	-0.079757	4.818353
400.673795	8000.472015	9.681242	-0.079674	4.818378
400.722012	8000.424317	9.686247	-0.079683	4.818364
400.925087	8000.481757	9.691251	-0.079721	4.818380
401.014980	8000.428320	9.696256	-0.079738	4.818364
401.306443	8000.472250	9.701261	-0.079792	4.818376
400.921998	8000.378699	9.706266	-0.079721	4.818349
401.393251	8000.417722	9.711271	-0.079808	4.818359
401.622844	8000.466064	9.716275	-0.079851	4.818373
401.445603	8000.484675	9.721280	-0.079818	4.818379
401.442134	8000.436271	9.726285	-0.079818	4.818364
401.731178	8000.467553	9.731290	-0.079872	4.818373
401.861346	8000.456717	9.736295	-0.079896	4.818369
401.975796	8000.453026	9.741299	-0.079917	4.818367
402.012361	8000.478760	9.746304	-0.079924	4.818375
401.782736	8000.358934	9.751309	-0.079881	4.818340
402.095543	8000.434695	9.756314	-0.079940	4.818361
402.161307	8000.418775	9.761319	-0.079952	4.818356
402.013115	8000.446192	9.766323	-0.079924	4.818365
401.863316	8000.506178	9.771328	-0.079896	4.818384
402.165359	8000.431456	9.776333	-0.079953	4.818360
401.685747	8000.514273	9.781338	-0.079864	4.818387
402.110920	8000.432822	9.786343	-0.079943	4.818361
401.776197	8000.459795	9.791347	-0.079880	4.818370
401.856310	8000.513457	9.796352	-0.079895	4.818386
402.042915	8000.456083	9.801357	-0.079930	4.818368
402.085020	8000.380967	9.806362	-0.079938	4.818345
402.008248	8000.467181	9.811367	-0.079924	4.818371
401.786146	8000.495691	9.816371	-0.079883	4.818381
401.830430	8000.494196	9.821376	-0.079891	4.818380
402.106225	8000.448553	9.826381	-0.079942	4.818365
402.234926	8000.437697	9.831386	-0.079966	4.818362
402.276651	8000.463502	9.836391	-0.079974	4.818369
402.194637	8000.430846	9.841395	-0.079959	4.818360
402.340712	8000.448613	9.846400	-0.079986	4.818364
402.220596	8000.418591	9.851405	-0.079964	4.818356
402.329985	8000.461089	9.856410	-0.079984	4.818368
402.370488	8000.446926	9.861415	-0.079992	4.818364
402.506806	8000.452996	9.866419	-0.080017	4.818365
402.344732	8000.471813	9.871424	-0.079987	4.818371
402.492121	8000.428622	9.876429	-0.080014	4.818358
402.650985	8000.392946	9.881434	-0.080044	4.818347
402.583468	8000.424619	9.886439	-0.080032	4.818356
402.465278	8000.428265	9.891443	-0.080010	4.818358
402.253136	8000.470578	9.896448	-0.079970	4.818371
402.333412	8000.432778	9.901453	-0.079985	4.818360
402.136677	8000.406967	9.906458	-0.079949	4.818353
402.217278	8000.485868	9.911463	-0.079964	4.818376
402.011618	8000.472550	9.916467	-0.079925	4.818373
402.093732	8000.493649	9.921472	-0.079941	4.818379
402.262394	8000.472826	9.926477	-0.079972	4.818372
402.320727	8000.484139	9.931482	-0.079983	4.818375
402.126506	8000.496209	9.936487	-0.079947	4.818379
402.290918	8000.446942	9.941491	-0.079978	4.818364
402.505970	8000.465651	9.946496	-0.080018	4.818369
402.313589	8000.453566	9.951501	-0.079982	4.818366
402.316707	8000.476741	9.956506	-0.079983	4.818373
402.527682	8000.470163	9.961511	-0.080022	4.818370
402.594285	8000.461613	9.966515	-0.080034	4.818367
402.123028	8000.395257	9.971520	-0.079947	4.818349
402.056790	8000.458486	9.976525	-0.079934	4.818369
402.118661	8000.484566	9.981530	-0.079946	4.818376
402.230132	8000.471372	9.986535	-0.079967	4.818372
402.568591	8000.433944	9.991539	-0.080030	4.818359
402.477607	8000.486322	9.996544	-0.080013	4.818375
402.520082	8000.470084	10.001549	-0.080021	4.818370
402.620501	8000.448330	10.006554	-0.080039	4.818363
402.969066	8000.427861	10.011559	-0.080104	4.818356
402.728386	8000.442450	10.016563	-0.080060	4.818361
402.838777	8000.460782	10.021568	-0.080080	4.818366
402.741551	8000.462611	10.026573	-0.080062	4.818367
402.926069	8000.432543	10.031578	-0.080097	4.818357
403.002698	8000.426234	10.036583	-0.080111	4.818355
402.739259	8000.408972	10.041587	-0.080062	4.818351
403.052461	8000.446895	10.046592	-0.080120	4.818361
402.775999	8000.452584	10.051597	-0.080069	4.818364
402.618026	8000.445174	10.056602	-0.080039	4.818362
402.577366	8000.416236	10.061607	-0.080032	4.818354
402.567168	8000.426613	10.066611	-0.080030	4.818357
402.791845	8000.449660	10.071616	-0.080072	4.818363
402.471881	8000.444242	10.076621	-0.080012	4.818363
402.809898	8000.405757	10.081626	-0.080075	4.818350
402.736417	8000.449964	10.086631	-0.080062	4.818363
402.568398	8000.423492	10.091635	-0.080031	4.818356
402.807383	8000.445682	10.096640	-0.080075	4.818362
402.889360	8000.438394	10.101645	-0.080090	4.818359
402.770433	8000.443081	10.106650	-0.080068	4.818361
402.389974	8000.483096	10.111655	-0.079997	4.818374
402.834272	8000.364059	10.116659	-0.080080	4.818337
402.813810	8000.469967	10.121664	-0.080076	4.818369
402.369326	8000.494388	10.126669	-0.079994	4.818378
402.491986	8000.487656	10.131674	-0.080017	4.818375
402.594104	8000.466976	10.136679	-0.080036	4.818369
402.575107	8000.461463	10.141683	-0.080032	4.818367
402.736046	8000.468921	10.146688	-0.080062	4.818369
402.685570	8000.452464	10.151693	-0.080053	4.818364
402.458330	8000.474596	10.156698	-0.080011	4.818372
402.662729	8000.467929	10.161703	-0.080049	4.818369
402.354133	8000.440589	10.166707	-0.079991	4.818362
402.511458	8000.470075	10.171712	-0.080021	4.818370
402.354805	8000.444810	10.176717	-0.079991	4.818363
402.385098	8000.480972	10.181722	-0.079997	4.818374
402.461763	8000.396864	10.186727	-0.080011	4.818349
402.164761	8000.492688	10.191731	-0.079956	4.818378
402.290932	8000.426078	10.196736	-0.079980	4.818358
402.563385	8000.489727	10.201741	-0.080031	4.818376
402.611006	8000.485124	10.206746	-0.080039	4.818374
402.750710	8000.474419	10.211751	-0.080066	4.818370
402.762258	8000.476682	10.216755	-0.080068	4.818371
402.790456	8000.527535	10.221760	-0.080073	4.818386
402.365272	8000.501756	10.226765	-0.079994	4.818380
402.801188	8000.397322	10.231770	-0.080075	4.818347
402.855708	8000.480074	10.236775	-0.080085	4.818372
402.583598	8000.484772	10.241779	-0.080035	4.818374
402.755497	8000.504995	10.246784	-0.080067	4.818379
402.779144	8000.433831	10.251789	-0.080071	4.818358
402.578612	8000.497329	10.256794	-0.080034	4.818378
402.887069	8000.483672	10.261799	-0.080091	4.818373
402.697542	8000.449547	10.266803	-0.080056	4.818363
402.863036	8000.458118	10.271808	-0.080087	4.818365
402.754350	8000.440867	10.276813	-0.080067	4.818360
402.417189	8000.490935	10.281818	-0.080004	4.818377
402.475363	8000.405524	10.286823	-0.080015	4.818351
402.337652	8000.477240	10.291827	-0.079989	4.818373
402.861466	8000.484396	10.296832	-0.080087	4.818373
402.966065	8000.413286	10.301837	-0.080106	4.818351
403.186336	8000.453094	10.306842	-0.080147	4.818362
402.829396	8000.457684	10.311847	-0.080081	4.818365
402.547177	8000.491681	10.316851	-0.080029	4.818376
402.862532	8000.416090	10.321856	-0.080087	4.818353
402.952202	8000.456217	10.326861	-0.080104	4.818364
402.895589	8000.509065	10.331866	-0.080094	4.818380
403.045670	8000.490092	10.336871	-0.080122	4.818374
402.535752	8000.504157	10.341875	-0.080027	4.818380
402.707626	8000.501251	10.346880	-0.080059	4.818379
402.599201	8000.402000	10.351885	-0.080038	4.818349
402.860245	8000.506496	10.356890	-0.080087	4.818379
402.604988	8000.516680	10.361895	-0.080040	4.818384
402.989444	8000.398928	10.366899	-0.080111	4.818347
402.745624	8000.532274	10.371904	-0.080066	4.818388
402.461774	8000.403293	10.376909	-0.080013	4.818350
402.743996	8000.490205	10.381914	-0.080066	4.818375
402.902823	8000.465043	10.386919	-0.080095	4.818367
402.941941	8000.457170	10.391923	-0.080103	4.818364
403.015016	8000.470787	10.396928	-0.080116	4.818368
402.672566	8000.445087	10.401933	-0.080053	4.818362
402.791625	8000.486666	10.406938	-0.080075	4.818374
402.867628	8000.464578	10.411943	-0.080089	4.818367
402.683910	8000.499920	10.416947	-0.080055	4.818378
402.784392	8000.415087	10.421952	-0.080074	4.818353
402.623801	8000.497003	10.426957	-0.080044	4.818378
402.560449	8000.386803	10.431962	-0.080032	4.818345
402.331920	8000.507742	10.436967	-0.079990	4.818382
402.521264	8000.393634	10.441971	-0.080025	4.818347
402.587538	8000.509136	10.446976	-0.080037	4.818381
402.507631	8000.428148	10.451981	-0.080022	4.818358
402.734265	8000.491171	10.456986	-0.080065	4.818375
402.431640	8000.509120	10.461991	-0.080008	4.818382
402.613082	8000.474804	10.466995	-0.080042	4.818371
402.755029	8000.429436	10.472000	-0.080069	4.818357
402.326799	8000.413079	10.477005	-0.079989	4.818354
402.580367	8000.527985	10.482010	-0.080036	4.818387
402.940468	8000.422516	10.487015	-0.080103	4.818354
403.034815	8000.496350	10.492019	-0.080121	4.818376
402.643035	8000.529901	10.497024	-0.080048	4.818387
402.419074	8000.445894	10.502029	-0.080006	4.818363
402.759667	8000.405341	10.507034	-0.080070	4.818350
402.617131	8000.455964	10.512039	-0.080043	4.818365
402.694624	8000.509592	10.517043	-0.080058	4.818381
403.124969	8000.499703	10.522048	-0.080138	4.818376
402.694361	8000.459131	10.527053	-0.080058	4.818366
402.781769	8000.397248	10.532058	-0.080074	4.818347
402.835838	8000.518893	10.537063	-0.080084	4.818383
402.474963	8000.532891	10.542067	-0.080017	4.818389
402.773268	8000.403449	10.547072	-0.080073	4.818349
403.183229	8000.476337	10.552077	-0.080149	4.818369
403.054588	8000.516637	10.557082	-0.080125	4.818382
403.400918	8000.490882	10.562087	-0.080190	4.818373
403.021981	8000.440501	10.567091	-0.080119	4.818359
403.307629	8000.499076	10.572096	-0.080172	4.818375
403.053430	8000.476683	10.577101	-0.080125	4.818370
402.790995	8000.434202	10.582106	-0.080076	4.818358
402.805429	8000.360810	10.587111	-0.080079	4.818336
403.084534	8000.529684	10.592115	-0.080131	4.818385
403.148430	8000.441196	10.597120	-0.080143	4.818359
402.991613	8000.500035	10.602125	-0.080114	4.818377
402.998118	8000.513795	10.607130	-0.080115	4.818381
402.877373	8000.423836	10.612135	-0.080093	4.818355
402.740819	8000.494517	10.617139	-0.080067	4.818376
403.049323	8000.445115	10.622144	-0.080125	4.818360
402.852428	8000.494996	10.627149	-0.080088	4.818376
402.502226	8000.446061	10.632154	-0.080023	4.818363
402.149538	8000.328758	10.637159	-0.079957	4.818329
402.623812	8000.380443	10.642163	-0.080046	4.818343
402.677920	8000.333875	10.647168	-0.080056	4.818329
402.682121	8000.496891	10.652173	-0.080057	4.818377
402.675768	8000.486294	10.657178	-0.080055	4.818374
402.622786	8000.362569	10.662183	-0.080046	4.818338
402.653522	8000.496510	10.667187	-0.080051	4.818377
402.782946	8000.436252	10.672192	-0.080075	4.818359
402.550122	8000.384715	10.677197	-0.080032	4.818344
402.803652	8000.375564	10.682202	-0.080079	4.818341
402.889847	8000.510264	10.687207	-0.080096	4.818380
403.188712	8000.482809	10.692211	-0.080151	4.818371
402.813555	8000.437738	10.697216	-0.080081	4.818359
402.909439	8000.491617	10.702221	-0.080099	4.818375
402.871333	8000.503716	10.707226	-0.080092	4.818379
403.107489	8000.451224	10.712231	-0.080136	4.818362
402.763406	8000.472811	10.717235	-0.080072	4.818370
402.751281	8000.442160	10.722240	-0.080070	4.818361
402.852201	8000.479286	10.727245	-0.080089	4.818371
402.802208	8000.519609	10.732250	-0.080080	4.818384
402.552061	8000.372164	10.737255	-0.080033	4.818341
402.801018	8000.494367	10.742259	-0.080080	4.818376
402.742506	8000.326410	10.747264	-0.080069	4.818326
402.748245	8000.498909	10.752269	-0.080070	4.818378
402.883985	8000.430327	10.757274	-0.080095	4.818357
402.790855	8000.452188	10.762279	-0.080078	4.818364
402.771457	8000.501338	10.767283	-0.080074	4.818378
402.618664	8000.450894	10.772288	-0.080046	4.818364
402.680341	8000.427559	10.777293	-0.080057	4.818357
402.747111	8000.326495	10.782298	-0.080070	4.818326
402.821512	8000.365362	10.787303	-0.080084	4.818338
402.733353	8000.404112	10.792307	-0.080067	4.818349
402.738125	8000.373691	10.797312	-0.080068	4.818340
402.319141	8000.447874	10.802317	-0.079990	4.818364
402.651038	8000.391432	10.807322	-0.080052	4.818346
402.276442	8000.448349	10.812327	-0.079982	4.818364
402.214013	8000.433833	10.817331	-0.079971	4.818360
402.112029	8000.163309	10.822336	-0.079952	4.818280
401.764393	8000.166980	10.827341	-0.079887	4.818283
401.864723	8000.275584	10.832346	-0.079906	4.818315
402.113175	8000.280029	10.837351	-0.079952	4.818315
402.223691	8000.449750	10.842355	-0.079973	4.818365
401.973035	8000.238173	10.847360	-0.079926	4.818303
401.739415	8000.204501	10.852365	-0.079883	4.818294
402.213805	8000.387597	10.857370	-0.079971	4.818347
402.310026	8000.382606	10.862375	-0.079989	4.818345
402.127836	8000.452663	10.867379	-0.079955	4.818366
402.257221	8000.366122	10.872384	-0.079979	4.818340
402.413392	8000.486005	10.877389	-0.080008	4.818375
402.564930	8000.432357	10.882394	-0.080037	4.818359
402.615091	8000.450918	10.887399	-0.080046	4.818364
402.296529	8000.433956	10.892403	-0.079987	4.818360
402.901060	8000.448522	10.897408	-0.080099	4.818362
403.067560	8000.506520	10.902413	-0.080131	4.818379
403.226190	8000.514998	10.907418	-0.080160	4.818380
403.190350	8000.418840	10.912423	-0.080153	4.818352
402.789959	8000.450171	10.917427	-0.080079	4.818363
402.573785	8000.416734	10.922432	-0.080039	4.818354
402.843706	8000.455117	10.927437	-0.080089	4.818364
403.370439	8000.466520	10.932442	-0.080187	4.818365
403.160293	8000.469961	10.937447	-0.080148	4.818367
402.477708	8000.452231	10.942451	-0.080021	4.818365
402.758692	8000.368811	10.947456	-0.080073	4.818339
402.898825	8000.527377	10.952461	-0.080100	4.818385
403.008016	8000.439507	10.957466	-0.080120	4.818359
403.244965	8000.526855	10.962471	-0.080164	4.818384
403.179414	8000.431341	10.967475	-0.080152	4.818356
403.575793	8000.492481	10.972480	-0.080226	4.818372
403.511466	8000.466373	10.977485	-0.080214	4.818365
403.372689	8000.483404	10.982490	-0.080188	4.818370
403.196949	8000.522009	10.987495	-0.080155	4.818383
403.327100	8000.471223	10.992499	-0.080180	4.818367
403.179027	8000.427150	10.997504	-0.080152	4.818354
402.826339	8000.429695	11.002509	-0.080086	4.818357
402.475027	8000.405977	11.007514	-0.080021	4.818351
402.897732	8000.438036	11.012519	-0.080100	4.818359
403.056177	8000.409715	11.017523	-0.080129	4.818350
403.042502	8000.425301	11.022528	-0.080127	4.818354
403.108250	8000.511361	11.027533	-0.080139	4.818380
403.538348	8000.497264	11.032538	-0.080219	4.818374
403.602054	8000.485522	11.037543	-0.080231	4.818370
403.664022	8000.453780	11.042547	-0.080243	4.818360
403.311977	8000.504695	11.047552	-0.080177	4.818377
403.298703	8000.458257	11.052557	-0.080175	4.818363
403.378645	8000.470917	11.057562	-0.080190	4.818367
403.750317	8000.472845	11.062567	-0.080259	4.818366
403.417131	8000.472501	11.067571	-0.080197	4.818367
403.455618	8000.427822	11.072576	-0.080204	4.818354
403.600549	8000.465551	11.077581	-0.080231	4.818364
403.535110	8000.495149	11.082586	-0.080219	4.818373
403.466133	8000.502621	11.087591	-0.080206	4.818376
403.445065	8000.482361	11.092595	-0.080202	4.818370
403.512760	8000.528497	11.097600	-0.080215	4.818383
403.314168	8000.426960	11.102605	-0.080178	4.818354
403.097396	8000.519674	11.107610	-0.080138	4.818382
403.277416	8000.502161	11.112615	-0.080171	4.818376
403.393853	8000.477471	11.117619	-0.080193	4.818369
403.179725	8000.361005	11.122624	-0.080153	4.818335
403.093404	8000.466014	11.127629	-0.080137	4.818366
403.333373	8000.484014	11.132634	-0.080182	4.818371
403.191304	8000.520976	11.137639	-0.080156	4.818382
402.757986	8000.408876	11.142643	-0.080075	4.818351
403.005381	8000.378615	11.147648	-0.080121	4.818341
403.124464	8000.503251	11.152653	-0.080143	4.818377
402.822831	8000.380334	11.157658	-0.080087	4.818342
403.261383	8000.435739	11.162663	-0.080169	4.818357
403.028388	8000.530334	11.167667	-0.080126	4.818386
402.790005	8000.337842	11.172672	-0.080081	4.818329
403.462486	8000.526809	11.177677	-0.080206	4.818383
403.375795	8000.513012	11.182682	-0.080190	4.818379
403.024782	8000.426215	11.187687	-0.080125	4.818355
403.342049	8000.477863	11.192691	-0.080184	4.818369
403.306389	8000.517330	11.197696	-0.080178	4.818381
403.282742	8000.425543	11.202701	-0.080173	4.818354
402.678919	8000.457250	11.207706	-0.080061	4.818365
402.764369	8000.393238	11.212711	-0.080077	4.818346
402.724331	8000.441055	11.217715	-0.080069	4.818360
403.318653	8000.520667	11.222720	-0.080180	4.818382
403.153522	8000.477412	11.227725	-0.080149	4.818369
403.071917	8000.417426	11.232730	-0.080134	4.818352
403.209067	8000.507615	11.237735	-0.080160	4.818378
403.286305	8000.484492	11.242739	-0.080174	4.818371
403.780048	8000.422903	11.247744	-0.080266	4.818351
403.370019	8000.498259	11.252749	-0.080190	4.818375
403.639859	8000.492486	11.257754	-0.080240	4.818372
403.449451	8000.507761	11.262759	-0.080205	4.818377
403.555353	8000.498698	11.267763	-0.080225	4.818374
403.409871	8000.522997	11.272768	-0.080197	4.818382
403.106681	8000.410570	11.277773	-0.080141	4.818350
403.101888	8000.515642	11.282778	-0.080140	4.818381
403.327880	8000.350517	11.287783	-0.080182	4.818331
403.238832	8000.478619	11.292787	-0.080166	4.818369
403.376951	8000.516255	11.297792	-0.080192	4.818380
403.502421	8000.418094	11.302797	-0.080215	4.818350
403.318096	8000.514406	11.307802	-0.080181	4.818380
403.340630	8000.476868	11.312807	-0.080185	4.818369
403.759928	8000.404800	11.317811	-0.080263	4.818345
403.548220	8000.517560	11.322816	-0.080224	4.818380
403.317946	8000.493390	11.327821	-0.080181	4.818374
403.473653	8000.491315	11.332826	-0.080210	4.818372
403.810604	8000.518000	11.337831	-0.080273	4.818379
403.828175	8000.468830	11.342835	-0.080276	4.818364
403.878096	8000.503159	11.347840	-0.080285	4.818374
403.766364	8000.487967	11.352845	-0.080265	4.818370
403.937589	8000.453513	11.357850	-0.080296	4.818359
403.701536	8000.486037	11.362855	-0.080253	4.818370
403.834614	8000.452112	11.367859	-0.080277	4.818359
403.833732	8000.480490	11.372864	-0.080277	4.818368
403.491736	8000.422201	11.377869	-0.080214	4.818352
403.385555	8000.542710	11.382874	-0.080194	4.818388
403.382674	8000.453309	11.387879	-0.080193	4.818361
403.338323	8000.468477	11.392883	-0.080185	4.818366
403.160277	8000.439764	11.397888	-0.080152	4.818358
403.307273	8000.509062	11.402893	-0.080179	4.818378
403.859490	8000.372574	11.407898	-0.080282	4.818335
403.694033	8000.504890	11.412903	-0.080252	4.818375
403.462800	8000.470193	11.417907	-0.080209	4.818366
403.244757	8000.469320	11.422912	-0.080168	4.818367
403.382238	8000.524821	11.427917	-0.080194	4.818383
403.325917	8000.404201	11.432922	-0.080183	4.818347
403.479666	8000.512491	11.437927	-0.080212	4.818379
403.189975	8000.525357	11.442931	-0.080158	4.818384
403.281895	8000.446714	11.447936	-0.080175	4.818360
403.501804	8000.447619	11.452941	-0.080216	4.818359
403.637853	8000.530435	11.457946	-0.080242	4.818383
403.277486	8000.466639	11.462951	-0.080174	4.818366
403.447281	8000.496297	11.467955	-0.080206	4.818374
403.601610	8000.491049	11.472960	-0.080235	4.818372
403.617349	8000.404005	11.477965	-0.080238	4.818346
403.486575	8000.447430	11.482970	-0.080214	4.818359
403.557647	8000.382169	11.487975	-0.080227	4.818339
404.009747	8000.451431	11.492979	-0.080311	4.818358
403.541348	8000.474472	11.497984	-0.080224	4.818367
403.605125	8000.517400	11.502989	-0.080236	4.818379
403.891230	8000.520262	11.507994	-0.080289	4.818379
403.664469	8000.427801	11.512999	-0.080247	4.818353
403.437557	8000.490939	11.518003	-0.080205	4.818372
403.517158	8000.421589	11.523008	-0.080220	4.818351
403.643011	8000.483239	11.528013	-0.080243	4.818369
403.554542	8000.475725	11.533018	-0.080227	4.818367
403.368927	8000.334415	11.538023	-0.080192	4.818326
404.067065	8000.498506	11.543027	-0.080322	4.818372
403.745955	8000.550894	11.548032	-0.080262	4.818389
403.860511	8000.494638	11.553037	-0.080284	4.818372
403.899423	8000.418424	11.558042	-0.080291	4.818349
404.122885	8000.504538	11.563047	-0.080333	4.818374
403.946669	8000.476900	11.568051	-0.080300	4.818366
403.973729	8000.516174	11.573056	-0.080305	4.818378
404.099784	8000.505283	11.578061	-0.080329	4.818374
403.895378	8000.433103	11.583066	-0.080291	4.818353
404.420791	8000.522294	11.588071	-0.080388	4.818378
404.046931	8000.510879	11.593075	-0.080319	4.818376
403.921043	8000.528086	11.598080	-0.080295	4.818381
403.783311	8000.493615	11.603085	-0.080270	4.818372
403.736627	8000.419385	11.608090	-0.080261	4.818350
403.538723	8000.502895	11.613095	-0.080224	4.818375
403.501822	8000.507651	11.618099	-0.080218	4.818377
403.554114	8000.441082	11.623104	-0.080227	4.818357
403.560837	8000.534748	11.628109	-0.080229	4.818385
403.462216	8000.426166	11.633114	-0.080210	4.818353
403.799257	8000.509625	11.638119	-0.080273	4.818376
403.550220	8000.524099	11.643123	-0.080227	4.818382
403.755600	8000.447005	11.648128	-0.080265	4.818358
403.488456	8000.440204	11.653133	-0.080215	4.818357
403.986871	8000.480661	11.658138	-0.080308	4.818367
403.848530	8000.455644	11.663143	-0.080283	4.818360
404.100285	8000.489577	11.668147	-0.080329	4.818369
404.193581	8000.519242	11.673152	-0.080347	4.818378
404.002412	8000.497708	11.678157	-0.080311	4.818372
403.655007	8000.413061	11.683162	-0.080247	4.818348
404.186307	8000.519153	11.688167	-0.080346	4.818378
404.097099	8000.483241	11.693171	-0.080329	4.818367
404.146640	8000.529130	11.698176	-0.080338	4.818381
403.838856	8000.509157	11.703181	-0.080281	4.818376
403.855088	8000.415811	11.708186	-0.080284	4.818348
403.915373	8000.520722	11.713191	-0.080295	4.818379
403.747737	8000.504767	11.718195	-0.080264	4.818375
403.955830	8000.438224	11.723200	-0.080303	4.818354
404.105452	8000.505456	11.728205	-0.080331	4.818374
403.873420	8000.504391	11.733210	-0.080288	4.818374
403.994468	8000.427196	11.738215	-0.080310	4.818351
404.041824	8000.490929	11.743219	-0.080319	4.818370
404.073499	8000.491365	11.748224	-0.080325	4.818370
403.964040	8000.500386	11.753229	-0.080305	4.818373
404.085785	8000.515720	11.758234	-0.080328	4.818377
403.971024	8000.422687	11.763239	-0.080306	4.818350
403.688134	8000.506087	11.768243	-0.080254	4.818376
404.013133	8000.422217	11.773248	-0.080314	4.818349
404.195303	8000.486740	11.778253	-0.080348	4.818368
403.749249	8000.502726	11.783258	-0.080265	4.818374
404.153234	8000.509302	11.788263	-0.080340	4.818375
404.134405	8000.455428	11.793267	-0.080337	4.818359
403.791541	8000.458105	11.798272	-0.080273	4.818361
403.647959	8000.470865	11.803277	-0.080246	4.818365
403.743247	8000.455349	11.808282	-0.080264	4.818360
403.768589	8000.431517	11.813287	-0.080269	4.818353
403.537514	8000.486188	11.818291	-0.080226	4.818370
403.555642	8000.427563	11.823296	-0.080229	4.818353
403.418784	8000.427799	11.828301	-0.080204	4.818354
403.014160	8000.328706	11.833306	-0.080129	4.818326
403.400536	8000.388656	11.838311	-0.080201	4.818342
403.429654	8000.438470	11.843315	-0.080206	4.818357
404.375487	8000.508172	11.848320	-0.080382	4.818374
403.611363	8000.500887	11.853325	-0.080240	4.818374
403.883929	8000.472022	11.858330	-0.080291	4.818365
403.887389	8000.517281	11.863335	-0.080292	4.818378
403.913687	8000.459819	11.868339	-0.080296	4.818361
403.906301	8000.504930	11.873344	-0.080295	4.818374
404.068928	8000.382043	11.878349	-0.080325	4.818337
403.956382	8000.524545	11.883354	-0.080305	4.818380
404.000209	8000.526199	11.888359	-0.080313	4.818380
404.056052	8000.455472	11.893363	-0.080323	4.818359
404.038565	8000.549859	11.898368	-0.080320	4.818387
403.706135	8000.430721	11.903373	-0.080258	4.818353
403.999441	8000.509379	11.908378	-0.080313	4.818375
404.101127	8000.522337	11.913383	-0.080332	4.818379
403.614034	8000.414753	11.918387	-0.080241	4.818349
404.264288	8000.517214	11.923392	-0.080362	4.818377
404.181959	8000.484551	11.928397	-0.080347	4.818367
404.145125	8000.477742	11.933402	-0.080340	4.818365
404.522954	8000.494475	11.938407	-0.080410	4.818369
404.354588	8000.484817	11.943411	-0.080379	4.818367
404.235382	8000.524194	11.948416	-0.080357	4.818379
404.203371	8000.516400	11.953421	-0.080351	4.818377
404.119599	8000.439560	11.958426	-0.080336	4.818354
404.250737	8000.316243	11.963431	-0.080360	4.818317
404.149842	8000.543014	11.968435	-0.080341	4.818385
403.814977	8000.431201	11.973440	-0.080279	4.818353
403.901296	8000.440795	11.978445	-0.080295	4.818355
403.855006	8000.523223	11.983450	-0.080287	4.818380
403.982490	8000.433500	11.988455	-0.080310	4.818353
403.974888	8000.495430	11.993459	-0.080309	4.818371
404.128059	8000.529067	11.998464	-0.080338	4.818381
404.182119	8000.481446	12.003469	-0.080348	4.818366
404.252310	8000.458227	12.008474	-0.080361	4.818359
404.429763	8000.493249	12.013479	-0.080394	4.818369
403.847843	8000.502120	12.018483	-0.080285	4.818374
404.028079	8000.505638	12.023488	-0.080319	4.818374
403.995644	8000.416883	12.028493	-0.080313	4.818348
403.640135	8000.491932	12.033498	-0.080247	4.818372
403.765226	8000.434768	12.038503	-0.080270	4.818354
404.073662	8000.442140	12.043507	-0.080328	4.818355
403.852655	8000.494846	12.048512	-0.080287	4.818372
403.903520	8000.476619	12.053517	-0.080296	4.818366
403.641865	8000.518256	12.058522	-0.080247	4.818379
403.525696	8000.520877	12.063527	-0.080226	4.818381
403.564659	8000.489872	12.068531	-0.080233	4.818371
403.766996	8000.473715	12.073536	-0.080271	4.818366
404.072634	8000.487357	12.078541	-0.080328	4.818369
404.139181	8000.427291	12.083546	-0.080340	4.818350
404.089864	8000.461315	12.088551	-0.080331	4.818361
404.149311	8000.386432	12.093555	-0.080342	4.818338
404.563117	8000.401553	12.098560	-0.080419	4.818341
404.577723	8000.405962	12.103565	-0.080422	4.818342
404.470365	8000.443398	12.108570	-0.080402	4.818354
404.483260	8000.502455	12.113575	-0.080405	4.818371
404.189485	8000.492134	12.118579	-0.080350	4.818369
404.174706	8000.501398	12.123584	-0.080347	4.818372
403.567637	8000.367994	12.128589	-0.080234	4.818335
403.783916	8000.327846	12.133594	-0.080274	4.818322
403.742578	8000.417701	12.138599	-0.080267	4.818349
403.639245	8000.540352	12.143603	-0.080248	4.818386
403.669774	8000.336810	12.148608	-0.080253	4.818325
404.185932	8000.435334	12.153613	-0.080350	4.818353
403.737974	8000.456551	12.158618	-0.080266	4.818361
403.905311	8000.432557	12.163623	-0.080297	4.818353
404.303178	8000.525261	12.168627	-0.080372	4.818379
404.001380	8000.464365	12.173632	-0.080315	4.818362
403.931724	8000.456057	12.178637	-0.080302	4.818360
404.005606	8000.448659	12.183642	-0.080316	4.818357
404.203226	8000.537575	12.188647	-0.080353	4.818383
403.946218	8000.486754	12.193651	-0.080305	4.818369
404.265651	8000.518459	12.198656	-0.080365	4.818377
404.123953	8000.494447	12.203661	-0.080338	4.818370
404.362130	8000.455650	12.208666	-0.080383	4.818358
404.414829	8000.504737	12.213671	-0.080393	4.818372
404.630504	8000.435143	12.218675	-0.080433	4.818351
404.351235	8000.494412	12.223680	-0.080381	4.818369
404.404685	8000.456245	12.228685	-0.080391	4.818358
404.312174	8000.376131	12.233690	-0.080374	4.818334
404.234324	8000.508594	12.238695	-0.080359	4.818374
404.147934	8000.475875	12.243699	-0.080343	4.818365
403.971972	8000.548120	12.248704	-0.080311	4.818387
403.903715	8000.454671	12.253709	-0.080298	4.818359
403.705079	8000.425676	12.258714	-0.080261	4.818352
404.079260	8000.519107	12.263719	-0.080331	4.818378
403.887201	8000.519639	12.268723	-0.080295	4.818379
404.038289	8000.444958	12.273728	-0.080323	4.818356
403.641988	8000.467932	12.278733	-0.080249	4.818364
403.902181	8000.471491	12.283738	-0.080298	4.818364
404.356604	8000.513451	12.288743	-0.080383	4.818375
404.518102	8000.480967	12.293747	-0.080413	4.818365
404.584243	8000.499747	12.298752	-0.080425	4.818370
404.351996	8000.410363	12.303757	-0.080382	4.818344
403.935083	8000.521370	12.308762	-0.080304	4.818379
403.592557	8000.352682	12.313767	-0.080240	4.818330
403.676493	8000.436888	12.318771	-0.080256	4.818355
404.055392	8000.514613	12.323776	-0.080327	4.818377
403.799405	8000.449088	12.328781	-0.080279	4.818358
403.683096	8000.371804	12.333786	-0.080257	4.818336
403.920887	8000.525401	12.338791	-0.080302	4.818380
404.043133	8000.397757	12.343795	-0.080325	4.818342
403.980973	8000.500996	12.348800	-0.080313	4.818373
404.119621	8000.492380	12.353805	-0.080339	4.818370
404.313607	8000.451928	12.358810	-0.080375	4.818357
404.333669	8000.506877	12.363815	-0.080379	4.818373
404.106565	8000.430181	12.368819	-0.080337	4.818351
403.939229	8000.433154	12.373824	-0.080306	4.818353
403.874398	8000.371292	12.378829	-0.080293	4.818335
404.049567	8000.512469	12.383834	-0.080326	4.818376
404.296372	8000.515846	12.388839	-0.080372	4.818376
404.019574	8000.520476	12.393843	-0.080321	4.818379
404.226443	8000.459174	12.398848	-0.080359	4.818359
404.557105	8000.448977	12.403853	-0.080421	4.818355
404.207221	8000.458917	12.408858	-0.080356	4.818359
404.632858	8000.514153	12.413863	-0.080435	4.818374
404.531342	8000.484381	12.418867	-0.080416	4.818366
404.685797	8000.510678	12.423872	-0.080445	4.818373
404.406440	8000.482680	12.428877	-0.080393	4.818366
404.469953	8000.503528	12.433882	-0.080405	4.818372
404.511954	8000.510413	12.438887	-0.080413	4.818374
404.753149	8000.432758	12.443891	-0.080458	4.818349
404.600415	8000.492704	12.448896	-0.080429	4.818368
404.340401	8000.484948	12.453901	-0.080381	4.818367
404.207331	8000.503108	12.458906	-0.080356	4.818373
404.303447	8000.490757	12.463911	-0.080374	4.818369
404.394700	8000.467826	12.468915	-0.080391	4.818361
404.404387	8000.500554	12.473920	-0.080393	4.818371
404.468405	8000.459378	12.478925	-0.080405	4.818359
404.522714	8000.438044	12.483930	-0.080415	4.818352
404.805010	8000.458728	12.488935	-0.080468	4.818357
404.558057	8000.461664	12.493939	-0.080422	4.818359
404.878449	8000.443968	12.498944	-0.080482	4.818352
404.947461	8000.420733	12.503949	-0.080494	4.818345
404.716876	8000.395505	12.508954	-0.080451	4.818339
404.698578	8000.459392	12.513959	-0.080448	4.818358
404.615230	8000.456153	12.518963	-0.080433	4.818357
404.657786	8000.484074	12.523968	-0.080441	4.818365
404.718370	8000.465981	12.528973	-0.080452	4.818359
404.952805	8000.380873	12.533978	-0.080496	4.818333
405.123577	8000.461013	12.538983	-0.080528	4.818356
404.879431	8000.462935	12.543987	-0.080482	4.818358
404.580899	8000.456754	12.548992	-0.080427	4.818357
404.634785	8000.443826	12.553997	-0.080437	4.818353
404.608722	8000.450833	12.559002	-0.080432	4.818355
404.819099	8000.457917	12.564007	-0.080471	4.818357
404.475369	8000.438503	12.569011	-0.080407	4.818352
404.530167	8000.464488	12.574016	-0.080417	4.818360
404.490848	8000.471313	12.579021	-0.080410	4.818362
404.474187	8000.486859	12.584026	-0.080407	4.818367
404.794932	8000.488093	12.589031	-0.080467	4.818366
404.866222	8000.442810	12.594035	-0.080480	4.818352
404.797989	8000.499707	12.599040	-0.080467	4.818369
404.764237	8000.465604	12.604045	-0.080461	4.818359
404.489953	8000.477628	12.609050	-0.080410	4.818364
404.157733	8000.425779	12.614055	-0.080348	4.818350
404.514252	8000.483224	12.619059	-0.080415	4.818365
404.549237	8000.518401	12.624064	-0.080421	4.818376
404.412538	8000.488148	12.629069	-0.080396	4.818367
404.374137	8000.494986	12.634074	-0.080389	4.818369
404.824512	8000.488529	12.639079	-0.080473	4.818366
404.761299	8000.458230	12.644083	-0.080461	4.818357
404.553944	8000.495350	12.649088	-0.080422	4.818369
404.453927	8000.501346	12.654093	-0.080404	4.818371
404.716718	8000.466041	12.659098	-0.080453	4.818359
404.375389	8000.479251	12.664103	-0.080389	4.818365
404.402701	8000.438624	12.669107	-0.080394	4.818353
404.397054	8000.443807	12.674112	-0.080393	4.818354
403.984988	8000.435025	12.679117	-0.080317	4.818353
403.820691	8000.445399	12.684122	-0.080286	4.818357
404.590633	8000.513751	12.689127	-0.080430	4.818374
404.465659	8000.539382	12.694131	-0.080406	4.818382
404.498605	8000.513551	12.699136	-0.080413	4.818374
404.518457	8000.508568	12.704141	-0.080416	4.818373
404.602457	8000.402479	12.709146	-0.080432	4.818341
404.352297	8000.535742	12.714151	-0.080385	4.818382
404.221568	8000.521341	12.719155	-0.080361	4.818378
404.330249	8000.421898	12.724160	-0.080381	4.818348
404.472762	8000.514268	12.729165	-0.080408	4.818375
404.366784	8000.524387	12.734170	-0.080388	4.818378
404.444290	8000.424518	12.739175	-0.080403	4.818348
404.431127	8000.481116	12.744179	-0.080400	4.818365
404.501940	8000.467367	12.749184	-0.080414	4.818361
404.399072	8000.494352	12.754189	-0.080394	4.818369
404.624916	8000.491134	12.759194	-0.080437	4.818367
404.705230	8000.524828	12.764199	-0.080452	4.818377
404.202589	8000.510600	12.769203	-0.080358	4.818375
404.355660	8000.430689	12.774208	-0.080387	4.818350
404.457004	8000.534060	12.779213	-0.080406	4.818381
404.264635	8000.421040	12.784218	-0.080370	4.818348
404.519355	8000.543330	12.789223	-0.080417	4.818383
404.256996	8000.434610	12.794227	-0.080368	4.818352
404.277502	8000.542133	12.799232	-0.080372	4.818384
404.260797	8000.443079	12.804237	-0.080369	4.818354
404.176413	8000.533398	12.809242	-0.080354	4.818382
404.297007	8000.443580	12.814247	-0.080376	4.818354
404.282897	8000.493856	12.819251	-0.080373	4.818369
404.208993	8000.539110	12.824256	-0.080360	4.818383
404.581073	8000.476911	12.829261	-0.080429	4.818363
404.466113	8000.433288	12.834266	-0.080408	4.818351
404.450392	8000.524546	12.839271	-0.080405	4.818378
404.125433	8000.433895	12.844275	-0.080344	4.818352
404.295963	8000.545571	12.849280	-0.080376	4.818385
404.247765	8000.432419	12.854285	-0.080367	4.818351
404.289639	8000.512899	12.859290	-0.080375	4.818375
404.442937	8000.540231	12.864295	-0.080404	4.818383
404.406793	8000.426191	12.869299	-0.080397	4.818349
404.275314	8000.453836	12.874304	-0.080372	4.818358
404.157934	8000.547909	12.879309	-0.080351	4.818386
404.307028	8000.414323	12.884314	-0.080378	4.818346
404.633404	8000.520771	12.889319	-0.080439	4.818376
404.421954	8000.500010	12.894323	-0.080400	4.818371
404.639566	8000.520862	12.899328	-0.080441	4.818376
404.533952	8000.501548	12.904333	-0.080421	4.818371
404.188133	8000.525211	12.909338	-0.080357	4.818379
404.147849	8000.351188	12.914343	-0.080349	4.818328
404.186091	8000.518881	12.919347	-0.080356	4.818377
404.342529	8000.525228	12.924352	-0.080385	4.818379
404.247670	8000.427209	12.929357	-0.080368	4.818350
404.226977	8000.486857	12.934362	-0.080364	4.818368
404.033229	8000.401154	12.939367	-0.080328	4.818343
403.959895	8000.523165	12.944371	-0.080314	4.818379
403.704865	8000.446088	12.949376	-0.080267	4.818358
403.702010	8000.476541	12.954381	-0.080266	4.818367
403.601228	8000.461500	12.959386	-0.080248	4.818363
403.893958	8000.353007	12.964391	-0.080302	4.818329
403.886591	8000.512717	12.969395	-0.080301	4.818377
404.041729	8000.455964	12.974400	-0.080330	4.818359
404.262716	8000.523121	12.979405	-0.080371	4.818378
404.164972	8000.426113	12.984410	-0.080353	4.818350
404.450020	8000.528842	12.989415	-0.080406	4.818379
404.353093	8000.512801	12.994419	-0.080388	4.818375
404.286222	8000.449859	12.999424	-0.080376	4.818356
404.274137	8000.512779	13.004429	-0.080373	4.818375
404.250229	8000.510353	13.009434	-0.080369	4.818374
404.440929	8000.532939	13.014439	-0.080405	4.818380
404.608773	8000.401712	13.019443	-0.080436	4.818341
404.558541	8000.525091	13.024448	-0.080427	4.818378
404.811989	8000.524354	13.029453	-0.080474	4.818376
404.576240	8000.447537	13.034458	-0.080430	4.818354
404.605615	8000.528898	13.039463	-0.080435	4.818379
404.129764	8000.532910	13.044467	-0.080347	4.818382
404.241627	8000.332579	13.049472	-0.080368	4.818322
404.299657	8000.520519	13.054477	-0.080379	4.818377
404.308097	8000.497508	13.059482	-0.080380	4.818370
404.146259	8000.441679	13.064487	-0.080350	4.818354
403.898491	8000.460375	13.069491	-0.080304	4.818361
404.437539	8000.501389	13.074496	-0.080404	4.818371
404.539666	8000.508046	13.079501	-0.080423	4.818373
404.343755	8000.433877	13.084506	-0.080387	4.818351
404.593848	8000.530872	13.089511	-0.080434	4.818379
404.596386	8000.480443	13.094515	-0.080434	4.818364
404.912182	8000.525768	13.099520	-0.080493	4.818376
404.765107	8000.525863	13.104525	-0.080466	4.818377
404.707097	8000.498789	13.109530	-0.080455	4.818369
404.905441	8000.493092	13.114535	-0.080492	4.818367
404.483465	8000.478916	13.119539	-0.080413	4.818364
404.732785	8000.415039	13.124544	-0.080460	4.818344
404.891644	8000.492913	13.129549	-0.080489	4.818367
404.729789	8000.471779	13.134554	-0.080459	4.818361
404.685640	8000.489052	13.139559	-0.080451	4.818366
404.543161	8000.500775	13.144563	-0.080425	4.818370
404.370714	8000.459520	13.149568	-0.080393	4.818359
404.682154	8000.506887	13.154573	-0.080451	4.818372
404.644298	8000.492705	13.159578	-0.080444	4.818368
404.955928	8000.523254	13.164583	-0.080502	4.818375
404.825933	8000.456293	13.169587	-0.080478	4.818356
404.721462	8000.507437	13.174592	-0.080458	4.818372
404.855926	8000.496662	13.179597	-0.080483	4.818368
404.737676	8000.449839	13.184602	-0.080461	4.818354
404.593357	8000.530929	13.189607	-0.080434	4.818379
404.848581	8000.494469	13.194611	-0.080482	4.818367
404.562404	8000.513690	13.199616	-0.080429	4.818374
404.865571	8000.507324	13.204621	-0.080485	4.818371
404.749041	8000.500477	13.209626	-0.080464	4.818369
404.728838	8000.427659	13.214631	-0.080460	4.818348
404.663023	8000.489845	13.219635	-0.080448	4.818367
404.660842	8000.515051	13.224640	-0.080447	4.818374
404.814844	8000.490876	13.229645	-0.080476	4.818366
404.796438	8000.481165	13.234650	-0.080473	4.818364
404.621136	8000.514518	13.239655	-0.080440	4.818374
404.881595	8000.486541	13.244659	-0.080489	4.818365
405.009244	8000.521934	13.249664	-0.080512	4.818375
404.964151	8000.524475	13.254669	-0.080504	4.818376
404.679920	8000.481690	13.259674	-0.080451	4.818364
404.860666	8000.504141	13.264679	-0.080485	4.818370
404.813032	8000.401509	13.269683	-0.080476	4.818340
404.981122	8000.506846	13.274688	-0.080507	4.818370
404.788853	8000.492655	13.279693	-0.080472	4.818367
404.988112	8000.457532	13.284698	-0.080509	4.818356
404.980521	8000.508950	13.289703	-0.080507	4.818371
404.901796	8000.479489	13.294707	-0.080493	4.818363
404.648542	8000.501263	13.299712	-0.080446	4.818370
404.985746	8000.500620	13.304717	-0.080508	4.818369
404.824121	8000.496310	13.309722	-0.080478	4.818368
405.145326	8000.508065	13.314727	-0.080538	4.818370
404.900160	8000.464763	13.319731	-0.080493	4.818358
404.773376	8000.468290	13.324736	-0.080469	4.818360
405.059629	8000.443820	13.329741	-0.080522	4.818351
404.977321	8000.442697	13.334746	-0.080507	4.818351
405.271076	8000.445666	13.339751	-0.080562	4.818351
404.829684	8000.446994	13.344755	-0.080480	4.818353
405.163517	8000.451561	13.349760	-0.080542	4.818353
405.055100	8000.484778	13.354765	-0.080522	4.818364
404.961935	8000.494021	13.359770	-0.080505	4.818367
404.960117	8000.512924	13.364775	-0.080504	4.818372
404.747142	8000.471114	13.369779	-0.080465	4.818361
404.720236	8000.442362	13.374784	-0.080460	4.818352
404.633450	8000.537906	13.379789	-0.080444	4.818381
404.742444	8000.416388	13.384794	-0.080464	4.818344
404.758628	8000.531213	13.389799	-0.080467	4.818379
404.632122	8000.470609	13.394803	-0.080443	4.818361
404.499180	8000.497182	13.399808	-0.080419	4.818369
404.535841	8000.510303	13.404813	-0.080426	4.818373
404.315593	8000.488371	13.409818	-0.080385	4.818368
404.740152	8000.537285	13.414823	-0.080464	4.818380
404.731905	8000.386827	13.419827	-0.080462	4.818336
404.875767	8000.512861	13.424832	-0.080489	4.818373
404.778743	8000.502075	13.429837	-0.080471	4.818370
404.869672	8000.489653	13.434842	-0.080488	4.818366
404.643098	8000.456068	13.439847	-0.080446	4.818357
405.195980	8000.481505	13.444851	-0.080549	4.818362
404.936439	8000.503192	13.449856	-0.080501	4.818369
405.182738	8000.479227	13.454861	-0.080546	4.818361
404.873998	8000.485522	13.459866	-0.080489	4.818364
405.230558	8000.500915	13.464871	-0.080555	4.818368
405.260171	8000.439291	13.469875	-0.080561	4.818349
405.133116	8000.460688	13.474880	-0.080537	4.818356
405.234173	8000.466278	13.479885	-0.080556	4.818357
405.123091	8000.437426	13.484890	-0.080536	4.818349
405.262761	8000.488755	13.489895	-0.080562	4.818364
405.031297	8000.475079	13.494899	-0.080519	4.818361
404.989564	8000.468203	13.499904	-0.080511	4.818359
405.074041	8000.472516	13.504909	-0.080527	4.818360
405.069112	8000.407265	13.509914	-0.080526	4.818340
405.272719	8000.357483	13.514919	-0.080564	4.818325
405.279023	8000.346007	13.519923	-0.080565	4.818321
405.185669	8000.424639	13.524928	-0.080548	4.818345
405.000772	8000.474684	13.529933	-0.080513	4.818361
404.963060	8000.441578	13.534938	-0.080506	4.818351
405.187219	8000.485651	13.539943	-0.080548	4.818363
405.272005	8000.446860	13.544947	-0.080564	4.818351
405.291481	8000.467106	13.549952	-0.080568	4.818357
405.113519	8000.519349	13.554957	-0.080534	4.818374
404.943064	8000.432910	13.559962	-0.080503	4.818349
404.899459	8000.489092	13.564967	-0.080495	4.818365
404.962400	8000.448951	13.569971	-0.080506	4.818353
404.741165	8000.514270	13.574976	-0.080465	4.818374
405.180720	8000.485587	13.579981	-0.080547	4.818363
404.907901	8000.453473	13.584986	-0.080496	4.818355
405.306733	8000.487317	13.589991	-0.080571	4.818363
405.177947	8000.471891	13.594995	-0.080547	4.818359
405.002247	8000.484211	13.600000	-0.080514	4.818364
405.190039	8000.446829	13.605005	-0.080549	4.818352
405.053371	8000.430244	13.610010	-0.080524	4.818347
405.132141	8000.478637	13.615015	-0.080538	4.818361
405.267167	8000.479435	13.620019	-0.080564	4.818361
405.407061	8000.466632	13.625024	-0.080590	4.818357
404.890772	8000.519505	13.630029	-0.080494	4.818374
405.005064	8000.501094	13.635034	-0.080515	4.818369
405.146830	8000.425233	13.640039	-0.080541	4.818345
404.680968	8000.501926	13.645043	-0.080455	4.818370
404.479281	8000.535970	13.650048	-0.080417	4.818381
404.976679	8000.508078	13.655053	-0.080510	4.818371
405.146008	8000.498832	13.660058	-0.080541	4.818367
405.084426	8000.511661	13.665063	-0.080530	4.818371
405.255062	8000.450914	13.670067	-0.080562	4.818353
405.184027	8000.477282	13.675072	-0.080549	4.818361
405.237257	8000.509555	13.680077	-0.080559	4.818370
405.282024	8000.452344	13.685082	-0.080567	4.818353
405.337959	8000.489911	13.690087	-0.080577	4.818364
405.093199	8000.480258	13.695091	-0.080532	4.818362
405.071753	8000.455786	13.700096	-0.080528	4.818355
405.280256	8000.481771	13.705101	-0.080567	4.818362
405.250360	8000.468749	13.710106	-0.080561	4.818358
405.215874	8000.494565	13.715111	-0.080555	4.818366
405.106005	8000.411057	13.720115	-0.080534	4.818341
404.968305	8000.472261	13.725120	-0.080509	4.818360
405.119255	8000.474328	13.730125	-0.080537	4.818360
404.752872	8000.452500	13.735130	-0.080469	4.818355
405.251792	8000.476147	13.740135	-0.080562	4.818360
405.210717	8000.453509	13.745139	-0.080554	4.818354
405.305243	8000.461114	13.750144	-0.080572	4.818355
405.402382	8000.478216	13.755149	-0.080590	4.818360
405.238028	8000.467561	13.760154	-0.080559	4.818358
405.071838	8000.502090	13.765159	-0.080529	4.818369
404.699459	8000.464409	13.770163	-0.080459	4.818359
404.464454	8000.489586	13.775168	-0.080416	4.818367
404.930604	8000.444445	13.780173	-0.080502	4.818352
404.953229	8000.493121	13.785178	-0.080507	4.818366
405.262205	8000.511018	13.790183	-0.080564	4.818370
404.950566	8000.484680	13.795187	-0.080506	4.818364
404.777562	8000.505448	13.800192	-0.080474	4.818371
405.141126	8000.488343	13.805197	-0.080542	4.818364
405.071579	8000.471625	13.810202	-0.080529	4.818359
405.153329	8000.499031	13.815207	-0.080544	4.818367
405.064700	8000.492565	13.820211	-0.080528	4.818366
405.352779	8000.462863	13.825216	-0.080581	4.818356
405.320673	8000.489763	13.830221	-0.080575	4.818364
405.125186	8000.489196	13.835226	-0.080539	4.818364
405.343439	8000.521623	13.840231	-0.080580	4.818373
405.180785	8000.481551	13.845235	-0.080549	4.818362
405.220855	8000.478948	13.850240	-0.080557	4.818361
405.343810	8000.507970	13.855245	-0.080580	4.818369
405.366857	8000.488311	13.860250	-0.080584	4.818363
405.436634	8000.486115	13.865255	-0.080597	4.818362
405.191117	8000.460681	13.870259	-0.080552	4.818356
405.354026	8000.489197	13.875264	-0.080582	4.818364
405.311006	8000.483355	13.880269	-0.080574	4.818362
405.195187	8000.475466	13.885274	-0.080553	4.818360
405.157876	8000.500192	13.890279	-0.080546	4.818368
405.266364	8000.485908	13.895283	-0.080566	4.818363
405.254362	8000.509929	13.900288	-0.080564	4.818370
405.175886	8000.514116	13.905293	-0.080549	4.818372
404.899985	8000.501935	13.910298	-0.080498	4.818369
405.204724	8000.510311	13.915303	-0.080555	4.818370
404.810316	8000.403988	13.920307	-0.080481	4.818340
405.159184	8000.513900	13.925312	-0.080546	4.818372
405.258643	8000.512109	13.930317	-0.080565	4.818371
405.209123	8000.469380	13.935322	-0.080556	4.818358
405.228865	8000.495938	13.940327	-0.080559	4.818366
405.539438	8000.439207	13.945331	-0.080617	4.818348
405.417893	8000.480655	13.950336	-0.080595	4.818361
405.448559	8000.492643	13.955341	-0.080600	4.818364
405.394893	8000.466679	13.960346	-0.080590	4.818357
405.309027	8000.539106	13.965351	-0.080574	4.818379
405.430507	8000.495560	13.970355	-0.080597	4.818365
405.255827	8000.478455	13.975360	-0.080565	4.818361
405.405110	8000.507836	13.980365	-0.080592	4.818369
405.162215	8000.466667	13.985370	-0.080547	4.818358
405.300724	8000.512723	13.990375	-0.080573	4.818371
405.216860	8000.469524	13.995379	-0.080557	4.818358
405.420756	8000.487035	14.000384	-0.080596	4.818363
405.092137	8000.506726	14.005389	-0.080534	4.818370
405.173815	8000.450019	14.010394	-0.080550	4.818353
405.204407	8000.490394	14.015399	-0.080555	4.818364
405.238985	8000.462482	14.020403	-0.080562	4.818356
405.211889	8000.525199	14.025408	-0.080557	4.818375
405.337214	8000.520608	14.030413	-0.080580	4.818373
405.198653	8000.446169	14.035418	-0.080554	4.818351
405.222256	8000.454906	14.040423	-0.080559	4.818354
405.325727	8000.459479	14.045427	-0.080578	4.818355
405.072649	8000.483357	14.050432	-0.080531	4.818363
405.079116	8000.500271	14.055437	-0.080532	4.818368
405.091256	8000.505698	14.060442	-0.080535	4.818369
405.280457	8000.425228	14.065447	-0.080570	4.818345
404.960497	8000.508121	14.070451	-0.080510	4.818371
405.231873	8000.520247	14.075456	-0.080561	4.818373
405.394984	8000.483579	14.080461	-0.080591	4.818362
405.232421	8000.447714	14.085466	-0.080561	4.818352
405.186737	8000.521742	14.090471	-0.080553	4.818374
405.589759	8000.518846	14.095475	-0.080628	4.818371
405.636515	8000.506872	14.100480	-0.080637	4.818368
405.338878	8000.499650	14.105485	-0.080581	4.818367
405.235049	8000.471948	14.110490	-0.080562	4.818359
405.427356	8000.514535	14.115495	-0.080598	4.818371
405.084070	8000.465685	14.120499	-0.080534	4.818358
405.289581	8000.463241	14.125504	-0.080572	4.818356
405.327549	8000.492151	14.130509	-0.080579	4.818364
405.108616	8000.446053	14.135514	-0.080539	4.818352
405.226446	8000.509700	14.140519	-0.080561	4.818370
405.473110	8000.456301	14.145523	-0.080607	4.818353
405.423287	8000.462983	14.150528	-0.080597	4.818355
405.227086	8000.479228	14.155533	-0.080561	4.818361
405.366073	8000.448538	14.160538	-0.080587	4.818351
405.415714	8000.473403	14.165543	-0.080596	4.818359
405.299259	8000.467608	14.170547	-0.080574	4.818357
405.152489	8000.485580	14.175552	-0.080547	4.818363
405.412270	8000.501753	14.180557	-0.080596	4.818367
405.099648	8000.486967	14.185562	-0.080537	4.818364
405.133150	8000.504250	14.190567	-0.080544	4.818369
405.304570	8000.481364	14.195571	-0.080576	4.818361
405.277881	8000.457872	14.200576	-0.080571	4.818354
405.280277	8000.485244	14.205581	-0.080571	4.818363
405.174114	8000.413352	14.210586	-0.080551	4.818342
405.492309	8000.461865	14.215591	-0.080611	4.818355
405.426653	8000.433634	14.220595	-0.080598	4.818347
405.337032	8000.500753	14.225600	-0.080582	4.818367
405.333922	8000.499662	14.230605	-0.080581	4.818367
405.290488	8000.462272	14.235610	-0.080573	4.818356
405.261496	8000.490267	14.240615	-0.080568	4.818364
405.489623	8000.426100	14.245619	-0.080610	4.818344
405.138636	8000.459154	14.250624	-0.080545	4.818355
404.990382	8000.466592	14.255629	-0.080518	4.818358
404.710014	8000.473276	14.260634	-0.080465	4.818361
404.930605	8000.503631	14.265639	-0.080507	4.818369
404.894829	8000.478963	14.270643	-0.080500	4.818362
404.892511	8000.475781	14.275648	-0.080500	4.818361
405.038698	8000.476731	14.280653	-0.080527	4.818361
405.151865	8000.487745	14.285658	-0.080548	4.818364
405.056227	8000.500108	14.290663	-0.080530	4.818368
405.214033	8000.497012	14.295667	-0.080560	4.818366
405.340425	8000.479819	14.300672	-0.080583	4.818361
405.367928	8000.489661	14.305677	-0.080588	4.818364
405.292162	8000.445520	14.310682	-0.080574	4.818351
405.487545	8000.477635	14.315687	-0.080611	4.818359
405.563798	8000.451344	14.320691	-0.080625	4.818351
405.330563	8000.419770	14.325696	-0.080581	4.818343
405.496989	8000.484082	14.330701	-0.080613	4.818361
405.381588	8000.446759	14.335706	-0.080591	4.818351
405.456145	8000.470913	14.340711	-0.080605	4.818358
405.442651	8000.442344	14.345715	-0.080603	4.818349
405.456164	8000.437275	14.350720	-0.080605	4.818348
405.468066	8000.473188	14.355725	-0.080607	4.818358
405.365797	8000.486512	14.360730	-0.080588	4.818363
405.299863	8000.515053	14.365735	-0.080576	4.818371
405.300820	8000.511915	14.370739	-0.080576	4.818370
405.381381	8000.475170	14.375744	-0.080591	4.818359
405.386105	8000.503625	14.380749	-0.080592	4.818368
405.310866	8000.436361	14.385754	-0.080578	4.818348
405.213902	7999.367909	14.390759	-0.080560	4.818031

405.361921	7996.300344	14.395763	-0.080585	4.817119
405.297289	7990.747317	14.400768	-0.080570	4.815470
405.310382	7984.028188	14.405773	-0.080568	4.813473
405.330371	7976.753406	14.410778	-0.080567	4.811310
405.406580	7969.164662	14.415783	-0.080576	4.809053
405.214398	7961.408225	14.420787	-0.080535	4.806745
405.109972	7953.504684	14.425792	-0.080511	4.804393
404.996492	7945.635337	14.430797	-0.080484	4.802049
405.050326	7937.545699	14.435802	-0.080489	4.799638
405.020201	7929.603564	14.440807	-0.080479	4.797270
405.118320	7921.548653	14.445811	-0.080492	4.794866
404.932054	7913.606355	14.450816	-0.080452	4.792496
405.046022	7905.581592	14.455821	-0.080468	4.790100
404.922017	7897.545614	14.460826	-0.080440	4.787699
405.255134	7889.565732	14.465831	-0.080496	4.785313
405.031632	7881.603532	14.470835	-0.080450	4.782932
404.994097	7873.548266	14.475840	-0.080437	4.780522
404.849943	7865.632555	14.480845	-0.080406	4.778153
405.041274	7857.503342	14.485850	-0.080436	4.775717
405.011608	7849.542643	14.490855	-0.080425	4.773332
405.043738	7841.545950	14.495859	-0.080426	4.770934
405.130574	7833.518424	14.500864	-0.080437	4.768526
405.123439	7825.550200	14.505869	-0.080431	4.766134
404.955088	7817.504460	14.510874	-0.080394	4.763719
404.978589	7809.638108	14.515879	-0.080393	4.761355
404.879384	7801.545089	14.520883	-0.080370	4.758923
404.924836	7793.612149	14.525888	-0.080373	4.756537
404.983064	7785.561919	14.530893	-0.080379	4.754115
404.864096	7777.509129	14.535898	-0.080351	4.751691
404.880592	7769.428436	14.540903	-0.080349	4.749257
404.710304	7761.554457	14.545907	-0.080312	4.746885
404.684023	7753.435071	14.550912	-0.080302	4.744437
404.739129	7745.535720	14.555917	-0.080307	4.742054
404.712391	7737.479433	14.560922	-0.080297	4.739622
404.607282	7729.583854	14.565927	-0.080272	4.737238
404.604660	7721.486385	14.570931	-0.080267	4.734792
404.406478	7713.505380	14.575936	-0.080225	4.732380
404.349442	7705.460302	14.580941	-0.080209	4.729947
404.522230	7697.464174	14.585946	-0.080236	4.727527
404.637418	7689.457294	14.590951	-0.080252	4.725103
404.419315	7681.531850	14.595955	-0.080206	4.722703
404.528720	7673.478522	14.600960	-0.080222	4.720262
404.612173	7665.534179	14.605965	-0.080232	4.717853
404.523343	7657.508580	14.610970	-0.080210	4.715418
404.557515	7649.542305	14.615975	-0.080211	4.713000
404.562436	7641.520355	14.620979	-0.080207	4.710564
404.415538	7633.490536	14.625984	-0.080175	4.708125
404.377537	7625.508567	14.630989	-0.080162	4.705698
404.284271	7617.462765	14.635994	-0.080140	4.703251
404.363564	7609.554231	14.640999	-0.080149	4.700844
404.012527	7601.524984	14.646003	-0.080079	4.698400
404.085349	7593.511922	14.651008	-0.080087	4.695959
404.365277	7585.503756	14.656013	-0.080134	4.693518
404.172391	7577.514413	14.661018	-0.080093	4.691082
404.112220	7569.504158	14.666023	-0.080077	4.688638
404.182261	7561.499529	14.671027	-0.080085	4.686194
404.124450	7553.458838	14.676032	-0.080069	4.683739
403.844504	7545.597485	14.681037	-0.080011	4.681337
404.042512	7537.484201	14.686042	-0.080043	4.678856
403.744312	7529.598498	14.691047	-0.079982	4.676444
403.670757	7521.512476	14.696051	-0.079964	4.673969
403.424518	7513.474277	14.701056	-0.079912	4.671508
403.664507	7505.485038	14.706061	-0.079952	4.669060
403.573938	7497.454616	14.711066	-0.079930	4.666598
403.823681	7489.432983	14.716071	-0.079971	4.664138
403.568414	7481.511565	14.721075	-0.079919	4.661707
403.592370	7473.417758	14.726080	-0.079918	4.659222
403.646844	7465.512187	14.731085	-0.079923	4.656793
403.622436	7457.418762	14.736090	-0.079913	4.654305
403.550953	7449.504235	14.741095	-0.079895	4.651871
403.626009	7441.376824	14.746099	-0.079903	4.649371
403.790649	7433.418003	14.751104	-0.079929	4.646921
403.860248	7425.412682	14.756109	-0.079937	4.644455
403.570690	7417.513035	14.761114	-0.079878	4.642020
403.568095	7409.430203	14.766119	-0.079872	4.639528
403.728260	7401.507387	14.771123	-0.079897	4.637084
403.783839	7393.405783	14.776128	-0.079902	4.634583
403.679122	7385.502773	14.781133	-0.079877	4.632142
403.514199	7377.390937	14.786138	-0.079841	4.629636
403.884546	7369.417978	14.791143	-0.079905	4.627171
403.511346	7361.395993	14.796147	-0.079830	4.624689
403.253664	7353.438742	14.801152	-0.079777	4.622226
403.403159	7345.450677	14.806157	-0.079800	4.619753
403.427960	7337.429866	14.811162	-0.079799	4.617268
403.495657	7329.353859	14.816167	-0.079807	4.614764
403.262928	7321.453112	14.821171	-0.079758	4.612313
403.247090	7313.358894	14.826176	-0.079750	4.609801
403.288042	7305.416685	14.831181	-0.079753	4.607335
403.145227	7297.335674	14.836186	-0.079721	4.604824
403.357694	7289.447645	14.841191	-0.079755	4.602373
403.367853	7281.410959	14.846195	-0.079752	4.599873
403.285875	7273.426150	14.851200	-0.079732	4.597388
403.029641	7265.429377	14.856205	-0.079679	4.594898
402.990022	7257.362970	14.861210	-0.079666	4.592385
402.961666	7249.334997	14.866215	-0.079656	4.589883
402.988842	7241.339182	14.871219	-0.079655	4.587390
403.214384	7233.330733	14.876224	-0.079692	4.584891
403.042755	7225.405577	14.881229	-0.079655	4.582417
403.000907	7217.355195	14.886234	-0.079642	4.579902
402.790330	7209.435016	14.891239	-0.079598	4.577426
402.790127	7201.357322	14.896243	-0.079593	4.574900
402.436920	7193.371965	14.901248	-0.079522	4.572401
402.306449	7185.356865	14.906253	-0.079492	4.569891
402.595382	7177.313701	14.911258	-0.079541	4.567373
402.507375	7169.322124	14.916263	-0.079519	4.564868
402.679213	7161.350164	14.921267	-0.079546	4.562368
402.732660	7153.318665	14.926272	-0.079551	4.559849
402.749133	7145.394260	14.931277	-0.079549	4.557361
402.151139	7137.353430	14.936282	-0.079432	4.554834
402.661031	7129.317008	14.941287	-0.079522	4.552310
402.479561	7121.307004	14.946291	-0.079483	4.549790
402.722046	7113.255540	14.951296	-0.079523	4.547258
402.976196	7105.299598	14.956301	-0.079565	4.544754
402.540022	7097.365509	14.961306	-0.079479	4.542254
402.759265	7089.292794	14.966311	-0.079514	4.539710
402.570198	7081.372553	14.971315	-0.079474	4.537212
402.788181	7073.278073	14.976320	-0.079510	4.534659
402.748452	7065.340677	14.981325	-0.079497	4.532154
402.668700	7057.221297	14.986330	-0.079477	4.529589
402.575808	7049.345681	14.991335	-0.079455	4.527100
402.573907	7041.274182	14.996339	-0.079449	4.524547
402.349578	7033.353448	15.001344	-0.079402	4.522041
402.503224	7025.227374	15.006349	-0.079425	4.519469
402.576864	7017.309677	15.011354	-0.079434	4.516961
402.516828	7009.283496	15.016359	-0.079418	4.514418
402.408728	7001.306671	15.021363	-0.079392	4.511888
402.347111	6993.267961	15.026368	-0.079376	4.509337
402.322884	6985.272750	15.031373	-0.079366	4.506799
402.337679	6977.199087	15.036378	-0.079364	4.504234
402.268675	6969.272390	15.041383	-0.079346	4.501715
402.192170	6961.243267	15.046387	-0.079326	4.499162
402.170415	6953.260280	15.051392	-0.079317	4.496621
402.094745	6945.261874	15.056397	-0.079298	4.494075
402.229184	6937.256681	15.061402	-0.079318	4.491525
402.190126	6929.247348	15.066407	-0.079305	4.488973
402.126272	6921.248776	15.071411	-0.079288	4.486422
402.062409	6913.170666	15.076416	-0.079271	4.483844
402.088592	6905.278886	15.081421	-0.079271	4.481324
402.074375	6897.208385	15.086426	-0.079263	4.478746
402.311436	6889.231981	15.091431	-0.079302	4.476198
402.303906	6881.241852	15.096435	-0.079295	4.473642
402.068479	6873.258433	15.101440	-0.079246	4.471087
401.984175	6865.182059	15.106445	-0.079225	4.468500
401.907239	6857.186289	15.111450	-0.079206	4.465938
401.930374	6849.207353	15.116455	-0.079205	4.463381
401.842658	6841.237507	15.121459	-0.079184	4.460824
402.079417	6833.205289	15.126464	-0.079222	4.458248
402.133878	6825.191020	15.131469	-0.079227	4.455675
401.887261	6817.215996	15.136474	-0.079176	4.453111
401.934993	6809.178092	15.141479	-0.079180	4.450527
401.856453	6801.191422	15.146483	-0.079160	4.447958
401.886201	6793.149535	15.151488	-0.079161	4.445370
401.743563	6785.205180	15.156493	-0.079129	4.442811
401.817211	6777.180650	15.161498	-0.079137	4.440225
401.725923	6769.228296	15.166503	-0.079115	4.437661
401.715733	6761.174770	15.171507	-0.079108	4.435063
401.567053	6753.182414	15.176512	-0.079075	4.432482
401.301620	6745.201566	15.181517	-0.079021	4.429903
401.165026	6737.184666	15.186522	-0.078990	4.427311
401.120143	6729.155509	15.191527	-0.078977	4.424715
401.366931	6721.207066	15.196531	-0.079017	4.422145
401.552092	6713.126371	15.201536	-0.079047	4.419530
401.379811	6705.170419	15.206541	-0.079009	4.416951
401.199607	6697.135554	15.211546	-0.078971	4.414346
401.299045	6689.197650	15.216551	-0.078984	4.411772
401.305945	6681.134272	15.221555	-0.078980	4.409156
401.133452	6673.149173	15.226560	-0.078943	4.406562
401.215723	6665.116059	15.231565	-0.078953	4.403953
401.352406	6657.180744	15.236570	-0.078973	4.401374
401.275422	6649.123611	15.241575	-0.078954	4.398753
401.145471	6641.199881	15.246579	-0.078924	4.396173
401.324973	6633.096580	15.251584	-0.078953	4.393535
401.285401	6625.189161	15.256589	-0.078940	4.390958
401.202591	6617.135062	15.261594	-0.078919	4.388332
401.216600	6609.173814	15.266599	-0.078917	4.385734
401.043470	6601.168485	15.271603	-0.078880	4.383120
401.131876	6593.186554	15.276608	-0.078891	4.380514
401.380340	6585.178353	15.281613	-0.078932	4.377898
401.040053	6577.184238	15.286618	-0.078863	4.375281
401.101539	6569.228576	15.291623	-0.078870	4.372679
401.393282	6561.190774	15.296627	-0.078919	4.370049
401.195743	6553.228187	15.301632	-0.078877	4.367439
401.111713	6545.223248	15.306637	-0.078856	4.364814
401.236961	6537.224316	15.311642	-0.078874	4.362191
401.254883	6529.267697	15.316647	-0.078872	4.359580
401.185889	6521.293061	15.321651	-0.078854	4.356961
400.564061	6513.265335	15.326656	-0.078733	4.354318
400.800975	6505.233810	15.331661	-0.078772	4.351679
400.594563	6497.186799	15.336666	-0.078729	4.349030
400.712323	6489.223618	15.341671	-0.078746	4.346410
400.710675	6481.184584	15.346675	-0.078740	4.343762
400.766117	6473.234351	15.351680	-0.078745	4.341142
400.937335	6465.200061	15.356685	-0.078772	4.338493
400.718691	6457.227153	15.361690	-0.078726	4.335860
400.826441	6449.189941	15.366695	-0.078741	4.333207
400.767245	6441.230596	15.371699	-0.078725	4.330577
400.402815	6433.255216	15.376704	-0.078652	4.327937
400.716586	6425.166349	15.381709	-0.078705	4.325264
400.562004	6417.236302	15.386714	-0.078671	4.322638
400.397326	6409.211513	15.391719	-0.078635	4.319979
400.421009	6401.255760	15.396723	-0.078634	4.317342
400.498637	6393.179272	15.401728	-0.078644	4.314664
400.575343	6385.194329	15.406733	-0.078653	4.312015
400.325509	6377.172830	15.411738	-0.078601	4.309350
400.601102	6369.168182	15.416743	-0.078647	4.306693
400.594223	6361.119400	15.421747	-0.078641	4.304017
400.366685	6353.164926	15.426752	-0.078593	4.301369
400.309045	6345.187518	15.431757	-0.078577	4.298713
400.369950	6337.195984	15.436762	-0.078584	4.296052
400.477599	6329.187529	15.441767	-0.078598	4.293383
400.323491	6321.166756	15.446771	-0.078565	4.290707
400.340019	6313.144542	15.451776	-0.078562	4.288030
400.132600	6305.175539	15.456781	-0.078519	4.285368
399.909950	6297.194252	15.461786	-0.078472	4.282699
400.023581	6289.176018	15.466791	-0.078488	4.280019
400.258183	6281.198565	15.471795	-0.078527	4.277353
400.199533	6273.127973	15.476800	-0.078510	4.274651
400.149766	6265.214145	15.481805	-0.078496	4.272000
400.139467	6257.131857	15.486810	-0.078489	4.269291
400.067848	6249.143951	15.491815	-0.078470	4.266611
400.026125	6241.139775	15.496819	-0.078457	4.263925
399.958638	6233.221350	15.501824	-0.078440	4.261265
399.924677	6225.170378	15.506829	-0.078428	4.258559
399.684468	6217.198399	15.511834	-0.078378	4.255877
400.056892	6209.126137	15.516839	-0.078442	4.253165
400.007243	6201.141041	15.521843	-0.078428	4.250476
399.724343	6193.143036	15.526848	-0.078370	4.247779
399.880536	6185.120257	15.531853	-0.078394	4.245076
399.867968	6177.162273	15.536858	-0.078387	4.242392
399.778857	6169.111818	15.541863	-0.078365	4.239674
399.755341	6161.168046	15.546867	-0.078355	4.236991
399.580929	6153.132424	15.551872	-0.078318	4.234273
399.581121	6145.174105	15.556877	-0.078313	4.231582
399.687739	6137.130805	15.561882	-0.078327	4.228862
399.405207	6129.192536	15.566887	-0.078269	4.226171
399.814717	6121.123170	15.571891	-0.078341	4.223441
399.705158	6113.121530	15.576896	-0.078315	4.220727
399.618441	6105.165751	15.581901	-0.078294	4.218027
399.700019	6097.083692	15.586906	-0.078304	4.215285
399.710813	6089.135052	15.591911	-0.078300	4.212585
399.498460	6081.168537	15.596915	-0.078256	4.209875
399.533046	6073.099072	15.601920	-0.078257	4.207130
399.380938	6065.120847	15.606925	-0.078224	4.204413
399.206529	6057.174254	15.611930	-0.078186	4.201705
399.374117	6049.114219	15.616935	-0.078212	4.198960
399.649054	6041.139965	15.621939	-0.078258	4.196244
399.313762	6033.118344	15.626944	-0.078190	4.193503
399.058680	6025.099371	15.631949	-0.078138	4.190762
399.371575	6017.036084	15.636954	-0.078191	4.188010
399.242044	6009.074515	15.641959	-0.078161	4.185287
399.183090	6001.135804	15.646963	-0.078145	4.182570
399.268366	5993.119750	15.651968	-0.078156	4.179827
399.236819	5985.127616	15.656973	-0.078145	4.177088
399.104793	5977.077834	15.661978	-0.078115	4.174327
399.200566	5969.094489	15.666983	-0.078128	4.171590
399.142205	5961.090948	15.671987	-0.078112	4.168842
398.967970	5953.139584	15.676992	-0.078074	4.166108
399.141357	5945.121937	15.681997	-0.078101	4.163355
398.947345	5937.124690	15.687002	-0.078060	4.160602
398.985439	5929.123441	15.692007	-0.078062	4.157849
399.065219	5921.135922	15.697011	-0.078072	4.155099
398.998784	5913.133704	15.702016	-0.078054	4.152340
399.172623	5905.144215	15.707021	-0.078081	4.149587
399.028971	5897.130200	15.712026	-0.078049	4.146820
398.943757	5889.096817	15.717031	-0.078028	4.144045
398.919703	5881.209258	15.722035	-0.078019	4.141319
398.777430	5873.168015	15.727040	-0.077987	4.138536
398.429955	5865.236570	15.732045	-0.077917	4.135788
398.722629	5857.157161	15.737050	-0.077967	4.132994
398.480083	5849.134307	15.742055	-0.077916	4.130211
398.623885	5841.156047	15.747059	-0.077938	4.127447
398.899662	5833.046618	15.752064	-0.077984	4.124637
399.003402	5825.182153	15.757069	-0.077998	4.121908
398.769503	5817.121397	15.762074	-0.077949	4.119105
398.733745	5809.202060	15.767079	-0.077938	4.116351
398.648988	5801.165284	15.772083	-0.077917	4.113554
398.455727	5793.170611	15.777088	-0.077876	4.110768
398.504873	5785.155622	15.782093	-0.077879	4.107977
398.501908	5777.103397	15.787098	-0.077874	4.105170
398.389398	5769.189052	15.792103	-0.077848	4.102407
398.338112	5761.132767	15.797107	-0.077833	4.099594
398.362659	5753.139703	15.802112	-0.077832	4.096803
398.444970	5745.155074	15.807117	-0.077842	4.094013
398.188717	5737.171061	15.812122	-0.077790	4.091217
397.965746	5729.124373	15.817127	-0.077743	4.088397
398.140574	5721.129176	15.822131	-0.077770	4.085599
398.196569	5713.088258	15.827136	-0.077775	4.082781
398.174666	5705.147788	15.832141	-0.077766	4.079996
398.222722	5697.136898	15.837146	-0.077770	4.077185
398.562738	5689.087173	15.842151	-0.077828	4.074362
398.380936	5681.149435	15.847155	-0.077789	4.071570
398.304799	5673.112443	15.852160	-0.077770	4.068742
398.382166	5665.148089	15.857165	-0.077779	4.065940
398.225045	5657.142596	15.862170	-0.077745	4.063118
398.195501	5649.146954	15.867175	-0.077734	4.060299
398.235327	5641.152098	15.872179	-0.077736	4.057480
397.972951	5633.166262	15.877184	-0.077682	4.054658
398.055839	5625.136494	15.882189	-0.077692	4.051823
398.108968	5617.083607	15.887194	-0.077697	4.048977
398.301095	5609.130805	15.892199	-0.077728	4.046168
398.179797	5601.152418	15.897203	-0.077700	4.043342
398.026259	5593.163483	15.902208	-0.077666	4.040510
398.203775	5585.163613	15.907213	-0.077694	4.037677
398.090087	5577.151608	15.912218	-0.077668	4.034834
397.927214	5569.150169	15.917223	-0.077632	4.031991
397.889314	5561.079356	15.922227	-0.077620	4.029124
397.739207	5553.113380	15.927232	-0.077587	4.026290
397.668510	5545.153832	15.932237	-0.077569	4.023458
397.621282	5537.150621	15.937242	-0.077555	4.020608
397.837997	5529.141792	15.942247	-0.077590	4.017759
397.812296	5521.170821	15.947251	-0.077580	4.014918
397.568580	5513.175421	15.952256	-0.077529	4.012062
397.871498	5505.155879	15.957261	-0.077581	4.009204
397.496604	5497.176397	15.962266	-0.077506	4.006347
397.269799	5489.192294	15.967271	-0.077458	4.003490
397.358812	5481.231314	15.972275	-0.077470	4.000643
397.435244	5473.212055	15.977280	-0.077479	3.997774
397.273859	5465.227308	15.982285	-0.077444	3.994911
397.290797	5457.199766	15.987290	-0.077441	3.992033
397.433040	5449.158060	15.992295	-0.077463	3.989151
397.572163	5441.191808	15.997299	-0.077484	3.986293
397.440485	5433.177471	16.002304	-0.077454	3.983411
397.449528	5425.235054	16.007309	-0.077450	3.980556
397.631562	5417.179717	16.012314	-0.077479	3.977661
397.257071	5409.189574	16.017319	-0.077404	3.974777
397.380348	5401.199910	16.022323	-0.077422	3.971901
397.478166	5393.155796	16.027328	-0.077435	3.969002
397.200000	5385.242589	16.032333	-0.077378	3.966142
396.825861	5377.226784	16.037338	-0.077303	3.963240
397.108795	5369.191019	16.042343	-0.077351	3.960342
397.215966	5361.221639	16.047347	-0.077366	3.957462
397.118792	5353.162265	16.052352	-0.077342	3.954543
397.232051	5345.212837	16.057357	-0.077358	3.951666
397.088897	5337.153893	16.062362	-0.077326	3.948743
397.133436	5329.197240	16.067367	-0.077329	3.945858
396.944164	5321.200766	16.072371	-0.077289	3.942952
397.059638	5313.149923	16.077376	-0.077305	3.940030
397.202987	5305.226344	16.082381	-0.077327	3.937152
397.217227	5297.123878	16.087386	-0.077324	3.934205
397.329771	5289.176681	16.092391	-0.077340	3.931314
397.135642	5281.190477	16.097395	-0.077299	3.928401
397.009040	5273.193052	16.102400	-0.077270	3.925483
396.989622	5265.231067	16.107405	-0.077261	3.922577
396.875750	5257.249212	16.112410	-0.077235	3.919661
396.670149	5249.269673	16.117415	-0.077192	3.916741
396.498423	5241.252558	16.122419	-0.077154	3.913806
396.332746	5233.251447	16.127424	-0.077118	3.910875
396.387737	5225.242889	16.132429	-0.077123	3.907943
396.085112	5217.251886	16.137434	-0.077062	3.905008
396.302992	5209.216820	16.142439	-0.077097	3.902065
396.716793	5201.178821	16.147443	-0.077169	3.899123
396.589879	5193.233024	16.152448	-0.077140	3.896202
396.538677	5185.250066	16.157453	-0.077126	3.893266
396.449114	5177.224359	16.162458	-0.077104	3.890312
396.592690	5169.220810	16.167463	-0.077125	3.887368
396.527969	5161.238137	16.172467	-0.077108	3.884426
396.466310	5153.301158	16.177472	-0.077092	3.881498
396.275453	5145.330855	16.182477	-0.077051	3.878553
396.446397	5137.292458	16.187482	-0.077077	3.875588
396.148169	5129.212901	16.192487	-0.077017	3.872596
396.245964	5121.168140	16.197491	-0.077030	3.869622
396.171465	5113.172106	16.202496	-0.077011	3.866661
396.320381	5105.199949	16.207501	-0.077033	3.863711
396.212600	5097.244160	16.212506	-0.077008	3.860760
396.226917	5089.254758	16.217511	-0.077006	3.857796
396.116453	5081.279456	16.222515	-0.076980	3.854833
396.109283	5073.246475	16.227520	-0.076973	3.851848
396.297877	5065.240377	16.232525	-0.077003	3.848875
396.069112	5057.284570	16.237530	-0.076956	3.845909
395.747301	5049.311057	16.242535	-0.076890	3.842932
395.920967	5041.326004	16.247539	-0.076918	3.839960
395.831566	5033.276206	16.252544	-0.076896	3.836955
395.799397	5025.274559	16.257549	-0.076885	3.833968
395.998279	5017.270642	16.262554	-0.076916	3.830982
396.365362	5009.242129	16.267559	-0.076980	3.827988
396.141226	5001.288814	16.272563	-0.076933	3.825007
395.990657	4993.282445	16.277568	-0.076900	3.822006
395.972963	4985.292036	16.282573	-0.076891	3.819011
395.659691	4977.341325	16.287578	-0.076828	3.816022
395.800803	4969.300823	16.292583	-0.076849	3.813007
395.754014	4961.314445	16.297587	-0.076835	3.810006
395.764989	4953.262015	16.302592	-0.076832	3.806979
395.605016	4945.315055	16.307597	-0.076797	3.803985
395.421016	4937.346875	16.312602	-0.076757	3.800980
395.543677	4929.330848	16.317607	-0.076775	3.797962
395.414008	4921.356379	16.322611	-0.076746	3.794952
395.438004	4913.333434	16.327616	-0.076745	3.791924
395.604655	4905.294103	16.332621	-0.076771	3.788891
395.606427	4897.296047	16.337626	-0.076766	3.785867
395.302090	4889.315026	16.342631	-0.076704	3.782840
395.460922	4881.339062	16.347635	-0.076729	3.779824
395.505273	4873.308983	16.352640	-0.076732	3.776782
395.489212	4865.345898	16.357645	-0.076724	3.773761
395.387344	4857.355099	16.362650	-0.076699	3.770726
395.533632	4849.347840	16.367655	-0.076721	3.767687
395.445798	4841.351850	16.372659	-0.076700	3.764645
395.367848	4833.391270	16.377664	-0.076680	3.761615
395.287627	4825.435652	16.382669	-0.076660	3.758583
395.184514	4817.441271	16.387674	-0.076636	3.755534
395.298383	4809.384809	16.392679	-0.076652	3.752464
395.219401	4801.389716	16.397683	-0.076632	3.749410
394.758277	4793.413392	16.402688	-0.076541	3.746351
395.108636	4785.387598	16.407693	-0.076601	3.743291
395.195239	4777.396626	16.412698	-0.076612	3.740235
395.366687	4769.423783	16.417703	-0.076639	3.737186
395.140422	4761.390333	16.422707	-0.076591	3.734101
395.076467	4753.420599	16.427712	-0.076574	3.731042
395.200596	4745.411849	16.432717	-0.076592	3.727970
395.115816	4737.381890	16.437722	-0.076571	3.724883
394.861834	4729.482522	16.442727	-0.076519	3.721838
394.996845	4721.426316	16.447731	-0.076539	3.718741
395.023866	4713.437360	16.452736	-0.076539	3.715664
394.871308	4705.430468	16.457741	-0.076505	3.712574
394.747581	4697.375027	16.462746	-0.076477	3.709462
394.943018	4689.397290	16.467751	-0.076508	3.706386
394.879780	4681.394912	16.472755	-0.076491	3.703292
394.713975	4673.407736	16.477760	-0.076455	3.700198
394.861527	4665.465935	16.482765	-0.076477	3.697127
394.628385	4657.420993	16.487770	-0.076429	3.694004
394.625019	4649.446314	16.492775	-0.076423	3.690911
394.946615	4641.389590	16.497779	-0.076478	3.687793
394.904319	4633.392370	16.502784	-0.076465	3.684685
394.862697	4625.494183	16.507789	-0.076452	3.681613
394.539519	4617.491912	16.512794	-0.076386	3.678491
394.673010	4609.502976	16.517799	-0.076406	3.675383
394.584662	4601.519163	16.522803	-0.076385	3.672269
394.589775	4593.464535	16.527808	-0.076380	3.669127
394.555839	4585.511424	16.532813	-0.076369	3.666021
394.611651	4577.485388	16.537818	-0.076374	3.662886
394.326843	4569.538531	16.542823	-0.076316	3.659770
394.370886	4561.558931	16.547827	-0.076319	3.656648
394.291457	4553.511915	16.552832	-0.076299	3.653493
394.244194	4545.556386	16.557837	-0.076285	3.650373
394.172522	4537.538631	16.562842	-0.076266	3.647224
394.343698	4529.516299	16.567847	-0.076293	3.644078
394.100895	4521.626898	16.572851	-0.076243	3.640969
394.106440	4513.553866	16.577856	-0.076239	3.637793
394.198106	4505.561016	16.582861	-0.076251	3.634648
394.161204	4497.549365	16.587866	-0.076239	3.631489
394.047093	4489.568412	16.592871	-0.076212	3.628338
394.315940	4481.559928	16.597875	-0.076257	3.625183
393.957795	4473.608034	16.602880	-0.076185	3.622030
393.941398	4465.606290	16.607885	-0.076177	3.618865
393.867763	4457.603078	16.612890	-0.076158	3.615695
393.625027	4449.597106	16.617895	-0.076108	3.612516
393.917341	4441.583089	16.622899	-0.076157	3.609346
394.036014	4433.568962	16.627904	-0.076174	3.606168
394.095004	4425.577985	16.632909	-0.076180	3.602995
393.838756	4417.622571	16.637914	-0.076127	3.599825
393.835326	4409.651047	16.642919	-0.076121	3.596652
393.841195	4401.620072	16.647923	-0.076117	3.593453
393.659425	4393.621039	16.652928	-0.076078	3.590259
393.925470	4385.627402	16.657933	-0.076122	3.587077
393.777621	4377.607339	16.662938	-0.076090	3.583869
393.798495	4369.653033	16.667943	-0.076088	3.580690
393.900541	4361.666205	16.672947	-0.076102	3.577498
393.505504	4353.655789	16.677952	-0.076023	3.574278
393.844682	4345.650749	16.682957	-0.076081	3.571079
393.735489	4337.634272	16.687962	-0.076056	3.567860
393.782717	4329.650617	16.692967	-0.076060	3.564656
393.642407	4321.737188	16.697971	-0.076028	3.561471
393.292097	4313.739740	16.702976	-0.075958	3.558243
393.609717	4305.733939	16.707981	-0.076012	3.555029
393.597919	4297.668139	16.712986	-0.076004	3.551778
393.524321	4289.661634	16.717991	-0.075986	3.548546
393.298467	4281.690328	16.722995	-0.075938	3.545321
393.128534	4273.729822	16.728000	-0.075902	3.542099
393.096263	4265.727496	16.733005	-0.075890	3.538861
393.133017	4257.749551	16.738010	-0.075892	3.535632
393.440037	4249.703347	16.743015	-0.075944	3.532381
393.299645	4241.693649	16.748019	-0.075913	3.529128
393.265923	4233.731557	16.753024	-0.075901	3.525895
393.304346	4225.763500	16.758029	-0.075903	3.522658
393.131558	4217.765512	16.763034	-0.075866	3.519400
393.079728	4209.842215	16.768039	-0.075851	3.516172
393.382952	4201.735283	16.773043	-0.075902	3.512879
393.123235	4193.760370	16.778048	-0.075849	3.509618
393.249289	4185.785552	16.783053	-0.075867	3.506366
393.177281	4177.774144	16.788058	-0.075849	3.503090
393.161770	4169.788687	16.793063	-0.075841	3.499824
392.885661	4161.848898	16.798067	-0.075784	3.496564
392.884240	4153.812559	16.803072	-0.075779	3.493271
393.061907	4145.814418	16.808077	-0.075807	3.489997
393.000219	4137.810907	16.813082	-0.075790	3.486709
392.929053	4129.805864	16.818087	-0.075771	3.483417
393.107193	4121.874900	16.823091	-0.075799	3.480161
392.945036	4113.863458	16.828096	-0.075764	3.476857
392.925958	4105.879215	16.833101	-0.075755	3.473566
392.743824	4097.916493	16.838106	-0.075716	3.470276
392.785488	4089.860893	16.843111	-0.075719	3.466951
392.824633	4081.866064	16.848115	-0.075721	3.463648
392.777391	4073.867025	16.853120	-0.075707	3.460338
392.909466	4065.885898	16.858125	-0.075726	3.457037
392.675328	4057.923480	16.863130	-0.075678	3.453729
392.530400	4049.914854	16.868135	-0.075646	3.450402
392.681885	4041.927227	16.873139	-0.075669	3.447090
392.723887	4033.864645	16.878144	-0.075671	3.443740
392.534966	4025.992467	16.883149	-0.075631	3.440458
392.300638	4018.024506	16.888154	-0.075582	3.437132
392.423037	4009.971141	16.893159	-0.075600	3.433779
392.281624	4002.005865	16.898163	-0.075568	3.430450
392.224444	3993.964418	16.903168	-0.075552	3.427089
392.244220	3985.979689	16.908173	-0.075551	3.423751
392.154740	3978.042464	16.913178	-0.075529	3.420426
392.171207	3970.007273	16.918183	-0.075527	3.417061
392.037011	3962.038811	16.923187	-0.075497	3.413715
392.071078	3954.005307	16.928192	-0.075498	3.410344
392.136068	3946.006827	16.933197	-0.075505	3.406986
391.905129	3938.028671	16.938202	-0.075457	3.403622
392.074104	3930.036409	16.943207	-0.075483	3.400263
392.087509	3922.082983	16.948211	-0.075481	3.396912
392.087748	3914.051237	16.953216	-0.075475	3.393524
392.048131	3906.051617	16.958221	-0.075463	3.390145
391.797517	3898.073649	16.963226	-0.075411	3.386764
391.944749	3890.020921	16.968231	-0.075433	3.383362
391.774759	3882.091950	16.973235	-0.075396	3.379998
392.131890	3874.047456	16.978240	-0.075458	3.376600
391.749459	3866.102788	16.983245	-0.075381	3.373215
391.614349	3858.111057	16.988250	-0.075351	3.369815
391.548033	3850.120017	16.993255	-0.075334	3.366415
391.628683	3842.138221	16.998259	-0.075343	3.363020
391.812021	3834.121802	17.003264	-0.075372	3.359611
392.023101	3826.143202	17.008269	-0.075407	3.356216
391.718935	3818.195808	17.013274	-0.075345	3.352811
391.758017	3810.166619	17.018279	-0.075347	3.349381
391.540706	3802.217075	17.023283	-0.075301	3.345972
391.636454	3794.173079	17.028288	-0.075314	3.342531
391.723965	3786.199921	17.033293	-0.075325	3.339116
391.556584	3778.243650	17.038298	-0.075289	3.335695
391.585729	3770.254204	17.043303	-0.075289	3.332264
391.408602	3762.238364	17.048307	-0.075251	3.328810
391.074673	3754.261588	17.053312	-0.075183	3.325363
391.410669	3746.267404	17.058317	-0.075241	3.321931
391.370214	3738.268024	17.063322	-0.075228	3.318479
391.349574	3730.265820	17.068327	-0.075219	3.315023
391.573264	3722.277427	17.073331	-0.075256	3.311578
391.545940	3714.246320	17.078336	-0.075245	3.308102
391.523110	3706.263603	17.083341	-0.075236	3.304643
391.395935	3698.310220	17.088346	-0.075207	3.301189
391.574259	3690.296535	17.093351	-0.075235	3.297717
391.615666	3682.321607	17.098355	-0.075238	3.294254
391.316397	3674.352378	17.103360	-0.075177	3.290775
391.140553	3666.389053	17.108365	-0.075139	3.287300
391.340208	3658.313983	17.113370	-0.075171	3.283788
391.132611	3650.388481	17.118375	-0.075127	3.280321
391.058092	3642.450661	17.123379	-0.075108	3.276850
391.076823	3634.404967	17.128384	-0.075106	3.273332
391.283177	3626.399781	17.133389	-0.075140	3.269836
391.380840	3618.392464	17.138394	-0.075153	3.266331
391.204537	3610.433311	17.143399	-0.075115	3.262832
391.236093	3602.428671	17.148403	-0.075115	3.259317
391.062478	3594.487229	17.153408	-0.075078	3.255818
391.140258	3586.472131	17.158413	-0.075087	3.252294
391.177385	3578.485065	17.163418	-0.075089	3.248776
391.203507	3570.498470	17.168423	-0.075089	3.245254
391.209719	3562.526644	17.173427	-0.075085	3.241734
391.172878	3554.535056	17.178432	-0.075073	3.238199
391.110857	3546.574329	17.183437	-0.075056	3.234674
391.121918	3538.556960	17.188442	-0.075053	3.231122
390.828325	3530.582851	17.193447	-0.074993	3.227573
390.449656	3522.603941	17.198451	-0.074917	3.224014
390.408412	3514.597769	17.203456	-0.074905	3.220453
390.484337	3506.618772	17.208461	-0.074913	3.216906
390.164005	3498.626801	17.213466	-0.074849	3.213332
390.297266	3490.583745	17.218471	-0.074868	3.209750
390.471997	3482.593851	17.223475	-0.074896	3.206190
390.357458	3474.615375	17.228480	-0.074869	3.202619
389.937075	3466.712915	17.233485	-0.074786	3.199065
389.880319	3458.707804	17.238490	-0.074770	3.195476
390.124421	3450.658325	17.243495	-0.074810	3.191876
390.267006	3442.660984	17.248499	-0.074832	3.188292
390.076484	3434.654876	17.253504	-0.074791	3.184684
390.410152	3426.659726	17.258509	-0.074848	3.181101
390.429947	3418.684571	17.263514	-0.074847	3.177509
390.290512	3410.700748	17.268519	-0.074815	3.173902
390.048156	3402.773441	17.273523	-0.074765	3.170311
389.703161	3394.776939	17.278528	-0.074696	3.166681
390.177075	3386.742555	17.283533	-0.074779	3.163066
390.126392	3378.768676	17.288538	-0.074764	3.159450
390.248411	3370.793826	17.293543	-0.074782	3.155838
390.219323	3362.817536	17.298547	-0.074771	3.152215
390.321267	3354.755132	17.303552	-0.074785	3.148553
390.543053	3346.786837	17.308557	-0.074821	3.144936
390.390453	3338.836682	17.313562	-0.074788	3.141306
390.386709	3330.842699	17.318567	-0.074782	3.137659
390.323036	3322.874914	17.323571	-0.074765	3.134016
389.978677	3314.913742	17.328576	-0.074695	3.130360
390.155641	3306.884696	17.333581	-0.074723	3.126692
389.980419	3298.915930	17.338586	-0.074685	3.123031
390.182547	3290.905117	17.343591	-0.074718	3.119364
390.160833	3282.962811	17.348595	-0.074709	3.115714
390.041911	3274.949412	17.353600	-0.074681	3.112022
389.988524	3266.976905	17.358605	-0.074666	3.108348
389.863397	3259.006902	17.363610	-0.074638	3.104667
390.011609	3251.018710	17.368615	-0.074660	3.100986
389.864920	3243.034101	17.373619	-0.074628	3.097289
389.989837	3235.009891	17.378624	-0.074646	3.093581
389.630133	3227.099192	17.383629	-0.074574	3.089899
389.699664	3219.075568	17.388634	-0.074582	3.086180
389.758376	3211.059330	17.393639	-0.074587	3.082460
389.799615	3203.117607	17.398643	-0.074590	3.078769
389.682922	3195.133250	17.403648	-0.074563	3.075047
389.636006	3187.115966	17.408653	-0.074549	3.071308
389.530694	3179.098446	17.413658	-0.074524	3.067561
389.436035	3171.106371	17.418663	-0.074501	3.063822
389.358320	3163.168368	17.423667	-0.074482	3.060105
389.407950	3155.149578	17.428672	-0.074486	3.056351
389.558584	3147.150748	17.433677	-0.074509	3.052607
389.508727	3139.172553	17.438682	-0.074494	3.048859
389.434833	3131.206040	17.443687	-0.074475	3.045110
389.713455	3123.219184	17.448691	-0.074522	3.041364
389.519301	3115.247807	17.453696	-0.074481	3.037597
389.297091	3107.290682	17.458701	-0.074434	3.033832
389.362445	3099.292878	17.463706	-0.074441	3.030056
389.520183	3091.277480	17.468711	-0.074466	3.026272
389.409281	3083.337894	17.473715	-0.074440	3.022506
389.030711	3075.390480	17.478720	-0.074364	3.018718
389.246378	3067.389050	17.483725	-0.074399	3.014930
389.157990	3059.401578	17.488730	-0.074378	3.011128
388.920029	3051.408666	17.493735	-0.074328	3.007311
388.855872	3043.452047	17.498739	-0.074311	3.003515
388.811630	3035.449138	17.503744	-0.074298	2.999694
388.920123	3027.461690	17.508749	-0.074313	2.995882
388.870586	3019.474520	17.513754	-0.074298	2.992058
388.902307	3011.460226	17.518759	-0.074299	2.988220
388.664486	3003.531978	17.523763	-0.074250	2.984405
388.608261	2995.517166	17.528768	-0.074234	2.980552
388.603439	2987.561701	17.533773	-0.074228	2.976726
388.555573	2979.553735	17.538778	-0.074214	2.972867
388.458717	2971.530431	17.543783	-0.074191	2.968993
388.597055	2963.563902	17.548787	-0.074211	2.965154
388.544113	2955.591590	17.553792	-0.074196	2.961297
388.575935	2947.615967	17.558797	-0.074197	2.957438
388.527065	2939.640215	17.563802	-0.074183	2.953570
388.701738	2931.614553	17.568807	-0.074210	2.949684
388.661708	2923.665853	17.573811	-0.074197	2.945819
388.555045	2915.712462	17.578816	-0.074172	2.941943
388.661153	2907.725145	17.583821	-0.074187	2.938056
388.746654	2899.719911	17.588826	-0.074198	2.934155
388.621871	2891.741397	17.593831	-0.074169	2.930250
388.515500	2883.802167	17.598835	-0.074144	2.926361
388.426482	2875.792659	17.603840	-0.074123	2.922432
388.429080	2867.835351	17.608845	-0.074118	2.918529
388.299835	2859.859472	17.613850	-0.074089	2.914605
388.074187	2851.844215	17.618855	-0.074042	2.910650
388.241386	2843.835554	17.623859	-0.074068	2.906715
388.151123	2835.844826	17.628864	-0.074046	2.902769
388.282217	2827.889583	17.633869	-0.074065	2.898847
388.169564	2819.911089	17.638874	-0.074039	2.894895
388.219101	2811.911527	17.643879	-0.074043	2.890937
388.252026	2803.942376	17.648883	-0.074044	2.886987
388.098125	2795.952332	17.653888	-0.074010	2.883011
388.249531	2788.002395	17.658893	-0.074033	2.879066
387.764729	2780.099298	17.663898	-0.073938	2.875103
387.656066	2772.096046	17.668903	-0.073912	2.871107
387.728877	2764.108456	17.673907	-0.073921	2.867122
387.007975	2756.190695	17.678912	-0.073781	2.863122
387.608248	2748.087660	17.683917	-0.073888	2.859099
387.786690	2740.092830	17.688922	-0.073916	2.855100
387.831144	2732.100756	17.693927	-0.073919	2.851090
387.643153	2724.172487	17.698931	-0.073879	2.847093
387.567061	2716.204871	17.703936	-0.073859	2.843076
387.685751	2708.230583	17.708941	-0.073876	2.839062
387.541875	2700.288355	17.713946	-0.073844	2.835043
387.363537	2692.296650	17.718951	-0.073806	2.830991
387.257359	2684.346989	17.723955	-0.073781	2.826959
387.347024	2676.296955	17.728960	-0.073793	2.822882
387.303505	2668.334691	17.733965	-0.073779	2.818835
387.369196	2660.345491	17.738970	-0.073787	2.814776
387.095647	2652.392993	17.743975	-0.073730	2.810709
386.965284	2644.422084	17.748979	-0.073701	2.806635
387.114450	2636.415668	17.753984	-0.073724	2.802554
387.151997	2628.450903	17.758989	-0.073725	2.798482
387.186803	2620.468190	17.763994	-0.073727	2.794394
387.238787	2612.480538	17.768999	-0.073731	2.790299
387.534785	2604.462065	17.774003	-0.073781	2.786197
387.121835	2596.539539	17.779008	-0.073699	2.782095
387.011890	2588.595776	17.784013	-0.073674	2.777995
386.906945	2580.645683	17.789018	-0.073649	2.773885
387.064482	2572.575720	17.794023	-0.073673	2.769724
387.111193	2564.627293	17.799027	-0.073677	2.765612
387.018820	2556.678211	17.804032	-0.073654	2.761485
386.992023	2548.728492	17.809037	-0.073644	2.757356
387.086913	2540.720472	17.814042	-0.073657	2.753198
386.811466	2532.718752	17.819047	-0.073600	2.749014
386.974474	2524.717292	17.824051	-0.073625	2.744851
386.784812	2516.772282	17.829056	-0.073585	2.740689
386.772706	2508.817066	17.834061	-0.073578	2.736526
386.745079	2500.835326	17.839066	-0.073567	2.732342
386.825046	2492.816682	17.844071	-0.073577	2.728140
386.820830	2484.852492	17.849075	-0.073571	2.723954
386.791257	2476.910110	17.854080	-0.073560	2.719771
386.754570	2468.949453	17.859085	-0.073548	2.715572
386.748354	2460.965553	17.864090	-0.073542	2.711356
386.578652	2452.999053	17.869095	-0.073505	2.707132
386.488088	2445.064375	17.874099	-0.073483	2.702924
386.141928	2437.101305	17.879104	-0.073414	2.698677
386.567035	2429.074471	17.884109	-0.073488	2.694440
386.368568	2421.115232	17.889114	-0.073446	2.690191
386.351221	2413.122651	17.894119	-0.073437	2.685930
386.441725	2405.177536	17.899123	-0.073449	2.681694
386.185316	2397.230659	17.904128	-0.073396	2.677429
386.121595	2389.276539	17.909133	-0.073379	2.673164
386.379436	2381.224249	17.914138	-0.073422	2.668862
386.040572	2373.272466	17.919143	-0.073354	2.664567
386.131636	2365.309305	17.924147	-0.073365	2.660288
386.267756	2357.303010	17.929152	-0.073386	2.655982
386.170995	2349.349860	17.934157	-0.073362	2.651681
385.964957	2341.390555	17.939162	-0.073319	2.647363
385.947740	2333.413533	17.944167	-0.073311	2.643042
385.880297	2325.482517	17.949171	-0.073293	2.638734
386.017419	2317.474265	17.954176	-0.073313	2.634391
385.997177	2309.515576	17.959181	-0.073304	2.630058
385.991205	2301.529333	17.964186	-0.073298	2.625703
385.852095	2293.587483	17.969191	-0.073267	2.621356
386.000813	2285.611865	17.974195	-0.073290	2.617004
385.944069	2277.617878	17.979200	-0.073274	2.612619
385.742470	2269.677627	17.984205	-0.073231	2.608247
385.852732	2261.686195	17.989210	-0.073247	2.603861
385.756278	2253.750527	17.994215	-0.073223	2.599484
385.859622	2245.804296	17.999219	-0.073238	2.595108
385.664670	2237.709125	18.004224	-0.073196	2.590621
385.847743	2229.701020	18.009229	-0.073225	2.586201
385.773881	2221.770157	18.014234	-0.073206	2.581798
385.777993	2213.806778	18.019239	-0.073202	2.577375
385.685129	2205.885882	18.024243	-0.073179	2.572961
385.542317	2197.908851	18.029248	-0.073148	2.568505
385.639551	2189.911897	18.034253	-0.073160	2.564047
385.512812	2182.013334	18.039258	-0.073132	2.559620
385.648838	2174.011233	18.044263	-0.073152	2.555147
385.534359	2166.083093	18.049267	-0.073125	2.550689
385.443515	2158.093735	18.054272	-0.073103	2.546190
385.658484	2150.112074	18.059277	-0.073138	2.541710
385.503643	2142.188440	18.064282	-0.073104	2.537228
385.402362	2134.217111	18.069287	-0.073080	2.532715
385.458699	2126.243084	18.074291	-0.073086	2.528204
385.334074	2118.279608	18.079296	-0.073057	2.523678
385.184597	2110.358121	18.084301	-0.073024	2.519165
385.318709	2102.363878	18.089306	-0.073044	2.514624
385.454090	2094.381361	18.094311	-0.073064	2.510081
385.229789	2086.430320	18.099315	-0.073017	2.505522
385.251940	2078.440387	18.104320	-0.073016	2.500950
385.167878	2070.512023	18.109325	-0.072995	2.496397
385.148433	2062.527866	18.114330	-0.072987	2.491808
385.121621	2054.560194	18.119335	-0.072977	2.487220
384.938670	2046.651410	18.124339	-0.072937	2.482646
384.720301	2038.697149	18.129344	-0.072892	2.478035
384.559421	2030.754880	18.134349	-0.072856	2.473426
384.737562	2022.741380	18.139354	-0.072884	2.468792
384.691946	2014.749093	18.144359	-0.072871	2.464146
384.893988	2006.793196	18.149363	-0.072903	2.459531
384.716841	1998.835433	18.154368	-0.072865	2.454876
384.498709	1990.918289	18.159373	-0.072819	2.450234
384.699783	1982.901779	18.164378	-0.072852	2.445557
384.517047	1974.976486	18.169383	-0.072813	2.440895
384.549096	1967.033221	18.174387	-0.072813	2.436230
384.554021	1959.024769	18.179392	-0.072809	2.431515
384.492180	1951.050224	18.184397	-0.072792	2.426806
383.847029	1943.181443	18.189402	-0.072667	2.422105
384.142908	1935.152167	18.194407	-0.072717	2.417373
384.199011	1927.207456	18.199411	-0.072722	2.412664
384.278121	1919.186740	18.204416	-0.072732	2.407901
384.180809	1911.264075	18.209421	-0.072709	2.403174
384.174485	1903.318473	18.214426	-0.072702	2.398431
383.801655	1895.422894	18.219431	-0.072628	2.393680
384.230006	1887.397061	18.224435	-0.072702	2.388905
384.071304	1879.423904	18.229440	-0.072668	2.384104
384.062640	1871.495668	18.234445	-0.072661	2.379334
384.045475	1863.541278	18.239450	-0.072653	2.374537
383.869392	1855.593977	18.244455	-0.072615	2.369722
384.018491	1847.621763	18.249459	-0.072637	2.364908
383.858417	1839.681346	18.254464	-0.072602	2.360079
383.924019	1831.739992	18.259469	-0.072610	2.355257
383.904262	1823.770117	18.264474	-0.072601	2.350402
383.691901	1815.828362	18.269479	-0.072556	2.345537
383.647459	1807.890017	18.274483	-0.072543	2.340679
383.718487	1799.910429	18.279488	-0.072551	2.335794
383.531591	1791.991104	18.284493	-0.072511	2.330915
383.663083	1784.004358	18.289498	-0.072530	2.326011
383.725338	1776.016285	18.294503	-0.072537	2.321090
383.534545	1768.147448	18.299507	-0.072496	2.316210
383.559644	1760.146296	18.304512	-0.072495	2.311257
383.463805	1752.206799	18.309517	-0.072472	2.306321
383.719874	1744.219053	18.314522	-0.072515	2.301374
383.513538	1736.292352	18.319527	-0.072471	2.296415
383.591814	1728.337823	18.324531	-0.072481	2.291453
383.091663	1720.433941	18.329536	-0.072383	2.286461
383.343898	1712.456293	18.334541	-0.072424	2.281478
383.463107	1704.490794	18.339546	-0.072441	2.276480
383.470961	1696.521550	18.344551	-0.072438	2.271458
383.406235	1688.555075	18.349555	-0.072421	2.266421
383.325283	1680.614023	18.354560	-0.072400	2.261387
383.414568	1672.665215	18.359565	-0.072412	2.256352
383.334639	1664.730991	18.364570	-0.072392	2.251300
383.111833	1656.801825	18.369575	-0.072345	2.246228
382.953656	1648.903382	18.374579	-0.072311	2.241169
382.893622	1640.936269	18.379584	-0.072294	2.236063
383.247330	1632.934343	18.384589	-0.072355	2.230961
382.904030	1625.022351	18.389594	-0.072286	2.225842
382.895486	1617.082344	18.394599	-0.072279	2.220723
382.861492	1609.160606	18.399603	-0.072268	2.215602
382.848273	1601.171428	18.404608	-0.072260	2.210427
382.470825	1593.300285	18.409613	-0.072185	2.205284
383.074646	1585.246430	18.414618	-0.072292	2.200099
382.867584	1577.362725	18.419623	-0.072248	2.194939
382.869839	1569.413573	18.424627	-0.072244	2.189743
382.718598	1561.464416	18.429632	-0.072210	2.184520
382.895766	1553.511793	18.434637	-0.072238	2.179314
382.831224	1545.582668	18.439642	-0.072221	2.174087
382.766784	1537.631990	18.444647	-0.072204	2.168834
382.727948	1529.708726	18.449651	-0.072192	2.163589
382.670632	1521.781237	18.454656	-0.072176	2.158326
382.475076	1513.880736	18.459661	-0.072134	2.153055
382.564828	1505.903527	18.464666	-0.072146	2.147747
382.430570	1497.967427	18.469671	-0.072116	2.142432
382.393326	1490.061110	18.474675	-0.072104	2.137134
382.525371	1482.081037	18.479680	-0.072123	2.131788
382.441875	1474.163095	18.484685	-0.072102	2.126451
382.100910	1466.287738	18.489690	-0.072034	2.121103
382.022590	1458.350444	18.494695	-0.072014	2.115726
382.489705	1450.312477	18.499699	-0.072096	2.110320
381.916847	1442.447956	18.504704	-0.071984	2.104916
381.631590	1434.554474	18.509709	-0.071926	2.099506
381.573163	1426.614995	18.514714	-0.071910	2.094074
381.690714	1418.621815	18.519719	-0.071927	2.088608
381.658194	1410.698116	18.524723	-0.071916	2.083161
381.388606	1402.811449	18.529728	-0.071860	2.077701
381.505344	1394.856005	18.534733	-0.071877	2.072218
381.704179	1386.857929	18.539738	-0.071909	2.066699
381.766960	1378.929282	18.544743	-0.071915	2.061200
381.810150	1370.998849	18.549747	-0.071918	2.055683
381.493259	1363.124064	18.554752	-0.071854	2.050153
381.207482	1355.236994	18.559757	-0.071796	2.044602
381.713196	1347.226642	18.564762	-0.071885	2.039032
381.577769	1339.325319	18.569767	-0.071854	2.033457
381.458665	1331.415945	18.574771	-0.071827	2.027862
381.439752	1323.474431	18.579776	-0.071819	2.022240
381.402067	1315.566779	18.584781	-0.071806	2.016624
381.347890	1307.633010	18.589786	-0.071791	2.010972
381.421506	1299.669812	18.594791	-0.071800	2.005296
381.463202	1291.777162	18.599795	-0.071802	1.999652
381.180388	1283.904256	18.604800	-0.071745	1.993971
381.132523	1275.986027	18.609805	-0.071731	1.988266
380.913944	1268.099187	18.614810	-0.071685	1.982549
381.016658	1260.145858	18.619815	-0.071699	1.976802
381.341917	1252.158178	18.624819	-0.071754	1.971038
381.042986	1244.271738	18.629824	-0.071693	1.965263
381.294858	1236.345433	18.634829	-0.071735	1.959501
381.289896	1228.452293	18.639834	-0.071729	1.953719
381.010602	1220.562041	18.644839	-0.071672	1.947891
381.085354	1212.626177	18.649843	-0.071681	1.942052
381.104380	1204.683271	18.654848	-0.071679	1.936183
380.945664	1196.789148	18.659853	-0.071645	1.930313
380.972671	1188.856671	18.664858	-0.071645	1.924417
380.966358	1180.975225	18.669863	-0.071638	1.918538
381.120871	1173.035612	18.674867	-0.071662	1.912615
380.931456	1165.132361	18.679872	-0.071622	1.906662
381.148429	1157.199382	18.684877	-0.071657	1.900714
381.059942	1149.315224	18.689882	-0.071635	1.894749
380.646834	1141.467557	18.694887	-0.071553	1.888756
380.949128	1133.514006	18.699891	-0.071604	1.882746
380.815046	1125.625042	18.704896	-0.071574	1.876715
380.989707	1117.692483	18.709901	-0.071602	1.870668
380.788197	1109.801779	18.714906	-0.071559	1.864589
380.678764	1101.921410	18.719911	-0.071534	1.858508
380.795270	1094.009797	18.724915	-0.071550	1.852411
380.541333	1086.112678	18.729920	-0.071498	1.846260
380.644474	1078.209739	18.734925	-0.071512	1.840127
380.491887	1070.353455	18.739930	-0.071478	1.833979
380.185713	1062.478036	18.744935	-0.071416	1.827777
380.413052	1054.539808	18.749939	-0.071454	1.821569
380.255934	1046.653071	18.754944	-0.071419	1.815334
380.193856	1038.768565	18.759949	-0.071403	1.809090
380.205426	1030.867864	18.764954	-0.071400	1.802821
380.229882	1022.983001	18.769959	-0.071399	1.796544
380.172980	1015.064378	18.774963	-0.071383	1.790209
379.851785	1007.199003	18.779968	-0.071318	1.783860
379.941933	999.303193	18.784973	-0.071330	1.777516
379.952888	991.398418	18.789978	-0.071327	1.771132
379.625881	983.554513	18.794983	-0.071261	1.764731
379.639722	975.678541	18.799987	-0.071259	1.758324
379.884619	967.731491	18.804992	-0.071299	1.751865
379.677070	959.881937	18.809997	-0.071255	1.745405
379.586155	952.017907	18.815002	-0.071233	1.738923
379.699725	944.114300	18.820007	-0.071249	1.732411
379.676816	936.236351	18.825011	-0.071240	1.725877
379.438647	928.400211	18.830016	-0.071191	1.719326
379.509232	920.517056	18.835021	-0.071199	1.712751
379.663371	912.594550	18.840026	-0.071222	1.706128
379.494099	904.752072	18.845031	-0.071186	1.699504
379.429884	896.901708	18.850035	-0.071169	1.692862
379.276908	889.036734	18.855040	-0.071135	1.686168
379.358565	881.164014	18.860045	-0.071145	1.679474
379.275079	873.318178	18.865050	-0.071125	1.672753
378.953590	865.484428	18.870055	-0.071060	1.665983
378.930311	857.630230	18.875059	-0.071050	1.659208
379.057359	849.723093	18.880064	-0.071069	1.652381
379.147292	841.836266	18.885069	-0.071080	1.645537
379.332037	833.971748	18.890074	-0.071110	1.638698
379.107364	826.141882	18.895079	-0.071063	1.631803
378.961320	818.279945	18.900083	-0.071031	1.624862
378.785963	810.454452	18.905088	-0.070993	1.617919
378.742022	802.597701	18.910093	-0.070980	1.610937
378.500173	794.787246	18.915098	-0.070930	1.603938
378.454858	786.941173	18.920103	-0.070916	1.596904
378.541856	779.076979	18.925107	-0.070927	1.589842
378.314035	771.248374	18.930112	-0.070880	1.582734
378.445892	763.382069	18.935117	-0.070899	1.575613
378.575735	755.514701	18.940122	-0.070918	1.568459
378.522235	747.679541	18.945127	-0.070903	1.561274
378.641079	739.855698	18.950131	-0.070920	1.554092
378.512401	732.032347	18.955136	-0.070891	1.546840
378.436942	724.213290	18.960141	-0.070872	1.539565
378.471021	716.385998	18.965146	-0.070873	1.532265
378.280731	708.560520	18.970151	-0.070833	1.524898
378.413152	700.749946	18.975155	-0.070853	1.517558
378.136668	692.955029	18.980160	-0.070796	1.510135
378.115075	685.142774	18.985165	-0.070787	1.502698
378.052330	677.336617	18.990170	-0.070770	1.495223
378.045176	669.508521	18.995175	-0.070764	1.487698
377.681430	661.771979	19.000179	-0.070691	1.480167
377.827060	653.922552	19.005184	-0.070713	1.472569
377.771222	646.089046	19.010189	-0.070698	1.464914
377.824287	638.278995	19.015194	-0.070703	1.457260
377.441201	630.529261	19.020199	-0.070626	1.449555
377.710196	622.688098	19.025203	-0.070671	1.441824
377.592683	614.923169	19.030208	-0.070644	1.434063
377.545720	607.136299	19.035213	-0.070631	1.426251
377.636206	599.330980	19.040218	-0.070642	1.418399
377.610571	591.543341	19.045223	-0.070633	1.410502
377.428138	583.808436	19.050227	-0.070594	1.402588
377.297486	576.054786	19.055232	-0.070564	1.394619
377.194351	568.283699	19.060237	-0.070540	1.386590
377.229257	560.504622	19.065242	-0.070541	1.378531
377.225298	552.721820	19.070247	-0.070536	1.370413
377.144473	544.991298	19.075251	-0.070516	1.362288
376.957957	537.255361	19.080256	-0.070476	1.354090
376.904069	529.500681	19.085261	-0.070461	1.345846
377.067555	521.736954	19.090266	-0.070486	1.337580
376.721773	514.032873	19.095271	-0.070417	1.329235
376.822819	506.279311	19.100275	-0.070431	1.320865
376.707078	498.531830	19.105280	-0.070404	1.312409
376.981682	490.690204	19.110285	-0.070450	1.303866
376.761814	483.007106	19.115290	-0.070404	1.295350
376.609459	475.308802	19.120295	-0.070371	1.286774
376.654928	467.595651	19.125299	-0.070375	1.278160
376.381843	459.929921	19.130304	-0.070319	1.269481
376.343077	452.226224	19.135309	-0.070307	1.260744
376.042679	444.579324	19.140314	-0.070246	1.251961
376.145328	436.846929	19.145319	-0.070260	1.243095
376.126830	429.175976	19.150323	-0.070251	1.234213
375.859330	421.516033	19.155328	-0.070197	1.225231
375.790808	413.848329	19.160333	-0.070179	1.216212
375.646315	406.187100	19.165338	-0.070147	1.207118
375.690332	398.506885	19.170343	-0.070150	1.197971
375.815394	390.830360	19.175347	-0.070169	1.188775
375.776434	383.174656	19.180352	-0.070156	1.179499
375.680000	375.555061	19.185357	-0.070134	1.170181
375.662326	367.925656	19.190362	-0.070125	1.160792
375.330513	360.347126	19.195367	-0.070059	1.151324
375.358456	352.693605	19.200371	-0.070059	1.141760
375.010521	345.132975	19.205376	-0.069989	1.132151
374.855496	337.546407	19.210381	-0.069955	1.122469
374.877095	329.938930	19.215386	-0.069955	1.112715
375.027351	322.309910	19.220391	-0.069978	1.102875
374.771500	314.787514	19.225395	-0.069925	1.092995
374.626157	307.226736	19.230400	-0.069893	1.082999
374.632031	299.665836	19.235405	-0.069889	1.072945
374.393059	292.141544	19.240410	-0.069840	1.062787
374.254153	284.620353	19.245415	-0.069809	1.052560
374.134833	277.109664	19.250419	-0.069782	1.042251
373.904978	269.622730	19.255424	-0.069735	1.031845
373.996491	262.092704	19.260429	-0.069747	1.021351
373.982724	254.604502	19.265434	-0.069739	1.010782
373.770545	247.149819	19.270439	-0.069695	1.000099
373.853527	239.654288	19.275443	-0.069706	0.989316
373.996994	232.153750	19.280448	-0.069728	0.978423
373.602781	224.783572	19.285453	-0.069649	0.967461
373.309891	217.409253	19.290458	-0.069590	0.956393
373.439394	209.960801	19.295463	-0.069609	0.945196
373.439046	202.575936	19.300467	-0.069605	0.933927
373.274769	195.215127	19.305472	-0.069569	0.922513
373.239118	187.871596	19.310477	-0.069558	0.911018
373.223865	180.523379	19.315482	-0.069550	0.899375
372.991595	173.232457	19.320487	-0.069502	0.887610
372.873616	165.959882	19.325491	-0.069476	0.875750
372.823719	158.682150	19.330496	-0.069462	0.863738
372.722737	151.448483	19.335501	-0.069438	0.851616
372.280284	144.290358	19.340506	-0.069351	0.839345
372.296120	137.049559	19.345511	-0.069349	0.826888
372.038205	129.907246	19.350515	-0.069297	0.814329
371.566930	122.810308	19.355520	-0.069204	0.801587
370.908752	115.789233	19.360525	-0.069077	0.788716
370.536075	108.733196	19.365530	-0.069003	0.775660
369.371423	101.841393	19.370535	-0.068782	0.762425
368.961744	94.840751	19.375539	-0.068701	0.749004
368.295850	87.905739	19.380544	-0.068573	0.735377
367.622582	81.011908	19.385549	-0.068443	0.721571
366.916017	74.342274	19.390554	-0.068307	0.707937