Fri Apr 16 19:10:53 2021

Number of Points = 3637
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.280097	0.034360	0.000000	-0.000023	0.312008

1.547456	-0.062832	0.005005	-0.000073	0.311783
1.490352	-0.067501	0.010010	-0.000062	0.311713
1.495577	-0.067247	0.015014	-0.000063	0.311719
1.515053	-0.070810	0.020019	-0.000067	0.311719
1.599660	-0.087795	0.025024	-0.000083	0.311711
1.610277	-0.088209	0.030029	-0.000085	0.311719
1.435758	-0.058924	0.035034	-0.000052	0.311708
1.489453	-0.067498	0.040038	-0.000062	0.311713
1.633343	-0.094437	0.045043	-0.000089	0.311710
1.579866	-0.085629	0.050048	-0.000079	0.311706
1.633721	-0.092814	0.055053	-0.000089	0.311718
1.562319	-0.082566	0.060058	-0.000076	0.311705
1.618752	-0.148796	0.065062	-0.000086	0.311446
1.697790	-0.176852	0.070067	-0.000101	0.311382
1.532220	-0.148039	0.075072	-0.000070	0.311377
1.362819	-0.114012	0.080077	-0.000039	0.311392
1.436111	-0.130145	0.085082	-0.000053	0.311379
1.516700	-0.144432	0.090086	-0.000068	0.311381
1.619280	-0.191788	0.095091	-0.000087	0.311247
1.282900	-0.167853	0.100096	-0.000024	0.311075
1.230643	-0.155673	0.105101	-0.000014	0.311087
1.499934	-0.207949	0.110106	-0.000065	0.311072
1.412632	-0.190871	0.115110	-0.000048	0.311078
1.307800	-0.189431	0.120115	-0.000029	0.310996
1.117028	-0.204092	0.125120	0.000007	0.310767
1.192128	-0.216500	0.130125	-0.000007	0.310773
1.494618	-0.274113	0.135130	-0.000064	0.310760
1.258988	-0.228872	0.140134	-0.000020	0.310772
1.437396	-0.309130	0.145139	-0.000053	0.310549
1.376832	-0.307524	0.150144	-0.000042	0.310506
1.766151	-0.376815	0.155149	-0.000114	0.310513
1.384910	-0.323973	0.160154	-0.000043	0.310436
1.511029	-0.404888	0.165158	-0.000067	0.310166
1.545154	-0.411397	0.170163	-0.000073	0.310165
1.294065	-0.365598	0.175168	-0.000027	0.310166
1.106141	-0.387591	0.180173	0.000008	0.309904
0.956287	-0.371360	0.185178	0.000036	0.309853
1.145901	-0.404615	0.190182	0.000001	0.309859
1.264207	-0.464909	0.195187	-0.000021	0.309678
1.199964	-0.488461	0.200192	-0.000009	0.309513
1.462116	-0.535089	0.205197	-0.000058	0.309518
1.220452	-0.532446	0.210202	-0.000013	0.309325
1.372968	-0.580408	0.215206	-0.000041	0.309231
1.481802	-0.599384	0.220211	-0.000062	0.309235
1.376137	-0.650017	0.225216	-0.000042	0.308908
1.295709	-0.637424	0.230221	-0.000027	0.308899
1.306183	-0.664427	0.235226	-0.000029	0.308781
1.284732	-0.701863	0.240230	-0.000025	0.308588
1.233787	-0.692477	0.245235	-0.000016	0.308588
1.277462	-0.764651	0.250240	-0.000024	0.308287
1.506396	-0.811751	0.255245	-0.000066	0.308262
1.364038	-0.822358	0.260250	-0.000040	0.308091
1.292610	-0.834469	0.265254	-0.000027	0.307973
1.401240	-0.879439	0.270259	-0.000047	0.307854
0.750354	-0.806509	0.275264	0.000074	0.307642
1.309867	-0.917808	0.280269	-0.000030	0.307596
1.201854	-0.958264	0.285274	-0.000010	0.307314
1.219338	-0.963206	0.290278	-0.000013	0.307306
1.281722	-1.041883	0.295283	-0.000025	0.306989
1.125964	-1.015403	0.300288	0.000004	0.306980
1.215432	-1.089143	0.305293	-0.000012	0.306709
0.943557	-1.042030	0.310298	0.000038	0.306699
1.029539	-1.126522	0.315302	0.000022	0.306374
0.994486	-1.123157	0.320307	0.000029	0.306360
0.903984	-1.170391	0.325312	0.000045	0.306059
1.117213	-1.217820	0.330317	0.000006	0.306018
1.055782	-1.266101	0.335322	0.000017	0.305737
0.998982	-1.271501	0.340326	0.000028	0.305663
1.096837	-1.325690	0.345331	0.000009	0.305491
0.945184	-1.337840	0.350336	0.000038	0.305303
0.929230	-1.366504	0.355341	0.000041	0.305154
0.959632	-1.426504	0.360346	0.000035	0.304895
0.845677	-1.423478	0.365350	0.000056	0.304812
0.682544	-1.456891	0.370355	0.000086	0.304512
0.472996	-1.438467	0.375360	0.000125	0.304419
0.477550	-1.478640	0.380365	0.000125	0.304232
0.440242	-1.514203	0.385370	0.000132	0.304031
0.047688	-1.470034	0.390374	0.000205	0.303902
-0.044579	-1.507094	0.395379	0.000222	0.303646
-0.095849	-1.516760	0.400384	0.000231	0.303556
0.006269	-1.595073	0.405389	0.000212	0.303271
-0.020959	-1.617487	0.410394	0.000217	0.303140
0.135887	-1.682162	0.415398	0.000188	0.302968
0.346255	-1.776847	0.420403	0.000149	0.302698
0.393483	-1.817938	0.425408	0.000140	0.302543
-0.480194	-1.707509	0.430413	0.000303	0.302312
-1.294220	-1.596110	0.435418	0.000454	0.302137
-1.378968	-1.610775	0.440422	0.000470	0.301993
-1.275894	-1.675699	0.445427	0.000451	0.301772
-1.392504	-1.672019	0.450432	0.000472	0.301688
-1.264034	-1.763845	0.455437	0.000448	0.301360
-1.494373	-1.740943	0.460442	0.000491	0.301269
-1.596975	-1.766671	0.465446	0.000510	0.301056
-1.379458	-1.845385	0.470451	0.000470	0.300868
-1.725775	-1.811840	0.475456	0.000534	0.300727
-2.539332	-1.707128	0.480461	0.000686	0.300519
-2.711453	-1.685651	0.485466	0.000718	0.300472
-2.125368	-1.857005	0.490470	0.000609	0.300160
-2.395730	-1.832600	0.495475	0.000659	0.300041
-3.565378	-1.663537	0.500480	0.000877	0.299831
-3.644847	-1.679745	0.505485	0.000891	0.299684
-3.148659	-1.806918	0.510490	0.000799	0.299505
-3.630572	-1.756477	0.515494	0.000889	0.299326
-4.229038	-1.667570	0.520499	0.001000	0.299230
-4.295166	-1.704529	0.525504	0.001012	0.298993
-4.016209	-1.773373	0.530509	0.000960	0.298906
-4.129908	-1.806068	0.535514	0.000982	0.298647
-4.240233	-1.799747	0.540518	0.001002	0.298581
-4.237541	-1.859816	0.545523	0.001002	0.298292
-4.487788	-1.824734	0.550528	0.001048	0.298242
-4.290841	-1.916930	0.555533	0.001011	0.297969
-4.926741	-1.816144	0.560538	0.001130	0.297897
-5.268063	-1.809648	0.565542	0.001193	0.297627
-4.972006	-1.878216	0.570547	0.001138	0.297556
-5.405703	-1.849839	0.575552	0.001219	0.297310
-5.702765	-1.816686	0.580557	0.001274	0.297209
-6.494069	-1.718760	0.585562	0.001421	0.296986
-5.825219	-1.855958	0.590566	0.001297	0.296910
-6.116402	-1.844641	0.595571	0.001351	0.296707
-6.415741	-1.808447	0.600576	0.001407	0.296618
-6.742321	-1.798077	0.605581	0.001467	0.296380
-7.311723	-1.702668	0.610586	0.001573	0.296340
-7.191554	-1.781075	0.615590	0.001551	0.296064
-6.589918	-1.894882	0.620595	0.001439	0.296043
-7.304000	-1.827884	0.625600	0.001572	0.295736
-7.336126	-1.820527	0.630605	0.001578	0.295743
-7.773637	-1.789533	0.635610	0.001659	0.295506
-7.650074	-1.813822	0.640614	0.001636	0.295497
-8.043218	-1.797702	0.645619	0.001709	0.295226
-8.752484	-1.680630	0.650624	0.001841	0.295168
-8.360667	-1.788067	0.655629	0.001768	0.294991
-8.812573	-1.734661	0.660634	0.001852	0.294850
-8.965649	-1.724116	0.665638	0.001881	0.294765
-9.236958	-1.720998	0.670643	0.001931	0.294539
-9.391089	-1.695220	0.675648	0.001960	0.294528
-9.569109	-1.713715	0.680653	0.001993	0.294278
-9.323013	-1.769050	0.685658	0.001947	0.294226
-9.202708	-1.829920	0.690662	0.001925	0.294034
-9.641280	-1.778272	0.695667	0.002007	0.293896
-9.860452	-1.758935	0.700672	0.002047	0.293796
-10.120241	-1.751863	0.705677	0.002096	0.293598
-10.137609	-1.750924	0.710682	0.002099	0.293587
-10.630152	-1.720821	0.715686	0.002190	0.293294
-10.366996	-1.771939	0.720691	0.002141	0.293278
-10.803436	-1.726816	0.725696	0.002223	0.293110
-10.989811	-1.717972	0.730701	0.002257	0.292986
-11.142992	-1.694199	0.735706	0.002286	0.292966
-10.714793	-1.840609	0.740710	0.002206	0.292628
-10.820858	-1.820084	0.745715	0.002226	0.292634
-11.395635	-1.766598	0.750720	0.002333	0.292382
-11.161508	-1.822852	0.755725	0.002289	0.292314
-11.653166	-1.755719	0.760730	0.002381	0.292204
-12.112965	-1.711428	0.765734	0.002466	0.292010
-11.903274	-1.749314	0.770739	0.002427	0.292011
-12.117055	-1.765754	0.775744	0.002467	0.291737
-12.479009	-1.702962	0.780749	0.002534	0.291722
-12.475332	-1.728627	0.785754	0.002533	0.291599
-12.474022	-1.772114	0.790758	0.002533	0.291384
-12.710945	-1.726129	0.795763	0.002577	0.291399
-13.512583	-1.636145	0.800768	0.002726	0.291122
-13.554075	-1.632549	0.805773	0.002734	0.291103
-12.680992	-1.811959	0.810778	0.002572	0.291000
-13.508289	-1.711405	0.815782	0.002726	0.290752
-12.962274	-1.811806	0.820787	0.002624	0.290747
-13.266182	-1.795135	0.825792	0.002680	0.290555
-13.371183	-1.788396	0.830797	0.002700	0.290493
-13.540702	-1.778716	0.835802	0.002732	0.290388
-13.754662	-1.787100	0.840806	0.002771	0.290153
-13.440974	-1.844332	0.845811	0.002713	0.290152
-14.224143	-1.761718	0.850816	0.002859	0.289854
-14.124127	-1.783551	0.855821	0.002840	0.289836
-14.187882	-1.798650	0.860826	0.002852	0.289703
-14.878263	-1.712269	0.865830	0.002980	0.289507
-14.691821	-1.744938	0.870835	0.002946	0.289514
-14.731706	-1.788905	0.875840	0.002953	0.289258
-14.985676	-1.749044	0.880845	0.003000	0.289226
-15.268801	-1.713877	0.885850	0.003053	0.289145
-15.286047	-1.762809	0.890854	0.003056	0.288884
-15.084332	-1.798760	0.895859	0.003018	0.288888
-15.992201	-1.678084	0.900864	0.003187	0.288666
-15.759901	-1.736367	0.905869	0.003144	0.288586
-15.828574	-1.727207	0.910874	0.003157	0.288569
-16.054793	-1.749238	0.915878	0.003199	0.288252
-16.062531	-1.746928	0.920883	0.003200	0.288257
-16.265361	-1.733314	0.925888	0.003238	0.288140
-16.290151	-1.761788	0.930893	0.003243	0.287975
-16.382063	-1.748571	0.935898	0.003260	0.287958
-16.638519	-1.756259	0.940902	0.003308	0.287685
-16.246536	-1.840168	0.945907	0.003235	0.287621
-16.902838	-1.737323	0.950912	0.003357	0.287538
-17.352827	-1.698372	0.955917	0.003440	0.287323
-17.401340	-1.689384	0.960922	0.003449	0.287324
-17.342219	-1.734005	0.965926	0.003438	0.287153
-18.166353	-1.611091	0.970931	0.003592	0.287018
-17.855276	-1.670734	0.975936	0.003534	0.287003
-17.918633	-1.696276	0.980941	0.003546	0.286816
-18.337672	-1.641575	0.985946	0.003623	0.286708
-17.836318	-1.734668	0.990950	0.003530	0.286698
-18.125467	-1.737256	0.995955	0.003584	0.286419
-18.858406	-1.612013	1.000960	0.003720	0.286379
-18.421810	-1.696933	1.005965	0.003639	0.286351
-18.424236	-1.752614	1.010970	0.003639	0.286068
-18.960202	-1.653583	1.015974	0.003739	0.286076
-19.514937	-1.568345	1.020979	0.003842	0.285997
-19.142673	-1.686487	1.025984	0.003773	0.285742
-18.761397	-1.753824	1.030989	0.003702	0.285752
-19.236517	-1.694051	1.035994	0.003791	0.285617
-19.368929	-1.694724	1.040998	0.003815	0.285492
-18.946377	-1.771649	1.046003	0.003736	0.285492
-19.916045	-1.653443	1.051008	0.003917	0.285197
-19.827049	-1.676496	1.056013	0.003900	0.285163
-20.033470	-1.641898	1.061018	0.003939	0.285148
-20.212477	-1.670333	1.066022	0.003972	0.284838
-20.338756	-1.643637	1.071027	0.003995	0.284858
-20.033027	-1.720912	1.076032	0.003939	0.284748
-20.209110	-1.735131	1.081037	0.003971	0.284513
-20.360244	-1.708738	1.086042	0.003999	0.284507
-20.356020	-1.744547	1.091046	0.003999	0.284329
-20.291508	-1.778287	1.096051	0.003987	0.284217
-20.375929	-1.768147	1.101056	0.004002	0.284191
-21.068658	-1.701477	1.106061	0.004131	0.283889
-20.823608	-1.747729	1.111066	0.004085	0.283881
-20.816495	-1.774608	1.116070	0.004084	0.283750
-21.243460	-1.730525	1.121075	0.004164	0.283579
-21.486006	-1.689284	1.126080	0.004209	0.283565
-21.399001	-1.747759	1.131085	0.004192	0.283347
-21.465180	-1.756885	1.136090	0.004205	0.283239
-21.692307	-1.721632	1.141094	0.004247	0.283209
-21.741751	-1.760905	1.146099	0.004256	0.282962
-21.919905	-1.730046	1.151104	0.004289	0.282954
-21.947923	-1.754941	1.156109	0.004294	0.282801
-22.337718	-1.718994	1.161114	0.004367	0.282622
-22.475635	-1.694142	1.166118	0.004393	0.282622
-22.329447	-1.769809	1.171123	0.004365	0.282370
-23.047610	-1.651995	1.176128	0.004499	0.282305
-22.404079	-1.774539	1.181133	0.004379	0.282277
-22.959855	-1.730667	1.186138	0.004483	0.281984
-22.958619	-1.732156	1.191142	0.004482	0.281977
-22.984366	-1.747535	1.196147	0.004487	0.281874
-23.458621	-1.695636	1.201152	0.004575	0.281698
-23.616179	-1.665499	1.206157	0.004605	0.281706
-23.874288	-1.659577	1.211162	0.004653	0.281495
-23.603376	-1.735104	1.216166	0.004602	0.281361
-23.762721	-1.703832	1.221171	0.004632	0.281373
-24.146201	-1.692298	1.226176	0.004703	0.281073
-24.433303	-1.639973	1.231181	0.004757	0.281074
-24.380312	-1.658786	1.236186	0.004747	0.281027
-24.787697	-1.638341	1.241190	0.004823	0.280751
-24.563980	-1.678769	1.246195	0.004781	0.280752
-24.882948	-1.633329	1.251200	0.004840	0.280688
-25.097455	-1.625770	1.256205	0.004880	0.280526
-24.631362	-1.715457	1.261210	0.004793	0.280500
-24.542112	-1.766000	1.266214	0.004777	0.280323
-25.001182	-1.713035	1.271219	0.004862	0.280166
-25.166722	-1.683629	1.276224	0.004893	0.280163
-25.013937	-1.763648	1.281229	0.004864	0.279893
-25.138372	-1.750877	1.286234	0.004888	0.279842
-25.406429	-1.720712	1.291238	0.004937	0.279746
-25.433289	-1.760577	1.296243	0.004942	0.279515
-25.677966	-1.716734	1.301248	0.004988	0.279511
-25.754155	-1.740164	1.306253	0.005002	0.279318
-26.311444	-1.654826	1.311258	0.005106	0.279236
-26.234898	-1.668865	1.316262	0.005091	0.279235
-26.161331	-1.740693	1.321267	0.005078	0.278932
-26.789193	-1.632742	1.326272	0.005195	0.278900
-26.218415	-1.753462	1.331277	0.005088	0.278812
-26.299135	-1.784866	1.336282	0.005103	0.278573
-26.796202	-1.693522	1.341286	0.005196	0.278578
-26.796502	-1.729992	1.346291	0.005196	0.278389
-26.863654	-1.743544	1.351296	0.005208	0.278255
-26.824470	-1.751007	1.356301	0.005201	0.278253
-27.527251	-1.675350	1.361306	0.005332	0.277982
-27.548114	-1.672916	1.366310	0.005336	0.277975
-27.745298	-1.648590	1.371315	0.005372	0.277915
-27.979106	-1.659905	1.376320	0.005416	0.277635
-27.360165	-1.772245	1.381325	0.005301	0.277636
-27.986540	-1.690390	1.386330	0.005417	0.277469
-28.442188	-1.636451	1.391334	0.005502	0.277319
-28.030525	-1.710454	1.396339	0.005425	0.277323
-28.376526	-1.697880	1.401344	0.005490	0.277061
-28.515956	-1.684529	1.406349	0.005516	0.276998
-29.032174	-1.587573	1.411354	0.005612	0.277014
-28.795624	-1.686766	1.416358	0.005568	0.276721
-28.747971	-1.696043	1.421363	0.005559	0.276718
-29.100203	-1.651137	1.426368	0.005624	0.276618
-29.229279	-1.672893	1.431373	0.005648	0.276381
-28.957540	-1.722893	1.436378	0.005598	0.276378
-29.217957	-1.712281	1.441382	0.005646	0.276186
-29.210218	-1.736430	1.446387	0.005645	0.276067
-29.383563	-1.705744	1.451392	0.005677	0.276063
-29.564526	-1.729083	1.456397	0.005710	0.275768
-29.659751	-1.716293	1.461402	0.005728	0.275744
-29.602434	-1.743176	1.466406	0.005717	0.275658
-29.668806	-1.760804	1.471411	0.005730	0.275502
-29.720123	-1.753425	1.476416	0.005739	0.275492
-29.647721	-1.818282	1.481421	0.005726	0.275220
-29.838992	-1.795400	1.486426	0.005761	0.275158
-30.380145	-1.720676	1.491430	0.005862	0.275033
-30.807160	-1.677407	1.496435	0.005941	0.274853
-30.552904	-1.726823	1.501440	0.005894	0.274836
-31.303815	-1.627702	1.506445	0.006034	0.274639
-31.541728	-1.605917	1.511450	0.006078	0.274526
-31.331181	-1.644951	1.516454	0.006039	0.274522
-31.307978	-1.689470	1.521459	0.006035	0.274310
-32.629745	-1.459112	1.526464	0.006280	0.274257
-31.987580	-1.578557	1.531469	0.006161	0.274243
-31.537634	-1.714744	1.536474	0.006077	0.273956
-31.842780	-1.673558	1.541478	0.006134	0.273881
-31.853481	-1.677887	1.546483	0.006136	0.273848
-32.094825	-1.684350	1.551488	0.006181	0.273582
-31.862510	-1.726286	1.556493	0.006138	0.273583
-32.579709	-1.623865	1.561498	0.006271	0.273435
-32.381391	-1.692422	1.566502	0.006234	0.273264
-32.213138	-1.721210	1.571507	0.006203	0.273273
-33.198866	-1.588010	1.576512	0.006386	0.273029
-32.859189	-1.660216	1.581517	0.006323	0.272974
-32.578381	-1.717112	1.586522	0.006271	0.272943
-33.331659	-1.635885	1.591526	0.006411	0.272648
-33.320153	-1.637552	1.596531	0.006409	0.272650
-33.377677	-1.649469	1.601536	0.006419	0.272531
-33.012994	-1.755369	1.606541	0.006351	0.272321
-33.244147	-1.715004	1.611546	0.006394	0.272313
-33.337885	-1.745233	1.616550	0.006412	0.272061
-33.389067	-1.748136	1.621555	0.006421	0.271996
-33.670012	-1.710917	1.626560	0.006474	0.271923
-34.025764	-1.687568	1.631565	0.006540	0.271703
-33.597691	-1.766085	1.636570	0.006460	0.271699
-33.963434	-1.742022	1.641574	0.006528	0.271473
-34.409110	-1.679628	1.646579	0.006611	0.271374
-34.512686	-1.662937	1.651584	0.006630	0.271363
-34.051881	-1.802543	1.656589	0.006544	0.271065
-34.558358	-1.710042	1.661594	0.006639	0.271067
-34.918263	-1.675125	1.666598	0.006706	0.270904
-34.683990	-1.745160	1.671603	0.006662	0.270758
-34.751893	-1.735175	1.676608	0.006675	0.270745
-34.999096	-1.735043	1.681613	0.006721	0.270506
-35.096891	-1.719462	1.686618	0.006739	0.270494
-35.332850	-1.703900	1.691622	0.006783	0.270348
-35.319685	-1.743564	1.696627	0.006780	0.270148
-35.380457	-1.733065	1.701632	0.006791	0.270146
-35.501317	-1.761429	1.706637	0.006814	0.269876
-35.811432	-1.713441	1.711642	0.006872	0.269831
-36.104702	-1.678639	1.716646	0.006926	0.269731
-35.841397	-1.768297	1.721651	0.006877	0.269507
-35.926792	-1.755148	1.726656	0.006893	0.269495
-36.234013	-1.738944	1.731661	0.006950	0.269282
-36.224538	-1.751723	1.736666	0.006948	0.269222
-36.356835	-1.746011	1.741670	0.006973	0.269124
-36.665223	-1.734851	1.746675	0.007030	0.268882
-36.868020	-1.699000	1.751680	0.007068	0.268877
-36.536195	-1.799667	1.756685	0.007006	0.268660
-36.927365	-1.744909	1.761690	0.007079	0.268572
-37.165903	-1.714829	1.766694	0.007123	0.268500
-37.169929	-1.758723	1.771699	0.007124	0.268260
-37.677875	-1.667478	1.776704	0.007219	0.268254
-37.491345	-1.736593	1.781709	0.007184	0.268064
-37.801228	-1.698754	1.786714	0.007242	0.267964
-37.645417	-1.731864	1.791718	0.007213	0.267938
-37.667283	-1.785407	1.796723	0.007217	0.267627
-38.044000	-1.719037	1.801728	0.007287	0.267616
-37.762809	-1.802926	1.806733	0.007234	0.267439
-38.122694	-1.762561	1.811738	0.007301	0.267303
-38.345949	-1.727594	1.816742	0.007343	0.267273
-38.250196	-1.798535	1.821747	0.007325	0.266983
-38.464571	-1.761252	1.826752	0.007365	0.266974
-38.781800	-1.733785	1.831757	0.007424	0.266810
-39.059521	-1.704358	1.836762	0.007475	0.266696
-38.852269	-1.745004	1.841766	0.007437	0.266680
-38.961352	-1.783096	1.846771	0.007457	0.266365
-39.589940	-1.669784	1.851776	0.007574	0.266360
-39.658076	-1.679365	1.856781	0.007587	0.266241
-39.888963	-1.669974	1.861786	0.007630	0.266063
-40.003597	-1.650870	1.866790	0.007651	0.266054
-39.756105	-1.736280	1.871795	0.007605	0.265834
-40.193897	-1.675331	1.876800	0.007686	0.265733
-40.220087	-1.674228	1.881805	0.007691	0.265713
-40.228626	-1.714560	1.886810	0.007693	0.265485
-40.369073	-1.691272	1.891814	0.007719	0.265473
-40.365270	-1.721001	1.896819	0.007718	0.265315
-41.066041	-1.626226	1.901824	0.007849	0.265136
-40.531679	-1.724275	1.906829	0.007749	0.265132
-40.644245	-1.753327	1.911834	0.007770	0.264861
-41.252332	-1.651527	1.916838	0.007883	0.264813
-41.222449	-1.669792	1.921843	0.007878	0.264743
-41.258679	-1.710105	1.926848	0.007884	0.264487
-41.457813	-1.671157	1.931853	0.007921	0.264502
-41.495795	-1.697246	1.936858	0.007928	0.264321
-41.808870	-1.660696	1.941862	0.007987	0.264210
-41.505629	-1.717699	1.946867	0.007930	0.264200
-42.408741	-1.612495	1.951872	0.008098	0.263876
-41.859532	-1.714061	1.956877	0.007996	0.263867
-41.738487	-1.758129	1.961882	0.007973	0.263746
-42.864388	-1.585893	1.966886	0.008183	0.263568
-42.358873	-1.677411	1.971891	0.008089	0.263570
-42.456948	-1.703653	1.976896	0.008107	0.263328
-42.762562	-1.663669	1.981901	0.008164	0.263242
-42.753514	-1.670452	1.986906	0.008162	0.263214
-42.733763	-1.724395	1.991910	0.008158	0.262937
-42.719458	-1.724993	1.996915	0.008156	0.262949
-43.130931	-1.698010	2.001920	0.008232	0.262685

-43.300870	-1.703330	2.011917	0.008264	0.262486
-43.526539	-1.697433	2.021914	0.008306	0.262292
-43.551136	-1.738786	2.031910	0.008310	0.262039
-43.706681	-1.723543	2.041907	0.008339	0.261968
-44.183707	-1.683792	2.051904	0.008428	0.261708
-43.870720	-1.746388	2.061901	0.008370	0.261677
-44.027553	-1.751935	2.071898	0.008399	0.261489
-44.276982	-1.732846	2.081894	0.008445	0.261343
-44.251810	-1.737601	2.091891	0.008440	0.261343
-44.349888	-1.732351	2.101888	0.008459	0.261274
-44.514605	-1.745915	2.111885	0.008489	0.261033
-44.508724	-1.746756	2.121882	0.008488	0.261034
-44.572386	-1.735027	2.131878	0.008500	0.261035
-44.484103	-1.751366	2.141875	0.008483	0.261034
-44.544848	-1.740893	2.151872	0.008494	0.261031
-44.611772	-1.728229	2.161869	0.008507	0.261035
-44.572216	-1.735810	2.171866	0.008499	0.261033
-44.603080	-1.730107	2.181862	0.008505	0.261034
-44.467180	-1.755696	2.191859	0.008480	0.261029
-44.739079	-1.705832	2.201856	0.008530	0.261032
-44.556859	-1.739203	2.211853	0.008496	0.261031
-44.588593	-1.733001	2.221850	0.008502	0.261034
-44.278948	-1.764669	2.231846	0.008444	0.261171
-44.113192	-1.764260	2.241843	0.008413	0.261341
-44.261084	-1.737550	2.251840	0.008441	0.261340
-44.097717	-1.767478	2.261837	0.008410	0.261340
-44.285542	-1.722376	2.271834	0.008445	0.261401
-43.825286	-1.756135	2.281830	0.008359	0.261678
-43.822132	-1.757500	2.291827	0.008359	0.261674
-43.804480	-1.762102	2.301824	0.008355	0.261667
-43.458607	-1.776302	2.311821	0.008291	0.261936
-43.667958	-1.734391	2.321818	0.008330	0.261958
-43.500998	-1.751683	2.331814	0.008299	0.262031
-43.396134	-1.724664	2.341811	0.008279	0.262286
-43.366624	-1.730524	2.351808	0.008274	0.262283
-42.921775	-1.760785	2.361805	0.008191	0.262564
-43.073182	-1.726725	2.371802	0.008219	0.262600
-42.707682	-1.752921	2.381798	0.008151	0.262822
-42.623104	-1.747478	2.391795	0.008135	0.262938
-42.628962	-1.716728	2.401792	0.008136	0.263101
-42.228210	-1.767191	2.411789	0.008061	0.263225
-42.352405	-1.708614	2.421786	0.008084	0.263424
-41.977279	-1.753164	2.431782	0.008014	0.263554
-41.925205	-1.720848	2.441779	0.008004	0.263784
-41.729459	-1.742158	2.451776	0.007968	0.263863
-41.445156	-1.735755	2.461773	0.007915	0.264182
-41.326651	-1.746219	2.471770	0.007893	0.264243
-41.024368	-1.756994	2.481766	0.007836	0.264486
-41.081924	-1.718999	2.491763	0.007847	0.264637
-40.633566	-1.769124	2.501760	0.007764	0.264810
-40.532081	-1.743496	2.511757	0.007745	0.265051
-40.335806	-1.760264	2.521754	0.007708	0.265155
-40.090309	-1.746546	2.531750	0.007662	0.265474
-40.013589	-1.737978	2.541747	0.007648	0.265597
-39.735347	-1.764758	2.551744	0.007596	0.265727
-39.831282	-1.694507	2.561741	0.007614	0.266015
-39.434300	-1.739748	2.571738	0.007540	0.266163
-38.917218	-1.798074	2.581734	0.007443	0.266357
-38.798009	-1.772621	2.591731	0.007421	0.266614
-38.925815	-1.723216	2.601728	0.007445	0.266756
-38.488932	-1.762442	2.611725	0.007363	0.266975
-38.292789	-1.752809	2.621722	0.007327	0.267221
-38.277208	-1.723782	2.631718	0.007324	0.267394
-37.797404	-1.770161	2.641715	0.007234	0.267616
-37.506925	-1.772737	2.651712	0.007180	0.267888
-37.717513	-1.704305	2.661709	0.007219	0.268051
-37.154043	-1.770156	2.671706	0.007114	0.268250
-37.201926	-1.707037	2.681702	0.007123	0.268543
-36.939281	-1.720142	2.691699	0.007074	0.268731
-36.468925	-1.773736	2.701696	0.006987	0.268903
-36.244011	-1.756835	2.711693	0.006945	0.269215
-36.126277	-1.744712	2.721690	0.006923	0.269396
-36.003612	-1.730772	2.731686	0.006900	0.269591
-35.650740	-1.750925	2.741683	0.006834	0.269827
-35.450550	-1.734949	2.751680	0.006797	0.270109
-35.397416	-1.705935	2.761677	0.006787	0.270317
-34.781439	-1.780551	2.771674	0.006672	0.270517
-34.717910	-1.749705	2.781670	0.006660	0.270745
-34.470283	-1.751398	2.791667	0.006614	0.270977
-34.339952	-1.739109	2.801664	0.006589	0.271169
-34.017893	-1.761125	2.811661	0.006529	0.271365
-33.691739	-1.757988	2.821658	0.006469	0.271698
-33.540598	-1.751664	2.831654	0.006440	0.271879
-33.259697	-1.768131	2.841651	0.006388	0.272064
-33.165954	-1.738578	2.851648	0.006370	0.272312
-32.762151	-1.758541	2.861645	0.006295	0.272596
-32.603511	-1.747744	2.871642	0.006266	0.272807
-32.585351	-1.707330	2.881638	0.006262	0.273040
-32.204208	-1.735064	2.891635	0.006191	0.273260
-31.932974	-1.730747	2.901632	0.006140	0.273545
-31.718713	-1.730905	2.911629	0.006100	0.273751
-31.370819	-1.752884	2.921626	0.006036	0.273969
-31.247974	-1.726536	2.931622	0.006013	0.274227
-30.838445	-1.750551	2.941619	0.005936	0.274494
-30.696624	-1.735730	2.951616	0.005910	0.274708
-30.482898	-1.735727	2.961613	0.005870	0.274913
-30.032357	-1.771401	2.971610	0.005786	0.275157
-29.810548	-1.753626	2.981606	0.005745	0.275463
-29.722327	-1.736218	2.991603	0.005728	0.275639
-29.546193	-1.734917	3.001600	0.005695	0.275815
-29.285612	-1.736500	3.011597	0.005647	0.276056
-29.009272	-1.730295	3.021594	0.005595	0.276352
-28.876744	-1.710706	3.031590	0.005570	0.276581
-28.330465	-1.769126	3.041587	0.005469	0.276796
-28.388551	-1.720393	3.051584	0.005479	0.276995
-27.894453	-1.750178	3.061581	0.005387	0.277310
-27.720329	-1.739315	3.071578	0.005355	0.277532
-27.490845	-1.738304	3.081574	0.005312	0.277755
-26.967923	-1.792119	3.091571	0.005215	0.277971
-26.703876	-1.786788	3.101568	0.005165	0.278249
-26.823390	-1.724124	3.111565	0.005187	0.278462
-26.528038	-1.734200	3.121562	0.005132	0.278689
-26.136357	-1.766360	3.131558	0.005059	0.278892
-25.918041	-1.742911	3.141555	0.005019	0.279220
-25.859222	-1.713591	3.151552	0.005008	0.279428
-25.450212	-1.746592	3.161549	0.004931	0.279643
-25.437549	-1.702052	3.171546	0.004929	0.279885
-25.005159	-1.727909	3.181542	0.004848	0.280159
-24.580443	-1.752207	3.191539	0.004769	0.280432
-24.832170	-1.671539	3.201536	0.004816	0.280613
-24.347133	-1.723552	3.211533	0.004726	0.280800
-23.976019	-1.743212	3.221530	0.004656	0.281047
-23.720738	-1.735822	3.231526	0.004609	0.281324
-23.441805	-1.741708	3.241523	0.004557	0.281555
-23.186914	-1.748529	3.251520	0.004509	0.281759
-22.788060	-1.780438	3.261517	0.004435	0.281967
-22.701984	-1.735829	3.271514	0.004419	0.282277
-22.328678	-1.762560	3.281510	0.004349	0.282488
-22.129990	-1.755758	3.291507	0.004312	0.282709
-21.781189	-1.773833	3.301504	0.004247	0.282941
-21.517372	-1.769557	3.311501	0.004198	0.283209
-21.334851	-1.762517	3.321498	0.004164	0.283415
-20.962427	-1.790211	3.331494	0.004094	0.283619
-20.707185	-1.788517	3.341491	0.004047	0.283865
-20.613865	-1.750493	3.351488	0.004029	0.284146
-20.406692	-1.749250	3.361485	0.003991	0.284344
-20.366675	-1.716041	3.371482	0.003983	0.284551
-19.655161	-1.793444	3.381478	0.003851	0.284815
-19.486550	-1.773035	3.391475	0.003819	0.285075
-19.322360	-1.760887	3.401472	0.003789	0.285288
-19.005641	-1.776877	3.411469	0.003730	0.285500
-18.735432	-1.782248	3.421466	0.003679	0.285722
-18.336825	-1.808291	3.431462	0.003605	0.285957
-18.354641	-1.764312	3.441459	0.003608	0.286164
-17.886137	-1.813321	3.451456	0.003521	0.286347
-17.669936	-1.787771	3.461453	0.003480	0.286675
-17.564119	-1.770770	3.471450	0.003461	0.286858
-17.152907	-1.808080	3.481446	0.003384	0.287048
-16.982747	-1.789972	3.491443	0.003352	0.287295
-16.737478	-1.781275	3.501440	0.003306	0.287564
-16.601959	-1.760917	3.511437	0.003281	0.287791
-16.215114	-1.791285	3.521434	0.003209	0.287992
-15.785464	-1.821358	3.531430	0.003129	0.288234
-15.703621	-1.787747	3.541427	0.003114	0.288477
-15.555284	-1.775023	3.551424	0.003086	0.288677
-15.193816	-1.801323	3.561421	0.003019	0.288875
-15.017024	-1.766803	3.571418	0.002986	0.289209
-14.644159	-1.795961	3.581414	0.002916	0.289402
-14.782139	-1.730789	3.591411	0.002942	0.289603
-14.187287	-1.795349	3.601408	0.002831	0.289821
-14.015921	-1.765759	3.611405	0.002799	0.290125
-13.704299	-1.778693	3.621402	0.002741	0.290343
-13.553869	-1.765096	3.631398	0.002713	0.290548
-13.284897	-1.776021	3.641395	0.002663	0.290737
-12.924908	-1.785369	3.651392	0.002595	0.291016
-12.808964	-1.767074	3.661389	0.002574	0.291212
-12.564963	-1.770716	3.671386	0.002528	0.291415
-12.173782	-1.784656	3.681382	0.002455	0.291699
-12.036205	-1.763094	3.691379	0.002430	0.291931
-11.681203	-1.787584	3.701376	0.002363	0.292129
-11.254179	-1.826025	3.711373	0.002284	0.292324
-10.928025	-1.824676	3.721370	0.002223	0.292624
-10.860488	-1.794088	3.731366	0.002210	0.292836
-10.664629	-1.791545	3.741363	0.002174	0.293025
-10.361746	-1.799436	3.751360	0.002117	0.293258
-10.183927	-1.779064	3.761357	0.002084	0.293519
-9.907700	-1.789587	3.771354	0.002033	0.293715
-9.615079	-1.803405	3.781350	0.001978	0.293909
-9.541218	-1.752146	3.791347	0.001964	0.294228
-8.935967	-1.821832	3.801344	0.001852	0.294426
-9.062372	-1.762336	3.811341	0.001875	0.294606
-8.667531	-1.785639	3.821338	0.001801	0.294844
-8.354408	-1.784244	3.831334	0.001743	0.295131
-8.333820	-1.742327	3.841331	0.001739	0.295355
-8.165472	-1.732116	3.851328	0.001708	0.295555
-7.892123	-1.741791	3.861325	0.001657	0.295751
-7.565258	-1.743011	3.871322	0.001596	0.296036
-7.320766	-1.746540	3.881318	0.001550	0.296237
-7.065410	-1.750562	3.891315	0.001503	0.296444
-7.699238	-1.577457	3.901312	0.001620	0.296727
-6.693673	-1.705021	3.911309	0.001433	0.296996
-6.411172	-1.709348	3.921306	0.001380	0.297226
-6.410045	-1.662739	3.931302	0.001380	0.297454
-6.015970	-1.688500	3.941299	0.001307	0.297677
-5.928358	-1.644155	3.951296	0.001290	0.297970
-5.707471	-1.633817	3.961293	0.001249	0.298216
-4.948452	-1.724043	3.971290	0.001108	0.298448
-5.245144	-1.626264	3.981286	0.001163	0.298660
-4.675139	-1.683680	3.991283	0.001057	0.298884
-4.691967	-1.610115	4.001280	0.001060	0.299226
-4.908272	-1.526378	4.011277	0.001100	0.299441
-5.091040	-1.436679	4.021274	0.001134	0.299714
-4.803073	-1.426673	4.031270	0.001080	0.300015
-4.252426	-1.468765	4.041267	0.000977	0.300295
-4.040331	-1.452518	4.051264	0.000938	0.300559
-3.529838	-1.505568	4.061261	0.000843	0.300751
-3.866622	-1.380697	4.071258	0.000905	0.301058
-2.746306	-1.524903	4.081254	0.000697	0.301343
-3.865345	-1.267765	4.091251	0.000905	0.301602
-3.696373	-1.236120	4.101248	0.000873	0.301901
-3.747697	-1.157467	4.111245	0.000883	0.302233
-2.687471	-1.283374	4.121242	0.000685	0.302553
-2.404125	-1.273238	4.131238	0.000632	0.302848
-2.607988	-1.175767	4.141235	0.000670	0.303137
-2.460888	-1.141052	4.151232	0.000643	0.303430
-2.580565	-1.052213	4.161229	0.000665	0.303751
-2.634930	-0.968540	4.171226	0.000675	0.304102
-1.949292	-1.026111	4.181222	0.000547	0.304421
-1.993185	-0.948589	4.191219	0.000555	0.304752
-1.617973	-0.947522	4.201216	0.000485	0.305081
-1.835583	-0.832703	4.211213	0.000526	0.305438
-1.766199	-0.779912	4.221210	0.000513	0.305748
-1.556675	-0.740024	4.231206	0.000474	0.306117
-1.415875	-0.690070	4.241203	0.000447	0.306474
-1.370622	-0.623130	4.251200	0.000439	0.306829
-1.322329	-0.556058	4.261197	0.000430	0.307187
-1.238951	-0.492078	4.271194	0.000414	0.307560
-0.985608	-0.443451	4.281190	0.000367	0.308005
-1.127937	-0.337534	4.291187	0.000393	0.308381
-0.965167	-0.286816	4.301184	0.000363	0.308758
-0.805980	-0.225162	4.311181	0.000333	0.309183
-0.581646	-0.176611	4.321178	0.000291	0.309601
-0.553651	-0.095284	4.331174	0.000286	0.310005
-0.689089	0.023146	4.341171	0.000311	0.310442
-0.429410	0.063861	4.351168	0.000262	0.310852
-0.287702	0.124092	4.361165	0.000236	0.311252
0.000000	0.163660	4.371162	0.000182	0.311679

-0.187257	0.473363	4.376166	0.000217	0.312957
0.309750	0.952292	4.381171	0.000124	0.315577
0.814149	1.714785	4.386176	0.000029	0.319469
1.047791	2.818727	4.391181	-0.000015	0.324619
1.811470	4.123476	4.396186	-0.000158	0.330990
2.868096	5.668508	4.401190	-0.000356	0.338496
3.731943	7.564745	4.406195	-0.000518	0.347160
5.528620	9.599616	4.411200	-0.000854	0.356862
9.757835	11.517930	4.416205	-0.001643	0.367587
13.996511	13.798084	4.421210	-0.002433	0.379393
17.956842	16.482647	4.426214	-0.003173	0.392148
22.630159	19.418364	4.431219	-0.004045	0.405856
27.654893	22.667083	4.436224	-0.004982	0.420411
31.699900	26.481130	4.441229	-0.005738	0.435764
36.484397	30.547052	4.446234	-0.006632	0.451826
41.178086	35.024101	4.451238	-0.007509	0.468553
45.393369	39.987024	4.456243	-0.008297	0.485888
49.997261	45.265523	4.461248	-0.009157	0.503731
54.904697	50.880054	4.466253	-0.010075	0.522041
59.082805	56.997440	4.471258	-0.010857	0.540720
61.811901	63.723581	4.476262	-0.011370	0.559671
64.308417	70.829017	4.481267	-0.011839	0.578841
66.831729	78.237190	4.486272	-0.012314	0.598137
69.072979	85.983578	4.491277	-0.012736	0.617501
71.574606	93.971476	4.496282	-0.013207	0.636927
73.659596	102.273463	4.501286	-0.013601	0.656304
75.634628	110.836733	4.506291	-0.013974	0.675639
77.605164	119.584032	4.511296	-0.014347	0.694815
79.239204	128.577714	4.516301	-0.014657	0.713851
80.840824	137.743599	4.521306	-0.014961	0.732720
82.037768	147.114469	4.526310	-0.015190	0.751368
83.518782	156.541040	4.531315	-0.015472	0.769763
84.704948	166.120560	4.536320	-0.015699	0.787912
85.761633	175.784987	4.541325	-0.015902	0.805762
86.730308	185.534606	4.546330	-0.016089	0.823346
87.420185	195.361662	4.551334	-0.016224	0.840611
88.501664	205.125999	4.556339	-0.016432	0.857537
89.321459	214.947197	4.561344	-0.016591	0.874153
89.774197	224.826080	4.566349	-0.016682	0.890447
90.580738	234.639192	4.571354	-0.016838	0.906442
90.885062	244.490042	4.576358	-0.016901	0.922081
92.583102	254.088875	4.581363	-0.017224	0.937446
93.458801	263.796835	4.586368	-0.017393	0.952509
94.020209	273.507350	4.591373	-0.017504	0.967259
94.030870	283.290645	4.596378	-0.017513	0.981753
94.935959	292.846457	4.601382	-0.017687	0.995932
95.278934	302.438595	4.606387	-0.017758	1.009823
96.263627	311.850197	4.611392	-0.017947	1.023429
98.105069	321.080930	4.616397	-0.018296	1.036810
99.011908	330.437895	4.621402	-0.018471	1.049971
99.847829	339.746199	4.626406	-0.018633	1.062885
100.562165	349.050051	4.631411	-0.018772	1.075610
101.309749	358.256067	4.636416	-0.018917	1.088063
102.005255	367.442346	4.641421	-0.019053	1.100337
102.497334	376.623600	4.646426	-0.019150	1.112423
102.873937	385.737955	4.651430	-0.019226	1.124268
104.418538	394.629948	4.656435	-0.019520	1.135962
105.216330	403.617418	4.661440	-0.019674	1.147494
105.598154	412.637838	4.666445	-0.019751	1.158863
106.299619	421.541760	4.671450	-0.019888	1.170046
107.511098	430.307658	4.676454	-0.020119	1.181060
108.083552	439.175127	4.681459	-0.020232	1.191963
108.489370	448.007441	4.686464	-0.020313	1.202690
109.132848	456.775742	4.691469	-0.020438	1.213294
109.724594	465.520700	4.696474	-0.020554	1.223768
110.793171	474.156724	4.701478	-0.020759	1.234120
112.039856	482.732881	4.706483	-0.020997	1.244352
112.746325	491.393397	4.711488	-0.021134	1.254490
113.267433	500.044974	4.716493	-0.021237	1.264502
113.906062	508.673730	4.721498	-0.021361	1.274431
114.361344	517.281068	4.726502	-0.021452	1.284224
115.430138	525.780160	4.731507	-0.021656	1.293937
116.010873	534.347484	4.736512	-0.021770	1.303562
116.311225	542.999769	4.741517	-0.021832	1.313158
117.139788	551.464757	4.746522	-0.021991	1.322576
117.828354	559.920374	4.751526	-0.022125	1.331892
118.646568	568.348050	4.756531	-0.022283	1.341137
119.461584	576.778205	4.761536	-0.022440	1.350319
119.862602	585.252909	4.766541	-0.022521	1.359413
120.366072	593.696649	4.771546	-0.022620	1.368432
121.378470	602.047348	4.776550	-0.022814	1.377383
122.140893	610.439964	4.781555	-0.022961	1.386276
123.049332	618.799144	4.786560	-0.023136	1.395103
123.623533	627.180547	4.791565	-0.023248	1.403839
123.921754	635.646356	4.796570	-0.023310	1.412561
124.020032	644.073868	4.801574	-0.023333	1.421156
124.801753	652.390863	4.806579	-0.023484	1.429702
125.115046	660.779560	4.811584	-0.023548	1.438192
125.310884	669.151632	4.816589	-0.023590	1.446596
125.791413	677.488049	4.821594	-0.023685	1.454962
126.891415	685.697274	4.826598	-0.023895	1.463255
127.473428	694.043627	4.831603	-0.024009	1.471552
127.797965	702.393425	4.836608	-0.024075	1.479765
128.708567	710.606085	4.841613	-0.024250	1.487892
129.357747	718.913089	4.846618	-0.024376	1.496024
129.778769	727.203911	4.851622	-0.024460	1.504061
130.235588	735.514542	4.856627	-0.024551	1.512079
130.835961	743.768699	4.861632	-0.024668	1.520024
130.947533	752.103045	4.866637	-0.024694	1.527927
131.351241	760.400792	4.871642	-0.024775	1.535800
131.754953	768.655975	4.876646	-0.024855	1.543593
132.415194	776.905076	4.881651	-0.024984	1.551380
132.923101	785.143905	4.886656	-0.025084	1.559095
133.312512	793.383381	4.891661	-0.025162	1.566755
134.191140	801.588323	4.896666	-0.025331	1.574419
134.515727	809.848862	4.901670	-0.025396	1.582014
135.133276	818.079902	4.906675	-0.025517	1.589589
136.061793	826.241393	4.911680	-0.025695	1.597110
136.386750	834.493795	4.916685	-0.025761	1.604590
136.889714	842.748844	4.921690	-0.025860	1.612063
137.038866	851.020224	4.926694	-0.025893	1.619465
137.610361	859.231652	4.931699	-0.026005	1.626840
137.910263	867.516589	4.936704	-0.026066	1.634209
138.100259	875.731422	4.941709	-0.026107	1.641467
138.827023	883.889266	4.946714	-0.026248	1.648718
139.180104	892.107833	4.951718	-0.026319	1.655938
139.767274	900.271923	4.956723	-0.026434	1.663112
140.203551	908.482048	4.961728	-0.026520	1.670274
140.702255	916.663345	4.966733	-0.026618	1.677389
141.001709	924.874210	4.971738	-0.026680	1.684472
141.465110	933.066900	4.976742	-0.026771	1.691532
141.851608	941.270121	4.981747	-0.026849	1.698561
142.412752	949.430105	4.986752	-0.026958	1.705547
142.726754	957.638563	4.991757	-0.027022	1.712513
143.227835	965.802891	4.996762	-0.027121	1.719438
143.924425	973.914183	5.001766	-0.027256	1.726317
144.037384	982.177840	5.006771	-0.027282	1.733218
144.593692	990.308434	5.011776	-0.027391	1.740040
145.119065	998.467507	5.016781	-0.027495	1.746854
145.554433	1006.664199	5.021786	-0.027581	1.753661
146.020828	1014.806004	5.026790	-0.027673	1.760401
146.445087	1022.987827	5.031795	-0.027758	1.767141
146.846192	1031.164630	5.036800	-0.027838	1.773850
147.190759	1039.338062	5.041805	-0.027907	1.780522
147.801112	1047.484289	5.046810	-0.028026	1.787182
148.228897	1055.676925	5.051814	-0.028111	1.793830
148.761033	1063.793528	5.056819	-0.028216	1.800407
149.153210	1071.957381	5.061824	-0.028294	1.806979
149.573630	1080.120871	5.066829	-0.028378	1.813531
149.826278	1088.291208	5.071834	-0.028430	1.820043
150.355734	1096.395276	5.076838	-0.028534	1.826514
150.873194	1104.543573	5.081843	-0.028636	1.832996
151.386244	1112.664136	5.086848	-0.028736	1.839432
151.352475	1120.876673	5.091853	-0.028736	1.845851
151.961340	1129.006324	5.096858	-0.028854	1.852261
152.436714	1137.116591	5.101862	-0.028948	1.858617
152.539499	1145.293261	5.106867	-0.028973	1.864959
152.915132	1153.449398	5.111872	-0.029048	1.871296
153.385647	1161.551925	5.116877	-0.029141	1.877581
153.447244	1169.741078	5.121882	-0.029158	1.883863
153.975152	1177.823225	5.126886	-0.029261	1.890097
154.415734	1185.952238	5.131891	-0.029349	1.896336
154.817357	1194.085732	5.136896	-0.029429	1.902553
155.128970	1202.228269	5.141901	-0.029492	1.908747
155.757353	1210.324366	5.146906	-0.029614	1.914921
156.023520	1218.460690	5.151910	-0.029669	1.921065
156.462418	1226.580672	5.156915	-0.029756	1.927196
156.722545	1234.743908	5.161920	-0.029810	1.933320
157.486262	1242.796716	5.166925	-0.029958	1.939398
158.218960	1250.887114	5.171930	-0.030099	1.945482
158.256830	1259.088504	5.176934	-0.030112	1.951552
158.967265	1267.140082	5.181939	-0.030249	1.957566
159.608504	1275.222986	5.186944	-0.030374	1.963578
159.940973	1283.342570	5.191949	-0.030441	1.969564
160.248051	1291.508304	5.196954	-0.030504	1.975562
160.536882	1299.629099	5.201958	-0.030563	1.981508
160.776528	1307.786856	5.206963	-0.030613	1.987457
161.052430	1315.918951	5.211968	-0.030670	1.993373
161.401777	1324.014047	5.216973	-0.030740	1.999254
161.903927	1332.086648	5.221978	-0.030839	2.005117
162.232365	1340.216331	5.226982	-0.030905	2.010985
162.746443	1348.312779	5.231987	-0.031006	2.016832
163.149500	1356.414566	5.236992	-0.031087	2.022654
163.310136	1364.555726	5.241997	-0.031122	2.028462
163.823654	1372.666428	5.247002	-0.031223	2.034268
164.179601	1380.743557	5.252006	-0.031295	2.040018
164.502186	1388.853802	5.257011	-0.031360	2.045771
165.167247	1396.930940	5.262016	-0.031489	2.051520
165.840610	1404.997752	5.267021	-0.031620	2.057247
166.333875	1413.101092	5.272026	-0.031717	2.062964
166.692443	1421.230277	5.277030	-0.031789	2.068670
166.851949	1429.380131	5.282035	-0.031824	2.074354
167.200496	1437.468259	5.287040	-0.031894	2.079999
167.497977	1445.561482	5.292045	-0.031955	2.085627
167.898366	1453.684466	5.297050	-0.032035	2.091270
168.096127	1461.799037	5.302054	-0.032077	2.096873
168.669657	1469.863265	5.307059	-0.032189	2.102463
168.972248	1477.986280	5.312064	-0.032251	2.108051
169.656281	1486.050788	5.317069	-0.032383	2.113622
170.142517	1494.160277	5.322074	-0.032479	2.119190
170.534128	1502.201571	5.327078	-0.032558	2.124687
170.722270	1510.354588	5.332083	-0.032598	2.130226
171.405101	1518.407138	5.337088	-0.032730	2.135731
171.725684	1526.479612	5.342093	-0.032795	2.141200
172.232874	1534.579162	5.347098	-0.032895	2.146690
172.513666	1542.687613	5.352102	-0.032953	2.152151
173.085680	1550.739547	5.357107	-0.033064	2.157588
173.493421	1558.827818	5.362112	-0.033146	2.163020
173.608471	1566.958430	5.367117	-0.033172	2.168439
174.117535	1575.046327	5.372122	-0.033273	2.173852
174.154178	1583.186795	5.377126	-0.033285	2.179243
174.407694	1591.266353	5.382131	-0.033337	2.184600
175.081919	1599.326234	5.387136	-0.033468	2.189971
175.483804	1607.392550	5.392141	-0.033548	2.195307
175.587245	1615.512585	5.397146	-0.033573	2.200637
176.061010	1623.551128	5.402150	-0.033666	2.205936
176.749892	1631.611264	5.407155	-0.033800	2.211256
176.820680	1639.753005	5.412160	-0.033818	2.216559
177.087331	1647.822362	5.417165	-0.033873	2.221820
177.468775	1655.916357	5.422170	-0.033950	2.227096
177.686549	1664.020454	5.427174	-0.033996	2.232350
178.399578	1672.041936	5.432179	-0.034134	2.237583
178.659802	1680.136086	5.437184	-0.034187	2.242810
178.706537	1688.263654	5.442189	-0.034201	2.248027
179.137878	1696.334573	5.447194	-0.034287	2.253231
179.625217	1704.383350	5.452198	-0.034383	2.258412
180.132761	1712.437849	5.457203	-0.034483	2.263588
180.745846	1720.525711	5.462208	-0.034602	2.268782
180.838311	1728.675453	5.467213	-0.034625	2.273957
181.409489	1736.708121	5.472218	-0.034736	2.279088
181.560775	1744.773769	5.477222	-0.034770	2.284192
181.781979	1752.863768	5.482227	-0.034816	2.289306
182.378789	1760.915805	5.487232	-0.034933	2.294417
182.334607	1769.019741	5.492237	-0.034930	2.299494
182.805450	1777.073228	5.497242	-0.035023	2.304572
183.232908	1785.149800	5.502246	-0.035108	2.309650
183.497439	1793.229743	5.507251	-0.035162	2.314705
183.739530	1801.310009	5.512256	-0.035213	2.319747
184.012675	1809.335222	5.517261	-0.035269	2.324746
184.480905	1817.439573	5.522266	-0.035361	2.329800
184.810236	1825.501136	5.527270	-0.035428	2.334805
185.086507	1833.591545	5.532275	-0.035485	2.339812
185.436721	1841.648470	5.537280	-0.035555	2.344795
185.653764	1849.737108	5.542285	-0.035601	2.349775
185.862781	1857.831904	5.547290	-0.035645	2.354747
186.144246	1865.879120	5.552294	-0.035703	2.359686
186.479686	1873.931972	5.557299	-0.035771	2.364622
186.896618	1882.006521	5.562304	-0.035854	2.369568
187.324096	1890.047381	5.567309	-0.035938	2.374484
187.658207	1898.128135	5.572314	-0.036006	2.379406
187.860395	1906.194278	5.577318	-0.036049	2.384299
188.141832	1914.268016	5.582323	-0.036107	2.389192
188.449019	1922.361532	5.587328	-0.036169	2.394089
188.648348	1930.417396	5.592333	-0.036211	2.398945
188.814208	1938.492129	5.597338	-0.036248	2.403799
189.032703	1946.573648	5.602342	-0.036294	2.408652
189.724931	1954.587604	5.607347	-0.036428	2.413493
189.948864	1962.698474	5.612352	-0.036475	2.418344
190.142362	1970.739993	5.617357	-0.036516	2.423142
190.706682	1978.800610	5.622362	-0.036626	2.427971
191.039849	1986.896778	5.627366	-0.036694	2.432793
191.272895	1994.952752	5.632371	-0.036743	2.437574
191.640422	2002.988607	5.637376	-0.036816	2.442344
191.942907	2011.044255	5.642381	-0.036878	2.447111
192.368266	2019.114205	5.647386	-0.036962	2.451887
192.514091	2027.183252	5.652390	-0.036995	2.456632
193.010198	2035.215713	5.657395	-0.037092	2.461372
193.432512	2043.272095	5.662400	-0.037176	2.466112
193.568357	2051.367155	5.667405	-0.037207	2.470844
193.761645	2059.446134	5.672410	-0.037248	2.475561
194.028227	2067.490177	5.677414	-0.037303	2.480254
194.286285	2075.537010	5.682419	-0.037357	2.484940
194.739002	2083.601056	5.687424	-0.037446	2.489641
195.148300	2091.637618	5.692429	-0.037528	2.494314
195.467662	2099.706922	5.697434	-0.037592	2.498991
195.799856	2107.755133	5.702438	-0.037659	2.503647
196.335753	2115.815503	5.707443	-0.037765	2.508317
196.718640	2123.893906	5.712448	-0.037841	2.512977
196.815276	2131.959890	5.717453	-0.037864	2.517600
197.181816	2140.008086	5.722458	-0.037938	2.522224
197.486841	2148.057033	5.727462	-0.038000	2.526836
197.774732	2156.128309	5.732467	-0.038059	2.531451
198.126171	2164.205780	5.737472	-0.038130	2.536065
198.453188	2172.240159	5.742477	-0.038196	2.540645
198.966012	2180.268185	5.747482	-0.038297	2.545226
199.199731	2188.367477	5.752486	-0.038345	2.549819
199.529784	2196.398847	5.757491	-0.038412	2.554372
199.925696	2204.453562	5.762496	-0.038491	2.558935
200.249608	2212.484264	5.767501	-0.038557	2.563471
200.485871	2220.579268	5.772506	-0.038606	2.568029
200.921848	2228.631907	5.777510	-0.038693	2.572569
201.098678	2236.715991	5.782515	-0.038731	2.577100
201.355801	2244.771772	5.787520	-0.038784	2.581614
201.779718	2252.796882	5.792525	-0.038868	2.586114
202.161909	2260.902201	5.797530	-0.038945	2.590647
202.442463	2269.022672	5.802534	-0.039002	2.595174
202.901043	2276.998339	5.807539	-0.039093	2.599625
203.283864	2285.016973	5.812544	-0.039169	2.604087
203.450404	2293.058632	5.817549	-0.039206	2.608539
203.926000	2301.127853	5.822554	-0.039300	2.613020
204.328756	2309.150776	5.827558	-0.039380	2.617463
204.601595	2317.188735	5.832563	-0.039436	2.621897
204.882469	2325.251437	5.837568	-0.039493	2.626338
205.179502	2333.315395	5.842573	-0.039554	2.630773
205.464196	2341.379533	5.847578	-0.039612	2.635200
205.700917	2349.399800	5.852582	-0.039662	2.639592
205.949568	2357.450740	5.857587	-0.039713	2.643994
206.661274	2365.479802	5.862592	-0.039851	2.648409
206.970883	2373.543585	5.867597	-0.039914	2.652807
207.439420	2381.593852	5.872602	-0.040007	2.657202
207.941050	2389.612661	5.877606	-0.040105	2.661574
208.444073	2397.663878	5.882611	-0.040204	2.665957
208.823801	2405.754215	5.887616	-0.040280	2.670345
209.029892	2413.813214	5.892621	-0.040324	2.674698
209.247446	2421.867794	5.897626	-0.040370	2.679042
209.338652	2429.928311	5.902630	-0.040392	2.683373
209.768504	2437.934374	5.907635	-0.040477	2.687691
210.124344	2446.004640	5.912640	-0.040549	2.692031
210.308347	2454.071593	5.917645	-0.040588	2.696352
210.602812	2462.124717	5.922650	-0.040648	2.700665
210.771150	2470.153943	5.927654	-0.040685	2.704950
211.070925	2478.213027	5.932659	-0.040746	2.709253
211.389449	2486.289908	5.937664	-0.040811	2.713559
211.694584	2494.284713	5.942669	-0.040873	2.717814
212.147873	2502.316334	5.947674	-0.040962	2.722092
212.274997	2510.406570	5.952678	-0.040991	2.726373
212.607556	2518.451771	5.957683	-0.041059	2.730636
212.991636	2526.514851	5.962688	-0.041135	2.734906
213.104915	2534.548852	5.967693	-0.041162	2.739136
213.508569	2542.592224	5.972698	-0.041242	2.743383
213.764332	2550.658777	5.977702	-0.041295	2.747626
213.901717	2558.740101	5.982707	-0.041326	2.751863
214.379079	2566.798954	5.987712	-0.041420	2.756102
214.481621	2574.801751	5.992717	-0.041445	2.760283
215.013828	2582.793457	5.997722	-0.041549	2.764478
214.966046	2590.870395	6.002726	-0.041545	2.768675
215.111939	2598.946337	6.007731	-0.041578	2.772878
215.356608	2606.989836	6.012736	-0.041629	2.777063
215.720433	2614.990555	6.017741	-0.041702	2.781226
216.135222	2623.037387	6.022746	-0.041784	2.785411
216.319005	2631.081274	6.027750	-0.041824	2.789573
216.716851	2639.122536	6.032755	-0.041903	2.793741
216.908418	2647.184360	6.037760	-0.041944	2.797901
217.011310	2655.221821	6.042765	-0.041968	2.802037
217.553926	2663.233402	6.047770	-0.042075	2.806179
217.691585	2671.315203	6.052774	-0.042106	2.810327
217.654762	2679.397524	6.057779	-0.042104	2.814459
218.102642	2687.425138	6.062784	-0.042193	2.818586
218.324583	2695.438845	6.067789	-0.042239	2.822686
218.443014	2703.520463	6.072794	-0.042267	2.826809
218.870155	2711.559926	6.077798	-0.042352	2.830922
219.135652	2719.599786	6.082803	-0.042406	2.835020
219.536603	2727.595817	6.087808	-0.042486	2.839098
219.455666	2735.658238	6.092813	-0.042476	2.843175
219.907785	2743.679801	6.097818	-0.042566	2.847257
220.309871	2751.714521	6.102822	-0.042646	2.851336
220.335126	2759.792832	6.107827	-0.042656	2.855410
220.819203	2767.815531	6.112832	-0.042751	2.859477
221.082263	2775.825343	6.117837	-0.042806	2.863518
221.380982	2783.894233	6.122842	-0.042867	2.867585
221.617952	2791.955575	6.127846	-0.042916	2.871640
221.851471	2799.992636	6.132851	-0.042965	2.875676
222.047361	2808.046625	6.137856	-0.043006	2.879712
222.374734	2816.042749	6.142861	-0.043073	2.883722
222.550353	2824.124937	6.147866	-0.043111	2.887760
222.992281	2832.146562	6.152870	-0.043198	2.891778
223.026135	2840.222854	6.157875	-0.043210	2.895794
223.390619	2848.245037	6.162880	-0.043283	2.899796
223.745928	2856.253691	6.167885	-0.043354	2.903785
223.955823	2864.340912	6.172890	-0.043399	2.907800
223.958196	2872.466972	6.177894	-0.043405	2.911817
224.586401	2880.434038	6.182899	-0.043527	2.915784
224.812611	2888.470867	6.187904	-0.043574	2.919758
225.269965	2896.418909	6.192909	-0.043665	2.923695
225.835374	2904.453033	6.197914	-0.043775	2.927675
225.971688	2912.537510	6.202918	-0.043806	2.931652
225.795157	2920.624831	6.207923	-0.043778	2.935607
226.484525	2928.609834	6.212928	-0.043912	2.939553
226.627653	2936.641019	6.217933	-0.043944	2.943488
226.850636	2944.701793	6.222938	-0.043991	2.947436
227.065065	2952.766108	6.227942	-0.044036	2.951379
227.469335	2960.775685	6.232947	-0.044116	2.955301
227.694613	2968.809221	6.237952	-0.044164	2.959220
227.851265	2976.831414	6.242957	-0.044198	2.963124
228.147504	2984.890335	6.247962	-0.044258	2.967049
228.398467	2992.973387	6.252966	-0.044310	2.970977
228.535918	3000.987216	6.257971	-0.044341	2.974861
228.595406	3009.045244	6.262976	-0.044358	2.978757
228.704280	3017.050256	6.267981	-0.044383	2.982625
229.276625	3025.063796	6.272986	-0.044495	2.986516
229.386373	3033.155999	6.277990	-0.044521	2.990415
229.663943	3041.144617	6.282995	-0.044578	2.994269
229.779059	3049.230073	6.288000	-0.044604	2.998155
229.781956	3057.251404	6.293005	-0.044610	3.002000
229.999867	3065.279009	6.298010	-0.044656	3.005854
230.511720	3073.285078	6.303014	-0.044757	3.009708
230.805236	3081.320973	6.308019	-0.044817	3.013560
230.859908	3089.392657	6.313024	-0.044832	3.017412
231.129457	3097.434877	6.318029	-0.044888	3.021256
231.391882	3105.469195	6.323034	-0.044942	3.025091
231.390094	3113.526611	6.328038	-0.044947	3.028918
231.701938	3121.550652	6.333043	-0.045010	3.032741
232.289180	3129.567240	6.338048	-0.045125	3.036569
232.208579	3137.597015	6.343053	-0.045115	3.040365
232.476286	3145.626741	6.348058	-0.045170	3.044173
232.855928	3153.651658	6.353062	-0.045246	3.047980
232.732294	3161.745963	6.358067	-0.045228	3.051790
232.963109	3169.776915	6.363072	-0.045276	3.055583
233.052504	3177.778208	6.368077	-0.045298	3.059351
233.578417	3185.809294	6.373082	-0.045402	3.063149
233.603418	3193.892525	6.378086	-0.045411	3.066942
233.885264	3201.931893	6.383091	-0.045469	3.070722
234.436483	3209.978225	6.388096	-0.045577	3.074514
234.507309	3217.963284	6.393101	-0.045596	3.078250
234.763205	3225.983896	6.398106	-0.045648	3.082006
235.201621	3234.005756	6.403110	-0.045735	3.085767
234.988259	3242.054743	6.408115	-0.045701	3.089505
235.244842	3250.126461	6.413120	-0.045754	3.093271
235.516089	3258.140084	6.418125	-0.045810	3.097007
235.875351	3266.172072	6.423130	-0.045882	3.100751
236.143400	3274.186153	6.428134	-0.045937	3.104477
236.308048	3282.244119	6.433139	-0.045973	3.108214
236.861371	3290.250902	6.438144	-0.046081	3.111942
236.921667	3298.302508	6.443149	-0.046098	3.115662
237.142532	3306.309651	6.448154	-0.046144	3.119365
237.564784	3314.331250	6.453158	-0.046228	3.123080
237.650455	3322.378781	6.458163	-0.046249	3.126786
237.773328	3330.463452	6.463168	-0.046278	3.130507
237.916233	3338.468691	6.468173	-0.046309	3.134188
237.974378	3346.543671	6.473178	-0.046326	3.137892
238.251756	3354.564764	6.478182	-0.046382	3.141578
238.426219	3362.572877	6.483187	-0.046420	3.145248
238.730102	3370.618619	6.488192	-0.046482	3.148938
238.826758	3378.663685	6.493197	-0.046505	3.152613
239.172619	3386.684638	6.498202	-0.046575	3.156284
239.327409	3394.737403	6.503206	-0.046609	3.159957
239.650991	3402.693681	6.508211	-0.046675	3.163589
239.993725	3410.739927	6.513216	-0.046744	3.167259
240.186164	3418.806990	6.518221	-0.046785	3.170927
240.473476	3426.826637	6.523226	-0.046844	3.174573
240.802073	3434.832295	6.528230	-0.046910	3.178211
240.863615	3442.894767	6.533235	-0.046927	3.181858
241.161741	3450.931046	6.538240	-0.046988	3.185500
241.381764	3458.953792	6.543245	-0.047034	3.189128
241.609200	3467.007261	6.548250	-0.047081	3.192766
241.602566	3475.079494	6.553254	-0.047086	3.196398
241.880684	3483.061140	6.558259	-0.047143	3.199998
242.280602	3491.056880	6.563264	-0.047222	3.203605
242.531668	3499.102622	6.568269	-0.047274	3.207224
242.663723	3507.161336	6.573274	-0.047304	3.210840
243.054063	3515.176543	6.578278	-0.047382	3.214443
243.167747	3523.199431	6.583283	-0.047409	3.218034
243.459935	3531.255599	6.588288	-0.047468	3.221643
243.527830	3539.291869	6.593293	-0.047486	3.225229
243.560629	3547.340459	6.598298	-0.047498	3.228816
243.968017	3555.372339	6.603302	-0.047579	3.232407
244.138491	3563.390088	6.608307	-0.047616	3.235977
244.317379	3571.406843	6.613312	-0.047654	3.239544
244.585827	3579.419160	6.618317	-0.047709	3.243108
244.796564	3587.452908	6.623322	-0.047754	3.246676
244.971339	3595.529334	6.628326	-0.047792	3.250257
245.503208	3603.497932	6.633331	-0.047896	3.253801
245.941085	3611.531671	6.638336	-0.047983	3.257366
246.032805	3619.564922	6.643341	-0.048005	3.260912
246.319701	3627.576046	6.648346	-0.048064	3.264453
246.479711	3635.671684	6.653350	-0.048099	3.268022
246.868268	3643.664834	6.658355	-0.048177	3.271552
247.190675	3651.694982	6.663360	-0.048242	3.275091
247.256060	3659.685055	6.668365	-0.048259	3.278598
247.612092	3667.718987	6.673370	-0.048331	3.282133
247.520502	3675.797175	6.678374	-0.048319	3.285665
247.729417	3683.812886	6.683379	-0.048363	3.289177
248.176169	3691.833398	6.688384	-0.048452	3.292698
248.268989	3699.896461	6.693389	-0.048474	3.296219
248.313280	3707.925312	6.698394	-0.048488	3.299720
248.692452	3715.927256	6.703398	-0.048564	3.303219
248.914377	3723.960756	6.708403	-0.048610	3.306721
249.112426	3732.041723	6.713408	-0.048653	3.310239
249.189465	3740.048020	6.718413	-0.048672	3.313716
249.522205	3748.075037	6.723418	-0.048739	3.317209
249.842931	3756.113927	6.728422	-0.048804	3.320703
249.991412	3764.060639	6.733427	-0.048837	3.324146
250.260454	3772.127763	6.738432	-0.048893	3.327642
250.225346	3780.214037	6.743437	-0.048891	3.331131
250.424958	3788.245117	6.748442	-0.048934	3.334602
250.567074	3796.251348	6.753446	-0.048966	3.338056
250.797910	3804.253718	6.758451	-0.049014	3.341508
251.170008	3812.286126	6.763456	-0.049088	3.344975
251.044360	3820.371763	6.768461	-0.049070	3.348443
251.512407	3828.371149	6.773466	-0.049163	3.351892
251.745341	3836.388027	6.778470	-0.049211	3.355336
251.860397	3844.385665	6.783475	-0.049238	3.358764
252.494754	3852.384036	6.788480	-0.049361	3.362208
252.742356	3860.446654	6.793485	-0.049413	3.365662
252.602421	3868.482667	6.798490	-0.049392	3.369086
252.985354	3876.547982	6.803494	-0.049469	3.372539
253.006276	3884.591567	6.808499	-0.049478	3.375965
253.552486	3892.572151	6.813504	-0.049585	3.379381
253.605689	3900.591918	6.818509	-0.049600	3.382791
253.763389	3908.643908	6.823514	-0.049634	3.386216
254.220963	3916.641514	6.828518	-0.049725	3.389624
254.180841	3924.738029	6.833523	-0.049723	3.393054
254.389944	3932.789650	6.838528	-0.049767	3.396469
254.694032	3940.739432	6.843533	-0.049829	3.399842
254.721671	3948.779976	6.848538	-0.049839	3.403240
254.959185	3956.805546	6.853542	-0.049889	3.406635
255.059610	3964.821980	6.858547	-0.049913	3.410019
255.248849	3972.897500	6.863552	-0.049953	3.413427
255.417453	3980.933192	6.868557	-0.049990	3.416814
255.716434	3988.927317	6.873562	-0.050051	3.420185
255.925136	3996.951199	6.878566	-0.050095	3.423561
256.129456	4004.946991	6.883571	-0.050138	3.426923
256.382063	4013.001851	6.888576	-0.050191	3.430307
256.542428	4021.033699	6.893581	-0.050226	3.433676
256.788613	4029.059647	6.898586	-0.050277	3.437041
256.947886	4037.096322	6.903590	-0.050312	3.440405
257.222097	4045.034141	6.908595	-0.050368	3.443728
257.469438	4053.134030	6.913600	-0.050419	3.447114
257.697969	4061.166339	6.918605	-0.050467	3.450469
257.543948	4069.214803	6.923610	-0.050444	3.453813
257.890085	4077.238945	6.928614	-0.050514	3.457162
258.086086	4085.254011	6.933619	-0.050555	3.460498
258.712705	4093.202577	6.938624	-0.050677	3.463818
258.996969	4101.247255	6.943629	-0.050735	3.467163
259.246034	4109.341165	6.948634	-0.050787	3.470523
259.372816	4117.349553	6.953638	-0.050816	3.473841
259.349453	4125.373285	6.958643	-0.050817	3.477158
259.527095	4133.423986	6.963648	-0.050855	3.480489
259.794749	4141.371527	6.968653	-0.050910	3.483777
259.644300	4149.492155	6.973658	-0.050888	3.487119
260.375731	4157.465621	6.978662	-0.051029	3.490427
260.528546	4165.498587	6.983667	-0.051063	3.493737
260.725946	4173.563051	6.988672	-0.051105	3.497058
261.100447	4181.529907	6.993677	-0.051180	3.500342
261.454263	4189.515965	6.998682	-0.051251	3.503629
261.564671	4197.606706	7.003686	-0.051277	3.506949
261.520708	4205.692956	7.008691	-0.051274	3.510259
261.837419	4213.681285	7.013696	-0.051338	3.513537
261.860265	4221.721728	7.018701	-0.051348	3.516824
261.931507	4229.722313	7.023706	-0.051366	3.520093
262.231916	4237.720106	7.028710	-0.051427	3.523365
262.636038	4245.719686	7.033715	-0.051508	3.526638
262.617051	4253.825795	7.038720	-0.051510	3.529938
262.792490	4261.832254	7.043725	-0.051548	3.533200
263.408895	4269.847406	7.048730	-0.051668	3.536477
263.584081	4277.851286	7.053734	-0.051705	3.539733
263.532941	4285.876980	7.058739	-0.051701	3.542987
263.951845	4293.957146	7.063744	-0.051784	3.546274
264.112726	4301.953708	7.068749	-0.051820	3.549517
264.259520	4310.030548	7.073754	-0.051852	3.552789
264.556376	4318.070232	7.078758	-0.051913	3.556048
264.797122	4326.003350	7.083763	-0.051963	3.559258
265.113114	4334.032496	7.088768	-0.052027	3.562507
265.196340	4342.075116	7.093773	-0.052048	3.565751
265.467461	4350.057400	7.098778	-0.052104	3.568974
265.741153	4358.128356	7.103782	-0.052160	3.572229
265.829184	4366.122837	7.108787	-0.052181	3.575445
266.081126	4374.158174	7.113792	-0.052234	3.578679
266.151495	4382.191114	7.118797	-0.052252	3.581904
266.520578	4390.171673	7.123802	-0.052326	3.585114
266.962373	4398.208749	7.128806	-0.052413	3.588346
267.278553	4406.251663	7.133811	-0.052478	3.591574
267.416303	4414.307342	7.138816	-0.052509	3.594798
267.705238	4422.297396	7.143821	-0.052568	3.597998
267.857922	4430.330550	7.148826	-0.052601	3.601208
268.323719	4438.291578	7.153830	-0.052693	3.604396
268.289998	4446.363060	7.158835	-0.052692	3.607610
268.705022	4454.421554	7.163840	-0.052775	3.610829
268.796313	4462.442647	7.168845	-0.052797	3.614021
268.830884	4470.493865	7.173850	-0.052809	3.617220
269.319459	4478.511511	7.178854	-0.052905	3.620416
269.329691	4486.510345	7.183859	-0.052912	3.623589
269.434579	4494.591373	7.188864	-0.052937	3.626793
269.608736	4502.597308	7.193869	-0.052975	3.629968
269.901107	4510.631093	7.198874	-0.053034	3.633153
270.319073	4518.627534	7.203878	-0.053118	3.636325
270.475375	4526.614972	7.208883	-0.053152	3.639483
270.499936	4534.636991	7.213888	-0.053162	3.642648
270.920594	4542.664903	7.218893	-0.053245	3.645824
270.916606	4550.684786	7.223898	-0.053250	3.648981
270.855351	4558.801392	7.228902	-0.053244	3.652173
271.228232	4566.759515	7.233907	-0.053318	3.655312
271.075449	4574.805998	7.238912	-0.053295	3.658468
271.494689	4582.767684	7.243917	-0.053379	3.661603
271.908568	4590.794122	7.248922	-0.053461	3.664762
272.176496	4598.835421	7.253926	-0.053516	3.667919
272.245701	4606.879183	7.258931	-0.053534	3.671069
272.645831	4614.881482	7.263936	-0.053614	3.674209
272.766371	4622.914062	7.268941	-0.053642	3.677351
272.793506	4630.941584	7.273946	-0.053652	3.680485
273.129649	4638.917176	7.278950	-0.053720	3.683605
273.160344	4646.983054	7.283955	-0.053731	3.686749
273.735802	4654.975437	7.288960	-0.053843	3.689877
273.833676	4663.016918	7.293965	-0.053867	3.693008
274.013652	4671.089448	7.298970	-0.053906	3.696150
274.314724	4679.069889	7.303974	-0.053967	3.699258
274.458906	4687.114422	7.308979	-0.053999	3.702383
274.885990	4695.140398	7.313984	-0.054084	3.705506
275.052891	4703.160918	7.318989	-0.054120	3.708617
275.034391	4711.262757	7.323994	-0.054122	3.711753
275.317696	4719.281917	7.328998	-0.054180	3.714861
275.614637	4727.237509	7.334003	-0.054241	3.717943
275.957491	4735.309253	7.339008	-0.054310	3.721068
275.859553	4743.262358	7.344013	-0.054297	3.724134
275.943555	4751.322656	7.349018	-0.054318	3.727243
276.493072	4759.308935	7.354022	-0.054425	3.730332
276.259758	4767.362169	7.359027	-0.054387	3.733425
276.708761	4775.383219	7.364032	-0.054476	3.736520
277.009161	4783.376061	7.369037	-0.054537	3.739598
276.976190	4791.435462	7.374042	-0.054536	3.742691
277.222222	4799.482694	7.379046	-0.054587	3.745783
277.488924	4807.432664	7.384051	-0.054642	3.748836
277.652276	4815.509259	7.389056	-0.054678	3.751933
277.593565	4823.534969	7.394061	-0.054672	3.755002
277.700341	4831.525621	7.399066	-0.054697	3.758059
278.123063	4839.592695	7.404070	-0.054781	3.761150
278.157133	4847.517734	7.409075	-0.054793	3.764175
278.346166	4855.607288	7.414080	-0.054833	3.767264
278.689521	4863.588101	7.419085	-0.054903	3.770313
279.002926	4871.593002	7.424090	-0.054966	3.773368
279.256784	4879.694479	7.429094	-0.055019	3.776456
279.269397	4887.634510	7.434099	-0.055026	3.779474
279.501363	4895.673343	7.439104	-0.055075	3.782532
279.638227	4903.720576	7.444109	-0.055106	3.785589
279.764936	4911.742057	7.449114	-0.055134	3.788633
279.775122	4919.844016	7.454118	-0.055142	3.791703
280.308440	4927.743009	7.459123	-0.055246	3.794705
280.214768	4935.839669	7.464128	-0.055234	3.797765
280.689479	4943.851099	7.469133	-0.055328	3.800804
280.910931	4951.780354	7.474138	-0.055374	3.803803
281.048158	4959.880838	7.479142	-0.055405	3.806863
281.115908	4967.891040	7.484147	-0.055423	3.809884
281.332588	4975.940944	7.489152	-0.055468	3.812922
281.425578	4983.970781	7.494157	-0.055491	3.815946
281.764333	4991.933358	7.499162	-0.055559	3.818949
281.908736	4999.997066	7.504166	-0.055592	3.821983
281.876739	5007.980433	7.509171	-0.055591	3.824980
282.124381	5016.076665	7.514176	-0.055642	3.828023
282.520592	5024.120692	7.519181	-0.055721	3.831048
282.911926	5032.046485	7.524186	-0.055799	3.834025
282.722986	5040.168716	7.529190	-0.055770	3.837062
283.229018	5048.093803	7.534195	-0.055869	3.840037
283.295603	5056.130285	7.539200	-0.055887	3.843042
283.327323	5064.195192	7.544205	-0.055898	3.846054
283.465429	5072.194156	7.549210	-0.055929	3.849042
284.011334	5080.216901	7.554214	-0.056036	3.852045
284.253322	5088.214180	7.559219	-0.056086	3.855030
284.463213	5096.295118	7.564224	-0.056130	3.858042
284.563326	5104.333329	7.569229	-0.056154	3.861034
284.882324	5112.259482	7.574234	-0.056219	3.863987
285.194212	5120.338570	7.579238	-0.056282	3.866994
285.153290	5128.379245	7.584243	-0.056280	3.869977
285.562038	5136.494255	7.589248	-0.056361	3.872995
285.539314	5144.515267	7.594253	-0.056362	3.875967
285.453824	5152.407603	7.599258	-0.056352	3.878887
286.053306	5160.444922	7.604262	-0.056469	3.881873
286.072494	5168.392540	7.609267	-0.056477	3.884811
286.225136	5176.482531	7.614272	-0.056511	3.887803
286.356325	5184.481859	7.619277	-0.056541	3.890758
286.185352	5192.553068	7.624282	-0.056514	3.893731
286.619509	5200.489584	7.629286	-0.056600	3.896665
286.894219	5208.494413	7.634291	-0.056657	3.899619
286.966590	5216.576709	7.639296	-0.056675	3.902594
287.421381	5224.545944	7.644301	-0.056765	3.905534
287.528027	5232.543599	7.649306	-0.056790	3.908474
287.883772	5240.622389	7.654310	-0.056862	3.911447
288.249227	5248.569049	7.659315	-0.056935	3.914370
288.302184	5256.651829	7.664320	-0.056950	3.917334
288.521258	5264.668819	7.669325	-0.056997	3.920275
288.803327	5272.651898	7.674330	-0.057054	3.923202
289.053055	5280.743540	7.679334	-0.057106	3.926167
289.124375	5288.699551	7.684339	-0.057125	3.929076
289.262504	5296.804229	7.689344	-0.057156	3.932038
289.400139	5304.832951	7.694349	-0.057187	3.934971
289.465107	5312.814986	7.699354	-0.057204	3.937883
289.689396	5320.883837	7.704358	-0.057251	3.940827
289.929350	5328.811338	7.709363	-0.057301	3.943718
289.936413	5336.922431	7.714368	-0.057307	3.946669
289.964176	5344.950063	7.719373	-0.057318	3.949588
290.150862	5352.961774	7.724378	-0.057358	3.952502
290.327263	5361.015282	7.729382	-0.057396	3.955429
290.522027	5368.956816	7.734387	-0.057438	3.958314
290.750447	5377.050726	7.739392	-0.057485	3.961252
290.898104	5384.963400	7.744397	-0.057518	3.964120
290.875908	5393.020683	7.749402	-0.057519	3.967036
291.462635	5401.034484	7.754406	-0.057634	3.969946
291.792940	5409.061128	7.759411	-0.057700	3.972852
291.984852	5417.106710	7.764416	-0.057742	3.975761
291.830474	5425.137288	7.769421	-0.057718	3.978657
292.205281	5433.158900	7.774426	-0.057793	3.981556
292.350957	5441.105877	7.779430	-0.057825	3.984423
292.396169	5449.163287	7.784435	-0.057839	3.987325
292.577956	5457.219959	7.789440	-0.057878	3.990227
292.837145	5465.220641	7.794445	-0.057932	3.993108
292.674918	5473.285772	7.799450	-0.057907	3.996003
292.940064	5481.216141	7.804454	-0.057961	3.998855
292.797134	5489.306719	7.809459	-0.057940	4.001756
293.255905	5497.254257	7.814464	-0.058031	4.004613
293.274165	5505.332293	7.819469	-0.058039	4.007507
293.363004	5513.320381	7.824474	-0.058061	4.010369
293.779203	5521.327635	7.829478	-0.058144	4.013240
293.829154	5529.385913	7.834483	-0.058159	4.016122
294.012051	5537.372120	7.839488	-0.058198	4.018978
294.320133	5545.378400	7.844493	-0.058261	4.021841
294.366575	5553.376358	7.849498	-0.058274	4.024695
294.680803	5561.475452	7.854502	-0.058338	4.027587
294.830272	5569.468823	7.859507	-0.058371	4.030437
295.198204	5577.523752	7.864512	-0.058445	4.033310
295.525676	5585.521454	7.869517	-0.058511	4.036160
295.878745	5593.481620	7.874522	-0.058582	4.038995
296.231601	5601.554817	7.879526	-0.058653	4.041868
296.230678	5609.492286	7.884531	-0.058658	4.044686
296.564950	5617.553279	7.889536	-0.058726	4.047550
296.798963	5625.576128	7.894541	-0.058775	4.050397
297.070717	5633.587184	7.899546	-0.058831	4.053239
296.877651	5641.720661	7.904550	-0.058800	4.056115
297.254070	5649.596420	7.909555	-0.058875	4.058906
297.515349	5657.658641	7.914560	-0.058929	4.061760
297.794933	5665.648037	7.919565	-0.058987	4.064586
297.860971	5673.713425	7.924570	-0.059004	4.067433
297.897755	5681.791075	7.929574	-0.059016	4.070283
298.009776	5689.757754	7.934579	-0.059042	4.073092
298.316934	5697.803230	7.939584	-0.059105	4.075930
298.633804	5705.806119	7.944589	-0.059169	4.078752
298.650047	5713.831858	7.949594	-0.059177	4.081575
298.837559	5721.831956	7.954598	-0.059218	4.084389
299.083632	5729.860101	7.959603	-0.059269	4.087212
299.389715	5737.883392	7.964608	-0.059331	4.090033
299.383629	5745.926221	7.969613	-0.059335	4.092853
299.607793	5753.956169	7.974618	-0.059382	4.095671
299.828853	5761.937482	7.979622	-0.059428	4.098470
299.855168	5769.982298	7.984627	-0.059439	4.101286
300.004590	5777.951743	7.989632	-0.059472	4.104075
300.273045	5786.037115	7.994637	-0.059527	4.106905
300.318419	5794.040624	7.999642	-0.059541	4.109701
300.396106	5802.078734	8.004646	-0.059560	4.112508
300.763957	5810.044510	8.009651	-0.059634	4.115291
300.817082	5818.086607	8.014656	-0.059649	4.118095
301.064213	5826.104114	8.019661	-0.059701	4.120891
301.269936	5834.043573	8.024666	-0.059744	4.123658
301.325286	5842.168534	8.029670	-0.059760	4.126485
301.481572	5850.108280	8.034675	-0.059794	4.129247
301.815768	5858.175969	8.039680	-0.059862	4.132054
302.029084	5866.199082	8.044685	-0.059907	4.134842
302.257746	5874.193806	8.049690	-0.059954	4.137618
302.290778	5882.213195	8.054694	-0.059966	4.140398
302.328660	5890.179213	8.059699	-0.059978	4.143159
302.827953	5898.233233	8.064704	-0.060076	4.145953
302.992108	5906.245043	8.069709	-0.060112	4.148727
303.121736	5914.315976	8.074714	-0.060142	4.151519
303.443470	5922.306602	8.079718	-0.060207	4.154284
303.536319	5930.286755	8.084723	-0.060229	4.157041
303.515951	5938.330734	8.089728	-0.060231	4.159816
303.596788	5946.351916	8.094733	-0.060251	4.162582
304.012244	5954.324572	8.099738	-0.060334	4.165335
304.167066	5962.405559	8.104742	-0.060368	4.168119
304.334314	5970.431672	8.109747	-0.060404	4.170883
304.521794	5978.426132	8.114752	-0.060444	4.173635
304.667307	5986.501972	8.119757	-0.060477	4.176412
304.561802	5994.453941	8.124762	-0.060462	4.179141
305.012555	6002.484244	8.129766	-0.060552	4.181903
305.204160	6010.489996	8.134771	-0.060592	4.184651
305.397209	6018.547518	8.139776	-0.060634	4.187415
305.471427	6026.566253	8.144781	-0.060653	4.190162
305.660659	6034.636499	8.149786	-0.060693	4.192926
305.810144	6042.722652	8.154790	-0.060726	4.195694
306.026320	6050.624643	8.159795	-0.060772	4.198398
306.206404	6058.681153	8.164800	-0.060811	4.201152
306.244810	6066.647183	8.169805	-0.060823	4.203872
306.238752	6074.674813	8.174810	-0.060827	4.206610
306.632230	6082.698927	8.179814	-0.060906	4.209351
306.701993	6090.725429	8.184819	-0.060924	4.212086
306.856699	6098.757135	8.189824	-0.060958	4.214823
307.140255	6106.742180	8.194829	-0.061016	4.217543
307.410158	6114.743052	8.199834	-0.061072	4.220266
307.673169	6122.759544	8.204838	-0.061126	4.222994
307.572590	6130.808675	8.209843	-0.061112	4.225726
307.936301	6138.826956	8.214848	-0.061185	4.228451
308.085398	6146.889622	8.219853	-0.061218	4.231187
307.780256	6154.895461	8.224858	-0.061167	4.233897
308.060186	6162.921120	8.229862	-0.061224	4.236619
308.174784	6170.847436	8.234867	-0.061251	4.239303
308.349690	6178.916358	8.239872	-0.061289	4.242035
308.557741	6186.901779	8.244877	-0.061333	4.244736
308.725147	6194.935222	8.249882	-0.061369	4.247452
309.004158	6202.968635	8.254886	-0.061426	4.250167
308.785137	6211.025151	8.259891	-0.061391	4.252884
308.843552	6219.090437	8.264896	-0.061407	4.255604
309.519888	6226.973790	8.269901	-0.061538	4.258267
309.615998	6235.010332	8.274906	-0.061561	4.260975
309.763299	6243.017118	8.279910	-0.061594	4.263671
309.762010	6251.081674	8.284915	-0.061599	4.266383
310.273641	6259.046326	8.289920	-0.061700	4.269065
310.246018	6267.172169	8.294925	-0.061700	4.271794
310.390578	6275.093596	8.299930	-0.061732	4.274455
310.699869	6283.151240	8.304934	-0.061795	4.277161
310.443553	6291.144433	8.309939	-0.061752	4.279839
310.501760	6299.179365	8.314944	-0.061768	4.282531
310.987700	6307.178532	8.319949	-0.061864	4.285214
311.214676	6315.146234	8.324954	-0.061912	4.287883
311.262251	6323.254674	8.329958	-0.061926	4.290595
311.390869	6331.269811	8.334963	-0.061955	4.293275
311.384571	6339.298351	8.339968	-0.061959	4.295956
311.801216	6347.253154	8.344973	-0.062042	4.298615
311.774135	6355.306376	8.349978	-0.062042	4.301301
312.190727	6363.268538	8.354982	-0.062125	4.303960
312.231884	6371.346930	8.359987	-0.062138	4.306651
312.346500	6379.335621	8.364992	-0.062165	4.309312
312.932596	6387.319876	8.369997	-0.062279	4.311974
313.117402	6395.292416	8.375002	-0.062319	4.314627
313.422378	6403.377759	8.380006	-0.062381	4.317316
313.556830	6411.335319	8.385011	-0.062411	4.319960
313.824893	6419.367839	8.390016	-0.062466	4.322629
314.052211	6427.395160	8.395021	-0.062514	4.325293
314.274464	6435.387148	8.400026	-0.062560	4.327945
314.512740	6443.449725	8.405030	-0.062610	4.330618
314.429928	6451.467686	8.410035	-0.062600	4.333272
314.564408	6459.514535	8.415040	-0.062630	4.335935
314.819641	6467.500220	8.420045	-0.062683	4.338578
314.995802	6475.517337	8.425050	-0.062721	4.341229
315.115262	6483.514297	8.430054	-0.062748	4.343871
315.082102	6491.568011	8.435059	-0.062748	4.346529
315.227416	6499.603568	8.440064	-0.062780	4.349181
315.194921	6507.676611	8.445069	-0.062779	4.351842
315.355289	6515.640231	8.450074	-0.062814	4.354467
315.574887	6523.702232	8.455078	-0.062860	4.357124
315.686061	6531.611297	8.460083	-0.062886	4.359727
315.833310	6539.587961	8.465088	-0.062919	4.362351
316.347603	6547.623157	8.470093	-0.063020	4.364996
316.189485	6555.666740	8.475098	-0.062996	4.367637
316.566334	6563.674046	8.480102	-0.063071	4.370268
316.810049	6571.672063	8.485107	-0.063122	4.372894
316.948974	6579.743899	8.490112	-0.063153	4.375541
317.159438	6587.728635	8.495117	-0.063197	4.378159
317.075863	6595.799726	8.500122	-0.063187	4.380801
317.361513	6603.747787	8.505126	-0.063246	4.383405
317.369384	6611.815239	8.510131	-0.063252	4.386043
317.444821	6619.829820	8.515136	-0.063272	4.388664
317.965088	6627.887122	8.520141	-0.063374	4.391299
318.215172	6635.862080	8.525146	-0.063426	4.393904
318.267624	6643.961590	8.530150	-0.063441	4.396548
318.128237	6651.923222	8.535155	-0.063420	4.399143
318.810370	6659.887036	8.540160	-0.063552	4.401743
319.123937	6667.845635	8.545165	-0.063616	4.404337
319.504940	6675.908520	8.550170	-0.063692	4.406963
319.932046	6683.958233	8.555174	-0.063777	4.409585
319.639307	6692.006099	8.560179	-0.063728	4.412199
319.748837	6700.032982	8.565184	-0.063753	4.414808
319.971646	6708.105885	8.570189	-0.063800	4.417431
320.027734	6716.079864	8.575194	-0.063816	4.420019
320.175327	6724.145503	8.580199	-0.063849	4.422636
320.263217	6732.202585	8.585203	-0.063870	4.425248
320.277497	6740.212729	8.590208	-0.063878	4.427843
320.798774	6748.220800	8.595213	-0.063980	4.430439
320.865728	6756.211585	8.600218	-0.063998	4.433025
321.085696	6764.235403	8.605223	-0.064044	4.435621
320.960985	6772.233021	8.610227	-0.064026	4.438205
321.090429	6780.296832	8.615232	-0.064056	4.440810
321.331167	6788.232066	8.620237	-0.064106	4.443373
321.677573	6796.254505	8.625242	-0.064176	4.445963
322.026958	6804.286564	8.630247	-0.064246	4.448554
322.148254	6812.372568	8.635251	-0.064274	4.451161
321.957451	6820.376064	8.640256	-0.064244	4.453737
322.140775	6828.472540	8.645261	-0.064283	4.456344
321.882440	6836.368843	8.650266	-0.064240	4.458883
322.427539	6844.397497	8.655271	-0.064347	4.461467
322.647010	6852.308477	8.660275	-0.064393	4.464010
322.704502	6860.360611	8.665280	-0.064409	4.466596
322.925447	6868.479333	8.670285	-0.064455	4.469202
323.053287	6876.447444	8.675290	-0.064484	4.471758
323.271484	6884.453016	8.680295	-0.064530	4.474326
323.523364	6892.468668	8.685299	-0.064582	4.476895
323.810548	6900.487581	8.690304	-0.064641	4.479464
323.919920	6908.522365	8.695309	-0.064667	4.482035
323.756493	6916.473600	8.700314	-0.064642	4.484577
323.940777	6924.557679	8.705319	-0.064681	4.487162
324.185594	6932.525486	8.710323	-0.064732	4.489708
324.247437	6940.584332	8.715328	-0.064749	4.492282
324.786730	6948.632164	8.720333	-0.064855	4.494852
324.650651	6956.651880	8.725338	-0.064835	4.497409
325.039253	6964.662017	8.730343	-0.064912	4.499963
325.049913	6972.650909	8.735347	-0.064919	4.502508
325.264283	6980.627268	8.740352	-0.064965	4.505048
325.377074	6988.635873	8.745357	-0.064991	4.507596
325.426227	6996.675307	8.750362	-0.065005	4.510153
325.792297	7004.693258	8.755367	-0.065079	4.512702
325.869333	7012.715073	8.760371	-0.065098	4.515250
326.150921	7020.700929	8.765376	-0.065156	4.517786
326.235313	7028.739700	8.770381	-0.065177	4.520337
326.101717	7036.745875	8.775386	-0.065157	4.522875
326.416610	7044.789472	8.780391	-0.065221	4.525425
326.557618	7052.737884	8.785395	-0.065253	4.527943
326.791486	7060.817156	8.790400	-0.065302	4.530501
327.051447	7068.821882	8.795405	-0.065355	4.533035
327.100708	7076.852888	8.800410	-0.065370	4.535574
327.149165	7084.843958	8.805415	-0.065384	4.538099
327.187488	7092.915732	8.810419	-0.065396	4.540649
327.326564	7100.877424	8.815424	-0.065427	4.543162
327.343845	7108.868370	8.820429	-0.065436	4.545683
327.878169	7116.876351	8.825434	-0.065541	4.548210
328.278117	7124.900983	8.830439	-0.065620	4.550740
328.292122	7132.937236	8.835443	-0.065628	4.553271
328.448099	7140.950102	8.840448	-0.065663	4.555793
328.673275	7148.953066	8.845453	-0.065710	4.558311
328.484630	7156.968518	8.850458	-0.065680	4.560831
328.791590	7164.936145	8.855463	-0.065742	4.563336
328.932658	7173.016802	8.860467	-0.065774	4.565874
329.042664	7180.997764	8.865472	-0.065800	4.568379
329.143986	7189.109634	8.870477	-0.065824	4.570924
329.578643	7196.992912	8.875482	-0.065910	4.573397
329.702164	7205.094788	8.880487	-0.065938	4.575936
329.797801	7213.056805	8.885491	-0.065961	4.578430
329.913253	7221.150795	8.890496	-0.065988	4.580964
329.690998	7229.128397	8.895501	-0.065952	4.583459
329.714393	7237.138927	8.900506	-0.065962	4.585964
329.788905	7245.193564	8.905511	-0.065981	4.588481
330.332607	7253.194365	8.910515	-0.066087	4.590981
330.311569	7261.160396	8.915520	-0.066088	4.593468
330.496040	7269.250927	8.920525	-0.066128	4.595992
330.704562	7277.206675	8.925530	-0.066172	4.598473
331.081109	7285.255296	8.930535	-0.066248	4.600982
331.311846	7293.143612	8.935539	-0.066296	4.603439
331.158493	7301.263383	8.940544	-0.066272	4.605967
331.580628	7309.251026	8.945549	-0.066356	4.608453
331.543267	7317.284865	8.950554	-0.066355	4.610951
331.832632	7325.286855	8.955559	-0.066414	4.613438
332.022579	7333.272467	8.960563	-0.066454	4.615919
332.055594	7341.251826	8.965568	-0.066466	4.618396
331.917123	7349.453319	8.970573	-0.066445	4.620941
332.034735	7357.349537	8.975578	-0.066472	4.623390
332.586923	7365.433420	8.980583	-0.066581	4.625896
332.561589	7373.414188	8.985587	-0.066581	4.628368
332.846777	7381.426905	8.990592	-0.066639	4.630849
332.840630	7389.464687	8.995597	-0.066644	4.633336
332.734283	7397.492798	9.000602	-0.066629	4.635819
333.086273	7405.416530	9.005607	-0.066700	4.638269
333.283099	7413.495359	9.010611	-0.066742	4.640765
333.780005	7421.378134	9.015616	-0.066839	4.643199
334.009843	7429.501178	9.020621	-0.066888	4.645706
333.756005	7437.512486	9.025626	-0.066846	4.648177
333.737867	7445.585650	9.030631	-0.066848	4.650666
334.162544	7453.528327	9.035635	-0.066932	4.653113
334.487080	7461.534156	9.040640	-0.066997	4.655579
335.018423	7469.577919	9.045645	-0.067102	4.658055
334.744199	7477.605432	9.050650	-0.067056	4.660524
334.795954	7485.664769	9.055655	-0.067071	4.663002
335.192740	7493.611879	9.060659	-0.067150	4.665444
335.247174	7501.654436	9.065664	-0.067165	4.667914
335.370476	7509.668819	9.070669	-0.067194	4.670374
335.620185	7517.728391	9.075674	-0.067245	4.672847
336.038947	7525.751892	9.080679	-0.067329	4.675307
336.256860	7533.704004	9.085683	-0.067374	4.677744
336.325975	7541.683489	9.090688	-0.067393	4.680188
336.307169	7549.700638	9.095693	-0.067394	4.682643
336.444416	7557.697890	9.100698	-0.067425	4.685090
336.628600	7565.743417	9.105703	-0.067465	4.687550
337.026744	7573.781610	9.110707	-0.067544	4.690007
336.986705	7581.764566	9.115712	-0.067542	4.692446
337.255122	7589.793586	9.120717	-0.067597	4.694897
337.017672	7597.815949	9.125722	-0.067558	4.697346
337.511432	7605.804143	9.130727	-0.067655	4.699782
337.593109	7613.847331	9.135731	-0.067676	4.702234
337.442234	7621.865117	9.140736	-0.067653	4.704677
337.900131	7629.904989	9.145741	-0.067744	4.707125
338.013987	7637.856395	9.150746	-0.067770	4.709545
338.219003	7645.930409	9.155751	-0.067813	4.712002
338.437617	7653.959492	9.160755	-0.067859	4.714443
338.409785	7662.032692	9.165760	-0.067860	4.716896
338.434066	7670.044567	9.170765	-0.067869	4.719330
338.401348	7677.941998	9.175770	-0.067868	4.721728
338.657827	7685.916070	9.180775	-0.067921	4.724147
338.819481	7694.006020	9.185779	-0.067957	4.726600
338.904352	7701.945252	9.190784	-0.067978	4.729006
339.291486	7710.030622	9.195789	-0.068055	4.731455
339.196180	7717.972875	9.200794	-0.068043	4.733861
339.416872	7726.126550	9.205799	-0.068089	4.736328
339.395555	7734.119817	9.210803	-0.068090	4.738746
339.439466	7742.227107	9.215808	-0.068104	4.741197
339.663487	7750.133228	9.220813	-0.068151	4.743586
339.867697	7758.175625	9.225818	-0.068194	4.746014
340.342495	7766.222207	9.230823	-0.068288	4.748442
340.300351	7774.282542	9.235827	-0.068285	4.750874
340.554968	7782.189887	9.240832	-0.068338	4.753258
340.715789	7790.293251	9.245837	-0.068373	4.755700
340.555337	7798.247862	9.250842	-0.068348	4.758097
340.967930	7806.260068	9.255847	-0.068431	4.760508
340.900937	7814.256749	9.260851	-0.068423	4.762915
341.139932	7822.293412	9.265856	-0.068473	4.765332
341.404895	7830.320988	9.270861	-0.068528	4.767745
341.649772	7838.301630	9.275866	-0.068579	4.770142
341.943855	7846.362761	9.280871	-0.068639	4.772562
342.077750	7854.367252	9.285875	-0.068669	4.774965
341.789287	7862.405998	9.290880	-0.068620	4.777377
342.378697	7870.394048	9.295885	-0.068735	4.779771
342.369984	7878.416645	9.300890	-0.068739	4.782175
342.526741	7886.401238	9.305895	-0.068773	4.784567
342.505921	7894.492292	9.310899	-0.068775	4.786990
342.680785	7902.483139	9.315904	-0.068813	4.789380
342.802387	7910.556808	9.320909	-0.068841	4.791795
343.139940	7918.436488	9.325914	-0.068909	4.794150
343.553774	7926.527975	9.330919	-0.068991	4.796566
343.756619	7934.481139	9.335923	-0.069034	4.798941
343.797301	7942.537878	9.340928	-0.069047	4.801345
344.057887	7950.491433	9.345933	-0.069101	4.803718
344.015776	7958.557366	9.350938	-0.069098	4.806123
344.233854	7966.544659	9.355943	-0.069144	4.808503
344.400612	7974.635981	9.360947	-0.069180	4.810913
344.586132	7982.561776	9.365952	-0.069220	4.813272
344.670580	7990.037993	9.370957	-0.069241	4.815497
344.442938	7994.748869	9.375962	-0.069201	4.816899

344.929554	7997.023496	9.380967	-0.069293	4.817574
344.960585	7998.578586	9.385971	-0.069300	4.818036
345.147652	7999.504916	9.390976	-0.069336	4.818311
345.356818	7999.611627	9.395981	-0.069375	4.818342
345.367687	8000.355103	9.400986	-0.069377	4.818563
345.503105	8000.297057	9.405991	-0.069403	4.818545
345.363300	8000.234309	9.410995	-0.069377	4.818527
345.494832	8000.328450	9.416000	-0.069401	4.818555
345.585992	8000.265617	9.421005	-0.069418	4.818536
345.576727	8000.324293	9.426010	-0.069416	4.818553
345.931947	8000.281762	9.431015	-0.069483	4.818539
345.496420	8000.082801	9.436019	-0.069401	4.818482
345.414698	8000.146815	9.441024	-0.069386	4.818501
345.715412	8000.145556	9.446029	-0.069442	4.818499
345.912452	8000.236367	9.451034	-0.069479	4.818526
345.879365	8000.282128	9.456039	-0.069473	4.818539
345.823643	8000.178498	9.461043	-0.069463	4.818509
345.767351	8000.125258	9.466048	-0.069452	4.818493
346.223686	8000.108216	9.471053	-0.069537	4.818486
346.190494	8000.146626	9.476058	-0.069531	4.818498
346.382332	8000.189072	9.481063	-0.069567	4.818510
346.312590	8000.310992	9.486067	-0.069554	4.818546
346.447013	8000.200435	9.491072	-0.069579	4.818513
346.578196	8000.169630	9.496077	-0.069603	4.818503
346.665621	8000.283138	9.501082	-0.069620	4.818536
346.469486	8000.071599	9.506087	-0.069583	4.818474
346.154879	8000.137773	9.511091	-0.069525	4.818495
346.614938	8000.179578	9.516096	-0.069610	4.818506
346.778021	8000.256292	9.521101	-0.069641	4.818528
346.658984	8000.210617	9.526106	-0.069619	4.818515
346.680524	8000.218255	9.531111	-0.069623	4.818517
346.821711	8000.195983	9.536115	-0.069649	4.818510
346.820123	8000.157116	9.541120	-0.069649	4.818498
347.033709	8000.213502	9.546125	-0.069689	4.818514
347.092952	8000.302488	9.551130	-0.069700	4.818541
346.923815	8000.206799	9.556135	-0.069668	4.818513
346.996725	8000.290716	9.561139	-0.069682	4.818537
346.909131	8000.348353	9.566144	-0.069666	4.818555
347.173696	8000.285721	9.571149	-0.069715	4.818535
346.977746	8000.275773	9.576154	-0.069678	4.818533
347.052207	8000.096172	9.581159	-0.069692	4.818479
347.385911	8000.272798	9.586163	-0.069754	4.818531
346.926562	8000.165906	9.591168	-0.069669	4.818501
347.079641	7999.934852	9.596173	-0.069697	4.818431
347.057436	8000.194947	9.601178	-0.069693	4.818509
347.295620	8000.162414	9.606183	-0.069738	4.818498
347.060039	8000.180288	9.611187	-0.069694	4.818504
347.152341	8000.412508	9.616192	-0.069711	4.818573
347.341726	8000.197683	9.621197	-0.069746	4.818508
347.035027	8000.197813	9.626202	-0.069689	4.818510
347.217246	8000.226484	9.631207	-0.069723	4.818517
347.520711	8000.180118	9.636211	-0.069780	4.818502
347.557423	8000.194258	9.641216	-0.069787	4.818507
347.453833	8000.181335	9.646221	-0.069768	4.818503
347.439118	8000.165393	9.651226	-0.069765	4.818498
347.509950	8000.116988	9.656231	-0.069778	4.818484
347.429796	8000.234573	9.661235	-0.069763	4.818519
347.511216	8000.087611	9.666240	-0.069778	4.818475
347.656452	8000.053844	9.671245	-0.069805	4.818464
347.329087	8000.179695	9.676250	-0.069745	4.818503
347.457940	8000.043864	9.681255	-0.069768	4.818462
347.433569	8000.189488	9.686259	-0.069764	4.818506
347.668586	8000.103364	9.691264	-0.069808	4.818479
347.525149	8000.015366	9.696269	-0.069781	4.818453
347.622795	8000.202508	9.701274	-0.069799	4.818509
347.716204	8000.073555	9.706279	-0.069817	4.818470
347.561103	8000.129247	9.711283	-0.069788	4.818487
347.401395	8000.169127	9.716288	-0.069758	4.818500
347.390408	8000.046139	9.721293	-0.069756	4.818463
347.658981	8000.155754	9.726298	-0.069806	4.818495
347.754605	8000.082478	9.731303	-0.069824	4.818472
347.773999	8000.239184	9.736307	-0.069828	4.818519
347.441510	8000.055228	9.741312	-0.069766	4.818466
347.679492	8000.214835	9.746317	-0.069810	4.818512
347.587715	8000.285017	9.751322	-0.069793	4.818533
347.560720	7999.907725	9.756327	-0.069788	4.818421
347.375556	8000.064863	9.761331	-0.069754	4.818469
347.126446	8000.025861	9.766336	-0.069707	4.818458
347.617951	7999.915842	9.771341	-0.069799	4.818423
347.936892	8000.171021	9.776346	-0.069858	4.818498
347.732607	8000.147311	9.781351	-0.069820	4.818492
347.561767	8000.156595	9.786355	-0.069789	4.818495
347.719835	8000.124048	9.791360	-0.069818	4.818485
347.721657	8000.031678	9.796365	-0.069818	4.818458
347.519460	8000.002748	9.801370	-0.069781	4.818450
347.750168	8000.002663	9.806375	-0.069824	4.818449
347.414776	8000.011863	9.811379	-0.069761	4.818453
347.667837	8000.114971	9.816384	-0.069809	4.818482
347.883552	8000.154587	9.821389	-0.069849	4.818493
347.902269	8000.152739	9.826394	-0.069852	4.818493
347.698872	7999.965247	9.831399	-0.069814	4.818438
347.851824	8000.152074	9.836403	-0.069843	4.818493
347.781017	8000.129087	9.841408	-0.069830	4.818486
347.677824	7999.957626	9.846413	-0.069811	4.818436
347.610216	8000.158324	9.851418	-0.069798	4.818496
348.123328	7999.960396	9.856423	-0.069894	4.818435
348.265753	8000.153385	9.861427	-0.069920	4.818492
348.065038	8000.247321	9.866432	-0.069883	4.818520
347.998810	8000.263243	9.871437	-0.069871	4.818525
348.403486	8000.267572	9.876442	-0.069946	4.818525
348.395409	8000.174018	9.881447	-0.069945	4.818497
348.302974	8000.267292	9.886451	-0.069928	4.818525
348.160749	8000.050159	9.891456	-0.069901	4.818461
348.249623	7999.831899	9.896461	-0.069917	4.818396
348.039140	7999.857456	9.901466	-0.069878	4.818404
347.786127	7999.923398	9.906471	-0.069831	4.818425
347.944763	7999.870908	9.911475	-0.069861	4.818409
347.825778	7999.930229	9.916480	-0.069839	4.818427
348.095892	8000.138562	9.921485	-0.069889	4.818488
347.720151	7999.946682	9.926490	-0.069819	4.818432
347.690371	7999.960989	9.931495	-0.069814	4.818437
347.715229	8000.061068	9.936499	-0.069818	4.818466
347.932422	8000.157402	9.941504	-0.069859	4.818494
348.194695	7999.956142	9.946509	-0.069908	4.818433
347.713990	7999.940314	9.951514	-0.069818	4.818430
348.157131	8000.062746	9.956519	-0.069901	4.818465
348.166811	7999.955780	9.961523	-0.069903	4.818433
348.268991	8000.045337	9.966528	-0.069922	4.818459
348.289571	7999.915417	9.971533	-0.069925	4.818421
348.439029	8000.067551	9.976538	-0.069953	4.818465
348.486466	8000.071333	9.981543	-0.069962	4.818466
348.649618	8000.165902	9.986547	-0.069993	4.818494
348.656659	8000.161799	9.991552	-0.069994	4.818492
348.845625	8000.126512	9.996557	-0.070029	4.818481
348.623327	8000.211761	10.001562	-0.069988	4.818507
348.483729	8000.052411	10.006567	-0.069962	4.818461
348.836623	8000.098051	10.011571	-0.070028	4.818473
348.612182	8000.144422	10.016576	-0.069986	4.818487
348.765737	8000.099215	10.021581	-0.070015	4.818473
348.457918	8000.142378	10.026586	-0.069957	4.818487
348.278522	7999.968851	10.031591	-0.069924	4.818437
348.466565	8000.129898	10.036595	-0.069959	4.818484
348.470337	7999.929405	10.041600	-0.069960	4.818424
348.627602	7999.902096	10.046605	-0.069989	4.818415
348.526167	8000.059299	10.051610	-0.069970	4.818462
348.720886	7999.982089	10.056615	-0.070006	4.818439
348.713865	8000.006148	10.061619	-0.070005	4.818446
348.562838	7999.915947	10.066624	-0.069977	4.818420
348.715766	7999.959980	10.071629	-0.070006	4.818432
348.853749	8000.164463	10.076634	-0.070031	4.818492
348.894128	8000.051603	10.081639	-0.070039	4.818459
348.765342	8000.006846	10.086643	-0.070015	4.818446
348.867444	8000.343154	10.091648	-0.070034	4.818546
348.957045	8000.134347	10.096653	-0.070051	4.818483
348.801312	8000.131230	10.101658	-0.070022	4.818483
348.822375	7999.945665	10.106663	-0.070026	4.818428
348.997306	8000.192640	10.111667	-0.070058	4.818500
348.912172	8000.093862	10.116672	-0.070043	4.818471
348.996546	8000.083435	10.121677	-0.070058	4.818468
349.064400	7999.987740	10.126682	-0.070071	4.818439
349.281019	8000.075670	10.131687	-0.070111	4.818464
349.007844	7999.943945	10.136691	-0.070060	4.818426
348.857375	8000.091047	10.141696	-0.070033	4.818471
349.161315	8000.088788	10.146701	-0.070089	4.818469
349.021458	8000.160433	10.151706	-0.070063	4.818491
348.967441	8000.100918	10.156711	-0.070053	4.818473
349.077385	8000.045681	10.161715	-0.070074	4.818456
349.119005	8000.147037	10.166720	-0.070082	4.818486
349.097875	7999.950409	10.171725	-0.070078	4.818428
349.075978	8000.100271	10.176730	-0.070074	4.818472
348.916525	8000.089755	10.181735	-0.070044	4.818470
349.139921	8000.232376	10.186739	-0.070086	4.818512
349.005192	8000.179138	10.191744	-0.070061	4.818496
349.173669	8000.166680	10.196749	-0.070092	4.818492
348.799255	8000.164857	10.201754	-0.070022	4.818493
348.983744	8000.053912	10.206759	-0.070057	4.818459
349.084645	8000.111955	10.211763	-0.070075	4.818476
349.053152	8000.308940	10.216768	-0.070070	4.818535
348.968840	8000.087322	10.221773	-0.070054	4.818469
348.906904	8000.366852	10.226778	-0.070043	4.818552
349.136133	8000.355202	10.231783	-0.070085	4.818548
349.075955	8000.289304	10.236787	-0.070074	4.818529
349.002816	8000.318785	10.241792	-0.070061	4.818538
349.270078	8000.286640	10.246797	-0.070110	4.818527
349.180654	8000.335854	10.251802	-0.070094	4.818542
349.460783	8000.145328	10.256807	-0.070146	4.818484
349.353554	8000.341308	10.261811	-0.070126	4.818543
349.330874	8000.198207	10.266816	-0.070122	4.818501
349.375657	8000.241856	10.271821	-0.070130	4.818513
349.497853	8000.181532	10.276826	-0.070153	4.818495
349.530354	8000.253368	10.281831	-0.070159	4.818516
349.435417	8000.245808	10.286835	-0.070141	4.818514
349.189081	8000.200536	10.291840	-0.070096	4.818502
349.387718	8000.171679	10.296845	-0.070133	4.818492
349.261547	8000.300206	10.301850	-0.070109	4.818531
349.379642	8000.244028	10.306855	-0.070131	4.818514
349.566142	8000.329462	10.311859	-0.070166	4.818539
349.440271	8000.342491	10.316864	-0.070143	4.818543
349.457619	8000.297574	10.321869	-0.070146	4.818530
349.449299	8000.258615	10.326874	-0.070144	4.818518
349.379970	8000.179995	10.331879	-0.070131	4.818495
349.261330	8000.260322	10.336883	-0.070109	4.818519
349.139113	8000.225100	10.341888	-0.070087	4.818509
349.258734	8000.166842	10.346893	-0.070109	4.818492
349.320140	8000.154010	10.351898	-0.070120	4.818487
349.203362	8000.203912	10.356903	-0.070099	4.818503
349.328937	8000.203483	10.361907	-0.070122	4.818502
349.332039	8000.284378	10.366912	-0.070123	4.818526
349.255716	8000.145815	10.371917	-0.070109	4.818485
349.125228	8000.302635	10.376922	-0.070084	4.818532
349.388171	8000.142331	10.381927	-0.070133	4.818484
349.399768	8000.168738	10.386931	-0.070135	4.818492
349.495001	8000.304409	10.391936	-0.070153	4.818531
349.693739	8000.209401	10.396941	-0.070190	4.818502
349.413471	8000.240329	10.401946	-0.070138	4.818513
349.278674	8000.191289	10.406951	-0.070113	4.818499
349.343248	8000.149100	10.411955	-0.070125	4.818486
349.381680	8000.255665	10.416960	-0.070132	4.818517
349.477570	8000.068990	10.421965	-0.070150	4.818462
349.294347	8000.165258	10.426970	-0.070116	4.818491
349.365530	8000.338410	10.431975	-0.070130	4.818542
349.631879	8000.185500	10.436979	-0.070179	4.818496
349.445536	8000.357330	10.441984	-0.070145	4.818547
349.300244	8000.103397	10.446989	-0.070117	4.818472
349.379768	8000.221008	10.451994	-0.070132	4.818507
349.466885	8000.325071	10.456999	-0.070149	4.818538
349.640434	8000.241279	10.462003	-0.070181	4.818512
349.675556	8000.335201	10.467008	-0.070188	4.818540
349.726384	8000.163675	10.472013	-0.070197	4.818489
349.584117	8000.347641	10.477018	-0.070171	4.818544
349.529278	8000.305963	10.482023	-0.070160	4.818532
349.752882	8000.179786	10.487027	-0.070202	4.818493
349.504433	8000.333989	10.492032	-0.070156	4.818540
349.453839	8000.261918	10.497037	-0.070146	4.818519
349.734834	8000.310807	10.502042	-0.070199	4.818532
349.382892	8000.123428	10.507047	-0.070133	4.818478
349.524593	8000.238716	10.512051	-0.070160	4.818512
349.501946	8000.310869	10.517056	-0.070156	4.818533
349.451644	8000.118050	10.522061	-0.070146	4.818476
349.594302	8000.439156	10.527066	-0.070173	4.818571
349.516694	8000.166171	10.532071	-0.070158	4.818490
349.437183	8000.212367	10.537075	-0.070144	4.818504
349.203012	8000.209257	10.542080	-0.070100	4.818504
349.602050	8000.140013	10.547085	-0.070174	4.818482
349.480989	8000.156257	10.552090	-0.070152	4.818487
349.468064	8000.272640	10.557095	-0.070150	4.818522
349.475515	8000.136239	10.562099	-0.070151	4.818482
349.512150	8000.224930	10.567104	-0.070158	4.818508
349.498889	8000.130255	10.572109	-0.070155	4.818480
349.477283	8000.264373	10.577114	-0.070151	4.818520
349.600521	8000.115861	10.582119	-0.070174	4.818475
349.637651	8000.055457	10.587123	-0.070181	4.818457
349.453717	8000.265118	10.592128	-0.070147	4.818520
349.553714	8000.109997	10.597133	-0.070166	4.818473
349.681270	8000.284949	10.602138	-0.070190	4.818525
349.636653	8000.159406	10.607143	-0.070181	4.818488
349.619234	8000.115076	10.612147	-0.070178	4.818475
349.620631	8000.331402	10.617152	-0.070178	4.818539
349.740631	8000.007494	10.622157	-0.070201	4.818442
349.615013	8000.172779	10.627162	-0.070177	4.818492
349.729324	8000.052499	10.632167	-0.070199	4.818456
349.794993	8000.041825	10.637171	-0.070211	4.818452
349.634720	8000.093248	10.642176	-0.070181	4.818468
349.715045	7999.914767	10.647181	-0.070196	4.818415
349.850275	8000.120269	10.652186	-0.070221	4.818475
349.849583	8000.057261	10.657191	-0.070221	4.818457
349.593251	8000.188259	10.662195	-0.070174	4.818497
349.490594	8000.312900	10.667200	-0.070155	4.818534
349.887497	8000.090324	10.672205	-0.070228	4.818466
349.650165	8000.099772	10.677210	-0.070184	4.818470
349.761377	8000.228306	10.682215	-0.070205	4.818508
349.877107	8000.301249	10.687219	-0.070227	4.818529
349.699070	8000.128781	10.692224	-0.070194	4.818478
349.651059	8000.067245	10.697229	-0.070185	4.818460
349.687724	8000.102385	10.702234	-0.070191	4.818471
349.905107	8000.084277	10.707239	-0.070232	4.818464
349.811306	8000.216386	10.712243	-0.070215	4.818504
349.576499	8000.162866	10.717248	-0.070171	4.818489
349.832186	7999.957314	10.722253	-0.070218	4.818427
349.716826	8000.290740	10.727258	-0.070197	4.818526
349.639890	8000.342221	10.732263	-0.070183	4.818542
349.849670	8000.048906	10.737267	-0.070222	4.818454
349.823918	8000.266971	10.742272	-0.070217	4.818519
349.660012	8000.031690	10.747277	-0.070187	4.818450
349.859436	8000.256948	10.752282	-0.070224	4.818516
349.750541	8000.150501	10.757287	-0.070204	4.818485
349.669418	8000.095874	10.762291	-0.070189	4.818469
349.586071	8000.085319	10.767296	-0.070173	4.818466
349.893669	7999.995959	10.772301	-0.070230	4.818438
349.673759	8000.199892	10.777306	-0.070189	4.818500
349.923547	8000.047812	10.782311	-0.070236	4.818453
349.863587	8000.226572	10.787315	-0.070225	4.818507
349.805324	8000.242600	10.792320	-0.070214	4.818512
349.891589	8000.185998	10.797325	-0.070230	4.818495
349.785531	8000.324245	10.802330	-0.070211	4.818536
349.766580	8000.313495	10.807335	-0.070207	4.818533
349.785048	8000.098488	10.812339	-0.070210	4.818469
349.538969	8000.226473	10.817344	-0.070165	4.818508
349.609819	8000.172816	10.822349	-0.070178	4.818492
349.695942	8000.179214	10.827354	-0.070194	4.818493
349.883495	8000.225811	10.832359	-0.070229	4.818507
349.918601	8000.167479	10.837363	-0.070236	4.818489
349.884253	8000.259427	10.842368	-0.070229	4.818517
349.847239	8000.049983	10.847373	-0.070222	4.818454
349.817304	8000.160890	10.852378	-0.070217	4.818487
349.776891	8000.151955	10.857383	-0.070209	4.818485
349.739892	8000.237568	10.862387	-0.070202	4.818511
349.782420	8000.364140	10.867392	-0.070211	4.818548
350.034934	8000.234146	10.872397	-0.070257	4.818508
349.891479	8000.271093	10.877402	-0.070231	4.818520
349.732800	8000.144033	10.882407	-0.070201	4.818483
349.938368	8000.118418	10.887411	-0.070240	4.818474
350.033592	8000.286641	10.892416	-0.070257	4.818524
349.815733	8000.196595	10.897421	-0.070217	4.818498
349.789112	8000.214094	10.902426	-0.070212	4.818503
349.894399	8000.216546	10.907431	-0.070232	4.818504
350.003720	8000.249503	10.912435	-0.070252	4.818513
349.761418	8000.204283	10.917440	-0.070207	4.818501
349.973291	8000.166152	10.922445	-0.070246	4.818488
349.850143	8000.217019	10.927450	-0.070223	4.818504
349.887888	8000.228024	10.932455	-0.070231	4.818507
349.996191	8000.207416	10.937459	-0.070251	4.818501
349.874244	8000.319200	10.942464	-0.070228	4.818534
349.913031	8000.294518	10.947469	-0.070235	4.818527
349.926855	8000.328306	10.952474	-0.070238	4.818537
350.000278	8000.362886	10.957479	-0.070252	4.818547
350.033594	8000.284579	10.962483	-0.070258	4.818523
350.120681	8000.210137	10.967488	-0.070274	4.818501
350.230293	8000.189547	10.972493	-0.070295	4.818494
349.969840	8000.262739	10.977498	-0.070246	4.818517
350.029050	8000.241478	10.982503	-0.070257	4.818511
350.055191	8000.281730	10.987507	-0.070262	4.818522
350.080106	8000.110909	10.992512	-0.070267	4.818472
350.160653	8000.063681	10.997517	-0.070282	4.818457
350.085116	8000.284236	11.002522	-0.070268	4.818523
350.165829	8000.077405	11.007527	-0.070283	4.818461
350.104129	8000.079738	11.012531	-0.070271	4.818462
349.868273	8000.243559	11.017536	-0.070228	4.818512
350.012356	8000.142575	11.022541	-0.070254	4.818481
350.015520	8000.078568	11.027546	-0.070255	4.818462
350.043348	8000.340399	11.032551	-0.070260	4.818540
350.137284	8000.330100	11.037555	-0.070278	4.818536
350.224459	8000.350163	11.042560	-0.070294	4.818542
350.096680	8000.130059	11.047565	-0.070270	4.818477
349.922900	8000.170803	11.052570	-0.070238	4.818490
350.155975	8000.257907	11.057575	-0.070281	4.818515
350.217560	8000.119074	11.062579	-0.070293	4.818473
350.121929	8000.257460	11.067584	-0.070275	4.818515
350.136674	8000.237708	11.072589	-0.070278	4.818509
350.101316	8000.281342	11.077594	-0.070271	4.818522
350.108624	8000.231040	11.082599	-0.070273	4.818507
350.281050	8000.347790	11.087603	-0.070305	4.818541
350.211851	8000.187267	11.092608	-0.070292	4.818494
349.987595	8000.143337	11.097613	-0.070250	4.818482
350.059848	8000.138000	11.102618	-0.070264	4.818480
349.987470	8000.009988	11.107623	-0.070250	4.818442
350.203563	7999.941461	11.112627	-0.070291	4.818421
349.994156	8000.340841	11.117632	-0.070252	4.818540
350.201440	8000.116792	11.122637	-0.070290	4.818473
350.259345	8000.288721	11.127642	-0.070301	4.818524
350.111109	8000.134497	11.132647	-0.070274	4.818478
350.236854	8000.085771	11.137651	-0.070297	4.818463
350.362689	8000.235501	11.142656	-0.070321	4.818507
350.257256	7999.955844	11.147661	-0.070301	4.818425
349.876155	8000.097784	11.152666	-0.070230	4.818468
350.080187	8000.099449	11.157671	-0.070268	4.818468
350.213624	8000.090725	11.162675	-0.070293	4.818465
350.133686	8000.191518	11.167680	-0.070278	4.818495
350.205851	8000.099028	11.172685	-0.070292	4.818467
350.023628	8000.201611	11.177690	-0.070258	4.818499
350.045299	8000.096899	11.182695	-0.070262	4.818467
349.934963	7999.997783	11.187699	-0.070241	4.818438
350.003034	8000.318949	11.192704	-0.070254	4.818534
350.159558	8000.121527	11.197709	-0.070283	4.818474
350.015357	8000.132212	11.202714	-0.070256	4.818478
349.986757	8000.116085	11.207719	-0.070251	4.818473
350.051022	8000.035040	11.212723	-0.070263	4.818449
350.028783	8000.035797	11.217728	-0.070259	4.818449
350.262085	8000.050451	11.222733	-0.070302	4.818453
350.091595	8000.146890	11.227738	-0.070271	4.818482
349.994272	8000.177100	11.232743	-0.070253	4.818492
349.800627	7999.927774	11.237747	-0.070216	4.818418
349.834138	8000.160276	11.242752	-0.070223	4.818487
349.982642	7999.896598	11.247757	-0.070250	4.818408
349.887003	8000.149434	11.252762	-0.070233	4.818484
349.866879	8000.054667	11.257767	-0.070229	4.818456
350.043342	8000.021315	11.262771	-0.070262	4.818445
350.101658	7999.970642	11.267776	-0.070273	4.818430
349.744209	7999.934394	11.272781	-0.070206	4.818420
349.750134	7999.972275	11.277786	-0.070207	4.818432
350.120957	8000.112659	11.282791	-0.070277	4.818472
349.889349	8000.043432	11.287795	-0.070233	4.818452
349.915102	8000.164529	11.292800	-0.070238	4.818488
350.270317	8000.041151	11.297805	-0.070304	4.818450
349.971616	7999.994133	11.302810	-0.070249	4.818437
350.037220	8000.189262	11.307815	-0.070261	4.818495
350.011267	7999.941114	11.312819	-0.070256	4.818421
349.983808	8000.145506	11.317824	-0.070251	4.818482
349.945626	8000.030549	11.322829	-0.070244	4.818448
350.010153	8000.121711	11.327834	-0.070256	4.818475
350.063572	8000.145524	11.332839	-0.070266	4.818482
350.069768	7999.986006	11.337843	-0.070267	4.818434
350.202618	8000.272333	11.342848	-0.070292	4.818519
350.296699	8000.011078	11.347853	-0.070310	4.818441
350.171106	8000.214167	11.352858	-0.070286	4.818502
350.053523	8000.269308	11.357863	-0.070265	4.818519
350.175186	8000.069323	11.362867	-0.070287	4.818459
350.030117	8000.148249	11.367872	-0.070260	4.818483
350.132536	8000.184264	11.372877	-0.070279	4.818493
350.063531	8000.178099	11.377882	-0.070267	4.818492
350.228879	8000.101548	11.382887	-0.070297	4.818468
350.141964	8000.062594	11.387891	-0.070281	4.818457
349.929581	8000.166876	11.392896	-0.070242	4.818489
350.239891	8000.051301	11.397901	-0.070300	4.818453
350.169072	8000.016762	11.402906	-0.070286	4.818443
350.140754	8000.069939	11.407911	-0.070281	4.818459
350.052243	8000.075066	11.412915	-0.070265	4.818461
349.926208	8000.157395	11.417920	-0.070241	4.818486
349.996103	8000.084825	11.422925	-0.070254	4.818464
350.087614	8000.318101	11.427930	-0.070272	4.818533
350.130852	8000.144373	11.432935	-0.070280	4.818481
350.164168	8000.073417	11.437939	-0.070286	4.818460
350.167535	8000.145916	11.442944	-0.070286	4.818482
350.297685	8000.178101	11.447949	-0.070311	4.818491
350.338258	8000.159742	11.452954	-0.070318	4.818485
350.145545	8000.205484	11.457959	-0.070283	4.818499
350.123647	8000.048741	11.462963	-0.070278	4.818453
350.227938	8000.328390	11.467968	-0.070298	4.818536
350.179347	8000.080988	11.472973	-0.070289	4.818462
350.073103	8000.175131	11.477978	-0.070269	4.818491
350.182840	8000.238545	11.482983	-0.070290	4.818509
350.189737	8000.148336	11.487987	-0.070291	4.818482
349.924053	8000.181558	11.492992	-0.070242	4.818493
350.068144	8000.093174	11.497997	-0.070268	4.818466
350.198847	8000.154766	11.503002	-0.070293	4.818484
350.194517	8000.068608	11.508007	-0.070292	4.818458
350.259421	8000.201778	11.513011	-0.070304	4.818498
350.293477	8000.188583	11.518016	-0.070311	4.818494
350.204108	8000.162197	11.523021	-0.070294	4.818486
350.183601	8000.169277	11.528026	-0.070290	4.818488
350.250543	8000.154419	11.533031	-0.070303	4.818484
350.420762	8000.220738	11.538035	-0.070334	4.818503
350.352360	8000.236632	11.543040	-0.070322	4.818508
350.375092	8000.218036	11.548045	-0.070326	4.818502
350.471570	8000.162619	11.553050	-0.070344	4.818485
349.803277	8000.051885	11.558055	-0.070219	4.818455
350.225988	8000.135208	11.563059	-0.070298	4.818478
349.797815	8000.215621	11.568064	-0.070219	4.818504
349.742922	7999.979690	11.573069	-0.070208	4.818434
349.750884	7999.981898	11.578074	-0.070210	4.818434
349.893383	8000.056246	11.583079	-0.070236	4.818456
350.267606	7999.988771	11.588083	-0.070306	4.818434
350.141908	8000.184508	11.593088	-0.070283	4.818493
350.165037	8000.179568	11.598093	-0.070287	4.818492
350.455573	8000.197085	11.603098	-0.070341	4.818496
350.410950	8000.208045	11.608103	-0.070333	4.818499
350.323072	8000.099775	11.613107	-0.070317	4.818467
350.305327	8000.216096	11.618112	-0.070314	4.818502
350.511147	8000.208336	11.623117	-0.070352	4.818499
350.362290	8000.111855	11.628122	-0.070324	4.818471
350.216787	8000.187626	11.633127	-0.070297	4.818494
350.221472	8000.040687	11.638131	-0.070298	4.818450
350.308225	8000.188847	11.643136	-0.070314	4.818494
350.176568	8000.021195	11.648141	-0.070290	4.818444
350.073817	8000.022982	11.653146	-0.070271	4.818445
350.085417	8000.033639	11.658151	-0.070273	4.818448
350.048555	7999.975400	11.663155	-0.070266	4.818431
350.194289	8000.061342	11.668160	-0.070293	4.818456
350.231665	7999.983090	11.673165	-0.070300	4.818433
349.869682	8000.022382	11.678170	-0.070233	4.818446
349.967730	8000.057289	11.683175	-0.070251	4.818456
350.330590	8000.099916	11.688179	-0.070319	4.818467
349.984799	7999.958819	11.693184	-0.070254	4.818427
349.946133	7999.944658	11.698189	-0.070247	4.818423
349.958760	7999.804127	11.703194	-0.070249	4.818381
349.995878	7999.844523	11.708199	-0.070256	4.818393
349.789990	7999.747291	11.713203	-0.070218	4.818364
349.759845	8000.075545	11.718208	-0.070213	4.818462
349.950920	7999.894335	11.723213	-0.070248	4.818408
350.125363	7999.943906	11.728218	-0.070281	4.818422
350.025148	8000.029728	11.733223	-0.070262	4.818448
350.163691	7999.976972	11.738227	-0.070288	4.818431
350.312892	8000.202614	11.743232	-0.070316	4.818498
350.190885	8000.122242	11.748237	-0.070293	4.818474
350.222838	8000.223473	11.753242	-0.070299	4.818504
350.183032	8000.235547	11.758247	-0.070292	4.818508
350.113563	8000.077121	11.763251	-0.070279	4.818461
350.137044	8000.174039	11.768256	-0.070283	4.818490
350.032288	8000.022495	11.773261	-0.070264	4.818445
349.947188	8000.048667	11.778266	-0.070248	4.818453
350.041824	7999.980626	11.783271	-0.070266	4.818433
350.186028	8000.017196	11.788275	-0.070292	4.818443
349.737281	8000.024885	11.793280	-0.070209	4.818447
350.062221	8000.145759	11.798285	-0.070270	4.818482
350.434829	8000.232619	11.803290	-0.070339	4.818506
350.327684	8000.224897	11.808295	-0.070319	4.818504
350.426740	7999.934308	11.813299	-0.070337	4.818418
350.490638	8000.197668	11.818304	-0.070350	4.818496
350.511718	8000.216852	11.823309	-0.070353	4.818501
350.465894	8000.107041	11.828314	-0.070345	4.818469
350.288707	8000.365098	11.833319	-0.070312	4.818546
350.429426	8000.095012	11.838323	-0.070338	4.818465
350.420505	8000.152648	11.843328	-0.070337	4.818482
350.213306	8000.205547	11.848333	-0.070298	4.818499
350.462827	8000.084963	11.853338	-0.070345	4.818462
350.276234	8000.320844	11.858343	-0.070310	4.818533
350.263877	7999.885969	11.863347	-0.070307	4.818404
350.404215	8000.106243	11.868352	-0.070334	4.818469
350.107815	8000.105455	11.873357	-0.070279	4.818470
350.369519	7999.947233	11.878362	-0.070327	4.818422
350.181108	8000.133736	11.883367	-0.070292	4.818478
350.216388	8000.175159	11.888371	-0.070299	4.818490
350.230137	8000.200545	11.893376	-0.070302	4.818497
350.116055	8000.034176	11.898381	-0.070280	4.818448
350.312545	8000.199546	11.903386	-0.070317	4.818497
350.468869	8000.089274	11.908391	-0.070346	4.818463
350.288970	8000.014433	11.913395	-0.070313	4.818442
349.990312	8000.104967	11.918400	-0.070257	4.818470
350.146237	8000.093393	11.923405	-0.070286	4.818466
350.307634	8000.135442	11.928410	-0.070316	4.818478
350.066367	8000.123837	11.933415	-0.070271	4.818475
350.295224	8000.143683	11.938419	-0.070314	4.818480
350.169680	8000.228119	11.943424	-0.070291	4.818506
350.319491	8000.167112	11.948429	-0.070319	4.818487
350.304200	8000.098659	11.953434	-0.070316	4.818467
350.222746	8000.318087	11.958439	-0.070301	4.818532
350.240582	8000.276325	11.963443	-0.070304	4.818520
349.965394	8000.218066	11.968448	-0.070253	4.818504
350.420180	7999.984709	11.973453	-0.070337	4.818433
350.155837	8000.076750	11.978458	-0.070288	4.818461
350.252765	8000.154693	11.983463	-0.070306	4.818484
350.323869	8000.035938	11.988467	-0.070320	4.818448
350.416880	8000.192582	11.993472	-0.070337	4.818494
350.423602	7999.950117	11.998477	-0.070338	4.818422
350.382922	8000.099733	12.003482	-0.070331	4.818467
350.405871	7999.966687	12.008487	-0.070335	4.818427
350.431395	8000.130834	12.013491	-0.070340	4.818476
350.209425	8000.257040	12.018496	-0.070299	4.818514
350.282776	8000.162464	12.023501	-0.070312	4.818486
350.393794	8000.107241	12.028506	-0.070333	4.818469
350.283322	8000.099475	12.033511	-0.070312	4.818467
350.193895	7999.939735	12.038515	-0.070296	4.818420
350.362155	8000.086878	12.043520	-0.070327	4.818463
350.372209	8000.104865	12.048525	-0.070329	4.818468
350.459896	8000.278241	12.053530	-0.070346	4.818520
350.349672	8000.349231	12.058535	-0.070325	4.818541
350.501986	8000.157001	12.063539	-0.070353	4.818483
350.466329	8000.256283	12.068544	-0.070347	4.818513
350.727744	8000.270264	12.073549	-0.070396	4.818516
350.585486	8000.062566	12.078554	-0.070369	4.818455
350.259950	8000.167444	12.083559	-0.070309	4.818487
350.428647	8000.062586	12.088563	-0.070340	4.818456
350.542272	8000.295109	12.093568	-0.070361	4.818524
350.506226	7999.996421	12.098573	-0.070354	4.818436
350.606724	7999.945258	12.103578	-0.070373	4.818420
350.578307	8000.146490	12.108583	-0.070368	4.818480
350.521382	8000.027081	12.113587	-0.070357	4.818445
350.256341	8000.041411	12.118592	-0.070308	4.818450
350.093396	8000.032947	12.123597	-0.070278	4.818448
350.533286	8000.006247	12.128602	-0.070360	4.818438
350.301164	8000.031515	12.133607	-0.070317	4.818447
350.419670	8000.029943	12.138611	-0.070339	4.818446
350.306041	7999.988534	12.143616	-0.070317	4.818434
350.453377	8000.080798	12.148621	-0.070345	4.818461
350.519538	8000.094281	12.153626	-0.070357	4.818465
350.484977	8000.082274	12.158631	-0.070351	4.818461
350.453808	7999.917007	12.163635	-0.070345	4.818412
350.474653	7999.996039	12.168640	-0.070349	4.818436
350.400666	8000.110562	12.173645	-0.070335	4.818470
350.355318	7999.961907	12.178650	-0.070327	4.818426
350.190652	8000.130876	12.183655	-0.070296	4.818477
350.215880	8000.117563	12.188659	-0.070301	4.818473
350.281183	8000.106884	12.193664	-0.070313	4.818469
350.580272	8000.210618	12.198669	-0.070369	4.818499
350.752736	8000.152011	12.203674	-0.070401	4.818481
350.658581	8000.085659	12.208679	-0.070384	4.818462
350.791160	8000.052774	12.213683	-0.070408	4.818451
350.552670	8000.033855	12.218688	-0.070364	4.818447
350.690537	7999.882386	12.223693	-0.070390	4.818401
350.886560	8000.113903	12.228698	-0.070426	4.818469
350.708729	8000.024387	12.233703	-0.070393	4.818443
350.762873	8000.028260	12.238707	-0.070403	4.818444
350.799602	8000.074953	12.243712	-0.070410	4.818458
350.667015	8000.165596	12.248717	-0.070386	4.818485
350.799687	8000.068659	12.253722	-0.070410	4.818456
350.629293	8000.205002	12.258727	-0.070379	4.818497
350.705976	7999.959265	12.263731	-0.070393	4.818424
350.696617	8000.119799	12.268736	-0.070391	4.818472
350.828045	8000.056447	12.273741	-0.070416	4.818452
350.890038	7999.920769	12.278746	-0.070427	4.818412
350.916140	8000.047123	12.283751	-0.070432	4.818449
350.969471	8000.036285	12.288755	-0.070442	4.818446
350.954443	8000.162094	12.293760	-0.070439	4.818483
350.949094	8000.120023	12.298765	-0.070438	4.818471
350.910883	8000.020813	12.303770	-0.070431	4.818441
350.795943	8000.211446	12.308775	-0.070410	4.818498
350.826935	7999.966151	12.313779	-0.070416	4.818425
350.762816	8000.240412	12.318784	-0.070404	4.818507
350.874574	8000.063393	12.323789	-0.070425	4.818454
350.958806	8000.168471	12.328794	-0.070441	4.818485
350.860605	8000.157717	12.333799	-0.070422	4.818482
350.770139	8000.122915	12.338803	-0.070405	4.818472
350.838586	8000.074476	12.343808	-0.070418	4.818458
350.918810	8000.059795	12.348813	-0.070433	4.818453
350.919866	8000.058762	12.353818	-0.070433	4.818453
350.784451	8000.283774	12.358823	-0.070408	4.818520
350.832650	7999.920052	12.363827	-0.070417	4.818412
350.753059	8000.116404	12.368832	-0.070403	4.818470
350.744811	8000.041744	12.373837	-0.070401	4.818448
350.787530	8000.233423	12.378842	-0.070409	4.818505
350.628838	8000.199814	12.383847	-0.070380	4.818496
350.765419	8000.131280	12.388851	-0.070405	4.818475
350.943110	8000.211350	12.393856	-0.070438	4.818498
350.866655	8000.125281	12.398861	-0.070424	4.818472
350.824449	7999.954616	12.403866	-0.070416	4.818422
350.578752	8000.071056	12.408871	-0.070370	4.818458
350.841703	7999.975852	12.413875	-0.070419	4.818428
350.856188	8000.165055	12.418880	-0.070422	4.818484
350.644030	8000.219988	12.423885	-0.070383	4.818502
350.788776	8000.064409	12.428890	-0.070410	4.818455
350.855462	8000.159803	12.433895	-0.070422	4.818483
350.850902	8000.101992	12.438899	-0.070421	4.818466
350.663752	8000.115257	12.443904	-0.070386	4.818470
350.714329	7999.940576	12.448909	-0.070396	4.818418
350.813161	8000.058447	12.453914	-0.070414	4.818453
350.750996	8000.043972	12.458919	-0.070403	4.818449
351.007293	7999.963380	12.463923	-0.070450	4.818424
350.820612	8000.157258	12.468928	-0.070416	4.818482
350.812642	8000.107803	12.473933	-0.070414	4.818467
350.986216	8000.024010	12.478938	-0.070447	4.818442
350.814494	8000.113083	12.483943	-0.070415	4.818469
350.729176	7999.954446	12.488947	-0.070399	4.818422
350.608772	8000.119803	12.493952	-0.070377	4.818472
350.844164	8000.038933	12.498957	-0.070420	4.818447
350.879720	7999.949105	12.503962	-0.070427	4.818420
350.504522	8000.103724	12.508967	-0.070357	4.818467
350.705797	8000.002450	12.513971	-0.070395	4.818437
350.634846	8000.080262	12.518976	-0.070382	4.818460
350.548659	8000.012966	12.523981	-0.070366	4.818440
350.544632	8000.116869	12.528986	-0.070365	4.818471
350.454058	8000.150319	12.533991	-0.070348	4.818482
350.745356	7999.972538	12.538995	-0.070402	4.818428
350.600419	8000.013665	12.544000	-0.070375	4.818440
350.825838	7999.997765	12.549005	-0.070417	4.818435
350.628275	7999.932139	12.554010	-0.070381	4.818416
350.681977	8000.167014	12.559015	-0.070391	4.818486
350.738884	7999.905264	12.564019	-0.070401	4.818408
350.625780	8000.058118	12.569024	-0.070380	4.818453
350.667860	8000.088081	12.574029	-0.070388	4.818462
350.606854	7999.996970	12.579034	-0.070377	4.818435
350.755822	8000.214212	12.584039	-0.070405	4.818499
350.817200	7999.880068	12.589043	-0.070416	4.818400
350.775119	8000.003415	12.594048	-0.070408	4.818437
350.851838	7999.919385	12.599053	-0.070423	4.818411
350.715033	7999.942770	12.604058	-0.070397	4.818419
350.692395	7999.929871	12.609063	-0.070393	4.818415
350.826882	7999.943212	12.614067	-0.070418	4.818418
350.784110	8000.151604	12.619072	-0.070410	4.818481
350.820842	8000.070192	12.624077	-0.070417	4.818456
350.950999	8000.033074	12.629082	-0.070441	4.818445
350.853151	8000.093728	12.634087	-0.070423	4.818463
351.008971	7999.955097	12.639091	-0.070452	4.818421
350.994192	7999.987455	12.644096	-0.070449	4.818431
351.025464	8000.081327	12.649101	-0.070455	4.818459
351.341019	8000.113879	12.654106	-0.070514	4.818467
350.766786	8000.083143	12.659111	-0.070407	4.818460
350.842988	7999.982305	12.664115	-0.070421	4.818430
350.895584	7999.949406	12.669120	-0.070431	4.818420
351.000149	7999.896197	12.674125	-0.070451	4.818404
350.889050	7999.910473	12.679130	-0.070430	4.818408
351.018943	8000.188365	12.684135	-0.070454	4.818491
350.920298	8000.027448	12.689139	-0.070436	4.818443
350.723374	7999.989131	12.694144	-0.070399	4.818433
350.707619	8000.105479	12.699149	-0.070397	4.818467
351.067586	7999.964312	12.704154	-0.070464	4.818424
350.919590	8000.100953	12.709159	-0.070436	4.818465
350.949197	7999.787388	12.714163	-0.070441	4.818372
351.256000	8000.089682	12.719168	-0.070499	4.818460
351.016820	8000.058152	12.724173	-0.070454	4.818452
350.786930	7999.924893	12.729178	-0.070411	4.818413
351.099196	8000.088654	12.734183	-0.070470	4.818461
350.839795	7999.981253	12.739187	-0.070421	4.818430
351.102561	8000.050903	12.744192	-0.070470	4.818449
351.180252	8000.048789	12.749197	-0.070485	4.818448
351.199398	8000.029095	12.754202	-0.070488	4.818443
351.267660	8000.235817	12.759207	-0.070501	4.818504
351.019309	7999.935352	12.764211	-0.070455	4.818415
350.779354	8000.020367	12.769216	-0.070410	4.818442
350.835427	8000.161822	12.774221	-0.070421	4.818483
351.103405	8000.269345	12.779226	-0.070471	4.818514
351.082043	8000.363569	12.784231	-0.070467	4.818542
350.975487	8000.090189	12.789235	-0.070447	4.818462
351.044425	8000.275919	12.794240	-0.070460	4.818517
350.952357	8000.182291	12.799245	-0.070443	4.818489
351.091439	8000.140042	12.804250	-0.070469	4.818476
351.006462	8000.213468	12.809255	-0.070453	4.818498
351.042354	8000.095292	12.814259	-0.070460	4.818463
351.284064	8000.155213	12.819264	-0.070505	4.818480
351.144867	8000.113462	12.824269	-0.070479	4.818468
351.027732	8000.085655	12.829274	-0.070457	4.818460
350.950503	8000.116132	12.834279	-0.070443	4.818469
351.260750	8000.078260	12.839283	-0.070501	4.818457
351.223178	8000.267824	12.844288	-0.070494	4.818513
351.021325	8000.058280	12.849293	-0.070456	4.818452
351.057548	8000.092366	12.854298	-0.070463	4.818462
351.125566	8000.286484	12.859303	-0.070476	4.818519
350.971593	8000.072327	12.864307	-0.070447	4.818456
350.917467	8000.171365	12.869312	-0.070437	4.818486
351.175628	8000.156951	12.874317	-0.070485	4.818481
351.181970	8000.045732	12.879322	-0.070486	4.818448
351.261896	8000.123452	12.884327	-0.070501	4.818470
351.212995	8000.121754	12.889331	-0.070492	4.818470
351.148284	8000.273155	12.894336	-0.070480	4.818515
350.972609	8000.107011	12.899341	-0.070447	4.818467
351.079759	8000.026535	12.904346	-0.070467	4.818442
350.993097	8000.161892	12.909351	-0.070451	4.818483
350.888824	7999.992500	12.914355	-0.070432	4.818433
351.026827	8000.101443	12.919360	-0.070458	4.818465
350.917216	7999.982383	12.924365	-0.070437	4.818430
350.968949	8000.038726	12.929370	-0.070447	4.818446
350.557949	7999.942961	12.934375	-0.070370	4.818419
351.052550	8000.026193	12.939379	-0.070463	4.818442
350.884893	7999.956763	12.944384	-0.070431	4.818422
350.843466	7999.907913	12.949389	-0.070424	4.818408
351.009511	8000.059230	12.954394	-0.070455	4.818452
351.053371	8000.194223	12.959399	-0.070463	4.818492
351.134570	8000.035697	12.964403	-0.070478	4.818445
351.057034	8000.138624	12.969408	-0.070464	4.818476
351.134717	8000.250966	12.974413	-0.070478	4.818509
351.150249	7999.946660	12.979418	-0.070481	4.818418
351.118177	8000.219250	12.984423	-0.070475	4.818499
351.233533	8000.076929	12.989427	-0.070497	4.818457
351.179982	8000.101421	12.994432	-0.070487	4.818464
351.162545	8000.114842	12.999437	-0.070484	4.818468
351.208412	8000.095504	13.004442	-0.070492	4.818462
351.063267	7999.986471	13.009447	-0.070465	4.818430
350.932916	7999.819885	13.014451	-0.070441	4.818381
350.898220	8000.153339	13.019456	-0.070435	4.818481
351.114166	8000.112112	13.024461	-0.070475	4.818467
351.044386	8000.117487	13.029466	-0.070462	4.818469
351.068844	8000.234372	13.034471	-0.070466	4.818504
351.189823	8000.050124	13.039475	-0.070489	4.818449
351.062945	8000.178645	13.044480	-0.070465	4.818487
350.807529	8000.122748	13.049485	-0.070418	4.818472
351.067770	8000.195516	13.054490	-0.070466	4.818492
351.101940	8000.149771	13.059495	-0.070473	4.818479
351.149855	8000.129410	13.064499	-0.070482	4.818472
350.934836	8000.155954	13.069504	-0.070442	4.818481
350.814142	8000.119700	13.074509	-0.070419	4.818471
350.895848	8000.055686	13.079514	-0.070434	4.818452
350.726657	8000.222496	13.084519	-0.070403	4.818502
351.024162	8000.089950	13.089523	-0.070458	4.818461
350.970579	8000.318152	13.094528	-0.070449	4.818529
350.881331	8000.257114	13.099533	-0.070432	4.818512
351.210523	8000.106087	13.104538	-0.070493	4.818465
351.108699	8000.037532	13.109543	-0.070474	4.818445
351.103929	8000.151927	13.114547	-0.070474	4.818479
350.998101	8000.314331	13.119552	-0.070454	4.818528
351.216907	8000.136635	13.124557	-0.070495	4.818474
351.147703	8000.007610	13.129562	-0.070482	4.818436
350.954735	8000.096401	13.134567	-0.070446	4.818463
351.026961	7999.918857	13.139571	-0.070459	4.818410
350.965325	8000.045095	13.144576	-0.070448	4.818448
350.765814	8000.057145	13.149581	-0.070411	4.818453
351.099026	7999.962875	13.154586	-0.070473	4.818423
351.035144	8000.146837	13.159591	-0.070461	4.818478
351.048310	7999.949605	13.164595	-0.070463	4.818419
350.974544	8000.060982	13.169600	-0.070450	4.818453
350.933115	8000.095085	13.174605	-0.070442	4.818463
351.082184	8000.014117	13.179610	-0.070470	4.818438
350.736155	8000.300381	13.184615	-0.070406	4.818525
351.140238	7999.935091	13.189619	-0.070481	4.818415
351.257402	8000.070008	13.194624	-0.070503	4.818454
350.812725	7999.940192	13.199629	-0.070420	4.818418
350.927563	8000.043575	13.204634	-0.070441	4.818448
350.890385	8000.068285	13.209639	-0.070434	4.818455
351.236910	8000.122249	13.214643	-0.070499	4.818470
350.985687	8000.155662	13.219648	-0.070452	4.818481
351.081149	8000.135933	13.224653	-0.070470	4.818475
351.254451	8000.055287	13.229658	-0.070502	4.818450
350.928044	8000.349164	13.234663	-0.070442	4.818539
350.902867	8000.066367	13.239667	-0.070437	4.818455
351.134663	8000.174458	13.244672	-0.070480	4.818486
351.067407	8000.080111	13.249677	-0.070468	4.818458
350.990649	8000.110595	13.254682	-0.070453	4.818467
351.053653	8000.083084	13.259687	-0.070465	4.818459
351.158831	8000.012032	13.264691	-0.070485	4.818438
350.913847	8000.216686	13.269696	-0.070439	4.818499
351.116509	8000.220435	13.274701	-0.070477	4.818500
351.179050	8000.040660	13.279706	-0.070489	4.818446
350.811270	8000.089324	13.284711	-0.070420	4.818462
350.877294	8000.119606	13.289715	-0.070433	4.818471
350.968902	8000.100877	13.294720	-0.070450	4.818465
351.117137	8000.205757	13.299725	-0.070477	4.818495
351.158435	8000.069801	13.304730	-0.070485	4.818455
351.016184	8000.099414	13.309735	-0.070459	4.818464
351.013246	8000.079426	13.314739	-0.070458	4.818458
350.866070	8000.161475	13.319744	-0.070431	4.818483
350.786692	8000.169873	13.324749	-0.070416	4.818486
351.063544	8000.167258	13.329754	-0.070468	4.818484
350.843310	8000.164331	13.334759	-0.070427	4.818484
350.846471	8000.175926	13.339763	-0.070427	4.818487
351.116476	8000.258275	13.344768	-0.070478	4.818511
350.747130	8000.050705	13.349773	-0.070409	4.818451
350.620891	7999.996527	13.354778	-0.070385	4.818435
350.792836	8000.063919	13.359783	-0.070417	4.818454
350.921908	7999.962734	13.364787	-0.070441	4.818424
350.868634	7999.997730	13.369792	-0.070432	4.818434
350.843958	8000.118159	13.374797	-0.070427	4.818470
351.138457	8000.066426	13.379802	-0.070482	4.818454
350.914154	8000.050845	13.384807	-0.070440	4.818450
351.090089	8000.138242	13.389811	-0.070473	4.818475
351.125290	8000.045258	13.394816	-0.070480	4.818448
350.903924	8000.133671	13.399821	-0.070438	4.818475
350.961974	8000.069343	13.404826	-0.070449	4.818455
350.909169	8000.120096	13.409831	-0.070439	4.818471
351.156339	8000.042532	13.414835	-0.070486	4.818447
350.998659	8000.198995	13.419840	-0.070456	4.818494
350.531908	8000.036334	13.424845	-0.070369	4.818447
350.995541	8000.022551	13.429850	-0.070456	4.818441
350.912815	8000.133808	13.434855	-0.070440	4.818475
351.063986	8000.268129	13.439859	-0.070469	4.818514
350.930109	8000.143494	13.444864	-0.070444	4.818477
350.836786	8000.048802	13.449869	-0.070426	4.818450
351.100034	8000.040755	13.454874	-0.070475	4.818446
350.989817	8000.207300	13.459879	-0.070455	4.818496
350.838700	8000.060386	13.464883	-0.070427	4.818453
350.886088	8000.055768	13.469888	-0.070436	4.818452
350.767808	8000.145552	13.474893	-0.070414	4.818479
350.893628	8000.000222	13.479898	-0.070437	4.818435
350.779569	8000.141514	13.484903	-0.070416	4.818477
350.841048	8000.085632	13.489907	-0.070427	4.818461
350.887881	8000.060006	13.494912	-0.070436	4.818453
351.054780	8000.004476	13.499917	-0.070467	4.818436
351.063902	7999.952098	13.504922	-0.070469	4.818420
350.972392	8000.275349	13.509927	-0.070452	4.818517
351.174722	8000.179338	13.514931	-0.070490	4.818487
350.955289	8000.119719	13.519936	-0.070449	4.818470
350.934686	8000.259105	13.524941	-0.070445	4.818512
351.120895	7999.933968	13.529946	-0.070480	4.818414
351.250435	8000.140454	13.534951	-0.070504	4.818475
351.179842	8000.303327	13.539955	-0.070491	4.818524
351.188722	8000.140688	13.544960	-0.070493	4.818476
350.910493	8000.285048	13.549965	-0.070441	4.818520
351.059717	8000.114826	13.554970	-0.070469	4.818468
350.943885	8000.276047	13.559975	-0.070447	4.818517
350.927855	7999.939821	13.564979	-0.070444	4.818417
351.186899	8000.204731	13.569984	-0.070492	4.818495
350.803195	8000.072574	13.574989	-0.070421	4.818457
351.005354	8000.002812	13.579994	-0.070459	4.818435
350.831175	8000.180056	13.584999	-0.070426	4.818489
350.936221	8000.146805	13.590003	-0.070446	4.818478
351.001911	7999.980723	13.595008	-0.070458	4.818429
350.751668	8000.003649	13.600013	-0.070412	4.818437
351.121372	8000.029570	13.605018	-0.070480	4.818443
350.871242	8000.065097	13.610023	-0.070434	4.818454
351.192587	7999.985370	13.615027	-0.070494	4.818429
351.187826	8000.134417	13.620032	-0.070493	4.818474
351.117551	8000.064181	13.625037	-0.070480	4.818453
351.299220	8000.032999	13.630042	-0.070514	4.818443
351.083121	8000.023827	13.635047	-0.070474	4.818441
351.057514	8000.036090	13.640051	-0.070469	4.818445
351.289762	7999.955177	13.645056	-0.070512	4.818420
351.381181	8000.087653	13.650061	-0.070529	4.818459
351.371066	8000.022417	13.655066	-0.070527	4.818440
351.240588	8000.146691	13.660071	-0.070503	4.818477
351.133058	8000.024507	13.665075	-0.070483	4.818441
351.388620	7999.974357	13.670080	-0.070531	4.818425
351.019084	8000.082850	13.675085	-0.070462	4.818459
351.141730	7999.916476	13.680090	-0.070485	4.818409
351.256751	8000.079716	13.685095	-0.070506	4.818457
351.236627	7999.932444	13.690099	-0.070502	4.818413
351.223618	7999.960625	13.695104	-0.070500	4.818422
351.300972	8000.077162	13.700109	-0.070515	4.818456
351.297939	7999.859764	13.705114	-0.070514	4.818392
351.154607	8000.003817	13.710119	-0.070487	4.818435
351.293392	8000.039268	13.715123	-0.070513	4.818445
351.167429	7999.966192	13.720128	-0.070490	4.818424
351.107852	8000.095608	13.725133	-0.070479	4.818462
351.095133	8000.048189	13.730138	-0.070477	4.818448
350.966262	8000.012877	13.735143	-0.070453	4.818438
351.016790	7999.964199	13.740147	-0.070462	4.818424
351.044263	8000.050671	13.745152	-0.070467	4.818449
350.929193	8000.009242	13.750157	-0.070446	4.818438
351.154198	8000.014337	13.755162	-0.070488	4.818438
351.196994	8000.296325	13.760167	-0.070496	4.818522
350.964898	7999.917321	13.765171	-0.070452	4.818410
351.090186	7999.984092	13.770176	-0.070476	4.818429
350.971378	7999.955214	13.775181	-0.070454	4.818421
351.129734	7999.907971	13.780186	-0.070483	4.818407
350.734094	7999.944714	13.785191	-0.070410	4.818419
350.959698	8000.063222	13.790195	-0.070452	4.818453
350.629100	7999.900273	13.795200	-0.070390	4.818406
350.826339	7999.956449	13.800205	-0.070427	4.818422
350.868967	7999.829965	13.805210	-0.070435	4.818384
350.755403	7999.934511	13.810215	-0.070414	4.818416
350.821502	8000.025696	13.815219	-0.070426	4.818443
351.169414	7999.945272	13.820224	-0.070491	4.818418
350.771711	8000.025039	13.825229	-0.070417	4.818443
350.971707	7999.944748	13.830234	-0.070454	4.818418
351.076383	7999.972394	13.835239	-0.070474	4.818426
351.096491	7999.999965	13.840243	-0.070478	4.818434
351.163038	7999.903199	13.845248	-0.070490	4.818405
351.229102	7999.981783	13.850253	-0.070502	4.818428
351.185959	7999.839456	13.855258	-0.070494	4.818386
350.743677	7999.871380	13.860263	-0.070412	4.818397
351.082571	7999.919990	13.865267	-0.070475	4.818410
351.079973	7999.945159	13.870272	-0.070475	4.818418
350.861489	7999.981108	13.875277	-0.070434	4.818429
350.913450	7999.905149	13.880282	-0.070444	4.818407
350.966786	7999.982514	13.885287	-0.070454	4.818429
350.925088	7999.906359	13.890291	-0.070446	4.818407
351.063639	7999.911354	13.895296	-0.070472	4.818408
351.027437	8000.046331	13.900301	-0.070465	4.818448
351.028336	7999.925591	13.905306	-0.070465	4.818412
351.028642	7999.951849	13.910311	-0.070465	4.818420
351.135452	7999.938571	13.915315	-0.070485	4.818416
351.223437	8000.094102	13.920320	-0.070502	4.818462
351.051768	8000.010967	13.925325	-0.070470	4.818438
351.145746	8000.011170	13.930330	-0.070487	4.818437
350.982553	8000.051004	13.935335	-0.070457	4.818450
350.956639	7999.888955	13.940339	-0.070452	4.818402
350.630226	7999.862568	13.945344	-0.070391	4.818395
350.683265	7999.912627	13.950349	-0.070401	4.818410
350.751580	7999.947139	13.955354	-0.070414	4.818420
350.826146	8000.014286	13.960359	-0.070428	4.818439
350.649648	7999.978341	13.965363	-0.070395	4.818429
350.921950	7999.988264	13.970368	-0.070446	4.818431
350.940630	7999.922363	13.975373	-0.070450	4.818412
350.948676	7999.847920	13.980378	-0.070451	4.818389
351.008582	7999.942172	13.985383	-0.070462	4.818417
351.110220	7999.931976	13.990387	-0.070481	4.818414
351.116606	8000.002417	13.995392	-0.070482	4.818435
351.180381	8000.031619	14.000397	-0.070494	4.818443
351.357436	7999.829217	14.005402	-0.070527	4.818382
351.234818	7999.923144	14.010407	-0.070505	4.818411
351.350240	7999.926781	14.015411	-0.070526	4.818411
351.366199	7999.979499	14.020416	-0.070529	4.818427
351.177310	7999.950738	14.025421	-0.070494	4.818419
351.006860	7999.743718	14.030426	-0.070462	4.818358
351.355210	8000.054965	14.035431	-0.070527	4.818449
351.311071	7999.919974	14.040435	-0.070519	4.818409
351.487802	7999.914977	14.045440	-0.070552	4.818407
351.346901	8000.045412	14.050445	-0.070526	4.818447
351.290417	7999.859855	14.055450	-0.070515	4.818392
351.256384	7999.906657	14.060455	-0.070509	4.818406
350.812896	7999.916513	14.065459	-0.070426	4.818410
350.934154	7999.937029	14.070464	-0.070449	4.818416
350.690108	7999.836134	14.075469	-0.070404	4.818387
350.688713	7999.772067	14.080474	-0.070403	4.818368
350.640959	7999.854387	14.085479	-0.070395	4.818393
350.988850	7999.907316	14.090483	-0.070459	4.818407
351.031009	8000.071686	14.095488	-0.070467	4.818456
350.784207	8000.054756	14.100493	-0.070421	4.818452
350.997141	8000.035539	14.105498	-0.070461	4.818445
351.349672	8000.080133	14.110503	-0.070527	4.818457
351.106910	7999.926750	14.115507	-0.070482	4.818412
350.937135	7999.975947	14.120512	-0.070450	4.818428
351.043619	7999.905963	14.125517	-0.070470	4.818406
351.029299	7999.912076	14.130522	-0.070467	4.818408
350.763688	8000.029301	14.135527	-0.070418	4.818444
351.116846	7999.939496	14.140531	-0.070484	4.818416
351.294754	7999.964966	14.145536	-0.070517	4.818423
351.250074	8000.022127	14.150541	-0.070509	4.818440
351.253496	7999.846818	14.155546	-0.070509	4.818388
351.176680	7999.961304	14.160551	-0.070495	4.818422
351.383975	8000.063819	14.165555	-0.070534	4.818452
351.287853	7999.915535	14.170560	-0.070516	4.818408
351.097472	7999.961309	14.175565	-0.070480	4.818423
351.413098	7999.809052	14.180570	-0.070539	4.818376
351.308489	8000.019773	14.185575	-0.070520	4.818439
351.328616	7999.937089	14.190579	-0.070523	4.818414
351.362235	7999.981641	14.195584	-0.070530	4.818428
350.901357	8000.026967	14.200589	-0.070444	4.818443
351.344459	7999.898456	14.205594	-0.070526	4.818403
351.178129	7999.921448	14.210599	-0.070496	4.818410
351.180935	8000.056945	14.215603	-0.070496	4.818451
351.240616	7999.863482	14.220608	-0.070507	4.818393
351.435981	8000.043542	14.225613	-0.070544	4.818446
351.501461	7999.884807	14.230618	-0.070556	4.818398
351.221932	8000.063801	14.235623	-0.070504	4.818453
350.828038	7999.833857	14.240627	-0.070431	4.818386
351.025138	7999.817579	14.245632	-0.070467	4.818380
350.561125	7999.935317	14.250637	-0.070381	4.818417
351.021987	7999.897346	14.255642	-0.070467	4.818404
351.064793	7999.929419	14.260647	-0.070475	4.818413
351.257882	8000.093697	14.265651	-0.070511	4.818461
350.940671	7999.998127	14.270656	-0.070452	4.818434
351.002211	8000.141754	14.275661	-0.070463	4.818477
351.239323	7999.913900	14.280666	-0.070507	4.818408
350.990539	7999.864393	14.285671	-0.070461	4.818394
351.122759	7999.896605	14.290675	-0.070486	4.818403
350.868327	7999.843873	14.295680	-0.070438	4.818389
350.511631	7999.936787	14.300685	-0.070372	4.818418
350.510929	7999.764576	14.305690	-0.070372	4.818366
350.574987	7999.952335	14.310695	-0.070384	4.818422
350.934787	7999.948721	14.315699	-0.070451	4.818419
351.000773	7999.802596	14.320704	-0.070463	4.818376
350.824689	7999.917861	14.325709	-0.070431	4.818411
350.794942	7999.862867	14.330714	-0.070425	4.818394
351.049265	7999.934503	14.335719	-0.070473	4.818415
350.542643	7999.845868	14.340723	-0.070378	4.818390
351.035659	7999.910177	14.345728	-0.070470	4.818408
350.733811	7999.924017	14.350733	-0.070414	4.818413
350.708667	7999.856483	14.355738	-0.070409	4.818393
350.681974	7999.864532	14.360743	-0.070404	4.818395
350.064298	7999.835325	14.365747	-0.070289	4.818389
350.464389	7999.772393	14.370752	-0.070364	4.818369
349.886183	7999.881264	14.375757	-0.070256	4.818403
350.524643	7999.506497	14.380762	-0.070375	4.818290

350.675648	7996.387142	14.385767	-0.070401	4.817361
350.215447	7990.827580	14.390771	-0.070312	4.815710
350.331149	7984.059577	14.395776	-0.070329	4.813695
349.964282	7976.863572	14.400781	-0.070256	4.811554
350.482181	7969.122360	14.405786	-0.070347	4.809247
350.331537	7961.422508	14.410791	-0.070314	4.806953
350.035410	7953.461826	14.415795	-0.070254	4.804581
350.306968	7945.585249	14.420800	-0.070300	4.802231
350.568513	7937.515673	14.425805	-0.070343	4.799822
350.798894	7929.577240	14.430810	-0.070381	4.797451
350.575410	7921.558065	14.435815	-0.070334	4.795057
350.542281	7913.599431	14.440819	-0.070323	4.792678
350.732261	7905.609646	14.445824	-0.070353	4.790289
350.745291	7897.546747	14.450829	-0.070350	4.787877
350.785842	7889.540350	14.455834	-0.070352	4.785480
350.635369	7881.574529	14.460839	-0.070319	4.783095
350.434987	7873.609111	14.465843	-0.070277	4.780709
350.521805	7865.579832	14.470848	-0.070288	4.778302
350.401455	7857.555657	14.475853	-0.070260	4.775896
350.683514	7849.575873	14.480858	-0.070308	4.773501
350.279425	7841.607019	14.485863	-0.070227	4.771110
350.191432	7833.492496	14.490867	-0.070205	4.768673
350.006580	7825.596280	14.495872	-0.070166	4.766300
350.168637	7817.470467	14.500877	-0.070191	4.763857
350.139083	7809.605462	14.505882	-0.070180	4.761491
349.864880	7801.541119	14.510887	-0.070124	4.759065
350.076372	7793.580392	14.515891	-0.070158	4.756667
350.002051	7785.541518	14.520896	-0.070139	4.754245
350.056833	7777.540934	14.525901	-0.070144	4.751833
350.299573	7769.484788	14.530906	-0.070184	4.749403
349.825826	7761.545215	14.535911	-0.070091	4.747009
349.344938	7753.512602	14.540915	-0.069996	4.744585
349.630269	7745.555885	14.545920	-0.070044	4.742181
349.729564	7737.479938	14.550925	-0.070057	4.739740
349.914108	7729.516055	14.555930	-0.070087	4.737332
349.882669	7721.463949	14.560935	-0.070076	4.734896
350.315728	7713.485990	14.565939	-0.070151	4.732480
350.306519	7705.466962	14.570944	-0.070144	4.730052
350.029130	7697.489609	14.575949	-0.070087	4.727636
350.186511	7689.457182	14.580954	-0.070111	4.725200
350.054366	7681.509558	14.585959	-0.070082	4.722790
349.792995	7673.536552	14.590963	-0.070028	4.720371
350.002758	7665.538321	14.595968	-0.070062	4.717943
350.166290	7657.522326	14.600973	-0.070087	4.715508
350.223271	7649.469852	14.605978	-0.070092	4.713060
349.993700	7641.550586	14.610983	-0.070044	4.710653
350.157864	7633.451512	14.615987	-0.070070	4.708188
350.097000	7625.535117	14.620992	-0.070053	4.705779
350.056040	7617.478381	14.625997	-0.070041	4.703325
350.167210	7609.580110	14.631002	-0.070056	4.700918
349.937244	7601.511579	14.636007	-0.070008	4.698459
350.131038	7593.517394	14.641011	-0.070039	4.696020
350.173525	7585.504302	14.646016	-0.070042	4.693575
349.574814	7577.518967	14.651021	-0.069925	4.691137
349.672930	7569.487918	14.656026	-0.069938	4.688684
349.394003	7561.568274	14.661031	-0.069881	4.686263
349.697102	7553.445061	14.666035	-0.069932	4.683779
349.898268	7545.560430	14.671040	-0.069965	4.681366
349.831606	7537.436583	14.676045	-0.069947	4.678879
349.783120	7529.606518	14.681050	-0.069933	4.676481
349.881841	7521.470117	14.686055	-0.069946	4.673987
349.417945	7513.470523	14.691059	-0.069854	4.671534
349.699095	7505.435606	14.696064	-0.069902	4.669069
349.683428	7497.420768	14.701069	-0.069893	4.666609
349.382782	7489.448524	14.706074	-0.069832	4.664161
349.522874	7481.460601	14.711079	-0.069853	4.661706
349.648446	7473.444345	14.716083	-0.069871	4.659242
349.323352	7465.548820	14.721088	-0.069806	4.656813
349.533193	7457.401052	14.726093	-0.069840	4.654306
349.481677	7449.478578	14.731098	-0.069825	4.651866
349.739583	7441.468027	14.736103	-0.069868	4.649398
349.629609	7433.428379	14.741107	-0.069842	4.646920
349.656945	7425.432455	14.746112	-0.069842	4.644454
349.592842	7417.498502	14.751117	-0.069825	4.642006
349.184778	7409.505425	14.756122	-0.069744	4.639538
348.976839	7401.535725	14.761127	-0.069700	4.637076
349.400049	7393.392748	14.766131	-0.069773	4.634559
349.560947	7385.500721	14.771136	-0.069798	4.632119
349.092031	7377.438395	14.776141	-0.069706	4.629624
349.201846	7369.410718	14.781146	-0.069721	4.627139
349.471457	7361.409141	14.786151	-0.069766	4.624660
349.157736	7353.482627	14.791155	-0.069702	4.622204
349.151942	7345.476123	14.796160	-0.069696	4.619721
348.794598	7337.498038	14.801165	-0.069625	4.617246
348.830690	7329.425689	14.806170	-0.069626	4.614740
349.004798	7321.449741	14.811175	-0.069653	4.612263
348.852166	7313.359583	14.816179	-0.069620	4.609749
348.996864	7305.425444	14.821184	-0.069641	4.607282
348.745794	7297.368553	14.826189	-0.069589	4.604775
348.849397	7289.454152	14.831194	-0.069604	4.602312
348.758455	7281.418475	14.836199	-0.069582	4.599810
348.468545	7273.433145	14.841203	-0.069522	4.597321
348.565361	7265.436507	14.846208	-0.069535	4.594828
348.698179	7257.400985	14.851213	-0.069555	4.592322
348.488008	7249.410483	14.856218	-0.069510	4.589828
348.497055	7241.400313	14.861223	-0.069507	4.587326
348.347827	7233.363385	14.866227	-0.069474	4.584815
348.555102	7225.394873	14.871232	-0.069507	4.582324
348.584327	7217.345813	14.876237	-0.069508	4.579807
348.519500	7209.371537	14.881242	-0.069490	4.577311
348.617621	7201.338861	14.886247	-0.069503	4.574796
348.408642	7193.352336	14.891251	-0.069459	4.572293
348.605918	7185.298959	14.896256	-0.069491	4.569769
348.602707	7177.317964	14.901261	-0.069485	4.567266
348.618618	7169.330284	14.906266	-0.069483	4.564759
348.533948	7161.381495	14.911271	-0.069462	4.562263
348.216773	7153.356315	14.916275	-0.069398	4.559741
348.601031	7145.413922	14.921280	-0.069464	4.557245
348.244115	7137.328541	14.926285	-0.069393	4.554702
348.370289	7129.379941	14.931290	-0.069411	4.552201
348.513019	7121.334426	14.936295	-0.069432	4.549668
348.221083	7113.366249	14.941299	-0.069373	4.547157
348.085412	7105.355739	14.946304	-0.069342	4.544631
348.147771	7097.360913	14.951309	-0.069349	4.542110
348.665593	7089.282452	14.956314	-0.069440	4.539562
348.532950	7081.372314	14.961319	-0.069410	4.537064
348.348373	7073.300102	14.966323	-0.069371	4.534514
348.528833	7065.365366	14.971328	-0.069399	4.532006
348.387328	7057.285064	14.976333	-0.069367	4.529450
348.407001	7049.352806	14.981338	-0.069366	4.526940
348.423192	7041.285006	14.986343	-0.069364	4.524385
348.273993	7033.344615	14.991347	-0.069331	4.521869
348.046270	7025.361272	14.996352	-0.069283	4.519338
348.032942	7017.351710	15.001357	-0.069276	4.516798
347.852404	7009.322885	15.006362	-0.069237	4.514249
347.727168	7001.355082	15.011367	-0.069208	4.511719
347.316387	6993.322274	15.016371	-0.069127	4.509165
347.443633	6985.306773	15.021376	-0.069145	4.506618
347.581855	6977.194564	15.026381	-0.069166	4.504038
347.735273	6969.246638	15.031386	-0.069189	4.501509
347.961960	6961.225803	15.036391	-0.069226	4.498956
348.104598	6953.206534	15.041395	-0.069247	4.496402
347.835108	6945.292770	15.046400	-0.069192	4.493878
347.533732	6937.282198	15.051405	-0.069131	4.491322
347.732816	6929.266078	15.056410	-0.069163	4.488764
347.928651	6921.265250	15.061415	-0.069194	4.486210
347.668999	6913.220137	15.066419	-0.069140	4.483638
348.034665	6905.305238	15.071424	-0.069203	4.481109
347.825000	6897.215044	15.076429	-0.069159	4.478521
347.665862	6889.307386	15.081434	-0.069124	4.475989
347.521259	6881.258857	15.086439	-0.069092	4.473411
347.574960	6873.267779	15.091443	-0.069097	4.470851
347.840839	6865.277283	15.096448	-0.069141	4.468290
347.618059	6857.221434	15.101453	-0.069095	4.465705
347.714822	6849.232784	15.106458	-0.069108	4.463141
347.529560	6841.258688	15.111463	-0.069068	4.460579
347.258093	6833.310940	15.116467	-0.069012	4.458024
347.608270	6825.247790	15.121472	-0.069072	4.455433
347.653209	6817.192913	15.126477	-0.069075	4.452841
347.603241	6809.202362	15.131482	-0.069061	4.450269
347.161322	6801.293361	15.136487	-0.068974	4.447719
346.904526	6793.210848	15.141491	-0.068920	4.445113
347.412097	6785.216678	15.146496	-0.069010	4.442537
346.992456	6777.230471	15.151501	-0.068926	4.439958
347.357131	6769.216796	15.156506	-0.068989	4.437373
347.459027	6761.198518	15.161511	-0.069003	4.434783
347.092202	6753.212122	15.166515	-0.068930	4.432200
347.289074	6745.191952	15.171520	-0.068961	4.429607
347.061896	6737.255107	15.176525	-0.068914	4.427037
346.828865	6729.164030	15.181530	-0.068865	4.424416
347.014286	6721.234217	15.186535	-0.068894	4.421848
346.879694	6713.162547	15.191539	-0.068864	4.419230
347.063833	6705.194842	15.196544	-0.068893	4.416647
346.772588	6697.149058	15.201549	-0.068834	4.414034
346.996272	6689.200534	15.206554	-0.068870	4.411454
346.922416	6681.111331	15.211559	-0.068851	4.408825
347.031168	6673.162736	15.216563	-0.068866	4.406241
347.283301	6665.199732	15.221568	-0.068908	4.403652
347.181809	6657.206888	15.226573	-0.068884	4.401049
347.246891	6649.205046	15.231578	-0.068891	4.398444
347.061030	6641.312443	15.236583	-0.068851	4.395870
347.218010	6633.222512	15.241587	-0.068875	4.393233
347.235302	6625.252087	15.246592	-0.068873	4.390632
346.981744	6617.262219	15.251597	-0.068821	4.388022
346.996364	6609.231624	15.256602	-0.068819	4.385399
347.125522	6601.246445	15.261607	-0.068837	4.382789
346.991228	6593.246640	15.266611	-0.068807	4.380172
347.019133	6585.290239	15.271616	-0.068807	4.377568
346.987042	6577.244529	15.276621	-0.068796	4.374933
346.756687	6569.302219	15.281626	-0.068748	4.372329
346.486774	6561.277062	15.286631	-0.068693	4.369696
347.126238	6553.227578	15.291635	-0.068806	4.367060
347.043370	6545.228022	15.296640	-0.068786	4.364433
346.778337	6537.298166	15.301645	-0.068731	4.361826
346.801981	6529.279355	15.306650	-0.068731	4.359191
346.727408	6521.342578	15.311655	-0.068712	4.356581
346.366105	6513.312772	15.316659	-0.068639	4.353936
346.580707	6505.264384	15.321664	-0.068674	4.351287
346.705061	6497.229534	15.326669	-0.068692	4.348641
346.487816	6489.276600	15.331674	-0.068646	4.346018
346.435876	6481.228171	15.336679	-0.068631	4.343362
346.325501	6473.288201	15.341683	-0.068606	4.340741
346.598634	6465.223908	15.346688	-0.068651	4.338080
346.380378	6457.267897	15.351693	-0.068606	4.335449
346.372923	6449.241851	15.356698	-0.068599	4.332795
346.524906	6441.262113	15.361703	-0.068622	4.330156
346.156746	6433.260410	15.366707	-0.068548	4.327504
346.022444	6425.307893	15.371712	-0.068518	4.324868
345.997474	6417.278459	15.376717	-0.068508	4.322206
346.135081	6409.289409	15.381722	-0.068529	4.319557
346.016937	6401.271276	15.386727	-0.068502	4.316895
346.139766	6393.252912	15.391731	-0.068519	4.314233
346.420385	6385.212842	15.396736	-0.068566	4.311564
346.174797	6377.221363	15.401741	-0.068515	4.308905
345.939240	6369.230910	15.406746	-0.068466	4.306244
346.063601	6361.223813	15.411751	-0.068484	4.303580
345.357600	6353.293361	15.416755	-0.068348	4.300932
346.081328	6345.210892	15.421760	-0.068477	4.298244
346.379290	6337.148420	15.426765	-0.068528	4.295557
346.524926	6329.178245	15.431770	-0.068550	4.292899
346.257915	6321.199945	15.436775	-0.068495	4.290232
346.331054	6313.186529	15.441779	-0.068503	4.287555
346.200003	6305.255633	15.446784	-0.068474	4.284902
345.481314	6297.327468	15.451789	-0.068335	4.282242
345.419825	6289.245275	15.456794	-0.068318	4.279536
345.570797	6281.300090	15.461799	-0.068341	4.276876
345.404950	6273.213346	15.466803	-0.068305	4.274163
345.826614	6265.220083	15.471808	-0.068378	4.271486
345.805564	6257.141248	15.476813	-0.068369	4.268774
345.845626	6249.214471	15.481818	-0.068371	4.266112
345.739574	6241.177110	15.486823	-0.068346	4.263410
345.738044	6233.165016	15.491827	-0.068341	4.260716
346.039004	6225.181484	15.496832	-0.068392	4.258033
345.821924	6217.173852	15.501837	-0.068346	4.255334
345.539378	6209.225239	15.506842	-0.068288	4.252653
345.915182	6201.183149	15.511847	-0.068353	4.249946
345.636713	6193.207596	15.516851	-0.068296	4.247253
345.429029	6185.224884	15.521856	-0.068252	4.244556
345.646779	6177.212964	15.526861	-0.068288	4.241852
345.707559	6169.160156	15.531866	-0.068294	4.239131
345.550677	6161.281714	15.536871	-0.068260	4.236465
345.696984	6153.157153	15.541875	-0.068282	4.233717
345.777009	6145.197509	15.546880	-0.068291	4.231022
345.704353	6137.154741	15.551885	-0.068273	4.228296
345.576985	6129.159449	15.556890	-0.068244	4.225584
345.982770	6121.166902	15.561895	-0.068314	4.222876
345.728419	6113.186915	15.566899	-0.068262	4.220164
345.602258	6105.213504	15.571904	-0.068233	4.217454
345.557499	6097.216904	15.576909	-0.068219	4.214735
345.249409	6089.305734	15.581914	-0.068157	4.212040
345.313533	6081.188454	15.586919	-0.068164	4.209278
345.168871	6073.156750	15.591923	-0.068131	4.206541
345.619140	6065.119536	15.596928	-0.068210	4.203806
345.539312	6057.202262	15.601933	-0.068190	4.201105
345.421002	6049.216438	15.606938	-0.068163	4.198378
345.333230	6041.218365	15.611943	-0.068141	4.195646
345.065308	6033.155927	15.616947	-0.068086	4.192888
345.157900	6025.161307	15.621952	-0.068098	4.190155
344.816964	6017.165944	15.626957	-0.068030	4.187415
344.555231	6009.154055	15.631962	-0.067976	4.184669
344.719809	6001.183585	15.636967	-0.068001	4.181940
344.887693	5993.107085	15.641971	-0.068027	4.179173
344.979317	5985.194138	15.646976	-0.068039	4.176459
344.917750	5977.141767	15.651981	-0.068023	4.173694
344.827749	5969.189361	15.656986	-0.068001	4.170961
344.915043	5961.181343	15.661991	-0.068012	4.168209
344.915256	5953.142728	15.666995	-0.068007	4.165444
345.049618	5945.152623	15.672000	-0.068026	4.162695
344.951097	5937.171752	15.677005	-0.068003	4.159945
344.919749	5929.205504	15.682010	-0.067992	4.157199
344.967990	5921.202681	15.687015	-0.067996	4.154440
344.785431	5913.227320	15.692019	-0.067957	4.151685
344.914429	5905.197780	15.697024	-0.067975	4.148913
345.019535	5897.190714	15.702029	-0.067990	4.146148
344.825246	5889.198471	15.707034	-0.067948	4.143381
344.652026	5881.272179	15.712039	-0.067911	4.140636
344.503930	5873.218678	15.717043	-0.067878	4.137845
344.581933	5865.230447	15.722048	-0.067888	4.135078
344.388390	5857.182413	15.727053	-0.067846	4.132285
344.709089	5849.173031	15.732058	-0.067901	4.129510
344.654730	5841.232064	15.737063	-0.067886	4.126752
344.539403	5833.164985	15.742067	-0.067859	4.123948
344.474977	5825.300719	15.747072	-0.067842	4.121212
344.164656	5817.271131	15.752077	-0.067779	4.118415
343.987551	5809.234670	15.757082	-0.067741	4.115614
344.167690	5801.227113	15.762087	-0.067769	4.112827
344.159358	5793.204731	15.767091	-0.067762	4.110030
344.070965	5785.249197	15.772096	-0.067741	4.107253
344.410830	5777.123500	15.777101	-0.067799	4.104421
344.431066	5769.232484	15.782106	-0.067797	4.101665
344.284817	5761.212526	15.787111	-0.067765	4.098859
343.871671	5753.226942	15.792115	-0.067683	4.096059
344.292498	5745.173327	15.797120	-0.067756	4.093246
344.193581	5737.208119	15.802125	-0.067733	4.090455
344.262616	5729.177294	15.807130	-0.067740	4.087640
344.208232	5721.168714	15.812135	-0.067725	4.084830
344.129774	5713.219142	15.817139	-0.067705	4.082039
344.197223	5705.199581	15.822144	-0.067712	4.079222
343.717367	5697.254057	15.827149	-0.067618	4.076422
343.911055	5689.185211	15.832154	-0.067649	4.073587
344.050486	5681.243928	15.837159	-0.067670	4.070794
343.958136	5673.169173	15.842163	-0.067647	4.067948
343.988328	5665.180697	15.847168	-0.067648	4.065133
343.852006	5657.213829	15.852173	-0.067617	4.062320
343.855798	5649.200454	15.857178	-0.067613	4.059492
343.983258	5641.243798	15.862183	-0.067631	4.056683
343.828310	5633.216742	15.867187	-0.067597	4.053843
343.641271	5625.263856	15.872192	-0.067557	4.051027
343.879775	5617.168085	15.877197	-0.067596	4.048165
343.695175	5609.191968	15.882202	-0.067557	4.045337
343.904173	5601.247908	15.887207	-0.067591	4.042525
343.413720	5593.275649	15.892211	-0.067494	4.039689
343.403191	5585.297192	15.897216	-0.067487	4.036857
343.202271	5577.260940	15.902221	-0.067444	4.033999
343.257866	5569.200351	15.907226	-0.067450	4.031134
343.643877	5561.131233	15.912231	-0.067516	4.028270
343.573456	5553.153549	15.917235	-0.067498	4.025429
343.508615	5545.205806	15.922240	-0.067481	4.022597
343.390377	5537.229399	15.927245	-0.067454	4.019751
343.251433	5529.263159	15.932250	-0.067423	4.016907
343.239363	5521.260856	15.937255	-0.067415	4.014050
343.263854	5513.246822	15.942259	-0.067415	4.011188
343.206243	5505.246738	15.947264	-0.067399	4.008327
343.270723	5497.207367	15.952269	-0.067405	4.005452
343.238212	5489.236760	15.957274	-0.067394	4.002598
342.966047	5481.331197	15.962279	-0.067338	3.999761
343.085503	5473.295970	15.967283	-0.067355	3.996882
342.924417	5465.323468	15.972288	-0.067320	3.994019
343.138395	5457.258685	15.977293	-0.067355	3.991127
342.960783	5449.247305	15.982298	-0.067317	3.988245
343.180697	5441.238079	15.987303	-0.067352	3.985369
343.104559	5433.262020	15.992307	-0.067333	3.982498
343.101980	5425.272544	15.997312	-0.067327	3.979621
343.136260	5417.306093	16.002317	-0.067329	3.976751
343.265389	5409.216937	16.007322	-0.067347	3.973836
342.716155	5401.332512	16.012327	-0.067240	3.970981
342.669065	5393.268241	16.017331	-0.067226	3.968068
342.876992	5385.248114	16.022336	-0.067260	3.965173
343.064942	5377.269283	16.027341	-0.067289	3.962291
342.892261	5369.271245	16.032346	-0.067252	3.959393
342.842742	5361.354770	16.037351	-0.067238	3.956525
342.969488	5353.227603	16.042355	-0.067256	3.953582
342.831074	5345.297199	16.047360	-0.067225	3.950702
342.864126	5337.262415	16.052365	-0.067226	3.947786
342.544754	5329.266269	16.057370	-0.067162	3.944876
342.840003	5321.275381	16.062375	-0.067211	3.941976
342.422110	5313.253388	16.067379	-0.067128	3.939050
342.673110	5305.307372	16.072384	-0.067170	3.936162
342.722613	5297.243112	16.077389	-0.067174	3.933225
342.553214	5289.265649	16.082394	-0.067137	3.930313
342.605185	5281.297089	16.087399	-0.067142	3.927406
342.655673	5273.228512	16.092403	-0.067146	3.924461
342.639007	5265.326671	16.097408	-0.067138	3.921573
342.512001	5257.317903	16.102413	-0.067109	3.918642
342.331281	5249.348751	16.107418	-0.067070	3.915722
342.231613	5241.381290	16.112423	-0.067046	3.912802
342.358624	5233.275679	16.117427	-0.067065	3.909834
342.452520	5225.320047	16.122432	-0.067077	3.906917
342.412054	5217.301921	16.127437	-0.067064	3.903973
342.457395	5209.348927	16.132442	-0.067068	3.901053
342.566096	5201.347491	16.137447	-0.067083	3.898113
342.112809	5193.370890	16.142451	-0.066993	3.895169
342.510805	5185.313142	16.147456	-0.067062	3.892211
342.465672	5177.311157	16.152461	-0.067049	3.889261
342.487477	5169.338654	16.157466	-0.067047	3.886322
342.349271	5161.370900	16.162471	-0.067017	3.883379
342.229592	5153.334704	16.167475	-0.066989	3.880409
342.541684	5145.381946	16.172480	-0.067042	3.877476
342.462760	5137.378509	16.177485	-0.067022	3.874514
342.214593	5129.292944	16.182490	-0.066971	3.871516
342.014412	5121.292768	16.187495	-0.066928	3.868548
342.064220	5113.261106	16.192499	-0.066932	3.865572
342.008213	5105.356863	16.197504	-0.066917	3.862638
341.930989	5097.353959	16.202509	-0.066897	3.859665
341.445859	5089.380584	16.207514	-0.066802	3.856692
342.210192	5081.283986	16.212519	-0.066939	3.853697
341.860685	5073.357263	16.217523	-0.066869	3.850740
341.743522	5065.403258	16.222528	-0.066842	3.847775
341.727878	5057.351597	16.227533	-0.066834	3.844773
341.807961	5049.397718	16.232538	-0.066843	3.841808
342.228963	5041.346469	16.237543	-0.066917	3.838811
342.052083	5033.410666	16.242547	-0.066878	3.835843
341.802987	5025.403533	16.247552	-0.066827	3.832843
341.542636	5017.408449	16.252557	-0.066773	3.829846
341.762805	5009.348840	16.257562	-0.066809	3.826833
341.659059	5001.363828	16.262567	-0.066785	3.823838
341.738070	4993.379242	16.267571	-0.066794	3.820845
341.842705	4985.379403	16.272576	-0.066808	3.817844
341.835862	4977.410765	16.277581	-0.066802	3.814850
341.749889	4969.370137	16.282586	-0.066781	3.811825
341.954317	4961.331705	16.287591	-0.066814	3.808806
341.837360	4953.401044	16.292595	-0.066787	3.805817
341.956099	4945.376252	16.297600	-0.066804	3.802795
341.776842	4937.408195	16.302605	-0.066765	3.799786
341.860397	4929.428012	16.307610	-0.066775	3.796776
341.982081	4921.384875	16.312615	-0.066793	3.793740
341.797420	4913.418953	16.317619	-0.066753	3.790724
341.553122	4905.477979	16.322624	-0.066703	3.787714
341.578514	4897.431158	16.327629	-0.066702	3.784667
341.345328	4889.459548	16.332634	-0.066654	3.781641
341.376284	4881.484580	16.337639	-0.066654	3.778617
341.470428	4873.435585	16.342643	-0.066667	3.775564
341.559223	4865.418045	16.347648	-0.066678	3.772520
341.529470	4857.460353	16.352653	-0.066667	3.769494
341.567234	4849.441665	16.357658	-0.066669	3.766444
341.577174	4841.460722	16.362663	-0.066666	3.763405
341.536732	4833.473043	16.367667	-0.066653	3.760360
341.645806	4825.522446	16.372672	-0.066668	3.757330
341.423759	4817.526571	16.377677	-0.066622	3.754272
341.182575	4809.527102	16.382682	-0.066572	3.751210
341.347482	4801.500069	16.387687	-0.066597	3.748145
341.272662	4793.484357	16.392691	-0.066578	3.745076
341.443604	4785.522140	16.397696	-0.066605	3.742031
341.208086	4777.505524	16.402701	-0.066556	3.738952
341.293099	4769.490270	16.407706	-0.066566	3.735879
341.333074	4761.513774	16.412711	-0.066569	3.732818
341.145196	4753.486407	16.417715	-0.066528	3.729729
341.279830	4745.530674	16.422720	-0.066548	3.726672
340.855791	4737.550814	16.427725	-0.066464	3.723590
341.078309	4729.561082	16.432730	-0.066501	3.720518
340.849086	4721.594755	16.437735	-0.066453	3.717441
340.906703	4713.480245	16.442739	-0.066458	3.714312
340.968660	4705.473280	16.447744	-0.066465	3.711221
340.746776	4697.498343	16.452749	-0.066418	3.708133
340.747393	4689.471713	16.457754	-0.066413	3.705029
340.998299	4681.537411	16.462759	-0.066455	3.701963
340.718181	4673.516412	16.467763	-0.066397	3.698848
340.598893	4665.592852	16.472768	-0.066370	3.695772
340.601671	4657.562361	16.477773	-0.066365	3.692656
340.461011	4649.547579	16.482778	-0.066334	3.689539
340.643013	4641.546590	16.487783	-0.066363	3.686433
340.649105	4633.520156	16.492787	-0.066359	3.683310
340.482901	4625.610081	16.497792	-0.066322	3.680225
340.170326	4617.640694	16.502797	-0.066259	3.677111
340.385750	4609.559488	16.507802	-0.066294	3.673964
340.473386	4601.648194	16.512807	-0.066305	3.670878
340.058807	4593.592980	16.517811	-0.066223	3.667719
340.264340	4585.583270	16.522816	-0.066256	3.664592
340.025897	4577.646272	16.527821	-0.066206	3.661479
340.417583	4569.587748	16.532826	-0.066274	3.658332
340.383057	4561.623899	16.537831	-0.066262	3.655209
340.220788	4553.637669	16.542835	-0.066227	3.652070
340.453883	4545.590055	16.547840	-0.066265	3.648916
340.319108	4537.675268	16.552845	-0.066235	3.645800
340.240662	4529.647529	16.557850	-0.066215	3.642640
340.437501	4521.688900	16.562855	-0.066247	3.639511
339.956917	4513.726609	16.567859	-0.066152	3.636360
339.903710	4505.695879	16.572864	-0.066137	3.633190
340.100032	4497.675688	16.577869	-0.066168	3.630029
339.689651	4489.708261	16.582874	-0.066087	3.626869
339.753934	4481.687813	16.587879	-0.066094	3.623699
339.493463	4473.726935	16.592883	-0.066040	3.620540
339.643685	4465.689101	16.597888	-0.066063	3.617359
339.261267	4457.726774	16.602893	-0.065986	3.614191
339.269491	4449.704699	16.607898	-0.065983	3.611007
339.426904	4441.692972	16.612903	-0.066007	3.607829
339.154750	4433.724326	16.617907	-0.065951	3.604652
339.008807	4425.766919	16.622912	-0.065919	3.601481
339.112187	4417.766163	16.627917	-0.065933	3.598298
339.240382	4409.726785	16.632922	-0.065951	3.595096
339.024483	4401.793429	16.637927	-0.065906	3.591924
338.786145	4393.751640	16.642931	-0.065857	3.588706
339.367341	4385.695400	16.647936	-0.065960	3.585502
339.383637	4377.709967	16.652941	-0.065957	3.582308
339.406549	4369.668041	16.657946	-0.065956	3.579088
339.622077	4361.729500	16.662951	-0.065991	3.575913
339.283806	4353.758539	16.667955	-0.065923	3.572705
339.496808	4345.733251	16.672960	-0.065958	3.569489
339.659731	4337.771680	16.677965	-0.065983	3.566294
339.378130	4329.829813	16.682970	-0.065925	3.563091
339.254209	4321.853049	16.687975	-0.065897	3.559876
339.338477	4313.856128	16.692979	-0.065908	3.556656
339.350745	4305.823931	16.697984	-0.065905	3.553416
339.280025	4297.796889	16.702989	-0.065886	3.550173
338.649979	4289.857089	16.707994	-0.065764	3.546946
338.983193	4281.827765	16.712999	-0.065821	3.543708
339.171017	4273.795229	16.718003	-0.065851	3.540463
338.971150	4265.862253	16.723008	-0.065808	3.537242
338.805328	4257.850868	16.728013	-0.065772	3.533987
338.912249	4249.826577	16.733018	-0.065787	3.530733
339.224296	4241.819050	16.738023	-0.065840	3.527490
339.146038	4233.812316	16.743027	-0.065820	3.524231
338.804981	4225.904072	16.748032	-0.065751	3.521001
339.097621	4217.880126	16.753037	-0.065801	3.517741
338.995319	4209.879171	16.758042	-0.065776	3.514475
338.937486	4201.934956	16.763047	-0.065761	3.511230
338.818823	4193.900570	16.768051	-0.065733	3.507943
338.847909	4185.891091	16.773056	-0.065734	3.504669
338.667330	4177.941530	16.778061	-0.065695	3.501409
339.014172	4169.880649	16.783066	-0.065754	3.498117
338.875489	4161.937380	16.788071	-0.065723	3.494855
338.448481	4153.959992	16.793075	-0.065639	3.491566
338.887606	4145.910397	16.798080	-0.065715	3.488273
338.519449	4137.975436	16.803085	-0.065641	3.484998
338.688139	4129.967809	16.808090	-0.065668	3.481707
338.468528	4122.032293	16.813095	-0.065622	3.478430
338.685486	4113.976794	16.818099	-0.065657	3.475114
338.629994	4106.015195	16.823104	-0.065641	3.471826
338.545667	4097.998568	16.828109	-0.065620	3.468510
338.356814	4089.987592	16.833114	-0.065580	3.465190
338.649588	4082.015204	16.838119	-0.065629	3.461899
338.405566	4074.010564	16.843123	-0.065579	3.458574
338.393346	4066.036122	16.848128	-0.065571	3.455265
338.755298	4058.007034	16.853133	-0.065634	3.451944
338.431055	4050.002958	16.858138	-0.065568	3.448606
338.477010	4042.046746	16.863143	-0.065571	3.445298
338.441281	4034.074942	16.868147	-0.065560	3.441977
338.447852	4026.068417	16.873152	-0.065556	3.438640
338.220909	4018.124222	16.878157	-0.065508	3.435317
338.620550	4010.031030	16.883162	-0.065577	3.431951
338.540759	4002.080419	16.888167	-0.065557	3.428625
338.282887	3994.095792	16.893171	-0.065504	3.425274
338.405840	3986.131862	16.898176	-0.065522	3.421943
338.184562	3978.178523	16.903181	-0.065476	3.418600
338.204748	3970.107145	16.908186	-0.065474	3.415214
338.069082	3962.162406	16.913191	-0.065444	3.411871
338.284566	3954.116398	16.918195	-0.065479	3.408495
338.215686	3946.155022	16.923200	-0.065461	3.405142
337.800538	3938.247262	16.928205	-0.065378	3.401795
338.003518	3930.188267	16.933210	-0.065411	3.398403
338.325253	3922.175124	16.938215	-0.065466	3.395032
337.963008	3914.137530	16.943219	-0.065393	3.391622
337.829270	3906.166038	16.948224	-0.065363	3.388245
338.214857	3898.135795	16.953229	-0.065429	3.384858
338.076434	3890.200536	16.958234	-0.065399	3.381490
337.812077	3882.249567	16.963239	-0.065344	3.378106
337.504921	3874.273664	16.968243	-0.065282	3.374708
337.803624	3866.224019	16.973248	-0.065332	3.371296
337.608623	3858.270777	16.978253	-0.065291	3.367904
337.516857	3850.260980	16.983258	-0.065269	3.364488
337.468126	3842.328777	16.988263	-0.065254	3.361104
337.388876	3834.313699	16.993267	-0.065234	3.357679
337.453902	3826.297832	16.998272	-0.065241	3.354256
337.532292	3818.318855	17.003277	-0.065251	3.350846
337.082766	3810.360239	17.008282	-0.065162	3.347421
337.209122	3802.314719	17.013287	-0.065180	3.343977
337.177723	3794.363390	17.018291	-0.065169	3.340564
337.254789	3786.358278	17.023296	-0.065178	3.337129
337.270454	3778.343612	17.028301	-0.065176	3.333684
337.066637	3770.341558	17.033306	-0.065133	3.330232
337.422643	3762.334854	17.038311	-0.065194	3.326795
336.922428	3754.389718	17.043315	-0.065096	3.323349
336.904204	3746.424299	17.048320	-0.065087	3.319910
337.006248	3738.431073	17.053325	-0.065101	3.316459
337.028368	3730.398506	17.058330	-0.065100	3.312984
336.940664	3722.410927	17.063335	-0.065079	3.309521
336.883730	3714.441927	17.068339	-0.065063	3.306064
337.067634	3706.399073	17.073344	-0.065092	3.302581
336.911430	3698.446505	17.078349	-0.065058	3.299119
336.826068	3690.500934	17.083354	-0.065037	3.295660
337.230291	3682.453159	17.088359	-0.065107	3.292172
336.838151	3674.461459	17.093363	-0.065028	3.288673
336.904553	3666.464345	17.098368	-0.065036	3.285187
337.076100	3658.493901	17.103373	-0.065062	3.281712
336.985246	3650.493158	17.108378	-0.065040	3.278210
336.807815	3642.557468	17.113383	-0.065002	3.274729
336.817354	3634.563898	17.118387	-0.064999	3.271227
336.969784	3626.546453	17.123392	-0.065022	3.267717
336.957888	3618.539297	17.128397	-0.065015	3.264200
336.730532	3610.608364	17.133402	-0.064967	3.260704
336.746994	3602.657667	17.138407	-0.064965	3.257206
336.821305	3594.616614	17.143411	-0.064974	3.253667
336.946984	3586.592208	17.148416	-0.064992	3.250133
336.910079	3578.641889	17.153421	-0.064980	3.246621
336.417310	3570.687942	17.158426	-0.064883	3.243085
336.817662	3562.660974	17.163431	-0.064952	3.239550
336.572256	3554.699954	17.168435	-0.064901	3.236014
336.407654	3546.728865	17.173440	-0.064866	3.232472
336.276566	3538.733902	17.178445	-0.064836	3.228917
336.140056	3530.708306	17.183450	-0.064805	3.225345
335.959643	3522.756161	17.188455	-0.064767	3.221799
336.069843	3514.715819	17.193459	-0.064782	3.218222
335.678379	3506.763047	17.198464	-0.064704	3.214660
335.956683	3498.740537	17.203469	-0.064751	3.211090
335.856326	3490.730295	17.208474	-0.064727	3.207506
335.947959	3482.739910	17.213479	-0.064739	3.203935
336.118997	3474.735423	17.218483	-0.064765	3.200357
336.071583	3466.793578	17.223488	-0.064751	3.196794
336.037327	3458.805126	17.228493	-0.064740	3.193207
335.954951	3450.799781	17.233498	-0.064719	3.189606
336.146262	3442.804016	17.238503	-0.064750	3.186017
335.833552	3434.865471	17.243507	-0.064686	3.182427
336.013322	3426.843788	17.248512	-0.064715	3.178818
335.840380	3418.875228	17.253517	-0.064677	3.175213
335.783840	3410.883713	17.258522	-0.064662	3.171598
335.883462	3402.856385	17.263527	-0.064675	3.167971
335.743625	3394.905797	17.268531	-0.064644	3.164363
335.983352	3386.894676	17.273536	-0.064683	3.160740
335.604911	3379.008526	17.278541	-0.064608	3.157143
335.515964	3370.971860	17.283546	-0.064586	3.153486
335.744705	3362.978264	17.288551	-0.064623	3.149858
335.722960	3354.970660	17.293555	-0.064614	3.146209
335.373401	3346.998766	17.298560	-0.064544	3.142557
335.112144	3339.052809	17.303565	-0.064490	3.138916
335.059589	3331.060588	17.308570	-0.064475	3.135260
335.073882	3323.071040	17.313575	-0.064473	3.131603
334.702720	3315.096045	17.318579	-0.064398	3.127932
334.803449	3307.051990	17.323584	-0.064412	3.124246
334.830312	3299.123973	17.328589	-0.064412	3.120605
334.980378	3291.100522	17.333594	-0.064435	3.116922
335.414116	3283.040923	17.338599	-0.064510	3.113231
335.114071	3275.084460	17.343603	-0.064449	3.109549
334.923006	3267.144115	17.348608	-0.064408	3.105876
335.077301	3259.147838	17.353613	-0.064432	3.102188
335.032443	3251.171795	17.358618	-0.064418	3.098496
334.730364	3243.227439	17.363623	-0.064357	3.094802
334.855963	3235.195932	17.368627	-0.064375	3.091083
334.739723	3227.255200	17.373632	-0.064348	3.087391
334.652436	3219.298243	17.378637	-0.064327	3.083688
334.402690	3211.304544	17.383642	-0.064275	3.079956
334.581330	3203.291352	17.388647	-0.064303	3.076230
334.482362	3195.250836	17.393651	-0.064280	3.072474
334.477763	3187.239855	17.398656	-0.064274	3.068732
334.480196	3179.247930	17.403661	-0.064269	3.064994
334.531928	3171.250653	17.408666	-0.064273	3.061252
334.330463	3163.339985	17.413671	-0.064231	3.057533
333.687545	3155.417812	17.418675	-0.064106	3.053783
334.097114	3147.332340	17.423680	-0.064177	3.050003
334.088904	3139.379845	17.428685	-0.064170	3.046260
333.799024	3131.415589	17.433690	-0.064111	3.042493
334.075240	3123.428505	17.438695	-0.064158	3.038739
334.295783	3115.404149	17.443699	-0.064193	3.034960
333.959860	3107.458732	17.448704	-0.064126	3.031186
334.032303	3099.442159	17.453709	-0.064134	3.027393
334.192807	3091.415772	17.458714	-0.064159	3.023596
334.101502	3083.536428	17.463719	-0.064137	3.019851
333.554672	3075.608802	17.468723	-0.064030	3.016056
333.735771	3067.544059	17.473728	-0.064058	3.012227
333.790482	3059.533685	17.478733	-0.064063	3.008413
333.547545	3051.571023	17.483738	-0.064013	3.004602
333.394123	3043.661946	17.488743	-0.063979	3.000816
333.550559	3035.615014	17.493747	-0.064003	2.996975
333.733817	3027.599550	17.498752	-0.064032	2.993145
333.906233	3019.568085	17.503757	-0.064059	2.989303
333.854507	3011.600833	17.508762	-0.064044	2.985474
333.845184	3003.644455	17.513767	-0.064037	2.981649
333.605101	2995.674569	17.518771	-0.063987	2.977800
333.590989	2987.701709	17.523776	-0.063980	2.973956
333.248018	2979.786389	17.528781	-0.063911	2.970118
333.485396	2971.727537	17.533786	-0.063950	2.966235
333.479717	2963.770627	17.538791	-0.063943	2.962385
333.664995	2955.739544	17.543795	-0.063973	2.958503
333.779677	2947.780616	17.548800	-0.063989	2.954648
333.505022	2939.837919	17.553805	-0.063933	2.950775
332.938650	2931.902429	17.558810	-0.063822	2.946884
333.428624	2923.853647	17.563815	-0.063908	2.942990
332.997053	2915.952233	17.568819	-0.063823	2.939113
332.597912	2907.999777	17.573824	-0.063743	2.935208
333.317650	2899.867246	17.578829	-0.063872	2.931269
333.417895	2891.863950	17.583834	-0.063885	2.927355
333.609877	2883.893615	17.588839	-0.063916	2.923458
333.169188	2876.000049	17.593843	-0.063829	2.919558
333.154751	2868.045237	17.598848	-0.063821	2.915646
333.207703	2859.998565	17.603853	-0.063826	2.911687
333.171085	2851.966450	17.608858	-0.063814	2.907726
333.281134	2843.999098	17.613863	-0.063829	2.903798
333.165912	2836.029128	17.618867	-0.063802	2.899852
333.182632	2828.072324	17.623872	-0.063800	2.895914
333.364187	2820.064429	17.628877	-0.063829	2.891955
333.206995	2812.102293	17.633882	-0.063794	2.887994
333.418612	2804.075792	17.638887	-0.063829	2.884016
333.143938	2796.190880	17.643891	-0.063772	2.880076
332.921996	2788.240221	17.648896	-0.063726	2.876101
333.169876	2780.212560	17.653901	-0.063767	2.872108
333.075529	2772.221572	17.658906	-0.063744	2.868109
333.243002	2764.217692	17.663911	-0.063770	2.864113
332.888355	2756.292310	17.668915	-0.063699	2.860120
332.814904	2748.311994	17.673920	-0.063680	2.856111
332.765058	2740.346440	17.678925	-0.063666	2.852104
332.718382	2732.328520	17.683930	-0.063652	2.848066
332.519467	2724.400690	17.688935	-0.063610	2.844059
332.799006	2716.399648	17.693939	-0.063657	2.840036
332.772935	2708.415240	17.698944	-0.063647	2.835999
332.652803	2700.448716	17.703949	-0.063619	2.831959
332.218191	2692.518149	17.708954	-0.063533	2.827914
332.320037	2684.499180	17.713959	-0.063547	2.823849
331.896160	2676.600316	17.718963	-0.063463	2.819808
332.176676	2668.529753	17.723968	-0.063510	2.815716
332.359921	2660.525488	17.728973	-0.063539	2.811646
332.233023	2652.560786	17.733978	-0.063510	2.807572
332.212065	2644.575257	17.738983	-0.063501	2.803487
332.387318	2636.586434	17.743987	-0.063528	2.799407
332.309090	2628.646044	17.748992	-0.063509	2.795330
332.640062	2620.636034	17.753997	-0.063565	2.791236
332.328337	2612.663110	17.759002	-0.063502	2.787117
332.135129	2604.751233	17.764007	-0.063461	2.783030
331.727926	2596.826636	17.769011	-0.063380	2.778917
331.936419	2588.772100	17.774016	-0.063413	2.774769
332.209042	2580.748461	17.779021	-0.063459	2.770634
332.187140	2572.770816	17.784026	-0.063450	2.766499
332.111717	2564.852316	17.789031	-0.063431	2.762385
331.775968	2556.924266	17.794035	-0.063363	2.758244
332.186772	2548.852610	17.799040	-0.063434	2.754068
332.049755	2540.874818	17.804045	-0.063403	2.749901
332.243197	2532.831620	17.809050	-0.063434	2.745713
332.381346	2524.882346	17.814055	-0.063455	2.741565
331.938631	2516.991150	17.819059	-0.063367	2.737405
331.814456	2509.027111	17.824064	-0.063339	2.733221
331.970044	2501.020442	17.829069	-0.063363	2.729025
331.945406	2493.031018	17.834074	-0.063353	2.724820
332.031514	2485.077336	17.839079	-0.063364	2.720635
331.415089	2477.205630	17.844083	-0.063244	2.716441
331.632254	2469.180999	17.849088	-0.063279	2.712214
331.560605	2461.194790	17.854093	-0.063261	2.707982
331.304973	2453.221000	17.859098	-0.063208	2.703738
331.653212	2445.210215	17.864103	-0.063268	2.699506
331.610148	2437.253404	17.869107	-0.063255	2.695271
331.447159	2429.285629	17.874112	-0.063219	2.691016
331.514393	2421.297846	17.879117	-0.063226	2.686759
331.347372	2413.351826	17.884122	-0.063190	2.682502
331.711096	2405.347876	17.889127	-0.063253	2.678241
331.468047	2397.409710	17.894131	-0.063202	2.673970
331.272159	2389.447798	17.899136	-0.063161	2.669682
331.338834	2381.447435	17.904141	-0.063168	2.665384
331.018749	2373.512673	17.909146	-0.063103	2.661088
331.272933	2365.502883	17.914151	-0.063145	2.656783
331.357084	2357.517071	17.919155	-0.063156	2.652473
331.134630	2349.540261	17.924160	-0.063109	2.648140
331.232610	2341.570667	17.929165	-0.063122	2.643825
331.294756	2333.606684	17.934170	-0.063129	2.639504
331.342933	2325.681806	17.939175	-0.063133	2.635197
331.175382	2317.685304	17.944179	-0.063096	2.630828
331.097097	2309.723649	17.949184	-0.063077	2.626477
331.227783	2301.743481	17.954189	-0.063096	2.622124
331.042622	2293.793121	17.959194	-0.063056	2.617757
330.919482	2285.847525	17.964199	-0.063028	2.613391
331.345689	2277.783768	17.969203	-0.063102	2.608989
331.564687	2269.811768	17.974208	-0.063138	2.604617
331.454293	2261.899759	17.979213	-0.063112	2.600248
331.078964	2253.999974	17.984218	-0.063037	2.595859
331.146957	2245.952473	17.989223	-0.063045	2.591412
331.073100	2237.908487	17.994227	-0.063026	2.586950
330.775833	2230.011457	17.999232	-0.062965	2.582546
330.944596	2222.020571	18.004237	-0.062991	2.578114
330.711185	2214.060683	18.009242	-0.062943	2.573665
330.697467	2206.110015	18.014247	-0.062935	2.569228
330.791746	2198.119730	18.019251	-0.062948	2.564768
330.703107	2190.167403	18.024256	-0.062926	2.560310
330.674411	2182.244413	18.029261	-0.062915	2.555864
330.653346	2174.259574	18.034266	-0.062906	2.551376
330.611132	2166.284291	18.039271	-0.062893	2.546884
330.560187	2158.325876	18.044275	-0.062879	2.542394
330.239229	2150.408728	18.049280	-0.062814	2.537899
330.463454	2142.402958	18.054285	-0.062850	2.533385
330.511863	2134.396790	18.059290	-0.062854	2.528850
330.131367	2126.498937	18.064295	-0.062778	2.524338
330.258481	2118.528545	18.069299	-0.062797	2.519813
329.987604	2110.599192	18.074304	-0.062741	2.515274
330.169241	2102.605529	18.079309	-0.062770	2.510723
330.216233	2094.577435	18.084314	-0.062773	2.506135
330.221058	2086.628269	18.089319	-0.062769	2.501580
329.711554	2078.747670	18.094323	-0.062669	2.497018
329.924722	2070.704712	18.099328	-0.062704	2.492408
330.107619	2062.725099	18.104333	-0.062733	2.487824
330.183316	2054.744354	18.109338	-0.062741	2.483223
329.685922	2046.899138	18.114343	-0.062644	2.478648
329.957123	2038.870337	18.119347	-0.062689	2.474017
330.171860	2030.865409	18.124352	-0.062724	2.469387
329.890761	2022.952553	18.129357	-0.062666	2.464763
329.946021	2014.964963	18.134362	-0.062672	2.460113
329.909150	2007.049986	18.139367	-0.062660	2.455490
329.938009	1999.060466	18.144371	-0.062660	2.450819
329.620157	1991.139146	18.149376	-0.062595	2.446153
329.926820	1983.157937	18.154381	-0.062647	2.441491
329.283690	1975.288997	18.159386	-0.062523	2.436812
329.431907	1967.277372	18.164391	-0.062545	2.432102
329.094296	1959.305326	18.169395	-0.062477	2.427367
329.109856	1951.320486	18.174400	-0.062475	2.422644
329.112997	1943.373373	18.179405	-0.062470	2.417933
329.210163	1935.359089	18.184410	-0.062483	2.413180
328.972299	1927.451421	18.189415	-0.062434	2.408455
328.803128	1919.498443	18.194419	-0.062397	2.403699
329.000904	1911.519424	18.199424	-0.062429	2.398947
329.201206	1903.552090	18.204429	-0.062461	2.394193
328.977000	1895.619558	18.209434	-0.062414	2.389416
329.216451	1887.597279	18.214439	-0.062453	2.384613
329.221402	1879.664555	18.219443	-0.062449	2.379835
329.192959	1871.706779	18.224448	-0.062439	2.375030
329.230767	1863.765442	18.229453	-0.062441	2.370231
329.338262	1855.764326	18.234458	-0.062455	2.365391
329.032422	1847.891534	18.239463	-0.062393	2.360585
328.922761	1839.949637	18.244467	-0.062368	2.355744
328.675261	1832.017808	18.249472	-0.062317	2.350887
329.050151	1823.989953	18.254477	-0.062381	2.346014
328.737353	1816.069238	18.259482	-0.062318	2.341138
328.900763	1808.103243	18.264487	-0.062343	2.336264
328.989598	1800.134019	18.269491	-0.062354	2.331372
328.552995	1792.240749	18.274496	-0.062268	2.326472
328.573934	1784.291040	18.279501	-0.062267	2.321565
328.403054	1776.362526	18.284506	-0.062230	2.316645
328.758050	1768.344692	18.289511	-0.062291	2.311704
328.779619	1760.379877	18.294515	-0.062290	2.306757
328.772896	1752.444035	18.299520	-0.062283	2.301815
328.586849	1744.537249	18.304525	-0.062244	2.296864
328.727057	1736.523470	18.309530	-0.062264	2.291865
328.563062	1728.596311	18.314535	-0.062229	2.286882
328.381437	1720.683759	18.319539	-0.062190	2.281896
328.364252	1712.750422	18.324544	-0.062182	2.276900
328.310594	1704.773823	18.329549	-0.062166	2.271863
328.225896	1696.780792	18.334554	-0.062145	2.266801
328.441629	1688.798460	18.339559	-0.062180	2.261762
328.322841	1680.889301	18.344563	-0.062153	2.256728
328.200939	1672.934361	18.349568	-0.062125	2.251653
328.254229	1664.985849	18.354573	-0.062130	2.246587
328.014876	1657.076738	18.359578	-0.062080	2.241508
328.065818	1649.132785	18.364583	-0.062085	2.236421
327.994607	1641.193686	18.369587	-0.062066	2.231315
328.014216	1633.234823	18.374592	-0.062065	2.226193
327.705426	1625.336437	18.379597	-0.062002	2.221068
327.922435	1617.318862	18.384602	-0.062038	2.215902
327.897947	1609.391468	18.389607	-0.062028	2.210760
327.726014	1601.471478	18.394611	-0.061991	2.205597
327.960775	1593.487118	18.399616	-0.062029	2.200418
328.043881	1585.560330	18.404621	-0.062040	2.195250
328.039595	1577.594508	18.409626	-0.062034	2.190037
327.738956	1569.702651	18.414631	-0.061973	2.184832
327.801124	1561.740161	18.419635	-0.061979	2.179602
327.660808	1553.821594	18.424640	-0.061948	2.174369
327.759327	1545.862325	18.429645	-0.061961	2.169119
327.708187	1537.899867	18.434650	-0.061946	2.163840
327.465219	1530.028253	18.439655	-0.061896	2.158591
327.431811	1522.089196	18.444659	-0.061885	2.153303
327.537678	1514.111783	18.449664	-0.061899	2.147990
327.539911	1506.177075	18.454669	-0.061894	2.142683
327.594795	1498.222103	18.459674	-0.061899	2.137354
327.633141	1490.299035	18.464679	-0.061901	2.132032
327.715692	1482.343746	18.469683	-0.061912	2.126679
327.559968	1474.441249	18.474688	-0.061878	2.121324
327.534022	1466.541156	18.479693	-0.061868	2.115971
327.369324	1458.560184	18.484698	-0.061832	2.110535
327.381699	1450.609658	18.489703	-0.061829	2.105124
327.465521	1442.665503	18.494707	-0.061839	2.099710
327.350846	1434.741490	18.499712	-0.061813	2.094276
327.432221	1426.807712	18.504717	-0.061823	2.088840
327.263700	1418.893581	18.509722	-0.061787	2.083379
327.173735	1410.998094	18.514727	-0.061765	2.077925
327.103346	1403.063484	18.519731	-0.061746	2.072431
327.082093	1395.109920	18.524736	-0.061737	2.066914
326.885350	1387.235175	18.529741	-0.061696	2.061419
326.758934	1379.305026	18.534746	-0.061667	2.055878
326.870657	1371.345685	18.539751	-0.061683	2.050326
326.942648	1363.398519	18.544755	-0.061691	2.044764
326.978299	1355.474486	18.549760	-0.061692	2.039199
326.842926	1347.595962	18.554765	-0.061662	2.033633
326.775071	1339.648364	18.559770	-0.061644	2.028009
326.695205	1331.719336	18.564775	-0.061624	2.022383
326.628846	1323.801196	18.569779	-0.061607	2.016749
326.564591	1315.872956	18.574784	-0.061590	2.011093
326.763158	1307.922524	18.579789	-0.061622	2.005433
326.584888	1300.031731	18.584794	-0.061583	1.999759
326.291325	1292.161760	18.589799	-0.061523	1.994072
326.273159	1284.224475	18.594803	-0.061515	1.988349
326.491418	1276.246450	18.599808	-0.061550	1.982606
326.487731	1268.341525	18.604813	-0.061545	1.976876
326.448596	1260.414635	18.609818	-0.061532	1.971109
326.407359	1252.511902	18.614823	-0.061519	1.965342
326.283984	1244.625947	18.619827	-0.061491	1.959562
326.055555	1236.747250	18.624832	-0.061444	1.953758
326.448197	1228.759840	18.629837	-0.061512	1.947925
326.233776	1220.845895	18.634842	-0.061467	1.942062
326.178506	1212.947979	18.639847	-0.061451	1.936211
326.106444	1205.027356	18.644851	-0.061433	1.930323
325.934161	1197.117626	18.649856	-0.061395	1.924414
325.947026	1189.229290	18.654861	-0.061393	1.918524
326.075426	1181.280829	18.659866	-0.061412	1.912584
326.154947	1173.352936	18.664871	-0.061421	1.906635
325.797085	1165.500287	18.669875	-0.061350	1.900674
325.895463	1157.566589	18.674880	-0.061363	1.894685
325.910385	1149.666676	18.679885	-0.061360	1.888693
325.766415	1141.766688	18.684890	-0.061328	1.882664
325.729939	1133.880970	18.689895	-0.061317	1.876639
325.704237	1125.963378	18.694899	-0.061307	1.870571
325.835245	1118.011146	18.699904	-0.061326	1.864476
325.570508	1110.183687	18.704909	-0.061272	1.858409
325.506033	1102.258742	18.709914	-0.061254	1.852271
325.501051	1094.356954	18.714919	-0.061248	1.846138
325.296529	1086.488903	18.719923	-0.061205	1.839987
325.271225	1078.585165	18.724928	-0.061195	1.833809
325.291954	1070.687817	18.729933	-0.061194	1.827620
325.093610	1062.806447	18.734938	-0.061152	1.821396
325.058983	1054.908847	18.739943	-0.061141	1.815158
325.132007	1046.995732	18.744947	-0.061149	1.808900
325.266915	1039.074214	18.749952	-0.061169	1.802621
325.231166	1031.213085	18.754957	-0.061157	1.796347
325.084537	1023.309040	18.759962	-0.061125	1.790002
324.786686	1015.459372	18.764967	-0.061064	1.783660
324.751026	1007.564887	18.769971	-0.061053	1.777292
324.700048	999.653305	18.774976	-0.061038	1.770885
324.984501	991.722918	18.779981	-0.061086	1.764482
324.656916	983.910268	18.784986	-0.061020	1.758074
324.480714	976.049874	18.789991	-0.060982	1.751623
324.705809	968.109864	18.794995	-0.061019	1.745134
324.426164	960.282926	18.800000	-0.060961	1.738649
324.353756	952.408737	18.805005	-0.060943	1.732127
324.027143	944.565205	18.810010	-0.060877	1.725573
324.442386	936.625079	18.815015	-0.060949	1.719011
324.518010	928.747735	18.820019	-0.060958	1.712431
324.306330	920.873946	18.825024	-0.060914	1.705791
324.511784	912.984014	18.830029	-0.060947	1.699167
324.407947	905.122216	18.835034	-0.060922	1.692499
324.051003	897.299310	18.840039	-0.060851	1.685804
324.047381	889.443102	18.845043	-0.060845	1.679101
323.926894	881.592765	18.850048	-0.060818	1.672361
323.788890	873.732363	18.855053	-0.060787	1.665583
323.932262	865.832683	18.860058	-0.060808	1.658781
324.014332	857.962395	18.865063	-0.060819	1.651968
324.060859	850.089661	18.870067	-0.060822	1.645121
323.904188	842.277985	18.875072	-0.060788	1.638269
323.900566	834.414434	18.880077	-0.060782	1.631365
323.658559	826.552709	18.885082	-0.060732	1.624399
323.925428	818.660997	18.890087	-0.060777	1.617449
323.856131	810.811318	18.895091	-0.060759	1.610458
323.835101	802.966162	18.900096	-0.060750	1.603448
323.726674	795.158225	18.905101	-0.060724	1.596428
323.575718	787.323082	18.910106	-0.060691	1.589346
323.428360	779.507741	18.915111	-0.060659	1.582251
323.406970	771.668295	18.920115	-0.060650	1.575120
323.259571	763.842050	18.925120	-0.060617	1.567951
323.391261	755.979315	18.930125	-0.060637	1.560756
323.307345	748.166959	18.935130	-0.060616	1.553542
323.294081	740.318551	18.940135	-0.060608	1.546272
323.183025	732.513339	18.945139	-0.060583	1.538993
323.044080	724.689666	18.950144	-0.060552	1.531658
323.193904	716.832785	18.955149	-0.060575	1.524300
322.833091	709.082354	18.960154	-0.060502	1.516929
322.847448	701.246764	18.965159	-0.060500	1.509498
322.830472	693.418500	18.970163	-0.060492	1.502034
322.653301	685.625392	18.975168	-0.060454	1.494540
322.636643	677.818654	18.980173	-0.060446	1.487021
322.633778	670.000791	18.985178	-0.060440	1.479455
322.658282	662.185190	18.990183	-0.060439	1.471856
322.499799	654.367293	18.995187	-0.060405	1.464187
322.611769	646.539740	19.000192	-0.060421	1.456511
322.606020	638.752279	19.005197	-0.060415	1.448816
322.518768	630.965000	19.010202	-0.060393	1.441066
322.268945	623.232906	19.015207	-0.060342	1.433302
322.375547	615.404585	19.020211	-0.060357	1.425458
322.308727	607.633009	19.025216	-0.060339	1.417600
322.319897	599.854618	19.030221	-0.060336	1.409704
322.264191	592.073906	19.035226	-0.060321	1.401749
322.089922	584.350032	19.040231	-0.060283	1.393788
322.020385	576.568729	19.045235	-0.060265	1.385739
321.682462	568.857810	19.050240	-0.060197	1.377670
321.666113	561.089926	19.055245	-0.060189	1.369549
321.700666	553.292583	19.060250	-0.060191	1.361359
321.599759	545.566669	19.065255	-0.060167	1.353170
321.391834	537.840186	19.070259	-0.060123	1.344911
321.313575	530.095837	19.075264	-0.060104	1.336606
321.663047	522.286563	19.080269	-0.060164	1.328256
321.441216	514.581074	19.085274	-0.060117	1.319862
321.356833	506.827154	19.090279	-0.060097	1.311387
321.249868	499.058191	19.095283	-0.060072	1.302835
321.390759	491.306015	19.100288	-0.060093	1.294292
321.505990	483.564785	19.105293	-0.060109	1.285699
321.312065	475.895259	19.110298	-0.060068	1.277071
321.409917	468.171554	19.115303	-0.060082	1.268378
321.357387	460.478912	19.120307	-0.060067	1.259632
321.352451	452.781135	19.125312	-0.060061	1.250828
321.285837	445.115338	19.130317	-0.060044	1.241986
321.160817	437.460108	19.135322	-0.060015	1.233082
321.042511	429.787608	19.140327	-0.059988	1.224094
320.847188	422.143245	19.145331	-0.059947	1.215057
320.881884	414.454531	19.150336	-0.059948	1.205947
320.907825	406.804892	19.155341	-0.059948	1.196811
320.722846	399.169174	19.160346	-0.059909	1.187579
320.840025	391.500102	19.165351	-0.059926	1.178297
320.892471	383.852763	19.170355	-0.059931	1.168955
320.486620	376.290133	19.175360	-0.059850	1.159544
320.423614	368.663941	19.180365	-0.059834	1.150051
320.281592	361.038034	19.185370	-0.059802	1.140462
320.294260	353.423241	19.190375	-0.059800	1.130839
320.073684	345.853072	19.195379	-0.059754	1.121139
319.918768	338.280973	19.200384	-0.059720	1.111367
320.118189	330.655128	19.205389	-0.059752	1.101517
319.837176	323.121668	19.210394	-0.059695	1.091592
319.728750	315.568053	19.215399	-0.059670	1.081587
319.814978	307.999412	19.220403	-0.059681	1.071515
319.451457	300.498736	19.225408	-0.059608	1.061333
319.478857	292.956020	19.230413	-0.059609	1.051088
319.463145	285.417845	19.235418	-0.059601	1.040737
319.545474	277.892647	19.240423	-0.059611	1.030325
319.410167	270.414337	19.245427	-0.059581	1.019819
319.312315	262.938525	19.250432	-0.059558	1.009216
319.235656	255.493019	19.255437	-0.059539	0.998550
319.241919	247.993717	19.260442	-0.059535	0.987711
319.225034	240.536213	19.265447	-0.059528	0.976807
319.173985	233.108903	19.270451	-0.059513	0.965817
319.038786	225.711955	19.275456	-0.059483	0.954723
318.971775	218.324375	19.280461	-0.059466	0.943531
318.723167	210.971346	19.285466	-0.059415	0.932209
318.626330	203.617013	19.290471	-0.059392	0.920787
318.670324	196.258677	19.295475	-0.059396	0.909254
318.393975	188.956982	19.300480	-0.059339	0.897574
318.574266	181.609765	19.305485	-0.059368	0.885796
318.040644	174.414447	19.310490	-0.059264	0.873902
317.676580	167.188637	19.315495	-0.059192	0.861843
317.298807	159.994842	19.320499	-0.059117	0.849662
316.900237	152.822251	19.325504	-0.059038	0.837334
316.420501	145.665611	19.330509	-0.058944	0.824825
315.888633	138.545637	19.335514	-0.058840	0.812171
315.265954	131.472678	19.340519	-0.058720	0.799372
314.752287	124.406983	19.345523	-0.058620	0.786412
313.994853	117.406440	19.350528	-0.058474	0.773276
313.433363	110.411181	19.355533	-0.058365	0.759988
312.848102	103.433668	19.360538	-0.058252	0.746489
312.303470	96.479868	19.365543	-0.058146	0.732802
311.864535	89.552312	19.370547	-0.058059	0.718943
311.041640	82.728794	19.375552	-0.057902	0.704885
310.204688	76.126788	19.380557	-0.057742	0.690995