Fri Apr 16 19:13:43 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.807459	-0.046781	0.000000	-0.000049	0.312012

1.951663	-0.099708	0.005005	-0.000076	0.311889
1.754305	-0.099678	0.010010	-0.000039	0.311723
1.296465	-0.015805	0.015014	0.000046	0.311726
1.260440	-0.005710	0.020019	0.000052	0.311743
1.524773	-0.057570	0.025024	0.000003	0.311725
1.302103	-0.016842	0.030029	0.000044	0.311727
1.431399	-0.039465	0.035034	0.000020	0.311731
1.711026	-0.093187	0.040038	-0.000032	0.311718
1.544608	-0.061539	0.045043	-0.000001	0.311724
1.858931	-0.119959	0.050048	-0.000059	0.311718
1.892214	-0.128599	0.055053	-0.000066	0.311707
2.068827	-0.159368	0.060058	-0.000098	0.311713
1.789707	-0.109612	0.065062	-0.000047	0.311709
1.812615	-0.110678	0.070067	-0.000051	0.311723
1.667986	-0.140056	0.075072	-0.000024	0.311465
1.570215	-0.140269	0.080077	-0.000006	0.311382
1.610282	-0.144725	0.085082	-0.000013	0.311395
1.870250	-0.193857	0.090086	-0.000062	0.311386
1.721563	-0.166217	0.095091	-0.000034	0.311390
1.355277	-0.098389	0.100096	0.000034	0.311396
1.418960	-0.130576	0.105101	0.000022	0.311300
1.113108	-0.117422	0.110106	0.000079	0.311103
1.116698	-0.121199	0.115110	0.000078	0.311089
1.599192	-0.208655	0.120115	-0.000012	0.311090
1.447270	-0.181087	0.125120	0.000017	0.311090
1.476675	-0.189503	0.130125	0.000011	0.311076
1.219440	-0.202633	0.135130	0.000059	0.310798
0.715340	-0.114995	0.140134	0.000153	0.310780
1.065831	-0.179346	0.145139	0.000088	0.310777
0.486125	-0.071861	0.150144	0.000195	0.310787
0.165636	-0.012146	0.155149	0.000255	0.310794
0.490064	-0.104180	0.160154	0.000195	0.310640
0.385624	-0.107728	0.165158	0.000214	0.310535
0.530113	-0.133212	0.170163	0.000187	0.310539
1.075237	-0.234805	0.175168	0.000086	0.310528
0.950691	-0.227302	0.180173	0.000109	0.310457
0.987334	-0.292109	0.185178	0.000102	0.310186
1.127249	-0.319177	0.190182	0.000076	0.310179
0.633776	-0.224981	0.195187	0.000168	0.310200
1.090218	-0.346889	0.200192	0.000083	0.310019
1.404829	-0.440958	0.205197	0.000024	0.309847
1.168522	-0.396294	0.210202	0.000068	0.309855
0.556338	-0.311742	0.215206	0.000182	0.309731
0.732565	-0.387394	0.220211	0.000149	0.309527
1.012124	-0.438874	0.225216	0.000097	0.309524
0.830227	-0.421223	0.230221	0.000131	0.309452
0.712759	-0.445002	0.235226	0.000153	0.309241
0.439984	-0.396867	0.240230	0.000203	0.309235
0.830877	-0.486769	0.245235	0.000131	0.309147
0.607410	-0.499231	0.250240	0.000172	0.308898
0.329830	-0.447910	0.255245	0.000224	0.308903
0.503432	-0.503593	0.260250	0.000191	0.308790
0.399759	-0.525832	0.265254	0.000211	0.308598
0.917910	-0.621231	0.270259	0.000114	0.308592
0.810010	-0.656009	0.275264	0.000134	0.308337
0.519092	-0.618798	0.280269	0.000188	0.308264
0.467830	-0.624781	0.285274	0.000198	0.308192
0.193206	-0.620809	0.290278	0.000249	0.307977
0.281447	-0.635276	0.295283	0.000232	0.307984
0.033729	-0.646554	0.300288	0.000279	0.307720
-0.495748	-0.567035	0.305293	0.000377	0.307642
-0.308764	-0.608207	0.310298	0.000342	0.307608
-0.344520	-0.661692	0.315302	0.000349	0.307326
-0.544789	-0.625427	0.320307	0.000386	0.307326
0.080217	-0.783829	0.325312	0.000270	0.307115
-0.209452	-0.755617	0.330317	0.000324	0.307000
-0.395099	-0.738916	0.335322	0.000358	0.306920
-0.515471	-0.762015	0.340326	0.000381	0.306708
-0.541060	-0.754303	0.345331	0.000385	0.306723
-1.000591	-0.737458	0.350336	0.000471	0.306408
-1.433619	-0.662056	0.355341	0.000551	0.306393
-1.461525	-0.684792	0.360346	0.000556	0.306262
-1.602460	-0.695566	0.365350	0.000583	0.306090
-1.936905	-0.634498	0.370355	0.000645	0.306092
-1.615346	-0.752508	0.375360	0.000585	0.305810
-1.654399	-0.752975	0.380365	0.000592	0.305775
-2.680156	-0.587764	0.385370	0.000783	0.305675
-2.916364	-0.575275	0.390374	0.000827	0.305531
-1.923473	-0.755006	0.395379	0.000642	0.305534
-2.096497	-0.783767	0.400384	0.000674	0.305249
-2.574270	-0.710551	0.405389	0.000763	0.305185
-2.610134	-0.725618	0.410394	0.000770	0.305083
-2.467773	-0.798319	0.415398	0.000743	0.304861
-2.589136	-0.777734	0.420403	0.000766	0.304854
-2.991234	-0.770245	0.425408	0.000841	0.304543
-2.989825	-0.775955	0.430413	0.000840	0.304517
-3.403697	-0.726041	0.435418	0.000917	0.304397
-3.289773	-0.778577	0.440422	0.000896	0.304246
-2.801817	-0.873445	0.445427	0.000805	0.304217
-3.068136	-0.890352	0.450432	0.000855	0.303906
-3.444773	-0.823719	0.455437	0.000925	0.303898
-2.912130	-0.970779	0.460442	0.000826	0.303659
-2.710635	-1.025946	0.465446	0.000788	0.303571
-3.410832	-0.939421	0.470451	0.000919	0.303377
-3.702476	-0.908218	0.475456	0.000973	0.303273
-3.051010	-1.057330	0.480461	0.000852	0.303127
-3.737083	-0.962365	0.485466	0.000979	0.302985
-4.228005	-0.893585	0.490470	0.001071	0.302888
-3.670055	-1.048254	0.495475	0.000967	0.302633
-3.854503	-1.022184	0.500480	0.001001	0.302598
-4.900688	-0.890839	0.505485	0.001196	0.302317
-4.528073	-0.957142	0.510490	0.001126	0.302324
-4.340420	-1.045019	0.515494	0.001091	0.302067
-4.808134	-0.975110	0.520499	0.001178	0.301995
-5.292785	-0.916657	0.525504	0.001268	0.301853
-5.033209	-0.993989	0.530509	0.001220	0.301708
-4.747589	-1.062931	0.535514	0.001167	0.301627
-5.094832	-1.054134	0.540518	0.001232	0.301366
-5.010997	-1.072869	0.545523	0.001216	0.301350
-5.089081	-1.117669	0.550528	0.001230	0.301067
-5.749339	-0.999427	0.555533	0.001353	0.301059
-5.374109	-1.123987	0.560538	0.001283	0.300788
-5.338089	-1.139724	0.565542	0.001277	0.300744
-5.861682	-1.081659	0.570547	0.001374	0.300565
-6.179035	-1.034824	0.575552	0.001433	0.300513
-5.549299	-1.190188	0.580557	0.001316	0.300317
-5.800092	-1.176183	0.585562	0.001363	0.300165
-6.906306	-1.001110	0.590566	0.001568	0.300040
-6.415406	-1.130904	0.595571	0.001477	0.299844
-5.993020	-1.223305	0.600576	0.001398	0.299769
-6.526598	-1.179089	0.605581	0.001498	0.299514
-6.294986	-1.227398	0.610586	0.001454	0.299484
-6.564326	-1.230641	0.615590	0.001505	0.299232
-7.359997	-1.082260	0.620595	0.001653	0.299251
-8.087998	-1.019771	0.625600	0.001788	0.298913
-7.993166	-1.040272	0.630605	0.001770	0.298898
-7.439203	-1.173037	0.635610	0.001667	0.298743
-8.249928	-1.057357	0.640614	0.001818	0.298589
-8.667371	-0.988347	0.645619	0.001896	0.298556
-8.007894	-1.163907	0.650624	0.001773	0.298286
-8.421721	-1.089481	0.655629	0.001850	0.298283
-9.008271	-1.030603	0.660634	0.001959	0.298051
-8.835374	-1.077538	0.665638	0.001927	0.297976
-8.340068	-1.195453	0.670643	0.001835	0.297841
-8.511538	-1.204201	0.675648	0.001867	0.297647
-8.214108	-1.275149	0.680653	0.001811	0.297565
-8.926909	-1.191593	0.685658	0.001944	0.297342
-9.595151	-1.071485	0.690662	0.002068	0.297336
-8.932943	-1.254618	0.695667	0.001945	0.297030
-8.472962	-1.345329	0.700672	0.001859	0.296996
-9.555842	-1.195889	0.705677	0.002061	0.296765
-9.838251	-1.155385	0.710682	0.002113	0.296712
-9.085471	-1.324647	0.715686	0.001973	0.296554
-9.820813	-1.221468	0.720691	0.002110	0.296406
-10.578594	-1.097362	0.725696	0.002251	0.296340
-11.397869	-0.999847	0.730701	0.002403	0.296089
-10.680321	-1.129351	0.735706	0.002270	0.296093
-10.077070	-1.284935	0.740710	0.002158	0.295869
-10.278979	-1.272110	0.745715	0.002195	0.295752
-10.759458	-1.204090	0.750720	0.002284	0.295658
-10.725400	-1.241571	0.755725	0.002278	0.295505
-10.379320	-1.314252	0.760730	0.002214	0.295457
-10.155777	-1.415082	0.765734	0.002172	0.295163
-10.305300	-1.397421	0.770739	0.002200	0.295116
-11.116856	-1.306184	0.775744	0.002351	0.294840
-10.559492	-1.407313	0.780749	0.002247	0.294842
-10.409746	-1.497829	0.785754	0.002219	0.294531
-11.431329	-1.316652	0.790758	0.002409	0.294509
-12.011770	-1.261174	0.795763	0.002517	0.294263
-11.744640	-1.316745	0.800768	0.002468	0.294229
-11.088961	-1.479607	0.805773	0.002345	0.294014
-11.738903	-1.385474	0.810778	0.002466	0.293896
-12.202279	-1.333259	0.815782	0.002553	0.293739
-11.815479	-1.434483	0.820787	0.002481	0.293587
-12.239621	-1.376957	0.825792	0.002559	0.293490
-12.819030	-1.316860	0.830797	0.002667	0.293268
-11.843944	-1.499250	0.835802	0.002486	0.293242
-12.218918	-1.486866	0.840806	0.002556	0.292967
-13.137405	-1.318318	0.845811	0.002726	0.292975
-12.977067	-1.409263	0.850816	0.002697	0.292670
-12.516354	-1.501453	0.855821	0.002611	0.292629
-13.186587	-1.424218	0.860826	0.002736	0.292408
-13.969190	-1.298693	0.865830	0.002881	0.292326
-13.904391	-1.333470	0.870835	0.002869	0.292212
-13.455512	-1.457616	0.875840	0.002785	0.292001
-13.664852	-1.429009	0.880845	0.002824	0.291955
-13.149742	-1.572276	0.885850	0.002729	0.291709
-13.370858	-1.539879	0.890854	0.002770	0.291670
-13.791467	-1.524392	0.895859	0.002848	0.291368
-13.719184	-1.537769	0.900864	0.002834	0.291367
-13.758058	-1.589348	0.905869	0.002842	0.291076
-14.063987	-1.535650	0.910874	0.002898	0.291066
-14.678589	-1.482469	0.915878	0.003013	0.290775
-14.134144	-1.588190	0.920883	0.002912	0.290742
-14.044105	-1.641105	0.925888	0.002895	0.290560
-14.456659	-1.582253	0.930893	0.002971	0.290480
-14.329932	-1.651122	0.935898	0.002948	0.290252
-14.869979	-1.575723	0.940902	0.003048	0.290138
-15.631105	-1.470994	0.945907	0.003190	0.289971
-15.266675	-1.565834	0.950912	0.003122	0.289828
-14.760083	-1.685945	0.955917	0.003028	0.289689
-14.972609	-1.684248	0.960922	0.003067	0.289504
-15.793085	-1.556018	0.965926	0.003220	0.289400
-16.008533	-1.554072	0.970931	0.003260	0.289214
-15.405652	-1.673203	0.975936	0.003148	0.289166
-15.628727	-1.690964	0.980941	0.003189	0.288875
-15.978214	-1.630436	0.985946	0.003254	0.288860
-16.744603	-1.549337	0.990950	0.003397	0.288568
-16.795466	-1.538186	0.995955	0.003406	0.288578
-16.061015	-1.723426	1.000960	0.003270	0.288319
-16.614862	-1.635047	1.005965	0.003373	0.288257
-17.401447	-1.530109	1.010970	0.003519	0.288066
-17.716733	-1.491871	1.015974	0.003578	0.287970
-16.954277	-1.648641	1.020979	0.003436	0.287879
-17.155786	-1.660510	1.025984	0.003473	0.287636
-17.600239	-1.587684	1.030989	0.003556	0.287596
-17.156596	-1.724205	1.035994	0.003473	0.287315
-17.072684	-1.742414	1.040998	0.003458	0.287300
-17.382825	-1.748311	1.046003	0.003515	0.286986
-18.368001	-1.566594	1.051008	0.003699	0.287000
-18.289781	-1.629592	1.056013	0.003684	0.286754
-17.995379	-1.692510	1.061018	0.003629	0.286707
-17.845703	-1.761177	1.066022	0.003601	0.286498
-18.198197	-1.722920	1.071027	0.003667	0.286367
-18.808520	-1.636524	1.076032	0.003780	0.286243
-18.981726	-1.641595	1.081037	0.003813	0.286059
-18.619574	-1.716029	1.086042	0.003745	0.286015
-18.913525	-1.715974	1.091046	0.003800	0.285745
-19.310293	-1.642718	1.096051	0.003874	0.285751
-19.137701	-1.720332	1.101056	0.003842	0.285517
-18.645373	-1.816312	1.106061	0.003750	0.285485
-19.110796	-1.783437	1.111066	0.003837	0.285222
-19.947512	-1.644966	1.116070	0.003992	0.285153
-19.733876	-1.718088	1.121075	0.003952	0.284979
-19.586689	-1.771732	1.126080	0.003925	0.284843
-20.292992	-1.666187	1.131085	0.004056	0.284727
-20.555959	-1.659982	1.136090	0.004105	0.284516
-20.153605	-1.736596	1.141094	0.004030	0.284498
-20.459587	-1.734956	1.146099	0.004087	0.284224
-20.800837	-1.671884	1.151104	0.004151	0.284229
-20.894675	-1.702967	1.156109	0.004168	0.283984
-20.804327	-1.737408	1.161114	0.004151	0.283892
-20.822817	-1.761363	1.166118	0.004155	0.283753
-20.644649	-1.828568	1.171123	0.004122	0.283576
-21.189615	-1.743874	1.176128	0.004223	0.283503
-21.764202	-1.688039	1.181133	0.004330	0.283255
-21.246209	-1.781184	1.186138	0.004233	0.283260
-21.457769	-1.795672	1.191142	0.004273	0.282990
-21.848838	-1.728172	1.196147	0.004346	0.282971
-21.864405	-1.767653	1.201152	0.004348	0.282755
-22.273377	-1.715936	1.206157	0.004424	0.282639
-22.294881	-1.732321	1.211162	0.004428	0.282536
-22.671541	-1.707631	1.216166	0.004499	0.282311
-22.315916	-1.771929	1.221171	0.004432	0.282314
-22.286040	-1.838157	1.226176	0.004427	0.282002
-22.378881	-1.824716	1.231181	0.004444	0.281984
-22.763298	-1.795943	1.236186	0.004515	0.281773
-22.936859	-1.777965	1.241190	0.004548	0.281704
-22.721171	-1.849866	1.246195	0.004508	0.281536
-22.793465	-1.870311	1.251200	0.004521	0.281364
-23.187762	-1.814415	1.256205	0.004594	0.281283
-23.293741	-1.838502	1.261210	0.004614	0.281060
-23.479223	-1.807030	1.266214	0.004649	0.281048
-23.086663	-1.939238	1.271219	0.004575	0.280735
-23.442612	-1.873774	1.276224	0.004642	0.280739
-23.958365	-1.819649	1.281229	0.004738	0.280535
-23.781830	-1.857987	1.286234	0.004705	0.280503
-23.655782	-1.921895	1.291238	0.004681	0.280291
-23.824877	-1.916678	1.296243	0.004713	0.280160
-23.949043	-1.922502	1.301248	0.004736	0.280013
-24.165357	-1.916486	1.306253	0.004776	0.279841
-24.465592	-1.876289	1.311258	0.004832	0.279767
-25.182434	-1.792994	1.316262	0.004965	0.279523
-24.731018	-1.876788	1.321267	0.004881	0.279515
-24.811856	-1.913227	1.326272	0.004896	0.279250
-25.619528	-1.767873	1.331277	0.005046	0.279243
-25.413469	-1.845234	1.336282	0.005008	0.279036
-25.469150	-1.860941	1.341286	0.005018	0.278902
-25.645418	-1.844431	1.346291	0.005051	0.278822
-26.232360	-1.778477	1.351296	0.005160	0.278610
-26.086287	-1.809459	1.356301	0.005133	0.278587
-25.529769	-1.964369	1.361306	0.005030	0.278308
-25.743512	-1.935251	1.366310	0.005069	0.278258
-25.904051	-1.943820	1.371315	0.005099	0.278062
-25.897541	-1.962365	1.376320	0.005098	0.277971
-26.309885	-1.920272	1.381325	0.005175	0.277800
-26.384595	-1.937355	1.386330	0.005188	0.277641
-26.540079	-1.923168	1.391334	0.005217	0.277567
-26.965441	-1.891276	1.396339	0.005296	0.277330
-26.979333	-1.889117	1.401344	0.005299	0.277329
-27.073014	-1.931391	1.406349	0.005316	0.277019
-26.769334	-1.991647	1.411354	0.005260	0.276993
-27.216305	-1.948209	1.416358	0.005343	0.276796
-27.495053	-1.913291	1.421363	0.005395	0.276713
-27.196417	-1.993895	1.426368	0.005339	0.276576
-27.758146	-1.930895	1.431373	0.005444	0.276371
-27.638293	-1.959327	1.436378	0.005421	0.276337
-27.766915	-1.988783	1.441382	0.005445	0.276060
-28.053931	-1.934384	1.446387	0.005499	0.276072
-28.140135	-1.972104	1.451392	0.005515	0.275792
-28.569015	-1.902564	1.456397	0.005595	0.275748
-28.177037	-1.999364	1.461402	0.005522	0.275614
-28.749277	-1.915992	1.466406	0.005628	0.275505
-28.613788	-1.956488	1.471411	0.005603	0.275422
-28.821865	-1.966500	1.476416	0.005641	0.275171
-29.184501	-1.901133	1.481421	0.005709	0.275168
-29.180198	-1.955399	1.486426	0.005708	0.274887
-29.267723	-1.946873	1.491430	0.005724	0.274848
-29.108376	-2.014847	1.496435	0.005695	0.274643
-29.605119	-1.946252	1.501440	0.005787	0.274528
-29.782754	-1.930178	1.506445	0.005820	0.274443
-29.564795	-2.009263	1.511450	0.005780	0.274235
-30.040943	-1.922916	1.516454	0.005868	0.274234
-30.513047	-1.895503	1.521459	0.005956	0.273925
-30.179956	-1.960690	1.526464	0.005894	0.273901
-30.147132	-2.002931	1.531469	0.005888	0.273710
-30.381057	-1.984018	1.536474	0.005931	0.273585
-30.329269	-2.010137	1.541478	0.005922	0.273497
-30.623667	-2.000423	1.546483	0.005976	0.273265
-30.884082	-1.952541	1.551488	0.006025	0.273268
-31.315234	-1.926172	1.556493	0.006105	0.272992
-30.861972	-2.011644	1.561498	0.006021	0.272976
-31.263200	-1.975770	1.566502	0.006095	0.272780
-31.441081	-1.971543	1.571507	0.006128	0.272631
-31.308251	-2.006429	1.576512	0.006104	0.272574
-31.940578	-1.939672	1.581517	0.006221	0.272318
-32.031791	-1.919749	1.586522	0.006238	0.272336
-31.938939	-1.984685	1.591526	0.006221	0.272080
-32.442768	-1.905117	1.596531	0.006315	0.272017
-32.266078	-1.954402	1.601536	0.006282	0.271925
-32.677664	-1.919356	1.606541	0.006358	0.271714
-32.408538	-1.967190	1.611546	0.006308	0.271720
-33.120913	-1.891207	1.616550	0.006441	0.271434
-33.382506	-1.852761	1.621555	0.006489	0.271386
-33.203352	-1.896630	1.626560	0.006456	0.271326
-33.335912	-1.919945	1.631565	0.006481	0.271073
-33.242275	-1.935892	1.636570	0.006463	0.271079
-33.454973	-1.939625	1.641574	0.006503	0.270853
-33.598079	-1.930814	1.646579	0.006529	0.270761
-33.537957	-1.953946	1.651584	0.006518	0.270696
-34.104656	-1.887380	1.656589	0.006623	0.270501
-33.579682	-1.982333	1.661594	0.006526	0.270504
-34.094004	-1.938441	1.666598	0.006621	0.270238
-34.145562	-1.945814	1.671603	0.006631	0.270149
-33.642008	-2.058617	1.676608	0.006537	0.270035
-34.251975	-1.986244	1.681613	0.006651	0.269828
-34.280238	-1.979923	1.686618	0.006656	0.269835
-34.535565	-1.995449	1.691622	0.006703	0.269503
-34.425554	-2.015016	1.696627	0.006683	0.269505
-34.723225	-1.992626	1.701632	0.006738	0.269335
-34.987696	-1.966838	1.706637	0.006787	0.269215
-34.432265	-2.082578	1.711642	0.006684	0.269136
-35.259742	-1.980760	1.716646	0.006838	0.268874
-35.411543	-1.952039	1.721651	0.006866	0.268881
-35.291171	-2.020454	1.726656	0.006844	0.268630
-35.527405	-1.989241	1.731661	0.006888	0.268567
-35.477419	-2.024471	1.736666	0.006878	0.268426
-36.044235	-1.954578	1.741670	0.006984	0.268247
-35.715775	-2.015826	1.746675	0.006923	0.268239
-35.950100	-2.024695	1.751680	0.006966	0.267962
-36.246563	-1.971471	1.756685	0.007021	0.267958
-36.072401	-2.041031	1.761690	0.006989	0.267754
-36.430259	-2.001175	1.766694	0.007055	0.267617
-36.511266	-2.000374	1.771699	0.007071	0.267542
-36.617921	-2.024288	1.776704	0.007090	0.267308
-36.726827	-2.005623	1.781709	0.007111	0.267302
-37.197818	-1.966739	1.786714	0.007198	0.267049
-37.398261	-1.942292	1.791718	0.007235	0.266984
-37.354959	-1.963739	1.796723	0.007227	0.266910
-37.554631	-1.964883	1.801728	0.007265	0.266707
-37.969871	-1.891103	1.806733	0.007342	0.266698
-37.780822	-1.966198	1.811738	0.007307	0.266477
-38.016973	-1.943787	1.816742	0.007350	0.266366
-38.226761	-1.914193	1.821747	0.007389	0.266319
-38.250177	-1.956779	1.826752	0.007394	0.266065
-38.381708	-1.933613	1.831757	0.007418	0.266061
-38.752927	-1.897285	1.836762	0.007487	0.265891
-39.142772	-1.852078	1.841766	0.007560	0.265751
-38.622857	-1.947912	1.846771	0.007463	0.265745
-39.085414	-1.903148	1.851776	0.007549	0.265530
-39.386208	-1.856811	1.856781	0.007605	0.265485
-38.890669	-1.964551	1.861786	0.007513	0.265389
-39.473779	-1.904418	1.866790	0.007621	0.265139
-39.580985	-1.884662	1.871795	0.007641	0.265140
-39.343325	-1.967430	1.876800	0.007597	0.264924
-39.375803	-1.982624	1.881805	0.007603	0.264809
-39.641982	-1.943933	1.886810	0.007652	0.264756
-40.126283	-1.904930	1.891814	0.007742	0.264488
-39.532918	-2.012906	1.896819	0.007632	0.264488
-39.655100	-2.026026	1.901824	0.007655	0.264295
-40.417784	-1.904921	1.906829	0.007797	0.264198
-39.918111	-2.009209	1.911834	0.007704	0.264125
-40.423628	-1.964070	1.916838	0.007798	0.263869
-40.894208	-1.876143	1.921843	0.007885	0.263882
-41.125655	-1.869176	1.926848	0.007928	0.263689
-41.348623	-1.849995	1.931853	0.007970	0.263572
-40.680590	-1.974046	1.936858	0.007845	0.263558
-41.692778	-1.845817	1.941862	0.008034	0.263251
-41.309161	-1.917301	1.946867	0.007962	0.263242
-41.056660	-1.983055	1.951872	0.007915	0.263133
-42.014965	-1.841615	1.956877	0.008094	0.262952
-41.589977	-1.919628	1.961882	0.008014	0.262949
-41.471021	-1.991343	1.966886	0.007992	0.262673
-41.846516	-1.934829	1.971891	0.008062	0.262608
-42.140999	-1.895187	1.976896	0.008117	0.262532
-42.260637	-1.916510	1.981901	0.008139	0.262294
-42.301631	-1.905055	1.986906	0.008147	0.262316
-42.664213	-1.883277	1.991910	0.008214	0.262073
-42.431271	-1.944941	1.996915	0.008171	0.261966
-42.785078	-1.908187	2.001920	0.008237	0.261814

-42.754790	-1.942426	2.011917	0.008231	0.261655
-43.377240	-1.883402	2.021914	0.008347	0.261356
-43.248532	-1.928253	2.031910	0.008323	0.261237
-43.647108	-1.891154	2.041907	0.008397	0.261041
-43.459190	-1.946554	2.051904	0.008362	0.260924
-43.954329	-1.891881	2.061901	0.008454	0.260728
-43.888805	-1.903262	2.071898	0.008441	0.260732
-44.118386	-1.889783	2.081894	0.008484	0.260575
-44.279857	-1.875555	2.091891	0.008514	0.260491
-44.101512	-1.908929	2.101888	0.008481	0.260487
-44.074092	-1.914173	2.111885	0.008476	0.260486
-44.083638	-1.912534	2.121882	0.008477	0.260486
-44.252027	-1.943653	2.131878	0.008508	0.260142
-44.690936	-1.863325	2.141875	0.008590	0.260146
-44.255486	-1.943212	2.151872	0.008509	0.260142
-44.542724	-1.890573	2.161869	0.008562	0.260145
-44.576302	-1.883843	2.171866	0.008568	0.260149
-44.414965	-1.914498	2.181862	0.008538	0.260142
-44.374026	-1.860499	2.191859	0.008531	0.260485
-44.378233	-1.858872	2.201856	0.008531	0.260490
-44.076270	-1.914809	2.211853	0.008475	0.260485
-44.236354	-1.884969	2.221850	0.008505	0.260489
-44.412477	-1.851982	2.231846	0.008537	0.260495
-44.364110	-1.853730	2.241843	0.008528	0.260535
-44.241201	-1.839695	2.251840	0.008505	0.260738
-44.312558	-1.825904	2.261837	0.008518	0.260743
-44.225851	-1.837769	2.271834	0.008502	0.260765
-44.111046	-1.805538	2.281830	0.008481	0.261060
-43.764893	-1.869800	2.291827	0.008416	0.261053
-43.836715	-1.839340	2.301824	0.008430	0.261150
-43.720307	-1.821064	2.311821	0.008408	0.261370
-43.453744	-1.869512	2.321818	0.008358	0.261370
-43.589096	-1.791409	2.331814	0.008383	0.261667
-43.352393	-1.828050	2.341811	0.008339	0.261703
-43.095862	-1.837656	2.351808	0.008291	0.261909
-43.065940	-1.828874	2.361805	0.008285	0.261988
-42.624332	-1.871538	2.371802	0.008203	0.262196
-42.343774	-1.903250	2.381798	0.008151	0.262304
-42.690718	-1.808401	2.391795	0.008215	0.262479
-42.401201	-1.832988	2.401792	0.008161	0.262635
-42.444286	-1.781816	2.411789	0.008169	0.262874
-42.056032	-1.834259	2.421786	0.008097	0.262975
-41.813232	-1.833043	2.431782	0.008052	0.263225
-41.465163	-1.888008	2.441779	0.007987	0.263271
-41.056091	-1.909590	2.451776	0.007910	0.263562
-40.865294	-1.935024	2.461773	0.007875	0.263614
-40.568891	-1.942628	2.471770	0.007820	0.263869
-40.596129	-1.916812	2.481766	0.007825	0.263984
-40.457280	-1.900256	2.491763	0.007799	0.264213
-39.977734	-1.959813	2.501760	0.007709	0.264366
-40.044416	-1.923557	2.511757	0.007722	0.264498
-39.863482	-1.907720	2.521754	0.007688	0.264765
-39.804693	-1.898611	2.531750	0.007677	0.264874
-39.102248	-1.978986	2.541747	0.007546	0.265134
-39.617213	-1.852568	2.551744	0.007642	0.265313
-39.335791	-1.870523	2.561741	0.007589	0.265495
-39.293567	-1.831671	2.571738	0.007581	0.265749
-39.224043	-1.813137	2.581734	0.007568	0.265919
-39.180139	-1.783727	2.591731	0.007560	0.266123
-39.168075	-1.735515	2.601728	0.007557	0.266398
-38.694334	-1.772390	2.611725	0.007469	0.266666
-38.270651	-1.814339	2.621722	0.007390	0.266858
-38.181246	-1.800619	2.631718	0.007373	0.267021
-37.830654	-1.806613	2.641715	0.007308	0.267334
-37.315966	-1.863603	2.651712	0.007212	0.267533
-36.975970	-1.894237	2.661709	0.007149	0.267702
-36.639670	-1.905041	2.671706	0.007086	0.267975
-36.608069	-1.873777	2.681702	0.007080	0.268176
-36.275616	-1.902169	2.691699	0.007018	0.268349
-36.300136	-1.852963	2.701696	0.007023	0.268591
-35.757860	-1.902328	2.711693	0.006921	0.268857
-35.677593	-1.883843	2.721690	0.006906	0.269036
-35.268343	-1.920606	2.731686	0.006830	0.269239
-35.131654	-1.896095	2.741683	0.006805	0.269505
-35.208553	-1.846597	2.751680	0.006819	0.269696
-34.623832	-1.917056	2.761677	0.006710	0.269889
-34.345885	-1.918331	2.771674	0.006658	0.270154
-33.704958	-1.991842	2.781670	0.006539	0.270385
-33.812588	-1.944100	2.791667	0.006559	0.270536
-33.664166	-1.930927	2.801664	0.006531	0.270752
-33.218974	-1.968796	2.811661	0.006448	0.270983
-33.517459	-1.876728	2.821658	0.006503	0.271185
-33.322456	-1.872837	2.831654	0.006467	0.271395
-33.173327	-1.838498	2.841651	0.006439	0.271724
-32.434624	-1.939248	2.851648	0.006301	0.271903
-32.499508	-1.889954	2.861645	0.006313	0.272103
-32.290778	-1.886323	2.871642	0.006274	0.272325
-31.557192	-1.964064	2.881638	0.006138	0.272621
-31.869188	-1.867701	2.891635	0.006196	0.272832
-31.165801	-1.960302	2.901632	0.006065	0.273020
-31.040748	-1.936985	2.911629	0.006041	0.273264
-30.860559	-1.921993	2.921626	0.006008	0.273518
-30.498930	-1.951899	2.931622	0.005940	0.273708
-30.284716	-1.956249	2.941619	0.005900	0.273892
-30.150807	-1.916883	2.951616	0.005875	0.274229
-29.699253	-1.964536	2.961613	0.005791	0.274411
-29.533926	-1.962055	2.971610	0.005760	0.274583
-29.151488	-1.982975	2.981606	0.005689	0.274840
-29.198636	-1.925511	2.991603	0.005698	0.275098
-28.928635	-1.934998	3.001600	0.005647	0.275307
-28.832817	-1.909812	3.011597	0.005629	0.275531
-28.643474	-1.903954	3.021594	0.005594	0.275743
-28.649130	-1.853696	3.031590	0.005595	0.276002
-28.375669	-1.858711	3.041587	0.005544	0.276237
-28.340616	-1.818890	3.051584	0.005537	0.276480
-28.028830	-1.827532	3.061581	0.005479	0.276732
-27.702434	-1.838088	3.071578	0.005418	0.276987
-27.289453	-1.859558	3.081574	0.005341	0.277268
-27.224187	-1.827371	3.091571	0.005329	0.277498
-26.919125	-1.835810	3.101568	0.005272	0.277744
-26.572060	-1.851259	3.111565	0.005207	0.277993
-26.504075	-1.814434	3.121562	0.005195	0.278249
-26.226172	-1.810679	3.131558	0.005143	0.278532
-26.151466	-1.777658	3.141555	0.005129	0.278775
-25.930884	-1.766927	3.151552	0.005088	0.279039
-25.647511	-1.769258	3.161549	0.005035	0.279295
-25.373757	-1.775441	3.171546	0.004984	0.279521
-25.183667	-1.750527	3.181542	0.004948	0.279829
-25.065547	-1.719342	3.191539	0.004926	0.280102
-24.879312	-1.698620	3.201536	0.004891	0.280384
-24.625644	-1.699483	3.211533	0.004844	0.280619
-24.414531	-1.694889	3.221530	0.004805	0.280841
-24.250023	-1.672090	3.231526	0.004774	0.281113
-24.050541	-1.656840	3.241523	0.004737	0.281378
-23.822339	-1.640601	3.251520	0.004694	0.281676
-23.667709	-1.613572	3.261517	0.004665	0.281959
-23.122293	-1.656897	3.271514	0.004563	0.282246
-23.139469	-1.601552	3.281510	0.004566	0.282515
-22.711925	-1.622733	3.291507	0.004487	0.282805
-22.811520	-1.551123	3.301504	0.004505	0.283079
-22.440091	-1.564913	3.311501	0.004436	0.283354
-22.185687	-1.555152	3.321498	0.004388	0.283640
-22.245400	-1.486327	3.331494	0.004399	0.283937
-21.637793	-1.539462	3.341491	0.004286	0.284229
-21.600880	-1.495003	3.351488	0.004279	0.284490
-21.291873	-1.487508	3.361485	0.004222	0.284814
-21.029221	-1.477038	3.371482	0.004173	0.285111
-21.092308	-1.403553	3.381478	0.004184	0.285426
-20.450746	-1.471000	3.391475	0.004065	0.285676
-20.516599	-1.405445	3.401472	0.004077	0.285947
-19.925329	-1.456266	3.411469	0.003967	0.286235
-20.183086	-1.350187	3.421466	0.004015	0.286534
-19.533446	-1.409685	3.431462	0.003894	0.286831
-19.546954	-1.351417	3.441459	0.003896	0.287113
-19.598215	-1.280083	3.451456	0.003905	0.287426
-19.067891	-1.315268	3.461453	0.003807	0.287734
-19.023314	-1.259212	3.471450	0.003798	0.288057
-18.444373	-1.309972	3.481446	0.003690	0.288331
-18.495413	-1.238268	3.491443	0.003700	0.288645
-18.010595	-1.267944	3.501440	0.003609	0.288939
-17.793818	-1.243853	3.511437	0.003569	0.289257
-17.380517	-1.264974	3.521434	0.003492	0.289528
-17.907268	-1.100793	3.531430	0.003590	0.289870
-17.007388	-1.203779	3.541427	0.003422	0.290173
-17.009655	-1.138189	3.551424	0.003422	0.290498
-16.776610	-1.128877	3.561421	0.003379	0.290756
-16.561958	-1.104633	3.571418	0.003339	0.291071
-16.685706	-1.020093	3.581414	0.003362	0.291380
-15.634139	-1.147745	3.591411	0.003166	0.291696
-16.004703	-1.023452	3.601408	0.003235	0.291978
-15.030653	-1.134812	3.611405	0.003053	0.292304
-15.139085	-1.056472	3.621402	0.003073	0.292595
-15.132030	-0.991624	3.631398	0.003072	0.292922
-14.329121	-1.079155	3.641395	0.002922	0.293211
-14.972497	-0.901670	3.651392	0.003042	0.293510
-13.736607	-1.060411	3.661389	0.002812	0.293836
-14.562443	-0.846096	3.671386	0.002965	0.294152
-13.235601	-1.024659	3.681382	0.002718	0.294460
-13.803422	-0.863018	3.691379	0.002824	0.294748
-12.513028	-1.032543	3.701376	0.002584	0.295067
-13.244965	-0.840032	3.711373	0.002720	0.295359
-12.299566	-0.950683	3.721370	0.002544	0.295659
-12.363692	-0.886679	3.731366	0.002555	0.295916
-12.607298	-0.777081	3.741363	0.002601	0.296236
-11.512460	-0.915495	3.751360	0.002397	0.296532
-11.981327	-0.765440	3.761357	0.002484	0.296849
-10.742190	-0.934099	3.771354	0.002253	0.297125
-11.507074	-0.733290	3.781350	0.002395	0.297426
-10.952694	-0.766979	3.791347	0.002292	0.297753
-10.145838	-0.854302	3.801344	0.002142	0.298041
-10.294465	-0.767231	3.811341	0.002169	0.298333
-9.975470	-0.765201	3.821338	0.002110	0.298624
-9.240957	-0.840840	3.831334	0.001973	0.298905
-9.396352	-0.747937	3.841331	0.002002	0.299218
-9.570390	-0.658481	3.851328	0.002034	0.299498
-8.962128	-0.702000	3.861325	0.001921	0.299823
-9.190807	-0.598546	3.871322	0.001963	0.300122
-8.050260	-0.735091	3.881318	0.001751	0.300463
-8.587344	-0.592275	3.891315	0.001851	0.300681
-7.241627	-0.774764	3.901312	0.001600	0.300980
-7.289305	-0.711813	3.911309	0.001609	0.301241
-7.533044	-0.607544	3.921306	0.001654	0.301530
-6.953217	-0.650244	3.931302	0.001546	0.301831
-6.978130	-0.591460	3.941299	0.001550	0.302091
-6.245606	-0.662651	3.951296	0.001414	0.302388
-6.357285	-0.581350	3.961293	0.001435	0.302680
-6.070134	-0.568636	3.971290	0.001381	0.302991
-5.806366	-0.560562	3.981286	0.001332	0.303259
-6.166090	-0.426874	3.991283	0.001399	0.303585
-5.272457	-0.527119	4.001280	0.001232	0.303881
-5.624150	-0.395486	4.011277	0.001298	0.304204
-4.641705	-0.512589	4.021274	0.001115	0.304496
-4.820704	-0.419339	4.031270	0.001148	0.304785
-4.225030	-0.463907	4.041267	0.001037	0.305088
-4.580016	-0.332813	4.051264	0.001103	0.305404
-4.274937	-0.330976	4.061261	0.001046	0.305676
-3.689190	-0.375170	4.071258	0.000937	0.305970
-3.517116	-0.342502	4.081254	0.000905	0.306273
-3.345986	-0.309847	4.091251	0.000873	0.306574
-2.634332	-0.378434	4.101248	0.000740	0.306861
-2.908934	-0.268013	4.111245	0.000791	0.307147
-2.283909	-0.317467	4.121242	0.000675	0.307449
-2.542008	-0.203380	4.131238	0.000722	0.307766
-1.728615	-0.286479	4.141235	0.000571	0.308070
-1.490283	-0.272459	4.151232	0.000527	0.308340
-1.553623	-0.195822	4.161229	0.000538	0.308646
-1.109764	-0.213755	4.171226	0.000455	0.308940
-1.024806	-0.162326	4.181222	0.000439	0.309253
-0.626157	-0.178633	4.191219	0.000365	0.309516
-0.422511	-0.147178	4.201216	0.000327	0.309836
-0.151003	-0.133090	4.211213	0.000276	0.310133
0.158234	-0.119910	4.221210	0.000219	0.310457
-0.113209	-0.016533	4.231206	0.000269	0.310709
0.000000	0.029351	4.241203	0.000248	0.311019

0.490579	0.221574	4.246208	0.000156	0.312325
1.248066	0.655573	4.251213	0.000015	0.314962
2.152135	1.352657	4.256218	-0.000154	0.318894
3.565393	2.253954	4.261222	-0.000418	0.324104
5.995647	3.276485	4.266227	-0.000871	0.330574
8.652718	4.568785	4.271232	-0.001366	0.338251
11.267341	6.184639	4.276237	-0.001854	0.347075
14.897952	7.949586	4.281242	-0.002532	0.357032
18.950672	9.972115	4.286246	-0.003288	0.368033
22.988886	12.353474	4.291251	-0.004041	0.380070
27.358084	15.041496	4.296256	-0.004856	0.393086
30.917133	18.240149	4.301261	-0.005521	0.406977
34.029089	21.896849	4.306266	-0.006103	0.421701
37.226590	25.912264	4.311270	-0.006701	0.437165
40.443098	30.294856	4.316275	-0.007303	0.453282
44.047084	34.994001	4.321280	-0.007977	0.470032
47.847647	40.036226	4.326285	-0.008688	0.487327
51.049903	45.579075	4.331290	-0.009288	0.505151
54.015903	51.523829	4.336294	-0.009844	0.523357
56.748422	57.856345	4.341299	-0.010357	0.541870
59.686857	64.502257	4.346304	-0.010909	0.560673
62.447309	71.507102	4.351309	-0.011427	0.579679
65.227661	78.829129	4.356314	-0.011950	0.598852
67.959175	86.453012	4.361318	-0.012463	0.618114
70.399205	94.410901	4.366323	-0.012923	0.637429
72.936036	102.609114	4.371328	-0.013401	0.656741
74.855644	111.145209	4.376333	-0.013764	0.675984
76.742866	119.880864	4.381338	-0.014121	0.695096
78.965327	128.749823	4.386342	-0.014541	0.714085
81.114029	137.786764	4.391347	-0.014947	0.732886
82.716101	147.085774	4.396352	-0.015251	0.751531
84.069521	156.524514	4.401357	-0.015509	0.769902
85.386416	166.077000	4.406362	-0.015761	0.788040
86.942090	175.656891	4.411366	-0.016057	0.805894
88.332950	185.330788	4.416371	-0.016322	0.823473
90.073763	195.002188	4.421376	-0.016652	0.840785
91.331215	204.767379	4.426381	-0.016893	0.857761
93.338487	214.417446	4.431386	-0.017273	0.874434
95.012620	224.135166	4.436390	-0.017591	0.890809
96.322868	233.917485	4.441395	-0.017842	0.906887
97.994450	243.622823	4.446400	-0.018159	0.922663
99.216073	253.374176	4.451405	-0.018393	0.938123
100.266581	263.132883	4.456410	-0.018595	0.953296
101.490041	272.812117	4.461414	-0.018829	0.968157
102.934587	282.413150	4.466419	-0.019105	0.982735
104.375380	292.008493	4.471424	-0.019379	0.997089
105.432581	301.561843	4.476429	-0.019582	1.011084
106.728610	311.031426	4.481434	-0.019830	1.024827
107.604110	320.533093	4.486438	-0.019999	1.038331
108.467303	329.972829	4.491443	-0.020166	1.051572
109.866529	339.258555	4.496448	-0.020433	1.064566
110.754845	348.578995	4.501453	-0.020604	1.077330
111.642477	357.844141	4.506458	-0.020775	1.089871
112.786588	367.005156	4.511462	-0.020995	1.102190
113.881225	376.135834	4.516467	-0.021204	1.114322
115.009451	385.201969	4.521472	-0.021420	1.126247
116.003438	394.252876	4.526477	-0.021611	1.137998
117.407545	403.210968	4.531482	-0.021879	1.149601
118.717318	412.137124	4.536486	-0.022128	1.161026
119.342632	421.119627	4.541491	-0.022251	1.172266
121.195794	429.855929	4.546496	-0.022602	1.183353
122.507821	438.662138	4.551501	-0.022852	1.194309
123.426282	447.491253	4.556506	-0.023029	1.205113
124.317180	456.309605	4.561510	-0.023200	1.215801
125.452122	465.028983	4.566515	-0.023417	1.226329
126.457708	473.763724	4.571520	-0.023610	1.236758
127.410488	482.431968	4.576525	-0.023793	1.247013
128.504083	491.093164	4.581530	-0.024003	1.257202
129.299169	499.770718	4.586534	-0.024156	1.267271
129.702146	508.470374	4.591539	-0.024237	1.277209
131.167294	516.941991	4.596544	-0.024516	1.287016
131.946452	525.552119	4.601549	-0.024666	1.296774
132.669778	534.133211	4.606554	-0.024807	1.306416
133.142229	542.830289	4.611558	-0.024900	1.316068
133.747156	551.324140	4.616563	-0.025018	1.325452
134.636912	559.795178	4.621568	-0.025190	1.334798
134.780903	568.349418	4.626573	-0.025222	1.344033
136.362697	576.649469	4.631578	-0.025522	1.353190
137.302155	585.063537	4.636582	-0.025703	1.362292
138.003341	593.506612	4.641587	-0.025839	1.371322
138.955009	601.908781	4.646592	-0.026021	1.380294
139.640841	610.337855	4.651597	-0.026155	1.389189
140.623820	618.708705	4.656602	-0.026343	1.398018
141.549113	627.071719	4.661606	-0.026521	1.406774
142.510153	635.412179	4.666611	-0.026705	1.415458
143.384036	643.781387	4.671616	-0.026874	1.424103
144.023041	652.179432	4.676621	-0.026998	1.432685
144.899385	660.500391	4.681626	-0.027167	1.441179
146.065598	668.795855	4.686630	-0.027389	1.449644
146.412112	677.216382	4.691635	-0.027459	1.458050
147.349506	685.520273	4.696640	-0.027639	1.466388
148.556884	693.794735	4.701645	-0.027870	1.474694
149.140924	702.129596	4.706650	-0.027984	1.482911
149.326910	710.534489	4.711654	-0.028024	1.491088
149.890681	718.844456	4.716659	-0.028135	1.499189
150.732266	727.118690	4.721664	-0.028297	1.507254
151.559424	735.364460	4.726669	-0.028456	1.515248
151.948070	743.693758	4.731674	-0.028534	1.523210
152.636473	751.979251	4.736678	-0.028668	1.531136
153.611213	760.185524	4.741683	-0.028854	1.538989
153.927272	768.523764	4.746688	-0.028919	1.546826
154.517645	776.785479	4.751693	-0.029034	1.554594
155.154908	785.018929	4.756698	-0.029158	1.562303
155.653907	793.301646	4.761702	-0.029257	1.570000
156.185246	801.555170	4.766707	-0.029361	1.577636
156.998592	809.757316	4.771712	-0.029518	1.585230
157.535406	818.022160	4.776717	-0.029623	1.592805
158.059023	826.251159	4.781722	-0.029726	1.600308
158.686710	834.492263	4.786726	-0.029848	1.607803
158.869798	842.785774	4.791731	-0.029888	1.615246
159.636341	850.969167	4.796736	-0.030036	1.622639
160.139190	859.203765	4.801741	-0.030135	1.630007
160.843476	867.412610	4.806746	-0.030272	1.637347
161.422525	875.597738	4.811750	-0.030385	1.644616
161.702643	883.848716	4.816755	-0.030442	1.651868
162.719365	891.973025	4.821760	-0.030637	1.659081
162.903803	900.217670	4.826765	-0.030677	1.666251
163.341819	908.453398	4.831770	-0.030764	1.673418
164.040786	916.598842	4.836774	-0.030899	1.680512
164.744805	924.760603	4.841779	-0.031036	1.687591
165.206747	932.994510	4.846784	-0.031127	1.694669
165.707240	941.183347	4.851789	-0.031226	1.701684
166.251828	949.379032	4.856794	-0.031332	1.708681
166.815069	957.563421	4.861798	-0.031443	1.715643
167.301501	965.723996	4.866803	-0.031539	1.722547
168.032206	973.881077	4.871808	-0.031680	1.729452
168.826565	982.002660	4.876813	-0.031833	1.736308
169.556240	990.162070	4.881818	-0.031975	1.743159
169.844036	998.405103	4.886822	-0.032034	1.749996
170.583723	1006.533383	4.891827	-0.032177	1.756769
171.544645	1014.653089	4.896832	-0.032361	1.763538
171.753363	1022.899518	4.901837	-0.032405	1.770288
172.446710	1031.052355	4.906842	-0.032540	1.776998
173.072565	1039.210721	4.911846	-0.032662	1.783678
173.412315	1047.422940	4.916851	-0.032730	1.790340
174.454146	1055.521724	4.921856	-0.032930	1.796975
175.157952	1063.650421	4.926861	-0.033066	1.803566
175.627452	1071.817070	4.931866	-0.033159	1.810135
175.945222	1080.025556	4.936870	-0.033223	1.816694
176.324575	1088.191691	4.941875	-0.033299	1.823203
176.845234	1096.349121	4.946880	-0.033402	1.829700
177.605449	1104.446777	4.951885	-0.033548	1.836155
178.354903	1112.553971	4.956890	-0.033693	1.842594
179.281598	1120.662185	4.961894	-0.033871	1.849032
179.700604	1128.850229	4.966899	-0.033955	1.855449
180.681195	1136.926771	4.971904	-0.034143	1.861824
181.464148	1145.066480	4.976909	-0.034294	1.868203
181.910068	1153.248562	4.981914	-0.034382	1.874552
182.332630	1161.408779	4.986918	-0.034466	1.880861
182.979346	1169.527402	4.991923	-0.034592	1.887142
183.411267	1177.715884	4.996928	-0.034678	1.893431
184.209730	1185.780236	5.001933	-0.034832	1.899647
185.011349	1193.878704	5.006938	-0.034986	1.905868
185.558080	1202.060920	5.011942	-0.035093	1.912103
186.120719	1210.174164	5.016947	-0.035204	1.918268
186.744718	1218.304738	5.021952	-0.035325	1.924432
187.172690	1226.461271	5.026957	-0.035410	1.930574
187.785226	1234.581236	5.031962	-0.035529	1.936690
188.659470	1242.682678	5.036966	-0.035698	1.942802
189.356551	1250.805427	5.041971	-0.035833	1.948890
190.152929	1258.900694	5.046976	-0.035986	1.954951
190.654553	1267.021021	5.051981	-0.036085	1.960978
191.305688	1275.123235	5.056986	-0.036212	1.966989
191.666422	1283.313600	5.061990	-0.036284	1.973015
192.385864	1291.383808	5.066995	-0.036423	1.978974
192.856863	1299.518698	5.072000	-0.036517	1.984934
193.574272	1307.630883	5.077005	-0.036655	1.990887
194.251239	1315.722046	5.082010	-0.036787	1.996803
195.029066	1323.818000	5.087014	-0.036937	2.002715
195.643776	1331.930573	5.092019	-0.037057	2.008603
196.473747	1340.031156	5.097024	-0.037217	2.014489
197.036075	1348.154650	5.102029	-0.037327	2.020346
197.791595	1356.254036	5.107034	-0.037473	2.026188
198.256611	1364.425482	5.112038	-0.037565	2.032034
198.849386	1372.498797	5.117043	-0.037680	2.037807
199.474430	1380.615571	5.122048	-0.037802	2.043598
200.388707	1388.660177	5.127053	-0.037978	2.049351
200.762481	1396.822376	5.132058	-0.038053	2.055115
201.364881	1404.926398	5.137062	-0.038170	2.060845
202.045687	1413.009930	5.142067	-0.038302	2.066553
202.592747	1421.150358	5.147072	-0.038409	2.072271
202.736882	1429.315443	5.152077	-0.038442	2.077950
203.944942	1437.298050	5.157082	-0.038672	2.083594
204.745845	1445.398946	5.162086	-0.038826	2.089263
205.441788	1453.472587	5.167091	-0.038961	2.094887
206.032994	1461.597632	5.172096	-0.039076	2.100521
206.472757	1469.746198	5.177101	-0.039164	2.106141
207.202245	1477.846443	5.182106	-0.039305	2.111741
208.089944	1485.913471	5.187110	-0.039475	2.117319
208.713057	1493.979298	5.192115	-0.039597	2.122856
208.952367	1502.149396	5.197120	-0.039647	2.128411
209.726644	1510.192768	5.202125	-0.039796	2.133918
210.251690	1518.298095	5.207130	-0.039899	2.139428
210.881813	1526.393096	5.212134	-0.040022	2.144927
210.862491	1534.582428	5.217139	-0.040024	2.150412
211.537730	1542.646905	5.222144	-0.040155	2.155867
212.395964	1550.662967	5.227149	-0.040320	2.161293
213.399198	1558.681198	5.232154	-0.040512	2.166721
213.684636	1566.860853	5.237158	-0.040570	2.172173
214.322586	1574.924041	5.242163	-0.040694	2.177568
215.274415	1582.980974	5.247168	-0.040877	2.182975
215.843992	1591.084066	5.252173	-0.040988	2.188363
216.429176	1599.189405	5.257178	-0.041103	2.193741
217.045840	1607.271489	5.262182	-0.041223	2.199093
217.831598	1615.290691	5.267187	-0.041374	2.204406
218.040694	1623.481234	5.272192	-0.041419	2.209765
218.696443	1631.530638	5.277197	-0.041546	2.215060
218.940546	1639.674531	5.282202	-0.041597	2.220366
219.497317	1647.757801	5.287206	-0.041706	2.225648
220.134491	1655.829288	5.292211	-0.041830	2.230918
220.671558	1663.943145	5.297216	-0.041935	2.236193
221.208406	1671.973725	5.302221	-0.042040	2.241402
221.731018	1680.040740	5.307226	-0.042143	2.246621
222.448839	1688.124991	5.312230	-0.042282	2.251856
222.984500	1696.198946	5.317235	-0.042387	2.257056
223.458078	1704.304513	5.322240	-0.042481	2.262258
224.339816	1712.326683	5.327245	-0.042650	2.267432
224.829528	1720.478364	5.332250	-0.042747	2.272641
225.211603	1728.581766	5.337254	-0.042823	2.277798
225.748859	1736.622823	5.342259	-0.042928	2.282918
225.889000	1744.784040	5.347264	-0.042960	2.288067
226.558711	1752.803614	5.352269	-0.043090	2.293161
227.215552	1760.832809	5.357274	-0.043217	2.298249
228.270077	1768.841386	5.362278	-0.043419	2.303347
228.969500	1776.882571	5.367283	-0.043555	2.308423
229.364189	1785.027328	5.372288	-0.043633	2.313526
229.861894	1793.080835	5.377293	-0.043731	2.318571
230.362046	1801.146607	5.382298	-0.043830	2.323611
230.415907	1809.347507	5.387302	-0.043845	2.328687
230.402964	1817.488108	5.392307	-0.043848	2.333708
231.486324	1825.454335	5.397312	-0.044055	2.338704
232.151470	1833.476074	5.402317	-0.044184	2.343688
231.938138	1841.676068	5.407322	-0.044150	2.348697
232.757577	1849.686783	5.412326	-0.044308	2.353665
233.314005	1857.706945	5.417331	-0.044417	2.358607
233.953131	1865.730022	5.422336	-0.044541	2.363547
233.951504	1873.901073	5.427341	-0.044546	2.368514
234.786655	1881.906562	5.432346	-0.044707	2.373438
235.487514	1889.971656	5.437350	-0.044843	2.378377
236.202702	1897.969804	5.442355	-0.044981	2.383267
236.491411	1906.109175	5.447360	-0.045040	2.388197
236.429795	1914.286436	5.452365	-0.045034	2.393111
236.875923	1922.315479	5.457370	-0.045122	2.397967
237.604562	1930.317753	5.462374	-0.045263	2.402819
238.274135	1938.339641	5.467379	-0.045393	2.407669
238.698212	1946.456280	5.472384	-0.045477	2.412546
238.942425	1954.583727	5.477389	-0.045528	2.417405
239.391342	1962.631789	5.482394	-0.045617	2.422223
239.824738	1970.728285	5.487398	-0.045703	2.427059
240.281735	1978.802979	5.492403	-0.045794	2.431874
240.572432	1986.898330	5.497408	-0.045853	2.436679
240.931320	1994.927410	5.502413	-0.045925	2.441440
241.588078	2002.920257	5.507418	-0.046053	2.446194
242.463167	2010.929786	5.512422	-0.046221	2.450966
242.937676	2018.993942	5.517427	-0.046315	2.455729
243.240358	2027.130627	5.522432	-0.046376	2.460511
243.848204	2035.131080	5.527437	-0.046495	2.465229
244.506884	2043.188585	5.532442	-0.046623	2.469974
245.228598	2051.230921	5.537446	-0.046762	2.474706
245.390578	2059.312599	5.542451	-0.046798	2.479409
246.432822	2067.281999	5.547456	-0.046997	2.484105
246.844520	2075.394851	5.552461	-0.047079	2.488827
247.218344	2083.497999	5.557466	-0.047154	2.493532
248.247557	2091.507824	5.562470	-0.047351	2.498223
248.767216	2099.553916	5.567475	-0.047453	2.502887
249.369320	2107.660210	5.572480	-0.047570	2.507584
249.716110	2115.769884	5.577485	-0.047640	2.512255
250.144299	2123.834612	5.582490	-0.047725	2.516897
251.018028	2131.843562	5.587494	-0.047893	2.521531
251.431976	2139.897463	5.592499	-0.047976	2.526149
252.071166	2147.984370	5.597504	-0.048100	2.530794
252.615338	2156.040666	5.602509	-0.048207	2.535405
253.579247	2164.025565	5.607514	-0.048391	2.539998
253.837412	2172.141388	5.612518	-0.048445	2.544606
254.485006	2180.207873	5.617523	-0.048571	2.549205
255.078424	2188.265755	5.622528	-0.048686	2.553787
255.424843	2196.339431	5.627533	-0.048756	2.558352
256.155181	2204.335438	5.632538	-0.048898	2.562893
256.524436	2212.441355	5.637542	-0.048972	2.567461
257.034117	2220.494119	5.642547	-0.049072	2.572001
257.420857	2228.581779	5.647552	-0.049149	2.576544
257.984515	2236.609710	5.652557	-0.049259	2.581059
258.729969	2244.628516	5.657562	-0.049403	2.585572
259.165600	2252.752375	5.662566	-0.049490	2.590115
259.841779	2260.862726	5.667571	-0.049621	2.594658
260.415364	2268.853824	5.672576	-0.049733	2.599121
260.653136	2276.942754	5.677581	-0.049783	2.603606
260.913489	2284.995081	5.682586	-0.049837	2.608065
261.820102	2292.987549	5.687590	-0.050011	2.612528
262.145374	2301.039899	5.692595	-0.050076	2.616976
262.890405	2309.067157	5.697600	-0.050220	2.621431
263.142493	2317.145419	5.702605	-0.050273	2.625873
264.044829	2325.147490	5.707610	-0.050446	2.630310
264.622751	2333.231682	5.712614	-0.050559	2.634763
264.942571	2341.277337	5.717619	-0.050624	2.639169
265.409253	2349.324774	5.722624	-0.050716	2.643578
265.900788	2357.389480	5.727629	-0.050813	2.647991
266.769219	2365.400108	5.732634	-0.050980	2.652393
267.184196	2373.489392	5.737638	-0.051062	2.656799
267.991226	2381.482845	5.742643	-0.051218	2.661173
268.717244	2389.538111	5.747648	-0.051358	2.665566
269.179789	2397.629557	5.752653	-0.051450	2.669955
269.780950	2405.661265	5.757658	-0.051567	2.674313
270.227015	2413.745769	5.762662	-0.051655	2.678683
270.684669	2421.767709	5.767667	-0.051746	2.683012
271.077545	2429.853988	5.772672	-0.051824	2.687364
271.701634	2437.891570	5.777677	-0.051946	2.691699
272.361804	2445.935174	5.782682	-0.052074	2.696031
273.064747	2453.966391	5.787686	-0.052210	2.700353
273.641043	2461.976268	5.792691	-0.052323	2.704648
274.279643	2470.044677	5.797696	-0.052447	2.708972
274.932323	2478.109920	5.802701	-0.052574	2.713287
275.010677	2486.229225	5.807706	-0.052594	2.717588
276.046532	2494.152844	5.812710	-0.052792	2.721839
276.833348	2502.165570	5.817715	-0.052944	2.726115
277.535851	2510.262568	5.822720	-0.053080	2.730422
277.672759	2518.381614	5.827725	-0.053111	2.734699
278.374163	2526.410899	5.832730	-0.053246	2.738958
278.862889	2534.462364	5.837734	-0.053343	2.743208
279.472868	2542.474549	5.842739	-0.053462	2.747438
279.932595	2550.615387	5.847744	-0.053553	2.751719
280.421837	2558.669237	5.852749	-0.053649	2.755951
281.141157	2566.669502	5.857754	-0.053788	2.760162
281.866336	2574.657678	5.862758	-0.053928	2.764360
282.318717	2582.733962	5.867763	-0.054018	2.768581
283.168056	2590.765196	5.872768	-0.054181	2.772796
283.582418	2598.842833	5.877773	-0.054264	2.777003
284.205229	2606.871595	5.882778	-0.054385	2.781190
285.237907	2614.849610	5.887782	-0.054583	2.785369
285.688756	2622.929557	5.892787	-0.054672	2.789560
286.633085	2630.932046	5.897792	-0.054853	2.793733
287.219026	2638.963326	5.902797	-0.054967	2.797894
287.665734	2647.043833	5.907802	-0.055056	2.802065
288.434474	2655.071128	5.912806	-0.055204	2.806222
288.966298	2663.159660	5.917811	-0.055309	2.810390
289.682300	2671.209792	5.922816	-0.055447	2.814543
290.184350	2679.257153	5.927821	-0.055546	2.818676
290.658126	2687.283673	5.932826	-0.055639	2.822790
291.611075	2695.316088	5.937830	-0.055822	2.826929
291.563723	2703.482130	5.942835	-0.055819	2.831071
292.600305	2711.444934	5.947840	-0.056017	2.835168
293.388430	2719.427975	5.952845	-0.056169	2.839254
294.021879	2727.448715	5.957850	-0.056292	2.843344
294.339150	2735.563947	5.962854	-0.056357	2.847457
294.746644	2743.628103	5.967859	-0.056438	2.851544
295.605999	2751.642025	5.972864	-0.056603	2.855626
296.206755	2759.676793	5.977869	-0.056720	2.859698
296.252577	2767.779511	5.982874	-0.056734	2.863766
297.018753	2775.798417	5.987878	-0.056882	2.867827
297.585848	2783.824795	5.992883	-0.056993	2.871874
298.095243	2791.906857	5.997888	-0.057093	2.875941
298.743466	2799.905461	6.002893	-0.057219	2.879968
299.202976	2807.928711	6.007898	-0.057310	2.883990
299.053199	2816.114154	6.012902	-0.057287	2.888054
299.640539	2824.090015	6.017907	-0.057402	2.892049
300.323361	2832.121334	6.022912	-0.057534	2.896071
300.782064	2840.165284	6.027917	-0.057625	2.900081
301.295432	2848.152637	6.032922	-0.057726	2.904061
302.034859	2856.194358	6.037926	-0.057869	2.908074
302.514992	2864.268195	6.042931	-0.057964	2.912083
302.979786	2872.338644	6.047936	-0.058055	2.916084
303.617193	2880.328920	6.052941	-0.058179	2.920050
304.199117	2888.317468	6.057946	-0.058293	2.924006
304.514143	2896.423038	6.062950	-0.058357	2.928000
305.064181	2904.464856	6.067955	-0.058465	2.931969
306.166511	2912.445637	6.072960	-0.058675	2.935933
306.459262	2920.522862	6.077965	-0.058735	2.939896
306.758870	2928.564938	6.082970	-0.058796	2.943836
307.414462	2936.598887	6.087974	-0.058923	2.947785
308.120988	2944.609520	6.092979	-0.059060	2.951721
308.478076	2952.703397	6.097984	-0.059132	2.955673
309.199791	2960.685589	6.102989	-0.059272	2.959585
309.762683	2968.715325	6.107994	-0.059382	2.963506
310.395588	2976.756807	6.112998	-0.059505	2.967431
310.366848	2984.882181	6.118003	-0.059505	2.971357
311.314046	2992.896042	6.123008	-0.059687	2.975275
312.018360	3000.879773	6.128013	-0.059823	2.979160
312.114557	3008.931326	6.133018	-0.059846	2.983042
312.710810	3017.017671	6.138022	-0.059962	2.986960
313.036448	3025.070463	6.143027	-0.060028	2.990844
313.784495	3033.059371	6.148032	-0.060173	2.994713
314.029760	3041.110778	6.153037	-0.060224	2.998582
314.582338	3049.100756	6.158042	-0.060332	3.002432
315.231644	3057.164241	6.163046	-0.060458	3.006316
315.268363	3065.262996	6.168051	-0.060470	3.010182
315.539542	3073.306013	6.173056	-0.060526	3.014027
315.604635	3081.404248	6.178061	-0.060544	3.017884
316.271831	3089.341451	6.183066	-0.060673	3.021689
316.727082	3097.383774	6.188070	-0.060763	3.025529
317.255308	3105.392631	6.193075	-0.060867	3.029352
317.866887	3113.434145	6.198080	-0.060986	3.033189
318.398940	3121.464779	6.203085	-0.061090	3.037012
318.705522	3129.520160	6.208090	-0.061153	3.040831
319.404171	3137.528309	6.213094	-0.061288	3.044642
319.572754	3145.579594	6.218099	-0.061325	3.048442
320.120640	3153.630096	6.223104	-0.061432	3.052256
320.566007	3161.696958	6.228109	-0.061520	3.056068
321.037221	3169.706871	6.233114	-0.061613	3.059849
321.510442	3177.757401	6.238118	-0.061707	3.063645
321.943635	3185.784260	6.243123	-0.061793	3.067423
322.602872	3193.840042	6.248128	-0.061921	3.071220
322.972782	3201.915848	6.253133	-0.061995	3.075009
323.424432	3209.894267	6.258138	-0.062084	3.078751
324.286493	3217.890864	6.263142	-0.062250	3.082516
324.911086	3225.897143	6.268147	-0.062371	3.086270
325.759367	3233.923606	6.273152	-0.062535	3.090039
326.301320	3241.977400	6.278157	-0.062641	3.093802
326.728248	3250.028048	6.283162	-0.062726	3.097553
327.201890	3258.085289	6.288166	-0.062819	3.101305
327.547889	3266.099253	6.293171	-0.062889	3.105026
328.079904	3274.170502	6.298176	-0.062993	3.108778
328.472672	3282.213005	6.303181	-0.063072	3.112505
328.996709	3290.220936	6.308186	-0.063175	3.116218
329.508294	3298.275934	6.313190	-0.063275	3.119947
329.946125	3306.257825	6.318195	-0.063362	3.123635
330.716655	3314.290247	6.323200	-0.063511	3.127358
331.253506	3322.357362	6.328205	-0.063616	3.131080
331.510376	3330.409074	6.333210	-0.063669	3.134779
332.231492	3338.427627	6.338214	-0.063809	3.138478
332.384912	3346.477548	6.343219	-0.063842	3.142162
332.950679	3354.509119	6.348224	-0.063953	3.145852
333.502134	3362.542920	6.353229	-0.064061	3.149538
333.778349	3370.591645	6.358234	-0.064118	3.153214
334.197731	3378.627550	6.363238	-0.064201	3.156886
334.727094	3386.618183	6.368243	-0.064305	3.160538
335.288746	3394.605521	6.373248	-0.064415	3.164186
335.621219	3402.681367	6.378253	-0.064482	3.167859
335.873099	3410.773953	6.383258	-0.064534	3.171532
335.899192	3418.869755	6.388262	-0.064544	3.175193
336.211614	3426.858460	6.393267	-0.064608	3.178813
336.412360	3434.904700	6.398272	-0.064650	3.182450
336.869021	3442.895895	6.403277	-0.064741	3.186069
336.981028	3450.958943	6.408282	-0.064767	3.189702
337.965022	3458.924055	6.413286	-0.064955	3.193324
337.903119	3467.018350	6.418291	-0.064949	3.196954
338.243149	3475.060851	6.423296	-0.065018	3.200575
338.537867	3483.047934	6.428301	-0.065078	3.204165
339.030012	3491.065709	6.433306	-0.065175	3.207773
339.727497	3499.092000	6.438310	-0.065310	3.211389
340.278230	3507.107407	6.443315	-0.065418	3.214990
341.083904	3515.106399	6.448320	-0.065573	3.218590
341.530466	3523.168532	6.453325	-0.065661	3.222199
341.781551	3531.219148	6.458330	-0.065713	3.225791
342.399493	3539.276485	6.463334	-0.065834	3.229396
342.365097	3547.341414	6.468339	-0.065833	3.232974
342.579550	3555.371375	6.473344	-0.065878	3.236543
343.149127	3563.347280	6.478349	-0.065989	3.240099
343.683789	3571.328450	6.483354	-0.066094	3.243651
344.057245	3579.409390	6.488358	-0.066169	3.247237
344.117297	3587.450896	6.493363	-0.066185	3.250789
344.892339	3595.459338	6.498368	-0.066335	3.254351
345.091341	3603.509994	6.503373	-0.066377	3.257905
345.714362	3611.501045	6.508378	-0.066499	3.261445
346.093364	3619.554281	6.513382	-0.066574	3.264999
346.603845	3627.573012	6.518387	-0.066675	3.268540
346.924727	3635.644555	6.523392	-0.066740	3.272092
347.204382	3643.691030	6.528397	-0.066797	3.275627
347.566341	3651.665950	6.533402	-0.066870	3.279131
348.019049	3659.686290	6.538406	-0.066959	3.282654
348.317170	3667.733917	6.543411	-0.067020	3.286179
348.972739	3675.751966	6.548416	-0.067148	3.289701
349.042175	3683.844537	6.553421	-0.067166	3.293229
349.533603	3691.827774	6.558426	-0.067263	3.296722
349.947746	3699.900758	6.563430	-0.067345	3.300248
350.533093	3707.854855	6.568435	-0.067459	3.303724
350.628664	3715.950449	6.573440	-0.067482	3.307240
351.250132	3723.973421	6.578445	-0.067603	3.310740
351.805637	3731.972877	6.583450	-0.067712	3.314224
352.246724	3740.005022	6.588454	-0.067799	3.317714
352.418402	3748.055506	6.593459	-0.067837	3.321197
352.724733	3756.062680	6.598464	-0.067899	3.324663
353.107294	3764.124479	6.603469	-0.067975	3.328153
353.323083	3772.154626	6.608474	-0.068021	3.331618
353.832402	3780.198421	6.613478	-0.068121	3.335097
354.283535	3788.174590	6.618483	-0.068210	3.338541
354.519113	3796.261970	6.623488	-0.068259	3.342021
354.790408	3804.294277	6.628493	-0.068315	3.345474
355.223664	3812.273365	6.633498	-0.068401	3.348908
355.761020	3820.323271	6.638502	-0.068507	3.352372
356.164964	3828.361297	6.643507	-0.068587	3.355823
356.632526	3836.321758	6.648512	-0.068679	3.359239
356.893203	3844.386225	6.653517	-0.068733	3.362688
357.254313	3852.423975	6.658522	-0.068806	3.366126
357.741943	3860.481892	6.663526	-0.068902	3.369573
358.061198	3868.509256	6.668531	-0.068967	3.372998
358.241596	3876.576058	6.673536	-0.069005	3.376431
358.718692	3884.589513	6.678541	-0.069100	3.379849
359.158894	3892.552587	6.683546	-0.069187	3.383240
359.493734	3900.625855	6.688550	-0.069254	3.386671
359.486168	3908.652617	6.693555	-0.069258	3.390066
359.957265	3916.710844	6.698560	-0.069351	3.393489
360.407370	3924.741492	6.703565	-0.069440	3.396895
360.802911	3932.725070	6.708570	-0.069519	3.400276
361.118802	3940.748014	6.713574	-0.069583	3.403668
361.384414	3948.787083	6.718579	-0.069638	3.407061
361.826819	3956.824570	6.723584	-0.069726	3.410456
362.025496	3964.863304	6.728589	-0.069768	3.413839
362.294364	3972.900493	6.733594	-0.069823	3.417221
363.067389	3980.893814	6.738598	-0.069973	3.420599
363.237915	3988.876452	6.743603	-0.070010	3.423948
363.477783	3996.973196	6.748608	-0.070060	3.427344
364.133838	4004.994857	6.753613	-0.070187	3.430720
364.600688	4012.949188	6.758618	-0.070279	3.434057
364.982517	4021.003147	6.763622	-0.070356	3.437430
365.540452	4029.041650	6.768627	-0.070465	3.440799
365.915519	4037.021601	6.773632	-0.070540	3.444134
366.233693	4045.073485	6.778637	-0.070604	3.447493
366.630902	4053.119375	6.783642	-0.070684	3.450850
367.179230	4061.170700	6.788646	-0.070791	3.454210
367.568293	4069.141453	6.793651	-0.070869	3.457529
367.763114	4077.226364	6.798656	-0.070910	3.460885
368.102306	4085.231255	6.803661	-0.070979	3.464209
368.078515	4093.290063	6.808666	-0.070980	3.467540
368.402466	4101.398049	6.813670	-0.071045	3.470900
368.905665	4109.311864	6.818675	-0.071144	3.474182
369.468750	4117.293739	6.823680	-0.071254	3.477492
369.690288	4125.395106	6.828685	-0.071301	3.480836
370.053604	4133.319175	6.833690	-0.071374	3.484108
370.715080	4141.363807	6.838694	-0.071502	3.487437
371.062243	4149.419449	6.843699	-0.071572	3.490756
371.259339	4157.460607	6.848704	-0.071614	3.494062
371.664249	4165.514327	6.853709	-0.071695	3.497376
371.831506	4173.548165	6.858714	-0.071731	3.500672
372.011960	4181.568765	6.863718	-0.071770	3.503959
372.106384	4189.632803	6.868723	-0.071793	3.507258
372.825416	4197.647765	6.873728	-0.071932	3.510554
373.220264	4205.634754	6.878733	-0.072011	3.513825
373.347135	4213.702437	6.883738	-0.072040	3.517117
373.917392	4221.716324	6.888742	-0.072151	3.520398
374.328505	4229.674323	6.893747	-0.072233	3.523648
374.452427	4237.753604	6.898752	-0.072261	3.526936
374.764750	4245.830524	6.903757	-0.072325	3.530225
374.826490	4253.838995	6.908762	-0.072342	3.533476
375.163043	4261.879187	6.913766	-0.072410	3.536745
375.214973	4269.890984	6.918771	-0.072424	3.539990
375.866226	4277.877380	6.923776	-0.072551	3.543241
376.510270	4285.917567	6.928781	-0.072676	3.546511
376.728627	4293.917471	6.933786	-0.072722	3.549748
377.240095	4302.013225	6.938790	-0.072823	3.553029
377.316590	4310.042737	6.943795	-0.072842	3.556268
377.997340	4317.954792	6.948800	-0.072974	3.559474
378.396080	4325.982531	6.953805	-0.073054	3.562716
378.636608	4334.047548	6.958810	-0.073104	3.565965
378.942230	4342.063038	6.963814	-0.073166	3.569192
379.183789	4350.117975	6.968819	-0.073216	3.572431
379.791500	4358.119501	6.973824	-0.073335	3.575657
379.866843	4366.111233	6.978829	-0.073354	3.578859
380.087066	4374.176694	6.983834	-0.073400	3.582093
380.689912	4382.175895	6.988838	-0.073518	3.585308
380.884746	4390.204874	6.993843	-0.073559	3.588520
381.117515	4398.286101	6.998848	-0.073608	3.591751
381.394307	4406.319773	7.003853	-0.073665	3.594962
381.878179	4414.268734	7.008858	-0.073760	3.598142
382.210883	4422.330976	7.013862	-0.073827	3.601360
382.689419	4430.292542	7.018867	-0.073922	3.604539
383.121053	4438.315882	7.023872	-0.074007	3.607739
383.505228	4446.410591	7.028877	-0.074084	3.610962
383.819089	4454.399637	7.033882	-0.074148	3.614139
384.069987	4462.473727	7.038886	-0.074200	3.617344
384.288929	4470.508470	7.043891	-0.074246	3.620531
384.791116	4478.501655	7.048896	-0.074345	3.623706
385.298182	4486.568143	7.053901	-0.074444	3.626907
385.509047	4494.575288	7.058906	-0.074489	3.630074
385.924816	4502.632769	7.063910	-0.074572	3.633263
386.106340	4510.624568	7.068915	-0.074611	3.636417
386.530100	4518.607057	7.073920	-0.074695	3.639572
386.856333	4526.632133	7.078925	-0.074761	3.642737
387.006963	4534.663184	7.083930	-0.074794	3.645898
387.400118	4542.692224	7.088934	-0.074873	3.649061
387.971222	4550.680942	7.093939	-0.074984	3.652211
388.541082	4558.725515	7.098944	-0.075096	3.655380
388.790767	4566.749356	7.103949	-0.075147	3.658529
388.861383	4574.774289	7.108954	-0.075166	3.661671
389.168066	4582.823383	7.113958	-0.075228	3.664826
389.646403	4590.811750	7.118963	-0.075323	3.667959
390.103336	4598.859861	7.123968	-0.075413	3.671113
390.234621	4606.901388	7.128973	-0.075443	3.674252
390.065773	4614.951939	7.133978	-0.075417	3.677384
390.935166	4622.927272	7.138982	-0.075584	3.680511
391.182610	4630.887819	7.143987	-0.075635	3.683614
391.317079	4638.977789	7.148992	-0.075665	3.686761
391.661283	4647.025169	7.153997	-0.075735	3.689895
391.820030	4655.050183	7.159002	-0.075770	3.693012
392.277796	4663.099837	7.164006	-0.075860	3.696144
392.547220	4671.075597	7.169011	-0.075915	3.699240
392.871077	4679.127981	7.174016	-0.075981	3.702364
393.351635	4687.140529	7.179021	-0.076076	3.705474
393.409841	4695.163014	7.184026	-0.076092	3.708575
393.859655	4703.269089	7.189030	-0.076181	3.711715
394.267012	4711.274890	7.194035	-0.076262	3.714813
394.707672	4719.227007	7.199040	-0.076349	3.717888
394.985496	4727.272857	7.204045	-0.076406	3.720992
395.232515	4735.235009	7.209050	-0.076458	3.724061
395.618938	4743.308522	7.214054	-0.076535	3.727174
395.754414	4751.328018	7.219059	-0.076565	3.730257
396.310824	4759.338318	7.224064	-0.076674	3.733344
396.559803	4767.391672	7.229069	-0.076726	3.736438
396.723230	4775.374163	7.234074	-0.076762	3.739500
397.281878	4783.418671	7.239078	-0.076871	3.742592
397.540099	4791.428895	7.244083	-0.076924	3.745662
397.769240	4799.423963	7.249088	-0.076972	3.748722
398.248741	4807.484181	7.254093	-0.077067	3.751811
398.778489	4815.462102	7.259098	-0.077171	3.754867
399.277515	4823.512625	7.264102	-0.077269	3.757948
399.451387	4831.565067	7.269107	-0.077307	3.761019
399.750638	4839.529287	7.274112	-0.077368	3.764056
400.115756	4847.596992	7.279117	-0.077441	3.767132
400.583224	4855.569695	7.284122	-0.077533	3.770172
401.034715	4863.623273	7.289126	-0.077622	3.773240
401.468412	4871.633660	7.294131	-0.077708	3.776288
401.858775	4879.622082	7.299136	-0.077786	3.779325
402.282093	4887.708282	7.304141	-0.077871	3.782396
402.428750	4895.691961	7.309146	-0.077903	3.785420
402.976082	4903.736019	7.314150	-0.078010	3.788474
403.122286	4911.781562	7.319155	-0.078043	3.791516
403.505435	4919.802655	7.324160	-0.078119	3.794553
403.888121	4927.843628	7.329165	-0.078196	3.797594
404.051937	4935.805005	7.334170	-0.078232	3.800597
404.358627	4943.837137	7.339174	-0.078294	3.803629
404.681228	4951.844144	7.344179	-0.078359	3.806648
405.228970	4959.883215	7.349184	-0.078467	3.809682
405.367252	4967.946752	7.354189	-0.078498	3.812714
405.598634	4975.975446	7.359194	-0.078546	3.815733
406.198400	4983.978750	7.364198	-0.078663	3.818747
406.296024	4992.011682	7.369203	-0.078687	3.821759
406.537616	5000.027498	7.374208	-0.078737	3.824766
406.956430	5008.046000	7.379213	-0.078820	3.827775
407.066156	5016.116675	7.384218	-0.078846	3.830794
407.342674	5024.123832	7.389222	-0.078903	3.833791
407.880688	5032.135560	7.394227	-0.079008	3.836793
408.239376	5040.146614	7.399232	-0.079080	3.839788
408.453443	5048.129696	7.404237	-0.079125	3.842767
408.705263	5056.179811	7.409242	-0.079177	3.845770
409.259279	5064.192969	7.414246	-0.079286	3.848763
409.422315	5072.242536	7.419251	-0.079321	3.851759
409.650639	5080.291364	7.424256	-0.079369	3.854754
410.008757	5088.255881	7.429261	-0.079441	3.857717
410.254554	5096.282727	7.434266	-0.079492	3.860699
410.448304	5104.307031	7.439270	-0.079533	3.863677
410.905992	5112.311815	7.444275	-0.079624	3.866651
411.199570	5120.347354	7.449280	-0.079684	3.869630
411.588863	5128.469199	7.454285	-0.079762	3.872641
411.921373	5136.482342	7.459290	-0.079829	3.875608
412.161781	5144.446812	7.464294	-0.079879	3.878553
412.407362	5152.475584	7.469299	-0.079930	3.881520
412.984876	5160.369475	7.474304	-0.080043	3.884441
413.405153	5168.434221	7.479309	-0.080126	3.887420
413.625897	5176.440715	7.484314	-0.080173	3.890371
413.844908	5184.515484	7.489318	-0.080219	3.893344
414.118494	5192.522171	7.494323	-0.080275	3.896292
414.587176	5200.529604	7.499328	-0.080367	3.899241
414.831198	5208.584353	7.504333	-0.080418	3.902201
415.073243	5216.538094	7.509338	-0.080468	3.905122
415.506046	5224.586599	7.514342	-0.080554	3.908079
415.745742	5232.620112	7.519347	-0.080604	3.911024
416.030846	5240.629203	7.524352	-0.080663	3.913959
416.307102	5248.673958	7.529357	-0.080719	3.916905
416.826073	5256.654811	7.534362	-0.080821	3.919829
417.350369	5264.678377	7.539366	-0.080924	3.922767
417.694450	5272.701342	7.544371	-0.080993	3.925700
417.994405	5280.741331	7.549376	-0.081055	3.928635
418.405981	5288.791970	7.554381	-0.081137	3.931574
418.708461	5296.791793	7.559386	-0.081198	3.934490
419.146092	5304.875776	7.564390	-0.081285	3.937437
419.258717	5312.866626	7.569395	-0.081311	3.940342
419.699258	5320.852690	7.574400	-0.081398	3.943250
419.975049	5328.947941	7.579405	-0.081455	3.946191
420.403591	5336.889101	7.584410	-0.081540	3.949077
420.691007	5344.978769	7.589414	-0.081599	3.952013
421.065032	5352.994286	7.594419	-0.081674	3.954921
421.437603	5360.998671	7.599424	-0.081748	3.957822
421.600247	5369.040321	7.604429	-0.081784	3.960731
421.929756	5376.975012	7.609434	-0.081851	3.963603
422.776977	5385.064786	7.614438	-0.082014	3.966537
423.353607	5393.001912	7.619443	-0.082126	3.969409
423.577023	5401.053411	7.624448	-0.082173	3.972314
423.955610	5409.127600	7.629453	-0.082249	3.975228
424.335390	5417.078481	7.634458	-0.082325	3.978095
424.827886	5425.175737	7.639462	-0.082422	3.981015
424.986531	5433.102306	7.644467	-0.082457	3.983865
425.224493	5441.196971	7.649472	-0.082506	3.986775
425.562798	5449.208396	7.654477	-0.082575	3.989655
425.944905	5457.205371	7.659482	-0.082651	3.992528
426.470239	5465.179665	7.664486	-0.082754	3.995394
426.949581	5473.195249	7.669491	-0.082849	3.998271
427.359089	5481.260280	7.674496	-0.082930	4.001162
427.867663	5489.255021	7.679501	-0.083030	4.004028
428.213342	5497.285195	7.684506	-0.083100	4.006902
428.620599	5505.342048	7.689510	-0.083181	4.009784
428.955458	5513.342558	7.694515	-0.083248	4.012643
429.272112	5521.379561	7.699520	-0.083313	4.015513
429.850198	5529.379733	7.704525	-0.083426	4.018371
430.010251	5537.397981	7.709530	-0.083461	4.021227
430.411898	5545.425916	7.714534	-0.083541	4.024089
430.522000	5553.464195	7.719539	-0.083567	4.026947
430.990175	5561.474456	7.724544	-0.083659	4.029799
431.240037	5569.552355	7.729549	-0.083711	4.032669
431.475643	5577.556612	7.734554	-0.083760	4.035511
431.761023	5585.591720	7.739558	-0.083818	4.038363
431.926962	5593.590312	7.744563	-0.083855	4.041197
432.428244	5601.527687	7.749568	-0.083953	4.044014
432.983148	5609.593877	7.754573	-0.084062	4.046874
433.065571	5617.591270	7.759578	-0.084082	4.049701
433.407484	5625.627194	7.764582	-0.084151	4.052544
433.795607	5633.664248	7.769587	-0.084229	4.055386
434.206322	5641.638813	7.774592	-0.084311	4.058204
434.722160	5649.728924	7.779597	-0.084412	4.061062
434.906849	5657.669726	7.784602	-0.084451	4.063860
435.417819	5665.743305	7.789606	-0.084552	4.066709
435.543660	5673.760953	7.794611	-0.084581	4.069529
435.998769	5681.791638	7.799616	-0.084671	4.072358
436.413098	5689.826264	7.804621	-0.084753	4.075184
436.583768	5697.805641	7.809626	-0.084790	4.077986
436.889922	5705.878471	7.814630	-0.084852	4.080821
437.321724	5713.816341	7.819635	-0.084938	4.083609
437.397620	5721.927058	7.824640	-0.084958	4.086449
437.408097	5729.925637	7.829645	-0.084965	4.089248
438.007802	5737.931511	7.834650	-0.085082	4.092055
438.551920	5745.950769	7.839654	-0.085188	4.094865
438.818374	5753.944081	7.844659	-0.085243	4.097659
439.067376	5761.953518	7.849664	-0.085295	4.100457
439.458923	5769.985213	7.854669	-0.085373	4.103263
439.715753	5778.048572	7.859674	-0.085426	4.106076
440.193133	5786.033466	7.864678	-0.085520	4.108863
440.533181	5794.108407	7.869683	-0.085589	4.111677
441.027551	5802.029361	7.874688	-0.085686	4.114438
441.250481	5810.107591	7.879693	-0.085733	4.117248
441.764617	5818.055074	7.884698	-0.085834	4.120014
442.246552	5826.085876	7.889702	-0.085929	4.122807
442.546583	5834.081606	7.894707	-0.085990	4.125583
442.997054	5842.105026	7.899712	-0.086079	4.128369
443.504617	5850.223884	7.904717	-0.086179	4.131187
443.876255	5858.150585	7.909722	-0.086253	4.133935
444.288589	5866.246468	7.914726	-0.086336	4.136740
444.618691	5874.213736	7.919731	-0.086402	4.139497
445.094420	5882.236188	7.924736	-0.086496	4.142274
445.361572	5890.239400	7.929741	-0.086551	4.145039
445.748699	5898.261751	7.934746	-0.086628	4.147810
446.238830	5906.331162	7.939750	-0.086725	4.150597
446.579901	5914.308278	7.944755	-0.086794	4.153349
446.718001	5922.356295	7.949760	-0.086825	4.156120
447.116005	5930.324972	7.954765	-0.086904	4.158865
447.318920	5938.387892	7.959770	-0.086947	4.161639
447.666196	5946.388373	7.964774	-0.087017	4.164391
447.921383	5954.412134	7.969779	-0.087070	4.167148
448.281207	5962.435797	7.974784	-0.087142	4.169904
448.631813	5970.457961	7.979789	-0.087213	4.172658
448.905532	5978.486446	7.984794	-0.087269	4.175412
449.374281	5986.527247	7.989798	-0.087362	4.178170
449.451783	5994.567935	7.994803	-0.087381	4.180921
449.801732	6002.508655	7.999808	-0.087452	4.183640
450.191377	6010.574919	8.004813	-0.087529	4.186400
450.349842	6018.583189	8.009818	-0.087564	4.189136
450.568956	6026.673438	8.014822	-0.087610	4.191898
451.013134	6034.698350	8.019827	-0.087698	4.194639
451.410840	6042.677092	8.024832	-0.087778	4.197363
451.645023	6050.698725	8.029837	-0.087827	4.200096
451.792588	6058.662468	8.034842	-0.087859	4.202808
452.311348	6066.711069	8.039846	-0.087961	4.205551
452.616586	6074.701354	8.044851	-0.088023	4.208269
452.877238	6082.765520	8.049856	-0.088077	4.211011
453.285341	6090.767722	8.054861	-0.088158	4.213731
453.600702	6098.769958	8.059866	-0.088222	4.216448
453.892495	6106.814180	8.064870	-0.088282	4.219178
454.175468	6114.788411	8.069875	-0.088340	4.221882
454.575818	6122.760493	8.074880	-0.088420	4.224584
454.947435	6130.872620	8.079885	-0.088494	4.227332
455.143477	6138.878317	8.084890	-0.088536	4.230041
455.634925	6146.885653	8.089894	-0.088633	4.232751
455.929717	6154.956171	8.094899	-0.088693	4.235479
456.109302	6162.888355	8.099904	-0.088732	4.238157
456.773141	6170.923964	8.104909	-0.088860	4.240873
457.014778	6178.911910	8.109914	-0.088911	4.243567
457.481827	6186.989187	8.114918	-0.089003	4.246291
457.804044	6194.963860	8.119923	-0.089068	4.248978
458.322920	6203.039140	8.124928	-0.089170	4.251699
458.651712	6211.006441	8.129933	-0.089237	4.254380
458.878886	6219.039519	8.134938	-0.089284	4.257080
459.434249	6227.064584	8.139942	-0.089393	4.259779
459.761421	6235.060563	8.144947	-0.089459	4.262464
459.877855	6243.071465	8.149952	-0.089486	4.265151
460.444265	6251.113876	8.154957	-0.089597	4.267850
460.809947	6259.095439	8.159962	-0.089670	4.270526
460.978082	6267.154891	8.164966	-0.089707	4.273224
461.354772	6275.150213	8.169971	-0.089782	4.275901
461.827607	6283.146189	8.174976	-0.089875	4.278577
462.090522	6291.207355	8.179981	-0.089930	4.281271
462.295283	6299.132116	8.184986	-0.089973	4.283918
462.636045	6307.227688	8.189990	-0.090042	4.286621
463.064770	6315.236212	8.194995	-0.090127	4.289294
463.213617	6323.237660	8.200000	-0.090160	4.291960
463.697816	6331.265330	8.205005	-0.090255	4.294637
464.198022	6339.285590	8.210010	-0.090354	4.297309
464.709355	6347.330493	8.215014	-0.090454	4.299988
465.056359	6355.304029	8.220019	-0.090524	4.302640
465.359734	6363.317609	8.225024	-0.090586	4.305304
465.776356	6371.386112	8.230029	-0.090669	4.307985
465.938163	6379.397491	8.235034	-0.090704	4.310643
466.560032	6387.388253	8.240038	-0.090825	4.313296
466.921849	6395.396303	8.245043	-0.090898	4.315951
467.111675	6403.366496	8.250048	-0.090938	4.318591
467.455058	6411.461577	8.255053	-0.091008	4.321272
467.875815	6419.381413	8.260058	-0.091091	4.323893
468.441930	6427.448314	8.265062	-0.091202	4.326563
468.723632	6435.456270	8.270067	-0.091260	4.329209
468.867609	6443.501841	8.275072	-0.091292	4.331865
469.707933	6451.519058	8.280077	-0.091453	4.334515
469.751107	6459.517403	8.285082	-0.091467	4.337151
470.076881	6467.583350	8.290086	-0.091533	4.339810
470.488397	6475.553751	8.295091	-0.091615	4.342437
470.676723	6483.548444	8.300096	-0.091655	4.345068
471.184536	6491.580796	8.305101	-0.091755	4.347713
471.610334	6499.632434	8.310106	-0.091839	4.350361
471.895472	6507.706527	8.315110	-0.091898	4.353014
472.134053	6515.714355	8.320115	-0.091947	4.355643
472.741693	6523.668662	8.325120	-0.092066	4.358256
473.151246	6531.720865	8.330125	-0.092147	4.360898
473.336307	6539.630340	8.335130	-0.092187	4.363490
473.612590	6547.734442	8.340134	-0.092244	4.366145
473.991855	6555.667702	8.345139	-0.092320	4.368742
474.446677	6563.780044	8.350144	-0.092410	4.371398
474.758269	6571.751336	8.355149	-0.092473	4.374004
475.051426	6579.810140	8.360154	-0.092533	4.376638
475.310753	6587.803786	8.365158	-0.092586	4.379248
475.771636	6595.801179	8.370163	-0.092677	4.381859
476.121626	6603.820090	8.375168	-0.092748	4.384475
476.642458	6611.890463	8.380173	-0.092850	4.387107
476.924950	6619.852506	8.385178	-0.092908	4.389701
477.310058	6627.957562	8.390182	-0.092985	4.392340
477.674217	6635.924943	8.395187	-0.093058	4.394933
477.970636	6643.964762	8.400192	-0.093118	4.397548
478.307512	6652.002974	8.405197	-0.093186	4.400160
478.674628	6659.963765	8.410202	-0.093260	4.402746
478.947668	6668.021597	8.415206	-0.093316	4.405361
479.178891	6676.095681	8.420211	-0.093365	4.407980
479.610507	6684.071831	8.425216	-0.093450	4.410567
480.191701	6692.171752	8.430221	-0.093564	4.413192
480.351011	6700.147971	8.435226	-0.093599	4.415774
480.643407	6708.154654	8.440230	-0.093658	4.418365
481.237012	6716.196812	8.445235	-0.093774	4.420968
481.533454	6724.185118	8.450240	-0.093835	4.423550
481.868878	6732.263672	8.455245	-0.093902	4.426159
481.853240	6740.238654	8.460250	-0.093905	4.428732
482.350848	6748.312651	8.465254	-0.094003	4.431338
482.842510	6756.258933	8.470259	-0.094099	4.433901
483.311428	6764.311225	8.475264	-0.094192	4.436497
483.757634	6772.280486	8.480269	-0.094280	4.439064
484.059514	6780.316957	8.485274	-0.094342	4.441651
484.618813	6788.325194	8.490278	-0.094451	4.444228
484.898526	6796.332777	8.495283	-0.094509	4.446802
485.444023	6804.347028	8.500288	-0.094615	4.449378
485.604063	6812.429184	8.505293	-0.094651	4.451972
485.882809	6820.398547	8.510298	-0.094708	4.454530
486.283024	6828.439085	8.515302	-0.094787	4.457109
486.611781	6836.416232	8.520307	-0.094854	4.459666
486.928392	6844.420699	8.525312	-0.094918	4.462230
487.333203	6852.480433	8.530317	-0.094999	4.464810
487.541218	6860.478299	8.535322	-0.095043	4.467369
487.950652	6868.504565	8.540326	-0.095124	4.469936
488.311080	6876.490300	8.545331	-0.095197	4.472488
488.478335	6884.546810	8.550336	-0.095233	4.475061
488.792788	6892.568979	8.555341	-0.095297	4.477621
488.967375	6900.536885	8.560346	-0.095335	4.480163
489.457946	6908.555510	8.565351	-0.095431	4.482720
489.746492	6916.584287	8.570355	-0.095490	4.485278
490.085293	6924.566159	8.575360	-0.095559	4.487820
490.512671	6932.675360	8.580365	-0.095644	4.490401
490.854700	6940.633222	8.585370	-0.095712	4.492933
491.180455	6948.719732	8.590375	-0.095778	4.495503
491.289927	6956.683590	8.595379	-0.095804	4.498033
491.576146	6964.688438	8.600384	-0.095863	4.500574
491.926773	6972.659835	8.605389	-0.095933	4.503104
492.232646	6980.708239	8.610394	-0.095995	4.505657
492.639589	6988.727775	8.615399	-0.096076	4.508199
492.868923	6996.787324	8.620403	-0.096124	4.510752
493.206192	7004.728115	8.625408	-0.096192	4.513266
493.577968	7012.779771	8.630413	-0.096267	4.515814
493.961095	7020.717476	8.635418	-0.096344	4.518324
494.104996	7028.769714	8.640423	-0.096376	4.520868
494.317745	7036.762632	8.645427	-0.096421	4.523393
494.638014	7044.799723	8.650432	-0.096485	4.525930
495.021748	7052.803283	8.655437	-0.096562	4.528456
495.178590	7060.870858	8.660442	-0.096597	4.530999
495.568126	7068.878656	8.665447	-0.096674	4.533523
495.995641	7076.918543	8.670451	-0.096759	4.536055
496.156813	7084.886806	8.675456	-0.096795	4.538563
496.422771	7092.962006	8.680461	-0.096849	4.541104
496.735194	7100.875578	8.685466	-0.096913	4.543592
497.072297	7108.953480	8.690471	-0.096981	4.546130
497.369333	7116.996539	8.695475	-0.097041	4.548657
497.665306	7125.029274	8.700480	-0.097102	4.551178
497.822756	7133.012754	8.705485	-0.097136	4.553682
497.884884	7141.060102	8.710490	-0.097153	4.556205
498.355562	7148.968800	8.715495	-0.097246	4.558683
498.726927	7157.033211	8.720499	-0.097321	4.561209
498.866108	7164.996844	8.725504	-0.097352	4.563701
499.235202	7173.096374	8.730509	-0.097426	4.566235
499.554405	7181.063961	8.735514	-0.097490	4.568726
499.827411	7189.131241	8.740519	-0.097547	4.571247
500.012811	7197.108524	8.745523	-0.097586	4.573738
500.339197	7205.164592	8.750528	-0.097652	4.576252
500.584439	7213.155524	8.755533	-0.097703	4.578745
500.728013	7221.181434	8.760538	-0.097735	4.581247
501.121813	7229.138529	8.765543	-0.097814	4.583726
501.490982	7237.231585	8.770547	-0.097888	4.586247
501.529433	7245.202113	8.775552	-0.097900	4.588727
501.821841	7253.250315	8.780557	-0.097960	4.591231
502.199314	7261.201263	8.785562	-0.098036	4.593703
502.478851	7269.318812	8.790567	-0.098093	4.596225
502.814909	7277.201397	8.795571	-0.098161	4.598673
503.100046	7285.320920	8.800576	-0.098219	4.601193
503.404077	7293.266755	8.805581	-0.098281	4.603658
503.698239	7301.307663	8.810586	-0.098341	4.606151
504.329700	7309.297811	8.815591	-0.098464	4.608627
504.584315	7317.380075	8.820595	-0.098517	4.611130
504.697496	7325.331912	8.825600	-0.098543	4.613591
504.888973	7333.444390	8.830605	-0.098584	4.616100
505.235893	7341.367167	8.835610	-0.098654	4.618550
505.311194	7349.438198	8.840615	-0.098673	4.621044
505.501128	7357.407306	8.845619	-0.098714	4.623505
505.938096	7365.456368	8.850624	-0.098800	4.625989
506.429303	7373.487622	8.855629	-0.098897	4.628467
506.640352	7381.487095	8.860634	-0.098942	4.630933
506.931167	7389.526357	8.865639	-0.099001	4.633410
507.105964	7397.553850	8.870643	-0.099039	4.635883
507.614048	7405.479160	8.875648	-0.099139	4.638322
507.801696	7413.532642	8.880653	-0.099179	4.640800
508.140113	7421.459544	8.885658	-0.099247	4.643237
508.425648	7429.555341	8.890663	-0.099306	4.645725
508.659012	7437.526437	8.895667	-0.099354	4.648173
508.876739	7445.579132	8.900672	-0.099400	4.650645
509.243537	7453.660799	8.905677	-0.099474	4.653125
509.296315	7461.654863	8.910682	-0.099489	4.655576
509.709343	7469.627222	8.915687	-0.099571	4.658020
510.093804	7477.692579	8.920691	-0.099648	4.660490
510.143677	7485.648516	8.925696	-0.099662	4.662926
510.380690	7493.699860	8.930701	-0.099712	4.665389
510.542777	7501.735988	8.935706	-0.099747	4.667847
510.886174	7509.781984	8.940711	-0.099817	4.670306
511.087644	7517.823803	8.945715	-0.099859	4.672763
511.300076	7525.802473	8.950720	-0.099904	4.675199
511.612778	7533.830728	8.955725	-0.099968	4.677649
511.915710	7541.776266	8.960730	-0.100029	4.680072
512.105429	7549.792236	8.965735	-0.100070	4.682516
512.548698	7557.762161	8.970739	-0.100158	4.684944
512.771128	7565.773488	8.975744	-0.100204	4.687383
512.756654	7573.835313	8.980749	-0.100207	4.689837
513.054284	7581.813388	8.985754	-0.100268	4.692264
513.276093	7589.942244	8.990759	-0.100314	4.694735
513.600730	7597.899213	8.995763	-0.100380	4.697153
513.753317	7605.880144	9.000768	-0.100414	4.699577
514.464122	7613.955513	9.005773	-0.100551	4.702027
514.344980	7621.936343	9.010778	-0.100534	4.704449
514.745492	7630.011601	9.015783	-0.100614	4.706897
514.971946	7637.981036	9.020787	-0.100662	4.709313
515.155407	7646.018318	9.025792	-0.100701	4.711747
515.215821	7654.031248	9.030797	-0.100718	4.714173
515.660110	7662.039374	9.035802	-0.100806	4.716596
516.016867	7670.040912	9.040807	-0.100877	4.719015
516.311558	7678.080381	9.045811	-0.100937	4.721445
516.514319	7686.007734	9.050816	-0.100980	4.723840
516.936440	7694.151678	9.055821	-0.101064	4.726299
517.314145	7702.081416	9.060826	-0.101140	4.728691
517.570990	7710.215245	9.065831	-0.101193	4.731145
517.605955	7718.148727	9.070835	-0.101205	4.733537
518.075019	7726.189100	9.075840	-0.101297	4.735959
518.443535	7734.214315	9.080845	-0.101371	4.738375
518.753424	7742.238111	9.085850	-0.101434	4.740790
519.048742	7750.218265	9.090855	-0.101494	4.743191
519.363710	7758.318008	9.095859	-0.101558	4.745626
519.327366	7766.325460	9.100864	-0.101557	4.748033
519.904635	7774.334158	9.105869	-0.101670	4.750437
519.996893	7782.351019	9.110874	-0.101692	4.752845
520.133462	7790.372402	9.115879	-0.101723	4.755252
520.529257	7798.373322	9.120883	-0.101802	4.757651
520.863679	7806.348678	9.125888	-0.101869	4.760041
521.172380	7814.367523	9.130893	-0.101932	4.762443
521.381320	7822.325931	9.135898	-0.101976	4.764826
521.968799	7830.351786	9.140903	-0.102091	4.767227
522.061471	7838.429935	9.145907	-0.102113	4.769643
522.431670	7846.423314	9.150912	-0.102188	4.772033
522.994255	7854.465788	9.155917	-0.102298	4.774435
523.437568	7862.468354	9.160922	-0.102385	4.776824
523.576713	7870.442376	9.165927	-0.102417	4.779205
524.000207	7878.508467	9.170931	-0.102501	4.781610
524.236412	7886.461438	9.175936	-0.102550	4.783982
524.745631	7894.541115	9.180941	-0.102650	4.786389
524.861686	7902.555326	9.185946	-0.102677	4.788777
525.262051	7910.612740	9.190951	-0.102757	4.791175
525.376587	7918.507130	9.195955	-0.102783	4.793525
525.438940	7926.594749	9.200960	-0.102800	4.795931
525.881467	7934.582158	9.205965	-0.102888	4.798304
525.982230	7942.609148	9.210970	-0.102912	4.800690
526.173754	7950.558343	9.215975	-0.102953	4.803051
526.291082	7958.597818	9.220979	-0.102980	4.805438
526.793566	7966.610838	9.225984	-0.103079	4.807814
526.995142	7974.712276	9.230989	-0.103122	4.810216
527.200362	7982.670447	9.235994	-0.103165	4.812575
527.516920	7990.121017	9.240999	-0.103229	4.814781
527.803491	7994.716928	9.246003	-0.103285	4.816142

528.211702	7997.224263	9.251008	-0.103363	4.816882
528.511334	7998.642369	9.256013	-0.103420	4.817301
528.646725	7999.066066	9.261018	-0.103445	4.817426
528.696782	7999.888153	9.266023	-0.103455	4.817669
528.808406	7999.886612	9.271027	-0.103476	4.817668
529.201695	7999.875450	9.276032	-0.103549	4.817663
529.330910	7999.907906	9.281037	-0.103574	4.817672
529.468765	7999.837154	9.286042	-0.103599	4.817651
529.755415	7999.904582	9.291047	-0.103653	4.817670
529.784840	7999.899741	9.296051	-0.103658	4.817668
529.742245	7999.887527	9.301056	-0.103650	4.817665
529.878264	7999.922192	9.306061	-0.103676	4.817674
529.959143	7999.902281	9.311066	-0.103691	4.817668
530.166923	7999.943259	9.316071	-0.103730	4.817679
530.145244	7999.898662	9.321075	-0.103726	4.817666
530.299735	7999.925160	9.326080	-0.103754	4.817673
530.424671	7999.937521	9.331085	-0.103778	4.817676
530.499334	7999.912248	9.336090	-0.103792	4.817669
530.762161	7999.959299	9.341095	-0.103841	4.817681
530.959660	7999.898903	9.346099	-0.103877	4.817663
531.022483	7999.902982	9.351104	-0.103889	4.817664
531.022111	7999.908252	9.356109	-0.103889	4.817665
531.100826	7999.863002	9.361114	-0.103904	4.817651
531.368785	7999.911184	9.366119	-0.103954	4.817665
531.317603	7999.927316	9.371123	-0.103944	4.817670
531.476488	7999.895884	9.376128	-0.103974	4.817660
531.587607	7999.903828	9.381133	-0.103995	4.817661
531.524911	7999.871287	9.386138	-0.103983	4.817652
531.769165	7999.910690	9.391143	-0.104029	4.817663
532.010242	7999.884670	9.396147	-0.104073	4.817654
531.886273	7999.888145	9.401152	-0.104050	4.817655
532.008648	7999.943705	9.406157	-0.104073	4.817671
532.256923	7999.881937	9.411162	-0.104120	4.817652
532.192712	7999.923187	9.416167	-0.104108	4.817665
531.983384	7999.898006	9.421171	-0.104069	4.817658
532.303551	7999.895279	9.426176	-0.104128	4.817656
532.443746	7999.934227	9.431181	-0.104155	4.817667
532.198622	7999.896925	9.436186	-0.104109	4.817657
532.461861	7999.931334	9.441191	-0.104158	4.817666
532.364222	7999.911992	9.446195	-0.104140	4.817660
532.405612	7999.916815	9.451200	-0.104148	4.817662
532.499128	7999.939267	9.456205	-0.104165	4.817668
532.439622	7999.878300	9.461210	-0.104154	4.817650
532.546814	7999.930477	9.466215	-0.104174	4.817665
532.492284	7999.900162	9.471219	-0.104164	4.817656
532.591900	7999.931139	9.476224	-0.104183	4.817665
532.799782	7999.973180	9.481229	-0.104221	4.817677
532.801830	7999.945796	9.486234	-0.104222	4.817669
532.879645	7999.947985	9.491239	-0.104236	4.817669
532.711422	7999.960308	9.496243	-0.104205	4.817673
532.798045	7999.930989	9.501248	-0.104221	4.817664
532.761380	7999.946278	9.506253	-0.104214	4.817669
532.799549	7999.973199	9.511258	-0.104222	4.817677
532.817007	7999.989274	9.516263	-0.104225	4.817681
533.074969	7999.944519	9.521267	-0.104273	4.817667
533.174290	7999.924876	9.526272	-0.104291	4.817661
533.335453	7999.931440	9.531277	-0.104321	4.817662
533.257372	7999.908163	9.536282	-0.104307	4.817655
533.316361	7999.944878	9.541287	-0.104318	4.817666
533.338252	7999.936764	9.546291	-0.104322	4.817664
533.321529	7999.988196	9.551296	-0.104319	4.817679
533.200178	8000.037053	9.556301	-0.104297	4.817694
533.016869	7999.958466	9.561306	-0.104262	4.817671
533.309368	7999.956394	9.566311	-0.104317	4.817670
533.673182	7999.938487	9.571315	-0.104385	4.817663
533.163998	7999.970106	9.576320	-0.104290	4.817674
533.493971	7999.980179	9.581325	-0.104351	4.817676
533.551340	7999.880837	9.586330	-0.104362	4.817646
533.620288	7999.931405	9.591335	-0.104375	4.817661
533.684335	7999.944994	9.596339	-0.104387	4.817665
533.874916	7999.929842	9.601344	-0.104423	4.817659
533.932981	7999.915926	9.606349	-0.104433	4.817655
533.879845	7999.921484	9.611354	-0.104424	4.817657
533.905986	7999.941904	9.616359	-0.104429	4.817663
533.933795	7999.949694	9.621363	-0.104434	4.817665
534.005067	7999.934916	9.626368	-0.104447	4.817660
534.091515	7999.985740	9.631373	-0.104463	4.817675
533.821775	7999.930149	9.636378	-0.104413	4.817660
534.056227	7999.955707	9.641383	-0.104457	4.817666
534.202417	7999.973654	9.646387	-0.104484	4.817671
534.182056	7999.956489	9.651392	-0.104480	4.817666
534.196523	7999.958812	9.656397	-0.104483	4.817666
534.162662	7999.921414	9.661402	-0.104477	4.817655
534.236462	7999.947800	9.666407	-0.104491	4.817663
534.123264	7999.942994	9.671411	-0.104469	4.817662
534.109382	7999.945959	9.676416	-0.104467	4.817663
534.248788	7999.985954	9.681421	-0.104493	4.817674
533.968529	7999.941809	9.686426	-0.104441	4.817662
534.028953	7999.942692	9.691431	-0.104452	4.817662
534.224405	7999.972955	9.696435	-0.104489	4.817670
534.493917	7999.951569	9.701440	-0.104539	4.817663
534.453145	7999.942544	9.706445	-0.104531	4.817660
534.453461	7999.916188	9.711450	-0.104531	4.817653
534.478544	7999.969284	9.716455	-0.104536	4.817668
534.451037	8000.002633	9.721459	-0.104531	4.817678
534.645704	7999.972777	9.726464	-0.104567	4.817669
534.578507	8000.043513	9.731469	-0.104555	4.817690
534.465492	7999.956454	9.736474	-0.104534	4.817665
534.327804	7999.987146	9.741479	-0.104508	4.817674
534.679792	7999.964851	9.746483	-0.104574	4.817666
534.335848	7999.987270	9.751488	-0.104510	4.817674
534.430483	8000.019232	9.756493	-0.104528	4.817683
534.419218	7999.977945	9.761498	-0.104525	4.817671
534.523552	7999.978411	9.766503	-0.104545	4.817671
534.540780	7999.970229	9.771507	-0.104548	4.817668
534.596938	7999.977377	9.776512	-0.104559	4.817670
534.525528	7999.979505	9.781517	-0.104545	4.817671
534.804373	7999.941383	9.786522	-0.104597	4.817659
534.800339	7999.975073	9.791527	-0.104597	4.817669
534.840128	8000.003074	9.796531	-0.104604	4.817677
534.869289	7999.953938	9.801536	-0.104610	4.817662
534.874876	7999.963514	9.806541	-0.104611	4.817665
534.454112	8000.017507	9.811546	-0.104532	4.817683
534.662763	8000.034255	9.816551	-0.104571	4.817687
534.739124	7999.987914	9.821555	-0.104586	4.817673
534.636714	7999.969555	9.826560	-0.104567	4.817668
534.736743	8000.032178	9.831565	-0.104585	4.817686
534.569426	8000.055057	9.836570	-0.104554	4.817693
534.734531	8000.013171	9.841575	-0.104585	4.817680
534.641157	8000.093017	9.846579	-0.104568	4.817704
534.867862	7999.981372	9.851584	-0.104610	4.817670
534.936962	8000.003472	9.856589	-0.104623	4.817676
534.664646	7999.995296	9.861594	-0.104572	4.817675
534.887072	7999.983771	9.866599	-0.104614	4.817671
535.027607	8000.000583	9.871603	-0.104640	4.817675
534.724483	7999.977195	9.876608	-0.104583	4.817670
534.913704	8000.006315	9.881613	-0.104619	4.817677
535.049739	7999.991425	9.886618	-0.104644	4.817672
534.992425	7999.977940	9.891623	-0.104633	4.817669
534.878807	8000.048001	9.896627	-0.104612	4.817690
535.101814	7999.975320	9.901632	-0.104654	4.817667
535.401901	8000.020819	9.906637	-0.104710	4.817679
535.036019	7999.978589	9.911642	-0.104642	4.817669
535.233749	7999.986742	9.916647	-0.104679	4.817670
535.300802	8000.009867	9.921651	-0.104691	4.817677
535.260155	7999.950223	9.926656	-0.104684	4.817659
535.220733	7999.989727	9.931661	-0.104676	4.817671
535.050144	7999.974594	9.936666	-0.104645	4.817667
535.365436	8000.002385	9.941671	-0.104703	4.817674
535.000419	8000.042425	9.946675	-0.104635	4.817688
534.941052	8000.061601	9.951680	-0.104624	4.817694
535.279428	8000.021182	9.956685	-0.104687	4.817680
535.248078	7999.984874	9.961690	-0.104682	4.817670
535.291418	7999.986562	9.966695	-0.104690	4.817670
535.316585	8000.000642	9.971699	-0.104694	4.817674
535.253798	8000.023987	9.976704	-0.104683	4.817681
535.287819	8000.023431	9.981709	-0.104689	4.817681
535.333484	8000.049409	9.986714	-0.104698	4.817688
535.163955	8000.060655	9.991719	-0.104666	4.817692
535.198572	8000.009488	9.996723	-0.104673	4.817677
535.043303	8000.033597	10.001728	-0.104644	4.817685
535.132624	8000.071810	10.006733	-0.104661	4.817696
535.366336	7999.979248	10.011738	-0.104704	4.817667
535.465177	8000.007055	10.016743	-0.104723	4.817675
535.568870	7999.995912	10.021747	-0.104742	4.817671
535.464159	7999.976464	10.026752	-0.104722	4.817666
535.400949	8000.075733	10.031757	-0.104711	4.817696
535.529684	8000.020663	10.036762	-0.104735	4.817679
535.509576	8000.036193	10.041767	-0.104731	4.817684
535.357815	8000.030824	10.046771	-0.104703	4.817683
535.406940	8000.011505	10.051776	-0.104712	4.817677
535.438153	8000.079456	10.056781	-0.104718	4.817697
535.148779	8000.064703	10.061786	-0.104664	4.817694
535.186456	8000.037836	10.066791	-0.104671	4.817685
535.571326	8000.051877	10.071795	-0.104743	4.817688
535.578220	8000.017180	10.076800	-0.104744	4.817678
535.554047	8000.026323	10.081805	-0.104740	4.817680
535.743293	7999.958424	10.086810	-0.104775	4.817660
535.815470	7999.999552	10.091815	-0.104788	4.817671
535.743757	8000.013276	10.096819	-0.104775	4.817676
535.767626	7999.964061	10.101824	-0.104780	4.817661
536.026038	8000.015282	10.106829	-0.104828	4.817675
535.722385	7999.963410	10.111834	-0.104771	4.817661
535.793278	7999.997138	10.116839	-0.104785	4.817671
535.771057	7999.987327	10.121843	-0.104780	4.817668
535.841599	7999.956719	10.126848	-0.104794	4.817659
535.768313	8000.015768	10.131853	-0.104780	4.817676
535.640477	8000.001256	10.136858	-0.104756	4.817673
535.800472	7999.997260	10.141863	-0.104786	4.817671
535.814505	8000.018560	10.146867	-0.104789	4.817677
535.849096	7999.960010	10.151872	-0.104795	4.817660
536.080364	7999.997127	10.156877	-0.104838	4.817670
535.629841	7999.990573	10.161882	-0.104755	4.817670
535.787072	8000.027666	10.166887	-0.104784	4.817680
536.080347	8000.043539	10.171891	-0.104839	4.817683
536.020959	8000.008932	10.176896	-0.104828	4.817673
535.991904	8000.065460	10.181901	-0.104822	4.817690
535.915576	7999.990531	10.186906	-0.104808	4.817668
535.923166	8000.011737	10.191911	-0.104809	4.817675
535.873292	7999.998360	10.196915	-0.104800	4.817671
535.974984	8000.005117	10.201920	-0.104819	4.817672
536.137589	8000.048616	10.206925	-0.104850	4.817684
536.011780	7999.994059	10.211930	-0.104826	4.817669
536.081313	7999.997184	10.216935	-0.104839	4.817670
536.160723	8000.007835	10.221939	-0.104854	4.817672
536.115859	7999.970275	10.226944	-0.104846	4.817661
536.224028	8000.027746	10.231949	-0.104866	4.817678
536.136054	8000.046507	10.236954	-0.104850	4.817684
536.070983	8000.033962	10.241959	-0.104837	4.817680
535.900656	8000.108472	10.246963	-0.104806	4.817703
536.185700	8000.020875	10.251968	-0.104859	4.817676
536.463787	8000.034419	10.256973	-0.104911	4.817679
536.079521	8000.035156	10.261978	-0.104839	4.817681
536.032013	8000.019703	10.266983	-0.104830	4.817676
536.185214	7999.995572	10.271987	-0.104859	4.817669
536.159051	7999.959339	10.276992	-0.104854	4.817658
536.199530	8000.074883	10.281997	-0.104862	4.817692
535.960840	7999.995481	10.287002	-0.104817	4.817670
536.171982	7999.989067	10.292007	-0.104857	4.817667
536.457101	7999.970019	10.297011	-0.104910	4.817660
535.939304	8000.022598	10.302016	-0.104814	4.817678
536.081083	8000.013064	10.307021	-0.104840	4.817674
536.390307	7999.933202	10.312026	-0.104898	4.817649
536.379433	7999.989995	10.317031	-0.104896	4.817666
536.199139	7999.963119	10.322035	-0.104862	4.817659
536.388430	7999.957441	10.327040	-0.104897	4.817656
536.391001	7999.990175	10.332045	-0.104898	4.817666
536.245331	7999.951147	10.337050	-0.104871	4.817655
536.331300	8000.004077	10.342055	-0.104887	4.817670
536.428598	8000.008661	10.347059	-0.104905	4.817671
536.137226	8000.010750	10.352064	-0.104851	4.817673
536.358559	8000.011867	10.357069	-0.104892	4.817673
536.126083	8000.013759	10.362074	-0.104849	4.817674
536.169694	7999.982760	10.367079	-0.104857	4.817665
536.285904	8000.018202	10.372083	-0.104879	4.817675
536.223936	8000.032068	10.377088	-0.104867	4.817679
536.355209	8000.045583	10.382093	-0.104892	4.817683
536.340606	8000.000027	10.387098	-0.104889	4.817669
536.338730	8000.001058	10.392103	-0.104889	4.817670
536.225571	8000.044762	10.397107	-0.104868	4.817683
536.206781	8000.012854	10.402112	-0.104864	4.817674
536.404281	8000.071627	10.407117	-0.104901	4.817690
536.546691	8000.001990	10.412122	-0.104928	4.817669
536.314343	8000.041850	10.417127	-0.104884	4.817682
536.095606	8000.085072	10.422131	-0.104844	4.817695
536.385826	8000.000714	10.427136	-0.104898	4.817669
536.639909	8000.001253	10.432141	-0.104945	4.817668
536.437362	7999.955069	10.437146	-0.104907	4.817655
536.213139	7999.993992	10.442151	-0.104866	4.817668
536.533474	8000.002878	10.447155	-0.104925	4.817669
536.542853	7999.961889	10.452160	-0.104927	4.817657
536.357024	8000.004535	10.457165	-0.104893	4.817670
536.425264	7999.972839	10.462170	-0.104905	4.817661
536.262284	7999.969416	10.467175	-0.104875	4.817660
536.572597	7999.967609	10.472179	-0.104933	4.817659
536.568611	7999.987592	10.477184	-0.104932	4.817665
536.617935	8000.000969	10.482189	-0.104942	4.817668
536.482098	7999.982121	10.487194	-0.104916	4.817663
536.851454	7999.967465	10.492199	-0.104985	4.817657
536.895609	8000.020842	10.497203	-0.104993	4.817673
536.532150	8000.005008	10.502208	-0.104926	4.817670
536.652126	7999.997267	10.507213	-0.104948	4.817667
536.712189	7999.966506	10.512218	-0.104959	4.817658
536.862087	7999.958146	10.517223	-0.104987	4.817655
536.904141	7999.997783	10.522227	-0.104995	4.817666
536.815697	7999.956424	10.527232	-0.104979	4.817654
536.826371	7999.994549	10.532237	-0.104981	4.817665
536.671313	7999.988076	10.537242	-0.104952	4.817664
536.843567	7999.969496	10.542247	-0.104984	4.817658
536.884451	7999.969040	10.547251	-0.104992	4.817658
536.813221	7999.979607	10.552256	-0.104979	4.817661
536.735304	8000.014333	10.557261	-0.104964	4.817672
536.866486	8000.008864	10.562266	-0.104989	4.817670
536.749005	7999.999775	10.567271	-0.104967	4.817667
536.732843	7999.980560	10.572275	-0.104964	4.817662
536.707286	7999.996011	10.577280	-0.104959	4.817666
536.775821	8000.029706	10.582285	-0.104972	4.817676
536.688613	8000.084334	10.587290	-0.104956	4.817693
536.640196	8000.028793	10.592295	-0.104947	4.817676
536.582039	8000.061697	10.597299	-0.104936	4.817686
536.532689	8000.033562	10.602304	-0.104927	4.817678
536.823979	8000.032534	10.607309	-0.104981	4.817677
536.706664	8000.021338	10.612314	-0.104959	4.817674
536.801828	8000.021673	10.617319	-0.104977	4.817674
537.005596	7999.966640	10.622323	-0.105015	4.817656
536.836673	7999.969457	10.627328	-0.104984	4.817658
536.958265	8000.009197	10.632333	-0.105006	4.817669
536.991491	7999.981210	10.637338	-0.105012	4.817661
536.938886	7999.984666	10.642343	-0.105003	4.817662
537.104476	7999.983917	10.647347	-0.105034	4.817661
536.841459	7999.953725	10.652352	-0.104985	4.817653
536.633386	8000.019249	10.657357	-0.104946	4.817674
536.901628	7999.971482	10.662362	-0.104996	4.817658
537.073395	8000.017227	10.667367	-0.105028	4.817671
536.801998	8000.045971	10.672371	-0.104978	4.817681
536.384506	8000.033568	10.677376	-0.104900	4.817679
536.900697	8000.028432	10.682381	-0.104996	4.817675
536.632907	8000.044574	10.687386	-0.104946	4.817681
536.796208	7999.994225	10.692391	-0.104977	4.817665
537.043098	8000.058992	10.697395	-0.105023	4.817684
536.757420	8000.021087	10.702400	-0.104970	4.817674
536.827843	7999.994697	10.707405	-0.104983	4.817665
536.859141	7999.963518	10.712410	-0.104989	4.817656
537.000647	8000.002493	10.717415	-0.105015	4.817667
536.887070	8000.000843	10.722419	-0.104994	4.817667
536.930038	7999.974052	10.727424	-0.105002	4.817659
537.083082	8000.024797	10.732429	-0.105030	4.817673
537.051315	8000.018010	10.737434	-0.105025	4.817671
537.323121	7999.999825	10.742439	-0.105075	4.817665
537.307257	7999.955304	10.747443	-0.105072	4.817652
537.192759	7999.947312	10.752448	-0.105051	4.817650
537.299135	7999.993159	10.757453	-0.105071	4.817663
537.215415	7999.979288	10.762458	-0.105055	4.817659
537.252989	8000.011477	10.767463	-0.105062	4.817669
537.058729	7999.992833	10.772467	-0.105026	4.817664
537.012750	7999.959474	10.777472	-0.105018	4.817654
537.311226	8000.046085	10.782477	-0.105073	4.817679
537.222220	8000.000498	10.787482	-0.105057	4.817665
537.010851	8000.004805	10.792487	-0.105018	4.817668
537.321429	7999.987185	10.797491	-0.105075	4.817661
537.237263	7999.965925	10.802496	-0.105060	4.817655
537.249771	8000.004077	10.807501	-0.105062	4.817666
537.147924	7999.944594	10.812506	-0.105043	4.817649
537.342800	7999.989620	10.817511	-0.105080	4.817662
537.231251	8000.052331	10.822515	-0.105059	4.817681
537.290305	7999.965661	10.827520	-0.105070	4.817655
537.403756	7999.981027	10.832525	-0.105091	4.817659
537.301941	7999.957401	10.837530	-0.105072	4.817652
537.311331	7999.988125	10.842535	-0.105074	4.817661
537.283916	7999.980347	10.847539	-0.105069	4.817659
537.500772	7999.958198	10.852544	-0.105109	4.817652
537.367756	8000.001613	10.857549	-0.105085	4.817665
537.327903	7999.954633	10.862554	-0.105077	4.817651
537.473673	7999.972579	10.867559	-0.105104	4.817656
537.336902	7999.995902	10.872563	-0.105079	4.817664
537.202072	7999.973904	10.877568	-0.105054	4.817658
537.173994	8000.035721	10.882573	-0.105049	4.817676
537.281951	7999.974020	10.887578	-0.105069	4.817657
537.272564	7999.980214	10.892583	-0.105067	4.817659
537.267738	7999.970656	10.897587	-0.105066	4.817656
537.122855	7999.946403	10.902592	-0.105039	4.817650
536.733536	8000.088383	10.907597	-0.104967	4.817694
536.423369	8000.146092	10.912602	-0.104909	4.817712
536.797886	8000.034488	10.917607	-0.104979	4.817677
537.249657	7999.991503	10.922611	-0.105063	4.817663
537.153145	7999.979555	10.927616	-0.105045	4.817660
537.197610	8000.033992	10.932621	-0.105054	4.817675
536.624575	8000.089982	10.937626	-0.104947	4.817694
536.453945	8000.086446	10.942631	-0.104915	4.817694
537.030006	8000.042108	10.947635	-0.105023	4.817679
537.066952	8000.028940	10.952640	-0.105029	4.817675
537.163629	8000.031406	10.957645	-0.105048	4.817675
537.098897	7999.996719	10.962650	-0.105036	4.817665
537.278799	8000.008834	10.967655	-0.105069	4.817668
537.320519	8000.038975	10.972659	-0.105077	4.817676
537.067868	7999.981513	10.977664	-0.105030	4.817660
536.966540	8000.058083	10.982669	-0.105011	4.817684
537.463193	7999.991496	10.987674	-0.105104	4.817662
537.287481	7999.987886	10.992679	-0.105071	4.817661
537.164306	8000.018789	10.997683	-0.105048	4.817671
537.340581	8000.019251	11.002688	-0.105081	4.817670
537.477218	7999.996988	11.007693	-0.105106	4.817663
537.431622	7999.974181	11.012698	-0.105098	4.817657
537.480610	7999.993881	11.017703	-0.105107	4.817662
537.577251	7999.961544	11.022707	-0.105125	4.817652
537.283442	7999.941449	11.027712	-0.105070	4.817648
537.448173	7999.976545	11.032717	-0.105101	4.817657
537.134370	7999.995181	11.037722	-0.105043	4.817664
537.311778	7999.986167	11.042727	-0.105076	4.817661
537.293727	7999.982744	11.047731	-0.105073	4.817660
537.234658	7999.976614	11.052736	-0.105062	4.817658
537.555227	8000.008707	11.057741	-0.105121	4.817666
537.547836	7999.953762	11.062746	-0.105120	4.817650
537.433973	8000.003784	11.067751	-0.105099	4.817665
537.670657	7999.975597	11.072755	-0.105143	4.817656
537.580015	7999.993263	11.077760	-0.105126	4.817662
537.461781	8000.034784	11.082765	-0.105104	4.817675
537.758736	8000.002202	11.087770	-0.105160	4.817664
537.849945	8000.009862	11.092775	-0.105177	4.817665
537.627329	8000.008732	11.097779	-0.105135	4.817666
537.542528	8000.004336	11.102784	-0.105119	4.817665
537.704652	8000.005647	11.107789	-0.105150	4.817665
537.714684	7999.987868	11.112794	-0.105152	4.817660
537.522982	8000.031483	11.117799	-0.105116	4.817673
537.770214	8000.043525	11.122803	-0.105162	4.817676
537.720488	7999.987963	11.127808	-0.105153	4.817660
537.537922	8000.026438	11.132813	-0.105119	4.817672
537.625609	7999.947567	11.137818	-0.105135	4.817648
537.860114	7999.987899	11.142823	-0.105179	4.817659
537.888596	7999.983044	11.147827	-0.105184	4.817657
537.844571	7999.960259	11.152832	-0.105176	4.817651
537.980289	7999.975950	11.157837	-0.105201	4.817655
537.850604	7999.936098	11.162842	-0.105177	4.817644
537.886828	7999.994634	11.167847	-0.105184	4.817661
537.789998	7999.983735	11.172851	-0.105166	4.817658
537.705075	7999.999376	11.177856	-0.105150	4.817663
537.601192	8000.012631	11.182861	-0.105131	4.817667
537.682636	7999.995892	11.187866	-0.105146	4.817662
537.687002	7999.994905	11.192871	-0.105147	4.817662
537.379297	8000.037885	11.197875	-0.105090	4.817676
537.291626	8000.045048	11.202880	-0.105074	4.817678
537.818371	8000.048507	11.207885	-0.105172	4.817677
537.572623	8000.039657	11.212890	-0.105126	4.817675
537.660196	7999.993478	11.217895	-0.105142	4.817661
537.777599	8000.017339	11.222899	-0.105164	4.817668
537.982515	7999.963377	11.227904	-0.105202	4.817651
537.988179	8000.010922	11.232909	-0.105204	4.817665
537.973089	7999.969575	11.237914	-0.105201	4.817653
537.892664	7999.972626	11.242919	-0.105186	4.817654
537.960918	7999.996826	11.247923	-0.105199	4.817661
537.706525	8000.002615	11.252928	-0.105151	4.817664
537.832912	8000.064574	11.257933	-0.105175	4.817682
537.838776	8000.009822	11.262938	-0.105176	4.817665
537.793892	8000.008117	11.267943	-0.105168	4.817665
537.983674	8000.026705	11.272947	-0.105203	4.817670
537.826694	7999.985400	11.277952	-0.105174	4.817658
538.092125	7999.992435	11.282957	-0.105223	4.817659
537.786008	7999.985869	11.287962	-0.105166	4.817659
537.718065	8000.030233	11.292967	-0.105154	4.817672
537.921711	8000.024766	11.297971	-0.105192	4.817670
537.798163	7999.982893	11.302976	-0.105169	4.817658
537.917821	8000.051083	11.307981	-0.105191	4.817677
537.551869	8000.014116	11.312986	-0.105123	4.817668
537.596400	8000.034806	11.317991	-0.105131	4.817674
537.874082	8000.029363	11.322995	-0.105183	4.817671
537.676732	8000.040202	11.328000	-0.105147	4.817675
537.540163	8000.050872	11.333005	-0.105121	4.817679
537.832187	7999.989742	11.338010	-0.105176	4.817660
538.153099	7999.998640	11.343015	-0.105235	4.817661
537.992784	8000.012127	11.348019	-0.105206	4.817665
537.869001	7999.977634	11.353024	-0.105182	4.817656
538.129189	8000.015177	11.358029	-0.105231	4.817666
538.046550	7999.991829	11.363034	-0.105216	4.817659
537.812936	8000.004248	11.368039	-0.105172	4.817664
538.091056	7999.978774	11.373043	-0.105224	4.817655
538.151831	7999.969117	11.378048	-0.105235	4.817652
538.148879	8000.008099	11.383053	-0.105235	4.817664
538.015020	7999.977677	11.388058	-0.105210	4.817655
538.111020	7999.979079	11.393063	-0.105228	4.817655
538.099459	8000.067505	11.398067	-0.105226	4.817681
538.036124	7999.992760	11.403072	-0.105214	4.817660
538.019832	7999.995691	11.408077	-0.105211	4.817660
537.984697	7999.993073	11.413082	-0.105205	4.817660
537.960094	8000.005374	11.418087	-0.105200	4.817664
538.141840	8000.014353	11.423091	-0.105234	4.817665
538.055368	7999.978294	11.428096	-0.105218	4.817655
538.076859	8000.039780	11.433101	-0.105222	4.817673
538.075988	8000.008132	11.438106	-0.105222	4.817664
538.210277	7999.967906	11.443111	-0.105247	4.817651
538.142922	8000.009114	11.448115	-0.105234	4.817664
538.128487	7999.960394	11.453120	-0.105232	4.817650
538.229980	8000.024100	11.458125	-0.105251	4.817668
538.136532	7999.975283	11.463130	-0.105233	4.817654
537.978675	7999.989861	11.468135	-0.105204	4.817659
538.097707	8000.027457	11.473139	-0.105226	4.817670
538.216182	7999.984892	11.478144	-0.105248	4.817656
538.293226	7999.997619	11.483149	-0.105263	4.817660
538.056945	7999.963595	11.488154	-0.105219	4.817651
538.147003	8000.000769	11.493159	-0.105236	4.817661
538.161631	8000.076920	11.498163	-0.105238	4.817684
538.045125	8000.014057	11.503168	-0.105217	4.817666
538.130183	8000.042721	11.508173	-0.105233	4.817674
538.327637	7999.994978	11.513178	-0.105269	4.817659
538.125249	7999.993088	11.518183	-0.105232	4.817659
538.050451	7999.989892	11.523187	-0.105218	4.817659
538.180435	7999.967533	11.528192	-0.105242	4.817651
538.125223	7999.997317	11.533197	-0.105232	4.817660
537.854615	8000.010252	11.538202	-0.105182	4.817665
537.957552	7999.990662	11.543207	-0.105201	4.817659
537.955282	7999.984305	11.548211	-0.105200	4.817657
538.041022	7999.952864	11.553216	-0.105216	4.817648
537.981777	8000.012119	11.558221	-0.105205	4.817665
537.857714	8000.012424	11.563226	-0.105182	4.817666
537.810783	8000.011744	11.568231	-0.105174	4.817666
537.862820	8000.013561	11.573235	-0.105183	4.817666
537.948219	8000.049612	11.578240	-0.105199	4.817677
538.187410	8000.023570	11.583245	-0.105244	4.817668
537.931713	7999.982936	11.588250	-0.105196	4.817657
537.775793	8000.042892	11.593255	-0.105167	4.817675
537.991794	8000.040769	11.598259	-0.105208	4.817674
538.104713	7999.968593	11.603264	-0.105229	4.817652
538.123535	8000.028986	11.608269	-0.105232	4.817670
538.091950	8000.089699	11.613274	-0.105226	4.817688
538.036950	8000.074136	11.618279	-0.105216	4.817684
537.997732	8000.085169	11.623283	-0.105209	4.817687
537.893023	8000.035133	11.628288	-0.105190	4.817673
537.910221	8000.020622	11.633293	-0.105193	4.817668
537.791428	8000.042097	11.638298	-0.105171	4.817675
537.910150	8000.018519	11.643303	-0.105193	4.817668
538.114403	8000.004625	11.648307	-0.105231	4.817663
538.102326	7999.970704	11.653312	-0.105229	4.817653
538.234720	8000.023259	11.658317	-0.105253	4.817668
538.320810	7999.966512	11.663322	-0.105269	4.817650
538.148405	8000.006189	11.668327	-0.105237	4.817663
537.907495	8000.067016	11.673331	-0.105193	4.817682
538.024322	8000.015990	11.678336	-0.105214	4.817666
538.024210	8000.037084	11.683341	-0.105214	4.817673
537.990906	7999.990199	11.688346	-0.105208	4.817659
538.117545	8000.009976	11.693351	-0.105232	4.817664
538.021162	8000.021231	11.698355	-0.105214	4.817668
538.080446	7999.973585	11.703360	-0.105225	4.817654
538.286629	8000.021943	11.708365	-0.105264	4.817667
538.081049	8000.033716	11.713370	-0.105225	4.817671
537.901685	8000.055363	11.718375	-0.105192	4.817679
538.209620	8000.014503	11.723379	-0.105249	4.817665
537.910253	7999.980615	11.728384	-0.105194	4.817656
538.230269	8000.035905	11.733389	-0.105253	4.817671
537.957809	8000.054086	11.738394	-0.105203	4.817678
537.925737	8000.029365	11.743399	-0.105197	4.817671
538.113955	8000.045822	11.748403	-0.105232	4.817675
537.901776	7999.966800	11.753408	-0.105192	4.817652
538.055657	7999.988029	11.758413	-0.105221	4.817658
538.080031	8000.004207	11.763418	-0.105226	4.817663
538.145747	8000.019933	11.768423	-0.105238	4.817667
538.157632	8000.026438	11.773427	-0.105240	4.817669
538.171248	8000.002383	11.778432	-0.105243	4.817662
538.083700	8000.064390	11.783437	-0.105227	4.817680
538.204244	8000.029237	11.788442	-0.105249	4.817670
538.168427	8000.026610	11.793447	-0.105242	4.817669
538.245752	8000.034068	11.798451	-0.105257	4.817671
538.257209	7999.998380	11.803456	-0.105259	4.817660
538.241142	8000.011860	11.808461	-0.105256	4.817664
538.287581	8000.026251	11.813466	-0.105265	4.817668
538.151465	8000.056965	11.818471	-0.105239	4.817678
538.137524	8000.062039	11.823475	-0.105237	4.817679
537.848251	8000.063101	11.828480	-0.105183	4.817681
538.129316	8000.109386	11.833485	-0.105235	4.817694
538.332805	8000.029038	11.838490	-0.105273	4.817669
538.040674	8000.038495	11.843495	-0.105219	4.817673
538.431484	8000.047357	11.848499	-0.105292	4.817674
538.369088	8000.033796	11.853504	-0.105280	4.817670
538.298205	8000.034876	11.858509	-0.105267	4.817671
538.214139	8000.060021	11.863514	-0.105252	4.817679
538.092449	8000.056142	11.868519	-0.105229	4.817678
538.033000	8000.083755	11.873523	-0.105218	4.817686
538.035168	8000.066915	11.878528	-0.105218	4.817681
538.422511	8000.048307	11.883533	-0.105291	4.817674
538.146701	8000.140264	11.888538	-0.105239	4.817703
537.902585	8000.069213	11.893543	-0.105194	4.817683
538.065950	8000.180226	11.898547	-0.105224	4.817715
537.721411	8000.118258	11.903552	-0.105160	4.817698
537.792564	8000.122462	11.908557	-0.105173	4.817699
538.020671	8000.119462	11.913562	-0.105216	4.817697
537.965576	8000.085969	11.918567	-0.105206	4.817687
538.123513	8000.100929	11.923571	-0.105235	4.817691
537.817684	8000.086985	11.928576	-0.105178	4.817688
538.072629	8000.110742	11.933581	-0.105226	4.817694
538.157058	8000.064516	11.938586	-0.105242	4.817680
538.010370	8000.017033	11.943591	-0.105214	4.817667
538.220227	8000.138215	11.948595	-0.105254	4.817702
537.938562	8000.106693	11.953600	-0.105201	4.817694
538.227050	8000.052895	11.958605	-0.105255	4.817676
537.908450	8000.079896	11.963610	-0.105196	4.817686
538.037190	8000.038535	11.968615	-0.105220	4.817673
537.994311	8000.107520	11.973619	-0.105212	4.817694
537.942223	8000.038213	11.978624	-0.105202	4.817673
538.227279	8000.051862	11.983629	-0.105255	4.817676
538.268041	8000.071443	11.988634	-0.105263	4.817682
538.174271	8000.099610	11.993639	-0.105245	4.817690
538.144850	8000.081256	11.998643	-0.105240	4.817685
538.350169	8000.001989	12.003648	-0.105278	4.817661
538.325702	8000.050150	12.008653	-0.105274	4.817675
538.200701	8000.078917	12.013658	-0.105250	4.817684
538.367551	8000.062368	12.018663	-0.105282	4.817679
538.413934	8000.063048	12.023667	-0.105290	4.817679
538.385340	7999.987755	12.028672	-0.105285	4.817656
538.288480	8000.045407	12.033677	-0.105267	4.817674
538.515936	8000.048726	12.038682	-0.105309	4.817674
538.420503	8000.057885	12.043687	-0.105292	4.817677
538.524174	8000.053072	12.048691	-0.105311	4.817675
538.427219	7999.988383	12.053696	-0.105293	4.817656
538.676619	8000.054246	12.058701	-0.105339	4.817675
538.648452	8000.036965	12.063706	-0.105334	4.817670
538.537311	8000.027966	12.068711	-0.105314	4.817668
538.671949	8000.067899	12.073715	-0.105339	4.817679
538.399370	8000.015416	12.078720	-0.105288	4.817665
538.589172	8000.073028	12.083725	-0.105323	4.817681
538.335182	8000.053510	12.088730	-0.105276	4.817676
538.430589	8000.029592	12.093735	-0.105294	4.817669
538.270988	8000.108479	12.098739	-0.105264	4.817693
538.085008	8000.119482	12.103744	-0.105230	4.817697
538.293776	8000.087725	12.108749	-0.105269	4.817686
538.377878	8000.090009	12.113754	-0.105284	4.817687
538.501477	8000.065447	12.118759	-0.105307	4.817679
538.524343	8000.093205	12.123763	-0.105312	4.817687
538.447387	8000.033027	12.128768	-0.105297	4.817670
538.280574	8000.091769	12.133773	-0.105266	4.817688
538.521641	8000.098450	12.138778	-0.105311	4.817689
538.630948	8000.010401	12.143783	-0.105332	4.817662
538.438375	8000.063495	12.148787	-0.105296	4.817679
538.061513	8000.164526	12.153792	-0.105226	4.817710
538.350629	8000.170853	12.158797	-0.105280	4.817711
538.045482	8000.096802	12.163802	-0.105223	4.817690
538.298899	8000.018236	12.168807	-0.105270	4.817666
538.396330	8000.149382	12.173811	-0.105288	4.817704
538.286006	7999.996962	12.178816	-0.105268	4.817660
538.500748	8000.054937	12.183821	-0.105308	4.817676
538.514231	8000.068848	12.188826	-0.105310	4.817680
538.561562	8000.023136	12.193831	-0.105319	4.817666
538.470292	8000.130440	12.198835	-0.105302	4.817698
538.575635	8000.037059	12.203840	-0.105322	4.817670
538.682816	8000.107178	12.208845	-0.105342	4.817690
538.191777	8000.074713	12.213850	-0.105251	4.817683
538.426322	8000.013801	12.218855	-0.105294	4.817664
538.460358	8000.098673	12.223859	-0.105301	4.817689
538.414827	8000.027351	12.228864	-0.105292	4.817668
538.315511	8000.068094	12.233869	-0.105274	4.817680
538.290675	8000.146835	12.238874	-0.105269	4.817704
538.520489	8000.075307	12.243879	-0.105312	4.817682
538.376808	8000.141769	12.248883	-0.105285	4.817702
538.283610	8000.021239	12.253888	-0.105268	4.817667
538.423455	8000.070740	12.258893	-0.105294	4.817681
538.465517	8000.048154	12.263898	-0.105302	4.817674
538.092404	8000.065922	12.268903	-0.105233	4.817681
538.546125	8000.109451	12.273907	-0.105317	4.817692
538.311697	8000.084945	12.278912	-0.105274	4.817685
538.465289	8000.084023	12.283917	-0.105302	4.817684
538.527293	8000.097587	12.288922	-0.105314	4.817688
538.553134	8000.053671	12.293927	-0.105319	4.817675
538.577996	8000.095169	12.298931	-0.105323	4.817687
538.332967	8000.105312	12.303936	-0.105278	4.817691
538.630794	8000.078016	12.308941	-0.105333	4.817682
538.652981	8000.135295	12.313946	-0.105337	4.817699
538.556725	8000.065343	12.318951	-0.105320	4.817679
538.657513	8000.120603	12.323955	-0.105338	4.817694
538.545672	8000.102102	12.328960	-0.105318	4.817689
538.375457	8000.084860	12.333965	-0.105286	4.817685
538.259930	8000.071578	12.338970	-0.105264	4.817682
538.433721	8000.018218	12.343975	-0.105297	4.817665
538.652062	8000.065699	12.348979	-0.105338	4.817678
538.544869	8000.036719	12.353984	-0.105318	4.817670
538.788372	8000.036054	12.358989	-0.105363	4.817669
538.781487	8000.015918	12.363994	-0.105362	4.817663
538.453348	8000.043834	12.368999	-0.105301	4.817673
538.696359	8000.079019	12.374003	-0.105346	4.817682
538.831561	8000.017714	12.379008	-0.105371	4.817663
538.838722	8000.011494	12.384013	-0.105373	4.817661
538.752179	8000.055586	12.389018	-0.105357	4.817675
539.044684	8000.007120	12.394023	-0.105411	4.817659
538.963089	8000.059723	12.399027	-0.105396	4.817675
538.791820	7999.999223	12.404032	-0.105364	4.817658
538.676889	8000.085089	12.409037	-0.105343	4.817684
538.698584	8000.043222	12.414042	-0.105347	4.817671
538.452348	8000.009052	12.419047	-0.105301	4.817662
538.863943	8000.082553	12.424051	-0.105378	4.817682
538.854446	8000.000154	12.429056	-0.105376	4.817658
538.746739	8000.013353	12.434061	-0.105356	4.817662
538.948713	8000.021574	12.439066	-0.105394	4.817664
538.898175	8000.048262	12.444071	-0.105384	4.817672
539.001582	8000.074031	12.449075	-0.105404	4.817679
538.688348	8000.019899	12.454080	-0.105345	4.817665
538.750097	8000.031349	12.459085	-0.105357	4.817668
538.857099	8000.093029	12.464090	-0.105377	4.817685
538.752481	8000.091507	12.469095	-0.105357	4.817685
538.778934	8000.067639	12.474099	-0.105362	4.817678
538.837250	8000.056892	12.479104	-0.105373	4.817675
539.039036	8000.044017	12.484109	-0.105411	4.817670
538.925070	8000.033922	12.489114	-0.105390	4.817668
538.924308	8000.015985	12.494119	-0.105390	4.817662
538.949218	8000.058538	12.499123	-0.105394	4.817675
538.761131	7999.997794	12.504128	-0.105359	4.817658
539.015445	8000.052128	12.509133	-0.105407	4.817673
538.881600	8000.062837	12.514138	-0.105382	4.817676
538.782748	8000.016049	12.519143	-0.105363	4.817663
538.891418	8000.079862	12.524147	-0.105384	4.817681
538.789018	8000.028803	12.529152	-0.105365	4.817667
538.711020	8000.086731	12.534157	-0.105350	4.817684
538.363883	8000.182923	12.539162	-0.105286	4.817714
538.412381	8000.118244	12.544167	-0.105295	4.817695
538.557326	8000.162547	12.549171	-0.105322	4.817707
538.537548	8000.143278	12.554176	-0.105318	4.817702
538.890615	8000.067219	12.559181	-0.105384	4.817678
538.926046	8000.052974	12.564186	-0.105391	4.817673
538.853156	8000.028713	12.569191	-0.105377	4.817666
538.921310	8000.066623	12.574195	-0.105390	4.817677
539.107601	8000.034538	12.579200	-0.105424	4.817667
538.791723	8000.077397	12.584205	-0.105366	4.817681
538.652680	8000.105959	12.589210	-0.105340	4.817690
538.924855	8000.042432	12.594215	-0.105391	4.817670
539.036222	8000.069371	12.599219	-0.105411	4.817678
538.943529	7999.999470	12.604224	-0.105394	4.817657
539.098756	8000.010174	12.609229	-0.105423	4.817660
539.137233	8000.068745	12.614234	-0.105430	4.817677
539.021882	8000.050192	12.619239	-0.105409	4.817672
538.956124	8000.069276	12.624243	-0.105397	4.817678
538.905894	8000.037962	12.629248	-0.105387	4.817669
538.929614	8000.091045	12.634253	-0.105392	4.817684
539.024097	8000.061840	12.639258	-0.105410	4.817675
539.022135	8000.012246	12.644263	-0.105409	4.817661
539.133505	8000.008600	12.649267	-0.105430	4.817659
538.954032	8000.016534	12.654272	-0.105397	4.817662
538.973882	8000.037920	12.659277	-0.105400	4.817669
539.072713	8000.023544	12.664282	-0.105419	4.817664
539.020668	7999.986931	12.669287	-0.105409	4.817653
538.986811	8000.038119	12.674291	-0.105403	4.817669
538.856815	7999.997206	12.679296	-0.105379	4.817657
539.020920	8000.016476	12.684301	-0.105409	4.817662
539.016173	8000.014301	12.689306	-0.105408	4.817661
539.070137	8000.004545	12.694311	-0.105419	4.817658
539.094999	8000.060808	12.699315	-0.105423	4.817675
539.068256	8000.025618	12.704320	-0.105418	4.817665
539.066968	8000.038259	12.709325	-0.105418	4.817668
539.196910	8000.012735	12.714330	-0.105442	4.817660
539.023616	8000.007049	12.719335	-0.105410	4.817659
539.137885	8000.073053	12.724339	-0.105431	4.817678
539.056348	8000.019134	12.729344	-0.105416	4.817663
539.019401	7999.995397	12.734349	-0.105409	4.817656
538.841171	8000.007568	12.739354	-0.105376	4.817660
538.871548	8000.030162	12.744359	-0.105382	4.817667
539.159862	8000.011166	12.749363	-0.105436	4.817660
539.133198	7999.983359	12.754368	-0.105431	4.817652
539.202834	8000.017073	12.759373	-0.105444	4.817661
538.934215	8000.075386	12.764378	-0.105394	4.817680
539.244731	8000.015581	12.769383	-0.105452	4.817661
539.145204	8000.012025	12.774387	-0.105433	4.817660
539.033023	8000.015666	12.779392	-0.105412	4.817662
539.045178	8000.109713	12.784397	-0.105415	4.817689
538.975717	8000.033822	12.789402	-0.105402	4.817667
538.856324	8000.017320	12.794407	-0.105380	4.817663
539.056027	8000.030782	12.799411	-0.105417	4.817666
539.137849	8000.010885	12.804416	-0.105432	4.817660
539.104493	8000.038878	12.809421	-0.105426	4.817668
539.218826	8000.026838	12.814426	-0.105447	4.817664
539.206153	8000.028766	12.819431	-0.105445	4.817665
539.077401	8000.036385	12.824435	-0.105421	4.817668
539.156463	7999.981643	12.829440	-0.105436	4.817651
539.172791	8000.006142	12.834445	-0.105439	4.817658
539.181160	8000.044236	12.839450	-0.105441	4.817670
538.904195	8000.017000	12.844455	-0.105389	4.817663
539.066378	8000.061554	12.849459	-0.105419	4.817675
539.013344	8000.008051	12.854464	-0.105409	4.817660
539.199735	8000.037139	12.859469	-0.105444	4.817667
539.110416	8000.021075	12.864474	-0.105428	4.817663
538.951995	8000.032480	12.869479	-0.105398	4.817667
539.096851	8000.027212	12.874483	-0.105425	4.817665
538.923578	8000.000433	12.879488	-0.105393	4.817658
539.118215	8000.039132	12.884493	-0.105429	4.817668
538.950976	8000.054628	12.889498	-0.105398	4.817674
538.820020	8000.063269	12.894503	-0.105374	4.817677
538.926618	8000.060608	12.899507	-0.105394	4.817675
538.806445	8000.087336	12.904512	-0.105371	4.817684
538.734648	8000.065199	12.909517	-0.105358	4.817678
538.802960	8000.057761	12.914522	-0.105371	4.817675
538.885405	8000.069513	12.919527	-0.105386	4.817678
539.101134	8000.025202	12.924531	-0.105426	4.817664
539.062448	8000.034133	12.929536	-0.105419	4.817667
539.135778	8000.090049	12.934541	-0.105433	4.817683
539.305638	8000.096748	12.939546	-0.105465	4.817684
538.926474	8000.032162	12.944551	-0.105394	4.817667
539.087031	8000.061928	12.949555	-0.105424	4.817675
539.187210	8000.051790	12.954560	-0.105443	4.817672
539.133217	8000.047843	12.959565	-0.105433	4.817671
538.910111	8000.051977	12.964570	-0.105391	4.817673
538.609373	8000.080291	12.969575	-0.105335	4.817683
538.927997	8000.129236	12.974579	-0.105395	4.817696
538.813316	8000.038975	12.979584	-0.105373	4.817670
538.993696	8000.034226	12.984589	-0.105407	4.817667
539.008629	8000.082962	12.989594	-0.105410	4.817682
538.908850	8000.061472	12.994599	-0.105391	4.817676
538.954416	8000.130694	12.999603	-0.105400	4.817696
539.079838	8000.063972	13.004608	-0.105423	4.817676
539.031940	8000.040075	13.009613	-0.105414	4.817669
538.873489	8000.059916	13.014618	-0.105385	4.817675
538.905597	8000.037185	13.019623	-0.105391	4.817669
538.994973	8000.044820	13.024627	-0.105408	4.817670
539.006339	8000.004912	13.029632	-0.105410	4.817659
538.971051	8000.030768	13.034637	-0.105403	4.817666
538.925214	8000.061743	13.039642	-0.105395	4.817676
538.639870	8000.033330	13.044647	-0.105342	4.817669
538.940336	8000.090447	13.049651	-0.105398	4.817684
538.724994	8000.062000	13.054656	-0.105358	4.817677
538.990642	8000.066930	13.059661	-0.105407	4.817677
538.890075	8000.090780	13.064666	-0.105389	4.817684
538.746450	8000.081307	13.069671	-0.105362	4.817682
538.910683	8000.109017	13.074675	-0.105392	4.817690
538.731110	8000.070544	13.079680	-0.105359	4.817679
538.875643	8000.097967	13.084685	-0.105386	4.817687
539.028086	8000.110739	13.089690	-0.105414	4.817690
539.227658	8000.056700	13.094695	-0.105452	4.817673
538.837381	8000.128005	13.099699	-0.105379	4.817696
538.945091	8000.062080	13.104704	-0.105399	4.817676
539.041940	8000.060332	13.109709	-0.105417	4.817675
538.853532	8000.106103	13.114714	-0.105382	4.817689
538.939668	8000.066231	13.119719	-0.105398	4.817677
538.834127	8000.149069	13.124723	-0.105379	4.817702
538.771974	8000.036372	13.129728	-0.105367	4.817669
538.927442	8000.068173	13.134733	-0.105396	4.817678
538.910447	8000.092186	13.139738	-0.105393	4.817685
538.875943	8000.058992	13.144743	-0.105387	4.817675
539.212292	8000.058625	13.149747	-0.105449	4.817674
539.072861	8000.093510	13.154752	-0.105423	4.817684
539.136135	8000.058577	13.159757	-0.105435	4.817674
539.157230	8000.068380	13.164762	-0.105439	4.817677
538.861350	8000.100984	13.169767	-0.105384	4.817688
539.144182	8000.166282	13.174771	-0.105437	4.817706
538.842947	8000.127090	13.179776	-0.105381	4.817695
539.056570	8000.115442	13.184781	-0.105421	4.817691
539.112401	8000.081456	13.189786	-0.105431	4.817681
538.843725	8000.111292	13.194791	-0.105381	4.817691
538.899795	8000.173284	13.199795	-0.105392	4.817709
539.026622	8000.124512	13.204800	-0.105415	4.817694
538.996636	8000.117751	13.209805	-0.105410	4.817692
539.133110	8000.112361	13.214810	-0.105435	4.817690
539.179575	8000.059254	13.219815	-0.105444	4.817674
539.148741	8000.160057	13.224819	-0.105438	4.817704
539.088917	8000.070595	13.229824	-0.105427	4.817678
539.263844	8000.066821	13.234829	-0.105460	4.817676
539.178330	8000.116203	13.239834	-0.105444	4.817691
539.197834	8000.026843	13.244839	-0.105447	4.817664
539.233028	8000.065328	13.249843	-0.105454	4.817675
539.166955	8000.009525	13.254848	-0.105442	4.817659
539.274421	8000.073322	13.259853	-0.105462	4.817678
539.169962	8000.026451	13.264858	-0.105442	4.817664
539.306301	8000.029497	13.269863	-0.105468	4.817665
539.500306	8000.069243	13.274867	-0.105504	4.817675
539.398512	8000.099403	13.279872	-0.105485	4.817685
539.327965	8000.094160	13.284877	-0.105472	4.817684
539.343063	8000.065907	13.289882	-0.105475	4.817675
539.345463	8000.042743	13.294887	-0.105475	4.817668
539.266068	8000.065846	13.299891	-0.105461	4.817675
539.428663	8000.052400	13.304896	-0.105491	4.817671
539.465535	8000.045559	13.309901	-0.105498	4.817669
539.177563	8000.064567	13.314906	-0.105444	4.817675
538.896626	8000.079459	13.319911	-0.105392	4.817681
539.238179	8000.134012	13.324915	-0.105456	4.817696
539.132116	8000.021728	13.329920	-0.105436	4.817663
539.190263	8000.074258	13.334925	-0.105447	4.817678
539.224715	8000.085311	13.339930	-0.105453	4.817681
539.216499	7999.996602	13.344935	-0.105452	4.817655
539.426589	8000.051348	13.349939	-0.105491	4.817670
539.266998	8000.037423	13.354944	-0.105461	4.817667
539.431069	8000.036655	13.359949	-0.105492	4.817666
539.409637	8000.011034	13.364954	-0.105488	4.817659
539.302810	7999.982058	13.369959	-0.105468	4.817650
539.494996	8000.032325	13.374963	-0.105504	4.817665
539.350008	8000.008066	13.379968	-0.105477	4.817658
539.285075	8000.060911	13.384973	-0.105465	4.817674
539.226152	8000.057947	13.389978	-0.105454	4.817673
539.297121	8000.025235	13.394983	-0.105467	4.817663
539.172940	8000.059287	13.399987	-0.105444	4.817674
539.247448	8000.003425	13.404992	-0.105458	4.817657
539.225962	8000.098036	13.409997	-0.105454	4.817685
539.196929	8000.073359	13.415002	-0.105449	4.817678
539.484777	8000.007950	13.420007	-0.105502	4.817657
539.593188	8000.041175	13.425011	-0.105523	4.817667
539.361028	8000.027247	13.430016	-0.105480	4.817664
539.230301	8000.045384	13.435021	-0.105455	4.817670
539.086506	8000.069658	13.440026	-0.105429	4.817677
539.141198	8000.031436	13.445031	-0.105439	4.817666
539.271818	8000.096624	13.450035	-0.105463	4.817684
538.973200	8000.073290	13.455040	-0.105408	4.817679
539.210491	8000.080972	13.460045	-0.105452	4.817680
539.412684	8000.041736	13.465050	-0.105489	4.817668
539.368455	8000.047423	13.470055	-0.105481	4.817670
539.542911	8000.058408	13.475059	-0.105514	4.817672
539.603463	8000.007615	13.480064	-0.105525	4.817657
539.382329	8000.002285	13.485069	-0.105484	4.817656
538.976284	8000.117657	13.490074	-0.105409	4.817692
539.211237	8000.059915	13.495079	-0.105452	4.817674
539.331089	8000.117564	13.500083	-0.105475	4.817690
539.255279	8000.059509	13.505088	-0.105461	4.817674
538.989492	8000.087278	13.510093	-0.105411	4.817683
539.274942	8000.062967	13.515098	-0.105464	4.817675
538.942594	8000.050743	13.520103	-0.105402	4.817672
539.349609	8000.070391	13.525107	-0.105478	4.817676
539.143432	8000.028366	13.530112	-0.105440	4.817665
539.257060	8000.067994	13.535117	-0.105461	4.817676
539.279449	8000.067270	13.540122	-0.105465	4.817676
539.468776	8000.036284	13.545127	-0.105501	4.817666
539.376500	8000.086622	13.550131	-0.105484	4.817681
539.331444	8000.029016	13.555136	-0.105475	4.817664
539.328981	8000.047968	13.560141	-0.105475	4.817670
539.287721	7999.998854	13.565146	-0.105467	4.817655
539.316552	8000.014044	13.570151	-0.105473	4.817660
539.438146	8000.083320	13.575155	-0.105495	4.817680
539.466825	8000.052101	13.580160	-0.105501	4.817670
539.361785	8000.051628	13.585165	-0.105481	4.817671
539.230743	8000.069760	13.590170	-0.105457	4.817677
539.349836	8000.045133	13.595175	-0.105479	4.817669
539.231292	8000.100361	13.600179	-0.105457	4.817686
539.202595	8000.054595	13.605184	-0.105452	4.817672
539.306798	8000.062446	13.610189	-0.105471	4.817674
539.585458	8000.137177	13.615194	-0.105523	4.817695
539.182252	8000.070129	13.620199	-0.105448	4.817677
539.132363	8000.135850	13.625203	-0.105439	4.817697
539.275372	8000.074658	13.630208	-0.105465	4.817678
539.129919	8000.093635	13.635213	-0.105438	4.817684
539.187691	8000.133504	13.640218	-0.105449	4.817696
539.158799	8000.083516	13.645223	-0.105444	4.817681
539.496526	8000.093718	13.650227	-0.105507	4.817683
539.261776	8000.056549	13.655232	-0.105463	4.817673
539.220814	8000.057010	13.660237	-0.105456	4.817673
539.413247	8000.051382	13.665242	-0.105491	4.817670
539.524133	8000.021362	13.670247	-0.105512	4.817661
539.429701	8000.059011	13.675251	-0.105495	4.817673
539.349644	8000.046246	13.680256	-0.105480	4.817669
539.498007	8000.116968	13.685261	-0.105507	4.817689
539.506064	8000.124472	13.690266	-0.105509	4.817692
539.236392	8000.154293	13.695271	-0.105459	4.817702
539.387216	8000.180754	13.700275	-0.105487	4.817709
539.210477	8000.081149	13.705280	-0.105454	4.817680
539.311645	8000.087901	13.710285	-0.105473	4.817682
539.440084	8000.087668	13.715290	-0.105497	4.817681
539.378877	8000.048811	13.720295	-0.105486	4.817670
539.501677	8000.072753	13.725299	-0.105508	4.817676
539.504997	8000.041165	13.730304	-0.105509	4.817667
539.508040	8000.073908	13.735309	-0.105510	4.817677
539.428464	8000.088572	13.740314	-0.105495	4.817681
539.403241	8000.053403	13.745319	-0.105490	4.817671
539.538799	8000.070149	13.750323	-0.105516	4.817675
539.572423	8000.063260	13.755328	-0.105522	4.817673
539.674111	8000.071075	13.760333	-0.105541	4.817675
539.483657	8000.132637	13.765338	-0.105506	4.817694
539.200476	8000.100035	13.770343	-0.105453	4.817686
539.317521	8000.136549	13.775347	-0.105475	4.817696
539.470104	8000.109247	13.780352	-0.105503	4.817687
539.421638	8000.097997	13.785357	-0.105494	4.817684
539.567876	8000.102242	13.790362	-0.105521	4.817685
539.214427	8000.085491	13.795367	-0.105456	4.817681
539.351545	8000.165540	13.800371	-0.105481	4.817704
539.507215	8000.109806	13.805376	-0.105510	4.817687
539.463837	8000.081755	13.810381	-0.105502	4.817679
539.516620	8000.095185	13.815386	-0.105512	4.817683
539.647052	8000.064395	13.820391	-0.105536	4.817673
539.477553	8000.081966	13.825395	-0.105505	4.817679
539.499973	8000.087570	13.830400	-0.105509	4.817681
539.515054	8000.094122	13.835405	-0.105512	4.817683
539.547189	8000.108305	13.840410	-0.105518	4.817687
539.310939	8000.095372	13.845415	-0.105474	4.817684
539.609018	8000.175660	13.850419	-0.105530	4.817706
539.562585	8000.107486	13.855424	-0.105521	4.817686
539.457697	8000.078538	13.860429	-0.105502	4.817678
539.789866	8000.074948	13.865434	-0.105563	4.817676
539.673634	8000.038452	13.870439	-0.105542	4.817665
539.516545	8000.118431	13.875443	-0.105513	4.817690
539.496992	8000.109711	13.880448	-0.105509	4.817687
539.738302	8000.092140	13.885453	-0.105554	4.817681
539.614588	8000.112488	13.890458	-0.105531	4.817688
539.580539	8000.053988	13.895463	-0.105525	4.817670
539.716981	8000.087622	13.900467	-0.105550	4.817680
539.622799	8000.113674	13.905472	-0.105533	4.817688
539.436658	8000.140494	13.910477	-0.105498	4.817697
539.602877	8000.154523	13.915482	-0.105529	4.817700
539.393699	8000.131437	13.920487	-0.105490	4.817694
539.529400	8000.167170	13.925491	-0.105516	4.817704
539.697062	8000.068368	13.930496	-0.105547	4.817674
539.468467	8000.098788	13.935501	-0.105504	4.817684
539.388441	8000.167234	13.940506	-0.105489	4.817705
539.076333	8000.180616	13.945511	-0.105431	4.817710
539.246239	8000.189426	13.950515	-0.105463	4.817712
539.258915	8000.149536	13.955520	-0.105465	4.817700
539.103449	8000.154656	13.960525	-0.105437	4.817702
539.143145	8000.179496	13.965530	-0.105444	4.817709
539.017086	8000.136529	13.970535	-0.105421	4.817697
539.092755	8000.182987	13.975539	-0.105435	4.817711
538.499420	8000.230237	13.980544	-0.105324	4.817727
538.859421	8000.223888	13.985549	-0.105391	4.817724
538.953852	8000.224214	13.990554	-0.105409	4.817724
538.845402	8000.120333	13.995559	-0.105389	4.817693
539.304776	8000.120706	14.000563	-0.105474	4.817691
539.740942	8000.104922	14.005568	-0.105556	4.817685
539.427153	8000.089803	14.010573	-0.105497	4.817682
539.423735	8000.097139	14.015578	-0.105497	4.817684
539.423888	8000.042302	14.020583	-0.105497	4.817668
539.352522	8000.106655	14.025587	-0.105484	4.817687
539.414181	8000.039003	14.030592	-0.105495	4.817667
539.484074	8000.059010	14.035597	-0.105508	4.817672
539.610167	8000.070345	14.040602	-0.105532	4.817675
538.948531	8000.080740	14.045607	-0.105408	4.817681
539.409351	8000.102228	14.050611	-0.105494	4.817685
539.088999	8000.210412	14.055616	-0.105435	4.817719
539.213403	8000.120472	14.060621	-0.105458	4.817692
539.746276	8000.154614	14.065626	-0.105557	4.817699
539.839253	8000.106403	14.070631	-0.105575	4.817685
539.867710	8000.123697	14.075635	-0.105580	4.817690
539.747825	8000.068163	14.080640	-0.105558	4.817674
539.897504	8000.047146	14.085645	-0.105585	4.817667
539.887399	8000.138761	14.090650	-0.105584	4.817694
539.520366	8000.111263	14.095655	-0.105515	4.817688
539.859060	8000.084565	14.100659	-0.105579	4.817678
539.599872	8000.068133	14.105664	-0.105530	4.817675
539.318399	8000.146297	14.110669	-0.105478	4.817699
539.489307	8000.063363	14.115674	-0.105510	4.817674
539.565403	8000.032836	14.120679	-0.105524	4.817664
539.307920	8000.142991	14.125683	-0.105476	4.817698
539.587474	8000.052149	14.130688	-0.105528	4.817670
539.761056	8000.103200	14.135693	-0.105561	4.817684
539.572757	8000.147919	14.140698	-0.105526	4.817698
539.413012	8000.118171	14.145703	-0.105496	4.817690
539.480490	8000.109666	14.150707	-0.105508	4.817687
539.644702	8000.098354	14.155712	-0.105539	4.817683
539.252985	8000.177020	14.160717	-0.105466	4.817708
539.498651	8000.172169	14.165722	-0.105512	4.817706
539.482392	8000.090724	14.170727	-0.105509	4.817682
539.553109	8000.114962	14.175731	-0.105522	4.817689
539.428007	8000.067790	14.180736	-0.105499	4.817675
539.160735	8000.175693	14.185741	-0.105449	4.817708
539.527555	8000.182101	14.190746	-0.105518	4.817709
539.473434	8000.094830	14.195751	-0.105508	4.817683
539.641970	8000.120495	14.200755	-0.105539	4.817690
539.561363	8000.100339	14.205760	-0.105524	4.817684
539.383366	8000.120950	14.210765	-0.105491	4.817691
539.172912	8000.178002	14.215770	-0.105452	4.817709
539.001163	8000.164954	14.220775	-0.105420	4.817706
539.511055	8000.148135	14.225779	-0.105515	4.817699
539.216368	8000.169154	14.230784	-0.105460	4.817706
539.564958	8000.084593	14.235789	-0.105525	4.817679
539.662212	8000.101835	14.240794	-0.105543	4.817684
539.316752	8000.108402	14.245799	-0.105479	4.817688
539.602252	7999.321570	14.250803	-0.105532	4.817453

539.558510	7996.059265	14.255808	-0.105521	4.816488
539.425798	7990.596350	14.260813	-0.105493	4.814871
539.447510	7984.037465	14.265818	-0.105493	4.812927
539.264641	7976.782199	14.270823	-0.105454	4.810778
539.537799	7969.087061	14.275827	-0.105500	4.808495
539.180256	7961.347950	14.280832	-0.105429	4.806201
539.057174	7953.418120	14.285837	-0.105400	4.803848
539.372593	7945.580031	14.290842	-0.105454	4.801519
539.145010	7937.491645	14.295847	-0.105407	4.799117
538.444939	7929.665946	14.300851	-0.105271	4.796794
538.429737	7921.572760	14.305856	-0.105263	4.794387
538.020798	7913.622456	14.310861	-0.105182	4.792023
537.739639	7905.571912	14.315866	-0.105124	4.789627
538.655991	7897.465579	14.320871	-0.105290	4.787210
539.074053	7889.448202	14.325875	-0.105362	4.784819
538.932387	7881.528637	14.330880	-0.105331	4.782459
538.998639	7873.472078	14.335885	-0.105338	4.780055
538.935452	7865.540459	14.340890	-0.105321	4.777689
538.771327	7857.540595	14.345895	-0.105285	4.775300
538.860760	7849.567427	14.350899	-0.105297	4.772918
538.852050	7841.520925	14.355904	-0.105290	4.770514
538.856349	7833.529776	14.360909	-0.105286	4.768124
538.603802	7825.493035	14.365914	-0.105233	4.765720
537.895092	7817.500666	14.370919	-0.105096	4.763330
538.362252	7809.557639	14.375923	-0.105178	4.760950
538.437410	7801.486464	14.380928	-0.105187	4.758531
538.282528	7793.495257	14.385933	-0.105153	4.756136
538.835886	7785.446099	14.390938	-0.105251	4.753720
538.647138	7777.475148	14.395943	-0.105210	4.751329
538.422243	7769.487174	14.400947	-0.105163	4.748931
538.427784	7761.485612	14.405952	-0.105159	4.746527
538.691878	7753.431137	14.410957	-0.105203	4.744106
538.727261	7745.526154	14.415962	-0.105205	4.741729
538.458135	7737.435888	14.420967	-0.105149	4.739296
538.742992	7729.542011	14.425971	-0.105197	4.736919
538.340737	7721.418614	14.430976	-0.105117	4.734473
538.457680	7713.489992	14.435981	-0.105134	4.732084
538.265736	7705.474003	14.440986	-0.105093	4.729668
537.884149	7697.508423	14.445991	-0.105017	4.727266
538.110396	7689.443760	14.450995	-0.105054	4.724832
537.922249	7681.510589	14.456000	-0.105014	4.722437
538.265228	7673.463137	14.461005	-0.105072	4.720005
538.039254	7665.484191	14.466010	-0.105025	4.717594
538.098756	7657.380125	14.471015	-0.105031	4.715144
538.520101	7649.427912	14.476019	-0.105104	4.712737
538.509389	7641.444074	14.481024	-0.105097	4.710320
538.299077	7633.406532	14.486029	-0.105053	4.707886
538.071522	7625.475114	14.491034	-0.105005	4.705483
537.881676	7617.458476	14.496039	-0.104965	4.703053
538.124731	7609.471937	14.501043	-0.105005	4.700630
537.958128	7601.476109	14.506048	-0.104969	4.698204
538.001089	7593.442300	14.511053	-0.104971	4.695764
538.104091	7585.439641	14.516058	-0.104985	4.693333
537.667410	7577.466489	14.521063	-0.104899	4.690910
537.775463	7569.457804	14.526067	-0.104914	4.688474
537.728540	7561.415711	14.531072	-0.104900	4.686027
537.772834	7553.375111	14.536077	-0.104903	4.683579
537.782213	7545.534297	14.541082	-0.104900	4.681191
537.750027	7537.443359	14.546087	-0.104888	4.678725
537.769374	7529.509388	14.551091	-0.104887	4.676306
537.554930	7521.439692	14.556096	-0.104842	4.673844
537.668482	7513.372180	14.561101	-0.104858	4.671381
537.684391	7505.387329	14.566106	-0.104855	4.668943
537.716135	7497.354595	14.571111	-0.104856	4.666488
537.912116	7489.359111	14.576115	-0.104888	4.664044
537.262714	7481.502802	14.581120	-0.104762	4.661641
537.208575	7473.381611	14.586125	-0.104746	4.659155
537.116856	7465.503240	14.591130	-0.104724	4.656743
537.103069	7457.410068	14.596135	-0.104716	4.654264
536.939463	7449.441193	14.601139	-0.104681	4.651821
536.632632	7441.389927	14.606144	-0.104618	4.649352
536.519522	7433.470366	14.611149	-0.104592	4.646922
536.973635	7425.347968	14.616154	-0.104671	4.644428
536.920974	7417.388051	14.621159	-0.104656	4.641983
537.115729	7409.398904	14.626163	-0.104688	4.639527
537.079075	7401.461613	14.631168	-0.104676	4.637086
536.875774	7393.411887	14.636173	-0.104633	4.634610
536.909836	7385.435416	14.641178	-0.104634	4.632154
536.973371	7377.346616	14.646183	-0.104640	4.629663
536.990411	7369.397906	14.651187	-0.104638	4.627213
536.960022	7361.362345	14.656192	-0.104628	4.624736
537.056868	7353.427083	14.661197	-0.104640	4.622288
537.262057	7345.390689	14.666202	-0.104674	4.619807
537.007227	7337.392584	14.671207	-0.104621	4.617337
536.948291	7329.384392	14.676211	-0.104605	4.614863
536.325405	7321.467409	14.681216	-0.104484	4.612415
536.618514	7313.311809	14.686221	-0.104533	4.609892
536.188499	7305.454676	14.691226	-0.104448	4.607460
536.740191	7297.267821	14.696231	-0.104545	4.604925
537.014416	7289.327781	14.701235	-0.104591	4.602465
537.105410	7281.327974	14.706240	-0.104603	4.599986
537.115196	7273.370943	14.711245	-0.104600	4.597518
536.980628	7265.384462	14.716250	-0.104569	4.595039
536.732585	7257.318305	14.721255	-0.104518	4.592534
536.835443	7249.371916	14.726259	-0.104532	4.590066
536.974042	7241.304118	14.731264	-0.104553	4.587558
537.073665	7233.248871	14.736269	-0.104566	4.585053
537.060058	7225.343913	14.741274	-0.104558	4.582593
537.121631	7217.306542	14.746279	-0.104565	4.580091
536.868157	7209.355157	14.751283	-0.104512	4.577614
536.403611	7201.364136	14.756288	-0.104421	4.575122
536.330085	7193.347678	14.761293	-0.104402	4.572622
536.451816	7185.293614	14.766298	-0.104419	4.570109
536.150685	7177.305207	14.771303	-0.104358	4.567615
536.669507	7169.272742	14.776307	-0.104449	4.565107
536.514246	7161.300325	14.781312	-0.104415	4.562615
536.491860	7153.283630	14.786317	-0.104406	4.560108
536.606444	7145.370269	14.791322	-0.104422	4.557632
536.436073	7137.298481	14.796327	-0.104385	4.555105
536.462123	7129.335582	14.801331	-0.104385	4.552611
536.278111	7121.283854	14.806336	-0.104346	4.550087
536.160105	7113.266075	14.811341	-0.104318	4.547572
536.597956	7105.253789	14.816346	-0.104395	4.545059
536.466502	7097.290711	14.821351	-0.104365	4.542559
536.357657	7089.290172	14.826355	-0.104340	4.540046
536.478957	7081.284391	14.831360	-0.104357	4.537530
536.269836	7073.235998	14.836365	-0.104313	4.534999
536.578712	7065.291158	14.841370	-0.104365	4.532500
536.492597	7057.233898	14.846375	-0.104344	4.529964
536.604267	7049.269686	14.851379	-0.104360	4.527455
536.266683	7041.247402	14.856384	-0.104292	4.524926
536.095449	7033.317350	14.861389	-0.104255	4.522425
536.407029	7025.258770	14.866394	-0.104308	4.519884
536.322045	7017.297272	14.871399	-0.104287	4.517370
536.452924	7009.234445	14.876403	-0.104306	4.514824
536.280987	7001.280773	14.881408	-0.104269	4.512310
536.091301	6993.218276	14.886413	-0.104228	4.509759
535.892103	6985.269029	14.891418	-0.104186	4.507244
536.101852	6977.172228	14.896423	-0.104220	4.504681
536.295795	6969.265373	14.901427	-0.104251	4.502177
536.163509	6961.225490	14.906432	-0.104221	4.499629
535.891996	6953.278344	14.911437	-0.104165	4.497108
535.816782	6945.235236	14.916442	-0.104146	4.494556
536.087053	6937.227268	14.921447	-0.104191	4.492014
536.021256	6929.188266	14.926451	-0.104174	4.489461
535.811530	6921.192860	14.931456	-0.104129	4.486919
535.802119	6913.151621	14.936461	-0.104122	4.484361
535.661027	6905.262713	14.941466	-0.104091	4.481851
535.758760	6897.163624	14.946471	-0.104104	4.479272
535.793994	6889.226706	14.951475	-0.104106	4.476744
535.712573	6881.175289	14.956480	-0.104085	4.474178
536.020439	6873.204788	14.961485	-0.104137	4.471637
535.889119	6865.188647	14.966490	-0.104108	4.469079
535.502537	6857.198112	14.971495	-0.104031	4.466526
535.486640	6849.153622	14.976499	-0.104022	4.463956
535.196952	6841.294219	14.981504	-0.103963	4.461442
535.370021	6833.168552	14.986509	-0.103990	4.458844
535.366546	6825.212893	14.991514	-0.103985	4.456298
535.175913	6817.136747	14.996519	-0.103944	4.453711
535.313088	6809.191216	15.001523	-0.103964	4.451166
535.183619	6801.184930	15.006528	-0.103935	4.448599
534.925536	6793.188138	15.011533	-0.103882	4.446033
535.424924	6785.139072	15.016538	-0.103970	4.443452
534.914210	6777.179728	15.021543	-0.103869	4.440893
534.872540	6769.193721	15.026547	-0.103856	4.438327
534.971043	6761.144174	15.031552	-0.103870	4.435739
534.880637	6753.144946	15.036557	-0.103848	4.433166
534.719803	6745.207764	15.041562	-0.103812	4.430610
534.648952	6737.115830	15.046567	-0.103794	4.428003
535.117345	6729.075124	15.051571	-0.103876	4.425415
534.876317	6721.145486	15.056576	-0.103826	4.422856
534.635123	6713.128641	15.061581	-0.103776	4.420269
535.014062	6705.151583	15.066586	-0.103841	4.417695
534.870806	6697.117397	15.071591	-0.103810	4.415099
534.562852	6689.162301	15.076595	-0.103747	4.412527
534.960188	6681.063597	15.081600	-0.103816	4.409910
534.997412	6673.081998	15.086605	-0.103818	4.407327
534.796331	6665.101607	15.091610	-0.103775	4.404742
534.648845	6657.123095	15.096615	-0.103742	4.402157
534.992016	6649.110554	15.101619	-0.103801	4.399561
534.988475	6641.159032	15.106624	-0.103795	4.396982
534.610097	6633.099907	15.111629	-0.103720	4.394364
534.748234	6625.163864	15.116634	-0.103740	4.391788
534.686008	6617.077745	15.121639	-0.103723	4.389160
534.496735	6609.166933	15.126643	-0.103683	4.386587
534.208124	6601.104471	15.131648	-0.103624	4.383962
534.587883	6593.132637	15.136653	-0.103690	4.381370
534.716596	6585.089846	15.141658	-0.103708	4.378751
534.542248	6577.166091	15.146663	-0.103671	4.376168
534.188065	6569.185633	15.151667	-0.103600	4.373563
534.423597	6561.117730	15.156672	-0.103638	4.370932
534.511913	6553.104464	15.161677	-0.103650	4.368317
534.095181	6545.195295	15.166682	-0.103567	4.365730
534.069640	6537.136713	15.171687	-0.103557	4.363096
534.624923	6529.166169	15.176691	-0.103655	4.360492
534.457579	6521.172661	15.181696	-0.103619	4.357875
534.515021	6513.223037	15.186701	-0.103624	4.355272
534.376356	6505.224302	15.191706	-0.103594	4.352651
534.193452	6497.125754	15.196711	-0.103554	4.349994
534.164874	6489.171529	15.201715	-0.103544	4.347384
534.301631	6481.135695	15.206720	-0.103564	4.344748
534.122699	6473.174505	15.211725	-0.103526	4.342131
534.166871	6465.183694	15.216730	-0.103529	4.339505
533.782133	6457.190438	15.221735	-0.103452	4.336874
534.021413	6449.174522	15.226739	-0.103491	4.334238
533.874336	6441.198923	15.231744	-0.103459	4.331611
533.786256	6433.149165	15.236749	-0.103437	4.328958
534.248123	6425.176586	15.241754	-0.103518	4.326333
533.807082	6417.116656	15.246759	-0.103431	4.323671
534.013948	6409.229744	15.251763	-0.103464	4.321070
534.136241	6401.135038	15.256768	-0.103482	4.318397
534.147091	6393.248242	15.261773	-0.103478	4.315791
534.016899	6385.194128	15.266778	-0.103449	4.313127
534.018422	6377.188004	15.271783	-0.103444	4.310478
534.107893	6369.128991	15.276787	-0.103456	4.307810
533.837261	6361.169747	15.281792	-0.103400	4.305171
533.680123	6353.134472	15.286797	-0.103366	4.302506
533.914087	6345.155399	15.291802	-0.103404	4.299862
533.633688	6337.201934	15.296807	-0.103347	4.297219
533.646623	6329.168800	15.301811	-0.103344	4.294552
533.761798	6321.131410	15.306816	-0.103360	4.291882
533.260662	6313.160286	15.311821	-0.103262	4.289227
533.810456	6305.111050	15.316826	-0.103359	4.286553
533.664237	6297.085244	15.321831	-0.103326	4.283880
533.624508	6289.188118	15.326835	-0.103314	4.281249
533.634728	6281.152203	15.331840	-0.103311	4.278570
533.417228	6273.177141	15.336845	-0.103265	4.275908
533.526815	6265.179433	15.341850	-0.103280	4.273240
533.339617	6257.124826	15.346855	-0.103240	4.270548
533.109950	6249.153147	15.351859	-0.103192	4.267882
533.383796	6241.096795	15.356864	-0.103238	4.265190
533.236855	6233.112368	15.361869	-0.103206	4.262517
533.339654	6225.138017	15.366874	-0.103220	4.259848
533.447374	6217.120047	15.371879	-0.103234	4.257163
533.473538	6209.094560	15.376883	-0.103234	4.254473
532.882105	6201.143282	15.381888	-0.103119	4.251800
532.971583	6193.112229	15.386893	-0.103130	4.249105
533.224056	6185.159490	15.391898	-0.103172	4.246436
533.028794	6177.088434	15.396903	-0.103131	4.243721
533.313164	6169.139157	15.401907	-0.103178	4.241051
533.387539	6161.097218	15.406912	-0.103187	4.238345
533.166647	6153.148104	15.411917	-0.103141	4.235666
533.187049	6145.152312	15.416922	-0.103139	4.232972
532.946618	6137.127020	15.421927	-0.103090	4.230264
533.245770	6129.116238	15.426931	-0.103140	4.227564
533.442734	6121.064632	15.431936	-0.103172	4.224848
533.034787	6113.145111	15.436941	-0.103090	4.222169
533.017990	6105.148334	15.441946	-0.103082	4.219465
533.097346	6097.135202	15.446951	-0.103092	4.216756
533.076446	6089.083358	15.451955	-0.103083	4.214030
532.870027	6081.131140	15.456960	-0.103039	4.211335
532.719604	6073.108630	15.461965	-0.103006	4.208614
532.636432	6065.108524	15.466970	-0.102985	4.205900
532.821664	6057.085566	15.471975	-0.103015	4.203180
532.369975	6049.193387	15.476979	-0.102925	4.200495
532.434651	6041.137867	15.481984	-0.102932	4.197758
532.223237	6033.130700	15.486989	-0.102888	4.195033
532.555124	6025.078599	15.491994	-0.102944	4.192298
531.948612	6017.094282	15.496999	-0.102826	4.189572
532.165059	6009.029927	15.502003	-0.102861	4.186828
532.066220	6001.030003	15.507008	-0.102838	4.184099
532.088385	5993.129111	15.512013	-0.102837	4.181404
532.049297	5985.123866	15.517018	-0.102824	4.178671
532.036902	5977.067223	15.522023	-0.102817	4.175919
532.395933	5969.074232	15.527027	-0.102878	4.173192
532.086563	5961.089586	15.532032	-0.102816	4.170457
532.014604	5953.044527	15.537037	-0.102797	4.167703
531.862823	5945.110620	15.542042	-0.102764	4.164984
532.275471	5937.053553	15.547047	-0.102835	4.162228
532.042872	5929.111150	15.552051	-0.102787	4.159501
532.138562	5921.116802	15.557056	-0.102800	4.156759
532.296275	5913.021843	15.562061	-0.102824	4.153982
532.465282	5905.083519	15.567066	-0.102850	4.151256
532.096232	5897.099164	15.572071	-0.102776	4.148506
532.131084	5889.106363	15.577075	-0.102777	4.145757
532.079995	5881.116586	15.582080	-0.102763	4.143005
532.153038	5873.095841	15.587085	-0.102771	4.140243
532.194649	5865.133198	15.592090	-0.102774	4.137498
532.035572	5857.082920	15.597095	-0.102739	4.134719
532.176830	5849.123564	15.602099	-0.102760	4.131973
532.195349	5841.081935	15.607104	-0.102758	4.129196
532.125384	5833.125825	15.612109	-0.102740	4.126445
531.877733	5825.157484	15.617114	-0.102689	4.123685
531.557307	5817.202792	15.622119	-0.102624	4.120927
531.458710	5809.193643	15.627123	-0.102601	4.118152
531.695875	5801.153506	15.632128	-0.102640	4.115368
531.709772	5793.114824	15.637133	-0.102637	4.112580
531.612664	5785.129106	15.642138	-0.102614	4.109807
531.507130	5777.141070	15.647143	-0.102589	4.107032
531.292323	5769.115217	15.652147	-0.102544	4.104239
531.281986	5761.173836	15.657152	-0.102537	4.101477
531.626687	5753.068488	15.662157	-0.102596	4.098661
531.600438	5745.137609	15.667162	-0.102586	4.095899
531.267710	5737.090131	15.672167	-0.102519	4.093090
531.452908	5729.091761	15.677171	-0.102548	4.090303
531.320421	5721.139437	15.682176	-0.102518	4.087526
531.167587	5713.087061	15.687181	-0.102484	4.084712
531.252541	5705.166277	15.692186	-0.102495	4.081945
531.264543	5697.085169	15.697191	-0.102492	4.079119
531.299333	5689.154984	15.702195	-0.102493	4.076345
531.296590	5681.155107	15.707200	-0.102488	4.073544
530.974872	5673.180341	15.712205	-0.102423	4.070744
530.912695	5665.154885	15.717210	-0.102406	4.067929
530.858790	5657.086642	15.722215	-0.102391	4.065097
530.903154	5649.115864	15.727219	-0.102394	4.062299
530.930161	5641.074036	15.732224	-0.102394	4.059474
530.917458	5633.105185	15.737229	-0.102386	4.056671
531.029382	5625.113425	15.742234	-0.102402	4.053861
531.113880	5617.113287	15.747239	-0.102412	4.051045
531.031163	5609.117977	15.752243	-0.102392	4.048227
530.931365	5601.107781	15.757248	-0.102368	4.045401
530.665580	5593.125544	15.762253	-0.102313	4.042580
530.630800	5585.191855	15.767258	-0.102302	4.039778
530.225358	5577.230625	15.772263	-0.102221	4.036958
530.771565	5569.098705	15.777267	-0.102318	4.034091
530.854243	5561.079457	15.782272	-0.102328	4.031255
530.604759	5553.050745	15.787277	-0.102276	4.028408
530.591072	5545.093831	15.792282	-0.102269	4.025588
530.663234	5537.055014	15.797287	-0.102277	4.022739
530.343999	5529.179475	15.802291	-0.102212	4.019939
530.551737	5521.133496	15.807296	-0.102246	4.017085
530.519997	5513.064598	15.812301	-0.102235	4.014217
530.496467	5505.150302	15.817306	-0.102225	4.011403
530.357183	5497.118882	15.822311	-0.102194	4.008542
530.669677	5489.098605	15.827315	-0.102247	4.005691
530.624172	5481.160132	15.832320	-0.102233	4.002861
530.203431	5473.183583	15.837325	-0.102150	4.000010
530.111140	5465.214102	15.842330	-0.102128	3.997164
530.082136	5457.172207	15.847335	-0.102117	3.994292
530.623775	5449.147528	15.852339	-0.102213	3.991433
530.338702	5441.197337	15.857344	-0.102154	3.988584
530.405525	5433.141985	15.862349	-0.102162	3.985703
530.784277	5425.158528	15.867354	-0.102227	3.982850
530.202308	5417.212925	15.872359	-0.102114	3.979992
530.359376	5409.197561	15.877363	-0.102138	3.977120
530.358769	5401.186009	15.882368	-0.102132	3.974244
530.292616	5393.188668	15.887373	-0.102115	3.971370
530.302937	5385.183863	15.892378	-0.102112	3.968493
530.050061	5377.181298	15.897383	-0.102059	3.965610
529.883432	5369.222899	15.902387	-0.102023	3.962742
530.407109	5361.135698	15.907392	-0.102115	3.959838
530.440328	5353.175527	15.912397	-0.102116	3.956969
530.132151	5345.224302	15.917402	-0.102054	3.954094
530.204948	5337.183860	15.922407	-0.102062	3.951193
529.835274	5329.168077	15.927411	-0.101988	3.948290
530.289756	5321.104699	15.932416	-0.102068	3.945383
530.160138	5313.186192	15.937421	-0.102038	3.942515
529.887575	5305.194584	15.942426	-0.101983	3.939617
529.882924	5297.200480	15.947431	-0.101977	3.936720
530.093258	5289.176302	15.952435	-0.102011	3.933814
529.968349	5281.184664	15.957440	-0.101982	3.930911
529.445356	5273.200626	15.962445	-0.101880	3.928002
529.557853	5265.164915	15.967450	-0.101895	3.925083
529.501099	5257.191989	15.972455	-0.101880	3.922182
529.804222	5249.199353	15.977459	-0.101931	3.919279
529.979187	5241.205523	15.982464	-0.101958	3.916370
529.894326	5233.149034	15.987469	-0.101937	3.913432
529.647484	5225.233798	15.992474	-0.101886	3.910540
529.629290	5217.142306	15.997479	-0.101878	3.907585
529.635146	5209.185507	16.002483	-0.101874	3.904678
529.570193	5201.249513	16.007488	-0.101856	3.901776
529.556603	5193.204975	16.012493	-0.101849	3.898832
529.232725	5185.308484	16.017498	-0.101783	3.895934
529.443684	5177.180517	16.022503	-0.101817	3.892960
529.396409	5169.208814	16.027507	-0.101803	3.890035
529.248605	5161.231585	16.032512	-0.101771	3.887105
529.330886	5153.161230	16.037517	-0.101781	3.884142
529.270022	5145.314553	16.042522	-0.101764	3.881257
529.227085	5137.241138	16.047527	-0.101751	3.878286
529.397278	5129.278337	16.052531	-0.101778	3.875359
528.834436	5121.227322	16.057536	-0.101668	3.872381
528.851791	5113.098925	16.062541	-0.101666	3.869385
528.996554	5105.171031	16.067546	-0.101687	3.866462
529.095445	5097.115565	16.072551	-0.101701	3.863490
529.003406	5089.208713	16.077555	-0.101678	3.860566
529.160755	5081.202728	16.082560	-0.101703	3.857609
529.085639	5073.206669	16.087565	-0.101683	3.854648
529.072885	5065.282351	16.092570	-0.101676	3.851712
528.834038	5057.208551	16.097575	-0.101626	3.848715
528.956151	5049.255168	16.102579	-0.101644	3.845767
529.136658	5041.234723	16.107584	-0.101672	3.842793
528.911941	5033.270562	16.112589	-0.101625	3.839829
528.894613	5025.320849	16.117594	-0.101617	3.836873
528.993125	5017.238908	16.122599	-0.101630	3.833868
528.878104	5009.311413	16.127603	-0.101603	3.830913
528.789239	5001.276359	16.132608	-0.101582	3.827917
528.880021	4993.217072	16.137613	-0.101593	3.824913
528.906834	4985.320829	16.142618	-0.101593	3.821966
528.631306	4977.278019	16.147623	-0.101537	3.818955
528.603808	4969.329723	16.152627	-0.101527	3.815983
528.844312	4961.278363	16.157632	-0.101566	3.812976
528.618284	4953.240115	16.162637	-0.101519	3.809961
528.773567	4945.285557	16.167642	-0.101543	3.806984
528.804233	4937.216461	16.172647	-0.101543	3.803958
528.574116	4929.343185	16.177651	-0.101495	3.800998
528.533888	4921.349247	16.182656	-0.101483	3.797994
528.494304	4913.305998	16.187661	-0.101470	3.794970
528.627265	4905.321782	16.192666	-0.101490	3.791969
528.614731	4897.259841	16.197671	-0.101482	3.788933
528.439537	4889.308691	16.202675	-0.101444	3.785933
528.479995	4881.301099	16.207680	-0.101447	3.782914
528.283125	4873.315264	16.212685	-0.101405	3.779895
528.443709	4865.298221	16.217690	-0.101430	3.776871
528.265574	4857.319164	16.222695	-0.101391	3.773850
528.193147	4849.377980	16.227699	-0.101373	3.770844
528.221145	4841.307535	16.232704	-0.101373	3.767789
528.173847	4833.312554	16.237709	-0.101359	3.764758
528.029804	4825.413189	16.242714	-0.101327	3.761758
528.164360	4817.317743	16.247719	-0.101347	3.758689
528.131711	4809.388884	16.252723	-0.101335	3.755676
528.057159	4801.381217	16.257728	-0.101316	3.752630
527.889880	4793.384314	16.262733	-0.101280	3.749583
528.117046	4785.386180	16.267738	-0.101317	3.746543
528.081482	4777.347290	16.272743	-0.101305	3.743479
528.030261	4769.410096	16.277747	-0.101291	3.740450
527.859998	4761.427301	16.282752	-0.101254	3.737398
528.008791	4753.366089	16.287757	-0.101276	3.734322
528.124664	4745.428660	16.292762	-0.101293	3.731290
527.642217	4737.417225	16.297767	-0.101198	3.728213
527.672096	4729.393281	16.302771	-0.101198	3.725140
527.374458	4721.499818	16.307776	-0.101138	3.722107
527.413733	4713.411186	16.312781	-0.101140	3.719005
527.478937	4705.489344	16.317786	-0.101147	3.715965
527.499788	4697.394951	16.322791	-0.101145	3.712855
527.401415	4689.381716	16.327795	-0.101122	3.709771
527.510640	4681.382583	16.332800	-0.101137	3.706695
527.204368	4673.411053	16.337805	-0.101075	3.703616
527.461683	4665.407281	16.342810	-0.101118	3.700537
526.916657	4657.445660	16.347815	-0.101011	3.697451
527.212875	4649.404894	16.352819	-0.101061	3.694354
527.304251	4641.400604	16.357824	-0.101073	3.691262
526.996188	4633.416890	16.362829	-0.101010	3.688166
526.931416	4625.459111	16.367834	-0.100993	3.685083
527.317672	4617.412341	16.372839	-0.101060	3.681975
527.561146	4609.381063	16.377843	-0.101100	3.678867
527.356560	4601.489001	16.382848	-0.101057	3.675798
527.266334	4593.438387	16.387853	-0.101035	3.672668
527.672571	4585.431412	16.392858	-0.101105	3.669566
527.406831	4577.466625	16.397863	-0.101051	3.666460
527.336028	4569.450453	16.402867	-0.101032	3.663336
527.254884	4561.514723	16.407872	-0.101012	3.660240
526.988278	4553.557759	16.412877	-0.100957	3.657129
527.065184	4545.511173	16.417882	-0.100966	3.653989
526.855598	4537.550463	16.422887	-0.100922	3.650872
526.893499	4529.510002	16.427891	-0.100924	3.647729
526.769121	4521.501346	16.432896	-0.100896	3.644590
526.676686	4513.557946	16.437901	-0.100873	3.641475
526.860921	4505.550233	16.442906	-0.100903	3.638340
527.022798	4497.538199	16.447911	-0.100927	3.635200
526.672004	4489.592259	16.452915	-0.100857	3.632069
526.487652	4481.562970	16.457920	-0.100818	3.628907
526.505821	4473.561283	16.462925	-0.100816	3.625759
526.504679	4465.567917	16.467930	-0.100810	3.622611
526.407804	4457.560634	16.472935	-0.100787	3.619451
526.660602	4449.574907	16.477939	-0.100829	3.616308
526.699859	4441.551283	16.482944	-0.100831	3.613141
526.581224	4433.548415	16.487949	-0.100804	3.609974
526.659869	4425.588880	16.492954	-0.100813	3.606828
526.683754	4417.540910	16.497959	-0.100813	3.603642
526.534184	4409.633910	16.502963	-0.100780	3.600505
526.774892	4401.599266	16.507968	-0.100819	3.597325
526.677023	4393.591601	16.512973	-0.100796	3.594143
526.478404	4385.656565	16.517978	-0.100754	3.590985
526.429281	4377.628971	16.522983	-0.100740	3.587791
526.286728	4369.648351	16.527987	-0.100708	3.584610
526.244085	4361.670652	16.532992	-0.100695	3.581431
526.281935	4353.615070	16.537997	-0.100697	3.578220
526.559570	4345.613836	16.543002	-0.100743	3.575035
526.461931	4337.600622	16.548007	-0.100720	3.571831
526.587278	4329.620964	16.553011	-0.100738	3.568644
526.283443	4321.671858	16.558016	-0.100676	3.565454
526.191102	4313.701707	16.563021	-0.100654	3.562259
526.187790	4305.699377	16.568026	-0.100648	3.559051
526.059994	4297.754080	16.573031	-0.100619	3.555859
526.119786	4289.672065	16.578035	-0.100625	3.552615
525.940351	4281.659758	16.583040	-0.100586	3.549389
525.914960	4273.648569	16.588045	-0.100577	3.546165
526.000174	4265.653318	16.593050	-0.100587	3.542947
526.172354	4257.631571	16.598055	-0.100614	3.539719
525.991046	4249.720658	16.603059	-0.100575	3.536522
525.791154	4241.744998	16.608064	-0.100533	3.533295
525.673250	4233.727960	16.613069	-0.100506	3.530051
525.783251	4225.731653	16.618074	-0.100521	3.526819
525.754241	4217.706354	16.623079	-0.100511	3.523569
525.803733	4209.752467	16.628083	-0.100515	3.520346
525.448211	4201.854961	16.633088	-0.100443	3.517131
525.499798	4193.751811	16.638093	-0.100448	3.513843
525.424874	4185.820418	16.643098	-0.100429	3.510617
525.461077	4177.741157	16.648103	-0.100430	3.507331
525.691982	4169.707840	16.653107	-0.100468	3.504067
525.456899	4161.846379	16.658112	-0.100419	3.500856
525.549952	4153.782052	16.663117	-0.100431	3.497569
525.703000	4145.792367	16.668122	-0.100455	3.494311
525.376026	4137.807592	16.673127	-0.100388	3.491037
525.575734	4129.780287	16.678131	-0.100420	3.487760
525.370945	4121.796421	16.683136	-0.100377	3.484484
525.643803	4113.798071	16.688141	-0.100423	3.481215
525.728908	4105.848741	16.693146	-0.100434	3.477956
525.687341	4097.818185	16.698151	-0.100421	3.474657
525.620879	4089.849663	16.703155	-0.100403	3.471380
525.559346	4081.849623	16.708160	-0.100386	3.468086
525.294330	4073.842569	16.713165	-0.100332	3.464780
525.329724	4065.904529	16.718170	-0.100333	3.461509
525.203585	4057.875145	16.723175	-0.100305	3.458192
525.188223	4049.887593	16.728179	-0.100297	3.454893
525.279631	4041.904269	16.733184	-0.100309	3.451596
525.120239	4033.899244	16.738189	-0.100274	3.448278
525.214993	4025.887979	16.743194	-0.100286	3.444963
525.089142	4017.925820	16.748199	-0.100258	3.441658
524.864212	4009.947939	16.753203	-0.100211	3.438339
524.921440	4001.954610	16.758208	-0.100216	3.435021
524.976801	3993.970638	16.763213	-0.100221	3.431703
525.202146	3985.939050	16.768218	-0.100258	3.428368
524.974914	3977.945257	16.773223	-0.100211	3.425030
524.817372	3970.010442	16.778227	-0.100176	3.421716
524.739037	3962.035669	16.783232	-0.100156	3.418384
524.774225	3953.977069	16.788237	-0.100158	3.415019
524.633685	3946.035136	16.793242	-0.100126	3.411692
524.655633	3938.001653	16.798247	-0.100125	3.408330
524.613220	3930.003106	16.803251	-0.100112	3.404976
524.669612	3922.053967	16.808256	-0.100118	3.401644
524.594491	3914.044198	16.813261	-0.100098	3.398278
524.518667	3906.085526	16.818266	-0.100079	3.394930
524.327806	3898.029554	16.823271	-0.100038	3.391534
524.387155	3889.998970	16.828275	-0.100044	3.388154
524.426326	3882.029912	16.833280	-0.100046	3.384796
524.310626	3874.056855	16.838285	-0.100020	3.381428
524.120389	3866.107056	16.843290	-0.099979	3.378063
524.129881	3858.099403	16.848295	-0.099976	3.374677
524.083098	3850.106844	16.853299	-0.099962	3.371293
524.128687	3842.100371	16.858304	-0.099965	3.367902
523.879512	3834.088447	16.863309	-0.099914	3.364495
524.172336	3826.134057	16.868314	-0.099963	3.361129
524.039103	3818.125395	16.873319	-0.099933	3.357721
524.087272	3810.130406	16.878323	-0.099937	3.354322
524.091334	3802.162009	16.883328	-0.099932	3.350929
523.969237	3794.145373	16.888333	-0.099905	3.347507
524.052633	3786.160664	16.893338	-0.099915	3.344103
523.825879	3778.239792	16.898343	-0.099868	3.340711
523.969121	3770.207648	16.903347	-0.099889	3.337282
523.703733	3762.246732	16.908352	-0.099835	3.333865
523.499700	3754.256639	16.913357	-0.099791	3.330434
523.546562	3746.260644	16.918362	-0.099795	3.327006
523.693781	3738.199999	16.923367	-0.099817	3.323551
523.592921	3730.268496	16.928371	-0.099793	3.320138
523.669331	3722.288768	16.933376	-0.099802	3.316708
523.546451	3714.256107	16.938381	-0.099774	3.313244
523.675117	3706.271615	16.943386	-0.099793	3.309807
523.634812	3698.254860	16.948391	-0.099780	3.306345
523.583155	3690.262713	16.953395	-0.099766	3.302891
523.493119	3682.307671	16.958400	-0.099744	3.299447
523.302089	3674.329747	16.963405	-0.099703	3.295985
523.281221	3666.358568	16.968410	-0.099694	3.292530
523.192545	3658.314179	16.973415	-0.099672	3.289036
523.508080	3650.293344	16.978419	-0.099726	3.285565
523.555373	3642.354094	16.983424	-0.099729	3.282116
523.247414	3634.370308	16.988429	-0.099667	3.278629
523.386192	3626.415863	16.993434	-0.099688	3.275168
523.479352	3618.380940	16.998439	-0.099700	3.271668
523.427871	3610.398603	17.003443	-0.099685	3.268180
523.356612	3602.378092	17.008448	-0.099667	3.264672
523.346103	3594.426240	17.013453	-0.099660	3.261192
523.315385	3586.454835	17.018458	-0.099649	3.257699
523.312937	3578.445258	17.023463	-0.099643	3.254187
522.988365	3570.507667	17.028467	-0.099577	3.250689
523.217328	3562.475415	17.033472	-0.099615	3.247169
523.030025	3554.480669	17.038477	-0.099575	3.243644
523.002784	3546.533591	17.043482	-0.099565	3.240143
522.852565	3538.557806	17.048487	-0.099532	3.236621
523.151406	3530.530952	17.053491	-0.099582	3.233090
523.140073	3522.529894	17.058496	-0.099575	3.229555
522.714906	3514.560389	17.063501	-0.099490	3.226012
522.563824	3506.606377	17.068506	-0.099457	3.222483
522.200459	3498.599598	17.073511	-0.099384	3.218919
522.383690	3490.594325	17.078515	-0.099413	3.215374
522.568936	3482.582152	17.083520	-0.099443	3.211822
522.261445	3474.569554	17.088525	-0.099380	3.208245
521.849142	3466.667145	17.093530	-0.099298	3.204709
521.721879	3458.704413	17.098535	-0.099269	3.201154
522.167909	3450.615958	17.103539	-0.099347	3.197563
522.467113	3442.560244	17.108544	-0.099398	3.193977
522.313450	3434.610016	17.113549	-0.099364	3.190414
522.697562	3426.607155	17.118554	-0.099430	3.186847
522.624368	3418.615472	17.123559	-0.099412	3.183262
522.410676	3410.690231	17.128563	-0.099367	3.179696
522.391379	3402.689163	17.133568	-0.099358	3.176100
522.449547	3394.711840	17.138573	-0.099364	3.172514
522.304525	3386.732803	17.143578	-0.099331	3.168915
521.838106	3378.812946	17.148583	-0.099239	3.165324
522.244162	3370.752738	17.153587	-0.099310	3.161704
522.060610	3362.824218	17.158592	-0.099271	3.158114
521.467373	3354.864311	17.163597	-0.099155	3.154486
521.834961	3346.851766	17.168602	-0.099218	3.150874
522.075372	3338.782308	17.173607	-0.099258	3.147226
521.786992	3330.803844	17.178611	-0.099199	3.143591
521.754069	3322.833517	17.183616	-0.099188	3.139968
522.048310	3314.788556	17.188621	-0.099237	3.136320
522.048022	3306.835480	17.193626	-0.099232	3.132698
521.739795	3298.853826	17.198631	-0.099170	3.129044
521.929476	3290.847054	17.203635	-0.099200	3.125397
521.855546	3282.916136	17.208640	-0.099181	3.121768
521.813274	3274.907452	17.213645	-0.099168	3.118101
521.877013	3266.924824	17.218650	-0.099174	3.114446
521.896094	3258.947179	17.223655	-0.099173	3.110787
521.831975	3250.952639	17.228659	-0.099156	3.107113
521.870642	3242.962654	17.233664	-0.099158	3.103441
521.572166	3234.994484	17.238669	-0.099097	3.099759
521.705658	3227.053133	17.243674	-0.099117	3.096105
521.616570	3219.036834	17.248679	-0.099095	3.092401
521.645266	3211.021594	17.253683	-0.099095	3.088700
521.711811	3203.060663	17.258688	-0.099102	3.085020
521.512302	3195.095238	17.263693	-0.099060	3.081322
521.374198	3187.145991	17.268698	-0.099029	3.077630
521.117794	3179.163356	17.273703	-0.098976	3.073912
520.945099	3171.126881	17.278707	-0.098939	3.070168
521.283737	3163.091994	17.283712	-0.098997	3.066445
521.034008	3155.118574	17.288717	-0.098945	3.062718
521.042119	3147.161162	17.293722	-0.098942	3.059006
520.777811	3139.191463	17.298727	-0.098887	3.055271
520.790514	3131.194287	17.303731	-0.098884	3.051532
520.915128	3123.169977	17.308736	-0.098903	3.047781
520.629498	3115.184149	17.313741	-0.098844	3.044023
520.528076	3107.293509	17.318746	-0.098820	3.040315
520.709318	3099.257582	17.323751	-0.098849	3.036547
520.357797	3091.309767	17.328755	-0.098778	3.032790
520.398769	3083.305056	17.333760	-0.098781	3.029021
520.513113	3075.280763	17.338765	-0.098797	3.025241
520.575608	3067.309545	17.343770	-0.098803	3.021479
520.189219	3059.368438	17.348775	-0.098726	3.017705
520.208062	3051.369022	17.353779	-0.098724	3.013918
520.228375	3043.383443	17.358784	-0.098723	3.010133
519.864907	3035.420928	17.363789	-0.098650	3.006336
520.219396	3027.393165	17.368794	-0.098711	3.002538
520.379325	3019.413754	17.373799	-0.098736	2.998749
520.059269	3011.488241	17.378803	-0.098671	2.994956
519.968032	3003.502101	17.383808	-0.098649	2.991141
519.970960	2995.468458	17.388813	-0.098644	2.987304
519.902331	2987.519983	17.393818	-0.098626	2.983498
519.676778	2979.525552	17.398823	-0.098579	2.979658
519.749168	2971.541419	17.403827	-0.098587	2.975833
520.041102	2963.512049	17.408832	-0.098637	2.971993
519.984127	2955.497427	17.413837	-0.098621	2.968136
520.136818	2947.504955	17.418842	-0.098644	2.964297
520.030177	2939.578650	17.423847	-0.098619	2.960470
520.279727	2931.577500	17.428851	-0.098660	2.956621
520.341798	2923.592794	17.433856	-0.098667	2.952766
520.111020	2915.623907	17.438861	-0.098619	2.948897
520.123762	2907.675763	17.443866	-0.098616	2.945047
520.009860	2899.683030	17.448871	-0.098590	2.941163
519.960570	2891.718254	17.453875	-0.098575	2.937290
519.987432	2883.747968	17.458880	-0.098575	2.933414
519.696416	2875.759042	17.463885	-0.098516	2.929507
519.692775	2867.790911	17.468890	-0.098510	2.925620
519.927893	2859.781525	17.473895	-0.098549	2.921721
519.958133	2851.804035	17.478899	-0.098549	2.917821
519.603900	2843.867583	17.483904	-0.098478	2.913915
519.639517	2835.791284	17.488909	-0.098479	2.909956
519.376301	2827.853763	17.493914	-0.098425	2.906044
519.424477	2819.841718	17.498919	-0.098429	2.902107
519.139506	2811.921950	17.503923	-0.098371	2.898192
519.417966	2803.879986	17.508928	-0.098417	2.894242
519.410960	2795.885156	17.513933	-0.098411	2.890294
519.358109	2787.934778	17.518938	-0.098396	2.886360
519.382413	2779.946920	17.523943	-0.098395	2.882407
519.385121	2771.976208	17.528947	-0.098391	2.878455
519.042319	2764.067234	17.533952	-0.098322	2.874510
518.919818	2756.091146	17.538957	-0.098294	2.870538
519.283902	2748.046816	17.543962	-0.098356	2.866553
519.113600	2740.075129	17.548967	-0.098320	2.862570
519.056234	2732.097469	17.553971	-0.098304	2.858584
518.996089	2724.150004	17.558976	-0.098287	2.854607
518.967798	2716.143968	17.563981	-0.098277	2.850598
518.806695	2708.208510	17.568986	-0.098242	2.846610
519.032701	2700.168041	17.573991	-0.098279	2.842587
519.326441	2692.161504	17.578995	-0.098328	2.838578
519.134198	2684.260746	17.584000	-0.098287	2.834590
518.824529	2676.301749	17.589005	-0.098225	2.830559
518.929959	2668.294255	17.594010	-0.098239	2.826522
518.601884	2660.354152	17.599015	-0.098173	2.822489
518.550247	2652.341372	17.604019	-0.098158	2.818428
518.437895	2644.400082	17.609024	-0.098132	2.814395
518.364539	2636.379719	17.614029	-0.098113	2.810318
518.403165	2628.401630	17.619034	-0.098115	2.806263
518.352391	2620.411722	17.624039	-0.098101	2.802191
518.160585	2612.506110	17.629043	-0.098060	2.798148
517.609919	2604.584142	17.634048	-0.097952	2.794069
517.657779	2596.542708	17.639053	-0.097956	2.789959
517.560267	2588.567821	17.644058	-0.097933	2.785868
517.460431	2580.583082	17.649063	-0.097909	2.781765
517.250925	2572.629698	17.654067	-0.097865	2.777666
517.802490	2564.538874	17.659072	-0.097962	2.773537
517.823575	2556.557230	17.664077	-0.097961	2.769425
517.643778	2548.648545	17.669082	-0.097922	2.765333
517.359430	2540.700611	17.674087	-0.097864	2.761207
517.693357	2532.664592	17.679091	-0.097921	2.757068
517.877686	2524.674993	17.684096	-0.097950	2.752938
517.712021	2516.651008	17.689101	-0.097914	2.748762
517.755828	2508.689452	17.694106	-0.097917	2.744625
517.355461	2500.805240	17.699111	-0.097838	2.740495
517.470580	2492.798801	17.704115	-0.097854	2.736326
517.246845	2484.838925	17.709120	-0.097807	2.732154
517.578134	2476.777938	17.714125	-0.097864	2.727958
517.415685	2468.868007	17.719130	-0.097828	2.723804
517.244616	2460.905872	17.724135	-0.097791	2.719615
517.530353	2452.910185	17.729139	-0.097839	2.715431
517.626181	2444.921627	17.734144	-0.097852	2.711232
517.269175	2436.983925	17.739149	-0.097780	2.707025
517.443537	2428.997647	17.744154	-0.097808	2.702819
517.138667	2421.059749	17.749159	-0.097746	2.698602
517.297719	2413.046508	17.754163	-0.097770	2.694368
517.382190	2405.068917	17.759168	-0.097781	2.690141
517.132413	2397.109147	17.764173	-0.097729	2.685896
517.170605	2389.165205	17.769178	-0.097731	2.681671
516.639277	2381.272070	17.774183	-0.097627	2.677429
516.786876	2373.252284	17.779187	-0.097649	2.673158
516.753500	2365.291833	17.784192	-0.097638	2.668899
516.511525	2357.273515	17.789197	-0.097588	2.664589
517.039323	2349.251342	17.794202	-0.097681	2.660320
516.907955	2341.308684	17.799207	-0.097651	2.656044
516.903773	2333.315729	17.804211	-0.097645	2.651742
516.803205	2325.360628	17.809216	-0.097622	2.647447
516.867948	2317.375867	17.814221	-0.097628	2.643140
516.635512	2309.476537	17.819226	-0.097580	2.638853
516.186992	2301.562192	17.824231	-0.097491	2.634536
516.638370	2293.472573	17.829235	-0.097570	2.630177
516.434101	2285.534830	17.834240	-0.097527	2.625849
516.116608	2277.595707	17.839245	-0.097463	2.621506
516.217546	2269.629009	17.844250	-0.097477	2.617169
516.443316	2261.595643	17.849255	-0.097513	2.612796
516.373832	2253.622135	17.854259	-0.097495	2.608429
516.466885	2245.647673	17.859264	-0.097507	2.604065
516.521070	2237.685419	17.864269	-0.097512	2.599698
516.497459	2229.779167	17.869274	-0.097503	2.595349
515.903674	2221.766371	17.874279	-0.097387	2.590895
516.024434	2213.720220	17.879283	-0.097404	2.586464
515.992606	2205.781505	17.884288	-0.097393	2.582074
515.662089	2197.865542	17.889293	-0.097327	2.577668
515.777517	2189.875732	17.894298	-0.097343	2.573245
515.678410	2181.907647	17.899303	-0.097319	2.568812
516.044479	2173.849843	17.904307	-0.097382	2.564353
516.095777	2165.933917	17.909312	-0.097387	2.559944
515.796941	2158.023606	17.914317	-0.097326	2.555506
515.561337	2150.116095	17.919322	-0.097277	2.551065
515.454169	2142.115656	17.924327	-0.097252	2.546574
515.264082	2134.183043	17.929331	-0.097211	2.542108
515.699359	2126.142608	17.934336	-0.097287	2.537617
515.509024	2118.175797	17.939341	-0.097247	2.533115
515.650542	2110.201959	17.944346	-0.097268	2.528625
515.146337	2102.299237	17.949351	-0.097169	2.524121
515.099945	2094.374863	17.954355	-0.097155	2.519629
515.135560	2086.373535	17.959360	-0.097157	2.515092
515.141651	2078.379455	17.964365	-0.097153	2.510548
515.155917	2070.400148	17.969370	-0.097150	2.506005
514.911982	2062.477745	17.974375	-0.097100	2.501468
515.204768	2054.444603	17.979379	-0.097149	2.496898
515.415110	2046.477812	17.984384	-0.097183	2.492352
515.327621	2038.498628	17.989389	-0.097162	2.487769
515.475162	2030.525568	17.994394	-0.097184	2.483198
515.328731	2022.605162	17.999399	-0.097151	2.478627
515.296030	2014.646201	18.004403	-0.097140	2.474033
515.157536	2006.718573	18.009408	-0.097109	2.469442
515.425219	1998.686560	18.014413	-0.097154	2.464812
515.198909	1990.803643	18.019418	-0.097107	2.460222
514.559157	1982.914755	18.024423	-0.096983	2.455589
514.620625	1974.907632	18.029427	-0.096989	2.450931
514.559681	1966.948923	18.034432	-0.096972	2.446284
514.260741	1959.008496	18.039437	-0.096912	2.441620
514.644832	1950.996342	18.044442	-0.096978	2.436958
514.345020	1943.065603	18.049447	-0.096917	2.432282
514.851706	1934.967519	18.054451	-0.097006	2.427561
514.538491	1927.078422	18.059456	-0.096943	2.422890
514.490005	1919.108493	18.064461	-0.096928	2.418183
514.449075	1911.165494	18.069466	-0.096916	2.413483
514.525147	1903.177371	18.074471	-0.096925	2.408757
514.497528	1895.218714	18.079475	-0.096914	2.404030
514.837667	1887.234146	18.084480	-0.096973	2.399308
514.649729	1879.316153	18.089485	-0.096932	2.394575
514.480451	1871.411166	18.094490	-0.096896	2.389841
514.173589	1863.458316	18.099495	-0.096834	2.385058
514.494774	1855.455095	18.104499	-0.096888	2.380286
514.183209	1847.573689	18.109504	-0.096825	2.375526
513.875859	1839.610552	18.114509	-0.096763	2.370708
513.781077	1831.679038	18.119514	-0.096740	2.365916
513.782242	1823.700354	18.124519	-0.096735	2.361094
513.744240	1815.744035	18.129523	-0.096723	2.356273
513.495912	1807.819441	18.134528	-0.096671	2.351443
513.227826	1799.850884	18.139533	-0.096616	2.346575
513.319921	1791.880998	18.144538	-0.096628	2.341726
513.495593	1783.864580	18.149543	-0.096656	2.336845
513.443530	1775.913685	18.154547	-0.096641	2.331976
513.347061	1767.984978	18.159552	-0.096618	2.327106
513.288542	1760.007335	18.164557	-0.096602	2.322199
512.793918	1752.181533	18.169562	-0.096505	2.317338
512.584792	1744.239305	18.174567	-0.096461	2.312419
512.659273	1736.226732	18.179571	-0.096469	2.307470
512.833821	1728.232111	18.184576	-0.096497	2.302530
512.609886	1720.299370	18.189581	-0.096450	2.297584
512.798953	1712.303325	18.194586	-0.096480	2.292624
512.846981	1704.348678	18.199591	-0.096484	2.287666
512.811461	1696.401834	18.204595	-0.096472	2.282695
512.607829	1688.521486	18.209600	-0.096429	2.277740
512.252283	1680.570958	18.214605	-0.096358	2.272718
512.783657	1672.500406	18.219610	-0.096451	2.267685
512.736531	1664.575829	18.224615	-0.096438	2.262684
512.686544	1656.630706	18.229619	-0.096423	2.257658
512.700888	1648.673892	18.234624	-0.096421	2.252619
512.662589	1640.727722	18.239629	-0.096408	2.247570
512.634317	1632.790908	18.244634	-0.096398	2.242517
512.012540	1624.960991	18.249639	-0.096277	2.237468
512.244284	1616.957730	18.254643	-0.096315	2.232373
512.547749	1608.957133	18.259648	-0.096366	2.227275
511.864777	1601.111187	18.264653	-0.096234	2.222175
512.253080	1593.078325	18.269658	-0.096301	2.217040
512.020798	1585.165086	18.274663	-0.096253	2.211914
511.810646	1577.246477	18.279667	-0.096209	2.206775
511.857798	1569.302361	18.284672	-0.096212	2.201630
511.851550	1561.345685	18.289677	-0.096206	2.196461
511.731541	1553.420987	18.294682	-0.096179	2.191289
511.473928	1545.484445	18.299687	-0.096126	2.186085
511.563289	1537.517155	18.304691	-0.096137	2.180881
511.581585	1529.568937	18.309696	-0.096135	2.175670
511.334123	1521.636357	18.314701	-0.096084	2.170431
511.487633	1513.664422	18.319706	-0.096108	2.165192
511.606846	1505.715847	18.324711	-0.096125	2.159952
511.374690	1497.826397	18.329715	-0.096076	2.154706
511.506704	1489.858547	18.334720	-0.096096	2.149429
511.431906	1481.891103	18.339725	-0.096077	2.144120
511.583813	1473.973009	18.344730	-0.096100	2.138852
511.098696	1466.110725	18.349735	-0.096004	2.133547
511.022209	1458.161773	18.354739	-0.095985	2.128211
510.684880	1450.290851	18.359744	-0.095917	2.122888
510.981195	1442.267127	18.364749	-0.095967	2.117510
510.972279	1434.324326	18.369754	-0.095960	2.112143
510.398856	1426.451953	18.374759	-0.095848	2.106755
510.505178	1418.459035	18.379763	-0.095863	2.101338
510.403898	1410.542663	18.384768	-0.095839	2.095939
510.329122	1402.583958	18.389773	-0.095820	2.090500
510.605407	1394.609447	18.394778	-0.095866	2.085070
510.853826	1386.632271	18.399783	-0.095907	2.079622
510.711898	1378.742540	18.404787	-0.095876	2.074181
510.595752	1370.851973	18.409792	-0.095849	2.068727
510.675725	1362.872181	18.414797	-0.095859	2.063217
510.695327	1354.970137	18.419802	-0.095858	2.057740
510.673506	1347.046291	18.424807	-0.095848	2.052228
510.578475	1339.126086	18.429811	-0.095826	2.046697
510.510702	1331.217528	18.434816	-0.095808	2.041162
510.697122	1323.244278	18.439821	-0.095837	2.035593
510.666491	1315.337794	18.444826	-0.095827	2.030033
510.663740	1307.384926	18.449831	-0.095821	2.024428
510.150795	1299.569033	18.454835	-0.095720	2.018851
510.479438	1291.575423	18.459840	-0.095776	2.013221
510.402939	1283.644906	18.464845	-0.095757	2.007577
510.012342	1275.798472	18.469850	-0.095679	2.001944
510.048991	1267.861353	18.474855	-0.095681	1.996275
510.305198	1259.874659	18.479859	-0.095723	1.990578
510.231613	1251.964757	18.484864	-0.095705	1.984885
510.319106	1244.037097	18.489869	-0.095716	1.979180
510.089188	1236.181804	18.494874	-0.095668	1.973476
509.771185	1228.283447	18.499879	-0.095604	1.967715
510.033302	1220.314858	18.504883	-0.095647	1.961949
510.319666	1212.364954	18.509888	-0.095695	1.956183
509.947286	1204.493314	18.514893	-0.095621	1.950384
509.945593	1196.567494	18.519898	-0.095616	1.944569
509.722453	1188.692145	18.524903	-0.095569	1.938749
509.877678	1180.724182	18.529907	-0.095593	1.932886
509.923924	1172.799641	18.534912	-0.095596	1.927024
509.801718	1164.888931	18.539917	-0.095568	1.921136
509.778544	1156.992570	18.544922	-0.095559	1.915252
509.752220	1149.082972	18.549927	-0.095549	1.909340
509.553573	1141.185758	18.554931	-0.095507	1.903398
509.601589	1133.294295	18.559936	-0.095511	1.897471
509.173995	1125.419406	18.564941	-0.095426	1.891483
509.371033	1117.451333	18.569946	-0.095458	1.885477
508.717698	1109.670827	18.574951	-0.095331	1.879496
508.923221	1101.703775	18.579955	-0.095364	1.873453
508.722728	1093.824922	18.584960	-0.095322	1.867411
508.650416	1085.895746	18.589965	-0.095303	1.861326
508.778681	1077.966027	18.594970	-0.095322	1.855244
508.955627	1070.004784	18.599975	-0.095350	1.849124
508.712841	1062.143485	18.604979	-0.095299	1.843010
508.648452	1054.271156	18.609984	-0.095282	1.836889
508.550149	1046.357506	18.614989	-0.095259	1.830712
508.497176	1038.471993	18.619994	-0.095244	1.824540
508.587511	1030.570565	18.624999	-0.095256	1.818353
508.889412	1022.612698	18.630003	-0.095307	1.812126
508.502899	1014.782163	18.635008	-0.095230	1.805894
508.396335	1006.893487	18.640013	-0.095205	1.799628
508.404052	999.003623	18.645018	-0.095201	1.793354
508.385983	991.070943	18.650023	-0.095192	1.787020
508.232326	983.193877	18.655027	-0.095159	1.780691
508.499758	975.278715	18.660032	-0.095203	1.774362
508.161726	967.429168	18.665037	-0.095135	1.767987
507.955652	959.587784	18.670042	-0.095092	1.761613
507.996461	951.689531	18.675047	-0.095095	1.755200
507.816114	943.833478	18.680051	-0.095056	1.748769
507.449540	936.009560	18.685056	-0.094983	1.742318
507.316491	928.113223	18.690061	-0.094953	1.735813
507.293087	920.222719	18.695066	-0.094943	1.729302
506.963911	912.387616	18.700071	-0.094877	1.722773
506.880372	904.507600	18.705075	-0.094856	1.716213
506.757578	896.645065	18.710080	-0.094828	1.709638
506.251743	888.803939	18.715085	-0.094729	1.703005
506.600811	880.842885	18.720090	-0.094789	1.696358
506.666415	872.926672	18.725095	-0.094796	1.689686
506.734197	865.046590	18.730099	-0.094804	1.683018
506.616897	857.216175	18.735104	-0.094777	1.676340
506.396387	849.367754	18.740109	-0.094730	1.669607
506.713225	841.438615	18.745114	-0.094784	1.662850
506.359198	833.638027	18.750119	-0.094713	1.656084
506.476492	825.728882	18.755123	-0.094730	1.649262
506.434492	817.896903	18.760128	-0.094717	1.642456
505.861920	810.140711	18.765133	-0.094606	1.635615
505.694726	802.253892	18.770138	-0.094569	1.628686
505.685681	794.377883	18.775143	-0.094563	1.621760
505.889132	786.463802	18.780147	-0.094595	1.614800
505.493767	778.677256	18.785152	-0.094517	1.607838
505.399925	770.806532	18.790157	-0.094494	1.600814
505.183159	763.011234	18.795162	-0.094449	1.593809
505.271626	755.119363	18.800167	-0.094460	1.586730
504.842177	747.340409	18.805171	-0.094375	1.579646
505.154954	739.433725	18.810176	-0.094428	1.572523
504.866405	731.608398	18.815181	-0.094370	1.565353
504.764992	723.805032	18.820186	-0.094346	1.558198
504.557486	715.983582	18.825191	-0.094302	1.550977
504.254636	708.172024	18.830195	-0.094241	1.543718
503.761126	700.417377	18.835200	-0.094144	1.536448
503.297866	692.612479	18.840205	-0.094052	1.529100
502.946897	684.821599	18.845210	-0.093982	1.521748
502.339233	677.061255	18.850215	-0.093864	1.514349
502.030828	669.220321	18.855219	-0.093801	1.506883
501.172497	661.520519	18.860224	-0.093637	1.499429
500.309727	653.771360	18.865229	-0.093471	1.491890
500.343664	645.860447	18.870234	-0.093472	1.484297
499.767496	638.098809	18.875239	-0.093360	1.476713
499.099955	630.305363	18.880243	-0.093230	1.469044
498.330395	622.542332	18.885248	-0.093082	1.461348
497.604340	614.789911	18.890253	-0.092942	1.453629
497.291265	606.950622	18.895258	-0.092879	1.445849
496.998641	599.136769	18.900263	-0.092819	1.438055
496.095836	591.418986	18.905267	-0.092646	1.430215
495.462097	583.668539	18.910272	-0.092523	1.422343
494.751613	575.913392	18.915277	-0.092386	1.414409
494.595409	568.060624	18.920282	-0.092351	1.406424
493.747142	560.359577	18.925287	-0.092189	1.398431
493.240070	552.587202	18.930291	-0.092089	1.390377
492.123118	544.929690	18.935296	-0.091876	1.382290
491.200335	537.201256	18.940301	-0.091699	1.374114
491.011820	529.358166	18.945306	-0.091659	1.365897
490.858084	521.548725	18.950311	-0.091626	1.357672
489.749153	513.889978	18.955315	-0.091414	1.349387
489.237087	506.137446	18.960320	-0.091314	1.341057
488.348285	498.445737	18.965325	-0.091143	1.332673
487.893481	490.680112	18.970330	-0.091054	1.324234
487.126779	482.983863	18.975335	-0.090906	1.315758
486.625057	475.150195	18.980339	-0.090807	1.307126
486.175000	467.405663	18.985344	-0.090719	1.298544
485.489223	459.702312	18.990349	-0.090586	1.289907
485.497601	451.893326	18.995354	-0.090582	1.281223
484.648200	444.276790	19.000359	-0.090419	1.272534
483.726314	436.636366	19.005363	-0.090243	1.263744
483.302875	428.921494	19.010368	-0.090159	1.254904
482.544968	421.257428	19.015373	-0.090013	1.245993
481.885401	413.610969	19.020378	-0.089885	1.237058
481.169092	405.948120	19.025383	-0.089747	1.228027
480.915925	398.208536	19.030387	-0.089695	1.218931
480.285032	390.573139	19.035392	-0.089572	1.209814
479.767320	382.891522	19.040397	-0.089471	1.200595
479.045455	375.289387	19.045402	-0.089332	1.191358
478.723844	367.598497	19.050407	-0.089267	1.182024
478.095479	359.974478	19.055411	-0.089145	1.172633
477.508826	352.363906	19.060416	-0.089031	1.163192
477.012047	344.734584	19.065421	-0.088933	1.153668
476.505081	337.096879	19.070426	-0.088834	1.144053
475.767852	329.527939	19.075431	-0.088692	1.134392
475.202769	321.922353	19.080435	-0.088582	1.124640
474.943447	314.294406	19.085440	-0.088528	1.114840
474.316109	306.721147	19.090445	-0.088407	1.104942
473.351468	299.245241	19.095450	-0.088222	1.095006
473.125195	291.620989	19.100455	-0.088175	1.084950
472.468421	284.104516	19.105459	-0.088048	1.074845
471.883952	276.573925	19.110464	-0.087934	1.064641
471.276358	269.048203	19.115469	-0.087816	1.054340
470.954870	261.486891	19.120474	-0.087752	1.043956
470.406312	253.995592	19.125479	-0.087645	1.033509
469.868610	246.501432	19.130483	-0.087540	1.022954
469.359635	239.033139	19.135488	-0.087440	1.012333
468.645170	231.592274	19.140493	-0.087302	1.001587
468.360662	224.094269	19.145498	-0.087245	0.990749
467.491278	216.707974	19.150503	-0.087078	0.979805
467.116741	209.243231	19.155507	-0.087003	0.968750
466.025652	201.935938	19.160512	-0.086795	0.957614
465.430180	194.539917	19.165517	-0.086680	0.946344
465.223093	187.107824	19.170522	-0.086636	0.934986
464.478934	179.782370	19.175527	-0.086493	0.923508
463.948998	172.434578	19.180531	-0.086390	0.911909
463.299492	165.132040	19.185536	-0.086264	0.900199
462.303258	157.895047	19.190541	-0.086074	0.888341
461.400108	150.679926	19.195546	-0.085901	0.876385
460.640691	143.447122	19.200551	-0.085755	0.864276
460.249041	136.156248	19.205555	-0.085677	0.852005
459.458708	128.983924	19.210560	-0.085526	0.839637
458.607850	121.813669	19.215565	-0.085363	0.827068
457.904739	114.661886	19.220570	-0.085227	0.814384
456.855473	107.591004	19.225575	-0.085027	0.801533
456.024727	100.513174	19.230579	-0.084868	0.788530
454.927737	93.514670	19.235584	-0.084659	0.775367
453.658586	86.556926	19.240589	-0.084418	0.761996
452.343172	79.643267	19.245594	-0.084169	0.748453
450.666552	73.009163	19.250599	-0.083852	0.735079