Fri Apr 16 19:22:53 2021

Number of Points = 3646
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.176469	-0.196921	0.000000	-0.000276	0.312348

0.540639	-0.078342	0.005005	-0.000157	0.312362
1.150303	-0.189697	0.010010	-0.000271	0.312360
1.172072	-0.264164	0.015014	-0.000275	0.312033
1.048622	-0.242899	0.020019	-0.000252	0.312028
1.009242	-0.236390	0.025024	-0.000245	0.312025
0.714743	-0.181277	0.030029	-0.000190	0.312033
1.376834	-0.303200	0.035034	-0.000313	0.312025
1.183583	-0.270105	0.040038	-0.000277	0.312016
1.195610	-0.272763	0.045043	-0.000280	0.312014
1.208661	-0.335915	0.050048	-0.000282	0.311732
0.802225	-0.260799	0.055053	-0.000206	0.311738
1.055322	-0.306269	0.060058	-0.000253	0.311741
0.934898	-0.284922	0.065062	-0.000231	0.311739
0.763920	-0.251220	0.070067	-0.000199	0.311751
0.464609	-0.234025	0.075072	-0.000144	0.311579
0.552862	-0.285889	0.080077	-0.000160	0.311412
0.997569	-0.367448	0.085082	-0.000243	0.311409
0.754519	-0.324369	0.090086	-0.000198	0.311404
0.825189	-0.335752	0.095091	-0.000211	0.311411
0.741100	-0.375472	0.100096	-0.000195	0.311156
1.141753	-0.464222	0.105101	-0.000270	0.311082
1.253513	-0.482699	0.110106	-0.000291	0.311090
0.987884	-0.438620	0.115110	-0.000241	0.311071
1.168267	-0.534492	0.120115	-0.000275	0.310778
1.024147	-0.509609	0.125120	-0.000248	0.310772
1.158036	-0.536711	0.130125	-0.000273	0.310759
1.477151	-0.634078	0.135130	-0.000332	0.310576
1.362031	-0.627372	0.140134	-0.000311	0.310510
1.298858	-0.615720	0.145139	-0.000299	0.310511
1.320186	-0.678422	0.150144	-0.000303	0.310237
1.416197	-0.712406	0.155149	-0.000321	0.310160
1.437170	-0.722326	0.160154	-0.000325	0.310132
1.420125	-0.781503	0.165158	-0.000322	0.309841
1.300462	-0.756885	0.170163	-0.000300	0.309855
0.918860	-0.720362	0.175168	-0.000229	0.309702
0.532740	-0.684572	0.180173	-0.000157	0.309541
0.886490	-0.748391	0.185178	-0.000223	0.309544
1.121792	-0.842531	0.190182	-0.000267	0.309304
1.130028	-0.854958	0.195187	-0.000268	0.309253
1.240461	-0.904012	0.200192	-0.000289	0.309117
0.764178	-0.859975	0.205197	-0.000200	0.308918
1.054111	-0.913354	0.210202	-0.000254	0.308915
1.618213	-1.087517	0.215206	-0.000359	0.308580
1.570407	-1.076248	0.220211	-0.000350	0.308592
1.161034	-1.065858	0.225216	-0.000274	0.308292
1.016621	-1.043255	0.230221	-0.000247	0.308275
1.162052	-1.117559	0.235226	-0.000274	0.308051
0.763725	-1.057721	0.240230	-0.000200	0.307992
0.801052	-1.112434	0.245235	-0.000207	0.307767
1.136372	-1.199090	0.250240	-0.000270	0.307646
0.897259	-1.198869	0.255245	-0.000225	0.307443
0.805330	-1.201244	0.260250	-0.000208	0.307353
0.372755	-1.169383	0.265254	-0.000127	0.307133
0.862724	-1.284174	0.270259	-0.000219	0.307012
0.715614	-1.297319	0.275264	-0.000191	0.306824
0.789431	-1.332142	0.280269	-0.000205	0.306724
1.286103	-1.477670	0.285274	-0.000298	0.306463
1.179013	-1.478589	0.290278	-0.000278	0.306367
0.682368	-1.445922	0.295283	-0.000185	0.306095
0.590965	-1.445320	0.300288	-0.000168	0.306020
0.875503	-1.551405	0.305293	-0.000221	0.305763
0.724786	-1.548448	0.310298	-0.000193	0.305647
0.826441	-1.597124	0.315302	-0.000212	0.305504
0.731818	-1.634412	0.320307	-0.000194	0.305247
1.019543	-1.713653	0.325312	-0.000248	0.305119
0.757403	-1.723434	0.330317	-0.000199	0.304847
0.869756	-1.778250	0.335322	-0.000220	0.304684
0.757121	-1.792924	0.340326	-0.000199	0.304517
0.816692	-1.859474	0.345331	-0.000210	0.304252
0.572640	-1.842363	0.350336	-0.000165	0.304123
0.605432	-1.894355	0.355341	-0.000171	0.303904
0.769499	-1.975019	0.360346	-0.000202	0.303662
0.577451	-1.974874	0.365350	-0.000166	0.303497
0.329207	-1.974696	0.370355	-0.000120	0.303283
0.546368	-2.061920	0.375360	-0.000160	0.303055
0.454125	-2.079241	0.380365	-0.000143	0.302892
0.653695	-2.168575	0.385370	-0.000180	0.302639
0.345557	-2.165306	0.390374	-0.000123	0.302387
0.382820	-2.207162	0.395379	-0.000130	0.302219
0.442176	-2.262928	0.400384	-0.000141	0.302004
0.353099	-2.303328	0.405389	-0.000124	0.301733
0.187215	-2.310293	0.410394	-0.000093	0.301555
0.301474	-2.374658	0.415398	-0.000115	0.301346
0.006165	-2.374451	0.420403	-0.000060	0.301090
-0.362233	-2.351221	0.425408	0.000009	0.300880
-0.515093	-2.355268	0.430413	0.000037	0.300727
-0.117920	-2.463837	0.435418	-0.000037	0.300552
-0.186334	-2.517447	0.440422	-0.000024	0.300234
-0.380695	-2.520742	0.445427	0.000012	0.300048
-0.341008	-2.570577	0.450432	0.000005	0.299843
0.115389	-2.717468	0.455437	-0.000080	0.299534
-0.617104	-2.627501	0.460442	0.000056	0.299326
-0.302157	-2.735484	0.465446	-0.000002	0.299081
-3.306493	-2.221965	0.470451	0.000557	0.298924
-3.402574	-2.263799	0.475456	0.000574	0.298637
-4.258590	-2.120474	0.480461	0.000734	0.298577
-4.119495	-2.203243	0.485466	0.000708	0.298299
-3.719902	-2.299712	0.490470	0.000633	0.298183
-4.241173	-2.242983	0.495475	0.000730	0.297999
-4.276115	-2.275197	0.500480	0.000737	0.297812
-4.581025	-2.254543	0.505485	0.000794	0.297643
-4.732453	-2.272899	0.510490	0.000822	0.297420
-4.945977	-2.250453	0.515494	0.000862	0.297341
-5.504414	-2.209560	0.520499	0.000965	0.297046
-5.406684	-2.235036	0.525504	0.000947	0.297009
-5.431293	-2.290890	0.530509	0.000952	0.296715
-5.396473	-2.304716	0.535514	0.000945	0.296679
-6.325677	-2.194291	0.540518	0.001118	0.296393
-6.070514	-2.253620	0.545523	0.001071	0.296330
-6.160184	-2.287711	0.550528	0.001087	0.296084
-6.076665	-2.326747	0.555533	0.001072	0.295968
-6.496493	-2.291624	0.560538	0.001150	0.295767
-6.503880	-2.310591	0.565542	0.001151	0.295668
-6.873109	-2.274648	0.570547	0.001220	0.295515
-6.926854	-2.293740	0.575552	0.001230	0.295374
-7.874478	-2.159874	0.580557	0.001406	0.295186
-7.403029	-2.267719	0.585562	0.001318	0.295078
-8.269380	-2.152506	0.590566	0.001480	0.294871
-8.173678	-2.180548	0.595571	0.001462	0.294819
-8.092224	-2.252883	0.600576	0.001447	0.294536
-8.207667	-2.238044	0.605581	0.001468	0.294506
-8.582616	-2.221742	0.610586	0.001538	0.294252
-8.798345	-2.183030	0.615590	0.001578	0.294249
-8.794455	-2.245025	0.620595	0.001577	0.293948
-9.383386	-2.144394	0.625600	0.001687	0.293917
-9.276831	-2.208055	0.630605	0.001667	0.293699
-9.237723	-2.232776	0.635610	0.001660	0.293612
-9.736525	-2.171737	0.640614	0.001752	0.293466
-9.892730	-2.179901	0.645619	0.001782	0.293286
-9.985609	-2.167313	0.650624	0.001799	0.293265
-9.870623	-2.244589	0.655629	0.001777	0.292987
-10.446225	-2.134960	0.660634	0.001884	0.293012
-10.748954	-2.138773	0.665638	0.001941	0.292721
-10.699953	-2.158746	0.670643	0.001932	0.292667
-11.051033	-2.122453	0.675648	0.001997	0.292531
-11.263116	-2.122359	0.680653	0.002036	0.292341
-10.779092	-2.209707	0.685658	0.001946	0.292344
-11.306222	-2.181777	0.690662	0.002044	0.292008
-11.586784	-2.128482	0.695667	0.002097	0.292020
-11.340533	-2.207101	0.700672	0.002051	0.291852
-11.786203	-2.152253	0.705677	0.002134	0.291723
-11.919813	-2.135926	0.710682	0.002158	0.291683
-12.268105	-2.131115	0.715686	0.002223	0.291393
-12.089712	-2.163610	0.720691	0.002190	0.291393
-12.558085	-2.117358	0.725696	0.002277	0.291200
-12.824066	-2.092416	0.730701	0.002327	0.291084
-12.047177	-2.243328	0.735706	0.002182	0.291036
-13.125539	-2.099565	0.740710	0.002383	0.290776
-12.987886	-2.126325	0.745715	0.002357	0.290768
-13.048167	-2.143764	0.750720	0.002368	0.290626
-13.461445	-2.089920	0.755725	0.002445	0.290521
-13.305994	-2.122820	0.760730	0.002416	0.290498
-13.693047	-2.117588	0.765734	0.002488	0.290173
-14.004362	-2.055914	0.770739	0.002546	0.290199
-13.977734	-2.089165	0.775744	0.002541	0.290057
-14.189801	-2.090089	0.780749	0.002580	0.289860
-13.959542	-2.128273	0.785754	0.002538	0.289879
-14.385471	-2.105081	0.790758	0.002617	0.289608
-14.865266	-2.030819	0.795763	0.002706	0.289544
-14.271836	-2.146430	0.800768	0.002596	0.289505
-14.778119	-2.105380	0.805773	0.002690	0.289250
-15.435469	-1.980064	0.810778	0.002812	0.289280
-15.156190	-2.058382	0.815782	0.002760	0.289142
-14.729155	-2.182677	0.820787	0.002681	0.288909
-15.081055	-2.114218	0.825792	0.002746	0.288931
-15.671462	-2.059948	0.830797	0.002856	0.288666
-14.988393	-2.198409	0.835802	0.002729	0.288594
-15.351041	-2.146921	0.840806	0.002796	0.288522
-16.108760	-2.056313	0.845811	0.002937	0.288286
-16.372895	-2.004972	0.850816	0.002986	0.288302
-15.627587	-2.173028	0.855821	0.002848	0.288139
-16.439613	-2.052761	0.860826	0.002999	0.288002
-16.498387	-2.042310	0.865830	0.003010	0.288001
-16.577691	-2.077634	0.870835	0.003024	0.287751
-17.063946	-2.004686	0.875840	0.003115	0.287674
-17.273742	-1.967562	0.880845	0.003154	0.287669
-16.784881	-2.110126	0.885850	0.003063	0.287399
-17.413822	-2.004345	0.890854	0.003180	0.287356
-17.219177	-2.046879	0.895859	0.003144	0.287320
-17.529780	-2.048274	0.900864	0.003201	0.287028
-17.416112	-2.071083	0.905869	0.003180	0.287018
-17.148832	-2.137924	0.910874	0.003130	0.286926
-17.842594	-2.051080	0.915878	0.003260	0.286728
-17.536160	-2.105201	0.920883	0.003202	0.286736
-17.572200	-2.143497	0.925888	0.003209	0.286510
-18.136733	-2.065650	0.930893	0.003314	0.286385
-17.727527	-2.140817	0.935898	0.003238	0.286381
-18.532934	-2.049955	0.940902	0.003388	0.286100
-18.606121	-2.038308	0.945907	0.003401	0.286092
-18.517907	-2.071592	0.950912	0.003385	0.286005
-18.911973	-2.044547	0.955917	0.003458	0.285780
-18.966229	-2.031895	0.960922	0.003468	0.285794
-19.330266	-1.987723	0.965926	0.003536	0.285683
-18.873597	-2.103837	0.970931	0.003451	0.285515
-18.734125	-2.127832	0.975936	0.003425	0.285522
-19.060473	-2.123749	0.980941	0.003486	0.285242
-18.953875	-2.158817	0.985946	0.003466	0.285163
-19.506963	-2.066785	0.990950	0.003569	0.285120
-19.840251	-2.057565	0.995955	0.003631	0.284859
-19.916377	-2.042770	1.000960	0.003645	0.284864
-19.911890	-2.069448	1.005965	0.003644	0.284733
-19.859849	-2.119630	1.010970	0.003634	0.284526
-19.811109	-2.130418	1.015974	0.003625	0.284516
-20.047149	-2.130649	1.020979	0.003669	0.284297
-20.925587	-1.977244	1.025984	0.003833	0.284265
-20.975887	-1.970150	1.030989	0.003842	0.284255
-21.004616	-2.023870	1.035994	0.003847	0.283955
-21.434872	-1.950812	1.040998	0.003927	0.283929
-21.776698	-1.886487	1.046003	0.003991	0.283940
-21.655869	-1.962220	1.051008	0.003968	0.283666
-21.768933	-1.951686	1.056013	0.003989	0.283615
-21.595807	-1.980277	1.061018	0.003957	0.283630
-22.203269	-1.925676	1.066022	0.004070	0.283345
-22.646246	-1.852340	1.071027	0.004153	0.283308
-22.184746	-1.937578	1.076032	0.004067	0.283302
-22.320730	-1.952218	1.081037	0.004092	0.283101
-22.685413	-1.901432	1.086042	0.004160	0.283021
-22.341668	-1.967915	1.091046	0.004096	0.283001
-21.976492	-2.083492	1.096051	0.004028	0.282750
-22.538096	-2.000284	1.101056	0.004132	0.282653
-22.674230	-1.976063	1.106061	0.004158	0.282651
-22.578164	-2.048172	1.111066	0.004140	0.282371
-22.606172	-2.051569	1.116070	0.004145	0.282328
-22.180974	-2.150885	1.121075	0.004066	0.282215
-22.402353	-2.153953	1.126080	0.004107	0.281993
-23.038888	-2.036058	1.131085	0.004225	0.282004
-22.975000	-2.087717	1.136090	0.004213	0.281799
-23.020490	-2.096394	1.141094	0.004222	0.281712
-23.108165	-2.086484	1.146099	0.004238	0.281681
-23.598779	-2.055514	1.151104	0.004329	0.281382
-23.984830	-1.983034	1.156109	0.004401	0.281394
-23.336813	-2.124116	1.161114	0.004281	0.281274
-24.311852	-1.981113	1.166118	0.004462	0.281098
-24.208967	-1.999526	1.171123	0.004443	0.281100
-24.420198	-1.995768	1.176128	0.004482	0.280922
-24.822448	-1.952664	1.181133	0.004557	0.280767
-24.728006	-1.966996	1.186138	0.004539	0.280782
-24.947431	-1.955761	1.191142	0.004580	0.280634
-24.828767	-1.996942	1.196147	0.004558	0.280533
-25.154383	-1.932519	1.201152	0.004619	0.280560
-25.096238	-2.001176	1.206157	0.004608	0.280261
-25.273605	-1.979537	1.211162	0.004641	0.280206
-25.140240	-2.008680	1.216166	0.004616	0.280181
-25.019102	-2.092029	1.221171	0.004593	0.279864
-25.009483	-2.093587	1.226176	0.004592	0.279865
-25.409598	-2.050556	1.231181	0.004666	0.279712
-25.970496	-1.978220	1.236186	0.004770	0.279559
-25.800358	-2.009901	1.241190	0.004739	0.279555
-25.749519	-2.059109	1.246195	0.004729	0.279348
-26.651171	-1.908674	1.251200	0.004897	0.279278
-26.534307	-1.931413	1.256205	0.004875	0.279271
-26.345999	-2.016016	1.261210	0.004840	0.279010
-26.509617	-2.002221	1.266214	0.004870	0.278927
-26.626710	-1.985626	1.271219	0.004892	0.278903
-26.715850	-2.023443	1.276224	0.004909	0.278623
-26.870078	-1.996005	1.281229	0.004937	0.278620
-27.053017	-1.980550	1.286234	0.004971	0.278527
-26.981140	-2.039235	1.291238	0.004958	0.278290
-26.488583	-2.129940	1.296243	0.004866	0.278285
-26.878197	-2.098453	1.301248	0.004939	0.278080
-27.594314	-1.983016	1.306253	0.005072	0.278003
-27.103769	-2.079020	1.311258	0.004981	0.277968
-27.667854	-2.035532	1.316262	0.005086	0.277660
-27.687133	-2.032848	1.321267	0.005089	0.277656
-27.740070	-2.045202	1.326272	0.005099	0.277542
-28.010365	-2.032176	1.331277	0.005149	0.277354
-28.396472	-1.958782	1.336282	0.005221	0.277370
-28.067096	-2.068777	1.341286	0.005160	0.277109
-28.353833	-2.032639	1.346291	0.005213	0.277025
-28.682767	-1.970716	1.351296	0.005274	0.277037
-28.799397	-2.007868	1.356301	0.005296	0.276732
-28.357632	-2.087387	1.361306	0.005214	0.276736
-28.712936	-2.049433	1.366310	0.005280	0.276597
-29.326388	-1.973291	1.371315	0.005394	0.276412
-28.929938	-2.045786	1.376320	0.005320	0.276410
-28.875386	-2.098571	1.381325	0.005310	0.276185
-29.330323	-2.032509	1.386330	0.005395	0.276098
-29.528306	-2.000322	1.391334	0.005432	0.276078
-29.335884	-2.092599	1.396339	0.005396	0.275778
-29.616264	-2.040699	1.401344	0.005448	0.275783
-29.635414	-2.059802	1.406349	0.005451	0.275665
-29.628288	-2.084457	1.411354	0.005450	0.275542
-29.903613	-2.036025	1.416358	0.005501	0.275534
-30.271495	-2.025368	1.421363	0.005570	0.275238
-30.540490	-1.983333	1.426368	0.005620	0.275202
-30.171107	-2.063983	1.431373	0.005551	0.275132
-30.475410	-2.055769	1.436378	0.005608	0.274884
-30.514607	-2.051218	1.441382	0.005615	0.274870
-30.409264	-2.109154	1.446387	0.005595	0.274666
-30.674430	-2.083433	1.451392	0.005645	0.274548
-31.413907	-1.947994	1.456397	0.005782	0.274553
-30.890290	-2.099071	1.461402	0.005685	0.274259
-31.116149	-2.059075	1.466406	0.005727	0.274253
-31.489653	-2.017913	1.471411	0.005796	0.274112
-31.939599	-1.968499	1.476416	0.005880	0.273941
-31.747534	-2.005926	1.481421	0.005844	0.273928
-31.636617	-2.064082	1.486426	0.005823	0.273727
-32.830409	-1.864190	1.491430	0.006045	0.273637
-32.171396	-1.985985	1.496435	0.005923	0.273626
-32.180728	-2.035299	1.501440	0.005925	0.273357
-32.648064	-1.961589	1.506445	0.006011	0.273297
-32.303462	-2.031514	1.511450	0.005947	0.273259
-32.388162	-2.065342	1.516454	0.005963	0.272998
-33.033118	-1.944190	1.521459	0.006083	0.273019
-33.209275	-1.938876	1.526464	0.006116	0.272877
-33.490026	-1.925051	1.531469	0.006168	0.272680
-33.267478	-1.962507	1.536474	0.006127	0.272696
-33.290681	-1.999056	1.541478	0.006131	0.272480
-33.336115	-2.014317	1.546483	0.006139	0.272355
-32.981353	-2.079122	1.551488	0.006073	0.272354
-33.909691	-1.970859	1.556493	0.006246	0.272032
-34.260503	-1.902932	1.561498	0.006311	0.272054
-33.715644	-2.016871	1.566502	0.006210	0.271975
-34.437424	-1.924656	1.571507	0.006344	0.271767
-34.467838	-1.919893	1.576512	0.006350	0.271763
-34.700162	-1.900341	1.581517	0.006393	0.271642
-34.995328	-1.883098	1.586522	0.006448	0.271448
-34.798235	-1.923376	1.591526	0.006411	0.271425
-34.715653	-1.966018	1.596531	0.006396	0.271278
-34.990591	-1.945807	1.601536	0.006447	0.271119
-35.485388	-1.853839	1.606541	0.006539	0.271130
-34.948719	-1.987530	1.611546	0.006439	0.270937
-35.399616	-1.932315	1.616550	0.006523	0.270794
-34.578316	-2.084542	1.621555	0.006370	0.270779
-34.709664	-2.108454	1.626560	0.006394	0.270524
-35.413137	-1.979083	1.631565	0.006525	0.270531
-35.145949	-2.058875	1.636570	0.006476	0.270365
-35.575095	-2.014855	1.641574	0.006555	0.270182
-35.708614	-1.987487	1.646579	0.006580	0.270199
-35.973897	-1.991609	1.651584	0.006630	0.269919
-36.358860	-1.928714	1.656589	0.006701	0.269881
-36.183388	-1.970905	1.661594	0.006669	0.269826
-36.666003	-1.932788	1.666598	0.006758	0.269559
-36.727202	-1.920095	1.671603	0.006770	0.269568
-36.549788	-1.976020	1.676608	0.006737	0.269441
-36.626281	-1.996718	1.681613	0.006751	0.269255
-36.590129	-1.998340	1.686618	0.006744	0.269282
-36.984474	-1.981372	1.691622	0.006817	0.268988
-37.438309	-1.910109	1.696627	0.006902	0.268927
-36.849390	-2.026441	1.701632	0.006792	0.268878
-37.116700	-2.027920	1.706637	0.006842	0.268608
-37.127730	-2.026163	1.711642	0.006844	0.268607
-37.148201	-2.060890	1.716646	0.006848	0.268400
-37.130788	-2.088410	1.721651	0.006845	0.268268
-36.947578	-2.133217	1.726656	0.006810	0.268207
-37.931009	-1.993664	1.731661	0.006993	0.267994
-37.255778	-2.117754	1.736666	0.006868	0.267988
-37.955518	-2.036837	1.741670	0.006998	0.267737
-37.834438	-2.075781	1.746675	0.006975	0.267646
-38.033542	-2.052627	1.751680	0.007012	0.267576
-38.693281	-1.974420	1.756685	0.007135	0.267350
-38.608633	-1.989964	1.761690	0.007119	0.267349
-38.990832	-1.953225	1.766694	0.007190	0.267172
-39.119799	-1.955565	1.771699	0.007214	0.267032
-38.949978	-1.986727	1.776704	0.007183	0.267031
-39.493807	-1.937072	1.781709	0.007284	0.266764
-39.359777	-1.963345	1.786714	0.007259	0.266754
-40.179111	-1.817420	1.791718	0.007411	0.266737
-40.344429	-1.843633	1.796723	0.007442	0.266431
-40.128327	-1.882729	1.801728	0.007402	0.266433
-40.298575	-1.862983	1.806733	0.007434	0.266372
-40.556723	-1.860556	1.811738	0.007482	0.266130
-40.276155	-1.915961	1.816742	0.007429	0.266106
-40.438564	-1.903527	1.821747	0.007459	0.266014
-40.972606	-1.845039	1.826752	0.007559	0.265803
-40.687724	-1.901725	1.831757	0.007506	0.265777
-40.371013	-1.980283	1.836762	0.007447	0.265663
-40.803338	-1.928158	1.841766	0.007527	0.265519
-40.562804	-1.971474	1.846771	0.007482	0.265521
-40.681005	-2.005382	1.851776	0.007504	0.265219
-41.409571	-1.879113	1.856781	0.007640	0.265185
-41.273842	-1.915321	1.861786	0.007615	0.265122
-41.331831	-1.951351	1.866790	0.007625	0.264868
-41.350726	-1.948114	1.871795	0.007629	0.264867
-41.392012	-1.977021	1.876800	0.007637	0.264668
-41.876006	-1.915862	1.881805	0.007727	0.264521
-41.178488	-2.041513	1.886810	0.007597	0.264528
-41.862347	-1.965827	1.891814	0.007724	0.264262
-42.174011	-1.909245	1.896819	0.007782	0.264261
-42.085610	-1.947136	1.901824	0.007766	0.264142
-42.023193	-2.001627	1.906829	0.007754	0.263906
-42.448709	-1.920515	1.911834	0.007833	0.263926
-42.661499	-1.928014	1.916838	0.007873	0.263673
-42.975782	-1.881110	1.921843	0.007931	0.263617
-42.491620	-1.977689	1.926848	0.007841	0.263570
-43.143925	-1.910900	1.931853	0.007962	0.263285
-42.914345	-1.951595	1.936858	0.007920	0.263291
-43.117105	-1.940923	1.941862	0.007957	0.263147
-43.825532	-1.838769	1.946867	0.008089	0.263000
-43.212267	-1.949924	1.951872	0.007975	0.263003
-43.341541	-1.978633	1.956877	0.007999	0.262715
-43.244533	-2.009496	1.961882	0.007981	0.262643
-43.417396	-1.994686	1.966886	0.008013	0.262551
-43.905002	-1.943634	1.971891	0.008104	0.262344
-43.739627	-1.975185	1.976896	0.008073	0.262336
-44.203275	-1.936888	1.981901	0.008159	0.262082
-43.900252	-2.006580	1.986906	0.008103	0.262001
-43.754294	-2.046241	1.991910	0.008076	0.261929
-44.498513	-1.948112	1.996915	0.008214	0.261723
-44.669898	-1.932453	2.001920	0.008246	0.261637

-45.010080	-1.914499	2.011917	0.008309	0.261395
-45.237495	-1.912314	2.021914	0.008351	0.261178
-45.193219	-1.936811	2.031910	0.008343	0.261087
-45.659713	-1.905344	2.041907	0.008430	0.260791
-45.742513	-1.894483	2.051904	0.008445	0.260768
-45.673781	-1.936942	2.061901	0.008432	0.260602
-45.997414	-1.889074	2.071898	0.008493	0.260542
-46.203595	-1.852217	2.081894	0.008531	0.260538
-46.080666	-1.895387	2.091891	0.008508	0.260423
-46.604027	-1.840578	2.101888	0.008605	0.260199
-46.665111	-1.828580	2.111885	0.008616	0.260204
-46.673294	-1.827180	2.121882	0.008618	0.260204
-46.566555	-1.848144	2.131878	0.008598	0.260196
-46.237800	-1.909438	2.141875	0.008537	0.260188
-46.027146	-1.950475	2.151872	0.008497	0.260173
-45.783937	-1.995582	2.161869	0.008452	0.260169
-45.811960	-1.989804	2.171866	0.008457	0.260173
-45.438419	-2.060885	2.181862	0.008388	0.260156
-45.387803	-2.070807	2.191859	0.008378	0.260153
-45.617128	-2.027868	2.201856	0.008421	0.260160
-45.744685	-2.002313	2.211853	0.008444	0.260174
-45.839563	-1.984598	2.221850	0.008462	0.260176
-45.632365	-2.023672	2.231846	0.008423	0.260169
-46.057115	-1.917798	2.241843	0.008502	0.260329
-45.290641	-2.025173	2.251840	0.008360	0.260508
-45.391788	-2.005734	2.261837	0.008378	0.260514
-45.295126	-2.023788	2.271834	0.008360	0.260512
-45.638606	-1.949828	2.281830	0.008424	0.260576
-44.831654	-2.067269	2.291827	0.008274	0.260739
-45.297299	-1.981115	2.301824	0.008360	0.260748
-44.825249	-2.067670	2.311821	0.008272	0.260745
-44.657847	-2.043544	2.321818	0.008241	0.261048
-44.630048	-2.045376	2.331814	0.008236	0.261066
-44.749285	-2.015360	2.341811	0.008258	0.261113
-44.633476	-1.989003	2.351808	0.008236	0.261376
-44.345876	-2.042593	2.361805	0.008183	0.261370
-44.264813	-2.008901	2.371802	0.008168	0.261638
-44.153485	-2.016545	2.381798	0.008147	0.261709
-43.715197	-2.068717	2.391795	0.008065	0.261861
-43.593514	-2.068989	2.401792	0.008042	0.261983
-43.423164	-2.081257	2.411789	0.008011	0.262087
-42.983872	-2.121491	2.421786	0.007929	0.262306
-43.301043	-2.053864	2.431782	0.007988	0.262362
-43.224425	-2.018696	2.441779	0.007973	0.262633
-43.510107	-1.941874	2.451776	0.008026	0.262770
-42.475860	-2.094406	2.461773	0.007834	0.262967
-42.401940	-2.083837	2.471770	0.007820	0.263100
-42.385643	-2.057919	2.481766	0.007817	0.263259
-42.665518	-1.965120	2.491763	0.007869	0.263490
-42.500486	-1.972958	2.501760	0.007838	0.263612
-42.032014	-2.004940	2.511757	0.007751	0.263905
-41.971186	-1.987892	2.521754	0.007739	0.264059
-41.823701	-1.980298	2.531750	0.007712	0.264249
-41.631706	-1.972292	2.541747	0.007676	0.264484
-41.551181	-1.958104	2.551744	0.007661	0.264642
-40.707952	-2.075093	2.561741	0.007504	0.264842
-40.946206	-1.988197	2.571738	0.007548	0.265080
-40.614430	-2.019648	2.581734	0.007486	0.265239
-40.903489	-1.914000	2.591731	0.007540	0.265529
-40.474717	-1.955787	2.601728	0.007460	0.265727
-39.746084	-2.065566	2.611725	0.007324	0.265851
-39.581530	-2.052979	2.621722	0.007294	0.266083
-39.526251	-2.020712	2.631718	0.007283	0.266314
-40.149992	-1.867329	2.641715	0.007399	0.266531
-39.303575	-1.983377	2.651712	0.007242	0.266737
-38.952881	-1.997692	2.661709	0.007176	0.267006
-38.603240	-2.030525	2.671706	0.007111	0.267173
-38.230899	-2.067891	2.681702	0.007042	0.267338
-38.283174	-2.001854	2.691699	0.007051	0.267645
-37.675445	-2.078327	2.701696	0.006938	0.267829
-37.416654	-2.093735	2.711693	0.006890	0.268001
-37.540816	-2.019635	2.721690	0.006913	0.268280
-36.647733	-2.147861	2.731686	0.006746	0.268465
-36.768845	-2.100306	2.741683	0.006769	0.268603
-36.578801	-2.080192	2.751680	0.006733	0.268898
-36.141414	-2.126132	2.761677	0.006652	0.269079
-36.067463	-2.105699	2.771674	0.006638	0.269262
-35.960969	-2.075381	2.781670	0.006618	0.269529
-36.285429	-1.975007	2.791667	0.006678	0.269752
-35.766699	-2.030836	2.801664	0.006582	0.269959
-35.945659	-1.951256	2.811661	0.006615	0.270212
-35.582778	-1.954775	2.821658	0.006547	0.270547
-35.263471	-1.979028	2.831654	0.006488	0.270728
-35.119937	-1.966106	2.841651	0.006461	0.270937
-34.546776	-2.033110	2.851648	0.006354	0.271136
-34.652900	-1.962016	2.861645	0.006374	0.271413
-34.528951	-1.930168	2.871642	0.006351	0.271704
-34.101647	-1.964959	2.881638	0.006271	0.271933
-33.783587	-1.987168	2.891635	0.006212	0.272123
-32.951059	-2.097973	2.901632	0.006057	0.272339
-33.218416	-1.992484	2.911629	0.006106	0.272642
-32.840855	-2.018500	2.921626	0.006036	0.272869
-33.113257	-1.922104	2.931622	0.006087	0.273117
-33.089324	-1.881723	2.941619	0.006082	0.273355
-32.638533	-1.910872	2.951616	0.005998	0.273635
-32.372763	-1.906832	2.961613	0.005948	0.273912
-32.034645	-1.919680	2.971610	0.005885	0.274170
-32.134099	-1.853558	2.981606	0.005904	0.274424
-31.744631	-1.879892	2.991603	0.005831	0.274659
-31.310254	-1.912619	3.001600	0.005750	0.274903
-30.887104	-1.931683	3.011597	0.005671	0.275208
-30.610686	-1.931571	3.021594	0.005620	0.275474
-30.539060	-1.906446	3.031590	0.005606	0.275674
-29.936588	-1.984510	3.041587	0.005494	0.275840
-30.159754	-1.890595	3.051584	0.005536	0.276120
-29.955383	-1.870700	3.061581	0.005498	0.276420
-29.183664	-1.966399	3.071578	0.005354	0.276654
-29.233995	-1.913408	3.081574	0.005363	0.276884
-28.808111	-1.950891	3.091571	0.005284	0.277093
-28.893810	-1.882790	3.101568	0.005300	0.277368
-28.355519	-1.924872	3.111565	0.005199	0.277659
-28.067981	-1.929785	3.121562	0.005146	0.277906
-28.397022	-1.823621	3.131558	0.005207	0.278148
-27.872493	-1.871480	3.141555	0.005109	0.278396
-27.826161	-1.831175	3.151552	0.005100	0.278649
-27.726533	-1.788042	3.161549	0.005082	0.278968
-26.982436	-1.869865	3.171546	0.004943	0.279246
-26.908259	-1.839923	3.181542	0.004929	0.279471
-26.475589	-1.875016	3.191539	0.004849	0.279697
-26.122293	-1.894309	3.201536	0.004783	0.279930
-25.655386	-1.925158	3.211533	0.004696	0.280210
-25.400589	-1.917725	3.221530	0.004648	0.280488
-25.198244	-1.922189	3.231526	0.004610	0.280655
-25.121402	-1.897658	3.241523	0.004596	0.280854
-25.001854	-1.869556	3.251520	0.004574	0.281111
-24.403365	-1.925476	3.261517	0.004462	0.281384
-24.232376	-1.912520	3.271514	0.004430	0.281611
-24.515258	-1.812249	3.281510	0.004483	0.281862
-23.894584	-1.883808	3.291507	0.004367	0.282074
-23.727856	-1.858170	3.301504	0.004336	0.282362
-23.773363	-1.794191	3.311501	0.004344	0.282648
-23.405519	-1.808656	3.321498	0.004276	0.282916
-23.038265	-1.828787	3.331494	0.004207	0.283155
-22.548919	-1.877468	3.341491	0.004116	0.283362
-22.075647	-1.915085	3.351488	0.004028	0.283609
-21.383492	-1.991286	3.361485	0.003899	0.283863
-21.245876	-1.980138	3.371482	0.003873	0.284048
-20.878550	-2.008756	3.381478	0.003805	0.284243
-20.722929	-1.981683	3.391475	0.003776	0.284525
-20.605265	-1.964271	3.401472	0.003754	0.284723
-19.983435	-2.045166	3.411469	0.003638	0.284886
-20.139198	-1.958518	3.421466	0.003667	0.285183
-19.384436	-2.052961	3.431462	0.003526	0.285400
-19.437084	-2.009745	3.441459	0.003536	0.285571
-18.871846	-2.077347	3.451456	0.003431	0.285750
-18.637029	-2.075170	3.461453	0.003387	0.285978
-18.729394	-2.025051	3.471450	0.003404	0.286147
-17.989723	-2.115228	3.481446	0.003266	0.286371
-18.114011	-2.042899	3.491443	0.003289	0.286623
-18.265229	-1.977128	3.501440	0.003317	0.286816
-17.444273	-2.089570	3.511437	0.003164	0.287002
-17.420378	-2.039432	3.521434	0.003160	0.287277
-17.103883	-2.059478	3.531430	0.003101	0.287466
-17.260621	-1.992341	3.541427	0.003130	0.287661
-16.784762	-2.014739	3.551424	0.003041	0.287984
-16.259394	-2.075405	3.561421	0.002943	0.288160
-16.350870	-2.023339	3.571418	0.002960	0.288338
-15.499660	-2.127214	3.581414	0.002802	0.288594
-15.728842	-2.042669	3.591411	0.002844	0.288809
-15.760470	-1.997290	3.601408	0.002850	0.289008
-15.275537	-2.036134	3.611405	0.002760	0.289255
-15.278507	-1.983711	3.621402	0.002760	0.289515
-14.982049	-1.993699	3.631398	0.002705	0.289735
-15.002074	-1.945946	3.641395	0.002709	0.289955
-14.654706	-1.960718	3.651392	0.002644	0.290197
-14.139816	-1.992953	3.661389	0.002548	0.290503
-14.092666	-1.967434	3.671386	0.002539	0.290673
-13.620194	-2.017859	3.681382	0.002451	0.290850
-13.525624	-1.982697	3.691379	0.002433	0.291111
-12.657167	-2.093816	3.701376	0.002272	0.291344
-12.580855	-2.075143	3.711373	0.002257	0.291506
-12.125500	-2.113415	3.721370	0.002172	0.291727
-11.604059	-2.160671	3.731366	0.002075	0.291963
-11.794579	-2.099323	3.741363	0.002111	0.292096
-10.968022	-2.203617	3.751360	0.001957	0.292324
-10.843997	-2.181396	3.761357	0.001934	0.292546
-11.098379	-2.102349	3.771354	0.001981	0.292708
-11.097503	-2.040897	3.781350	0.001980	0.293013
-10.129393	-2.177597	3.791347	0.001800	0.293208
-9.913368	-2.195189	3.801344	0.001760	0.293315
-10.408254	-2.043923	3.811341	0.001852	0.293618
-10.174433	-2.036536	3.821338	0.001808	0.293864
-9.684122	-2.085627	3.831334	0.001717	0.294061
-9.915389	-1.997632	3.841331	0.001760	0.294288
-9.690436	-1.980389	3.851328	0.001718	0.294574
-9.281513	-2.007666	3.861325	0.001642	0.294805
-8.822141	-2.052745	3.871322	0.001556	0.294994
-8.930967	-1.985497	3.881318	0.001576	0.295227
-8.321863	-2.031300	3.891315	0.001463	0.295546
-8.329914	-1.996458	3.901312	0.001464	0.295709
-8.583464	-1.903892	3.911309	0.001511	0.295937
-7.801049	-2.003497	3.921306	0.001366	0.296146
-7.130507	-2.070952	3.931302	0.001241	0.296412
-6.931646	-2.062516	3.941299	0.001204	0.296630
-7.017154	-2.007902	3.951296	0.001219	0.296821
-7.249321	-1.915730	3.961293	0.001262	0.297065
-6.858391	-1.920413	3.971290	0.001190	0.297388
-6.380044	-1.964155	3.981286	0.001100	0.297599
-6.659845	-1.861559	3.991283	0.001152	0.297850
-6.159992	-1.901442	4.001280	0.001059	0.298098
-6.002642	-1.882318	4.011277	0.001030	0.298330
-5.439907	-1.923142	4.021274	0.000925	0.298628
-4.965067	-1.967552	4.031270	0.000837	0.298832
-4.711938	-1.972454	4.041267	0.000789	0.299031
-4.888768	-1.885263	4.051264	0.000822	0.299298
-4.486024	-1.903142	4.061261	0.000747	0.299565
-4.485719	-1.850789	4.071258	0.000747	0.299819
-4.123842	-1.867336	4.081254	0.000679	0.300057
-3.539784	-1.930537	4.091251	0.000571	0.300264
-3.631663	-1.852464	4.101248	0.000588	0.300560
-3.774706	-1.778292	4.111245	0.000614	0.300792
-3.197044	-1.834757	4.121242	0.000507	0.301026
-2.860389	-1.849304	4.131238	0.000444	0.301250
-2.548495	-1.858025	4.141235	0.000386	0.301481
-2.183859	-1.869057	4.151232	0.000318	0.301746
-2.130014	-1.825568	4.161229	0.000308	0.302002
-1.980699	-1.802998	4.171226	0.000280	0.302240
-2.203071	-1.706444	4.181222	0.000321	0.302509
-2.385302	-1.609419	4.191219	0.000355	0.302815
-2.236120	-1.575489	4.201216	0.000327	0.303107
-1.893479	-1.584873	4.211213	0.000263	0.303360
-1.820375	-1.533239	4.221210	0.000249	0.303669
-1.311397	-1.567406	4.231206	0.000154	0.303948
-0.826815	-1.591903	4.241203	0.000064	0.304250
-0.593680	-1.582468	4.251200	0.000021	0.304497
-0.386143	-1.561100	4.261197	-0.000018	0.304778
-0.445650	-1.489973	4.271194	-0.000007	0.305064
-0.233274	-1.462701	4.281190	-0.000047	0.305377
0.052803	-1.459608	4.291187	-0.000100	0.305638
-0.040172	-1.385766	4.301184	-0.000083	0.305908
0.005422	-1.327674	4.311181	-0.000092	0.306222
-0.522305	-1.155392	4.321178	0.000006	0.306583
-0.604479	-1.068367	4.331174	0.000022	0.306924
-0.721964	-0.969607	4.341171	0.000043	0.307289
-0.383301	-0.948109	4.351168	-0.000020	0.307680
-0.214620	-0.894716	4.361165	-0.000051	0.308075
-0.311030	-0.799865	4.371162	-0.000034	0.308438
-0.255751	-0.728363	4.381158	-0.000044	0.308821
-0.388505	-0.613053	4.391155	-0.000019	0.309248
-0.179008	-0.561411	4.401152	-0.000059	0.309668
0.245366	-0.556227	4.411149	-0.000138	0.310052
-0.017006	-0.411696	4.421146	-0.000089	0.310504
0.024610	-0.333751	4.431142	-0.000097	0.310903
-0.126483	-0.218427	4.441139	-0.000069	0.311312
-0.124209	-0.110325	4.451136	-0.000069	0.311816
0.000000	-0.042299	4.461133	-0.000093	0.312237

0.008040	0.242719	4.466138	-0.000094	0.313561
0.476222	0.722232	4.471142	-0.000182	0.316156
0.404162	1.590640	4.476147	-0.000169	0.320046
0.654204	2.689395	4.481152	-0.000216	0.325177
0.606441	4.140354	4.486157	-0.000209	0.331531
0.981884	5.799703	4.491162	-0.000280	0.338986
1.157789	7.804666	4.496166	-0.000314	0.347570
1.619506	10.058281	4.501171	-0.000401	0.357167
1.930595	12.650618	4.506176	-0.000461	0.367739
2.138823	15.585433	4.511181	-0.000502	0.379253
2.298337	18.851011	4.516186	-0.000533	0.391618
2.379871	22.468658	4.521190	-0.000551	0.404814
2.456953	26.420496	4.526195	-0.000568	0.418746
2.425317	30.737784	4.531200	-0.000565	0.433385
2.827714	35.310151	4.536205	-0.000643	0.448623
3.415156	40.193166	4.541210	-0.000755	0.464432
3.998480	45.433046	4.546214	-0.000868	0.480793
3.879861	51.141878	4.551219	-0.000849	0.497611
4.617794	57.029399	4.556224	-0.000990	0.514816
4.881022	63.335434	4.561229	-0.001044	0.532368
5.021185	69.973991	4.566234	-0.001074	0.550177
5.344539	76.893634	4.571238	-0.001139	0.568227
5.960957	84.048362	4.576243	-0.001258	0.586431
6.722815	91.453429	4.581248	-0.001405	0.604748
6.769446	99.270315	4.586253	-0.001419	0.623183
6.745231	107.337762	4.591258	-0.001420	0.641626
7.372764	115.513823	4.596262	-0.001542	0.660046
7.209538	124.042251	4.601267	-0.001517	0.678416
8.289483	132.527474	4.606272	-0.001724	0.696673
13.406679	140.497139	4.611277	-0.002682	0.714875
13.833822	149.500025	4.616282	-0.002767	0.733012
14.518347	158.606984	4.621286	-0.002901	0.750999
15.288512	167.795134	4.626291	-0.003050	0.768746
16.127177	177.079109	4.631296	-0.003212	0.786290
17.332999	186.389367	4.636301	-0.003443	0.803615
18.156804	195.845304	4.641306	-0.003603	0.820711
18.882404	205.396719	4.646310	-0.003744	0.837592
19.536304	214.954445	4.651315	-0.003872	0.854129
20.363750	224.524843	4.656320	-0.004032	0.870422
20.630287	234.195126	4.661325	-0.004088	0.886417
21.091663	243.836628	4.666330	-0.004181	0.902138
22.553199	253.298701	4.671334	-0.004459	0.917582
22.996152	262.919328	4.676339	-0.004548	0.932739
23.844044	272.454706	4.681344	-0.004712	0.947631
24.614565	281.977079	4.686349	-0.004862	0.962252
25.513049	291.445864	4.691354	-0.005035	0.976608
26.601395	300.891599	4.696358	-0.005244	0.990769
27.381913	310.299134	4.701363	-0.005395	1.004598
28.154639	319.689112	4.706368	-0.005545	1.018212
28.963720	329.027341	4.711373	-0.005702	1.031583
29.625785	338.327650	4.716378	-0.005832	1.044693
30.242681	347.630508	4.721382	-0.005953	1.057634
31.370188	356.782025	4.726387	-0.006168	1.070333
31.883953	365.991531	4.731392	-0.006270	1.082818
32.758000	375.093865	4.736397	-0.006439	1.095101
33.226648	384.218295	4.741402	-0.006532	1.107184
34.109845	393.241804	4.746406	-0.006703	1.119099
34.289765	402.343044	4.751411	-0.006742	1.130833
34.720922	411.346169	4.756416	-0.006828	1.142376
35.659987	420.242541	4.761421	-0.007009	1.153779
36.280031	429.111775	4.766426	-0.007130	1.164969
36.669533	438.019561	4.771430	-0.007209	1.176050
37.516511	446.783033	4.776435	-0.007372	1.186948
38.177356	455.559688	4.781440	-0.007501	1.197723
39.160310	464.242425	4.786445	-0.007690	1.208355
39.852629	472.965966	4.791450	-0.007824	1.218884
40.397066	481.698163	4.796454	-0.007931	1.229303
40.738776	490.409366	4.801459	-0.008001	1.239569
41.211489	499.081683	4.806464	-0.008094	1.249732
42.224694	507.620832	4.811469	-0.008289	1.259764
42.187254	516.347409	4.816474	-0.008287	1.269728
42.336314	525.002619	4.821478	-0.008321	1.279570
43.179383	533.492495	4.826483	-0.008483	1.289282
43.649701	542.050174	4.831488	-0.008577	1.298926
44.132476	550.600295	4.836493	-0.008672	1.308493
44.549646	559.177725	4.841498	-0.008755	1.318009
45.325285	567.586124	4.846502	-0.008905	1.327337
45.456047	576.111614	4.851507	-0.008935	1.336610
45.697336	584.589703	4.856512	-0.008986	1.345788
46.805628	592.909953	4.861517	-0.009198	1.354890
47.290022	601.323080	4.866522	-0.009293	1.363918
47.272814	609.843564	4.871526	-0.009296	1.372912
47.978795	618.183271	4.876531	-0.009433	1.381784
48.520426	626.577909	4.881536	-0.009539	1.390628
48.986654	634.949183	4.886541	-0.009631	1.399379
49.537584	643.297227	4.891546	-0.009739	1.408066
50.335372	651.627274	4.896550	-0.009893	1.416723
50.877126	659.971683	4.901555	-0.010000	1.425298
51.617710	668.309092	4.906560	-0.010143	1.433848
52.144911	676.647720	4.911565	-0.010247	1.442313
52.843800	684.944210	4.916570	-0.010382	1.450714
53.262361	693.304033	4.921574	-0.010466	1.459084
53.610837	701.663333	4.926579	-0.010536	1.467394
54.323440	709.965460	4.931584	-0.010674	1.475660
54.945972	718.243863	4.936589	-0.010796	1.483841
55.173676	726.591195	4.941594	-0.010843	1.491982
56.128262	734.793680	4.946598	-0.011027	1.500054
56.728147	743.058439	4.951603	-0.011144	1.508086
56.446092	751.506429	4.956608	-0.011097	1.516113
56.850957	759.785901	4.961613	-0.011178	1.524044
57.633149	767.978083	4.966618	-0.011329	1.531909
58.103476	776.252188	4.971622	-0.011422	1.539763
58.973013	784.438758	4.976627	-0.011589	1.547556
59.388262	792.719290	4.981632	-0.011672	1.555329
59.309837	801.069158	4.986637	-0.011662	1.563052
59.530279	809.337392	4.991642	-0.011709	1.570707
59.995454	817.588635	4.996646	-0.011801	1.578346
60.271191	825.822289	5.001651	-0.011858	1.585904
61.582982	833.898158	5.006656	-0.012107	1.593434
61.775814	842.173181	5.011661	-0.012149	1.600945
61.975337	850.437779	5.016666	-0.012191	1.608413
62.175569	858.731536	5.021670	-0.012234	1.615873
62.014253	867.038087	5.026675	-0.012209	1.623257
62.829915	875.192223	5.031680	-0.012367	1.630613
63.135051	883.428194	5.036685	-0.012429	1.637934
63.450708	891.598201	5.041690	-0.012493	1.645167
64.051979	899.781448	5.046694	-0.012610	1.652420
64.510837	907.960583	5.051699	-0.012701	1.659617
65.049354	916.127415	5.056704	-0.012807	1.666783
65.475572	924.333609	5.061709	-0.012891	1.673937
65.585577	932.565898	5.066714	-0.012917	1.681039
66.646408	940.634256	5.071718	-0.013120	1.688101
66.888864	948.870615	5.076723	-0.013171	1.695165
67.068425	957.108727	5.081728	-0.013210	1.702193
66.858440	965.412979	5.086733	-0.013176	1.709196
67.458013	973.518077	5.091738	-0.013293	1.716110
67.730040	981.713225	5.096742	-0.013349	1.723029
68.295035	989.837702	5.101747	-0.013459	1.729899
68.940298	997.987539	5.106752	-0.013585	1.736774
69.552412	1006.132229	5.111757	-0.013704	1.743612
69.597653	1014.383577	5.116762	-0.013718	1.750438
69.813829	1022.588953	5.121766	-0.013764	1.757222
70.538436	1030.654221	5.126771	-0.013904	1.763931
71.005251	1038.820159	5.131776	-0.013996	1.770662
71.259633	1047.034325	5.136781	-0.014049	1.777381
71.918168	1055.129272	5.141786	-0.014177	1.784028
72.324567	1063.342957	5.146790	-0.014258	1.790715
72.378882	1071.556080	5.151795	-0.014274	1.797332
72.417640	1079.749325	5.156800	-0.014286	1.803907
72.718022	1087.908456	5.161805	-0.014347	1.810464
72.955120	1096.062506	5.166810	-0.014397	1.816985
73.154530	1104.217050	5.171814	-0.014439	1.823478
73.271632	1112.386304	5.176819	-0.014467	1.829949
74.163320	1120.415414	5.181824	-0.014638	1.836382
74.277663	1128.590801	5.186829	-0.014665	1.842812
74.640735	1136.722799	5.191834	-0.014738	1.849217
74.946881	1144.883484	5.196838	-0.014800	1.855614
75.369860	1152.989682	5.201843	-0.014884	1.861961
75.421464	1161.187992	5.206848	-0.014899	1.868314
75.532174	1169.372193	5.211853	-0.014925	1.874641
75.780795	1177.472986	5.216858	-0.014977	1.880898
76.180963	1185.590101	5.221862	-0.015056	1.887166
76.050869	1193.799331	5.226867	-0.015038	1.893421
76.544695	1201.862489	5.231872	-0.015135	1.899616
76.732731	1210.001248	5.236877	-0.015175	1.905814
76.782121	1218.174952	5.241882	-0.015190	1.912001
77.397813	1226.240707	5.246886	-0.015310	1.918152
77.658111	1234.351226	5.251891	-0.015363	1.924277
77.660855	1242.528714	5.256896	-0.015369	1.930403
78.449015	1250.559420	5.261901	-0.015521	1.936488
78.699254	1258.686623	5.266906	-0.015573	1.942566
79.262993	1266.791818	5.271910	-0.015684	1.948643
79.330537	1274.960581	5.276915	-0.015702	1.954693
79.285513	1283.121634	5.281920	-0.015698	1.960706
79.744913	1291.201963	5.286925	-0.015789	1.966697
80.269466	1299.252990	5.291930	-0.015892	1.972656
80.603416	1307.389481	5.296934	-0.015960	1.978638
80.490772	1315.552921	5.301939	-0.015944	1.984573
80.960826	1323.632123	5.306944	-0.016037	1.990492
80.922095	1331.827269	5.311949	-0.016035	1.996422
81.282675	1339.872069	5.316954	-0.016108	2.002269
81.646195	1347.984568	5.321958	-0.016181	2.008149
81.528138	1356.165750	5.326963	-0.016164	2.014009
82.067827	1364.224545	5.331968	-0.016270	2.019834
82.166844	1372.362549	5.336973	-0.016294	2.025652
82.155534	1380.513368	5.341978	-0.016297	2.031451
83.094069	1388.483147	5.346982	-0.016477	2.037205
83.181385	1396.605257	5.351987	-0.016498	2.042961
83.191921	1404.781629	5.356992	-0.016506	2.048731
83.863555	1412.811062	5.361997	-0.016636	2.054450
84.028824	1420.916297	5.367002	-0.016672	2.060154
84.598160	1428.985018	5.372006	-0.016783	2.065858
84.510938	1437.166555	5.377011	-0.016773	2.071557
84.832896	1445.237397	5.382016	-0.016838	2.077206
84.999546	1453.367171	5.387021	-0.016874	2.082865
85.197661	1461.455882	5.392026	-0.016916	2.088482
85.975751	1469.491211	5.397030	-0.017067	2.094107
86.364313	1477.581914	5.402035	-0.017144	2.099715
86.676068	1485.682295	5.407040	-0.017208	2.105307
86.613492	1493.893800	5.412045	-0.017201	2.110923
87.195386	1501.929925	5.417050	-0.017315	2.116468
87.608522	1510.004247	5.422054	-0.017397	2.122008
87.649529	1518.117966	5.427059	-0.017410	2.127523
87.816085	1526.239259	5.432064	-0.017447	2.133042
88.304912	1534.302601	5.437069	-0.017543	2.138538
88.223542	1542.425439	5.442074	-0.017533	2.144005
88.348636	1550.554824	5.447078	-0.017562	2.149483
88.549865	1558.629552	5.452083	-0.017604	2.154917
88.541179	1566.753096	5.457088	-0.017608	2.160350
89.052018	1574.773900	5.462093	-0.017709	2.165751
89.594258	1582.807106	5.467098	-0.017815	2.171149
89.696437	1590.960602	5.472102	-0.017839	2.176572
90.300314	1598.955044	5.477107	-0.017957	2.181923
90.366875	1607.103200	5.482112	-0.017975	2.187312
90.415802	1615.259560	5.487117	-0.017989	2.192692
90.763140	1623.283259	5.492122	-0.018059	2.197999
90.910468	1631.360978	5.497126	-0.018092	2.203310
90.944066	1639.486380	5.502131	-0.018103	2.208629
91.517678	1647.508731	5.507136	-0.018215	2.213918
91.693232	1655.618984	5.512141	-0.018253	2.219214
91.732571	1663.706151	5.517146	-0.018266	2.224470
91.977411	1671.835610	5.522150	-0.018317	2.229760
92.064625	1679.910301	5.527155	-0.018339	2.234988
92.674590	1687.911084	5.532160	-0.018457	2.240204
93.089852	1695.961461	5.537165	-0.018540	2.245421
93.566741	1704.041468	5.542170	-0.018634	2.250651
94.099440	1712.100600	5.547174	-0.018739	2.255860
94.026469	1720.235562	5.552179	-0.018730	2.261051
94.540955	1728.299799	5.557184	-0.018831	2.266237
94.597617	1736.454346	5.562189	-0.018847	2.271429
94.648390	1744.545428	5.567194	-0.018862	2.276568
94.822284	1752.626615	5.572198	-0.018900	2.281700
95.143806	1760.653436	5.577203	-0.018965	2.286798
95.009544	1768.792102	5.582208	-0.018945	2.291916
95.092373	1776.884530	5.587213	-0.018966	2.297013
95.534552	1784.892522	5.592218	-0.019054	2.302076
95.672578	1792.970691	5.597222	-0.019085	2.307146
95.958677	1801.041321	5.602227	-0.019143	2.312213
96.455427	1809.047718	5.607232	-0.019241	2.317246
96.991886	1817.065415	5.612237	-0.019346	2.322279
96.630270	1825.242812	5.617242	-0.019284	2.327324
96.934049	1833.325806	5.622246	-0.019346	2.332356
97.643371	1841.315583	5.627251	-0.019483	2.337353
98.196756	1849.340219	5.632256	-0.019592	2.342348
98.357312	1857.459615	5.637261	-0.019627	2.347358
98.550382	1865.543183	5.642266	-0.019668	2.352337
98.860175	1873.627626	5.647270	-0.019731	2.357317
98.970455	1881.697208	5.652275	-0.019757	2.362260
98.616883	1889.874392	5.657280	-0.019696	2.367220
98.964854	1897.915680	5.662285	-0.019767	2.372145
99.174627	1905.966908	5.667290	-0.019811	2.377054
99.537975	1914.014180	5.672294	-0.019884	2.381963
99.887784	1922.045015	5.677299	-0.019954	2.386851
100.122031	1930.119256	5.682304	-0.020003	2.391746
100.294206	1938.201183	5.687309	-0.020040	2.396630
100.781474	1946.210621	5.692314	-0.020136	2.401486
101.127280	1954.279276	5.697318	-0.020206	2.406356
101.105525	1962.418452	5.702323	-0.020207	2.411229
101.369222	1970.471077	5.707328	-0.020262	2.416064
101.571909	1978.565191	5.712333	-0.020305	2.420908
101.692402	1986.605787	5.717338	-0.020333	2.425705
101.803192	1994.737316	5.722342	-0.020359	2.430545
102.304194	2002.758147	5.727347	-0.020457	2.435341
102.532842	2010.796440	5.732352	-0.020505	2.440116
102.782128	2018.847637	5.737357	-0.020557	2.444891
102.860187	2026.942453	5.742362	-0.020577	2.449669
103.592284	2034.916743	5.747366	-0.020718	2.454417
103.176463	2043.088823	5.752371	-0.020646	2.459184
103.407642	2051.124301	5.757376	-0.020694	2.463911
103.644581	2059.189037	5.762381	-0.020744	2.468646
104.106499	2067.186328	5.767386	-0.020835	2.473351
104.271495	2075.276191	5.772390	-0.020871	2.478077
104.411820	2083.337297	5.777395	-0.020903	2.482776
104.605154	2091.401724	5.782400	-0.020944	2.487472
105.178996	2099.436671	5.787405	-0.021056	2.492171
105.290534	2107.507744	5.792410	-0.021082	2.496847
105.719678	2115.542375	5.797414	-0.021167	2.501517
105.651947	2123.639835	5.802419	-0.021160	2.506177
105.641035	2131.778105	5.807424	-0.021163	2.510856
106.378683	2139.756921	5.812429	-0.021306	2.515491
107.011052	2147.700194	5.817434	-0.021429	2.520088
107.195721	2155.799859	5.822438	-0.021468	2.524734
107.379280	2163.885696	5.827443	-0.021508	2.529363
107.105971	2172.054126	5.832448	-0.021462	2.533997
107.702359	2180.039720	5.837453	-0.021579	2.538582
107.957282	2188.052632	5.842458	-0.021631	2.543150
108.518142	2196.102905	5.847462	-0.021741	2.547752
108.559805	2204.210571	5.852467	-0.021754	2.552341
108.392159	2212.315913	5.857472	-0.021728	2.556906
108.622380	2220.382063	5.862477	-0.021777	2.561468
109.182927	2228.306493	5.867482	-0.021886	2.565967
109.316549	2236.452820	5.872486	-0.021916	2.570552
109.433884	2244.499641	5.877491	-0.021943	2.575071
109.605827	2252.563799	5.882496	-0.021981	2.579596
109.986182	2260.574149	5.887501	-0.022057	2.584098
110.227873	2268.649316	5.892506	-0.022107	2.588619
110.687124	2276.803886	5.897510	-0.022198	2.593191
110.855447	2284.835806	5.902515	-0.022235	2.597666
111.410656	2292.805363	5.907520	-0.022343	2.602126
111.452706	2300.879422	5.912525	-0.022356	2.606600
111.656116	2308.918304	5.917530	-0.022400	2.611058
111.806181	2316.985106	5.922534	-0.022433	2.615521
111.900399	2325.038462	5.927539	-0.022456	2.619964
112.197686	2333.060012	5.932544	-0.022516	2.624397
112.317473	2341.151034	5.937549	-0.022544	2.628848
113.039929	2349.098684	5.942554	-0.022684	2.633254
112.960684	2357.228040	5.947558	-0.022674	2.637697
113.268702	2365.248903	5.952563	-0.022737	2.642100
113.671710	2373.274998	5.957568	-0.022817	2.646504
113.890993	2381.359840	5.962573	-0.022863	2.650921
114.199135	2389.412833	5.967578	-0.022926	2.655319
114.696055	2397.426421	5.972582	-0.023024	2.659701
115.146694	2405.451734	5.977587	-0.023113	2.664079
115.226504	2413.538454	5.982592	-0.023133	2.668459
115.384856	2421.651435	5.987597	-0.023168	2.672850
115.191558	2429.731725	5.992602	-0.023137	2.677193
115.509019	2437.756695	5.997606	-0.023202	2.681534
115.527664	2445.818596	6.002611	-0.023210	2.685867
115.651509	2453.861479	6.007616	-0.023239	2.690190
115.442083	2462.009905	6.012621	-0.023205	2.694541
115.707481	2469.992094	6.017626	-0.023260	2.698827
116.354520	2477.941366	6.022630	-0.023385	2.703113
116.584327	2486.009920	6.027635	-0.023433	2.707429
117.107084	2494.010819	6.032640	-0.023536	2.711721
117.235797	2502.107616	6.037645	-0.023565	2.716031
117.404823	2510.131219	6.042650	-0.023602	2.720299
117.744392	2518.175885	6.047654	-0.023671	2.724581
117.843623	2526.256416	6.052659	-0.023694	2.728861
117.904960	2534.336496	6.057664	-0.023711	2.733131
117.965988	2542.415071	6.062669	-0.023728	2.737394
118.259533	2550.424433	6.067674	-0.023788	2.741628
118.594840	2558.447903	6.072678	-0.023855	2.745866
118.581872	2566.552317	6.077683	-0.023858	2.750118
118.784323	2574.622146	6.082688	-0.023901	2.754359
119.082031	2582.609591	6.087693	-0.023962	2.758556
119.273843	2590.620155	6.092698	-0.024003	2.762752
119.680851	2598.660044	6.097702	-0.024084	2.766970
119.949056	2606.712067	6.102707	-0.024139	2.771179
120.157381	2614.754123	6.107712	-0.024183	2.775373
121.119881	2622.712901	6.112717	-0.024368	2.779564
120.894680	2630.806013	6.117722	-0.024331	2.783745
120.690373	2638.958821	6.122726	-0.024298	2.787952
120.654804	2647.042368	6.127731	-0.024297	2.792128
120.969106	2655.052811	6.132736	-0.024361	2.796280
121.434056	2663.035290	6.137741	-0.024453	2.800421
121.792705	2671.017977	6.142746	-0.024525	2.804550
121.763592	2679.146634	6.147750	-0.024525	2.808724
121.888438	2687.199413	6.152755	-0.024553	2.812862
121.829327	2695.261104	6.157760	-0.024548	2.816988
122.546251	2703.251291	6.162765	-0.024686	2.821117
122.427930	2711.313611	6.167770	-0.024670	2.825228
122.495513	2719.390628	6.172774	-0.024687	2.829350
123.126816	2727.374533	6.177779	-0.024810	2.833453
123.767308	2735.353334	6.182784	-0.024935	2.837548
123.622938	2743.466298	6.187789	-0.024913	2.841658
123.568727	2751.516496	6.192794	-0.024908	2.845737
124.298852	2759.485225	6.197798	-0.025050	2.849813
124.216910	2767.591462	6.202803	-0.025040	2.853907
124.716753	2775.563617	6.207808	-0.025138	2.857960
125.175060	2783.594875	6.212813	-0.025228	2.862035
125.105341	2791.715956	6.217818	-0.025221	2.866119
125.648496	2799.731074	6.222822	-0.025327	2.870178
125.666013	2807.796946	6.227827	-0.025336	2.874228
125.809690	2815.854935	6.232832	-0.025368	2.878275
126.455831	2823.828839	6.237837	-0.025493	2.882303
126.493176	2831.899853	6.242842	-0.025506	2.886339
127.068307	2839.925978	6.247846	-0.025618	2.890377
126.869528	2848.052582	6.252851	-0.025586	2.894416
127.256520	2856.054988	6.257856	-0.025664	2.898421
127.719738	2864.053221	6.262861	-0.025755	2.902422
127.712502	2872.129242	6.267866	-0.025759	2.906430
127.929285	2880.228579	6.272870	-0.025805	2.910457
128.091464	2888.292328	6.277875	-0.025840	2.914457
128.275224	2896.305436	6.282880	-0.025880	2.918428
128.334031	2904.359905	6.287885	-0.025896	2.922407
128.322616	2912.379942	6.292890	-0.025899	2.926360
128.687853	2920.396408	6.297894	-0.025972	2.930326
128.891282	2928.445002	6.302899	-0.026016	2.934293
128.532964	2936.539227	6.307904	-0.025954	2.938248
129.014364	2944.488596	6.312909	-0.026049	2.942171
129.673565	2952.466300	6.317914	-0.026177	2.946113
129.865752	2960.579145	6.322918	-0.026218	2.950090
130.042411	2968.592787	6.327923	-0.026256	2.954012
130.027219	2976.666352	6.332928	-0.026259	2.957949
130.695352	2984.644639	6.337933	-0.026388	2.961870
130.579006	2992.722562	6.342938	-0.026372	2.965792
130.800250	3000.771187	6.347942	-0.026419	2.969713
131.326550	3008.762670	6.352947	-0.026522	2.973617
131.794241	3016.759043	6.357952	-0.026614	2.977515
132.362604	3024.791422	6.362957	-0.026725	2.981431
132.462986	3032.865168	6.367962	-0.026749	2.985337
132.805698	3040.913712	6.372966	-0.026818	2.989238
132.828813	3049.000869	6.377971	-0.026828	2.993136
133.096784	3057.030092	6.382976	-0.026883	2.997014
133.277344	3065.081835	6.387981	-0.026922	3.000893
133.458678	3073.065915	6.392986	-0.026961	3.004735
133.825490	3081.100457	6.397990	-0.027035	3.008605
134.393858	3089.109045	6.402995	-0.027146	3.012468
134.167279	3097.229166	6.408000	-0.027109	3.016339
134.178527	3105.300974	6.413005	-0.027116	3.020194
134.377310	3113.262345	6.418010	-0.027158	3.024001
134.978335	3121.281792	6.423014	-0.027276	3.027851
135.039264	3129.366207	6.428019	-0.027292	3.031700
135.226596	3137.406836	6.433024	-0.027332	3.035529
135.628254	3145.395659	6.438029	-0.027412	3.039340
135.674285	3153.417590	6.443034	-0.027426	3.043144
136.049893	3161.453966	6.448038	-0.027502	3.046966
136.207534	3169.549228	6.453043	-0.027536	3.050801
136.194648	3177.589207	6.458048	-0.027539	3.054596
136.467780	3185.625920	6.463053	-0.027595	3.058399
136.650202	3193.624516	6.468058	-0.027634	3.062174
137.429666	3201.632156	6.473062	-0.027785	3.065979
137.415882	3209.719120	6.478067	-0.027788	3.069777
137.233436	3217.846209	6.483072	-0.027759	3.073581
137.849195	3225.802813	6.488077	-0.027879	3.077340
137.798483	3233.867566	6.493082	-0.027875	3.081112
137.846899	3241.896560	6.498086	-0.027889	3.084867
137.878368	3249.932428	6.503091	-0.027900	3.088620
137.989839	3257.985298	6.508096	-0.027926	3.092381
138.178013	3266.017381	6.513101	-0.027966	3.096131
138.957354	3273.921687	6.518106	-0.028117	3.099845
139.290430	3281.968786	6.523110	-0.028184	3.103599
139.244152	3290.061718	6.528115	-0.028181	3.107352
139.423378	3298.131406	6.533120	-0.028219	3.111101
140.090409	3306.076450	6.538125	-0.028349	3.114810
140.233226	3314.118130	6.543130	-0.028381	3.118535
140.264596	3322.223375	6.548134	-0.028392	3.122280
140.554608	3330.242550	6.553139	-0.028451	3.125992
140.881176	3338.218236	6.558144	-0.028517	3.129682
141.177469	3346.280543	6.563149	-0.028578	3.133405
140.839194	3354.393073	6.568154	-0.028520	3.137118
141.796705	3362.302446	6.573158	-0.028703	3.140793
141.873963	3370.365980	6.578163	-0.028723	3.144494
141.832666	3378.461782	6.583168	-0.028721	3.148200
142.216518	3386.489332	6.588173	-0.028798	3.151889
142.257111	3394.530466	6.593178	-0.028810	3.155565
142.308174	3402.536844	6.598182	-0.028825	3.159221
143.137319	3410.470830	6.603187	-0.028985	3.162875
143.199749	3418.545619	6.608192	-0.029002	3.166555
143.377193	3426.634314	6.613197	-0.029040	3.170241
143.428087	3434.666558	6.618202	-0.029055	3.173892
143.582582	3442.747495	6.623206	-0.029089	3.177565
143.902117	3450.763817	6.628211	-0.029154	3.181212
144.076793	3458.760179	6.633216	-0.029191	3.184840
144.830415	3466.770810	6.638221	-0.029337	3.188495
145.012278	3474.805828	6.643226	-0.029376	3.192132
145.211462	3482.873355	6.648230	-0.029419	3.195780
145.405359	3490.857129	6.653235	-0.029460	3.199386
145.528937	3498.890127	6.658240	-0.029488	3.203007
145.581740	3506.994701	6.663245	-0.029503	3.206653
146.168157	3514.936106	6.668250	-0.029618	3.210244
146.433566	3522.989980	6.673254	-0.029672	3.213868
146.320916	3531.093527	6.678259	-0.029657	3.217494
146.234047	3539.144369	6.683264	-0.029646	3.221093
146.717163	3547.116195	6.688269	-0.029741	3.224678
147.002915	3555.143933	6.693274	-0.029800	3.228275
147.219563	3563.199253	6.698278	-0.029845	3.231877
147.718929	3571.176538	6.703283	-0.029943	3.235452
147.636029	3579.223681	6.708288	-0.029933	3.239030
148.003699	3587.252546	6.713293	-0.030007	3.242615
148.352014	3595.264877	6.718298	-0.030077	3.246187
148.430914	3603.327073	6.723302	-0.030097	3.249767
148.681357	3611.360230	6.728307	-0.030149	3.253336
149.074227	3619.386163	6.733312	-0.030227	3.256905
149.222296	3627.435527	6.738317	-0.030260	3.260469
149.620035	3635.376389	6.743322	-0.030340	3.263993
149.854041	3643.465210	6.748326	-0.030388	3.267570
150.012997	3651.521793	6.753331	-0.030423	3.271127
150.437111	3659.524303	6.758336	-0.030508	3.274667
150.596188	3667.568754	6.763341	-0.030542	3.278210
150.396682	3675.622410	6.768346	-0.030511	3.281739
151.119969	3683.576063	6.773350	-0.030650	3.285258
151.467737	3691.613782	6.778355	-0.030721	3.288795
151.761478	3699.668146	6.783360	-0.030780	3.292333
152.020662	3707.745205	6.788365	-0.030834	3.295875
152.372553	3715.712491	6.793370	-0.030905	3.299370
152.726574	3723.737600	6.798374	-0.030976	3.302886
152.966396	3731.789002	6.803379	-0.031026	3.306405
153.185406	3739.824454	6.808384	-0.031072	3.309912
153.499940	3747.907282	6.813389	-0.031136	3.313440
153.404778	3755.936013	6.818394	-0.031123	3.316925
154.179477	3763.890324	6.823398	-0.031273	3.320408
154.374445	3771.904857	6.828403	-0.031314	3.323891
154.338704	3779.958726	6.833408	-0.031313	3.327378
154.410351	3788.061218	6.838413	-0.031332	3.330886
154.560909	3796.080678	6.843418	-0.031365	3.334358
154.767095	3804.127484	6.848422	-0.031409	3.337840
154.557755	3812.224886	6.853427	-0.031375	3.341325
155.075641	3820.135510	6.858432	-0.031477	3.344753
155.257219	3828.203352	6.863437	-0.031516	3.348233
155.836403	3836.152956	6.868442	-0.031629	3.351673
155.899332	3844.249687	6.873446	-0.031646	3.355153
156.158778	3852.233444	6.878451	-0.031699	3.358588
156.491800	3860.251103	6.883456	-0.031767	3.362038
156.869359	3868.291493	6.888461	-0.031842	3.365495
156.848231	3876.339451	6.893466	-0.031844	3.368936
157.126104	3884.387800	6.898470	-0.031901	3.372386
156.896801	3892.481404	6.903475	-0.031863	3.375832
157.482536	3900.408304	6.908480	-0.031978	3.379234
157.666741	3908.451632	6.913485	-0.032017	3.382667
157.671587	3916.515080	6.918490	-0.032023	3.386099
158.167985	3924.520759	6.923494	-0.032121	3.389521
158.272846	3932.620725	6.928499	-0.032146	3.392965
158.302229	3940.664789	6.933504	-0.032157	3.396379
158.489295	3948.635641	6.938509	-0.032197	3.399764
158.649023	3956.628676	6.943514	-0.032232	3.403154
159.042429	3964.654858	6.948518	-0.032310	3.406563
159.163853	3972.685832	6.953523	-0.032338	3.409961
159.190789	3980.714415	6.958528	-0.032348	3.413351
159.311141	3988.804553	6.963533	-0.032376	3.416767
159.569921	3996.768807	6.968538	-0.032430	3.420132
159.664394	4004.805368	6.973542	-0.032452	3.423518
159.939402	4012.841419	6.978547	-0.032509	3.426907
160.238018	4020.861269	6.983552	-0.032570	3.430286
160.482619	4028.872117	6.988557	-0.032621	3.433656
160.398275	4036.942311	6.993562	-0.032610	3.437036
160.808279	4044.934420	6.998566	-0.032692	3.440398
161.126878	4052.926477	7.003571	-0.032756	3.443753
161.432096	4060.968697	7.008576	-0.032818	3.447125
162.076861	4069.006521	7.013581	-0.032944	3.450503
161.948667	4077.052776	7.018586	-0.032925	3.453855
161.982644	4085.124153	7.023590	-0.032937	3.457220
162.114574	4093.169850	7.028595	-0.032967	3.460575
162.295308	4101.100765	7.033600	-0.033006	3.463879
162.195115	4109.230724	7.038605	-0.032992	3.467254
162.192652	4117.252986	7.043610	-0.032997	3.470585
163.150687	4125.132389	7.048614	-0.033181	3.473885
163.468102	4133.181880	7.053619	-0.033245	3.477231
163.518018	4141.239091	7.058624	-0.033260	3.480568
163.914610	4149.226921	7.063629	-0.033339	3.483884
164.406305	4157.217903	7.068634	-0.033435	3.487202
164.554150	4165.316310	7.073638	-0.033468	3.490549
164.800255	4173.342712	7.078643	-0.033519	3.493867
164.806979	4181.382397	7.083648	-0.033526	3.497179
164.716692	4189.489076	7.088653	-0.033514	3.500512
165.065473	4197.439295	7.093658	-0.033585	3.503793
165.589192	4205.472185	7.098662	-0.033687	3.507110
165.990267	4213.492978	7.103667	-0.033767	3.510414
166.001973	4221.542435	7.108672	-0.033775	3.513715
166.284712	4229.559011	7.113677	-0.033833	3.517008
166.323656	4237.584883	7.118682	-0.033845	3.520293
166.440227	4245.587732	7.123686	-0.033872	3.523569
166.961194	4253.602338	7.128691	-0.033974	3.526859
167.369315	4261.619721	7.133696	-0.034056	3.530144
167.678452	4269.683898	7.138701	-0.034119	3.533441
167.754034	4277.694937	7.143706	-0.034138	3.536706
168.099081	4285.757759	7.148710	-0.034207	3.539998
168.101102	4293.774897	7.153715	-0.034213	3.543258
168.209505	4301.817359	7.158720	-0.034239	3.546528
168.546098	4309.840493	7.163725	-0.034307	3.549794
168.812029	4317.887392	7.168730	-0.034361	3.553064
168.950589	4325.947738	7.173734	-0.034392	3.556334
169.208989	4333.900668	7.178739	-0.034446	3.559560
169.516738	4341.878810	7.183744	-0.034508	3.562795
169.579891	4349.952540	7.188749	-0.034525	3.566058
169.801789	4357.911759	7.193754	-0.034572	3.569277
170.004711	4365.992810	7.198758	-0.034615	3.572541
169.960043	4374.086074	7.203763	-0.034612	3.575800
170.273437	4381.996784	7.208768	-0.034676	3.578993
170.451305	4390.061595	7.213773	-0.034714	3.582241
170.584078	4398.072658	7.218778	-0.034744	3.585463
171.109403	4406.050790	7.223782	-0.034847	3.588681
171.449509	4414.125678	7.228787	-0.034916	3.591929
171.786337	4422.141234	7.233792	-0.034984	3.595151
171.957655	4430.153770	7.238797	-0.035021	3.598363
171.849761	4438.197305	7.243802	-0.035006	3.601576
172.284515	4446.191578	7.248806	-0.035092	3.604783
172.499173	4454.242995	7.253811	-0.035137	3.608004
172.914967	4462.283835	7.258816	-0.035220	3.611223
172.836976	4470.354035	7.263821	-0.035211	3.614436
173.219473	4478.342113	7.268826	-0.035287	3.617627
173.635629	4486.380522	7.273830	-0.035370	3.620837
173.681679	4494.378433	7.278835	-0.035384	3.624017
173.610618	4502.478397	7.283840	-0.035376	3.627231
173.701245	4510.536066	7.288845	-0.035398	3.630430
173.920672	4518.486030	7.293850	-0.035444	3.633587
174.556343	4526.457320	7.298854	-0.035568	3.636762
175.078554	4534.464513	7.303859	-0.035670	3.639945
174.991615	4542.482915	7.308864	-0.035659	3.643112
175.295332	4550.535031	7.313869	-0.035721	3.646301
175.603107	4558.535481	7.318874	-0.035784	3.649467
175.547546	4566.638448	7.323878	-0.035779	3.652660
176.021604	4574.668298	7.328883	-0.035872	3.655836
176.263667	4582.640732	7.333888	-0.035923	3.658981
176.287807	4590.689445	7.338893	-0.035932	3.662146
176.487223	4598.690741	7.343898	-0.035975	3.665295
176.779185	4606.718016	7.348902	-0.036034	3.668455
176.949923	4614.787862	7.353907	-0.036072	3.671624
177.168276	4622.749081	7.358912	-0.036117	3.674750
177.428330	4630.779708	7.363917	-0.036171	3.677901
177.650403	4638.815976	7.368922	-0.036218	3.681051
177.862739	4646.808763	7.373926	-0.036263	3.684181
177.794311	4654.890097	7.378931	-0.036255	3.687335
178.143797	4662.889696	7.383936	-0.036325	3.690466
178.369581	4670.947153	7.388941	-0.036373	3.693613
178.409009	4678.976962	7.393946	-0.036385	3.696742
178.660866	4687.010422	7.398950	-0.036438	3.699875
179.152946	4694.973519	7.403955	-0.036534	3.702985
178.924519	4703.049211	7.408960	-0.036497	3.706117
179.352880	4711.047236	7.413965	-0.036582	3.709233
179.523996	4719.106478	7.418970	-0.036619	3.712363
179.997462	4727.125794	7.423974	-0.036713	3.715483
179.917997	4735.149410	7.428979	-0.036703	3.718588
180.236319	4743.137921	7.433984	-0.036768	3.721687
180.635134	4751.115784	7.438989	-0.036847	3.724781
180.597452	4759.159233	7.443994	-0.036846	3.727887
181.148949	4767.178649	7.448998	-0.036954	3.730996
181.122344	4775.249468	7.454003	-0.036954	3.734107
181.622422	4783.217931	7.459008	-0.037052	3.737190
181.716198	4791.304119	7.464013	-0.037075	3.740305
181.928318	4799.317120	7.469018	-0.037120	3.743392
182.291985	4807.348129	7.474022	-0.037193	3.746488
182.615420	4815.335684	7.479027	-0.037258	3.749563
182.969985	4823.354800	7.484032	-0.037329	3.752648
183.133457	4831.427194	7.489037	-0.037365	3.755747
183.426482	4839.345543	7.494042	-0.037425	3.758787
183.808790	4847.383876	7.499046	-0.037501	3.761873
184.149021	4855.422684	7.504051	-0.037570	3.764955
184.355402	4863.432602	7.509056	-0.037614	3.768021
184.370005	4871.541466	7.514061	-0.037622	3.771117
184.661854	4879.488842	7.519066	-0.037681	3.774156
185.031544	4887.546843	7.524070	-0.037755	3.777236
185.295636	4895.542769	7.529075	-0.037810	3.780287
185.653773	4903.548423	7.534080	-0.037882	3.783342
185.847170	4911.630133	7.539085	-0.037923	3.786420
185.911371	4919.632823	7.544090	-0.037940	3.789461
185.907679	4927.688149	7.549094	-0.037945	3.792519
186.151219	4935.743761	7.554099	-0.037996	3.795580
186.629858	4943.647288	7.559104	-0.038090	3.798587
186.694416	4951.720458	7.564109	-0.038107	3.801645
186.720996	4959.708389	7.569114	-0.038117	3.804668
187.283766	4967.744324	7.574118	-0.038228	3.807719
187.529914	4975.792161	7.579123	-0.038279	3.810765
187.696698	4983.738005	7.584128	-0.038315	3.813768
188.037496	4991.869311	7.589133	-0.038384	3.816843
188.215988	4999.872071	7.594138	-0.038422	3.819863
188.242077	5007.895376	7.599142	-0.038432	3.822885
188.291936	5015.957660	7.604147	-0.038447	3.825919
188.692561	5023.904929	7.609152	-0.038527	3.828916
188.979861	5031.984235	7.614157	-0.038586	3.831957
189.001763	5039.995125	7.619162	-0.038595	3.834965
189.531937	5047.998952	7.624166	-0.038699	3.837978
189.747429	5056.047836	7.629171	-0.038744	3.841000
189.980285	5063.986206	7.634176	-0.038793	3.843977
190.311871	5072.073644	7.639181	-0.038860	3.847011
190.405719	5080.090418	7.644186	-0.038883	3.850010
190.455529	5088.162868	7.649190	-0.038897	3.853027
190.558193	5096.216859	7.654195	-0.038922	3.856035
190.556130	5104.214574	7.659200	-0.038926	3.859019
191.054340	5112.185525	7.664205	-0.039024	3.862000
191.195244	5120.190045	7.669210	-0.039056	3.864984
191.763324	5128.205795	7.674214	-0.039167	3.867979
191.606466	5136.323874	7.679219	-0.039143	3.870994
191.735807	5144.398363	7.684224	-0.039173	3.873997
192.081038	5152.386214	7.689229	-0.039242	3.876970
192.770808	5160.256545	7.694234	-0.039376	3.879904
193.023093	5168.287452	7.699238	-0.039428	3.882886
193.090296	5176.356928	7.704243	-0.039446	3.885876
193.500235	5184.292875	7.709248	-0.039527	3.888822
193.907030	5192.397346	7.714253	-0.039608	3.891827
194.134376	5200.393958	7.719258	-0.039656	3.894787
194.517939	5208.380528	7.724262	-0.039733	3.897744
194.940870	5216.421960	7.729267	-0.039817	3.900719
195.134154	5224.397587	7.734272	-0.039858	3.903664
195.509415	5232.469433	7.739277	-0.039933	3.906645
195.621049	5240.483046	7.744282	-0.039959	3.909597
195.825419	5248.562276	7.749286	-0.040002	3.912573
195.791777	5256.562886	7.754291	-0.040001	3.915513
196.139627	5264.550679	7.759296	-0.040071	3.918454
196.370081	5272.621555	7.764301	-0.040120	3.921420
196.670020	5280.555266	7.769306	-0.040181	3.924336
196.837042	5288.661466	7.774310	-0.040217	3.927309
196.978974	5296.667747	7.779315	-0.040249	3.930244
197.115757	5304.704252	7.784320	-0.040280	3.933187
197.632734	5312.736231	7.789325	-0.040381	3.936133
197.529330	5320.731756	7.794330	-0.040367	3.939052
197.798290	5328.766766	7.799334	-0.040422	3.941991
198.252208	5336.727206	7.804339	-0.040512	3.944903
198.358848	5344.760574	7.809344	-0.040537	3.947834
198.370268	5352.854613	7.814349	-0.040545	3.950782
198.271948	5360.909732	7.819354	-0.040532	3.953712
198.909638	5368.872950	7.824358	-0.040656	3.956620
199.017919	5376.886530	7.829363	-0.040681	3.959535
199.561762	5384.851228	7.834368	-0.040788	3.962437
199.906760	5392.894049	7.839373	-0.040857	3.965362
199.796090	5400.918596	7.844378	-0.040842	3.968270
200.043872	5409.019741	7.849382	-0.040893	3.971210
200.650300	5416.970165	7.854387	-0.041011	3.974100
200.669636	5424.984422	7.859392	-0.041020	3.977000
200.802970	5433.033430	7.864397	-0.041050	3.979912
201.096268	5441.000949	7.869402	-0.041110	3.982796
201.538070	5449.039718	7.874406	-0.041198	3.985706
201.520737	5457.111439	7.879411	-0.041200	3.988618
201.647640	5465.149080	7.884416	-0.041229	3.991517
201.986189	5473.092146	7.889421	-0.041297	3.994385
202.357205	5481.093286	7.894426	-0.041371	3.997271
202.275598	5489.178691	7.899430	-0.041361	4.000178
202.782671	5497.120832	7.904435	-0.041461	4.003042
202.817507	5505.208911	7.909440	-0.041473	4.005947
203.150835	5513.210316	7.914445	-0.041540	4.008825
203.390537	5521.236005	7.919450	-0.041590	4.011707
203.554410	5529.265066	7.924454	-0.041626	4.014588
203.643860	5537.292144	7.929459	-0.041648	4.017464
204.152416	5545.263444	7.934464	-0.041748	4.020325
204.421945	5553.278025	7.939469	-0.041803	4.023196
204.902495	5561.290370	7.944474	-0.041898	4.026067
204.777023	5569.326264	7.949478	-0.041880	4.028935
205.080280	5577.419798	7.954483	-0.041942	4.031828
205.387198	5585.448172	7.959488	-0.042004	4.034696
205.668370	5593.452021	7.964493	-0.042062	4.037552
205.363640	5601.475230	7.969498	-0.042010	4.040404
205.358215	5609.475474	7.974502	-0.042014	4.043251
205.834926	5617.477124	7.979507	-0.042108	4.046104
205.482293	5625.496483	7.984512	-0.042048	4.048948
206.538104	5633.487222	7.989517	-0.042250	4.051802
206.751267	5641.482931	7.994522	-0.042295	4.054642
207.001212	5649.561103	7.999526	-0.042347	4.057511
206.970156	5657.594072	8.004531	-0.042346	4.060356
207.481581	5665.539091	8.009536	-0.042447	4.063177
207.727161	5673.644508	8.014541	-0.042498	4.066049
207.391418	5681.684864	8.019546	-0.042440	4.068886
207.671613	5689.690669	8.024550	-0.042498	4.071719
207.883468	5697.693632	8.029555	-0.042543	4.074548
208.377219	5705.658243	8.034560	-0.042640	4.077366
208.682701	5713.737632	8.039565	-0.042702	4.080219
208.341056	5721.787499	8.044570	-0.042644	4.083050
208.367491	5729.809437	8.049574	-0.042654	4.085875
208.960573	5737.755279	8.054579	-0.042769	4.088679
209.128102	5745.810023	8.059584	-0.042806	4.091514
209.422606	5753.792220	8.064589	-0.042866	4.094323
209.634352	5761.826176	8.069594	-0.042911	4.097147
209.824186	5769.863121	8.074598	-0.042951	4.099969
210.118182	5777.900497	8.079603	-0.043011	4.102791
210.209990	5785.875195	8.084608	-0.043034	4.105587
210.384639	5793.946532	8.089613	-0.043072	4.108415
211.025312	5801.985784	8.094618	-0.043196	4.111237
210.970410	5809.952742	8.099622	-0.043191	4.114022
210.699297	5818.083073	8.104627	-0.043146	4.116859
210.479936	5826.045993	8.109632	-0.043110	4.119636
211.393774	5833.974291	8.114637	-0.043286	4.122416
211.740710	5841.938929	8.119642	-0.043356	4.125198
211.672088	5850.023231	8.124646	-0.043348	4.128014
212.196283	5858.069961	8.129651	-0.043451	4.130823
212.286012	5866.062230	8.134656	-0.043473	4.133605
212.564189	5874.120839	8.139661	-0.043530	4.136411
213.015379	5882.052512	8.144666	-0.043619	4.139174
213.215930	5890.126156	8.149670	-0.043662	4.141980
213.201870	5898.153310	8.154675	-0.043665	4.144765
213.412349	5906.160177	8.159680	-0.043709	4.147545
214.026808	5914.211227	8.164685	-0.043829	4.150343
214.259032	5922.165195	8.169690	-0.043877	4.153101
214.289759	5930.255758	8.174694	-0.043888	4.155901
214.434818	5938.270766	8.179699	-0.043920	4.158675
214.773760	5946.281265	8.184704	-0.043989	4.161448
214.980977	5954.224370	8.189709	-0.044033	4.164194
215.362733	5962.285817	8.194714	-0.044109	4.166982
215.770293	5970.287597	8.199718	-0.044190	4.169747
215.739535	5978.369732	8.204723	-0.044190	4.172532
215.791003	5986.395349	8.209728	-0.044205	4.175297
216.239731	5994.416529	8.214733	-0.044293	4.178064
216.352291	6002.442564	8.219738	-0.044320	4.180827
216.592263	6010.421268	8.224742	-0.044370	4.183572
216.833624	6018.474359	8.229747	-0.044420	4.186342
217.052681	6026.455446	8.234752	-0.044466	4.189085
217.329642	6034.554525	8.239757	-0.044523	4.191867
217.549553	6042.553612	8.244762	-0.044569	4.194612
217.618716	6050.583319	8.249766	-0.044587	4.197364
217.864966	6058.572092	8.254771	-0.044638	4.200102
218.257480	6066.523750	8.259776	-0.044716	4.202828
218.559725	6074.599804	8.264781	-0.044778	4.205593
218.688609	6082.572947	8.269786	-0.044807	4.208319
218.911229	6090.621320	8.274790	-0.044854	4.211070
219.055316	6098.614546	8.279795	-0.044886	4.213800
219.549082	6106.657226	8.284800	-0.044983	4.216548
219.700094	6114.685566	8.289805	-0.045017	4.219286
219.995976	6122.700666	8.294810	-0.045077	4.222019
220.195955	6130.668261	8.299814	-0.045120	4.224734
220.325700	6138.792086	8.304819	-0.045149	4.227499
220.341132	6146.761460	8.309824	-0.045157	4.230208
220.924152	6154.790332	8.314829	-0.045271	4.232942
221.111833	6162.791280	8.319834	-0.045311	4.235660
221.374076	6170.791402	8.324838	-0.045365	4.238377
221.429985	6178.902764	8.329843	-0.045381	4.241128
221.665798	6186.797181	8.334848	-0.045430	4.243805
221.975226	6194.916662	8.339853	-0.045493	4.246558
222.312875	6202.847788	8.344858	-0.045561	4.249246
222.500166	6210.930002	8.349862	-0.045601	4.251981
222.742375	6218.935429	8.354867	-0.045652	4.254689
222.712228	6226.947869	8.359872	-0.045651	4.257395
223.232765	6234.932115	8.364877	-0.045753	4.260095
223.610004	6242.899097	8.369882	-0.045829	4.262786
223.619081	6250.985086	8.374886	-0.045836	4.265512
223.308476	6259.051426	8.379891	-0.045783	4.268226
223.600085	6267.052188	8.384896	-0.045843	4.270923
224.237161	6275.063816	8.389901	-0.045967	4.273624
223.949500	6283.131777	8.394906	-0.045919	4.276334
224.498867	6291.037480	8.399910	-0.046026	4.278996
224.963678	6299.089327	8.404915	-0.046118	4.281704
225.090106	6307.015576	8.409920	-0.046147	4.284366
225.211791	6315.144356	8.414925	-0.046175	4.287093
225.253864	6323.166926	8.419930	-0.046188	4.289782
225.844038	6331.135464	8.424934	-0.046303	4.292457
225.585827	6339.247443	8.429939	-0.046260	4.295170
225.714011	6347.225945	8.434944	-0.046289	4.297840
226.253874	6355.264561	8.439949	-0.046395	4.300533
226.265091	6363.180682	8.444954	-0.046402	4.303177
227.037156	6371.210298	8.449958	-0.046551	4.305866
227.076579	6379.263874	8.454963	-0.046564	4.308553
226.949164	6387.326923	8.459968	-0.046546	4.311241
227.635145	6395.235816	8.464973	-0.046678	4.313883
227.964963	6403.278223	8.469978	-0.046745	4.316564
227.952838	6411.306485	8.474982	-0.046748	4.319236
228.247122	6419.344047	8.479987	-0.046808	4.321913
228.160313	6427.362624	8.484992	-0.046797	4.324578
228.544722	6435.369485	8.489997	-0.046874	4.327241
228.434209	6443.423980	8.495002	-0.046859	4.329914
228.874171	6451.404747	8.500006	-0.046946	4.332566
229.020729	6459.462830	8.505011	-0.046979	4.335240
229.249422	6467.415570	8.510016	-0.047026	4.337877
229.247216	6475.536338	8.515021	-0.047031	4.340567
229.971604	6483.400232	8.520026	-0.047171	4.343175
230.395123	6491.475562	8.525030	-0.047256	4.345850
230.750788	6499.461303	8.530035	-0.047327	4.348493
230.529326	6507.582867	8.535040	-0.047291	4.351174
230.646954	6515.665492	8.540045	-0.047318	4.353844
230.648628	6523.673482	8.545050	-0.047324	4.356486
231.112748	6531.518512	8.550054	-0.047415	4.359077
231.639668	6539.580173	8.555059	-0.047519	4.361738
231.669003	6547.529271	8.560064	-0.047530	4.364356
231.930690	6555.628805	8.565069	-0.047584	4.367024
232.047711	6563.622701	8.570074	-0.047611	4.369655
232.293718	6571.650926	8.575079	-0.047662	4.372296
232.865626	6579.636132	8.580083	-0.047773	4.374924
233.177666	6587.668136	8.585088	-0.047837	4.377564
233.327045	6595.743816	8.590093	-0.047870	4.380215
233.453037	6603.697356	8.595098	-0.047899	4.382824
233.870897	6611.682903	8.600103	-0.047982	4.385444
234.519454	6619.700056	8.605107	-0.048108	4.388075
234.545906	6627.724635	8.610112	-0.048118	4.390702
234.555857	6635.845057	8.615117	-0.048125	4.393359
234.555307	6643.859827	8.620122	-0.048130	4.395980
234.921659	6651.830934	8.625127	-0.048204	4.398587
235.078823	6659.898098	8.630131	-0.048238	4.401222
235.441970	6667.767097	8.635136	-0.048311	4.403793
236.175216	6675.876820	8.640141	-0.048453	4.406443
236.060405	6683.901737	8.645146	-0.048437	4.409058
236.300795	6691.970614	8.650151	-0.048487	4.411689
236.351179	6700.021143	8.655155	-0.048502	4.414310
236.573991	6707.977293	8.660160	-0.048548	4.416900
236.812122	6716.017629	8.665165	-0.048598	4.419517
237.135080	6724.014199	8.670170	-0.048663	4.422118
237.389387	6732.013972	8.675175	-0.048716	4.424718
237.511189	6740.101740	8.680179	-0.048744	4.427344
237.757198	6748.121900	8.685184	-0.048795	4.429947
238.014908	6756.182315	8.690189	-0.048848	4.432562
237.979845	6764.199668	8.695194	-0.048847	4.435160
238.249061	6772.183718	8.700199	-0.048902	4.437747
238.602213	6780.191383	8.705203	-0.048973	4.440341
238.491178	6788.207786	8.710208	-0.048958	4.442934
238.899828	6796.242455	8.715213	-0.049039	4.445533
238.805847	6804.251553	8.720218	-0.049027	4.448121
239.367351	6812.282743	8.725223	-0.049137	4.450717
239.443967	6820.301432	8.730227	-0.049156	4.453305
239.576821	6828.345239	8.735232	-0.049186	4.455900
240.288204	6836.339256	8.740237	-0.049324	4.458480
240.525545	6844.335787	8.745242	-0.049374	4.461057
240.358404	6852.356762	8.750247	-0.049348	4.463639
240.460139	6860.444291	8.755251	-0.049372	4.466242
240.309165	6868.404367	8.760256	-0.049349	4.468801
240.513406	6876.449277	8.765261	-0.049392	4.471388
241.492315	6884.311806	8.770266	-0.049580	4.473918
241.885788	6892.423888	8.775271	-0.049658	4.476524
242.002815	6900.416247	8.780275	-0.049685	4.479088
242.097064	6908.464200	8.785280	-0.049708	4.481669
242.680748	6916.423443	8.790285	-0.049822	4.484222
242.615035	6924.529761	8.795290	-0.049815	4.486818
242.696702	6932.505144	8.800295	-0.049836	4.489372
243.234967	6940.573850	8.805299	-0.049941	4.491955
243.315472	6948.529247	8.810304	-0.049961	4.494499
243.720275	6956.615078	8.815309	-0.050042	4.497084
243.893002	6964.539441	8.820314	-0.050080	4.499615
243.899449	6972.598556	8.825319	-0.050086	4.502188
244.730613	6980.576967	8.830323	-0.050246	4.504736
244.783400	6988.599827	8.835328	-0.050261	4.507294
245.161192	6996.655830	8.840333	-0.050337	4.509862
245.082731	7004.721813	8.845338	-0.050327	4.512430
245.513147	7012.630610	8.850343	-0.050413	4.514949
245.633479	7020.681945	8.855347	-0.050440	4.517510
245.975000	7028.666731	8.860352	-0.050509	4.520049
246.036609	7036.728930	8.865357	-0.050526	4.522611
246.344241	7044.687916	8.870362	-0.050589	4.525139
246.792956	7052.727771	8.875367	-0.050677	4.527692
247.082903	7060.776907	8.880371	-0.050737	4.530246
247.039019	7068.762093	8.885376	-0.050734	4.532777
247.242314	7076.815379	8.890381	-0.050777	4.535329
247.204771	7084.792729	8.895386	-0.050775	4.537854
247.603553	7092.809925	8.900391	-0.050855	4.540393
247.980855	7100.781611	8.905395	-0.050930	4.542915
248.156802	7108.833778	8.910400	-0.050968	4.545461
248.525539	7116.842393	8.915405	-0.051042	4.547992
248.510610	7124.923189	8.920410	-0.051045	4.550543
248.731406	7132.878890	8.925415	-0.051091	4.553054
249.220550	7140.939872	8.930419	-0.051187	4.555597
249.341211	7148.889599	8.935424	-0.051215	4.558103
249.790344	7156.952235	8.940429	-0.051304	4.560644
249.641976	7164.938769	8.945434	-0.051282	4.563159
250.101233	7172.908309	8.950439	-0.051372	4.565667
250.003565	7181.005573	8.955443	-0.051359	4.568214
250.469868	7188.998075	8.960448	-0.051452	4.570727
250.583247	7197.082058	8.965453	-0.051478	4.573267
250.525749	7205.072248	8.970458	-0.051473	4.575775
250.866167	7213.050331	8.975463	-0.051541	4.578279
251.243833	7221.127290	8.980467	-0.051617	4.580813
251.111190	7229.097364	8.985472	-0.051597	4.583311
251.379451	7237.092341	8.990477	-0.051653	4.585816
251.896442	7245.131302	8.995482	-0.051754	4.588334
252.018908	7253.149082	9.000487	-0.051782	4.590843
252.201635	7261.172988	9.005491	-0.051821	4.593353
252.480542	7269.187890	9.010496	-0.051879	4.595859
252.812396	7277.165044	9.015501	-0.051946	4.598351
252.750462	7285.172493	9.020506	-0.051939	4.600851
253.103771	7293.120392	9.025511	-0.052010	4.603332
253.385024	7301.228227	9.030515	-0.052068	4.605861
253.323977	7309.206777	9.035520	-0.052062	4.608348
253.264541	7317.308896	9.040525	-0.052056	4.610872
253.590779	7325.236512	9.045530	-0.052122	4.613341
254.215591	7333.263807	9.050535	-0.052244	4.615840
254.337155	7341.307390	9.055539	-0.052272	4.618342
254.352715	7349.292429	9.060544	-0.052280	4.620824
254.962777	7357.259961	9.065549	-0.052399	4.623300
255.132622	7365.326718	9.070554	-0.052436	4.625806
255.506785	7373.311887	9.075559	-0.052510	4.628284
255.670407	7381.419764	9.080563	-0.052546	4.630799
255.803677	7389.359934	9.085568	-0.052576	4.633261
256.144668	7397.451138	9.090573	-0.052645	4.635768
256.314940	7405.358584	9.095578	-0.052682	4.638217
256.754560	7413.496889	9.100583	-0.052769	4.640736
256.579797	7421.412457	9.105587	-0.052742	4.643185
256.711393	7429.486334	9.110592	-0.052772	4.645681
257.009881	7437.490686	9.115597	-0.052833	4.648155
257.110036	7445.543049	9.120602	-0.052856	4.650642
257.199567	7453.531994	9.125607	-0.052878	4.653108
257.504757	7461.574745	9.130611	-0.052940	4.655589
257.877522	7469.495309	9.135616	-0.053015	4.658032
258.106199	7477.572169	9.140621	-0.053063	4.660521
258.394805	7485.532812	9.145626	-0.053122	4.662973
258.589455	7493.608292	9.150631	-0.053163	4.665459
258.757113	7501.626235	9.155635	-0.053200	4.667926
258.711298	7509.699089	9.160640	-0.053197	4.670408
259.300904	7517.702712	9.165645	-0.053312	4.672868
259.342341	7525.712152	9.170650	-0.053325	4.675329
259.643755	7533.643820	9.175655	-0.053386	4.677764
259.834577	7541.712876	9.180659	-0.053427	4.680240
259.871668	7549.661792	9.185664	-0.053439	4.682678
260.260964	7557.686888	9.190669	-0.053517	4.685138
260.462214	7565.755698	9.195674	-0.053560	4.687610
260.579945	7573.771545	9.200679	-0.053587	4.690064
260.748016	7581.761165	9.205683	-0.053623	4.692509
260.696519	7589.788104	9.210688	-0.053619	4.694965
260.844051	7597.830039	9.215693	-0.053652	4.697423
261.002642	7605.803729	9.220698	-0.053686	4.699860
261.293283	7613.834216	9.225703	-0.053746	4.702312
261.448069	7621.869556	9.230707	-0.053780	4.704765
261.586594	7629.842564	9.235712	-0.053811	4.707197
261.667689	7637.884049	9.240717	-0.053831	4.709649
262.012950	7645.938031	9.245722	-0.053901	4.712103
262.356097	7653.877425	9.250727	-0.053970	4.714521
262.478316	7661.965684	9.255731	-0.053998	4.716984
262.658294	7669.854273	9.260736	-0.054037	4.719384
263.094464	7677.938172	9.265741	-0.054123	4.721842
263.197007	7685.922019	9.270746	-0.054148	4.724269
263.215098	7694.000020	9.275751	-0.054156	4.726723
263.343237	7702.021139	9.280755	-0.054186	4.729158
263.347961	7710.063237	9.285760	-0.054192	4.731599
263.653291	7718.028914	9.290765	-0.054254	4.734015
263.984455	7726.106063	9.295770	-0.054321	4.736463
264.635283	7734.020531	9.300775	-0.054447	4.738860
264.654390	7742.152723	9.305779	-0.054456	4.741323
264.782981	7750.007229	9.310784	-0.054485	4.743701
265.402335	7758.104434	9.315789	-0.054606	4.746149
265.186501	7766.122710	9.320794	-0.054571	4.748574
265.149328	7774.211399	9.325799	-0.054569	4.751019
265.598849	7782.193137	9.330803	-0.054658	4.753429
266.029113	7790.190336	9.335808	-0.054744	4.755843
266.055593	7798.221714	9.340813	-0.054754	4.758267
265.601814	7806.333060	9.345818	-0.054675	4.760714
266.080151	7814.210598	9.350823	-0.054769	4.763088
266.274682	7822.245319	9.355827	-0.054810	4.765508
266.330110	7830.269527	9.360832	-0.054826	4.767925
266.809339	7838.326476	9.365837	-0.054920	4.770349
267.059189	7846.342051	9.370842	-0.054972	4.772759
267.416915	7854.337852	9.375847	-0.055044	4.775163
267.513398	7862.391477	9.380851	-0.055067	4.777583
268.089680	7870.376913	9.385856	-0.055180	4.779980
268.295235	7878.405595	9.390861	-0.055223	4.782390
268.093589	7886.352131	9.395866	-0.055191	4.784775
268.324641	7894.446490	9.400871	-0.055239	4.787202
268.330380	7902.497920	9.405875	-0.055246	4.789616
268.303666	7910.517643	9.410880	-0.055246	4.792019
268.772245	7918.556113	9.415885	-0.055339	4.794425
268.969289	7926.516539	9.420890	-0.055381	4.796807
268.976509	7934.451745	9.425895	-0.055387	4.799181
269.295869	7942.540644	9.430899	-0.055452	4.801598
269.511606	7950.437164	9.435904	-0.055497	4.803958
269.832661	7958.565743	9.440909	-0.055562	4.806385
269.650058	7966.542976	9.445914	-0.055534	4.808767
269.988229	7974.594261	9.450919	-0.055602	4.811169
270.370627	7982.584293	9.455923	-0.055678	4.813550
270.575260	7990.068180	9.460928	-0.055721	4.815781
270.922906	7994.745999	9.465933	-0.055789	4.817173

271.011991	7997.188642	9.470938	-0.055807	4.817901
271.090163	7998.490185	9.475943	-0.055823	4.818288
271.297572	7998.900517	9.480947	-0.055862	4.818410
271.261136	8000.004745	9.485952	-0.055856	4.818739
270.894133	8000.112211	9.490957	-0.055787	4.818772
271.159514	8000.014983	9.495962	-0.055837	4.818742
271.368593	8000.060629	9.500967	-0.055876	4.818755
271.672353	8000.061367	9.505971	-0.055932	4.818754
271.409959	8000.109377	9.510976	-0.055884	4.818769
271.881157	8000.078714	9.515981	-0.055971	4.818758
272.299042	8000.010685	9.520986	-0.056049	4.818737
272.495948	7999.971277	9.525991	-0.056086	4.818724
272.151033	8000.025570	9.530995	-0.056022	4.818742
271.942801	8000.048068	9.536000	-0.055983	4.818749
272.499912	8000.030033	9.541005	-0.056087	4.818742
272.448972	7999.993747	9.546010	-0.056077	4.818731
272.817922	8000.006850	9.551015	-0.056146	4.818733
272.964796	8000.025501	9.556019	-0.056173	4.818738
272.927812	8000.006164	9.561024	-0.056167	4.818733
273.326562	8000.008119	9.566029	-0.056241	4.818732
273.140838	8000.037193	9.571034	-0.056206	4.818741
273.273038	8000.049367	9.576039	-0.056231	4.818744
273.227136	8000.040398	9.581043	-0.056223	4.818742
273.312698	8000.016338	9.586048	-0.056238	4.818734
273.504281	8000.053380	9.591053	-0.056274	4.818745
273.194246	8000.059901	9.596058	-0.056217	4.818748
273.369220	8000.051659	9.601063	-0.056249	4.818745
273.550288	8000.061314	9.606067	-0.056283	4.818747
273.376043	8000.059089	9.611072	-0.056251	4.818747
273.557335	8000.057217	9.616077	-0.056284	4.818746
273.914787	8000.002043	9.621082	-0.056351	4.818728
274.133842	8000.019522	9.626087	-0.056392	4.818732
274.105379	7999.990860	9.631091	-0.056386	4.818724
274.040509	8000.012045	9.636096	-0.056374	4.818730
274.276858	8000.050709	9.641101	-0.056418	4.818741
274.420273	7999.994895	9.646106	-0.056445	4.818724
274.112738	8000.005640	9.651111	-0.056388	4.818728
274.560260	8000.002981	9.656115	-0.056471	4.818726
274.285641	8000.025676	9.661120	-0.056420	4.818733
273.988920	8000.060667	9.666125	-0.056365	4.818745
274.292143	8000.035198	9.671130	-0.056422	4.818736
273.949946	8000.061222	9.676135	-0.056358	4.818745
273.781475	8000.093661	9.681139	-0.056327	4.818756
274.156944	8000.048152	9.686144	-0.056397	4.818741
274.147270	8000.093104	9.691149	-0.056395	4.818754
274.332381	8000.070318	9.696154	-0.056429	4.818747
273.798195	8000.113802	9.701159	-0.056330	4.818762
274.347292	8000.079948	9.706163	-0.056432	4.818749
273.980400	8000.118234	9.711168	-0.056364	4.818762
274.242089	8000.133115	9.716173	-0.056413	4.818766
274.448661	8000.079157	9.721178	-0.056451	4.818749
274.686068	8000.092679	9.726183	-0.056495	4.818752
274.689714	8000.051848	9.731187	-0.056496	4.818740
274.795059	8000.034330	9.736192	-0.056516	4.818734
275.026666	8000.050923	9.741197	-0.056559	4.818738
274.850255	8000.061248	9.746202	-0.056526	4.818742
274.915691	8000.046364	9.751207	-0.056538	4.818737
275.266007	8000.046657	9.756211	-0.056604	4.818736
274.870396	8000.041598	9.761216	-0.056530	4.818736
274.826985	8000.062009	9.766221	-0.056522	4.818742
274.971370	8000.020882	9.771226	-0.056549	4.818729
274.816592	8000.055593	9.776231	-0.056520	4.818740
274.765274	8000.074855	9.781235	-0.056511	4.818746
274.172957	8000.132269	9.786240	-0.056400	4.818766
274.647638	8000.124718	9.791245	-0.056489	4.818762
274.727969	8000.068097	9.796250	-0.056504	4.818744
274.782736	8000.062511	9.801255	-0.056514	4.818743
274.630096	8000.100393	9.806259	-0.056486	4.818754
274.968730	8000.032401	9.811264	-0.056549	4.818733
275.099154	8000.072857	9.816269	-0.056573	4.818744
275.173912	8000.051804	9.821274	-0.056587	4.818738
275.564980	8000.018027	9.826279	-0.056660	4.818726
275.650780	8000.015983	9.831283	-0.056676	4.818725
275.657229	8000.027599	9.836288	-0.056677	4.818729
275.394868	8000.066173	9.841293	-0.056628	4.818741
275.250329	8000.049651	9.846298	-0.056601	4.818737
275.356465	8000.045771	9.851303	-0.056621	4.818735
275.696471	8000.057463	9.856307	-0.056685	4.818738
275.655295	8000.030733	9.861312	-0.056677	4.818730
275.777133	8000.054308	9.866317	-0.056700	4.818736
275.727557	8000.009650	9.871322	-0.056690	4.818723
275.690162	8000.047959	9.876327	-0.056684	4.818735
275.638587	8000.050447	9.881331	-0.056674	4.818736
275.375217	8000.062802	9.886336	-0.056625	4.818740
275.469825	8000.089173	9.891341	-0.056643	4.818748
275.493442	8000.061176	9.896346	-0.056647	4.818739
275.693062	8000.032287	9.901351	-0.056684	4.818730
275.663384	8000.081177	9.906355	-0.056679	4.818745
275.663587	8000.036108	9.911360	-0.056679	4.818731
276.059124	8000.057946	9.916365	-0.056753	4.818736
275.628353	8000.038807	9.921370	-0.056672	4.818732
275.726654	8000.020152	9.926375	-0.056691	4.818726
275.992742	8000.058153	9.931379	-0.056740	4.818737
276.044936	7999.986495	9.936384	-0.056750	4.818715
276.284618	8000.046172	9.941389	-0.056795	4.818732
276.142624	8000.013957	9.946394	-0.056768	4.818723
275.979510	8000.012920	9.951399	-0.056738	4.818723
276.051343	8000.019084	9.956403	-0.056751	4.818725
276.150966	8000.004638	9.961408	-0.056770	4.818720
276.079889	8000.055095	9.966413	-0.056757	4.818735
275.827238	8000.066539	9.971418	-0.056710	4.818740
276.027576	8000.027176	9.976423	-0.056747	4.818727
276.048885	8000.074623	9.981427	-0.056751	4.818741
275.925806	8000.057326	9.986432	-0.056728	4.818737
276.016192	8000.077355	9.991437	-0.056745	4.818742
275.955247	8000.032551	9.996442	-0.056734	4.818729
275.910768	8000.081252	10.001447	-0.056726	4.818744
276.101100	8000.071113	10.006451	-0.056761	4.818740
276.122538	8000.022122	10.011456	-0.056765	4.818725
276.113555	8000.056602	10.016461	-0.056764	4.818736
276.008250	8000.051064	10.021466	-0.056744	4.818734
276.494248	8000.051000	10.026471	-0.056834	4.818733
276.468581	8000.039143	10.031475	-0.056830	4.818729
276.035177	8000.053513	10.036480	-0.056749	4.818735
276.295395	8000.076765	10.041485	-0.056798	4.818741
276.118287	8000.069258	10.046490	-0.056765	4.818739
276.046073	8000.115508	10.051495	-0.056751	4.818753
276.392125	8000.098977	10.056499	-0.056816	4.818747
275.971086	8000.068430	10.061504	-0.056737	4.818740
276.139786	8000.086317	10.066509	-0.056769	4.818744
275.690255	8000.089998	10.071514	-0.056685	4.818747
275.992486	8000.063471	10.076519	-0.056741	4.818738
276.140571	8000.072708	10.081523	-0.056769	4.818740
276.359244	8000.041966	10.086528	-0.056810	4.818730
276.123660	8000.072497	10.091533	-0.056766	4.818740
276.302066	8000.071639	10.096538	-0.056799	4.818739
276.492857	8000.035300	10.101543	-0.056835	4.818728
276.439244	8000.044050	10.106547	-0.056825	4.818731
276.563702	8000.029923	10.111552	-0.056848	4.818726
276.402821	8000.071892	10.116557	-0.056818	4.818739
276.340687	8000.037555	10.121562	-0.056807	4.818729
276.411762	8000.013310	10.126567	-0.056820	4.818722
276.490176	8000.047861	10.131571	-0.056835	4.818732
276.367575	8000.006460	10.136576	-0.056812	4.818720
276.393177	8000.055011	10.141581	-0.056817	4.818734
276.059688	8000.070660	10.146586	-0.056755	4.818740
276.208451	8000.073616	10.151591	-0.056782	4.818740
276.300227	8000.063263	10.156595	-0.056799	4.818737
276.095489	8000.067982	10.161600	-0.056761	4.818739
276.283455	8000.090309	10.166605	-0.056796	4.818745
276.347344	8000.053392	10.171610	-0.056808	4.818734
276.370049	8000.046348	10.176615	-0.056813	4.818732
276.075921	8000.126445	10.181619	-0.056758	4.818757
275.847955	8000.098371	10.186624	-0.056715	4.818749
276.373484	8000.076800	10.191629	-0.056813	4.818741
276.267355	8000.067057	10.196634	-0.056794	4.818738
276.720473	8000.082297	10.201639	-0.056878	4.818741
276.655011	8000.047917	10.206643	-0.056866	4.818731
276.715895	8000.008866	10.211648	-0.056877	4.818719
276.757028	8000.058664	10.216653	-0.056885	4.818734
276.469233	8000.050788	10.221658	-0.056831	4.818733
276.461914	8000.066421	10.226663	-0.056830	4.818737
276.674409	8000.086965	10.231667	-0.056870	4.818743
276.758270	7999.980071	10.236672	-0.056885	4.818710
276.948108	8000.021291	10.241677	-0.056921	4.818722
276.978326	8000.031115	10.246682	-0.056926	4.818725
277.079913	8000.002019	10.251687	-0.056945	4.818716
276.715578	8000.050817	10.256691	-0.056878	4.818732
277.077625	8000.030299	10.261696	-0.056945	4.818724
276.888054	8000.065611	10.266701	-0.056910	4.818735
276.985337	8000.038557	10.271706	-0.056928	4.818727
276.671400	8000.067035	10.276711	-0.056869	4.818737
276.906708	8000.029169	10.281715	-0.056913	4.818724
277.038246	8000.005698	10.286720	-0.056938	4.818717
276.859357	8000.065257	10.291725	-0.056905	4.818735
276.989640	8000.018709	10.296730	-0.056929	4.818721
277.088137	8000.056663	10.301735	-0.056947	4.818732
276.971059	8000.068793	10.306739	-0.056926	4.818736
276.914017	8000.016700	10.311744	-0.056915	4.818721
277.127523	8000.055079	10.316749	-0.056955	4.818731
276.991947	8000.022945	10.321754	-0.056929	4.818722
276.976184	8000.025891	10.326759	-0.056927	4.818723
277.211639	8000.058261	10.331763	-0.056971	4.818732
277.176796	7999.988632	10.336768	-0.056964	4.818711
277.002946	8000.060835	10.341773	-0.056932	4.818733
276.647923	8000.023794	10.346778	-0.056866	4.818724
276.705524	8000.076948	10.351783	-0.056876	4.818739
276.901662	8000.084704	10.356787	-0.056913	4.818741
276.823320	8000.055400	10.361792	-0.056898	4.818733
277.266117	8000.025434	10.366797	-0.056981	4.818722
277.124428	8000.033056	10.371802	-0.056955	4.818725
277.006138	8000.047268	10.376807	-0.056933	4.818729
277.121512	8000.068666	10.381811	-0.056954	4.818735
277.137511	8000.061535	10.386816	-0.056957	4.818733
277.108102	8000.048582	10.391821	-0.056952	4.818729
277.028417	8000.036033	10.396826	-0.056937	4.818726
276.892060	8000.077268	10.401831	-0.056912	4.818739
277.085785	8000.086042	10.406835	-0.056948	4.818741
277.080710	8000.029373	10.411840	-0.056947	4.818724
277.353675	8000.055935	10.416845	-0.056998	4.818731
277.116272	8000.037172	10.421850	-0.056953	4.818726
276.980916	8000.046972	10.426855	-0.056928	4.818729
277.214125	8000.069880	10.431859	-0.056972	4.818735
276.965143	8000.058307	10.436864	-0.056925	4.818733
277.028039	8000.065405	10.441869	-0.056937	4.818735
276.706865	8000.103225	10.446874	-0.056877	4.818747
276.871117	8000.044532	10.451879	-0.056908	4.818729
277.064200	8000.072166	10.456883	-0.056944	4.818737
276.834198	8000.034630	10.461888	-0.056901	4.818726
276.871878	8000.105349	10.466893	-0.056908	4.818747
277.190586	8000.057021	10.471898	-0.056968	4.818732
276.936834	8000.075787	10.476903	-0.056921	4.818738
277.094130	8000.088288	10.481907	-0.056950	4.818741
277.163934	8000.075557	10.486912	-0.056963	4.818737
277.232759	8000.095311	10.491917	-0.056976	4.818743
277.242182	8000.080758	10.496922	-0.056978	4.818738
277.272543	8000.057039	10.501927	-0.056983	4.818731
277.304504	8000.062693	10.506931	-0.056989	4.818733
277.111883	8000.048697	10.511936	-0.056953	4.818729
277.454723	8000.074058	10.516941	-0.057017	4.818736
277.357251	8000.075957	10.521946	-0.056999	4.818737
277.324689	8000.088122	10.526951	-0.056993	4.818740
277.517766	8000.087454	10.531955	-0.057029	4.818739
277.722099	8000.074350	10.536960	-0.057067	4.818735
277.703946	8000.094038	10.541965	-0.057064	4.818741
277.446887	8000.069781	10.546970	-0.057016	4.818734
277.665795	8000.076782	10.551975	-0.057057	4.818736
277.863075	8000.080361	10.556979	-0.057094	4.818736
277.773428	8000.017366	10.561984	-0.057077	4.818718
277.763661	8000.036113	10.566989	-0.057075	4.818723
277.639167	8000.056534	10.571994	-0.057052	4.818730
277.723806	8000.101650	10.576999	-0.057068	4.818743
277.334192	8000.112385	10.582003	-0.056995	4.818748
277.578357	8000.066246	10.587008	-0.057041	4.818733
277.621142	8000.078329	10.592013	-0.057049	4.818736
277.723570	8000.033519	10.597018	-0.057068	4.818723
277.379233	8000.064752	10.602023	-0.057004	4.818733
277.396360	8000.086988	10.607027	-0.057007	4.818740
277.254910	8000.078889	10.612032	-0.056981	4.818738
277.704301	8000.088843	10.617037	-0.057065	4.818739
277.867535	8000.029088	10.622042	-0.057095	4.818721
277.138843	8000.082651	10.627047	-0.056959	4.818739
277.430548	8000.076957	10.632051	-0.057014	4.818737
277.418876	8000.093583	10.637056	-0.057012	4.818742
277.632613	8000.065924	10.642061	-0.057051	4.818733
277.345310	8000.067487	10.647066	-0.056998	4.818734
277.381717	8000.075294	10.652071	-0.057005	4.818736
278.014214	8000.090740	10.657075	-0.057123	4.818738
277.565702	8000.057740	10.662080	-0.057039	4.818730
277.229346	8000.099557	10.667085	-0.056977	4.818744
277.125712	8000.073074	10.672090	-0.056957	4.818737
277.288845	8000.064684	10.677095	-0.056988	4.818733
277.354490	8000.102217	10.682099	-0.057000	4.818744
277.272686	8000.073917	10.687104	-0.056985	4.818736
277.443811	8000.102319	10.692109	-0.057017	4.818744
277.376328	8000.099361	10.697114	-0.057004	4.818743
277.639288	8000.057657	10.702119	-0.057053	4.818730
277.677076	8000.067578	10.707123	-0.057060	4.818733
277.444455	8000.030007	10.712128	-0.057017	4.818723
277.521184	8000.104373	10.717133	-0.057031	4.818744
277.741745	8000.043256	10.722138	-0.057072	4.818725
277.845042	8000.012086	10.727143	-0.057092	4.818716
277.904080	8000.073646	10.732147	-0.057103	4.818734
278.000961	8000.019331	10.737152	-0.057121	4.818717
278.002624	8000.036128	10.742157	-0.057121	4.818722
277.672069	8000.051812	10.747162	-0.057060	4.818728
277.664944	8000.056965	10.752167	-0.057058	4.818730
277.861881	8000.076264	10.757171	-0.057095	4.818735
277.733465	8000.049462	10.762176	-0.057071	4.818727
277.638196	8000.088079	10.767181	-0.057053	4.818739
277.564773	8000.090286	10.772186	-0.057040	4.818740
277.467183	8000.103714	10.777191	-0.057022	4.818744
277.634721	8000.109009	10.782195	-0.057053	4.818745
277.678772	8000.073934	10.787200	-0.057061	4.818735
277.546267	8000.129895	10.792205	-0.057037	4.818752
277.676024	8000.106401	10.797210	-0.057061	4.818744
277.717871	8000.094361	10.802215	-0.057069	4.818741
277.514722	8000.124257	10.807219	-0.057031	4.818750
277.606574	8000.091892	10.812224	-0.057048	4.818740
277.704649	8000.093152	10.817229	-0.057066	4.818740
277.591520	8000.100091	10.822234	-0.057045	4.818743
277.623555	8000.099456	10.827239	-0.057051	4.818743
277.721768	8000.091283	10.832243	-0.057070	4.818740
277.587365	8000.090611	10.837248	-0.057045	4.818740
277.951993	8000.103674	10.842253	-0.057113	4.818743
277.578781	8000.098893	10.847258	-0.057043	4.818743
277.553265	8000.089135	10.852263	-0.057038	4.818740
277.796054	8000.114263	10.857267	-0.057084	4.818746
277.806676	8000.071422	10.862272	-0.057086	4.818733
277.715197	8000.082832	10.867277	-0.057069	4.818737
277.938969	8000.077316	10.872282	-0.057110	4.818735
277.738926	8000.103059	10.877287	-0.057073	4.818743
278.009381	8000.090804	10.882291	-0.057124	4.818738
277.980009	8000.082043	10.887296	-0.057118	4.818736
277.788589	8000.114187	10.892301	-0.057082	4.818746
277.648749	8000.102963	10.897306	-0.057056	4.818743
277.442556	8000.119192	10.902311	-0.057018	4.818749
277.374160	8000.137188	10.907315	-0.057005	4.818755
277.651949	8000.103012	10.912320	-0.057057	4.818743
277.735679	8000.100943	10.917325	-0.057073	4.818743
277.998603	8000.084398	10.922330	-0.057122	4.818737
277.818746	8000.098868	10.927335	-0.057088	4.818742
277.913708	8000.113716	10.932339	-0.057106	4.818746
277.950924	8000.070167	10.937344	-0.057113	4.818733
278.173968	8000.085608	10.942349	-0.057155	4.818736
277.978870	8000.083111	10.947354	-0.057118	4.818736
277.816853	8000.090471	10.952359	-0.057088	4.818739
277.685680	8000.140160	10.957363	-0.057064	4.818754
278.048395	8000.086107	10.962368	-0.057131	4.818737
278.104863	8000.110944	10.967373	-0.057142	4.818744
277.685324	8000.123391	10.972378	-0.057064	4.818749
277.887708	8000.120746	10.977383	-0.057102	4.818748
277.661254	8000.139860	10.982387	-0.057060	4.818754
277.562037	8000.123916	10.987392	-0.057041	4.818750
277.838624	8000.133753	10.992397	-0.057093	4.818752
277.873603	8000.115335	10.997402	-0.057099	4.818746
277.769058	8000.117142	11.002407	-0.057080	4.818747
277.971320	8000.127076	11.007411	-0.057117	4.818749
278.008218	8000.091909	11.012416	-0.057124	4.818739
277.877836	8000.110159	11.017421	-0.057100	4.818745
277.865469	8000.123631	11.022426	-0.057098	4.818749
278.332479	8000.084543	11.027431	-0.057185	4.818735
278.047882	8000.106057	11.032435	-0.057132	4.818743
277.989134	8000.107403	11.037440	-0.057121	4.818743
278.114564	8000.137318	11.042445	-0.057144	4.818752
278.164769	8000.080307	11.047450	-0.057154	4.818735
277.846597	8000.128647	11.052455	-0.057095	4.818750
277.729127	8000.148110	11.057459	-0.057073	4.818757
277.755379	8000.123290	11.062464	-0.057078	4.818749
277.516061	8000.134902	11.067469	-0.057033	4.818753
277.411696	8000.190175	11.072474	-0.057014	4.818770
277.794406	8000.134282	11.077479	-0.057085	4.818752
277.883469	8000.180503	11.082483	-0.057102	4.818766
277.876087	8000.094451	11.087488	-0.057100	4.818740
277.665838	8000.169333	11.092493	-0.057061	4.818763
277.901096	8000.115743	11.097498	-0.057105	4.818746
278.037438	8000.081851	11.102503	-0.057131	4.818736
278.010278	8000.115051	11.107507	-0.057126	4.818746
277.846849	8000.114007	11.112512	-0.057095	4.818746
278.090656	8000.080445	11.117517	-0.057141	4.818735
277.569607	8000.135619	11.122522	-0.057044	4.818753
277.587697	8000.174640	11.127527	-0.057047	4.818765
277.993679	8000.184040	11.132531	-0.057123	4.818766
278.122752	8000.131186	11.137536	-0.057147	4.818750
277.724948	8000.176408	11.142541	-0.057073	4.818765
277.740339	8000.148304	11.147546	-0.057076	4.818757
277.616375	8000.151959	11.152551	-0.057053	4.818758
277.107722	8000.288011	11.157555	-0.056958	4.818801
277.829904	8000.151557	11.162560	-0.057092	4.818757
277.884334	8000.144919	11.167565	-0.057103	4.818755
277.270138	8000.233493	11.172570	-0.056988	4.818784
277.542616	8000.159414	11.177575	-0.057039	4.818761
278.018588	8000.149793	11.182579	-0.057128	4.818756
277.931434	8000.100457	11.187584	-0.057111	4.818742
277.471283	8000.166895	11.192589	-0.057026	4.818763
277.386101	8000.167903	11.197594	-0.057010	4.818764
277.388969	8000.132300	11.202599	-0.057011	4.818753
277.720825	8000.144942	11.207603	-0.057072	4.818756
277.830133	8000.125380	11.212608	-0.057093	4.818749
278.151888	8000.104348	11.217613	-0.057153	4.818742
278.308998	8000.072819	11.222618	-0.057182	4.818732
277.517605	8000.121383	11.227623	-0.057035	4.818749
277.560268	8000.153381	11.232627	-0.057043	4.818759
277.128133	8000.179295	11.237632	-0.056962	4.818768
276.899909	8000.202581	11.242637	-0.056920	4.818776
277.387007	8000.187859	11.247642	-0.057011	4.818770
277.706516	8000.150025	11.252647	-0.057070	4.818757
277.104492	8000.173762	11.257651	-0.056958	4.818767
277.609115	8000.099513	11.262656	-0.057052	4.818743
277.730108	8000.147191	11.267661	-0.057075	4.818756
277.556695	8000.147068	11.272666	-0.057042	4.818757
277.500816	8000.136920	11.277671	-0.057032	4.818754
277.633629	8000.153301	11.282675	-0.057057	4.818758
277.515496	8000.167514	11.287680	-0.057035	4.818763
277.558300	8000.181693	11.292685	-0.057043	4.818767
277.715647	8000.172182	11.297690	-0.057072	4.818764
278.170148	8000.114064	11.302695	-0.057157	4.818745
277.870300	8000.166831	11.307699	-0.057101	4.818762
277.922247	8000.083636	11.312704	-0.057111	4.818737
277.943834	8000.141572	11.317709	-0.057115	4.818754
277.630185	8000.170052	11.322714	-0.057057	4.818763
277.374020	8000.197172	11.327719	-0.057009	4.818773
277.754292	8000.156972	11.332723	-0.057080	4.818759
277.396030	8000.147142	11.337728	-0.057013	4.818758
277.721774	8000.154464	11.342733	-0.057074	4.818758
278.007630	8000.105716	11.347738	-0.057127	4.818743
277.430961	8000.175902	11.352743	-0.057020	4.818766
277.000859	8000.257401	11.357747	-0.056940	4.818792
276.998623	8000.235361	11.362752	-0.056939	4.818785
276.920095	8000.333945	11.367757	-0.056925	4.818815
277.112866	8000.300776	11.372762	-0.056961	4.818804
277.200236	8000.216987	11.377767	-0.056977	4.818779
277.641258	8000.229980	11.382771	-0.057059	4.818781
277.582362	8000.213504	11.387776	-0.057048	4.818777
277.578705	8000.200880	11.392781	-0.057048	4.818773
277.668273	8000.192596	11.397786	-0.057064	4.818770
276.998012	8000.243761	11.402791	-0.056939	4.818788
277.289113	8000.335552	11.407795	-0.056994	4.818814
276.970160	8000.285342	11.412800	-0.056934	4.818800
277.610278	8000.204443	11.417805	-0.057054	4.818774
277.102676	8000.272369	11.422810	-0.056959	4.818796
276.982944	8000.271886	11.427815	-0.056937	4.818796
277.381713	8000.275951	11.432819	-0.057011	4.818796
277.236931	8000.187090	11.437824	-0.056984	4.818770
277.580073	8000.141172	11.442829	-0.057048	4.818755
277.800149	8000.106257	11.447834	-0.057089	4.818744
278.047845	8000.136691	11.452839	-0.057135	4.818752
277.829052	8000.160096	11.457843	-0.057095	4.818760
277.413892	8000.164213	11.462848	-0.057017	4.818763
277.893148	8000.196566	11.467853	-0.057107	4.818770
278.140424	8000.152565	11.472858	-0.057153	4.818756
278.082490	8000.145535	11.477863	-0.057142	4.818754
277.965001	8000.162901	11.482867	-0.057120	4.818760
278.082863	8000.109903	11.487872	-0.057142	4.818744
278.174309	8000.103740	11.492877	-0.057159	4.818742
277.461816	8000.184764	11.497882	-0.057027	4.818768
277.632187	8000.167033	11.502887	-0.057058	4.818763
277.635693	8000.218447	11.507891	-0.057059	4.818778
277.446396	8000.205541	11.512896	-0.057024	4.818775
277.980251	8000.185131	11.517901	-0.057123	4.818767
277.455857	8000.252841	11.522906	-0.057026	4.818789
277.242168	8000.210270	11.527911	-0.056986	4.818777
277.433394	8000.244172	11.532915	-0.057022	4.818786
277.491737	8000.205087	11.537920	-0.057032	4.818774
277.368162	8000.276887	11.542925	-0.057010	4.818796
277.147333	8000.290832	11.547930	-0.056968	4.818801
277.615430	8000.173136	11.552935	-0.057056	4.818764
277.430496	8000.253583	11.557939	-0.057021	4.818789
276.942702	8000.260962	11.562944	-0.056930	4.818793
277.077237	8000.286800	11.567949	-0.056956	4.818800
277.524659	8000.238026	11.572954	-0.057039	4.818784
277.633038	8000.206921	11.577959	-0.057059	4.818774
277.754380	8000.207431	11.582963	-0.057082	4.818774
277.629866	8000.225755	11.587968	-0.057059	4.818780
277.792488	8000.183814	11.592973	-0.057089	4.818767
277.420055	8000.248230	11.597978	-0.057020	4.818787
277.172611	8000.276511	11.602983	-0.056974	4.818797
277.227950	8000.324396	11.607987	-0.056984	4.818811
277.391694	8000.223764	11.612992	-0.057014	4.818780
277.500661	8000.189522	11.617997	-0.057035	4.818770
277.434313	8000.213833	11.623002	-0.057022	4.818777
277.239416	8000.251173	11.628007	-0.056986	4.818789
277.729664	8000.279475	11.633011	-0.057078	4.818796
278.085288	8000.192834	11.638016	-0.057144	4.818768
277.453165	8000.283274	11.643021	-0.057026	4.818798
277.816934	8000.219800	11.648026	-0.057094	4.818778
277.931201	8000.198205	11.653031	-0.057115	4.818771
277.939031	8000.204598	11.658035	-0.057117	4.818773
277.652000	8000.203018	11.663040	-0.057063	4.818773
277.232259	8000.303519	11.668045	-0.056985	4.818805
277.827553	8000.274462	11.673050	-0.057096	4.818794
277.669327	8000.186475	11.678055	-0.057067	4.818768
277.604053	8000.196125	11.683059	-0.057055	4.818771
277.708089	8000.193268	11.688064	-0.057074	4.818770
277.761506	8000.206535	11.693069	-0.057084	4.818774
277.487559	8000.254393	11.698074	-0.057033	4.818789
277.284644	8000.217201	11.703079	-0.056995	4.818779
277.419448	8000.278684	11.708083	-0.057020	4.818797
277.414318	8000.230400	11.713088	-0.057020	4.818782
277.543697	8000.269800	11.718093	-0.057044	4.818793
277.803999	8000.209193	11.723098	-0.057092	4.818774
277.945742	8000.174322	11.728103	-0.057119	4.818763
277.636890	8000.232215	11.733107	-0.057061	4.818782
277.840198	8000.182409	11.738112	-0.057099	4.818766
277.849773	8000.199308	11.743117	-0.057101	4.818771
277.590772	8000.176073	11.748122	-0.057053	4.818765
277.592821	8000.157232	11.753127	-0.057053	4.818760
277.600076	8000.230709	11.758131	-0.057054	4.818782
277.281578	8000.267513	11.763136	-0.056995	4.818794
277.262117	8000.204369	11.768141	-0.056992	4.818775
276.799709	8000.338917	11.773146	-0.056906	4.818817
277.059194	8000.257333	11.778151	-0.056954	4.818792
277.209252	8000.316915	11.783155	-0.056982	4.818809
277.755851	8000.210708	11.788160	-0.057084	4.818775
278.356007	8000.177521	11.793165	-0.057195	4.818763
278.071220	8000.208467	11.798170	-0.057142	4.818773
277.641842	8000.210303	11.803175	-0.057063	4.818775
277.470079	8000.322369	11.808179	-0.057031	4.818809
277.110492	8000.249624	11.813184	-0.056964	4.818789
277.484086	8000.246029	11.818189	-0.057033	4.818787
277.952344	8000.172363	11.823194	-0.057121	4.818763
277.970110	8000.191463	11.828199	-0.057124	4.818768
278.151674	8000.171779	11.833203	-0.057158	4.818762
277.954247	8000.146188	11.838208	-0.057121	4.818755
277.745431	8000.215847	11.843213	-0.057082	4.818777
277.742268	8000.196940	11.848218	-0.057082	4.818771
278.235466	8000.145608	11.853223	-0.057173	4.818754
278.243451	8000.167728	11.858227	-0.057175	4.818760
277.620842	8000.212164	11.863232	-0.057059	4.818776
277.529645	8000.247689	11.868237	-0.057042	4.818787
277.759135	8000.232812	11.873242	-0.057085	4.818782
277.745055	8000.219006	11.878247	-0.057082	4.818778
278.164170	8000.196078	11.883251	-0.057160	4.818769
278.419442	8000.135407	11.888256	-0.057208	4.818750
278.426590	8000.134453	11.893261	-0.057209	4.818750
278.396426	8000.135117	11.898266	-0.057204	4.818750
278.112803	8000.103179	11.903271	-0.057151	4.818742
278.103870	8000.160724	11.908275	-0.057149	4.818759
278.039523	8000.159902	11.913280	-0.057137	4.818759
277.829654	8000.208582	11.918285	-0.057098	4.818774
278.463692	8000.158008	11.923290	-0.057217	4.818757
278.075668	8000.163519	11.928295	-0.057144	4.818760
277.921134	8000.248550	11.933299	-0.057116	4.818786
277.771846	8000.174306	11.938304	-0.057088	4.818764
277.565158	8000.279635	11.943309	-0.057049	4.818796
278.035989	8000.181891	11.948314	-0.057137	4.818765
278.135883	8000.180029	11.953319	-0.057156	4.818764
277.844408	8000.258064	11.958323	-0.057102	4.818789
277.614133	8000.231003	11.963328	-0.057059	4.818782
277.785922	8000.219580	11.968333	-0.057091	4.818778
277.667332	8000.229594	11.973338	-0.057069	4.818781
277.944774	8000.212188	11.978343	-0.057120	4.818775
277.916573	8000.243278	11.983347	-0.057115	4.818784
277.965100	8000.164232	11.988352	-0.057124	4.818760
277.583007	8000.264167	11.993357	-0.057053	4.818792
277.623637	8000.285656	11.998362	-0.057061	4.818798
277.677976	8000.267486	12.003367	-0.057071	4.818792
277.857534	8000.304385	12.008371	-0.057104	4.818802
277.786954	8000.228005	12.013376	-0.057091	4.818780
277.713865	8000.246989	12.018381	-0.057078	4.818786
277.667536	8000.225431	12.023386	-0.057069	4.818780
277.820489	8000.206429	12.028391	-0.057098	4.818773
277.648104	8000.301714	12.033395	-0.057066	4.818802
277.227352	8000.308903	12.038400	-0.056987	4.818806
277.281185	8000.330562	12.043405	-0.056997	4.818812
277.813573	8000.197965	12.048410	-0.057097	4.818771
277.365850	8000.268755	12.053415	-0.057013	4.818794
277.353810	8000.301100	12.058419	-0.057011	4.818803
277.600616	8000.241369	12.063424	-0.057057	4.818785
277.787181	8000.230135	12.068429	-0.057092	4.818781
277.593823	8000.269591	12.073434	-0.057056	4.818793
277.281526	8000.263494	12.078439	-0.056998	4.818792
277.537973	8000.256301	12.083443	-0.057046	4.818789
277.507018	8000.228651	12.088448	-0.057040	4.818781
277.390333	8000.293201	12.093453	-0.057018	4.818801
277.999595	8000.218199	12.098458	-0.057132	4.818776
277.322452	8000.281854	12.103463	-0.057006	4.818798
277.260793	8000.351302	12.108467	-0.056994	4.818819
277.764761	8000.284385	12.113472	-0.057088	4.818797
277.863754	8000.240579	12.118477	-0.057106	4.818783
277.724424	8000.262907	12.123482	-0.057081	4.818791
277.572316	8000.260960	12.128487	-0.057052	4.818791
278.195011	8000.202902	12.133491	-0.057168	4.818771
277.567320	8000.254611	12.138496	-0.057051	4.818789
277.306699	8000.297399	12.143501	-0.057003	4.818802
277.318139	8000.342625	12.148506	-0.057005	4.818816
276.982666	8000.281720	12.153511	-0.056943	4.818799
277.172522	8000.348102	12.158515	-0.056978	4.818818
277.377297	8000.231224	12.163520	-0.057016	4.818783
277.592958	8000.222459	12.168525	-0.057056	4.818779
277.681981	8000.227797	12.173530	-0.057073	4.818780
277.866575	8000.195572	12.178535	-0.057107	4.818770
277.811788	8000.232611	12.183539	-0.057097	4.818781
277.883566	8000.202085	12.188544	-0.057111	4.818772
277.773351	8000.192288	12.193549	-0.057090	4.818769
277.965920	8000.216774	12.198554	-0.057126	4.818776
277.758163	8000.178471	12.203559	-0.057087	4.818765
277.452696	8000.317127	12.208563	-0.057031	4.818808
277.508405	8000.304216	12.213568	-0.057041	4.818804
277.838270	8000.212004	12.218573	-0.057103	4.818775
277.918524	8000.229808	12.223578	-0.057118	4.818780
277.884663	8000.186397	12.228583	-0.057111	4.818767
278.079421	8000.304211	12.233587	-0.057148	4.818802
277.863620	8000.236451	12.238592	-0.057107	4.818782
277.848118	8000.224724	12.243597	-0.057105	4.818779
277.985137	8000.229628	12.248602	-0.057130	4.818780
277.609501	8000.243685	12.253607	-0.057060	4.818785
277.408245	8000.316585	12.258611	-0.057023	4.818808
277.863822	8000.220743	12.263616	-0.057108	4.818778
277.554732	8000.263957	12.268621	-0.057050	4.818792
277.608714	8000.265700	12.273626	-0.057060	4.818792
277.621936	8000.265872	12.278631	-0.057063	4.818792
277.705660	8000.332992	12.283635	-0.057078	4.818812
277.083429	8000.381626	12.288640	-0.056963	4.818828
277.248529	8000.357538	12.293645	-0.056993	4.818821
277.264863	8000.381861	12.298650	-0.056996	4.818828
277.307421	8000.354105	12.303655	-0.057004	4.818819
277.513566	8000.354654	12.308659	-0.057043	4.818819
277.221424	8000.368733	12.313664	-0.056989	4.818824
277.307491	8000.335245	12.318669	-0.057005	4.818814
277.176571	8000.357680	12.323674	-0.056980	4.818821
277.788429	8000.221909	12.328679	-0.057094	4.818778
277.844526	8000.292868	12.333683	-0.057105	4.818799
277.818322	8000.247457	12.338688	-0.057100	4.818786
277.622454	8000.352925	12.343693	-0.057063	4.818818
277.705167	8000.319394	12.348698	-0.057079	4.818807
277.845227	8000.241521	12.353703	-0.057105	4.818784
277.894775	8000.214903	12.358707	-0.057114	4.818776
278.334553	8000.149259	12.363712	-0.057196	4.818754
278.329086	8000.204752	12.368717	-0.057195	4.818771
278.310963	8000.170976	12.373722	-0.057192	4.818761
278.339208	8000.182873	12.378727	-0.057197	4.818764
278.580320	8000.200644	12.383731	-0.057242	4.818769
277.887133	8000.252561	12.388736	-0.057113	4.818787
278.188278	8000.214492	12.393741	-0.057169	4.818774
278.430625	8000.178815	12.398746	-0.057214	4.818763
277.728651	8000.293518	12.403751	-0.057084	4.818800
277.527280	8000.317147	12.408755	-0.057046	4.818807
277.466683	8000.330000	12.413760	-0.057035	4.818812
277.994004	8000.252899	12.418765	-0.057133	4.818787
277.784119	8000.298433	12.423770	-0.057094	4.818801
277.464514	8000.292242	12.428775	-0.057035	4.818800
277.741488	8000.281119	12.433779	-0.057086	4.818796
277.782342	8000.238665	12.438784	-0.057094	4.818783
277.925589	8000.260422	12.443789	-0.057121	4.818789
277.719850	8000.326976	12.448794	-0.057082	4.818810
277.774968	8000.273173	12.453799	-0.057093	4.818793
277.364226	8000.302504	12.458803	-0.057016	4.818804
277.886271	8000.243156	12.463808	-0.057113	4.818784
278.078282	8000.262394	12.468813	-0.057149	4.818789
277.901295	8000.317785	12.473818	-0.057116	4.818806
277.642052	8000.311319	12.478823	-0.057068	4.818805
278.145782	8000.267461	12.483827	-0.057162	4.818790
277.902097	8000.276919	12.488832	-0.057117	4.818794
278.118908	8000.269219	12.493837	-0.057157	4.818791
277.614929	8000.342431	12.498842	-0.057063	4.818815
277.818857	8000.258039	12.503847	-0.057101	4.818789
277.955905	8000.299635	12.508851	-0.057127	4.818801
277.904720	8000.258097	12.513856	-0.057117	4.818788
278.494385	8000.160829	12.518861	-0.057227	4.818757
278.624128	8000.148867	12.523866	-0.057251	4.818753
278.779048	8000.121504	12.528871	-0.057280	4.818744
279.001720	8000.175731	12.533875	-0.057322	4.818760
278.604971	8000.159113	12.538880	-0.057248	4.818756
278.585343	8000.166203	12.543885	-0.057244	4.818758
278.680299	8000.145408	12.548890	-0.057262	4.818752
278.705116	8000.163551	12.553895	-0.057267	4.818757
278.869305	8000.153079	12.558899	-0.057297	4.818753
278.190233	8000.198887	12.563904	-0.057171	4.818770
278.309352	8000.205659	12.568909	-0.057193	4.818771
278.179350	8000.242782	12.573914	-0.057169	4.818783
278.315887	8000.145994	12.578919	-0.057194	4.818753
278.459646	8000.208643	12.583923	-0.057221	4.818772
278.607070	8000.167555	12.588928	-0.057249	4.818759
278.602873	8000.151779	12.593933	-0.057248	4.818754
278.504766	8000.155765	12.598938	-0.057230	4.818756
278.505929	8000.150541	12.603943	-0.057230	4.818754
278.656280	8000.171342	12.608947	-0.057258	4.818760
278.248492	8000.172405	12.613952	-0.057182	4.818762
278.658246	8000.174518	12.618957	-0.057258	4.818761
278.675821	8000.181036	12.623962	-0.057262	4.818763
278.727266	8000.143959	12.628967	-0.057271	4.818751
278.868856	8000.175130	12.633971	-0.057298	4.818760
278.604997	8000.207392	12.638976	-0.057249	4.818771
278.710990	8000.191981	12.643981	-0.057268	4.818766
278.610400	8000.179162	12.648986	-0.057250	4.818762
278.731139	8000.179665	12.653991	-0.057272	4.818762
279.148594	8000.129461	12.658995	-0.057350	4.818745
278.079470	8000.223730	12.664000	-0.057151	4.818778
278.411762	8000.223801	12.669005	-0.057213	4.818776
278.643433	8000.192180	12.674010	-0.057256	4.818766
278.508325	8000.168435	12.679015	-0.057231	4.818759
278.898907	8000.183930	12.684019	-0.057304	4.818763
278.634434	8000.204653	12.689024	-0.057255	4.818770
278.563451	8000.205842	12.694029	-0.057241	4.818770
278.379977	8000.250666	12.699034	-0.057207	4.818784
277.886356	8000.253774	12.704039	-0.057115	4.818787
278.084092	8000.299293	12.709043	-0.057152	4.818800
278.262241	8000.214570	12.714048	-0.057185	4.818774
278.335073	8000.212362	12.719053	-0.057199	4.818773
278.138423	8000.316771	12.724058	-0.057163	4.818805
278.309359	8000.212038	12.729063	-0.057194	4.818773
278.811568	8000.183886	12.734067	-0.057288	4.818763
278.946453	8000.177232	12.739072	-0.057313	4.818760
278.497012	8000.192438	12.744077	-0.057229	4.818767
278.367018	8000.242141	12.749082	-0.057205	4.818782
278.444800	8000.217982	12.754087	-0.057220	4.818774
278.226259	8000.318966	12.759091	-0.057179	4.818805
278.535389	8000.207617	12.764096	-0.057237	4.818771
278.229935	8000.267651	12.769101	-0.057180	4.818790
278.332006	8000.264769	12.774106	-0.057199	4.818789
277.985944	8000.227837	12.779111	-0.057135	4.818779
277.906928	8000.361010	12.784115	-0.057120	4.818819
278.188579	8000.233585	12.789120	-0.057172	4.818780
278.016226	8000.252344	12.794125	-0.057140	4.818786
278.172459	8000.314105	12.799130	-0.057169	4.818804
277.763010	8000.318292	12.804135	-0.057093	4.818807
277.681376	8000.375953	12.809139	-0.057078	4.818824
277.716183	8000.301972	12.814144	-0.057085	4.818802
278.087930	8000.324563	12.819149	-0.057154	4.818807
278.454068	8000.265314	12.824154	-0.057222	4.818788
278.278364	8000.253628	12.829159	-0.057189	4.818786
278.364797	8000.272561	12.834163	-0.057206	4.818791
277.789723	8000.351152	12.839168	-0.057099	4.818817
277.880279	8000.292562	12.844173	-0.057115	4.818799
277.651056	8000.324220	12.849178	-0.057073	4.818809
277.524132	8000.327837	12.854183	-0.057049	4.818811
277.937287	8000.331040	12.859187	-0.057126	4.818810
278.385334	8000.185831	12.864192	-0.057210	4.818765
277.879094	8000.239096	12.869197	-0.057115	4.818783
278.397406	8000.205909	12.874202	-0.057212	4.818771
278.021120	8000.233585	12.879207	-0.057142	4.818781
278.451593	8000.206609	12.884211	-0.057222	4.818771
278.209225	8000.213988	12.889216	-0.057177	4.818774
278.291949	8000.222389	12.894221	-0.057192	4.818776
277.981219	8000.300176	12.899226	-0.057135	4.818801
277.914281	8000.290934	12.904231	-0.057122	4.818798
278.190955	8000.268277	12.909235	-0.057174	4.818790
278.505457	8000.171674	12.914240	-0.057232	4.818760
278.523205	8000.196016	12.919245	-0.057236	4.818768
278.858503	8000.198222	12.924250	-0.057298	4.818767
278.324866	8000.234362	12.929255	-0.057199	4.818780
278.533774	8000.246479	12.934259	-0.057238	4.818783
278.192518	8000.273555	12.939264	-0.057174	4.818792
278.110199	8000.272502	12.944269	-0.057159	4.818792
278.428638	8000.248284	12.949274	-0.057218	4.818783
278.350257	8000.200107	12.954279	-0.057204	4.818769
278.875503	8000.214185	12.959283	-0.057302	4.818772
278.179201	8000.302751	12.964288	-0.057172	4.818801
278.387613	8000.232044	12.969293	-0.057211	4.818779
278.893288	8000.164101	12.974298	-0.057305	4.818757
278.675338	8000.141391	12.979303	-0.057264	4.818751
278.576826	8000.246011	12.984307	-0.057246	4.818782
278.581944	8000.218823	12.989312	-0.057247	4.818774
278.810188	8000.215463	12.994317	-0.057290	4.818772
278.900675	8000.191466	12.999322	-0.057307	4.818765
278.863061	8000.157440	13.004327	-0.057300	4.818755
279.209593	8000.153501	13.009331	-0.057364	4.818752
278.575303	8000.241815	13.014336	-0.057246	4.818781
278.643644	8000.235356	13.019341	-0.057259	4.818779
278.294225	8000.259182	13.024346	-0.057194	4.818787
278.285987	8000.252789	13.029351	-0.057192	4.818785
278.645455	8000.220711	13.034355	-0.057259	4.818774
278.672884	8000.226307	13.039360	-0.057265	4.818776
278.653009	8000.191460	13.044365	-0.057261	4.818766
278.752064	8000.182250	13.049370	-0.057279	4.818763
278.425454	8000.201127	13.054375	-0.057219	4.818769
278.955756	8000.200593	13.059379	-0.057317	4.818767
278.806775	8000.173525	13.064384	-0.057290	4.818760
278.988482	8000.172713	13.069389	-0.057324	4.818759
279.183539	8000.175218	13.074394	-0.057360	4.818759
279.013586	8000.159413	13.079399	-0.057328	4.818755
279.199204	8000.156555	13.084403	-0.057363	4.818753
278.775206	8000.193052	13.089408	-0.057284	4.818766
279.121085	8000.173380	13.094413	-0.057348	4.818758
278.822206	8000.166404	13.099418	-0.057293	4.818758
278.773851	8000.132240	13.104423	-0.057284	4.818748
279.181075	8000.145853	13.109427	-0.057360	4.818750
278.895833	8000.187275	13.114432	-0.057307	4.818763
278.376833	8000.218361	13.119437	-0.057210	4.818775
278.624570	8000.199526	13.124442	-0.057256	4.818768
278.687093	8000.163640	13.129447	-0.057268	4.818757
278.741799	8000.197890	13.134451	-0.057278	4.818767
278.653708	8000.176845	13.139456	-0.057262	4.818761
278.860480	8000.140712	13.144461	-0.057300	4.818750
278.836380	8000.212740	13.149466	-0.057296	4.818771
278.804984	8000.153634	13.154471	-0.057290	4.818754
279.121384	8000.180758	13.159475	-0.057349	4.818761
279.022800	8000.171110	13.164480	-0.057331	4.818758
278.825017	8000.187446	13.169485	-0.057294	4.818764
278.398168	8000.297290	13.174490	-0.057215	4.818798
278.584795	8000.215820	13.179495	-0.057249	4.818773
278.568234	8000.259640	13.184499	-0.057246	4.818786
279.145834	8000.121333	13.189504	-0.057354	4.818743
278.834706	8000.170811	13.194509	-0.057296	4.818759
278.978387	8000.181043	13.199514	-0.057323	4.818761
278.793573	8000.167144	13.204519	-0.057288	4.818758
279.426348	8000.140668	13.209523	-0.057406	4.818748
279.168845	8000.138416	13.214528	-0.057358	4.818748
279.106793	8000.162783	13.219533	-0.057347	4.818755
278.609653	8000.250759	13.224538	-0.057254	4.818783
278.540258	8000.217373	13.229543	-0.057241	4.818774
278.721516	8000.217604	13.234547	-0.057275	4.818773
278.747558	8000.185443	13.239552	-0.057280	4.818763
278.793659	8000.208052	13.244557	-0.057289	4.818770
278.467708	8000.375800	13.249562	-0.057228	4.818821
278.302527	8000.306591	13.254567	-0.057197	4.818801
278.768558	8000.292653	13.259571	-0.057284	4.818795
278.587979	8000.266228	13.264576	-0.057251	4.818788
278.759898	8000.240131	13.269581	-0.057283	4.818780
278.955961	8000.232165	13.274586	-0.057319	4.818777
278.647199	8000.249174	13.279591	-0.057262	4.818783
278.818200	8000.260805	13.284595	-0.057294	4.818786
278.925808	8000.218158	13.289600	-0.057314	4.818773
278.798783	8000.235402	13.294605	-0.057290	4.818778
278.867296	8000.284507	13.299610	-0.057303	4.818792
278.998373	8000.198131	13.304615	-0.057327	4.818766
279.202144	8000.180829	13.309619	-0.057365	4.818760
278.495758	8000.291281	13.314624	-0.057234	4.818796
278.470949	8000.281531	13.319629	-0.057229	4.818793
278.357610	8000.295805	13.324634	-0.057208	4.818798
278.831705	8000.215925	13.329639	-0.057296	4.818772
279.208366	8000.196648	13.334643	-0.057367	4.818765
279.058065	8000.172708	13.339648	-0.057339	4.818758
278.711111	8000.293012	13.344653	-0.057274	4.818796
278.630450	8000.349638	13.349658	-0.057259	4.818813
278.907293	8000.226344	13.354663	-0.057311	4.818775
279.008247	8000.243367	13.359667	-0.057330	4.818780
279.299344	8000.156947	13.364672	-0.057384	4.818753
278.858188	8000.207901	13.369677	-0.057302	4.818770
278.838989	8000.256929	13.374682	-0.057298	4.818784
278.594422	8000.233876	13.379687	-0.057253	4.818778
278.283877	8000.386097	13.384691	-0.057195	4.818825
278.387327	8000.281545	13.389696	-0.057214	4.818793
278.585029	8000.224329	13.394701	-0.057251	4.818776
278.572222	8000.280777	13.399706	-0.057249	4.818792
278.500043	8000.294531	13.404711	-0.057235	4.818797
278.487958	8000.339457	13.409715	-0.057233	4.818810
278.268546	8000.330356	13.414720	-0.057192	4.818808
278.336827	8000.333331	13.419725	-0.057205	4.818809
278.463874	8000.312948	13.424730	-0.057229	4.818802
278.550658	8000.261648	13.429735	-0.057245	4.818787
278.561189	8000.297429	13.434739	-0.057247	4.818797
278.433441	8000.304180	13.439744	-0.057223	4.818800
278.482815	8000.252399	13.444749	-0.057232	4.818784
278.667437	8000.294607	13.449754	-0.057267	4.818796
278.825271	8000.235831	13.454759	-0.057296	4.818778
278.314887	8000.335168	13.459763	-0.057201	4.818810
278.469063	8000.310940	13.464768	-0.057230	4.818802
278.749758	8000.262127	13.469773	-0.057282	4.818786
278.891704	8000.244032	13.474778	-0.057309	4.818780
278.596645	8000.275894	13.479783	-0.057254	4.818791
278.899932	8000.261965	13.484787	-0.057310	4.818786
278.647478	8000.269213	13.489792	-0.057263	4.818789
278.371970	8000.254150	13.494797	-0.057212	4.818785
279.190008	8000.186021	13.499802	-0.057365	4.818762
279.128659	8000.189430	13.504807	-0.057353	4.818763
279.502074	8000.154387	13.509811	-0.057423	4.818751
279.220425	8000.157066	13.514816	-0.057370	4.818753
279.192450	8000.198644	13.519821	-0.057365	4.818766
279.420936	8000.178514	13.524826	-0.057408	4.818759
279.357840	8000.149402	13.529831	-0.057396	4.818750
279.727991	8000.141574	13.534835	-0.057465	4.818747
279.368734	8000.131726	13.539840	-0.057398	4.818745
279.553869	8000.177086	13.544845	-0.057433	4.818758
279.638398	8000.156158	13.549850	-0.057448	4.818751
278.914951	8000.230747	13.554855	-0.057314	4.818776
279.427530	8000.203778	13.559859	-0.057409	4.818766
279.271342	8000.192342	13.564864	-0.057380	4.818763
279.110069	8000.248983	13.569869	-0.057350	4.818781
278.712186	8000.286864	13.574874	-0.057276	4.818794
279.319443	8000.178291	13.579879	-0.057389	4.818759
279.577971	8000.175321	13.584883	-0.057437	4.818757
279.533813	8000.154838	13.589888	-0.057429	4.818751
279.062173	8000.172902	13.594893	-0.057341	4.818758
279.380346	8000.194809	13.599898	-0.057401	4.818764
279.209857	8000.167464	13.604903	-0.057369	4.818756
279.152586	8000.210762	13.609907	-0.057358	4.818769
279.678963	8000.126312	13.614912	-0.057456	4.818742
279.879628	8000.158244	13.619917	-0.057494	4.818751
279.554430	8000.178186	13.624922	-0.057433	4.818758
279.542349	8000.124568	13.629927	-0.057431	4.818742
279.929695	8000.158895	13.634931	-0.057503	4.818751
279.299421	8000.200083	13.639936	-0.057386	4.818766
279.422058	8000.197466	13.644941	-0.057409	4.818764
279.561710	8000.190873	13.649946	-0.057435	4.818762
279.662239	8000.179586	13.654951	-0.057454	4.818758
279.671998	8000.203826	13.659955	-0.057456	4.818765
279.472057	8000.192876	13.664960	-0.057418	4.818763
279.788947	8000.169688	13.669965	-0.057477	4.818755
279.790718	8000.170762	13.674970	-0.057478	4.818755
279.711288	8000.167649	13.679975	-0.057463	4.818754
279.953028	8000.163415	13.684979	-0.057508	4.818752
279.602805	8000.147392	13.689984	-0.057443	4.818749
279.461742	8000.156069	13.694989	-0.057417	4.818752
279.796166	8000.138347	13.699994	-0.057479	4.818745
279.524559	8000.108656	13.704999	-0.057428	4.818738
279.760043	8000.132647	13.710003	-0.057472	4.818744
279.504348	8000.123079	13.715008	-0.057425	4.818742
279.526225	8000.150620	13.720013	-0.057429	4.818750
279.152273	8000.169937	13.725018	-0.057359	4.818757
279.116996	8000.156907	13.730023	-0.057353	4.818753
279.769968	8000.168433	13.735027	-0.057474	4.818754
279.938600	8000.130762	13.740032	-0.057506	4.818743
280.291419	8000.112229	13.745037	-0.057572	4.818736
279.874553	8000.139381	13.750042	-0.057494	4.818745
279.436347	8000.193517	13.755047	-0.057412	4.818763
279.635747	8000.227529	13.760051	-0.057450	4.818773
279.613034	8000.172726	13.765056	-0.057445	4.818756
279.705013	8000.126733	13.770061	-0.057463	4.818742
279.754927	8000.145198	13.775066	-0.057472	4.818748
279.652999	8000.110346	13.780071	-0.057453	4.818738
279.719396	8000.180392	13.785075	-0.057465	4.818758
279.843286	8000.133760	13.790080	-0.057488	4.818744
279.418302	8000.197501	13.795085	-0.057409	4.818764
279.626299	8000.178157	13.800090	-0.057448	4.818758
279.328034	8000.182720	13.805095	-0.057393	4.818760
279.611368	8000.195793	13.810099	-0.057445	4.818763
279.495096	8000.164950	13.815104	-0.057424	4.818754
279.608908	8000.168510	13.820109	-0.057445	4.818755
279.604688	8000.189426	13.825114	-0.057444	4.818761
278.960576	8000.202132	13.830119	-0.057324	4.818768
278.889632	8000.214853	13.835123	-0.057311	4.818772
278.306159	8000.380346	13.840128	-0.057203	4.818823
278.984482	8000.222365	13.845133	-0.057329	4.818773
278.929764	8000.232149	13.850138	-0.057319	4.818777
278.714869	8000.227299	13.855143	-0.057279	4.818776
278.818175	8000.223385	13.860147	-0.057298	4.818774
278.870624	8000.191562	13.865152	-0.057308	4.818765
278.578015	8000.271678	13.870157	-0.057254	4.818790
278.966607	8000.249409	13.875162	-0.057326	4.818782
279.357126	8000.170555	13.880167	-0.057399	4.818757
279.388147	8000.160472	13.885171	-0.057405	4.818753
279.087250	8000.160808	13.890176	-0.057349	4.818755
279.103409	8000.190372	13.895181	-0.057352	4.818763
278.870373	8000.278590	13.900186	-0.057308	4.818791
278.682688	8000.254170	13.905191	-0.057273	4.818784
278.788396	8000.290124	13.910195	-0.057293	4.818794
278.579959	8000.273825	13.915200	-0.057254	4.818790
278.885021	8000.216937	13.920205	-0.057311	4.818772
278.837852	8000.337942	13.925210	-0.057302	4.818808
278.426151	8000.251942	13.930215	-0.057226	4.818784
279.062519	8000.224464	13.935219	-0.057344	4.818774
278.852753	8000.191375	13.940224	-0.057305	4.818765
278.939814	8000.255394	13.945229	-0.057322	4.818783
278.829263	8000.259221	13.950234	-0.057301	4.818785
278.525597	8000.264763	13.955239	-0.057245	4.818788
278.903908	8000.283247	13.960243	-0.057315	4.818792
278.523604	8000.283613	13.965248	-0.057244	4.818793
279.015833	8000.165178	13.970253	-0.057336	4.818756
278.403978	8000.340791	13.975258	-0.057222	4.818811
278.176793	8000.299092	13.980263	-0.057180	4.818799
278.382162	8000.319550	13.985267	-0.057218	4.818805
278.699870	8000.264921	13.990272	-0.057277	4.818787
279.048224	8000.211734	13.995277	-0.057342	4.818770
278.539473	8000.331011	14.000282	-0.057248	4.818807
278.341738	8000.333719	14.005287	-0.057211	4.818809
278.839628	8000.266725	14.010291	-0.057303	4.818787
278.863790	8000.262845	14.015296	-0.057308	4.818786
278.610008	8000.275317	14.020301	-0.057261	4.818791
278.334821	8000.362995	14.025306	-0.057210	4.818818
278.726179	8000.239073	14.030311	-0.057282	4.818779
279.055539	8000.268461	14.035315	-0.057344	4.818787
278.990360	8000.258192	14.040320	-0.057332	4.818784
279.047528	8000.232720	14.045325	-0.057342	4.818776
279.166728	8000.276186	14.050330	-0.057365	4.818789
278.680975	8000.299310	14.055335	-0.057274	4.818797
279.395029	8000.224607	14.060339	-0.057407	4.818773
279.794508	8000.153206	14.065344	-0.057482	4.818750
279.196938	8000.176992	14.070349	-0.057370	4.818759
278.952662	8000.288130	14.075354	-0.057325	4.818793
278.947239	8000.226211	14.080359	-0.057324	4.818775
279.199818	8000.193811	14.085363	-0.057371	4.818764
279.181211	8000.193575	14.090368	-0.057368	4.818764
279.193173	8000.209456	14.095373	-0.057370	4.818769
278.908390	8000.344186	14.100378	-0.057317	4.818810
278.626933	8000.299693	14.105383	-0.057265	4.818798
279.026111	8000.209418	14.110387	-0.057339	4.818769
279.373060	8000.183470	14.115392	-0.057404	4.818760
279.298877	8000.178328	14.120397	-0.057390	4.818759
279.555091	8000.148071	14.125402	-0.057438	4.818749
279.084276	8000.192354	14.130407	-0.057350	4.818764
279.561511	8000.165980	14.135411	-0.057439	4.818754
279.548159	8000.123878	14.140416	-0.057436	4.818742
279.440046	8000.157089	14.145421	-0.057416	4.818752
279.563513	8000.156579	14.150426	-0.057439	4.818752
279.124719	8000.168775	14.155431	-0.057358	4.818757
278.958179	8000.248411	14.160435	-0.057327	4.818781
278.662549	8000.308570	14.165440	-0.057272	4.818800
278.893704	8000.237106	14.170445	-0.057315	4.818778
278.989908	8000.248827	14.175450	-0.057333	4.818781
278.697384	8000.252415	14.180455	-0.057278	4.818783
279.250573	8000.246935	14.185459	-0.057381	4.818780
279.398130	8000.182785	14.190464	-0.057409	4.818760
279.528127	8000.172924	14.195469	-0.057433	4.818757
279.803149	8000.180649	14.200474	-0.057484	4.818758
279.584389	8000.142201	14.205479	-0.057444	4.818747
279.693511	8000.183441	14.210483	-0.057464	4.818759
279.584556	8000.157934	14.215488	-0.057444	4.818752
279.778718	8000.168815	14.220493	-0.057480	4.818754
279.543372	8000.236037	14.225498	-0.057436	4.818775
279.421431	8000.215605	14.230503	-0.057414	4.818770
279.545686	8000.251798	14.235507	-0.057437	4.818780
279.062186	8000.320029	14.240512	-0.057347	4.818802
279.537384	8000.224440	14.245517	-0.057435	4.818772
279.376306	8000.225521	14.250522	-0.057405	4.818773
279.825454	8000.147419	14.255527	-0.057489	4.818748
279.572472	8000.200786	14.260531	-0.057442	4.818765
279.911316	8000.177880	14.265536	-0.057505	4.818757
279.675208	8000.163321	14.270541	-0.057461	4.818753
279.730515	8000.175565	14.275546	-0.057471	4.818757
279.751886	8000.152779	14.280551	-0.057475	4.818750
279.861990	8000.167823	14.285555	-0.057496	4.818754
279.493320	8000.250108	14.290560	-0.057427	4.818780
279.480518	8000.208012	14.295565	-0.057425	4.818767
279.925038	8000.135093	14.300570	-0.057508	4.818744
279.726397	8000.141982	14.305575	-0.057471	4.818747
279.629113	8000.202589	14.310579	-0.057453	4.818765
279.797386	8000.177494	14.315584	-0.057484	4.818757
279.504589	8000.184223	14.320589	-0.057430	4.818760
279.997171	8000.189499	14.325594	-0.057521	4.818760
280.086902	8000.119365	14.330599	-0.057538	4.818738
280.115481	8000.193119	14.335603	-0.057544	4.818760
279.936315	8000.130018	14.340608	-0.057510	4.818742
279.771336	8000.175080	14.345613	-0.057480	4.818756
280.331105	8000.168638	14.350618	-0.057584	4.818752
280.138115	8000.117939	14.355623	-0.057548	4.818738
279.555403	8000.193284	14.360627	-0.057440	4.818763
280.217825	8000.109532	14.365632	-0.057563	4.818735
279.886969	8000.144079	14.370637	-0.057501	4.818747
279.448199	8000.171999	14.375642	-0.057420	4.818757
279.675466	8000.148709	14.380647	-0.057462	4.818749
279.962508	8000.157637	14.385651	-0.057515	4.818750
279.614425	8000.174140	14.390656	-0.057451	4.818757
280.094683	8000.129984	14.395661	-0.057540	4.818742
279.886010	8000.158760	14.400666	-0.057501	4.818751
279.848746	8000.106915	14.405671	-0.057494	4.818736
279.919905	8000.148717	14.410675	-0.057508	4.818748
280.168286	8000.125698	14.415680	-0.057554	4.818740
279.820782	8000.141160	14.420685	-0.057489	4.818746
279.850697	8000.155176	14.425690	-0.057495	4.818750
279.820919	8000.112862	14.430695	-0.057489	4.818738
279.914229	8000.158093	14.435699	-0.057507	4.818751
279.755240	8000.175974	14.440704	-0.057477	4.818757
279.802980	8000.141994	14.445709	-0.057486	4.818746
280.170553	8000.151956	14.450714	-0.057555	4.818748
279.741010	8000.148543	14.455719	-0.057475	4.818748
279.861035	8000.165811	14.460723	-0.057497	4.818753
279.735372	8000.168395	14.465728	-0.057474	4.818754
280.047094	7999.129314	14.470733	-0.057531	4.818444

280.109637	7996.093496	14.475738	-0.057541	4.817539
279.872138	7990.652850	14.480743	-0.057493	4.815919
279.967919	7984.033706	14.485747	-0.057507	4.813946
279.992872	7976.805016	14.490752	-0.057507	4.811791
279.826136	7969.148242	14.495757	-0.057471	4.809507
280.137008	7961.398363	14.500762	-0.057524	4.807193
280.074797	7953.443901	14.505767	-0.057507	4.804818
279.946334	7945.608615	14.510771	-0.057478	4.802478
279.662220	7937.669969	14.515776	-0.057420	4.800106
279.385898	7929.631074	14.520781	-0.057363	4.797703
279.940361	7921.597058	14.525786	-0.057461	4.795298
279.411993	7913.615719	14.530791	-0.057358	4.792910
279.376971	7905.647937	14.535795	-0.057346	4.790524
279.022763	7897.668344	14.540800	-0.057275	4.788134
279.636226	7889.521549	14.545805	-0.057384	4.785690
279.978999	7881.526881	14.550810	-0.057443	4.783291
279.796456	7873.618338	14.555815	-0.057403	4.780919
279.758869	7865.567567	14.560819	-0.057391	4.778501
279.574867	7857.581861	14.565824	-0.057352	4.776103
279.704150	7849.527313	14.570829	-0.057371	4.773682
279.908678	7841.591666	14.575834	-0.057404	4.771295
279.889179	7833.500252	14.580839	-0.057395	4.768861
279.751291	7825.602765	14.585843	-0.057364	4.766484
279.671475	7817.513882	14.590848	-0.057344	4.764048
279.789041	7809.588253	14.595853	-0.057361	4.761660
279.672535	7801.577714	14.600858	-0.057334	4.759246
279.514443	7793.644441	14.605863	-0.057299	4.756853
279.675489	7785.571829	14.610867	-0.057324	4.754417
279.635903	7777.560732	14.615872	-0.057311	4.751998
279.423772	7769.557653	14.620877	-0.057267	4.749581
279.564908	7761.567427	14.625882	-0.057288	4.747166
279.553572	7753.479020	14.630887	-0.057281	4.744720
279.799502	7745.548169	14.635891	-0.057321	4.742320
279.778594	7737.529807	14.640896	-0.057312	4.739893
279.334682	7729.558257	14.645901	-0.057224	4.737480
279.662926	7721.508095	14.650906	-0.057280	4.735040
279.664731	7713.512546	14.655911	-0.057275	4.732616
279.604770	7705.499139	14.660915	-0.057259	4.730186
279.630624	7697.526353	14.665920	-0.057259	4.727766
279.406080	7689.529588	14.670925	-0.057212	4.725338
279.580757	7681.589418	14.675930	-0.057239	4.722926
279.284422	7673.534881	14.680935	-0.057179	4.720478
279.421835	7665.567784	14.685939	-0.057199	4.718055
279.027620	7657.566415	14.690944	-0.057121	4.715622
279.192981	7649.541012	14.695949	-0.057146	4.713178
279.320273	7641.546201	14.700954	-0.057165	4.710743
279.355060	7633.521317	14.705959	-0.057166	4.708298
279.547041	7625.540091	14.710963	-0.057197	4.705864
279.380382	7617.554484	14.715968	-0.057160	4.703428
279.222199	7609.587431	14.720973	-0.057126	4.700997
279.320484	7601.534419	14.725978	-0.057139	4.698538
279.071880	7593.525418	14.730983	-0.057087	4.696091
279.453908	7585.520420	14.735987	-0.057153	4.693644
279.308743	7577.591561	14.740992	-0.057121	4.691219
279.091586	7569.490234	14.745997	-0.057076	4.688740
279.117985	7561.593635	14.751002	-0.057075	4.686322
279.290373	7553.484377	14.756007	-0.057102	4.683838
279.012988	7545.599526	14.761011	-0.057045	4.681422
278.800601	7537.512345	14.766016	-0.057001	4.678942
278.959405	7529.571483	14.771021	-0.057025	4.676505
279.041745	7521.515649	14.776026	-0.057035	4.674032
278.795447	7513.484032	14.781031	-0.056984	4.671566
278.823894	7505.436684	14.786035	-0.056984	4.669093
278.774717	7497.523485	14.791040	-0.056970	4.666660
278.480655	7489.463145	14.796045	-0.056910	4.664180
278.579420	7481.519886	14.801050	-0.056923	4.661735
278.711902	7473.434818	14.806055	-0.056943	4.659246
278.716236	7465.510044	14.811059	-0.056938	4.656804
278.572753	7457.459882	14.816064	-0.056907	4.654322
278.601709	7449.498993	14.821069	-0.056907	4.651867
278.586394	7441.432095	14.826074	-0.056899	4.649377
278.350432	7433.516297	14.831079	-0.056850	4.646933
278.346931	7425.449938	14.836083	-0.056844	4.644441
278.109781	7417.536649	14.841088	-0.056794	4.641995
278.089049	7409.445655	14.846093	-0.056785	4.639493
278.329310	7401.502851	14.851098	-0.056825	4.637035
278.142151	7393.461125	14.856103	-0.056785	4.634545
278.339220	7385.463320	14.861107	-0.056816	4.632068
278.012743	7377.390332	14.866112	-0.056750	4.629566
278.084881	7369.449709	14.871117	-0.056759	4.627103
277.818961	7361.477964	14.876122	-0.056704	4.624630
277.946946	7353.472286	14.881127	-0.056723	4.622145
277.932284	7345.436130	14.886131	-0.056715	4.619649
278.203369	7337.466690	14.891136	-0.056760	4.617172
277.766541	7329.409476	14.896141	-0.056674	4.614667
277.815753	7321.447370	14.901146	-0.056678	4.612190
277.846459	7313.383314	14.906151	-0.056678	4.609679
278.201692	7305.421569	14.911155	-0.056739	4.607200
277.955780	7297.414404	14.916160	-0.056688	4.604705
277.770581	7289.471483	14.921165	-0.056649	4.602228
278.103438	7281.435505	14.926170	-0.056705	4.599722
277.969429	7273.463003	14.931175	-0.056675	4.597233
277.816459	7265.436006	14.936179	-0.056642	4.594726
277.934588	7257.417058	14.941184	-0.056658	4.592221
277.493324	7249.392455	14.946189	-0.056571	4.589711
277.714377	7241.398693	14.951194	-0.056607	4.587211
277.725577	7233.353569	14.956199	-0.056604	4.584693
277.570302	7225.446415	14.961203	-0.056570	4.582217
277.490673	7217.363833	14.966208	-0.056550	4.579685
277.262255	7209.388251	14.971213	-0.056502	4.577184
277.288708	7201.386612	14.976218	-0.056502	4.574674
277.273963	7193.396600	14.981223	-0.056494	4.572166
277.037037	7185.366793	14.986227	-0.056445	4.569644
277.261551	7177.357127	14.991232	-0.056481	4.567128
277.507616	7169.298025	14.996237	-0.056522	4.564596
277.325889	7161.470766	15.001242	-0.056483	4.562133
277.434583	7153.333177	15.006247	-0.056498	4.559573
277.162606	7145.444971	15.011251	-0.056442	4.557088
276.975292	7137.365338	15.016256	-0.056402	4.554542
277.038477	7129.370420	15.021261	-0.056409	4.552022
277.366856	7121.319291	15.026266	-0.056465	4.549484
277.381273	7113.320739	15.031271	-0.056462	4.546959
277.205867	7105.296675	15.036275	-0.056424	4.544425
277.297281	7097.342924	15.041280	-0.056436	4.541913
276.952363	7089.306728	15.046285	-0.056367	4.539371
276.978223	7081.392079	15.051290	-0.056366	4.536868
276.993007	7073.288597	15.056295	-0.056364	4.534304
277.261525	7065.311415	15.061299	-0.056409	4.531779
276.890077	7057.279951	15.066304	-0.056334	4.529233
276.781393	7049.340080	15.071309	-0.056309	4.526716
276.857228	7041.301407	15.076314	-0.056318	4.524166
276.883965	7033.353325	15.081319	-0.056318	4.521644
277.133497	7025.313901	15.086323	-0.056359	4.519092
276.852233	7017.399679	15.091328	-0.056302	4.516577
276.839644	7009.287679	15.096333	-0.056294	4.513998
276.787287	7001.362312	15.101338	-0.056279	4.511477
276.756789	6993.269528	15.106343	-0.056268	4.508901
276.961255	6985.276648	15.111347	-0.056301	4.506357
276.921570	6977.286222	15.116352	-0.056289	4.503811
276.520817	6969.356600	15.121357	-0.056209	4.501281
276.708662	6961.284435	15.126362	-0.056239	4.498707
276.734015	6953.267751	15.131367	-0.056238	4.496149
276.456362	6945.294660	15.136371	-0.056181	4.493602
276.091342	6937.298030	15.141376	-0.056108	4.491045
275.976088	6929.281360	15.146381	-0.056081	4.488481
276.213614	6921.266591	15.151386	-0.056121	4.485919
276.058645	6913.242102	15.156391	-0.056086	4.483350
276.430725	6905.227749	15.161395	-0.056151	4.480784
276.444737	6897.232549	15.166400	-0.056148	4.478223
276.161390	6889.291857	15.171405	-0.056090	4.475675
276.120138	6881.285227	15.176410	-0.056077	4.473107
276.394883	6873.205734	15.181415	-0.056123	4.470514
276.297468	6865.242194	15.186419	-0.056100	4.467956
276.155977	6857.191651	15.191424	-0.056068	4.465368
275.637503	6849.272831	15.196429	-0.055967	4.462820
275.563351	6841.286993	15.201434	-0.055948	4.460250
275.403968	6833.250876	15.206439	-0.055913	4.457662
275.710468	6825.230638	15.211443	-0.055965	4.455080
275.613631	6817.259074	15.216448	-0.055942	4.452510
275.627751	6809.195538	15.221453	-0.055939	4.449910
275.655295	6801.256440	15.226458	-0.055939	4.447348
275.802907	6793.137241	15.231463	-0.055961	4.444728
276.014313	6785.227509	15.236467	-0.055995	4.442174
275.797129	6777.178805	15.241472	-0.055950	4.439571
276.073794	6769.201812	15.246477	-0.055996	4.436992
275.929844	6761.202811	15.251482	-0.055964	4.434403
275.573325	6753.224766	15.256487	-0.055893	4.431818
275.818549	6745.188953	15.261491	-0.055933	4.429216
275.718368	6737.207222	15.266496	-0.055909	4.426627
275.339823	6729.152449	15.271501	-0.055834	4.424012
275.499853	6721.242849	15.276506	-0.055858	4.421446
275.146526	6713.221290	15.281511	-0.055787	4.418839
275.286888	6705.242540	15.286515	-0.055808	4.416247
275.122315	6697.192537	15.291520	-0.055772	4.413629
275.136445	6689.178544	15.296525	-0.055770	4.411021
275.125070	6681.235933	15.301530	-0.055763	4.408436
274.996101	6673.200609	15.306535	-0.055733	4.405818
275.372858	6665.144950	15.311539	-0.055798	4.403195
275.446660	6657.208056	15.316544	-0.055807	4.400607
275.036467	6649.243334	15.321549	-0.055725	4.398005
275.196338	6641.251991	15.326554	-0.055750	4.395397
275.584752	6633.181414	15.331559	-0.055817	4.392763
275.444498	6625.181713	15.336563	-0.055786	4.390147
275.182601	6617.258058	15.341568	-0.055732	4.387554
274.847270	6609.259670	15.346573	-0.055664	4.384934
274.790874	6601.328008	15.351578	-0.055649	4.382336
274.642314	6593.276353	15.356583	-0.055616	4.379697
274.522555	6585.364175	15.361587	-0.055588	4.377102
274.752789	6577.239887	15.366592	-0.055626	4.374438
275.013817	6569.239589	15.371597	-0.055669	4.371813
274.779408	6561.269145	15.376602	-0.055621	4.369194
275.018050	6553.235163	15.381607	-0.055660	4.366555
275.320192	6545.187445	15.386611	-0.055711	4.363911
275.260657	6537.284495	15.391616	-0.055695	4.361310
274.999055	6529.298941	15.396621	-0.055641	4.358679
275.151919	6521.325861	15.401626	-0.055664	4.356053
274.927322	6513.231830	15.406631	-0.055617	4.353383
274.792968	6505.238214	15.411635	-0.055587	4.350745
274.856935	6497.229710	15.416640	-0.055594	4.348102
274.626011	6489.221715	15.421645	-0.055546	4.345456
274.255012	6481.324051	15.426650	-0.055471	4.342843
274.237354	6473.267978	15.431655	-0.055463	4.340179
274.135576	6465.285886	15.436659	-0.055439	4.337537
273.963440	6457.255752	15.441664	-0.055401	4.334877
274.161587	6449.189446	15.446669	-0.055433	4.332207
273.955514	6441.259564	15.451674	-0.055390	4.329577
273.726870	6433.296578	15.456679	-0.055342	4.326933
273.835232	6425.208726	15.461683	-0.055357	4.324250
274.193866	6417.263275	15.466688	-0.055419	4.321614
274.033362	6409.225968	15.471693	-0.055383	4.318942
274.343003	6401.258519	15.476698	-0.055436	4.316296
274.120640	6393.252478	15.481703	-0.055389	4.313630
273.856753	6385.261010	15.486707	-0.055335	4.310968
273.980280	6377.211883	15.491712	-0.055353	4.308287
273.686041	6369.232222	15.496717	-0.055293	4.305625
274.469717	6361.151971	15.501722	-0.055434	4.302937
274.616831	6353.130134	15.506727	-0.055456	4.300261
274.115592	6345.212193	15.511731	-0.055357	4.297612
274.252614	6337.222073	15.516736	-0.055378	4.294944
273.995810	6329.213204	15.521741	-0.055325	4.292263
273.879808	6321.238186	15.526746	-0.055298	4.289594
273.704645	6313.219500	15.531751	-0.055260	4.286908
273.678679	6305.201715	15.536755	-0.055250	4.284222
273.461902	6297.283774	15.541760	-0.055205	4.281565
273.672090	6289.160448	15.546765	-0.055239	4.278843
273.765127	6281.259462	15.551770	-0.055251	4.276192
273.633873	6273.188623	15.556775	-0.055221	4.273480
273.578563	6265.231272	15.561779	-0.055206	4.270805
273.503965	6257.200609	15.566784	-0.055187	4.268104
273.555795	6249.141652	15.571789	-0.055191	4.265393
274.086684	6241.166259	15.576794	-0.055285	4.262713
273.905853	6233.165095	15.581799	-0.055246	4.260016
273.851977	6225.194881	15.586803	-0.055231	4.257328
273.511505	6217.235641	15.591808	-0.055162	4.254640
273.515091	6209.187866	15.596813	-0.055158	4.251924
273.228245	6201.236395	15.601818	-0.055099	4.249235
273.263651	6193.161926	15.606823	-0.055100	4.246506
273.578194	6185.133794	15.611827	-0.055154	4.243794
273.150287	6177.260248	15.616832	-0.055069	4.241125
273.055266	6169.233894	15.621837	-0.055046	4.238407
273.034113	6161.203030	15.626842	-0.055037	4.235685
272.808860	6153.161756	15.631847	-0.054990	4.232956
272.681625	6145.199894	15.636851	-0.054961	4.230253
272.750846	6137.179848	15.641856	-0.054969	4.227531
273.197273	6129.069107	15.646861	-0.055047	4.224781
273.244473	6121.180322	15.651866	-0.055050	4.222100
272.865650	6113.160050	15.656871	-0.054975	4.219367
272.709667	6105.215715	15.661875	-0.054940	4.216661
273.025210	6097.149095	15.666880	-0.054994	4.213918
272.551970	6089.225681	15.671885	-0.054901	4.211212
272.594598	6081.206032	15.676890	-0.054903	4.208477
272.357884	6073.205600	15.681895	-0.054854	4.205744
272.167294	6065.230840	15.686899	-0.054814	4.203019
272.233497	6057.219678	15.691904	-0.054821	4.200282
272.175443	6049.200648	15.696909	-0.054805	4.197539
272.353143	6041.175091	15.701914	-0.054833	4.194795
272.038821	6033.147216	15.706919	-0.054769	4.192043
271.908623	6025.126510	15.711923	-0.054739	4.189293
271.699697	6017.165789	15.716928	-0.054695	4.186562
271.556506	6009.107052	15.721933	-0.054664	4.183795
271.902240	6001.194521	15.726938	-0.054723	4.181083
272.192177	5993.093648	15.731943	-0.054772	4.178304
272.329321	5985.143366	15.736947	-0.054792	4.175573
272.016200	5977.169134	15.741952	-0.054728	4.172826
271.962388	5969.105638	15.746957	-0.054713	4.170050
272.286736	5961.150626	15.751962	-0.054768	4.167314
272.119278	5953.123681	15.756967	-0.054732	4.164546
272.116394	5945.225485	15.761971	-0.054726	4.161822
272.148801	5937.169280	15.766976	-0.054727	4.159042
272.479471	5929.166984	15.771981	-0.054784	4.156283
272.219209	5921.202855	15.776986	-0.054730	4.153527
272.016419	5913.195932	15.781991	-0.054687	4.150756
271.949819	5905.208231	15.786995	-0.054670	4.147991
271.830643	5897.211668	15.792000	-0.054642	4.145220
272.071074	5889.168021	15.797005	-0.054682	4.142436
271.739658	5881.233585	15.802010	-0.054615	4.139681
271.569923	5873.191286	15.807015	-0.054578	4.136888
271.884000	5865.116831	15.812019	-0.054631	4.134089
271.837955	5857.192030	15.817024	-0.054618	4.131335
271.526843	5849.220095	15.822029	-0.054555	4.128559
271.879934	5841.181728	15.827034	-0.054615	4.125768
271.230296	5833.244856	15.832039	-0.054489	4.122996
271.406244	5825.210861	15.837043	-0.054517	4.120199
271.657370	5817.232965	15.842048	-0.054558	4.117422
271.546129	5809.177399	15.847053	-0.054532	4.114610
271.723127	5801.188172	15.852058	-0.054560	4.111824
271.469417	5793.170844	15.857063	-0.054508	4.109019
270.949826	5785.234224	15.862067	-0.054406	4.106238
271.113804	5777.192229	15.867072	-0.054431	4.103427
271.266036	5769.167758	15.872077	-0.054454	4.100620
271.841513	5761.117860	15.877082	-0.054556	4.097809
271.716685	5753.112140	15.882087	-0.054528	4.095001
271.519023	5745.181743	15.887091	-0.054486	4.092217
271.687538	5737.153452	15.892096	-0.054512	4.089401
271.791931	5729.136883	15.897101	-0.054526	4.086587
271.410665	5721.178316	15.902106	-0.054450	4.083784
271.183904	5713.231233	15.907111	-0.054403	4.080985
271.390503	5705.212675	15.912115	-0.054436	4.078166
271.284985	5697.198793	15.917120	-0.054411	4.075342
271.847308	5689.127209	15.922125	-0.054511	4.072506
271.766510	5681.191500	15.927130	-0.054491	4.069706
271.803090	5673.133279	15.932135	-0.054492	4.066862
271.703992	5665.141395	15.937139	-0.054469	4.064038
271.692348	5657.215741	15.942144	-0.054461	4.061237
271.622027	5649.168437	15.947149	-0.054443	4.058389
271.711183	5641.193831	15.952154	-0.054454	4.055568
271.150455	5633.213972	15.957159	-0.054345	4.052733
270.762354	5625.247203	15.962163	-0.054267	4.049903
271.238500	5617.200793	15.967168	-0.054351	4.047057
270.886789	5609.174261	15.972173	-0.054280	4.044203
271.379436	5601.248933	15.977178	-0.054367	4.041396
271.152354	5593.176320	15.982183	-0.054319	4.038523
271.141128	5585.228695	15.987187	-0.054312	4.035696
271.169316	5577.225222	15.992192	-0.054312	4.032848
270.998299	5569.167338	15.997197	-0.054275	4.029975
271.359605	5561.139727	16.002202	-0.054337	4.027119
270.806320	5553.174081	16.007207	-0.054229	4.024269
271.117460	5545.197668	16.012211	-0.054282	4.021427
270.945196	5537.211806	16.017216	-0.054245	4.018572
270.473167	5529.286810	16.022221	-0.054152	4.015731
270.339015	5521.280154	16.027226	-0.054121	4.012865
270.489672	5513.211744	16.032231	-0.054144	4.009979
270.731499	5505.188312	16.037235	-0.054184	4.007109
270.814192	5497.136341	16.042240	-0.054194	4.004224
270.738612	5489.274334	16.047245	-0.054175	4.001402
270.490953	5481.287094	16.052250	-0.054124	3.998531
270.709010	5473.213707	16.057255	-0.054159	3.995634
270.649293	5465.220329	16.062259	-0.054143	3.992759
270.720590	5457.213348	16.067264	-0.054151	3.989880
270.543072	5449.239024	16.072269	-0.054113	3.987006
270.640302	5441.218068	16.077274	-0.054126	3.984118
270.426914	5433.259748	16.082279	-0.054081	3.981244
270.439096	5425.226050	16.087283	-0.054078	3.978346
270.204271	5417.307279	16.092288	-0.054029	3.975482
270.404599	5409.231843	16.097293	-0.054061	3.972568
270.321981	5401.224747	16.102298	-0.054041	3.969671
270.256073	5393.233911	16.107303	-0.054023	3.966778
270.317020	5385.234783	16.112307	-0.054029	3.963883
269.871530	5377.317072	16.117312	-0.053941	3.961005
270.555298	5369.158597	16.122317	-0.054063	3.958059
270.464948	5361.242324	16.127322	-0.054041	3.955184
270.475653	5353.211534	16.132327	-0.054038	3.952267
270.452514	5345.216748	16.137331	-0.054029	3.949361
270.368447	5337.234440	16.142336	-0.054008	3.946456
270.440381	5329.165094	16.147341	-0.054016	3.943520
270.291891	5321.257979	16.152346	-0.053983	3.940637
270.237221	5313.222554	16.157351	-0.053968	3.937707
270.633941	5305.189176	16.162355	-0.054037	3.934784
270.620325	5297.250707	16.167360	-0.054029	3.931885
270.221905	5289.238464	16.172365	-0.053950	3.928950
270.601247	5281.237293	16.177370	-0.054015	3.926032
270.027578	5273.279770	16.182375	-0.053903	3.923109
269.866773	5265.305555	16.187379	-0.053868	3.920186
270.213323	5257.294874	16.192384	-0.053927	3.917257
270.296444	5249.248030	16.197389	-0.053938	3.914308
270.114573	5241.334607	16.202394	-0.053899	3.911400
269.855246	5233.297938	16.207399	-0.053845	3.908443
269.665836	5225.307824	16.212403	-0.053805	3.905503
270.003948	5217.305247	16.217408	-0.053862	3.902566
269.357459	5209.321713	16.222413	-0.053737	3.899614
269.704595	5201.338258	16.227418	-0.053796	3.896680
269.198679	5193.349252	16.232423	-0.053697	3.893724
269.458211	5185.304771	16.237427	-0.053740	3.890762
269.779681	5177.266258	16.242432	-0.053795	3.887800
269.636075	5169.258782	16.247437	-0.053763	3.884838
269.638151	5161.343019	16.252442	-0.053758	3.881911
269.809314	5153.246666	16.257447	-0.053785	3.878918
269.673950	5145.376808	16.262451	-0.053754	3.876001
269.726770	5137.252248	16.267456	-0.053759	3.872990
269.429247	5129.207673	16.272461	-0.053698	3.870000
269.462153	5121.278459	16.277466	-0.053699	3.867057
269.479306	5113.224284	16.282471	-0.053697	3.864066
269.574251	5105.317112	16.287475	-0.053710	3.861128
269.580765	5097.285959	16.292480	-0.053706	3.858140
269.341811	5089.296961	16.297485	-0.053656	3.855160
269.632113	5081.293714	16.302490	-0.053705	3.852184
269.046813	5073.320524	16.307495	-0.053591	3.849197
268.953625	5065.361943	16.312499	-0.053569	3.846225
269.354521	5057.287982	16.317504	-0.053638	3.843218
269.116308	5049.296838	16.322509	-0.053588	3.840225
269.952358	5041.298133	16.327514	-0.053739	3.837251
269.187845	5033.359611	16.332519	-0.053591	3.834262
269.094452	5025.369604	16.337523	-0.053569	3.831266
268.811051	5017.354724	16.342528	-0.053511	3.828255
268.907833	5009.319490	16.347533	-0.053524	3.825241
268.856885	5001.380806	16.352538	-0.053509	3.822259
268.735016	4993.338019	16.357543	-0.053481	3.819233
269.003915	4985.386856	16.362547	-0.053526	3.816248
268.972500	4977.316503	16.367552	-0.053515	3.813209
268.900227	4969.310571	16.372557	-0.053497	3.810191
269.180141	4961.333512	16.377562	-0.053543	3.807189
268.894438	4953.332559	16.382567	-0.053485	3.804163
268.742090	4945.449775	16.387571	-0.053452	3.801183
268.954645	4937.398965	16.392576	-0.053486	3.798145
268.942158	4929.392267	16.397581	-0.053479	3.795116
268.894656	4921.419686	16.402586	-0.053465	3.792097
268.542091	4913.397395	16.407591	-0.053394	3.789049
268.551151	4905.432531	16.412595	-0.053390	3.786029
268.928502	4897.341729	16.417600	-0.053455	3.782968
268.039984	4889.450562	16.422605	-0.053285	3.779949
268.034541	4881.452496	16.427610	-0.053279	3.776909
268.039722	4873.375714	16.432615	-0.053274	3.773837
267.706749	4865.481744	16.437619	-0.053207	3.770824
267.431491	4857.490665	16.442624	-0.053151	3.767772
267.339296	4849.450389	16.447629	-0.053128	3.764704
267.769020	4841.456298	16.452634	-0.053203	3.761663
267.716603	4833.420808	16.457639	-0.053188	3.758593
267.858241	4825.436643	16.462643	-0.053209	3.755544
268.038392	4817.429517	16.467648	-0.053238	3.752485
267.471405	4809.456560	16.472653	-0.053127	3.749418
268.077623	4801.388581	16.477658	-0.053235	3.746342
267.947732	4793.407182	16.482663	-0.053205	3.743277
268.168586	4785.417733	16.487667	-0.053241	3.740216
268.291544	4777.433800	16.492672	-0.053259	3.737152
268.351165	4769.379333	16.497677	-0.053265	3.734057
268.456912	4761.455024	16.502682	-0.053280	3.731011
268.075416	4753.457334	16.507687	-0.053203	3.727921
267.999718	4745.486779	16.512691	-0.053184	3.724847
267.903400	4737.554140	16.517696	-0.053161	3.721785
267.629623	4729.536373	16.522701	-0.053105	3.718683
267.502857	4721.575418	16.527706	-0.053076	3.715603
267.626115	4713.483403	16.532711	-0.053094	3.712477
267.719493	4705.432405	16.537715	-0.053106	3.709364
267.132995	4697.524769	16.542720	-0.052992	3.706285
267.572509	4689.413280	16.547725	-0.053068	3.703152
267.398195	4681.518774	16.552730	-0.053031	3.700085
267.347752	4673.488315	16.557735	-0.053016	3.696965
267.308165	4665.484802	16.562739	-0.053004	3.693853
267.720426	4657.450094	16.567744	-0.053075	3.690739
267.662450	4649.446060	16.572749	-0.053059	3.687621
268.030307	4641.402870	16.577754	-0.053123	3.684497
267.919478	4633.492017	16.582759	-0.053097	3.681409
267.666014	4625.546499	16.587763	-0.053044	3.678301
267.702951	4617.573398	16.592768	-0.053046	3.675187
267.509006	4609.554373	16.597773	-0.053005	3.672047
267.857820	4601.525375	16.602778	-0.053065	3.668914
267.886574	4593.532526	16.607783	-0.053065	3.665785
267.372139	4585.627388	16.612787	-0.052964	3.662672
267.389360	4577.590982	16.617792	-0.052962	3.659520
267.446987	4569.582507	16.622797	-0.052967	3.656377
267.683446	4561.573081	16.627802	-0.053006	3.653236
267.621965	4553.567660	16.632807	-0.052990	3.650086
267.540517	4545.607854	16.637811	-0.052969	3.646950
267.165987	4537.633748	16.642816	-0.052894	3.643798
267.378979	4529.607517	16.647821	-0.052929	3.640639
267.269145	4521.666534	16.652826	-0.052903	3.637501
266.698479	4513.681676	16.657831	-0.052792	3.634331
267.026833	4505.615112	16.662835	-0.052848	3.631151
266.755186	4497.655393	16.667840	-0.052792	3.627993
266.828077	4489.589647	16.672845	-0.052800	3.624801
267.280988	4481.609780	16.677850	-0.052880	3.621650
266.744747	4473.639929	16.682855	-0.052775	3.618473
266.798608	4465.651727	16.687859	-0.052780	3.615302
266.881359	4457.658202	16.692864	-0.052790	3.612127
266.876807	4449.562741	16.697869	-0.052784	3.608906
267.102009	4441.618348	16.702874	-0.052820	3.605750
267.089675	4433.650497	16.707879	-0.052813	3.602574
266.787416	4425.686780	16.712883	-0.052752	3.599389
266.765408	4417.758026	16.717888	-0.052742	3.596223
266.730817	4409.674759	16.722893	-0.052731	3.592992
266.867050	4401.670374	16.727898	-0.052751	3.589795
266.693350	4393.682875	16.732903	-0.052713	3.586592
266.729646	4385.653435	16.737907	-0.052715	3.583376
266.769468	4377.724310	16.742912	-0.052717	3.580197
266.847976	4369.678025	16.747917	-0.052727	3.576970
266.843713	4361.732195	16.752922	-0.052721	3.573778
266.486576	4353.736254	16.757927	-0.052649	3.570552
266.480548	4345.740557	16.762931	-0.052643	3.567334
266.448809	4337.725368	16.767936	-0.052632	3.564104
266.397685	4329.784725	16.772941	-0.052617	3.560901
266.511244	4321.791544	16.777946	-0.052633	3.557679
266.585815	4313.762181	16.782951	-0.052642	3.554438
266.907253	4305.688027	16.787955	-0.052696	3.551183
266.642644	4297.723168	16.792960	-0.052642	3.547952
266.458939	4289.742518	16.797965	-0.052603	3.544714
266.473169	4281.804787	16.802970	-0.052600	3.541497
266.225280	4273.793790	16.807975	-0.052549	3.538238
266.071601	4265.812186	16.812979	-0.052515	3.534992
266.222125	4257.796697	16.817984	-0.052538	3.531738
266.190925	4249.777379	16.822989	-0.052527	3.528474
266.391925	4241.771888	16.827994	-0.052559	3.525220
265.761412	4233.857164	16.832999	-0.052436	3.521973
265.037021	4225.982637	16.838003	-0.052297	3.518737
265.253373	4217.917143	16.843008	-0.052332	3.515450
265.610039	4209.800706	16.848013	-0.052393	3.512143
265.561492	4201.841994	16.853018	-0.052379	3.508885
265.538842	4193.857410	16.858023	-0.052369	3.505614
265.164946	4185.896780	16.863027	-0.052294	3.502338
265.536382	4177.834227	16.868032	-0.052358	3.499042
265.551904	4169.834110	16.873037	-0.052356	3.495757
265.547993	4161.899995	16.878042	-0.052350	3.492495
265.152405	4153.856841	16.883047	-0.052271	3.489172
265.219643	4145.901753	16.888051	-0.052279	3.485898
265.427713	4137.874639	16.893056	-0.052312	3.482596
265.315390	4129.911182	16.898061	-0.052286	3.479306
265.226794	4121.965480	16.903066	-0.052265	3.476021
265.392905	4113.890426	16.908071	-0.052290	3.472688
265.671987	4105.874182	16.913075	-0.052337	3.469379
265.245930	4097.943314	16.918080	-0.052253	3.466080
265.333117	4089.954907	16.923085	-0.052264	3.462771
265.329167	4081.964277	16.928090	-0.052258	3.459454
265.150583	4073.994911	16.933095	-0.052219	3.456137
264.614331	4066.050727	16.938099	-0.052114	3.452815
265.286376	4057.903013	16.943104	-0.052234	3.449447
265.024916	4049.974239	16.948109	-0.052180	3.446135
265.194291	4041.977084	16.953114	-0.052207	3.442805
265.384248	4033.930564	16.958119	-0.052237	3.439453
265.147639	4026.057282	16.963123	-0.052188	3.436155
265.079691	4018.073141	16.968128	-0.052170	3.432813
265.666811	4009.930187	16.973133	-0.052274	3.429424
265.497713	4002.027470	16.978138	-0.052237	3.426107
265.438595	3994.035467	16.983143	-0.052221	3.422752
265.632798	3986.025525	16.988147	-0.052252	3.419396
265.420134	3978.077771	16.993152	-0.052208	3.416048
265.192801	3970.084270	16.998157	-0.052160	3.412676
265.583042	3962.030819	17.003162	-0.052228	3.409299
265.316013	3954.091400	17.008167	-0.052173	3.405942
265.382693	3946.108569	17.013171	-0.052180	3.402576
265.243528	3938.119430	17.018176	-0.052149	3.399197
265.218140	3930.146276	17.023181	-0.052139	3.395824
265.260605	3922.120677	17.028186	-0.052142	3.392429
264.659318	3914.126795	17.033191	-0.052025	3.389021
264.800878	3906.105168	17.038195	-0.052046	3.385624
265.016764	3898.113040	17.043200	-0.052081	3.382239
264.903625	3890.113246	17.048205	-0.052054	3.378835
264.954475	3882.139616	17.053210	-0.052059	3.375446
264.971776	3874.155642	17.058215	-0.052057	3.372047
264.504103	3866.205883	17.063219	-0.051965	3.368641
264.445650	3858.218400	17.068224	-0.051949	3.365231
263.682162	3850.361415	17.073229	-0.051801	3.361846
263.857985	3842.295991	17.078234	-0.051829	3.358405
263.574069	3834.301059	17.083239	-0.051771	3.354972
264.103696	3826.229635	17.088243	-0.051864	3.351534
263.994571	3818.258318	17.093248	-0.051839	3.348112
264.074531	3810.178889	17.098253	-0.051848	3.344646
264.185003	3802.274278	17.103258	-0.051864	3.341254
263.995585	3794.271566	17.108263	-0.051823	3.337804
264.062602	3786.252199	17.113267	-0.051831	3.334353
264.221251	3778.280699	17.118272	-0.051855	3.330923
264.157689	3770.263465	17.123277	-0.051838	3.327461
264.060294	3762.264145	17.128282	-0.051815	3.324002
264.225656	3754.313090	17.133287	-0.051840	3.320570
264.057202	3746.361317	17.138291	-0.051804	3.317122
263.805505	3738.420371	17.143296	-0.051752	3.313671
263.839780	3730.384264	17.148301	-0.051753	3.310186
263.512610	3722.441827	17.153306	-0.051687	3.306725
263.309964	3714.431233	17.158311	-0.051644	3.303235
263.472738	3706.388771	17.163315	-0.051669	3.299741
263.729594	3698.375536	17.168320	-0.051712	3.296261
263.544748	3690.368807	17.173325	-0.051672	3.292762
263.707616	3682.374567	17.178330	-0.051697	3.289279
263.001971	3674.488447	17.183335	-0.051561	3.285804
263.239960	3666.461431	17.188339	-0.051600	3.282303
262.858353	3658.510680	17.193344	-0.051524	3.278805
263.279322	3650.420430	17.198349	-0.051597	3.275276
263.518258	3642.444428	17.203354	-0.051636	3.271785
263.253124	3634.472452	17.208359	-0.051582	3.268272
263.574433	3626.427702	17.213363	-0.051636	3.264747
263.503876	3618.500281	17.218368	-0.051618	3.261253
263.420497	3610.493388	17.223373	-0.051598	3.257721
263.149713	3602.586300	17.228378	-0.051542	3.254221
262.930675	3594.603180	17.233383	-0.051496	3.250685
262.858301	3586.596027	17.238387	-0.051477	3.247142
262.893244	3578.593897	17.243392	-0.051479	3.243601
262.934950	3570.582955	17.248397	-0.051481	3.240052
262.947955	3562.628497	17.253402	-0.051479	3.236524
262.871523	3554.613198	17.258407	-0.051459	3.232961
262.535651	3546.664379	17.263411	-0.051391	3.229412
262.428422	3538.675385	17.268416	-0.051366	3.225851
262.218236	3530.640659	17.273421	-0.051322	3.222262
262.976164	3522.566622	17.278426	-0.051458	3.218692
263.136510	3514.566729	17.283431	-0.051483	3.215126
262.847982	3506.631925	17.288435	-0.051424	3.211566
262.565570	3498.678986	17.293440	-0.051366	3.207994
262.759774	3490.631379	17.298445	-0.051397	3.204397
262.866888	3482.683191	17.303450	-0.051412	3.200836
262.511645	3474.744707	17.308455	-0.051341	3.197255
262.283282	3466.791211	17.313459	-0.051293	3.193669
262.226930	3458.794722	17.318464	-0.051277	3.190067
262.645474	3450.678732	17.323469	-0.051350	3.186428
262.537330	3442.756595	17.328474	-0.051325	3.182850
262.800408	3434.686985	17.333479	-0.051368	3.179216
263.066042	3426.725591	17.338483	-0.051413	3.175628
262.664175	3418.829510	17.343488	-0.051333	3.172036
262.545248	3410.829424	17.348493	-0.051305	3.168405
262.696657	3402.830546	17.353498	-0.051328	3.164783
262.721782	3394.833966	17.358503	-0.051328	3.161152
262.860770	3386.828459	17.363507	-0.051349	3.157517
262.779965	3378.879894	17.368512	-0.051328	3.153895
262.233560	3370.946960	17.373517	-0.051222	3.150254
262.489598	3362.897951	17.378522	-0.051264	3.146593
262.380823	3354.901324	17.383527	-0.051239	3.142934
262.372955	3346.914917	17.388531	-0.051232	3.139281
262.090474	3338.989098	17.393536	-0.051174	3.135639
262.487270	3330.903910	17.398541	-0.051243	3.131950
262.702690	3322.902661	17.403546	-0.051278	3.128287
262.633335	3314.923679	17.408551	-0.051260	3.124617
262.264297	3307.041927	17.413555	-0.051186	3.120974
262.569747	3299.022272	17.418560	-0.051238	3.117294
262.694645	3290.985531	17.423565	-0.051256	3.113594
262.538969	3283.080626	17.428570	-0.051222	3.109936
262.111322	3275.110099	17.433575	-0.051137	3.106232
262.098679	3267.103070	17.438579	-0.051129	3.102525
262.057354	3259.117292	17.443584	-0.051116	3.098823
262.111046	3251.095069	17.448589	-0.051121	3.095104
261.791322	3243.188483	17.453594	-0.051057	3.091416
261.472253	3235.199512	17.458599	-0.050992	3.087686
261.438644	3227.164934	17.463603	-0.050981	3.083943
261.457834	3219.239779	17.468608	-0.050979	3.080249
261.351418	3211.228097	17.473613	-0.050954	3.076505
261.723310	3203.147489	17.478618	-0.051018	3.072747
261.705697	3195.130853	17.483623	-0.051010	3.068995
261.431048	3187.175298	17.488627	-0.050953	3.065255
261.744374	3179.143300	17.493632	-0.051006	3.061503
261.472776	3171.214360	17.498637	-0.050951	3.057766
261.597574	3163.236046	17.503642	-0.050969	3.054021
261.166223	3155.298320	17.508647	-0.050883	3.050263
261.131877	3147.317178	17.513651	-0.050872	3.046499
261.440249	3139.300766	17.518656	-0.050924	3.042731
261.715756	3131.257957	17.523661	-0.050970	3.038945
261.803374	3123.303479	17.528666	-0.050981	3.035186
261.452034	3115.372766	17.533671	-0.050911	3.031412
261.446555	3107.377466	17.538675	-0.050905	3.027619
261.380569	3099.393984	17.543680	-0.050887	3.023825
261.158116	3091.450909	17.548685	-0.050841	3.020037
261.292837	3083.444633	17.553690	-0.050861	3.016232
261.257872	3075.430427	17.558695	-0.050849	3.012410
261.291483	3067.441988	17.563699	-0.050850	3.008599
261.345187	3059.476529	17.568704	-0.050855	3.004795
261.397901	3051.486676	17.573709	-0.050859	3.000975
261.110880	3043.570693	17.578714	-0.050801	2.997168
260.823962	3035.602471	17.583719	-0.050742	2.993330
261.211326	3027.517612	17.588723	-0.050809	2.989467
261.056965	3019.566180	17.593728	-0.050775	2.985635
261.211982	3011.554752	17.598733	-0.050799	2.981784
260.883444	3003.651115	17.603738	-0.050733	2.977956
260.866005	2995.614944	17.608743	-0.050724	2.974075
260.717992	2987.653764	17.613747	-0.050692	2.970219
261.044147	2979.639264	17.618752	-0.050747	2.966356
260.966860	2971.643520	17.623757	-0.050728	2.962476
260.892966	2963.711278	17.628762	-0.050709	2.958623
260.486901	2955.779452	17.633767	-0.050628	2.954746
260.861219	2947.717122	17.638771	-0.050692	2.950843
260.516263	2939.788887	17.643776	-0.050623	2.946961
260.495629	2931.781972	17.648781	-0.050614	2.943054
260.419526	2923.844805	17.653786	-0.050595	2.939172
260.491904	2915.813165	17.658791	-0.050603	2.935246
260.336323	2907.851138	17.663795	-0.050569	2.931338
260.502151	2899.819767	17.668800	-0.050595	2.927407
260.529445	2891.832217	17.673805	-0.050594	2.923485
260.381072	2883.906573	17.678810	-0.050562	2.919579
260.227688	2875.968099	17.683815	-0.050528	2.915661
260.391912	2867.900647	17.688819	-0.050553	2.911691
260.002290	2859.941869	17.693824	-0.050476	2.907739
259.921822	2851.934356	17.698829	-0.050456	2.903775
260.141227	2843.954674	17.703834	-0.050491	2.899836
260.336076	2835.940024	17.708839	-0.050522	2.895872
260.164518	2828.006906	17.713843	-0.050485	2.891924
260.097429	2820.031556	17.718848	-0.050468	2.887954
260.216415	2811.992359	17.723853	-0.050485	2.883958
260.342225	2804.061708	17.728858	-0.050503	2.880011
260.137609	2796.119849	17.733863	-0.050460	2.876034
260.503437	2788.072705	17.738867	-0.050523	2.872031
260.066418	2780.167518	17.743872	-0.050436	2.868049
260.010389	2772.153727	17.748877	-0.050420	2.864028
259.960556	2764.240615	17.753882	-0.050406	2.860052
259.918286	2756.225359	17.758887	-0.050393	2.856019
259.854123	2748.230142	17.763891	-0.050376	2.851990
259.713831	2740.278479	17.768896	-0.050345	2.847973
259.599227	2732.285739	17.773901	-0.050318	2.843930
259.553792	2724.351399	17.778906	-0.050305	2.839916
259.670431	2716.331423	17.783911	-0.050321	2.835861
259.911294	2708.321466	17.788915	-0.050361	2.831814
259.940618	2700.352759	17.793920	-0.050361	2.827769
259.628994	2692.362439	17.798925	-0.050298	2.823687
259.673121	2684.416182	17.803930	-0.050301	2.819643
259.515464	2676.448416	17.808935	-0.050266	2.815570
259.502325	2668.455938	17.813939	-0.050259	2.811487
259.310535	2660.494636	17.818944	-0.050218	2.807403
259.262478	2652.493563	17.823949	-0.050204	2.803302
259.296214	2644.551844	17.828954	-0.050205	2.799230
258.940570	2636.630741	17.833959	-0.050134	2.795139
258.769627	2628.656754	17.838963	-0.050097	2.791026
258.604307	2620.655207	17.843968	-0.050061	2.786893
258.385418	2612.667077	17.848973	-0.050015	2.782758
258.739279	2604.633209	17.853978	-0.050075	2.778628
258.973741	2596.625761	17.858983	-0.050114	2.774498
258.908944	2588.646774	17.863987	-0.050097	2.770358
259.188731	2580.646215	17.868992	-0.050144	2.766222
259.449755	2572.647084	17.873997	-0.050187	2.762079
259.599923	2564.695724	17.879002	-0.050210	2.757948
259.152373	2556.797894	17.884007	-0.050121	2.753802
259.391593	2548.740873	17.889011	-0.050161	2.749610
259.241642	2540.802038	17.894016	-0.050128	2.745448
258.820949	2532.895738	17.899021	-0.050044	2.741280
259.272666	2524.860502	17.904026	-0.050123	2.737093
258.879400	2516.939702	17.909031	-0.050045	2.732906
258.672513	2508.965627	17.914035	-0.050001	2.728697
258.724754	2500.968690	17.919040	-0.050006	2.724485
259.125878	2492.942096	17.924045	-0.050075	2.720274
258.939156	2485.037509	17.929050	-0.050035	2.716083
258.643614	2477.078244	17.934055	-0.049975	2.711849
258.608393	2469.092445	17.939059	-0.049963	2.707612
258.782323	2461.103814	17.944064	-0.049991	2.703380
258.384232	2453.177053	17.949069	-0.049911	2.699137
258.859454	2445.155106	17.954074	-0.049995	2.694893
258.414591	2437.230610	17.959079	-0.049907	2.690635
258.377176	2429.242984	17.964083	-0.049895	2.686363
258.277171	2421.293205	17.969088	-0.049871	2.682100
258.293200	2413.290737	17.974093	-0.049869	2.677810
257.973873	2405.375261	17.979098	-0.049804	2.673537
257.610750	2397.413049	17.984103	-0.049731	2.669230
257.916789	2389.352156	17.989107	-0.049783	2.664906
257.606340	2381.452851	17.994112	-0.049720	2.660622
257.898803	2373.393463	17.999117	-0.049769	2.656285
257.855297	2365.454211	18.004122	-0.049756	2.651983
257.542523	2357.500763	18.009127	-0.049693	2.647649
257.662770	2349.482781	18.014131	-0.049710	2.643301
257.817425	2341.507186	18.019136	-0.049734	2.638972
257.754869	2333.569275	18.024141	-0.049717	2.634641
257.704626	2325.608634	18.029146	-0.049702	2.630291
257.337938	2317.676941	18.034151	-0.049629	2.625929
257.148389	2309.711763	18.039155	-0.049589	2.621553
257.394094	2301.695644	18.044160	-0.049629	2.617172
256.949160	2293.776413	18.049165	-0.049541	2.612789
256.735794	2285.841699	18.054170	-0.049496	2.608406
256.757020	2277.836402	18.059175	-0.049495	2.603993
256.895527	2269.833862	18.064179	-0.049516	2.599582
257.049991	2261.860284	18.069184	-0.049539	2.595180
256.509799	2253.858884	18.074189	-0.049433	2.590708
256.892708	2245.796856	18.079194	-0.049500	2.586258
256.858311	2237.845013	18.084199	-0.049488	2.581833
256.590767	2229.955399	18.089203	-0.049433	2.577419
256.765666	2221.936954	18.094208	-0.049460	2.572956
256.273475	2214.046393	18.099213	-0.049364	2.568509
256.438715	2206.047944	18.104218	-0.049389	2.564042
256.623875	2198.061904	18.109223	-0.049419	2.559575
256.404386	2190.155229	18.114227	-0.049373	2.555115
256.383940	2182.184675	18.119232	-0.049364	2.550626
256.568608	2174.144648	18.124237	-0.049393	2.546105
256.621598	2166.180942	18.129242	-0.049398	2.541610
256.160869	2158.313258	18.134247	-0.049307	2.537123
256.096951	2150.330326	18.139251	-0.049290	2.532592
256.351085	2142.316068	18.144256	-0.049332	2.528059
256.165716	2134.354095	18.149261	-0.049292	2.523515
256.122243	2126.435566	18.154266	-0.049279	2.518997
256.548359	2118.386651	18.159271	-0.049353	2.514432
256.341954	2110.469498	18.164275	-0.049310	2.509887
256.472228	2102.461068	18.169280	-0.049329	2.505307
256.178551	2094.545392	18.174285	-0.049269	2.500740
256.214276	2086.596589	18.179290	-0.049270	2.496170
256.234129	2078.601874	18.184295	-0.049269	2.491564
256.031516	2070.656642	18.189299	-0.049226	2.486961
255.784217	2062.768747	18.194304	-0.049175	2.482379
255.835387	2054.763636	18.199309	-0.049179	2.477744
255.577285	2046.841154	18.204314	-0.049126	2.473124
255.764212	2038.829068	18.209319	-0.049156	2.468478
255.905856	2030.828265	18.214323	-0.049177	2.463826
255.727809	2022.922779	18.219328	-0.049139	2.459196
255.281142	2015.019470	18.224333	-0.049050	2.454538
256.079509	2006.903902	18.229338	-0.049194	2.449843
255.658116	1999.017859	18.234343	-0.049110	2.445179
255.805696	1991.050004	18.239347	-0.049132	2.440503
255.997467	1983.068970	18.244352	-0.049163	2.435813
255.998743	1975.074888	18.249357	-0.049158	2.431091
256.230330	1967.087816	18.254362	-0.049196	2.426383
255.946356	1959.169276	18.259367	-0.049138	2.421665
256.103612	1951.176483	18.264371	-0.049162	2.416929
255.617421	1943.330562	18.269376	-0.049067	2.412220
255.503816	1935.351828	18.274381	-0.049040	2.407452
255.511747	1927.409991	18.279386	-0.049037	2.402706
255.523819	1919.422594	18.284391	-0.049034	2.397924
255.731495	1911.433398	18.289395	-0.049067	2.393148
255.796455	1903.477662	18.294400	-0.049074	2.388370
255.552560	1895.538008	18.299405	-0.049024	2.383567
255.320173	1887.648862	18.304410	-0.048975	2.378786
255.329851	1879.671837	18.309415	-0.048972	2.373962
255.077250	1871.734424	18.314419	-0.048920	2.369130
255.305209	1863.713547	18.319424	-0.048957	2.364278
255.090091	1855.800644	18.324429	-0.048912	2.359445
255.083707	1847.876732	18.329434	-0.048905	2.354612
255.043689	1839.906547	18.334439	-0.048893	2.349738
255.014259	1831.905378	18.339443	-0.048882	2.344836
254.864952	1824.007198	18.344448	-0.048849	2.339977
254.704174	1816.040606	18.349453	-0.048814	2.335065
254.597203	1808.112609	18.354458	-0.048789	2.330170
254.563899	1800.132896	18.359463	-0.048778	2.325240
254.644213	1792.154520	18.364467	-0.048788	2.320309
254.975940	1784.172046	18.369472	-0.048844	2.315387
254.667349	1776.258338	18.374477	-0.048782	2.310443
254.856101	1768.271415	18.379482	-0.048812	2.305485
254.679513	1760.375707	18.384487	-0.048774	2.300542
254.237303	1752.486435	18.389491	-0.048686	2.295569
254.276523	1744.512322	18.394496	-0.048688	2.290574
253.821735	1736.616608	18.399501	-0.048599	2.285574
253.984968	1728.622700	18.404506	-0.048624	2.280555
253.908042	1720.666061	18.409511	-0.048604	2.275528
254.458852	1712.567902	18.414515	-0.048702	2.270455
254.696321	1704.576886	18.419520	-0.048741	2.265411
254.485051	1696.672269	18.424525	-0.048696	2.260371
253.923629	1688.860815	18.429530	-0.048587	2.255348
254.366898	1680.798933	18.434535	-0.048664	2.250244
253.954540	1672.913726	18.439539	-0.048582	2.245164
254.208401	1664.947769	18.444544	-0.048624	2.240081
254.248638	1657.004728	18.449549	-0.048627	2.234982
254.231616	1649.066521	18.454554	-0.048618	2.229869
254.024778	1641.130509	18.459559	-0.048575	2.224728
254.839082	1633.049806	18.464563	-0.048721	2.219576
254.514837	1625.199886	18.469568	-0.048656	2.214456
254.035980	1617.317038	18.474573	-0.048561	2.209289
253.846510	1609.411468	18.479578	-0.048521	2.204122
253.804616	1601.498360	18.484583	-0.048508	2.198951
253.540892	1593.565122	18.489587	-0.048454	2.193735
254.169731	1585.493982	18.494592	-0.048566	2.188498
254.032515	1577.547041	18.499597	-0.048535	2.183259
253.993387	1569.636954	18.504602	-0.048523	2.178042
253.934214	1561.682868	18.509607	-0.048506	2.172780
253.484655	1553.820161	18.514611	-0.048418	2.167529
253.826130	1545.829456	18.519616	-0.048476	2.162256
253.463298	1537.918714	18.524621	-0.048403	2.156956
254.079868	1529.894702	18.529626	-0.048513	2.151661
253.949889	1521.983355	18.534631	-0.048484	2.146356
254.235057	1514.002328	18.539635	-0.048532	2.141032
253.983714	1506.132205	18.544640	-0.048480	2.135717
253.956434	1498.190263	18.549645	-0.048469	2.130362
253.657826	1490.313750	18.554650	-0.048409	2.125011
253.784525	1482.353580	18.559655	-0.048427	2.119632
253.834953	1474.425707	18.564659	-0.048431	2.114254
253.580016	1466.504567	18.569664	-0.048379	2.108836
253.739274	1458.493957	18.574669	-0.048403	2.103384
253.661588	1450.597235	18.579674	-0.048384	2.097973
253.854064	1442.624290	18.584679	-0.048414	2.092522
253.361646	1434.768271	18.589683	-0.048318	2.087069
253.331589	1426.841618	18.594688	-0.048307	2.081599
253.161784	1418.924009	18.599693	-0.048270	2.076106
253.294616	1410.970755	18.604698	-0.048290	2.070606
253.338702	1403.013631	18.609703	-0.048293	2.065078
253.463471	1395.073504	18.614707	-0.048311	2.059557
253.407732	1387.178870	18.619712	-0.048295	2.054033
253.557319	1379.198954	18.624717	-0.048318	2.048456
253.102184	1371.365073	18.629722	-0.048228	2.042904
253.138386	1363.422089	18.634727	-0.048230	2.037311
253.311237	1355.464998	18.639731	-0.048257	2.031706
253.411937	1347.500339	18.644736	-0.048271	2.026074
252.856404	1339.675617	18.649741	-0.048162	2.020456
252.773017	1331.768431	18.654746	-0.048141	2.014813
252.957134	1323.780850	18.659751	-0.048171	2.009125
252.545853	1315.924976	18.664755	-0.048089	2.003452
252.611384	1307.993497	18.669760	-0.048096	1.997760
252.350588	1300.084557	18.674765	-0.048042	1.992033
252.186804	1292.175644	18.679770	-0.048007	1.986299
252.273189	1284.221715	18.684775	-0.048018	1.980543
252.637130	1276.219865	18.689779	-0.048080	1.974766
252.240891	1268.392507	18.694784	-0.048001	1.969016
252.272466	1260.431770	18.699789	-0.048002	1.963199
252.467116	1252.526380	18.704794	-0.048033	1.957423
252.095063	1244.667980	18.709799	-0.047959	1.951602
251.967184	1236.732911	18.714803	-0.047930	1.945733
252.227220	1228.769003	18.719808	-0.047973	1.939869
251.903006	1220.902715	18.724813	-0.047908	1.933995
252.021612	1212.934536	18.729818	-0.047925	1.928076
251.970665	1205.025349	18.734823	-0.047910	1.922164
251.854983	1197.131182	18.739827	-0.047883	1.916237
252.078022	1189.183719	18.744832	-0.047920	1.910291
252.426094	1181.194620	18.749837	-0.047980	1.904309
252.392962	1173.337795	18.754842	-0.047968	1.898364
252.127975	1165.466327	18.759847	-0.047914	1.892363
251.859756	1157.589791	18.764851	-0.047859	1.886339
251.786898	1149.728360	18.769856	-0.047840	1.880329
251.982919	1141.768118	18.774861	-0.047871	1.874256
251.814339	1133.897031	18.779866	-0.047835	1.868189
251.597851	1126.001349	18.784871	-0.047790	1.862077
251.489446	1118.116149	18.789875	-0.047764	1.855966
251.560718	1110.191184	18.794880	-0.047772	1.849826
251.588749	1102.262654	18.799885	-0.047773	1.843657
252.152612	1094.289964	18.804890	-0.047872	1.837498
252.010968	1086.425308	18.809895	-0.047841	1.831317
251.668146	1078.575969	18.814899	-0.047772	1.825103
251.598025	1070.726052	18.819904	-0.047754	1.818900
251.320756	1062.852754	18.824909	-0.047697	1.812632
251.180239	1054.965683	18.829914	-0.047666	1.806348
251.519050	1047.002776	18.834919	-0.047724	1.800041
251.504896	1039.128338	18.839923	-0.047716	1.793739
251.597632	1031.178538	18.844928	-0.047728	1.787368
251.660403	1023.279606	18.849933	-0.047735	1.781011
251.563900	1015.429771	18.854938	-0.047712	1.774650
251.282076	1007.585622	18.859943	-0.047654	1.768249
251.252245	999.684001	18.864947	-0.047644	1.761808
251.388598	991.802563	18.869952	-0.047664	1.755383
251.499864	983.888037	18.874957	-0.047679	1.748903
251.117795	976.091683	18.879962	-0.047603	1.742432
251.151997	968.196591	18.884967	-0.047605	1.735910
251.342033	960.269567	18.889971	-0.047635	1.729357
251.554237	952.378770	18.894976	-0.047669	1.722813
251.097780	944.593001	18.899981	-0.047579	1.716243
251.161370	936.699419	18.904986	-0.047586	1.709626
250.884135	928.861704	18.909991	-0.047529	1.702985
250.458738	921.049140	18.914995	-0.047445	1.696319
250.683356	913.122043	18.920000	-0.047482	1.689617
250.578441	905.250276	18.925005	-0.047457	1.682891
250.740916	897.375722	18.930010	-0.047482	1.676173
250.393034	889.549912	18.935015	-0.047412	1.669399
250.531930	881.645766	18.940019	-0.047433	1.662597
250.543221	873.791593	18.945024	-0.047430	1.655792
250.250815	865.961906	18.950029	-0.047371	1.648939
250.304813	858.099291	18.955034	-0.047376	1.642076
250.090118	850.282598	18.960039	-0.047331	1.635188
249.641084	842.457003	18.965043	-0.047242	1.628229
249.319207	834.641350	18.970048	-0.047177	1.621266
249.496788	826.710090	18.975053	-0.047205	1.614243
249.743369	818.795357	18.980058	-0.047246	1.607213
249.991296	810.892804	18.985063	-0.047287	1.600164
249.942249	803.084705	18.990067	-0.047273	1.593125
249.725062	795.283983	18.995072	-0.047227	1.586038
249.564578	787.465245	19.000077	-0.047192	1.578910
249.658006	779.602273	19.005082	-0.047204	1.571747
249.831042	771.726906	19.010087	-0.047232	1.564552
249.509785	763.973720	19.015091	-0.047167	1.557363
249.202495	756.190058	19.020096	-0.047104	1.550114
249.011950	748.359612	19.025101	-0.047064	1.542804
248.505926	740.618567	19.030106	-0.046965	1.535496
248.739919	732.700096	19.035111	-0.047003	1.528099
248.974119	724.812468	19.040115	-0.047042	1.520695
249.633734	716.892771	19.045120	-0.047159	1.513291
249.286202	709.124260	19.050125	-0.047090	1.505837
249.587552	701.287851	19.055130	-0.047141	1.498383
249.535407	693.489141	19.060135	-0.047126	1.490873
249.192816	685.745930	19.065139	-0.047057	1.483332
248.776631	678.026134	19.070144	-0.046975	1.475763
248.965598	670.134969	19.075149	-0.047005	1.468085
249.297226	662.278387	19.080154	-0.047061	1.460423
248.972241	654.542320	19.085159	-0.046996	1.452734
248.463524	646.829813	19.090163	-0.046896	1.444996
249.005222	638.947121	19.095168	-0.046992	1.437221
248.729698	631.196871	19.100173	-0.046936	1.429400
248.352229	623.478520	19.105178	-0.046860	1.421551
248.800789	615.604118	19.110183	-0.046939	1.413640
248.721076	607.829909	19.115187	-0.046919	1.405696
248.327788	600.155041	19.120192	-0.046841	1.397757
248.541747	592.309290	19.125197	-0.046875	1.389699
248.554383	584.535088	19.130202	-0.046873	1.381634
248.331485	576.809146	19.135207	-0.046826	1.373531
248.506057	568.988828	19.140211	-0.046854	1.365350
248.546479	561.255084	19.145216	-0.046856	1.357188
248.288946	553.536651	19.150221	-0.046803	1.348940
248.043202	545.825750	19.155226	-0.046753	1.340651
248.311442	538.040360	19.160231	-0.046798	1.332323
247.998137	530.343336	19.165235	-0.046734	1.323933
247.798398	522.654826	19.170240	-0.046692	1.315519
248.054690	514.765138	19.175245	-0.046735	1.306914
247.816597	507.098739	19.180250	-0.046685	1.298407
247.569781	499.409810	19.185255	-0.046634	1.289818
247.889585	491.622665	19.190259	-0.046689	1.281167
247.835874	483.949707	19.195264	-0.046674	1.272516
247.643046	476.262556	19.200269	-0.046633	1.263763
247.259084	468.640351	19.205274	-0.046557	1.254985
246.985373	460.970671	19.210279	-0.046501	1.246113
247.228950	453.240695	19.215283	-0.046541	1.237208
246.905422	445.605152	19.220288	-0.046476	1.228237
246.656485	437.945723	19.225293	-0.046425	1.219187
246.690539	430.257491	19.230298	-0.046426	1.210092
246.214360	422.657138	19.235303	-0.046332	1.200929
246.056401	415.015477	19.240307	-0.046298	1.191711
246.290823	407.303716	19.245312	-0.046337	1.182417
246.275258	399.645012	19.250317	-0.046329	1.173063
246.112515	392.030361	19.255322	-0.046294	1.163656
245.935392	384.429530	19.260327	-0.046256	1.154187
245.571340	376.837384	19.265331	-0.046183	1.144610
245.395509	369.241795	19.270336	-0.046145	1.134989
244.881052	361.694701	19.275341	-0.046045	1.125273
244.843261	354.091360	19.280346	-0.046033	1.115506
244.608789	346.520929	19.285351	-0.045984	1.105650
244.236174	338.979862	19.290355	-0.045910	1.095714
244.025412	331.431699	19.295360	-0.045866	1.085713
243.689102	323.900070	19.300365	-0.045798	1.075613
243.565103	316.338486	19.305370	-0.045770	1.065426
242.869160	308.906569	19.310375	-0.045636	1.055183
242.680376	301.359095	19.315379	-0.045596	1.044800
242.445277	293.855393	19.320384	-0.045547	1.034363
241.669283	286.442967	19.325389	-0.045398	1.023815
241.572254	278.937673	19.330394	-0.045375	1.013193
240.769006	271.557190	19.335399	-0.045221	1.002462
240.718403	264.036668	19.340403	-0.045207	0.991600
239.944278	256.673778	19.345408	-0.045058	0.980665
239.722443	249.197864	19.350413	-0.045012	0.969581
239.699695	241.735314	19.355418	-0.045002	0.958441
239.000752	234.411881	19.360423	-0.044868	0.947202
238.895642	226.985079	19.365427	-0.044843	0.935828
238.623985	219.619374	19.370432	-0.044788	0.924364
237.796885	212.376994	19.375437	-0.044629	0.912796
237.563539	205.031268	19.380442	-0.044581	0.901081
236.387777	197.875113	19.385447	-0.044357	0.889250
236.343303	190.512203	19.390451	-0.044344	0.877247
235.823388	183.281764	19.395456	-0.044243	0.865157
235.495985	176.027199	19.400461	-0.044177	0.852913
235.023280	168.834405	19.405466	-0.044085	0.840552
234.461424	161.663249	19.410471	-0.043975	0.828016
234.019694	154.497688	19.415475	-0.043889	0.815335
233.193864	147.431456	19.420480	-0.043730	0.802509
233.034538	140.270011	19.425485	-0.043696	0.789516
232.769945	133.168831	19.430490	-0.043642	0.776382
232.224782	126.146227	19.435495	-0.043536	0.763077
231.826914	119.136299	19.440499	-0.043457	0.749609
231.465580	112.144740	19.445504	-0.043386	0.735943
231.056643	105.198626	19.450509	-0.043305	0.722093
230.412610	98.347281	19.455514	-0.043181	0.708078
229.977464	91.493870	19.460519	-0.043095	0.693853
229.579292	84.675495	19.465523	-0.043017	0.679418
228.978150	78.107509	19.470528	-0.042900	0.665132