Fri Apr 16 19:25:47 2021

Number of Points = 3644
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.537465	0.024369	0.000000	0.000097	0.311391

0.762989	-0.019081	0.005005	0.000055	0.311380
0.826135	-0.028831	0.010010	0.000043	0.311388
0.570982	0.016651	0.015014	0.000090	0.311384
0.741713	-0.015861	0.020019	0.000059	0.311378
0.914261	-0.045584	0.025024	0.000026	0.311385
0.899601	-0.044818	0.030029	0.000029	0.311377
1.012676	-0.066083	0.035034	0.000008	0.311374
0.869171	-0.038751	0.040038	0.000035	0.311380
0.798026	-0.026334	0.045043	0.000048	0.311377
0.446099	0.040754	0.050048	0.000113	0.311392
0.692675	-0.006844	0.055053	0.000067	0.311379
0.866715	-0.037963	0.060058	0.000035	0.311382
0.552778	0.020883	0.065062	0.000093	0.311391
0.856196	-0.037634	0.070067	0.000037	0.311375
1.019270	-0.066156	0.075072	0.000006	0.311380
0.941995	-0.053813	0.080077	0.000021	0.311373
0.948387	-0.083546	0.085082	0.000020	0.311240
0.856334	-0.102576	0.090086	0.000037	0.311074
0.970632	-0.125171	0.095091	0.000015	0.311066
0.772310	-0.087466	0.100096	0.000052	0.311074
1.006530	-0.132304	0.105101	0.000009	0.311063
0.991695	-0.128375	0.110106	0.000011	0.311069
1.111162	-0.166301	0.115110	-0.000011	0.310994
1.164609	-0.230433	0.120115	-0.000021	0.310741
1.118042	-0.219210	0.125120	-0.000012	0.310754
0.874060	-0.176748	0.130125	0.000033	0.310745
0.714751	-0.145700	0.135130	0.000063	0.310755
0.854905	-0.192292	0.140134	0.000037	0.310657
1.284327	-0.305914	0.145139	-0.000043	0.310491
1.078936	-0.265642	0.150144	-0.000005	0.310505
0.727202	-0.203270	0.155149	0.000060	0.310499
0.964505	-0.268039	0.160154	0.000016	0.310398
0.928564	-0.313713	0.165158	0.000023	0.310155
0.934440	-0.315676	0.170163	0.000022	0.310151
0.916660	-0.310592	0.175168	0.000025	0.310159
0.813776	-0.337564	0.180173	0.000044	0.309947
0.670471	-0.333696	0.185178	0.000071	0.309843
0.831314	-0.363035	0.190182	0.000041	0.309843
1.028604	-0.417899	0.195187	0.000004	0.309754
0.586193	-0.387916	0.200192	0.000086	0.309519
0.537108	-0.381519	0.205197	0.000095	0.309507
0.869501	-0.443493	0.210202	0.000033	0.309500
0.703391	-0.469616	0.215206	0.000064	0.309237
0.604078	-0.452105	0.220211	0.000083	0.309235
0.765875	-0.486644	0.225216	0.000053	0.309211
0.764318	-0.556228	0.230221	0.000053	0.308884
0.649832	-0.533656	0.235226	0.000074	0.308893
0.391476	-0.503340	0.240230	0.000122	0.308815
0.450843	-0.561640	0.245235	0.000111	0.308592
0.176452	-0.508247	0.250240	0.000162	0.308609
0.079799	-0.526521	0.255245	0.000180	0.308441
-0.127668	-0.521980	0.260250	0.000219	0.308286
0.409288	-0.623354	0.265254	0.000119	0.308268
0.133882	-0.622351	0.270259	0.000170	0.308038
0.293699	-0.661733	0.275264	0.000140	0.307990
0.228104	-0.672507	0.280269	0.000152	0.307883
0.180508	-0.715154	0.285274	0.000161	0.307642
0.275452	-0.732451	0.290278	0.000144	0.307642
0.106643	-0.760206	0.295283	0.000175	0.307368
0.070171	-0.760763	0.300288	0.000182	0.307334
0.145769	-0.815555	0.305293	0.000168	0.307141
0.066634	-0.829611	0.310298	0.000182	0.307007
0.150243	-0.864174	0.315302	0.000167	0.306916
0.198909	-0.917140	0.320307	0.000158	0.306708
-0.238653	-0.844811	0.325312	0.000239	0.306675
-0.112027	-0.929558	0.330317	0.000215	0.306383
-0.108588	-0.931402	0.335322	0.000215	0.306378
-0.063719	-1.003719	0.340326	0.000206	0.306075
0.193517	-1.052491	0.345331	0.000159	0.306065
0.206597	-1.121589	0.350336	0.000156	0.305750
-0.057956	-1.077803	0.355341	0.000205	0.305730
-0.190864	-1.102809	0.360346	0.000230	0.305498
0.190336	-1.185268	0.365350	0.000159	0.305435
-0.192500	-1.175839	0.370355	0.000230	0.305150
-0.246620	-1.184757	0.375360	0.000240	0.305062
-0.301673	-1.224574	0.380365	0.000251	0.304826
-0.156848	-1.279046	0.385370	0.000224	0.304692
-0.177585	-1.313964	0.390374	0.000227	0.304509
0.206817	-1.426307	0.395379	0.000156	0.304307
0.098180	-1.426531	0.400384	0.000176	0.304212
0.084284	-1.494241	0.405389	0.000179	0.303878
-0.369165	-1.430054	0.410394	0.000263	0.303792
-0.193539	-1.509846	0.415398	0.000230	0.303564
-0.760738	-1.444717	0.420403	0.000336	0.303383
-0.753223	-1.471553	0.425408	0.000334	0.303262
-0.623317	-1.550489	0.430413	0.000310	0.302998
-0.523615	-1.590630	0.435418	0.000292	0.302893
-0.639957	-1.625665	0.440422	0.000313	0.302624
-0.766320	-1.639800	0.445427	0.000337	0.302447
-0.947371	-1.633799	0.450432	0.000370	0.302319
-1.270736	-1.639464	0.455437	0.000431	0.302010
-1.081782	-1.695158	0.460442	0.000395	0.301908
-0.885000	-1.777104	0.465446	0.000359	0.301687
-0.958533	-1.810613	0.470451	0.000372	0.301462
-1.296392	-1.773295	0.475456	0.000435	0.301347
-1.700326	-1.759449	0.480461	0.000510	0.301061
-1.800341	-1.769965	0.485466	0.000529	0.300923
-1.298536	-1.897544	0.490470	0.000436	0.300749
-1.329296	-1.937682	0.495475	0.000441	0.300529
-1.524109	-1.932949	0.500480	0.000478	0.300381
-2.160336	-1.863470	0.505485	0.000596	0.300159
-2.218481	-1.899686	0.510490	0.000607	0.299934
-1.815926	-2.005342	0.515494	0.000532	0.299777
-2.325171	-1.965418	0.520499	0.000627	0.299523
-1.986711	-2.065563	0.525504	0.000564	0.299337
-1.687736	-2.155056	0.530509	0.000508	0.299167
-2.048788	-2.145798	0.535514	0.000575	0.298895
-2.260491	-2.152832	0.540518	0.000614	0.298674
-2.143712	-2.208640	0.545523	0.000593	0.298507
-2.245012	-2.239079	0.550528	0.000612	0.298270
-2.284598	-2.280020	0.555533	0.000619	0.298037
-2.067539	-2.356587	0.560538	0.000579	0.297857
-2.379003	-2.345492	0.565542	0.000636	0.297636
-3.087022	-2.277328	0.570547	0.000768	0.297342
-3.279604	-2.271994	0.575552	0.000804	0.297198
-3.685243	-2.237031	0.580557	0.000880	0.297009
-3.410481	-2.339855	0.585562	0.000828	0.296751
-3.564493	-2.345715	0.590566	0.000857	0.296587
-3.670388	-2.371437	0.595571	0.000877	0.296367
-3.798786	-2.401395	0.600576	0.000901	0.296107
-4.189058	-2.361358	0.605581	0.000973	0.295956
-4.782909	-2.291814	0.610586	0.001084	0.295769
-5.023414	-2.288444	0.615590	0.001128	0.295572
-5.169028	-2.285412	0.620595	0.001155	0.295457
-5.183982	-2.341057	0.625600	0.001158	0.295171
-5.942285	-2.234539	0.630605	0.001299	0.295018
-6.382316	-2.184522	0.635610	0.001381	0.294871
-5.863586	-2.329413	0.640614	0.001285	0.294623
-6.195878	-2.290360	0.645619	0.001346	0.294518
-6.749372	-2.242868	0.650624	0.001449	0.294257
-6.740554	-2.265853	0.655629	0.001448	0.294152
-7.175906	-2.235237	0.660634	0.001529	0.293914
-7.203622	-2.258037	0.665638	0.001534	0.293777
-8.053424	-2.136226	0.670643	0.001692	0.293616
-7.683785	-2.237052	0.675648	0.001623	0.293451
-8.280544	-2.160218	0.680653	0.001734	0.293295
-8.128397	-2.223652	0.685658	0.001706	0.293118
-8.341502	-2.208142	0.690662	0.001746	0.293004
-8.443037	-2.240728	0.695667	0.001764	0.292752
-8.662424	-2.221233	0.700672	0.001805	0.292651
-8.447292	-2.310478	0.705677	0.001765	0.292404
-8.437924	-2.325824	0.710682	0.001763	0.292336
-9.482582	-2.192937	0.715686	0.001958	0.292054
-9.702911	-2.160721	0.720691	0.001999	0.292016
-9.168313	-2.306736	0.725696	0.001899	0.291774
-10.024069	-2.160482	0.730701	0.002058	0.291728
-10.315243	-2.162422	0.735706	0.002113	0.291456
-10.340550	-2.168139	0.740710	0.002117	0.291405
-10.559257	-2.170605	0.745715	0.002158	0.291195
-10.782548	-2.149167	0.750720	0.002200	0.291100
-10.537406	-2.230795	0.755725	0.002154	0.290916
-10.957975	-2.181825	0.760730	0.002232	0.290779
-10.870163	-2.219451	0.765734	0.002216	0.290672
-11.263951	-2.181632	0.770739	0.002289	0.290504
-10.924938	-2.260105	0.775744	0.002226	0.290420
-11.412855	-2.222636	0.780749	0.002317	0.290165
-11.447917	-2.225681	0.785754	0.002323	0.290118
-11.676444	-2.237018	0.790758	0.002366	0.289854
-11.921508	-2.190479	0.795763	0.002411	0.289865
-11.683961	-2.302627	0.800768	0.002367	0.289520
-11.709757	-2.301523	0.805773	0.002372	0.289503
-11.953822	-2.306573	0.810778	0.002417	0.289256
-12.493277	-2.213364	0.815782	0.002518	0.289232
-13.027391	-2.165658	0.820787	0.002617	0.288985
-12.693669	-2.242710	0.825792	0.002555	0.288903
-12.578989	-2.299653	0.830797	0.002533	0.288722
-12.946576	-2.262549	0.835802	0.002602	0.288573
-13.071473	-2.259468	0.840806	0.002625	0.288475
-12.758985	-2.362575	0.845811	0.002567	0.288243
-13.025704	-2.324780	0.850816	0.002616	0.288189
-13.953511	-2.201284	0.855821	0.002789	0.287963
-13.649024	-2.254634	0.860826	0.002732	0.287973
-13.911206	-2.270472	0.865830	0.002781	0.287654
-14.188904	-2.224966	0.870835	0.002833	0.287629
-13.974414	-2.306277	0.875840	0.002793	0.287416
-14.069482	-2.313517	0.880845	0.002811	0.287293
-14.009405	-2.355579	0.885850	0.002799	0.287136
-14.764756	-2.246795	0.890854	0.002940	0.286992
-14.527366	-2.306479	0.895859	0.002896	0.286909
-15.078095	-2.246268	0.900864	0.002998	0.286708
-14.746806	-2.311153	0.905869	0.002936	0.286685
-15.399470	-2.249799	0.910874	0.003058	0.286396
-15.426279	-2.249179	0.915878	0.003063	0.286374
-15.881959	-2.202367	0.920883	0.003148	0.286192
-15.810631	-2.238707	0.925888	0.003134	0.286074
-15.294122	-2.351308	0.930893	0.003038	0.285980
-15.683803	-2.328801	0.935898	0.003111	0.285735
-16.003272	-2.270519	0.940902	0.003170	0.285737
-15.836089	-2.348471	0.945907	0.003139	0.285496
-15.713145	-2.373139	0.950912	0.003116	0.285484
-16.588112	-2.262103	0.955917	0.003279	0.285241
-16.554497	-2.287061	0.960922	0.003273	0.285145
-16.784295	-2.260917	0.965926	0.003315	0.285066
-17.137702	-2.244267	0.970931	0.003381	0.284825
-17.030624	-2.262490	0.975936	0.003361	0.284831
-17.133206	-2.302769	0.980941	0.003380	0.284532
-17.150543	-2.306494	0.985946	0.003383	0.284497
-17.338583	-2.300205	0.990950	0.003418	0.284355
-17.568502	-2.288023	0.995955	0.003461	0.284205
-17.599841	-2.288233	1.000960	0.003467	0.284175
-17.828652	-2.308173	1.005965	0.003509	0.283861
-17.601609	-2.347863	1.010970	0.003467	0.283870
-17.524038	-2.410654	1.015974	0.003453	0.283622
-18.192732	-2.303380	1.020979	0.003577	0.283549
-18.234571	-2.321909	1.025984	0.003585	0.283416
-18.128626	-2.377582	1.030989	0.003565	0.283230
-18.907179	-2.234049	1.035994	0.003710	0.283240
-19.057032	-2.262461	1.040998	0.003738	0.282956
-19.213744	-2.234005	1.046003	0.003767	0.282956
-18.921134	-2.320142	1.051008	0.003712	0.282787
-19.527252	-2.245300	1.056013	0.003825	0.282607
-19.333362	-2.281448	1.061018	0.003789	0.282602
-19.405990	-2.328074	1.066022	0.003803	0.282296
-19.574735	-2.299379	1.071027	0.003834	0.282286
-19.670390	-2.314771	1.076032	0.003852	0.282118
-19.947391	-2.294054	1.081037	0.003903	0.281966
-19.596799	-2.366853	1.086042	0.003838	0.281920
-20.188401	-2.305521	1.091046	0.003948	0.281682
-19.897380	-2.360463	1.096051	0.003894	0.281672
-19.926867	-2.401307	1.101056	0.003899	0.281435
-20.773310	-2.264323	1.106061	0.004057	0.281348
-20.618667	-2.309357	1.111066	0.004028	0.281261
-20.405377	-2.390397	1.116070	0.003988	0.281044
-20.511559	-2.375023	1.121075	0.004008	0.281024
-20.756058	-2.385309	1.126080	0.004054	0.280742
-20.963204	-2.352790	1.131085	0.004092	0.280716
-21.330732	-2.306212	1.136090	0.004160	0.280611
-21.730288	-2.255832	1.141094	0.004235	0.280497
-21.797172	-2.244782	1.146099	0.004247	0.280491
-21.658710	-2.327927	1.151104	0.004221	0.280192
-22.272562	-2.223267	1.156109	0.004336	0.280156
-21.904618	-2.313508	1.161114	0.004267	0.280036
-21.915322	-2.352084	1.166118	0.004269	0.279827
-22.035160	-2.331191	1.171123	0.004291	0.279822
-22.149745	-2.366404	1.176128	0.004313	0.279532
-22.604821	-2.290140	1.181133	0.004397	0.279499
-22.373209	-2.355160	1.186138	0.004354	0.279381
-22.760993	-2.316916	1.191142	0.004426	0.279214
-22.405130	-2.383540	1.196147	0.004360	0.279204
-22.669181	-2.397032	1.201152	0.004409	0.278885
-23.143461	-2.313054	1.206157	0.004497	0.278873
-23.352958	-2.302840	1.211162	0.004536	0.278729
-23.397017	-2.325290	1.216166	0.004544	0.278571
-23.423973	-2.322000	1.221171	0.004549	0.278563
-23.512812	-2.364741	1.226176	0.004566	0.278257
-23.758032	-2.322292	1.231181	0.004612	0.278246
-23.544337	-2.390086	1.236186	0.004572	0.278095
-24.034365	-2.327785	1.241190	0.004663	0.277956
-24.015623	-2.334168	1.246195	0.004659	0.277941
-23.851670	-2.426794	1.251200	0.004629	0.277614
-24.189543	-2.366870	1.256205	0.004692	0.277606
-24.064961	-2.425491	1.261210	0.004669	0.277419
-24.550091	-2.359208	1.266214	0.004759	0.277304
-24.511994	-2.379089	1.271219	0.004752	0.277237
-24.997259	-2.339627	1.276224	0.004842	0.276982
-25.189887	-2.306088	1.281229	0.004878	0.276975
-24.803230	-2.411620	1.286234	0.004806	0.276791
-25.297308	-2.341137	1.291238	0.004898	0.276690
-25.416804	-2.328167	1.296243	0.004920	0.276644
-25.336697	-2.396924	1.301248	0.004905	0.276361
-25.917403	-2.291819	1.306253	0.005013	0.276358
-25.948030	-2.321349	1.311258	0.005019	0.276174
-25.966745	-2.342743	1.316262	0.005022	0.276045
-25.775688	-2.381706	1.321267	0.004987	0.276023
-26.243060	-2.351621	1.326272	0.005073	0.275735
-26.629360	-2.282480	1.331277	0.005145	0.275729
-26.421924	-2.339428	1.336282	0.005107	0.275628
-26.850342	-2.286025	1.341286	0.005186	0.275500
-26.869830	-2.285014	1.346291	0.005190	0.275487
-26.525156	-2.399697	1.351296	0.005126	0.275214
-26.874800	-2.348728	1.356301	0.005191	0.275148
-27.414760	-2.266348	1.361306	0.005291	0.275065
-27.256024	-2.339196	1.366310	0.005262	0.274833
-27.198274	-2.350869	1.371315	0.005251	0.274827
-27.758636	-2.291056	1.376320	0.005355	0.274606
-27.952213	-2.274744	1.381325	0.005391	0.274506
-27.557948	-2.351395	1.386330	0.005318	0.274480
-27.949596	-2.328120	1.391334	0.005391	0.274228
-28.329948	-2.261035	1.396339	0.005461	0.274217
-28.079381	-2.333594	1.401344	0.005415	0.274074
-28.708233	-2.254918	1.406349	0.005532	0.273886
-28.747388	-2.246790	1.411354	0.005539	0.273892
-28.509230	-2.333370	1.416358	0.005495	0.273663
-28.664634	-2.323263	1.421363	0.005524	0.273567
-28.772814	-2.311539	1.426368	0.005544	0.273525
-29.300780	-2.267199	1.431373	0.005642	0.273252
-29.008281	-2.319695	1.436378	0.005587	0.273256
-29.208317	-2.308714	1.441382	0.005625	0.273121
-29.675415	-2.253883	1.446387	0.005712	0.272962
-29.307177	-2.319467	1.451392	0.005643	0.272969
-29.314016	-2.375039	1.456397	0.005644	0.272668
-29.648625	-2.323258	1.461402	0.005706	0.272620
-29.663022	-2.337867	1.466406	0.005709	0.272529
-29.921476	-2.333771	1.471411	0.005757	0.272301
-30.023390	-2.312144	1.476416	0.005776	0.272318
-30.317593	-2.305704	1.481421	0.005831	0.272068
-30.487452	-2.288191	1.486426	0.005862	0.271997
-30.242912	-2.341676	1.491430	0.005817	0.271949
-30.898669	-2.270631	1.496435	0.005939	0.271692
-30.626968	-2.318520	1.501440	0.005888	0.271701
-30.742757	-2.329869	1.506445	0.005910	0.271528
-30.881885	-2.336660	1.511450	0.005936	0.271357
-30.989134	-2.316125	1.516454	0.005956	0.271363
-30.974713	-2.373474	1.521459	0.005953	0.271071
-31.249299	-2.326249	1.526464	0.006004	0.271057
-31.435743	-2.315627	1.531469	0.006039	0.270932
-31.450589	-2.349797	1.536474	0.006041	0.270736
-31.388577	-2.361062	1.541478	0.006030	0.270736
-31.903582	-2.308963	1.546483	0.006126	0.270514
-31.960294	-2.303582	1.551488	0.006136	0.270488
-31.638306	-2.383130	1.556493	0.006076	0.270375
-32.051908	-2.352301	1.561498	0.006153	0.270138
-32.307340	-2.305849	1.566502	0.006201	0.270138
-32.399737	-2.333028	1.571507	0.006218	0.269902
-32.241420	-2.376263	1.576512	0.006188	0.269825
-32.660940	-2.314316	1.581517	0.006266	0.269748
-32.937899	-2.311470	1.586522	0.006318	0.269493
-32.599245	-2.373193	1.591526	0.006255	0.269493
-33.009538	-2.333696	1.596531	0.006331	0.269304
-33.245885	-2.307547	1.601536	0.006375	0.269214
-33.135886	-2.333367	1.606541	0.006355	0.269183
-33.276495	-2.366098	1.611546	0.006381	0.268869
-33.442619	-2.335747	1.616550	0.006412	0.268870
-33.441725	-2.368311	1.621555	0.006411	0.268696
-33.460717	-2.389395	1.626560	0.006415	0.268564
-33.605694	-2.369984	1.631565	0.006442	0.268527
-33.970992	-2.358100	1.636570	0.006510	0.268232
-33.959210	-2.359511	1.641574	0.006508	0.268237
-34.239946	-2.340416	1.646579	0.006560	0.268064
-34.459876	-2.321078	1.651584	0.006601	0.267953
-34.170802	-2.377486	1.656589	0.006547	0.267932
-34.594726	-2.359822	1.661594	0.006626	0.267611
-34.837240	-2.315789	1.666598	0.006671	0.267611
-34.867992	-2.337666	1.671603	0.006677	0.267462
-34.870528	-2.367170	1.676608	0.006677	0.267300
-35.300535	-2.290086	1.681613	0.006757	0.267295
-35.610383	-2.286001	1.686618	0.006815	0.267011
-35.309757	-2.347559	1.691622	0.006759	0.266974
-35.327720	-2.361383	1.696627	0.006762	0.266882
-35.627450	-2.342055	1.701632	0.006818	0.266691
-35.731578	-2.324234	1.706637	0.006837	0.266685
-36.037449	-2.313231	1.711642	0.006894	0.266443
-36.269865	-2.287582	1.716646	0.006937	0.266353
-36.347290	-2.277112	1.721651	0.006951	0.266333
-36.105724	-2.373792	1.726656	0.006907	0.266047
-36.579025	-2.288782	1.731661	0.006995	0.266041
-36.565057	-2.319795	1.736666	0.006992	0.265886
-36.599896	-2.343364	1.741670	0.006998	0.265724
-36.840558	-2.300897	1.746675	0.007043	0.265717
-37.040055	-2.305373	1.751680	0.007080	0.265495
-37.208520	-2.280019	1.756685	0.007112	0.265466
-36.866539	-2.362612	1.761690	0.007048	0.265355
-37.320478	-2.323025	1.766694	0.007132	0.265121
-37.433958	-2.303524	1.771699	0.007153	0.265115
-37.383672	-2.353538	1.776704	0.007144	0.264892
-37.863528	-2.283648	1.781709	0.007233	0.264797
-37.846638	-2.294558	1.786714	0.007230	0.264754
-38.052980	-2.306306	1.791718	0.007269	0.264485
-38.170993	-2.286659	1.796723	0.007290	0.264475
-38.101831	-2.323377	1.801728	0.007278	0.264343
-38.581752	-2.263438	1.806733	0.007367	0.264193
-38.174249	-2.338268	1.811738	0.007291	0.264189
-38.647437	-2.308005	1.816742	0.007379	0.263884
-38.698023	-2.304971	1.821747	0.007388	0.263850
-38.500652	-2.358916	1.826752	0.007352	0.263751
-38.990541	-2.308377	1.831757	0.007443	0.263540
-38.996413	-2.307009	1.836762	0.007444	0.263541
-38.930627	-2.365446	1.841766	0.007432	0.263286
-39.343685	-2.303193	1.846771	0.007508	0.263215
-39.289098	-2.326051	1.851776	0.007498	0.263145
-39.655638	-2.298118	1.856781	0.007566	0.262932
-39.292735	-2.364661	1.861786	0.007499	0.262929
-39.600133	-2.353210	1.866790	0.007556	0.262684
-40.119011	-2.276142	1.871795	0.007653	0.262589
-39.950187	-2.316007	1.876800	0.007621	0.262538
-40.106888	-2.335529	1.881805	0.007650	0.262274
-40.258328	-2.307385	1.886810	0.007678	0.262277
-40.266700	-2.342218	1.891814	0.007680	0.262077
-40.291927	-2.361218	1.896819	0.007685	0.261946
-40.381713	-2.350534	1.901824	0.007701	0.261915
-40.814566	-2.317271	1.906829	0.007782	0.261664
-40.646110	-2.347436	1.911834	0.007750	0.261667
-40.870381	-2.343550	1.916838	0.007792	0.261463
-41.360174	-2.279062	1.921843	0.007883	0.261327
-40.898049	-2.366806	1.926848	0.007797	0.261307
-41.526943	-2.304023	1.931853	0.007914	0.261021
-41.731087	-2.266195	1.936858	0.007952	0.261025
-41.480812	-2.337977	1.941862	0.007906	0.260879
-41.809326	-2.309669	1.946867	0.007967	0.260705
-41.781003	-2.314066	1.951872	0.007961	0.260709
-42.246390	-2.270906	1.956877	0.008048	0.260479
-42.036235	-2.311516	1.961882	0.008009	0.260466
-41.858101	-2.368793	1.966886	0.007976	0.260328
-42.589676	-2.273390	1.971891	0.008112	0.260118
-42.162576	-2.348635	1.976896	0.008032	0.260132
-42.371645	-2.363338	1.981901	0.008071	0.259838
-42.989578	-2.256827	1.986906	0.008186	0.259806
-42.831795	-2.304272	1.991910	0.008157	0.259701
-43.017672	-2.311571	1.996915	0.008191	0.259472
-43.110094	-2.312512	2.001920	0.008208	0.259373

-43.210938	-2.326345	2.011917	0.008227	0.259194
-43.583734	-2.315865	2.021914	0.008296	0.258874
-43.634236	-2.326511	2.031910	0.008306	0.258764
-43.955047	-2.306594	2.041907	0.008365	0.258549
-44.058181	-2.304994	2.051904	0.008384	0.258453
-44.189326	-2.321699	2.061901	0.008409	0.258226
-44.404109	-2.282627	2.071898	0.008449	0.258226
-44.473123	-2.303210	2.081894	0.008461	0.258041
-44.840400	-2.254352	2.091891	0.008530	0.257941
-44.579000	-2.302155	2.101888	0.008481	0.257940
-44.512266	-2.314707	2.111885	0.008469	0.257938
-44.686351	-2.283090	2.121882	0.008501	0.257938
-44.907136	-2.295988	2.131878	0.008542	0.257640
-45.057639	-2.275394	2.141875	0.008570	0.257603
-45.187497	-2.251320	2.151872	0.008594	0.257606
-45.112389	-2.263768	2.161869	0.008580	0.257613
-45.461003	-2.163921	2.171866	0.008645	0.257818
-44.728836	-2.274475	2.181862	0.008508	0.257946
-44.612806	-2.296360	2.191859	0.008487	0.257942
-44.821149	-2.257279	2.201856	0.008525	0.257949
-44.783947	-2.263849	2.211853	0.008518	0.257951
-44.686398	-2.283655	2.221850	0.008500	0.257940
-44.663843	-2.287369	2.231846	0.008496	0.257942
-44.527813	-2.289817	2.241843	0.008470	0.258068
-44.337558	-2.295363	2.251840	0.008435	0.258231
-44.387661	-2.286940	2.261837	0.008444	0.258228
-44.559755	-2.254732	2.271834	0.008476	0.258233
-44.071998	-2.297509	2.281830	0.008385	0.258492
-44.233725	-2.257250	2.291827	0.008415	0.258553
-44.226968	-2.257066	2.301824	0.008414	0.258561
-44.130444	-2.225636	2.311821	0.008396	0.258836
-43.874406	-2.266734	2.321818	0.008348	0.258867
-43.600644	-2.292310	2.331814	0.008297	0.259003
-43.560205	-2.264119	2.341811	0.008289	0.259202
-43.379814	-2.295691	2.351808	0.008256	0.259210
-43.145157	-2.289253	2.361805	0.008212	0.259484
-43.071994	-2.302513	2.371802	0.008198	0.259485
-43.105528	-2.246475	2.381798	0.008204	0.259764
-43.021949	-2.252679	2.391795	0.008189	0.259815
-42.628383	-2.275322	2.401792	0.008115	0.260088
-42.522547	-2.286837	2.411789	0.008095	0.260132
-42.064128	-2.315437	2.421786	0.008010	0.260437
-42.418318	-2.243472	2.431782	0.008076	0.260479
-42.160005	-2.248494	2.441779	0.008028	0.260713
-42.140466	-2.233864	2.451776	0.008024	0.260814
-42.159903	-2.188427	2.461773	0.008027	0.261047
-41.813911	-2.213900	2.471770	0.007963	0.261256
-41.543767	-2.241915	2.481766	0.007913	0.261373
-41.230880	-2.242981	2.491763	0.007854	0.261683
-41.067762	-2.248390	2.501760	0.007824	0.261818
-40.841989	-2.263301	2.511757	0.007782	0.261963
-40.363520	-2.297937	2.521754	0.007693	0.262253
-40.393839	-2.272553	2.531750	0.007698	0.262363
-40.070641	-2.289156	2.541747	0.007638	0.262596
-39.616961	-2.333349	2.551744	0.007553	0.262808
-39.689157	-2.295477	2.561741	0.007567	0.262945
-39.445588	-2.287205	2.571738	0.007521	0.263235
-39.400434	-2.268610	2.581734	0.007513	0.263383
-39.261471	-2.261973	2.591731	0.007487	0.263558
-39.110219	-2.233032	2.601728	0.007458	0.263869
-38.683699	-2.278149	2.611725	0.007379	0.264047
-38.224943	-2.333523	2.621722	0.007293	0.264202
-38.177804	-2.291969	2.631718	0.007285	0.264477
-37.852779	-2.320818	2.641715	0.007224	0.264643
-37.633388	-2.329831	2.651712	0.007183	0.264813
-37.464095	-2.304375	2.661709	0.007151	0.265120
-37.097863	-2.336166	2.671706	0.007083	0.265311
-37.129586	-2.299348	2.681702	0.007089	0.265481
-37.102131	-2.258594	2.691699	0.007084	0.265731
-36.670638	-2.298633	2.701696	0.007003	0.265941
-36.600318	-2.277085	2.711693	0.006990	0.266128
-36.366471	-2.277272	2.721690	0.006947	0.266359
-36.427140	-2.210490	2.731686	0.006958	0.266662
-36.067333	-2.237363	2.741683	0.006891	0.266872
-35.618697	-2.285079	2.751680	0.006807	0.267056
-35.453428	-2.269862	2.761677	0.006776	0.267302
-34.945394	-2.310590	2.771674	0.006682	0.267582
-35.014997	-2.260389	2.781670	0.006694	0.267786
-34.592671	-2.298854	2.791667	0.006616	0.267994
-34.539267	-2.263253	2.801664	0.006606	0.268239
-34.152251	-2.284510	2.811661	0.006534	0.268504
-33.962965	-2.279033	2.821658	0.006498	0.268720
-33.718250	-2.288911	2.831654	0.006453	0.268907
-33.552259	-2.262647	2.841651	0.006422	0.269211
-33.169710	-2.291037	2.851648	0.006350	0.269433
-32.894265	-2.304562	2.861645	0.006299	0.269630
-32.642583	-2.311345	2.871642	0.006252	0.269840
-32.299307	-2.319781	2.881638	0.006188	0.270130
-32.091365	-2.312382	2.891635	0.006149	0.270372
-32.010483	-2.291796	2.901632	0.006134	0.270562
-31.485332	-2.355296	2.911629	0.006036	0.270733
-31.305544	-2.332650	2.921626	0.006003	0.271030
-31.085178	-2.337005	2.931622	0.005961	0.271221
-31.147568	-2.286617	2.941619	0.005973	0.271430
-30.794160	-2.302601	2.951616	0.005907	0.271688
-30.339247	-2.335379	2.961613	0.005822	0.271954
-30.363441	-2.291325	2.971610	0.005827	0.272166
-30.154900	-2.289879	2.981606	0.005788	0.272375
-29.786662	-2.312082	2.991603	0.005719	0.272614
-29.559796	-2.294622	3.001600	0.005677	0.272926
-29.159102	-2.330088	3.011597	0.005602	0.273125
-29.091141	-2.303315	3.021594	0.005589	0.273332
-28.876485	-2.297364	3.031590	0.005549	0.273571
-28.645562	-2.284669	3.041587	0.005506	0.273861
-28.588811	-2.249551	3.051584	0.005496	0.274101
-27.867671	-2.340749	3.061581	0.005361	0.274313
-27.885092	-2.299772	3.071578	0.005364	0.274513
-27.391755	-2.331184	3.081574	0.005272	0.274820
-27.336085	-2.298471	3.091571	0.005262	0.275046
-26.985704	-2.322815	3.101568	0.005197	0.275254
-26.826328	-2.306301	3.111565	0.005167	0.275494
-26.772025	-2.270893	3.121562	0.005157	0.275732
-26.203523	-2.329790	3.131558	0.005051	0.275966
-26.143554	-2.301759	3.141555	0.005039	0.276170
-25.852983	-2.312605	3.151552	0.004985	0.276391
-25.528418	-2.315053	3.161549	0.004925	0.276688
-25.200869	-2.330790	3.171546	0.004864	0.276917
-25.139736	-2.299847	3.181542	0.004852	0.277137
-24.871378	-2.308484	3.191539	0.004802	0.277348
-24.499410	-2.324658	3.201536	0.004733	0.277616
-24.262045	-2.312419	3.211533	0.004689	0.277906
-24.329071	-2.260385	3.221530	0.004701	0.278114
-23.622652	-2.351672	3.231526	0.004569	0.278307
-23.561181	-2.314554	3.241523	0.004558	0.278559
-23.382631	-2.292028	3.251520	0.004524	0.278845
-23.035934	-2.311190	3.261517	0.004460	0.279073
-22.802566	-2.313054	3.271514	0.004416	0.279284
-22.451008	-2.336270	3.281510	0.004351	0.279495
-22.053822	-2.351428	3.291507	0.004277	0.279791
-21.808642	-2.357337	3.301504	0.004231	0.279992
-22.067346	-2.263454	3.311501	0.004279	0.280234
-21.632088	-2.292484	3.321498	0.004198	0.280493
-21.338516	-2.304310	3.331494	0.004143	0.280708
-21.154833	-2.296444	3.341491	0.004109	0.280921
-20.796061	-2.321604	3.351488	0.004042	0.281128
-20.519309	-2.330131	3.361485	0.003990	0.281344
-20.275592	-2.309861	3.371482	0.003945	0.281676
-20.018850	-2.317711	3.381478	0.003897	0.281876
-20.094684	-2.261590	3.391475	0.003911	0.282094
-19.291325	-2.367971	3.401472	0.003761	0.282298
-19.143984	-2.336308	3.411469	0.003734	0.282598
-18.835440	-2.346369	3.421466	0.003676	0.282834
-18.816210	-2.308862	3.431462	0.003673	0.283044
-18.466897	-2.335354	3.441459	0.003608	0.283234
-18.259972	-2.310730	3.451456	0.003569	0.283552
-18.029305	-2.310956	3.461453	0.003526	0.283765
-17.756690	-2.317917	3.471450	0.003475	0.283983
-17.294275	-2.360071	3.481446	0.003389	0.284197
-17.452389	-2.274779	3.491443	0.003418	0.284485
-16.960261	-2.317078	3.501440	0.003327	0.284725
-16.904191	-2.285354	3.511437	0.003316	0.284939
-16.401092	-2.335692	3.521434	0.003222	0.285148
-16.146948	-2.320009	3.531430	0.003175	0.285463
-15.842787	-2.340506	3.541427	0.003118	0.285639
-15.510129	-2.365552	3.551424	0.003056	0.285819
-15.312769	-2.358881	3.561421	0.003019	0.286035
-15.025268	-2.352406	3.571418	0.002966	0.286333
-14.818158	-2.348811	3.581414	0.002927	0.286541
-14.522085	-2.365187	3.591411	0.002872	0.286731
-14.088210	-2.398049	3.601408	0.002791	0.286964
-13.966895	-2.369948	3.611405	0.002768	0.287217
-13.614082	-2.395672	3.621402	0.002702	0.287411
-13.561754	-2.366603	3.631398	0.002693	0.287605
-13.007066	-2.400118	3.641395	0.002589	0.287944
-12.977900	-2.372227	3.651392	0.002584	0.288112
-12.924761	-2.344245	3.661389	0.002574	0.288301
-12.486661	-2.373259	3.671386	0.002492	0.288555
-12.443435	-2.330165	3.681382	0.002484	0.288811
-12.127168	-2.344030	3.691379	0.002425	0.289030
-11.765356	-2.370228	3.701376	0.002358	0.289229
-11.393307	-2.387115	3.711373	0.002288	0.289483
-11.214204	-2.371021	3.721370	0.002255	0.289726
-11.083236	-2.356841	3.731366	0.002230	0.289917
-10.831811	-2.359657	3.741363	0.002183	0.290131
-10.626672	-2.330863	3.751360	0.002145	0.290461
-10.314625	-2.354156	3.761357	0.002087	0.290628
-10.230451	-2.331727	3.771354	0.002071	0.290816
-9.788954	-2.366161	3.781350	0.001989	0.291044
-9.547666	-2.354368	3.791347	0.001944	0.291321
-9.431393	-2.332117	3.801344	0.001922	0.291537
-9.163307	-2.339069	3.811341	0.001872	0.291745
-8.805957	-2.356922	3.821338	0.001805	0.291979
-8.651142	-2.329402	3.831334	0.001777	0.292255
-8.554938	-2.304002	3.841331	0.001759	0.292468
-8.118279	-2.342724	3.851328	0.001677	0.292669
-7.663354	-2.367942	3.861325	0.001592	0.292954
-7.649914	-2.323839	3.871322	0.001590	0.293184
-7.291057	-2.350060	3.881318	0.001523	0.293377
-7.151015	-2.333421	3.891315	0.001497	0.293585
-6.993139	-2.303287	3.901312	0.001467	0.293875
-6.756550	-2.296302	3.911309	0.001423	0.294121
-6.596420	-2.282702	3.921306	0.001393	0.294332
-6.458385	-2.265925	3.931302	0.001367	0.294538
-6.364006	-2.225172	3.941299	0.001350	0.294823
-5.901304	-2.251811	3.951296	0.001263	0.295105
-5.985805	-2.186320	3.961293	0.001279	0.295351
-5.487475	-2.231475	3.971290	0.001186	0.295574
-5.419944	-2.203662	3.981286	0.001174	0.295771
-5.388348	-2.152264	3.991283	0.001168	0.296050
-5.050131	-2.154441	4.001280	0.001104	0.296340
-5.244769	-2.062435	4.011277	0.001141	0.296617
-4.677064	-2.114649	4.021274	0.001035	0.296866
-4.525119	-2.090572	4.031270	0.001006	0.297118
-4.316068	-2.074783	4.041267	0.000967	0.297381
-4.021674	-2.073262	4.051264	0.000913	0.297649
-3.909513	-2.031281	4.061261	0.000892	0.297952
-3.680190	-2.015025	4.071258	0.000849	0.298234
-3.449282	-2.000899	4.081254	0.000806	0.298506
-3.412853	-1.951320	4.091251	0.000799	0.298779
-2.981323	-1.969085	4.101248	0.000718	0.299073
-2.968775	-1.914064	4.111245	0.000716	0.299350
-2.721403	-1.901674	4.121242	0.000670	0.299628
-2.574450	-1.867882	4.131238	0.000642	0.299920
-2.532991	-1.812630	4.141235	0.000634	0.300223
-2.319359	-1.786740	4.151232	0.000595	0.300535
-2.421047	-1.715702	4.161229	0.000613	0.300789
-1.958188	-1.734908	4.171226	0.000527	0.301101
-1.897750	-1.681700	4.181222	0.000516	0.301410
-1.928129	-1.607314	4.191219	0.000521	0.301741
-1.879287	-1.549108	4.201216	0.000512	0.302063
-1.583676	-1.531648	4.211213	0.000457	0.302404
-1.417989	-1.489864	4.221210	0.000426	0.302748
-1.324362	-1.435397	4.231206	0.000408	0.303090
-1.483861	-1.335466	4.241203	0.000438	0.303429
-1.420411	-1.271605	4.251200	0.000426	0.303788
-1.361508	-1.200503	4.261197	0.000415	0.304178
-1.058952	-1.175668	4.271194	0.000358	0.304558
-1.259530	-1.056380	4.281190	0.000396	0.304951
-1.120324	-0.998397	4.291187	0.000370	0.305347
-0.904550	-0.965307	4.301184	0.000329	0.305689
-0.801838	-0.891702	4.311181	0.000310	0.306126
-0.808144	-0.807590	4.321178	0.000311	0.306518
-0.666446	-0.752518	4.331174	0.000285	0.306900
-0.642702	-0.658354	4.341171	0.000280	0.307364
-0.552421	-0.583043	4.351168	0.000263	0.307796
-0.689546	-0.467850	4.361165	0.000288	0.308221
-0.262867	-0.444071	4.371162	0.000209	0.308696
-0.157432	-0.374746	4.381158	0.000189	0.309111
0.308633	-0.358182	4.391155	0.000102	0.309585
0.140714	-0.236027	4.401152	0.000133	0.310013
0.107371	-0.123169	4.411149	0.000139	0.310512
-0.017746	-0.010684	4.421146	0.000162	0.310930
-0.036471	0.103761	4.431142	0.000166	0.311447
0.000000	0.187083	4.441139	0.000159	0.311865

-0.141155	0.490070	4.446144	0.000185	0.313149
0.424887	0.946456	4.451149	0.000079	0.315722
1.004438	1.695658	4.456154	-0.000029	0.319614
1.518765	2.747090	4.461158	-0.000126	0.324755
1.813464	4.135626	4.466163	-0.000182	0.331117
2.340525	5.776261	4.471168	-0.000281	0.338618
3.013216	7.695359	4.476173	-0.000407	0.347229
3.672784	9.928431	4.481178	-0.000532	0.356897
5.447159	12.267463	4.486182	-0.000864	0.367525
7.203805	14.944841	4.491187	-0.001193	0.379133
9.180794	17.928738	4.496192	-0.001563	0.391677
11.503357	21.193481	4.501197	-0.001997	0.405059
14.216672	24.753115	4.506202	-0.002505	0.419274
16.454193	28.770873	4.511206	-0.002924	0.434262
19.483032	32.995315	4.516211	-0.003491	0.449873
24.618116	37.235745	4.521216	-0.004450	0.466190
28.849360	42.028957	4.526221	-0.005241	0.483119
33.015467	47.221384	4.531226	-0.006020	0.500591
41.317369	52.080247	4.536230	-0.007569	0.518619
55.996120	56.217079	4.541235	-0.010305	0.537182
89.230507	57.559661	4.546240	-0.016494	0.556526
128.860753	58.631301	4.551245	-0.023874	0.577389
130.011339	67.130636	4.556250	-0.024094	0.598741
131.475421	75.845352	4.561254	-0.024372	0.619988
132.745615	84.842520	4.566259	-0.024615	0.641087
134.776563	93.938901	4.571264	-0.024999	0.662024
137.138820	103.168561	4.576269	-0.025445	0.682724
139.336446	112.622833	4.581274	-0.025860	0.703213
142.072102	122.134870	4.586278	-0.026376	0.723426
144.728790	131.805955	4.591283	-0.026877	0.743367
147.574657	141.566488	4.596288	-0.027413	0.763018
151.591091	151.226429	4.601293	-0.028167	0.782369
153.697442	161.309513	4.606298	-0.028566	0.801403
156.018171	171.397319	4.611302	-0.029005	0.820067
157.604321	181.651053	4.616307	-0.029307	0.838377
159.311447	191.869288	4.621312	-0.029631	0.856269
161.156815	202.048603	4.626317	-0.029982	0.873770
162.511288	212.288644	4.631322	-0.030241	0.890885
164.061777	222.468847	4.636326	-0.030536	0.907635
165.549943	232.588426	4.641331	-0.030820	0.923969
166.947836	242.690857	4.646336	-0.031087	0.939967
168.091599	252.773045	4.651341	-0.031306	0.955599
169.116823	262.785208	4.656346	-0.031504	0.970844
170.256044	272.735186	4.661350	-0.031722	0.985790
171.668426	282.538047	4.666355	-0.031992	1.000369
172.912441	292.297134	4.671360	-0.032230	1.014634
173.734950	302.048891	4.676365	-0.032389	1.028588
174.629554	311.700293	4.681370	-0.032562	1.042232
176.000046	321.218387	4.686374	-0.032824	1.055631
177.058260	330.704896	4.691379	-0.033027	1.068745
178.337623	340.084091	4.696384	-0.033271	1.081607
179.468385	349.426901	4.701389	-0.033488	1.094236
180.345296	358.740404	4.706394	-0.033657	1.106625
181.161189	368.009738	4.711398	-0.033815	1.118806
181.882136	377.219964	4.716403	-0.033956	1.130759
182.766650	386.348544	4.721408	-0.034126	1.142519
183.405064	395.478998	4.726413	-0.034251	1.154109
184.277198	404.454448	4.731418	-0.034419	1.165440
185.407435	413.363496	4.736422	-0.034636	1.176635
185.576087	422.388893	4.741427	-0.034673	1.187666
186.335145	431.264475	4.746432	-0.034820	1.198536
187.351470	440.046716	4.751437	-0.035015	1.209249
187.776009	448.890322	4.756442	-0.035100	1.219821
188.378378	457.682449	4.761446	-0.035218	1.230277
188.759490	466.444800	4.766451	-0.035295	1.240567
189.282401	475.157851	4.771456	-0.035398	1.250742
189.744291	483.839102	4.776461	-0.035490	1.260787
190.361123	492.466302	4.781466	-0.035610	1.270721
191.189968	501.029142	4.786470	-0.035770	1.280546
191.716444	509.625848	4.791475	-0.035874	1.290276
192.055350	518.234639	4.796480	-0.035942	1.299911
192.775635	526.791911	4.801485	-0.036082	1.309489
193.030851	535.396928	4.806490	-0.036135	1.318964
193.742331	543.838846	4.811494	-0.036273	1.328278
194.418046	552.285894	4.816499	-0.036405	1.337525
194.928029	560.748079	4.821504	-0.036505	1.346695
195.457238	569.196372	4.826509	-0.036609	1.355792
196.054883	577.598167	4.831514	-0.036726	1.364791
196.520226	586.048576	4.836518	-0.036818	1.373758
196.951385	594.460442	4.841523	-0.036904	1.382621
197.558936	602.853674	4.846528	-0.037023	1.391438
198.192158	611.203234	4.851533	-0.037146	1.400159
198.574679	619.600273	4.856538	-0.037223	1.408832
198.788672	628.029077	4.861542	-0.037268	1.417455
199.265846	636.370534	4.866547	-0.037363	1.425982
199.694390	644.732319	4.871552	-0.037448	1.434471
200.500464	653.000672	4.876557	-0.037603	1.442878
200.951028	661.332376	4.881562	-0.037693	1.451241
201.420210	669.677662	4.886566	-0.037786	1.459572
201.971493	677.983216	4.891571	-0.037894	1.467830
202.365960	686.331720	4.896576	-0.037973	1.476059
202.895503	694.606130	4.901581	-0.038077	1.484191
203.199909	702.933168	4.906586	-0.038139	1.492294
203.734683	711.210172	4.911590	-0.038244	1.500341
204.125816	719.496980	4.916595	-0.038322	1.508332
205.195730	727.668849	4.921600	-0.038527	1.516276
205.695285	735.940804	4.926605	-0.038625	1.524186
206.260529	744.213340	4.931610	-0.038736	1.532065
206.989164	752.447231	4.936614	-0.038877	1.539892
207.338410	760.747847	4.941619	-0.038947	1.547685
207.708554	769.028200	4.946624	-0.039022	1.555422
208.044769	777.301896	4.951629	-0.039090	1.563110
208.373521	785.563154	4.956634	-0.039156	1.570747
208.526141	793.865817	4.961638	-0.039190	1.578360
209.081307	802.053879	4.966643	-0.039299	1.585890
209.582444	810.289076	4.971648	-0.039398	1.593420
209.733068	818.544438	4.976653	-0.039431	1.600881
210.311086	826.734234	4.981658	-0.039544	1.608310
210.603458	834.992907	4.986662	-0.039604	1.615726
211.248395	843.165231	4.991667	-0.039730	1.623081
211.569424	851.428723	4.996672	-0.039795	1.630437
211.983858	859.652483	5.001677	-0.039877	1.637739
212.216128	867.844620	5.006682	-0.039926	1.644955
212.578130	876.071148	5.011686	-0.039999	1.652187
212.689003	884.302755	5.016691	-0.040025	1.659357
213.307175	892.453399	5.021696	-0.040145	1.666496
213.969753	900.596710	5.026701	-0.040274	1.673604
214.268856	908.792296	5.031706	-0.040335	1.680677
214.675387	916.987614	5.036710	-0.040416	1.687735
214.917248	925.201524	5.041715	-0.040467	1.694757
214.885844	933.457413	5.046720	-0.040466	1.701749
215.406763	941.620884	5.051725	-0.040569	1.708707
215.804748	949.768767	5.056730	-0.040648	1.715608
216.215322	957.927937	5.061734	-0.040730	1.722493
216.450373	966.111454	5.066739	-0.040779	1.729347
216.805647	974.299026	5.071744	-0.040851	1.736193
217.150129	982.463535	5.076749	-0.040920	1.742991
217.314234	990.666012	5.081754	-0.040956	1.749771
218.294969	998.744591	5.086758	-0.041144	1.756528
218.434873	1006.945323	5.091763	-0.041175	1.763251
218.156606	1015.230193	5.096768	-0.041129	1.769964
218.603360	1023.359141	5.101773	-0.041217	1.776617
218.998629	1031.497268	5.106778	-0.041296	1.783246
219.405654	1039.663301	5.111782	-0.041378	1.789874
219.778846	1047.810336	5.116787	-0.041452	1.796458
219.942530	1055.972063	5.121792	-0.041488	1.803003
220.352226	1064.093894	5.126797	-0.041570	1.809524
220.120760	1072.330739	5.131802	-0.041532	1.816033
220.272202	1080.502146	5.136806	-0.041566	1.822514
220.882271	1088.561544	5.141811	-0.041685	1.828940
221.455776	1096.652346	5.146816	-0.041797	1.835363
221.754420	1104.791826	5.151821	-0.041858	1.841769
221.939769	1112.961546	5.156826	-0.041898	1.848163
222.214593	1121.121263	5.161830	-0.041954	1.854537
222.638941	1129.229660	5.166835	-0.042038	1.860867
222.708681	1137.424490	5.171840	-0.042057	1.867201
222.951840	1145.589390	5.176845	-0.042107	1.873510
223.325430	1153.667494	5.181850	-0.042182	1.879747
223.752072	1161.779018	5.186854	-0.042267	1.885995
224.196179	1169.878443	5.191859	-0.042355	1.892215
224.390362	1178.050418	5.196864	-0.042397	1.898440
224.689831	1186.171412	5.201869	-0.042458	1.904619
225.301207	1194.242881	5.206874	-0.042577	1.910776
225.772479	1202.376557	5.211878	-0.042670	1.916944
225.831740	1210.533766	5.216883	-0.042686	1.923063
226.392811	1218.621440	5.221888	-0.042796	1.929167
227.032030	1226.720921	5.226893	-0.042920	1.935269
227.434813	1234.849154	5.231898	-0.043001	1.941347
227.772362	1243.007149	5.236902	-0.043069	1.947420
228.215764	1251.109712	5.241907	-0.043157	1.953446
228.674977	1259.200663	5.246912	-0.043248	1.959446
228.888840	1267.329985	5.251917	-0.043293	1.965428
229.323264	1275.430041	5.256922	-0.043379	1.971395
229.641542	1283.585295	5.261926	-0.043444	1.977372
230.649388	1291.582573	5.266931	-0.043637	1.983290
231.086912	1299.732509	5.271936	-0.043723	1.989240
231.233738	1307.897969	5.276941	-0.043756	1.995151
231.585473	1315.985183	5.281946	-0.043827	2.001011
231.840795	1324.133189	5.286950	-0.043880	2.006887
232.016068	1332.270017	5.291955	-0.043918	2.012729
232.392100	1340.383789	5.296960	-0.043993	2.018559
232.572145	1348.496994	5.301965	-0.044032	2.024350
232.820631	1356.622158	5.306970	-0.044084	2.030141
233.285873	1364.719723	5.311974	-0.044176	2.035919
233.681892	1372.781992	5.316979	-0.044255	2.041648
233.893662	1380.917948	5.321984	-0.044299	2.047394
234.269189	1389.018762	5.326989	-0.044375	2.053115
234.323230	1397.151750	5.331994	-0.044390	2.058811
234.542269	1405.246587	5.336998	-0.044436	2.064480
234.794531	1413.355633	5.342003	-0.044488	2.070148
234.870532	1421.494443	5.347008	-0.044508	2.075802
234.902590	1429.612925	5.352013	-0.044519	2.081423
235.507946	1437.634157	5.357018	-0.044637	2.087019
235.887366	1445.745550	5.362022	-0.044713	2.092639
235.606032	1453.911255	5.367027	-0.044666	2.098216
235.930547	1461.991004	5.372032	-0.044732	2.103779
236.257995	1470.093359	5.377037	-0.044798	2.109343
236.527686	1478.185583	5.382042	-0.044854	2.114880
236.935261	1486.247058	5.387046	-0.044935	2.120395
237.021342	1494.327416	5.392051	-0.044956	2.125877
237.095879	1502.465315	5.397056	-0.044976	2.131383
237.239774	1510.554721	5.402061	-0.045008	2.136848
237.360854	1518.635928	5.407066	-0.045035	2.142292
237.721206	1526.708754	5.412070	-0.045108	2.147739
237.873554	1534.808630	5.417075	-0.045142	2.153171
238.101500	1542.888727	5.422080	-0.045189	2.158582
238.391226	1550.952726	5.427085	-0.045249	2.163976
238.547163	1559.052678	5.432090	-0.045283	2.169367
238.706852	1567.173085	5.437094	-0.045318	2.174758
238.809697	1575.254443	5.442099	-0.045342	2.180105
239.354380	1583.289957	5.447104	-0.045449	2.185451
239.469890	1591.413026	5.452109	-0.045476	2.190800
239.773747	1599.466841	5.457114	-0.045538	2.196109
240.203503	1607.523482	5.462118	-0.045623	2.201418
240.364075	1615.616232	5.467123	-0.045658	2.206713
240.541434	1623.725938	5.472128	-0.045697	2.212007
241.034466	1631.780305	5.477133	-0.045794	2.217282
241.178542	1639.863157	5.482138	-0.045826	2.222531
241.287245	1647.984971	5.487142	-0.045852	2.227790
241.508528	1656.060298	5.492147	-0.045898	2.233016
241.949421	1664.108564	5.497152	-0.045985	2.238233
242.284660	1672.170788	5.502157	-0.046053	2.243437
242.606843	1680.250641	5.507162	-0.046118	2.248638
243.003713	1688.339004	5.512166	-0.046198	2.253840
243.186060	1696.430700	5.517171	-0.046237	2.259013
243.624655	1704.469458	5.522176	-0.046324	2.264163
243.952174	1712.589125	5.527181	-0.046390	2.269342
243.902729	1720.737549	5.532186	-0.046386	2.274495
244.251874	1728.771359	5.537190	-0.046457	2.279599
244.420111	1736.829921	5.542195	-0.046493	2.284691
244.698503	1744.883630	5.547200	-0.046550	2.289778
244.777171	1752.993793	5.552205	-0.046570	2.294872
245.050242	1761.040762	5.557210	-0.046627	2.299932
245.576635	1769.077476	5.562214	-0.046730	2.304996
245.666766	1777.176021	5.567219	-0.046752	2.310049
245.946185	1785.258052	5.572224	-0.046809	2.315098
246.308439	1793.303986	5.577229	-0.046882	2.320121
246.560814	1801.358198	5.582234	-0.046934	2.325128
246.839797	1809.460216	5.587238	-0.046992	2.330156
247.009221	1817.539142	5.592243	-0.047028	2.335150
247.125719	1825.626709	5.597248	-0.047055	2.340134
247.463673	1833.684103	5.602253	-0.047124	2.345107
247.602807	1841.779279	5.607258	-0.047155	2.350076
248.493578	1849.775193	5.612262	-0.047326	2.355037
248.467478	1857.863084	5.617267	-0.047326	2.359967
248.803361	1865.920867	5.622272	-0.047394	2.364898
249.359005	1873.968534	5.627277	-0.047503	2.369831
249.738337	1882.030371	5.632282	-0.047579	2.374748
249.663983	1890.169900	5.637286	-0.047570	2.379664
249.697338	1898.232219	5.642291	-0.047582	2.384533
250.203009	1906.283550	5.647296	-0.047681	2.389423
250.472321	1914.371527	5.652301	-0.047737	2.394306
250.450809	1922.436035	5.657306	-0.047738	2.399141
250.711099	1930.497064	5.662310	-0.047792	2.403988
251.158155	1938.535953	5.667315	-0.047880	2.408826
251.381344	1946.620434	5.672320	-0.047927	2.413664
251.476394	1954.705823	5.677325	-0.047950	2.418482
251.541949	1962.775026	5.682330	-0.047968	2.423279
251.831765	1970.865773	5.687334	-0.048027	2.428096
251.938363	1978.952742	5.692339	-0.048052	2.432888
252.260606	1986.992989	5.697344	-0.048118	2.437659
252.535529	1995.019671	5.702349	-0.048174	2.442410
252.525123	2003.092456	5.707354	-0.048177	2.447156
252.927270	2011.155203	5.712358	-0.048258	2.451918
253.384677	2019.178594	5.717363	-0.048348	2.456653
253.504002	2027.252117	5.722368	-0.048375	2.461382
253.684520	2035.334818	5.727373	-0.048414	2.466111
253.889668	2043.386731	5.732378	-0.048458	2.470816
254.454604	2051.421767	5.737382	-0.048568	2.475529
254.681381	2059.454251	5.742387	-0.048616	2.480206
255.065625	2067.490113	5.747392	-0.048693	2.484888
255.474161	2075.576339	5.752397	-0.048774	2.489592
255.865652	2083.614798	5.757402	-0.048852	2.494258
256.124271	2091.711634	5.762406	-0.048906	2.498939
256.403511	2099.762420	5.767411	-0.048963	2.503586
256.678461	2107.841438	5.772416	-0.049020	2.508241
256.809858	2115.938952	5.777421	-0.049049	2.512886
257.196297	2123.939008	5.782426	-0.049127	2.517487
257.520985	2131.991503	5.787430	-0.049192	2.522104
257.606806	2140.064236	5.792435	-0.049214	2.526706
257.971411	2148.134569	5.797440	-0.049287	2.531320
258.402668	2156.173839	5.802445	-0.049372	2.535912
258.273611	2164.276125	5.807450	-0.049354	2.540490
258.604881	2172.319609	5.812454	-0.049421	2.545061
258.968343	2180.364512	5.817459	-0.049494	2.549626
259.314187	2188.413282	5.822464	-0.049563	2.554184
259.605084	2196.464484	5.827469	-0.049623	2.558731
259.621002	2204.516212	5.832474	-0.049631	2.563251
259.821795	2212.607195	5.837478	-0.049674	2.567798
259.973463	2220.669157	5.842483	-0.049707	2.572317
260.320893	2228.706593	5.847488	-0.049777	2.576828
260.562684	2236.768341	5.852493	-0.049827	2.581337
260.742775	2244.823211	5.857498	-0.049866	2.585831
260.950216	2252.931246	5.862502	-0.049910	2.590348
261.247549	2261.044784	5.867507	-0.049971	2.594866
261.439980	2269.047502	5.872512	-0.050012	2.599308
261.852435	2277.024528	5.877517	-0.050094	2.603743
262.130863	2285.052898	5.882522	-0.050151	2.608190
262.497838	2293.112442	5.887526	-0.050225	2.612652
262.440215	2301.194717	5.892531	-0.050219	2.617090
262.516969	2309.237752	5.897536	-0.050239	2.621508
262.900200	2317.278476	5.902541	-0.050316	2.625938
263.017240	2325.346130	5.907546	-0.050343	2.630358
263.178234	2333.415677	5.912550	-0.050378	2.634774
263.529283	2341.399616	5.917555	-0.050449	2.639148
263.354878	2349.531282	5.922560	-0.050421	2.643561
263.828746	2357.529858	5.927565	-0.050515	2.647937
264.377170	2365.529299	5.932570	-0.050622	2.652311
264.692226	2373.601917	5.937574	-0.050686	2.656702
264.842341	2381.666176	5.942579	-0.050720	2.661071
265.158755	2389.702509	5.947584	-0.050784	2.665428
265.478101	2397.784312	5.952589	-0.050849	2.669802
265.594204	2405.827761	5.957594	-0.050875	2.674136
265.956109	2413.853705	5.962598	-0.050948	2.678469
266.244320	2421.871551	5.967603	-0.051007	2.682786
266.375759	2429.942027	5.972608	-0.051037	2.687113
266.726328	2438.003033	5.977613	-0.051107	2.691443
266.896343	2446.062852	5.982618	-0.051144	2.695754
267.177807	2454.114538	5.987622	-0.051202	2.700060
267.142003	2462.153029	5.992627	-0.051201	2.704332
267.270148	2470.229129	5.997632	-0.051230	2.708628
267.662703	2478.285636	6.002637	-0.051308	2.712924
267.880383	2486.312456	6.007642	-0.051354	2.717186
268.133071	2494.351941	6.012646	-0.051406	2.721450
268.427360	2502.377281	6.017651	-0.051466	2.725702
268.774334	2510.425032	6.022656	-0.051536	2.729963
269.058619	2518.494258	6.027661	-0.051595	2.734225
269.196960	2526.524067	6.032666	-0.051626	2.738450
269.665879	2534.574005	6.037670	-0.051718	2.742699
269.878235	2542.624888	6.042675	-0.051763	2.746927
270.024488	2550.729643	6.047680	-0.051796	2.751172
270.572609	2558.763374	6.052685	-0.051903	2.755398
270.701031	2566.767760	6.057690	-0.051932	2.759577
271.045812	2574.798395	6.062694	-0.052002	2.763776
271.177520	2582.859402	6.067699	-0.052031	2.767971
271.502531	2590.902092	6.072704	-0.052097	2.772162
271.650154	2598.967176	6.077709	-0.052130	2.776348
271.796880	2606.996290	6.082714	-0.052163	2.780509
272.300393	2615.013200	6.087718	-0.052262	2.784678
272.425929	2623.086097	6.092723	-0.052290	2.788848
272.533427	2631.140490	6.097728	-0.052316	2.793000
272.766058	2639.184425	6.102733	-0.052364	2.797149
273.195005	2647.180422	6.107738	-0.052449	2.801278
273.417942	2655.254508	6.112742	-0.052496	2.805429
273.688245	2663.276570	6.117747	-0.052552	2.809550
274.056347	2671.320628	6.122752	-0.052625	2.813682
274.149066	2679.383505	6.127757	-0.052648	2.817802
274.116371	2687.454339	6.132762	-0.052647	2.821911
274.685398	2695.481003	6.137766	-0.052758	2.826028
274.725476	2703.546191	6.142771	-0.052771	2.830127
274.859861	2711.590698	6.147776	-0.052802	2.834215
275.203145	2719.614900	6.152781	-0.052871	2.838300
275.696617	2727.581137	6.157786	-0.052968	2.842357
276.221417	2735.646392	6.162790	-0.053071	2.846461
276.625280	2743.668015	6.167795	-0.053151	2.850530
276.906441	2751.716562	6.172800	-0.053209	2.854599
277.180175	2759.783817	6.177805	-0.053265	2.858671
277.254681	2767.833110	6.182810	-0.053284	2.862717
277.677026	2775.888650	6.187814	-0.053368	2.866780
277.805688	2783.936707	6.192819	-0.053398	2.870818
277.945523	2791.996157	6.197824	-0.053429	2.874855
278.213160	2800.031325	6.202829	-0.053484	2.878882
278.433672	2808.034961	6.207834	-0.053530	2.882885
278.689451	2816.097335	6.212838	-0.053583	2.886914
278.863013	2824.153959	6.217843	-0.053621	2.890929
279.015183	2832.214847	6.222848	-0.053655	2.894940
279.293104	2840.238280	6.227853	-0.053712	2.898934
279.308832	2848.276982	6.232858	-0.053720	2.902915
279.580625	2856.344943	6.237862	-0.053776	2.906919
279.795563	2864.406468	6.242867	-0.053821	2.910912
280.036718	2872.447763	6.247872	-0.053871	2.914890
280.313969	2880.438445	6.252877	-0.053928	2.918840
280.434058	2888.465766	6.257882	-0.053956	2.922794
280.773364	2896.488710	6.262886	-0.054024	2.926753
280.881295	2904.553964	6.267891	-0.054050	2.930714
281.230571	2912.565345	6.272896	-0.054120	2.934656
281.295433	2920.630458	6.277901	-0.054137	2.938604
281.411342	2928.661842	6.282906	-0.054164	2.942533
281.782172	2936.697882	6.287910	-0.054238	2.946473
282.113428	2944.737669	6.292915	-0.054305	2.950407
282.362880	2952.766475	6.297920	-0.054357	2.954326
282.640577	2960.801720	6.302925	-0.054414	2.958245
283.009714	2968.797264	6.307930	-0.054488	2.962143
283.161772	2976.874825	6.312934	-0.054522	2.966065
283.279321	2984.909446	6.317939	-0.054549	2.969959
283.679011	2992.955840	6.322944	-0.054629	2.973869
284.024085	3000.992401	6.327949	-0.054698	2.977765
283.929435	3009.039755	6.332954	-0.054686	2.981639
284.227987	3017.074701	6.337958	-0.054747	2.985522
284.479789	3025.098000	6.342963	-0.054799	2.989392
284.595709	3033.178938	6.347968	-0.054826	2.993278
284.880744	3041.191105	6.352973	-0.054884	2.997134
284.875809	3049.234933	6.357978	-0.054888	3.000986
285.300802	3057.215177	6.362982	-0.054973	3.004824
285.347516	3065.293202	6.367987	-0.054987	3.008685
285.465765	3073.359629	6.372992	-0.055014	3.012538
285.812483	3081.383380	6.377997	-0.055084	3.016378
285.850753	3089.418671	6.383002	-0.055096	3.020204
286.313115	3097.410832	6.388006	-0.055188	3.024025
286.602934	3105.455899	6.393011	-0.055247	3.027857
286.512024	3113.550068	6.398016	-0.055235	3.031689
286.795877	3121.585375	6.403021	-0.055293	3.035507
286.937487	3129.571863	6.408026	-0.055325	3.039290
287.176710	3137.626310	6.413030	-0.055375	3.043105
287.177012	3145.663623	6.418035	-0.055380	3.046895
287.570116	3153.705149	6.423040	-0.055459	3.050702
287.554941	3161.778171	6.428045	-0.055461	3.054499
287.671818	3169.787681	6.433050	-0.055488	3.058268
287.606592	3177.863964	6.438054	-0.055481	3.062055
288.113680	3185.832337	6.443059	-0.055581	3.065814
288.035101	3193.921306	6.448064	-0.055572	3.069597
288.561851	3201.953135	6.453069	-0.055675	3.073377
288.544853	3209.985522	6.458074	-0.055677	3.077127
288.955829	3217.995807	6.463078	-0.055759	3.080882
288.971762	3226.021036	6.468083	-0.055767	3.084621
289.162716	3234.056240	6.473088	-0.055808	3.088369
289.382727	3242.105737	6.478093	-0.055854	3.092119
289.532114	3250.137998	6.483098	-0.055887	3.095854
289.698858	3258.166821	6.488102	-0.055924	3.099584
290.148056	3266.140291	6.493107	-0.056013	3.103297
290.473585	3274.184720	6.498112	-0.056078	3.107032
290.431615	3282.278202	6.503117	-0.056076	3.110768
290.415497	3290.306332	6.508122	-0.056078	3.114471
291.042078	3298.303668	6.513126	-0.056200	3.118184
291.024677	3306.338969	6.518131	-0.056202	3.121882
291.077807	3314.395064	6.523136	-0.056217	3.125587
291.355808	3322.425981	6.528141	-0.056274	3.129287
291.474306	3330.466148	6.533146	-0.056302	3.132979
291.802503	3338.481986	6.538150	-0.056368	3.136666
292.105145	3346.516119	6.543155	-0.056430	3.140355
292.381956	3354.520041	6.548160	-0.056487	3.144025
292.391852	3362.607850	6.553165	-0.056494	3.147717
292.622500	3370.642198	6.558170	-0.056542	3.151390
292.927522	3378.684869	6.563174	-0.056604	3.155066
293.145888	3386.680375	6.568179	-0.056650	3.158712
293.517491	3394.674970	6.573184	-0.056724	3.162360
293.670173	3402.754193	6.578189	-0.056758	3.166033
293.725162	3410.780775	6.583194	-0.056774	3.169673
293.831297	3418.850258	6.588198	-0.056799	3.173331
294.132226	3426.842393	6.593203	-0.056860	3.176958
294.302513	3434.876605	6.598208	-0.056897	3.180594
294.430876	3442.890252	6.603213	-0.056926	3.184215
294.613407	3450.929325	6.608218	-0.056965	3.187846
294.754758	3459.027455	6.613222	-0.056997	3.191497
294.652175	3467.080695	6.618227	-0.056983	3.195113
294.971910	3475.021590	6.623232	-0.057048	3.198693
295.117783	3483.085080	6.628237	-0.057080	3.202316
295.206279	3491.111704	6.633242	-0.057102	3.205917
295.362537	3499.142302	6.638246	-0.057137	3.209518
295.635211	3507.198116	6.643251	-0.057193	3.213131
295.752776	3515.242974	6.648256	-0.057220	3.216728
295.771023	3523.280457	6.653261	-0.057228	3.220314
295.999827	3531.250104	6.658266	-0.057276	3.223875
296.284121	3539.316764	6.663270	-0.057335	3.227477
296.523049	3547.358235	6.668275	-0.057384	3.231062
296.437328	3555.399350	6.673280	-0.057374	3.234629
296.719564	3563.425164	6.678285	-0.057431	3.238201
296.656678	3571.431842	6.683290	-0.057425	3.241746
297.275937	3579.410712	6.688294	-0.057546	3.245303
297.187483	3587.469223	6.693299	-0.057534	3.248862
297.053156	3595.535168	6.698304	-0.057515	3.252419
297.598864	3603.532244	6.703309	-0.057622	3.255969
297.416344	3611.565043	6.708314	-0.057593	3.259502
297.882539	3619.562494	6.713318	-0.057685	3.263041
298.173587	3627.578006	6.718323	-0.057744	3.266577
298.364753	3635.635070	6.723328	-0.057785	3.270124
298.741351	3643.684565	6.728333	-0.057861	3.273671
298.769504	3651.713804	6.733338	-0.057871	3.277191
298.877792	3659.767158	6.738342	-0.057897	3.280721
299.022247	3667.726642	6.743347	-0.057929	3.284208
299.203100	3675.773557	6.748352	-0.057968	3.287730
299.482681	3683.824470	6.753357	-0.058025	3.291255
299.734044	3691.845884	6.758362	-0.058077	3.294761
299.977172	3699.892506	6.763366	-0.058128	3.298275
299.868367	3707.934549	6.768371	-0.058113	3.301769
300.008468	3715.948134	6.773376	-0.058144	3.305256
300.256506	3724.006555	6.778381	-0.058196	3.308764
300.380865	3732.026461	6.783386	-0.058224	3.312246
300.544200	3740.108337	6.788390	-0.058260	3.315753
300.643562	3748.069603	6.793395	-0.058283	3.319201
300.822081	3756.079803	6.798400	-0.058322	3.322671
301.200237	3764.133425	6.803405	-0.058398	3.326163
301.259124	3772.153946	6.808410	-0.058414	3.329624
301.447976	3780.228548	6.813414	-0.058454	3.333111
301.445054	3788.266331	6.818419	-0.058459	3.336570
301.396325	3796.292550	6.823424	-0.058455	3.340019
301.565076	3804.316535	6.828429	-0.058492	3.343472
302.146687	3812.273147	6.833434	-0.058606	3.346908
302.575693	3820.326724	6.838438	-0.058691	3.350377
302.553740	3828.352625	6.843443	-0.058692	3.353812
302.607378	3836.391077	6.848448	-0.058707	3.357253
302.785998	3844.477311	6.853453	-0.058746	3.360715
303.098539	3852.392715	6.858458	-0.058809	3.364105
303.256406	3860.479894	6.863462	-0.058844	3.367560
303.582010	3868.502955	6.868467	-0.058910	3.370990
303.315436	3876.560744	6.873472	-0.058865	3.374409
303.598689	3884.587832	6.878477	-0.058923	3.377832
303.995760	3892.581754	6.883482	-0.059003	3.381241
303.911276	3900.651185	6.888486	-0.058992	3.384662
304.232714	3908.644485	6.893491	-0.059057	3.388061
304.426477	3916.707824	6.898496	-0.059099	3.391482
304.863576	3924.754897	6.903501	-0.059185	3.394902
304.849654	3932.754171	6.908506	-0.059188	3.398281
304.949336	3940.788732	6.913510	-0.059212	3.401677
305.216634	3948.793433	6.918515	-0.059267	3.405062
305.287119	3956.808828	6.923520	-0.059285	3.408441
305.268491	3964.902840	6.928525	-0.059287	3.411847
305.514091	3972.894236	6.933530	-0.059338	3.415216
305.761925	3980.898662	6.938534	-0.059389	3.418586
305.736719	3988.948188	6.943539	-0.059390	3.421963
305.693895	3996.963920	6.948544	-0.059387	3.425322
305.990001	4004.994227	6.953549	-0.059448	3.428695
305.983142	4013.026500	6.958554	-0.059452	3.432055
306.818261	4020.986876	6.963558	-0.059612	3.435411
306.895533	4029.046774	6.968563	-0.059632	3.438779
306.914246	4037.123210	6.973568	-0.059641	3.442149
307.519564	4045.072914	6.978573	-0.059759	3.445483
307.783389	4053.082013	6.983578	-0.059813	3.448826
307.840706	4061.199360	6.988582	-0.059829	3.452204
307.862666	4069.238885	6.993587	-0.059839	3.455545
308.059425	4077.195151	6.998592	-0.059881	3.458855
308.440380	4085.272142	7.003597	-0.059957	3.462217
308.604339	4093.280602	7.008602	-0.059993	3.465540
308.708492	4101.317540	7.013606	-0.060017	3.468870
308.788540	4109.370255	7.018611	-0.060037	3.472203
308.856722	4117.407513	7.023616	-0.060055	3.475525
309.087772	4125.356867	7.028621	-0.060104	3.478814
309.175858	4133.410967	7.033626	-0.060125	3.482137
309.285495	4141.468047	7.038630	-0.060151	3.485460
309.581215	4149.451177	7.043635	-0.060211	3.488755
309.188526	4157.582846	7.048640	-0.060144	3.492085
309.755468	4165.523950	7.053645	-0.060254	3.495365
309.937035	4173.531584	7.058650	-0.060293	3.498657
310.093267	4181.569433	7.063654	-0.060328	3.501957
310.396218	4189.575119	7.068659	-0.060389	3.505246
310.486994	4197.616666	7.073664	-0.060412	3.508539
310.684783	4205.690248	7.078669	-0.060454	3.511846
310.893414	4213.667442	7.083674	-0.060498	3.515111
311.511524	4221.675197	7.088678	-0.060618	3.518398
311.633015	4229.691227	7.093683	-0.060646	3.521670
311.665959	4237.736247	7.098688	-0.060658	3.524947
311.994761	4245.758867	7.103693	-0.060724	3.528222
312.240509	4253.790161	7.108698	-0.060775	3.531494
312.629110	4261.801056	7.113702	-0.060853	3.534760
312.706645	4269.875878	7.118707	-0.060872	3.538039
312.957719	4277.890171	7.123712	-0.060924	3.541295
312.702105	4285.945463	7.128717	-0.060882	3.544550
312.720880	4293.981632	7.133722	-0.060891	3.547802
313.511329	4301.972434	7.138726	-0.061043	3.551056
313.384661	4310.073287	7.143731	-0.061025	3.554324
313.537050	4318.026424	7.148736	-0.061059	3.557538
313.876100	4326.047836	7.153741	-0.061127	3.560782
314.071159	4333.980592	7.158746	-0.061169	3.563983
314.223228	4342.062757	7.163750	-0.061202	3.567240
314.395994	4350.084791	7.168755	-0.061240	3.570470
314.626616	4358.096616	7.173760	-0.061288	3.573695
314.731340	4366.172690	7.178765	-0.061313	3.576939
314.757279	4374.160755	7.183770	-0.061323	3.580143
314.813239	4382.194305	7.188774	-0.061338	3.583363
314.823596	4390.270496	7.193779	-0.061346	3.586595
315.016150	4398.282692	7.198784	-0.061387	3.589805
315.024879	4406.314945	7.203789	-0.061394	3.593014
315.332900	4414.301828	7.208794	-0.061456	3.596211
315.591075	4422.308243	7.213798	-0.061510	3.599411
315.694256	4430.316016	7.218803	-0.061534	3.602604
315.929994	4438.385604	7.223808	-0.061583	3.605824
316.176018	4446.398155	7.228813	-0.061634	3.609017
316.246974	4454.436148	7.233818	-0.061653	3.612213
316.520562	4462.492575	7.238822	-0.061709	3.615420
316.590870	4470.491448	7.243827	-0.061727	3.618594
316.743109	4478.502512	7.248832	-0.061761	3.621774
316.896291	4486.543499	7.253837	-0.061795	3.624962
317.057940	4494.553138	7.258842	-0.061830	3.628135
317.251539	4502.618949	7.263846	-0.061872	3.631328
317.211856	4510.627917	7.268851	-0.061869	3.634490
317.546037	4518.603010	7.273856	-0.061937	3.637646
317.779594	4526.644616	7.278861	-0.061986	3.640823
317.877207	4534.581644	7.283866	-0.062009	3.643952
317.848375	4542.709074	7.288870	-0.062009	3.647149
318.348174	4550.686495	7.293875	-0.062107	3.650300
318.336051	4558.748293	7.298880	-0.062110	3.653466
318.243457	4566.837039	7.303885	-0.062098	3.656638
318.369469	4574.781333	7.308890	-0.062127	3.659757
318.468224	4582.803713	7.313894	-0.062151	3.662903
319.110692	4590.805700	7.318899	-0.062276	3.666053
319.294216	4598.830639	7.323904	-0.062315	3.669197
319.444904	4606.887993	7.328909	-0.062349	3.672350
319.366329	4614.916122	7.333914	-0.062339	3.675483
319.660048	4622.909526	7.338918	-0.062399	3.678609
319.877427	4630.939930	7.343923	-0.062445	3.681745
320.128234	4638.933303	7.348928	-0.062497	3.684865
320.149509	4646.996534	7.353933	-0.062506	3.688003
320.086124	4655.070783	7.358938	-0.062500	3.691141
320.319057	4663.065919	7.363942	-0.062548	3.694253
320.192068	4671.146086	7.368947	-0.062530	3.697386
320.046555	4679.174705	7.373952	-0.062508	3.700496
320.179951	4687.180041	7.378957	-0.062538	3.703601
320.324909	4695.167995	7.383962	-0.062570	3.706698
320.661319	4703.202423	7.388966	-0.062638	3.709814
321.305255	4711.219292	7.393971	-0.062763	3.712929
321.244465	4719.293109	7.398976	-0.062757	3.716046
321.534054	4727.231552	7.403981	-0.062817	3.719116
321.764926	4735.246987	7.408986	-0.062865	3.722212
322.251453	4743.236203	7.413990	-0.062961	3.725302
322.309286	4751.288742	7.418995	-0.062977	3.728403
322.245763	4759.327513	7.424000	-0.062970	3.731493
322.861428	4767.337669	7.429005	-0.063090	3.734586
322.309229	4775.413434	7.434010	-0.062993	3.737673
322.686818	4783.404554	7.439014	-0.063068	3.740748
323.017289	4791.384276	7.444019	-0.063135	3.743814
323.104833	4799.436061	7.449024	-0.063156	3.746900
323.325631	4807.485171	7.454029	-0.063203	3.749986
323.517870	4815.467688	7.459034	-0.063244	3.753042
323.738478	4823.526125	7.464038	-0.063290	3.756126
323.740110	4831.512738	7.469043	-0.063296	3.759175
324.238019	4839.513723	7.474048	-0.063394	3.762239
324.364659	4847.555549	7.479053	-0.063423	3.765306
324.558221	4855.564515	7.484058	-0.063464	3.768361
324.723155	4863.623733	7.489062	-0.063500	3.771431
324.744917	4871.667332	7.494067	-0.063509	3.774489
324.688703	4879.676288	7.499072	-0.063504	3.777530
324.989062	4887.718892	7.504077	-0.063565	3.780589
325.561140	4895.614601	7.509082	-0.063677	3.783597
325.759523	4903.713023	7.514086	-0.063719	3.786671
325.839063	4911.746243	7.519091	-0.063739	3.789714
326.020994	4919.777202	7.524096	-0.063779	3.792756
326.049802	4927.881076	7.529101	-0.063789	3.795820
326.119844	4935.806253	7.534106	-0.063807	3.798815
326.446337	4943.852063	7.539110	-0.063874	3.801859
326.608698	4951.860580	7.544115	-0.063909	3.804883
326.833919	4959.858487	7.549120	-0.063956	3.807901
326.981753	4967.938019	7.554125	-0.063989	3.810947
326.890049	4975.929698	7.559130	-0.063977	3.813951
327.291627	4983.975414	7.564134	-0.064057	3.816984
327.701224	4991.960711	7.569139	-0.064139	3.819993
327.888637	4999.959866	7.574144	-0.064179	3.822999
328.291372	5008.019284	7.579149	-0.064259	3.826030
328.284396	5016.032776	7.584154	-0.064263	3.829032
328.574241	5024.092658	7.589158	-0.064322	3.832056
328.653355	5032.105443	7.594163	-0.064342	3.835056
328.732583	5040.107826	7.599168	-0.064363	3.838049
328.977483	5048.179594	7.604173	-0.064413	3.841069
328.857690	5056.120003	7.609178	-0.064396	3.844030
328.869166	5064.250677	7.614182	-0.064404	3.847062
328.883535	5072.250994	7.619187	-0.064412	3.850044
329.138395	5080.261320	7.624192	-0.064464	3.853032
329.412828	5088.293650	7.629197	-0.064521	3.856026
329.381213	5096.250686	7.634202	-0.064520	3.858984
329.527865	5104.286073	7.639206	-0.064553	3.861972
329.389931	5112.334633	7.644211	-0.064532	3.864956
329.538046	5120.356358	7.649216	-0.064565	3.867935
329.770864	5128.436874	7.654221	-0.064614	3.870934
329.801117	5136.502241	7.659226	-0.064625	3.873922
330.166288	5144.478321	7.664230	-0.064698	3.876881
329.994637	5152.466921	7.669235	-0.064671	3.879831
330.348577	5160.365571	7.674240	-0.064742	3.882757
330.620825	5168.438127	7.679245	-0.064798	3.885743
330.764973	5176.418254	7.684250	-0.064830	3.888689
330.964607	5184.481097	7.689254	-0.064873	3.891666
331.043673	5192.544936	7.694259	-0.064893	3.894637
331.386137	5200.496235	7.699264	-0.064962	3.897571
331.464675	5208.561436	7.704269	-0.064982	3.900539
331.480786	5216.512974	7.709274	-0.064990	3.903461
331.729891	5224.565924	7.714278	-0.065042	3.906423
331.975156	5232.600624	7.719283	-0.065093	3.909376
332.024088	5240.621366	7.724288	-0.065107	3.912318
332.221909	5248.693077	7.729293	-0.065149	3.915280
332.239680	5256.664549	7.734298	-0.065158	3.918198
332.538592	5264.701355	7.739302	-0.065219	3.921144
332.738361	5272.658158	7.744307	-0.065261	3.924057
332.857727	5280.720100	7.749312	-0.065289	3.927004
333.230916	5288.740628	7.754317	-0.065363	3.929939
333.258437	5296.763104	7.759322	-0.065374	3.932865
333.460547	5304.807344	7.764326	-0.065417	3.935801
333.637361	5312.825550	7.769331	-0.065455	3.938724
333.789668	5320.832180	7.774336	-0.065489	3.941641
334.025396	5328.867146	7.779341	-0.065538	3.944567
334.045257	5336.945033	7.784346	-0.065547	3.947503
334.386100	5344.925692	7.789350	-0.065615	3.950407
334.422936	5352.958821	7.794355	-0.065628	3.953322
334.560302	5360.990227	7.799360	-0.065658	3.956236
334.805622	5368.964417	7.804365	-0.065709	3.959130
334.933875	5376.957337	7.809370	-0.065738	3.962026
335.216438	5385.001967	7.814374	-0.065796	3.964941
335.334954	5393.007262	7.819379	-0.065824	3.967837
335.356789	5401.067360	7.824384	-0.065833	3.970749
335.664168	5409.102824	7.829389	-0.065896	3.973655
335.794000	5417.123618	7.834394	-0.065925	3.976550
335.981327	5425.102440	7.839398	-0.065965	3.979430
336.093519	5433.125486	7.844403	-0.065991	3.982321
336.238087	5441.127677	7.849408	-0.066024	3.985204
336.399794	5449.233028	7.854413	-0.066059	3.988121
336.245892	5457.255355	7.859418	-0.066036	3.991002
336.777671	5465.167806	7.864422	-0.066140	3.993853
337.009799	5473.213642	7.869427	-0.066188	3.996744
337.126158	5481.221292	7.874432	-0.066215	3.999617
337.115911	5489.263437	7.879437	-0.066219	4.002499
337.345822	5497.291289	7.884442	-0.066267	4.005377
337.398569	5505.307188	7.889446	-0.066282	4.008247
337.576581	5513.364906	7.894451	-0.066320	4.011131
337.529653	5521.333258	7.899456	-0.066317	4.013977
337.652393	5529.434059	7.904461	-0.066345	4.016871
338.015880	5537.359784	7.909466	-0.066418	4.019705
338.211145	5545.405896	7.914470	-0.066459	4.022577
338.204355	5553.425939	7.919475	-0.066463	4.025434
338.406340	5561.430722	7.924480	-0.066506	4.028288
338.642227	5569.532780	7.929485	-0.066556	4.031174
338.904889	5577.529727	7.934490	-0.066610	4.034021
339.153611	5585.564720	7.939494	-0.066661	4.036880
339.326346	5593.520966	7.944499	-0.066699	4.039707
339.370815	5601.529108	7.949504	-0.066712	4.042549
339.686983	5609.538720	7.954509	-0.066776	4.045393
339.625423	5617.562952	7.959514	-0.066770	4.048235
340.108034	5625.608441	7.964518	-0.066865	4.051090
340.409741	5633.565371	7.969523	-0.066927	4.053910
340.429931	5641.676367	7.974528	-0.066936	4.056777
340.693096	5649.641945	7.979533	-0.066990	4.059595
340.781498	5657.688006	7.984538	-0.067012	4.062437
341.145097	5665.716335	7.989542	-0.067085	4.065275
341.293624	5673.740200	7.994547	-0.067118	4.068105
341.506480	5681.782926	7.999552	-0.067163	4.070942
341.742410	5689.797548	8.004557	-0.067212	4.073766
341.814020	5697.843460	8.009562	-0.067230	4.076598
341.843592	5705.811488	8.014566	-0.067241	4.079399
342.164494	5713.845660	8.019571	-0.067306	4.082226
342.310782	5721.812784	8.024576	-0.067339	4.085025
342.423111	5729.901704	8.029581	-0.067365	4.087864
342.322406	5737.912485	8.034586	-0.067351	4.090671
342.514817	5745.943375	8.039590	-0.067392	4.093487
342.648750	5753.982287	8.044595	-0.067423	4.096303
342.724683	5761.953281	8.049600	-0.067442	4.099092
343.152353	5769.977068	8.054605	-0.067527	4.101904
343.290687	5777.956582	8.059610	-0.067558	4.104693
343.321738	5786.040743	8.064614	-0.067569	4.107516
343.432900	5794.044014	8.069619	-0.067595	4.110309
343.546450	5802.038356	8.074624	-0.067621	4.113098
343.705526	5810.094637	8.079629	-0.067656	4.115907
343.743029	5818.057244	8.084634	-0.067669	4.118679
344.032586	5826.109577	8.089638	-0.067728	4.121485
344.003038	5834.052461	8.094643	-0.067727	4.124246
344.173981	5842.086337	8.099648	-0.067765	4.127039
344.421564	5850.184831	8.104653	-0.067816	4.129854
344.311632	5858.152429	8.109658	-0.067801	4.132617
344.611566	5866.204169	8.114662	-0.067862	4.135413
344.926218	5874.182512	8.119667	-0.067926	4.138182
344.953241	5882.234986	8.124672	-0.067936	4.140970
344.962377	5890.225890	8.129677	-0.067943	4.143736
345.153861	5898.259543	8.134682	-0.067984	4.146516
345.423588	5906.274059	8.139686	-0.068039	4.149289
345.542568	5914.288810	8.144691	-0.068067	4.152058
345.494951	5922.274411	8.149696	-0.068063	4.154813
345.790994	5930.345018	8.154701	-0.068124	4.157600
345.879775	5938.342672	8.159706	-0.068145	4.160358
345.924076	5946.339135	8.164710	-0.068159	4.163112
346.042193	5954.420819	8.169715	-0.068186	4.165895
346.410902	5962.359099	8.174720	-0.068260	4.168630
346.530108	5970.451622	8.179725	-0.068288	4.171413
346.612809	5978.419978	8.184730	-0.068308	4.174151
346.772649	5986.490044	8.189734	-0.068343	4.176923
346.803969	5994.489957	8.194739	-0.068354	4.179668
346.723158	6002.535521	8.199744	-0.068345	4.182425
346.826176	6010.589988	8.204749	-0.068369	4.185185
347.242128	6018.518556	8.209754	-0.068452	4.187904
347.366990	6026.582074	8.214758	-0.068480	4.190665
347.655994	6034.642601	8.219763	-0.068539	4.193424
347.578070	6042.701874	8.224768	-0.068530	4.196176
347.869891	6050.631321	8.229773	-0.068590	4.198887
347.995381	6058.627453	8.234778	-0.068618	4.201617
348.284467	6066.612374	8.239782	-0.068677	4.204343
347.996656	6074.719879	8.244787	-0.068629	4.207103
348.391985	6082.672418	8.249792	-0.068708	4.209816
348.815488	6090.733942	8.254797	-0.068792	4.212564
348.996531	6098.756505	8.259802	-0.068831	4.215294
348.962279	6106.785840	8.264806	-0.068830	4.218023
348.845326	6114.843271	8.269811	-0.068814	4.220758
349.270445	6122.727459	8.274816	-0.068898	4.223439
349.418711	6130.855842	8.279821	-0.068931	4.226198
349.323635	6138.800183	8.284826	-0.068918	4.228890
349.650308	6146.877288	8.289830	-0.068985	4.231630
349.591384	6154.911903	8.294835	-0.068979	4.234350
349.625525	6162.929383	8.299840	-0.068990	4.237063
349.984235	6170.880089	8.304845	-0.069062	4.239755
349.959212	6178.952248	8.309850	-0.069063	4.242482
350.151410	6186.924001	8.314854	-0.069104	4.245176
350.323319	6194.951492	8.319859	-0.069141	4.247887
350.393490	6202.981704	8.324864	-0.069160	4.250596
350.850167	6210.966566	8.329869	-0.069250	4.253292
350.855464	6218.991463	8.334874	-0.069256	4.255995
351.130227	6227.011639	8.339878	-0.069313	4.258697
351.353029	6235.057125	8.344883	-0.069360	4.261406
351.177250	6243.020073	8.349888	-0.069332	4.264081
351.574210	6251.105193	8.354893	-0.069411	4.266801
351.558435	6259.094990	8.359898	-0.069414	4.269484
351.403258	6267.137550	8.364902	-0.069390	4.272181
351.722502	6275.143705	8.369907	-0.069455	4.274869
351.870924	6283.130040	8.374912	-0.069488	4.277546
351.962552	6291.190180	8.379917	-0.069510	4.280247
351.875186	6299.110213	8.384922	-0.069499	4.282897
352.116460	6307.192226	8.389926	-0.069549	4.285602
352.119125	6315.228082	8.394931	-0.069555	4.288288
352.351540	6323.221585	8.399936	-0.069603	4.290961
352.807064	6331.236585	8.404941	-0.069693	4.293641
352.674407	6339.281955	8.409946	-0.069674	4.296324
353.093102	6347.272638	8.414950	-0.069757	4.298992
352.954793	6355.308521	8.419955	-0.069737	4.301668
353.113656	6363.275901	8.424960	-0.069772	4.304323
353.328580	6371.349092	8.429965	-0.069817	4.307012
353.463336	6379.355320	8.434970	-0.069847	4.309676
353.606418	6387.377625	8.439974	-0.069879	4.312343
354.002613	6395.337397	8.444979	-0.069958	4.314991
353.867855	6403.354237	8.449984	-0.069938	4.317651
354.046360	6411.428348	8.454989	-0.069977	4.320331
354.440089	6419.351485	8.459994	-0.070055	4.322962
354.661004	6427.396985	8.464998	-0.070102	4.325629
354.885550	6435.438030	8.470003	-0.070149	4.328294
354.954239	6443.465274	8.475008	-0.070167	4.330951
354.991322	6451.487861	8.480013	-0.070179	4.333605
354.851947	6459.521504	8.485018	-0.070158	4.336259
355.176415	6467.487550	8.490022	-0.070224	4.338893
355.558286	6475.534792	8.495027	-0.070301	4.341553
355.527245	6483.485087	8.500032	-0.070300	4.344176
355.662458	6491.600182	8.505037	-0.070330	4.346852
355.868507	6499.544334	8.510042	-0.070374	4.349472
355.679016	6507.674967	8.515046	-0.070344	4.352148
356.117995	6515.671087	8.520051	-0.070431	4.354783
356.112512	6523.662250	8.525056	-0.070435	4.357411
356.346143	6531.637734	8.530061	-0.070484	4.360035
356.449789	6539.632390	8.535066	-0.070509	4.362662
356.818268	6547.613773	8.540070	-0.070583	4.365285
356.775499	6555.681337	8.545075	-0.070580	4.367932
357.250046	6563.710324	8.550080	-0.070673	4.370568
357.526830	6571.721873	8.555085	-0.070730	4.373196
357.553142	6579.745533	8.560090	-0.070740	4.375824
357.695420	6587.750630	8.565095	-0.070772	4.378445
357.825712	6595.797113	8.570099	-0.070802	4.381078
357.985621	6603.735173	8.575104	-0.070837	4.383674
357.959440	6611.853824	8.580109	-0.070837	4.386327
358.488932	6619.775923	8.585114	-0.070941	4.388917
358.519434	6627.889868	8.590119	-0.070952	4.391565
358.856377	6635.816942	8.595123	-0.071020	4.394153
358.647232	6643.978871	8.600128	-0.070986	4.396812
358.947643	6651.901922	8.605133	-0.071048	4.399394
358.907992	6659.954233	8.610138	-0.071045	4.402016
358.945632	6667.967644	8.615143	-0.071058	4.404623
359.321860	6675.980458	8.620147	-0.071133	4.407231
359.540672	6683.960727	8.625152	-0.071179	4.409826
359.941211	6692.079007	8.630157	-0.071259	4.412465
359.759872	6700.051211	8.635162	-0.071230	4.415051
359.655545	6708.116177	8.640167	-0.071216	4.417667
360.018948	6716.163154	8.645171	-0.071289	4.420278
360.379411	6724.099433	8.650176	-0.071362	4.422851
360.610050	6732.106386	8.655181	-0.071410	4.425445
360.786294	6740.152843	8.660186	-0.071448	4.428050
361.171540	6748.239201	8.665191	-0.071525	4.430668
361.281480	6756.239462	8.670195	-0.071551	4.433254
361.411416	6764.290519	8.675200	-0.071580	4.435856
361.283470	6772.344772	8.680205	-0.071562	4.438456
360.991810	6780.354086	8.685210	-0.071513	4.441039
361.320204	6788.231200	8.690215	-0.071579	4.443581
361.447046	6796.342875	8.695219	-0.071608	4.446195
361.791544	6804.296992	8.700224	-0.071677	4.448759
362.395160	6812.313946	8.705229	-0.071795	4.451343
362.410513	6820.317555	8.710234	-0.071803	4.453918
362.815363	6828.371451	8.715239	-0.071884	4.456510
362.921565	6836.369508	8.720243	-0.071909	4.459080
363.261300	6844.352293	8.725248	-0.071977	4.461646
363.202643	6852.437979	8.730253	-0.071972	4.464241
363.313248	6860.465594	8.735258	-0.071997	4.466816
363.302646	6868.451861	8.740263	-0.072001	4.469377
363.808397	6876.502831	8.745267	-0.072100	4.471959
363.838394	6884.439337	8.750272	-0.072111	4.474500
363.970904	6892.510729	8.755277	-0.072141	4.477084
364.108083	6900.460835	8.760282	-0.072172	4.479627
364.459724	6908.507485	8.765287	-0.072242	4.482201
364.685820	6916.495029	8.770291	-0.072290	4.484754
364.719417	6924.585502	8.775296	-0.072301	4.487338
364.949399	6932.615585	8.780301	-0.072349	4.489901
365.326163	6940.580017	8.785306	-0.072425	4.492443
365.523926	6948.578706	8.790311	-0.072467	4.494993
365.832070	6956.642474	8.795315	-0.072530	4.497563
365.545272	6964.677706	8.800320	-0.072481	4.500120
365.510127	6972.707648	8.805325	-0.072480	4.502675
365.705466	6980.612874	8.810330	-0.072522	4.505190
365.669804	6988.730506	8.815335	-0.072520	4.507770
365.794207	6996.737986	8.820339	-0.072549	4.510314
365.922199	7004.715578	8.825344	-0.072578	4.512847
366.062328	7012.735968	8.830349	-0.072609	4.515393
366.226101	7020.692754	8.835354	-0.072645	4.517917
366.475801	7028.695561	8.840359	-0.072697	4.520454
366.808523	7036.735668	8.845363	-0.072764	4.523002
367.168452	7044.720012	8.850368	-0.072836	4.525531
367.273391	7052.794306	8.855373	-0.072861	4.528086
367.253543	7060.810183	8.860378	-0.072863	4.530620
367.525894	7068.830845	8.865383	-0.072919	4.533156
367.413458	7076.914917	8.870387	-0.072903	4.535709
367.560733	7084.817243	8.875392	-0.072936	4.538204
367.959628	7092.881185	8.880397	-0.073015	4.540750
368.152758	7100.796053	8.885402	-0.073056	4.543246
368.073494	7108.938547	8.890407	-0.073047	4.545812
368.603845	7116.892391	8.895411	-0.073151	4.548319
368.439776	7124.990151	8.900416	-0.073126	4.550868
368.384978	7133.043924	8.905421	-0.073121	4.553401
368.711224	7140.988131	8.910426	-0.073187	4.555900
369.064335	7148.906833	8.915431	-0.073258	4.558390
369.384668	7157.006214	8.920435	-0.073323	4.560934
369.103261	7164.953185	8.925440	-0.073276	4.563429
369.704775	7173.023989	8.930445	-0.073393	4.565962
369.992426	7180.999948	8.935450	-0.073452	4.568464
370.016931	7189.075698	8.940455	-0.073462	4.570995
369.843163	7197.100304	8.945459	-0.073434	4.573508
370.211333	7205.110153	8.950464	-0.073508	4.576016
370.275280	7213.077351	8.955469	-0.073525	4.578509
370.459847	7221.141143	8.960474	-0.073565	4.581031
370.416509	7229.101740	8.965479	-0.073562	4.583519
370.487792	7237.211037	8.970483	-0.073581	4.586052
370.157938	7245.174752	8.975488	-0.073525	4.588538
370.216151	7253.297991	8.980493	-0.073541	4.591073
370.607342	7261.182935	8.985498	-0.073619	4.593532
370.811858	7269.265429	8.990503	-0.073662	4.596052
370.695588	7277.247486	8.995507	-0.073646	4.598538
371.163290	7285.218527	9.000512	-0.073738	4.601020
371.737357	7293.174606	9.005517	-0.073850	4.603497
371.948389	7301.214784	9.010522	-0.073895	4.605997
371.896778	7309.293440	9.015527	-0.073891	4.608508
371.954695	7317.359062	9.020531	-0.073907	4.611014
372.153561	7325.259724	9.025536	-0.073949	4.613467
372.415223	7333.347658	9.030541	-0.074003	4.615978
372.453378	7341.303728	9.035546	-0.074015	4.618445
372.606618	7349.380671	9.040551	-0.074049	4.620949
372.901080	7357.348872	9.045555	-0.074109	4.623418
373.186524	7365.363830	9.050560	-0.074168	4.625900
373.260690	7373.427974	9.055565	-0.074187	4.628396
373.364485	7381.402569	9.060570	-0.074211	4.630862
373.401666	7389.457313	9.065575	-0.074223	4.633352
373.685560	7397.495920	9.070579	-0.074282	4.635836
373.758739	7405.445109	9.075584	-0.074300	4.638291
373.682706	7413.502870	9.080589	-0.074292	4.640778
373.953376	7421.419979	9.085594	-0.074347	4.643220
374.001734	7429.529840	9.090599	-0.074361	4.645721
374.204078	7437.551853	9.095603	-0.074404	4.648193
374.290393	7445.557939	9.100608	-0.074426	4.650659
374.659313	7453.563308	9.105613	-0.074500	4.653123
374.668706	7461.577995	9.110618	-0.074507	4.655589
374.746062	7469.561439	9.115623	-0.074526	4.658043
374.552845	7477.663735	9.120627	-0.074496	4.660533
374.539820	7485.586462	9.125632	-0.074499	4.662967
375.034608	7493.648210	9.130637	-0.074596	4.665442
375.308356	7501.621517	9.135642	-0.074652	4.667888
375.470376	7509.682442	9.140647	-0.074688	4.670360
375.833238	7517.741956	9.145651	-0.074760	4.672830
375.891343	7525.716593	9.150656	-0.074777	4.675273
376.260752	7533.716508	9.155661	-0.074851	4.677723
376.298059	7541.757735	9.160666	-0.074863	4.680183
376.292657	7549.725511	9.165671	-0.074867	4.682620
376.689014	7557.743502	9.170675	-0.074946	4.685071
376.825628	7565.742598	9.175680	-0.074977	4.687515
376.846426	7573.777266	9.180685	-0.074986	4.689969
376.904123	7581.816280	9.185690	-0.075002	4.692422
377.320352	7589.777885	9.190695	-0.075085	4.694851
377.164850	7597.875816	9.195699	-0.075061	4.697320
377.579461	7605.813162	9.200704	-0.075143	4.699738
377.992720	7613.942391	9.205709	-0.075226	4.702213
377.811344	7621.865251	9.210714	-0.075197	4.704626
377.484023	7629.965939	9.215719	-0.075142	4.707091
377.733993	7637.973867	9.220723	-0.075193	4.709526
378.255370	7645.939086	9.225728	-0.075296	4.711946
378.440675	7653.971657	9.230733	-0.075335	4.714386
378.443082	7661.983843	9.235738	-0.075341	4.716818
378.960849	7669.917595	9.240743	-0.075443	4.719225
378.921223	7678.067617	9.245747	-0.075441	4.721697
378.868207	7685.978714	9.250752	-0.075436	4.724095
379.348208	7694.066086	9.255757	-0.075531	4.726545
379.238280	7702.032464	9.260762	-0.075516	4.728957
379.434857	7710.108032	9.265767	-0.075557	4.731401
379.813364	7718.023910	9.270771	-0.075633	4.733795
379.943701	7726.102328	9.275776	-0.075663	4.736238
380.012314	7734.135973	9.280781	-0.075681	4.738665
380.181339	7742.164162	9.285786	-0.075718	4.741090
380.562260	7750.116394	9.290791	-0.075794	4.743490
380.722431	7758.189103	9.295795	-0.075829	4.745925
380.555586	7766.204443	9.300800	-0.075803	4.748343
380.582705	7774.326899	9.305805	-0.075813	4.750791
380.756110	7782.271300	9.310810	-0.075851	4.753184
380.744141	7790.281479	9.315815	-0.075854	4.755596
380.968374	7798.269748	9.320819	-0.075901	4.758000
381.338992	7806.261364	9.325824	-0.075975	4.760403
381.824895	7814.234319	9.330829	-0.076071	4.762799
381.981999	7822.255220	9.335834	-0.076105	4.765209
382.038426	7830.312575	9.340839	-0.076121	4.767628
381.985771	7838.405254	9.345843	-0.076117	4.770058
381.956138	7846.364890	9.350848	-0.076116	4.772446
382.218223	7854.429304	9.355853	-0.076171	4.774864
382.433459	7862.398463	9.360858	-0.076216	4.777252
382.228790	7870.389235	9.365863	-0.076183	4.779647
382.497049	7878.426484	9.370867	-0.076238	4.782052
382.591889	7886.422202	9.375872	-0.076261	4.784445
382.521172	7894.495316	9.380877	-0.076253	4.786860
382.376420	7902.493328	9.385882	-0.076232	4.789252
382.886626	7910.566467	9.390887	-0.076332	4.791663
382.797663	7918.508361	9.395891	-0.076321	4.794035
382.723552	7926.555804	9.400896	-0.076312	4.796438
383.480401	7934.475888	9.405901	-0.076458	4.798799
383.474751	7942.559506	9.410906	-0.076462	4.801209
382.803346	7950.561467	9.415911	-0.076343	4.803597
383.009273	7958.645219	9.420915	-0.076386	4.806005
383.405045	7966.538377	9.425920	-0.076465	4.808354
383.584610	7974.654141	9.430925	-0.076504	4.810769
383.660045	7982.602643	9.435930	-0.076523	4.813133
383.839116	7990.133227	9.440935	-0.076562	4.815371
383.883125	7994.971801	9.445939	-0.076573	4.816809

383.945525	7997.535074	9.450944	-0.076586	4.817571
384.252394	7998.874703	9.455949	-0.076644	4.817968
384.319996	7999.337972	9.460954	-0.076657	4.818105
384.190854	8000.293551	9.465959	-0.076634	4.818389
384.463937	8000.432814	9.470963	-0.076685	4.818430
384.642706	8000.377438	9.475968	-0.076718	4.818413
384.558370	8000.380503	9.480973	-0.076702	4.818414
384.436730	8000.397776	9.485978	-0.076680	4.818419
384.683904	8000.356987	9.490983	-0.076726	4.818406
384.642967	8000.453118	9.495987	-0.076718	4.818435
384.548595	8000.419266	9.500992	-0.076701	4.818425
384.806741	8000.484767	9.505997	-0.076749	4.818444
384.715213	8000.386848	9.511002	-0.076732	4.818415
384.802614	8000.395390	9.516007	-0.076748	4.818417
384.684553	8000.475765	9.521011	-0.076726	4.818442
384.959595	8000.347078	9.526016	-0.076778	4.818402
385.268627	8000.357571	9.531021	-0.076835	4.818404
385.160446	8000.391840	9.536026	-0.076815	4.818415
385.276871	8000.423896	9.541031	-0.076837	4.818424
385.619378	8000.406468	9.546035	-0.076901	4.818417
385.210958	8000.412500	9.551040	-0.076825	4.818421
385.325736	8000.436127	9.556045	-0.076846	4.818427
385.454645	8000.396890	9.561050	-0.076870	4.818415
385.214427	8000.310619	9.566055	-0.076825	4.818390
385.238497	8000.471737	9.571059	-0.076830	4.818438
385.284977	8000.465013	9.576064	-0.076839	4.818436
385.435545	8000.442884	9.581069	-0.076867	4.818429
385.488086	8000.343762	9.586074	-0.076876	4.818399
385.396564	8000.401377	9.591079	-0.076860	4.818417
385.551098	8000.428694	9.596083	-0.076888	4.818424
386.076175	8000.338073	9.601088	-0.076986	4.818395
385.841953	8000.372737	9.606093	-0.076943	4.818406
386.112006	8000.307037	9.611098	-0.076993	4.818386
386.337885	8000.310099	9.616103	-0.077035	4.818386
386.216868	8000.299005	9.621107	-0.077012	4.818383
386.191525	8000.318632	9.626112	-0.077008	4.818389
386.284113	8000.387149	9.631117	-0.077025	4.818409
386.344076	8000.353284	9.636122	-0.077036	4.818398
386.269179	8000.369087	9.641127	-0.077022	4.818403
386.558732	8000.316262	9.646131	-0.077076	4.818387
386.312210	8000.324486	9.651136	-0.077030	4.818390
386.142397	8000.392602	9.656141	-0.076999	4.818411
386.191866	8000.362798	9.661146	-0.077008	4.818402
386.031803	8000.317545	9.666151	-0.076978	4.818389
385.628871	8000.469729	9.671155	-0.076903	4.818436
386.251701	8000.391993	9.676160	-0.077019	4.818410
386.448977	8000.423044	9.681165	-0.077056	4.818419
386.350503	8000.378624	9.686170	-0.077038	4.818406
386.409482	8000.348949	9.691175	-0.077049	4.818397
386.423684	8000.410099	9.696179	-0.077052	4.818415
386.420239	8000.378527	9.701184	-0.077051	4.818406
386.407234	8000.383609	9.706189	-0.077049	4.818407
386.328093	8000.391998	9.711194	-0.077034	4.818410
386.794413	8000.359435	9.716199	-0.077121	4.818398
386.794480	8000.364693	9.721203	-0.077121	4.818400
386.780166	8000.377114	9.726208	-0.077118	4.818404
386.625631	8000.413908	9.731213	-0.077090	4.818415
386.631279	8000.366695	9.736218	-0.077091	4.818401
386.480904	8000.375170	9.741223	-0.077063	4.818404
386.660348	8000.396522	9.746227	-0.077096	4.818410
386.531332	8000.365350	9.751232	-0.077072	4.818401
386.416996	8000.421606	9.756237	-0.077051	4.818418
386.352118	8000.441749	9.761242	-0.077039	4.818425
386.687402	8000.369576	9.766247	-0.077101	4.818402
386.610167	8000.387450	9.771251	-0.077087	4.818408
386.586818	8000.398697	9.776256	-0.077083	4.818411
386.644048	8000.471991	9.781261	-0.077093	4.818433
386.785287	8000.353049	9.786266	-0.077120	4.818397
386.736424	8000.393377	9.791271	-0.077111	4.818409
386.678756	8000.382089	9.796275	-0.077100	4.818406
386.559253	8000.395186	9.801280	-0.077078	4.818410
386.748206	8000.416666	9.806285	-0.077113	4.818416
386.371539	8000.459909	9.811290	-0.077043	4.818430
386.832788	8000.424124	9.816295	-0.077129	4.818418
386.383770	8000.487405	9.821299	-0.077045	4.818438
386.357592	8000.438711	9.826304	-0.077040	4.818424
386.773277	8000.389697	9.831309	-0.077118	4.818408
386.630479	8000.441363	9.836314	-0.077091	4.818423
386.851137	8000.386554	9.841319	-0.077132	4.818406
386.781123	8000.377201	9.846323	-0.077119	4.818404
386.975829	8000.356722	9.851328	-0.077156	4.818397
387.073295	8000.386421	9.856333	-0.077174	4.818405
387.222188	8000.341149	9.861338	-0.077202	4.818391
387.406254	8000.374125	9.866343	-0.077236	4.818400
387.180825	8000.381582	9.871347	-0.077194	4.818403
387.245016	8000.337264	9.876352	-0.077206	4.818390
387.374380	8000.392620	9.881357	-0.077230	4.818406
387.085083	8000.354020	9.886362	-0.077176	4.818396
387.046444	8000.385028	9.891367	-0.077169	4.818405
387.285707	8000.358847	9.896371	-0.077214	4.818396
387.066737	8000.362188	9.901376	-0.077173	4.818398
386.983619	8000.398899	9.906381	-0.077158	4.818409
387.234332	8000.335039	9.911386	-0.077204	4.818389
387.280472	8000.275763	9.916391	-0.077213	4.818372
387.288704	8000.380973	9.921395	-0.077215	4.818403
386.854278	8000.384548	9.926400	-0.077134	4.818406
387.030537	8000.410060	9.931405	-0.077167	4.818413
387.022206	8000.412052	9.936410	-0.077165	4.818413
386.942877	8000.406777	9.941415	-0.077150	4.818412
387.185036	8000.428979	9.946419	-0.077196	4.818418
387.417205	8000.356460	9.951424	-0.077239	4.818395
387.496950	8000.396429	9.956429	-0.077254	4.818407
387.480103	8000.354166	9.961434	-0.077251	4.818394
387.206219	8000.403004	9.966439	-0.077200	4.818410
387.334665	8000.443634	9.971443	-0.077224	4.818421
387.274369	8000.359794	9.976448	-0.077212	4.818397
387.702164	8000.368749	9.981453	-0.077292	4.818398
387.653990	8000.354436	9.986458	-0.077283	4.818393
387.287158	8000.402015	9.991463	-0.077215	4.818409
387.287898	8000.387315	9.996467	-0.077215	4.818405
387.569348	8000.329126	10.001472	-0.077268	4.818386
387.324184	8000.390966	10.006477	-0.077222	4.818406
387.499442	8000.380733	10.011482	-0.077255	4.818402
387.362160	8000.368365	10.016487	-0.077229	4.818399
387.451977	8000.405319	10.021491	-0.077246	4.818409
387.597914	8000.366312	10.026496	-0.077273	4.818397
387.590154	8000.392485	10.031501	-0.077272	4.818405
387.518464	8000.397822	10.036506	-0.077258	4.818407
387.616435	8000.365522	10.041511	-0.077277	4.818397
387.773419	8000.373959	10.046515	-0.077306	4.818399
387.527936	8000.354870	10.051520	-0.077260	4.818394
387.495653	8000.471093	10.056525	-0.077254	4.818429
387.471372	8000.411912	10.061530	-0.077250	4.818411
387.447680	8000.386371	10.066535	-0.077245	4.818404
387.727904	8000.409090	10.071539	-0.077298	4.818409
387.710273	8000.351051	10.076544	-0.077294	4.818392
387.647927	8000.403808	10.081549	-0.077283	4.818408
387.245810	8000.427788	10.086554	-0.077208	4.818417
387.530464	8000.374897	10.091559	-0.077261	4.818400
387.346104	8000.317751	10.096563	-0.077227	4.818384
387.466128	8000.384541	10.101568	-0.077249	4.818403
387.559082	8000.385804	10.106573	-0.077267	4.818403
387.838912	8000.333899	10.111578	-0.077319	4.818387
387.727936	8000.380742	10.116583	-0.077298	4.818401
388.072402	8000.402231	10.121587	-0.077362	4.818406
387.853408	8000.375093	10.126592	-0.077322	4.818399
387.811677	8000.406059	10.131597	-0.077314	4.818408
387.776577	8000.413994	10.136602	-0.077307	4.818411
387.428579	8000.417688	10.141607	-0.077243	4.818413
387.581927	8000.454451	10.146611	-0.077271	4.818423
387.674685	8000.422081	10.151616	-0.077288	4.818413
387.480106	8000.455179	10.156621	-0.077252	4.818424
387.913878	8000.410617	10.161626	-0.077333	4.818409
387.416935	8000.498470	10.166631	-0.077241	4.818437
387.720351	8000.399591	10.171635	-0.077297	4.818407
387.303895	8000.448599	10.176640	-0.077220	4.818423
387.825000	8000.407322	10.181645	-0.077317	4.818408
387.954031	8000.340761	10.186650	-0.077341	4.818388
387.656174	8000.397683	10.191655	-0.077285	4.818406
387.908253	8000.392695	10.196659	-0.077332	4.818404
387.770942	8000.381378	10.201664	-0.077307	4.818401
387.237183	8000.493956	10.206669	-0.077208	4.818437
387.285173	8000.459928	10.211674	-0.077216	4.818426
387.645159	8000.411211	10.216679	-0.077284	4.818410
387.943666	8000.397395	10.221683	-0.077339	4.818405
388.042225	8000.369307	10.226688	-0.077358	4.818396
388.118809	8000.369298	10.231693	-0.077372	4.818396
387.972453	8000.367316	10.236698	-0.077345	4.818396
387.951761	8000.360733	10.241703	-0.077341	4.818394
387.876760	8000.383892	10.246707	-0.077327	4.818401
387.815652	8000.374658	10.251712	-0.077316	4.818399
388.014864	8000.414147	10.256717	-0.077353	4.818410
388.063784	8000.331786	10.261722	-0.077362	4.818385
387.703476	8000.394166	10.266727	-0.077295	4.818405
387.876295	8000.407022	10.271731	-0.077327	4.818408
387.762790	8000.405487	10.276736	-0.077306	4.818408
387.932104	8000.446671	10.281741	-0.077338	4.818420
388.107451	8000.366025	10.286746	-0.077370	4.818395
388.083442	8000.423506	10.291751	-0.077366	4.818412
388.284719	8000.389454	10.296755	-0.077403	4.818401
388.032545	8000.373426	10.301760	-0.077356	4.818398
388.286639	8000.391588	10.306765	-0.077404	4.818402
388.208209	8000.346387	10.311770	-0.077389	4.818389
388.139707	8000.353869	10.316775	-0.077376	4.818391
388.471690	8000.334201	10.321779	-0.077438	4.818384
388.129192	8000.375803	10.326784	-0.077375	4.818398
388.055517	8000.416846	10.331789	-0.077361	4.818410
388.091481	8000.360584	10.336794	-0.077368	4.818393
387.981727	8000.425311	10.341799	-0.077347	4.818413
387.889576	8000.482919	10.346803	-0.077330	4.818431
388.103785	8000.414360	10.351808	-0.077370	4.818409
388.335232	8000.413298	10.356813	-0.077413	4.818408
388.057755	8000.463139	10.361818	-0.077362	4.818424
388.087050	8000.396276	10.366823	-0.077367	4.818404
388.255321	8000.398561	10.371827	-0.077398	4.818404
388.268204	8000.357750	10.376832	-0.077401	4.818392
388.338294	8000.401794	10.381837	-0.077414	4.818405
388.396628	8000.346886	10.386842	-0.077425	4.818388
388.434055	8000.336887	10.391847	-0.077432	4.818385
388.521281	8000.365399	10.396851	-0.077448	4.818393
388.324658	8000.376398	10.401856	-0.077412	4.818397
388.142187	8000.370774	10.406861	-0.077378	4.818396
387.872677	8000.464864	10.411866	-0.077328	4.818425
387.587461	8000.465204	10.416871	-0.077275	4.818427
387.899825	8000.489411	10.421875	-0.077333	4.818433
387.663971	8000.466247	10.426880	-0.077289	4.818427
387.794507	8000.411267	10.431885	-0.077313	4.818410
388.015989	8000.427936	10.436890	-0.077354	4.818414
388.288796	8000.406415	10.441895	-0.077405	4.818406
388.176895	8000.433277	10.446899	-0.077385	4.818415
388.043524	8000.404146	10.451904	-0.077360	4.818407
388.226488	8000.407682	10.456909	-0.077394	4.818407
388.092472	8000.435295	10.461914	-0.077369	4.818416
388.147563	8000.416076	10.466919	-0.077379	4.818410
388.024367	8000.496386	10.471923	-0.077356	4.818434
388.217179	8000.418078	10.476928	-0.077392	4.818410
388.259575	8000.328271	10.481933	-0.077400	4.818383
388.295279	8000.413888	10.486938	-0.077407	4.818408
388.338784	8000.396614	10.491943	-0.077415	4.818403
388.203410	8000.423158	10.496947	-0.077390	4.818412
388.386104	8000.368886	10.501952	-0.077424	4.818395
388.492069	8000.388193	10.506957	-0.077444	4.818400
388.355934	8000.407369	10.511962	-0.077418	4.818406
388.271669	8000.405179	10.516967	-0.077403	4.818406
388.324059	8000.401688	10.521971	-0.077413	4.818405
388.180019	8000.396585	10.526976	-0.077386	4.818404
388.543921	8000.374197	10.531981	-0.077454	4.818396
388.634889	8000.321834	10.536986	-0.077470	4.818380
388.611503	8000.336234	10.541991	-0.077466	4.818384
388.988928	8000.357121	10.546995	-0.077537	4.818389
388.512395	8000.347508	10.552000	-0.077448	4.818388
388.684821	8000.353002	10.557005	-0.077480	4.818389
388.462708	8000.378370	10.562010	-0.077439	4.818397
388.688300	8000.350953	10.567015	-0.077481	4.818388
388.395679	8000.416353	10.572019	-0.077426	4.818409
388.607092	8000.345654	10.577024	-0.077466	4.818387
388.639032	8000.376569	10.582029	-0.077472	4.818396
388.605632	8000.347743	10.587034	-0.077465	4.818388
388.396417	8000.385897	10.592039	-0.077427	4.818400
388.587713	8000.426330	10.597043	-0.077462	4.818411
388.417562	8000.344151	10.602048	-0.077431	4.818387
388.648018	8000.364095	10.607053	-0.077474	4.818392
388.625128	8000.408980	10.612058	-0.077469	4.818406
388.522901	8000.373965	10.617063	-0.077450	4.818396
388.544115	8000.355338	10.622067	-0.077454	4.818390
388.574660	8000.335787	10.627072	-0.077460	4.818384
388.600937	8000.375033	10.632077	-0.077465	4.818396
388.610917	8000.362559	10.637082	-0.077467	4.818392
388.585033	8000.349599	10.642087	-0.077462	4.818388
388.756328	8000.341416	10.647091	-0.077494	4.818385
388.543376	8000.361653	10.652096	-0.077454	4.818392
388.607547	8000.420331	10.657101	-0.077466	4.818409
388.630084	8000.368090	10.662106	-0.077471	4.818393
388.924879	8000.352122	10.667111	-0.077526	4.818388
389.005207	8000.367929	10.672115	-0.077541	4.818392
388.860907	8000.332343	10.677120	-0.077514	4.818382
388.997819	8000.372039	10.682125	-0.077539	4.818393
388.828736	8000.321403	10.687130	-0.077508	4.818379
388.884707	8000.372613	10.692135	-0.077518	4.818394
388.962360	8000.344241	10.697139	-0.077533	4.818385
388.896831	8000.355968	10.702144	-0.077521	4.818389
388.903887	8000.332944	10.707149	-0.077522	4.818382
389.090779	8000.314463	10.712154	-0.077557	4.818376
389.046815	8000.354858	10.717159	-0.077549	4.818388
388.945902	8000.393431	10.722163	-0.077530	4.818400
389.194046	8000.360015	10.727168	-0.077576	4.818389
389.110333	8000.394617	10.732173	-0.077561	4.818399
388.873572	8000.346215	10.737178	-0.077517	4.818386
388.904776	8000.407599	10.742183	-0.077523	4.818404
388.959966	8000.412555	10.747187	-0.077533	4.818405
389.092310	8000.312406	10.752192	-0.077557	4.818375
388.961107	8000.367384	10.757197	-0.077533	4.818392
388.913708	8000.348877	10.762202	-0.077524	4.818387
389.053801	8000.340270	10.767207	-0.077550	4.818384
389.018508	8000.313520	10.772211	-0.077544	4.818376
389.124591	8000.313911	10.777216	-0.077564	4.818375
389.210154	8000.316125	10.782221	-0.077580	4.818376
389.049954	8000.302394	10.787226	-0.077550	4.818372
388.972409	8000.333927	10.792231	-0.077536	4.818382
389.115033	8000.335864	10.797235	-0.077562	4.818382
388.851757	8000.355418	10.802240	-0.077513	4.818389
388.966322	8000.334904	10.807245	-0.077534	4.818382
389.069049	8000.343658	10.812250	-0.077554	4.818384
389.132734	8000.361341	10.817255	-0.077566	4.818389
388.847517	8000.392158	10.822259	-0.077513	4.818400
388.993939	8000.319526	10.827264	-0.077540	4.818378
389.209142	8000.356081	10.832269	-0.077580	4.818388
388.811885	8000.339134	10.837274	-0.077506	4.818384
388.860862	8000.337700	10.842279	-0.077515	4.818384
389.259839	8000.331554	10.847283	-0.077589	4.818380
389.030588	8000.337906	10.852288	-0.077547	4.818383
389.084338	8000.364913	10.857293	-0.077557	4.818391
389.064570	8000.356240	10.862298	-0.077553	4.818388
389.101559	8000.344133	10.867303	-0.077560	4.818384
389.186781	8000.338986	10.872307	-0.077576	4.818383
389.130466	8000.307746	10.877312	-0.077566	4.818374
389.399715	8000.352391	10.882317	-0.077616	4.818386
389.128166	8000.340302	10.887322	-0.077565	4.818383
389.110157	8000.345316	10.892327	-0.077562	4.818385
389.233710	8000.354352	10.897331	-0.077585	4.818387
389.198750	8000.329708	10.902336	-0.077579	4.818380
388.989151	8000.395183	10.907341	-0.077540	4.818400
388.930574	8000.336587	10.912346	-0.077529	4.818383
388.728216	8000.391650	10.917351	-0.077491	4.818400
388.918418	8000.393182	10.922355	-0.077527	4.818400
388.803639	8000.359047	10.927360	-0.077505	4.818390
388.979247	8000.390860	10.932365	-0.077538	4.818399
389.080679	8000.350199	10.937370	-0.077557	4.818386
389.066888	8000.362627	10.942375	-0.077554	4.818390
389.284326	8000.337203	10.947379	-0.077595	4.818382
389.277614	8000.310840	10.952384	-0.077594	4.818374
389.064896	8000.361559	10.957389	-0.077554	4.818390
388.985039	8000.357325	10.962394	-0.077539	4.818389
389.323584	8000.364023	10.967399	-0.077602	4.818389
389.325863	8000.358802	10.972403	-0.077603	4.818388
388.964569	8000.328680	10.977408	-0.077536	4.818380
389.145154	8000.345847	10.982413	-0.077569	4.818385
389.181634	8000.329529	10.987418	-0.077576	4.818380
389.104621	8000.381037	10.992423	-0.077562	4.818395
388.974523	8000.397143	10.997427	-0.077538	4.818401
389.157955	8000.349186	11.002432	-0.077572	4.818386
389.156257	8000.372288	11.007437	-0.077572	4.818393
389.212653	8000.324710	11.012442	-0.077582	4.818378
389.300361	8000.350076	11.017447	-0.077598	4.818385
389.315345	8000.390221	11.022451	-0.077601	4.818397
389.144293	8000.340608	11.027456	-0.077570	4.818383
389.242694	8000.365068	11.032461	-0.077588	4.818390
389.289486	8000.321564	11.037466	-0.077597	4.818377
389.275154	8000.339240	11.042471	-0.077594	4.818382
389.409417	8000.334758	11.047475	-0.077619	4.818380
389.466054	8000.330275	11.052480	-0.077630	4.818379
389.526391	8000.354219	11.057485	-0.077641	4.818386
389.477748	8000.324133	11.062490	-0.077632	4.818377
389.522425	8000.331049	11.067495	-0.077640	4.818379
389.388583	8000.369174	11.072499	-0.077615	4.818391
389.302144	8000.321760	11.077504	-0.077599	4.818377
389.354271	8000.370817	11.082509	-0.077609	4.818391
389.365908	8000.334193	11.087514	-0.077611	4.818380
389.392596	8000.346119	11.092519	-0.077616	4.818384
389.517233	8000.344660	11.097523	-0.077640	4.818383
389.559682	8000.329474	11.102528	-0.077647	4.818378
389.405986	8000.366279	11.107533	-0.077619	4.818390
389.523189	8000.333189	11.112538	-0.077641	4.818379
389.347274	8000.363387	11.117543	-0.077608	4.818389
389.533021	8000.350145	11.122547	-0.077643	4.818384
389.413594	8000.326456	11.127552	-0.077620	4.818378
389.458670	8000.369112	11.132557	-0.077629	4.818390
389.623343	8000.336666	11.137562	-0.077660	4.818380
389.541525	8000.338712	11.142567	-0.077644	4.818381
389.398079	8000.366197	11.147571	-0.077618	4.818390
389.484113	8000.353704	11.152576	-0.077634	4.818386
389.481279	8000.349465	11.157581	-0.077633	4.818384
389.392628	8000.343010	11.162586	-0.077617	4.818383
389.399614	8000.339955	11.167591	-0.077618	4.818382
389.629811	8000.344132	11.172595	-0.077661	4.818382
389.360273	8000.334172	11.177600	-0.077611	4.818380
389.531528	8000.359621	11.182605	-0.077643	4.818387
389.606460	8000.322804	11.187610	-0.077657	4.818376
389.371646	8000.346948	11.192615	-0.077613	4.818384
389.257241	8000.377980	11.197619	-0.077592	4.818394
389.358214	8000.356231	11.202624	-0.077611	4.818387
389.658445	8000.388685	11.207629	-0.077667	4.818395
389.222232	8000.363851	11.212634	-0.077586	4.818390
389.250223	8000.392611	11.217639	-0.077591	4.818398
389.628300	8000.407204	11.222643	-0.077661	4.818401
389.359850	8000.340503	11.227648	-0.077611	4.818382
389.235883	8000.364049	11.232653	-0.077588	4.818390
389.459829	8000.350274	11.237658	-0.077630	4.818385
389.455866	8000.361785	11.242663	-0.077629	4.818388
389.478863	8000.365253	11.247667	-0.077634	4.818389
389.489492	8000.369604	11.252672	-0.077636	4.818390
389.410336	8000.382196	11.257677	-0.077621	4.818394
389.299722	8000.355474	11.262682	-0.077600	4.818387
389.383680	8000.352413	11.267687	-0.077616	4.818386
389.513661	8000.403577	11.272691	-0.077640	4.818400
389.425317	8000.346678	11.277696	-0.077624	4.818384
389.562479	8000.374817	11.282701	-0.077650	4.818392
389.544035	8000.369315	11.287706	-0.077646	4.818390
389.606421	8000.369114	11.292711	-0.077658	4.818390
389.555602	8000.354764	11.297715	-0.077648	4.818386
389.557426	8000.329567	11.302720	-0.077649	4.818378
389.571629	8000.398079	11.307725	-0.077652	4.818398
389.473620	8000.377834	11.312730	-0.077633	4.818393
389.428124	8000.391934	11.317735	-0.077625	4.818397
389.309527	8000.422909	11.322739	-0.077603	4.818407
389.233114	8000.363019	11.327744	-0.077589	4.818389
389.254324	8000.397993	11.332749	-0.077593	4.818400
389.440505	8000.380553	11.337754	-0.077627	4.818394
389.158856	8000.379888	11.342759	-0.077575	4.818395
389.235806	8000.410364	11.347763	-0.077589	4.818403
389.043795	8000.398303	11.352768	-0.077554	4.818401
389.350491	8000.395110	11.357773	-0.077611	4.818398
389.517445	8000.339572	11.362778	-0.077642	4.818381
389.299035	8000.384959	11.367783	-0.077601	4.818396
389.406963	8000.374865	11.372787	-0.077621	4.818392
389.447599	8000.338634	11.377792	-0.077629	4.818381
389.289673	8000.431085	11.382797	-0.077600	4.818409
389.605820	8000.384930	11.387802	-0.077659	4.818394
389.366652	8000.380636	11.392807	-0.077614	4.818394
389.213914	8000.427965	11.397811	-0.077586	4.818409
389.150449	8000.426056	11.402816	-0.077574	4.818408
388.703061	8000.457825	11.407821	-0.077491	4.818420
388.758019	8000.349270	11.412826	-0.077501	4.818387
388.565117	8000.382391	11.417831	-0.077465	4.818398
389.188773	8000.405568	11.422835	-0.077581	4.818402
388.769445	8000.436667	11.427840	-0.077503	4.818413
388.776717	8000.442024	11.432845	-0.077505	4.818415
388.990083	8000.427055	11.437850	-0.077544	4.818409
389.213526	8000.377539	11.442855	-0.077586	4.818394
389.177497	8000.433808	11.447859	-0.077579	4.818411
389.263329	8000.374017	11.452864	-0.077595	4.818393
389.638074	8000.367543	11.457869	-0.077665	4.818389
389.485935	8000.348666	11.462874	-0.077637	4.818384
389.254528	8000.349733	11.467879	-0.077594	4.818385
389.638002	8000.371756	11.472883	-0.077665	4.818390
389.434645	8000.375306	11.477888	-0.077627	4.818392
389.760631	8000.392345	11.482893	-0.077688	4.818396
389.545641	8000.366308	11.487898	-0.077648	4.818389
389.785810	8000.350652	11.492903	-0.077693	4.818384
389.845712	8000.356723	11.497907	-0.077704	4.818385
389.612203	8000.314670	11.502912	-0.077661	4.818374
389.711361	8000.354906	11.507917	-0.077679	4.818385
389.688759	8000.332531	11.512922	-0.077675	4.818379
389.444731	8000.361804	11.517927	-0.077630	4.818388
389.723046	8000.383451	11.522931	-0.077682	4.818393
389.682932	8000.349277	11.527936	-0.077674	4.818384
389.692886	8000.396711	11.532941	-0.077676	4.818398
389.600542	8000.359727	11.537946	-0.077659	4.818387
389.349372	8000.371036	11.542951	-0.077612	4.818391
389.265009	8000.411935	11.547955	-0.077596	4.818404
389.359370	8000.340699	11.552960	-0.077614	4.818382
389.615661	8000.374659	11.557965	-0.077662	4.818391
389.692335	8000.364141	11.562970	-0.077676	4.818388
389.554032	8000.359114	11.567975	-0.077650	4.818387
389.591966	8000.361734	11.572979	-0.077658	4.818388
389.788240	8000.342329	11.577984	-0.077694	4.818381
389.758201	8000.378710	11.582989	-0.077689	4.818392
389.534621	8000.389343	11.587994	-0.077647	4.818396
389.586413	8000.339600	11.592999	-0.077657	4.818381
389.778635	8000.392660	11.598003	-0.077693	4.818396
389.699363	8000.355853	11.603008	-0.077678	4.818385
389.737267	8000.366881	11.608013	-0.077685	4.818389
389.769021	8000.353651	11.613018	-0.077691	4.818384
389.684557	8000.355661	11.618023	-0.077675	4.818385
389.859588	8000.372754	11.623027	-0.077708	4.818390
389.831260	8000.354505	11.628032	-0.077703	4.818384
389.663049	8000.369042	11.633037	-0.077671	4.818389
389.533849	8000.368343	11.638042	-0.077647	4.818390
389.712277	8000.372869	11.643047	-0.077681	4.818390
389.820324	8000.365931	11.648051	-0.077701	4.818388
389.725422	8000.356238	11.653056	-0.077683	4.818385
389.735060	8000.381596	11.658061	-0.077685	4.818393
389.967658	8000.358480	11.663066	-0.077728	4.818385
389.605285	8000.359872	11.668071	-0.077661	4.818387
389.537949	8000.393645	11.673075	-0.077648	4.818397
389.681367	8000.340941	11.678080	-0.077675	4.818381
389.945964	8000.337178	11.683085	-0.077724	4.818379
389.801816	8000.333123	11.688090	-0.077698	4.818378
389.937210	8000.342320	11.693095	-0.077723	4.818380
389.977283	8000.392265	11.698099	-0.077730	4.818395
389.747805	8000.343960	11.703104	-0.077688	4.818382
389.743292	8000.362820	11.708109	-0.077687	4.818387
389.693175	8000.387368	11.713114	-0.077678	4.818395
389.793730	8000.395042	11.718119	-0.077696	4.818397
389.967051	8000.406856	11.723123	-0.077729	4.818399
389.934372	8000.351763	11.728128	-0.077723	4.818383
389.850416	8000.388463	11.733133	-0.077707	4.818394
389.804048	8000.352102	11.738138	-0.077698	4.818384
389.860203	8000.350765	11.743143	-0.077709	4.818383
389.994463	8000.354693	11.748147	-0.077734	4.818384
389.706271	8000.344479	11.753152	-0.077680	4.818382
389.645263	8000.359419	11.758157	-0.077669	4.818387
389.860408	8000.360240	11.763162	-0.077709	4.818386
389.932363	8000.350709	11.768167	-0.077723	4.818383
389.801509	8000.365753	11.773171	-0.077698	4.818388
389.745860	8000.331368	11.778176	-0.077688	4.818378
389.869747	8000.349869	11.783181	-0.077711	4.818383
389.802910	8000.338455	11.788186	-0.077699	4.818380
389.934400	8000.340242	11.793191	-0.077723	4.818380
389.813584	8000.361728	11.798195	-0.077701	4.818387
389.791775	8000.337262	11.803200	-0.077697	4.818379
389.820600	8000.359727	11.808205	-0.077702	4.818386
389.815602	8000.337591	11.813210	-0.077701	4.818379
389.826458	8000.329334	11.818215	-0.077703	4.818377
389.841848	8000.357923	11.823219	-0.077706	4.818385
389.868294	8000.334112	11.828224	-0.077711	4.818378
389.927976	8000.358047	11.833229	-0.077722	4.818385
389.895662	8000.340795	11.838234	-0.077716	4.818380
389.942058	8000.350887	11.843239	-0.077725	4.818383
390.004413	8000.344379	11.848243	-0.077737	4.818381
389.935833	8000.344503	11.853248	-0.077724	4.818381
389.680910	8000.365220	11.858253	-0.077677	4.818388
389.801172	8000.356345	11.863258	-0.077699	4.818385
389.979411	8000.377685	11.868263	-0.077732	4.818391
389.783759	8000.380288	11.873267	-0.077696	4.818392
389.861195	8000.331944	11.878272	-0.077710	4.818378
389.952343	8000.355256	11.883277	-0.077727	4.818384
389.812342	8000.363869	11.888282	-0.077701	4.818387
389.907878	8000.360965	11.893287	-0.077719	4.818386
389.859323	8000.418115	11.898291	-0.077710	4.818403
389.626196	8000.364505	11.903296	-0.077667	4.818388
389.875251	8000.362633	11.908301	-0.077713	4.818387
389.872095	8000.345777	11.913306	-0.077713	4.818382
389.988346	8000.345256	11.918311	-0.077734	4.818381
389.996999	8000.367448	11.923315	-0.077736	4.818388
389.892763	8000.345016	11.928320	-0.077717	4.818381
390.048267	8000.379711	11.933325	-0.077746	4.818391
389.858984	8000.359278	11.938330	-0.077710	4.818386
389.572381	8000.366953	11.943335	-0.077657	4.818389
389.742388	8000.374518	11.948339	-0.077689	4.818391
389.692931	8000.367544	11.953344	-0.077680	4.818389
389.767186	8000.382218	11.958349	-0.077693	4.818393
389.494544	8000.495185	11.963354	-0.077643	4.818428
389.387686	8000.428574	11.968359	-0.077623	4.818408
389.783469	8000.466530	11.973363	-0.077697	4.818418
389.450311	8000.376880	11.978368	-0.077635	4.818393
389.895437	8000.389229	11.983373	-0.077718	4.818394
390.042909	8000.346040	11.988378	-0.077745	4.818381
389.680637	8000.348484	11.993383	-0.077678	4.818383
389.995422	8000.369575	11.998387	-0.077736	4.818388
390.115762	8000.353344	12.003392	-0.077759	4.818383
390.019754	8000.367810	12.008397	-0.077741	4.818388
389.939240	8000.386689	12.013402	-0.077726	4.818393
389.907219	8000.368390	12.018407	-0.077720	4.818388
389.913682	8000.372685	12.023411	-0.077721	4.818389
389.929057	8000.338213	12.028416	-0.077724	4.818379
390.106225	8000.358488	12.033421	-0.077757	4.818384
390.140279	8000.338984	12.038426	-0.077764	4.818379
389.993722	8000.342253	12.043431	-0.077736	4.818380
390.080223	8000.383370	12.048435	-0.077752	4.818392
390.020562	8000.342624	12.053440	-0.077741	4.818380
389.889707	8000.350310	12.058445	-0.077717	4.818383
390.154910	8000.338147	12.063450	-0.077766	4.818378
390.026882	8000.354280	12.068455	-0.077743	4.818384
389.998635	8000.365461	12.073459	-0.077738	4.818387
389.729713	8000.351304	12.078464	-0.077687	4.818384
389.615110	8000.386538	12.083469	-0.077666	4.818395
389.725200	8000.364913	12.088474	-0.077687	4.818388
389.652992	8000.360783	12.093479	-0.077673	4.818387
389.815897	8000.369303	12.098483	-0.077704	4.818389
389.815051	8000.373498	12.103488	-0.077704	4.818390
389.658865	8000.395555	12.108493	-0.077675	4.818397
389.622405	8000.432901	12.113498	-0.077668	4.818408
389.535637	8000.382328	12.118503	-0.077652	4.818394
389.925991	8000.377119	12.123507	-0.077724	4.818391
389.798747	8000.363834	12.128512	-0.077701	4.818387
389.970862	8000.382989	12.133517	-0.077733	4.818392
389.884404	8000.378666	12.138522	-0.077717	4.818391
390.006488	8000.350897	12.143527	-0.077740	4.818383
390.188061	8000.384895	12.148531	-0.077773	4.818392
389.980332	8000.432528	12.153536	-0.077735	4.818407
389.955420	8000.396458	12.158541	-0.077730	4.818396
389.716499	8000.403729	12.163546	-0.077686	4.818399
389.198687	8000.458715	12.168551	-0.077589	4.818418
389.189455	8000.418655	12.173555	-0.077588	4.818406
389.225621	8000.462240	12.178560	-0.077595	4.818419
389.319364	8000.440393	12.183565	-0.077612	4.818412
389.543319	8000.453945	12.188570	-0.077654	4.818415
389.735030	8000.406101	12.193575	-0.077689	4.818400
389.787812	8000.455168	12.198579	-0.077699	4.818414
389.447335	8000.450550	12.203584	-0.077636	4.818414
389.743222	8000.421987	12.208589	-0.077691	4.818405
389.713616	8000.446813	12.213594	-0.077686	4.818412
389.971795	8000.383054	12.218599	-0.077734	4.818392
389.804074	8000.392342	12.223603	-0.077703	4.818396
389.838782	8000.343418	12.228608	-0.077709	4.818381
389.862815	8000.395248	12.233613	-0.077714	4.818396
389.944804	8000.393211	12.238618	-0.077729	4.818395
389.581482	8000.366212	12.243623	-0.077661	4.818389
389.871670	8000.423755	12.248627	-0.077715	4.818405
390.066241	8000.389613	12.253632	-0.077752	4.818394
390.139647	8000.369592	12.258637	-0.077765	4.818388
390.022022	8000.362743	12.263642	-0.077743	4.818386
389.775759	8000.379374	12.268647	-0.077698	4.818392
390.042321	8000.442904	12.273651	-0.077747	4.818410
389.725359	8000.449115	12.278656	-0.077688	4.818413
389.986202	8000.440046	12.283661	-0.077737	4.818409
389.860129	8000.421521	12.288666	-0.077714	4.818404
389.874888	8000.405959	12.293671	-0.077716	4.818399
389.423318	8000.532263	12.298675	-0.077632	4.818439
389.594943	8000.422136	12.303680	-0.077664	4.818405
389.681463	8000.338180	12.308685	-0.077680	4.818380
389.793329	8000.489998	12.313690	-0.077701	4.818425
389.650887	8000.417649	12.318695	-0.077675	4.818404
389.588322	8000.435721	12.323699	-0.077663	4.818409
389.717094	8000.420656	12.328704	-0.077687	4.818404
389.657653	8000.421954	12.333709	-0.077676	4.818405
389.879779	8000.396594	12.338714	-0.077718	4.818397
389.846628	8000.386688	12.343719	-0.077712	4.818394
389.525644	8000.479029	12.348723	-0.077652	4.818423
389.610445	8000.437091	12.353728	-0.077668	4.818410
389.793253	8000.395432	12.358733	-0.077702	4.818397
389.263772	8000.520678	12.363738	-0.077603	4.818436
389.736534	8000.369444	12.368743	-0.077691	4.818389
390.001572	8000.411933	12.373747	-0.077741	4.818401
389.776293	8000.376296	12.378752	-0.077699	4.818391
389.756218	8000.425425	12.383757	-0.077695	4.818406
389.735022	8000.390457	12.388762	-0.077691	4.818395
389.584377	8000.393671	12.393767	-0.077663	4.818397
389.724656	8000.414496	12.398771	-0.077689	4.818403
389.921502	8000.381436	12.403776	-0.077726	4.818392
390.016685	8000.352251	12.408781	-0.077744	4.818383
390.251113	8000.390120	12.413786	-0.077787	4.818393
389.633094	8000.392245	12.418791	-0.077672	4.818396
390.010571	8000.443617	12.423795	-0.077743	4.818410
389.594508	8000.440075	12.428800	-0.077665	4.818411
389.507226	8000.498801	12.433805	-0.077649	4.818428
389.006242	8000.461527	12.438810	-0.077556	4.818419
389.457852	8000.500240	12.443815	-0.077640	4.818429
389.035330	8000.321093	12.448819	-0.077561	4.818378
389.709876	8000.408023	12.453824	-0.077687	4.818401
389.325184	8000.416469	12.458829	-0.077615	4.818405
389.520956	8000.503211	12.463834	-0.077652	4.818430
389.064484	8000.405581	12.468839	-0.077567	4.818403
389.237916	8000.415294	12.473843	-0.077599	4.818405
389.617176	8000.436209	12.478848	-0.077670	4.818409
389.599398	8000.480114	12.483853	-0.077667	4.818423
389.698066	8000.473048	12.488858	-0.077685	4.818420
389.540403	8000.445687	12.493863	-0.077656	4.818413
390.018292	8000.423798	12.498867	-0.077745	4.818404
389.591589	8000.346541	12.503872	-0.077665	4.818383
389.741656	8000.452632	12.508877	-0.077693	4.818414
389.835127	8000.456006	12.513882	-0.077711	4.818414
389.759654	8000.411892	12.518887	-0.077697	4.818402
389.985788	8000.506404	12.523891	-0.077739	4.818429
389.702936	8000.467884	12.528896	-0.077686	4.818418
389.773136	8000.465687	12.533901	-0.077699	4.818418
389.594851	8000.431739	12.538906	-0.077666	4.818408
389.557331	8000.464866	12.543911	-0.077659	4.818418
389.815076	8000.465214	12.548915	-0.077707	4.818417
389.689594	8000.442494	12.553920	-0.077684	4.818411
390.028254	8000.431328	12.558925	-0.077747	4.818406
389.950964	8000.419772	12.563930	-0.077733	4.818403
389.824899	8000.413860	12.568935	-0.077709	4.818402
389.963152	8000.414688	12.573939	-0.077735	4.818402
389.908485	8000.399235	12.578944	-0.077725	4.818397
389.956660	8000.439831	12.583949	-0.077734	4.818409
389.880134	8000.374683	12.588954	-0.077720	4.818390
389.670993	8000.413888	12.593959	-0.077681	4.818403
389.698681	8000.492043	12.598963	-0.077686	4.818426
389.303889	8000.474076	12.603968	-0.077613	4.818422
389.537432	8000.473044	12.608973	-0.077656	4.818421
389.903296	8000.406543	12.613978	-0.077724	4.818399
389.797789	8000.403013	12.618983	-0.077705	4.818399
389.749806	8000.453865	12.623987	-0.077696	4.818414
390.045885	8000.400080	12.628992	-0.077751	4.818397
389.820644	8000.435914	12.633997	-0.077709	4.818408
390.035731	8000.393642	12.639002	-0.077749	4.818395
389.774207	8000.421626	12.644007	-0.077701	4.818404
389.786150	8000.439659	12.649011	-0.077703	4.818410
389.888258	8000.385344	12.654016	-0.077722	4.818393
389.879270	8000.410449	12.659021	-0.077720	4.818401
390.133386	8000.362401	12.664026	-0.077768	4.818385
389.943801	8000.368239	12.669031	-0.077732	4.818388
389.955821	8000.424110	12.674035	-0.077735	4.818404
389.567808	8000.408337	12.679040	-0.077662	4.818401
389.744142	8000.442264	12.684045	-0.077695	4.818411
390.146674	8000.430914	12.689050	-0.077770	4.818406
389.898173	8000.383401	12.694055	-0.077724	4.818393
389.880710	8000.449382	12.699059	-0.077721	4.818412
389.849457	8000.391154	12.704064	-0.077715	4.818395
389.953104	8000.391513	12.709069	-0.077734	4.818395
390.065591	8000.410911	12.714074	-0.077755	4.818400
389.889249	8000.390653	12.719079	-0.077723	4.818395
389.522278	8000.478165	12.724083	-0.077654	4.818422
389.600371	8000.473973	12.729088	-0.077669	4.818421
389.666527	8000.496946	12.734093	-0.077681	4.818427
389.840527	8000.426790	12.739098	-0.077714	4.818406
390.111373	8000.344285	12.744103	-0.077764	4.818380
389.944712	8000.425057	12.749107	-0.077733	4.818405
390.063740	8000.357308	12.754112	-0.077755	4.818384
390.019001	8000.401898	12.759117	-0.077747	4.818398
390.071647	8000.370034	12.764122	-0.077757	4.818388
389.917355	8000.390014	12.769127	-0.077728	4.818394
389.898384	8000.452821	12.774131	-0.077725	4.818413
389.972549	8000.343473	12.779136	-0.077739	4.818380
389.650699	8000.473639	12.784141	-0.077679	4.818420
390.145739	8000.379463	12.789146	-0.077771	4.818390
389.681112	8000.448834	12.794151	-0.077685	4.818413
389.553550	8000.503861	12.799155	-0.077661	4.818430
389.235415	8000.493240	12.804160	-0.077602	4.818428
389.730333	8000.411674	12.809165	-0.077694	4.818402
389.824414	8000.427669	12.814170	-0.077711	4.818406
389.841063	8000.403724	12.819175	-0.077715	4.818399
389.655371	8000.420125	12.824179	-0.077680	4.818404
389.931935	8000.388147	12.829184	-0.077732	4.818394
389.825999	8000.424549	12.834189	-0.077712	4.818405
389.790661	8000.395695	12.839194	-0.077705	4.818397
390.010202	8000.368198	12.844199	-0.077746	4.818388
390.139110	8000.426707	12.849203	-0.077770	4.818404
389.916746	8000.381650	12.854208	-0.077729	4.818392
389.797550	8000.411566	12.859213	-0.077707	4.818401
390.091053	8000.390329	12.864218	-0.077761	4.818394
389.751644	8000.402541	12.869223	-0.077698	4.818399
389.405332	8000.440937	12.874227	-0.077634	4.818412
389.637054	8000.518707	12.879232	-0.077677	4.818434
389.341813	8000.411703	12.884237	-0.077622	4.818403
389.635431	8000.499773	12.889242	-0.077677	4.818428
389.722136	8000.437891	12.894247	-0.077693	4.818409
390.055047	8000.429801	12.899251	-0.077755	4.818406
389.859396	8000.372495	12.904256	-0.077719	4.818389
389.870805	8000.415745	12.909261	-0.077721	4.818402
390.059703	8000.385730	12.914266	-0.077756	4.818393
390.016664	8000.378843	12.919271	-0.077748	4.818391
389.910426	8000.426802	12.924275	-0.077728	4.818405
389.189314	8000.489539	12.929280	-0.077594	4.818427
389.398351	8000.476614	12.934285	-0.077633	4.818422
389.267821	8000.406529	12.939290	-0.077609	4.818402
389.482941	8000.429421	12.944295	-0.077649	4.818408
389.697241	8000.499598	12.949299	-0.077689	4.818428
389.717253	8000.412638	12.954304	-0.077693	4.818402
389.637508	8000.458855	12.959309	-0.077678	4.818416
390.067404	8000.428958	12.964314	-0.077758	4.818405
389.944587	8000.415733	12.969319	-0.077735	4.818402
389.656188	8000.375036	12.974323	-0.077681	4.818391
389.352422	8000.510702	12.979328	-0.077625	4.818433
389.086999	8000.417767	12.984333	-0.077576	4.818406
389.580999	8000.396096	12.989338	-0.077668	4.818398
389.286358	8000.484590	12.994343	-0.077613	4.818425
389.817278	8000.483391	12.999347	-0.077712	4.818423
389.442150	8000.468843	13.004352	-0.077642	4.818420
389.567786	8000.391725	13.009357	-0.077665	4.818396
389.662541	8000.522290	13.014362	-0.077683	4.818435
389.724375	8000.372836	13.019367	-0.077694	4.818390
389.919352	8000.424883	13.024371	-0.077731	4.818405
389.780757	8000.473455	13.029376	-0.077705	4.818420
389.875984	8000.431658	13.034381	-0.077723	4.818407
389.582695	8000.478130	13.039386	-0.077668	4.818422
389.296701	8000.461639	13.044391	-0.077615	4.818418
389.420629	8000.370835	13.049395	-0.077638	4.818391
389.503874	8000.519110	13.054400	-0.077654	4.818434
389.500153	8000.453899	13.059405	-0.077653	4.818415
389.590332	8000.424647	13.064410	-0.077670	4.818406
389.143901	8000.377603	13.069415	-0.077587	4.818394
388.896723	8000.431007	13.074419	-0.077541	4.818411
389.592160	8000.402609	13.079424	-0.077670	4.818399
389.638209	8000.444227	13.084429	-0.077679	4.818412
389.529718	8000.432248	13.089434	-0.077659	4.818408
389.394716	8000.472460	13.094439	-0.077634	4.818421
389.176298	8000.452682	13.099443	-0.077593	4.818416
389.119449	8000.499210	13.104448	-0.077583	4.818430
389.001489	8000.415634	13.109453	-0.077561	4.818406
389.091990	8000.429477	13.114458	-0.077578	4.818409
388.951179	8000.407600	13.119463	-0.077551	4.818403
389.091556	8000.332784	13.124467	-0.077578	4.818381
388.699431	8000.458843	13.129472	-0.077505	4.818420
389.312502	8000.467165	13.134477	-0.077619	4.818420
389.154004	8000.438742	13.139482	-0.077589	4.818412
389.082235	8000.436720	13.144487	-0.077576	4.818412
389.475952	8000.346423	13.149491	-0.077649	4.818383
389.115447	8000.540176	13.154496	-0.077582	4.818442
388.815014	8000.330106	13.159501	-0.077526	4.818381
389.236646	8000.430419	13.164506	-0.077605	4.818409
389.476097	8000.477815	13.169511	-0.077650	4.818422
389.346246	8000.423505	13.174515	-0.077625	4.818407
389.780496	8000.422044	13.179520	-0.077706	4.818404
389.379525	8000.395585	13.184525	-0.077632	4.818398
389.491908	8000.549511	13.189530	-0.077653	4.818443
389.634018	8000.458953	13.194535	-0.077679	4.818416
389.584188	8000.423596	13.199539	-0.077670	4.818406
389.191029	8000.523366	13.204544	-0.077597	4.818437
389.439393	8000.366984	13.209549	-0.077643	4.818389
389.223737	8000.471265	13.214554	-0.077603	4.818421
389.083666	8000.432582	13.219559	-0.077577	4.818410
389.288964	8000.424860	13.224563	-0.077615	4.818407
389.251254	8000.467443	13.229568	-0.077608	4.818420
389.767934	8000.462898	13.234573	-0.077704	4.818417
389.834737	8000.465910	13.239578	-0.077717	4.818417
390.034862	8000.379291	13.244583	-0.077754	4.818391
390.064505	8000.430146	13.249587	-0.077760	4.818406
389.931036	8000.406266	13.254592	-0.077735	4.818399
389.467403	8000.460936	13.259597	-0.077649	4.818417
389.904794	8000.415376	13.264602	-0.077730	4.818402
389.929127	8000.418862	13.269607	-0.077735	4.818403
389.587463	8000.386901	13.274611	-0.077671	4.818395
389.798555	8000.392922	13.279616	-0.077711	4.818396
390.094088	8000.405345	13.284621	-0.077766	4.818398
390.216708	8000.396502	13.289626	-0.077788	4.818395
390.233716	8000.382022	13.294631	-0.077792	4.818391
390.235022	8000.385196	13.299635	-0.077792	4.818392
390.071667	8000.427125	13.304640	-0.077762	4.818405
389.836196	8000.429187	13.309645	-0.077718	4.818406
389.677888	8000.451215	13.314650	-0.077688	4.818413
390.084605	8000.389472	13.319655	-0.077764	4.818393
390.252829	8000.412780	13.324659	-0.077796	4.818400
389.837995	8000.432377	13.329664	-0.077718	4.818407
390.059939	8000.407015	13.334669	-0.077760	4.818399
390.205447	8000.385870	13.339674	-0.077787	4.818392
389.685044	8000.425055	13.344679	-0.077690	4.818406
390.007557	8000.326435	13.349683	-0.077750	4.818375
390.032949	8000.386691	13.354688	-0.077755	4.818393
389.697320	8000.456762	13.359693	-0.077692	4.818415
389.995188	8000.460808	13.364698	-0.077748	4.818415
389.830354	8000.431247	13.369703	-0.077717	4.818407
390.183796	8000.410823	13.374707	-0.077783	4.818399
389.998493	8000.420923	13.379712	-0.077749	4.818403
390.189275	8000.428771	13.384717	-0.077784	4.818405
390.356556	8000.406871	13.389722	-0.077815	4.818398
390.208586	8000.379641	13.394727	-0.077788	4.818390
390.209435	8000.385961	13.399731	-0.077788	4.818392
389.935130	8000.517824	13.404736	-0.077737	4.818432
389.852691	8000.330676	13.409741	-0.077722	4.818377
389.901161	8000.429083	13.414746	-0.077731	4.818406
389.749681	8000.416519	13.419751	-0.077703	4.818403
389.937404	8000.460061	13.424755	-0.077738	4.818415
389.673139	8000.462783	13.429760	-0.077688	4.818417
389.483610	8000.452857	13.434765	-0.077653	4.818415
389.637039	8000.399238	13.439770	-0.077682	4.818398
389.350961	8000.496257	13.444775	-0.077629	4.818428
389.588004	8000.460589	13.449779	-0.077673	4.818417
390.136907	8000.389215	13.454784	-0.077775	4.818393
389.923361	8000.354789	13.459789	-0.077735	4.818384
389.927055	8000.491476	13.464794	-0.077736	4.818424
389.733107	8000.434193	13.469799	-0.077700	4.818408
389.553529	8000.432810	13.474803	-0.077667	4.818408
389.488661	8000.554903	13.479808	-0.077655	4.818445
389.912818	8000.375682	13.484813	-0.077734	4.818390
390.088283	8000.455843	13.489818	-0.077766	4.818413
390.153967	8000.404186	13.494823	-0.077779	4.818398
390.231182	8000.426258	13.499827	-0.077793	4.818404
390.363502	8000.355536	13.504832	-0.077818	4.818382
390.570632	8000.370964	13.509837	-0.077856	4.818386
390.538157	8000.362117	13.514842	-0.077850	4.818384
390.202005	8000.379629	13.519847	-0.077788	4.818390
390.617363	8000.386322	13.524851	-0.077865	4.818390
390.528024	8000.344121	13.529856	-0.077848	4.818378
390.441107	8000.366067	13.534861	-0.077832	4.818385
390.440164	8000.375517	13.539866	-0.077832	4.818388
390.469162	8000.341230	13.544871	-0.077838	4.818378
390.420197	8000.365793	13.549875	-0.077829	4.818385
390.420515	8000.366851	13.554880	-0.077829	4.818385
390.408003	8000.418186	13.559885	-0.077826	4.818401
390.418330	8000.396257	13.564890	-0.077828	4.818394
390.207867	8000.394454	13.569895	-0.077789	4.818394
390.055288	8000.471214	13.574899	-0.077761	4.818418
390.064865	8000.356784	13.579904	-0.077763	4.818384
389.584045	8000.508966	13.584909	-0.077673	4.818431
390.142842	8000.492381	13.589914	-0.077777	4.818424
390.081605	8000.445307	13.594919	-0.077766	4.818410
390.103034	8000.380437	13.599923	-0.077770	4.818391
390.092257	8000.474887	13.604928	-0.077768	4.818419
390.653343	8000.425752	13.609933	-0.077873	4.818402
390.389191	8000.441087	13.614938	-0.077823	4.818408
390.395717	8000.367606	13.619943	-0.077825	4.818386
390.210853	8000.521705	13.624947	-0.077790	4.818432
390.004169	8000.457941	13.629952	-0.077752	4.818414
390.008191	8000.455897	13.634957	-0.077753	4.818413
389.836817	8000.446216	13.639962	-0.077721	4.818411
389.810676	8000.454273	13.644967	-0.077716	4.818414
389.917320	8000.391611	13.649971	-0.077736	4.818395
390.230003	8000.436849	13.654976	-0.077794	4.818407
390.269094	8000.407954	13.659981	-0.077801	4.818398
390.279989	8000.411258	13.664986	-0.077803	4.818399
390.335802	8000.402559	13.669991	-0.077814	4.818396
390.279919	8000.457509	13.674995	-0.077804	4.818413
390.147954	8000.408423	13.680000	-0.077779	4.818399
389.861905	8000.415054	13.685005	-0.077726	4.818402
389.831027	8000.503976	13.690010	-0.077720	4.818428
389.847599	8000.449550	13.695015	-0.077723	4.818412
389.925458	8000.362324	13.700019	-0.077738	4.818386
390.108771	8000.438387	13.705024	-0.077772	4.818408
389.852382	8000.481155	13.710029	-0.077724	4.818422
390.169767	8000.478110	13.715034	-0.077783	4.818419
389.620067	8000.496927	13.720039	-0.077681	4.818427
389.642555	8000.376367	13.725043	-0.077685	4.818391
389.648747	8000.533057	13.730048	-0.077687	4.818438
389.600357	8000.363188	13.735053	-0.077677	4.818388
389.859469	8000.489678	13.740058	-0.077726	4.818424
389.806496	8000.401727	13.745063	-0.077716	4.818398
389.674618	8000.499788	13.750067	-0.077692	4.818428
388.989551	8000.526228	13.755072	-0.077564	4.818438
389.557683	8000.335298	13.760077	-0.077670	4.818379
390.168900	8000.446598	13.765082	-0.077784	4.818410
390.127146	8000.401891	13.770087	-0.077776	4.818397
390.275049	8000.430178	13.775091	-0.077803	4.818405
390.082767	8000.443336	13.780096	-0.077768	4.818409
390.247963	8000.410897	13.785101	-0.077799	4.818399
390.174910	8000.461410	13.790106	-0.077785	4.818414
390.463863	8000.407528	13.795111	-0.077839	4.818397
390.550866	8000.447602	13.800115	-0.077855	4.818409
390.539990	8000.383343	13.805120	-0.077853	4.818390
390.806952	8000.377512	13.810125	-0.077903	4.818387
390.679523	8000.394703	13.815130	-0.077879	4.818393
390.512635	8000.382981	13.820135	-0.077848	4.818390
390.393541	8000.406592	13.825139	-0.077826	4.818397
390.828685	8000.351543	13.830144	-0.077907	4.818379
390.664917	8000.369292	13.835149	-0.077877	4.818385
390.549004	8000.397151	13.840154	-0.077855	4.818394
390.524369	8000.364237	13.845159	-0.077850	4.818384
390.523474	8000.374739	13.850163	-0.077850	4.818387
390.457742	8000.377002	13.855168	-0.077838	4.818388
390.503022	8000.391284	13.860173	-0.077847	4.818392
390.574746	8000.328147	13.865178	-0.077860	4.818373
390.019097	8000.489824	13.870183	-0.077757	4.818423
390.411534	8000.465726	13.875187	-0.077830	4.818415
390.658276	8000.391302	13.880192	-0.077876	4.818392
390.674762	8000.413601	13.885197	-0.077879	4.818398
390.523636	8000.434675	13.890202	-0.077851	4.818405
390.531629	8000.368571	13.895207	-0.077852	4.818385
390.577637	8000.414394	13.900211	-0.077861	4.818399
390.490411	8000.457356	13.905216	-0.077845	4.818412
390.454581	8000.344411	13.910221	-0.077838	4.818379
390.653888	8000.401775	13.915226	-0.077875	4.818395
390.303104	8000.392811	13.920231	-0.077810	4.818393
390.069498	8000.468471	13.925235	-0.077767	4.818417
390.166187	8000.405673	13.930240	-0.077785	4.818398
390.030236	8000.424851	13.935245	-0.077759	4.818404
390.368300	8000.464128	13.940250	-0.077822	4.818414
390.397336	8000.441403	13.945255	-0.077828	4.818408
390.453510	8000.382259	13.950259	-0.077838	4.818390
390.537141	8000.494809	13.955264	-0.077854	4.818423
390.186020	8000.470074	13.960269	-0.077789	4.818417
390.321999	8000.491893	13.965274	-0.077814	4.818423
390.285513	8000.431492	13.970279	-0.077807	4.818405
390.228849	8000.380276	13.975283	-0.077797	4.818390
390.361169	8000.474567	13.980288	-0.077821	4.818418
390.372647	8000.415867	13.985293	-0.077823	4.818400
390.460075	8000.439129	13.990298	-0.077840	4.818407
390.174775	8000.411085	13.995303	-0.077787	4.818399
390.429477	8000.464996	14.000307	-0.077834	4.818414
390.352889	8000.425071	14.005312	-0.077820	4.818403
390.068914	8000.378126	14.010317	-0.077767	4.818390
390.674153	8000.460971	14.015322	-0.077880	4.818412
390.752640	8000.418947	14.020327	-0.077894	4.818399
390.272576	8000.497566	14.025331	-0.077805	4.818425
390.438211	8000.414683	14.030336	-0.077836	4.818399
390.876048	8000.398560	14.035341	-0.077918	4.818393
390.779799	8000.384643	14.040346	-0.077900	4.818389
390.378053	8000.400212	14.045351	-0.077825	4.818395
390.428683	8000.502854	14.050355	-0.077834	4.818426
390.559754	8000.392175	14.055360	-0.077859	4.818392
390.327832	8000.465756	14.060365	-0.077816	4.818415
390.200703	8000.441961	14.065370	-0.077792	4.818408
390.055037	8000.519865	14.070375	-0.077765	4.818432
390.283856	8000.446249	14.075379	-0.077808	4.818409
390.194248	8000.398790	14.080384	-0.077791	4.818396
390.290808	8000.485238	14.085389	-0.077809	4.818421
390.579876	8000.473401	14.090394	-0.077863	4.818416
390.486282	8000.434295	14.095399	-0.077846	4.818405
390.652371	8000.423941	14.100403	-0.077877	4.818401
390.310229	8000.423503	14.105408	-0.077813	4.818403
390.164068	8000.358460	14.110413	-0.077786	4.818384
390.353600	8000.484007	14.115418	-0.077821	4.818420
390.380700	8000.445490	14.120423	-0.077826	4.818409
390.136387	8000.526259	14.125427	-0.077781	4.818434
390.308331	8000.444513	14.130432	-0.077813	4.818409
390.473716	8000.425741	14.135437	-0.077844	4.818403
390.214836	8000.431689	14.140442	-0.077795	4.818405
390.160879	8000.400479	14.145447	-0.077785	4.818396
390.046039	8000.526099	14.150451	-0.077764	4.818434
390.279739	8000.412609	14.155456	-0.077808	4.818399
390.273671	8000.456674	14.160461	-0.077807	4.818413
390.465778	8000.400427	14.165466	-0.077842	4.818395
390.654911	8000.437683	14.170471	-0.077878	4.818405
390.662870	8000.418875	14.175475	-0.077879	4.818400
390.412872	8000.492210	14.180480	-0.077833	4.818423
390.359952	8000.464167	14.185485	-0.077823	4.818414
390.702209	8000.465665	14.190490	-0.077887	4.818413
390.667471	8000.407388	14.195495	-0.077880	4.818396
390.750178	8000.454761	14.200499	-0.077896	4.818410
390.669937	8000.417938	14.205504	-0.077881	4.818399
390.383235	8000.468703	14.210509	-0.077827	4.818416
390.424552	8000.470318	14.215514	-0.077835	4.818416
390.382566	8000.431914	14.220519	-0.077827	4.818405
390.524793	8000.427542	14.225523	-0.077854	4.818403
390.401640	8000.420617	14.230528	-0.077831	4.818401
390.563063	8000.433323	14.235533	-0.077861	4.818404
390.502985	8000.369447	14.240538	-0.077850	4.818386
390.313288	8000.422580	14.245543	-0.077815	4.818402
390.627069	8000.498315	14.250547	-0.077873	4.818423
390.508463	8000.434696	14.255552	-0.077851	4.818405
390.374850	8000.489641	14.260557	-0.077826	4.818422
390.305480	8000.498162	14.265562	-0.077813	4.818425
390.269046	8000.348422	14.270567	-0.077807	4.818380
390.542127	8000.405736	14.275571	-0.077857	4.818396
390.055670	8000.469554	14.280576	-0.077767	4.818417
390.140453	8000.454943	14.285581	-0.077783	4.818413
390.262689	8000.518617	14.290586	-0.077806	4.818431
390.274835	8000.381099	14.295591	-0.077808	4.818390
390.544667	8000.483564	14.300595	-0.077858	4.818419
390.642601	8000.394506	14.305600	-0.077876	4.818393
390.541732	8000.473019	14.310605	-0.077858	4.818416
390.613091	8000.454022	14.315610	-0.077871	4.818410
390.570923	8000.422972	14.320615	-0.077863	4.818401
390.825353	8000.442196	14.325619	-0.077911	4.818406
390.617925	8000.388932	14.330624	-0.077872	4.818391
390.715887	8000.396571	14.335629	-0.077890	4.818393
390.629419	8000.484739	14.340634	-0.077874	4.818419
390.588972	8000.313924	14.345639	-0.077867	4.818369
390.558348	8000.450147	14.350643	-0.077861	4.818409
390.381555	8000.461413	14.355648	-0.077828	4.818413
390.409991	8000.415556	14.360653	-0.077834	4.818400
390.663282	8000.415845	14.365658	-0.077881	4.818399
390.640432	8000.381905	14.370663	-0.077877	4.818389
390.739537	8000.467338	14.375667	-0.077895	4.818414
390.423524	8000.509295	14.380672	-0.077836	4.818428
390.487296	8000.412417	14.385677	-0.077848	4.818398
390.388882	8000.358532	14.390682	-0.077830	4.818383
390.046416	8000.443224	14.395687	-0.077766	4.818409
390.303727	8000.447772	14.400691	-0.077814	4.818410
390.254473	8000.464974	14.405696	-0.077805	4.818415
390.236059	8000.451063	14.410701	-0.077802	4.818411
390.197376	8000.487328	14.415706	-0.077795	4.818422
390.516048	8000.370787	14.420711	-0.077854	4.818386
390.546377	8000.442673	14.425715	-0.077860	4.818407
390.776584	8000.414271	14.430720	-0.077902	4.818398
390.679191	8000.435024	14.435725	-0.077884	4.818404
391.143831	8000.396141	14.440730	-0.077971	4.818391
390.799237	8000.377801	14.445735	-0.077907	4.818387
390.893849	7999.389028	14.450739	-0.077924	4.818093

390.885403	7996.295103	14.455744	-0.077920	4.817174
391.014716	7990.676098	14.460749	-0.077941	4.815503
390.835645	7984.055317	14.465754	-0.077903	4.813536
390.796960	7976.786321	14.470759	-0.077891	4.811374
390.796289	7969.165479	14.475763	-0.077886	4.809107
390.371210	7961.408667	14.480768	-0.077802	4.806799
389.858241	7953.515270	14.485773	-0.077701	4.804450
390.541246	7945.571451	14.490778	-0.077823	4.802081
390.441972	7937.506707	14.495783	-0.077800	4.799677
390.658237	7929.590015	14.500787	-0.077835	4.797315
390.687509	7921.550502	14.505792	-0.077835	4.794915
390.606497	7913.590058	14.510797	-0.077815	4.792539
390.729934	7905.593070	14.515802	-0.077833	4.790150
390.627609	7897.517114	14.520807	-0.077808	4.787736
390.862131	7889.556462	14.525811	-0.077847	4.785355
390.542535	7881.549942	14.530816	-0.077782	4.782961
390.482299	7873.574272	14.535821	-0.077766	4.780574
390.648495	7865.591402	14.540826	-0.077792	4.778183
390.490069	7857.533143	14.545831	-0.077757	4.775769
390.401446	7849.531780	14.550835	-0.077735	4.773370
390.257809	7841.604711	14.555840	-0.077703	4.770993
390.356474	7833.507141	14.560845	-0.077717	4.768563
390.409714	7825.535921	14.565850	-0.077721	4.766170
390.054211	7817.496374	14.570855	-0.077650	4.763756
390.031569	7809.633312	14.575859	-0.077641	4.761393
389.937926	7801.561789	14.580864	-0.077618	4.758966
389.849447	7793.563984	14.585869	-0.077596	4.756560
389.971189	7785.527437	14.590874	-0.077614	4.754141
389.831383	7777.538409	14.595879	-0.077583	4.751736
389.730803	7769.510293	14.600883	-0.077559	4.749317
389.989988	7761.494292	14.605888	-0.077602	4.746900
390.048783	7753.440402	14.610893	-0.077608	4.744471
389.657316	7745.571401	14.615898	-0.077530	4.742097
389.728747	7737.492735	14.620903	-0.077538	4.739658
389.657282	7729.581498	14.625907	-0.077519	4.737268
389.482405	7721.515572	14.630912	-0.077481	4.734831
389.563626	7713.468990	14.635917	-0.077491	4.732398
389.734054	7705.497253	14.640922	-0.077518	4.729986
389.841536	7697.500260	14.645927	-0.077533	4.727565
389.743567	7689.437036	14.650931	-0.077509	4.725123
389.589718	7681.515733	14.655936	-0.077476	4.722723
389.892754	7673.508447	14.660941	-0.077527	4.720295
389.774484	7665.541974	14.665946	-0.077500	4.717879
389.721687	7657.484330	14.670951	-0.077485	4.715434
390.054469	7649.519201	14.675955	-0.077541	4.713015
389.947705	7641.491167	14.680960	-0.077516	4.710576
389.879552	7633.487031	14.685965	-0.077498	4.708144
389.695930	7625.479364	14.690970	-0.077459	4.705709
389.388305	7617.473336	14.695975	-0.077397	4.703273
389.544993	7609.542184	14.700979	-0.077421	4.700859
389.598536	7601.507050	14.705984	-0.077425	4.698411
389.384223	7593.547815	14.710989	-0.077380	4.695986
389.313584	7585.520605	14.715994	-0.077362	4.693539
389.353224	7577.497986	14.720999	-0.077364	4.691092
389.575412	7569.483187	14.726003	-0.077400	4.688645
389.134568	7561.552311	14.731008	-0.077313	4.686224
389.246837	7553.452544	14.736013	-0.077329	4.683749
389.498181	7545.580985	14.741018	-0.077371	4.681343
389.030246	7537.493298	14.746023	-0.077278	4.678869
388.811476	7529.579930	14.751027	-0.077232	4.676448
388.916779	7521.479741	14.756032	-0.077247	4.673968
388.828017	7513.473136	14.761037	-0.077225	4.671515
389.198860	7505.404295	14.766042	-0.077289	4.669042
389.096104	7497.421379	14.771047	-0.077265	4.666594
389.294852	7489.397283	14.776051	-0.077296	4.664132
389.073724	7481.521312	14.781056	-0.077250	4.661714
389.051019	7473.406807	14.786061	-0.077241	4.659222
389.368759	7465.472580	14.791066	-0.077295	4.656784
389.184113	7457.420366	14.796071	-0.077255	4.654308
389.318158	7449.484195	14.801075	-0.077275	4.651866
389.252363	7441.420312	14.806080	-0.077258	4.649384
388.964206	7433.473304	14.811085	-0.077199	4.646937
389.113860	7425.463592	14.816090	-0.077221	4.644469
388.834908	7417.476545	14.821095	-0.077164	4.642007
389.106649	7409.450946	14.826099	-0.077210	4.639531
389.316172	7401.461955	14.831104	-0.077244	4.637066
389.040042	7393.409962	14.836109	-0.077187	4.634580
388.958024	7385.460146	14.841114	-0.077167	4.632124
389.024044	7377.400263	14.846119	-0.077174	4.629632
389.041643	7369.417444	14.851123	-0.077172	4.627163
388.842605	7361.397947	14.856128	-0.077130	4.624682
388.603158	7353.456515	14.861133	-0.077080	4.622223
388.879971	7345.426540	14.866138	-0.077126	4.619735
388.545357	7337.414394	14.871143	-0.077059	4.617252
388.694741	7329.414458	14.876147	-0.077081	4.614771
388.713775	7321.418143	14.881152	-0.077080	4.612290
388.817858	7313.374596	14.886157	-0.077094	4.609793
388.707511	7305.434549	14.891162	-0.077068	4.607327
388.743545	7297.356693	14.896167	-0.077070	4.604816
388.902871	7289.465470	14.901171	-0.077094	4.602363
388.914739	7281.398388	14.906176	-0.077091	4.599853
388.905266	7273.433058	14.911181	-0.077084	4.597373
388.956526	7265.398625	14.916186	-0.077089	4.594871
388.742976	7257.393766	14.921191	-0.077044	4.592376
388.541554	7249.359258	14.926195	-0.077001	4.589871
388.438775	7241.397782	14.931200	-0.076977	4.587387
388.399961	7233.342353	14.936205	-0.076964	4.584873
388.417807	7225.415994	14.941210	-0.076963	4.582397
388.196271	7217.357372	14.946215	-0.076916	4.579879
388.493531	7209.376247	14.951219	-0.076966	4.577384
388.282389	7201.349425	14.956224	-0.076922	4.574873
388.092559	7193.378829	14.961229	-0.076881	4.572377
388.027302	7185.363061	14.966234	-0.076864	4.569867
387.964953	7177.362671	14.971239	-0.076847	4.567360
387.946998	7169.365419	14.976243	-0.076839	4.564853
387.896404	7161.419560	14.981248	-0.076824	4.562360
387.702163	7153.302061	14.986253	-0.076783	4.559812
387.362332	7145.440681	14.991258	-0.076714	4.557343
387.549005	7137.333493	14.996263	-0.076744	4.554796
387.860174	7129.338050	15.001267	-0.076797	4.552283
387.266380	7121.355883	15.006272	-0.076681	4.549770
387.712586	7113.274929	15.011277	-0.076759	4.547228
387.584307	7105.286243	15.016282	-0.076730	4.544712
387.669368	7097.310173	15.021287	-0.076740	4.542199
387.737745	7089.325763	15.026291	-0.076748	4.539682
387.533115	7081.347146	15.031296	-0.076705	4.537165
388.130083	7073.231428	15.036301	-0.076811	4.534605
387.984071	7065.301756	15.041306	-0.076778	4.532101
387.796312	7057.263318	15.046311	-0.076738	4.529560
387.552502	7049.363284	15.051315	-0.076688	4.527062
387.856403	7041.266067	15.056320	-0.076739	4.524502
387.756029	7033.321284	15.061325	-0.076715	4.521987
388.015883	7025.293573	15.066330	-0.076758	4.519446
387.618687	7017.332175	15.071335	-0.076679	4.516922
387.799080	7009.282727	15.076339	-0.076708	4.514371
388.024603	7001.340602	15.081344	-0.076744	4.511852
387.822984	6993.250111	15.086349	-0.076702	4.509284
387.654162	6985.310397	15.091354	-0.076665	4.506762
387.421064	6977.231529	15.096359	-0.076617	4.504194
387.435354	6969.318492	15.101363	-0.076614	4.501678
387.770217	6961.222686	15.106368	-0.076671	4.499104
387.840884	6953.264924	15.111373	-0.076679	4.496572
387.995035	6945.257703	15.116378	-0.076703	4.494022
387.819643	6937.241355	15.121383	-0.076665	4.491467
387.861388	6929.253391	15.126387	-0.076667	4.488920
387.577723	6921.235885	15.131392	-0.076609	4.486362
387.599197	6913.193755	15.136397	-0.076608	4.483795
387.809354	6905.285716	15.141402	-0.076642	4.481270
387.435416	6897.251047	15.146407	-0.076567	4.478701
387.719309	6889.264101	15.151411	-0.076615	4.476148
387.614210	6881.246875	15.156416	-0.076590	4.473583
387.385677	6873.248667	15.161421	-0.076543	4.471022
387.588297	6865.233546	15.166426	-0.076575	4.468455
387.561308	6857.167766	15.171431	-0.076565	4.465870
387.402424	6849.225362	15.176435	-0.076530	4.463323
387.327595	6841.264943	15.181440	-0.076511	4.460768
387.547730	6833.200758	15.186445	-0.076547	4.458181
387.631194	6825.247179	15.191450	-0.076557	4.455626
387.336553	6817.206732	15.196455	-0.076497	4.453040
387.540972	6809.178982	15.201459	-0.076530	4.450460
387.355490	6801.238475	15.206464	-0.076491	4.447904
387.184790	6793.154066	15.211469	-0.076454	4.445300
387.486876	6785.246202	15.216474	-0.076505	4.442754
387.241378	6777.177263	15.221479	-0.076454	4.440152
387.122327	6769.216584	15.226483	-0.076426	4.437584
386.876085	6761.218172	15.231488	-0.076375	4.435001
387.143496	6753.224677	15.236493	-0.076420	4.432422
386.641019	6745.200398	15.241498	-0.076321	4.429826
386.746517	6737.171642	15.246503	-0.076336	4.427231
386.880171	6729.137426	15.251507	-0.076355	4.424633
386.719927	6721.201718	15.256512	-0.076320	4.422064
386.638166	6713.141135	15.261517	-0.076300	4.419453
386.778302	6705.208543	15.266522	-0.076321	4.416883
386.703885	6697.167906	15.271527	-0.076302	4.414276
386.593628	6689.142331	15.276531	-0.076276	4.411671
386.567846	6681.120954	15.281536	-0.076266	4.409067
386.698714	6673.171570	15.286541	-0.076285	4.406486
387.038627	6665.137406	15.291546	-0.076344	4.403877
386.812647	6657.173314	15.296551	-0.076296	4.401285
386.531261	6649.193012	15.301555	-0.076239	4.398687
386.566530	6641.206623	15.306560	-0.076240	4.396087
386.554376	6633.154027	15.311565	-0.076233	4.393464
386.578651	6625.202238	15.316570	-0.076232	4.390872
386.543397	6617.117579	15.321575	-0.076220	4.388235
386.581259	6609.191256	15.326579	-0.076222	4.385648
386.459407	6601.200208	15.331584	-0.076194	4.383038
386.461665	6593.199015	15.336589	-0.076190	4.380423
386.328843	6585.280817	15.341594	-0.076160	4.377834
385.897968	6577.240983	15.346599	-0.076074	4.375201
386.213892	6569.234273	15.351603	-0.076128	4.372582
386.384242	6561.217236	15.356608	-0.076155	4.369957
386.231229	6553.244282	15.361613	-0.076121	4.367343
386.204722	6545.242971	15.366618	-0.076111	4.364719
386.039417	6537.263795	15.371623	-0.076075	4.362100
386.103482	6529.246400	15.376627	-0.076082	4.359468
385.808943	6521.393815	15.381632	-0.076022	4.356886
385.467744	6513.286908	15.386637	-0.075953	4.354218
385.911551	6505.240397	15.391642	-0.076030	4.351575
385.835349	6497.103327	15.396647	-0.076011	4.348896
385.828521	6489.130820	15.401651	-0.076004	4.346271
385.732140	6481.227734	15.406656	-0.075981	4.343666
386.047926	6473.208085	15.411661	-0.076035	4.341024
386.230466	6465.271080	15.416666	-0.076064	4.338407
385.985447	6457.244982	15.421671	-0.076013	4.335755
386.271143	6449.251790	15.426675	-0.076061	4.333117
386.111104	6441.235429	15.431680	-0.076026	4.330466
386.005546	6433.244425	15.436685	-0.076001	4.327823
386.078650	6425.241701	15.441690	-0.076010	4.325175
385.948706	6417.242290	15.446695	-0.075980	4.322525
386.077753	6409.251738	15.451699	-0.075999	4.319878
386.131368	6401.278293	15.456704	-0.076004	4.317235
386.057986	6393.226384	15.461709	-0.075985	4.314563
385.948990	6385.289474	15.466714	-0.075960	4.311928
385.826379	6377.193385	15.471719	-0.075932	4.309238
385.997318	6369.195270	15.476723	-0.075958	4.306581
385.834040	6361.161027	15.481728	-0.075923	4.303907
385.969661	6353.208388	15.486733	-0.075943	4.301262
385.949996	6345.220660	15.491738	-0.075934	4.298602
385.649229	6337.253832	15.496743	-0.075873	4.295945
385.676102	6329.173720	15.501747	-0.075873	4.293251
385.594735	6321.210131	15.506752	-0.075852	4.290594
385.659472	6313.157772	15.511757	-0.075859	4.287907
385.596489	6305.226079	15.516762	-0.075842	4.285257
385.429631	6297.189213	15.521767	-0.075806	4.282569
385.630744	6289.207866	15.526771	-0.075838	4.279901
385.623610	6281.187839	15.531776	-0.075832	4.277217
385.735081	6273.181620	15.536781	-0.075847	4.274537
385.712962	6265.206542	15.541786	-0.075838	4.271865
385.435109	6257.145128	15.546791	-0.075781	4.269160
385.259618	6249.232044	15.551795	-0.075743	4.266503
385.303654	6241.173490	15.556800	-0.075746	4.263798
385.209530	6233.239287	15.561805	-0.075724	4.261132
384.889874	6225.257308	15.566810	-0.075659	4.258446
384.889529	6217.168973	15.571815	-0.075654	4.255725
385.426957	6209.185697	15.576819	-0.075749	4.253044
385.214019	6201.155627	15.581824	-0.075704	4.250337
384.803085	6193.182128	15.586829	-0.075622	4.247646
384.830429	6185.214416	15.591834	-0.075622	4.244960
384.810291	6177.167175	15.596839	-0.075613	4.242244
384.460014	6169.191655	15.601843	-0.075543	4.239548
384.421367	6161.268054	15.606848	-0.075531	4.236870
383.917064	6153.219063	15.611853	-0.075431	4.234144
384.296329	6145.199414	15.616858	-0.075497	4.231435
384.127569	6137.174395	15.621863	-0.075460	4.228716
384.654969	6129.077216	15.626867	-0.075553	4.225979
384.810439	6121.097329	15.631872	-0.075577	4.223276
384.668003	6113.148636	15.636877	-0.075545	4.220579
384.703412	6105.159794	15.641882	-0.075547	4.217868
384.938248	6097.094233	15.646887	-0.075585	4.215132
385.117136	6089.122904	15.651891	-0.075613	4.212425
385.007872	6081.098198	15.656896	-0.075588	4.209695
384.988767	6073.152813	15.661901	-0.075579	4.206991
384.874562	6065.169885	15.666906	-0.075553	4.204272
384.880822	6057.215623	15.671911	-0.075549	4.201562
384.870997	6049.163591	15.676915	-0.075542	4.198817
384.622590	6041.252089	15.681920	-0.075490	4.196115
384.508235	6033.140082	15.686925	-0.075464	4.193345
384.914572	6025.095132	15.691930	-0.075534	4.190601
384.755611	6017.084820	15.696935	-0.075500	4.187862
384.303225	6009.098208	15.701939	-0.075410	4.185125
384.590427	6001.124060	15.706944	-0.075459	4.182399
384.495651	5993.099132	15.711949	-0.075436	4.179649
384.675707	5985.168198	15.716954	-0.075464	4.176933
384.469725	5977.096772	15.721959	-0.075420	4.174163
384.471417	5969.182555	15.726963	-0.075416	4.171447
384.443011	5961.140063	15.731968	-0.075405	4.168685
384.379016	5953.123276	15.736973	-0.075388	4.165930
384.271748	5945.186915	15.741978	-0.075363	4.163199
384.313110	5937.166042	15.746983	-0.075366	4.160440
384.102379	5929.231319	15.751987	-0.075321	4.157706
384.335816	5921.161463	15.756992	-0.075359	4.154928
384.483205	5913.155318	15.761997	-0.075382	4.152170
384.448984	5905.142195	15.767002	-0.075370	4.149405
384.065163	5897.191799	15.772007	-0.075294	4.146656
384.337786	5889.116476	15.777011	-0.075339	4.143869
384.287922	5881.246449	15.782016	-0.075325	4.141148
384.162072	5873.185109	15.787021	-0.075296	4.138358
384.070845	5865.209091	15.792026	-0.075274	4.135596
383.923456	5857.200956	15.797031	-0.075241	4.132820
384.020866	5849.192436	15.802035	-0.075254	4.130046
383.878020	5841.181474	15.807040	-0.075222	4.127265
383.990455	5833.109389	15.812045	-0.075238	4.124465
384.036163	5825.224180	15.817050	-0.075242	4.121727
383.961329	5817.175622	15.822055	-0.075222	4.118929
384.165764	5809.248072	15.827059	-0.075255	4.116175
383.943549	5801.226105	15.832064	-0.075209	4.113380
383.642429	5793.225384	15.837069	-0.075148	4.110590
383.716801	5785.197265	15.842074	-0.075156	4.107793
383.882560	5777.114526	15.847079	-0.075182	4.104977
384.142155	5769.130958	15.852083	-0.075225	4.102194
383.914260	5761.160019	15.857088	-0.075177	4.099407
383.782614	5753.204959	15.862093	-0.075148	4.096626
384.046680	5745.141834	15.867098	-0.075192	4.093810
383.831535	5737.158327	15.872103	-0.075147	4.091013
383.916305	5729.198250	15.877107	-0.075157	4.088227
384.072412	5721.171128	15.882112	-0.075181	4.085417
383.801972	5713.207367	15.887117	-0.075126	4.082620
383.752100	5705.212341	15.892122	-0.075111	4.079814
383.842223	5697.175158	15.897127	-0.075123	4.076994
383.786230	5689.155032	15.902131	-0.075107	4.074175
383.555302	5681.219837	15.907136	-0.075059	4.071381
383.260701	5673.198010	15.912141	-0.074999	4.068554
383.591745	5665.160307	15.917146	-0.075055	4.065729
383.468228	5657.143262	15.922151	-0.075027	4.062903
383.791616	5649.152300	15.927155	-0.075082	4.060090
383.662675	5641.210339	15.932160	-0.075053	4.057286
383.604690	5633.138238	15.937165	-0.075037	4.054435
383.725141	5625.185895	15.942170	-0.075054	4.051627
383.634963	5617.127397	15.947175	-0.075032	4.048776
383.834507	5609.167616	15.952179	-0.075064	4.045963
383.766302	5601.193489	15.957184	-0.075047	4.043138
383.596714	5593.233028	15.962189	-0.075010	4.040315
383.627049	5585.263947	15.967194	-0.075010	4.037490
383.323237	5577.194133	15.972199	-0.074949	4.034622
383.520644	5569.163732	15.977203	-0.074980	4.031774
383.639707	5561.121415	15.982208	-0.074997	4.028918
383.182697	5553.190958	15.987213	-0.074907	4.026091
383.292145	5545.193785	15.992218	-0.074922	4.023247
383.149199	5537.211231	15.997223	-0.074890	4.020402
383.192867	5529.250280	16.002227	-0.074893	4.017566
382.503101	5521.300148	16.007232	-0.074760	4.014720
382.518196	5513.261831	16.012237	-0.074757	4.011852
382.793943	5505.199567	16.017242	-0.074803	4.008977
382.789423	5497.196340	16.022247	-0.074797	4.006117
382.456053	5489.217868	16.027251	-0.074730	4.003258
382.633281	5481.241945	16.032256	-0.074758	4.000407
382.735210	5473.222069	16.037261	-0.074772	3.997537
382.801245	5465.233148	16.042266	-0.074779	3.994675
382.771714	5457.227544	16.047271	-0.074768	3.991803
383.081551	5449.163528	16.052275	-0.074821	3.988914
382.929221	5441.242309	16.057280	-0.074787	3.986067
382.573995	5433.235958	16.062285	-0.074716	3.983183
382.761967	5425.288879	16.067290	-0.074746	3.980328
382.946192	5417.214953	16.072295	-0.074775	3.977425
382.960409	5409.202866	16.077299	-0.074772	3.974539
382.653625	5401.278253	16.082304	-0.074710	3.971677
382.828089	5393.171246	16.087309	-0.074737	3.968756
382.639933	5385.283575	16.092314	-0.074697	3.965905
382.682840	5377.218197	16.097319	-0.074700	3.962992
382.899827	5369.267411	16.102323	-0.074735	3.960122
382.545799	5361.315689	16.107328	-0.074664	3.957239
382.347330	5353.275854	16.112333	-0.074622	3.954325
382.717414	5345.244198	16.117338	-0.074686	3.951421
382.544705	5337.217537	16.122343	-0.074648	3.948508
382.477104	5329.235372	16.127347	-0.074631	3.945610
382.702960	5321.213104	16.132352	-0.074668	3.942702
382.652749	5313.195430	16.137357	-0.074653	3.939787
382.536860	5305.266926	16.142362	-0.074626	3.936902
382.456661	5297.224093	16.147367	-0.074606	3.933973
382.563521	5289.240100	16.152371	-0.074621	3.931068
382.533761	5281.247709	16.157376	-0.074610	3.928154
382.291955	5273.239025	16.162381	-0.074560	3.925229
382.605265	5265.275581	16.167386	-0.074613	3.922328
382.432908	5257.253014	16.172391	-0.074576	3.919394
382.195926	5249.318508	16.177395	-0.074527	3.916489
382.213620	5241.278326	16.182400	-0.074525	3.913548
382.388482	5233.259654	16.187405	-0.074552	3.910616
382.460121	5225.271207	16.192410	-0.074560	3.907691
382.004263	5217.273708	16.197415	-0.074470	3.904750
382.207700	5209.324211	16.202419	-0.074503	3.901837
381.977136	5201.314865	16.207424	-0.074455	3.898891
382.137969	5193.315005	16.212429	-0.074480	3.895955
382.037925	5185.305662	16.217434	-0.074456	3.893007
381.785048	5177.301482	16.222439	-0.074404	3.890056
381.621735	5169.367198	16.227443	-0.074368	3.887131
381.746776	5161.301127	16.232448	-0.074386	3.884160
381.912997	5153.370879	16.237453	-0.074412	3.881238
381.870009	5145.317831	16.242458	-0.074399	3.878264
381.589553	5137.378841	16.247463	-0.074341	3.875326
381.902180	5129.221196	16.252467	-0.074394	3.872316
381.503180	5121.251431	16.257472	-0.074315	3.869359
381.425620	5113.240323	16.262477	-0.074295	3.866391
381.153900	5105.320495	16.267482	-0.074240	3.863450
381.522138	5097.240073	16.272487	-0.074303	3.860461
381.359700	5089.287625	16.277491	-0.074268	3.857506
381.705830	5081.273642	16.282496	-0.074327	3.854537
381.722849	5073.277003	16.287501	-0.074325	3.851565
381.475036	5065.345392	16.292506	-0.074274	3.848609
381.657753	5057.312992	16.297511	-0.074302	3.845622
381.456569	5049.360083	16.302515	-0.074260	3.842655
381.332011	5041.356230	16.307520	-0.074231	3.839668
381.298462	5033.353361	16.312525	-0.074220	3.836681
381.608264	5025.344185	16.317530	-0.074273	3.833696
381.359688	5017.323785	16.322535	-0.074221	3.830693
381.210341	5009.359012	16.327539	-0.074188	3.827711
381.296590	5001.313237	16.332544	-0.074199	3.824701
381.213502	4993.347111	16.337549	-0.074178	3.821715
380.900498	4985.410912	16.342554	-0.074115	3.818732
381.118914	4977.313785	16.347559	-0.074150	3.815699
381.338842	4969.330956	16.352563	-0.074186	3.812706
381.343345	4961.332362	16.357568	-0.074182	3.809700
381.125066	4953.346036	16.362573	-0.074136	3.806692
381.176635	4945.350648	16.367578	-0.074140	3.803683
381.111989	4937.400095	16.372583	-0.074123	3.800687
381.109726	4929.395765	16.377587	-0.074118	3.797669
381.044939	4921.403272	16.382592	-0.074100	3.794652
381.023105	4913.354211	16.387597	-0.074091	3.791612
381.254599	4905.353048	16.392602	-0.074129	3.788594
380.940835	4897.371943	16.397607	-0.074066	3.785568
381.083062	4889.380735	16.402611	-0.074087	3.782546
381.028809	4881.380023	16.407616	-0.074072	3.779514
381.037662	4873.395832	16.412621	-0.074068	3.776487
381.071132	4865.391835	16.417626	-0.074069	3.773451
381.168812	4857.373818	16.422631	-0.074082	3.770409
380.912104	4849.438670	16.427635	-0.074029	3.767387
380.585971	4841.451198	16.432640	-0.073963	3.764341
380.716748	4833.460349	16.437645	-0.073982	3.761303
380.898183	4825.442390	16.442650	-0.074011	3.758252
380.740238	4817.463883	16.447655	-0.073977	3.755207
380.892891	4809.472953	16.452659	-0.074000	3.752161
380.947371	4801.424448	16.457664	-0.074005	3.749089
380.641216	4793.470143	16.462669	-0.073943	3.746041
380.580527	4785.504223	16.467674	-0.073926	3.742992
380.497714	4777.467181	16.472679	-0.073905	3.739914
380.490154	4769.516640	16.477683	-0.073899	3.736867
380.221635	4761.520347	16.482688	-0.073844	3.733794
380.091658	4753.507923	16.487693	-0.073814	3.730716
380.424622	4745.467900	16.492698	-0.073871	3.727636
380.109859	4737.458109	16.497703	-0.073807	3.724549
380.421746	4729.489397	16.502707	-0.073860	3.721491
380.604813	4721.499115	16.507712	-0.073889	3.718419
380.332301	4713.521154	16.512717	-0.073833	3.715337
380.352571	4705.456108	16.517722	-0.073832	3.712227
380.388348	4697.421849	16.522727	-0.073833	3.709127
380.286341	4689.479407	16.527731	-0.073809	3.706056
380.206057	4681.475967	16.532736	-0.073789	3.702959
380.166098	4673.455596	16.537741	-0.073777	3.699854
380.562813	4665.510129	16.542746	-0.073845	3.696787
380.285021	4657.483708	16.547751	-0.073788	3.693669
380.471382	4649.495567	16.552755	-0.073818	3.690574
380.257829	4641.491325	16.557760	-0.073773	3.687461
380.036518	4633.488048	16.562765	-0.073727	3.684345
380.186042	4625.560240	16.567770	-0.073749	3.681265
380.184297	4617.520278	16.572775	-0.073744	3.678135
380.078663	4609.573586	16.577779	-0.073719	3.675036
380.053175	4601.572918	16.582784	-0.073709	3.671916
380.185690	4593.527395	16.587789	-0.073729	3.668780
380.365453	4585.545353	16.592794	-0.073757	3.665667
380.005706	4577.565911	16.597799	-0.073685	3.662537
380.126835	4569.569593	16.602803	-0.073702	3.659412
379.623646	4561.666616	16.607808	-0.073603	3.656303
379.662668	4553.610865	16.612813	-0.073605	3.653147
379.941426	4545.534122	16.617818	-0.073652	3.649986
379.839849	4537.573653	16.622823	-0.073628	3.646858
379.704251	4529.624846	16.627827	-0.073598	3.643731
379.714711	4521.675780	16.632832	-0.073594	3.640605
379.477037	4513.639349	16.637837	-0.073545	3.637435
379.771793	4505.625265	16.642842	-0.073595	3.634286
379.620388	4497.641882	16.647847	-0.073561	3.631133
379.498002	4489.631014	16.652851	-0.073533	3.627968
379.452433	4481.619323	16.657856	-0.073520	3.624802
379.423159	4473.645059	16.662861	-0.073509	3.621649
379.623533	4465.635192	16.667866	-0.073541	3.618485
379.400911	4457.624978	16.672871	-0.073495	3.615306
379.718873	4449.634722	16.677875	-0.073549	3.612148
379.469069	4441.635915	16.682880	-0.073497	3.608967
379.532871	4433.641090	16.687885	-0.073504	3.605794
379.710166	4425.660696	16.692890	-0.073531	3.602628
379.554405	4417.664556	16.697895	-0.073497	3.599442
379.505480	4409.713187	16.702899	-0.073483	3.596275
379.496049	4401.713479	16.707904	-0.073476	3.593087
379.446651	4393.672974	16.712909	-0.073462	3.589878
379.430297	4385.682579	16.717914	-0.073454	3.586688
379.350252	4377.655609	16.722919	-0.073433	3.583478
379.278595	4369.732005	16.727923	-0.073415	3.580307
379.119934	4361.778287	16.732928	-0.073380	3.577119
379.241497	4353.695516	16.737933	-0.073398	3.573884
379.525349	4345.712906	16.742938	-0.073445	3.570691
379.424775	4337.720324	16.747943	-0.073421	3.567480
379.179670	4329.733447	16.752947	-0.073371	3.564264
379.014061	4321.848783	16.757952	-0.073335	3.561089
379.025686	4313.798859	16.762957	-0.073332	3.557850
378.844811	4305.844472	16.767962	-0.073293	3.554640
379.055004	4297.731378	16.772967	-0.073327	3.551375
378.853564	4289.754490	16.777971	-0.073284	3.548150
378.873963	4281.750215	16.782976	-0.073283	3.544917
378.614884	4273.773897	16.787981	-0.073229	3.541684
378.989015	4265.746280	16.792986	-0.073294	3.538448
378.902512	4257.782917	16.797991	-0.073273	3.535219
378.708551	4249.847491	16.802995	-0.073231	3.531996
378.695607	4241.818482	16.808000	-0.073224	3.528738
378.745624	4233.795084	16.813005	-0.073228	3.525481
378.571371	4225.872534	16.818010	-0.073190	3.522254
378.507656	4217.812961	16.823015	-0.073173	3.518973
378.545393	4209.862567	16.828019	-0.073175	3.515736
378.685143	4201.845652	16.833024	-0.073196	3.512472
378.669878	4193.820785	16.838029	-0.073188	3.509197
378.623779	4185.863155	16.843034	-0.073174	3.505946
378.590322	4177.841709	16.848039	-0.073163	3.502665
378.678375	4169.841814	16.853043	-0.073174	3.499395
378.765840	4161.875315	16.858048	-0.073185	3.496135
378.709593	4153.853051	16.863053	-0.073169	3.492844
378.395986	4145.924311	16.868058	-0.073106	3.489580
378.281365	4137.918087	16.873063	-0.073079	3.486288
378.365956	4129.911863	16.878067	-0.073090	3.483000
378.470248	4121.913100	16.883072	-0.073104	3.479711
378.331213	4113.936152	16.888077	-0.073073	3.476421
378.440453	4105.938452	16.893082	-0.073088	3.473127
378.307380	4097.927074	16.898087	-0.073058	3.469817
378.285384	4089.939325	16.903091	-0.073049	3.466517
378.275671	4081.945369	16.908096	-0.073042	3.463211
378.186013	4073.992716	16.913101	-0.073020	3.459917
378.373597	4065.984352	16.918106	-0.073050	3.456606
378.250718	4057.994710	16.923111	-0.073022	3.453288
378.371943	4049.970963	16.928115	-0.073039	3.449962
378.553320	4041.992014	16.933120	-0.073068	3.446653
378.352610	4034.001138	16.938125	-0.073026	3.443324
378.150169	4026.070709	16.943130	-0.072983	3.440015
378.026798	4018.079294	16.948135	-0.072955	3.436682
378.359206	4010.018931	16.953139	-0.073011	3.433331
378.066836	4002.078100	16.958144	-0.072952	3.430006
378.087426	3994.018931	16.963149	-0.072950	3.426639
378.034089	3986.063382	16.968154	-0.072935	3.423309
378.002827	3978.073507	16.973159	-0.072924	3.419963
378.010371	3970.088955	16.978163	-0.072920	3.416617
377.955782	3962.101839	16.983168	-0.072905	3.413264
378.097983	3954.058432	16.988173	-0.072926	3.409891
378.071610	3946.101025	16.993178	-0.072916	3.406545
378.002400	3938.084633	16.998183	-0.072898	3.403170
378.013703	3930.119027	17.003187	-0.072895	3.399815
377.897162	3922.189936	17.008192	-0.072868	3.396468
377.946942	3914.129559	17.013197	-0.072873	3.393068
377.810392	3906.130861	17.018202	-0.072842	3.389684
377.615932	3898.120834	17.023207	-0.072801	3.386290
377.602311	3890.150568	17.028211	-0.072793	3.382916
377.729296	3882.143010	17.033216	-0.072811	3.379528
377.582203	3874.170039	17.038221	-0.072779	3.376141
377.514330	3866.190936	17.043226	-0.072761	3.372750
376.926748	3858.245150	17.048231	-0.072646	3.369352
377.028852	3850.220566	17.053235	-0.072660	3.365942
377.229121	3842.210904	17.058240	-0.072692	3.362538
377.102362	3834.214396	17.063245	-0.072664	3.359124
376.955813	3826.325798	17.068250	-0.072631	3.355753
376.950296	3818.248017	17.073255	-0.072625	3.352302
377.294231	3810.202572	17.078259	-0.072684	3.348875
377.442779	3802.209389	17.083264	-0.072706	3.345459
377.375672	3794.243344	17.088269	-0.072689	3.342043
377.290229	3786.291467	17.093274	-0.072668	3.338629
377.269738	3778.278053	17.098279	-0.072659	3.335188
377.256741	3770.316545	17.103283	-0.072651	3.331765
377.245382	3762.298533	17.108288	-0.072644	3.328315
377.145950	3754.301777	17.113293	-0.072620	3.324867
377.333233	3746.342003	17.118298	-0.072650	3.321443
377.409797	3738.346052	17.123303	-0.072659	3.317995
376.952914	3730.409191	17.128307	-0.072569	3.314548
377.091922	3722.409845	17.133312	-0.072589	3.311094
377.020989	3714.369256	17.138317	-0.072571	3.307610
377.011922	3706.362541	17.143322	-0.072564	3.304140
377.085441	3698.376182	17.148327	-0.072573	3.300678
377.116241	3690.394147	17.153331	-0.072573	3.297212
376.866385	3682.447466	17.158336	-0.072522	3.293747
376.869832	3674.398705	17.163341	-0.072517	3.290245
377.201031	3666.391591	17.168346	-0.072573	3.286769
376.988092	3658.429026	17.173351	-0.072529	3.283288
376.933137	3650.479097	17.178355	-0.072513	3.279815
376.858018	3642.511631	17.183360	-0.072494	3.276329
376.733030	3634.480973	17.188365	-0.072466	3.272810
376.521250	3626.553941	17.193370	-0.072421	3.269330
376.597339	3618.514172	17.198375	-0.072430	3.265807
376.829983	3610.491272	17.203379	-0.072468	3.262295
376.505370	3602.548571	17.208384	-0.072403	3.258792
376.571704	3594.578876	17.213389	-0.072410	3.255288
376.778337	3586.562126	17.218394	-0.072443	3.251767
376.524734	3578.570812	17.223399	-0.072391	3.248233
376.515026	3570.575366	17.228403	-0.072384	3.244704
376.645686	3562.602991	17.233408	-0.072403	3.241187
376.483380	3554.627972	17.238413	-0.072368	3.237653
376.387223	3546.653393	17.243418	-0.072345	3.234118
376.482673	3538.643436	17.248423	-0.072357	3.230571
376.297522	3530.653327	17.253427	-0.072318	3.227018
376.406711	3522.632953	17.258432	-0.072333	3.223459
375.998517	3514.655132	17.263437	-0.072251	3.219894
376.293772	3506.685223	17.268442	-0.072301	3.216358
376.255590	3498.651455	17.273447	-0.072289	3.212776
376.175250	3490.641191	17.278451	-0.072269	3.209198
376.122006	3482.719028	17.283456	-0.072254	3.205656
376.045757	3474.692736	17.288461	-0.072234	3.202064
375.529822	3466.846032	17.293466	-0.072133	3.198528
375.424101	3458.804423	17.298471	-0.072108	3.194919
375.871302	3450.738705	17.303475	-0.072186	3.191319
375.917713	3442.735252	17.308480	-0.072190	3.187726
375.790277	3434.729914	17.313485	-0.072161	3.184120
375.895985	3426.790747	17.318490	-0.072176	3.180550
375.694405	3418.823914	17.323495	-0.072133	3.176950
375.564140	3410.833674	17.328499	-0.072104	3.173338
375.624268	3402.833294	17.333504	-0.072110	3.169727
375.642807	3394.836422	17.338509	-0.072108	3.166110
375.697757	3386.870600	17.343514	-0.072113	3.162506
375.365054	3378.911353	17.348519	-0.072046	3.158883
375.605500	3370.889804	17.353523	-0.072085	3.155253
375.680073	3362.908852	17.358528	-0.072094	3.151630
375.609518	3354.902702	17.363533	-0.072076	3.147984
375.616001	3346.907134	17.368538	-0.072072	3.144343
375.575194	3338.941947	17.373543	-0.072059	3.140709
375.402661	3330.954680	17.378547	-0.072022	3.137055
375.596174	3322.966258	17.383552	-0.072053	3.133413
375.454287	3314.935975	17.388557	-0.072021	3.129732
375.563829	3306.986767	17.393562	-0.072036	3.126096
375.367665	3298.999175	17.398567	-0.071995	3.122424
375.585620	3290.988988	17.403571	-0.072030	3.118755
375.646406	3283.032445	17.408576	-0.072036	3.115101
375.022331	3275.101406	17.413581	-0.071915	3.111421
374.870822	3267.140440	17.418586	-0.071882	3.107746
375.166284	3259.044301	17.423591	-0.071931	3.104024
375.273256	3251.095730	17.428595	-0.071946	3.100358
375.273357	3243.097204	17.433600	-0.071941	3.096659
375.103820	3235.129553	17.438605	-0.071904	3.092962
375.002113	3227.153827	17.443610	-0.071880	3.089260
374.694379	3219.208775	17.448615	-0.071818	3.085558
374.569174	3211.225181	17.453619	-0.071789	3.081842
374.768038	3203.227422	17.458624	-0.071821	3.078130
374.671385	3195.230066	17.463629	-0.071798	3.074401
374.993399	3187.159879	17.468634	-0.071853	3.070652
374.913710	3179.173572	17.473639	-0.071833	3.066919
374.950884	3171.174272	17.478643	-0.071834	3.063181
374.738664	3163.253208	17.483648	-0.071790	3.059463
374.782614	3155.256717	17.488653	-0.071793	3.055718
374.394812	3147.343483	17.493658	-0.071715	3.051986
374.538655	3139.287137	17.498663	-0.071737	3.048208
374.516350	3131.297838	17.503667	-0.071728	3.044449
374.517052	3123.367027	17.508672	-0.071723	3.040714
374.359566	3115.399670	17.513677	-0.071688	3.036949
374.328148	3107.409224	17.518682	-0.071677	3.033174
374.136440	3099.413910	17.523687	-0.071636	3.029385
374.352848	3091.396271	17.528691	-0.071671	3.025601
374.243993	3083.441958	17.533696	-0.071646	3.021826
374.316206	3075.416699	17.538701	-0.071654	3.018022
374.418039	3067.446983	17.543706	-0.071668	3.014240
374.101126	3059.504744	17.548711	-0.071604	3.010446
373.825810	3051.549267	17.553715	-0.071548	3.006643
374.191941	3043.494497	17.558720	-0.071611	3.002820
374.082917	3035.513539	17.563725	-0.071585	2.999003
374.063649	3027.599768	17.568730	-0.071576	2.995218
374.127258	3019.562663	17.573735	-0.071583	2.991374
374.260482	3011.546618	17.578739	-0.071603	2.987538
374.125753	3003.559183	17.583744	-0.071572	2.983698
374.175504	2995.589517	17.588749	-0.071577	2.979870
374.285307	2987.640449	17.593754	-0.071592	2.976051
373.853540	2979.660951	17.598759	-0.071506	2.972183
373.862833	2971.655984	17.603763	-0.071503	2.968322
374.057975	2963.643868	17.608768	-0.071534	2.964461
373.903053	2955.729764	17.613773	-0.071500	2.960625
373.727752	2947.777329	17.618778	-0.071462	2.956764
373.832738	2939.745003	17.623783	-0.071477	2.952874
374.140065	2931.717180	17.628787	-0.071529	2.948992
373.888537	2923.791678	17.633792	-0.071477	2.945125
373.802267	2915.799025	17.638797	-0.071455	2.941228
373.640282	2907.874592	17.643802	-0.071420	2.937356
373.622572	2899.859838	17.648807	-0.071412	2.933442
373.753325	2891.831143	17.653811	-0.071431	2.929525
373.629234	2883.903058	17.658816	-0.071403	2.925637
373.581972	2875.918527	17.663821	-0.071389	2.921721
373.518603	2867.962402	17.668826	-0.071372	2.917812
373.574424	2859.949795	17.673831	-0.071377	2.913877
373.607937	2851.881361	17.678835	-0.071378	2.909908
373.587518	2843.914751	17.683840	-0.071369	2.905981
373.361987	2835.941959	17.688845	-0.071322	2.902034
373.616131	2827.966341	17.693850	-0.071364	2.898107
373.356284	2820.029894	17.698855	-0.071311	2.894166
373.241974	2812.047164	17.703859	-0.071284	2.890204
373.092693	2804.108290	17.708864	-0.071251	2.886256
373.340639	2796.047155	17.713869	-0.071292	2.882265
373.537863	2788.069231	17.718874	-0.071324	2.878307
373.053114	2780.167229	17.723879	-0.071228	2.874342
373.072756	2772.184363	17.728883	-0.071227	2.870360
372.897153	2764.213438	17.733888	-0.071189	2.866368
372.842293	2756.198866	17.738893	-0.071174	2.862355
373.012237	2748.222951	17.743898	-0.071200	2.858369
372.747332	2740.264651	17.748903	-0.071146	2.854361
372.644914	2732.289837	17.753907	-0.071121	2.850348
372.636957	2724.310562	17.758912	-0.071115	2.846333
372.495634	2716.343564	17.763917	-0.071083	2.842310
373.001299	2708.303281	17.768922	-0.071172	2.838283
372.758270	2700.337214	17.773927	-0.071122	2.834243
372.679752	2692.375438	17.778931	-0.071102	2.830210
372.842618	2684.370784	17.783936	-0.071127	2.826163
372.782324	2676.366974	17.788941	-0.071111	2.822098
372.644588	2668.467780	17.793946	-0.071080	2.818076
372.415148	2660.496760	17.798951	-0.071032	2.814006
372.330855	2652.508331	17.803955	-0.071011	2.809929
372.229611	2644.557346	17.808960	-0.070987	2.805865
372.152469	2636.554099	17.813965	-0.070968	2.801769
372.230565	2628.584733	17.818970	-0.070977	2.797695
372.532021	2620.535144	17.823975	-0.071028	2.793586
372.428196	2612.595644	17.828979	-0.071004	2.789504
372.459452	2604.602860	17.833984	-0.071004	2.785396
371.947696	2596.707340	17.838989	-0.070904	2.781300
372.029104	2588.727439	17.843994	-0.070914	2.777190
372.089187	2580.694762	17.848999	-0.070920	2.773045
371.459503	2572.794558	17.854003	-0.070798	2.768920
371.578916	2564.794559	17.859008	-0.070815	2.764784
372.241836	2556.713334	17.864013	-0.070933	2.760632
372.287717	2548.778816	17.869018	-0.070936	2.756513
372.249622	2540.779756	17.874023	-0.070924	2.752348
372.385056	2532.745863	17.879027	-0.070944	2.748170
372.586140	2524.765311	17.884032	-0.070976	2.744017
372.212529	2516.854487	17.889037	-0.070902	2.739859
372.147186	2508.930995	17.894042	-0.070884	2.735707
372.400406	2500.897571	17.899047	-0.070926	2.731511
372.381219	2492.938085	17.904051	-0.070918	2.727331
372.220492	2484.998303	17.909056	-0.070882	2.723145
372.035897	2477.044072	17.914061	-0.070843	2.718944
372.048969	2469.081995	17.919066	-0.070840	2.714744
371.970561	2461.103697	17.924071	-0.070821	2.710524
372.327122	2453.058818	17.929075	-0.070882	2.706290
372.174253	2445.112065	17.934080	-0.070848	2.702068
372.010544	2437.148571	17.939085	-0.070812	2.697830
372.194631	2429.173673	17.944090	-0.070842	2.693602
372.153879	2421.170555	17.949095	-0.070829	2.689338
372.001990	2413.250412	17.954099	-0.070795	2.685104
371.839602	2405.321352	17.959104	-0.070760	2.680857
371.899682	2397.327058	17.964109	-0.070766	2.676584
372.083109	2389.353694	17.969114	-0.070795	2.672323
371.760116	2381.367207	17.974119	-0.070730	2.668015
371.754289	2373.378106	17.979123	-0.070724	2.663719
371.403968	2365.489983	17.984128	-0.070653	2.659449
371.237588	2357.511126	17.989133	-0.070617	2.655134
371.237592	2349.517608	17.994138	-0.070612	2.650815
371.202019	2341.516716	17.999143	-0.070600	2.646484
370.765355	2333.634070	18.004147	-0.070514	2.642182
370.802035	2325.633789	18.009152	-0.070515	2.637841
371.001751	2317.609795	18.014157	-0.070547	2.633491
371.136707	2309.615286	18.019162	-0.070567	2.629145
371.414422	2301.581845	18.024167	-0.070614	2.624781
371.110208	2293.686907	18.029171	-0.070552	2.620446
371.101210	2285.735315	18.034176	-0.070545	2.616092
371.338511	2277.714408	18.039181	-0.070584	2.611710
371.127689	2269.790742	18.044186	-0.070540	2.607344
371.305755	2261.784655	18.049191	-0.070568	2.602951
371.363256	2253.823525	18.054195	-0.070573	2.598568
371.254132	2245.886008	18.059200	-0.070548	2.594178
371.048641	2237.831408	18.064205	-0.070505	2.589710
371.208567	2229.835957	18.069210	-0.070529	2.585292
371.074512	2221.910608	18.074215	-0.070499	2.580885
371.025524	2213.954996	18.079219	-0.070485	2.576460
371.081784	2205.996939	18.084224	-0.070490	2.572033
371.005348	2198.008986	18.089229	-0.070471	2.567572
370.979297	2190.042229	18.094234	-0.070461	2.563119
370.983806	2182.109123	18.099239	-0.070456	2.558679
370.974863	2174.141978	18.104243	-0.070450	2.554211
370.832820	2166.208267	18.109248	-0.070418	2.549745
370.726816	2158.210195	18.114253	-0.070393	2.545238
370.856363	2150.263975	18.119258	-0.070412	2.540768
370.686925	2142.305644	18.124263	-0.070375	2.536262
370.579202	2134.349490	18.129267	-0.070350	2.531754
370.812358	2126.344996	18.134272	-0.070388	2.527235
370.705959	2118.377539	18.139277	-0.070364	2.522705
370.794692	2110.437944	18.144282	-0.070375	2.518196
370.499080	2102.510163	18.149287	-0.070315	2.513658
370.578024	2094.515609	18.154291	-0.070324	2.509101
370.260068	2086.579331	18.159296	-0.070260	2.504539
370.447468	2078.571410	18.164301	-0.070290	2.499966
370.678496	2070.590827	18.169306	-0.070328	2.495403
370.594690	2062.635569	18.174311	-0.070307	2.490823
370.337140	2054.686504	18.179315	-0.070254	2.486226
370.477195	2046.724703	18.184320	-0.070275	2.481642
370.545806	2038.763121	18.189325	-0.070282	2.477044
370.480134	2030.813662	18.194330	-0.070265	2.472435
370.344209	2022.853876	18.199335	-0.070234	2.467805
370.357847	2014.879801	18.204339	-0.070232	2.463170
370.282475	2006.954650	18.209344	-0.070213	2.458548
370.225375	1998.966408	18.214349	-0.070197	2.453882
370.367345	1990.996465	18.219354	-0.070218	2.449233
370.013441	1983.061547	18.224359	-0.070147	2.444558
370.038519	1975.119783	18.229363	-0.070147	2.439898
370.166534	1967.147171	18.234368	-0.070165	2.435220
369.974721	1959.159442	18.239373	-0.070124	2.430499
369.852575	1951.214808	18.244378	-0.070097	2.425799
369.570233	1943.275585	18.249383	-0.070039	2.421081
369.769374	1935.266526	18.254387	-0.070071	2.416350
369.879290	1927.292539	18.259392	-0.070086	2.411624
369.797491	1919.325130	18.264397	-0.070066	2.406877
369.905232	1911.388920	18.269402	-0.070081	2.402155
369.508676	1903.484405	18.274407	-0.070002	2.397402
369.714473	1895.489420	18.279411	-0.070035	2.392633
369.724469	1887.530572	18.284416	-0.070032	2.387861
369.672126	1879.567982	18.289421	-0.070017	2.383072
369.489777	1871.660446	18.294426	-0.069978	2.378296
369.750076	1863.633152	18.299431	-0.070021	2.373474
369.809151	1855.671636	18.304435	-0.070027	2.368666
369.689578	1847.747850	18.309440	-0.069999	2.363856
369.389238	1839.846016	18.314445	-0.069938	2.359034
369.352118	1831.897867	18.319450	-0.069926	2.354197
369.263276	1823.936516	18.324455	-0.069905	2.349337
369.203169	1815.954331	18.329459	-0.069888	2.344456
369.405365	1807.985386	18.334464	-0.069921	2.339595
369.253822	1800.033867	18.339469	-0.069887	2.334706
369.149331	1792.120064	18.344474	-0.069863	2.329833
369.120426	1784.130243	18.349479	-0.069852	2.324909
369.334606	1776.150549	18.354483	-0.069887	2.320002
369.272917	1768.230757	18.359488	-0.069870	2.315098
369.129116	1760.290513	18.364493	-0.069838	2.310164
369.008262	1752.358385	18.369498	-0.069811	2.305227
368.667335	1744.443610	18.374503	-0.069742	2.300270
368.820655	1736.441622	18.379507	-0.069766	2.295291
368.644226	1728.527167	18.384512	-0.069728	2.290328
368.464493	1720.575935	18.389517	-0.069689	2.285330
368.729718	1712.600619	18.394522	-0.069733	2.280345
368.741694	1704.644759	18.399527	-0.069730	2.275339
368.703627	1696.660438	18.404531	-0.069718	2.270300
368.447460	1688.742973	18.409536	-0.069665	2.265273
368.353267	1680.790882	18.414541	-0.069643	2.260227
368.718032	1672.774838	18.419546	-0.069705	2.255169
368.485956	1664.860692	18.424551	-0.069657	2.250112
368.484968	1656.888615	18.429555	-0.069652	2.245027
368.521950	1648.981703	18.434560	-0.069653	2.239976
368.647578	1641.017596	18.439565	-0.069672	2.234885
368.532088	1633.094749	18.444570	-0.069645	2.229786
368.605105	1625.117039	18.449575	-0.069654	2.224658
368.494536	1617.203113	18.454579	-0.069628	2.219543
368.434563	1609.279615	18.459584	-0.069612	2.214414
368.136947	1601.348193	18.464589	-0.069551	2.209246
368.020153	1593.431290	18.469594	-0.069524	2.204092
368.254541	1585.449196	18.474599	-0.069563	2.198916
368.022689	1577.553318	18.479603	-0.069514	2.193741
367.827642	1569.621186	18.484608	-0.069473	2.188533
367.986592	1561.597531	18.489613	-0.069497	2.183285
367.982558	1553.680056	18.494618	-0.069491	2.178080
367.817667	1545.747427	18.499623	-0.069456	2.172837
367.828837	1537.789772	18.504627	-0.069453	2.167582
367.987677	1529.827670	18.509632	-0.069477	2.162324
367.770316	1521.930948	18.514637	-0.069431	2.157062
367.714635	1514.016383	18.519642	-0.069416	2.151790
367.799720	1506.048659	18.524647	-0.069427	2.146483
367.518085	1498.139789	18.529651	-0.069369	2.141167
367.584812	1490.192428	18.534656	-0.069376	2.135846
367.518870	1482.245431	18.539661	-0.069359	2.130499
367.326911	1474.344020	18.544666	-0.069318	2.125157
367.348433	1466.392949	18.549671	-0.069317	2.119788
367.418826	1458.453756	18.554675	-0.069325	2.114419
367.278325	1450.513795	18.559680	-0.069294	2.109015
367.158046	1442.552168	18.564685	-0.069266	2.103584
366.841322	1434.698216	18.569690	-0.069202	2.098193
367.032861	1426.697704	18.574695	-0.069233	2.092738
367.041302	1418.741619	18.579699	-0.069229	2.087282
366.814976	1410.853725	18.584704	-0.069182	2.081834
366.835020	1402.913316	18.589709	-0.069180	2.076361
367.067515	1394.955497	18.594714	-0.069218	2.070883
366.766818	1387.058439	18.599719	-0.069157	2.065378
366.633044	1379.142450	18.604723	-0.069127	2.059862
366.667019	1371.211467	18.609728	-0.069129	2.054338
366.642442	1363.272455	18.614733	-0.069119	2.048787
367.070287	1355.265170	18.619738	-0.069193	2.043221
367.005171	1347.381788	18.624743	-0.069176	2.037675
366.860540	1339.468799	18.629747	-0.069144	2.032085
366.793095	1331.562066	18.634752	-0.069126	2.026492
366.810443	1323.613366	18.639757	-0.069124	2.020862
366.688281	1315.733350	18.644762	-0.069097	2.015251
366.553475	1307.805459	18.649767	-0.069066	2.009589
366.625627	1299.857665	18.654771	-0.069075	2.003919
366.658749	1291.960718	18.659776	-0.069076	1.998264
366.619408	1284.025707	18.664781	-0.069063	1.992559
366.372524	1276.150887	18.669786	-0.069012	1.986858
366.359315	1268.227472	18.674791	-0.069005	1.981131
366.377664	1260.292117	18.679795	-0.069003	1.975382
366.320733	1252.382733	18.684800	-0.068987	1.969627
366.353829	1244.440856	18.689805	-0.068988	1.963841
366.353264	1236.550194	18.694810	-0.068983	1.958072
366.267348	1228.636286	18.699815	-0.068962	1.952259
365.820233	1220.767948	18.704819	-0.068874	1.946423
365.958083	1212.814659	18.709824	-0.068894	1.940571
365.835890	1204.890973	18.714829	-0.068866	1.934694
365.921540	1196.971569	18.719834	-0.068877	1.928826
365.841704	1189.034418	18.724839	-0.068857	1.922908
365.965007	1181.113286	18.729843	-0.068875	1.917007
365.814144	1173.229496	18.734848	-0.068842	1.911084
365.739468	1165.300173	18.739853	-0.068823	1.905118
366.039920	1157.365130	18.744858	-0.068874	1.899171
365.895305	1149.477903	18.749863	-0.068842	1.893191
365.719205	1141.581448	18.754867	-0.068804	1.887181
365.797794	1133.680802	18.759872	-0.068813	1.881178
365.821486	1125.768541	18.764877	-0.068812	1.875140
365.838402	1117.868497	18.769882	-0.068811	1.869092
365.594710	1109.987051	18.774887	-0.068760	1.863008
365.593253	1102.089308	18.779891	-0.068755	1.856920
365.605103	1094.184553	18.784896	-0.068752	1.850808
365.417771	1086.286087	18.789901	-0.068712	1.844656
365.370824	1078.421298	18.794906	-0.068698	1.838527
364.840659	1070.605575	18.799911	-0.068594	1.832358
364.847226	1062.653225	18.804915	-0.068590	1.826126
365.003172	1054.732226	18.809920	-0.068614	1.819915
364.796041	1046.854191	18.814925	-0.068571	1.813672
365.048209	1038.911787	18.819930	-0.068612	1.807413
365.024655	1031.017238	18.824935	-0.068603	1.801137
365.018988	1023.139785	18.829939	-0.068597	1.794854
364.924804	1015.237825	18.834944	-0.068574	1.788519
364.501072	1007.395238	18.839949	-0.068490	1.782168
364.805426	999.453131	18.844954	-0.068542	1.775805
364.662851	991.574250	18.849959	-0.068510	1.769414
364.476565	983.706377	18.854963	-0.068470	1.763003
364.593418	975.824209	18.859968	-0.068487	1.756595
364.364309	967.960443	18.864973	-0.068439	1.750135
364.658620	960.020801	18.869978	-0.068489	1.743656
364.253197	952.217018	18.874983	-0.068408	1.737175
364.236572	944.326356	18.879987	-0.068400	1.730648
364.113528	936.458717	18.884992	-0.068372	1.724101
364.106775	928.569600	18.889997	-0.068366	1.717526
364.000581	920.730619	18.895002	-0.068341	1.710955
364.208962	912.798431	18.900007	-0.068375	1.704323
363.825762	904.985088	18.905011	-0.068298	1.697685
363.701838	897.121793	18.910016	-0.068270	1.691014
363.502616	889.259543	18.915021	-0.068228	1.684307
363.606886	881.379467	18.920026	-0.068242	1.677599
363.585446	873.509980	18.925031	-0.068233	1.670857
363.390537	865.665587	18.930035	-0.068192	1.664084
363.570187	857.768320	18.935040	-0.068220	1.657290
363.413312	849.910518	18.940045	-0.068186	1.650456
363.558984	842.035604	18.945050	-0.068208	1.643620
363.733213	834.160334	18.950055	-0.068235	1.636760
363.479368	826.320363	18.955059	-0.068183	1.629841
363.475853	818.456616	18.960064	-0.068177	1.622908
363.537736	810.575980	18.965069	-0.068184	1.615939
363.664893	802.706452	18.970074	-0.068202	1.608959
363.354718	794.912441	18.975079	-0.068139	1.601953
363.318870	787.087595	18.980083	-0.068128	1.594928
363.271589	779.257888	18.985088	-0.068114	1.587866
363.142187	771.417908	18.990093	-0.068085	1.580752
362.972109	763.619863	18.995098	-0.068048	1.573637
362.742447	755.794360	19.000103	-0.068000	1.566456
362.794913	747.947159	19.005107	-0.068005	1.559264
362.955312	740.085906	19.010112	-0.068030	1.552041
362.876077	732.239352	19.015117	-0.068010	1.544763
362.901824	724.413553	19.020122	-0.068009	1.537485
362.676157	716.606809	19.025127	-0.067962	1.530152
362.666517	708.778917	19.030131	-0.067956	1.522797
362.673512	700.966419	19.035136	-0.067952	1.515424
362.550450	693.156285	19.040141	-0.067924	1.507996
362.478259	685.347940	19.045146	-0.067905	1.500542
362.494335	677.530617	19.050151	-0.067903	1.493055
362.193443	669.756793	19.055155	-0.067842	1.485522
362.339955	661.933642	19.060160	-0.067864	1.477975
362.076247	654.134649	19.065165	-0.067810	1.470346
362.225631	646.291852	19.070170	-0.067833	1.462701
362.132948	638.492558	19.075175	-0.067811	1.455020
362.172216	630.680721	19.080179	-0.067813	1.447307
362.014156	622.922088	19.085184	-0.067779	1.439573
361.840748	615.154934	19.090189	-0.067741	1.431786
361.747592	607.378267	19.095194	-0.067719	1.423960
361.757234	599.580465	19.100199	-0.067716	1.416087
361.812921	591.785918	19.105203	-0.067721	1.408181
361.500513	584.068602	19.110208	-0.067658	1.400247
361.331077	576.319117	19.115213	-0.067621	1.392259
361.262381	568.537626	19.120218	-0.067603	1.384209
360.832621	560.830780	19.125223	-0.067518	1.376127
361.009028	552.999203	19.130227	-0.067546	1.367972
361.469850	545.166026	19.135232	-0.067627	1.359817
361.134785	537.470123	19.140237	-0.067560	1.351617
361.019115	529.733505	19.145242	-0.067533	1.343363
361.037917	521.983419	19.150247	-0.067532	1.335067
360.539056	514.318218	19.155251	-0.067434	1.326718
360.471395	506.592859	19.160256	-0.067416	1.318328
360.275692	498.818291	19.165261	-0.067375	1.309808
360.605126	490.985978	19.170266	-0.067431	1.301265
360.352029	483.299236	19.175271	-0.067379	1.292719
360.246349	475.582975	19.180275	-0.067354	1.284110
360.423099	467.848140	19.185280	-0.067382	1.275476
360.261888	460.158837	19.190285	-0.067347	1.266770
360.160678	452.482795	19.195290	-0.067323	1.258030
359.858317	444.821784	19.200295	-0.067262	1.249208
359.765044	437.138344	19.205299	-0.067240	1.240337
359.299234	429.536513	19.210304	-0.067148	1.231424
359.435933	421.792424	19.215309	-0.067169	1.222399
359.658050	414.075042	19.220314	-0.067205	1.213356
359.718642	406.383456	19.225319	-0.067211	1.204243
359.526569	398.761745	19.230323	-0.067171	1.195092
359.280763	391.147776	19.235328	-0.067120	1.185869
359.188370	383.504964	19.240333	-0.067098	1.176571
359.258300	375.847527	19.245338	-0.067106	1.167214
359.151662	368.232763	19.250343	-0.067081	1.157797
358.794670	360.641228	19.255347	-0.067010	1.148279
358.492637	353.065778	19.260352	-0.066948	1.138713
358.273996	345.459932	19.265357	-0.066903	1.129045
358.264323	337.851253	19.270362	-0.066896	1.119336
358.049933	330.280689	19.275367	-0.066851	1.109545
357.494370	322.775564	19.280371	-0.066743	1.099677
357.689331	315.144642	19.285376	-0.066774	1.089723
356.918904	307.695018	19.290381	-0.066626	1.079697
356.330334	300.218738	19.295386	-0.066512	1.069583
355.936856	292.699592	19.300391	-0.066434	1.059360
355.662378	285.170971	19.305395	-0.066378	1.049052
354.939820	277.734884	19.310400	-0.066238	1.038662
354.459200	270.254898	19.315405	-0.066144	1.028164
353.558374	262.867909	19.320410	-0.065971	1.017586
352.625666	255.473368	19.325415	-0.065793	1.006878
351.389813	248.146917	19.330419	-0.065558	0.996076
350.028084	240.818663	19.335424	-0.065300	0.985120
348.822602	233.475349	19.340429	-0.065071	0.974059
347.509579	226.153786	19.345434	-0.064821	0.962874
346.126351	218.860072	19.350439	-0.064559	0.951580
344.921190	211.537342	19.355443	-0.064330	0.940153
343.940469	204.192477	19.360448	-0.064143	0.928612
342.863174	196.879441	19.365453	-0.063937	0.916947
341.603178	189.624769	19.370458	-0.063698	0.905174
340.621475	182.320723	19.375463	-0.063511	0.893244
339.157259	175.127117	19.380467	-0.063233	0.881194
338.260643	167.862241	19.385472	-0.063062	0.869022
337.095794	160.661169	19.390477	-0.062840	0.856705
335.445913	153.571386	19.395482	-0.062528	0.844252
334.257906	146.407760	19.400487	-0.062302	0.831624
333.626232	139.150630	19.405491	-0.062180	0.818809
332.426883	132.061312	19.410496	-0.061952	0.805910
331.271221	124.975013	19.415501	-0.061733	0.792820
330.043595	117.947933	19.420506	-0.061499	0.779595
329.352791	110.840962	19.425511	-0.061366	0.766169
328.344184	103.843483	19.430515	-0.061174	0.752605
327.418467	96.854044	19.435520	-0.060997	0.738836
326.360102	89.926036	19.440525	-0.060795	0.724879
325.428538	83.035248	19.445530	-0.060618	0.710768
324.382744	76.370366	19.450535	-0.060419	0.696794