Fri Apr 16 19:28:58 2021

Number of Points = 3629
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.799462	0.195386	0.000000	0.000127	0.312981

2.134913	0.134642	0.005005	0.000065	0.312982
1.991175	0.160432	0.010010	0.000092	0.312981
1.725208	0.212403	0.015014	0.000141	0.312998
2.012646	0.156675	0.020019	0.000087	0.312982
1.823165	0.192058	0.025024	0.000123	0.312987
2.018138	0.156066	0.030029	0.000086	0.312984
1.721775	0.210060	0.035034	0.000141	0.312985
1.620362	0.231495	0.040038	0.000160	0.313000
1.779055	0.200106	0.045043	0.000131	0.312988
1.938446	0.169378	0.050048	0.000101	0.312980
2.054297	0.149423	0.055053	0.000079	0.312986
1.704969	0.212195	0.060058	0.000144	0.312983
1.734144	0.208598	0.065062	0.000139	0.312991
1.709761	0.211367	0.070067	0.000143	0.312983
1.880265	0.179233	0.075072	0.000111	0.312978
2.013253	0.156490	0.080077	0.000087	0.312985
2.035627	0.129336	0.085082	0.000082	0.312879
1.965679	0.090780	0.090086	0.000095	0.312642
1.801677	0.122057	0.095091	0.000126	0.312649
1.847716	0.111528	0.100096	0.000117	0.312639
1.921677	0.100510	0.105101	0.000103	0.312651
1.596597	0.157280	0.110106	0.000164	0.312640
1.136247	0.246311	0.115110	0.000249	0.312666
1.760084	0.128903	0.120115	0.000133	0.312647
1.723648	0.102132	0.125120	0.000140	0.312493
1.707988	0.071636	0.130125	0.000143	0.312339
1.902734	0.033263	0.135130	0.000107	0.312325
1.855792	0.044093	0.140134	0.000115	0.312336
1.708451	0.068277	0.145139	0.000143	0.312324
1.570703	0.092942	0.150144	0.000168	0.312323
2.086256	-0.065706	0.155149	0.000072	0.312022
2.121812	-0.079162	0.160154	0.000065	0.311990
2.156392	-0.084697	0.165158	0.000059	0.311994
2.264434	-0.104298	0.170163	0.000039	0.311994
2.167473	-0.144096	0.175168	0.000057	0.311728
2.043777	-0.125897	0.180173	0.000080	0.311709
1.982479	-0.116873	0.185178	0.000091	0.311699
1.942902	-0.122099	0.190182	0.000098	0.311642
2.082574	-0.205569	0.195187	0.000072	0.311372
1.638708	-0.123759	0.200192	0.000155	0.311378
1.609213	-0.114636	0.205197	0.000160	0.311396
1.500812	-0.143519	0.210202	0.000181	0.311170
1.394297	-0.144588	0.215206	0.000200	0.311075
1.351645	-0.135600	0.220211	0.000208	0.311081
1.694742	-0.219552	0.225216	0.000144	0.310981
1.308171	-0.195423	0.230221	0.000216	0.310767
1.132459	-0.164378	0.235226	0.000249	0.310763
1.564265	-0.245371	0.240230	0.000168	0.310752
1.655707	-0.314360	0.245235	0.000151	0.310508
1.257369	-0.242356	0.250240	0.000225	0.310507
1.148916	-0.228383	0.255245	0.000246	0.310480
1.290109	-0.321925	0.260250	0.000219	0.310164
1.247694	-0.313100	0.265254	0.000227	0.310169
1.328152	-0.350269	0.270259	0.000212	0.310064
1.225123	-0.379727	0.275264	0.000231	0.309840
1.485711	-0.425391	0.280269	0.000183	0.309848
0.986153	-0.382525	0.285274	0.000276	0.309625
1.361224	-0.473842	0.290278	0.000206	0.309517
1.328200	-0.476059	0.295283	0.000212	0.309478
1.187045	-0.503220	0.300288	0.000238	0.309232
1.534004	-0.566199	0.305293	0.000173	0.309232
1.045476	-0.534801	0.310298	0.000264	0.308964
0.849412	-0.512226	0.315302	0.000301	0.308903
1.024429	-0.570886	0.320307	0.000268	0.308778
1.104298	-0.626662	0.325312	0.000253	0.308585
1.376518	-0.687191	0.330317	0.000203	0.308533
0.835603	-0.647249	0.335322	0.000303	0.308260
1.023704	-0.680676	0.340326	0.000268	0.308263
1.245392	-0.781938	0.345331	0.000227	0.307977
0.915470	-0.724484	0.350336	0.000288	0.307966
1.059120	-0.812641	0.355341	0.000261	0.307675
0.676728	-0.749344	0.360346	0.000332	0.307646
0.942819	-0.853345	0.365350	0.000283	0.307384
0.796062	-0.840652	0.370355	0.000310	0.307319
1.091265	-0.953666	0.375360	0.000255	0.307039
1.118430	-0.968742	0.380365	0.000250	0.306992
0.248088	-0.866388	0.385370	0.000412	0.306729
0.610840	-0.935203	0.390374	0.000345	0.306716
0.700832	-1.018612	0.395379	0.000328	0.306400
0.436415	-0.978941	0.400384	0.000377	0.306360
0.252906	-1.003086	0.405389	0.000411	0.306089
0.133770	-0.990812	0.410394	0.000433	0.306045
0.433932	-1.106045	0.415398	0.000377	0.305758
0.270442	-1.092059	0.420403	0.000408	0.305684
0.217425	-1.123020	0.425408	0.000417	0.305492
0.473933	-1.202520	0.430413	0.000370	0.305337
0.185033	-1.188849	0.435418	0.000423	0.305153
0.365640	-1.270598	0.440422	0.000390	0.304921
0.287353	-1.275217	0.445427	0.000404	0.304832
0.350920	-1.357260	0.450432	0.000392	0.304498
0.294042	-1.366769	0.455437	0.000403	0.304404
0.105515	-1.372108	0.460442	0.000438	0.304216
0.125676	-1.425536	0.465446	0.000434	0.303979
0.140211	-1.454782	0.470451	0.000431	0.303853
0.043302	-1.498109	0.475456	0.000449	0.303563
0.320682	-1.578815	0.480461	0.000398	0.303419
-0.166201	-1.527112	0.485466	0.000488	0.303244
0.111259	-1.632708	0.490470	0.000437	0.302980
0.170711	-1.676658	0.495475	0.000426	0.302822
-0.214614	-1.649354	0.500480	0.000497	0.302619
-0.160580	-1.713782	0.505485	0.000487	0.302358
-0.331175	-1.714795	0.510490	0.000519	0.302205
-0.442810	-1.740592	0.515494	0.000540	0.301984
-1.120370	-1.661167	0.520499	0.000666	0.301775
-1.467476	-1.621214	0.525504	0.000730	0.301665
-1.050686	-1.756866	0.530509	0.000653	0.301377
-1.218759	-1.765935	0.535514	0.000684	0.301187
-1.877258	-1.671924	0.540518	0.000806	0.301064
-2.164602	-1.681694	0.545523	0.000860	0.300767
-2.092647	-1.712830	0.550528	0.000846	0.300680
-2.661057	-1.642806	0.555533	0.000952	0.300520
-2.947310	-1.631328	0.560538	0.001005	0.300325
-2.874536	-1.677274	0.565542	0.000992	0.300168
-2.919004	-1.722139	0.570547	0.001000	0.299913
-3.466170	-1.640412	0.575552	0.001102	0.299828
-3.334320	-1.729156	0.580557	0.001077	0.299515
-3.603136	-1.695541	0.585562	0.001127	0.299442
-3.319344	-1.791255	0.590566	0.001074	0.299229
-4.015025	-1.701093	0.595571	0.001204	0.299054
-3.971894	-1.743617	0.600576	0.001196	0.298886
-3.575648	-1.862950	0.605581	0.001122	0.298657
-4.249551	-1.759880	0.610586	0.001247	0.298563
-4.307688	-1.813958	0.615590	0.001258	0.298250
-4.324035	-1.825956	0.620595	0.001261	0.298178
-4.781397	-1.787969	0.625600	0.001346	0.297959
-5.009011	-1.776509	0.630605	0.001388	0.297814
-5.110266	-1.798282	0.635610	0.001407	0.297619
-5.001825	-1.856894	0.640614	0.001387	0.297430
-5.407056	-1.806656	0.645619	0.001462	0.297317
-5.881472	-1.776184	0.650624	0.001551	0.297046
-5.686486	-1.821401	0.655629	0.001514	0.296998
-6.077803	-1.807532	0.660634	0.001587	0.296719
-6.266061	-1.777326	0.665638	0.001622	0.296700
-6.437590	-1.812913	0.670643	0.001654	0.296375
-6.320142	-1.841962	0.675648	0.001632	0.296337
-6.846808	-1.801267	0.680653	0.001730	0.296069
-7.259754	-1.734190	0.685658	0.001807	0.296030
-7.482655	-1.750023	0.690662	0.001848	0.295755
-7.422906	-1.764800	0.695667	0.001837	0.295736
-7.680120	-1.767950	0.700672	0.001885	0.295492
-7.585802	-1.784708	0.705677	0.001867	0.295494
-7.675614	-1.838392	0.710682	0.001884	0.295151
-7.926572	-1.793090	0.715686	0.001931	0.295150
-8.060738	-1.831777	0.720691	0.001956	0.294841
-8.308956	-1.788984	0.725696	0.002002	0.294830
-8.499506	-1.816706	0.730701	0.002037	0.294524
-9.164875	-1.698580	0.735706	0.002161	0.294511
-8.904408	-1.793798	0.740710	0.002112	0.294276
-9.557895	-1.683276	0.745715	0.002234	0.294235
-9.538260	-1.730590	0.750720	0.002230	0.294020
-9.320904	-1.797421	0.755725	0.002190	0.293886
-9.675407	-1.758674	0.760730	0.002256	0.293760
-10.397997	-1.663632	0.765734	0.002390	0.293581
-9.883258	-1.765750	0.770739	0.002294	0.293539
-9.907779	-1.820678	0.775744	0.002299	0.293247
-10.092340	-1.784036	0.780749	0.002333	0.293262
-10.686522	-1.733089	0.785754	0.002444	0.292981
-10.539954	-1.764172	0.790758	0.002416	0.292959
-10.357652	-1.841701	0.795763	0.002382	0.292740
-11.078342	-1.733950	0.800768	0.002516	0.292626
-11.209313	-1.732895	0.805773	0.002541	0.292513
-11.752529	-1.673873	0.810778	0.002642	0.292317
-11.353490	-1.747139	0.815782	0.002567	0.292314
-11.323616	-1.819429	0.820787	0.002562	0.291983
-11.249206	-1.835110	0.825792	0.002548	0.291973
-11.508631	-1.829284	0.830797	0.002596	0.291768
-12.119868	-1.733703	0.835802	0.002710	0.291691
-12.324033	-1.722689	0.840806	0.002748	0.291562
-12.211981	-1.781842	0.845811	0.002727	0.291370
-12.542750	-1.724020	0.850816	0.002788	0.291359
-12.416221	-1.806302	0.855821	0.002765	0.291064
-12.529498	-1.787824	0.860826	0.002786	0.291054
-12.753775	-1.790541	0.865830	0.002828	0.290838
-13.477823	-1.677513	0.870835	0.002962	0.290746
-13.342501	-1.714104	0.875840	0.002937	0.290686
-13.177340	-1.782039	0.880845	0.002906	0.290498
-13.644713	-1.698390	0.885850	0.002993	0.290492
-13.901380	-1.702219	0.890854	0.003041	0.290240
-13.691725	-1.757975	0.895859	0.003002	0.290153
-13.853164	-1.747776	0.900864	0.003032	0.290057
-13.704256	-1.820686	0.905869	0.003004	0.289829
-14.023359	-1.763079	0.910874	0.003063	0.289827
-14.063340	-1.813670	0.915878	0.003071	0.289539
-14.638109	-1.715905	0.920883	0.003178	0.289505
-14.389140	-1.787613	0.925888	0.003131	0.289373
-14.280467	-1.839345	0.930893	0.003111	0.289214
-14.392968	-1.827318	0.935898	0.003132	0.289172
-14.896934	-1.795884	0.940902	0.003226	0.288871
-14.641344	-1.843013	0.945907	0.003178	0.288868
-14.964652	-1.830439	0.950912	0.003238	0.288636
-15.105861	-1.819786	0.955917	0.003264	0.288561
-14.912539	-1.877971	0.960922	0.003228	0.288446
-15.477592	-1.816457	0.965926	0.003334	0.288240
-15.926621	-1.734309	0.970931	0.003417	0.288242
-15.854706	-1.798595	0.975936	0.003404	0.287986
-15.677478	-1.835748	0.980941	0.003371	0.287961
-16.349958	-1.742517	0.985946	0.003496	0.287815
-16.883836	-1.684543	0.990950	0.003595	0.287619
-16.413466	-1.771022	0.995955	0.003507	0.287615
-16.652498	-1.777722	1.000960	0.003552	0.287362
-16.896510	-1.746364	1.005965	0.003597	0.287297
-16.804862	-1.776963	1.010970	0.003580	0.287227
-16.967029	-1.798427	1.015974	0.003610	0.286971
-17.143206	-1.765523	1.020979	0.003643	0.286975
-17.373483	-1.762367	1.025984	0.003686	0.286780
-17.555751	-1.744496	1.030989	0.003720	0.286704
-17.832394	-1.696025	1.035994	0.003771	0.286695
-18.299511	-1.675725	1.040998	0.003858	0.286369
-18.116698	-1.710381	1.046003	0.003824	0.286362
-17.984849	-1.754008	1.051008	0.003799	0.286263
-18.291674	-1.740598	1.056013	0.003856	0.286049
-18.274922	-1.744596	1.061018	0.003853	0.286044
-18.143856	-1.809619	1.066022	0.003829	0.285836
-18.557007	-1.756843	1.071027	0.003906	0.285723
-19.045458	-1.666922	1.076032	0.003996	0.285729
-18.765631	-1.764045	1.081037	0.003944	0.285495
-18.909667	-1.740937	1.086042	0.003971	0.285480
-18.858925	-1.777964	1.091046	0.003962	0.285339
-19.137294	-1.767635	1.096051	0.004013	0.285135
-19.211169	-1.754688	1.101056	0.004027	0.285133
-19.424339	-1.764576	1.106061	0.004067	0.284886
-19.854131	-1.701189	1.111066	0.004147	0.284811
-19.725346	-1.730112	1.116070	0.004123	0.284784
-20.039017	-1.729415	1.121075	0.004181	0.284498
-20.084721	-1.724027	1.126080	0.004189	0.284483
-19.781996	-1.800656	1.131085	0.004133	0.284374
-20.505926	-1.702584	1.136090	0.004268	0.284203
-20.249426	-1.749809	1.141094	0.004220	0.284200
-20.857779	-1.686496	1.146099	0.004333	0.283960
-20.907048	-1.695629	1.151104	0.004342	0.283868
-20.545266	-1.764414	1.156109	0.004275	0.283853
-21.006200	-1.740463	1.161114	0.004360	0.283548
-20.551926	-1.822308	1.166118	0.004276	0.283552
-20.731532	-1.818179	1.171123	0.004309	0.283406
-21.426415	-1.727500	1.176128	0.004439	0.283225
-20.968884	-1.809595	1.181133	0.004353	0.283230
-21.193168	-1.821746	1.186138	0.004395	0.282960
-21.392112	-1.790448	1.191142	0.004432	0.282935
-21.523431	-1.789104	1.196147	0.004456	0.282820
-21.932304	-1.757391	1.201152	0.004532	0.282603
-21.712174	-1.797065	1.206157	0.004491	0.282605
-22.263728	-1.743267	1.211162	0.004594	0.282367
-22.206747	-1.768375	1.216166	0.004583	0.282291
-22.221763	-1.771467	1.221171	0.004586	0.282262
-23.095478	-1.668929	1.226176	0.004749	0.281973
-22.522340	-1.773656	1.231181	0.004642	0.281971
-22.586099	-1.784206	1.236186	0.004654	0.281857
-22.861555	-1.769645	1.241190	0.004705	0.281675
-22.778895	-1.784721	1.246195	0.004690	0.281675
-22.977910	-1.800629	1.251200	0.004727	0.281408
-23.179703	-1.776868	1.256205	0.004764	0.281342
-23.373640	-1.752166	1.261210	0.004800	0.281288
-23.618382	-1.755395	1.266214	0.004846	0.281042
-23.740780	-1.731959	1.271219	0.004868	0.281049
-23.664685	-1.778092	1.276224	0.004854	0.280882
-24.017724	-1.744331	1.281229	0.004920	0.280726
-24.008261	-1.748217	1.286234	0.004918	0.280715
-24.142051	-1.759775	1.291238	0.004943	0.280530
-24.443512	-1.712674	1.296243	0.004999	0.280491
-24.191266	-1.768113	1.301248	0.004952	0.280442
-24.394784	-1.786922	1.306253	0.004990	0.280154
-24.852655	-1.706170	1.311258	0.005075	0.280141
-25.156371	-1.675378	1.316262	0.005131	0.280015
-24.948521	-1.748756	1.321267	0.005093	0.279831
-25.210179	-1.702050	1.326272	0.005141	0.279827
-25.055774	-1.771803	1.331277	0.005112	0.279612
-25.404285	-1.729036	1.336282	0.005177	0.279505
-25.373368	-1.736117	1.341286	0.005171	0.279498
-25.699961	-1.730087	1.346291	0.005232	0.279222
-25.803067	-1.713217	1.351296	0.005251	0.279213
-25.811636	-1.730101	1.356301	0.005253	0.279117
-26.435336	-1.662545	1.361306	0.005369	0.278880
-26.000426	-1.743004	1.366310	0.005288	0.278873
-25.589131	-1.850843	1.371315	0.005211	0.278702
-26.463313	-1.719655	1.376320	0.005374	0.278558
-26.104475	-1.783796	1.381325	0.005307	0.278564
-26.374456	-1.797312	1.386330	0.005357	0.278238
-26.609638	-1.755331	1.391334	0.005401	0.278235
-26.700794	-1.757964	1.396339	0.005418	0.278135
-26.884719	-1.760777	1.401344	0.005452	0.277947
-26.674113	-1.796202	1.406349	0.005413	0.277962
-27.218057	-1.747993	1.411354	0.005514	0.277698
-27.497034	-1.713808	1.416358	0.005566	0.277612
-27.402571	-1.732821	1.421363	0.005548	0.277603
-27.716483	-1.734407	1.426368	0.005607	0.277297
-27.783976	-1.720191	1.431373	0.005619	0.277307
-28.185065	-1.663157	1.436378	0.005694	0.277225
-28.177004	-1.711976	1.441382	0.005692	0.276978
-27.990575	-1.745114	1.446387	0.005657	0.276982
-28.426606	-1.697270	1.451392	0.005738	0.276818
-28.426918	-1.721146	1.456397	0.005739	0.276693
-28.684226	-1.674719	1.461402	0.005786	0.276691
-28.507496	-1.758664	1.466406	0.005753	0.276420
-28.521093	-1.768515	1.471411	0.005756	0.276356
-28.870178	-1.715344	1.476416	0.005821	0.276302
-29.473851	-1.651262	1.481421	0.005933	0.276063
-29.155498	-1.710946	1.486426	0.005874	0.276054
-29.117476	-1.740172	1.491430	0.005867	0.275937
-29.413426	-1.725879	1.496435	0.005922	0.275730
-29.545028	-1.703662	1.501440	0.005946	0.275722
-29.158643	-1.803332	1.506445	0.005874	0.275567
-29.723590	-1.717849	1.511450	0.005979	0.275477
-29.873829	-1.691086	1.516454	0.006007	0.275475
-29.682699	-1.789181	1.521459	0.005972	0.275142
-29.883668	-1.753771	1.526464	0.006009	0.275136
-29.833448	-1.787539	1.531469	0.006000	0.275007
-30.081168	-1.778423	1.536474	0.006046	0.274818
-30.273063	-1.741909	1.541478	0.006081	0.274827
-30.746094	-1.708836	1.546483	0.006169	0.274548
-30.702608	-1.727279	1.551488	0.006161	0.274493
-30.219666	-1.825831	1.556493	0.006071	0.274436
-30.920468	-1.743411	1.561498	0.006202	0.274199
-30.863796	-1.752977	1.566502	0.006191	0.274203
-30.652639	-1.830107	1.571507	0.006152	0.273999
-31.263835	-1.743972	1.576512	0.006265	0.273867
-31.396485	-1.721980	1.581517	0.006290	0.273856
-31.509580	-1.757228	1.586522	0.006311	0.273561
-31.278104	-1.799279	1.591526	0.006268	0.273562
-31.387758	-1.808898	1.596531	0.006288	0.273406
-32.230015	-1.686084	1.601536	0.006445	0.273245
-31.735161	-1.774940	1.606541	0.006353	0.273252
-32.070297	-1.762189	1.611546	0.006415	0.272996
-32.527269	-1.685890	1.616550	0.006500	0.272961
-32.338519	-1.730952	1.621555	0.006465	0.272904
-32.621680	-1.734417	1.626560	0.006517	0.272612
-32.633192	-1.730180	1.631565	0.006520	0.272624
-32.792784	-1.731382	1.636570	0.006549	0.272464
-33.022189	-1.717329	1.641574	0.006592	0.272317
-33.030567	-1.715870	1.646579	0.006593	0.272317
-33.237682	-1.732174	1.651584	0.006632	0.272030
-32.860128	-1.808752	1.656589	0.006562	0.271989
-33.296521	-1.743563	1.661594	0.006643	0.271913
-33.806702	-1.691492	1.666598	0.006738	0.271697
-33.428133	-1.760531	1.671603	0.006667	0.271696
-33.539522	-1.779689	1.676608	0.006688	0.271486
-34.201698	-1.681295	1.681613	0.006811	0.271369
-34.052837	-1.710613	1.686618	0.006783	0.271357
-33.782824	-1.812280	1.691622	0.006733	0.271077
-34.157339	-1.748450	1.696627	0.006803	0.271055
-34.892118	-1.632809	1.701632	0.006939	0.270959
-34.521790	-1.740784	1.706637	0.006870	0.270742
-34.347953	-1.774454	1.711642	0.006838	0.270731
-34.878239	-1.709919	1.716646	0.006936	0.270561
-34.910354	-1.719206	1.721651	0.006942	0.270480
-34.577938	-1.785050	1.726656	0.006880	0.270452
-34.891730	-1.787272	1.731661	0.006939	0.270134
-35.324007	-1.709862	1.736666	0.007019	0.270128
-35.287665	-1.743800	1.741670	0.007012	0.269982
-35.642732	-1.708688	1.746675	0.007078	0.269824
-35.589385	-1.720655	1.751680	0.007068	0.269812
-35.720348	-1.742719	1.756685	0.007093	0.269566
-35.794466	-1.744332	1.761690	0.007107	0.269486
-35.815824	-1.752691	1.766694	0.007110	0.269420
-35.963025	-1.766609	1.771699	0.007138	0.269202
-36.191079	-1.725130	1.776704	0.007180	0.269202
-36.207283	-1.759350	1.781709	0.007183	0.269002
-36.586776	-1.716143	1.786714	0.007254	0.268864
-36.513112	-1.729892	1.791718	0.007240	0.268862
-36.397491	-1.807750	1.796723	0.007218	0.268556
-37.031295	-1.693962	1.801728	0.007336	0.268549
-36.922987	-1.735238	1.806733	0.007316	0.268432
-37.021288	-1.755146	1.811738	0.007334	0.268229
-37.391052	-1.686419	1.816742	0.007403	0.268237
-37.687406	-1.670789	1.821747	0.007458	0.268031
-37.581966	-1.706418	1.826752	0.007439	0.267942
-37.634059	-1.698420	1.831757	0.007448	0.267935
-38.162803	-1.662917	1.836762	0.007547	0.267607
-37.972345	-1.696019	1.841766	0.007511	0.267615
-38.063504	-1.696139	1.846771	0.007528	0.267525
-39.183487	-1.531089	1.851776	0.007736	0.267316
-38.632097	-1.630891	1.856781	0.007634	0.267319
-38.481787	-1.683190	1.861786	0.007606	0.267184
-38.869600	-1.650577	1.866790	0.007678	0.266979
-38.925414	-1.638622	1.871795	0.007688	0.266989
-39.054290	-1.650448	1.876800	0.007712	0.266798
-38.899203	-1.697638	1.881805	0.007683	0.266696
-39.252481	-1.634850	1.886810	0.007749	0.266688
-39.301748	-1.681977	1.891814	0.007758	0.266383
-39.535514	-1.642113	1.896819	0.007801	0.266369
-39.697481	-1.623235	1.901824	0.007831	0.266312
-39.440783	-1.717538	1.906829	0.007784	0.266053
-39.739572	-1.663162	1.911834	0.007839	0.266054
-40.032424	-1.639315	1.916838	0.007894	0.265894
-40.384722	-1.603660	1.921843	0.007959	0.265740
-40.115699	-1.654633	1.926848	0.007909	0.265729
-39.871280	-1.730675	1.931853	0.007864	0.265557
-40.605153	-1.611774	1.936858	0.008000	0.265478
-40.490262	-1.636289	1.941862	0.007979	0.265458
-40.484713	-1.695632	1.946867	0.007978	0.265140
-40.724329	-1.653436	1.951872	0.008022	0.265133
-40.705314	-1.678674	1.956877	0.008018	0.265014
-41.250003	-1.615981	1.961882	0.008120	0.264816
-41.243270	-1.616664	1.966886	0.008118	0.264819
-41.483934	-1.608273	1.971891	0.008163	0.264626
-41.837773	-1.568379	1.976896	0.008229	0.264492
-41.437977	-1.639123	1.981901	0.008155	0.264503
-41.734802	-1.630870	1.986906	0.008210	0.264253
-41.929002	-1.604160	1.991910	0.008246	0.264206
-41.271879	-1.734949	1.996915	0.008123	0.264145
-41.847811	-1.682490	2.001920	0.008231	0.263858

-42.047203	-1.684097	2.011917	0.008268	0.263651
-42.364375	-1.648712	2.021914	0.008327	0.263529
-42.643425	-1.650933	2.031910	0.008378	0.263238
-42.951148	-1.596651	2.041907	0.008436	0.263230
-42.941009	-1.650004	2.051904	0.008434	0.262947
-42.954739	-1.649722	2.061901	0.008436	0.262935
-43.013222	-1.671540	2.071898	0.008447	0.262757
-42.877954	-1.725949	2.081894	0.008421	0.262593
-42.954270	-1.711594	2.091891	0.008436	0.262597
-43.326963	-1.643976	2.101888	0.008505	0.262596
-43.471313	-1.666607	2.111885	0.008532	0.262327
-43.699742	-1.631237	2.121882	0.008574	0.262294
-43.401353	-1.686850	2.131878	0.008518	0.262287
-43.424653	-1.682419	2.141875	0.008522	0.262289
-43.640546	-1.642680	2.151872	0.008563	0.262292
-43.312893	-1.704628	2.161869	0.008501	0.262280
-43.988736	-1.578346	2.171866	0.008627	0.262299
-43.202545	-1.724076	2.181862	0.008481	0.262285
-43.514574	-1.666668	2.191859	0.008539	0.262289
-43.360069	-1.691688	2.201856	0.008510	0.262307
-43.353687	-1.638567	2.211853	0.008508	0.262607
-43.801370	-1.554346	2.221850	0.008592	0.262623
-43.379711	-1.632282	2.231846	0.008513	0.262617
-43.600811	-1.592506	2.241843	0.008554	0.262615
-43.322017	-1.595685	2.251840	0.008502	0.262878
-43.417167	-1.563010	2.261837	0.008520	0.262963
-43.163745	-1.611155	2.271834	0.008472	0.262952
-42.973422	-1.611542	2.281830	0.008437	0.263142
-42.991283	-1.588994	2.291827	0.008440	0.263248
-42.819424	-1.620055	2.301824	0.008408	0.263250
-42.699279	-1.586209	2.311821	0.008385	0.263557
-42.483623	-1.623833	2.321818	0.008345	0.263567
-42.266632	-1.636070	2.331814	0.008304	0.263717
-42.353452	-1.590520	2.341811	0.008320	0.263881
-41.945325	-1.654562	2.351808	0.008244	0.263938
-41.829504	-1.625685	2.361805	0.008223	0.264212
-41.424724	-1.702062	2.371802	0.008147	0.264198
-41.341298	-1.668156	2.381798	0.008132	0.264467
-41.637945	-1.609739	2.391795	0.008187	0.264492
-41.404517	-1.596799	2.401792	0.008143	0.264796
-41.693003	-1.531691	2.411789	0.008197	0.264866
-41.271535	-1.555287	2.421786	0.008118	0.265157
-41.321639	-1.520243	2.431782	0.008127	0.265299
-40.893011	-1.562256	2.441779	0.008047	0.265496
-40.409289	-1.617238	2.451776	0.007957	0.265676
-40.593126	-1.570138	2.461773	0.007991	0.265752
-39.962802	-1.628708	2.471770	0.007874	0.266058
-40.129569	-1.577709	2.481766	0.007905	0.266171
-39.870764	-1.586414	2.491763	0.007856	0.266380
-39.366489	-1.636009	2.501760	0.007762	0.266610
-39.429357	-1.603981	2.511757	0.007774	0.266722
-39.075288	-1.619326	2.521754	0.007708	0.266989
-38.984545	-1.607168	2.531750	0.007691	0.267145
-38.363866	-1.690439	2.541747	0.007575	0.267306
-38.128732	-1.687009	2.551744	0.007531	0.267557
-38.096472	-1.673539	2.561741	0.007525	0.267663
-37.719830	-1.687011	2.571738	0.007455	0.267961
-37.477653	-1.705742	2.581734	0.007410	0.268098
-37.376607	-1.697563	2.591731	0.007391	0.268242
-37.038239	-1.705113	2.601728	0.007328	0.268534
-37.266386	-1.639661	2.611725	0.007370	0.268664
-37.088500	-1.629633	2.621722	0.007337	0.268893
-36.774752	-1.636731	2.631718	0.007278	0.269163
-36.730998	-1.613108	2.641715	0.007270	0.269333
-36.692943	-1.585666	2.651712	0.007263	0.269519
-36.324565	-1.593298	2.661709	0.007194	0.269838
-35.963815	-1.624725	2.671706	0.007127	0.270022
-35.631943	-1.651886	2.681702	0.007065	0.270201
-35.639332	-1.593264	2.691699	0.007066	0.270508
-35.844422	-1.516491	2.701696	0.007104	0.270720
-35.592303	-1.524282	2.711693	0.007057	0.270924
-34.957506	-1.603502	2.721690	0.006939	0.271118
-34.599489	-1.620735	2.731686	0.006872	0.271375
-34.082390	-1.669163	2.741683	0.006775	0.271619
-34.500365	-1.553095	2.751680	0.006853	0.271833
-33.970867	-1.616324	2.761677	0.006754	0.272009
-33.623695	-1.620714	2.771674	0.006690	0.272323
-33.161310	-1.669252	2.781670	0.006603	0.272512
-33.433870	-1.578895	2.791667	0.006654	0.272730
-33.412421	-1.534198	2.801664	0.006650	0.272988
-33.127180	-1.531824	2.811661	0.006597	0.273276
-33.096454	-1.490402	2.821658	0.006591	0.273526
-32.705283	-1.519752	2.831654	0.006518	0.273748
-32.194456	-1.569468	2.841651	0.006423	0.273977
-31.690115	-1.613634	2.851648	0.006329	0.274229
-31.491135	-1.604430	2.861645	0.006291	0.274469
-31.178264	-1.623303	2.871642	0.006233	0.274670
-31.163895	-1.584781	2.881638	0.006230	0.274887
-30.541137	-1.647680	2.891635	0.006114	0.275153
-30.484586	-1.609748	2.901632	0.006103	0.275407
-30.133600	-1.639570	2.911629	0.006038	0.275587
-29.963960	-1.642081	2.921626	0.006006	0.275736
-29.770382	-1.616545	2.931622	0.005970	0.276055
-29.479752	-1.630684	2.941619	0.005916	0.276259
-29.492538	-1.585323	2.951616	0.005918	0.276485
-29.027211	-1.629320	2.961613	0.005831	0.276698
-28.671742	-1.639682	2.971610	0.005765	0.276983
-28.262788	-1.677785	2.981606	0.005689	0.277173
-28.167018	-1.655618	2.991603	0.005671	0.277380
-27.824977	-1.672427	3.001600	0.005607	0.277618
-27.383065	-1.698579	3.011597	0.005525	0.277901
-27.849287	-1.576872	3.021594	0.005611	0.278094
-27.388905	-1.618853	3.031590	0.005525	0.278312
-27.263077	-1.587965	3.041587	0.005502	0.278592
-26.842160	-1.616974	3.051584	0.005423	0.278839
-26.695750	-1.598254	3.061581	0.005396	0.279075
-27.083940	-1.480042	3.071578	0.005468	0.279323
-26.422465	-1.557235	3.081574	0.005345	0.279547
-26.075524	-1.561474	3.091571	0.005280	0.279852
-25.541372	-1.612588	3.101568	0.005181	0.280091
-25.550077	-1.565918	3.111565	0.005182	0.280324
-25.665985	-1.496879	3.121562	0.005203	0.280572
-25.005843	-1.583050	3.131558	0.005080	0.280748
-24.904418	-1.542588	3.141555	0.005061	0.281052
-25.013869	-1.476450	3.151552	0.005082	0.281291
-24.393088	-1.540303	3.161549	0.004966	0.281543
-24.061906	-1.559305	3.171546	0.004904	0.281756
-23.643956	-1.589510	3.181542	0.004826	0.281992
-23.264774	-1.603588	3.191539	0.004756	0.282274
-22.991233	-1.614195	3.201536	0.004704	0.282475
-22.694266	-1.628877	3.211533	0.004649	0.282677
-22.341053	-1.639311	3.221530	0.004583	0.282953
-22.033721	-1.649504	3.231526	0.004526	0.283187
-22.306919	-1.556716	3.241523	0.004577	0.283408
-21.313911	-1.704029	3.251520	0.004392	0.283578
-21.419195	-1.627329	3.261517	0.004411	0.283873
-21.245971	-1.611949	3.271514	0.004379	0.284112
-21.693181	-1.482862	3.281510	0.004462	0.284356
-21.099467	-1.547703	3.291507	0.004351	0.284576
-20.604258	-1.585163	3.301504	0.004259	0.284844
-20.261756	-1.597113	3.311501	0.004195	0.285100
-20.280332	-1.548143	3.321498	0.004198	0.285332
-20.068717	-1.540558	3.331494	0.004159	0.285566
-19.623014	-1.585626	3.341491	0.004076	0.285749
-19.023594	-1.637443	3.351488	0.003964	0.286039
-18.931343	-1.619578	3.361485	0.003947	0.286215
-18.677336	-1.625462	3.371482	0.003899	0.286420
-18.488809	-1.603393	3.381478	0.003864	0.286705
-17.857409	-1.673270	3.391475	0.003746	0.286932
-17.891011	-1.629536	3.401472	0.003752	0.287122
-17.155608	-1.728992	3.411469	0.003615	0.287296
-17.087366	-1.681934	3.421466	0.003602	0.287596
-16.894895	-1.680454	3.431462	0.003566	0.287780
-16.763868	-1.665066	3.441459	0.003542	0.287977
-16.319565	-1.692177	3.451456	0.003459	0.288248
-16.483526	-1.618546	3.461453	0.003489	0.288468
-15.951090	-1.680744	3.471450	0.003390	0.288642
-15.585432	-1.699936	3.481446	0.003322	0.288880
-15.818843	-1.599563	3.491443	0.003365	0.289171
-14.933602	-1.724372	3.501440	0.003200	0.289352
-14.928698	-1.695942	3.511437	0.003199	0.289499
-14.583912	-1.694235	3.521434	0.003135	0.289822
-14.031221	-1.762017	3.531430	0.003032	0.289985
-13.961934	-1.742849	3.541427	0.003019	0.290144
-13.575668	-1.746156	3.551424	0.002947	0.290479
-13.608422	-1.713174	3.561421	0.002953	0.290614
-13.463007	-1.709870	3.571418	0.002926	0.290762
-12.965079	-1.743005	3.581414	0.002833	0.291049
-13.014842	-1.693074	3.591411	0.002842	0.291252
-12.728342	-1.706499	3.601408	0.002789	0.291445
-12.237625	-1.746966	3.611405	0.002697	0.291687
-12.147105	-1.717212	3.621402	0.002680	0.291917
-11.977623	-1.711827	3.631398	0.002648	0.292097
-11.616989	-1.733707	3.641395	0.002581	0.292314
-11.275354	-1.738514	3.651392	0.002517	0.292598
-11.265145	-1.705237	3.661389	0.002515	0.292773
-10.751594	-1.758378	3.671386	0.002420	0.292972
-10.866386	-1.680346	3.681382	0.002441	0.293255
-10.766154	-1.655862	3.691379	0.002422	0.293466
-10.209610	-1.715364	3.701376	0.002318	0.293672
-10.120983	-1.688098	3.711373	0.002302	0.293886
-10.079322	-1.633117	3.721370	0.002294	0.294195
-9.410400	-1.718058	3.731366	0.002169	0.294375
-9.614112	-1.640812	3.741363	0.002207	0.294574
-9.089270	-1.682206	3.751360	0.002109	0.294839
-9.011590	-1.644899	3.761357	0.002094	0.295092
-9.115122	-1.577239	3.771354	0.002114	0.295332
-8.485371	-1.647911	3.781350	0.001996	0.295547
-8.963612	-1.519205	3.791347	0.002085	0.295753
-8.369705	-1.562567	3.801344	0.001974	0.296069
-7.791224	-1.623156	3.811341	0.001867	0.296287
-7.692652	-1.597759	3.821338	0.001848	0.296499
-7.633889	-1.560319	3.831334	0.001837	0.296735
-7.866741	-1.466023	3.841331	0.001880	0.296989
-7.133141	-1.534310	3.851328	0.001744	0.297306
-7.148956	-1.482490	3.861325	0.001746	0.297545
-7.013908	-1.452399	3.871322	0.001721	0.297811
-6.494851	-1.496590	3.881318	0.001624	0.298055
-6.383434	-1.468583	3.891315	0.001603	0.298290
-6.704517	-1.348005	3.901312	0.001663	0.298592
-6.946320	-1.240890	3.911309	0.001708	0.298899
-6.292725	-1.294929	3.921306	0.001586	0.299213
-5.817819	-1.329566	3.931302	0.001497	0.299463
-5.705060	-1.291418	3.941299	0.001476	0.299747
-4.959151	-1.369860	3.951296	0.001337	0.300023
-5.411667	-1.230254	3.961293	0.001421	0.300300
-5.574834	-1.137031	3.971290	0.001452	0.300607
-4.802201	-1.227828	3.981286	0.001308	0.300846
-4.776012	-1.169490	3.991283	0.001303	0.301150
-4.284097	-1.202025	4.001280	0.001211	0.301424
-4.386653	-1.119533	4.011277	0.001230	0.301731
-3.905459	-1.151386	4.021274	0.001140	0.301998
-3.889220	-1.089025	4.031270	0.001137	0.302311
-4.022550	-0.998865	4.041267	0.001162	0.302627
-3.502142	-1.024361	4.051264	0.001065	0.302958
-3.504325	-0.961847	4.061261	0.001065	0.303255
-3.585605	-0.875380	4.071258	0.001080	0.303597
-3.040470	-0.911231	4.081254	0.000978	0.303899
-2.786832	-0.885421	4.091251	0.000931	0.304242
-2.859797	-0.808308	4.101248	0.000944	0.304546
-3.105931	-0.688080	4.111245	0.000990	0.304905
-2.821824	-0.663710	4.121242	0.000937	0.305266
-2.244798	-0.701861	4.131238	0.000829	0.305582
-2.317237	-0.620497	4.141235	0.000843	0.305906
-2.747791	-0.464838	4.151232	0.000923	0.306272
-2.290978	-0.468871	4.161229	0.000837	0.306646
-1.823074	-0.475298	4.171226	0.000750	0.307017
-2.023810	-0.359129	4.181222	0.000787	0.307393
-1.869086	-0.304385	4.191219	0.000758	0.307783
-1.717478	-0.252981	4.201216	0.000730	0.308155
-1.682614	-0.177678	4.211213	0.000723	0.308538
-1.638314	-0.090746	4.221210	0.000715	0.308984
-1.273507	-0.076552	4.231206	0.000647	0.309361
-1.055294	-0.034554	4.241203	0.000606	0.309743
-1.158227	0.077788	4.251200	0.000625	0.310181
-1.017064	0.142626	4.261197	0.000598	0.310603
-0.517131	0.127771	4.271194	0.000505	0.310957
-0.570124	0.228485	4.281190	0.000515	0.311382
0.000000	0.226766	4.291187	0.000409	0.311855

-0.090715	0.526392	4.296192	0.000425	0.313166
0.436746	0.996311	4.301197	0.000327	0.315769
1.322059	1.695793	4.306202	0.000161	0.319687
2.756550	2.587274	4.311206	-0.000106	0.324859
4.421655	3.747358	4.316211	-0.000417	0.331307
5.702225	5.274903	4.321216	-0.000657	0.338905
8.534405	6.839703	4.326221	-0.001185	0.347666
12.276649	8.567644	4.331226	-0.001883	0.357539
15.656283	10.693456	4.336230	-0.002514	0.368452
19.983395	13.006237	4.341235	-0.003321	0.380415
25.306640	15.500192	4.346240	-0.004314	0.393343
31.617660	18.199910	4.351245	-0.005491	0.407223
40.849304	20.785585	4.356250	-0.007212	0.422064
53.599201	23.179959	4.361254	-0.009587	0.437866
67.297152	25.889292	4.366259	-0.012140	0.454656
76.795211	29.824658	4.371264	-0.013911	0.472268
87.272160	34.036182	4.376269	-0.015865	0.490573
98.626853	38.563458	4.381274	-0.017982	0.509555
107.206933	44.033995	4.386278	-0.019583	0.529056
115.254329	50.022813	4.391283	-0.021085	0.548967
123.621166	56.354658	4.396288	-0.022647	0.569189
132.656397	62.979692	4.401293	-0.024334	0.589720
144.413601	69.502012	4.406298	-0.026528	0.610463
156.860525	76.317198	4.411302	-0.028850	0.631463
163.891006	84.473105	4.416307	-0.030164	0.652597
167.567377	93.498242	4.421312	-0.030855	0.673638
170.938272	102.775053	4.426317	-0.031489	0.694446
173.710983	112.350611	4.431322	-0.032011	0.715034
176.416024	122.068097	4.436326	-0.032521	0.735296
180.187744	131.744454	4.441331	-0.033230	0.755296
184.238689	141.472221	4.446336	-0.033991	0.774963
190.846719	150.867978	4.451341	-0.035227	0.794360
201.716454	159.688385	4.456346	-0.037257	0.813604
204.845243	169.996415	4.461350	-0.037846	0.832601
207.349935	180.398300	4.466355	-0.038320	0.851144
209.034709	190.927881	4.471360	-0.038640	0.869262
211.515496	201.277006	4.476365	-0.039109	0.886943
214.014082	211.596821	4.481370	-0.039581	0.904234
216.003778	221.943039	4.486374	-0.039958	0.921100
218.006612	232.229602	4.491379	-0.040338	0.937574
220.378727	242.369772	4.496384	-0.040786	0.953638
222.441643	252.500171	4.501389	-0.041177	0.969339
224.459386	262.576535	4.506394	-0.041559	0.984698
226.728796	272.516381	4.511398	-0.041988	0.999686
228.929723	282.381838	4.516403	-0.042405	1.014329
231.116636	292.163998	4.521408	-0.042818	1.028642
233.167990	301.888940	4.526413	-0.043207	1.042646
235.746481	311.456575	4.531418	-0.043693	1.056372
238.200907	320.976515	4.536422	-0.044156	1.069828
240.939049	330.372420	4.541427	-0.044672	1.083016
243.206552	339.794512	4.546432	-0.045101	1.095971
245.222180	349.187666	4.551437	-0.045482	1.108679
247.165926	358.511531	4.556442	-0.045850	1.121138
248.913985	367.801660	4.561446	-0.046182	1.133372
250.615061	377.049208	4.566451	-0.046505	1.145412
251.890851	386.292028	4.571456	-0.046749	1.157229
253.295325	395.415507	4.576461	-0.047016	1.168806
254.662069	404.495267	4.581466	-0.047277	1.180208
255.345207	413.623754	4.586470	-0.047410	1.191418
256.284563	422.625477	4.591475	-0.047591	1.202423
257.175417	431.577391	4.596480	-0.047762	1.213260
258.099169	440.478880	4.601485	-0.047940	1.223947
258.656635	449.397125	4.606490	-0.048050	1.234489
259.456549	458.186108	4.611494	-0.048205	1.244839
260.017401	467.005319	4.616499	-0.048315	1.255091
260.682094	475.730050	4.621504	-0.048444	1.265173
261.260155	484.453036	4.626509	-0.048558	1.275157
261.664189	493.151045	4.631514	-0.048639	1.285001
262.342476	501.771629	4.636518	-0.048771	1.294737
262.961715	510.384090	4.641523	-0.048892	1.304379
263.208281	519.094214	4.646528	-0.048943	1.313988
263.726981	527.628651	4.651533	-0.049046	1.323386
264.319546	536.130109	4.656538	-0.049161	1.332696
264.803557	544.620443	4.661542	-0.049257	1.341909
265.545016	553.066706	4.666547	-0.049401	1.351059
266.055465	561.511124	4.671552	-0.049501	1.360103
266.694888	569.925601	4.676557	-0.049626	1.369079
267.234548	578.369768	4.681562	-0.049732	1.378010
267.353317	586.855772	4.686566	-0.049760	1.386853
267.571732	595.315429	4.691571	-0.049806	1.395631
268.273585	603.625492	4.696576	-0.049942	1.404282
268.814814	611.995827	4.701581	-0.050048	1.412915
269.086320	620.391871	4.706586	-0.050105	1.421475
269.257072	628.786258	4.711590	-0.050142	1.429966
269.748314	637.126886	4.716595	-0.050239	1.438406
270.689639	645.364021	4.721600	-0.050420	1.446768
271.523049	653.654694	4.726605	-0.050580	1.455116
272.020883	661.990443	4.731610	-0.050678	1.463406
272.339300	670.359431	4.736614	-0.050743	1.471653
272.821653	678.672472	4.741619	-0.050839	1.479826
273.252187	686.962304	4.746624	-0.050924	1.487923
273.789911	695.241398	4.751629	-0.051030	1.495983
274.009601	703.568743	4.756634	-0.051076	1.503995
274.329955	711.870721	4.761638	-0.051141	1.511957
274.756942	720.133685	4.766643	-0.051226	1.519856
274.967802	728.431647	4.771648	-0.051271	1.527714
274.999006	736.763372	4.776653	-0.051282	1.535536
275.474241	744.991618	4.781658	-0.051376	1.543289
275.589679	753.284063	4.786662	-0.051403	1.551009
275.810570	761.552687	4.791667	-0.051450	1.558684
276.256083	769.739777	4.796672	-0.051538	1.566280
276.693968	777.972888	4.801677	-0.051625	1.573880
276.889536	786.231054	4.806682	-0.051667	1.581431
276.809138	794.532066	4.811686	-0.051657	1.588944
277.522060	802.688360	4.816691	-0.051795	1.596406
277.910248	810.891346	4.821696	-0.051873	1.603829
277.964669	819.161617	4.826701	-0.051889	1.611229
278.590005	827.342014	4.831706	-0.052011	1.618597
278.956772	835.534777	4.836710	-0.052084	1.625906
279.092936	843.833905	4.841715	-0.052115	1.633243
279.732827	851.957427	4.846720	-0.052240	1.640464
279.939212	860.179031	4.851725	-0.052283	1.647678
280.037236	868.424387	4.856730	-0.052307	1.654867
280.415114	876.586425	4.861734	-0.052383	1.661990
280.896874	884.776847	4.866739	-0.052478	1.669122
281.390613	892.920293	4.871744	-0.052575	1.676185
281.622107	901.123820	4.876749	-0.052624	1.683233
282.061649	909.302611	4.881754	-0.052711	1.690259
282.380959	917.491461	4.886758	-0.052776	1.697248
282.668449	925.691891	4.891763	-0.052835	1.704214
282.756520	933.921640	4.896768	-0.052857	1.711150
283.212010	942.072471	4.901773	-0.052947	1.718040
283.396471	950.248059	4.906778	-0.052987	1.724888
283.483112	958.459712	4.911782	-0.053008	1.731725
283.974925	966.599688	4.916787	-0.053105	1.738529
284.350109	974.738054	4.921792	-0.053180	1.745290
284.489458	982.950491	4.926797	-0.053212	1.752055
284.909654	991.095096	4.931802	-0.053295	1.758774
285.193155	999.237810	4.936806	-0.053353	1.765449
285.354567	1007.464225	4.941811	-0.053389	1.772151
285.422606	1015.638737	4.946816	-0.053407	1.778774
285.876367	1023.759705	4.951821	-0.053497	1.785378
286.255991	1031.946699	4.956826	-0.053573	1.792001
286.451546	1040.096235	4.961830	-0.053615	1.798546
286.827310	1048.218506	4.966835	-0.053690	1.805069
287.248269	1056.347604	4.971840	-0.053774	1.811578
287.439517	1064.515050	4.976845	-0.053815	1.818067
288.009369	1072.611754	4.981850	-0.053926	1.824523
288.414360	1080.744446	4.986854	-0.054007	1.830964
288.822740	1088.897083	4.991859	-0.054088	1.837398
288.924253	1097.043597	4.996864	-0.054113	1.843768
289.499770	1105.161228	5.001869	-0.054225	1.850150
289.674922	1113.339064	5.006874	-0.054263	1.856510
289.713281	1121.520356	5.011878	-0.054276	1.862833
290.212974	1129.639576	5.016883	-0.054374	1.869143
290.649496	1137.738086	5.021888	-0.054461	1.875407
290.555073	1145.929450	5.026893	-0.054449	1.881659
290.965199	1154.032059	5.031898	-0.054530	1.887882
291.405385	1162.139518	5.036902	-0.054618	1.894092
291.910454	1170.249472	5.041907	-0.054717	1.900290
292.017231	1178.411679	5.046912	-0.054742	1.906462
292.394463	1186.541335	5.051917	-0.054818	1.912620
292.873486	1194.645426	5.056922	-0.054912	1.918750
292.718998	1202.811937	5.061926	-0.054889	1.924836
293.194103	1210.927700	5.066931	-0.054983	1.930936
293.629561	1219.030711	5.071936	-0.055069	1.937003
294.086852	1227.123930	5.076941	-0.055160	1.943046
294.434714	1235.268773	5.081946	-0.055230	1.949096
294.780675	1243.358148	5.086950	-0.055300	1.955086
295.145642	1251.458716	5.091955	-0.055373	1.961068
295.251084	1259.590778	5.096960	-0.055398	1.967026
295.595569	1267.712667	5.101965	-0.055467	1.972985
296.030611	1275.814909	5.106970	-0.055554	1.978921
296.027164	1283.956888	5.111974	-0.055558	1.984821
296.426010	1292.071323	5.116979	-0.055638	1.990726
296.680568	1300.182229	5.121984	-0.055691	1.996597
296.933124	1308.281189	5.126989	-0.055743	2.002441
297.025449	1316.425667	5.131994	-0.055766	2.008283
297.063175	1324.578200	5.136998	-0.055778	2.014109
297.363495	1332.691105	5.142003	-0.055839	2.019917
297.663205	1340.768490	5.147008	-0.055901	2.025683
298.028923	1348.871766	5.152013	-0.055974	2.031458
298.050608	1357.011334	5.157018	-0.055983	2.037206
298.255176	1365.070804	5.162022	-0.056027	2.042901
298.933356	1373.115961	5.167027	-0.056158	2.048619
299.302879	1381.209888	5.172032	-0.056233	2.054322
299.540168	1389.329470	5.177037	-0.056282	2.060015
299.778448	1397.435424	5.182042	-0.056332	2.065682
300.169272	1405.521473	5.187046	-0.056410	2.071335
300.678895	1413.617766	5.192051	-0.056510	2.076992
300.768501	1421.723406	5.197056	-0.056532	2.082598
300.849958	1429.866691	5.202061	-0.056553	2.088213
301.277247	1437.968642	5.207066	-0.056638	2.093820
301.310302	1446.078337	5.212070	-0.056649	2.099378
301.650002	1454.145122	5.217075	-0.056718	2.104922
302.102667	1462.242309	5.222080	-0.056807	2.110483
302.408724	1470.340134	5.227085	-0.056870	2.116015
302.744470	1478.413828	5.232090	-0.056937	2.121520
302.731073	1486.531917	5.237094	-0.056940	2.127006
303.167135	1494.604744	5.242099	-0.057027	2.132491
303.086022	1502.728121	5.247104	-0.057017	2.137946
303.485745	1510.779258	5.252109	-0.057097	2.143385
303.721538	1518.906956	5.257114	-0.057146	2.148846
303.887837	1526.994531	5.262118	-0.057182	2.154259
303.991668	1535.092757	5.267123	-0.057207	2.159660
304.427313	1543.120330	5.272128	-0.057293	2.165032
304.695993	1551.223186	5.277133	-0.057349	2.170424
304.996174	1559.315896	5.282138	-0.057410	2.175799
305.250362	1567.390120	5.287142	-0.057463	2.181145
305.916588	1575.437375	5.292147	-0.057592	2.186498
306.062159	1583.563832	5.297152	-0.057625	2.191841
306.209964	1591.658327	5.302157	-0.057657	2.197151
306.517004	1599.729848	5.307162	-0.057720	2.202447
306.712290	1607.814050	5.312166	-0.057762	2.207729
307.014438	1615.898339	5.317171	-0.057823	2.213008
307.281139	1623.968096	5.322176	-0.057878	2.218262
307.890271	1631.994918	5.327181	-0.057997	2.223506
308.029806	1640.131948	5.332186	-0.058028	2.228766
308.072705	1648.236070	5.337190	-0.058042	2.233985
308.135906	1656.355608	5.342195	-0.058059	2.239202
308.236575	1664.414219	5.347200	-0.058083	2.244372
308.603880	1672.475711	5.352205	-0.058156	2.249556
309.056664	1680.546582	5.357210	-0.058246	2.254741
309.494529	1688.590780	5.362214	-0.058333	2.259896
309.753452	1696.682301	5.367219	-0.058386	2.265053
310.044536	1704.768978	5.372224	-0.058446	2.270198
310.291826	1712.883029	5.377229	-0.058497	2.275345
310.599514	1720.941549	5.382234	-0.058560	2.280451
310.648524	1729.006483	5.387238	-0.058574	2.285526
310.870047	1737.102138	5.392243	-0.058621	2.290625
311.334351	1745.137521	5.397248	-0.058713	2.295695
311.447486	1753.227199	5.402253	-0.058739	2.300758
311.829545	1761.257368	5.407258	-0.058816	2.305796
311.866515	1769.386526	5.412262	-0.058828	2.310854
312.067279	1777.469984	5.417267	-0.058871	2.315887
312.276283	1785.519572	5.422272	-0.058915	2.320889
312.785592	1793.533656	5.427277	-0.059015	2.325884
313.012411	1801.635656	5.432282	-0.059063	2.330898
313.174214	1809.705219	5.437286	-0.059098	2.335876
313.529358	1817.768292	5.442291	-0.059169	2.340855
313.532617	1825.880392	5.447296	-0.059175	2.345825
313.964666	1833.924546	5.452301	-0.059261	2.350778
314.161728	1842.017886	5.457306	-0.059303	2.355731
314.487187	1850.036544	5.462310	-0.059369	2.360639
314.690112	1858.131419	5.467315	-0.059412	2.365572
314.888636	1866.203722	5.472320	-0.059454	2.370482
314.903884	1874.303703	5.477325	-0.059463	2.375383
314.941666	1882.402900	5.482330	-0.059475	2.380275
315.201207	1890.422277	5.487334	-0.059529	2.385127
315.792618	1898.459817	5.492339	-0.059644	2.390007
316.042512	1906.525918	5.497344	-0.059696	2.394866
316.498709	1914.557437	5.502349	-0.059786	2.399712
316.477214	1922.661075	5.507354	-0.059787	2.404552
316.858353	1930.707309	5.512358	-0.059864	2.409380
316.853341	1938.832248	5.517363	-0.059868	2.414215
317.058591	1946.876533	5.522368	-0.059912	2.419009
317.188098	1954.936721	5.527373	-0.059941	2.423797
317.673313	1963.008468	5.532378	-0.060037	2.428610
317.565675	1971.142926	5.537382	-0.060022	2.433404
317.726165	1979.198446	5.542387	-0.060057	2.438164
318.278136	1987.164363	5.547392	-0.060165	2.442891
318.105905	1995.280606	5.552397	-0.060139	2.447642
318.556651	2003.319680	5.557402	-0.060228	2.452386
318.776912	2011.371840	5.562406	-0.060274	2.457111
318.750574	2019.474490	5.567411	-0.060275	2.461837
318.869262	2027.534494	5.572416	-0.060302	2.466540
319.006164	2035.585272	5.577421	-0.060333	2.471231
319.217653	2043.643565	5.582426	-0.060378	2.475923
319.223321	2051.688613	5.587430	-0.060384	2.480582
319.960541	2059.669534	5.592435	-0.060526	2.485251
320.276052	2067.745821	5.597440	-0.060590	2.489934
320.449714	2075.825594	5.602445	-0.060628	2.494600
320.479846	2083.939536	5.607450	-0.060639	2.499265
320.610198	2091.982950	5.612454	-0.060669	2.503890
320.727896	2100.086349	5.617459	-0.060696	2.508539
320.750386	2108.145833	5.622464	-0.060705	2.513147
321.104987	2116.169299	5.627469	-0.060777	2.517751
321.453494	2124.189812	5.632474	-0.060847	2.522344
321.918070	2132.192361	5.637478	-0.060939	2.526927
321.872576	2140.304230	5.642483	-0.060936	2.531526
321.774906	2148.420152	5.647488	-0.060923	2.536115
322.404062	2156.392064	5.652493	-0.061045	2.540668
322.579148	2164.476656	5.657498	-0.061083	2.545243
322.741163	2172.545686	5.662502	-0.061119	2.549800
323.256840	2180.544128	5.667507	-0.061220	2.554334
323.132153	2188.662070	5.672512	-0.061202	2.558882
323.573015	2196.665844	5.677517	-0.061289	2.563398
323.823933	2204.746407	5.682522	-0.061341	2.567936
323.620579	2212.847261	5.687526	-0.061309	2.572444
323.790621	2220.913253	5.692531	-0.061346	2.576952
324.214401	2228.917318	5.697536	-0.061430	2.581435
324.156185	2237.003717	5.702541	-0.061425	2.585922
324.612560	2245.059010	5.707546	-0.061515	2.590420
324.946814	2253.176987	5.712550	-0.061582	2.594936
324.961302	2261.232140	5.717555	-0.061590	2.599387
324.911524	2269.242898	5.722560	-0.061586	2.603802
325.141750	2277.269617	5.727565	-0.061635	2.608238
325.638150	2285.296760	5.732570	-0.061732	2.612685
325.720799	2293.339151	5.737574	-0.061753	2.617103
325.775594	2301.412639	5.742579	-0.061769	2.621530
326.279612	2309.403911	5.747584	-0.061868	2.625935
326.161106	2317.514885	5.752589	-0.061851	2.630355
326.194925	2325.601051	5.757594	-0.061863	2.634765
326.317305	2333.616609	5.762598	-0.061891	2.639134
326.766226	2341.616076	5.767603	-0.061980	2.643510
326.945265	2349.656350	5.772608	-0.062018	2.647883
326.456626	2357.827838	5.777613	-0.061933	2.652275
327.059361	2365.811195	5.782618	-0.062050	2.656630
327.211720	2373.839631	5.787622	-0.062084	2.660973
327.563535	2381.873046	5.792627	-0.062155	2.665324
327.804972	2389.915321	5.797632	-0.062205	2.669666
328.009461	2397.997469	5.802637	-0.062248	2.674020
328.388516	2406.010408	5.807642	-0.062324	2.678340
328.596952	2414.042728	5.812646	-0.062368	2.682653
329.129090	2422.068582	5.817651	-0.062473	2.686977
329.005037	2430.177474	5.822656	-0.062455	2.691296
329.197394	2438.222810	5.827661	-0.062496	2.695594
329.535939	2446.252824	5.832666	-0.062564	2.699886
329.684567	2454.291725	5.837670	-0.062597	2.704164
329.840436	2462.364972	5.842675	-0.062632	2.708454
329.899633	2470.438571	5.847680	-0.062648	2.712731
330.175311	2478.451010	5.852685	-0.062705	2.716983
330.733171	2486.441078	5.857690	-0.062814	2.721234
330.785977	2494.514049	5.862694	-0.062829	2.725490
331.130651	2502.574227	5.867699	-0.062898	2.729752
331.194518	2510.630809	5.872704	-0.062916	2.733987
331.062607	2518.739388	5.877709	-0.062896	2.738230
331.480774	2526.745384	5.882714	-0.062980	2.742448
331.609203	2534.791853	5.887718	-0.063009	2.746662
331.904227	2542.883054	5.892723	-0.063069	2.750903
331.869661	2550.971448	5.897728	-0.063068	2.755116
332.348184	2558.918987	5.902733	-0.063162	2.759281
332.540657	2566.968555	5.907738	-0.063203	2.763474
332.774897	2574.993618	5.912742	-0.063252	2.767652
332.824691	2583.073790	5.917747	-0.063267	2.771840
332.945227	2591.115006	5.922752	-0.063295	2.776006
333.011280	2599.183246	5.927757	-0.063312	2.780176
333.501867	2607.149649	5.932762	-0.063409	2.784313
333.554466	2615.221925	5.937766	-0.063424	2.788473
333.904481	2623.275796	5.942771	-0.063494	2.792634
334.006477	2631.306906	5.947776	-0.063519	2.796762
334.117482	2639.353775	5.952781	-0.063545	2.800893
334.723497	2647.358103	5.957786	-0.063663	2.805026
334.650143	2655.443034	5.962790	-0.063655	2.809153
335.253142	2663.463299	5.967795	-0.063772	2.813282
335.790822	2671.470134	5.972800	-0.063877	2.817393
335.741946	2679.545035	5.977805	-0.063874	2.821498
336.047970	2687.599992	5.982810	-0.063936	2.825608
336.220495	2695.637877	5.987814	-0.063973	2.829696
336.644084	2703.681467	5.992819	-0.064058	2.833795
336.855865	2711.716149	5.997824	-0.064102	2.837872
336.982904	2719.755511	6.002829	-0.064131	2.841940
337.346921	2727.806022	6.007834	-0.064204	2.846021
337.276087	2735.874491	6.012838	-0.064197	2.850081
337.516084	2743.923998	6.017843	-0.064247	2.854143
337.747072	2751.957521	6.022848	-0.064295	2.858190
338.000852	2759.968831	6.027853	-0.064347	2.862222
338.241656	2768.042342	6.032858	-0.064398	2.866279
338.180447	2776.100369	6.037862	-0.064391	2.870305
338.437776	2784.130586	6.042867	-0.064445	2.874330
338.349738	2792.211766	6.047872	-0.064434	2.878355
338.695517	2800.173211	6.052877	-0.064503	2.882339
339.227453	2808.204742	6.057882	-0.064608	2.886362
338.822720	2816.340869	6.062886	-0.064538	2.890380
339.008050	2824.380465	6.067891	-0.064577	2.894377
338.669099	2832.479780	6.072896	-0.064520	2.898369
339.194202	2840.419778	6.077901	-0.064623	2.902325
339.430516	2848.466322	6.082906	-0.064672	2.906312
339.536037	2856.515786	6.087910	-0.064697	2.910287
340.144302	2864.543368	6.092915	-0.064815	2.914274
340.410558	2872.568079	6.097920	-0.064870	2.918235
340.747775	2880.550836	6.102925	-0.064938	2.922174
340.949685	2888.621274	6.107930	-0.064981	2.926143
340.841657	2896.694844	6.112934	-0.064966	2.930092
341.278936	2904.704583	6.117939	-0.065053	2.934034
341.679102	2912.726214	6.122944	-0.065133	2.937974
341.376774	2920.826227	6.127949	-0.065082	2.941909
340.807882	2928.977638	6.132954	-0.064981	2.945850
341.492643	2936.878822	6.137958	-0.065114	2.949731
342.010174	2944.879097	6.142963	-0.065216	2.953645
342.357285	2952.886926	6.147968	-0.065286	2.957549
342.629759	2960.923953	6.152973	-0.065342	2.961458
342.899294	2968.962388	6.157978	-0.065397	2.965363
343.142638	2976.991133	6.162982	-0.065448	2.969256
343.346973	2985.072308	6.167987	-0.065491	2.973167
343.645827	2993.095071	6.172992	-0.065552	2.977050
343.810707	3001.131216	6.177997	-0.065588	2.980927
343.968827	3009.190342	6.183002	-0.065623	2.984810
344.187945	3017.217075	6.188006	-0.065669	2.988675
344.562991	3025.297566	6.193011	-0.065744	2.992569
344.743077	3033.330691	6.198016	-0.065783	2.996426
345.133003	3041.313999	6.203021	-0.065861	3.000264
345.194941	3049.375367	6.208026	-0.065878	3.004118
345.272701	3057.414667	6.213030	-0.065898	3.007957
345.673046	3065.445146	6.218035	-0.065977	3.011803
345.718735	3073.515785	6.223040	-0.065991	3.015646
345.933856	3081.524279	6.228045	-0.066037	3.019462
345.814060	3089.621802	6.233050	-0.066020	3.023300
346.341015	3097.564571	6.238054	-0.066123	3.027091
346.778109	3105.641845	6.243059	-0.066210	3.030937
346.825785	3113.691184	6.248064	-0.066224	3.034745
346.981304	3121.692403	6.253069	-0.066258	3.038531
347.168860	3129.732135	6.258074	-0.066298	3.042332
346.989831	3137.814304	6.263078	-0.066270	3.046130
347.141909	3145.870667	6.268083	-0.066304	3.049928
347.455906	3153.863150	6.273088	-0.066368	3.053699
347.768197	3161.886495	6.278093	-0.066431	3.057479
347.820312	3169.954879	6.283098	-0.066446	3.061263
347.885807	3177.973174	6.288102	-0.066464	3.065020
348.041214	3186.036169	6.293107	-0.066498	3.068797
348.278622	3194.092048	6.298112	-0.066547	3.072570
348.496330	3202.109748	6.303117	-0.066593	3.076320
349.063155	3210.090811	6.308122	-0.066704	3.080065
349.123660	3218.090078	6.313126	-0.066721	3.083790
349.312301	3226.149153	6.318131	-0.066761	3.087544
349.411737	3234.230605	6.323136	-0.066785	3.091299
349.588143	3242.237283	6.328141	-0.066823	3.095019
349.581194	3250.287163	6.333146	-0.066827	3.098746
349.838641	3258.283449	6.338150	-0.066880	3.102455
349.992089	3266.360165	6.343155	-0.066914	3.106193
349.586924	3274.455045	6.348160	-0.066844	3.109909
349.554478	3282.476406	6.353165	-0.066843	3.113603
349.946221	3290.487000	6.358170	-0.066921	3.117308
350.034384	3298.495686	6.363174	-0.066943	3.120994
350.576060	3306.439176	6.368179	-0.067049	3.124666
350.868663	3314.466256	6.373184	-0.067109	3.128360
350.894361	3322.552136	6.378189	-0.067119	3.132065
351.145686	3330.621030	6.383194	-0.067171	3.135768
351.060473	3338.666074	6.388198	-0.067161	3.139441
351.131620	3346.723461	6.393203	-0.067179	3.143121
351.471558	3354.692446	6.398208	-0.067248	3.146770
351.734127	3362.737506	6.403213	-0.067302	3.150445
352.024913	3370.759782	6.408218	-0.067361	3.154107
352.344952	3378.762525	6.413222	-0.067426	3.157757
352.408519	3386.822621	6.418227	-0.067443	3.161417
352.712138	3394.823751	6.423232	-0.067505	3.165057
352.810769	3402.872949	6.428237	-0.067529	3.168705
353.037772	3410.922394	6.433242	-0.067577	3.172355
353.127017	3418.973914	6.438246	-0.067598	3.175996
353.253106	3427.022831	6.443251	-0.067627	3.179633
353.476921	3435.009848	6.448256	-0.067674	3.183242
353.489629	3443.072312	6.453261	-0.067682	3.186871
353.831001	3451.117750	6.458266	-0.067751	3.190503
354.079952	3459.109116	6.463270	-0.067802	3.194103
354.482401	3467.099717	6.468275	-0.067883	3.197705
354.654375	3475.167703	6.473280	-0.067920	3.201327
354.774494	3483.163351	6.478285	-0.067948	3.204911
355.149132	3491.233085	6.483290	-0.068023	3.208535
355.183765	3499.266275	6.488294	-0.068034	3.212124
355.469828	3507.327919	6.493299	-0.068093	3.215732
355.652449	3515.340604	6.498304	-0.068132	3.219310
355.740669	3523.362842	6.503309	-0.068154	3.222884
356.086729	3531.386464	6.508314	-0.068224	3.226465
356.281731	3539.454571	6.513318	-0.068265	3.230056
356.369956	3547.490429	6.518323	-0.068287	3.233624
356.568209	3555.498060	6.523328	-0.068329	3.237181
356.863825	3563.517449	6.528333	-0.068390	3.240742
356.871320	3571.519845	6.533338	-0.068396	3.244280
356.999797	3579.559981	6.538342	-0.068425	3.247836
357.164359	3587.619792	6.543347	-0.068461	3.251398
357.380585	3595.679462	6.548352	-0.068507	3.254959
357.722011	3603.649844	6.553357	-0.068576	3.258481
357.891390	3611.703251	6.558362	-0.068613	3.262029
357.916361	3619.734795	6.563366	-0.068623	3.265557
358.109864	3627.759468	6.568371	-0.068664	3.269086
358.237885	3635.795389	6.573376	-0.068693	3.272613
358.438581	3643.823371	6.578381	-0.068736	3.276135
358.713073	3651.845463	6.583386	-0.068792	3.279654
358.548483	3659.881515	6.588390	-0.068767	3.283158
358.580333	3667.968960	6.593395	-0.068778	3.286689
358.772207	3675.950195	6.598400	-0.068819	3.290175
359.002697	3683.953696	6.603405	-0.068867	3.293669
359.261640	3692.002010	6.608410	-0.068921	3.297180
359.444919	3700.043611	6.613414	-0.068960	3.300682
359.423569	3708.068461	6.618419	-0.068962	3.304164
359.692566	3716.066195	6.623424	-0.069017	3.307642
359.792872	3724.130954	6.628429	-0.069041	3.311139
360.024414	3732.163619	6.633434	-0.069089	3.314624
360.137339	3740.185864	6.638438	-0.069116	3.318095
360.454765	3748.201887	6.643443	-0.069180	3.321569
360.677803	3756.186366	6.648448	-0.069227	3.325021
360.668731	3764.251417	6.653453	-0.069230	3.328495
360.840334	3772.320445	6.658458	-0.069268	3.331975
361.016777	3780.346712	6.663462	-0.069306	3.335432
361.124334	3788.375862	6.668467	-0.069331	3.338885
361.476453	3796.352466	6.673472	-0.069402	3.342321
361.618805	3804.388007	6.678477	-0.069434	3.345770
361.992040	3812.432041	6.683482	-0.069509	3.349229
361.758445	3820.490353	6.688486	-0.069470	3.352667
362.211094	3828.517220	6.693491	-0.069560	3.356113
362.527496	3836.503726	6.698496	-0.069624	3.359534
362.245157	3844.551450	6.703501	-0.069577	3.362955
362.412809	3852.596705	6.708506	-0.069613	3.366388
362.531245	3860.609021	6.713510	-0.069641	3.369802
362.897945	3868.626402	6.718515	-0.069714	3.373224
362.832603	3876.697517	6.723520	-0.069708	3.376649
362.938740	3884.720792	6.728525	-0.069733	3.380057
363.235854	3892.716637	6.733530	-0.069793	3.383456
363.225733	3900.781707	6.738534	-0.069797	3.386871
363.545606	3908.809684	6.743539	-0.069861	3.390278
363.867505	3916.872337	6.748544	-0.069927	3.393696
363.760696	3924.874728	6.753549	-0.069912	3.397070
364.140960	3932.871771	6.758554	-0.069988	3.400456
364.358431	3940.829978	6.763558	-0.070034	3.403816
364.400652	3948.940879	6.768563	-0.070047	3.407231
364.544699	3956.963676	6.773568	-0.070079	3.410609
364.928909	3964.933369	6.778573	-0.070156	3.413970
365.212526	3972.990280	6.783578	-0.070214	3.417360
365.190196	3981.048197	6.788582	-0.070215	3.420737
365.351161	3989.020419	6.793587	-0.070251	3.424081
365.402525	3997.108969	6.798592	-0.070265	3.427466
365.735204	4005.115607	6.803597	-0.070333	3.430824
365.835336	4013.133110	6.808602	-0.070357	3.434175
365.910533	4021.171049	6.813606	-0.070376	3.437530
366.266418	4029.186932	6.818611	-0.070447	3.440882
366.323484	4037.165671	6.823616	-0.070463	3.444206
366.637822	4045.188062	6.828621	-0.070527	3.447553
366.841652	4053.308671	6.833626	-0.070570	3.450934
366.923034	4061.271279	6.838630	-0.070591	3.454242
367.249601	4069.287821	6.843635	-0.070657	3.457577
367.361839	4077.364417	6.848640	-0.070683	3.460926
367.509517	4085.330541	6.853645	-0.070716	3.464228
367.675694	4093.415404	6.858650	-0.070752	3.467577
368.022953	4101.448143	6.863654	-0.070822	3.470906
368.183219	4109.410758	6.868659	-0.070857	3.474197
368.478290	4117.436064	6.873664	-0.070918	3.477516
368.545143	4125.500407	6.878669	-0.070935	3.480839
368.686345	4133.483038	6.883674	-0.070967	3.484129
368.686780	4141.563559	6.888678	-0.070972	3.487451
368.811531	4149.620583	6.893683	-0.071001	3.490764
369.011236	4157.632165	6.898688	-0.071043	3.494057
369.145438	4165.653558	6.903693	-0.071074	3.497350
369.190943	4173.739176	6.908698	-0.071087	3.500663
369.386371	4181.655743	6.913702	-0.071129	3.503908
369.593768	4189.730103	6.918707	-0.071173	3.507215
369.816468	4197.758974	6.923712	-0.071220	3.510501
369.854375	4205.792355	6.928717	-0.071232	3.513780
370.040129	4213.815574	6.933722	-0.071272	3.517056
370.058473	4221.831811	6.938726	-0.071281	3.520321
370.388735	4229.818187	6.943731	-0.071347	3.523581
370.597045	4237.871532	6.948736	-0.071391	3.526861
370.912187	4245.881135	6.953741	-0.071455	3.530123
371.100172	4253.948152	6.958746	-0.071496	3.533402
370.920931	4262.000949	6.963750	-0.071468	3.536660
371.405319	4269.986978	6.968755	-0.071563	3.539909
371.463013	4277.980845	6.973760	-0.071579	3.543145
371.411534	4286.013580	6.978765	-0.071575	3.546391
371.988737	4294.045946	6.983770	-0.071688	3.549652
372.437492	4302.070194	6.988774	-0.071776	3.552903
372.426155	4310.146200	6.993779	-0.071780	3.556158
372.818683	4318.081942	6.998784	-0.071858	3.559366
373.046469	4326.072392	7.003789	-0.071906	3.562588
373.192500	4334.157149	7.008794	-0.071938	3.565843
373.236241	4342.185495	7.013798	-0.071952	3.569068
373.504547	4350.208210	7.018803	-0.072007	3.572295
373.557610	4358.252824	7.023808	-0.072022	3.575522
373.699873	4366.246625	7.028813	-0.072054	3.578728
374.197386	4374.277475	7.033818	-0.072152	3.581956
374.311043	4382.277839	7.038822	-0.072178	3.585158
374.316486	4390.319996	7.043827	-0.072185	3.588371
374.354849	4398.402946	7.048832	-0.072197	3.591598
374.377899	4406.414414	7.053837	-0.072207	3.594793
374.614851	4414.428323	7.058842	-0.072256	3.597992
374.679095	4422.436995	7.063846	-0.072273	3.601182
375.229944	4430.416535	7.068851	-0.072381	3.604371
375.545434	4438.454321	7.073856	-0.072445	3.607573
375.494234	4446.526783	7.078861	-0.072441	3.610776
375.700198	4454.531878	7.083866	-0.072485	3.613957
375.768385	4462.581654	7.088870	-0.072503	3.617149
375.865631	4470.615185	7.093875	-0.072526	3.620332
375.915646	4478.617376	7.098880	-0.072541	3.623498
375.935375	4486.657217	7.103885	-0.072550	3.626676
376.179109	4494.694468	7.108890	-0.072600	3.629857
376.301255	4502.672325	7.113894	-0.072628	3.633007
376.685492	4510.724151	7.118899	-0.072705	3.636192
376.790697	4518.714135	7.123904	-0.072730	3.639341
376.711915	4526.762977	7.128909	-0.072721	3.642506
377.300222	4534.759126	7.133914	-0.072835	3.645666
377.516997	4542.721767	7.138918	-0.072881	3.648799
377.583307	4550.836393	7.143923	-0.072899	3.651986
377.464080	4558.876300	7.148928	-0.072882	3.655135
377.587651	4566.888655	7.153933	-0.072910	3.658277
378.515527	4574.873682	7.158938	-0.073088	3.661428
378.586834	4582.840639	7.163942	-0.073107	3.664546
378.872577	4590.911528	7.168947	-0.073165	3.667707
378.940835	4599.008484	7.173952	-0.073183	3.670870
378.965002	4606.970557	7.178957	-0.073193	3.673976
379.253551	4615.025476	7.183962	-0.073252	3.677123
379.342586	4622.979931	7.188966	-0.073274	3.680223
379.576777	4631.034017	7.193971	-0.073323	3.683363
379.503672	4639.115133	7.198976	-0.073314	3.686502
379.692324	4647.096145	7.203981	-0.073355	3.689607
380.252244	4655.111239	7.208986	-0.073464	3.692732
380.052233	4663.185300	7.213990	-0.073432	3.695858
380.281809	4671.188126	7.218995	-0.073481	3.698964
380.525195	4679.227526	7.224000	-0.073531	3.702082
380.668492	4687.180356	7.229005	-0.073563	3.705162
380.828453	4695.267276	7.234010	-0.073598	3.708291
381.121871	4703.308577	7.239014	-0.073658	3.711403
381.371697	4711.341836	7.244019	-0.073710	3.714509
381.539844	4719.335459	7.249024	-0.073747	3.717594
381.746750	4727.333260	7.254029	-0.073790	3.720680
382.071310	4735.331714	7.259034	-0.073856	3.723766
382.094578	4743.378565	7.264038	-0.073866	3.726860
382.176840	4751.433971	7.269043	-0.073886	3.729957
382.337049	4759.457695	7.274048	-0.073921	3.733041
382.415008	4767.462510	7.279053	-0.073941	3.736113
382.641680	4775.464360	7.284058	-0.073989	3.739185
382.870103	4783.459733	7.289062	-0.074037	3.742252
382.898322	4791.536659	7.294067	-0.074047	3.745343
382.987295	4799.553480	7.299072	-0.074069	3.748410
382.945827	4807.585228	7.304077	-0.074067	3.751476
383.357612	4815.588183	7.309082	-0.074148	3.754541
383.518800	4823.549038	7.314086	-0.074184	3.757580
383.713214	4831.590553	7.319091	-0.074225	3.760649
383.874775	4839.602239	7.324096	-0.074261	3.763703
384.059003	4847.642077	7.329101	-0.074300	3.766766
384.037016	4855.744184	7.334106	-0.074301	3.769844
384.119368	4863.713994	7.339110	-0.074322	3.772873
384.299431	4871.776359	7.344115	-0.074361	3.775937
384.460324	4879.754288	7.349120	-0.074396	3.778965
384.602138	4887.748942	7.354125	-0.074428	3.781998
385.107622	4895.785433	7.359130	-0.074527	3.785051
384.845119	4903.832041	7.364134	-0.074484	3.788089
385.133983	4911.871908	7.369139	-0.074543	3.791134
385.515253	4919.843261	7.374144	-0.074619	3.794153
385.578231	4927.862018	7.379149	-0.074636	3.797180
385.835200	4935.905270	7.384154	-0.074689	3.800218
385.803632	4943.885463	7.389158	-0.074689	3.803224
386.376202	4951.946755	7.394163	-0.074800	3.806271
386.733288	4959.948815	7.399168	-0.074872	3.809289
386.557983	4968.029970	7.404173	-0.074845	3.812322
386.662215	4976.110796	7.409178	-0.074870	3.815359
386.624643	4984.077524	7.414182	-0.074868	3.818347
386.940650	4992.102004	7.419187	-0.074932	3.821363
386.996231	5000.093327	7.424192	-0.074948	3.824358
387.178450	5008.116029	7.429197	-0.074987	3.827365
387.551869	5016.144765	7.434202	-0.075062	3.830376
387.590880	5024.184503	7.439206	-0.075074	3.833382
387.794178	5032.225181	7.444211	-0.075117	3.836389
388.056082	5040.153352	7.449216	-0.075171	3.839353
388.200671	5048.208484	7.454221	-0.075204	3.842359
388.392775	5056.236236	7.459226	-0.075245	3.845354
388.450619	5064.269669	7.464230	-0.075261	3.848346
388.451800	5072.324389	7.469235	-0.075266	3.851342
388.802849	5080.307425	7.474240	-0.075337	3.854317
388.941410	5088.325701	7.479245	-0.075368	3.857298
389.004190	5096.431133	7.484250	-0.075385	3.860307
389.275299	5104.334059	7.489254	-0.075441	3.863243
389.484306	5112.420257	7.494259	-0.075485	3.866244
389.670546	5120.401921	7.499264	-0.075525	3.869203
389.903110	5128.539149	7.504269	-0.075574	3.872218
390.397001	5136.564340	7.509274	-0.075671	3.875195
390.625622	5144.503279	7.514278	-0.075719	3.878132
390.487719	5152.542248	7.519283	-0.075698	3.881096
390.876087	5160.461743	7.524288	-0.075776	3.884025
391.038648	5168.479463	7.529293	-0.075811	3.886983
391.034911	5176.584568	7.534298	-0.075816	3.889968
391.029197	5184.588218	7.539302	-0.075820	3.892913
391.464203	5192.596049	7.544307	-0.075907	3.895866
391.746734	5200.574210	7.549312	-0.075964	3.898803
391.868941	5208.594396	7.554317	-0.075992	3.901750
392.058443	5216.654544	7.559322	-0.076033	3.904710
391.848420	5224.699714	7.564326	-0.075999	3.907655
391.552309	5232.797249	7.569331	-0.075949	3.910616
392.223577	5240.721326	7.574336	-0.076080	3.913529
392.399804	5248.734210	7.579341	-0.076118	3.916463
392.393135	5256.771393	7.584346	-0.076122	3.919400
392.441386	5264.783497	7.589350	-0.076136	3.922327
393.195031	5272.704714	7.594355	-0.076282	3.925232
393.245104	5280.780232	7.599360	-0.076296	3.928178
393.087883	5288.874342	7.604365	-0.076272	3.931124
393.299208	5296.897026	7.609370	-0.076317	3.934049
393.309716	5304.929284	7.614374	-0.076324	3.936972
393.689777	5312.886651	7.619379	-0.076400	3.939872
393.874458	5320.924546	7.624384	-0.076440	3.942795
393.816808	5328.938712	7.629389	-0.076435	3.945703
394.356208	5336.955949	7.634394	-0.076540	3.948621
394.222182	5345.077246	7.639398	-0.076521	3.951563
394.477050	5353.032287	7.644403	-0.076573	3.954449
394.667538	5361.049994	7.649408	-0.076614	3.957354
394.870070	5369.010039	7.654413	-0.076657	3.960236
395.116129	5377.079235	7.659418	-0.076708	3.963157
395.317087	5385.077174	7.664422	-0.076751	3.966049
395.205178	5393.114708	7.669427	-0.076735	3.968947
395.282056	5401.173884	7.674432	-0.076755	3.971855
395.646848	5409.122590	7.679437	-0.076828	3.974726
395.860568	5417.209495	7.684442	-0.076873	3.977641
395.565117	5425.193573	7.689446	-0.076824	3.980509
396.070696	5433.173075	7.694451	-0.076923	3.983387
396.512070	5441.225131	7.699456	-0.077010	3.986287
396.357079	5449.251065	7.704461	-0.076987	3.989166
396.445770	5457.311099	7.709466	-0.077009	3.992059
396.543441	5465.275541	7.714470	-0.077032	3.994916
396.926713	5473.251329	7.719475	-0.077109	3.997780
397.201984	5481.334960	7.724480	-0.077165	4.000679
397.261389	5489.296817	7.729485	-0.077182	4.003528
397.558192	5497.358943	7.734490	-0.077242	4.006415
397.508991	5505.361890	7.739494	-0.077238	4.009272
398.018886	5513.388237	7.744499	-0.077339	4.012146
398.198026	5521.429776	7.749504	-0.077377	4.015017
398.196809	5529.428532	7.754509	-0.077382	4.017868
398.547549	5537.477289	7.759514	-0.077453	4.020741
398.504977	5545.435025	7.764518	-0.077450	4.023572
398.776101	5553.506102	7.769523	-0.077506	4.026448
398.643739	5561.548671	7.774528	-0.077487	4.029304
398.724681	5569.599564	7.779533	-0.077507	4.032165
399.359585	5577.628636	7.784538	-0.077631	4.035024
399.434344	5585.582236	7.789542	-0.077650	4.037846
399.532670	5593.621459	7.794547	-0.077673	4.040697
399.811071	5601.574631	7.799552	-0.077730	4.043518
399.932438	5609.640148	7.804557	-0.077758	4.046374
400.166240	5617.618160	7.809562	-0.077807	4.049199
400.591560	5625.661498	7.814566	-0.077892	4.052049
400.648688	5633.704649	7.819571	-0.077908	4.054890
400.775351	5641.716822	7.824576	-0.077936	4.057719
400.788882	5649.753712	7.829581	-0.077944	4.060554
401.033952	5657.753468	7.834586	-0.077995	4.063377
400.901341	5665.837170	7.839590	-0.077976	4.066222
401.203305	5673.772156	7.844595	-0.078037	4.069019
401.444408	5681.872509	7.849600	-0.078088	4.071871
401.381533	5689.837763	7.854605	-0.078081	4.074669
401.892210	5697.872370	7.859610	-0.078181	4.077498
401.885605	5705.883727	7.864614	-0.078186	4.080310
402.209345	5713.854777	7.869619	-0.078251	4.083110
402.102175	5721.967854	7.874624	-0.078236	4.085951
402.354041	5729.949533	7.879629	-0.078289	4.088750
402.609160	5738.034825	7.884634	-0.078341	4.091583
402.611682	5745.968284	7.889638	-0.078347	4.094358
402.955802	5753.992412	7.894643	-0.078417	4.097167
402.961051	5762.044878	7.899648	-0.078423	4.099979
402.784734	5770.026089	7.904653	-0.078395	4.102762
403.278330	5778.045756	7.909658	-0.078492	4.105566
403.325544	5786.077302	7.914662	-0.078507	4.108366
403.482798	5794.159300	7.919667	-0.078541	4.111183
403.708728	5802.118571	7.924672	-0.078588	4.113956
403.867598	5810.128157	7.929677	-0.078623	4.116744
404.309459	5818.115987	7.934682	-0.078711	4.119527
404.354378	5826.122182	7.939686	-0.078725	4.122308
404.383073	5834.145237	7.944691	-0.078735	4.125093
404.605658	5842.206770	7.949696	-0.078782	4.127892
404.830453	5850.213423	7.954701	-0.078829	4.130671
405.165895	5858.216834	7.959706	-0.078897	4.133447
405.109179	5866.278568	7.964710	-0.078892	4.136237
405.309803	5874.267386	7.969715	-0.078934	4.139003
405.511836	5882.295012	7.974720	-0.078977	4.141781
405.310262	5890.291689	7.979725	-0.078945	4.144541
405.944450	5898.323125	7.984730	-0.079068	4.147321
406.154207	5906.329768	7.989734	-0.079113	4.150086
406.019109	5914.368133	7.994739	-0.079093	4.152856
406.411874	5922.393385	7.999744	-0.079171	4.155626
406.016598	5930.447434	8.004749	-0.079103	4.158394
406.723409	5938.418641	8.009754	-0.079240	4.161145
406.532054	5946.392378	8.014758	-0.079209	4.163884
407.001238	5954.425777	8.019763	-0.079302	4.166650
407.032062	5962.469433	8.024768	-0.079313	4.169413
407.109762	5970.495849	8.029773	-0.079333	4.172168
407.296222	5978.579329	8.034778	-0.079373	4.174942
407.281839	5986.514919	8.039782	-0.079375	4.177661
407.495986	5994.539816	8.044787	-0.079421	4.180412
407.912768	6002.507401	8.049792	-0.079503	4.183144
407.945937	6010.562089	8.054797	-0.079515	4.185899
408.130792	6018.632438	8.059802	-0.079555	4.188660
408.111727	6026.700518	8.064806	-0.079556	4.191415
408.514908	6034.699205	8.069811	-0.079637	4.194150
408.594636	6042.715105	8.074816	-0.079657	4.196885
408.415258	6050.710143	8.079821	-0.079629	4.199608
408.598240	6058.754154	8.084826	-0.079668	4.202351
409.101027	6066.685579	8.089830	-0.079767	4.205057
409.349910	6074.718810	8.094835	-0.079819	4.207792
409.299677	6082.791971	8.099840	-0.079815	4.210537
409.661951	6090.764130	8.104845	-0.079887	4.213249
409.611032	6098.838643	8.109850	-0.079883	4.215991
409.904103	6106.799659	8.114854	-0.079943	4.218695
409.815681	6114.900587	8.119859	-0.079932	4.221441
410.421258	6122.790275	8.124864	-0.080050	4.224122
410.512945	6130.862824	8.129869	-0.080072	4.226856
410.552849	6138.886905	8.134874	-0.080085	4.229573
410.617888	6146.907997	8.139878	-0.080102	4.232286
410.800087	6154.921404	8.144883	-0.080142	4.234997
411.100003	6162.954894	8.149888	-0.080203	4.237713
411.041938	6170.923207	8.154893	-0.080197	4.240403
411.183303	6178.956228	8.159898	-0.080229	4.243114
411.377717	6186.960429	8.164902	-0.080270	4.245815
411.387005	6195.004102	8.169907	-0.080277	4.248525
411.754105	6203.071938	8.174912	-0.080351	4.251245
411.578457	6211.041446	8.179917	-0.080324	4.253925
411.814131	6219.083682	8.184922	-0.080373	4.256632
411.960616	6227.068698	8.189926	-0.080405	4.259317
412.306159	6235.082797	8.194931	-0.080475	4.262012
412.422415	6243.089188	8.199936	-0.080502	4.264700
412.460188	6251.101072	8.204941	-0.080514	4.267388
412.981003	6259.143421	8.209946	-0.080616	4.270089
413.099298	6267.158636	8.214950	-0.080644	4.272775
413.206214	6275.191396	8.219955	-0.080669	4.275465
413.308434	6283.188327	8.224960	-0.080693	4.278142
413.472953	6291.215679	8.229965	-0.080729	4.280827
413.830298	6299.166212	8.234970	-0.080801	4.283487
413.822605	6307.241212	8.239974	-0.080805	4.286183
413.933919	6315.230116	8.244979	-0.080831	4.288851
414.246191	6323.296363	8.249984	-0.080894	4.291544
414.620023	6331.259355	8.254989	-0.080969	4.294201
414.736415	6339.331764	8.259994	-0.080996	4.296891
414.480379	6347.304624	8.264998	-0.080954	4.299543
414.728673	6355.356450	8.270003	-0.081005	4.302224
414.719271	6363.418203	8.275008	-0.081009	4.304904
414.792317	6371.374777	8.280013	-0.081028	4.307548
415.081909	6379.438907	8.285018	-0.081087	4.310229
415.566445	6387.322560	8.290022	-0.081182	4.312849
415.684658	6395.436053	8.295027	-0.081210	4.315541
415.647405	6403.416264	8.300032	-0.081208	4.318185
415.785896	6411.477153	8.305037	-0.081239	4.320856
416.014745	6419.418233	8.310042	-0.081287	4.323487
416.069447	6427.503479	8.315046	-0.081302	4.326162
416.217033	6435.450776	8.320051	-0.081335	4.328791
416.550761	6443.569585	8.325056	-0.081403	4.331476
416.608798	6451.465580	8.330061	-0.081419	4.334084
416.893280	6459.582464	8.335066	-0.081477	4.336765
416.841924	6467.504969	8.340070	-0.081473	4.339377
417.169119	6475.648964	8.345075	-0.081539	4.342064
417.224992	6483.616659	8.350080	-0.081555	4.344689
417.287809	6491.628888	8.355085	-0.081572	4.347327
417.550707	6499.677568	8.360090	-0.081626	4.349977
417.768355	6507.652498	8.365094	-0.081672	4.352601
417.893916	6515.687602	8.370099	-0.081700	4.355242
418.366474	6523.655342	8.375104	-0.081794	4.357862
418.289561	6531.679070	8.380109	-0.081785	4.360495
418.425509	6539.703023	8.385114	-0.081815	4.363128
418.732317	6547.698692	8.390118	-0.081878	4.365751
418.944359	6555.733725	8.395123	-0.081922	4.368385
418.848136	6563.795443	8.400128	-0.081910	4.371023
419.018236	6571.792506	8.405133	-0.081947	4.373641
419.383184	6579.823841	8.410138	-0.082020	4.376270
419.415086	6587.746562	8.415142	-0.082031	4.378859
419.689345	6595.812511	8.420147	-0.082088	4.381495
419.958885	6603.782115	8.425152	-0.082143	4.384099
420.013212	6611.907317	8.430157	-0.082158	4.386749
420.201608	6619.901677	8.435162	-0.082199	4.389357
420.404880	6627.957136	8.440166	-0.082242	4.391983
420.526107	6635.965379	8.445171	-0.082270	4.394591
420.690636	6644.012157	8.450176	-0.082306	4.397211
420.947458	6651.910352	8.455181	-0.082359	4.399781
421.227929	6660.057834	8.460186	-0.082416	4.402431
421.108002	6668.028357	8.465190	-0.082399	4.405020
421.319690	6676.044597	8.470195	-0.082444	4.407623
421.649863	6684.108764	8.475200	-0.082511	4.410242
421.704793	6692.128859	8.480205	-0.082526	4.412843
421.712838	6700.183454	8.485210	-0.082533	4.415453
422.117246	6708.138499	8.490214	-0.082614	4.418032
422.418355	6716.153215	8.495219	-0.082675	4.420628
422.579512	6724.152961	8.500224	-0.082710	4.423217
422.545256	6732.227424	8.505229	-0.082709	4.425827
422.969735	6740.248715	8.510234	-0.082794	4.428421
422.827560	6748.288123	8.515238	-0.082772	4.431016
422.923357	6756.256702	8.520243	-0.082796	4.433589
423.097967	6764.327440	8.525248	-0.082833	4.436193
423.112805	6772.282510	8.530253	-0.082841	4.438757
423.299685	6780.373255	8.535258	-0.082881	4.441365
423.166689	6788.335113	8.540262	-0.082862	4.443927
423.641121	6796.365948	8.545267	-0.082956	4.446514
423.758561	6804.341038	8.550272	-0.082983	4.449079
423.819706	6812.381870	8.555277	-0.082999	4.451664
424.245598	6820.411323	8.560282	-0.083084	4.454245
424.356602	6828.398646	8.565287	-0.083110	4.456810
424.408768	6836.377842	8.570291	-0.083125	4.459370
424.632903	6844.460496	8.575296	-0.083172	4.461963
424.731432	6852.426925	8.580301	-0.083196	4.464517
424.876204	6860.527002	8.585306	-0.083228	4.467112
424.747921	6868.474597	8.590311	-0.083209	4.469655
425.082593	6876.525890	8.595315	-0.083277	4.472232
425.279886	6884.523228	8.600320	-0.083319	4.474790
424.939333	6892.548847	8.605325	-0.083261	4.477353
425.442622	6900.606247	8.610330	-0.083360	4.479929
425.430437	6908.572271	8.615335	-0.083363	4.482471
425.635030	6916.549914	8.620339	-0.083406	4.485017
425.747305	6924.600896	8.625344	-0.083432	4.487584
425.921010	6932.541130	8.630349	-0.083470	4.490115
426.206395	6940.654249	8.635354	-0.083528	4.492700
426.427710	6948.689504	8.640359	-0.083575	4.495258
426.514365	6956.665197	8.645363	-0.083596	4.497795
426.469912	6964.763811	8.650368	-0.083593	4.500369
426.422544	6972.692128	8.655373	-0.083590	4.502888
426.893242	6980.704798	8.660378	-0.083683	4.505434
427.004644	6988.690608	8.665383	-0.083709	4.507969
427.244089	6996.725897	8.670387	-0.083759	4.510518
427.374037	7004.742333	8.675392	-0.083788	4.513060
427.353223	7012.763884	8.680397	-0.083790	4.515601
427.846892	7020.755272	8.685402	-0.083887	4.518133
428.010001	7028.743698	8.690407	-0.083922	4.520662
428.165670	7036.687371	8.695411	-0.083957	4.523175
428.449372	7044.802287	8.700416	-0.084015	4.525741
428.437646	7052.787221	8.705421	-0.084018	4.528263
428.679773	7060.849514	8.710426	-0.084068	4.530810
428.789851	7068.839419	8.715431	-0.084094	4.533331
429.090058	7076.879729	8.720435	-0.084155	4.535868
429.122405	7084.877364	8.725440	-0.084166	4.538389
429.240251	7092.908508	8.730445	-0.084194	4.540919
429.427702	7100.858335	8.735450	-0.084234	4.543423
429.522414	7108.942359	8.740455	-0.084257	4.545967
429.672921	7116.923295	8.745459	-0.084290	4.548477
429.755829	7125.026440	8.750464	-0.084311	4.551025
429.788192	7132.944662	8.755469	-0.084322	4.553512
430.060140	7141.034646	8.760474	-0.084378	4.556053
430.370618	7148.954846	8.765479	-0.084441	4.558539
430.438658	7157.069286	8.770483	-0.084459	4.561084
430.484495	7164.985194	8.775488	-0.084473	4.563565
430.515590	7173.071000	8.780493	-0.084484	4.566099
430.600755	7181.098157	8.785498	-0.084505	4.568612
430.686585	7189.114803	8.790503	-0.084526	4.571121
430.981319	7197.026887	8.795507	-0.084587	4.573596
431.276880	7205.122203	8.800512	-0.084647	4.576127
431.185343	7213.080204	8.805517	-0.084635	4.578613
431.462711	7221.163665	8.810522	-0.084692	4.581138
431.703099	7229.108781	8.815527	-0.084742	4.583617
431.560330	7237.198249	8.820531	-0.084721	4.586140
431.829670	7245.195123	8.825536	-0.084776	4.588633
431.904864	7253.241388	8.830541	-0.084796	4.591140
432.150371	7261.251282	8.835546	-0.084847	4.593635
432.173864	7269.293583	8.840551	-0.084856	4.596138
432.358759	7277.210180	8.845555	-0.084896	4.598600
432.462661	7285.288088	8.850560	-0.084921	4.601112
432.480187	7293.208923	8.855565	-0.084929	4.603573
432.776184	7301.329250	8.860570	-0.084990	4.606095
433.031258	7309.285232	8.865575	-0.085042	4.608564
433.197996	7317.344485	8.870579	-0.085079	4.611064
433.320669	7325.343830	8.875584	-0.085107	4.613545
433.409412	7333.351643	8.880589	-0.085129	4.616026
433.604191	7341.363586	8.885594	-0.085170	4.618507
433.569473	7349.405580	8.890599	-0.085169	4.620996
433.922449	7357.354335	8.895603	-0.085240	4.623456
434.128968	7365.470301	8.900608	-0.085284	4.625965
433.936380	7373.451831	8.905613	-0.085253	4.628431
434.147968	7381.496752	8.910618	-0.085298	4.630916
434.351772	7389.460102	8.915623	-0.085341	4.633375
434.474466	7397.483498	8.920627	-0.085369	4.635850
434.586984	7405.479848	8.925632	-0.085395	4.638316
434.560930	7413.486633	8.930637	-0.085396	4.640783
434.641007	7421.470289	8.935642	-0.085416	4.643243
434.677446	7429.541391	8.940647	-0.085428	4.645727
434.864791	7437.521472	8.945651	-0.085468	4.648183
435.142091	7445.609469	8.950656	-0.085525	4.650670
435.272992	7453.548404	8.955661	-0.085555	4.653110
435.435636	7461.624757	8.960666	-0.085590	4.655591
435.527801	7469.568113	8.965671	-0.085613	4.658030
435.800444	7477.639026	8.970675	-0.085669	4.660507
435.914672	7485.611289	8.975680	-0.085696	4.662952
435.737365	7493.672890	8.980685	-0.085668	4.665423
436.041088	7501.696764	8.985690	-0.085730	4.667882
436.137963	7509.761293	8.990695	-0.085753	4.670351
436.322909	7517.738501	8.995699	-0.085793	4.672793
436.317060	7525.825674	9.000704	-0.085797	4.675267
436.448924	7533.743853	9.005709	-0.085827	4.677687
436.776920	7541.763822	9.010714	-0.085893	4.680138
436.988860	7549.753019	9.015719	-0.085938	4.682578
436.891693	7557.792554	9.020723	-0.085925	4.685032
437.275925	7565.778527	9.025728	-0.086002	4.687468
437.311160	7573.759376	9.030733	-0.086014	4.689902
437.625921	7581.818190	9.035738	-0.086078	4.692357
437.644541	7589.815602	9.040743	-0.086086	4.694793
437.767547	7597.884286	9.045747	-0.086115	4.697250
437.864590	7605.916086	9.050752	-0.086138	4.699694
438.059936	7613.885818	9.055757	-0.086180	4.702117
438.147677	7621.865400	9.060762	-0.086201	4.704543
438.358434	7629.938143	9.065767	-0.086246	4.706995
438.500362	7637.885256	9.070771	-0.086277	4.709408
438.731833	7646.012931	9.075776	-0.086326	4.711875
438.552942	7653.958425	9.080781	-0.086298	4.714285
439.120737	7662.044025	9.085786	-0.086409	4.716735
439.245607	7669.969648	9.090791	-0.086437	4.719137
439.299568	7678.049469	9.095795	-0.086453	4.721584
439.647117	7685.962047	9.100800	-0.086523	4.723979
439.550394	7694.054461	9.105805	-0.086510	4.726427
439.809132	7702.086292	9.110810	-0.086563	4.728855
439.710710	7710.184996	9.115815	-0.086550	4.731303
439.888924	7718.154401	9.120819	-0.086589	4.733710
439.919835	7726.217884	9.125824	-0.086600	4.736145
439.970721	7734.188413	9.130829	-0.086615	4.738550
440.324771	7742.204683	9.135834	-0.086686	4.740967
440.211259	7750.168687	9.140839	-0.086670	4.743368
440.236315	7758.183408	9.145843	-0.086680	4.745783
440.557232	7766.264810	9.150848	-0.086745	4.748216
440.921583	7774.227395	9.155853	-0.086818	4.750612
441.055336	7782.309453	9.160858	-0.086848	4.753043
440.739861	7790.310737	9.165863	-0.086795	4.755450
440.854302	7798.296980	9.170867	-0.086821	4.757850
441.339523	7806.291764	9.175872	-0.086917	4.760250
441.345814	7814.248826	9.180877	-0.086924	4.762639
441.444591	7822.338782	9.185882	-0.086947	4.765066
441.694999	7830.310494	9.190887	-0.086999	4.767456
442.005554	7838.328581	9.195891	-0.087062	4.769859
442.027714	7846.452124	9.200896	-0.087072	4.772293
442.014381	7854.402190	9.205901	-0.087074	4.774674
442.309228	7862.416869	9.210906	-0.087135	4.777072
442.201104	7870.428223	9.215911	-0.087120	4.779469
442.474352	7878.461326	9.220915	-0.087176	4.781870
442.743254	7886.433748	9.225920	-0.087231	4.784252
442.592886	7894.493305	9.230925	-0.087209	4.786660
442.992784	7902.479555	9.235930	-0.087288	4.789043
443.123709	7910.546315	9.240935	-0.087318	4.791450
443.375191	7918.465769	9.245939	-0.087370	4.793811
443.503215	7926.567905	9.250944	-0.087399	4.796226
443.384480	7934.497161	9.255949	-0.087382	4.798589
443.865030	7942.613959	9.260954	-0.087477	4.801004
443.642006	7950.534095	9.265959	-0.087441	4.803363
444.033209	7958.594038	9.270963	-0.087519	4.805759
444.363638	7966.577554	9.275968	-0.087586	4.808132
444.262954	7974.634006	9.280973	-0.087572	4.810527
444.470338	7982.652352	9.285978	-0.087616	4.812908
444.473071	7990.084044	9.290983	-0.087622	4.815114
444.764424	7994.785610	9.295987	-0.087679	4.816509

444.818857	7997.446056	9.300992	-0.087691	4.817298
444.834567	7998.684741	9.305997	-0.087695	4.817665
444.996003	7999.052130	9.311002	-0.087725	4.817774
445.034265	8000.164975	9.316007	-0.087733	4.818104
445.130774	8000.130544	9.321011	-0.087751	4.818093
445.212153	8000.182197	9.326016	-0.087766	4.818108
445.341405	8000.118757	9.331021	-0.087791	4.818089
445.142425	8000.195967	9.336026	-0.087754	4.818113
445.469361	8000.135283	9.341031	-0.087814	4.818093
445.798204	8000.053578	9.346035	-0.087876	4.818068
445.782304	8000.143865	9.351040	-0.087873	4.818094
445.857706	8000.121769	9.356045	-0.087887	4.818088
446.068900	8000.135243	9.361050	-0.087926	4.818091
446.053388	8000.129769	9.366055	-0.087924	4.818089
446.050462	8000.136048	9.371059	-0.087923	4.818091
446.266983	8000.169591	9.376064	-0.087963	4.818100
446.075280	8000.158503	9.381069	-0.087928	4.818098
446.066905	8000.224692	9.386074	-0.087926	4.818117
446.222595	8000.167934	9.391079	-0.087955	4.818100
446.119635	8000.131774	9.396083	-0.087936	4.818089
446.104789	8000.190505	9.401088	-0.087934	4.818107
446.100939	8000.146256	9.406093	-0.087933	4.818094
446.225073	8000.227974	9.411098	-0.087956	4.818118
446.111460	8000.211660	9.416103	-0.087935	4.818113
446.301986	8000.172227	9.421107	-0.087971	4.818101
446.397866	8000.212507	9.426112	-0.087988	4.818112
446.514192	8000.204663	9.431117	-0.088010	4.818109
446.484072	8000.195829	9.436122	-0.088005	4.818107
446.456658	8000.162827	9.441127	-0.088000	4.818097
446.694947	8000.174575	9.446131	-0.088044	4.818100
446.723376	8000.189710	9.451136	-0.088049	4.818104
446.753864	8000.155410	9.456141	-0.088055	4.818094
446.867635	8000.233828	9.461146	-0.088076	4.818117
446.612024	8000.188170	9.466151	-0.088029	4.818104
446.701813	8000.187323	9.471155	-0.088046	4.818103
446.814418	8000.224680	9.476160	-0.088067	4.818114
446.782357	8000.171617	9.481165	-0.088061	4.818098
446.812745	8000.210985	9.486170	-0.088066	4.818110
446.800387	8000.202398	9.491175	-0.088064	4.818108
446.887596	8000.249926	9.496179	-0.088081	4.818121
446.750493	8000.253279	9.501184	-0.088055	4.818123
446.941931	8000.132823	9.506189	-0.088091	4.818086
447.154500	8000.172629	9.511194	-0.088130	4.818097
446.919173	8000.185136	9.516199	-0.088087	4.818102
447.013900	8000.150680	9.521203	-0.088104	4.818091
447.163463	8000.227493	9.526208	-0.088132	4.818113
447.106290	8000.148822	9.531213	-0.088122	4.818090
447.143697	8000.233541	9.536218	-0.088129	4.818115
447.146908	8000.223067	9.541223	-0.088129	4.818112
447.035915	8000.221523	9.546227	-0.088109	4.818112
447.068838	8000.225144	9.551232	-0.088115	4.818113
446.977069	8000.210187	9.556237	-0.088098	4.818109
447.176434	8000.235074	9.561242	-0.088135	4.818116
447.038297	8000.219470	9.566247	-0.088109	4.818112
446.916892	8000.273558	9.571251	-0.088087	4.818128
447.223460	8000.253636	9.576256	-0.088144	4.818121
447.117649	8000.223748	9.581261	-0.088124	4.818113
447.139345	8000.246157	9.586266	-0.088129	4.818119
447.291989	8000.191461	9.591271	-0.088157	4.818102
447.511009	8000.214519	9.596275	-0.088198	4.818108
447.521545	8000.222037	9.601280	-0.088200	4.818110
447.392550	8000.199193	9.606285	-0.088176	4.818104
447.413371	8000.232114	9.611290	-0.088180	4.818114
447.090266	8000.248657	9.616295	-0.088120	4.818120
447.059816	8000.229293	9.621299	-0.088114	4.818114
447.332359	8000.215211	9.626304	-0.088165	4.818109
447.057300	8000.247159	9.631309	-0.088114	4.818120
447.303910	8000.231662	9.636314	-0.088160	4.818114
447.102332	8000.227801	9.641319	-0.088122	4.818114
447.259728	8000.237369	9.646323	-0.088152	4.818116
447.167644	8000.267661	9.651328	-0.088135	4.818125
446.710154	8000.265491	9.656333	-0.088050	4.818127
447.314462	8000.224465	9.661338	-0.088162	4.818112
447.258994	8000.197386	9.666343	-0.088152	4.818104
447.308485	8000.212815	9.671347	-0.088161	4.818108
447.245451	8000.266666	9.676352	-0.088149	4.818125
447.044800	8000.252293	9.681357	-0.088112	4.818121
447.101084	8000.273079	9.686362	-0.088123	4.818127
447.126977	8000.249240	9.691367	-0.088128	4.818120
447.404647	8000.252068	9.696371	-0.088179	4.818120
447.281684	8000.272457	9.701376	-0.088157	4.818126
447.291682	8000.238924	9.706381	-0.088158	4.818116
447.560401	8000.254256	9.711386	-0.088209	4.818120
447.359928	8000.204103	9.716391	-0.088171	4.818106
447.264009	8000.252233	9.721395	-0.088153	4.818120
447.396862	8000.267774	9.726400	-0.088178	4.818124
447.527026	8000.228551	9.731405	-0.088203	4.818112
447.845171	8000.239311	9.736410	-0.088262	4.818114
447.635239	8000.226913	9.741415	-0.088223	4.818111
447.845388	8000.224589	9.746419	-0.088262	4.818110
447.792361	8000.263846	9.751424	-0.088252	4.818122
447.615065	8000.223488	9.756429	-0.088219	4.818110
447.673607	8000.212734	9.761434	-0.088230	4.818107
447.681465	8000.251788	9.766439	-0.088232	4.818118
447.575330	8000.254521	9.771443	-0.088212	4.818120
447.623802	8000.306771	9.776448	-0.088221	4.818135
447.512059	8000.279958	9.781453	-0.088200	4.818128
447.749992	8000.273812	9.786458	-0.088245	4.818125
447.779358	8000.260545	9.791463	-0.088250	4.818121
447.774389	8000.266795	9.796467	-0.088249	4.818123
448.150956	8000.247851	9.801472	-0.088320	4.818115
447.715800	8000.227046	9.806477	-0.088239	4.818111
447.833356	8000.257108	9.811482	-0.088261	4.818119
447.984377	8000.231858	9.816487	-0.088289	4.818111
447.793724	8000.190261	9.821491	-0.088253	4.818100
447.933744	8000.254314	9.826496	-0.088280	4.818118
447.780447	8000.258493	9.831501	-0.088251	4.818120
447.760715	8000.290848	9.836506	-0.088247	4.818130
447.880667	8000.205175	9.841511	-0.088270	4.818104
447.939558	8000.199687	9.846515	-0.088281	4.818102
448.126731	8000.249665	9.851520	-0.088316	4.818116
448.037641	8000.217905	9.856525	-0.088299	4.818107
448.074776	8000.260526	9.861530	-0.088306	4.818119
447.975051	8000.243351	9.866535	-0.088288	4.818115
448.041089	8000.276904	9.871539	-0.088300	4.818124
448.374255	8000.262617	9.876544	-0.088362	4.818119
448.088193	8000.234421	9.881549	-0.088309	4.818112
448.318457	8000.278686	9.886554	-0.088352	4.818124
448.275154	8000.219149	9.891559	-0.088344	4.818106
448.529596	8000.241651	9.896563	-0.088391	4.818112
448.395022	8000.240829	9.901568	-0.088366	4.818112
448.319607	8000.209259	9.906573	-0.088352	4.818103
448.308615	8000.139649	9.911578	-0.088350	4.818083
448.491074	8000.189562	9.916583	-0.088384	4.818097
448.348461	8000.194942	9.921587	-0.088358	4.818099
448.404175	8000.258872	9.926592	-0.088368	4.818118
448.294749	8000.228932	9.931597	-0.088348	4.818109
448.254745	8000.274686	9.936602	-0.088341	4.818123
448.350325	8000.236032	9.941607	-0.088359	4.818111
448.091180	8000.227156	9.946611	-0.088310	4.818109
448.303450	8000.262751	9.951616	-0.088350	4.818119
448.085317	8000.228136	9.956621	-0.088309	4.818110
447.918160	8000.270010	9.961626	-0.088278	4.818123
448.337701	8000.248509	9.966631	-0.088356	4.818115
448.303395	8000.193307	9.971635	-0.088350	4.818098
448.336652	8000.221140	9.976640	-0.088356	4.818107
448.003506	8000.247014	9.981645	-0.088294	4.818116
448.491621	8000.184373	9.986650	-0.088385	4.818095
448.450825	8000.186965	9.991655	-0.088378	4.818096
448.398651	8000.222025	9.996659	-0.088368	4.818107
448.476960	8000.267326	10.001664	-0.088383	4.818120
448.336149	8000.222214	10.006669	-0.088357	4.818107
448.168535	8000.259871	10.011674	-0.088326	4.818119
448.461223	8000.238704	10.016679	-0.088380	4.818111
448.483917	8000.230606	10.021683	-0.088384	4.818109
448.331149	8000.263208	10.026688	-0.088356	4.818119
448.174847	8000.197884	10.031693	-0.088327	4.818100
448.105883	8000.284278	10.036698	-0.088314	4.818126
447.884423	8000.256985	10.041703	-0.088273	4.818119
447.824992	8000.299309	10.046707	-0.088262	4.818132
447.916876	8000.283758	10.051712	-0.088279	4.818127
448.062860	8000.260542	10.056717	-0.088306	4.818119
447.801195	8000.297939	10.061722	-0.088258	4.818132
447.856411	8000.294505	10.066727	-0.088268	4.818130
447.907008	8000.338366	10.071731	-0.088278	4.818143
447.892798	8000.335015	10.076736	-0.088275	4.818142
447.891602	8000.281328	10.081741	-0.088275	4.818126
448.176675	8000.294786	10.086746	-0.088328	4.818129
448.179530	8000.281149	10.091751	-0.088329	4.818125
448.230814	8000.293446	10.096755	-0.088338	4.818128
448.415412	8000.270770	10.101760	-0.088373	4.818121
448.436470	8000.251072	10.106765	-0.088377	4.818115
448.578275	8000.254110	10.111770	-0.088403	4.818115
448.606374	8000.258717	10.116775	-0.088408	4.818117
448.654458	8000.212033	10.121779	-0.088417	4.818103
448.673682	8000.252299	10.126784	-0.088421	4.818114
448.433046	8000.224737	10.131789	-0.088376	4.818107
448.668564	8000.264867	10.136794	-0.088420	4.818118
448.251123	8000.272723	10.141799	-0.088343	4.818122
448.502003	8000.309910	10.146803	-0.088389	4.818132
448.565811	8000.306596	10.151808	-0.088401	4.818131
448.549865	8000.230601	10.156813	-0.088398	4.818108
448.784495	8000.269667	10.161818	-0.088442	4.818119
448.614817	8000.253620	10.166823	-0.088411	4.818115
448.594679	8000.252291	10.171827	-0.088407	4.818115
448.696984	8000.283193	10.176832	-0.088426	4.818123
448.485284	8000.237090	10.181837	-0.088387	4.818111
448.394196	8000.282131	10.186842	-0.088370	4.818124
448.450069	8000.255552	10.191847	-0.088380	4.818116
448.452258	8000.237696	10.196851	-0.088381	4.818111
448.703497	8000.262258	10.201856	-0.088428	4.818117
448.779590	8000.222280	10.206861	-0.088442	4.818105
448.718595	8000.262479	10.211866	-0.088430	4.818117
448.669545	8000.242854	10.216871	-0.088421	4.818112
448.649998	8000.222589	10.221875	-0.088418	4.818106
448.764166	8000.232608	10.226880	-0.088439	4.818108
448.857542	8000.149720	10.231885	-0.088457	4.818083
448.967315	8000.262819	10.236890	-0.088477	4.818116
448.843548	8000.243203	10.241895	-0.088454	4.818111
448.746693	8000.229225	10.246899	-0.088436	4.818107
448.854259	8000.239152	10.251904	-0.088456	4.818110
448.946175	8000.199395	10.256909	-0.088473	4.818098
448.556507	8000.281311	10.261914	-0.088401	4.818123
448.670286	8000.237649	10.266919	-0.088422	4.818110
448.585480	8000.254361	10.271923	-0.088406	4.818115
448.583712	8000.274338	10.276928	-0.088406	4.818121
448.612139	8000.260005	10.281933	-0.088412	4.818117
448.732388	8000.283791	10.286938	-0.088434	4.818123
448.817516	8000.252358	10.291943	-0.088450	4.818114
448.908302	8000.206270	10.296947	-0.088467	4.818100
449.052023	8000.215650	10.301952	-0.088494	4.818102
448.929671	8000.196054	10.306957	-0.088471	4.818097
449.000930	8000.234942	10.311962	-0.088484	4.818108
448.983172	8000.227332	10.316967	-0.088481	4.818106
448.971254	8000.257691	10.321971	-0.088479	4.818115
448.963251	8000.292316	10.326976	-0.088477	4.818125
449.051579	8000.259875	10.331981	-0.088494	4.818115
448.984700	8000.289467	10.336986	-0.088482	4.818124
449.052501	8000.268317	10.341991	-0.088494	4.818118
448.956509	8000.232250	10.346995	-0.088476	4.818107
449.064262	8000.233760	10.352000	-0.088497	4.818107
449.035913	8000.228106	10.357005	-0.088491	4.818106
449.124768	8000.254611	10.362010	-0.088508	4.818113
449.057224	8000.249463	10.367015	-0.088495	4.818112
449.082874	8000.220356	10.372019	-0.088500	4.818103
449.146016	8000.287549	10.377024	-0.088512	4.818123
448.974995	8000.220964	10.382029	-0.088480	4.818104
449.076413	8000.236067	10.387034	-0.088499	4.818108
449.110114	8000.241805	10.392039	-0.088506	4.818109
448.922750	8000.248665	10.397043	-0.088471	4.818112
449.030534	8000.285959	10.402048	-0.088491	4.818123
449.051448	8000.232580	10.407053	-0.088495	4.818107
449.144245	8000.285452	10.412058	-0.088512	4.818122
449.123855	8000.251493	10.417063	-0.088508	4.818112
449.162287	8000.207831	10.422067	-0.088516	4.818099
449.160282	8000.280428	10.427072	-0.088515	4.818121
449.017036	8000.257382	10.432077	-0.088489	4.818114
449.259627	8000.237621	10.437082	-0.088534	4.818108
449.185661	8000.211333	10.442087	-0.088520	4.818100
449.243696	8000.225831	10.447091	-0.088531	4.818104
449.262559	8000.249254	10.452096	-0.088535	4.818111
449.205093	8000.224249	10.457101	-0.088524	4.818104
449.128286	8000.261069	10.462106	-0.088510	4.818115
449.011784	8000.246817	10.467111	-0.088488	4.818111
449.067977	8000.248659	10.472115	-0.088499	4.818112
449.189155	8000.276668	10.477120	-0.088521	4.818119
448.881717	8000.248171	10.482125	-0.088464	4.818112
448.848508	8000.268762	10.487130	-0.088458	4.818118
449.185584	8000.245058	10.492135	-0.088521	4.818110
449.156718	8000.237293	10.497139	-0.088516	4.818108
449.066311	8000.267608	10.502144	-0.088499	4.818117
448.855583	8000.273089	10.507149	-0.088460	4.818120
449.053268	8000.239019	10.512154	-0.088497	4.818109
449.053979	8000.239034	10.517159	-0.088497	4.818109
449.149708	8000.187752	10.522163	-0.088515	4.818093
449.182514	8000.239786	10.527168	-0.088521	4.818108
449.230240	8000.220461	10.532173	-0.088530	4.818103
448.917181	8000.270820	10.537178	-0.088472	4.818119
449.101110	8000.244978	10.542183	-0.088506	4.818110
449.250960	8000.224974	10.547187	-0.088534	4.818104
449.143760	8000.262423	10.552192	-0.088514	4.818115
449.152020	8000.261490	10.557197	-0.088515	4.818115
449.255571	8000.280834	10.562202	-0.088535	4.818120
449.248821	8000.241803	10.567207	-0.088534	4.818109
449.134594	8000.281258	10.572211	-0.088512	4.818121
449.240902	8000.291168	10.577216	-0.088532	4.818123
449.214460	8000.249756	10.582221	-0.088527	4.818111
449.071639	8000.269868	10.587226	-0.088501	4.818118
449.235240	8000.213220	10.592231	-0.088531	4.818100
449.147703	8000.172008	10.597235	-0.088515	4.818088
449.158956	8000.229003	10.602240	-0.088517	4.818105
449.068576	8000.206696	10.607245	-0.088501	4.818099
449.090361	8000.278572	10.612250	-0.088505	4.818120
449.155210	8000.277378	10.617255	-0.088517	4.818120
449.009393	8000.255349	10.622259	-0.088490	4.818114
449.178112	8000.293495	10.627264	-0.088521	4.818124
449.317790	8000.275454	10.632269	-0.088547	4.818118
449.305632	8000.284761	10.637274	-0.088545	4.818121
449.328960	8000.245098	10.642279	-0.088549	4.818109
449.439769	8000.226653	10.647283	-0.088570	4.818103
449.261266	8000.276788	10.652288	-0.088537	4.818119
449.127430	8000.229667	10.657293	-0.088512	4.818106
449.412991	8000.253658	10.662298	-0.088565	4.818112
449.404127	8000.219859	10.667303	-0.088564	4.818102
449.213710	8000.245621	10.672307	-0.088528	4.818110
449.368425	8000.287781	10.677312	-0.088557	4.818122
449.241079	8000.242855	10.682317	-0.088534	4.818109
449.314645	8000.251255	10.687322	-0.088547	4.818111
449.348623	8000.238052	10.692327	-0.088554	4.818107
449.542808	8000.260767	10.697331	-0.088590	4.818113
449.456373	8000.263774	10.702336	-0.088574	4.818114
449.409001	8000.244172	10.707341	-0.088565	4.818109
449.549078	8000.261921	10.712346	-0.088591	4.818113
449.457513	8000.278539	10.717351	-0.088574	4.818119
449.508769	8000.208743	10.722355	-0.088584	4.818098
449.629907	8000.248330	10.727360	-0.088607	4.818109
449.498277	8000.229656	10.732365	-0.088582	4.818104
449.474869	8000.234596	10.737370	-0.088578	4.818106
449.360595	8000.242476	10.742375	-0.088557	4.818108
449.439261	8000.245685	10.747379	-0.088571	4.818109
449.486214	8000.237926	10.752384	-0.088580	4.818107
449.227434	8000.199584	10.757389	-0.088532	4.818096
449.336690	8000.250581	10.762394	-0.088552	4.818111
449.515918	8000.235198	10.767399	-0.088586	4.818106
449.312120	8000.221830	10.772403	-0.088548	4.818103
449.155366	8000.300685	10.777408	-0.088519	4.818127
449.037972	8000.271686	10.782413	-0.088497	4.818118
449.282316	8000.275104	10.787418	-0.088543	4.818118
449.215160	8000.248911	10.792423	-0.088530	4.818111
449.143744	8000.257390	10.797427	-0.088517	4.818114
449.332284	8000.246347	10.802432	-0.088552	4.818110
449.244796	8000.220922	10.807437	-0.088536	4.818103
449.310292	8000.274466	10.812442	-0.088548	4.818118
449.426238	8000.285563	10.817447	-0.088570	4.818121
449.357280	8000.280394	10.822451	-0.088557	4.818120
449.418671	8000.279152	10.827456	-0.088569	4.818119
449.466212	8000.222987	10.832461	-0.088577	4.818102
449.440103	8000.251044	10.837466	-0.088573	4.818111
449.302082	8000.247015	10.842471	-0.088547	4.818110
449.433599	8000.240437	10.847475	-0.088572	4.818108
449.450113	8000.276457	10.852480	-0.088575	4.818118
449.238300	8000.232456	10.857485	-0.088535	4.818106
449.468055	8000.287242	10.862490	-0.088578	4.818121
449.293559	8000.255339	10.867495	-0.088546	4.818113
449.284673	8000.213121	10.872499	-0.088544	4.818100
449.432878	8000.228878	10.877504	-0.088572	4.818104
449.360062	8000.233128	10.882509	-0.088558	4.818106
449.389580	8000.251437	10.887514	-0.088564	4.818111
449.536291	8000.245072	10.892519	-0.088591	4.818108
449.485481	8000.264364	10.897523	-0.088582	4.818114
449.383325	8000.268204	10.902528	-0.088563	4.818116
449.366748	8000.237455	10.907533	-0.088560	4.818107
449.456216	8000.253444	10.912538	-0.088577	4.818111
449.527613	8000.222872	10.917543	-0.088590	4.818102
449.558033	8000.252772	10.922547	-0.088596	4.818111
449.601856	8000.286016	10.927552	-0.088604	4.818120
449.564474	8000.241294	10.932557	-0.088597	4.818107
449.612023	8000.183024	10.937562	-0.088606	4.818090
449.348191	8000.225651	10.942567	-0.088557	4.818103
449.502304	8000.215180	10.947571	-0.088586	4.818100
449.642346	8000.272923	10.952576	-0.088612	4.818116
449.563808	8000.280250	10.957581	-0.088597	4.818119
449.343876	8000.265604	10.962586	-0.088556	4.818115
449.706042	8000.244357	10.967591	-0.088624	4.818108
449.591641	8000.258551	10.972595	-0.088603	4.818112
449.693165	8000.243134	10.977600	-0.088622	4.818107
449.555323	8000.218058	10.982605	-0.088596	4.818100
449.557873	8000.246516	10.987610	-0.088596	4.818109
449.278351	8000.251034	10.992615	-0.088544	4.818111
449.455621	8000.211417	10.997619	-0.088578	4.818099
449.656397	8000.297373	11.002624	-0.088615	4.818123
449.529079	8000.229292	11.007629	-0.088591	4.818104
449.720103	8000.271961	11.012634	-0.088627	4.818116
449.645685	8000.269873	11.017639	-0.088613	4.818115
449.324127	8000.248545	11.022643	-0.088553	4.818110
449.646180	8000.265679	11.027648	-0.088613	4.818114
449.664420	8000.242784	11.032653	-0.088617	4.818107
449.682003	8000.257769	11.037658	-0.088620	4.818112
449.461642	8000.201019	11.042663	-0.088579	4.818096
449.613903	8000.210518	11.047667	-0.088608	4.818098
449.681832	8000.272516	11.052672	-0.088620	4.818116
449.559547	8000.233975	11.057677	-0.088598	4.818105
449.633324	8000.271847	11.062682	-0.088611	4.818116
449.555940	8000.233934	11.067687	-0.088597	4.818105
449.685656	8000.217859	11.072691	-0.088621	4.818100
449.621592	8000.266435	11.077696	-0.088609	4.818114
449.613214	8000.213699	11.082701	-0.088608	4.818099
449.745691	8000.247129	11.087706	-0.088633	4.818108
449.571528	8000.224703	11.092711	-0.088600	4.818102
449.524334	8000.244045	11.097715	-0.088592	4.818108
449.711296	8000.264555	11.102720	-0.088626	4.818113
449.548069	8000.246491	11.107725	-0.088596	4.818109
449.258462	8000.318228	11.112730	-0.088542	4.818131
449.328856	8000.289747	11.117735	-0.088555	4.818123
449.372164	8000.305091	11.122739	-0.088564	4.818127
449.161010	8000.327405	11.127744	-0.088524	4.818134
449.328478	8000.273968	11.132749	-0.088556	4.818118
449.643986	8000.244702	11.137754	-0.088614	4.818108
449.396309	8000.252824	11.142759	-0.088568	4.818111
449.411012	8000.297238	11.147763	-0.088571	4.818124
449.642151	8000.271003	11.152768	-0.088614	4.818116
449.581021	8000.244894	11.157773	-0.088603	4.818108
449.495939	8000.265812	11.162778	-0.088587	4.818115
449.572572	8000.251100	11.167783	-0.088601	4.818110
449.475985	8000.265542	11.172787	-0.088584	4.818115
449.646264	8000.292134	11.177792	-0.088615	4.818122
449.518936	8000.241945	11.182797	-0.088592	4.818108
449.807181	8000.277552	11.187802	-0.088645	4.818117
449.652456	8000.240663	11.192807	-0.088617	4.818107
449.637041	8000.237294	11.197811	-0.088614	4.818106
449.656498	8000.300720	11.202816	-0.088618	4.818124
449.605992	8000.203191	11.207821	-0.088608	4.818096
449.541273	8000.244390	11.212826	-0.088596	4.818108
449.653637	8000.245965	11.217831	-0.088617	4.818108
449.630302	8000.229856	11.222835	-0.088613	4.818103
449.659075	8000.251313	11.227840	-0.088618	4.818110
449.730511	8000.254421	11.232845	-0.088632	4.818110
449.650108	8000.300664	11.237850	-0.088617	4.818124
449.713410	8000.262611	11.242855	-0.088629	4.818113
449.757920	8000.219033	11.247859	-0.088637	4.818100
450.059053	8000.240086	11.252864	-0.088693	4.818105
449.992699	8000.224429	11.257869	-0.088681	4.818100
449.643117	8000.260595	11.262874	-0.088616	4.818113
449.722735	8000.276447	11.267879	-0.088631	4.818117
449.727691	8000.291256	11.272883	-0.088632	4.818121
449.718199	8000.272183	11.277888	-0.088630	4.818116
449.735046	8000.228219	11.282893	-0.088633	4.818103
449.957929	8000.270281	11.287898	-0.088675	4.818114
449.876243	8000.263881	11.292903	-0.088660	4.818113
449.587580	8000.290374	11.297907	-0.088606	4.818122
449.815221	8000.290403	11.302912	-0.088648	4.818121
449.730956	8000.272390	11.307917	-0.088633	4.818116
449.733706	8000.318742	11.312922	-0.088633	4.818129
449.642812	8000.293270	11.317927	-0.088616	4.818122
449.809311	8000.247187	11.322931	-0.088647	4.818108
449.765379	8000.307622	11.327936	-0.088639	4.818126
449.497740	8000.270207	11.332941	-0.088590	4.818116
449.618924	8000.326634	11.337946	-0.088612	4.818132
449.857092	8000.238401	11.342951	-0.088657	4.818105
449.900250	8000.236904	11.347955	-0.088665	4.818104
449.695075	8000.302453	11.352960	-0.088627	4.818125
449.754934	8000.274877	11.357965	-0.088638	4.818116
449.923777	8000.262506	11.362970	-0.088669	4.818112
449.904707	8000.285399	11.367975	-0.088666	4.818119
450.009396	8000.308970	11.372979	-0.088685	4.818125
450.046070	8000.273702	11.377984	-0.088692	4.818115
449.544465	8000.270907	11.382989	-0.088599	4.818116
449.805102	8000.245084	11.387994	-0.088647	4.818107
449.709644	8000.251122	11.392999	-0.088630	4.818109
449.661059	8000.293600	11.398003	-0.088621	4.818122
449.751858	8000.288559	11.403008	-0.088638	4.818120
449.766299	8000.272978	11.408013	-0.088641	4.818116
449.944845	8000.288108	11.413018	-0.088674	4.818119
449.878999	8000.261932	11.418023	-0.088662	4.818112
449.662392	8000.210496	11.423027	-0.088621	4.818098
450.024191	8000.263971	11.428032	-0.088689	4.818112
449.958936	8000.218859	11.433037	-0.088677	4.818099
449.991835	8000.259318	11.438042	-0.088683	4.818111
450.006792	8000.231115	11.443047	-0.088686	4.818102
449.927334	8000.172122	11.448051	-0.088671	4.818085
449.994968	8000.258324	11.453056	-0.088684	4.818110
450.068121	8000.235143	11.458061	-0.088697	4.818103
450.151881	8000.250001	11.463066	-0.088713	4.818107
449.993664	8000.267792	11.468071	-0.088684	4.818113
449.965753	8000.256882	11.473075	-0.088678	4.818110
449.905216	8000.270775	11.478080	-0.088667	4.818114
450.003064	8000.227943	11.483085	-0.088686	4.818101
450.132890	8000.240287	11.488090	-0.088710	4.818104
450.156764	8000.254308	11.493095	-0.088714	4.818108
449.916568	8000.190963	11.498099	-0.088670	4.818091
450.185436	8000.268400	11.503104	-0.088720	4.818113
450.165147	8000.235494	11.508109	-0.088716	4.818103
450.138350	8000.280382	11.513114	-0.088711	4.818116
449.966744	8000.261148	11.518119	-0.088679	4.818111
449.955086	8000.247307	11.523123	-0.088677	4.818107
450.211508	8000.272998	11.528128	-0.088725	4.818114
450.058131	8000.255072	11.533133	-0.088696	4.818109
450.302465	8000.276384	11.538138	-0.088742	4.818114
450.018581	8000.239793	11.543143	-0.088689	4.818105
449.971894	8000.219148	11.548147	-0.088681	4.818099
450.152228	8000.246933	11.553152	-0.088714	4.818106
450.068276	8000.199455	11.558157	-0.088699	4.818093
450.174938	8000.243050	11.563162	-0.088719	4.818105
450.226846	8000.241675	11.568167	-0.088728	4.818104
450.133760	8000.228802	11.573171	-0.088711	4.818101
450.330297	8000.283126	11.578176	-0.088748	4.818116
450.119512	8000.274922	11.583181	-0.088708	4.818115
449.998240	8000.291124	11.588186	-0.088686	4.818120
450.006216	8000.296502	11.593191	-0.088688	4.818122
449.985612	8000.203600	11.598195	-0.088684	4.818094
449.967634	8000.259135	11.603200	-0.088680	4.818111
449.840873	8000.241581	11.608205	-0.088657	4.818106
450.164876	8000.270321	11.613210	-0.088717	4.818113
449.843384	8000.290040	11.618215	-0.088658	4.818120
449.538699	8000.253160	11.623219	-0.088601	4.818111
449.937581	8000.280841	11.628224	-0.088675	4.818117
449.659754	8000.265385	11.633229	-0.088624	4.818114
449.766809	8000.241627	11.638234	-0.088643	4.818106
449.900283	8000.244549	11.643239	-0.088668	4.818107
449.812697	8000.262274	11.648243	-0.088652	4.818112
450.066419	8000.265825	11.653248	-0.088699	4.818112
449.941526	8000.238825	11.658253	-0.088676	4.818105
450.117137	8000.253914	11.663258	-0.088709	4.818108
450.116264	8000.242329	11.668263	-0.088709	4.818105
450.032700	8000.233798	11.673267	-0.088693	4.818103
450.218825	8000.283767	11.678272	-0.088728	4.818117
449.899932	8000.264579	11.683277	-0.088669	4.818113
449.868014	8000.290450	11.688282	-0.088663	4.818120
450.159178	8000.255582	11.693287	-0.088717	4.818109
449.973879	8000.256154	11.698291	-0.088683	4.818110
450.147423	8000.248060	11.703296	-0.088715	4.818107
450.082728	8000.252423	11.708301	-0.088703	4.818108
450.220556	8000.269089	11.713306	-0.088729	4.818113
450.185704	8000.280184	11.718311	-0.088723	4.818116
450.122975	8000.246684	11.723315	-0.088711	4.818106
449.989852	8000.295348	11.728320	-0.088686	4.818121
449.754716	8000.298381	11.733325	-0.088642	4.818123
450.034671	8000.262304	11.738330	-0.088695	4.818111
450.395399	8000.232619	11.743335	-0.088762	4.818101
450.431302	8000.193130	11.748339	-0.088769	4.818089
450.386465	8000.272498	11.753344	-0.088760	4.818113
450.264790	8000.253962	11.758349	-0.088738	4.818108
450.326896	8000.257992	11.763354	-0.088749	4.818109
450.208669	8000.242662	11.768359	-0.088727	4.818105
450.107223	8000.178099	11.773363	-0.088709	4.818086
450.361661	8000.261650	11.778368	-0.088756	4.818110
450.230062	8000.249290	11.783373	-0.088732	4.818107
450.415328	8000.245570	11.788378	-0.088766	4.818105
450.484633	8000.228651	11.793383	-0.088779	4.818099
450.371944	8000.217608	11.798387	-0.088758	4.818097
450.274349	8000.265715	11.803392	-0.088740	4.818111
450.011406	8000.264150	11.808397	-0.088691	4.818112
450.244153	8000.287405	11.813402	-0.088735	4.818118
450.339390	8000.271901	11.818407	-0.088752	4.818113
450.162712	8000.234704	11.823411	-0.088720	4.818103
450.359661	8000.291139	11.828416	-0.088756	4.818118
450.299933	8000.253471	11.833421	-0.088745	4.818108
450.179605	8000.284421	11.838426	-0.088723	4.818117
450.449761	8000.293465	11.843431	-0.088773	4.818119
450.383062	8000.271488	11.848435	-0.088761	4.818113
450.326968	8000.273866	11.853440	-0.088751	4.818113
450.282526	8000.255356	11.858445	-0.088742	4.818108
450.454483	8000.251450	11.863450	-0.088774	4.818106
450.465036	8000.298965	11.868455	-0.088776	4.818120
450.187689	8000.250887	11.873459	-0.088725	4.818107
450.365780	8000.291272	11.878464	-0.088758	4.818118
450.351423	8000.270026	11.883469	-0.088755	4.818112
450.299498	8000.293512	11.888474	-0.088746	4.818119
450.181068	8000.276074	11.893479	-0.088724	4.818115
450.223325	8000.292457	11.898483	-0.088732	4.818119
450.194675	8000.253118	11.903488	-0.088726	4.818108
450.079730	8000.243096	11.908493	-0.088705	4.818105
450.242352	8000.271687	11.913498	-0.088736	4.818113
450.387203	8000.272664	11.918503	-0.088763	4.818113
450.257784	8000.236127	11.923507	-0.088738	4.818103
450.273169	8000.295287	11.928512	-0.088741	4.818120
450.344176	8000.241554	11.933517	-0.088755	4.818104
450.356712	8000.276466	11.938522	-0.088757	4.818114
450.403342	8000.270808	11.943527	-0.088766	4.818112
450.368474	8000.256643	11.948531	-0.088759	4.818108
450.501900	8000.273248	11.953536	-0.088784	4.818113
450.313272	8000.236935	11.958541	-0.088749	4.818103
450.309288	8000.246357	11.963546	-0.088749	4.818105
450.282756	8000.275461	11.968551	-0.088744	4.818114
450.060558	8000.294462	11.973555	-0.088702	4.818121
450.398451	8000.291823	11.978560	-0.088765	4.818118
450.577820	8000.251182	11.983565	-0.088799	4.818106
450.519089	8000.288256	11.988570	-0.088788	4.818117
450.231611	8000.290557	11.993575	-0.088735	4.818119
450.321248	8000.318127	11.998579	-0.088751	4.818127
450.376007	8000.310477	12.003584	-0.088762	4.818124
450.181791	8000.268824	12.008589	-0.088725	4.818113
450.129369	8000.299671	12.013594	-0.088716	4.818122
450.238330	8000.285412	12.018599	-0.088736	4.818117
450.244056	8000.274971	12.023603	-0.088737	4.818114
450.239001	8000.290693	12.028608	-0.088736	4.818119
450.064249	8000.301937	12.033613	-0.088704	4.818123
449.941218	8000.326535	12.038618	-0.088681	4.818131
449.997829	8000.298913	12.043623	-0.088692	4.818122
449.993972	8000.316757	12.048627	-0.088691	4.818128
449.993879	8000.322022	12.053632	-0.088691	4.818129
450.111280	8000.276306	12.058637	-0.088713	4.818115
450.093511	8000.331845	12.063642	-0.088710	4.818132
449.857919	8000.345396	12.068647	-0.088666	4.818137
449.847238	8000.336831	12.073651	-0.088664	4.818134
450.035673	8000.340523	12.078656	-0.088699	4.818134
450.031706	8000.329947	12.083661	-0.088698	4.818131
450.168234	8000.328703	12.088666	-0.088724	4.818130
450.122139	8000.333326	12.093671	-0.088715	4.818132
449.896977	8000.345970	12.098675	-0.088674	4.818137
449.832586	8000.368230	12.103680	-0.088662	4.818143
449.647008	8000.328803	12.108685	-0.088627	4.818133
449.598990	8000.343924	12.113690	-0.088618	4.818137
449.821220	8000.348088	12.118695	-0.088660	4.818137
449.942982	8000.299274	12.123699	-0.088682	4.818123
449.960214	8000.324780	12.128704	-0.088686	4.818130
449.905203	8000.301913	12.133709	-0.088676	4.818123
449.892102	8000.325942	12.138714	-0.088673	4.818131
450.002451	8000.304334	12.143719	-0.088694	4.818124
449.793663	8000.339311	12.148723	-0.088655	4.818135
450.042344	8000.331214	12.153728	-0.088701	4.818132
449.853103	8000.305419	12.158733	-0.088666	4.818125
449.802759	8000.356292	12.163738	-0.088657	4.818140
449.826157	8000.356624	12.168743	-0.088661	4.818140
449.908320	8000.304099	12.173747	-0.088677	4.818124
449.974387	8000.329235	12.178752	-0.088689	4.818131
449.983618	8000.305161	12.183757	-0.088691	4.818124
450.284114	8000.313577	12.188762	-0.088747	4.818125
450.207464	8000.290407	12.193767	-0.088733	4.818119
450.163944	8000.292961	12.198771	-0.088724	4.818120
450.478774	8000.307892	12.203776	-0.088783	4.818123
450.046516	8000.312379	12.208781	-0.088703	4.818126
450.189020	8000.295431	12.213786	-0.088729	4.818120
450.310731	8000.290822	12.218791	-0.088752	4.818118
450.268741	8000.290240	12.223795	-0.088744	4.818118
450.423850	8000.279783	12.228800	-0.088773	4.818115
450.315515	8000.297218	12.233805	-0.088753	4.818120
450.274459	8000.329276	12.238810	-0.088746	4.818130
450.346575	8000.302924	12.243815	-0.088759	4.818122
450.259208	8000.302760	12.248819	-0.088743	4.818122
450.319445	8000.332024	12.253824	-0.088754	4.818131
450.266246	8000.255505	12.258829	-0.088744	4.818108
450.180757	8000.302730	12.263834	-0.088728	4.818123
450.254004	8000.312179	12.268839	-0.088742	4.818125
450.351920	8000.279872	12.273843	-0.088760	4.818115
450.182747	8000.329084	12.278848	-0.088729	4.818130
450.262575	8000.239690	12.283853	-0.088744	4.818103
450.213765	8000.271640	12.288858	-0.088735	4.818113
450.571420	8000.296642	12.293863	-0.088802	4.818119
450.137025	8000.297941	12.298867	-0.088721	4.818121
450.437215	8000.318983	12.303872	-0.088777	4.818126
450.249484	8000.265843	12.308877	-0.088742	4.818111
450.426394	8000.284108	12.313882	-0.088775	4.818116
450.540244	8000.309913	12.318887	-0.088796	4.818123
450.671005	8000.309641	12.323891	-0.088820	4.818123
450.291827	8000.328551	12.328896	-0.088750	4.818130
450.482148	8000.317534	12.333901	-0.088785	4.818126
450.460428	8000.319340	12.338906	-0.088781	4.818126
450.453870	8000.300308	12.343911	-0.088780	4.818121
450.380704	8000.255085	12.348915	-0.088767	4.818108
450.698577	8000.298477	12.353920	-0.088826	4.818119
450.485016	8000.304968	12.358925	-0.088786	4.818122
450.620089	8000.315281	12.363930	-0.088812	4.818124
450.473262	8000.297445	12.368935	-0.088784	4.818120
450.445374	8000.249697	12.373939	-0.088779	4.818106
450.515892	8000.290683	12.378944	-0.088792	4.818118
450.461174	8000.228878	12.383949	-0.088782	4.818099
450.453004	8000.281393	12.388954	-0.088781	4.818115
450.486181	8000.272389	12.393959	-0.088787	4.818112
450.447774	8000.221337	12.398963	-0.088780	4.818097
450.768056	8000.310020	12.403968	-0.088840	4.818122
450.709387	8000.254474	12.408973	-0.088829	4.818106
450.642168	8000.291429	12.413978	-0.088816	4.818117
450.558802	8000.300793	12.418983	-0.088801	4.818120
450.657797	8000.289552	12.423987	-0.088819	4.818117
450.674546	8000.318209	12.428992	-0.088822	4.818125
450.641155	8000.286171	12.433997	-0.088816	4.818116
450.585073	8000.254869	12.439002	-0.088806	4.818107
450.620422	8000.269051	12.444007	-0.088813	4.818111
450.517673	8000.262356	12.449011	-0.088793	4.818109
450.784500	8000.294510	12.454016	-0.088843	4.818118
450.839300	8000.290018	12.459021	-0.088853	4.818116
450.703710	8000.250236	12.464026	-0.088828	4.818105
450.542170	8000.274295	12.469031	-0.088798	4.818113
450.513085	8000.299154	12.474035	-0.088793	4.818120
450.616206	8000.261657	12.479040	-0.088812	4.818108
450.669560	8000.281353	12.484045	-0.088822	4.818114
450.617702	8000.285895	12.489050	-0.088813	4.818116
450.690247	8000.256391	12.494055	-0.088826	4.818107
450.661997	8000.207586	12.499059	-0.088821	4.818092
450.770857	8000.267001	12.504064	-0.088841	4.818109
450.905007	8000.241516	12.509069	-0.088866	4.818101
450.801070	8000.260065	12.514074	-0.088847	4.818107
450.734888	8000.300192	12.519079	-0.088835	4.818119
450.738293	8000.293929	12.524083	-0.088836	4.818118
450.854392	8000.306083	12.529088	-0.088857	4.818121
450.494474	8000.286320	12.534093	-0.088790	4.818116
450.635101	8000.311446	12.539098	-0.088816	4.818123
450.754433	8000.313119	12.544103	-0.088839	4.818123
450.775476	8000.282895	12.549107	-0.088843	4.818114
450.765770	8000.324865	12.554112	-0.088841	4.818127
450.676295	8000.298358	12.559117	-0.088824	4.818119
450.801016	8000.302212	12.564122	-0.088848	4.818120
450.706789	8000.286164	12.569127	-0.088830	4.818115
450.662268	8000.260286	12.574131	-0.088822	4.818108
450.934588	8000.294621	12.579136	-0.088873	4.818117
450.648358	8000.269573	12.584141	-0.088819	4.818111
450.706286	8000.239865	12.589146	-0.088830	4.818102
450.922008	8000.247096	12.594151	-0.088871	4.818103
450.676395	8000.219459	12.599155	-0.088825	4.818096
450.765701	8000.296493	12.604160	-0.088842	4.818118
450.901749	8000.267877	12.609165	-0.088867	4.818109
450.906813	8000.281635	12.614170	-0.088868	4.818113
450.667474	8000.273031	12.619175	-0.088823	4.818112
450.430545	8000.293931	12.624179	-0.088779	4.818119
450.724972	8000.314892	12.629184	-0.088834	4.818124
450.669492	8000.276231	12.634189	-0.088824	4.818113
450.744165	8000.267807	12.639194	-0.088838	4.818110
450.922002	8000.275561	12.644199	-0.088871	4.818111
450.831822	8000.225889	12.649203	-0.088854	4.818097
450.889418	8000.276167	12.654208	-0.088865	4.818112
450.824196	8000.236317	12.659213	-0.088853	4.818100
450.886777	8000.224566	12.664218	-0.088865	4.818096
450.738137	8000.260383	12.669223	-0.088837	4.818108
450.761872	8000.254405	12.674227	-0.088842	4.818106
450.910935	8000.279649	12.679232	-0.088870	4.818113
450.669760	8000.241549	12.684237	-0.088825	4.818102
450.738565	8000.247778	12.689242	-0.088838	4.818104
450.803458	8000.293948	12.694247	-0.088850	4.818117
450.590364	8000.286763	12.699251	-0.088810	4.818116
450.588798	8000.323584	12.704256	-0.088810	4.818127
450.721328	8000.297024	12.709261	-0.088835	4.818118
450.537161	8000.333396	12.714266	-0.088800	4.818130
450.519723	8000.279479	12.719271	-0.088797	4.818114
450.613871	8000.275538	12.724275	-0.088815	4.818113
451.007265	8000.269466	12.729280	-0.088888	4.818109
450.809309	8000.278280	12.734285	-0.088851	4.818113
450.828058	8000.259601	12.739290	-0.088855	4.818107
450.719797	8000.255987	12.744295	-0.088835	4.818106
450.893068	8000.236312	12.749299	-0.088867	4.818100
450.732342	8000.311955	12.754304	-0.088837	4.818123
450.658135	8000.264612	12.759309	-0.088824	4.818109
450.773153	8000.300958	12.764314	-0.088845	4.818119
450.856797	8000.289502	12.769319	-0.088861	4.818116
450.820385	8000.252159	12.774323	-0.088854	4.818105
450.806248	8000.287752	12.779328	-0.088851	4.818115
450.614213	8000.281914	12.784333	-0.088816	4.818114
450.654067	8000.296159	12.789338	-0.088823	4.818118
450.622212	8000.304138	12.794343	-0.088817	4.818121
450.738744	8000.297352	12.799347	-0.088839	4.818118
450.793002	8000.283380	12.804352	-0.088849	4.818114
450.769648	8000.257798	12.809357	-0.088845	4.818107
450.497977	8000.309787	12.814362	-0.088794	4.818123
450.527956	8000.286003	12.819367	-0.088800	4.818116
450.606280	8000.252370	12.824371	-0.088815	4.818106
450.712347	8000.286486	12.829376	-0.088834	4.818115
450.774850	8000.236844	12.834381	-0.088846	4.818100
450.853634	8000.266368	12.839386	-0.088861	4.818109
450.815514	8000.267945	12.844391	-0.088854	4.818109
450.820694	8000.263812	12.849395	-0.088855	4.818108
451.016625	8000.311815	12.854400	-0.088891	4.818122
450.808215	8000.283645	12.859405	-0.088853	4.818114
450.845757	8000.299962	12.864410	-0.088860	4.818119
450.906048	8000.313440	12.869415	-0.088871	4.818123
450.623019	8000.242126	12.874419	-0.088818	4.818103
450.767137	8000.303087	12.879424	-0.088845	4.818120
450.630071	8000.250654	12.884429	-0.088820	4.818105
450.541416	8000.289415	12.889434	-0.088803	4.818117
450.714800	8000.297107	12.894439	-0.088836	4.818118
450.723446	8000.305652	12.899443	-0.088837	4.818121
450.641943	8000.306622	12.904448	-0.088822	4.818122
450.539987	8000.283099	12.909453	-0.088803	4.818115
450.750275	8000.286044	12.914458	-0.088843	4.818115
450.561402	8000.274987	12.919463	-0.088808	4.818113
450.447251	8000.292341	12.924467	-0.088786	4.818118
450.543641	8000.336847	12.929472	-0.088804	4.818131
450.878069	8000.276272	12.934477	-0.088867	4.818112
450.960386	8000.239537	12.939482	-0.088882	4.818100
450.783748	8000.265490	12.944487	-0.088849	4.818109
450.699028	8000.272730	12.949491	-0.088834	4.818111
450.861964	8000.286591	12.954496	-0.088864	4.818115
450.819320	8000.233373	12.959501	-0.088856	4.818099
451.000046	8000.239063	12.964506	-0.088890	4.818100
450.990567	8000.246303	12.969511	-0.088888	4.818102
450.837304	8000.255742	12.974515	-0.088860	4.818106
450.973741	8000.295545	12.979520	-0.088885	4.818117
450.979012	8000.250365	12.984525	-0.088886	4.818103
450.928737	8000.251772	12.989530	-0.088877	4.818104
450.975549	8000.284007	12.994535	-0.088886	4.818113
450.851771	8000.252810	12.999539	-0.088863	4.818105
450.877977	8000.288967	13.004544	-0.088868	4.818115
450.712512	8000.266660	13.009549	-0.088837	4.818109
450.831933	8000.257809	13.014554	-0.088859	4.818106
450.878803	8000.303728	13.019559	-0.088868	4.818120
450.944638	8000.260447	13.024563	-0.088880	4.818107
451.010189	8000.298207	13.029568	-0.088892	4.818118
450.988250	8000.287380	13.034573	-0.088888	4.818114
450.956396	8000.295359	13.039578	-0.088883	4.818117
450.762332	8000.285282	13.044583	-0.088846	4.818115
450.964785	8000.266015	13.049587	-0.088884	4.818108
450.954097	8000.259555	13.054592	-0.088882	4.818106
450.848482	8000.263346	13.059597	-0.088863	4.818108
450.864819	8000.275156	13.064602	-0.088866	4.818111
450.753268	8000.268339	13.069607	-0.088845	4.818110
450.933575	8000.199294	13.074611	-0.088879	4.818088
450.995674	8000.265423	13.079616	-0.088890	4.818108
450.863505	8000.236214	13.084621	-0.088866	4.818100
450.946570	8000.270008	13.089626	-0.088881	4.818109
450.850563	8000.283405	13.094631	-0.088864	4.818114
450.845588	8000.246503	13.099635	-0.088863	4.818103
450.948314	8000.246891	13.104640	-0.088882	4.818103
450.777429	8000.276082	13.109645	-0.088850	4.818112
450.864907	8000.246787	13.114650	-0.088866	4.818103
450.899692	8000.287274	13.119655	-0.088873	4.818115
450.807255	8000.238622	13.124659	-0.088856	4.818101
450.675662	8000.269415	13.129664	-0.088831	4.818110
451.077387	8000.218201	13.134669	-0.088906	4.818093
451.028162	8000.263829	13.139674	-0.088897	4.818107
451.064877	8000.216983	13.144679	-0.088904	4.818093
450.997930	8000.236050	13.149683	-0.088892	4.818099
450.947622	8000.321658	13.154688	-0.088882	4.818125
450.936610	8000.213099	13.159693	-0.088880	4.818093
450.979915	8000.289490	13.164698	-0.088889	4.818115
451.021100	8000.282703	13.169703	-0.088896	4.818113
450.914495	8000.240169	13.174707	-0.088876	4.818101
450.971027	8000.279907	13.179712	-0.088887	4.818112
450.854456	8000.240391	13.184717	-0.088865	4.818101
450.892795	8000.193569	13.189722	-0.088873	4.818087
450.923029	8000.231887	13.194727	-0.088878	4.818098
450.813642	8000.235625	13.199731	-0.088858	4.818100
450.828937	8000.290574	13.204736	-0.088861	4.818116
450.831332	8000.213779	13.209741	-0.088861	4.818093
450.647961	8000.232270	13.214746	-0.088827	4.818099
450.778575	8000.274096	13.219751	-0.088852	4.818111
450.810717	8000.246133	13.224755	-0.088858	4.818103
450.720647	8000.284873	13.229760	-0.088841	4.818115
450.859641	8000.282612	13.234765	-0.088867	4.818113
450.887767	8000.294587	13.239770	-0.088872	4.818117
450.802874	8000.306035	13.244775	-0.088857	4.818121
450.614445	8000.272882	13.249779	-0.088822	4.818112
450.608235	8000.304375	13.254784	-0.088820	4.818121
450.630242	8000.267850	13.259789	-0.088825	4.818110
450.675265	8000.272694	13.264794	-0.088833	4.818111
450.691504	8000.282398	13.269799	-0.088836	4.818114
450.562578	8000.224817	13.274803	-0.088812	4.818098
450.591745	8000.253648	13.279808	-0.088818	4.818106
450.557620	8000.221600	13.284813	-0.088811	4.818097
450.861250	8000.262688	13.289818	-0.088868	4.818108
450.902804	8000.225383	13.294823	-0.088876	4.818096
450.782259	8000.198442	13.299827	-0.088853	4.818089
450.951130	8000.282904	13.304832	-0.088885	4.818113
450.962648	8000.249390	13.309837	-0.088887	4.818103
450.870118	8000.197580	13.314842	-0.088870	4.818088
450.924307	8000.247810	13.319847	-0.088880	4.818103
450.807460	8000.287229	13.324851	-0.088858	4.818115
450.882897	8000.299867	13.329856	-0.088873	4.818118
450.723692	8000.255544	13.334861	-0.088843	4.818106
450.837904	8000.192943	13.339866	-0.088864	4.818087
450.953811	8000.245089	13.344871	-0.088886	4.818102
450.854971	8000.199506	13.349875	-0.088868	4.818089
451.006477	8000.275305	13.354880	-0.088896	4.818111
451.000313	8000.278381	13.359885	-0.088895	4.818112
450.703020	8000.300542	13.364890	-0.088839	4.818119
450.684599	8000.287659	13.369895	-0.088836	4.818116
450.931155	8000.227960	13.374899	-0.088882	4.818097
450.956554	8000.270421	13.379904	-0.088887	4.818109
450.919126	8000.254114	13.384909	-0.088880	4.818105
450.992750	8000.305669	13.389914	-0.088894	4.818120
450.704709	8000.289016	13.394919	-0.088840	4.818116
450.758153	8000.252930	13.399923	-0.088850	4.818105
450.852690	8000.287937	13.404928	-0.088868	4.818115
450.822454	8000.267521	13.409933	-0.088862	4.818109
450.547923	8000.253162	13.414938	-0.088811	4.818106
450.686138	8000.294042	13.419943	-0.088837	4.818118
450.649623	8000.226176	13.424947	-0.088830	4.818098
450.539734	8000.283584	13.429952	-0.088810	4.818115
450.781640	8000.250134	13.434957	-0.088855	4.818104
450.747853	8000.181253	13.439962	-0.088849	4.818084
450.887866	8000.262154	13.444967	-0.088875	4.818107
450.833127	8000.206662	13.449971	-0.088865	4.818091
451.052196	8000.245516	13.454976	-0.088906	4.818102
451.021025	8000.162988	13.459981	-0.088900	4.818077
450.941576	8000.131359	13.464986	-0.088885	4.818068
450.915938	8000.219416	13.469991	-0.088880	4.818094
450.864024	8000.165017	13.474995	-0.088871	4.818078
451.080182	8000.272244	13.480000	-0.088911	4.818109
450.865261	8000.262928	13.485005	-0.088871	4.818108
450.954533	8000.245235	13.490010	-0.088888	4.818102
451.230854	8000.214371	13.495015	-0.088939	4.818092
450.989321	8000.203631	13.500019	-0.088894	4.818089
451.048747	8000.209729	13.505024	-0.088906	4.818091
451.011892	8000.194483	13.510029	-0.088899	4.818087
450.989610	8000.206806	13.515034	-0.088895	4.818090
450.964684	8000.241195	13.520039	-0.088890	4.818101
450.882596	8000.200057	13.525043	-0.088875	4.818089
451.129232	8000.237191	13.530048	-0.088921	4.818099
450.941736	8000.221943	13.535053	-0.088886	4.818095
451.030099	8000.224236	13.540058	-0.088903	4.818095
451.047092	8000.272895	13.545063	-0.088906	4.818110
450.948002	8000.238885	13.550067	-0.088887	4.818100
451.206958	8000.259352	13.555072	-0.088936	4.818105
451.057362	8000.268842	13.560077	-0.088908	4.818108
451.076438	8000.261746	13.565082	-0.088911	4.818106
451.052672	8000.294047	13.570087	-0.088907	4.818116
451.021499	8000.256777	13.575091	-0.088901	4.818105
451.194582	8000.305514	13.580096	-0.088934	4.818119
451.269630	8000.249731	13.585101	-0.088948	4.818102
450.827670	8000.286709	13.590106	-0.088865	4.818115
450.760513	8000.291037	13.595111	-0.088853	4.818116
450.680252	8000.281499	13.600115	-0.088838	4.818114
450.849179	8000.290181	13.605120	-0.088870	4.818116
450.792430	8000.299917	13.610125	-0.088859	4.818119
450.765776	8000.289024	13.615130	-0.088854	4.818116
450.860830	8000.280886	13.620135	-0.088872	4.818113
450.953138	8000.219030	13.625139	-0.088889	4.818094
451.131443	8000.227843	13.630144	-0.088923	4.818096
451.065114	8000.250076	13.635149	-0.088910	4.818103
450.974162	8000.256176	13.640154	-0.088893	4.818105
451.042236	8000.291866	13.645159	-0.088906	4.818115
451.016698	8000.231520	13.650163	-0.088901	4.818098
451.124452	8000.262502	13.655168	-0.088922	4.818106
451.163659	8000.282001	13.660173	-0.088929	4.818112
450.962840	8000.270777	13.665178	-0.088892	4.818109
450.963926	8000.268692	13.670183	-0.088892	4.818109
450.840135	8000.285910	13.675187	-0.088869	4.818114
451.091947	8000.251546	13.680192	-0.088916	4.818103
451.193420	8000.265600	13.685197	-0.088935	4.818107
451.090238	8000.263109	13.690202	-0.088916	4.818107
451.175064	8000.257985	13.695207	-0.088931	4.818105
451.012753	8000.292558	13.700211	-0.088901	4.818116
451.131644	8000.315276	13.705216	-0.088924	4.818122
451.028494	8000.288578	13.710221	-0.088904	4.818114
450.920608	8000.297599	13.715226	-0.088884	4.818118
451.093552	8000.266341	13.720231	-0.088917	4.818108
451.168068	8000.257915	13.725235	-0.088931	4.818105
451.086168	8000.237829	13.730240	-0.088915	4.818099
450.952893	8000.254916	13.735245	-0.088891	4.818105
451.073479	8000.197666	13.740250	-0.088913	4.818087
451.199361	8000.274160	13.745255	-0.088937	4.818109
451.108710	8000.239216	13.750259	-0.088920	4.818099
451.048565	8000.291006	13.755264	-0.088909	4.818115
451.067934	8000.259706	13.760269	-0.088912	4.818106
451.010080	8000.255744	13.765274	-0.088902	4.818105
451.005635	8000.262001	13.770279	-0.088901	4.818107
450.924650	8000.219825	13.775283	-0.088886	4.818094
450.930850	8000.313591	13.780288	-0.088887	4.818122
450.938875	8000.260029	13.785293	-0.088889	4.818106
450.760883	8000.298593	13.790298	-0.088856	4.818118
450.813970	8000.304603	13.795303	-0.088866	4.818120
450.828378	8000.283759	13.800307	-0.088868	4.818114
451.017307	8000.281143	13.805312	-0.088903	4.818112
450.864452	8000.279010	13.810317	-0.088875	4.818112
450.701706	8000.303052	13.815322	-0.088845	4.818120
450.684069	8000.305967	13.820327	-0.088842	4.818121
450.837749	8000.254443	13.825331	-0.088870	4.818105
451.137046	8000.246003	13.830336	-0.088926	4.818101
450.698410	8000.291447	13.835341	-0.088844	4.818117
450.741598	8000.296265	13.840346	-0.088853	4.818118
450.824828	8000.313222	13.845351	-0.088868	4.818123
450.968797	8000.266824	13.850355	-0.088895	4.818108
451.023533	8000.310748	13.855360	-0.088905	4.818121
450.787044	8000.295867	13.860365	-0.088861	4.818118
450.843100	8000.321916	13.865370	-0.088872	4.818125
451.026983	8000.293970	13.870375	-0.088906	4.818116
450.892121	8000.285773	13.875379	-0.088881	4.818114
451.280853	8000.309108	13.880384	-0.088954	4.818119
450.868492	8000.287557	13.885389	-0.088877	4.818115
451.015148	8000.296981	13.890394	-0.088904	4.818117
451.003038	8000.307341	13.895399	-0.088902	4.818120
450.638887	8000.284361	13.900403	-0.088834	4.818115
450.657018	8000.322509	13.905408	-0.088838	4.818126
450.645265	8000.276039	13.910413	-0.088836	4.818112
450.904502	8000.260723	13.915418	-0.088884	4.818107
450.916509	8000.267211	13.920423	-0.088886	4.818108
450.898387	8000.243807	13.925427	-0.088883	4.818102
451.176489	8000.258226	13.930432	-0.088935	4.818105
451.083422	8000.254824	13.935437	-0.088917	4.818104
451.018644	8000.312864	13.940442	-0.088905	4.818122
451.213365	8000.287174	13.945447	-0.088942	4.818113
451.161633	8000.270668	13.950451	-0.088932	4.818108
451.036934	8000.307872	13.955456	-0.088909	4.818120
450.985875	8000.218750	13.960461	-0.088900	4.818094
451.328885	8000.236182	13.965466	-0.088963	4.818098
451.181346	8000.272015	13.970471	-0.088936	4.818109
450.912840	8000.243004	13.975475	-0.088886	4.818101
450.935554	8000.259114	13.980480	-0.088890	4.818106
451.099828	8000.249838	13.985485	-0.088921	4.818103
450.950832	8000.267757	13.990490	-0.088893	4.818108
450.815134	8000.303755	13.995495	-0.088868	4.818120
450.783035	8000.291733	14.000499	-0.088862	4.818116
451.069900	8000.287329	14.005504	-0.088916	4.818114
451.059406	8000.270347	14.010509	-0.088914	4.818109
450.856346	8000.285405	14.015514	-0.088876	4.818114
451.057583	8000.329272	14.020519	-0.088914	4.818126
450.715710	8000.288710	14.025523	-0.088850	4.818116
450.927614	8000.339042	14.030528	-0.088890	4.818130
451.053452	8000.308178	14.035533	-0.088913	4.818120
451.106737	8000.317348	14.040538	-0.088923	4.818123
451.023607	8000.319348	14.045543	-0.088908	4.818123
451.095027	8000.297196	14.050547	-0.088921	4.818117
450.531536	8000.355629	14.055552	-0.088816	4.818136
450.417389	8000.357195	14.060557	-0.088795	4.818137
450.573228	8000.362536	14.065562	-0.088824	4.818138
450.619259	8000.348450	14.070567	-0.088833	4.818134
450.567459	8000.321417	14.075571	-0.088823	4.818126
450.478872	8000.310710	14.080576	-0.088807	4.818123
450.298842	8000.362928	14.085581	-0.088773	4.818139
450.761375	8000.333615	14.090586	-0.088859	4.818129
450.690075	8000.338938	14.095591	-0.088846	4.818131
450.855859	8000.287583	14.100595	-0.088877	4.818115
451.147239	8000.325344	14.105600	-0.088931	4.818125
450.646539	8000.318346	14.110605	-0.088838	4.818125
450.417876	8000.373041	14.115610	-0.088796	4.818142
450.789967	8000.345621	14.120615	-0.088865	4.818132
450.731834	8000.316395	14.125619	-0.088854	4.818124
450.927255	8000.345446	14.130624	-0.088891	4.818132
451.059646	8000.313621	14.135629	-0.088916	4.818122
450.935581	8000.259265	14.140634	-0.088892	4.818106
451.046762	8000.269244	14.145639	-0.088913	4.818108
451.135061	8000.259959	14.150643	-0.088930	4.818105
451.476321	8000.298418	14.155648	-0.088993	4.818115
451.081174	8000.253952	14.160653	-0.088920	4.818104
451.118732	8000.280795	14.165658	-0.088927	4.818112
451.222495	8000.284356	14.170663	-0.088946	4.818112
451.285853	8000.259986	14.175667	-0.088958	4.818105
451.250928	8000.306866	14.180672	-0.088952	4.818119
451.280775	8000.246242	14.185677	-0.088957	4.818101
451.294432	8000.260120	14.190682	-0.088960	4.818105
451.287338	8000.289497	14.195687	-0.088959	4.818113
451.299260	8000.260197	14.200691	-0.088961	4.818105
451.344646	8000.280835	14.205696	-0.088969	4.818111
451.291803	8000.267470	14.210701	-0.088960	4.818107
451.187697	8000.274439	14.215706	-0.088940	4.818109
451.469196	8000.291012	14.220711	-0.088993	4.818113
451.111112	8000.271272	14.225715	-0.088926	4.818109
451.080753	8000.316111	14.230720	-0.088921	4.818122
450.618268	8000.333856	14.235725	-0.088835	4.818129
450.534985	8000.349536	14.240730	-0.088819	4.818134
450.808937	8000.321796	14.245735	-0.088870	4.818125
451.071720	8000.311793	14.250739	-0.088919	4.818121
451.073660	8000.334981	14.255744	-0.088920	4.818128
451.201287	8000.302037	14.260749	-0.088943	4.818118
451.108087	8000.336524	14.265754	-0.088926	4.818128
451.180174	8000.333327	14.270759	-0.088940	4.818127
450.911443	8000.279052	14.275763	-0.088890	4.818112
451.030440	8000.331242	14.280768	-0.088912	4.818127
450.970413	8000.274624	14.285773	-0.088901	4.818110
451.119753	8000.310398	14.290778	-0.088929	4.818120
451.043340	8000.309334	14.295783	-0.088914	4.818120
451.171070	7999.243895	14.300787	-0.088938	4.817804

450.982559	7996.239943	14.305792	-0.088901	4.816913
451.001543	7990.659981	14.310797	-0.088901	4.815257
450.480035	7984.023090	14.315802	-0.088799	4.813289
451.033891	7976.779222	14.320807	-0.088898	4.811136
450.979280	7969.067084	14.325811	-0.088883	4.808845
451.009391	7961.400705	14.330816	-0.088883	4.806565
450.930151	7953.404916	14.335821	-0.088863	4.804188
450.982845	7945.543816	14.340826	-0.088868	4.801848
450.763829	7937.587739	14.345831	-0.088822	4.799481
450.551754	7929.564508	14.350835	-0.088778	4.797092
450.805934	7921.547851	14.355840	-0.088820	4.794702
450.764687	7913.550436	14.360845	-0.088807	4.792318
450.659230	7905.485124	14.365850	-0.088782	4.789912
451.004690	7897.542043	14.370855	-0.088841	4.787540
450.655561	7889.514438	14.375859	-0.088771	4.785144
450.423055	7881.535127	14.380864	-0.088723	4.782761
450.611141	7873.569700	14.385869	-0.088753	4.780380
450.745708	7865.490708	14.390874	-0.088772	4.777964
450.907139	7857.491154	14.395879	-0.088797	4.775570
450.772861	7849.486247	14.400883	-0.088767	4.773174
450.969136	7841.531498	14.405888	-0.088799	4.770791
450.605036	7833.514670	14.410893	-0.088726	4.768390
450.415018	7825.537041	14.415898	-0.088685	4.765998
450.553557	7817.520851	14.420903	-0.088706	4.763594
450.650990	7809.512439	14.425907	-0.088719	4.761190
450.615929	7801.514105	14.430912	-0.088707	4.758789
450.635404	7793.518242	14.435917	-0.088706	4.756386
450.728634	7785.453336	14.440922	-0.088718	4.753962
450.439508	7777.572949	14.445927	-0.088659	4.751593
450.356913	7769.457663	14.450931	-0.088638	4.749152
450.717915	7761.490206	14.455936	-0.088700	4.746753
450.418548	7753.451926	14.460941	-0.088639	4.744332
450.215021	7745.531524	14.465946	-0.088596	4.741946
450.253984	7737.491771	14.470951	-0.088598	4.739522
450.174049	7729.469730	14.475955	-0.088578	4.737103
450.366234	7721.485853	14.480960	-0.088609	4.734693
450.561251	7713.456378	14.485965	-0.088640	4.732268
450.497338	7705.393020	14.490970	-0.088623	4.729832
450.350962	7697.491296	14.495975	-0.088591	4.727444
450.333182	7689.450994	14.500979	-0.088582	4.725013
450.326569	7681.528390	14.505984	-0.088576	4.722616
450.072107	7673.489745	14.510989	-0.088523	4.720183
450.015982	7665.521438	14.515994	-0.088508	4.717769
450.102619	7657.513758	14.520999	-0.088519	4.715343
450.103617	7649.497353	14.526003	-0.088514	4.712912
450.210736	7641.506231	14.531008	-0.088529	4.710488
450.057199	7633.449989	14.536013	-0.088495	4.708043
449.942735	7625.427998	14.541018	-0.088468	4.705607
449.876875	7617.456672	14.546023	-0.088451	4.703186
449.710204	7609.530103	14.551027	-0.088415	4.700776
449.553596	7601.497903	14.556032	-0.088380	4.698334
449.628656	7593.534499	14.561037	-0.088389	4.695910
449.471305	7585.445099	14.566042	-0.088355	4.693448
449.643433	7577.518014	14.571047	-0.088382	4.691033
449.779320	7569.406387	14.576051	-0.088402	4.688561
449.963312	7561.412772	14.581056	-0.088431	4.686123
449.681362	7553.443271	14.586061	-0.088373	4.683692
449.579577	7545.556268	14.591066	-0.088349	4.681284
449.797629	7537.457593	14.596071	-0.088385	4.678811
449.519302	7529.500766	14.601075	-0.088328	4.676380
449.159797	7521.473474	14.606080	-0.088256	4.673926
449.285868	7513.456705	14.611085	-0.088274	4.671474
449.703147	7505.293748	14.616090	-0.088346	4.668975
449.425983	7497.453821	14.621095	-0.088290	4.666575
449.624974	7489.396713	14.626099	-0.088322	4.664106
449.676488	7481.468837	14.631104	-0.088326	4.661676
449.499893	7473.413525	14.636109	-0.088288	4.659205
449.051869	7465.527064	14.641114	-0.088199	4.656786
449.255215	7457.453280	14.646119	-0.088232	4.654307
449.103354	7449.427195	14.651123	-0.088199	4.651841
449.225805	7441.411643	14.656128	-0.088216	4.649378
449.311828	7433.414503	14.661133	-0.088227	4.646918
449.137052	7425.363735	14.666138	-0.088189	4.644441
448.875784	7417.518105	14.671143	-0.088136	4.642026
449.040919	7409.433312	14.676147	-0.088161	4.639536
449.062048	7401.503791	14.681152	-0.088160	4.637093
448.464137	7393.432123	14.686157	-0.088044	4.634604
448.627011	7385.439194	14.691162	-0.088069	4.632138
449.335890	7377.407384	14.696167	-0.088196	4.629659
449.325372	7369.343160	14.701171	-0.088188	4.627169
448.906613	7361.388958	14.706176	-0.088105	4.624711
448.837883	7353.473895	14.711181	-0.088087	4.622264
448.749207	7345.389542	14.716186	-0.088066	4.619763
448.784890	7337.463648	14.721191	-0.088067	4.617310
448.831516	7329.345385	14.726195	-0.088071	4.614796
448.806326	7321.400957	14.731200	-0.088061	4.612335
448.723404	7313.379386	14.736205	-0.088040	4.609848
448.893090	7305.371523	14.741210	-0.088067	4.607365
448.874627	7297.376542	14.746215	-0.088058	4.604883
448.826309	7289.408097	14.751219	-0.088044	4.602409
448.931114	7281.419325	14.756224	-0.088058	4.599928
448.911991	7273.418211	14.761229	-0.088050	4.597441
448.901168	7265.366214	14.766234	-0.088043	4.594936
448.945143	7257.376574	14.771239	-0.088046	4.592450
448.737719	7249.312113	14.776243	-0.088002	4.589939
448.766656	7241.382367	14.781248	-0.088002	4.587469
448.451974	7233.333297	14.786253	-0.087938	4.584960
448.786412	7225.335687	14.791258	-0.087995	4.582467
448.894620	7217.347441	14.796263	-0.088010	4.579974
448.949805	7209.343789	14.801267	-0.088016	4.577476
448.753123	7201.353844	14.806272	-0.087974	4.574980
448.514371	7193.377567	14.811277	-0.087924	4.572486
448.366113	7185.370286	14.816282	-0.087891	4.569982
448.615750	7177.319196	14.821287	-0.087933	4.567464
448.309561	7169.253950	14.826291	-0.087871	4.564938
448.503225	7161.386420	14.831296	-0.087901	4.562474
448.471014	7153.337318	14.836301	-0.087890	4.559952
448.061537	7145.395769	14.841306	-0.087809	4.557461
447.810170	7137.386006	14.846311	-0.087757	4.554947
447.927476	7129.313513	14.851315	-0.087774	4.552414
448.079140	7121.304847	14.856320	-0.087797	4.549898
447.895680	7113.339827	14.861325	-0.087757	4.547395
448.170025	7105.235782	14.866330	-0.087803	4.544847
447.970692	7097.314531	14.871335	-0.087761	4.542355
447.960942	7089.270255	14.876339	-0.087754	4.539822
447.961572	7081.344354	14.881344	-0.087749	4.537326
448.123999	7073.299628	14.886349	-0.087774	4.534791
448.066035	7065.287985	14.891354	-0.087758	4.532265
448.193207	7057.315800	14.896359	-0.087777	4.529750
448.143353	7049.277428	14.901363	-0.087762	4.527213
448.328791	7041.275008	14.906368	-0.087792	4.524686
448.357556	7033.334773	14.911373	-0.087792	4.522177
448.027727	7025.286914	14.916378	-0.087725	4.519631
447.998255	7017.338435	14.921383	-0.087715	4.517116
447.889972	7009.271947	14.926387	-0.087689	4.514562
447.972814	7001.315528	14.931392	-0.087700	4.512043
447.631358	6993.281287	14.936397	-0.087631	4.509495
447.542644	6985.267745	14.941402	-0.087609	4.506954
447.636110	6977.254826	14.946407	-0.087621	4.504412
447.650281	6969.292502	14.951411	-0.087619	4.501885
447.529968	6961.234949	14.956416	-0.087591	4.499325
447.618382	6953.303397	14.961421	-0.087603	4.496804
447.719734	6945.208275	14.966426	-0.087616	4.494231
447.949669	6937.217282	14.971431	-0.087654	4.491689
447.850959	6929.200353	14.976435	-0.087631	4.489136
447.900793	6921.273429	14.981440	-0.087635	4.486612
447.615825	6913.222893	14.986445	-0.087576	4.484045
447.332106	6905.294519	14.991450	-0.087519	4.481515
447.239215	6897.261686	14.996455	-0.087496	4.478952
447.159274	6889.271455	15.001459	-0.087476	4.476401
447.349469	6881.227552	15.006464	-0.087506	4.473832
447.444977	6873.245125	15.011469	-0.087519	4.471281
447.485547	6865.210388	15.016474	-0.087521	4.468711
447.486726	6857.247130	15.021479	-0.087516	4.466163
447.202352	6849.206619	15.026483	-0.087458	4.463588
447.213491	6841.257300	15.031488	-0.087455	4.461041
447.311342	6833.204178	15.036493	-0.087468	4.458460
447.361124	6825.202123	15.041498	-0.087472	4.455894
447.417442	6817.189008	15.046503	-0.087478	4.453322
447.236603	6809.193761	15.051507	-0.087439	4.450754
447.070617	6801.191326	15.056512	-0.087403	4.448182
446.856851	6793.232188	15.061517	-0.087358	4.445623
446.609078	6785.273401	15.066522	-0.087307	4.443061
446.963438	6777.227445	15.071527	-0.087367	4.440473
447.042322	6769.189449	15.076531	-0.087377	4.437885
446.827035	6761.230582	15.081536	-0.087332	4.435320
447.076330	6753.187547	15.086541	-0.087373	4.432728
446.804267	6745.162539	15.091546	-0.087317	4.430137
446.886951	6737.191550	15.096551	-0.087327	4.427565
447.030150	6729.131380	15.101555	-0.087349	4.424962
447.067756	6721.210014	15.106560	-0.087351	4.422403
447.091892	6713.110068	15.111565	-0.087350	4.419784
447.136973	6705.148642	15.116570	-0.087353	4.417208
447.228517	6697.161145	15.121575	-0.087365	4.414623
446.830906	6689.137869	15.126579	-0.087286	4.412021
446.832163	6681.107497	15.131584	-0.087281	4.409419
446.663772	6673.148477	15.136589	-0.087245	4.406836
446.611649	6665.129542	15.141594	-0.087230	4.404234
446.652341	6657.209774	15.146599	-0.087232	4.401663
446.770963	6649.165393	15.151603	-0.087249	4.399050
446.674272	6641.245048	15.156608	-0.087226	4.396474
446.357276	6633.138829	15.161613	-0.087162	4.393836
446.741641	6625.188016	15.166618	-0.087228	4.391250
446.639075	6617.194717	15.171623	-0.087204	4.388647
446.448367	6609.144735	15.176627	-0.087163	4.386022
446.681385	6601.156298	15.181632	-0.087202	4.383419
446.598486	6593.202798	15.186637	-0.087181	4.380824
446.434377	6585.203119	15.191642	-0.087145	4.378211
446.405886	6577.198815	15.196647	-0.087135	4.375597
446.352733	6569.219881	15.201651	-0.087120	4.372989
446.586511	6561.193926	15.206656	-0.087158	4.370365
446.501147	6553.226175	15.211661	-0.087137	4.367758
446.522530	6545.194225	15.216666	-0.087136	4.365128
446.581354	6537.288250	15.221671	-0.087142	4.362538
446.146249	6529.273892	15.226675	-0.087056	4.359908
446.342760	6521.296407	15.231680	-0.087087	4.357293
446.397234	6513.301101	15.236685	-0.087092	4.354669
446.218052	6505.221716	15.241690	-0.087054	4.352014
445.961449	6497.210815	15.246695	-0.087001	4.349380
446.128758	6489.193376	15.251699	-0.087027	4.346745
446.342976	6481.187257	15.256704	-0.087061	4.344113
446.215056	6473.297135	15.261709	-0.087032	4.341514
445.929636	6465.225958	15.266714	-0.086974	4.338853
446.076980	6457.284175	15.271719	-0.086996	4.336237
445.782696	6449.215619	15.276723	-0.086936	4.333573
445.744321	6441.235899	15.281728	-0.086924	4.330940
445.956338	6433.229524	15.286733	-0.086958	4.328297
445.953089	6425.199167	15.291738	-0.086953	4.325644
445.753949	6417.253102	15.296743	-0.086910	4.323015
445.677553	6409.207993	15.301747	-0.086891	4.320353
445.431317	6401.304089	15.306752	-0.086840	4.317735
445.252073	6393.242286	15.311757	-0.086802	4.315063
445.265099	6385.262641	15.316762	-0.086799	4.312418
445.837062	6377.187133	15.321767	-0.086900	4.309745
445.492961	6369.219774	15.326771	-0.086831	4.307098
445.629867	6361.146377	15.331776	-0.086851	4.304418
445.759299	6353.202147	15.336781	-0.086870	4.301780
445.608270	6345.148040	15.341786	-0.086837	4.299101
445.592394	6337.267149	15.346791	-0.086829	4.296479
445.541673	6329.117290	15.351795	-0.086814	4.293766
445.543314	6321.231700	15.356800	-0.086809	4.291139
445.497745	6313.151818	15.361805	-0.086796	4.288446
445.594952	6305.222902	15.366810	-0.086809	4.285803
445.727369	6297.189394	15.371815	-0.086828	4.283123
445.626053	6289.198140	15.376819	-0.086804	4.280454
445.438798	6281.284357	15.381824	-0.086764	4.277808
445.380597	6273.250597	15.386829	-0.086748	4.275121
445.381979	6265.214648	15.391834	-0.086743	4.272433
445.134951	6257.222487	15.396839	-0.086692	4.269755
445.116194	6249.176772	15.401843	-0.086683	4.267060
445.099870	6241.169606	15.406848	-0.086675	4.264376
444.870207	6233.216460	15.411853	-0.086627	4.261706
445.162680	6225.142559	15.416858	-0.086677	4.259000
445.052452	6217.242526	15.421863	-0.086651	4.256346
444.997779	6209.188868	15.426867	-0.086636	4.253639
445.299560	6201.150222	15.431872	-0.086687	4.250939
445.041614	6193.193562	15.436877	-0.086634	4.248259
445.164538	6185.177757	15.441882	-0.086651	4.245562
445.090985	6177.188691	15.446887	-0.086632	4.242870
444.859362	6169.181766	15.451891	-0.086584	4.240168
445.131590	6161.218288	15.456896	-0.086630	4.237485
445.075205	6153.174632	15.461901	-0.086614	4.234769
444.469899	6145.269613	15.466906	-0.086496	4.232093
444.537569	6137.216801	15.471911	-0.086504	4.229372
444.848156	6129.117228	15.476915	-0.086556	4.226637
444.876825	6121.144202	15.481920	-0.086556	4.223939
444.603258	6113.234719	15.486925	-0.086500	4.221258
444.308312	6105.205791	15.491930	-0.086440	4.218534
444.528880	6097.226352	15.496935	-0.086476	4.215831
444.125006	6089.226155	15.501939	-0.086396	4.213112
444.328977	6081.168303	15.506944	-0.086429	4.210379
444.426455	6073.131956	15.511949	-0.086442	4.207650
444.382472	6065.122894	15.516954	-0.086428	4.204927
444.158946	6057.227757	15.521959	-0.086382	4.202239
444.050918	6049.163372	15.526963	-0.086356	4.199493
444.532163	6041.212849	15.531968	-0.086441	4.196791
444.306088	6033.177549	15.536973	-0.086394	4.194049
444.195083	6025.125399	15.541978	-0.086368	4.191302
444.253454	6017.094755	15.546983	-0.086373	4.188562
444.151318	6009.143399	15.551987	-0.086349	4.185846
444.163796	6001.125714	15.556992	-0.086346	4.183106
443.832022	5993.184551	15.561997	-0.086280	4.180387
444.226488	5985.132155	15.567002	-0.086348	4.177636
444.398798	5977.108196	15.572007	-0.086375	4.174891
444.513096	5969.131578	15.577011	-0.086391	4.172160
444.470815	5961.100151	15.582016	-0.086378	4.169406
444.343952	5953.162587	15.587021	-0.086349	4.166681
444.416682	5945.101293	15.592026	-0.086357	4.163915
444.438766	5937.213425	15.597031	-0.086356	4.161206
443.987735	5929.138095	15.602035	-0.086267	4.158424
444.303770	5921.203743	15.607040	-0.086321	4.155699
444.294974	5913.201133	15.612045	-0.086314	4.152945
444.136580	5905.200289	15.617050	-0.086280	4.150187
444.231597	5897.223530	15.622055	-0.086292	4.147439
444.003490	5889.140069	15.627059	-0.086244	4.144648
443.941117	5881.250388	15.632064	-0.086228	4.141924
443.941177	5873.202718	15.637069	-0.086223	4.139145
443.610624	5865.256942	15.642074	-0.086156	4.136395
443.842213	5857.197775	15.647079	-0.086194	4.133611
443.727834	5849.211269	15.652083	-0.086167	4.130846
443.664977	5841.235398	15.657088	-0.086151	4.128083
443.597620	5833.212834	15.662093	-0.086133	4.125303
443.550252	5825.197640	15.667098	-0.086119	4.122523
443.773960	5817.204306	15.672103	-0.086155	4.119752
443.672256	5809.189449	15.677107	-0.086131	4.116968
443.145184	5801.267758	15.682112	-0.086028	4.114209
443.111961	5793.268353	15.687117	-0.086017	4.111427
443.284984	5785.205193	15.692122	-0.086044	4.108624
443.336388	5777.173838	15.697127	-0.086048	4.105828
443.194450	5769.187048	15.702131	-0.086017	4.103044
443.319088	5761.175307	15.707136	-0.086035	4.100253
443.111959	5753.251297	15.712141	-0.085991	4.097485
442.848173	5745.211670	15.717146	-0.085937	4.094675
443.102605	5737.227960	15.722151	-0.085979	4.091889
443.412986	5729.112483	15.727155	-0.086031	4.089057
443.540240	5721.161731	15.732160	-0.086050	4.086277
443.478389	5713.152861	15.737165	-0.086033	4.083473
443.436282	5705.191467	15.742170	-0.086020	4.080683
443.480779	5697.202537	15.747175	-0.086024	4.077883
443.178427	5689.208755	15.752179	-0.085962	4.075075
442.945217	5681.265707	15.757184	-0.085914	4.072283
443.271084	5673.172104	15.762189	-0.085969	4.069445
443.077057	5665.186976	15.767194	-0.085928	4.066635
443.112848	5657.185191	15.772199	-0.085929	4.063821
443.041529	5649.231673	15.777203	-0.085911	4.061020
443.065414	5641.203370	15.782208	-0.085910	4.058193
443.100310	5633.158046	15.787213	-0.085911	4.055357
443.266752	5625.163923	15.792218	-0.085937	4.052540
443.166582	5617.189624	15.797223	-0.085914	4.049724
442.852912	5609.240915	15.802227	-0.085850	4.046911
442.777171	5601.158455	15.807232	-0.085831	4.044053
443.007891	5593.242840	15.812237	-0.085869	4.041256
442.970498	5585.177046	15.817242	-0.085856	4.038401
442.814000	5577.278257	15.822247	-0.085822	4.035600
442.644581	5569.223604	15.827251	-0.085785	4.032742
442.711255	5561.171119	15.832256	-0.085793	4.029887
442.674689	5553.183510	15.837261	-0.085781	4.027051
442.616339	5545.147194	15.842266	-0.085765	4.024195
442.758368	5537.256698	15.847271	-0.085786	4.021393
442.211222	5529.262053	15.852275	-0.085679	4.018540
442.374567	5521.269485	15.857280	-0.085704	4.015697
442.324574	5513.225814	15.862285	-0.085690	4.012831
442.526871	5505.182314	15.867290	-0.085722	4.009967
442.549227	5497.216747	15.872295	-0.085721	4.007125
442.351831	5489.161356	15.877299	-0.085679	4.004246
442.399935	5481.294219	15.882304	-0.085683	4.001437
442.096284	5473.312173	15.887309	-0.085622	3.998578
442.294229	5465.254584	15.892314	-0.085653	3.995698
442.560255	5457.251783	15.897319	-0.085698	3.992838
442.473168	5449.252350	15.902323	-0.085676	3.989970
442.326229	5441.257235	15.907328	-0.085644	3.987101
442.107145	5433.230545	15.912333	-0.085598	3.984217
442.414559	5425.259008	15.917338	-0.085650	3.981360
442.219364	5417.278432	15.922343	-0.085608	3.978489
442.168473	5409.281904	15.927347	-0.085594	3.975613
442.264553	5401.270978	15.932352	-0.085607	3.972732
442.164748	5393.237337	15.937357	-0.085583	3.969837
441.883242	5385.275742	15.942362	-0.085525	3.966963
442.064202	5377.250369	15.947367	-0.085554	3.964072
442.090626	5369.305064	15.952371	-0.085554	3.961205
442.139568	5361.273647	15.957376	-0.085558	3.958305
442.069498	5353.277388	15.962381	-0.085539	3.955414
442.047451	5345.258708	15.967386	-0.085530	3.952513
442.128635	5337.251918	15.972391	-0.085540	3.949617
442.091279	5329.235453	15.977395	-0.085528	3.946713
442.168148	5321.219090	15.982400	-0.085537	3.943808
442.072284	5313.287130	15.987405	-0.085514	3.940929
441.822237	5305.259750	15.992410	-0.085462	3.938010
442.026745	5297.288024	15.997415	-0.085495	3.935118
441.765516	5289.296387	16.002419	-0.085442	3.932208
441.746183	5281.235605	16.007424	-0.085433	3.929275
441.821827	5273.284762	16.012429	-0.085442	3.926381
441.636058	5265.260930	16.017434	-0.085402	3.923454
441.860944	5257.275525	16.022439	-0.085439	3.920546
441.626825	5249.292781	16.027443	-0.085390	3.917629
441.936793	5241.280471	16.032448	-0.085443	3.914709
441.798619	5233.325988	16.037453	-0.085412	3.911799
441.519050	5225.304813	16.042458	-0.085354	3.908860
441.551069	5217.332818	16.047463	-0.085355	3.905943
441.362447	5209.285746	16.052467	-0.085315	3.902992
441.186911	5201.347159	16.057472	-0.085277	3.900078
441.529354	5193.322775	16.062477	-0.085336	3.897141
441.414895	5185.299338	16.067482	-0.085309	3.894194
441.606647	5177.349454	16.072487	-0.085340	3.891277
441.457351	5169.294224	16.077491	-0.085307	3.888312
441.344960	5161.353446	16.082496	-0.085281	3.885388
441.408902	5153.332719	16.087501	-0.085288	3.882436
441.204309	5145.327821	16.092506	-0.085244	3.879482
441.546079	5137.375842	16.097511	-0.085303	3.876556
441.425516	5129.315070	16.102515	-0.085275	3.873579
441.138782	5121.245326	16.107520	-0.085217	3.870592
440.942640	5113.280714	16.112525	-0.085175	3.867644
440.471877	5105.319139	16.117530	-0.085082	3.864689
441.193665	5097.296610	16.122535	-0.085211	3.861734
440.710095	5089.341387	16.127539	-0.085116	3.858777
440.699557	5081.387502	16.132544	-0.085109	3.855827
440.672956	5073.352320	16.137549	-0.085099	3.852845
440.867698	5065.311563	16.142554	-0.085130	3.849863
440.675564	5057.369689	16.147559	-0.085089	3.846908
440.580857	5049.316801	16.152563	-0.085066	3.843911
440.704783	5041.418595	16.157568	-0.085084	3.840973
440.528411	5033.389630	16.162573	-0.085046	3.837979
440.524163	5025.360356	16.167578	-0.085040	3.834985
440.794893	5017.390747	16.172583	-0.085086	3.832018
440.487727	5009.364902	16.177587	-0.085023	3.829015
440.760224	5001.324819	16.182592	-0.085069	3.826016
440.491616	4993.390401	16.187597	-0.085014	3.823043
440.378065	4985.392241	16.192602	-0.084988	3.820047
440.373108	4977.415634	16.197607	-0.084981	3.817059
440.173389	4969.380275	16.202611	-0.084939	3.814043
440.083502	4961.447131	16.207616	-0.084917	3.811065
439.862205	4953.424200	16.212621	-0.084871	3.808048
440.194892	4945.342886	16.217626	-0.084928	3.805019
440.515297	4937.387287	16.222631	-0.084982	3.802035
440.385588	4929.364675	16.227635	-0.084953	3.799012
440.474509	4921.423081	16.232640	-0.084964	3.796023
440.421584	4913.378773	16.237645	-0.084949	3.792990
440.264754	4905.410145	16.242650	-0.084915	3.789980
440.337989	4897.428872	16.247655	-0.084923	3.786969
439.850660	4889.409894	16.252659	-0.084828	3.783928
440.329381	4881.417276	16.257664	-0.084912	3.780917
440.378667	4873.392223	16.262669	-0.084916	3.777881
440.194386	4865.407042	16.267674	-0.084876	3.774852
440.196623	4857.456272	16.272679	-0.084871	3.771839
440.132575	4849.371212	16.277683	-0.084854	3.768770
440.151141	4841.440488	16.282688	-0.084853	3.765759
440.336022	4833.417780	16.287693	-0.084882	3.762715
440.270003	4825.446835	16.292698	-0.084864	3.759683
440.353922	4817.512245	16.297703	-0.084875	3.756665
440.226510	4809.476948	16.302707	-0.084846	3.753601
440.473506	4801.476871	16.307712	-0.084887	3.750558
440.146822	4793.488676	16.312717	-0.084821	3.747502
439.965893	4785.474123	16.317722	-0.084782	3.744438
439.947906	4777.567647	16.322727	-0.084774	3.741416
439.649596	4769.556681	16.327731	-0.084713	3.738345
439.738927	4761.512746	16.332736	-0.084724	3.735268
439.885444	4753.507548	16.337741	-0.084747	3.732205
439.827735	4745.452933	16.342746	-0.084731	3.729115
439.656083	4737.542572	16.347751	-0.084694	3.726076
439.567212	4729.513884	16.352755	-0.084672	3.722990
439.723290	4721.546493	16.357760	-0.084696	3.719932
439.713645	4713.577008	16.362765	-0.084689	3.716866
439.614547	4705.521108	16.367770	-0.084665	3.713762
439.679274	4697.500853	16.372775	-0.084672	3.710674
439.508184	4689.474559	16.377779	-0.084635	3.707574
439.447762	4681.491365	16.382784	-0.084619	3.704492
439.601224	4673.523212	16.387789	-0.084642	3.701418
439.426169	4665.506893	16.392794	-0.084604	3.698314
439.679181	4657.539662	16.397799	-0.084646	3.695238
439.665309	4649.490529	16.402803	-0.084639	3.692121
439.668785	4641.484880	16.407808	-0.084634	3.689018
439.590303	4633.556680	16.412813	-0.084614	3.685941
439.455036	4625.535297	16.417818	-0.084584	3.682823
439.653628	4617.592034	16.422823	-0.084616	3.679742
439.293116	4609.597982	16.427827	-0.084544	3.676624
439.246044	4601.618303	16.432832	-0.084530	3.673517
439.421121	4593.582096	16.437837	-0.084557	3.670391
439.196691	4585.585748	16.442842	-0.084510	3.667267
439.281267	4577.582999	16.447847	-0.084521	3.664147
439.237926	4569.615062	16.452851	-0.084508	3.661034
439.262463	4561.610098	16.457856	-0.084507	3.657906
439.369496	4553.613417	16.462861	-0.084522	3.654780
439.260769	4545.629021	16.467866	-0.084496	3.651651
439.258866	4537.648033	16.472871	-0.084491	3.648523
439.255800	4529.625442	16.477875	-0.084485	3.645377
439.169579	4521.692745	16.482880	-0.084464	3.642260
439.299156	4513.617428	16.487885	-0.084483	3.639091
439.212568	4505.700085	16.492890	-0.084462	3.635975
439.136842	4497.688103	16.497895	-0.084442	3.632820
439.090897	4489.655654	16.502899	-0.084429	3.629655
439.061769	4481.683654	16.507904	-0.084418	3.626511
438.909742	4473.660152	16.512909	-0.084385	3.623340
438.909038	4465.666084	16.517914	-0.084379	3.620183
439.176756	4457.703907	16.522919	-0.084424	3.617043
439.077007	4449.669324	16.527923	-0.084400	3.613862
438.934199	4441.691475	16.532928	-0.084369	3.610699
438.930184	4433.715353	16.537933	-0.084363	3.607537
438.773813	4425.705380	16.542938	-0.084328	3.604355
438.778893	4417.765462	16.547943	-0.084324	3.601203
438.689719	4409.718450	16.552947	-0.084303	3.598003
438.613055	4401.735002	16.557952	-0.084283	3.594825
438.853799	4393.740046	16.562957	-0.084323	3.591649
438.589279	4385.715642	16.567962	-0.084268	3.588444
438.468830	4377.741888	16.572967	-0.084241	3.585261
438.556096	4369.734102	16.577971	-0.084252	3.582067
438.651752	4361.724208	16.582976	-0.084265	3.578870
438.633810	4353.789978	16.587981	-0.084256	3.575696
438.776375	4345.746351	16.592986	-0.084277	3.572481
438.637083	4337.737218	16.597991	-0.084246	3.569269
438.408316	4329.797334	16.602995	-0.084199	3.566079
438.453817	4321.805941	16.608000	-0.084202	3.562873
438.324486	4313.824804	16.613005	-0.084173	3.559663
438.305484	4305.834055	16.618010	-0.084164	3.556450
438.540283	4297.815802	16.623015	-0.084203	3.553231
438.202213	4289.817236	16.628019	-0.084135	3.549999
438.090100	4281.797297	16.633024	-0.084108	3.546762
437.918371	4273.803980	16.638029	-0.084071	3.543531
438.063981	4265.818473	16.643034	-0.084093	3.540311
438.092757	4257.829837	16.648039	-0.084094	3.537082
437.901497	4249.833021	16.653043	-0.084053	3.533841
437.956411	4241.861636	16.658048	-0.084058	3.530614
437.804927	4233.862667	16.663053	-0.084025	3.527367
437.506806	4225.842510	16.668058	-0.083964	3.524104
437.446897	4217.967400	16.673063	-0.083948	3.520903
437.495499	4209.868398	16.678067	-0.083951	3.517613
437.649347	4201.864610	16.683072	-0.083975	3.514361
437.735289	4193.905663	16.688077	-0.083986	3.511123
437.578488	4185.898814	16.693082	-0.083951	3.507854
437.656783	4177.894014	16.698087	-0.083961	3.504591
437.362013	4169.934465	16.703091	-0.083901	3.501331
437.565232	4161.927069	16.708096	-0.083934	3.498064
437.391635	4153.958452	16.713101	-0.083896	3.494798
437.309074	4145.938322	16.718106	-0.083876	3.491511
437.356856	4137.968696	16.723111	-0.083879	3.488246
437.267183	4129.944476	16.728115	-0.083857	3.484950
437.006253	4122.002383	16.733120	-0.083804	3.481680
437.147645	4113.979430	16.738125	-0.083825	3.478387
436.892948	4106.008000	16.743130	-0.083772	3.475098
437.037263	4098.018136	16.748135	-0.083794	3.471812
436.943493	4089.967206	16.753139	-0.083771	3.468490
436.943103	4081.958067	16.758144	-0.083766	3.465185
436.757929	4074.048636	16.763149	-0.083727	3.461912
436.688889	4066.012787	16.768154	-0.083709	3.458588
436.826597	4058.024390	16.773159	-0.083729	3.455286
436.697028	4050.036796	16.778163	-0.083700	3.451973
436.431459	4042.087651	16.783168	-0.083645	3.448668
436.674918	4034.020224	16.788173	-0.083685	3.445329
436.488738	4026.068752	16.793178	-0.083646	3.442019
436.784930	4018.040178	16.798183	-0.083696	3.438691
436.513923	4010.072920	16.803187	-0.083640	3.435365
436.638537	4002.097924	16.808192	-0.083658	3.432047
436.525691	3994.107677	16.813197	-0.083632	3.428710
436.687695	3986.049291	16.818202	-0.083657	3.425352
436.325565	3978.188130	16.823207	-0.083584	3.422055
436.390022	3970.110260	16.828211	-0.083591	3.418678
436.624371	3962.115529	16.833216	-0.083630	3.415339
436.523249	3954.144063	16.838221	-0.083606	3.411995
436.614764	3946.089843	16.843226	-0.083618	3.408619
436.764918	3938.108462	16.848231	-0.083640	3.405273
436.401806	3930.168668	16.853235	-0.083568	3.401923
436.745117	3922.136129	16.858240	-0.083626	3.398556
436.633335	3914.216046	16.863245	-0.083601	3.395216
436.557166	3906.166062	16.868250	-0.083581	3.391820
436.524672	3898.152985	16.873255	-0.083570	3.388437
436.295194	3890.161845	16.878259	-0.083522	3.385053
436.452983	3882.184680	16.883264	-0.083546	3.381686
436.349382	3874.187745	16.888269	-0.083522	3.378297
436.340169	3866.199588	16.893274	-0.083515	3.374912
436.637303	3858.231239	16.898279	-0.083565	3.371543
436.269690	3850.245234	16.903283	-0.083492	3.368139
436.268137	3842.209274	16.908288	-0.083486	3.364724
436.448546	3834.281542	16.913293	-0.083515	3.361359
436.238784	3826.271116	16.918298	-0.083470	3.357940
436.136355	3818.313743	16.923303	-0.083446	3.354544
435.890542	3810.363874	16.928307	-0.083395	3.351142
435.950015	3802.332578	16.933312	-0.083401	3.347714
436.029064	3794.307032	16.938317	-0.083411	3.344286
435.878998	3786.352165	16.943322	-0.083378	3.340875
436.020330	3778.346250	16.948327	-0.083399	3.337450
435.795967	3770.345948	16.953331	-0.083352	3.334010
435.939934	3762.365663	16.958336	-0.083374	3.330590
435.911871	3754.373961	16.963341	-0.083363	3.327154
436.071525	3746.328108	16.968346	-0.083388	3.323698
436.053863	3738.418691	16.973351	-0.083379	3.320291
435.845103	3730.421598	16.978355	-0.083335	3.316836
435.812866	3722.439522	16.983360	-0.083324	3.313390
435.943801	3714.440268	16.988365	-0.083344	3.309939
435.694392	3706.425119	16.993370	-0.083292	3.306463
435.784277	3698.417440	16.998375	-0.083304	3.303000
435.745835	3690.441972	17.003379	-0.083291	3.299542
435.661409	3682.505668	17.008384	-0.083270	3.296095
435.382976	3674.519177	17.013389	-0.083213	3.292616
435.419901	3666.447957	17.018394	-0.083215	3.289108
435.437931	3658.498184	17.023399	-0.083213	3.285649
435.503013	3650.503774	17.028403	-0.083220	3.282169
435.618615	3642.528926	17.033408	-0.083237	3.278695
435.371249	3634.573654	17.038413	-0.083186	3.275212
435.363912	3626.543482	17.043418	-0.083179	3.271702
435.510389	3618.549827	17.048423	-0.083201	3.268210
435.578378	3610.525595	17.053427	-0.083209	3.264698
435.510789	3602.561663	17.058432	-0.083191	3.261203
435.450632	3594.577890	17.063437	-0.083175	3.257696
435.354237	3586.610378	17.068442	-0.083151	3.254191
435.438586	3578.642460	17.073447	-0.083162	3.250690
435.296094	3570.619246	17.078451	-0.083130	3.247151
435.351533	3562.625259	17.083456	-0.083136	3.243629
435.155774	3554.708734	17.088461	-0.083094	3.240127
435.246816	3546.699762	17.093466	-0.083106	3.236592
435.336226	3538.670729	17.098471	-0.083117	3.233044
435.104231	3530.702636	17.103475	-0.083069	3.229507
435.294713	3522.673886	17.108480	-0.083099	3.225956
435.290953	3514.677210	17.113485	-0.083093	3.222407
434.985351	3506.713786	17.118490	-0.083031	3.218856
435.149197	3498.734995	17.123495	-0.083057	3.215315
434.977692	3490.722595	17.128499	-0.083020	3.211740
434.891272	3482.734878	17.133504	-0.082998	3.208176
434.943835	3474.701527	17.138509	-0.083003	3.204593
434.750887	3466.797766	17.143514	-0.082962	3.201054
434.714073	3458.828537	17.148519	-0.082950	3.197489
434.917004	3450.746176	17.153523	-0.082983	3.193879
434.407161	3442.879452	17.158528	-0.082883	3.190331
434.367776	3434.866391	17.163533	-0.082870	3.186733
434.316020	3426.847625	17.168538	-0.082855	3.183128
434.495478	3418.832180	17.173543	-0.082884	3.179531
433.956757	3410.945458	17.178547	-0.082778	3.175956
434.056632	3402.912905	17.183552	-0.082792	3.172340
434.420569	3394.862990	17.188557	-0.082854	3.168723
433.911659	3386.931651	17.193562	-0.082754	3.165117
434.341474	3378.907241	17.198567	-0.082829	3.161507
434.259762	3370.936516	17.203571	-0.082809	3.157894
434.176055	3362.959323	17.208576	-0.082788	3.154273
434.232290	3354.977535	17.213581	-0.082793	3.150653
434.415491	3346.933298	17.218586	-0.082822	3.147006
434.373981	3338.980898	17.223591	-0.082810	3.143386
434.306221	3330.998496	17.228595	-0.082792	3.139747
434.226593	3323.023826	17.233600	-0.082772	3.136108
434.114058	3315.034395	17.238605	-0.082746	3.132455
434.117395	3307.008648	17.243610	-0.082741	3.128787
433.943895	3299.064539	17.248615	-0.082704	3.125144
433.967777	3291.082091	17.253619	-0.082703	3.121488
433.581035	3283.149510	17.258624	-0.082626	3.117832
433.725449	3275.124107	17.263629	-0.082648	3.114153
433.280622	3267.192582	17.268634	-0.082560	3.110486
433.384290	3259.169187	17.273639	-0.082574	3.106798
433.401482	3251.136932	17.278643	-0.082572	3.103097
433.450227	3243.154335	17.283648	-0.082576	3.099416
433.429110	3235.213956	17.288653	-0.082567	3.095747
433.067485	3227.231281	17.293658	-0.082494	3.092038
433.204769	3219.214272	17.298663	-0.082515	3.088332
433.018049	3211.207591	17.303667	-0.082475	3.084612
433.567243	3203.185140	17.308672	-0.082572	3.080914
433.670731	3195.213017	17.313677	-0.082586	3.077214
433.464209	3187.250071	17.318682	-0.082542	3.073499
433.699437	3179.206546	17.323687	-0.082581	3.069763
433.348917	3171.254465	17.328691	-0.082511	3.066038
433.180256	3163.342897	17.333696	-0.082474	3.062335
433.116366	3155.340059	17.338701	-0.082457	3.058590
432.922489	3147.364527	17.343706	-0.082416	3.054847
432.916879	3139.402623	17.348711	-0.082410	3.051115
432.822132	3131.375965	17.353715	-0.082387	3.047344
432.637112	3123.422489	17.358720	-0.082347	3.043598
432.698298	3115.410749	17.363725	-0.082354	3.039832
432.904315	3107.397071	17.368730	-0.082387	3.036067
433.227446	3099.388893	17.373735	-0.082442	3.032306
432.947993	3091.431944	17.378739	-0.082385	3.028535
432.750899	3083.484969	17.383744	-0.082343	3.024768
433.096698	3075.482221	17.388749	-0.082402	3.020997
432.982759	3067.504908	17.393754	-0.082376	3.017210
433.069541	3059.500663	17.398759	-0.082387	3.013416
432.752356	3051.522992	17.403763	-0.082322	3.009610
432.682332	3043.596236	17.408768	-0.082304	3.005835
432.293000	3035.655139	17.413773	-0.082227	3.002032
432.414114	3027.639838	17.418778	-0.082244	2.998215
432.088209	3019.683698	17.423783	-0.082178	2.994399
432.290236	3011.642278	17.428787	-0.082211	2.990564
432.171359	3003.646095	17.433792	-0.082183	2.986729
432.364592	2995.654735	17.438797	-0.082214	2.982908
432.584486	2987.613455	17.443802	-0.082250	2.979059
432.736530	2979.676090	17.448807	-0.082273	2.975252
432.487166	2971.707838	17.453811	-0.082222	2.971404
432.369761	2963.740310	17.458816	-0.082195	2.967558
432.674022	2955.689023	17.463821	-0.082246	2.963689
432.304583	2947.798008	17.468826	-0.082172	2.959857
432.297623	2939.839970	17.473831	-0.082166	2.956007
431.787313	2931.889777	17.478835	-0.082066	2.952129
432.015343	2923.829266	17.483840	-0.082103	2.948231
431.810290	2915.865788	17.488845	-0.082060	2.944352
431.662259	2907.935541	17.493850	-0.082027	2.940487
431.565623	2899.969803	17.498855	-0.082004	2.936603
431.401113	2891.972206	17.503859	-0.081968	2.932694
431.731197	2883.908583	17.508864	-0.082024	2.928774
431.428653	2875.976986	17.513869	-0.081963	2.924880
431.340191	2868.003804	17.518874	-0.081941	2.920972
431.667983	2860.003579	17.523879	-0.081997	2.917067
431.438951	2851.989783	17.528883	-0.081949	2.913121
431.499203	2843.960576	17.533888	-0.081956	2.909177
431.315262	2836.005500	17.538893	-0.081916	2.905251
431.654971	2827.976374	17.543898	-0.081974	2.901312
431.962163	2819.986248	17.548903	-0.082026	2.897385
431.931650	2811.990876	17.553907	-0.082015	2.893432
431.670502	2804.088369	17.558912	-0.081962	2.889506
431.229031	2796.193672	17.563917	-0.081874	2.885569
431.353187	2788.184841	17.568922	-0.081892	2.881601
431.246784	2780.254978	17.573927	-0.081867	2.877654
431.281040	2772.190428	17.578931	-0.081869	2.873643
431.465698	2764.201521	17.583936	-0.081898	2.869672
430.778054	2756.340364	17.588941	-0.081765	2.865710
431.060705	2748.288121	17.593946	-0.081812	2.861702
430.711250	2740.353656	17.598951	-0.081742	2.857712
430.569163	2732.357086	17.603955	-0.081710	2.853696
430.674322	2724.349286	17.608960	-0.081725	2.849683
430.596697	2716.378525	17.613965	-0.081705	2.845673
430.422369	2708.416454	17.618970	-0.081668	2.841656
431.041105	2700.368152	17.623975	-0.081778	2.837636
430.589005	2692.441330	17.628979	-0.081688	2.833609
430.140658	2684.549666	17.633984	-0.081600	2.829594
429.965930	2676.537499	17.638989	-0.081562	2.825529
430.313824	2668.482889	17.643994	-0.081622	2.821466
430.261423	2660.520925	17.648999	-0.081607	2.817422
430.208176	2652.523876	17.654003	-0.081592	2.813354
429.611928	2644.635631	17.659008	-0.081476	2.809303
429.599794	2636.643597	17.664013	-0.081468	2.805228
429.930752	2628.577486	17.669018	-0.081525	2.801129
430.220594	2620.611373	17.674023	-0.081574	2.797073
430.333832	2612.608393	17.679027	-0.081590	2.792982
430.226984	2604.640952	17.684032	-0.081565	2.788890
429.878605	2596.713516	17.689037	-0.081495	2.784798
429.597539	2588.783365	17.694042	-0.081437	2.780703
430.002284	2580.743379	17.699047	-0.081507	2.776586
429.891512	2572.781738	17.704051	-0.081482	2.772473
430.214791	2564.731346	17.709056	-0.081537	2.768333
429.816520	2556.829164	17.714061	-0.081457	2.764221
430.202350	2548.804190	17.719066	-0.081524	2.760086
429.962648	2540.919745	17.724071	-0.081474	2.755980
429.934316	2532.862458	17.729075	-0.081464	2.751791
430.060599	2524.852442	17.734080	-0.081482	2.747630
430.532195	2516.814625	17.739085	-0.081565	2.743469
430.077779	2508.950408	17.744090	-0.081475	2.739335
429.946222	2501.021617	17.749095	-0.081446	2.735182
430.093005	2492.970411	17.754099	-0.081468	2.730975
430.432826	2484.954224	17.759104	-0.081526	2.726792
430.356504	2477.030314	17.764109	-0.081506	2.722625
430.062122	2469.109768	17.769114	-0.081447	2.718439
430.282641	2461.121905	17.774119	-0.081482	2.714245
430.258597	2453.142023	17.779123	-0.081473	2.710032
430.211763	2445.176718	17.784128	-0.081459	2.705819
430.355840	2437.194882	17.789133	-0.081481	2.701603
430.077141	2429.269524	17.794138	-0.081424	2.697384
430.186037	2421.272145	17.799143	-0.081439	2.693144
429.467659	2413.381868	17.804147	-0.081300	2.688901
428.907946	2405.482234	17.809152	-0.081191	2.684657
429.217465	2397.463232	17.814157	-0.081243	2.680398
429.049986	2389.468282	17.819162	-0.081207	2.676115
429.223298	2381.449832	17.824167	-0.081234	2.671835
429.409932	2373.405258	17.829171	-0.081264	2.667534
429.390746	2365.429561	17.834176	-0.081255	2.663250
429.067800	2357.526037	17.839181	-0.081190	2.658978
429.130675	2349.526000	17.844186	-0.081196	2.654672
429.147882	2341.556666	17.849191	-0.081194	2.650373
429.017398	2333.575754	17.854195	-0.081165	2.646051
429.510715	2325.529740	17.859200	-0.081251	2.641728
429.641365	2317.574554	17.864205	-0.081271	2.637424
429.690624	2309.587223	17.869210	-0.081275	2.633089
429.789981	2301.627724	17.874215	-0.081288	2.628766
429.727242	2293.677935	17.879219	-0.081271	2.624429
429.760081	2285.748564	17.884224	-0.081272	2.620104
429.460978	2277.822018	17.889229	-0.081211	2.615750
429.388831	2269.850595	17.894234	-0.081193	2.611379
429.480659	2261.864084	17.899239	-0.081205	2.607005
429.051458	2253.951647	17.904243	-0.081120	2.602628
428.919667	2246.014892	17.909248	-0.081090	2.598250
429.317519	2237.968173	17.914253	-0.081159	2.593841
429.352970	2229.846639	17.919258	-0.081160	2.589358
429.306504	2221.932997	17.924263	-0.081147	2.584977
429.154195	2213.997466	17.929267	-0.081113	2.580569
429.297684	2206.004188	17.934272	-0.081135	2.576142
429.163397	2198.061975	17.939277	-0.081105	2.571716
429.127857	2190.095788	17.944282	-0.081093	2.567276
429.327052	2182.114983	17.949287	-0.081125	2.562836
428.999542	2174.198136	17.954291	-0.081059	2.558388
429.064376	2166.229393	17.959296	-0.081066	2.553931
429.259170	2158.241254	17.964301	-0.081097	2.549464
429.240586	2150.265944	17.969306	-0.081088	2.544981
429.059182	2142.349633	17.974311	-0.081049	2.540512
429.078858	2134.378715	17.979315	-0.081048	2.536018
429.100900	2126.390405	17.984320	-0.081047	2.531508
428.875718	2118.459393	17.989325	-0.081000	2.527003
428.918380	2110.470760	17.994330	-0.081003	2.522477
429.260137	2102.477638	17.999335	-0.081061	2.517963
428.996579	2094.545275	18.004339	-0.081007	2.513430
428.821172	2086.614608	18.009344	-0.080969	2.508897
428.757979	2078.637414	18.014349	-0.080952	2.504337
428.946056	2070.629650	18.019354	-0.080982	2.499770
428.811444	2062.705253	18.024359	-0.080952	2.495218
428.879074	2054.708781	18.029363	-0.080959	2.490632
428.718130	2046.770325	18.034368	-0.080924	2.486054
428.654090	2038.832859	18.039373	-0.080907	2.481475
428.424438	2030.883906	18.044378	-0.080859	2.476868
428.890575	2022.863950	18.049383	-0.080941	2.472264
428.588750	2014.928865	18.054387	-0.080880	2.467643
428.296189	2007.004390	18.059392	-0.080820	2.463020
428.241733	1999.053485	18.064397	-0.080805	2.458391
428.461493	1991.027969	18.069402	-0.080841	2.453730
428.186200	1983.117533	18.074407	-0.080784	2.449090
427.833158	1975.182404	18.079411	-0.080714	2.444421
427.939668	1967.230365	18.084416	-0.080728	2.439768
427.640140	1959.305487	18.089421	-0.080667	2.435091
427.767513	1951.245853	18.094426	-0.080686	2.430358
428.260180	1943.190881	18.099431	-0.080772	2.425648
427.965444	1935.296598	18.104435	-0.080712	2.420962
428.181674	1927.314159	18.109440	-0.080748	2.416255
428.021775	1919.376516	18.114445	-0.080713	2.411535
427.904945	1911.424080	18.119450	-0.080686	2.406801
427.905655	1903.482639	18.124455	-0.080681	2.402073
427.718579	1895.540407	18.129459	-0.080641	2.397321
428.107011	1887.527706	18.134464	-0.080708	2.392563
427.851192	1879.614882	18.139469	-0.080655	2.387804
427.846362	1871.631991	18.144474	-0.080649	2.383013
428.202087	1863.667926	18.149479	-0.080710	2.378253
428.140763	1855.710341	18.154483	-0.080694	2.373454
427.986290	1847.779399	18.159488	-0.080660	2.368653
427.678288	1839.872767	18.164493	-0.080598	2.363845
427.347268	1831.970612	18.169498	-0.080531	2.359028
427.494371	1823.992723	18.174503	-0.080553	2.354194
427.603741	1815.994477	18.179507	-0.080568	2.349335
427.480158	1808.033143	18.184512	-0.080540	2.344469
427.549148	1800.082070	18.189517	-0.080548	2.339615
427.313703	1792.126602	18.194522	-0.080499	2.334723
427.435070	1784.181375	18.199527	-0.080516	2.329856
427.169816	1776.232032	18.204531	-0.080462	2.324945
427.179738	1768.285983	18.209536	-0.080459	2.320048
427.238522	1760.324234	18.214541	-0.080464	2.315136
427.375030	1752.334391	18.219546	-0.080485	2.310202
427.337146	1744.386766	18.224551	-0.080473	2.305269
427.016069	1736.488165	18.229555	-0.080408	2.300331
426.926404	1728.551517	18.234560	-0.080386	2.295379
427.128984	1720.554447	18.239565	-0.080418	2.290404
426.921333	1712.614670	18.244570	-0.080375	2.285418
427.023921	1704.675220	18.249575	-0.080389	2.280449
426.977693	1696.723520	18.254579	-0.080375	2.275448
426.952040	1688.746847	18.259584	-0.080365	2.270422
426.718864	1680.816964	18.264589	-0.080317	2.265396
426.647372	1672.860360	18.269594	-0.080298	2.260356
426.788271	1664.895836	18.274599	-0.080319	2.255319
426.748066	1656.937737	18.279603	-0.080307	2.250259
426.761371	1648.983210	18.284608	-0.080304	2.245194
426.701401	1641.065424	18.289613	-0.080288	2.240135
426.673028	1633.124805	18.294618	-0.080277	2.235052
426.763284	1625.175861	18.299623	-0.080289	2.229963
426.781715	1617.201470	18.304627	-0.080287	2.224840
426.457928	1609.328727	18.309632	-0.080222	2.219739
426.488609	1601.364882	18.314637	-0.080223	2.214600
426.621089	1593.380531	18.319642	-0.080242	2.209445
426.580098	1585.459672	18.324647	-0.080229	2.204303
426.364301	1577.549454	18.329651	-0.080184	2.199140
426.280683	1569.621738	18.334656	-0.080163	2.193966
426.526220	1561.626877	18.339661	-0.080204	2.188766
426.227608	1553.702258	18.344666	-0.080143	2.183549
426.093038	1545.810706	18.349671	-0.080113	2.178356
426.452251	1537.770718	18.354675	-0.080175	2.173100
426.466673	1529.826321	18.359680	-0.080172	2.167861
426.264217	1521.929280	18.364685	-0.080130	2.162621
426.248849	1513.992964	18.369690	-0.080122	2.157360
426.299337	1506.073834	18.374695	-0.080126	2.152103
425.971527	1498.160186	18.379699	-0.080060	2.146801
425.845888	1490.224871	18.384704	-0.080031	2.141491
426.347981	1482.238748	18.389709	-0.080120	2.136194
425.884637	1474.342892	18.394714	-0.080028	2.130851
425.836316	1466.413057	18.399719	-0.080014	2.125512
425.827681	1458.469221	18.404723	-0.080007	2.120154
425.674797	1450.563561	18.409728	-0.079974	2.114794
425.591209	1442.604744	18.414733	-0.079953	2.109392
425.578418	1434.635897	18.419738	-0.079946	2.103975
425.792687	1426.682257	18.424743	-0.079980	2.098577
425.535046	1418.781035	18.429747	-0.079927	2.093155
425.551078	1410.833276	18.434752	-0.079925	2.087714
425.598423	1402.898684	18.439757	-0.079929	2.082270
425.449547	1394.985363	18.444762	-0.079896	2.076807
425.403344	1387.079066	18.449767	-0.079882	2.071346
425.455601	1379.103531	18.454771	-0.079887	2.065831
425.113797	1371.251044	18.459776	-0.079818	2.060347
425.106969	1363.307560	18.464781	-0.079812	2.054820
425.121053	1355.340127	18.469786	-0.079809	2.049262
425.101661	1347.423264	18.474791	-0.079801	2.043722
424.971167	1339.520235	18.479795	-0.079771	2.038165
424.917026	1331.598758	18.484800	-0.079756	2.032588
425.094312	1323.635000	18.489805	-0.079784	2.026989
424.705853	1315.758947	18.494810	-0.079707	2.021378
424.545105	1307.854381	18.499815	-0.079672	2.015755
424.571952	1299.893074	18.504819	-0.079672	2.010095
424.527627	1291.951600	18.509824	-0.079658	2.004426
424.818829	1283.993805	18.514829	-0.079707	1.998765
424.695685	1276.093929	18.519834	-0.079679	1.993085
424.723733	1268.186295	18.524839	-0.079679	1.987400
424.540612	1260.281561	18.529843	-0.079640	1.981678
424.419310	1252.386874	18.534848	-0.079613	1.975953
424.398647	1244.473863	18.539853	-0.079604	1.970209
424.231312	1236.542502	18.544858	-0.079567	1.964419
424.433186	1228.634956	18.549863	-0.079600	1.958669
424.365767	1220.712119	18.554867	-0.079582	1.952862
424.235277	1212.807929	18.559872	-0.079553	1.947044
423.916451	1204.932324	18.564877	-0.079488	1.941209
423.531879	1197.046029	18.569882	-0.079412	1.935341
423.901440	1189.050886	18.574887	-0.079475	1.929458
423.559686	1181.169116	18.579891	-0.079407	1.923563
423.842052	1173.205962	18.584896	-0.079454	1.917658
423.709712	1165.336193	18.589901	-0.079424	1.911759
423.330135	1157.437319	18.594906	-0.079349	1.905791
423.477502	1149.503677	18.599911	-0.079371	1.899838
423.703904	1141.541824	18.604915	-0.079408	1.893854
423.898312	1133.604015	18.609920	-0.079439	1.887866
423.698684	1125.752130	18.614925	-0.079397	1.881879
423.339903	1117.907349	18.619930	-0.079325	1.875859
423.593480	1109.958271	18.624935	-0.079367	1.869812
423.455312	1102.047099	18.629939	-0.079336	1.863728
423.681569	1094.096641	18.634944	-0.079373	1.857637
423.476823	1086.240013	18.639949	-0.079330	1.851547
423.385012	1078.332658	18.644954	-0.079308	1.845412
423.408587	1070.460351	18.649959	-0.079307	1.839297
423.563363	1062.535784	18.654963	-0.079331	1.833136
423.368268	1054.661385	18.659968	-0.079290	1.826952
423.426959	1046.756112	18.664973	-0.079295	1.820753
423.420685	1038.856456	18.669978	-0.079289	1.814530
423.308499	1030.999676	18.674983	-0.079263	1.808306
423.266093	1023.093758	18.679987	-0.079250	1.802030
422.889068	1015.289060	18.684992	-0.079175	1.795771
422.940700	1007.327596	18.689997	-0.079179	1.789419
423.051035	999.382840	18.695002	-0.079195	1.783064
422.792740	991.548492	18.700007	-0.079142	1.776730
422.390512	983.721694	18.705011	-0.079062	1.770360
422.908869	975.721891	18.710016	-0.079153	1.763944
422.871047	967.861402	18.715021	-0.079141	1.757547
422.637477	959.998887	18.720026	-0.079093	1.751100
422.705969	952.115477	18.725031	-0.079100	1.744651
422.387694	944.299451	18.730035	-0.079036	1.738184
422.047051	936.452287	18.735040	-0.078967	1.731663
422.088488	928.536466	18.740045	-0.078970	1.725111
422.311775	920.633588	18.745050	-0.079007	1.718568
422.046191	912.816183	18.750055	-0.078952	1.712008
421.909080	904.924622	18.755059	-0.078921	1.705377
421.783856	897.065287	18.760064	-0.078893	1.698748
422.137915	889.120233	18.765069	-0.078954	1.692086
421.959967	881.249592	18.770074	-0.078916	1.685388
421.785477	873.438904	18.775079	-0.078878	1.678716
421.686929	865.585163	18.780083	-0.078855	1.671990
421.631505	857.708275	18.785088	-0.078839	1.665223
421.308129	849.912763	18.790093	-0.078774	1.658462
421.561091	841.982145	18.795098	-0.078816	1.651636
421.166812	834.182114	18.800103	-0.078738	1.644805
421.168404	826.318165	18.805107	-0.078733	1.637945
421.071666	818.441306	18.810112	-0.078710	1.631030
421.290752	810.518596	18.815117	-0.078746	1.624091
421.363993	802.640497	18.820122	-0.078754	1.617141
421.097638	794.841002	18.825127	-0.078699	1.610182
420.963733	787.014292	18.830131	-0.078670	1.603187
420.628690	779.221302	18.835136	-0.078602	1.596163
420.903172	771.317376	18.840141	-0.078648	1.589096
420.696835	763.488561	18.845146	-0.078605	1.581996
420.750369	755.642246	18.850151	-0.078610	1.574886
421.121348	747.721092	18.855155	-0.078674	1.567722
421.086495	739.902724	18.860160	-0.078662	1.560559
421.031354	732.117401	18.865165	-0.078647	1.553391
420.921962	724.278025	18.870170	-0.078621	1.546131
420.619675	716.512555	18.875175	-0.078560	1.538877
420.764733	708.632381	18.880179	-0.078582	1.531549
420.522623	700.852224	18.885184	-0.078532	1.524220
420.201531	693.092626	18.890189	-0.078467	1.516863
420.000633	685.274325	18.895194	-0.078425	1.509433
420.639219	677.340754	18.900199	-0.078538	1.501988
420.339912	669.577304	18.905203	-0.078478	1.494521
420.345919	661.754103	18.910208	-0.078474	1.487007
420.212269	653.981788	18.915213	-0.078444	1.479482
419.689924	646.243903	18.920218	-0.078342	1.471890
419.720286	638.401029	18.925223	-0.078342	1.464245
420.050874	630.522727	18.930227	-0.078399	1.456573
419.566613	622.809876	18.935232	-0.078304	1.448892
419.708498	614.975438	18.940237	-0.078325	1.441151
419.290982	607.257367	18.945242	-0.078242	1.433393
419.429463	599.429901	18.950247	-0.078263	1.425574
419.683389	591.583318	18.955251	-0.078305	1.417713
419.055317	583.910130	18.960256	-0.078183	1.409835
419.327780	576.081617	18.965261	-0.078229	1.401907
419.102572	568.337772	18.970266	-0.078182	1.393936
418.983851	560.573852	18.975271	-0.078155	1.385916
418.889943	552.801652	18.980275	-0.078133	1.377846
418.538972	545.083179	18.985280	-0.078062	1.369739
419.188749	537.193168	18.990285	-0.078178	1.361579
419.246377	529.427079	18.995290	-0.078184	1.353397
419.253503	521.681130	19.000295	-0.078180	1.345177
418.948401	513.993684	19.005299	-0.078119	1.336913
419.284067	506.184100	19.010304	-0.078176	1.328582
419.275917	498.461337	19.015309	-0.078170	1.320230
419.258929	490.688685	19.020314	-0.078161	1.311769
419.388591	482.895638	19.025319	-0.078180	1.303258
418.938794	475.268748	19.030323	-0.078092	1.294766
419.052240	467.520847	19.035328	-0.078108	1.286190
419.216585	459.796406	19.040333	-0.078134	1.277591
419.108636	452.106039	19.045338	-0.078109	1.268921
419.310578	444.380924	19.050343	-0.078141	1.260211
419.270704	436.694944	19.055347	-0.078129	1.251439
418.851338	429.086123	19.060352	-0.078046	1.242620
418.684256	421.441848	19.065357	-0.078010	1.233746
418.721468	413.722752	19.070362	-0.078012	1.224760
418.349583	406.118778	19.075367	-0.077938	1.215762
418.665578	398.368131	19.080371	-0.077991	1.206661
418.647523	390.720440	19.085376	-0.077983	1.197547
418.603021	383.069351	19.090381	-0.077970	1.188353
418.213384	375.484771	19.095386	-0.077893	1.179096
418.528977	367.781483	19.100391	-0.077946	1.169769
418.492455	360.147994	19.105395	-0.077935	1.160378
417.913717	352.624015	19.110400	-0.077822	1.150931
418.104464	344.946199	19.115405	-0.077853	1.141379
418.078038	337.317449	19.120410	-0.077843	1.131760
418.143453	329.699371	19.125415	-0.077850	1.122093
418.098160	322.116896	19.130419	-0.077837	1.112364
418.006736	314.540771	19.135424	-0.077815	1.102546
417.974389	306.972082	19.140429	-0.077804	1.092663
417.420746	299.493605	19.145434	-0.077696	1.082691
417.805119	291.877472	19.150439	-0.077763	1.072658
417.510109	284.360748	19.155443	-0.077703	1.062506
417.305550	276.862307	19.160448	-0.077660	1.052302
417.552480	269.277815	19.165453	-0.077701	1.041987
417.482621	261.775606	19.170458	-0.077683	1.031607
417.213069	254.320623	19.175463	-0.077628	1.021139
416.788697	246.899832	19.180467	-0.077545	1.010573
416.866151	239.397392	19.185472	-0.077554	0.999904
416.983027	231.889281	19.190477	-0.077571	0.989120
416.723047	224.461568	19.195482	-0.077518	0.978240
416.910366	216.984858	19.200487	-0.077548	0.967280
416.947160	209.549843	19.205491	-0.077550	0.956218
416.839173	202.162504	19.210496	-0.077525	0.945060
416.535082	194.830070	19.215501	-0.077464	0.933800
416.348271	187.477894	19.220506	-0.077424	0.922404
416.471730	180.102702	19.225511	-0.077443	0.910914
416.344143	172.768663	19.230515	-0.077414	0.899274
416.347802	165.444156	19.235520	-0.077410	0.887533
416.089247	158.200876	19.240525	-0.077357	0.875692
416.001913	150.923235	19.245530	-0.077336	0.863681
416.095924	143.652968	19.250535	-0.077349	0.851567
415.773473	136.476274	19.255539	-0.077284	0.839313
415.734242	129.250084	19.260544	-0.077273	0.826878
415.660354	122.075391	19.265549	-0.077254	0.814332
415.668423	114.898290	19.270554	-0.077251	0.801612
415.565275	107.797473	19.275559	-0.077227	0.788790
415.468092	100.706511	19.280563	-0.077205	0.775776
415.403316	93.645506	19.285568	-0.077188	0.762606
415.239451	86.646380	19.290573	-0.077153	0.749290
414.961775	79.678812	19.295578	-0.077097	0.735755
414.837047	72.912584	19.300583	-0.077069	0.722419