Fri Apr 16 19:32:09 2021

Number of Points = 3635
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.456017	-0.108507	0.000000	-0.000078	0.313266

3.591202	-0.134031	0.005005	-0.000103	0.313262
3.322496	-0.085070	0.010010	-0.000053	0.313263
3.617391	-0.138010	0.015014	-0.000108	0.313266
3.496914	-0.118643	0.020019	-0.000086	0.313255
3.415619	-0.102043	0.025024	-0.000071	0.313263
3.535593	-0.124676	0.030029	-0.000093	0.313260
3.594578	-0.136357	0.035034	-0.000104	0.313256
3.253706	-0.071839	0.040038	-0.000041	0.313268
2.831424	0.005719	0.045043	0.000037	0.313272
3.106686	-0.042577	0.050048	-0.000014	0.313281
3.269193	-0.074577	0.055053	-0.000044	0.313270
3.189523	-0.061846	0.060058	-0.000030	0.313262
3.180327	-0.105237	0.065062	-0.000028	0.313054
2.781647	-0.045882	0.070067	0.000046	0.312994
2.498924	0.007019	0.075072	0.000099	0.313001
2.860917	-0.060168	0.080077	0.000031	0.312995
2.762298	-0.043373	0.085082	0.000050	0.312990
2.626575	-0.016983	0.090086	0.000075	0.312999
2.565914	-0.008552	0.095091	0.000086	0.312987
2.887478	-0.066867	0.100096	0.000026	0.312988
3.231308	-0.178904	0.105101	-0.000038	0.312759
3.165057	-0.193652	0.110106	-0.000026	0.312636
3.033644	-0.167566	0.115110	-0.000001	0.312646
3.496223	-0.256408	0.120115	-0.000087	0.312624
3.368811	-0.231981	0.125120	-0.000064	0.312631
3.274555	-0.271474	0.130125	-0.000046	0.312369
3.577651	-0.337742	0.135130	-0.000103	0.312317
3.425889	-0.307940	0.140134	-0.000075	0.312328
3.240299	-0.276640	0.145139	-0.000040	0.312317
3.399094	-0.365042	0.150144	-0.000070	0.312042
3.376549	-0.370795	0.155149	-0.000066	0.311996
3.008546	-0.303688	0.160154	0.000003	0.311998
3.246327	-0.358187	0.165158	-0.000042	0.311946
3.044673	-0.372020	0.170163	-0.000004	0.311712
2.952626	-0.354017	0.175168	0.000013	0.311718
2.908868	-0.345338	0.180173	0.000021	0.311722
2.918402	-0.401464	0.185178	0.000019	0.311470
2.990116	-0.430877	0.190182	0.000006	0.311394
2.979018	-0.432307	0.195187	0.000008	0.311378
3.074457	-0.482990	0.200192	-0.000010	0.311224
3.347481	-0.565313	0.205197	-0.000061	0.311072
3.238423	-0.547083	0.210202	-0.000041	0.311065
3.110835	-0.567408	0.215206	-0.000017	0.310863
3.096194	-0.587996	0.220211	-0.000014	0.310755
3.164124	-0.600826	0.225216	-0.000027	0.310753
3.150145	-0.653429	0.230221	-0.000025	0.310497
2.928146	-0.610518	0.235226	0.000017	0.310509
2.888465	-0.630578	0.240230	0.000024	0.310382
2.700206	-0.643018	0.245235	0.000059	0.310165
2.938010	-0.685343	0.250240	0.000015	0.310170
3.186688	-0.789855	0.255245	-0.000032	0.309893
3.188761	-0.802501	0.260250	-0.000032	0.309836
3.177625	-0.838252	0.265254	-0.000030	0.309660
3.294504	-0.893442	0.270259	-0.000052	0.309502
3.270456	-0.911643	0.275264	-0.000047	0.309397
3.073377	-0.911459	0.280269	-0.000011	0.309231
3.074170	-0.929067	0.285274	-0.000011	0.309149
3.200593	-1.007278	0.290278	-0.000035	0.308891
3.158694	-1.013162	0.295283	-0.000027	0.308828
3.508775	-1.131278	0.300288	-0.000092	0.308573
3.308485	-1.111948	0.305293	-0.000055	0.308494
3.212211	-1.147859	0.310298	-0.000037	0.308243
3.306114	-1.184228	0.315302	-0.000055	0.308153
3.408263	-1.245314	0.320307	-0.000074	0.307954
3.457587	-1.292286	0.325312	-0.000083	0.307775
3.220456	-1.282579	0.330317	-0.000039	0.307619
3.209267	-1.331319	0.335322	-0.000037	0.307380
3.376742	-1.377281	0.340326	-0.000068	0.307308
3.148529	-1.406107	0.345331	-0.000026	0.306977
3.243742	-1.439101	0.350336	-0.000043	0.306903
2.965601	-1.432223	0.355341	0.000008	0.306698
2.937130	-1.468340	0.360346	0.000014	0.306503
3.083474	-1.524916	0.365350	-0.000014	0.306362
3.014325	-1.570840	0.370355	-0.000001	0.306086
3.012427	-1.594245	0.375360	-0.000001	0.305974
2.918300	-1.627775	0.380365	0.000017	0.305735
3.086147	-1.693958	0.385370	-0.000014	0.305567
3.045314	-1.708699	0.390374	-0.000007	0.305462
2.783837	-1.730526	0.395379	0.000042	0.305134
2.649570	-1.736568	0.400384	0.000067	0.304990
2.954829	-1.827572	0.405389	0.000010	0.304822
2.855079	-1.876894	0.410394	0.000028	0.304502
3.043705	-1.938726	0.415398	-0.000007	0.304371
2.892805	-1.947303	0.420403	0.000021	0.304200
2.935104	-2.023292	0.425408	0.000013	0.303876
2.722196	-2.020046	0.430413	0.000053	0.303707
2.653813	-2.045328	0.435418	0.000066	0.303528
2.863558	-2.143525	0.440422	0.000026	0.303242
2.561612	-2.129837	0.445427	0.000083	0.303046
2.627028	-2.178790	0.450432	0.000070	0.302869
2.796390	-2.264348	0.455437	0.000039	0.302608
2.616545	-2.289344	0.460442	0.000072	0.302332
2.471846	-2.303149	0.465446	0.000099	0.302141
2.403249	-2.334538	0.470451	0.000112	0.301931
2.585406	-2.419461	0.475456	0.000078	0.301683
2.574013	-2.471453	0.480461	0.000080	0.301424
2.310376	-2.469263	0.485466	0.000129	0.301205
2.540348	-2.552899	0.490470	0.000086	0.301004
2.510457	-2.606340	0.495475	0.000092	0.300721
2.364366	-2.621104	0.500480	0.000119	0.300523
2.273862	-2.653040	0.505485	0.000136	0.300290
2.094276	-2.671459	0.510490	0.000169	0.300045
2.126147	-2.722710	0.515494	0.000163	0.299826
2.042264	-2.776951	0.520499	0.000179	0.299491
2.186026	-2.846406	0.525504	0.000152	0.299282
1.800079	-2.824665	0.530509	0.000224	0.299048
1.711272	-2.860282	0.535514	0.000240	0.298798
1.598222	-2.887877	0.540518	0.000261	0.298565
1.331122	-2.904635	0.545523	0.000311	0.298249
1.008103	-2.888478	0.550528	0.000371	0.298043
0.535034	-2.846091	0.555533	0.000459	0.297832
0.102244	-2.813118	0.560538	0.000539	0.297610
-0.332873	-2.796376	0.565542	0.000620	0.297307
-0.887189	-2.737210	0.570547	0.000723	0.297105
-0.900634	-2.768341	0.575552	0.000726	0.296942
-1.193245	-2.766287	0.580557	0.000780	0.296693
-1.451319	-2.764965	0.585562	0.000828	0.296471
-1.658225	-2.758516	0.590566	0.000866	0.296319
-1.652490	-2.816404	0.595571	0.000865	0.296042
-1.728136	-2.843626	0.600576	0.000879	0.295842
-1.899836	-2.843509	0.605581	0.000911	0.295690
-1.964762	-2.875863	0.610586	0.000923	0.295475
-2.470142	-2.827502	0.615590	0.001017	0.295262
-2.985946	-2.764883	0.620595	0.001113	0.295110
-2.962542	-2.827796	0.625600	0.001109	0.294822
-2.951370	-2.863504	0.630605	0.001107	0.294657
-3.347196	-2.826082	0.635610	0.001180	0.294488
-3.276003	-2.891920	0.640614	0.001167	0.294229
-3.583970	-2.864634	0.645619	0.001224	0.294088
-3.687103	-2.890495	0.650624	0.001243	0.293869
-4.039423	-2.873084	0.655629	0.001309	0.293639
-4.175539	-2.872709	0.660634	0.001334	0.293520
-4.277662	-2.910219	0.665638	0.001353	0.293244
-4.592689	-2.883018	0.670643	0.001412	0.293096
-4.923610	-2.852833	0.675648	0.001473	0.292948
-5.110187	-2.872399	0.680653	0.001508	0.292684
-5.389447	-2.841415	0.685658	0.001560	0.292587
-5.671639	-2.848650	0.690662	0.001612	0.292297
-5.768175	-2.850546	0.695667	0.001630	0.292202
-6.114151	-2.833963	0.700672	0.001694	0.291973
-6.506290	-2.789023	0.705677	0.001767	0.291842
-6.630909	-2.798930	0.710682	0.001790	0.291681
-6.649248	-2.833110	0.715686	0.001794	0.291495
-7.118876	-2.778409	0.720691	0.001881	0.291344
-7.286398	-2.789279	0.725696	0.001912	0.291139
-7.305811	-2.804904	0.730701	0.001916	0.291044
-7.659366	-2.789898	0.735706	0.001982	0.290799
-7.862490	-2.765830	0.740710	0.002019	0.290736
-7.954884	-2.790782	0.745715	0.002036	0.290528
-8.128358	-2.770321	0.750720	0.002069	0.290473
-8.449234	-2.765564	0.755725	0.002128	0.290207
-8.705234	-2.735507	0.760730	0.002176	0.290125
-8.613188	-2.795420	0.765734	0.002159	0.289910
-9.312582	-2.688256	0.770739	0.002289	0.289811
-9.634720	-2.667409	0.775744	0.002349	0.289623
-9.664373	-2.689609	0.780749	0.002354	0.289485
-9.699248	-2.705533	0.785754	0.002361	0.289374
-10.098530	-2.666982	0.790758	0.002435	0.289204
-10.313621	-2.634848	0.795763	0.002475	0.289170
-10.317300	-2.695775	0.800768	0.002475	0.288862
-10.567434	-2.650026	0.805773	0.002522	0.288864
-10.839234	-2.650958	0.810778	0.002572	0.288612
-10.951622	-2.641122	0.815782	0.002593	0.288559
-11.409470	-2.583877	0.820787	0.002678	0.288429
-11.552599	-2.597102	0.825792	0.002705	0.288232
-11.388399	-2.626440	0.830797	0.002674	0.288235
-12.002262	-2.569901	0.835802	0.002788	0.287959
-12.191511	-2.537182	0.840806	0.002824	0.287951
-12.127468	-2.575289	0.845811	0.002812	0.287818
-12.353419	-2.576752	0.850816	0.002854	0.287605
-12.440390	-2.560964	0.855821	0.002870	0.287605
-12.860601	-2.536319	0.860826	0.002948	0.287345
-12.664314	-2.582533	0.865830	0.002911	0.287292
-12.772753	-2.578083	0.870835	0.002931	0.287216
-13.119614	-2.565030	0.875840	0.002996	0.286964
-12.901736	-2.604795	0.880845	0.002955	0.286964
-13.162891	-2.596946	0.885850	0.003004	0.286764
-13.445890	-2.562526	0.890854	0.003056	0.286679
-13.676818	-2.526646	0.895859	0.003099	0.286648
-13.896225	-2.547174	0.900864	0.003140	0.286343
-14.084537	-2.512642	0.905869	0.003175	0.286345
-14.097612	-2.531363	0.910874	0.003177	0.286239
-13.965904	-2.594470	0.915878	0.003153	0.286041
-14.336951	-2.529573	0.920883	0.003222	0.286029
-14.635586	-2.520586	0.925888	0.003277	0.285800
-14.597505	-2.544257	0.930893	0.003270	0.285715
-14.595277	-2.548738	0.935898	0.003270	0.285695
-14.800924	-2.555937	0.940902	0.003308	0.285470
-14.919796	-2.536704	0.945907	0.003330	0.285458
-14.795172	-2.585473	0.950912	0.003307	0.285326
-15.362545	-2.521975	0.955917	0.003412	0.285125
-15.621529	-2.475556	0.960922	0.003460	0.285122
-15.438884	-2.550166	0.965926	0.003426	0.284912
-15.843513	-2.497498	0.970931	0.003502	0.284806
-15.931369	-2.481326	0.975936	0.003518	0.284808
-16.063984	-2.517770	0.980941	0.003542	0.284500
-16.329481	-2.474425	0.985946	0.003592	0.284476
-16.289563	-2.487586	0.990950	0.003584	0.284446
-16.513896	-2.496703	0.995955	0.003626	0.284192
-16.520021	-2.495078	1.000960	0.003627	0.284195
-16.850158	-2.454596	1.005965	0.003688	0.284096
-17.345818	-2.412028	1.010970	0.003781	0.283854
-16.764472	-2.516846	1.015974	0.003672	0.283859
-17.023378	-2.500388	1.020979	0.003720	0.283703
-17.587351	-2.427610	1.025984	0.003825	0.283552
-17.240662	-2.491745	1.030989	0.003761	0.283547
-17.449785	-2.495811	1.035994	0.003800	0.283332
-17.854426	-2.441585	1.040998	0.003875	0.283234
-17.850969	-2.443876	1.046003	0.003874	0.283226
-17.635929	-2.527706	1.051008	0.003834	0.282997
-17.928874	-2.486732	1.056013	0.003888	0.282935
-18.396477	-2.402485	1.061018	0.003975	0.282931
-18.532611	-2.440119	1.066022	0.004001	0.282612
-18.754453	-2.401240	1.071027	0.004042	0.282605
-18.805284	-2.392480	1.076032	0.004051	0.282603
-18.771463	-2.460196	1.081037	0.004045	0.282288
-18.844130	-2.447723	1.086042	0.004058	0.282285
-18.819593	-2.460238	1.091046	0.004054	0.282244
-19.344519	-2.420497	1.096051	0.004151	0.281958
-18.906602	-2.499419	1.101056	0.004070	0.281962
-19.279345	-2.447827	1.106061	0.004139	0.281880
-19.805247	-2.392972	1.111066	0.004237	0.281671
-19.615595	-2.426185	1.116070	0.004202	0.281678
-19.498972	-2.475563	1.121075	0.004180	0.281533
-20.189752	-2.387672	1.126080	0.004308	0.281340
-19.928609	-2.434507	1.131085	0.004260	0.281343
-19.805658	-2.491765	1.136090	0.004237	0.281164
-19.966657	-2.487548	1.141094	0.004267	0.281036
-20.542114	-2.384239	1.146099	0.004374	0.281029
-20.517979	-2.433306	1.151104	0.004369	0.280799
-20.377693	-2.475294	1.156109	0.004343	0.280715
-20.702554	-2.417370	1.161114	0.004403	0.280709
-20.651769	-2.466316	1.166118	0.004394	0.280505
-20.806356	-2.443447	1.171123	0.004422	0.280478
-20.882853	-2.440862	1.176128	0.004437	0.280420
-21.261760	-2.426229	1.181133	0.004507	0.280140
-21.228504	-2.433514	1.186138	0.004501	0.280134
-21.137077	-2.470135	1.191142	0.004484	0.280031
-21.807421	-2.389845	1.196147	0.004608	0.279817
-21.631457	-2.421206	1.201152	0.004576	0.279820
-21.703202	-2.440399	1.206157	0.004589	0.279654
-22.433670	-2.338126	1.211162	0.004725	0.279496
-22.062392	-2.404637	1.216166	0.004656	0.279502
-22.016095	-2.447596	1.221171	0.004647	0.279323
-22.344350	-2.410154	1.226176	0.004708	0.279208
-22.343154	-2.409884	1.231181	0.004708	0.279211
-22.388537	-2.455022	1.236186	0.004716	0.278935
-22.367566	-2.470327	1.241190	0.004712	0.278875
-22.900648	-2.377805	1.246195	0.004811	0.278853
-22.879016	-2.437995	1.251200	0.004807	0.278561
-22.636885	-2.481531	1.256205	0.004762	0.278564
-22.960767	-2.444864	1.261210	0.004822	0.278449
-23.395161	-2.404661	1.266214	0.004903	0.278248
-23.121629	-2.456255	1.271219	0.004852	0.278238
-23.224019	-2.469842	1.276224	0.004871	0.278071
-23.719240	-2.402885	1.281229	0.004963	0.277951
-23.590274	-2.427287	1.286234	0.004939	0.277947
-23.638500	-2.470343	1.291238	0.004948	0.277677
-24.035339	-2.411121	1.296243	0.005022	0.277610
-24.161907	-2.389920	1.301248	0.005045	0.277601
-24.213129	-2.438062	1.306253	0.005055	0.277302
-24.438429	-2.399039	1.311258	0.005096	0.277292
-24.587621	-2.384806	1.316262	0.005124	0.277225
-24.903426	-2.375122	1.321267	0.005183	0.276976
-24.928115	-2.368970	1.326272	0.005187	0.276985
-25.006132	-2.371894	1.331277	0.005202	0.276896
-25.156862	-2.384321	1.336282	0.005230	0.276688
-25.074893	-2.398215	1.341286	0.005214	0.276694
-25.326456	-2.383914	1.346291	0.005261	0.276530
-25.690447	-2.351350	1.351296	0.005329	0.276354
-25.270433	-2.427289	1.356301	0.005251	0.276357
-25.531894	-2.420082	1.361306	0.005299	0.276146
-25.858354	-2.378585	1.366310	0.005360	0.276052
-26.139144	-2.327940	1.371315	0.005412	0.276051
-25.681361	-2.461234	1.376320	0.005327	0.275788
-26.039326	-2.406462	1.381325	0.005393	0.275735
-26.469956	-2.331838	1.386330	0.005473	0.275716
-25.938151	-2.472161	1.391334	0.005374	0.275487
-26.417943	-2.385986	1.396339	0.005464	0.275482
-26.373007	-2.418187	1.401344	0.005455	0.275356
-26.656125	-2.406037	1.406349	0.005508	0.275149
-26.897839	-2.363048	1.411354	0.005553	0.275145
-26.855971	-2.407618	1.416358	0.005545	0.274951
-27.403486	-2.330550	1.421363	0.005647	0.274833
-27.137778	-2.379230	1.426368	0.005597	0.274831
-27.229141	-2.412860	1.431373	0.005614	0.274567
-27.523033	-2.372405	1.436378	0.005669	0.274499
-27.188837	-2.437695	1.441382	0.005606	0.274475
-27.551054	-2.421637	1.446387	0.005674	0.274213
-27.808341	-2.375575	1.451392	0.005722	0.274209
-27.575595	-2.441709	1.456397	0.005678	0.274084
-27.952707	-2.414053	1.461402	0.005748	0.273868
-27.984495	-2.406390	1.466406	0.005754	0.273878
-28.225450	-2.406248	1.471411	0.005799	0.273648
-28.318976	-2.405395	1.476416	0.005816	0.273563
-28.408336	-2.390040	1.481421	0.005833	0.273558
-28.729537	-2.391677	1.486426	0.005893	0.273241
-28.509582	-2.429760	1.491430	0.005852	0.273251
-28.716284	-2.412314	1.496435	0.005890	0.273145
-28.992073	-2.398200	1.501440	0.005941	0.272954
-29.031307	-2.390610	1.506445	0.005949	0.272957
-29.287304	-2.385522	1.511450	0.005996	0.272738
-29.506132	-2.367650	1.516454	0.006037	0.272622
-29.401152	-2.387912	1.521459	0.006017	0.272616
-29.257632	-2.466740	1.526464	0.005990	0.272336
-29.613697	-2.408106	1.531469	0.006057	0.272304
-29.924128	-2.367431	1.536474	0.006114	0.272220
-29.861065	-2.423461	1.541478	0.006102	0.271984
-29.870812	-2.423657	1.546483	0.006104	0.271974
-30.124989	-2.408867	1.551488	0.006151	0.271807
-30.384595	-2.383210	1.556493	0.006200	0.271692
-30.277759	-2.404146	1.561498	0.006180	0.271685
-30.626074	-2.395015	1.566502	0.006244	0.271396
-30.934797	-2.346384	1.571507	0.006302	0.271356
-30.556171	-2.425997	1.576512	0.006231	0.271299
-30.645043	-2.456098	1.581517	0.006248	0.271053
-31.005071	-2.391887	1.586522	0.006315	0.271046
-30.829455	-2.456788	1.591526	0.006282	0.270871
-31.273055	-2.402168	1.596531	0.006364	0.270732
-31.319247	-2.393866	1.601536	0.006373	0.270732
-31.503824	-2.404845	1.606541	0.006407	0.270494
-31.630497	-2.385580	1.611546	0.006431	0.270474
-31.670135	-2.395552	1.616550	0.006438	0.270382
-32.067135	-2.370740	1.621555	0.006512	0.270129
-31.715687	-2.434316	1.626560	0.006446	0.270131
-31.984466	-2.422573	1.631565	0.006496	0.269932
-32.509403	-2.349837	1.636570	0.006594	0.269811
-32.221138	-2.400297	1.641574	0.006540	0.269822
-32.345867	-2.438675	1.646579	0.006563	0.269494
-32.737922	-2.369110	1.651584	0.006636	0.269485
-32.793659	-2.373237	1.656589	0.006647	0.269409
-32.888608	-2.394533	1.661594	0.006664	0.269202
-32.984011	-2.375920	1.666598	0.006682	0.269209
-33.244409	-2.369056	1.671603	0.006730	0.268992
-33.085130	-2.421875	1.676608	0.006701	0.268864
-33.034219	-2.432107	1.681613	0.006691	0.268859
-33.841079	-2.341999	1.686618	0.006841	0.268554
-33.749359	-2.357297	1.691622	0.006824	0.268562
-33.523124	-2.417604	1.696627	0.006782	0.268459
-33.915786	-2.387719	1.701632	0.006855	0.268236
-34.508636	-2.277619	1.706637	0.006965	0.268248
-34.276735	-2.351059	1.711642	0.006922	0.268080
-34.288158	-2.372128	1.716646	0.006924	0.267955
-34.613216	-2.314035	1.721651	0.006984	0.267950
-34.613819	-2.364987	1.726656	0.006984	0.267674
-34.718923	-2.357315	1.731661	0.007004	0.267613
-34.975383	-2.317244	1.736666	0.007052	0.267578
-34.846555	-2.392164	1.741670	0.007028	0.267299
-35.024944	-2.361368	1.746675	0.007061	0.267291
-35.323502	-2.331509	1.751680	0.007116	0.267159
-35.671857	-2.301460	1.756685	0.007181	0.266979
-35.431655	-2.347718	1.761690	0.007136	0.266965
-35.287682	-2.406418	1.766694	0.007109	0.266789
-36.261204	-2.248182	1.771699	0.007290	0.266687
-35.800958	-2.331299	1.776704	0.007205	0.266691
-35.727446	-2.399138	1.781709	0.007191	0.266396
-36.320281	-2.300525	1.786714	0.007301	0.266346
-36.246192	-2.321677	1.791718	0.007287	0.266305
-36.227577	-2.373027	1.796723	0.007284	0.266044
-36.315734	-2.357048	1.801728	0.007300	0.266044
-36.515358	-2.350353	1.806733	0.007337	0.265883
-37.037006	-2.285530	1.811738	0.007434	0.265720
-36.702839	-2.344169	1.816742	0.007372	0.265732
-37.159388	-2.298809	1.821747	0.007457	0.265527
-37.419899	-2.261475	1.826752	0.007505	0.265473
-37.013987	-2.335405	1.831757	0.007430	0.265473
-37.736887	-2.266195	1.836762	0.007564	0.265133
-37.480157	-2.313204	1.841766	0.007516	0.265132
-37.529623	-2.318565	1.846771	0.007525	0.265054
-37.714426	-2.330221	1.851776	0.007560	0.264807
-37.787746	-2.316666	1.856781	0.007573	0.264808
-37.928118	-2.326023	1.861786	0.007599	0.264618
-37.970980	-2.343022	1.866790	0.007607	0.264483
-38.158257	-2.310491	1.871795	0.007642	0.264475
-38.403787	-2.311310	1.876800	0.007688	0.264226
-38.428126	-2.311675	1.881805	0.007692	0.264200
-38.530802	-2.307256	1.886810	0.007711	0.264122
-38.738233	-2.317355	1.891814	0.007750	0.263860
-38.901938	-2.288465	1.896819	0.007780	0.263856
-38.779674	-2.338517	1.901824	0.007757	0.263704
-39.227545	-2.285452	1.906829	0.007841	0.263548
-39.249217	-2.282508	1.911834	0.007845	0.263543
-38.901277	-2.389795	1.916838	0.007780	0.263302
-39.550273	-2.286079	1.921843	0.007900	0.263223
-39.434334	-2.316248	1.926848	0.007879	0.263174
-39.158971	-2.410020	1.931853	0.007828	0.262934
-39.736641	-2.304929	1.936858	0.007935	0.262934
-39.497243	-2.385347	1.941862	0.007890	0.262731
-40.089593	-2.303792	1.946867	0.008000	0.262587
-39.706317	-2.375584	1.951872	0.007929	0.262576
-40.030534	-2.370588	1.956877	0.007989	0.262279
-40.316851	-2.320147	1.961882	0.008043	0.262270
-39.905343	-2.421311	1.966886	0.007966	0.262125
-40.585746	-2.328271	1.971891	0.008092	0.261956
-41.217485	-2.213060	1.976896	0.008210	0.261958
-40.743351	-2.340015	1.981901	0.008122	0.261733
-41.064264	-2.292969	1.986906	0.008181	0.261671
-41.328021	-2.250752	1.991910	0.008230	0.261639
-41.700318	-2.236803	1.996915	0.008300	0.261342
-41.210667	-2.335594	2.001920	0.008208	0.261289

-41.687208	-2.295118	2.011917	0.008297	0.261033
-41.982257	-2.276867	2.021914	0.008352	0.260837
-42.100966	-2.276412	2.031910	0.008374	0.260721
-42.211974	-2.287958	2.041907	0.008394	0.260545
-42.050793	-2.331352	2.051904	0.008364	0.260468
-42.115219	-2.348458	2.061901	0.008376	0.260309
-42.581426	-2.296455	2.071898	0.008462	0.260127
-42.790831	-2.256711	2.081894	0.008501	0.260137
-42.588033	-2.309697	2.091891	0.008463	0.260048
-42.616987	-2.347550	2.101888	0.008469	0.259809
-42.700194	-2.333199	2.111885	0.008484	0.259805
-42.507988	-2.368896	2.121882	0.008448	0.259802
-42.747634	-2.324971	2.131878	0.008492	0.259805
-42.798296	-2.315552	2.141875	0.008502	0.259807
-42.755579	-2.323142	2.151872	0.008494	0.259809
-42.714473	-2.331417	2.161869	0.008486	0.259805
-42.933444	-2.290394	2.171866	0.008526	0.259813
-42.917252	-2.293001	2.181862	0.008523	0.259815
-42.836064	-2.308642	2.191859	0.008508	0.259811
-42.521664	-2.366632	2.201856	0.008449	0.259808
-42.799494	-2.316167	2.211853	0.008501	0.259808
-42.786493	-2.317443	2.221850	0.008498	0.259815
-43.374902	-2.190224	2.231846	0.008608	0.259928
-42.616986	-2.291246	2.241843	0.008466	0.260135
-42.298989	-2.350196	2.251840	0.008407	0.260129
-42.732060	-2.271408	2.261837	0.008487	0.260130
-42.153264	-2.347765	2.271834	0.008380	0.260292
-42.172944	-2.312663	2.281830	0.008383	0.260468
-42.059277	-2.333181	2.291827	0.008362	0.260470
-41.845384	-2.359438	2.301824	0.008322	0.260541
-41.854657	-2.328147	2.311821	0.008323	0.260707
-42.032753	-2.294430	2.321818	0.008356	0.260715
-41.710046	-2.312517	2.331814	0.008296	0.260941
-41.733908	-2.291406	2.341811	0.008300	0.261035
-41.495791	-2.311610	2.351808	0.008256	0.261164
-41.748248	-2.232959	2.361805	0.008303	0.261346
-41.210411	-2.313557	2.371802	0.008202	0.261443
-41.264390	-2.261510	2.381798	0.008212	0.261678
-41.175749	-2.255570	2.391795	0.008196	0.261800
-40.937507	-2.268589	2.401792	0.008151	0.261969
-41.058038	-2.210501	2.411789	0.008173	0.262170
-40.568547	-2.277583	2.421786	0.008082	0.262292
-40.212964	-2.298046	2.431782	0.008016	0.262537
-39.931286	-2.337731	2.441779	0.007963	0.262601
-39.795419	-2.304347	2.451776	0.007938	0.262922
-39.506747	-2.348880	2.461773	0.007884	0.262967
-39.156728	-2.366297	2.471770	0.007818	0.263223
-39.204906	-2.339702	2.481766	0.007827	0.263322
-38.773677	-2.376817	2.491763	0.007747	0.263550
-38.774998	-2.346560	2.501760	0.007747	0.263715
-38.567706	-2.358653	2.511757	0.007708	0.263857
-38.395141	-2.338050	2.521754	0.007676	0.264143
-38.370815	-2.324302	2.531750	0.007671	0.264243
-37.864837	-2.372961	2.541747	0.007577	0.264482
-38.107786	-2.294184	2.551744	0.007622	0.264672
-37.745512	-2.333659	2.561741	0.007554	0.264817
-37.718507	-2.281548	2.571738	0.007549	0.265130
-37.372788	-2.312740	2.581734	0.007485	0.265304
-37.024692	-2.346720	2.591731	0.007420	0.265465
-37.089764	-2.286070	2.601728	0.007431	0.265732
-36.930452	-2.282657	2.611725	0.007402	0.265909
-36.827515	-2.267179	2.621722	0.007382	0.266096
-36.494223	-2.279969	2.631718	0.007320	0.266357
-36.236936	-2.279725	2.641715	0.007272	0.266613
-36.150671	-2.262142	2.651712	0.007256	0.266795
-35.673519	-2.315336	2.661709	0.007167	0.266978
-35.662755	-2.260216	2.671706	0.007165	0.267288
-35.531303	-2.246782	2.681702	0.007140	0.267491
-35.136404	-2.278716	2.691699	0.007066	0.267708
-35.102196	-2.236414	2.701696	0.007060	0.267971
-34.498202	-2.300429	2.711693	0.006947	0.268220
-34.840193	-2.199729	2.721690	0.007011	0.268428
-34.145310	-2.288504	2.731686	0.006881	0.268632
-34.032535	-2.262119	2.741683	0.006860	0.268885
-33.760084	-2.257206	2.751680	0.006809	0.269179
-33.410089	-2.286640	2.761677	0.006744	0.269364
-33.309676	-2.269299	2.771674	0.006725	0.269556
-32.918101	-2.290303	2.781670	0.006652	0.269827
-32.615357	-2.296869	2.791667	0.006595	0.270088
-32.880986	-2.204234	2.801664	0.006645	0.270326
-32.282051	-2.272820	2.811661	0.006533	0.270543
-32.222970	-2.245115	2.821658	0.006522	0.270750
-31.827571	-2.266086	2.831654	0.006448	0.271023
-31.353057	-2.315142	2.841651	0.006360	0.271222
-31.073232	-2.329530	2.851648	0.006307	0.271418
-30.938400	-2.302052	2.861645	0.006282	0.271696
-30.875034	-2.269709	2.871642	0.006270	0.271931
-30.545610	-2.290285	2.881638	0.006209	0.272141
-30.458654	-2.263704	2.891635	0.006192	0.272367
-29.904616	-2.317050	2.901632	0.006089	0.272620
-29.559449	-2.327145	2.911629	0.006024	0.272900
-29.693210	-2.266418	2.921626	0.006049	0.273094
-29.518928	-2.256896	2.931622	0.006017	0.273313
-29.158622	-2.273814	2.941619	0.005949	0.273572
-28.812904	-2.285826	2.951616	0.005885	0.273841
-28.727906	-2.256635	2.961613	0.005869	0.274078
-28.715385	-2.216419	2.971610	0.005866	0.274303
-28.172458	-2.274642	2.981606	0.005765	0.274518
-28.170769	-2.214336	2.991603	0.005765	0.274838
-27.578244	-2.276515	3.001600	0.005654	0.275079
-27.553959	-2.236231	3.011597	0.005649	0.275315
-27.119266	-2.275432	3.021594	0.005568	0.275525
-26.968719	-2.263603	3.031590	0.005540	0.275732
-26.771628	-2.246677	3.041587	0.005503	0.276010
-26.417009	-2.268727	3.051584	0.005437	0.276233
-26.371368	-2.232715	3.061581	0.005428	0.276466
-26.182959	-2.219790	3.071578	0.005393	0.276714
-26.121682	-2.177154	3.081574	0.005382	0.276996
-25.875711	-2.170343	3.091571	0.005336	0.277266
-25.476038	-2.194749	3.101568	0.005261	0.277519
-25.701368	-2.100198	3.111565	0.005303	0.277799
-25.661945	-2.050914	3.121562	0.005295	0.278094
-24.764395	-2.175169	3.131558	0.005128	0.278297
-24.577242	-2.153529	3.141555	0.005093	0.278587
-24.209495	-2.166174	3.151552	0.005024	0.278870
-23.691401	-2.215576	3.161549	0.004928	0.279103
-23.623521	-2.183908	3.171546	0.004915	0.279332
-23.318017	-2.197691	3.181542	0.004858	0.279549
-23.290237	-2.145922	3.191539	0.004853	0.279844
-22.543594	-2.230473	3.201536	0.004713	0.280110
-22.531236	-2.186751	3.211533	0.004711	0.280348
-22.378289	-2.171079	3.221530	0.004682	0.280573
-22.187823	-2.172464	3.231526	0.004647	0.280745
-21.792602	-2.185610	3.241523	0.004573	0.281049
-21.515105	-2.188872	3.251520	0.004521	0.281293
-21.569829	-2.129915	3.261517	0.004531	0.281546
-21.117135	-2.167381	3.271514	0.004447	0.281777
-20.554059	-2.232072	3.281510	0.004342	0.281971
-20.385823	-2.200292	3.291507	0.004310	0.282292
-19.880502	-2.250434	3.301504	0.004216	0.282507
-19.723310	-2.238827	3.311501	0.004187	0.282713
-19.336016	-2.263772	3.321498	0.004114	0.282947
-19.212941	-2.232767	3.331494	0.004091	0.283221
-18.736764	-2.281196	3.341491	0.004002	0.283416
-18.670510	-2.253122	3.351488	0.003990	0.283622
-18.248202	-2.282104	3.361485	0.003911	0.283866
-18.171291	-2.241276	3.371482	0.003897	0.284147
-18.087793	-2.217956	3.381478	0.003881	0.284343
-17.735536	-2.243269	3.391475	0.003815	0.284541
-17.845935	-2.166587	3.401472	0.003835	0.284830
-17.275357	-2.216095	3.411469	0.003729	0.285106
-17.274850	-2.168739	3.421466	0.003729	0.285348
-16.897744	-2.197994	3.431462	0.003658	0.285548
-16.777859	-2.181537	3.441459	0.003636	0.285742
-16.437667	-2.180858	3.451456	0.003572	0.286060
-15.809765	-2.254279	3.461453	0.003455	0.286267
-15.604455	-2.252821	3.471450	0.003417	0.286463
-15.459432	-2.234529	3.481446	0.003390	0.286690
-15.159337	-2.232904	3.491443	0.003334	0.286974
-14.957384	-2.227792	3.501440	0.003296	0.287186
-14.589838	-2.255069	3.511437	0.003228	0.287386
-14.218555	-2.277239	3.521434	0.003158	0.287614
-14.033448	-2.250083	3.531430	0.003124	0.287921
-13.845865	-2.247434	3.541427	0.003088	0.288107
-13.402717	-2.294754	3.551424	0.003006	0.288274
-13.097964	-2.291657	3.561421	0.002949	0.288569
-12.932185	-2.279343	3.571418	0.002918	0.288782
-12.760224	-2.274393	3.581414	0.002886	0.288964
-12.149262	-2.337327	3.591411	0.002772	0.289206
-12.114541	-2.296696	3.601408	0.002765	0.289442
-11.800813	-2.318157	3.611405	0.002707	0.289620
-11.819771	-2.273061	3.621402	0.002710	0.289829
-11.567501	-2.256048	3.631398	0.002663	0.290144
-11.271015	-2.266980	3.641395	0.002607	0.290359
-10.920966	-2.294187	3.651392	0.002542	0.290541
-10.618405	-2.309445	3.661389	0.002486	0.290740
-11.005547	-2.184706	3.671386	0.002558	0.291011
-10.458238	-2.242411	3.681382	0.002455	0.291219
-10.560065	-2.176968	3.691379	0.002474	0.291453
-9.978035	-2.232129	3.701376	0.002366	0.291705
-9.520362	-2.263974	3.711373	0.002280	0.291961
-9.254626	-2.274165	3.721370	0.002231	0.292150
-9.238387	-2.236489	3.731366	0.002228	0.292352
-8.839766	-2.254343	3.741363	0.002153	0.292623
-8.773422	-2.209994	3.751360	0.002141	0.292903
-8.345077	-2.248403	3.761357	0.002061	0.293098
-7.953911	-2.284406	3.771354	0.001988	0.293272
-7.667583	-2.275577	3.781350	0.001934	0.293573
-7.765702	-2.213860	3.791347	0.001952	0.293790
-7.204447	-2.275475	3.801344	0.001848	0.293990
-7.076670	-2.251223	3.811341	0.001824	0.294224
-6.787683	-2.249957	3.821338	0.001770	0.294490
-6.472527	-2.267191	3.831334	0.001711	0.294687
-6.532853	-2.213704	3.841331	0.001722	0.294896
-6.214053	-2.220048	3.851328	0.001663	0.295150
-5.885794	-2.218599	3.861325	0.001601	0.295451
-5.872158	-2.185100	3.871322	0.001599	0.295627
-5.667111	-2.185170	3.881318	0.001560	0.295810
-5.608937	-2.144872	3.891315	0.001549	0.296060
-5.193555	-2.158651	3.901312	0.001472	0.296362
-5.150483	-2.116758	3.911309	0.001463	0.296605
-5.042465	-2.087802	3.921306	0.001443	0.296843
-5.008262	-2.045291	3.931302	0.001437	0.297081
-4.675613	-2.052097	3.941299	0.001375	0.297343
-4.239085	-2.074113	3.951296	0.001293	0.297623
-4.250288	-2.008441	3.961293	0.001295	0.297933
-4.095053	-1.988020	3.971290	0.001266	0.298170
-4.435361	-1.866977	3.981286	0.001329	0.298457
-4.134423	-1.862697	3.991283	0.001273	0.298744
-4.023376	-1.820412	4.001280	0.001252	0.299047
-3.522734	-1.851734	4.011277	0.001159	0.299336
-3.491326	-1.798609	4.021274	0.001153	0.299621
-3.566125	-1.717099	4.031270	0.001166	0.299950
-3.636121	-1.636152	4.041267	0.001179	0.300280
-3.549711	-1.583757	4.051264	0.001163	0.300608
-3.012360	-1.625813	4.061261	0.001063	0.300877
-2.553197	-1.646061	4.071258	0.000977	0.301181
-2.448128	-1.599053	4.081254	0.000957	0.301499
-2.311059	-1.558438	4.091251	0.000932	0.301814
-2.200530	-1.511519	4.101248	0.000911	0.302136
-2.063526	-1.466505	4.111245	0.000885	0.302471
-2.158840	-1.374243	4.121242	0.000903	0.302830
-1.978571	-1.337438	4.131238	0.000869	0.303163
-1.750870	-1.308407	4.141235	0.000826	0.303500
-1.528439	-1.274623	4.151232	0.000785	0.303854
-1.531005	-1.189258	4.161229	0.000785	0.304259
-1.724456	-1.078001	4.171226	0.000821	0.304621
-1.229882	-1.093153	4.181222	0.000728	0.304977
-0.893237	-1.075296	4.191219	0.000666	0.305352
-0.883538	-1.006545	4.201216	0.000664	0.305687
-1.080933	-0.887939	4.211213	0.000700	0.306079
-0.649162	-0.881206	4.221210	0.000620	0.306482
-0.253055	-0.876864	4.231206	0.000546	0.306843
-0.018308	-0.843832	4.241203	0.000502	0.307200
0.022348	-0.768568	4.251200	0.000494	0.307590
0.188924	-0.703545	4.261197	0.000463	0.308038
0.375927	-0.660684	4.271194	0.000428	0.308400
0.141875	-0.536176	4.281190	0.000471	0.308785
0.235626	-0.454697	4.291187	0.000453	0.309247
0.169078	-0.354690	4.301184	0.000466	0.309659
-0.011567	-0.228100	4.311181	0.000499	0.310097
0.320628	-0.180153	4.321178	0.000437	0.310603
0.611847	-0.156120	4.331174	0.000383	0.310962
0.554838	-0.042311	4.341171	0.000393	0.311443
0.000000	0.153456	4.351168	0.000496	0.311885

-0.078868	0.436802	4.356173	0.000510	0.313131
0.334529	0.922590	4.361178	0.000433	0.315712
1.133061	1.625582	4.366182	0.000284	0.319575
1.676479	2.671228	4.371187	0.000182	0.324714
2.621818	3.945658	4.376192	0.000005	0.331095
3.932315	5.446607	4.381197	-0.000240	0.338607
6.441010	7.047395	4.386202	-0.000708	0.347281
9.973974	8.788487	4.391206	-0.001367	0.357065
14.415842	10.695015	4.396211	-0.002196	0.367888
20.221500	12.726021	4.401216	-0.003278	0.379817
28.445370	14.700449	4.406221	-0.004811	0.392786
40.909591	16.332107	4.411226	-0.007133	0.406849
54.745955	18.185378	4.416230	-0.009711	0.422046
63.027389	21.493986	4.421235	-0.011255	0.438193
73.071597	24.921780	4.426240	-0.013127	0.455151
80.699812	29.236130	4.431245	-0.014551	0.472868
88.214934	33.994695	4.436250	-0.015953	0.491185
96.734940	39.016586	4.441254	-0.017543	0.510097
103.883777	44.697310	4.446259	-0.018878	0.529449
112.566706	50.517687	4.451264	-0.020498	0.549205
117.683426	57.374808	4.456269	-0.021456	0.569269
122.727630	64.602161	4.461274	-0.022400	0.589521
128.007178	72.112513	4.466278	-0.023388	0.609864
131.756084	80.215852	4.471283	-0.024091	0.630275
134.240498	88.810194	4.476288	-0.024559	0.650629
136.650322	97.644838	4.481293	-0.025014	0.670851
138.930266	106.708491	4.486298	-0.025444	0.690908
141.267182	115.943475	4.491302	-0.025886	0.710766
144.404546	125.193780	4.496307	-0.026476	0.730392
147.100331	134.693291	4.501312	-0.026984	0.749831
149.336668	144.370529	4.506317	-0.027407	0.768956
153.092351	153.883448	4.511322	-0.028113	0.787807
155.981838	163.635671	4.516326	-0.028657	0.806367
158.631035	173.496347	4.521331	-0.029157	0.824623
161.995168	183.290825	4.526336	-0.029790	0.842583
164.910623	193.180031	4.531341	-0.030339	0.860192
167.764245	203.093282	4.536346	-0.030877	0.877467
170.563838	213.012590	4.541350	-0.031405	0.894400
173.771906	222.859688	4.546355	-0.032009	0.911016
176.336551	232.798078	4.551360	-0.032493	0.927298
178.366294	242.791801	4.556365	-0.032877	0.943238
181.205105	252.595448	4.561370	-0.033412	0.958839
184.437426	262.298454	4.566374	-0.034021	0.974141
187.170232	272.058743	4.571379	-0.034536	0.989160
189.954492	281.748086	4.576384	-0.035061	1.003864
192.467285	291.407225	4.581389	-0.035535	1.018244
194.741811	301.060945	4.586394	-0.035965	1.032357
196.362792	310.740913	4.591398	-0.036273	1.046158
197.558985	320.430891	4.596403	-0.036502	1.059692
199.438694	329.922224	4.601408	-0.036858	1.072947
200.967578	339.373195	4.606413	-0.037149	1.085905
202.780696	348.724490	4.611418	-0.037493	1.098642
204.712389	357.992891	4.616422	-0.037859	1.111152
206.083048	367.286557	4.621427	-0.038120	1.123430
208.151633	376.407648	4.626432	-0.038511	1.135508
209.958113	385.510843	4.631437	-0.038854	1.147378
211.772237	394.585935	4.636442	-0.039198	1.159092
213.232034	403.636932	4.641446	-0.039475	1.170585
214.534899	412.651594	4.646451	-0.039724	1.181887
216.264415	421.569614	4.651456	-0.040052	1.193054
217.910051	430.425884	4.656461	-0.040364	1.204024
220.549122	439.107521	4.661466	-0.040861	1.214888
222.665464	447.858721	4.666470	-0.041261	1.225632
224.275819	456.656299	4.671475	-0.041567	1.236236
225.787991	465.421755	4.676480	-0.041854	1.246692
227.073112	474.184120	4.681485	-0.042099	1.257013
228.896405	482.832646	4.686490	-0.042444	1.267223
230.575530	491.484387	4.691494	-0.042763	1.277327
232.054003	500.113563	4.696499	-0.043044	1.287288
234.293899	508.632000	4.701504	-0.043467	1.297191
236.001735	517.209704	4.706509	-0.043790	1.306985
237.551028	525.867030	4.711514	-0.044084	1.316763
239.039388	534.395728	4.716518	-0.044367	1.326317
240.580652	542.914436	4.721523	-0.044660	1.335801
242.375253	551.365927	4.726528	-0.045000	1.345192
243.456770	559.927274	4.731533	-0.045207	1.354506
244.912202	568.387985	4.736538	-0.045483	1.363716
246.111259	576.900367	4.741542	-0.045712	1.372873
246.767334	585.448851	4.746547	-0.045840	1.381912
247.836805	593.926373	4.751552	-0.046045	1.390890
248.849174	602.356072	4.756557	-0.046239	1.399750
249.698098	610.806288	4.761562	-0.046402	1.408548
250.751251	619.215481	4.766566	-0.046604	1.417284
251.528171	627.631472	4.771571	-0.046754	1.425927
252.477776	636.036794	4.776576	-0.046937	1.434535
253.308388	644.404490	4.781581	-0.047097	1.443034
254.318965	652.762391	4.786586	-0.047290	1.451502
255.353564	661.098492	4.791590	-0.047489	1.459904
255.979670	669.496760	4.796595	-0.047611	1.468252
257.324097	677.785912	4.801600	-0.047867	1.476562
258.769814	685.982904	4.806605	-0.048141	1.484751
259.695091	694.340432	4.811610	-0.048319	1.492967
261.732817	702.476300	4.816614	-0.048704	1.501100
263.612720	710.665801	4.821619	-0.049059	1.509215
265.129224	718.930707	4.826624	-0.049347	1.517300
266.474516	727.174715	4.831629	-0.049603	1.525297
267.733117	735.493871	4.836634	-0.049843	1.533308
268.877337	743.782895	4.841638	-0.050061	1.541232
269.694030	752.122817	4.846643	-0.050219	1.549113
270.519506	760.453466	4.851648	-0.050378	1.556946
271.390853	768.725066	4.856653	-0.050546	1.564692
271.915924	777.097350	4.861658	-0.050649	1.572441
273.015520	785.313972	4.866662	-0.050859	1.580094
274.209456	793.530550	4.871667	-0.051087	1.587724
275.954921	801.664097	4.876672	-0.051418	1.595322
277.361924	809.866885	4.881677	-0.051685	1.602896
279.309002	817.988232	4.886682	-0.052053	1.610440
280.892730	826.193364	4.891686	-0.052353	1.617970
281.969136	834.448593	4.896691	-0.052559	1.625437
282.541305	842.852899	4.901696	-0.052671	1.632929
283.418242	851.069039	4.906701	-0.052840	1.640265
284.212900	859.327370	4.911706	-0.052993	1.647593
284.967223	867.582917	4.916710	-0.053139	1.654881
286.410744	875.704029	4.921715	-0.053413	1.662115
287.458370	883.925867	4.926720	-0.053614	1.669349
287.951236	892.202935	4.931725	-0.053711	1.676524
288.860222	900.394223	4.936730	-0.053886	1.683651
289.803471	908.594509	4.941734	-0.054067	1.690761
290.526197	916.827817	4.946739	-0.054207	1.697838
291.341072	925.028747	4.951744	-0.054364	1.704871
292.044053	933.259602	4.956749	-0.054500	1.711885
292.607136	941.475327	4.961754	-0.054611	1.718839
293.113682	949.683970	4.966758	-0.054710	1.725751
293.967021	957.845948	4.971763	-0.054875	1.732642
294.715263	966.034786	4.976768	-0.055019	1.739514
295.483787	974.192329	4.981773	-0.055168	1.746336
296.322714	982.377662	4.986778	-0.055330	1.753163
297.419307	990.486426	4.991782	-0.055539	1.759933
297.741031	998.715413	4.996787	-0.055604	1.766677
299.317180	1006.795677	5.001792	-0.055903	1.773432
300.337884	1014.924693	5.006797	-0.056099	1.780131
301.150050	1023.121142	5.011802	-0.056255	1.786833
301.895155	1031.345398	5.016806	-0.056400	1.793523
302.814169	1039.456138	5.021811	-0.056576	1.800119
303.909489	1047.584363	5.026816	-0.056785	1.806727
304.703233	1055.752095	5.031821	-0.056939	1.813304
305.274637	1063.933428	5.036826	-0.057050	1.819841
306.066919	1072.099528	5.041830	-0.057203	1.826369
306.566341	1080.299960	5.046835	-0.057302	1.832865
307.044684	1088.490048	5.051840	-0.057396	1.839328
307.774878	1096.595829	5.056845	-0.057538	1.845732
308.762495	1104.716903	5.061850	-0.057727	1.852156
309.301137	1112.902276	5.066854	-0.057832	1.858554
309.582017	1121.086341	5.071859	-0.057890	1.864899
310.341630	1129.230184	5.076864	-0.058037	1.871247
310.707231	1137.393022	5.081869	-0.058111	1.877543
311.337239	1145.514789	5.086874	-0.058233	1.883816
311.946258	1153.645237	5.091878	-0.058352	1.890073
312.633357	1161.773174	5.096883	-0.058485	1.896316
312.948605	1169.951156	5.101888	-0.058549	1.902533
313.235075	1178.125080	5.106893	-0.058608	1.908724
314.122938	1186.191315	5.111898	-0.058779	1.914882
315.098087	1194.259204	5.116902	-0.058966	1.921031
315.717268	1202.383156	5.121907	-0.059086	1.927162
316.662098	1210.498449	5.126912	-0.059268	1.933303
317.131487	1218.649065	5.131917	-0.059360	1.939398
317.890596	1226.757358	5.136922	-0.059507	1.945475
318.531335	1234.911832	5.141926	-0.059632	1.951553
319.075350	1243.006573	5.146931	-0.059739	1.957558
319.661009	1251.127032	5.151936	-0.059853	1.963567
320.158571	1259.244971	5.156941	-0.059951	1.969547
320.755359	1267.374470	5.161946	-0.060067	1.975527
321.439847	1275.477238	5.166950	-0.060200	1.981480
322.033152	1283.583786	5.171955	-0.060316	1.987407
322.970279	1291.684188	5.176960	-0.060496	1.993349
323.184004	1299.848548	5.181965	-0.060541	1.999242
323.640994	1307.963958	5.186970	-0.060632	2.005108
324.021825	1316.101940	5.191974	-0.060708	2.010965
324.732916	1324.179044	5.196979	-0.060846	2.016796
325.359064	1332.288532	5.201984	-0.060968	2.022624
325.646368	1340.448667	5.206989	-0.061026	2.028436
326.324118	1348.552900	5.211994	-0.061158	2.034232
327.318848	1356.573058	5.216998	-0.061349	2.039986
327.767492	1364.677973	5.222003	-0.061437	2.045726
328.161538	1372.842854	5.227008	-0.061516	2.051486
328.111472	1381.029565	5.232013	-0.061512	2.057199
328.572160	1389.106204	5.237018	-0.061603	2.062873
329.123241	1397.218104	5.242022	-0.061711	2.068564
329.800909	1405.271108	5.247027	-0.061843	2.074211
330.394670	1413.352088	5.252032	-0.061959	2.079854
330.630167	1421.471017	5.257037	-0.062008	2.085472
331.186363	1429.588525	5.262042	-0.062117	2.091105
331.566607	1437.722275	5.267046	-0.062193	2.096717
331.966906	1445.799519	5.272051	-0.062273	2.102277
332.670991	1453.879853	5.277056	-0.062410	2.107855
333.130284	1462.010961	5.282061	-0.062500	2.113428
333.578142	1470.093174	5.287066	-0.062589	2.118952
333.801470	1478.201089	5.292070	-0.062636	2.124456
334.154112	1486.271706	5.297075	-0.062707	2.129934
334.439921	1494.409959	5.302080	-0.062766	2.135437
334.913396	1502.471159	5.307085	-0.062859	2.140892
335.553634	1510.544278	5.312090	-0.062984	2.146357
336.136243	1518.622868	5.317094	-0.063098	2.151807
336.614506	1526.685949	5.322099	-0.063192	2.157222
337.320702	1534.746928	5.327104	-0.063329	2.162643
337.882771	1542.833244	5.332109	-0.063439	2.168054
338.364856	1550.942157	5.337114	-0.063534	2.173459
338.604156	1559.089877	5.342118	-0.063584	2.178852
339.036101	1567.152610	5.347123	-0.063670	2.184195
339.538843	1575.250376	5.352128	-0.063769	2.189554
339.898439	1583.347609	5.357133	-0.063841	2.194886
340.493919	1591.401695	5.362138	-0.063957	2.200199
341.174825	1599.442493	5.367142	-0.064089	2.205498
341.782620	1607.496158	5.372147	-0.064208	2.210786
342.195635	1615.630579	5.377152	-0.064290	2.216096
342.691043	1623.698036	5.382157	-0.064388	2.221357
342.992965	1631.820951	5.387162	-0.064449	2.226624
343.419005	1639.931802	5.392166	-0.064534	2.231881
343.861330	1647.978018	5.397171	-0.064622	2.237086
344.423195	1656.047784	5.402176	-0.064732	2.242305
344.771869	1664.136766	5.407181	-0.064802	2.247505
345.675615	1672.171095	5.412186	-0.064975	2.252707
346.337926	1680.247788	5.417190	-0.065104	2.257903
346.366206	1688.393264	5.422195	-0.065115	2.263073
346.647907	1696.537691	5.427200	-0.065173	2.268254
347.144426	1704.616915	5.432205	-0.065270	2.273401
347.618440	1712.658917	5.437210	-0.065364	2.278510
348.223535	1720.675306	5.442214	-0.065482	2.283604
348.710037	1728.742383	5.447219	-0.065578	2.288707
349.415290	1736.818318	5.452224	-0.065714	2.293823
349.771731	1744.873596	5.457229	-0.065786	2.298885
350.066354	1752.971206	5.462234	-0.065846	2.303956
350.798835	1761.022363	5.467238	-0.065988	2.309025
350.989560	1769.141230	5.472243	-0.066029	2.314079
351.742818	1777.169263	5.477248	-0.066175	2.319112
352.301798	1785.195087	5.482253	-0.066284	2.324118
352.698418	1793.305694	5.487258	-0.066363	2.329150
353.163357	1801.410571	5.492262	-0.066455	2.334174
353.519108	1809.490846	5.497267	-0.066527	2.339163
354.168703	1817.540439	5.502272	-0.066653	2.344147
354.487479	1825.631134	5.507277	-0.066718	2.349117
354.872678	1833.718900	5.512282	-0.066795	2.354081
355.574864	1841.757913	5.517286	-0.066931	2.359031
355.977453	1849.802371	5.522291	-0.067011	2.363949
356.111968	1857.962520	5.527296	-0.067042	2.368905
356.817797	1865.956255	5.532301	-0.067178	2.373796
357.092727	1874.058981	5.537306	-0.067235	2.378708
357.435665	1882.132649	5.542310	-0.067304	2.383598
357.990297	1890.158016	5.547315	-0.067413	2.388465
358.509896	1898.252262	5.552320	-0.067515	2.393361
358.851267	1906.317097	5.557325	-0.067584	2.398215
359.108587	1914.391185	5.562330	-0.067637	2.403058
359.633245	1922.462532	5.567334	-0.067740	2.407911
360.006974	1930.548860	5.572339	-0.067815	2.412751
360.356400	1938.632549	5.577344	-0.067885	2.417578
360.773169	1946.659851	5.582349	-0.067968	2.422367
361.203766	1954.726326	5.587354	-0.068054	2.427170
361.456144	1962.857608	5.592358	-0.068106	2.431988
361.790091	1970.910284	5.597363	-0.068174	2.436757
362.104878	1978.972725	5.602368	-0.068237	2.441521
362.230175	1987.027145	5.607373	-0.068266	2.446255
362.454922	1995.103896	5.612378	-0.068313	2.451002
363.051035	2003.119218	5.617382	-0.068430	2.455732
363.155629	2011.212870	5.622387	-0.068454	2.460460
363.494667	2019.285487	5.627392	-0.068523	2.465185
363.712889	2027.354967	5.632397	-0.068569	2.469890
364.045463	2035.402924	5.637402	-0.068636	2.474583
364.313784	2043.447781	5.642406	-0.068691	2.479259
364.529743	2051.475355	5.647411	-0.068737	2.483913
365.153304	2059.522739	5.652416	-0.068858	2.488600
365.246937	2067.619356	5.657421	-0.068881	2.493267
365.026534	2075.752424	5.662426	-0.068846	2.497922
365.696412	2083.747997	5.667430	-0.068976	2.502557
365.640930	2091.857956	5.672435	-0.068971	2.507194
365.794422	2099.947950	5.677440	-0.069005	2.511827
365.974183	2107.988214	5.682445	-0.069043	2.516424
366.542112	2115.979535	5.687450	-0.069154	2.521014
366.544340	2124.068235	5.692454	-0.069160	2.525610
366.561001	2132.150261	5.697459	-0.069169	2.530194
367.252606	2140.143507	5.702464	-0.069303	2.534769
367.457375	2148.194386	5.707469	-0.069346	2.539333
367.396384	2156.291120	5.712474	-0.069340	2.543895
367.553439	2164.388935	5.717478	-0.069375	2.548465
367.971748	2172.395787	5.722483	-0.069458	2.552995
368.422122	2180.425297	5.727488	-0.069547	2.557532
368.342015	2188.519792	5.732493	-0.069537	2.562059
368.608636	2196.548764	5.737498	-0.069592	2.566566
368.772276	2204.643997	5.742502	-0.069628	2.571095
368.915357	2212.699558	5.747507	-0.069660	2.575592
369.194202	2220.761691	5.752512	-0.069717	2.580094
369.353864	2228.788108	5.757517	-0.069753	2.584561
369.495202	2236.877912	5.762522	-0.069784	2.589053
369.877209	2245.016835	5.767526	-0.069861	2.593582
370.202523	2253.005885	5.772531	-0.069927	2.598016
370.217129	2261.061074	5.777536	-0.069935	2.602457
370.421887	2269.070176	5.782541	-0.069978	2.606879
370.796978	2277.089348	5.787546	-0.070053	2.611310
371.101843	2285.157352	5.792550	-0.070115	2.615756
370.760870	2293.254410	5.797555	-0.070057	2.620166
371.258780	2301.258250	5.802560	-0.070155	2.624574
371.541079	2309.291474	5.807565	-0.070213	2.628977
371.642842	2317.377943	5.812570	-0.070237	2.633388
371.732897	2325.434103	5.817574	-0.070259	2.637776
372.014748	2333.430528	5.822579	-0.070317	2.642136
372.475912	2341.476429	5.827584	-0.070408	2.646528
372.423194	2349.582281	5.832589	-0.070404	2.650911
372.633051	2357.631619	5.837594	-0.070448	2.655273
373.044682	2365.637675	5.842598	-0.070530	2.659618
372.880606	2373.725372	5.847603	-0.070505	2.663962
373.239376	2381.781914	5.852608	-0.070577	2.668317
373.001714	2389.920689	5.857613	-0.070538	2.672669
373.299253	2397.918628	5.862618	-0.070599	2.676974
373.408268	2405.954354	5.867622	-0.070625	2.681280
373.805176	2413.930011	5.872627	-0.070704	2.685565
373.746796	2422.059512	5.877632	-0.070698	2.689897
374.020624	2430.065544	5.882637	-0.070755	2.694176
374.549167	2438.067150	5.887642	-0.070858	2.698464
375.166272	2446.072857	5.892646	-0.070979	2.702752
375.023098	2454.176931	5.897651	-0.070957	2.707036
375.219262	2462.268825	5.902656	-0.070999	2.711329
376.003010	2470.193528	5.907661	-0.071150	2.715565
376.265901	2478.255251	5.912666	-0.071205	2.719832
376.477264	2486.300964	5.917670	-0.071249	2.724082
376.648310	2494.376086	5.922675	-0.071286	2.728337
376.849517	2502.486512	5.927680	-0.071329	2.732607
376.842540	2510.555291	5.932685	-0.071333	2.736835
377.264088	2518.572360	5.937690	-0.071417	2.741056
377.716925	2526.572000	5.942694	-0.071507	2.745263
378.040229	2534.626518	5.947699	-0.071572	2.749484
378.127222	2542.778617	5.952704	-0.071594	2.753735
378.705428	2550.738024	5.957709	-0.071707	2.757909
378.719037	2558.801212	5.962714	-0.071715	2.762097
379.040703	2566.822233	5.967718	-0.071780	2.766274
379.151619	2574.883408	5.972723	-0.071806	2.770454
379.410061	2582.936461	5.977728	-0.071859	2.774632
379.376938	2590.997887	5.982733	-0.071858	2.778790
379.716456	2599.008310	5.987738	-0.071927	2.782938
380.085985	2607.037089	5.992742	-0.072001	2.787091
380.183618	2615.090964	5.997747	-0.072025	2.791235
380.539783	2623.143171	6.002752	-0.072096	2.795387
380.898441	2631.156643	6.007757	-0.072168	2.799513
381.137388	2639.188116	6.012762	-0.072218	2.803635
381.141604	2647.277747	6.017766	-0.072224	2.807767
381.843172	2655.261171	6.022771	-0.072360	2.811879
382.057218	2663.378702	6.027776	-0.072405	2.816025
382.103577	2671.433664	6.032781	-0.072419	2.820123
382.490655	2679.418658	6.037786	-0.072497	2.824200
382.908225	2687.494486	6.042790	-0.072580	2.828319
383.319037	2695.494848	6.047795	-0.072662	2.832393
383.936778	2703.506113	6.052800	-0.072782	2.836478
383.763852	2711.599956	6.057805	-0.072755	2.840553
384.171168	2719.588839	6.062810	-0.072836	2.844604
384.311385	2727.691809	6.067814	-0.072868	2.848690
384.850670	2735.700768	6.072819	-0.072973	2.852746
385.040158	2743.783599	6.077824	-0.073014	2.856813
385.128337	2751.829086	6.082829	-0.073036	2.860851
385.204178	2759.889265	6.087834	-0.073055	2.864889
385.754066	2767.900389	6.092838	-0.073163	2.868923
386.156129	2775.900345	6.097843	-0.073243	2.872938
386.274998	2783.979992	6.102848	-0.073271	2.876971
386.286688	2792.067409	6.107853	-0.073278	2.880996
386.465082	2800.078906	6.112858	-0.073317	2.884987
386.568034	2808.140278	6.117862	-0.073341	2.888994
386.890919	2816.149838	6.122867	-0.073407	2.892981
387.515851	2824.172247	6.127872	-0.073528	2.896985
387.398702	2832.266091	6.132877	-0.073512	2.900979
387.612198	2840.293712	6.137882	-0.073557	2.904952
388.240306	2848.292086	6.142886	-0.073679	2.908928
388.353921	2856.405794	6.147891	-0.073706	2.912927
388.783550	2864.411824	6.152896	-0.073791	2.916886
389.305766	2872.402186	6.157901	-0.073893	2.920835
389.615230	2880.413741	6.162906	-0.073956	2.924779
389.822745	2888.466020	6.167910	-0.074000	2.928731
389.704541	2896.561909	6.172915	-0.073984	2.932682
390.254162	2904.574254	6.177920	-0.074091	2.936623
390.407818	2912.610277	6.182925	-0.074125	2.940548
390.840116	2920.602276	6.187930	-0.074211	2.944462
391.274412	2928.659549	6.192934	-0.074297	2.948402
391.437572	2936.727142	6.197939	-0.074333	2.952328
391.687381	2944.783902	6.202944	-0.074385	2.956248
392.033628	2952.817802	6.207949	-0.074455	2.960156
392.279315	2960.802347	6.212954	-0.074506	2.964030
392.765042	2968.858839	6.217958	-0.074601	2.967946
393.035921	2976.898915	6.222963	-0.074657	2.971838
393.679177	2984.925764	6.227968	-0.074782	2.975738
393.690492	2992.993161	6.232973	-0.074790	2.979619
394.091956	3001.007085	6.237978	-0.074870	2.983490
394.372102	3009.064174	6.242982	-0.074927	2.987370
394.441091	3017.128408	6.247987	-0.074945	2.991238
394.847573	3025.168386	6.252992	-0.075026	2.995106
394.990739	3033.192140	6.257997	-0.075058	2.998948
395.262901	3041.209923	6.263002	-0.075114	3.002788
395.522149	3049.257189	6.268006	-0.075168	3.006637
395.699491	3057.299971	6.273011	-0.075206	3.010475
396.302930	3065.317884	6.278016	-0.075324	3.014318
396.492215	3073.346677	6.283021	-0.075364	3.018140
396.708242	3081.392157	6.288026	-0.075410	3.021966
396.795803	3089.472026	6.293030	-0.075432	3.025798
397.228112	3097.453335	6.298035	-0.075517	3.029594
396.970283	3105.597915	6.303040	-0.075475	3.033430
397.728566	3113.515253	6.308045	-0.075621	3.037203
398.252114	3121.536962	6.313050	-0.075724	3.041009
398.737648	3129.551062	6.318054	-0.075820	3.044805
398.808874	3137.627174	6.323059	-0.075838	3.048604
399.049440	3145.705134	6.328064	-0.075888	3.052409
399.438542	3153.733270	6.333069	-0.075966	3.056192
399.405545	3161.781215	6.338074	-0.075965	3.059959
399.965077	3169.783889	6.343078	-0.076075	3.063729
400.195831	3177.843313	6.348083	-0.076123	3.067505
400.532366	3185.919990	6.353088	-0.076191	3.071290
401.129725	3193.923718	6.358093	-0.076308	3.075048
401.360788	3201.924753	6.363098	-0.076356	3.078783
401.606683	3209.984516	6.368102	-0.076407	3.082541
401.921168	3217.991400	6.373107	-0.076471	3.086274
402.622153	3225.984256	6.378112	-0.076607	3.090013
402.830604	3234.053443	6.383117	-0.076651	3.093760
403.118748	3242.093374	6.388122	-0.076710	3.097493
403.630523	3250.110361	6.393126	-0.076811	3.101221
403.869410	3258.143872	6.398131	-0.076860	3.104939
404.064212	3266.213280	6.403136	-0.076902	3.108667
404.406527	3274.247768	6.408141	-0.076971	3.112382
404.843910	3282.261418	6.413146	-0.077058	3.116087
405.586322	3290.214781	6.418150	-0.077201	3.119774
405.759486	3298.275801	6.423155	-0.077239	3.123479
406.052912	3306.348789	6.428160	-0.077299	3.127191
406.211153	3314.421799	6.433165	-0.077334	3.130893
406.588047	3322.419807	6.438170	-0.077409	3.134565
406.837212	3330.481140	6.443174	-0.077461	3.138257
407.114653	3338.502710	6.448179	-0.077518	3.141927
407.243342	3346.568418	6.453184	-0.077547	3.145606
407.500861	3354.585597	6.458189	-0.077600	3.149265
407.502158	3362.663616	6.463194	-0.077606	3.152935
408.003985	3370.670846	6.468198	-0.077705	3.156592
408.088510	3378.682420	6.473203	-0.077726	3.160228
408.384005	3386.688118	6.478208	-0.077786	3.163866
408.714207	3394.725349	6.483213	-0.077853	3.167515
408.866045	3402.779056	6.488218	-0.077886	3.171160
409.253924	3410.812203	6.493222	-0.077964	3.174802
409.315288	3418.876809	6.498227	-0.077981	3.178439
409.837566	3426.842145	6.503232	-0.078083	3.182048
409.996410	3434.907548	6.508237	-0.078118	3.185682
410.227428	3442.943978	6.513242	-0.078166	3.189301
410.635880	3450.997620	6.518246	-0.078248	3.192932
410.638689	3459.055059	6.523251	-0.078254	3.196543
411.120950	3467.038594	6.528256	-0.078349	3.200138
411.469156	3475.021841	6.533261	-0.078419	3.203722
411.821013	3483.069815	6.538266	-0.078490	3.207331
411.852206	3491.168843	6.543270	-0.078501	3.210946
412.019989	3499.158158	6.548275	-0.078537	3.214513
412.853647	3507.164736	6.553280	-0.078698	3.218112
412.769547	3515.262124	6.558285	-0.078688	3.221709
413.450291	3523.244787	6.563290	-0.078820	3.225282
413.979193	3531.278455	6.568294	-0.078923	3.228868
414.255454	3539.292969	6.573299	-0.078980	3.232431
414.416364	3547.389425	6.578304	-0.079016	3.236021
414.963531	3555.332236	6.583309	-0.079123	3.239556
415.203176	3563.358777	6.588314	-0.079173	3.243110
415.394517	3571.421425	6.593318	-0.079214	3.246675
415.641667	3579.444588	6.598323	-0.079265	3.250221
416.325463	3587.475740	6.603328	-0.079398	3.253784
416.456537	3595.511255	6.608333	-0.079427	3.257322
416.815895	3603.534420	6.613338	-0.079499	3.260861
417.217582	3611.566840	6.618342	-0.079580	3.264401
417.597306	3619.564596	6.623347	-0.079656	3.267922
417.775845	3627.669615	6.628352	-0.079694	3.271477
418.054642	3635.677899	6.633357	-0.079751	3.274990
418.336009	3643.700411	6.638362	-0.079809	3.278506
418.605302	3651.722046	6.643366	-0.079865	3.282017
418.653032	3659.774791	6.648371	-0.079879	3.285529
419.102299	3667.783812	6.653376	-0.079968	3.289034
419.192327	3675.855095	6.658381	-0.079990	3.292548
419.510158	3683.886344	6.663386	-0.080054	3.296050
419.747805	3691.929958	6.668390	-0.080104	3.299550
420.035227	3699.936672	6.673395	-0.080163	3.303033
420.248311	3707.984650	6.678400	-0.080208	3.306527
420.852648	3715.970681	6.683405	-0.080326	3.310005
421.120524	3724.030304	6.688410	-0.080381	3.313499
421.084141	3732.102664	6.693414	-0.080379	3.316982
421.358732	3740.092698	6.698419	-0.080436	3.320439
422.122979	3748.012734	6.703424	-0.080583	3.323880
422.311790	3756.086906	6.708429	-0.080624	3.327362
422.534197	3764.173193	6.713434	-0.080671	3.330847
422.826885	3772.217469	6.718438	-0.080730	3.334313
423.046003	3780.203225	6.723443	-0.080776	3.337747
423.338609	3788.233113	6.728448	-0.080836	3.341199
423.655057	3796.232875	6.733453	-0.080900	3.344636
423.817069	3804.269189	6.738458	-0.080936	3.348079
424.012281	3812.370908	6.743462	-0.080978	3.351547
424.105464	3820.401477	6.748467	-0.081000	3.354978
424.313781	3828.426615	6.753472	-0.081044	3.358407
424.730623	3836.425784	6.758477	-0.081127	3.361830
424.570069	3844.473159	6.763482	-0.081103	3.365248
425.464979	3852.412237	6.768486	-0.081275	3.368655
425.829124	3860.444648	6.773491	-0.081348	3.372079
425.592265	3868.601294	6.778496	-0.081309	3.375530
426.101276	3876.554582	6.783501	-0.081409	3.378919
426.256754	3884.593674	6.788506	-0.081443	3.382327
426.357287	3892.650095	6.793510	-0.081467	3.385738
426.356401	3900.700438	6.798515	-0.081473	3.389138
426.615767	3908.766295	6.803520	-0.081526	3.392552
427.244819	3916.757101	6.808525	-0.081649	3.395943
427.591981	3924.694090	6.813530	-0.081718	3.399298
427.613385	3932.790649	6.818534	-0.081728	3.402706
427.503918	3940.852890	6.823539	-0.081713	3.406091
428.159381	3948.797648	6.828544	-0.081840	3.409450
428.754564	3956.801794	6.833549	-0.081956	3.412828
428.954317	3964.863727	6.838554	-0.081999	3.416214
429.245746	3972.900720	6.843558	-0.082058	3.419589
429.456233	3980.867415	6.848563	-0.082103	3.422928
429.979995	3988.940003	6.853568	-0.082206	3.426319
430.525799	3996.935200	6.858573	-0.082313	3.429675
430.725877	4004.986628	6.863578	-0.082355	3.433040
431.128928	4013.041268	6.868582	-0.082436	3.436409
431.136001	4021.063126	6.873587	-0.082442	3.439748
431.147024	4029.161582	6.878592	-0.082450	3.443115
431.912029	4037.081984	6.883597	-0.082597	3.446431
432.427891	4045.054124	6.888602	-0.082699	3.449756
432.549387	4053.176443	6.893606	-0.082727	3.453128
432.535579	4061.221254	6.898611	-0.082729	3.456459
433.213671	4069.190376	6.903616	-0.082861	3.459779
433.370390	4077.264189	6.908621	-0.082895	3.463121
433.386819	4085.277812	6.913626	-0.082904	3.466431
434.230186	4093.264900	6.918630	-0.083066	3.469754
434.327828	4101.316321	6.923635	-0.083090	3.473075
434.374745	4109.436474	6.928640	-0.083104	3.476420
434.694231	4117.391521	6.933645	-0.083168	3.479703
435.197516	4125.341820	6.938650	-0.083267	3.482987
435.226537	4133.470069	6.943654	-0.083278	3.486325
435.359596	4141.477530	6.948659	-0.083308	3.489614
435.352911	4149.538007	6.953664	-0.083312	3.492916
436.172941	4157.500988	6.958669	-0.083470	3.496203
436.280432	4165.530417	6.963674	-0.083496	3.499490
436.666117	4173.569235	6.968678	-0.083573	3.502787
436.935676	4181.582090	6.973683	-0.083628	3.506067
437.005821	4189.652678	6.978688	-0.083647	3.509361
437.382200	4197.655580	6.983693	-0.083722	3.512634
437.427545	4205.761006	6.988698	-0.083736	3.515934
438.197322	4213.628011	6.993702	-0.083884	3.519158
438.360852	4221.649576	6.998707	-0.083920	3.522423
438.274414	4229.786505	7.003712	-0.083909	3.525723
438.732543	4237.771138	7.008717	-0.084000	3.528975
439.036580	4245.783703	7.013722	-0.084062	3.532231
439.572256	4253.828454	7.018726	-0.084167	3.535504
439.750254	4261.848080	7.023731	-0.084205	3.538753
439.954967	4269.900180	7.028736	-0.084249	3.542013
439.764476	4277.945050	7.033741	-0.084219	3.545254
439.918859	4285.990339	7.038746	-0.084253	3.548504
440.639760	4293.989261	7.043750	-0.084392	3.551749
440.644189	4302.032969	7.048755	-0.084398	3.554987
441.146511	4310.026259	7.053760	-0.084497	3.558217
441.665839	4318.025771	7.058765	-0.084599	3.561447
441.644088	4326.034503	7.063770	-0.084601	3.564661
442.014070	4334.083434	7.068774	-0.084675	3.567901
442.178148	4342.083521	7.073779	-0.084711	3.571112
442.296351	4350.151258	7.078784	-0.084738	3.574345
442.923138	4358.137829	7.083789	-0.084860	3.577558
442.886863	4366.194282	7.088794	-0.084859	3.580777
443.151283	4374.193514	7.093798	-0.084913	3.583978
443.408390	4382.231101	7.098803	-0.084966	3.587192
443.597112	4390.270860	7.103808	-0.085007	3.590402
444.151871	4398.282447	7.108813	-0.085115	3.593608
444.044623	4406.346705	7.113818	-0.085101	3.596813
444.069441	4414.418702	7.118822	-0.085111	3.600022
444.599117	4422.291321	7.123827	-0.085214	3.603164
445.077125	4430.344843	7.128832	-0.085309	3.606373
445.036390	4438.403096	7.133837	-0.085307	3.609566
445.372970	4446.429430	7.138842	-0.085375	3.612755
445.903424	4454.498798	7.143846	-0.085479	3.615963
445.897089	4462.474251	7.148851	-0.085483	3.619116
445.828915	4470.542532	7.153856	-0.085475	3.622301
446.331123	4478.523380	7.158861	-0.085574	3.625465
446.641605	4486.521115	7.163866	-0.085637	3.628627
446.916860	4494.583178	7.168870	-0.085694	3.631811
446.937188	4502.620495	7.173875	-0.085703	3.634975
447.313014	4510.616714	7.178880	-0.085778	3.638130
447.340450	4518.673978	7.183885	-0.085789	3.641297
447.603728	4526.610343	7.188890	-0.085843	3.644420
447.738672	4534.700378	7.193894	-0.085873	3.647597
448.042153	4542.737158	7.198899	-0.085935	3.650754
448.010588	4550.780425	7.203904	-0.085935	3.653903
448.169404	4558.801444	7.208909	-0.085970	3.657045
448.587841	4566.749151	7.213914	-0.086053	3.660163
448.808546	4574.783051	7.218918	-0.086099	3.663307
449.091834	4582.795640	7.223923	-0.086157	3.666441
449.387697	4590.883255	7.228928	-0.086218	3.669602
449.647978	4598.867361	7.233933	-0.086271	3.672719
449.871089	4606.932332	7.238938	-0.086318	3.675864
449.991768	4614.921327	7.243942	-0.086346	3.678974
450.194403	4622.953386	7.248947	-0.086389	3.682100
450.177034	4630.982306	7.253952	-0.086391	3.685216
450.574919	4639.008540	7.258957	-0.086471	3.688340
450.763706	4647.044540	7.263962	-0.086511	3.691459
450.728784	4655.118559	7.268966	-0.086510	3.694584
450.745989	4663.120036	7.273971	-0.086518	3.697680
451.495974	4671.132719	7.278976	-0.086663	3.700797
451.484669	4679.135973	7.283981	-0.086666	3.703888
451.637891	4687.183573	7.288986	-0.086700	3.706997
452.021163	4695.222808	7.293990	-0.086777	3.710107
452.085693	4703.281043	7.298995	-0.086794	3.713213
452.653370	4711.284620	7.304000	-0.086905	3.716308
452.897223	4719.201827	7.309005	-0.086956	3.719359
452.927027	4727.271292	7.314010	-0.086967	3.722461
453.056975	4735.351564	7.319014	-0.086996	3.725567
453.341056	4743.302453	7.324019	-0.087055	3.728624
453.520584	4751.379207	7.329024	-0.087093	3.731725
453.728900	4759.359790	7.334029	-0.087137	3.734786
453.978331	4767.359883	7.339034	-0.087189	3.737854
454.091623	4775.468513	7.344038	-0.087216	3.740957
454.224050	4783.409400	7.349043	-0.087246	3.743994
454.733249	4791.458790	7.354048	-0.087346	3.747079
454.915098	4799.471153	7.359053	-0.087385	3.750140
455.038641	4807.510232	7.364058	-0.087413	3.753207
455.331858	4815.530473	7.369062	-0.087473	3.756268
455.257737	4823.516484	7.374067	-0.087465	3.759305
455.431962	4831.551674	7.379072	-0.087502	3.762364
455.789884	4839.558154	7.384077	-0.087574	3.765413
456.098723	4847.561185	7.389082	-0.087637	3.768458
456.509633	4855.638609	7.394086	-0.087719	3.771531
456.788912	4863.628760	7.399091	-0.087776	3.774566
456.750998	4871.689607	7.404096	-0.087774	3.777617
457.236772	4879.694998	7.409101	-0.087870	3.780657
457.629830	4887.678042	7.414106	-0.087949	3.783683
457.821216	4895.765168	7.419110	-0.087990	3.786742
457.905769	4903.761164	7.424115	-0.088011	3.789762
458.290344	4911.802494	7.429120	-0.088088	3.792803
458.145089	4919.902450	7.434125	-0.088066	3.795852
458.286471	4927.829782	7.439130	-0.088098	3.798839
458.472900	4935.896041	7.444134	-0.088138	3.801878
459.140967	4943.810321	7.449139	-0.088267	3.804868
459.315179	4951.893713	7.454144	-0.088305	3.807908
459.610786	4959.934800	7.459149	-0.088365	3.810932
459.654691	4967.957387	7.464154	-0.088379	3.813942
460.129510	4975.979157	7.469158	-0.088473	3.816958
460.123435	4983.999999	7.474163	-0.088477	3.819960
460.438904	4992.039967	7.479168	-0.088541	3.822975
460.273893	5000.110420	7.484173	-0.088515	3.825988
460.476692	5008.110487	7.489178	-0.088558	3.828981
460.742750	5016.135819	7.494182	-0.088613	3.831981
460.902524	5024.137721	7.499187	-0.088648	3.834969
461.491074	5032.090959	7.504192	-0.088763	3.837945
461.498354	5040.188165	7.509197	-0.088770	3.840960
461.887490	5048.094344	7.514202	-0.088848	3.843910
462.267340	5056.228268	7.519206	-0.088924	3.846941
462.410004	5064.238534	7.524211	-0.088956	3.849920
462.312493	5072.275465	7.529216	-0.088943	3.852901
462.455190	5080.320970	7.534221	-0.088975	3.855888
462.509212	5088.282557	7.539226	-0.088990	3.858839
462.938286	5096.349770	7.544230	-0.089075	3.861835
463.280773	5104.260324	7.549235	-0.089144	3.864769
463.383739	5112.355158	7.554240	-0.089169	3.867764
463.554589	5120.411113	7.559245	-0.089206	3.870744
463.817441	5128.529168	7.564250	-0.089260	3.873746
464.233661	5136.511378	7.569254	-0.089343	3.876699
464.531639	5144.414012	7.574259	-0.089404	3.879618
464.654612	5152.451067	7.579264	-0.089432	3.882580
464.911419	5160.454747	7.584269	-0.089485	3.885531
465.171927	5168.433852	7.589274	-0.089539	3.888470
465.698795	5176.464990	7.594278	-0.089642	3.891432
465.740143	5184.499844	7.599283	-0.089655	3.894382
466.108291	5192.518934	7.604288	-0.089729	3.897332
466.327491	5200.533527	7.609293	-0.089775	3.900274
466.634067	5208.509525	7.614298	-0.089838	3.903202
466.925543	5216.623000	7.619302	-0.089897	3.906178
466.957506	5224.659247	7.624307	-0.089908	3.909118
467.015225	5232.687384	7.629312	-0.089924	3.912053
467.253865	5240.701774	7.634317	-0.089974	3.914985
467.483409	5248.665419	7.639322	-0.090022	3.917895
467.762540	5256.742979	7.644326	-0.090080	3.920846
467.888143	5264.717339	7.649331	-0.090108	3.923754
468.268582	5272.772776	7.654336	-0.090184	3.926695
468.353877	5280.796487	7.659341	-0.090206	3.929615
468.773332	5288.797805	7.664346	-0.090289	3.932532
468.713805	5296.880589	7.669350	-0.090283	3.935468
469.118087	5304.830360	7.674355	-0.090364	3.938361
469.280748	5312.920737	7.679360	-0.090399	3.941299
469.601689	5320.864436	7.684365	-0.090464	3.944184
469.875004	5328.912216	7.689370	-0.090521	3.947104
469.879860	5336.998599	7.694374	-0.090527	3.950031
470.203636	5344.970485	7.699379	-0.090592	3.952920
470.703278	5352.981031	7.704384	-0.090691	3.955824
470.823717	5360.978528	7.709389	-0.090719	3.958715
471.075058	5369.016973	7.714394	-0.090771	3.961620
471.398533	5376.985117	7.719398	-0.090836	3.964499
471.447028	5384.998740	7.724403	-0.090850	3.967388
471.623738	5393.087403	7.729408	-0.090889	3.970303
472.097507	5401.094672	7.734413	-0.090982	3.973193
472.098418	5409.155307	7.739418	-0.090988	3.976091
472.314219	5417.153177	7.744422	-0.091033	3.978968
472.626801	5425.149654	7.749427	-0.091097	3.981844
472.926393	5433.144843	7.754432	-0.091158	3.984718
473.014221	5441.193536	7.759437	-0.091179	3.987605
473.278943	5449.196082	7.764442	-0.091234	3.990476
473.583915	5457.211325	7.769446	-0.091296	3.993351
473.692605	5465.287162	7.774451	-0.091322	3.996241
474.008301	5473.232463	7.779456	-0.091386	3.999087
474.272849	5481.284764	7.784461	-0.091440	4.001967
474.715498	5489.261170	7.789466	-0.091528	4.004822
474.994203	5497.280857	7.794470	-0.091585	4.007687
475.065135	5505.351080	7.799475	-0.091604	4.010564
475.174275	5513.418360	7.804480	-0.091629	4.013439
475.597128	5521.406873	7.809485	-0.091713	4.016289
475.672391	5529.377623	7.814490	-0.091733	4.019125
475.990017	5537.444944	7.819494	-0.091797	4.021998
476.128487	5545.426044	7.824499	-0.091828	4.024834
476.205215	5553.486909	7.829504	-0.091848	4.027696
476.429410	5561.541637	7.834509	-0.091895	4.030556
476.933824	5569.535892	7.839514	-0.091994	4.033397
476.933562	5577.602582	7.844518	-0.091999	4.036254
476.969419	5585.544541	7.849523	-0.092011	4.039065
477.546704	5593.557346	7.854528	-0.092124	4.041908
477.792294	5601.532295	7.859533	-0.092175	4.044730
477.728718	5609.589247	7.864538	-0.092169	4.047574
478.022910	5617.660156	7.869542	-0.092229	4.050426
477.894320	5625.699427	7.874547	-0.092210	4.053259
478.467441	5633.719295	7.879552	-0.092322	4.056094
478.672754	5641.659723	7.884557	-0.092366	4.058893
478.581310	5649.774629	7.889562	-0.092354	4.061747
478.722712	5657.726315	7.894566	-0.092386	4.064546
479.091311	5665.751237	7.899571	-0.092460	4.067371
479.520457	5673.798025	7.904576	-0.092545	4.070203
479.898290	5681.789569	7.909581	-0.092620	4.073013
479.814170	5689.832830	7.914586	-0.092610	4.075832
480.128668	5697.850784	7.919590	-0.092674	4.078646
480.164756	5705.891297	7.924595	-0.092686	4.081462
480.365118	5713.869032	7.929600	-0.092729	4.084257
480.447097	5721.942025	7.934605	-0.092749	4.087081
480.878486	5729.901810	7.939610	-0.092835	4.089869
481.163750	5737.978685	7.944614	-0.092893	4.092693
481.112166	5745.992551	7.949619	-0.092889	4.095489
481.635854	5753.959172	7.954624	-0.092992	4.098274
481.806075	5762.015501	7.959629	-0.093029	4.101084
481.520776	5770.022047	7.964634	-0.092981	4.103868
481.957440	5778.046569	7.969638	-0.093068	4.106667
482.112619	5786.043858	7.974643	-0.093102	4.109450
482.299141	5794.098432	7.979648	-0.093142	4.112252
482.374432	5802.106275	7.984653	-0.093161	4.115034
482.547077	5810.053699	7.989658	-0.093199	4.117794
482.478474	5818.124828	7.994662	-0.093191	4.120592
482.700896	5826.072175	7.999667	-0.093238	4.123350
483.071272	5834.173471	8.004672	-0.093312	4.126161
483.466605	5842.135127	8.009677	-0.093391	4.128921
483.531666	5850.176203	8.014682	-0.093408	4.131703
483.536556	5858.223195	8.019686	-0.093415	4.134485
483.723742	5866.222663	8.024691	-0.093455	4.137250
483.963372	5874.253661	8.029696	-0.093505	4.140025
484.126503	5882.239576	8.034701	-0.093540	4.142782
484.598682	5890.222191	8.039706	-0.093634	4.145540
484.719164	5898.297586	8.044710	-0.093661	4.148323
484.795509	5906.318383	8.049715	-0.093681	4.151085
485.392651	5914.286599	8.054720	-0.093797	4.153834
485.259239	5922.371237	8.059725	-0.093778	4.156611
485.439556	5930.327236	8.064730	-0.093817	4.159347
485.512074	5938.453418	8.069734	-0.093836	4.162138
485.813303	5946.370327	8.074739	-0.093897	4.164857
486.153213	5954.433273	8.079744	-0.093966	4.167626
486.233251	5962.491725	8.084749	-0.093986	4.170388
486.328784	5970.434623	8.089754	-0.094009	4.173109
486.872265	5978.539674	8.094758	-0.094115	4.175889
487.049842	5986.545194	8.099763	-0.094154	4.178628
487.218522	5994.607533	8.104768	-0.094190	4.181385
487.391289	6002.535210	8.109773	-0.094228	4.184095
487.427473	6010.608183	8.114778	-0.094240	4.186850
487.708693	6018.627852	8.119782	-0.094298	4.189588
487.775000	6026.657362	8.124787	-0.094315	4.192326
487.865724	6034.731686	8.129792	-0.094338	4.195077
488.281302	6042.687710	8.134797	-0.094420	4.197790
488.567411	6050.702912	8.139802	-0.094479	4.200519
488.690449	6058.661737	8.144806	-0.094507	4.203226
488.650907	6066.708277	8.149811	-0.094505	4.205959
488.973091	6074.730835	8.154816	-0.094570	4.208686
489.201382	6082.782935	8.159821	-0.094618	4.211420
489.218585	6090.755018	8.164826	-0.094626	4.214123
489.296616	6098.863027	8.169830	-0.094646	4.216871
489.233736	6106.811114	8.174835	-0.094640	4.219562
489.546265	6114.822591	8.179840	-0.094703	4.222276
489.445570	6122.855969	8.184845	-0.094690	4.224992
489.687041	6130.855205	8.189850	-0.094740	4.227697
490.033692	6138.908211	8.194854	-0.094810	4.230421
490.067366	6146.890101	8.199859	-0.094822	4.233115
490.473332	6154.927787	8.204864	-0.094903	4.235830
490.499209	6162.891516	8.209869	-0.094913	4.238515
490.662222	6170.985981	8.214874	-0.094948	4.241243
490.826811	6178.929832	8.219878	-0.094984	4.243919
490.932357	6186.990990	8.224883	-0.095009	4.246632
491.364557	6194.973408	8.229888	-0.095095	4.249320
491.375619	6203.053341	8.234893	-0.095102	4.252035
491.195746	6211.028678	8.239898	-0.095074	4.254711
491.546216	6219.113693	8.244902	-0.095145	4.257428
491.731306	6227.023450	8.249907	-0.095185	4.260082
492.198587	6235.028018	8.254912	-0.095277	4.262769
492.456108	6243.067089	8.259917	-0.095330	4.265464
492.270260	6251.163017	8.264922	-0.095301	4.268172
492.264226	6259.246859	8.269926	-0.095305	4.270876
492.644788	6267.162548	8.274931	-0.095381	4.273526
493.284052	6275.177147	8.279936	-0.095505	4.276209
493.548190	6283.152118	8.284941	-0.095560	4.278874
493.476288	6291.207757	8.289946	-0.095552	4.281561
493.811457	6299.173167	8.294950	-0.095620	4.284220
494.131372	6307.155324	8.299955	-0.095684	4.286883
494.532531	6315.204193	8.304960	-0.095764	4.289567
494.633070	6323.258694	8.309965	-0.095788	4.292248
494.988053	6331.296599	8.314970	-0.095860	4.294925
495.080042	6339.323952	8.319974	-0.095882	4.297594
495.037051	6347.353239	8.324979	-0.095880	4.300261
495.209657	6355.341533	8.329984	-0.095917	4.302914
495.609592	6363.380836	8.334989	-0.095997	4.305585
495.826732	6371.340425	8.339994	-0.096043	4.308225
496.544250	6379.407470	8.344998	-0.096182	4.310904
496.642408	6387.349015	8.350003	-0.096205	4.313535
496.669589	6395.464231	8.355008	-0.096215	4.316221
496.860997	6403.395437	8.360013	-0.096256	4.318846
497.140813	6411.456965	8.365018	-0.096314	4.321512
497.530783	6419.379134	8.370022	-0.096392	4.324132
497.190199	6427.507203	8.375027	-0.096334	4.326813
497.492313	6435.455556	8.380032	-0.096395	4.329438
497.812354	6443.551465	8.385037	-0.096460	4.332109
498.065299	6451.475889	8.390042	-0.096512	4.334723
498.623848	6459.542311	8.395046	-0.096622	4.337383
498.670815	6467.573417	8.400051	-0.096636	4.340026
498.649049	6475.586315	8.405056	-0.096637	4.342662
499.065542	6483.610389	8.410061	-0.096720	4.345302
499.206294	6491.598125	8.415066	-0.096751	4.347927
499.205677	6499.721340	8.420070	-0.096757	4.350594
499.477166	6507.661794	8.425075	-0.096812	4.353201
499.907500	6515.728451	8.430080	-0.096898	4.355849
499.935328	6523.688763	8.435085	-0.096908	4.358458
499.994563	6531.702781	8.440090	-0.096925	4.361083
500.729809	6539.630118	8.445094	-0.097067	4.363683
500.723016	6547.691601	8.450099	-0.097071	4.366320
500.780206	6555.750906	8.455104	-0.097087	4.368955
500.877028	6563.804736	8.460109	-0.097110	4.371586
501.140473	6571.752958	8.465114	-0.097165	4.374183
501.197294	6579.872871	8.470118	-0.097181	4.376833
501.401180	6587.787000	8.475123	-0.097224	4.379416
501.591271	6595.899719	8.480128	-0.097265	4.382061
501.815995	6603.893064	8.485133	-0.097312	4.384666
502.042836	6611.865318	8.490138	-0.097359	4.387262
502.226280	6619.945937	8.495142	-0.097399	4.389892
502.494982	6627.949185	8.500147	-0.097454	4.392496
502.483443	6635.944289	8.505152	-0.097457	4.395094
502.838798	6643.995984	8.510157	-0.097529	4.397711
502.808168	6651.966370	8.515162	-0.097528	4.400297
503.310236	6659.972209	8.520166	-0.097627	4.402897
503.325608	6668.033154	8.525171	-0.097635	4.405510
503.509686	6676.052525	8.530176	-0.097675	4.408109
503.638840	6684.120115	8.535181	-0.097704	4.410722
503.610114	6692.130628	8.540186	-0.097704	4.413314
503.839729	6700.223493	8.545190	-0.097752	4.415932
504.150863	6708.154647	8.550195	-0.097815	4.418497
504.400023	6716.217269	8.555200	-0.097867	4.421103
504.450259	6724.212597	8.560205	-0.097882	4.423684
504.543779	6732.251600	8.565210	-0.097904	4.426278
504.835970	6740.280525	8.570215	-0.097964	4.428869
504.849367	6748.307106	8.575219	-0.097972	4.431455
505.372259	6756.261489	8.580224	-0.098075	4.434020
505.352959	6764.348499	8.585229	-0.098076	4.436622
505.337132	6772.236331	8.590234	-0.098079	4.439160
505.548398	6780.332125	8.595239	-0.098123	4.441764
505.965316	6788.294570	8.600243	-0.098206	4.444324
506.053653	6796.347373	8.605248	-0.098228	4.446910
506.096112	6804.349138	8.610253	-0.098241	4.449478
506.387177	6812.415250	8.615258	-0.098301	4.452067
506.484992	6820.424633	8.620263	-0.098324	4.454635
506.488189	6828.431241	8.625267	-0.098330	4.457200
506.700922	6836.407379	8.630272	-0.098375	4.459754
506.892782	6844.448977	8.635277	-0.098416	4.462328
506.903882	6852.443052	8.640282	-0.098423	4.464885
507.072882	6860.518767	8.645287	-0.098460	4.467467
507.062993	6868.521403	8.650291	-0.098464	4.470023
507.087756	6876.534047	8.655296	-0.098474	4.472581
507.312487	6884.525270	8.660301	-0.098521	4.475132
507.568342	6892.531532	8.665306	-0.098574	4.477686
507.566506	6900.583858	8.670311	-0.098579	4.480252
507.589157	6908.556195	8.675315	-0.098588	4.482792
507.709058	6916.587827	8.680320	-0.098616	4.485349
508.113408	6924.593286	8.685325	-0.098696	4.487898
508.424832	6932.621229	8.690330	-0.098760	4.490451
508.393346	6940.671512	8.695335	-0.098759	4.493010
508.339098	6948.683367	8.700339	-0.098754	4.495554
508.550372	6956.687010	8.705344	-0.098799	4.498095
508.451785	6964.732064	8.710349	-0.098786	4.500647
508.769406	6972.651196	8.715354	-0.098850	4.503159
509.025602	6980.709545	8.720359	-0.098903	4.505714
509.162762	6988.720537	8.725363	-0.098934	4.508251
509.317928	6996.766511	8.730368	-0.098968	4.510798
509.744257	7004.779907	8.735373	-0.099053	4.513335
509.680496	7012.770075	8.740378	-0.099047	4.515861
509.692944	7020.753115	8.745383	-0.099054	4.518383
509.880218	7028.772647	8.750387	-0.099094	4.520917
510.052425	7036.755339	8.755392	-0.099132	4.523437
510.140667	7044.850212	8.760397	-0.099153	4.525990
510.426087	7052.777636	8.765402	-0.099212	4.528491
510.475058	7060.894895	8.770407	-0.099226	4.531048
510.520192	7068.880945	8.775411	-0.099240	4.533563
510.458929	7076.950689	8.780416	-0.099234	4.536103
510.645310	7084.895936	8.785421	-0.099274	4.538603
511.059360	7092.914436	8.790426	-0.099356	4.541125
511.032474	7100.937851	8.795431	-0.099357	4.543646
511.398551	7108.935041	8.800435	-0.099430	4.546158
511.478512	7116.970654	8.805440	-0.099450	4.548681
511.453205	7125.097102	8.810445	-0.099451	4.551230
511.409037	7132.998132	8.815450	-0.099448	4.553707
512.158212	7141.017945	8.820455	-0.099593	4.556221
512.181757	7149.019097	8.825459	-0.099602	4.558727
512.414819	7157.070297	8.830464	-0.099651	4.561247
512.597745	7164.999558	8.835469	-0.099690	4.563728
512.816744	7173.086833	8.840474	-0.099737	4.566257
513.038703	7181.076729	8.845479	-0.099783	4.568754
512.939200	7189.158779	8.850483	-0.099770	4.571278
513.369335	7197.102509	8.855488	-0.099855	4.573758
513.588791	7205.178889	8.860493	-0.099902	4.576277
513.554876	7213.114762	8.865498	-0.099900	4.578752
513.815519	7221.250029	8.870503	-0.099954	4.581287
513.711470	7229.148814	8.875507	-0.099940	4.583747
513.884722	7237.237283	8.880512	-0.099978	4.586265
514.301853	7245.213884	8.885517	-0.100061	4.588747
514.488616	7253.289234	8.890522	-0.100101	4.591258
514.600284	7261.277900	8.895527	-0.100127	4.593740
514.794864	7269.290775	8.900531	-0.100169	4.596229
515.118880	7277.224175	8.905536	-0.100234	4.598692
515.358751	7285.306148	8.910541	-0.100284	4.601200
515.574505	7293.227527	8.915546	-0.100330	4.603656
515.735927	7301.312580	8.920551	-0.100365	4.606162
515.863845	7309.284221	8.925555	-0.100394	4.608631
515.781031	7317.388760	8.930560	-0.100384	4.611140
516.085217	7325.373800	8.935565	-0.100446	4.613611
516.154295	7333.405062	8.940570	-0.100464	4.616094
516.450367	7341.402948	8.945575	-0.100525	4.618566
516.426379	7349.421850	8.950579	-0.100525	4.621043
516.769574	7357.354604	8.955584	-0.100595	4.623492
516.882915	7365.479158	8.960589	-0.100621	4.625999
517.013875	7373.450190	8.965594	-0.100651	4.628458
517.272015	7381.536894	8.970599	-0.100704	4.630950
517.432860	7389.502402	8.975603	-0.100739	4.633404
517.502310	7397.547272	8.980608	-0.100758	4.635881
517.639997	7405.452382	8.985613	-0.100788	4.638314
517.847043	7413.541430	8.990618	-0.100832	4.640802
518.035353	7421.519091	8.995623	-0.100873	4.643254
518.091479	7429.583301	9.000627	-0.100888	4.645732
518.323118	7437.591985	9.005632	-0.100937	4.648191
518.432010	7445.670007	9.010637	-0.100962	4.650670
518.481380	7453.598593	9.015642	-0.100977	4.653102
518.681265	7461.697593	9.020647	-0.101020	4.655585
518.890987	7469.620631	9.025651	-0.101064	4.658013
518.577556	7477.730504	9.030656	-0.101011	4.660497
518.941026	7485.693910	9.035661	-0.101084	4.662934
519.098677	7493.733661	9.040666	-0.101118	4.665394
519.473021	7501.763937	9.045671	-0.101193	4.667849
519.719587	7509.714476	9.050675	-0.101245	4.670278
520.042373	7517.774775	9.055680	-0.101310	4.672740
520.054886	7525.784328	9.060685	-0.101318	4.675185
520.194874	7533.765736	9.065690	-0.101349	4.677620
520.576824	7541.808495	9.070695	-0.101425	4.680073
520.539759	7549.776281	9.075699	-0.101424	4.682501
520.337901	7557.820364	9.080704	-0.101392	4.684952
520.819864	7565.822042	9.085709	-0.101487	4.687388
521.046266	7573.784952	9.090714	-0.101534	4.689811
521.161881	7581.933325	9.095719	-0.101561	4.692289
521.075584	7589.895106	9.100723	-0.101550	4.694709
521.380901	7597.961481	9.105728	-0.101612	4.697160
521.444706	7605.927150	9.110733	-0.101629	4.699579
521.277172	7613.985287	9.115738	-0.101604	4.702025
521.839603	7621.885695	9.120743	-0.101714	4.704421
522.097559	7629.980250	9.125747	-0.101767	4.706875
522.240412	7637.936279	9.130752	-0.101799	4.709285
522.450879	7646.065930	9.135757	-0.101843	4.711747
522.423887	7653.984951	9.140762	-0.101844	4.714145
522.635905	7662.105593	9.145767	-0.101888	4.716602
522.541553	7670.003468	9.150771	-0.101876	4.718990
522.943104	7678.104916	9.155776	-0.101956	4.721438
523.142529	7686.065665	9.160781	-0.101999	4.723843
523.052484	7694.170200	9.165786	-0.101987	4.726290
523.283970	7702.147757	9.170791	-0.102036	4.728697
523.556376	7710.185687	9.175795	-0.102092	4.731121
523.780172	7718.174653	9.180800	-0.102139	4.733529
523.972257	7726.256661	9.185805	-0.102180	4.735964
524.212919	7734.172213	9.190810	-0.102230	4.738347
524.398351	7742.268796	9.195815	-0.102270	4.740784
523.936719	7750.295669	9.200819	-0.102189	4.743200
524.225337	7758.237389	9.205824	-0.102248	4.745587
524.595598	7766.311745	9.210829	-0.102322	4.748013
524.593520	7774.313220	9.215834	-0.102327	4.750417
524.739783	7782.373164	9.220839	-0.102360	4.752836
524.510155	7790.372351	9.225843	-0.102322	4.755238
524.845170	7798.351765	9.230848	-0.102390	4.757630
524.991801	7806.381405	9.235853	-0.102423	4.760037
525.407629	7814.295924	9.240858	-0.102505	4.762407
525.541524	7822.326383	9.245863	-0.102535	4.764812
525.511198	7830.419765	9.250867	-0.102535	4.767234
525.701774	7838.408952	9.255872	-0.102576	4.769624
526.032114	7846.466392	9.260877	-0.102643	4.772032
526.157743	7854.403545	9.265882	-0.102671	4.774404
526.180949	7862.486776	9.270887	-0.102681	4.776818
526.528031	7870.461694	9.275891	-0.102751	4.779198
526.440325	7878.526749	9.280896	-0.102740	4.781605
526.436445	7886.474330	9.285901	-0.102745	4.783976
526.786229	7894.530641	9.290906	-0.102815	4.786376
527.272610	7902.542492	9.295911	-0.102911	4.788762
527.118983	7910.578953	9.300915	-0.102888	4.791156
527.463253	7918.549035	9.305920	-0.102957	4.793527
527.593455	7926.631740	9.310925	-0.102987	4.795931
527.914989	7934.525704	9.315930	-0.103052	4.798277
528.074177	7942.665288	9.320935	-0.103087	4.800696
528.121126	7950.566828	9.325939	-0.103101	4.803043
528.383839	7958.664481	9.330944	-0.103155	4.805447
528.656431	7966.679096	9.335949	-0.103211	4.807824
528.704400	7974.648348	9.340954	-0.103225	4.810188
528.847892	7982.736648	9.345959	-0.103257	4.812585
528.613132	7990.166068	9.350963	-0.103218	4.814788
528.953819	7994.923171	9.355968	-0.103285	4.816195

529.339028	7997.498841	9.360973	-0.103359	4.816956
529.286610	7998.924586	9.365978	-0.103350	4.817379
529.473283	7999.405988	9.370983	-0.103385	4.817521
529.346640	8000.211849	9.375987	-0.103362	4.817760
529.510278	8000.238483	9.380992	-0.103393	4.817767
529.900491	8000.216740	9.385997	-0.103465	4.817759
529.751998	8000.214590	9.391002	-0.103438	4.817759
529.955767	8000.257625	9.396007	-0.103476	4.817771
529.989727	8000.238089	9.401011	-0.103482	4.817765
529.929369	8000.249872	9.406016	-0.103471	4.817768
530.057845	8000.247527	9.411021	-0.103495	4.817767
530.247294	8000.265047	9.416026	-0.103530	4.817772
530.321411	8000.254531	9.421031	-0.103544	4.817768
530.357307	8000.250841	9.426035	-0.103551	4.817767
530.209769	8000.275066	9.431040	-0.103524	4.817775
530.308926	8000.236442	9.436045	-0.103542	4.817763
530.308001	8000.258579	9.441050	-0.103542	4.817769
530.493472	8000.274988	9.446055	-0.103577	4.817773
530.266706	8000.270645	9.451059	-0.103535	4.817773
530.263334	8000.288529	9.456064	-0.103534	4.817778
530.647267	8000.264587	9.461069	-0.103606	4.817770
530.654360	8000.241497	9.466074	-0.103607	4.817763
530.787341	8000.284561	9.471079	-0.103632	4.817775
530.783528	8000.248659	9.476083	-0.103631	4.817764
531.026678	8000.282778	9.481088	-0.103677	4.817773
530.838901	8000.276893	9.486093	-0.103642	4.817773
530.880437	8000.278557	9.491098	-0.103649	4.817773
531.027147	8000.291240	9.496103	-0.103677	4.817776
530.769434	8000.266411	9.501107	-0.103629	4.817770
530.873239	8000.321705	9.506112	-0.103648	4.817786
531.141316	8000.269719	9.511117	-0.103698	4.817769
531.154395	8000.258315	9.516122	-0.103701	4.817766
531.463669	8000.292343	9.521127	-0.103759	4.817774
531.318857	8000.256500	9.526131	-0.103732	4.817764
531.384455	8000.284877	9.531136	-0.103744	4.817773
531.451835	8000.267936	9.536141	-0.103757	4.817767
531.358329	8000.259201	9.541146	-0.103739	4.817765
531.618375	8000.271423	9.546151	-0.103788	4.817768
531.536125	8000.250198	9.551155	-0.103772	4.817762
531.518278	8000.286853	9.556160	-0.103769	4.817773
531.525986	8000.282753	9.561165	-0.103771	4.817771
531.558574	8000.281124	9.566170	-0.103777	4.817771
531.716759	8000.308738	9.571175	-0.103806	4.817778
531.575630	8000.268730	9.576179	-0.103780	4.817767
531.682750	8000.319856	9.581184	-0.103800	4.817782
531.579737	8000.287783	9.586189	-0.103781	4.817773
531.339105	8000.277965	9.591194	-0.103736	4.817771
531.470236	8000.295695	9.596199	-0.103761	4.817775
531.562182	8000.281220	9.601203	-0.103778	4.817771
531.325389	8000.342109	9.606208	-0.103734	4.817790
531.632329	8000.309669	9.611213	-0.103791	4.817779
531.515722	8000.314308	9.616218	-0.103770	4.817781
531.541073	8000.344209	9.621223	-0.103775	4.817789
531.273772	8000.319239	9.626227	-0.103725	4.817783
531.590586	8000.310142	9.631232	-0.103784	4.817779
531.524290	8000.356638	9.636237	-0.103772	4.817793
531.150833	8000.376524	9.641242	-0.103702	4.817801
530.908812	8000.434173	9.646247	-0.103657	4.817819
531.155631	8000.423004	9.651251	-0.103703	4.817814
531.279325	8000.364701	9.656256	-0.103726	4.817797
531.553343	8000.337055	9.661261	-0.103778	4.817787
531.529197	8000.362019	9.666266	-0.103773	4.817795
531.562583	8000.386764	9.671271	-0.103779	4.817802
531.550445	8000.379212	9.676275	-0.103777	4.817800
531.398783	8000.399159	9.681280	-0.103749	4.817806
532.001797	8000.342551	9.686285	-0.103861	4.817787
531.843076	8000.343414	9.691290	-0.103832	4.817788
532.209730	8000.316060	9.696295	-0.103900	4.817778
532.135325	8000.299167	9.701299	-0.103886	4.817773
532.154351	8000.309995	9.706304	-0.103890	4.817777
531.996067	8000.305591	9.711309	-0.103861	4.817776
532.174636	8000.302921	9.716314	-0.103894	4.817774
532.095880	8000.316545	9.721319	-0.103879	4.817779
531.976734	8000.297947	9.726323	-0.103857	4.817774
532.062959	8000.316079	9.731328	-0.103873	4.817779
532.379395	8000.310141	9.736333	-0.103932	4.817776
532.291748	8000.274073	9.741338	-0.103916	4.817765
532.434968	8000.310962	9.746343	-0.103943	4.817776
532.370547	8000.285777	9.751347	-0.103931	4.817768
532.263834	8000.352776	9.756352	-0.103911	4.817789
531.882244	8000.421051	9.761357	-0.103840	4.817811
532.100816	8000.366236	9.766362	-0.103881	4.817793
532.391725	8000.363091	9.771367	-0.103935	4.817791
532.468742	8000.347344	9.776371	-0.103950	4.817786
532.305831	8000.377672	9.781376	-0.103920	4.817796
532.474703	8000.375916	9.786381	-0.103951	4.817795
532.361158	8000.328926	9.791386	-0.103930	4.817781
532.132902	8000.390994	9.796391	-0.103888	4.817801
532.582352	8000.316337	9.801395	-0.103971	4.817777
532.793459	8000.358432	9.806400	-0.104011	4.817788
532.598563	8000.350331	9.811405	-0.103975	4.817787
532.573583	8000.299356	9.816410	-0.103970	4.817772
532.709855	8000.315053	9.821415	-0.103995	4.817776
532.515176	8000.304846	9.826419	-0.103959	4.817773
532.693690	8000.332757	9.831424	-0.103993	4.817781
532.818344	8000.299777	9.836429	-0.104016	4.817771
532.458241	8000.336727	9.841434	-0.103949	4.817783
532.513181	8000.371278	9.846439	-0.103959	4.817793
532.441015	8000.388162	9.851443	-0.103946	4.817798
532.631543	8000.351921	9.856448	-0.103981	4.817787
532.600705	8000.357806	9.861453	-0.103976	4.817789
532.432364	8000.322673	9.866458	-0.103944	4.817779
532.893610	8000.350479	9.871463	-0.104030	4.817785
532.576097	8000.315285	9.876467	-0.103971	4.817776
532.688892	8000.316932	9.881472	-0.103992	4.817776
532.631030	8000.319260	9.886477	-0.103982	4.817777
532.750540	8000.333659	9.891482	-0.104004	4.817781
532.693176	8000.358140	9.896487	-0.103994	4.817788
532.224552	8000.427257	9.901491	-0.103906	4.817811
532.179112	8000.458239	9.906496	-0.103898	4.817820
532.370380	8000.419900	9.911501	-0.103934	4.817808
532.235451	8000.374707	9.916506	-0.103909	4.817795
532.777106	8000.363610	9.921511	-0.104010	4.817790
533.027590	8000.308205	9.926515	-0.104056	4.817772
532.545876	8000.389786	9.931520	-0.103967	4.817798
532.472371	8000.429851	9.936525	-0.103953	4.817811
532.332368	8000.382475	9.941530	-0.103927	4.817797
532.630458	8000.378381	9.946535	-0.103983	4.817795
532.820304	8000.327366	9.951539	-0.104018	4.817779
532.835754	8000.371888	9.956544	-0.104021	4.817792
532.825065	8000.384394	9.961549	-0.104019	4.817796
532.796721	8000.351297	9.966554	-0.104014	4.817786
533.136031	8000.366784	9.971559	-0.104077	4.817789
533.101092	8000.316718	9.976563	-0.104071	4.817774
532.781708	8000.366915	9.981568	-0.104011	4.817791
532.685409	8000.347593	9.986573	-0.103993	4.817785
532.777969	8000.337346	9.991578	-0.104011	4.817782
532.885691	8000.366337	9.996583	-0.104031	4.817790
532.903800	8000.294897	10.001587	-0.104034	4.817769
532.986242	8000.316139	10.006592	-0.104050	4.817775
532.981927	8000.334010	10.011597	-0.104049	4.817780
533.050979	8000.303384	10.016602	-0.104062	4.817771
533.157195	8000.298608	10.021607	-0.104082	4.817769
533.194113	8000.287551	10.026611	-0.104089	4.817765
533.123750	8000.358244	10.031616	-0.104076	4.817787
533.020381	8000.308237	10.036621	-0.104057	4.817772
532.884395	8000.310483	10.041626	-0.104031	4.817773
532.793055	8000.356615	10.046631	-0.104014	4.817788
532.985895	8000.318299	10.051635	-0.104050	4.817775
532.914742	8000.360507	10.056640	-0.104037	4.817788
532.593304	8000.443365	10.061645	-0.103978	4.817814
532.205866	8000.400827	10.066650	-0.103906	4.817803
532.550341	8000.407953	10.071655	-0.103970	4.817804
532.574308	8000.444162	10.076659	-0.103974	4.817814
532.910237	8000.422691	10.081664	-0.104037	4.817807
533.309139	8000.373664	10.086669	-0.104111	4.817790
533.131965	8000.332074	10.091674	-0.104078	4.817779
533.181358	8000.349672	10.096679	-0.104088	4.817784
532.964757	8000.360236	10.101683	-0.104047	4.817788
533.232487	8000.332501	10.106688	-0.104097	4.817778
533.301465	8000.293437	10.111693	-0.104110	4.817767
533.288113	8000.333322	10.116698	-0.104108	4.817778
533.356940	8000.367021	10.121703	-0.104121	4.817788
533.465561	8000.333807	10.126707	-0.104141	4.817778
533.418847	8000.324697	10.131712	-0.104132	4.817775
533.011710	8000.386272	10.136717	-0.104057	4.817795
532.933320	8000.385138	10.141722	-0.104042	4.817795
533.188963	8000.427882	10.146727	-0.104090	4.817807
533.239979	8000.370630	10.151731	-0.104099	4.817790
533.510418	8000.392498	10.156736	-0.104150	4.817795
533.536670	8000.389723	10.161741	-0.104155	4.817794
533.152031	8000.415769	10.166746	-0.104083	4.817803
533.438681	8000.402019	10.171751	-0.104137	4.817798
533.147331	8000.391459	10.176755	-0.104083	4.817796
533.395130	8000.369761	10.181760	-0.104129	4.817789
533.492002	8000.384886	10.186765	-0.104147	4.817793
533.632554	8000.345809	10.191770	-0.104173	4.817781
533.620629	8000.412080	10.196775	-0.104171	4.817800
533.599293	8000.352720	10.201779	-0.104167	4.817783
533.463174	8000.392928	10.206784	-0.104142	4.817795
533.627605	8000.402709	10.211789	-0.104173	4.817798
533.689127	8000.367755	10.216794	-0.104184	4.817787
533.826926	8000.366603	10.221799	-0.104210	4.817786
533.936681	8000.338678	10.226803	-0.104230	4.817777
533.964175	8000.325375	10.231808	-0.104235	4.817773
533.634901	8000.341681	10.236813	-0.104174	4.817779
533.641113	8000.345996	10.241818	-0.104175	4.817781
533.804338	8000.355759	10.246823	-0.104206	4.817783
533.715322	8000.321779	10.251827	-0.104189	4.817773
533.614256	8000.317150	10.256832	-0.104171	4.817772
533.669503	8000.368580	10.261837	-0.104181	4.817787
533.837819	8000.316198	10.266842	-0.104213	4.817771
533.723515	8000.351451	10.271847	-0.104191	4.817782
533.614557	8000.356199	10.276851	-0.104171	4.817784
533.124214	8000.402853	10.281856	-0.104080	4.817800
533.359044	8000.493805	10.286861	-0.104124	4.817826
533.696329	8000.354244	10.291866	-0.104187	4.817783
534.165372	8000.400096	10.296871	-0.104274	4.817794
533.959381	8000.328556	10.301875	-0.104236	4.817774
534.104111	8000.338051	10.306880	-0.104263	4.817776
534.073217	8000.344989	10.311885	-0.104257	4.817778
533.954341	8000.339047	10.316890	-0.104235	4.817777
533.693069	8000.387980	10.321895	-0.104186	4.817793
533.974361	8000.347788	10.326899	-0.104239	4.817780
533.885458	8000.341227	10.331904	-0.104222	4.817778
533.589516	8000.385437	10.336909	-0.104167	4.817793
533.711729	8000.331329	10.341914	-0.104190	4.817776
533.851845	8000.356575	10.346919	-0.104216	4.817783
534.148841	8000.320830	10.351923	-0.104272	4.817771
533.870550	8000.322059	10.356928	-0.104220	4.817773
534.160938	8000.317855	10.361933	-0.104274	4.817770
533.854138	8000.335542	10.366938	-0.104217	4.817777
533.855299	8000.375639	10.371943	-0.104217	4.817788
534.057850	8000.317428	10.376947	-0.104255	4.817770
534.064231	8000.348110	10.381952	-0.104257	4.817779
533.895689	8000.400501	10.386957	-0.104225	4.817796
533.902950	8000.359484	10.391962	-0.104227	4.817783
534.019558	8000.424462	10.396967	-0.104248	4.817802
533.950173	8000.350693	10.401971	-0.104236	4.817781
534.053468	8000.312128	10.406976	-0.104255	4.817769
533.906173	8000.386975	10.411981	-0.104228	4.817792
533.895096	8000.345692	10.416986	-0.104226	4.817779
533.920334	8000.348174	10.421991	-0.104230	4.817780
534.107513	8000.340359	10.426995	-0.104265	4.817777
534.254305	8000.344611	10.432000	-0.104293	4.817778
533.956924	8000.425710	10.437005	-0.104237	4.817803
533.901432	8000.379561	10.442010	-0.104227	4.817789
533.879266	8000.422483	10.447015	-0.104223	4.817802
533.580439	8000.407594	10.452019	-0.104168	4.817799
533.748741	8000.463833	10.457024	-0.104199	4.817815
533.935177	8000.459171	10.462029	-0.104234	4.817813
533.534891	8000.494479	10.467034	-0.104159	4.817825
533.949754	8000.436195	10.472039	-0.104237	4.817806
533.769581	8000.443070	10.477043	-0.104203	4.817809
533.675620	8000.459636	10.482048	-0.104186	4.817814
533.201847	8000.308273	10.487053	-0.104098	4.817771
533.337966	8000.412552	10.492058	-0.104123	4.817802
533.594918	8000.290804	10.497063	-0.104171	4.817764
533.357826	8000.497219	10.502067	-0.104127	4.817827
533.299850	8000.397252	10.507072	-0.104116	4.817797
534.113232	8000.416478	10.512077	-0.104268	4.817799
533.754636	8000.427083	10.517082	-0.104201	4.817804
533.860642	8000.497180	10.522087	-0.104221	4.817824
533.938189	8000.435040	10.527091	-0.104235	4.817806
533.927862	8000.433842	10.532096	-0.104234	4.817805
533.964418	8000.451253	10.537101	-0.104240	4.817810
533.938099	8000.423457	10.542106	-0.104236	4.817802
534.294741	8000.457129	10.547111	-0.104302	4.817811
534.365104	8000.426522	10.552115	-0.104315	4.817801
534.303961	8000.318070	10.557120	-0.104304	4.817769
534.218004	8000.398028	10.562125	-0.104288	4.817793
534.037586	8000.355334	10.567130	-0.104255	4.817782
534.257630	8000.374362	10.572135	-0.104296	4.817786
533.668999	8000.478641	10.577139	-0.104186	4.817820
533.790406	8000.415030	10.582144	-0.104209	4.817800
533.613009	8000.392418	10.587149	-0.104176	4.817794
533.750526	8000.367006	10.592154	-0.104201	4.817786
533.994325	8000.440163	10.597159	-0.104247	4.817807
534.309355	8000.386753	10.602163	-0.104306	4.817790
533.601338	8000.438674	10.607168	-0.104174	4.817808
533.500617	8000.440378	10.612173	-0.104155	4.817809
534.073099	8000.439225	10.617178	-0.104262	4.817806
534.134236	8000.394774	10.622183	-0.104273	4.817793
533.996405	8000.400156	10.627187	-0.104248	4.817795
534.079476	8000.346533	10.632192	-0.104263	4.817779
534.062438	8000.481279	10.637197	-0.104260	4.817819
533.720105	8000.456265	10.642202	-0.104197	4.817813
533.571442	8000.277994	10.647207	-0.104169	4.817761
534.245335	8000.329990	10.652211	-0.104295	4.817773
534.028318	8000.414368	10.657216	-0.104254	4.817799
534.024288	8000.440680	10.662221	-0.104254	4.817807
534.358302	8000.367509	10.667226	-0.104316	4.817784
534.494957	8000.393760	10.672231	-0.104341	4.817791
534.213562	8000.368578	10.677235	-0.104289	4.817785
534.132905	8000.386393	10.682240	-0.104274	4.817790
534.179297	8000.422930	10.687245	-0.104283	4.817801
534.098091	8000.388008	10.692250	-0.104268	4.817791
533.979865	8000.435859	10.697255	-0.104246	4.817806
534.223043	8000.446787	10.702259	-0.104291	4.817808
533.990943	8000.409668	10.707264	-0.104248	4.817798
534.114794	8000.426241	10.712269	-0.104271	4.817802
534.168459	8000.331061	10.717274	-0.104281	4.817774
534.193739	8000.441112	10.722279	-0.104286	4.817806
534.246302	8000.391263	10.727283	-0.104296	4.817791
534.107851	8000.409291	10.732288	-0.104270	4.817797
534.736947	8000.400528	10.737293	-0.104387	4.817792
534.318253	8000.365965	10.742298	-0.104310	4.817783
534.479581	8000.378865	10.747303	-0.104340	4.817787
534.545627	8000.384052	10.752307	-0.104352	4.817788
534.480845	8000.402097	10.757312	-0.104340	4.817793
534.676371	8000.404950	10.762317	-0.104377	4.817793
534.626679	8000.348339	10.767322	-0.104367	4.817777
534.399296	8000.445222	10.772327	-0.104325	4.817807
534.334285	8000.364133	10.777331	-0.104313	4.817783
534.830559	8000.339726	10.782336	-0.104406	4.817773
535.133397	8000.386326	10.787341	-0.104462	4.817786
534.883524	8000.352110	10.792346	-0.104416	4.817777
534.906196	8000.384085	10.797351	-0.104420	4.817786
534.801649	8000.370968	10.802355	-0.104401	4.817783
534.819533	8000.363852	10.807360	-0.104404	4.817781
534.958177	8000.360604	10.812365	-0.104430	4.817779
534.896614	8000.372369	10.817370	-0.104418	4.817783
534.772097	8000.421183	10.822375	-0.104395	4.817798
534.497886	8000.439343	10.827379	-0.104344	4.817804
534.869414	8000.366719	10.832384	-0.104414	4.817781
534.806472	8000.428030	10.837389	-0.104402	4.817800
534.486550	8000.422324	10.842394	-0.104343	4.817799
534.665957	8000.434433	10.847399	-0.104376	4.817802
534.550265	8000.402172	10.852403	-0.104355	4.817793
534.636226	8000.376010	10.857408	-0.104371	4.817785
534.855306	8000.370769	10.862413	-0.104411	4.817783
534.951181	8000.341588	10.867418	-0.104429	4.817773
535.158481	8000.363596	10.872423	-0.104468	4.817779
535.067603	8000.352787	10.877427	-0.104451	4.817776
535.153004	8000.366692	10.882432	-0.104467	4.817780
535.299506	8000.394143	10.887437	-0.104495	4.817788
535.069313	8000.335957	10.892442	-0.104452	4.817771
534.899392	8000.377782	10.897447	-0.104420	4.817784
534.892320	8000.419870	10.902451	-0.104419	4.817797
534.773248	8000.380177	10.907456	-0.104397	4.817786
534.683810	8000.362007	10.912461	-0.104380	4.817781
535.035552	8000.373462	10.917466	-0.104446	4.817783
535.060973	8000.443443	10.922471	-0.104451	4.817803
534.717630	8000.437395	10.927475	-0.104387	4.817803
534.610696	8000.417916	10.932480	-0.104367	4.817798
534.773825	8000.440335	10.937485	-0.104398	4.817803
534.566005	8000.412004	10.942490	-0.104359	4.817796
534.658001	8000.428114	10.947495	-0.104376	4.817800
534.352089	8000.401520	10.952499	-0.104319	4.817794
534.433146	8000.489183	10.957504	-0.104334	4.817819
534.181788	8000.175483	10.962509	-0.104288	4.817728
534.531421	8000.445279	10.967514	-0.104353	4.817806
534.723705	8000.491324	10.972519	-0.104389	4.817819
534.773661	8000.407689	10.977523	-0.104398	4.817794
534.714779	8000.386801	10.982528	-0.104387	4.817788
534.326671	8000.326318	10.987533	-0.104315	4.817772
533.977358	8000.454117	10.992538	-0.104250	4.817811
534.633163	8000.419378	10.997543	-0.104372	4.817798
534.869415	8000.373258	11.002547	-0.104416	4.817783
535.044799	8000.382146	11.007552	-0.104449	4.817785
534.803710	8000.442972	11.012557	-0.104404	4.817804
534.796801	8000.378547	11.017562	-0.104403	4.817785
535.085171	8000.412282	11.022567	-0.104457	4.817794
534.832997	8000.331630	11.027571	-0.104410	4.817771
534.971251	8000.365287	11.032576	-0.104436	4.817780
535.204465	8000.408765	11.037581	-0.104479	4.817792
535.303256	8000.339551	11.042586	-0.104498	4.817771
535.219521	8000.383686	11.047591	-0.104482	4.817785
535.054411	8000.383397	11.052595	-0.104452	4.817785
535.295129	8000.348942	11.057600	-0.104496	4.817774
535.172214	8000.389343	11.062605	-0.104474	4.817787
534.915175	8000.381388	11.067610	-0.104426	4.817785
535.007960	8000.381691	11.072615	-0.104443	4.817785
535.254584	8000.366305	11.077619	-0.104489	4.817779
535.068015	8000.359376	11.082624	-0.104455	4.817778
535.128577	8000.359210	11.087629	-0.104466	4.817778
535.231436	8000.340676	11.092634	-0.104485	4.817772
534.935631	8000.450272	11.097639	-0.104430	4.817806
535.147677	8000.463913	11.102643	-0.104470	4.817809
535.224582	8000.375397	11.107648	-0.104484	4.817782
535.173941	8000.425287	11.112653	-0.104475	4.817797
534.660544	8000.456838	11.117658	-0.104379	4.817809
534.854021	8000.491299	11.122663	-0.104415	4.817818
534.880153	8000.417864	11.127667	-0.104420	4.817796
534.745946	8000.450718	11.132672	-0.104395	4.817807
535.014766	8000.486277	11.137677	-0.104446	4.817816
534.784291	8000.418596	11.142682	-0.104403	4.817797
535.359106	8000.379515	11.147687	-0.104510	4.817783
535.105106	8000.371604	11.152691	-0.104463	4.817782
535.111723	8000.394908	11.157696	-0.104464	4.817788
535.217510	8000.422820	11.162701	-0.104484	4.817796
535.342096	8000.379293	11.167706	-0.104507	4.817783
535.405368	8000.368620	11.172711	-0.104519	4.817779
535.269473	8000.389848	11.177715	-0.104494	4.817786
535.128129	8000.410997	11.182720	-0.104467	4.817793
535.282325	8000.380556	11.187725	-0.104496	4.817783
535.137021	8000.380556	11.192730	-0.104469	4.817784
535.227523	8000.374498	11.197735	-0.104486	4.817782
535.179123	8000.337942	11.202739	-0.104477	4.817771
534.949231	8000.403150	11.207744	-0.104434	4.817792
535.155407	8000.387176	11.212749	-0.104473	4.817786
535.304889	8000.371431	11.217754	-0.104501	4.817781
535.129710	8000.388923	11.222759	-0.104468	4.817787
535.273953	8000.402631	11.227763	-0.104495	4.817790
535.343122	8000.368842	11.232768	-0.104508	4.817780
535.573547	8000.400680	11.237773	-0.104551	4.817788
535.259627	8000.386622	11.242778	-0.104493	4.817785
535.265614	8000.395152	11.247783	-0.104494	4.817788
534.967305	8000.411906	11.252787	-0.104439	4.817794
535.442414	8000.371374	11.257792	-0.104527	4.817780
535.473324	8000.415070	11.262797	-0.104533	4.817793
535.047382	8000.400436	11.267802	-0.104454	4.817790
535.297856	8000.452602	11.272807	-0.104500	4.817805
535.390999	8000.425491	11.277811	-0.104518	4.817796
535.238312	8000.378979	11.282816	-0.104489	4.817783
534.939381	8000.364086	11.287821	-0.104434	4.817780
534.879145	8000.430710	11.292826	-0.104423	4.817800
534.792052	8000.475850	11.297831	-0.104407	4.817814
535.126522	8000.377376	11.302835	-0.104469	4.817783
534.994582	8000.391280	11.307840	-0.104445	4.817788
535.310215	8000.420139	11.312845	-0.104503	4.817795
535.096154	8000.408591	11.317850	-0.104464	4.817793
535.121823	8000.422681	11.322855	-0.104468	4.817797
535.176819	8000.321191	11.327859	-0.104479	4.817766
534.860079	8000.349278	11.332864	-0.104420	4.817776
534.980907	8000.436466	11.337869	-0.104442	4.817801
534.723024	8000.474901	11.342874	-0.104395	4.817814
534.973081	8000.481713	11.347879	-0.104441	4.817815
534.688356	8000.479682	11.352883	-0.104388	4.817815
535.006578	8000.412609	11.357888	-0.104448	4.817794
535.447737	8000.401112	11.362893	-0.104530	4.817789
535.228179	8000.403193	11.367898	-0.104489	4.817790
535.135605	8000.457746	11.372903	-0.104472	4.817807
535.191303	8000.395287	11.377907	-0.104482	4.817788
535.806184	8000.361009	11.382912	-0.104597	4.817775
535.671325	8000.355887	11.387917	-0.104572	4.817774
535.803322	8000.335669	11.392922	-0.104596	4.817768
535.814564	8000.369587	11.397927	-0.104599	4.817778
535.744014	8000.344309	11.402931	-0.104586	4.817771
535.752747	8000.346552	11.407936	-0.104587	4.817771
535.564208	8000.378615	11.412941	-0.104552	4.817782
535.750275	8000.344419	11.417946	-0.104587	4.817771
535.628271	8000.348976	11.422951	-0.104564	4.817773
535.609861	8000.337113	11.427955	-0.104561	4.817769
535.745733	8000.362300	11.432960	-0.104586	4.817776
535.316407	8000.401402	11.437965	-0.104507	4.817789
535.704455	8000.354329	11.442970	-0.104579	4.817774
535.755847	8000.384614	11.447975	-0.104588	4.817783
535.608039	8000.396177	11.452979	-0.104561	4.817787
535.620088	8000.379485	11.457984	-0.104563	4.817782
535.721780	8000.394682	11.462989	-0.104582	4.817786
535.481617	8000.400682	11.467994	-0.104538	4.817788
535.443787	8000.383263	11.472999	-0.104531	4.817783
535.471413	8000.406873	11.478003	-0.104536	4.817790
535.661710	8000.391723	11.483008	-0.104572	4.817785
535.512224	8000.373732	11.488013	-0.104544	4.817780
535.297722	8000.368505	11.493018	-0.104504	4.817780
535.669535	8000.379200	11.498023	-0.104573	4.817781
535.761880	8000.325711	11.503027	-0.104590	4.817765
535.617123	8000.363684	11.508032	-0.104564	4.817777
535.728075	8000.383235	11.513037	-0.104584	4.817782
535.813114	8000.335968	11.518042	-0.104600	4.817768
535.826778	8000.366757	11.523047	-0.104603	4.817777
535.432464	8000.372620	11.528051	-0.104530	4.817780
535.457010	8000.378257	11.533056	-0.104534	4.817782
535.114791	8000.380662	11.538061	-0.104471	4.817784
534.716038	8000.382244	11.543066	-0.104396	4.817786
535.291637	8000.388523	11.548071	-0.104504	4.817786
535.318049	8000.369931	11.553075	-0.104509	4.817780
535.294509	8000.386468	11.558080	-0.104504	4.817785
535.374713	8000.418226	11.563085	-0.104519	4.817794
535.957895	8000.353958	11.568090	-0.104628	4.817773
535.797958	8000.357963	11.573095	-0.104598	4.817774
535.707241	8000.360866	11.578099	-0.104581	4.817776
535.587656	8000.407643	11.583104	-0.104559	4.817790
535.632400	8000.406192	11.588109	-0.104568	4.817789
535.445485	8000.378164	11.593114	-0.104533	4.817782
535.793814	8000.376917	11.598119	-0.104598	4.817780
535.745310	8000.340359	11.603123	-0.104589	4.817769
535.753448	8000.407980	11.608128	-0.104591	4.817789
535.915985	8000.419846	11.613133	-0.104621	4.817792
536.018612	8000.347523	11.618138	-0.104640	4.817770
535.991203	8000.376659	11.623143	-0.104635	4.817779
535.850107	8000.341917	11.628147	-0.104609	4.817769
535.975571	8000.346915	11.633152	-0.104632	4.817770
535.978231	8000.348014	11.638157	-0.104633	4.817771
535.587270	8000.353926	11.643162	-0.104560	4.817774
535.641031	8000.395846	11.648167	-0.104570	4.817786
535.734739	8000.371906	11.653171	-0.104588	4.817779
535.608220	8000.409090	11.658176	-0.104564	4.817790
535.878768	8000.369798	11.663181	-0.104615	4.817778
535.807472	8000.332909	11.668186	-0.104602	4.817767
535.997812	8000.365217	11.673191	-0.104637	4.817776
536.012214	8000.334849	11.678195	-0.104640	4.817767
535.866619	8000.372810	11.683200	-0.104613	4.817778
535.730698	8000.386656	11.688205	-0.104588	4.817783
535.728886	8000.318085	11.693210	-0.104587	4.817763
535.910466	8000.368194	11.698215	-0.104621	4.817777
536.143145	8000.339951	11.703219	-0.104665	4.817768
535.956308	8000.364656	11.708224	-0.104630	4.817776
535.838508	8000.380875	11.713229	-0.104608	4.817781
535.742554	8000.367882	11.718234	-0.104590	4.817778
535.764054	8000.390349	11.723239	-0.104594	4.817784
535.614689	8000.382906	11.728243	-0.104567	4.817783
535.762605	8000.350265	11.733248	-0.104594	4.817772
535.900783	8000.360721	11.738253	-0.104620	4.817775
535.681093	8000.340653	11.743258	-0.104579	4.817770
535.983559	8000.358775	11.748263	-0.104636	4.817774
535.949761	8000.371999	11.753267	-0.104629	4.817778
535.780041	8000.371642	11.758272	-0.104598	4.817778
535.916959	8000.352550	11.763277	-0.104623	4.817772
535.875353	8000.336131	11.768282	-0.104616	4.817768
535.918306	8000.382112	11.773287	-0.104624	4.817781
535.949417	8000.338277	11.778291	-0.104630	4.817768
535.941366	8000.345549	11.783296	-0.104628	4.817770
536.224540	8000.351790	11.788301	-0.104681	4.817771
535.895241	8000.315360	11.793306	-0.104620	4.817761
535.877722	8000.333039	11.798311	-0.104617	4.817767
535.890902	8000.337456	11.803315	-0.104619	4.817768
536.143788	8000.329545	11.808320	-0.104666	4.817764
536.097884	8000.373177	11.813325	-0.104658	4.817778
536.137697	8000.328414	11.818330	-0.104665	4.817764
536.269308	8000.373578	11.823335	-0.104690	4.817777
536.259070	8000.347069	11.828339	-0.104688	4.817769
536.315397	8000.359497	11.833344	-0.104699	4.817773
536.236580	8000.360464	11.838349	-0.104684	4.817773
536.003815	8000.363407	11.843354	-0.104641	4.817775
536.033853	8000.401818	11.848359	-0.104647	4.817786
536.219313	8000.361286	11.853363	-0.104681	4.817773
536.242718	8000.378508	11.858368	-0.104686	4.817778
536.324533	8000.369160	11.863373	-0.104701	4.817775
536.168404	8000.333143	11.868378	-0.104672	4.817765
536.436979	8000.348663	11.873383	-0.104722	4.817769
536.309559	8000.343649	11.878387	-0.104698	4.817768
536.192960	8000.375705	11.883392	-0.104677	4.817778
536.098123	8000.388039	11.888397	-0.104659	4.817782
536.038170	8000.343932	11.893402	-0.104648	4.817769
536.159204	8000.372067	11.898407	-0.104671	4.817777
536.183168	8000.334456	11.903411	-0.104675	4.817766
536.134165	8000.380152	11.908416	-0.104666	4.817779
535.710475	8000.485776	11.913421	-0.104588	4.817812
535.979190	8000.401109	11.918426	-0.104638	4.817786
535.978147	8000.367351	11.923431	-0.104637	4.817776
536.097443	8000.353276	11.928435	-0.104660	4.817772
536.133174	8000.351694	11.933440	-0.104666	4.817771
536.215517	8000.401413	11.938445	-0.104682	4.817785
535.839564	8000.430745	11.943450	-0.104612	4.817796
535.799093	8000.449144	11.948455	-0.104605	4.817801
536.098506	8000.396563	11.953459	-0.104660	4.817784
535.583355	8000.435468	11.958464	-0.104565	4.817798
536.004147	8000.419457	11.963469	-0.104643	4.817792
535.691110	8000.407520	11.968474	-0.104585	4.817789
535.869526	8000.403798	11.973479	-0.104618	4.817788
536.042701	8000.385235	11.978483	-0.104650	4.817781
535.979741	8000.391706	11.983488	-0.104639	4.817783
535.780674	8000.347682	11.988493	-0.104602	4.817771
535.851736	8000.386690	11.993498	-0.104615	4.817783
535.759567	8000.400118	11.998503	-0.104598	4.817787
535.995734	8000.363489	12.003507	-0.104642	4.817775
536.017241	8000.369082	12.008512	-0.104646	4.817777
535.962713	8000.451609	12.013517	-0.104636	4.817801
535.829512	8000.391670	12.018522	-0.104611	4.817784
535.804967	8000.440886	12.023527	-0.104607	4.817799
535.869369	8000.421793	12.028531	-0.104619	4.817793
535.964588	8000.385220	12.033536	-0.104637	4.817782
536.225862	8000.420672	12.038541	-0.104685	4.817791
536.047843	8000.381172	12.043546	-0.104652	4.817780
535.956684	8000.450511	12.048551	-0.104635	4.817801
536.045892	8000.394866	12.053555	-0.104652	4.817784
536.190249	8000.346353	12.058560	-0.104679	4.817769
536.229590	8000.376463	12.063565	-0.104686	4.817778
536.101791	8000.359842	12.068570	-0.104663	4.817773
536.423794	8000.395125	12.073575	-0.104723	4.817783
536.236610	8000.444081	12.078579	-0.104688	4.817798
535.931960	8000.416446	12.083584	-0.104631	4.817791
536.291531	8000.421691	12.088589	-0.104698	4.817791
536.227690	8000.395456	12.093594	-0.104687	4.817783
536.033615	8000.407399	12.098599	-0.104651	4.817788
536.134030	8000.383557	12.103603	-0.104669	4.817780
536.176465	8000.397892	12.108608	-0.104677	4.817784
536.113560	8000.448659	12.113613	-0.104666	4.817800
535.970746	8000.410727	12.118618	-0.104639	4.817789
536.147822	8000.430187	12.123623	-0.104672	4.817794
535.890049	8000.332575	12.128627	-0.104624	4.817766
535.909014	8000.390863	12.133632	-0.104628	4.817783
536.182081	8000.350553	12.138637	-0.104679	4.817770
536.151406	8000.339566	12.143642	-0.104673	4.817767
536.172964	8000.390508	12.148647	-0.104677	4.817782
536.157255	8000.370248	12.153651	-0.104674	4.817776
536.266953	8000.403491	12.158656	-0.104695	4.817786
536.170542	8000.446388	12.163661	-0.104677	4.817799
535.934234	8000.398656	12.168666	-0.104633	4.817786
535.757900	8000.521594	12.173671	-0.104600	4.817823
535.826260	8000.419243	12.178675	-0.104613	4.817792
536.089852	8000.391450	12.183680	-0.104662	4.817783
536.153580	8000.445117	12.188685	-0.104674	4.817798
535.942986	8000.400924	12.193690	-0.104635	4.817786
536.169890	8000.435875	12.198695	-0.104678	4.817796
535.986235	8000.404730	12.203699	-0.104643	4.817787
535.568861	8000.427131	12.208704	-0.104566	4.817796
535.598929	8000.382226	12.213709	-0.104571	4.817782
535.510704	8000.391494	12.218714	-0.104555	4.817785
535.938226	8000.384018	12.223719	-0.104635	4.817781
535.537182	8000.366581	12.228723	-0.104560	4.817778
535.251714	8000.322354	12.233728	-0.104507	4.817766
535.962524	8000.410756	12.238733	-0.104640	4.817789
536.348334	8000.359434	12.243738	-0.104711	4.817772
535.867251	8000.410435	12.248743	-0.104622	4.817789
535.614398	8000.448943	12.253747	-0.104575	4.817802
535.799393	8000.451644	12.258752	-0.104610	4.817802
536.179547	8000.444534	12.263757	-0.104680	4.817798
535.782083	8000.407110	12.268762	-0.104606	4.817789
535.922995	8000.459792	12.273767	-0.104633	4.817804
535.887962	8000.481435	12.278771	-0.104626	4.817810
535.394922	8000.475313	12.283776	-0.104535	4.817811
535.803703	8000.417996	12.288781	-0.104611	4.817792
535.812779	8000.442391	12.293786	-0.104613	4.817799
536.388743	8000.419151	12.298791	-0.104720	4.817790
535.986603	8000.415407	12.303795	-0.104645	4.817790
536.087037	8000.401057	12.308800	-0.104664	4.817786
535.938900	8000.416833	12.313805	-0.104636	4.817791
536.155713	8000.340901	12.318810	-0.104677	4.817768
536.043849	8000.457397	12.323815	-0.104656	4.817803
536.479220	8000.393086	12.328819	-0.104737	4.817782
536.114877	8000.428914	12.333824	-0.104669	4.817794
536.011417	8000.374681	12.338829	-0.104650	4.817778
535.907833	8000.445948	12.343834	-0.104631	4.817800
535.728756	8000.499241	12.348839	-0.104598	4.817816
535.680621	8000.521747	12.353843	-0.104589	4.817823
535.634658	8000.357617	12.358848	-0.104580	4.817775
536.243782	8000.426611	12.363853	-0.104694	4.817793
535.826574	8000.401555	12.368858	-0.104616	4.817787
535.931313	8000.429453	12.373863	-0.104636	4.817795
535.737093	8000.452996	12.378867	-0.104600	4.817803
535.617953	8000.402753	12.383872	-0.104578	4.817788
535.416105	8000.569614	12.388877	-0.104540	4.817838
535.478669	8000.341678	12.393882	-0.104552	4.817771
535.589383	8000.474070	12.398887	-0.104573	4.817809
535.423647	8000.503301	12.403891	-0.104542	4.817819
535.932439	8000.420022	12.408896	-0.104637	4.817792
535.924710	8000.425188	12.413901	-0.104635	4.817793
535.413279	8000.404034	12.418906	-0.104540	4.817789
535.695647	8000.460885	12.423911	-0.104593	4.817805
536.222715	8000.395801	12.428915	-0.104691	4.817783
536.209822	8000.409330	12.433920	-0.104689	4.817788
536.132022	8000.464098	12.438925	-0.104674	4.817804
535.894447	8000.449042	12.443930	-0.104630	4.817801
536.188048	8000.395321	12.448935	-0.104685	4.817783
536.071222	8000.372532	12.453939	-0.104663	4.817777
535.827441	8000.409063	12.458944	-0.104618	4.817789
536.050288	8000.435518	12.463949	-0.104660	4.817796
535.903627	8000.403857	12.468954	-0.104632	4.817787
535.871381	8000.317969	12.473959	-0.104626	4.817762
535.675316	8000.434292	12.478963	-0.104590	4.817797
535.509735	8000.433995	12.483968	-0.104559	4.817798
535.489464	8000.489601	12.488973	-0.104556	4.817814
535.850941	8000.354608	12.493978	-0.104623	4.817773
536.224435	8000.364274	12.498983	-0.104692	4.817774
535.771845	8000.403035	12.503987	-0.104608	4.817788
535.941126	8000.419218	12.508992	-0.104640	4.817792
536.252547	8000.408997	12.513997	-0.104698	4.817787
536.190629	8000.372244	12.519002	-0.104686	4.817777
536.129702	8000.321794	12.524007	-0.104675	4.817762
536.245486	8000.427897	12.529011	-0.104697	4.817793
536.461681	8000.423671	12.534016	-0.104737	4.817791
536.199763	8000.507396	12.539021	-0.104689	4.817817
536.013299	8000.425587	12.544026	-0.104654	4.817793
535.982280	8000.483146	12.549031	-0.104648	4.817810
535.836324	8000.414583	12.554035	-0.104621	4.817791
535.856785	8000.464456	12.559040	-0.104625	4.817805
536.148645	8000.459223	12.564045	-0.104679	4.817803
535.741115	8000.438526	12.569050	-0.104604	4.817798
535.757524	8000.433498	12.574055	-0.104607	4.817797
535.867066	8000.481505	12.579059	-0.104627	4.817810
535.810231	8000.369946	12.584064	-0.104617	4.817778
535.444381	8000.521762	12.589069	-0.104549	4.817824
535.970682	8000.376515	12.594074	-0.104647	4.817779
535.636312	8000.501369	12.599079	-0.104585	4.817817
535.863434	8000.474100	12.604083	-0.104627	4.817808
535.955433	8000.399513	12.609088	-0.104644	4.817786
535.864490	8000.451981	12.614093	-0.104627	4.817802
536.348051	8000.376771	12.619098	-0.104717	4.817777
536.509485	8000.404442	12.624103	-0.104748	4.817785
536.566184	8000.385236	12.629107	-0.104758	4.817779
536.389946	8000.405876	12.634112	-0.104725	4.817786
536.688440	8000.391249	12.639117	-0.104781	4.817780
536.689398	8000.339591	12.644122	-0.104781	4.817765
536.611591	8000.396469	12.649127	-0.104767	4.817782
536.324839	8000.419717	12.654131	-0.104714	4.817790
536.552718	8000.340782	12.659136	-0.104756	4.817766
536.540337	8000.417597	12.664141	-0.104754	4.817788
536.361820	8000.385471	12.669146	-0.104721	4.817780
536.552283	8000.397745	12.674151	-0.104756	4.817783
536.528828	8000.390027	12.679155	-0.104752	4.817780
536.419837	8000.404265	12.684160	-0.104732	4.817785
535.748635	8000.476752	12.689165	-0.104607	4.817809
535.747138	8000.408185	12.694170	-0.104607	4.817789
535.759184	8000.182678	12.699175	-0.104609	4.817722
536.266211	8000.438963	12.704179	-0.104704	4.817796
536.252011	8000.421888	12.709184	-0.104701	4.817791
536.545861	8000.416685	12.714189	-0.104756	4.817788
536.591614	8000.336150	12.719194	-0.104764	4.817764
536.612374	8000.360716	12.724199	-0.104768	4.817771
536.625037	8000.363016	12.729203	-0.104771	4.817772
536.623962	8000.368280	12.734208	-0.104771	4.817773
536.548807	8000.386174	12.739213	-0.104757	4.817779
536.449447	8000.373131	12.744218	-0.104738	4.817776
536.421781	8000.415975	12.749223	-0.104733	4.817788
536.631204	8000.385285	12.754227	-0.104772	4.817778
536.697387	8000.366217	12.759232	-0.104785	4.817773
536.727562	8000.395139	12.764237	-0.104790	4.817781
536.780298	8000.355837	12.769242	-0.104800	4.817769
536.683500	8000.374471	12.774247	-0.104782	4.817775
536.716854	8000.363362	12.779251	-0.104789	4.817772
536.661768	8000.365729	12.784256	-0.104778	4.817773
536.876022	8000.377295	12.789261	-0.104818	4.817775
536.559329	8000.376904	12.794266	-0.104760	4.817776
536.555991	8000.400064	12.799271	-0.104759	4.817783
536.296800	8000.453244	12.804275	-0.104711	4.817800
536.671356	8000.383829	12.809280	-0.104781	4.817778
536.524515	8000.418608	12.814285	-0.104753	4.817789
536.332231	8000.397883	12.819290	-0.104718	4.817783
536.576068	8000.415153	12.824295	-0.104763	4.817788
536.573047	8000.407733	12.829299	-0.104763	4.817785
536.552110	8000.398997	12.834304	-0.104759	4.817783
536.500065	8000.445704	12.839309	-0.104749	4.817797
536.384374	8000.428204	12.844314	-0.104728	4.817792
536.347655	8000.407637	12.849319	-0.104721	4.817786
536.585141	8000.413213	12.854323	-0.104765	4.817787
536.444193	8000.425931	12.859328	-0.104739	4.817791
536.538321	8000.416762	12.864333	-0.104757	4.817788
536.654783	8000.403701	12.869338	-0.104778	4.817784
536.538573	8000.414669	12.874343	-0.104757	4.817788
536.709940	8000.388697	12.879347	-0.104789	4.817779
536.603519	8000.387152	12.884352	-0.104769	4.817779
536.565931	8000.420360	12.889357	-0.104762	4.817789
536.485726	8000.353809	12.894362	-0.104747	4.817770
536.763388	8000.363135	12.899367	-0.104799	4.817771
536.525946	8000.399757	12.904371	-0.104755	4.817783
536.203622	8000.421432	12.909376	-0.104695	4.817791
536.449682	8000.417642	12.914381	-0.104741	4.817789
536.420128	8000.430928	12.919386	-0.104736	4.817793
536.674247	8000.399834	12.924391	-0.104783	4.817783
536.395643	8000.355704	12.929395	-0.104731	4.817771
536.157648	8000.475635	12.934400	-0.104687	4.817807
536.381124	8000.367106	12.939405	-0.104729	4.817774
536.414471	8000.432986	12.944410	-0.104735	4.817793
536.254049	8000.395851	12.949415	-0.104705	4.817783
536.178677	8000.490732	12.954419	-0.104691	4.817812
536.252211	8000.436968	12.959424	-0.104705	4.817795
536.356705	8000.475410	12.964429	-0.104725	4.817806
536.051916	8000.382384	12.969434	-0.104668	4.817780
535.986608	8000.056615	12.974439	-0.104656	4.817684
536.070019	8000.444884	12.979443	-0.104671	4.817798
536.014926	8000.464126	12.984448	-0.104661	4.817804
536.401529	8000.470821	12.989453	-0.104733	4.817805
536.451032	8000.381903	12.994458	-0.104743	4.817778
536.542985	8000.425436	12.999463	-0.104760	4.817791
536.487901	8000.397218	13.004467	-0.104750	4.817783
536.575127	8000.443846	13.009472	-0.104766	4.817796
536.479384	8000.535266	13.014477	-0.104748	4.817823
536.380180	8000.477930	13.019482	-0.104730	4.817807
536.756259	8000.407482	13.024487	-0.104800	4.817784
536.612448	8000.400119	13.029491	-0.104773	4.817783
536.324234	8000.376942	13.034496	-0.104720	4.817777
536.785287	8000.415307	13.039501	-0.104806	4.817787
536.252794	8000.483487	13.044506	-0.104706	4.817809
536.390017	8000.347334	13.049511	-0.104732	4.817768
536.699170	8000.416179	13.054515	-0.104790	4.817787
536.791123	8000.399597	13.059520	-0.104807	4.817782
536.758126	8000.423379	13.064525	-0.104801	4.817789
536.716213	8000.404845	13.069530	-0.104793	4.817784
536.861914	8000.436506	13.074535	-0.104820	4.817793
536.588579	8000.398779	13.079539	-0.104770	4.817783
536.294967	8000.420872	13.084544	-0.104715	4.817790
536.613123	8000.477194	13.089549	-0.104774	4.817806
536.505390	8000.416569	13.094554	-0.104754	4.817788
536.486287	8000.407860	13.099559	-0.104751	4.817786
536.593806	8000.419979	13.104563	-0.104771	4.817789
536.599475	8000.414795	13.109568	-0.104772	4.817787
536.800962	8000.406137	13.114573	-0.104810	4.817784
536.692227	8000.377137	13.119578	-0.104789	4.817776
536.292673	8000.382922	13.124583	-0.104715	4.817779
536.549197	8000.458383	13.129587	-0.104763	4.817800
536.127264	8000.465950	13.134592	-0.104685	4.817804
536.667695	8000.460122	13.139597	-0.104785	4.817800
536.675015	8000.402229	13.144602	-0.104787	4.817783
536.577655	8000.341756	13.149607	-0.104769	4.817766
536.630548	8000.452217	13.154611	-0.104779	4.817798
536.662333	8000.425265	13.159616	-0.104785	4.817790
536.633622	8000.452274	13.164621	-0.104779	4.817798
536.482436	8000.411055	13.169626	-0.104751	4.817787
536.638184	8000.356380	13.174631	-0.104780	4.817770
536.519091	8000.487536	13.179635	-0.104758	4.817809
536.352932	8000.457700	13.184640	-0.104727	4.817801
536.573004	8000.453531	13.189645	-0.104768	4.817799
536.681258	8000.405546	13.194650	-0.104789	4.817784
536.626840	8000.441672	13.199655	-0.104779	4.817795
536.861910	8000.403973	13.204659	-0.104822	4.817783
536.893134	8000.372795	13.209664	-0.104828	4.817773
536.867838	8000.381925	13.214669	-0.104824	4.817776
536.741197	8000.379030	13.219674	-0.104800	4.817776
536.752866	8000.396081	13.224679	-0.104802	4.817781
536.552504	8000.422697	13.229683	-0.104765	4.817790
536.129913	8000.363813	13.234688	-0.104687	4.817774
536.418938	8000.479823	13.239693	-0.104741	4.817807
536.389655	8000.460419	13.244698	-0.104735	4.817802
536.312191	8000.344340	13.249703	-0.104721	4.817768
536.699792	8000.395345	13.254707	-0.104793	4.817781
536.802092	8000.371530	13.259712	-0.104812	4.817773
536.873213	8000.393666	13.264717	-0.104825	4.817780
536.780035	8000.351183	13.269722	-0.104808	4.817768
536.954747	8000.387485	13.274727	-0.104841	4.817778
536.822811	8000.400333	13.279731	-0.104816	4.817782
536.410309	8000.408038	13.284736	-0.104740	4.817786
536.936616	8000.395676	13.289741	-0.104838	4.817780
537.035679	8000.368651	13.294746	-0.104856	4.817772
537.035804	8000.405572	13.299751	-0.104856	4.817783
536.962661	8000.342287	13.304755	-0.104843	4.817764
537.153255	8000.347181	13.309760	-0.104878	4.817765
536.888110	8000.424531	13.314765	-0.104829	4.817789
536.881673	8000.360109	13.319770	-0.104828	4.817770
537.047478	8000.396282	13.324775	-0.104859	4.817780
536.902111	8000.354092	13.329779	-0.104832	4.817768
536.609650	8000.406787	13.334784	-0.104777	4.817785
537.093623	8000.408574	13.339789	-0.104868	4.817783
536.996477	8000.361814	13.344794	-0.104850	4.817770
536.789765	8000.391501	13.349799	-0.104811	4.817779
537.055774	8000.361636	13.354803	-0.104861	4.817769
537.131400	8000.369073	13.359808	-0.104875	4.817771
537.117994	8000.379430	13.364813	-0.104873	4.817774
537.270792	8000.359516	13.369818	-0.104901	4.817768
537.226339	8000.377858	13.374823	-0.104893	4.817773
537.292686	8000.356684	13.379827	-0.104905	4.817767
537.093133	8000.376983	13.384832	-0.104868	4.817774
536.901480	8000.415328	13.389837	-0.104833	4.817786
536.872777	8000.380112	13.394842	-0.104827	4.817776
536.485134	8000.440911	13.399847	-0.104755	4.817795
536.377218	8000.462547	13.404851	-0.104735	4.817802
536.541828	8000.405892	13.409856	-0.104766	4.817785
536.402592	8000.453437	13.414861	-0.104740	4.817799
536.462785	8000.394206	13.419866	-0.104751	4.817782
536.197041	8000.448345	13.424871	-0.104702	4.817799
536.515158	8000.456151	13.429875	-0.104761	4.817800
536.944858	8000.380158	13.434880	-0.104841	4.817775
536.906277	8000.397531	13.439885	-0.104834	4.817781
536.525130	8000.339249	13.444890	-0.104763	4.817765
536.832509	8000.345844	13.449895	-0.104821	4.817766
536.719226	8000.433845	13.454899	-0.104800	4.817792
536.320069	8000.445963	13.459904	-0.104726	4.817798
536.851868	8000.466376	13.464909	-0.104825	4.817801
536.609613	8000.336293	13.469914	-0.104780	4.817764
536.620947	8000.403962	13.474919	-0.104782	4.817784
536.756679	8000.379580	13.479923	-0.104807	4.817776
536.432310	8000.431810	13.484928	-0.104747	4.817793
536.725738	8000.367540	13.489933	-0.104802	4.817773
536.752859	8000.460752	13.494938	-0.104807	4.817800
536.745709	8000.375226	13.499943	-0.104805	4.817775
536.706375	8000.443212	13.504947	-0.104798	4.817795
536.577979	8000.447675	13.509952	-0.104774	4.817797
536.691479	8000.457773	13.514957	-0.104796	4.817799
536.691086	8000.402931	13.519962	-0.104796	4.817783
536.722547	8000.319024	13.524967	-0.104801	4.817758
536.680274	8000.462901	13.529971	-0.104794	4.817801
536.497899	8000.425446	13.534976	-0.104760	4.817791
536.654860	8000.428794	13.539981	-0.104789	4.817791
536.631423	8000.415803	13.544986	-0.104785	4.817787
536.482590	8000.435788	13.549991	-0.104757	4.817794
536.522737	8000.490166	13.554995	-0.104765	4.817810
536.695076	8000.441007	13.560000	-0.104797	4.817794
537.147357	8000.350577	13.565005	-0.104881	4.817766
536.795721	8000.423502	13.570010	-0.104816	4.817789
536.885773	8000.396345	13.575015	-0.104833	4.817780
537.069515	8000.412741	13.580019	-0.104867	4.817784
536.937567	8000.413987	13.585024	-0.104843	4.817785
537.085665	8000.419317	13.590029	-0.104870	4.817786
536.983260	8000.423103	13.595034	-0.104851	4.817788
536.999015	8000.440214	13.600039	-0.104854	4.817793
537.008005	8000.459335	13.605043	-0.104856	4.817798
537.112337	8000.423949	13.610048	-0.104875	4.817788
537.112639	8000.425014	13.615053	-0.104876	4.817788
536.820193	8000.413375	13.620058	-0.104821	4.817786
537.067735	8000.420154	13.625063	-0.104867	4.817787
536.978803	8000.422027	13.630067	-0.104851	4.817788
536.890855	8000.427079	13.635072	-0.104835	4.817789
536.643001	8000.429801	13.640077	-0.104789	4.817791
536.511020	8000.455304	13.645082	-0.104764	4.817799
536.796013	8000.465793	13.650087	-0.104817	4.817801
536.591264	8000.308835	13.655091	-0.104779	4.817756
536.386606	8000.499914	13.660096	-0.104741	4.817813
536.620011	8000.459027	13.665101	-0.104785	4.817800
536.901857	8000.410409	13.670106	-0.104837	4.817784
536.818066	8000.410248	13.675111	-0.104822	4.817785
536.936218	8000.423578	13.680115	-0.104844	4.817788
536.676459	8000.414525	13.685120	-0.104796	4.817787
536.955492	8000.391177	13.690125	-0.104848	4.817778
536.449387	8000.375370	13.695130	-0.104753	4.817776
536.739318	8000.441826	13.700135	-0.104807	4.817794
536.572405	8000.447837	13.705139	-0.104776	4.817797
536.741160	8000.419718	13.710144	-0.104808	4.817788
536.922626	8000.352761	13.715149	-0.104842	4.817767
536.783132	8000.488895	13.720154	-0.104816	4.817808
536.714650	8000.366617	13.725159	-0.104803	4.817772
537.182494	8000.455707	13.730163	-0.104890	4.817797
536.822348	8000.459955	13.735168	-0.104824	4.817799
536.408113	8000.453923	13.740173	-0.104746	4.817799
536.461036	8000.510597	13.745178	-0.104756	4.817816
536.636195	8000.508938	13.750183	-0.104789	4.817815
536.517121	8000.410180	13.755187	-0.104767	4.817786
536.347963	8000.204176	13.760192	-0.104735	4.817726
536.795247	8000.463816	13.765197	-0.104819	4.817801
536.401937	8000.497111	13.770202	-0.104746	4.817812
536.300647	8000.182412	13.775207	-0.104727	4.817719
536.515185	8000.352178	13.780211	-0.104767	4.817769
536.636067	8000.483668	13.785216	-0.104790	4.817807
536.681837	8000.368329	13.790221	-0.104798	4.817773
536.703403	8000.431929	13.795226	-0.104802	4.817792
536.931256	8000.420491	13.800231	-0.104845	4.817787
536.947217	8000.438660	13.805235	-0.104848	4.817793
536.839716	8000.401240	13.810240	-0.104828	4.817782
536.904532	8000.443323	13.815245	-0.104840	4.817794
536.806729	8000.404991	13.820250	-0.104822	4.817783
536.967068	8000.401006	13.825255	-0.104852	4.817781
536.858929	8000.396272	13.830259	-0.104832	4.817780
536.695194	8000.407602	13.835264	-0.104801	4.817784
536.435843	8000.416484	13.840269	-0.104753	4.817788
536.495187	8000.450050	13.845274	-0.104764	4.817798
536.960020	8000.411481	13.850279	-0.104851	4.817784
536.901575	8000.370558	13.855283	-0.104840	4.817773
536.754349	8000.425370	13.860288	-0.104813	4.817789
536.610403	8000.501323	13.865293	-0.104786	4.817812
536.736429	8000.435668	13.870298	-0.104810	4.817793
536.685350	8000.341065	13.875303	-0.104800	4.817765
536.879506	8000.481007	13.880307	-0.104836	4.817805
536.856026	8000.435321	13.885312	-0.104832	4.817792
536.961254	8000.503305	13.890317	-0.104852	4.817812
536.630356	8000.444700	13.895322	-0.104790	4.817796
537.118204	8000.402248	13.900327	-0.104881	4.817781
537.232511	8000.391265	13.905331	-0.104903	4.817777
537.215261	8000.377309	13.910336	-0.104899	4.817773
537.029362	8000.448432	13.915341	-0.104865	4.817795
536.899985	8000.433896	13.920346	-0.104841	4.817791
537.116387	8000.385378	13.925351	-0.104881	4.817776
537.098813	8000.418878	13.930355	-0.104878	4.817786
537.065811	8000.339303	13.935360	-0.104872	4.817763
537.206343	8000.440497	13.940365	-0.104898	4.817792
537.316405	8000.399921	13.945370	-0.104919	4.817779
537.135333	8000.469004	13.950375	-0.104885	4.817801
537.159421	8000.440886	13.955379	-0.104890	4.817792
536.900731	8000.410754	13.960384	-0.104842	4.817784
537.190277	8000.407599	13.965389	-0.104896	4.817782
536.917622	8000.415231	13.970394	-0.104845	4.817786
537.043521	8000.430784	13.975399	-0.104868	4.817790
537.033492	8000.404277	13.980403	-0.104867	4.817782
537.069806	8000.371063	13.985408	-0.104874	4.817772
537.184104	8000.407540	13.990413	-0.104895	4.817782
536.943472	8000.397710	13.995418	-0.104850	4.817780
537.019912	8000.442072	14.000423	-0.104865	4.817793
537.051612	8000.424611	14.005427	-0.104870	4.817788
537.030874	8000.404276	14.010432	-0.104867	4.817782
536.894573	8000.481395	14.015437	-0.104841	4.817805
537.457656	8000.380980	14.020442	-0.104946	4.817773
536.913935	8000.408918	14.025447	-0.104845	4.817784
537.074742	8000.405995	14.030451	-0.104875	4.817782
537.263389	8000.338089	14.035456	-0.104910	4.817761
537.508055	8000.373303	14.040461	-0.104956	4.817771
537.367084	8000.377582	14.045466	-0.104930	4.817773
537.256101	8000.377024	14.050471	-0.104909	4.817773
537.173898	8000.462315	14.055475	-0.104894	4.817798
536.934332	8000.432462	14.060480	-0.104850	4.817791
537.057454	8000.373092	14.065485	-0.104872	4.817773
537.270281	8000.387803	14.070490	-0.104912	4.817776
536.979961	8000.442638	14.075495	-0.104858	4.817793
537.059157	8000.448017	14.080499	-0.104873	4.817795
536.906548	8000.394120	14.085504	-0.104845	4.817779
537.139832	8000.417566	14.090509	-0.104888	4.817785
536.903685	8000.354014	14.095514	-0.104844	4.817768
536.925693	8000.426058	14.100519	-0.104849	4.817789
536.942262	8000.480094	14.105523	-0.104852	4.817805
537.251711	8000.404457	14.110528	-0.104909	4.817781
537.270221	8000.427935	14.115533	-0.104913	4.817788
537.195592	8000.415252	14.120538	-0.104899	4.817784
537.259238	8000.417241	14.125543	-0.104911	4.817785
537.124855	8000.440600	14.130547	-0.104886	4.817792
536.948905	8000.378980	14.135552	-0.104853	4.817775
536.791659	8000.392514	14.140557	-0.104824	4.817779
537.007311	8000.378789	14.145562	-0.104864	4.817774
536.860521	8000.398804	14.150567	-0.104837	4.817781
537.171363	8000.404396	14.155571	-0.104895	4.817781
537.034868	8000.417178	14.160576	-0.104870	4.817786
536.938678	8000.456913	14.165581	-0.104852	4.817798
536.578529	8000.402101	14.170586	-0.104785	4.817783
536.906996	8000.386856	14.175591	-0.104846	4.817777
536.937499	8000.442150	14.180595	-0.104852	4.817793
536.850192	8000.323816	14.185600	-0.104836	4.817759
537.282944	8000.438761	14.190605	-0.104917	4.817791
537.450986	8000.374773	14.195610	-0.104948	4.817771
537.271372	8000.386926	14.200615	-0.104914	4.817776
537.322983	8000.399286	14.205619	-0.104924	4.817779
537.481469	8000.371018	14.210624	-0.104954	4.817770
537.496432	8000.404992	14.215629	-0.104957	4.817780
537.167336	8000.400200	14.220634	-0.104895	4.817780
537.246189	8000.414012	14.225639	-0.104910	4.817784
537.092522	8000.452909	14.230643	-0.104882	4.817796
537.252660	8000.401462	14.235648	-0.104912	4.817780
537.298561	8000.428505	14.240653	-0.104920	4.817788
537.423637	8000.364945	14.245658	-0.104944	4.817768
537.152313	8000.426385	14.250663	-0.104893	4.817788
537.212647	8000.416724	14.255667	-0.104904	4.817785
537.289679	8000.411525	14.260672	-0.104919	4.817783
537.069911	8000.473717	14.265677	-0.104878	4.817802
537.083703	8000.438065	14.270682	-0.104881	4.817792
537.161317	8000.461351	14.275687	-0.104895	4.817798
537.451592	8000.429731	14.280691	-0.104949	4.817788
537.079728	8000.428534	14.285696	-0.104880	4.817789
537.072137	8000.484327	14.290701	-0.104879	4.817805
537.092922	8000.426630	14.295706	-0.104883	4.817788
536.959466	8000.439456	14.300711	-0.104858	4.817793
536.933943	8000.453855	14.305715	-0.104853	4.817797
537.145390	8000.398937	14.310720	-0.104893	4.817780
536.675226	8000.429003	14.315725	-0.104805	4.817791
536.913493	8000.420881	14.320730	-0.104850	4.817787
536.620557	8000.339628	14.325735	-0.104795	4.817764
537.148359	8000.364202	14.330739	-0.104894	4.817769
536.914453	8000.363962	14.335744	-0.104850	4.817770
536.881139	8000.418325	14.340749	-0.104844	4.817787
536.885621	8000.407850	14.345754	-0.104845	4.817783
537.150838	8000.334732	14.350759	-0.104894	4.817761
537.228102	8000.398090	14.355763	-0.104909	4.817779
537.361452	7999.482501	14.360768	-0.104933	4.817507

537.267912	7996.264902	14.365773	-0.104914	4.816555
536.977348	7990.655457	14.370778	-0.104856	4.814895
537.134938	7983.996545	14.375783	-0.104881	4.812922
537.239007	7976.805622	14.380787	-0.104896	4.810790
537.168059	7969.109112	14.385792	-0.104878	4.808508
537.042040	7961.353464	14.390797	-0.104849	4.806208
536.900079	7953.392098	14.395802	-0.104818	4.803846
537.024907	7945.569632	14.400807	-0.104836	4.801522
536.988120	7937.529232	14.405811	-0.104824	4.799134
536.958378	7929.557001	14.410816	-0.104813	4.796764
537.003112	7921.593871	14.415821	-0.104817	4.794396
536.885544	7913.564458	14.420826	-0.104790	4.792007
536.857395	7905.496164	14.425831	-0.104779	4.789605
536.805001	7897.543774	14.430835	-0.104764	4.787237
537.127105	7889.451064	14.435840	-0.104819	4.784824
537.184376	7881.573841	14.440845	-0.104825	4.782475
537.170997	7873.552120	14.445850	-0.104817	4.780083
537.123966	7865.519406	14.450855	-0.104803	4.777686
537.074973	7857.553449	14.455859	-0.104789	4.775307
537.221131	7849.535109	14.460864	-0.104811	4.772912
537.068276	7841.557224	14.465869	-0.104777	4.770528
537.013094	7833.503008	14.470874	-0.104762	4.768119
536.964268	7825.504076	14.475879	-0.104748	4.765726
537.249340	7817.467738	14.480883	-0.104796	4.763320
536.980727	7809.553873	14.485888	-0.104741	4.760951
536.972956	7801.532020	14.490893	-0.104734	4.758547
536.934492	7793.506650	14.495898	-0.104722	4.756141
536.881055	7785.477940	14.500903	-0.104707	4.753733
536.796761	7777.522729	14.505907	-0.104686	4.751346
536.332935	7769.439247	14.510912	-0.104594	4.748920
536.591511	7761.457857	14.515917	-0.104637	4.746522
536.365085	7753.466901	14.520922	-0.104590	4.744121
536.621930	7745.516317	14.525927	-0.104633	4.741729
536.819598	7737.421854	14.530931	-0.104664	4.739293
536.570398	7729.455446	14.535936	-0.104613	4.736896
536.625306	7721.474824	14.540941	-0.104618	4.734492
536.732672	7713.446849	14.545946	-0.104633	4.732073
536.603082	7705.438788	14.550951	-0.104603	4.729659
536.552381	7697.496496	14.555955	-0.104589	4.727264
536.499048	7689.378280	14.560960	-0.104574	4.724814
536.624007	7681.503277	14.565965	-0.104592	4.722436
536.431845	7673.453418	14.570970	-0.104551	4.720005
536.423746	7665.510176	14.575975	-0.104544	4.717604
536.458606	7657.463917	14.580979	-0.104546	4.715170
536.331718	7649.447648	14.585984	-0.104517	4.712745
536.376665	7641.468533	14.590989	-0.104520	4.710330
536.494390	7633.459908	14.595994	-0.104537	4.707904
536.701702	7625.409514	14.600999	-0.104570	4.705464
536.685830	7617.411460	14.606003	-0.104562	4.703039
536.546988	7609.427208	14.611008	-0.104531	4.700618
536.589968	7601.456250	14.616013	-0.104534	4.698198
536.311547	7593.470404	14.621018	-0.104477	4.695774
536.316896	7585.427410	14.626023	-0.104473	4.693330
536.428926	7577.458895	14.631027	-0.104489	4.690908
536.465088	7569.415125	14.636032	-0.104490	4.688461
536.248152	7561.482256	14.641037	-0.104445	4.686048
536.443557	7553.405427	14.646042	-0.104476	4.683589
536.523557	7545.501433	14.651047	-0.104486	4.681181
536.292994	7537.494959	14.656051	-0.104438	4.678741
536.128126	7529.506271	14.661056	-0.104402	4.676305
536.078425	7521.473053	14.666061	-0.104388	4.673854
536.144174	7513.418831	14.671066	-0.104395	4.671396
536.049973	7505.344917	14.676071	-0.104372	4.668930
536.019134	7497.431743	14.681075	-0.104361	4.666512
535.978884	7489.332782	14.686080	-0.104348	4.664036
535.932646	7481.477919	14.691085	-0.104335	4.661633
535.938345	7473.394703	14.696090	-0.104331	4.659159
535.879459	7465.425766	14.701095	-0.104315	4.656719
535.890344	7457.403066	14.706099	-0.104312	4.654261
535.837623	7449.424242	14.711104	-0.104297	4.651816
535.789900	7441.394693	14.716109	-0.104283	4.649353
535.782960	7433.389802	14.721114	-0.104276	4.646897
535.906698	7425.354672	14.726119	-0.104294	4.644430
535.864651	7417.470011	14.731123	-0.104281	4.642008
535.844584	7409.368113	14.736128	-0.104272	4.639517
535.801412	7401.415720	14.741133	-0.104259	4.637072
535.784904	7393.360014	14.746138	-0.104251	4.634593
535.760114	7385.410023	14.751143	-0.104241	4.632146
535.755252	7377.380133	14.756147	-0.104235	4.629673
535.596011	7369.370862	14.761152	-0.104200	4.627205
535.754186	7361.391959	14.766157	-0.104225	4.624744
535.745796	7353.412377	14.771162	-0.104218	4.622283
535.411217	7345.392996	14.776167	-0.104150	4.619807
535.672079	7337.402416	14.781171	-0.104194	4.617340
535.510002	7329.350071	14.786176	-0.104159	4.614851
535.712941	7321.381200	14.791181	-0.104191	4.612388
535.395254	7313.386328	14.796186	-0.104127	4.609915
535.550460	7305.387736	14.801191	-0.104151	4.607439
535.470137	7297.360714	14.806195	-0.104131	4.604953
535.262259	7289.384748	14.811200	-0.104087	4.602482
535.508260	7281.373591	14.816205	-0.104127	4.599999
535.420697	7273.424047	14.821210	-0.104106	4.597533
535.281567	7265.357284	14.826215	-0.104075	4.595029
535.430071	7257.357313	14.831219	-0.104097	4.592546
535.377747	7249.295042	14.836224	-0.104083	4.590041
535.070841	7241.348630	14.841229	-0.104020	4.587570
535.158558	7233.290628	14.846234	-0.104031	4.585064
535.298959	7225.330061	14.851239	-0.104052	4.582587
535.313363	7217.305140	14.856243	-0.104050	4.580089
535.034736	7209.333045	14.861248	-0.103993	4.577605
534.959222	7201.339381	14.866253	-0.103974	4.575113
535.210954	7193.292425	14.871258	-0.104016	4.572604
535.110678	7185.262631	14.876263	-0.103992	4.570098
534.976743	7177.328444	14.881267	-0.103962	4.567621
534.845071	7169.256727	14.886272	-0.103932	4.565099
535.015766	7161.338571	14.891277	-0.103959	4.562625
534.830149	7153.319989	14.896282	-0.103919	4.560117
534.877397	7145.357329	14.901287	-0.103923	4.557626
534.744604	7137.351309	14.906291	-0.103893	4.555119
534.631256	7129.298811	14.911296	-0.103867	4.552596
534.615177	7121.270089	14.916301	-0.103858	4.550080
534.795380	7113.225547	14.921306	-0.103887	4.547558
534.859523	7105.255868	14.926311	-0.103894	4.545057
534.904010	7097.333453	14.931315	-0.103897	4.542570
534.543241	7089.312100	14.936320	-0.103824	4.540050
534.356578	7081.337701	14.941325	-0.103785	4.537543
534.273238	7073.289553	14.946330	-0.103764	4.535012
534.610744	7065.242521	14.951335	-0.103822	4.532481
534.768785	7057.212258	14.956339	-0.103846	4.529954
534.568663	7049.236042	14.961344	-0.103803	4.527441
534.791120	7041.229964	14.966349	-0.103840	4.524918
534.615396	7033.318913	14.971354	-0.103802	4.522423
534.537838	7025.325350	14.976359	-0.103782	4.519901
534.485897	7017.303423	14.981363	-0.103768	4.517368
534.455218	7009.224559	14.986368	-0.103757	4.514816
534.633564	7001.321085	14.991373	-0.103785	4.512319
534.224872	6993.234261	14.996378	-0.103704	4.509761
534.157110	6985.256288	15.001383	-0.103686	4.507236
534.391783	6977.188030	15.006387	-0.103724	4.504683
534.346490	6969.227692	15.011392	-0.103711	4.502161
534.398489	6961.209748	15.016397	-0.103715	4.499620
534.396345	6953.271708	15.021402	-0.103710	4.497103
534.232536	6945.205143	15.026407	-0.103674	4.494543
534.248678	6937.252317	15.031411	-0.103672	4.492018
534.063357	6929.149058	15.036416	-0.103632	4.489443
534.291993	6921.203819	15.041421	-0.103670	4.486919
534.164172	6913.139593	15.046426	-0.103641	4.484354
534.160445	6905.219796	15.051431	-0.103635	4.481834
534.285307	6897.193098	15.056435	-0.103653	4.479279
533.960397	6889.270569	15.061440	-0.103588	4.476754
533.992250	6881.200297	15.066445	-0.103588	4.474181
534.185376	6873.205998	15.071450	-0.103619	4.471633
534.213584	6865.143995	15.076455	-0.103619	4.469060
534.022049	6857.229309	15.081459	-0.103578	4.466532
533.978428	6849.120843	15.086464	-0.103565	4.463942
534.217906	6841.206595	15.091469	-0.103605	4.461413
534.001643	6833.126390	15.096474	-0.103559	4.458827
533.892560	6825.202586	15.101479	-0.103534	4.456291
533.967750	6817.160850	15.106483	-0.103543	4.453716
533.787240	6809.180012	15.111488	-0.103504	4.451159
534.157340	6801.147162	15.116493	-0.103568	4.448585
534.159129	6793.163165	15.121498	-0.103563	4.446024
534.107702	6785.129140	15.126503	-0.103548	4.443445
534.072184	6777.250209	15.131507	-0.103536	4.440915
533.724671	6769.198926	15.136512	-0.103467	4.438326
533.833957	6761.191033	15.141517	-0.103482	4.435752
533.686879	6753.134535	15.146522	-0.103449	4.433160
533.571621	6745.163759	15.151527	-0.103423	4.430593
533.615154	6737.154401	15.156531	-0.103426	4.428014
533.732926	6729.087477	15.161536	-0.103442	4.425415
533.731669	6721.135621	15.166541	-0.103437	4.422851
533.770039	6713.134520	15.171546	-0.103439	4.420269
533.818240	6705.108916	15.176551	-0.103443	4.417679
533.694596	6697.123790	15.181555	-0.103415	4.415099
533.388863	6689.111766	15.186560	-0.103353	4.412508
533.556043	6681.105016	15.191565	-0.103379	4.409919
533.452831	6673.075847	15.196570	-0.103354	4.407320
533.523594	6665.026191	15.201575	-0.103362	4.404714
533.458766	6657.153277	15.206579	-0.103345	4.402163
533.461101	6649.147978	15.211584	-0.103340	4.399568
533.413656	6641.188741	15.216589	-0.103327	4.396986
533.463003	6633.135275	15.221594	-0.103331	4.394373
533.330146	6625.147680	15.226599	-0.103301	4.391778
533.141239	6617.095813	15.231603	-0.103260	4.389161
533.127039	6609.099237	15.236608	-0.103253	4.386561
533.249080	6601.070238	15.241613	-0.103270	4.383950
533.165035	6593.103709	15.246618	-0.103249	4.381356
533.138460	6585.094807	15.251623	-0.103239	4.378747
533.009097	6577.186601	15.256627	-0.103210	4.376169
532.743048	6569.124120	15.261632	-0.103155	4.373538
533.129940	6561.128880	15.266637	-0.103222	4.370932
532.952675	6553.119264	15.271642	-0.103184	4.368316
533.077923	6545.116848	15.276647	-0.103202	4.365702
533.164520	6537.154365	15.281651	-0.103213	4.363100
533.113628	6529.131759	15.286656	-0.103199	4.360476
533.150116	6521.189395	15.291661	-0.103200	4.357877
533.175141	6513.198635	15.296666	-0.103200	4.355260
532.936371	6505.156490	15.301671	-0.103150	4.352623
532.894042	6497.157855	15.306675	-0.103137	4.350000
532.829114	6489.148396	15.311680	-0.103120	4.347372
532.905161	6481.146376	15.316685	-0.103129	4.344746
532.564459	6473.229808	15.321690	-0.103061	4.342143
532.412298	6465.188505	15.326695	-0.103027	4.339499
532.222514	6457.252682	15.331699	-0.102987	4.336888
532.306934	6449.163642	15.336704	-0.102997	4.334227
532.291988	6441.230672	15.341709	-0.102989	4.331615
532.610371	6433.123220	15.346714	-0.103043	4.328946
532.173127	6425.199463	15.351719	-0.102957	4.326330
532.650852	6417.135862	15.356723	-0.103041	4.323674
532.261669	6409.208505	15.361728	-0.102963	4.321054
532.268818	6401.175400	15.366733	-0.102959	4.318401
532.323200	6393.195192	15.371738	-0.102964	4.315764
532.248897	6385.155061	15.376743	-0.102945	4.313105
532.301297	6377.172432	15.381747	-0.102950	4.310464
532.412293	6369.080098	15.386752	-0.102965	4.307786
532.544270	6361.086438	15.391757	-0.102985	4.305139
532.238098	6353.154911	15.396762	-0.102923	4.302507
532.416319	6345.077657	15.401767	-0.102951	4.299829
532.442717	6337.143752	15.406771	-0.102951	4.297196
532.371024	6329.076293	15.411776	-0.102932	4.294516
532.126645	6321.199685	15.416781	-0.102882	4.291896
532.031657	6313.141029	15.421786	-0.102859	4.289216
531.644109	6305.165579	15.426791	-0.102781	4.286559
531.526468	6297.127085	15.431795	-0.102754	4.283881
531.219805	6289.215869	15.436800	-0.102692	4.281243
531.915573	6281.116730	15.441805	-0.102817	4.278549
531.608649	6273.160243	15.446810	-0.102754	4.275892
531.525788	6265.125052	15.451815	-0.102734	4.273210
531.186995	6257.172132	15.456819	-0.102665	4.270550
531.601161	6249.108960	15.461824	-0.102737	4.267860
531.582750	6241.103009	15.466829	-0.102729	4.265182
531.549206	6233.064288	15.471834	-0.102717	4.262492
531.850673	6225.044414	15.476839	-0.102768	4.259809
531.647562	6217.143636	15.481843	-0.102726	4.257160
531.422298	6209.105139	15.486848	-0.102678	4.254463
531.368766	6201.178485	15.491853	-0.102663	4.251804
531.658877	6193.049645	15.496858	-0.102712	4.249078
531.528678	6185.125994	15.501863	-0.102683	4.246415
531.379126	6177.147590	15.506867	-0.102650	4.243732
531.107210	6169.144547	15.511872	-0.102594	4.241038
531.278202	6161.156578	15.516877	-0.102621	4.238351
531.112305	6153.147659	15.521882	-0.102585	4.235653
531.165901	6145.107597	15.526887	-0.102590	4.232944
531.419513	6137.077644	15.531891	-0.102632	4.230239
530.944523	6129.129779	15.536896	-0.102538	4.227553
531.246580	6121.076154	15.541901	-0.102589	4.224837
531.290010	6113.111425	15.546906	-0.102592	4.222147
531.171415	6105.060834	15.551911	-0.102565	4.219424
531.042236	6097.145002	15.556915	-0.102536	4.216745
530.844444	6089.087069	15.561920	-0.102494	4.214015
531.487097	6081.058227	15.566925	-0.102608	4.211303
531.180951	6073.059327	15.571930	-0.102546	4.208589
531.319154	6065.112986	15.576935	-0.102567	4.205895
531.383962	6057.103262	15.581939	-0.102574	4.203178
531.194975	6049.104260	15.586944	-0.102533	4.200460
531.193375	6041.145675	15.591949	-0.102528	4.197755
531.372777	6033.060470	15.596954	-0.102556	4.195008
531.356135	6025.042991	15.601959	-0.102548	4.192280
531.080818	6016.993591	15.606963	-0.102492	4.189537
530.627682	6009.089336	15.611968	-0.102402	4.186839
531.184533	6001.008688	15.616973	-0.102501	4.184090
530.860319	5993.112337	15.621978	-0.102435	4.181393
531.219194	5985.037764	15.626983	-0.102497	4.178641
531.184115	5977.093445	15.631987	-0.102485	4.175927
531.084566	5969.020498	15.636992	-0.102462	4.173166
531.137987	5961.075350	15.641997	-0.102466	4.170450
531.275437	5953.044871	15.647002	-0.102487	4.167703
531.279126	5945.027093	15.652007	-0.102482	4.164957
531.139586	5937.122604	15.657011	-0.102451	4.162247
531.090915	5929.064455	15.662016	-0.102437	4.159483
531.251480	5921.121507	15.667021	-0.102462	4.156759
531.014701	5913.094427	15.672026	-0.102413	4.154000
530.954584	5905.162657	15.677031	-0.102396	4.151274
531.068521	5897.053688	15.682035	-0.102412	4.148487
530.893170	5889.065956	15.687040	-0.102375	4.145736
530.897750	5881.093290	15.692045	-0.102370	4.142992
530.800228	5873.129696	15.697050	-0.102347	4.140247
530.831269	5865.126811	15.702055	-0.102348	4.137488
530.721805	5857.117328	15.707059	-0.102322	4.134724
530.556124	5849.106330	15.712064	-0.102286	4.131956
530.687310	5841.084125	15.717069	-0.102305	4.129186
530.357193	5833.152508	15.722074	-0.102239	4.126440
530.361190	5825.091744	15.727079	-0.102234	4.123652
530.610403	5817.165871	15.732083	-0.102276	4.120912
530.561377	5809.134145	15.737088	-0.102261	4.118129
530.314006	5801.154289	15.742093	-0.102210	4.115360
530.451503	5793.080326	15.747098	-0.102231	4.112561
530.272177	5785.090765	15.752103	-0.102192	4.109786
530.480009	5777.101320	15.757107	-0.102226	4.107014
530.118072	5769.099329	15.762112	-0.102153	4.104228
530.117996	5761.169302	15.767117	-0.102148	4.101470
530.137652	5753.125455	15.772122	-0.102147	4.098671
529.865517	5745.140043	15.777127	-0.102091	4.095886
530.180455	5737.118582	15.782131	-0.102144	4.093095
529.914388	5729.091124	15.787136	-0.102090	4.090292
529.935131	5721.111261	15.792141	-0.102088	4.087507
529.709789	5713.079880	15.797146	-0.102041	4.084699
529.760739	5705.122243	15.802151	-0.102046	4.081919
529.818171	5697.109059	15.807155	-0.102051	4.079118
529.617267	5689.131708	15.812160	-0.102009	4.076323
529.594862	5681.129301	15.817165	-0.101999	4.073520
529.832751	5673.100136	15.822170	-0.102039	4.070710
530.095074	5665.051364	15.827175	-0.102082	4.067892
529.956381	5657.069498	15.832179	-0.102051	4.065089
530.082313	5649.096179	15.837184	-0.102070	4.062291
529.858008	5641.097960	15.842189	-0.102023	4.059477
529.622080	5633.157363	15.847194	-0.101974	4.056681
529.459809	5625.100326	15.852199	-0.101938	4.053844
529.573999	5617.128334	15.857203	-0.101954	4.051038
529.910841	5609.031695	15.862208	-0.102012	4.048190
529.972425	5601.089820	15.867213	-0.102018	4.045391
529.350040	5593.157761	15.872218	-0.101897	4.042582
529.444750	5585.123011	15.877223	-0.101910	4.039747
529.711490	5577.129537	15.882227	-0.101954	4.036926
529.694291	5569.091495	15.887232	-0.101946	4.034084
529.599310	5561.105820	15.892237	-0.101923	4.031256
529.385883	5553.053545	15.897242	-0.101878	4.028402
529.230914	5545.096037	15.902247	-0.101844	4.025579
529.505313	5537.085169	15.907251	-0.101890	4.022743
529.317184	5529.080612	15.912256	-0.101850	4.019899
529.168740	5521.174912	15.917261	-0.101817	4.017090
529.130027	5513.116097	15.922266	-0.101805	4.014225
529.534743	5505.088305	15.927271	-0.101875	4.011377
529.493472	5497.101553	15.932275	-0.101862	4.008534
529.430174	5489.105738	15.937280	-0.101845	4.005686
529.446229	5481.147854	15.942285	-0.101843	4.002850
528.950954	5473.157384	15.947290	-0.101746	3.999992
529.038978	5465.146329	15.952295	-0.101757	3.997134
529.112299	5457.129433	15.957299	-0.101766	3.994272
529.181763	5449.136778	15.962304	-0.101774	3.991417
529.029874	5441.152489	15.967309	-0.101740	3.988559
528.793608	5433.173661	15.972314	-0.101691	3.985699
529.126689	5425.133301	15.977319	-0.101748	3.982825
529.050257	5417.192326	15.982323	-0.101729	3.979977
528.943188	5409.127170	15.987328	-0.101703	3.977083
529.196486	5401.126971	15.992333	-0.101746	3.974215
528.832051	5393.179902	15.997338	-0.101673	3.971354
529.071908	5385.127568	16.002343	-0.101712	3.968464
529.253246	5377.177575	16.007347	-0.101741	3.965607
528.816799	5369.176122	16.012352	-0.101654	3.962719
528.502603	5361.246549	16.017357	-0.101591	3.959857
528.472902	5353.217825	16.022362	-0.101580	3.956962
528.908180	5345.125967	16.027367	-0.101656	3.954050
528.565226	5337.179113	16.032371	-0.101587	3.951175
528.671932	5329.130090	16.037376	-0.101602	3.948269
528.460866	5321.166855	16.042381	-0.101557	3.945386
528.428558	5313.209110	16.047386	-0.101546	3.942506
528.650210	5305.118461	16.052391	-0.101582	3.939580
528.849944	5297.167481	16.057395	-0.101614	3.936702
528.715214	5289.130932	16.062400	-0.101584	3.933786
528.592329	5281.168595	16.067405	-0.101556	3.930894
528.477227	5273.167950	16.072410	-0.101529	3.927986
528.428068	5265.159565	16.077415	-0.101515	3.925074
528.532744	5257.226375	16.082419	-0.101530	3.922191
528.274589	5249.168729	16.087424	-0.101476	3.919253
528.725882	5241.201739	16.092429	-0.101555	3.916359
528.473507	5233.169575	16.097434	-0.101503	3.913427
528.546799	5225.146037	16.102439	-0.101512	3.910501
528.534087	5217.158680	16.107443	-0.101504	3.907585
528.323104	5209.141711	16.112448	-0.101460	3.904652
528.622538	5201.178744	16.117453	-0.101510	3.901746
528.498155	5193.164959	16.122458	-0.101482	3.898811
528.348337	5185.232782	16.127463	-0.101449	3.895904
528.213449	5177.226591	16.132467	-0.101419	3.892967
527.991817	5169.213330	16.137472	-0.101372	3.890024
528.190658	5161.202952	16.142477	-0.101404	3.887088
528.092129	5153.197765	16.147482	-0.101381	3.884146
528.240131	5145.251430	16.152487	-0.101403	3.881228
528.111717	5137.266802	16.157491	-0.101374	3.878289
528.105508	5129.247646	16.162496	-0.101368	3.875336
528.051947	5121.164376	16.167501	-0.101353	3.872357
527.828853	5113.119618	16.172506	-0.101306	3.869387
527.618700	5105.165001	16.177511	-0.101262	3.866447
527.670658	5097.173993	16.182515	-0.101266	3.863498
527.546263	5089.193894	16.187520	-0.101238	3.860546
528.034979	5081.178710	16.192525	-0.101324	3.857592
527.693212	5073.207074	16.197530	-0.101255	3.854635
527.610029	5065.233800	16.202535	-0.101235	3.851680
528.073019	5057.188494	16.207539	-0.101316	3.848707
527.807444	5049.200020	16.212544	-0.101261	3.845738
527.713531	5041.253405	16.217549	-0.101238	3.842786
527.527615	5033.275388	16.222554	-0.101199	3.839818
527.816958	5025.291350	16.227559	-0.101247	3.836855
527.719515	5017.275337	16.232563	-0.101224	3.833871
527.667644	5009.293141	16.237568	-0.101209	3.830897
527.647603	5001.229071	16.242573	-0.101200	3.827891
527.648410	4993.226191	16.247578	-0.101195	3.824906
527.483224	4985.298650	16.252583	-0.101160	3.821943
527.649535	4977.240892	16.257587	-0.101185	3.818937
527.270348	4969.301720	16.262592	-0.101110	3.815960
527.058681	4961.300616	16.267597	-0.101065	3.812962
526.929129	4953.281861	16.272602	-0.101036	3.809956
527.239129	4945.234155	16.277607	-0.101088	3.806947
527.294249	4937.222891	16.282611	-0.101094	3.803944
527.045001	4929.330137	16.287616	-0.101042	3.800976
527.052832	4921.296935	16.292621	-0.101038	3.797958
527.308173	4913.236924	16.297626	-0.101081	3.794934
527.441262	4905.239572	16.302631	-0.101100	3.791928
527.215780	4897.293490	16.307635	-0.101053	3.788931
526.698421	4889.325204	16.312640	-0.100952	3.785917
526.702671	4881.296866	16.317645	-0.100948	3.782889
526.757187	4873.278492	16.322650	-0.100953	3.779864
526.896264	4865.277017	16.327655	-0.100973	3.776844
527.165832	4857.224306	16.332659	-0.101018	3.773806
527.075826	4849.299200	16.337664	-0.100997	3.770806
527.215796	4841.282105	16.342669	-0.101017	3.767773
526.840990	4833.333937	16.347674	-0.100943	3.764752
526.950213	4825.329168	16.352679	-0.100958	3.761719
526.876314	4817.338178	16.357683	-0.100939	3.758684
526.776539	4809.389811	16.362688	-0.100915	3.755662
526.730852	4801.377171	16.367693	-0.100902	3.752615
526.409081	4793.411492	16.372698	-0.100836	3.749576
526.646594	4785.370224	16.377703	-0.100876	3.746520
527.159271	4777.305629	16.382707	-0.100966	3.743459
526.752304	4769.354381	16.387712	-0.100885	3.740416
526.800878	4761.387164	16.392717	-0.100889	3.737376
526.951172	4753.354535	16.397722	-0.100912	3.734311
526.798864	4745.400166	16.402727	-0.100878	3.731266
526.954783	4737.347641	16.407731	-0.100902	3.728188
527.010253	4729.326137	16.412736	-0.100907	3.725117
526.700320	4721.421276	16.417741	-0.100845	3.722079
526.653205	4713.412329	16.422746	-0.100831	3.719006
526.794446	4705.436730	16.427751	-0.100852	3.715947
526.859510	4697.368684	16.432755	-0.100859	3.712849
526.637392	4689.329482	16.437760	-0.100812	3.709751
526.889828	4681.350929	16.442765	-0.100854	3.706687
526.544712	4673.423259	16.447770	-0.100785	3.703624
526.310469	4665.435051	16.452775	-0.100736	3.700538
526.363191	4657.435330	16.457779	-0.100741	3.697453
525.867039	4649.440920	16.462784	-0.100643	3.694353
526.281715	4641.411861	16.467789	-0.100715	3.691260
526.306817	4633.384042	16.472794	-0.100715	3.688155
526.285431	4625.359658	16.477799	-0.100706	3.685048
526.374703	4617.456196	16.482803	-0.100717	3.681988
526.170539	4609.422226	16.487808	-0.100674	3.678867
526.453575	4601.458568	16.492813	-0.100722	3.675783
526.305677	4593.456911	16.497818	-0.100689	3.672671
526.175917	4585.437594	16.502823	-0.100660	3.669549
526.402800	4577.409562	16.507827	-0.100697	3.666431
526.158466	4569.430240	16.512832	-0.100646	3.663317
525.909029	4561.516612	16.517837	-0.100595	3.660226
525.904349	4553.509693	16.522842	-0.100589	3.657102
525.677839	4545.497813	16.527847	-0.100541	3.653967
525.486235	4537.587911	16.532851	-0.100500	3.650871
525.701037	4529.463428	16.537856	-0.100535	3.647699
526.042490	4521.441503	16.542861	-0.100594	3.644568
526.111067	4513.507559	16.547866	-0.100601	3.641461
525.841645	4505.525314	16.552871	-0.100546	3.638324
525.716328	4497.554245	16.557875	-0.100518	3.635192
525.772898	4489.547871	16.562880	-0.100523	3.632048
525.828584	4481.509579	16.567885	-0.100528	3.628889
525.652456	4473.519310	16.572890	-0.100490	3.625740
525.336366	4465.576934	16.577895	-0.100426	3.622603
525.749930	4457.506371	16.582899	-0.100498	3.619433
525.749318	4449.534832	16.587904	-0.100493	3.616288
525.431707	4441.577972	16.592909	-0.100429	3.613137
525.507485	4433.547778	16.597914	-0.100438	3.609965
525.495706	4425.548285	16.602919	-0.100430	3.606801
525.363902	4417.558993	16.607923	-0.100401	3.603634
525.128686	4409.609491	16.612928	-0.100352	3.600477
525.279797	4401.598056	16.617933	-0.100375	3.597304
524.985801	4393.600939	16.622938	-0.100315	3.594120
525.251848	4385.581081	16.627943	-0.100359	3.590942
525.538367	4377.535321	16.632947	-0.100407	3.587750
525.154015	4369.560032	16.637952	-0.100331	3.584565
525.121794	4361.637335	16.642957	-0.100320	3.581407
525.392715	4353.587326	16.647962	-0.100365	3.578205
525.188468	4345.621840	16.652967	-0.100322	3.575020
525.108441	4337.644946	16.657971	-0.100302	3.571831
524.922416	4329.608186	16.662976	-0.100262	3.568613
525.081192	4321.622417	16.667981	-0.100286	3.565422
525.086383	4313.639649	16.672986	-0.100282	3.562224
524.653476	4305.704724	16.677991	-0.100197	3.559030
524.862220	4297.724163	16.682995	-0.100230	3.555834
524.425216	4289.671991	16.688000	-0.100144	3.552587
524.495451	4281.623942	16.693005	-0.100152	3.549354
524.742710	4273.612428	16.698010	-0.100193	3.546138
524.586145	4265.631809	16.703015	-0.100158	3.542919
524.548951	4257.692772	16.708019	-0.100146	3.539718
524.331877	4249.679553	16.713024	-0.100101	3.536478
524.692040	4241.671278	16.718029	-0.100163	3.533255
524.676594	4233.656542	16.723034	-0.100155	3.530015
524.361047	4225.693887	16.728039	-0.100091	3.526784
524.538455	4217.699077	16.733043	-0.100119	3.523552
524.294529	4209.737979	16.738048	-0.100068	3.520318
524.586909	4201.709623	16.743053	-0.100117	3.517070
524.591789	4193.740891	16.748058	-0.100113	3.513834
523.725579	4185.890426	16.753063	-0.099947	3.510616
523.237801	4177.883742	16.758067	-0.099851	3.507343
523.290361	4169.795669	16.763072	-0.099856	3.504052
523.370959	4161.825518	16.768077	-0.099865	3.500806
523.316594	4153.792278	16.773082	-0.099850	3.497527
523.602590	4145.701518	16.778087	-0.099898	3.494232
523.175206	4137.880099	16.783091	-0.099814	3.491021
523.409270	4129.761121	16.788096	-0.099852	3.487707
523.167581	4121.789710	16.793101	-0.099802	3.484435
523.649791	4113.762094	16.798106	-0.099887	3.481160
523.196535	4105.862217	16.803111	-0.099797	3.477904
522.912154	4097.902470	16.808115	-0.099739	3.474626
522.700511	4089.909609	16.813120	-0.099694	3.471334
523.432706	4081.761987	16.818125	-0.099826	3.468006
523.472110	4073.764895	16.823130	-0.099828	3.464714
523.119612	4065.850243	16.828135	-0.099757	3.461439
523.135834	4057.874779	16.833139	-0.099755	3.458149
523.085427	4049.818630	16.838144	-0.099740	3.454820
523.207793	4041.846021	16.843149	-0.099758	3.451528
522.868702	4033.903571	16.848154	-0.099690	3.448230
522.955608	4025.867712	16.853159	-0.099701	3.444905
522.804992	4017.953901	16.858163	-0.099668	3.441618
522.830958	4009.873792	16.863168	-0.099667	3.438266
523.141948	4001.872706	16.868173	-0.099720	3.434953
522.712321	3993.958414	16.873178	-0.099635	3.431647
522.342236	3985.993790	16.878183	-0.099561	3.428320
522.582664	3977.942946	16.883187	-0.099601	3.424974
522.783584	3969.922604	16.888192	-0.099633	3.421636
523.257712	3961.838618	16.893197	-0.099716	3.418278
522.988102	3953.940296	16.898202	-0.099661	3.414968
523.137151	3945.934101	16.903207	-0.099683	3.411625
523.098808	3937.949192	16.908211	-0.099671	3.408281
522.688875	3930.007150	16.913216	-0.099590	3.404938
522.973280	3922.026416	16.918221	-0.099638	3.401600
523.026764	3914.018667	16.923226	-0.099642	3.398240
523.370195	3905.970482	16.928231	-0.099701	3.394869
522.971382	3898.039921	16.933235	-0.099622	3.391518
522.887881	3889.992736	16.938240	-0.099601	3.388126
522.742266	3881.997445	16.943245	-0.099569	3.384750
522.924592	3874.019862	16.948250	-0.099598	3.381391
522.908886	3865.989541	16.953255	-0.099590	3.377998
523.107711	3858.028565	16.958259	-0.099622	3.374639
522.738142	3850.066136	16.963264	-0.099548	3.371255
522.779342	3842.049910	16.968269	-0.099550	3.367860
522.766675	3834.034640	16.973274	-0.099543	3.364461
522.765246	3826.116913	16.978279	-0.099537	3.361099
522.690774	3818.109927	16.983283	-0.099518	3.357694
522.998410	3810.063889	16.988288	-0.099570	3.354282
522.741563	3802.156503	16.993293	-0.099517	3.350905
522.471446	3794.148571	16.998298	-0.099462	3.347482
522.602190	3786.102849	17.003303	-0.099481	3.344054
522.778559	3778.180388	17.008307	-0.099509	3.340676
522.287815	3770.212947	17.013312	-0.099412	3.337251
522.700927	3762.151554	17.018317	-0.099484	3.333816
522.456342	3754.213983	17.023322	-0.099434	3.330406
522.282464	3746.194729	17.028327	-0.099396	3.326960
522.318823	3738.229150	17.033331	-0.099398	3.323541
522.352228	3730.239346	17.038336	-0.099399	3.320109
522.063145	3722.320654	17.043341	-0.099340	3.316691
522.061672	3714.265728	17.048346	-0.099334	3.313222
521.986206	3706.243245	17.053351	-0.099315	3.309760
521.949584	3698.290776	17.058355	-0.099303	3.306326
521.490854	3690.308022	17.063360	-0.099213	3.302860
522.079471	3682.238686	17.068365	-0.099317	3.299393
522.145730	3674.248552	17.073370	-0.099324	3.295936
522.359519	3666.203730	17.078375	-0.099359	3.292458
522.326109	3658.246568	17.083379	-0.099348	3.289004
522.445465	3650.265924	17.088384	-0.099365	3.285543
522.359174	3642.327456	17.093389	-0.099344	3.282088
522.378899	3634.308843	17.098394	-0.099342	3.278599
522.406471	3626.338864	17.103399	-0.099342	3.275128
522.139470	3618.398626	17.108403	-0.099287	3.271654
522.169639	3610.345300	17.113408	-0.099288	3.268139
522.347776	3602.321975	17.118413	-0.099316	3.264639
522.548042	3594.398548	17.123418	-0.099348	3.261180
522.162234	3586.435073	17.128423	-0.099271	3.257676
522.315889	3578.430343	17.133427	-0.099295	3.254172
522.415530	3570.408617	17.138432	-0.099308	3.250655
521.846433	3562.506779	17.143437	-0.099197	3.247159
521.902459	3554.461078	17.148442	-0.099202	3.243622
521.878383	3546.516638	17.153447	-0.099193	3.240122
522.595076	3538.456909	17.158451	-0.099321	3.236599
522.338041	3530.468734	17.163456	-0.099268	3.233062
522.495821	3522.468065	17.168461	-0.099292	3.229534
522.146142	3514.541533	17.173466	-0.099222	3.226013
522.021931	3506.523613	17.178471	-0.099194	3.222457
521.863101	3498.561523	17.183475	-0.099159	3.218921
522.197852	3490.508017	17.188480	-0.099216	3.215361
522.188276	3482.507932	17.193485	-0.099209	3.211806
521.913705	3474.544751	17.198490	-0.099153	3.208253
521.634401	3466.601495	17.203495	-0.099096	3.204704
521.995789	3458.602419	17.208499	-0.099158	3.201154
521.697367	3450.612329	17.213504	-0.099097	3.197575
521.784547	3442.618062	17.218509	-0.099109	3.194008
521.698906	3434.628383	17.223514	-0.099087	3.190430
521.314249	3426.665383	17.228519	-0.099011	3.186848
521.627236	3418.647629	17.233523	-0.099064	3.183268
521.319261	3410.677286	17.238528	-0.099001	3.179677
521.454711	3402.709215	17.243533	-0.099022	3.176103
521.630735	3394.660781	17.248538	-0.099049	3.172491
521.442029	3386.671491	17.253543	-0.099009	3.168885
521.748937	3378.683878	17.258547	-0.099061	3.165297
521.365698	3370.749815	17.263552	-0.098984	3.161700
521.554980	3362.730925	17.268557	-0.099015	3.158085
521.808831	3354.722376	17.273562	-0.099057	3.154473
521.724008	3346.768576	17.278567	-0.099036	3.150867
521.470159	3338.813051	17.283571	-0.098983	3.147249
521.446558	3330.778090	17.288576	-0.098974	3.143600
521.342269	3322.831854	17.293581	-0.098949	3.139984
521.289881	3314.817677	17.298586	-0.098934	3.136336
521.214555	3306.830201	17.303591	-0.098915	3.132694
521.308227	3298.822242	17.308595	-0.098928	3.129046
520.894736	3290.878915	17.313600	-0.098845	3.125401
520.919488	3282.906074	17.318605	-0.098845	3.121757
520.748565	3274.925979	17.323610	-0.098808	3.118097
520.917465	3266.891987	17.328615	-0.098834	3.114424
521.121377	3258.899923	17.333619	-0.098867	3.110767
521.118775	3250.867967	17.338624	-0.098862	3.107078
521.093308	3242.917072	17.343629	-0.098852	3.103421
520.996789	3234.966477	17.348634	-0.098829	3.099757
521.171821	3226.947075	17.353639	-0.098856	3.096068
521.177803	3219.007703	17.358643	-0.098852	3.092405
521.121447	3210.974666	17.363648	-0.098836	3.088691
520.981625	3203.030645	17.368653	-0.098805	3.085010
521.002244	3195.056233	17.373658	-0.098804	3.081318
520.891299	3187.080592	17.378663	-0.098778	3.077615
520.921941	3179.086669	17.383667	-0.098779	3.073905
520.605995	3171.073494	17.388672	-0.098715	3.070166
520.843867	3163.064280	17.393677	-0.098754	3.066450
520.693928	3155.091865	17.398682	-0.098721	3.062728
520.728439	3147.085444	17.403687	-0.098722	3.058995
520.672967	3139.144175	17.408691	-0.098707	3.055283
520.493152	3131.159409	17.413696	-0.098668	3.051540
520.326067	3123.205203	17.418701	-0.098632	3.047808
520.455121	3115.163491	17.423706	-0.098651	3.044044
520.466635	3107.200403	17.428711	-0.098648	3.040307
520.359932	3099.255450	17.433715	-0.098623	3.036568
520.291709	3091.229452	17.438720	-0.098605	3.032789
520.439874	3083.236535	17.443725	-0.098628	3.029030
520.393833	3075.235472	17.448730	-0.098614	3.025254
520.081825	3067.324567	17.453735	-0.098551	3.021502
519.956688	3059.361747	17.458739	-0.098522	3.017731
520.212334	3051.259393	17.463744	-0.098565	3.013907
520.521311	3043.279357	17.468749	-0.098617	3.010139
520.459467	3035.302402	17.473754	-0.098600	3.006350
520.443061	3027.337285	17.478759	-0.098592	3.002564
520.082610	3019.434518	17.483763	-0.098520	2.998785
520.063660	3011.417802	17.488768	-0.098511	2.994964
519.929262	3003.481189	17.493773	-0.098481	2.991171
519.712882	2995.479220	17.498778	-0.098436	2.987337
519.615791	2987.482695	17.503783	-0.098413	2.983507
519.971672	2979.440100	17.508787	-0.098474	2.979674
519.744115	2971.502876	17.513792	-0.098426	2.975856
519.853101	2963.491007	17.518797	-0.098441	2.972015
520.067385	2955.484576	17.523802	-0.098476	2.968177
519.662271	2947.542974	17.528807	-0.098396	2.964332
519.285642	2939.666412	17.533811	-0.098321	2.960516
518.950233	2931.674858	17.538816	-0.098253	2.956641
519.507031	2923.579645	17.543821	-0.098351	2.952758
519.567265	2915.589421	17.548826	-0.098357	2.948895
519.174458	2907.649349	17.553831	-0.098279	2.945027
519.287111	2899.682742	17.558835	-0.098295	2.941167
519.337134	2891.675586	17.563840	-0.098299	2.937280
519.710201	2883.648104	17.568845	-0.098364	2.933394
519.578584	2875.665311	17.573850	-0.098334	2.929499
519.154440	2867.771420	17.578855	-0.098250	2.925626
519.486328	2859.757676	17.583859	-0.098307	2.921729
519.215917	2851.803670	17.588864	-0.098251	2.917825
519.382296	2843.801353	17.593869	-0.098277	2.913915
519.396900	2835.748874	17.598874	-0.098275	2.909967
519.105920	2827.788223	17.603879	-0.098215	2.906042
519.397635	2819.785166	17.608883	-0.098264	2.902122
519.588500	2811.778009	17.613888	-0.098295	2.898190
519.481641	2803.832526	17.618893	-0.098270	2.894267
519.322680	2795.877786	17.623898	-0.098235	2.890330
519.154190	2787.921151	17.628903	-0.098199	2.886387
519.035058	2779.949152	17.633907	-0.098171	2.882434
518.941461	2771.987176	17.638912	-0.098149	2.878481
519.264853	2763.975469	17.643917	-0.098204	2.874522
519.253052	2755.997321	17.648922	-0.098197	2.870555
519.235020	2747.987669	17.653927	-0.098188	2.866567
519.044376	2740.073145	17.658931	-0.098147	2.862611
518.989825	2732.063011	17.663936	-0.098132	2.858609
518.845290	2724.118640	17.668941	-0.098100	2.854629
518.757467	2716.138473	17.673946	-0.098079	2.850629
518.762782	2708.135306	17.678951	-0.098075	2.846618
518.504854	2700.207608	17.683955	-0.098021	2.842623
518.315395	2692.223801	17.688960	-0.097981	2.838598
518.534843	2684.194110	17.693965	-0.098017	2.834569
518.405050	2676.244199	17.698970	-0.097987	2.830553
518.708036	2668.179344	17.703975	-0.098039	2.826499
518.745955	2660.217454	17.708979	-0.098041	2.822476
518.727048	2652.233389	17.713984	-0.098032	2.818432
518.491114	2644.309207	17.718989	-0.097983	2.814400
518.154647	2636.380478	17.723994	-0.097915	2.810354
518.089473	2628.381645	17.728999	-0.097898	2.806283
518.384563	2620.372291	17.734003	-0.097948	2.802222
518.266165	2612.385087	17.739008	-0.097921	2.798141
518.176887	2604.431866	17.744013	-0.097899	2.794074
518.033267	2596.480138	17.749018	-0.097867	2.789998
518.007089	2588.477679	17.754023	-0.097857	2.785897
518.085340	2580.504607	17.759027	-0.097867	2.781812
517.954916	2572.540311	17.764032	-0.097837	2.777712
518.040291	2564.537674	17.769037	-0.097848	2.773600
517.918713	2556.560876	17.774042	-0.097820	2.769482
517.950956	2548.573676	17.779047	-0.097821	2.765363
518.189867	2540.612027	17.784051	-0.097860	2.761262
518.102207	2532.615639	17.789056	-0.097839	2.757118
518.288037	2524.609811	17.794061	-0.097868	2.752980
518.221627	2516.619954	17.799066	-0.097851	2.748828
518.090335	2508.649301	17.804071	-0.097821	2.744676
518.253443	2500.683356	17.809075	-0.097847	2.740538
518.054555	2492.743722	17.814080	-0.097804	2.736385
518.266466	2484.726660	17.819085	-0.097839	2.732211
517.828825	2476.826727	17.824090	-0.097752	2.728051
517.567019	2468.869231	17.829095	-0.097698	2.723865
517.780361	2460.877295	17.834099	-0.097733	2.719685
517.378673	2452.974884	17.839104	-0.097653	2.715507
517.252663	2444.977050	17.844109	-0.097625	2.711290
517.372150	2436.974011	17.849114	-0.097642	2.707078
517.466147	2428.948023	17.854119	-0.097654	2.702847
517.262008	2421.026596	17.859123	-0.097611	2.698645
517.530151	2412.976854	17.864128	-0.097656	2.694399
517.676827	2405.004934	17.869133	-0.097678	2.690179
517.485889	2397.069376	17.874138	-0.097637	2.685951
517.275595	2389.139981	17.879143	-0.097593	2.681718
517.558116	2381.143917	17.884147	-0.097640	2.677474
517.517130	2373.150720	17.889152	-0.097628	2.673205
517.236385	2365.214763	17.894157	-0.097570	2.668943
517.293220	2357.192683	17.899162	-0.097576	2.664651
517.495719	2349.199959	17.904167	-0.097608	2.660377
517.325398	2341.302283	17.909171	-0.097572	2.656122
517.209466	2333.299373	17.914176	-0.097545	2.651808
517.225690	2325.323088	17.919181	-0.097543	2.647510
517.183961	2317.362266	17.924186	-0.097530	2.643209
516.980447	2309.412189	17.929191	-0.097487	2.638896
516.908234	2301.493252	17.934195	-0.097468	2.634602
516.756923	2293.493569	17.939200	-0.097435	2.630252
516.752512	2285.499602	17.944205	-0.097429	2.625907
517.121133	2277.470222	17.949210	-0.097493	2.621562
516.892531	2269.546847	17.954215	-0.097445	2.617226
516.813878	2261.596911	17.959219	-0.097425	2.612879
516.691863	2253.595240	17.964224	-0.097397	2.608493
516.770028	2245.616793	17.969229	-0.097407	2.604126
516.742771	2237.668003	17.974234	-0.097397	2.599761
516.825093	2229.699259	17.979239	-0.097407	2.595385
516.572722	2221.695886	17.984243	-0.097355	2.590960
516.720303	2213.644998	17.989248	-0.097377	2.586528
516.575732	2205.725615	17.994253	-0.097345	2.582142
516.709443	2197.760429	17.999258	-0.097365	2.577741
516.584980	2189.799760	18.004263	-0.097336	2.573318
516.867373	2181.810338	18.009267	-0.097384	2.568900
516.732962	2173.832384	18.014272	-0.097354	2.564451
516.829966	2165.905563	18.019277	-0.097367	2.560039
516.586731	2157.986442	18.024282	-0.097316	2.555600
516.458812	2150.009937	18.029287	-0.097287	2.551129
516.597368	2142.022968	18.034291	-0.097308	2.546664
516.435597	2134.077440	18.039296	-0.097273	2.542192
516.425544	2126.123805	18.044301	-0.097266	2.537719
516.074407	2118.194665	18.049306	-0.097195	2.533227
516.270279	2110.179216	18.054311	-0.097227	2.528718
516.411999	2102.186275	18.059315	-0.097248	2.524210
516.071963	2094.289069	18.064320	-0.097180	2.519712
516.349018	2086.297769	18.069325	-0.097226	2.515199
516.490224	2078.301952	18.074330	-0.097247	2.510664
516.291967	2070.331773	18.079335	-0.097205	2.506112
516.345464	2062.379963	18.084339	-0.097210	2.501580
516.333101	2054.412584	18.089344	-0.097203	2.497025
515.990256	2046.494480	18.094349	-0.097134	2.492467
515.818733	2038.535890	18.099354	-0.097097	2.487889
515.543352	2030.594718	18.104359	-0.097040	2.483305
515.693176	2022.606685	18.109363	-0.097063	2.478718
515.761177	2014.612931	18.114368	-0.097071	2.474112
515.926779	2006.652821	18.119373	-0.097096	2.469525
515.728612	1998.701976	18.124378	-0.097054	2.464907
515.450398	1990.776650	18.129383	-0.096997	2.460289
515.341656	1982.845178	18.134387	-0.096972	2.455672
515.334418	1974.835772	18.139392	-0.096966	2.451008
515.049418	1966.918045	18.144397	-0.096907	2.446368
515.146137	1958.922710	18.149402	-0.096920	2.441703
515.033881	1950.992310	18.154407	-0.096894	2.437051
515.087137	1943.004703	18.159411	-0.096899	2.432369
514.737552	1935.036482	18.164416	-0.096829	2.427658
514.894328	1927.038176	18.169421	-0.096853	2.422959
514.991718	1919.061054	18.174426	-0.096866	2.418260
515.033859	1911.075071	18.179431	-0.096869	2.413542
515.062580	1903.121199	18.184435	-0.096869	2.408832
515.342153	1895.099180	18.189440	-0.096916	2.404093
515.180961	1887.212819	18.194445	-0.096881	2.399390
514.964437	1879.312001	18.199450	-0.096835	2.394664
514.901296	1871.346269	18.204455	-0.096819	2.389903
515.210418	1863.339676	18.209459	-0.096871	2.385138
515.021493	1855.412987	18.214464	-0.096831	2.380371
515.045732	1847.467093	18.219469	-0.096830	2.375600
515.116935	1839.501525	18.224474	-0.096838	2.370811
514.962755	1831.543129	18.229479	-0.096804	2.365999
514.812975	1823.644803	18.234483	-0.096772	2.361214
514.791658	1815.675650	18.239488	-0.096762	2.356386
514.723415	1807.715318	18.244493	-0.096745	2.351550
514.835806	1799.718652	18.249498	-0.096760	2.346697
514.953726	1791.744087	18.254503	-0.096777	2.341848
514.882260	1783.836520	18.259507	-0.096759	2.337014
514.631881	1775.892532	18.264512	-0.096707	2.332132
514.676766	1767.916353	18.269517	-0.096710	2.327246
514.575092	1759.986323	18.274522	-0.096686	2.322365
514.566412	1752.029639	18.279527	-0.096680	2.317465
514.413698	1744.101447	18.284531	-0.096646	2.312560
514.266528	1736.146029	18.289536	-0.096614	2.307628
514.244548	1728.201808	18.294541	-0.096604	2.302704
514.229949	1720.244439	18.299546	-0.096597	2.297761
514.363677	1712.244391	18.304551	-0.096616	2.292794
514.411778	1704.292405	18.309555	-0.096620	2.287838
514.287989	1696.363417	18.314560	-0.096592	2.282872
514.314316	1688.434945	18.319565	-0.096592	2.277908
514.249749	1680.487152	18.324570	-0.096575	2.272912
513.729950	1672.557397	18.329575	-0.096473	2.267878
513.592927	1664.622273	18.334579	-0.096442	2.262862
513.632927	1656.634272	18.339584	-0.096445	2.257818
513.677905	1648.676435	18.344589	-0.096448	2.252781
513.742468	1640.691856	18.349594	-0.096455	2.247718
513.602356	1632.770746	18.354599	-0.096424	2.242666
513.952973	1624.795165	18.359603	-0.096484	2.237612
513.978661	1616.839738	18.364608	-0.096483	2.232529
513.631935	1608.937660	18.369613	-0.096414	2.227436
513.682389	1600.972039	18.374618	-0.096418	2.222327
513.327252	1593.092955	18.379623	-0.096347	2.217224
513.458901	1585.118148	18.384627	-0.096366	2.212092
513.364442	1577.162799	18.389632	-0.096344	2.206940
513.674766	1569.172445	18.394637	-0.096396	2.201790
513.772185	1561.231655	18.399642	-0.096409	2.196641
513.537805	1553.327469	18.404647	-0.096361	2.191474
513.485437	1545.397601	18.409651	-0.096346	2.186294
513.146592	1537.489383	18.414656	-0.096278	2.181089
513.183104	1529.525192	18.419661	-0.096279	2.175870
513.217008	1521.557429	18.424666	-0.096281	2.170636
513.106616	1513.618557	18.429671	-0.096255	2.165394
512.971398	1505.721402	18.434675	-0.096225	2.160165
513.155569	1497.725674	18.439680	-0.096254	2.154889
512.979554	1489.823085	18.444685	-0.096216	2.149627
512.955158	1481.865474	18.449690	-0.096206	2.144330
512.784320	1473.965634	18.454695	-0.096169	2.139044
513.079467	1465.984790	18.459699	-0.096219	2.133736
513.004926	1458.042421	18.464704	-0.096200	2.128404
512.751620	1450.156455	18.469709	-0.096148	2.123080
512.748576	1442.235997	18.474714	-0.096142	2.117744
512.554584	1434.289942	18.479719	-0.096101	2.112358
512.332016	1426.364274	18.484723	-0.096055	2.106969
512.539432	1418.359220	18.489728	-0.096088	2.101555
512.629041	1410.419215	18.494733	-0.096100	2.096160
512.570227	1402.489625	18.499738	-0.096084	2.090743
512.382009	1394.570290	18.504743	-0.096044	2.085306
512.495264	1386.641172	18.509747	-0.096060	2.079878
512.312702	1378.737761	18.514752	-0.096020	2.074424
512.299919	1370.800585	18.519757	-0.096013	2.068949
512.234893	1362.879201	18.524762	-0.095996	2.063466
512.148238	1354.954638	18.529767	-0.095975	2.057963
512.098602	1347.037579	18.534771	-0.095960	2.052455
511.922320	1339.106279	18.539776	-0.095922	2.046909
512.118212	1331.160100	18.544781	-0.095954	2.041376
511.880037	1323.277458	18.549786	-0.095904	2.035827
511.753405	1315.337450	18.554791	-0.095876	2.030234
512.133240	1307.337479	18.559795	-0.095941	2.024637
511.951892	1299.446525	18.564800	-0.095902	2.019042
511.793630	1291.546641	18.569805	-0.095868	2.013428
511.515804	1283.660080	18.574810	-0.095811	2.007795
511.601420	1275.693300	18.579815	-0.095822	2.002127
511.538145	1267.810609	18.584819	-0.095805	1.996488
511.090615	1259.936739	18.589824	-0.095717	1.990798
511.434787	1251.916262	18.594829	-0.095776	1.985071
511.600585	1243.990238	18.599834	-0.095801	1.979376
511.046372	1236.162147	18.604839	-0.095693	1.973658
511.454344	1228.161969	18.609843	-0.095764	1.967902
511.264945	1220.265998	18.614848	-0.095724	1.962141
510.979587	1212.405606	18.619853	-0.095666	1.956378
511.107469	1204.458961	18.624858	-0.095684	1.950581
510.789834	1196.553961	18.629863	-0.095620	1.944747
510.780083	1188.648776	18.634867	-0.095613	1.938930
510.566889	1180.724477	18.639872	-0.095568	1.933058
510.639658	1172.775739	18.644877	-0.095577	1.927182
510.948858	1164.806787	18.649882	-0.095629	1.921300
510.712844	1156.935495	18.654887	-0.095580	1.915412
510.864295	1149.006677	18.659891	-0.095603	1.909506
510.929079	1141.063594	18.664896	-0.095610	1.903561
510.698923	1133.210171	18.669901	-0.095562	1.897631
510.564635	1125.316851	18.674906	-0.095532	1.891663
510.714502	1117.361545	18.679911	-0.095555	1.885663
510.818709	1109.472453	18.684915	-0.095570	1.879688
510.766177	1101.574528	18.689920	-0.095555	1.873669
510.461147	1093.705917	18.694925	-0.095493	1.867624
510.389764	1085.804249	18.699930	-0.095474	1.861561
510.100875	1077.934735	18.704935	-0.095416	1.855477
509.954797	1070.041843	18.709939	-0.095383	1.849373
509.894403	1062.114607	18.714944	-0.095367	1.843231
509.769942	1054.243134	18.719949	-0.095339	1.837104
509.643366	1046.362106	18.724954	-0.095310	1.830950
509.724807	1038.405381	18.729959	-0.095320	1.824740
509.616555	1030.558770	18.734963	-0.095295	1.818573
509.821826	1022.582425	18.739968	-0.095328	1.812320
509.555201	1014.729143	18.744973	-0.095273	1.806086
509.487488	1006.857194	18.749978	-0.095256	1.799839
509.299966	998.993567	18.754983	-0.095216	1.793563
509.267062	991.056432	18.759987	-0.095205	1.787225
509.214929	983.149067	18.764992	-0.095190	1.780885
508.921565	975.315781	18.769997	-0.095130	1.774553
508.856739	967.412054	18.775002	-0.095113	1.768170
509.203692	959.450235	18.780007	-0.095173	1.761768
508.902105	951.645823	18.785011	-0.095111	1.755389
508.768712	943.751582	18.790016	-0.095082	1.748934
508.628435	935.892779	18.795021	-0.095050	1.742484
508.538342	928.022469	18.800026	-0.095029	1.736007
508.601579	920.102298	18.805031	-0.095035	1.729484
508.297417	912.285133	18.810035	-0.094974	1.722974
508.162832	904.416848	18.815040	-0.094943	1.716419
507.768729	896.592731	18.820045	-0.094865	1.709841
507.653705	888.704556	18.825050	-0.094839	1.703222
507.966906	880.745296	18.830055	-0.094892	1.696573
507.732049	872.902881	18.835059	-0.094843	1.689924
507.456947	865.061293	18.840064	-0.094787	1.683243
507.173532	857.244678	18.845069	-0.094729	1.676557
507.552538	849.286921	18.850074	-0.094794	1.669812
507.419525	841.418870	18.855079	-0.094765	1.663047
507.417917	833.567044	18.860083	-0.094759	1.656287
507.116711	825.728668	18.865088	-0.094698	1.649470
506.921665	817.904025	18.870093	-0.094657	1.642650
506.876957	810.045988	18.875098	-0.094643	1.635794
506.393301	802.223850	18.880103	-0.094548	1.628879
506.836102	794.258065	18.885107	-0.094626	1.621939
506.505339	786.436150	18.890112	-0.094559	1.614986
506.476410	778.575839	18.895117	-0.094549	1.608012
506.607678	770.694796	18.900122	-0.094568	1.601012
506.288013	762.905961	18.905127	-0.094504	1.593999
505.929166	755.113611	18.910131	-0.094432	1.586946
505.996696	747.224429	18.915136	-0.094439	1.579836
505.694695	739.433394	18.920141	-0.094378	1.572729
505.406934	731.616183	18.925146	-0.094319	1.565568
505.070545	723.829745	18.930151	-0.094252	1.558395
505.489463	715.891095	18.935155	-0.094325	1.551161
505.245903	708.064731	18.940160	-0.094274	1.543897
504.722557	700.325046	18.945165	-0.094172	1.536638
504.173215	692.557181	18.950170	-0.094065	1.529314
503.835618	684.741716	18.955175	-0.093997	1.521941
504.121821	676.846325	18.960179	-0.094045	1.514554
503.412468	669.105949	18.965184	-0.093908	1.507123
502.734358	661.376779	18.970189	-0.093777	1.499671
502.401571	653.564059	18.975194	-0.093710	1.492155
501.909261	645.774487	18.980199	-0.093613	1.484598
501.338495	638.034873	18.985203	-0.093502	1.477038
500.961327	630.177856	18.990208	-0.093427	1.469356
500.990232	622.276052	18.995213	-0.093427	1.461655
500.010756	614.615856	19.000218	-0.093240	1.453987
499.243916	606.862941	19.005223	-0.093092	1.446222
499.207408	599.012403	19.010227	-0.093080	1.438436
498.783587	591.220764	19.015232	-0.092996	1.430604
498.375920	583.439714	19.020237	-0.092915	1.422741
497.455292	575.762737	19.025242	-0.092739	1.414854
497.060784	567.949641	19.030247	-0.092660	1.406873
496.645149	560.184627	19.035251	-0.092578	1.398891
495.865161	552.460620	19.040256	-0.092428	1.390843
495.207198	544.723428	19.045261	-0.092300	1.382756
494.545660	536.990065	19.050266	-0.092172	1.374624
493.984043	529.226284	19.055271	-0.092063	1.366429
493.077391	521.553193	19.060275	-0.091889	1.358219
492.507742	513.794061	19.065280	-0.091778	1.349928
492.048494	506.019222	19.070285	-0.091687	1.341588
491.609859	498.268664	19.075290	-0.091601	1.333225
490.919944	490.543649	19.080295	-0.091467	1.324791
490.389404	482.838247	19.085299	-0.091364	1.316354
489.732721	475.035041	19.090304	-0.091236	1.307731
489.060966	467.316281	19.095309	-0.091106	1.299142
488.628939	459.593810	19.100314	-0.091021	1.290535
487.852381	451.922689	19.105319	-0.090871	1.281863
487.099357	444.264359	19.110323	-0.090726	1.273150
486.511084	436.556552	19.115328	-0.090612	1.264353
486.024421	428.845279	19.120333	-0.090516	1.255509
485.423192	421.171486	19.125338	-0.090399	1.246623
484.893451	413.477121	19.130343	-0.090296	1.237663
484.032873	405.859040	19.135347	-0.090131	1.228661
483.398062	398.183914	19.140352	-0.090008	1.219571
483.063593	390.477692	19.145357	-0.089940	1.210435
482.103803	382.896977	19.150362	-0.089757	1.201252
481.681702	375.212634	19.155367	-0.089673	1.191984
481.274224	367.542269	19.160371	-0.089592	1.182663
480.703166	359.901149	19.165376	-0.089481	1.173269
480.452340	352.219614	19.170381	-0.089430	1.163817
479.971105	344.604137	19.175386	-0.089335	1.154320
478.903557	337.061939	19.180391	-0.089131	1.144710
478.680371	329.402552	19.185395	-0.089085	1.135053
478.030189	321.807865	19.190400	-0.088959	1.125303
477.459346	314.239849	19.195405	-0.088848	1.115518
476.543851	306.728271	19.200410	-0.088673	1.105643
476.559899	299.041639	19.205415	-0.088671	1.095659
475.961667	291.514504	19.210419	-0.088554	1.085654
475.375932	283.979829	19.215424	-0.088441	1.075548
474.921647	276.419230	19.220429	-0.088351	1.065342
474.989056	268.789068	19.225434	-0.088359	1.055066
474.318648	261.299274	19.230439	-0.088229	1.044705
473.740763	253.827033	19.235443	-0.088117	1.034286
473.354338	246.309333	19.240448	-0.088040	1.023745
472.712701	238.863196	19.245453	-0.087916	1.013131
472.137588	231.422340	19.250458	-0.087804	1.002429
471.137571	224.062026	19.255463	-0.087613	0.991621
470.576166	216.612188	19.260467	-0.087504	0.980674
469.670401	209.239568	19.265472	-0.087330	0.969628
469.669631	201.717374	19.270477	-0.087325	0.958467
469.360451	194.285818	19.275482	-0.087263	0.947230
468.572092	186.962560	19.280487	-0.087111	0.935896
468.237154	179.570092	19.285491	-0.087044	0.924438
467.561020	172.263992	19.290496	-0.086914	0.912877
467.099358	164.924758	19.295501	-0.086823	0.901175
466.286435	157.673299	19.300506	-0.086667	0.889360
466.174201	150.305401	19.305511	-0.086642	0.877397
465.948450	143.004946	19.310515	-0.086595	0.865347
465.178215	135.817786	19.315520	-0.086447	0.853156
464.791005	128.584340	19.320525	-0.086370	0.840823
464.126836	121.422760	19.325530	-0.086242	0.828347
463.441088	114.273909	19.330535	-0.086110	0.815695
463.064696	107.108224	19.335539	-0.086035	0.802910
462.529112	100.005350	19.340544	-0.085931	0.789982
461.862881	92.954135	19.345549	-0.085802	0.776890
461.603085	85.859512	19.350554	-0.085749	0.763627
460.787488	78.907843	19.355559	-0.085593	0.750213
460.553384	72.062827	19.360563	-0.085545	0.736963