Fri Apr 16 19:35:20 2021

Number of Points = 3641
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.563152	0.029761	0.000000	-0.000039	0.313890

1.381912	-0.002682	0.005005	-0.000005	0.313589
1.211963	0.028310	0.010010	0.000026	0.313590
1.263908	0.016136	0.015014	0.000017	0.313577
1.505690	-0.027040	0.020019	-0.000028	0.313581
1.194164	0.030623	0.025024	0.000030	0.313586
1.329057	0.003993	0.030029	0.000004	0.313577
1.484974	-0.022442	0.035034	-0.000025	0.313586
1.341422	0.002586	0.040038	0.000002	0.313581
1.032263	0.061151	0.045043	0.000060	0.313592
1.260911	0.018725	0.050048	0.000017	0.313588
1.130925	0.042930	0.055053	0.000041	0.313591
1.265242	0.018181	0.060058	0.000016	0.313590
1.088012	0.048778	0.065062	0.000049	0.313583
1.491923	-0.024536	0.070067	-0.000026	0.313583
1.128629	0.042387	0.075072	0.000041	0.313588
1.065323	0.014702	0.080077	0.000053	0.313407
1.173325	-0.032682	0.085082	0.000033	0.313279
1.213405	-0.043737	0.090086	0.000025	0.313262
0.888054	0.019217	0.095091	0.000086	0.313280
0.984504	0.001255	0.100096	0.000068	0.313278
1.133051	-0.028445	0.105101	0.000040	0.313266
1.099447	-0.020508	0.110106	0.000046	0.313275
1.025376	-0.043352	0.115110	0.000060	0.313107
1.545189	-0.167278	0.120115	-0.000037	0.312971
1.622375	-0.183003	0.125120	-0.000051	0.312964
1.243034	-0.114014	0.130125	0.000020	0.312964
1.600294	-0.178521	0.135130	-0.000047	0.312966
1.616444	-0.250080	0.140134	-0.000050	0.312649
1.428774	-0.221364	0.145139	-0.000015	0.312625
1.567017	-0.246741	0.150144	-0.000041	0.312624
1.567408	-0.248968	0.155149	-0.000041	0.312614
1.475602	-0.296410	0.160154	-0.000024	0.312317
1.273229	-0.260606	0.165158	0.000014	0.312313
1.706197	-0.338566	0.170163	-0.000067	0.312317
1.325882	-0.302000	0.175168	0.000004	0.312166
0.983112	-0.277322	0.180173	0.000067	0.311992
1.080862	-0.292309	0.185178	0.000049	0.312005
1.355032	-0.346988	0.190182	-0.000002	0.311983
1.291756	-0.394384	0.195187	0.000010	0.311710
1.275551	-0.392972	0.200192	0.000013	0.311703
1.265168	-0.391477	0.205197	0.000015	0.311701
1.287281	-0.462209	0.210202	0.000011	0.311392
1.105948	-0.434465	0.215206	0.000044	0.311368
1.390460	-0.491049	0.220211	-0.000009	0.311345
1.348294	-0.544328	0.225216	-0.000001	0.311062
1.409821	-0.556485	0.230221	-0.000012	0.311058
1.531710	-0.606434	0.235226	-0.000035	0.310929
1.561812	-0.652253	0.240230	-0.000041	0.310741
1.278555	-0.598600	0.245235	0.000012	0.310752
1.297698	-0.655192	0.250240	0.000008	0.310505
1.420141	-0.679776	0.255245	-0.000014	0.310494
1.480319	-0.733247	0.260250	-0.000026	0.310296
1.255315	-0.724926	0.265254	0.000016	0.310144
1.145809	-0.720960	0.270259	0.000037	0.310070
1.267201	-0.791755	0.275264	0.000014	0.309843
1.186361	-0.779952	0.280269	0.000029	0.309830
1.017419	-0.815596	0.285274	0.000060	0.309520
0.993749	-0.812812	0.290278	0.000065	0.309513
0.780808	-0.820861	0.295283	0.000104	0.309295
0.759685	-0.829188	0.300288	0.000108	0.309238
0.939976	-0.908694	0.305293	0.000075	0.309020
0.804567	-0.908814	0.310298	0.000100	0.308904
0.774284	-0.940230	0.315302	0.000105	0.308732
1.065092	-1.025162	0.320307	0.000051	0.308582
0.880898	-1.024366	0.325312	0.000085	0.308429
0.827615	-1.050773	0.330317	0.000095	0.308259
0.632836	-1.045691	0.335322	0.000132	0.308117
0.527303	-1.056030	0.340326	0.000151	0.307979
0.661876	-1.120228	0.345331	0.000126	0.307793
0.651179	-1.152382	0.350336	0.000128	0.307633
0.808003	-1.226388	0.355341	0.000099	0.307419
1.114371	-1.303427	0.360346	0.000042	0.307318
0.841856	-1.317509	0.365350	0.000093	0.307019
0.597179	-1.283517	0.370355	0.000138	0.306970
0.757245	-1.366777	0.375360	0.000108	0.306715
0.748357	-1.393710	0.380365	0.000110	0.306580
0.822513	-1.451223	0.385370	0.000096	0.306373
0.770521	-1.489046	0.390374	0.000106	0.306150
0.880907	-1.532828	0.395379	0.000085	0.306038
0.445629	-1.513480	0.400384	0.000166	0.305755
0.635403	-1.572098	0.405389	0.000131	0.305641
0.490249	-1.574180	0.410394	0.000158	0.305507
0.446523	-1.627291	0.415398	0.000166	0.305218
0.733419	-1.709930	0.420403	0.000112	0.305074
0.582367	-1.733594	0.425408	0.000140	0.304831
0.424671	-1.752687	0.430413	0.000170	0.304605
0.326292	-1.763392	0.435418	0.000188	0.304469
0.525197	-1.854378	0.440422	0.000151	0.304209
0.697752	-1.930026	0.445427	0.000119	0.303998
0.595194	-1.948341	0.450432	0.000138	0.303823
0.550798	-1.995205	0.455437	0.000146	0.303561
0.361503	-2.007525	0.460442	0.000181	0.303339
-0.032948	-1.972054	0.465446	0.000255	0.303166
-0.165535	-1.990531	0.470451	0.000279	0.302963
0.060811	-2.088446	0.475456	0.000237	0.302692
0.110725	-2.139649	0.480461	0.000228	0.302491
0.073847	-2.173206	0.485466	0.000235	0.302299
-0.059447	-2.216107	0.490470	0.000260	0.301978
-0.141576	-2.234533	0.495475	0.000275	0.301818
-0.075161	-2.286482	0.500480	0.000262	0.301627
-0.482499	-2.270819	0.505485	0.000338	0.301347
-0.684785	-2.280268	0.510490	0.000376	0.301126
-1.156407	-2.232476	0.515494	0.000464	0.300944
-1.447633	-2.224372	0.520499	0.000518	0.300728
-1.791939	-2.202682	0.525504	0.000582	0.300532
-2.194115	-2.157088	0.530509	0.000657	0.300400
-2.108563	-2.223621	0.535514	0.000641	0.300154
-2.344348	-2.232188	0.540518	0.000685	0.299907
-2.642240	-2.205697	0.545523	0.000740	0.299774
-2.861090	-2.220890	0.550528	0.000781	0.299508
-2.812373	-2.268718	0.555533	0.000772	0.299320
-3.306391	-2.199713	0.560538	0.000863	0.299220
-3.594249	-2.220028	0.565542	0.000917	0.298869
-3.786172	-2.204032	0.570547	0.000953	0.298778
-4.361373	-2.142008	0.575552	0.001060	0.298572
-4.345242	-2.187590	0.580557	0.001057	0.298366
-4.253835	-2.228086	0.585562	0.001040	0.298250
-4.579138	-2.225667	0.590566	0.001100	0.297975
-4.478367	-2.263572	0.595571	0.001081	0.297880
-5.157811	-2.192330	0.600576	0.001208	0.297626
-5.147373	-2.226368	0.605581	0.001206	0.297470
-5.567791	-2.184095	0.610586	0.001284	0.297305
-5.601198	-2.223163	0.615590	0.001290	0.297085
-5.926036	-2.185106	0.620595	0.001351	0.296983
-6.131691	-2.195852	0.625600	0.001389	0.296749
-6.363439	-2.167656	0.630605	0.001432	0.296681
-6.286518	-2.244018	0.635610	0.001418	0.296377
-6.658784	-2.186740	0.640614	0.001487	0.296327
-7.061171	-2.170576	0.645619	0.001562	0.296049
-7.065933	-2.176928	0.650624	0.001562	0.296014
-7.429546	-2.168649	0.655629	0.001630	0.295731
-7.512366	-2.159848	0.660634	0.001645	0.295701
-7.741520	-2.163463	0.665638	0.001688	0.295479
-7.475013	-2.223445	0.670643	0.001638	0.295423
-8.066070	-2.172948	0.675648	0.001748	0.295144
-8.084534	-2.182991	0.680653	0.001752	0.295079
-8.281601	-2.198079	0.685658	0.001788	0.294829
-8.400335	-2.188678	0.690662	0.001811	0.294770
-8.837101	-2.165020	0.695667	0.001892	0.294496
-8.764587	-2.183601	0.700672	0.001878	0.294470
-8.886812	-2.215451	0.705677	0.001901	0.294205
-8.951431	-2.204924	0.710682	0.001913	0.294199
-9.542258	-2.163905	0.715686	0.002023	0.293872
-9.339286	-2.200296	0.720691	0.001985	0.293875
-9.589837	-2.213532	0.725696	0.002032	0.293586
-10.061046	-2.134050	0.730701	0.002119	0.293556
-10.111945	-2.171603	0.735706	0.002129	0.293325
-10.307990	-2.153092	0.740710	0.002165	0.293241
-10.316479	-2.185478	0.745715	0.002167	0.293074
-10.451474	-2.185808	0.750720	0.002192	0.292951
-10.393593	-2.225005	0.755725	0.002181	0.292810
-10.814585	-2.186936	0.760730	0.002259	0.292620
-11.220473	-2.126974	0.765734	0.002335	0.292552
-11.202126	-2.180674	0.770739	0.002331	0.292303
-11.174007	-2.185730	0.775744	0.002326	0.292303
-11.684705	-2.156486	0.780749	0.002421	0.291989
-11.759939	-2.144476	0.785754	0.002435	0.291981
-11.911256	-2.154234	0.790758	0.002463	0.291796
-12.144777	-2.133866	0.795763	0.002507	0.291687
-12.137025	-2.152681	0.800768	0.002505	0.291601
-12.523008	-2.132160	0.805773	0.002577	0.291355
-12.603524	-2.115364	0.810778	0.002592	0.291366
-13.050627	-2.089571	0.815782	0.002675	0.291090
-13.074024	-2.089844	0.820787	0.002679	0.291068
-13.000786	-2.130180	0.825792	0.002666	0.290934
-13.687327	-2.044858	0.830797	0.002793	0.290738
-13.370183	-2.101753	0.835802	0.002734	0.290742
-13.145548	-2.191635	0.840806	0.002692	0.290498
-13.711707	-2.091511	0.845811	0.002798	0.290484
-13.936511	-2.080456	0.850816	0.002840	0.290336
-14.331014	-2.047058	0.855821	0.002913	0.290145
-13.693159	-2.163206	0.860826	0.002794	0.290144
-14.789880	-2.023854	0.865830	0.002998	0.289845
-14.874170	-2.008633	0.870835	0.003014	0.289845
-14.826760	-2.035121	0.875840	0.003005	0.289756
-15.090132	-2.039472	0.880845	0.003054	0.289495
-14.962634	-2.060141	0.885850	0.003030	0.289508
-15.296257	-2.036645	0.890854	0.003092	0.289322
-15.223078	-2.071411	0.895859	0.003079	0.289215
-15.233253	-2.071263	0.900864	0.003081	0.289207
-15.635080	-2.065524	0.905869	0.003155	0.288870
-15.783105	-2.035223	0.910874	0.003183	0.288887
-16.018813	-2.014980	0.915878	0.003227	0.288774
-15.957818	-2.067842	0.920883	0.003215	0.288565
-15.891684	-2.078819	0.925888	0.003203	0.288571
-16.386099	-2.036560	0.930893	0.003295	0.288332
-16.754071	-1.986201	0.935898	0.003363	0.288249
-16.666081	-2.002629	0.940902	0.003347	0.288247
-16.708986	-2.046987	0.945907	0.003355	0.287986
-17.015004	-1.996791	0.950912	0.003412	0.287958
-16.700831	-2.071522	0.955917	0.003353	0.287870
-16.562460	-2.146540	0.960922	0.003327	0.287620
-16.965225	-2.076756	0.965926	0.003402	0.287603
-17.253507	-2.065896	0.970931	0.003456	0.287394
-17.224691	-2.090211	0.975936	0.003451	0.287298
-17.315271	-2.080144	0.980941	0.003467	0.287266
-17.718666	-2.064381	0.985946	0.003542	0.286976
-18.149248	-1.984934	0.990950	0.003622	0.286982
-17.917185	-2.045031	0.995955	0.003579	0.286892
-18.330897	-2.010011	1.000960	0.003656	0.286689
-18.656418	-1.949302	1.005965	0.003717	0.286697
-18.220703	-2.059715	1.010970	0.003636	0.286540
-18.628073	-2.023559	1.015974	0.003711	0.286349
-18.610554	-2.025707	1.020979	0.003708	0.286354
-18.606995	-2.074174	1.025984	0.003707	0.286113
-19.262110	-1.968688	1.030989	0.003829	0.286044
-19.331489	-1.952822	1.035994	0.003842	0.286061
-19.520430	-1.980223	1.040998	0.003877	0.285749
-19.509791	-1.983619	1.046003	0.003875	0.285741
-19.719501	-1.949354	1.051008	0.003914	0.285722
-19.988684	-1.947674	1.056013	0.003964	0.285483
-19.556522	-2.023859	1.061018	0.003884	0.285495
-19.999915	-1.961089	1.066022	0.003966	0.285405
-20.467804	-1.926590	1.071027	0.004053	0.285149
-20.147131	-1.985104	1.076032	0.003994	0.285148
-19.966022	-2.045834	1.081037	0.003960	0.285007
-20.409580	-2.001528	1.086042	0.004042	0.284823
-20.792154	-1.931410	1.091046	0.004113	0.284826
-20.735277	-1.975305	1.096051	0.004103	0.284655
-21.007084	-1.955932	1.101056	0.004153	0.284503
-20.988102	-1.960907	1.106061	0.004150	0.284495
-21.202414	-1.958896	1.111066	0.004190	0.284308
-21.605045	-1.904993	1.116070	0.004265	0.284210
-21.617387	-1.899578	1.121075	0.004267	0.284226
-21.474059	-1.972467	1.126080	0.004240	0.283988
-21.805092	-1.934796	1.131085	0.004302	0.283873
-21.662824	-1.959375	1.136090	0.004275	0.283880
-21.605269	-2.026851	1.141094	0.004264	0.283589
-21.720776	-2.011303	1.146099	0.004286	0.283562
-21.817934	-2.006032	1.151104	0.004304	0.283499
-22.090687	-2.009943	1.156109	0.004355	0.283226
-21.648462	-2.088792	1.161114	0.004272	0.283234
-21.747213	-2.105497	1.166118	0.004291	0.283057
-22.285118	-2.031309	1.171123	0.004391	0.282937
-22.141440	-2.056438	1.176128	0.004364	0.282942
-22.202709	-2.112160	1.181133	0.004375	0.282600
-22.603828	-2.037483	1.186138	0.004450	0.282609
-22.834959	-2.020728	1.191142	0.004493	0.282480
-22.925627	-2.041541	1.196147	0.004510	0.282289
-22.916247	-2.042712	1.201152	0.004508	0.282292
-23.414446	-1.999049	1.206157	0.004601	0.282052
-23.415719	-2.014231	1.211162	0.004601	0.281973
-23.393217	-2.019944	1.216166	0.004597	0.281965
-23.615291	-2.034641	1.221171	0.004638	0.281682
-23.677535	-2.023456	1.226176	0.004649	0.281682
-23.929706	-1.996372	1.231181	0.004696	0.281585
-24.019743	-2.025457	1.236186	0.004713	0.281352
-24.131421	-2.007300	1.241190	0.004734	0.281341
-23.934207	-2.077411	1.246195	0.004697	0.281165
-24.518870	-1.995478	1.251200	0.004806	0.281040
-24.678606	-1.966944	1.256205	0.004835	0.281038
-24.338050	-2.079339	1.261210	0.004772	0.280778
-24.967279	-1.975973	1.266214	0.004889	0.280721
-24.849359	-2.005241	1.271219	0.004867	0.280681
-25.072091	-2.000342	1.276224	0.004908	0.280498
-25.060432	-2.003417	1.281229	0.004906	0.280493
-25.499748	-1.949144	1.286234	0.004988	0.280361
-25.750426	-1.944708	1.291238	0.005035	0.280149
-25.709154	-1.950142	1.296243	0.005027	0.280160
-25.815470	-1.965110	1.301248	0.005047	0.279983
-26.189210	-1.926194	1.306253	0.005116	0.279833
-25.550572	-2.041723	1.311258	0.004997	0.279836
-25.867207	-2.036341	1.316262	0.005056	0.279566
-26.255960	-1.978386	1.321267	0.005128	0.279501
-25.951892	-2.042106	1.326272	0.005072	0.279457
-26.052651	-2.072884	1.331277	0.005091	0.279203
-26.213386	-2.041533	1.336282	0.005120	0.279214
-26.722238	-1.983851	1.341286	0.005215	0.279034
-27.121256	-1.938396	1.346291	0.005289	0.278893
-26.692212	-2.018148	1.351296	0.005209	0.278885
-27.441721	-1.928889	1.356301	0.005349	0.278641
-27.846363	-1.863680	1.361306	0.005424	0.278597
-27.770614	-1.878459	1.366310	0.005410	0.278593
-27.880295	-1.906909	1.371315	0.005430	0.278341
-28.502191	-1.804724	1.376320	0.005546	0.278285
-27.976922	-1.904615	1.381325	0.005448	0.278262
-27.611003	-2.012090	1.386330	0.005380	0.278049
-28.029726	-1.954518	1.391334	0.005458	0.277953
-28.153063	-1.930512	1.396339	0.005481	0.277962
-27.941482	-2.033536	1.401344	0.005441	0.277625
-28.449761	-1.943140	1.406349	0.005536	0.277615
-28.142068	-2.016810	1.411354	0.005479	0.277523
-28.551118	-1.983507	1.416358	0.005555	0.277309
-28.488413	-1.995376	1.421363	0.005543	0.277307
-28.533070	-2.027505	1.426368	0.005551	0.277097
-28.745318	-2.010800	1.431373	0.005591	0.276983
-28.763206	-2.009585	1.436378	0.005594	0.276972
-29.140288	-1.996290	1.441382	0.005664	0.276683
-28.957362	-2.028007	1.446387	0.005630	0.276692
-28.663779	-2.108730	1.451392	0.005575	0.276549
-29.452264	-2.002947	1.456397	0.005722	0.276352
-29.307821	-2.027515	1.461402	0.005695	0.276362
-29.522144	-2.041123	1.466406	0.005735	0.276086
-29.780197	-2.001072	1.471411	0.005783	0.276050
-29.880364	-1.995006	1.476416	0.005802	0.275987
-30.344190	-1.957513	1.481421	0.005888	0.275741
-29.917665	-2.034006	1.486426	0.005809	0.275747
-30.226727	-2.004914	1.491430	0.005866	0.275605
-30.471255	-1.981652	1.496435	0.005911	0.275494
-30.078718	-2.051829	1.501440	0.005838	0.275501
-30.776450	-1.989556	1.506445	0.005968	0.275161
-30.946053	-1.958197	1.511450	0.006000	0.275164
-30.903507	-1.983380	1.516454	0.005992	0.275073
-31.266335	-1.959591	1.521459	0.006059	0.274851
-31.160742	-1.979549	1.526464	0.006040	0.274847
-31.331891	-1.985361	1.531469	0.006071	0.274653
-31.255414	-2.024818	1.536474	0.006057	0.274518
-31.714207	-1.941202	1.541478	0.006142	0.274519
-31.816483	-1.970732	1.546483	0.006161	0.274266
-31.897718	-1.962080	1.551488	0.006176	0.274234
-32.160818	-1.924680	1.556493	0.006225	0.274179
-32.205752	-1.971174	1.561498	0.006234	0.273890
-32.052509	-2.000634	1.566502	0.006205	0.273882
-31.984133	-2.042195	1.571507	0.006192	0.273728
-32.846545	-1.913296	1.576512	0.006353	0.273581
-32.897757	-1.904765	1.581517	0.006362	0.273577
-32.645744	-1.991060	1.586522	0.006315	0.273363
-33.029516	-1.941738	1.591526	0.006387	0.273255
-32.941164	-1.958892	1.596531	0.006370	0.273249
-33.070728	-1.987698	1.601536	0.006394	0.272972
-32.917584	-2.018982	1.606541	0.006366	0.272954
-33.073837	-2.014260	1.611546	0.006395	0.272829
-33.714951	-1.936197	1.616550	0.006514	0.272624
-33.537286	-1.967238	1.621555	0.006481	0.272631
-33.851829	-1.949552	1.626560	0.006540	0.272422
-34.554128	-1.840026	1.631565	0.006670	0.272325
-33.625013	-2.010426	1.636570	0.006497	0.272318
-34.460571	-1.915353	1.641574	0.006653	0.272016
-34.601661	-1.894059	1.646579	0.006679	0.271993
-34.608421	-1.892969	1.651584	0.006680	0.271992
-34.629162	-1.942930	1.656589	0.006684	0.271706
-34.618776	-1.945201	1.661594	0.006682	0.271704
-35.081456	-1.879142	1.666598	0.006768	0.271608
-34.981303	-1.940928	1.671603	0.006749	0.271376
-35.084182	-1.923728	1.676608	0.006768	0.271368
-35.489299	-1.879852	1.681613	0.006844	0.271210
-35.056272	-1.985801	1.686618	0.006763	0.271065
-35.100940	-1.979317	1.691622	0.006771	0.271056
-35.715502	-1.917852	1.696627	0.006886	0.270788
-35.914443	-1.887782	1.701632	0.006923	0.270755
-35.557527	-1.960551	1.706637	0.006856	0.270713
-36.086411	-1.903775	1.711642	0.006955	0.270503
-36.362996	-1.853282	1.716646	0.007006	0.270504
-36.122045	-1.917369	1.721651	0.006961	0.270396
-36.808675	-1.834723	1.726656	0.007089	0.270170
-36.840524	-1.830249	1.731661	0.007095	0.270163
-35.954506	-2.021096	1.736666	0.006930	0.270004
-36.477147	-1.959142	1.741670	0.007027	0.269827
-36.331839	-1.985972	1.746675	0.007000	0.269825
-36.610441	-1.991646	1.751680	0.007052	0.269523
-37.008795	-1.922823	1.756685	0.007126	0.269503
-36.913826	-1.953801	1.761690	0.007108	0.269430
-37.127580	-1.955861	1.766694	0.007148	0.269210
-36.830313	-2.009473	1.771699	0.007093	0.269213
-37.156696	-1.996144	1.776704	0.007153	0.268966
-38.357616	-1.790666	1.781709	0.007377	0.268896
-37.552977	-1.938318	1.786714	0.007227	0.268889
-37.403887	-2.025773	1.791718	0.007199	0.268565
-37.988008	-1.917327	1.796723	0.007308	0.268577
-37.982161	-1.943781	1.801728	0.007307	0.268440
-38.177588	-1.944508	1.806733	0.007343	0.268245
-38.053586	-1.963568	1.811738	0.007320	0.268264
-38.386884	-1.946877	1.816742	0.007382	0.268027
-38.212341	-1.991654	1.821747	0.007349	0.267957
-38.314655	-1.984231	1.826752	0.007368	0.267896
-38.790993	-1.949489	1.831757	0.007457	0.267616
-39.106298	-1.886482	1.836762	0.007516	0.267647
-39.014313	-1.940254	1.841766	0.007498	0.267447
-39.375860	-1.899105	1.846771	0.007566	0.267314
-38.931986	-1.980966	1.851776	0.007483	0.267308
-39.003070	-2.026329	1.856781	0.007496	0.266992
-39.373437	-1.959468	1.861786	0.007565	0.266990
-39.792108	-1.903772	1.866790	0.007643	0.266879
-39.847912	-1.924658	1.871795	0.007653	0.266711
-39.881726	-1.918405	1.876800	0.007660	0.266712
-39.856380	-1.971595	1.881805	0.007655	0.266448
-39.859537	-1.987427	1.886810	0.007655	0.266359
-39.989083	-1.974617	1.891814	0.007679	0.266301
-40.114382	-1.998212	1.896819	0.007703	0.266049
-40.272857	-1.968778	1.901824	0.007732	0.266053
-40.258510	-2.011821	1.906829	0.007730	0.265833
-40.288949	-2.024920	1.911834	0.007735	0.265731
-40.712425	-1.956578	1.916838	0.007814	0.265684
-40.764320	-1.986703	1.921843	0.007824	0.265469
-40.567901	-2.022179	1.926848	0.007787	0.265471
-41.091100	-1.970985	1.931853	0.007884	0.265231
-40.982277	-2.009705	1.936858	0.007864	0.265128
-40.879608	-2.041898	1.941862	0.007845	0.265054
-41.227833	-2.025021	1.946867	0.007910	0.264801
-41.435600	-1.986020	1.951872	0.007948	0.264807
-41.548697	-2.011790	1.956877	0.007969	0.264554
-41.663789	-2.004125	1.961882	0.007991	0.264482
-41.818346	-1.990194	1.966886	0.008019	0.264404
-41.799266	-2.032394	1.971891	0.008016	0.264192
-41.716760	-2.046820	1.976896	0.008000	0.264196
-42.340884	-1.985434	1.981901	0.008116	0.263910
-42.819768	-1.904437	1.986906	0.008206	0.263877
-42.275321	-2.021421	1.991910	0.008104	0.263779
-42.585068	-2.007911	1.996915	0.008162	0.263544
-42.581214	-2.029542	2.001920	0.008161	0.263429

-43.014863	-1.988851	2.011917	0.008242	0.263220
-43.318856	-1.981272	2.021914	0.008298	0.262957
-43.400085	-1.985525	2.031910	0.008313	0.262853
-43.702207	-1.978619	2.041907	0.008369	0.262589
-43.711484	-1.989964	2.051904	0.008371	0.262518
-43.915189	-1.996470	2.061901	0.008409	0.262278
-43.799922	-2.017658	2.071898	0.008387	0.262277
-44.164233	-1.992165	2.081894	0.008455	0.262052
-44.029031	-2.035366	2.091891	0.008430	0.261950
-44.474282	-1.953034	2.101888	0.008512	0.261958
-44.307636	-1.982792	2.111885	0.008481	0.261962
-44.451640	-1.962491	2.121882	0.008508	0.261930
-44.905148	-1.924748	2.131878	0.008592	0.261683
-44.975833	-1.912074	2.141875	0.008605	0.261682
-44.907360	-1.925099	2.151872	0.008592	0.261680
-44.942840	-1.916659	2.161869	0.008599	0.261691
-44.792661	-1.893901	2.171866	0.008571	0.261969
-44.443318	-1.958841	2.181862	0.008506	0.261962
-44.280065	-1.988172	2.191859	0.008475	0.261964
-44.802576	-1.892361	2.201856	0.008572	0.261969
-44.154805	-2.012024	2.211853	0.008452	0.261959
-44.281093	-1.988684	2.221850	0.008475	0.261962
-44.073886	-2.026086	2.231846	0.008437	0.261964
-44.615808	-1.908151	2.241843	0.008537	0.262072
-44.173296	-1.950689	2.251840	0.008455	0.262282
-44.018380	-1.979013	2.261837	0.008426	0.262282
-44.098582	-1.964052	2.271834	0.008441	0.262284
-43.904800	-1.959959	2.281830	0.008404	0.262502
-43.909607	-1.940753	2.291827	0.008405	0.262604
-43.821464	-1.958066	2.301824	0.008389	0.262597
-43.699710	-1.927175	2.311821	0.008366	0.262890
-43.795059	-1.899683	2.321818	0.008384	0.262947
-43.478150	-1.936877	2.331814	0.008324	0.263060
-43.529972	-1.894840	2.341811	0.008334	0.263240
-43.461447	-1.896544	2.351808	0.008321	0.263300
-42.736270	-1.983003	2.361805	0.008186	0.263550
-43.328898	-1.865108	2.371802	0.008296	0.263606
-42.705809	-1.931113	2.381798	0.008180	0.263867
-42.716684	-1.922560	2.391795	0.008182	0.263903
-42.196984	-1.963390	2.401792	0.008085	0.264199
-42.158130	-1.964167	2.411789	0.008078	0.264234
-41.884002	-1.968641	2.421786	0.008027	0.264483
-41.904282	-1.952440	2.431782	0.008030	0.264552
-41.734435	-1.935428	2.441779	0.007999	0.264815
-41.706866	-1.916028	2.451776	0.007993	0.264949
-41.528365	-1.913526	2.461773	0.007960	0.265140
-41.124253	-1.943724	2.471770	0.007885	0.265377
-40.821673	-1.981201	2.481766	0.007828	0.265474
-40.742138	-1.950798	2.491763	0.007813	0.265719
-40.512890	-1.976595	2.501760	0.007771	0.265806
-40.284795	-1.973097	2.511757	0.007728	0.266052
-40.171298	-1.960785	2.521754	0.007707	0.266231
-39.862837	-1.994045	2.531750	0.007649	0.266356
-39.574368	-1.990516	2.541747	0.007595	0.266661
-39.359424	-2.012476	2.551744	0.007555	0.266755
-39.245333	-1.991925	2.561741	0.007534	0.266979
-39.118875	-1.976559	2.571738	0.007510	0.267188
-38.911511	-1.987466	2.581734	0.007472	0.267334
-39.310508	-1.860516	2.591731	0.007546	0.267629
-38.427331	-1.980443	2.601728	0.007381	0.267850
-38.428546	-1.953000	2.611725	0.007381	0.267997
-38.113513	-1.964044	2.621722	0.007323	0.268248
-37.779916	-1.985807	2.631718	0.007260	0.268458
-37.832698	-1.946962	2.641715	0.007270	0.268616
-37.861535	-1.891545	2.651712	0.007275	0.268887
-37.029815	-1.995574	2.661709	0.007120	0.269142
-37.190727	-1.935399	2.671706	0.007150	0.269309
-36.814764	-1.966940	2.681702	0.007080	0.269507
-36.774492	-1.919351	2.691699	0.007072	0.269803
-36.255916	-1.980113	2.701696	0.006976	0.269983
-36.136857	-1.966253	2.711693	0.006954	0.270174
-35.811237	-1.966651	2.721690	0.006893	0.270490
-35.627318	-1.969903	2.731686	0.006858	0.270652
-35.496532	-1.964032	2.741683	0.006834	0.270811
-35.196680	-1.971367	2.751680	0.006778	0.271064
-35.100556	-1.940065	2.761677	0.006760	0.271325
-34.980992	-1.922571	2.771674	0.006738	0.271535
-34.549725	-1.961614	2.781670	0.006657	0.271746
-34.572285	-1.910416	2.791667	0.006661	0.271997
-33.882767	-1.986735	2.801664	0.006533	0.272259
-33.889122	-1.950343	2.811661	0.006534	0.272447
-33.464999	-1.990855	2.821658	0.006455	0.272642
-33.377036	-1.945531	2.831654	0.006438	0.272968
-33.247079	-1.931172	2.841651	0.006414	0.273170
-32.751602	-1.985786	2.851648	0.006322	0.273358
-32.488506	-1.993654	2.861645	0.006273	0.273570
-32.231255	-1.984387	2.871642	0.006225	0.273868
-32.412470	-1.909177	2.881638	0.006258	0.274091
-32.134363	-1.918840	2.891635	0.006206	0.274308
-31.562801	-1.984487	2.901632	0.006100	0.274511
-31.800519	-1.881262	2.911629	0.006144	0.274827
-31.218960	-1.944102	2.921626	0.006036	0.275054
-31.000398	-1.942902	2.931622	0.005995	0.275270
-30.479813	-1.994787	2.941619	0.005898	0.275495
-30.471085	-1.952779	2.951616	0.005896	0.275725
-30.007995	-1.998772	2.961613	0.005810	0.275926
-29.893701	-1.978270	2.971610	0.005788	0.276143
-30.009469	-1.913867	2.981606	0.005810	0.276371
-29.042004	-2.031448	2.991603	0.005630	0.276677
-28.937791	-2.017963	3.001600	0.005610	0.276847
-28.800743	-2.009823	3.011597	0.005584	0.277020
-28.497898	-2.010563	3.021594	0.005528	0.277305
-28.403326	-1.979707	3.031590	0.005510	0.277556
-28.194119	-1.975738	3.041587	0.005471	0.277776
-28.137845	-1.943427	3.051584	0.005460	0.277998
-27.578502	-1.997411	3.061581	0.005356	0.278247
-27.203079	-2.018998	3.071578	0.005286	0.278490
-27.362286	-1.949296	3.081574	0.005316	0.278702
-26.768612	-2.020120	3.091571	0.005205	0.278896
-27.044934	-1.906612	3.101568	0.005256	0.279224
-26.584770	-1.946627	3.111565	0.005171	0.279451
-26.323467	-1.949945	3.121562	0.005122	0.279681
-25.892590	-1.990402	3.131558	0.005042	0.279877
-25.656039	-1.979838	3.141555	0.004997	0.280155
-25.312287	-1.989515	3.151552	0.004933	0.280428
-25.105690	-1.995136	3.161549	0.004895	0.280593
-25.163177	-1.949563	3.171546	0.004905	0.280775
-24.711611	-1.980049	3.181542	0.004821	0.281042
-24.556862	-1.959036	3.191539	0.004792	0.281295
-24.542565	-1.915530	3.201536	0.004789	0.281533
-24.196844	-1.933079	3.211533	0.004725	0.281766
-23.871575	-1.951271	3.221530	0.004664	0.281977
-23.897975	-1.882271	3.231526	0.004669	0.282307
-23.630880	-1.884119	3.241523	0.004619	0.282547
-23.171685	-1.922595	3.251520	0.004534	0.282778
-22.750323	-1.955782	3.261517	0.004455	0.283001
-22.286980	-1.993390	3.271514	0.004369	0.283240
-22.065257	-1.982718	3.281510	0.004327	0.283501
-21.961330	-1.962508	3.291507	0.004308	0.283701
-21.573771	-1.994485	3.301504	0.004236	0.283898
-21.330371	-1.977377	3.311501	0.004190	0.284211
-21.182766	-1.961227	3.321498	0.004163	0.284430
-21.373371	-1.880925	3.331494	0.004198	0.284663
-20.700725	-1.961224	3.341491	0.004073	0.284877
-20.463279	-1.951757	3.351488	0.004028	0.285145
-20.307823	-1.923008	3.361485	0.003999	0.285435
-20.552825	-1.837328	3.371482	0.004045	0.285644
-19.751620	-1.944871	3.381478	0.003895	0.285837
-19.114115	-2.019167	3.391475	0.003777	0.286048
-18.985450	-1.988134	3.401472	0.003753	0.286324
-18.707280	-1.999013	3.411469	0.003701	0.286525
-18.535615	-1.990079	3.421466	0.003669	0.286729
-18.176968	-2.005762	3.431462	0.003602	0.286979
-17.770471	-2.031837	3.441459	0.003526	0.287221
-17.652196	-2.018712	3.451456	0.003504	0.287395
-17.578067	-1.987550	3.461453	0.003490	0.287621
-17.516914	-1.931628	3.471450	0.003478	0.287958
-17.271455	-1.936050	3.481446	0.003433	0.288161
-17.195651	-1.905435	3.491443	0.003418	0.288384
-16.640736	-1.967420	3.501440	0.003315	0.288580
-16.212957	-1.984637	3.511437	0.003235	0.288884
-16.773934	-1.831788	3.521434	0.003339	0.289139
-16.210664	-1.885508	3.531430	0.003235	0.289383
-16.308474	-1.822579	3.541427	0.003253	0.289610
-15.346164	-1.950326	3.551424	0.003073	0.289846
-15.361453	-1.889132	3.561421	0.003076	0.290138
-15.065280	-1.894944	3.571418	0.003021	0.290378
-14.437436	-1.971318	3.581414	0.002904	0.290566
-14.202385	-1.978104	3.591411	0.002860	0.290746
-14.164254	-1.926000	3.601408	0.002853	0.291040
-13.954515	-1.922433	3.611405	0.002814	0.291248
-13.521905	-1.962224	3.621402	0.002733	0.291441
-13.197092	-1.967242	3.631398	0.002672	0.291710
-12.854351	-1.984064	3.641395	0.002608	0.291936
-12.290735	-2.053056	3.651392	0.002503	0.292102
-11.913120	-2.081672	3.661389	0.002433	0.292301
-11.764125	-2.054429	3.671386	0.002405	0.292570
-11.518112	-2.064220	3.681382	0.002359	0.292744
-11.259647	-2.067346	3.691379	0.002311	0.292961
-11.022254	-2.060267	3.701376	0.002267	0.293209
-11.222996	-1.989847	3.711373	0.002304	0.293377
-10.636152	-2.056050	3.721370	0.002195	0.293577
-10.895404	-1.946129	3.731366	0.002243	0.293887
-10.511885	-1.974182	3.741363	0.002171	0.294093
-10.316877	-1.969153	3.751360	0.002135	0.294292
-10.302663	-1.923465	3.761357	0.002132	0.294530
-9.689214	-1.974531	3.771354	0.002018	0.294827
-9.265056	-2.013558	3.781350	0.001939	0.295015
-8.865157	-2.053576	3.791347	0.001864	0.295175
-8.699395	-2.017238	3.801344	0.001833	0.295502
-8.669094	-1.991337	3.811341	0.001827	0.295656
-8.862849	-1.913164	3.821338	0.001863	0.295867
-8.074331	-2.013865	3.831334	0.001716	0.296075
-7.609656	-2.041527	3.841331	0.001630	0.296353
-7.417251	-2.041274	3.851328	0.001594	0.296526
-7.348707	-2.014381	3.861325	0.001581	0.296718
-6.778618	-2.062075	3.871322	0.001475	0.296991
-6.602525	-2.058193	3.881318	0.001442	0.297167
-6.348832	-2.070329	3.891315	0.001395	0.297332
-5.984553	-2.077115	3.901312	0.001327	0.297622
-5.902237	-2.052420	3.911309	0.001311	0.297815
-5.668573	-2.058514	3.921306	0.001268	0.297992
-5.717779	-1.994621	3.931302	0.001277	0.298260
-5.541940	-1.979165	3.941299	0.001244	0.298490
-5.157254	-2.011158	3.951296	0.001172	0.298674
-4.878730	-2.020807	3.961293	0.001120	0.298873
-4.621112	-2.000118	3.971290	0.001072	0.299200
-4.539861	-1.977257	3.981286	0.001057	0.299383
-4.164094	-2.008249	3.991283	0.000987	0.299563
-4.141404	-1.958685	4.001280	0.000982	0.299823
-4.105731	-1.908722	4.011277	0.000976	0.300096
-3.861664	-1.902393	4.021274	0.000930	0.300341
-3.733806	-1.880442	4.031270	0.000906	0.300559
-3.441372	-1.897936	4.041267	0.000851	0.300731
-3.545257	-1.814768	4.051264	0.000871	0.301040
-3.260894	-1.813122	4.061261	0.000818	0.301297
-2.927760	-1.819792	4.071258	0.000755	0.301556
-2.873489	-1.778228	4.081254	0.000745	0.301803
-2.594825	-1.779410	4.091251	0.000693	0.302041
-2.627510	-1.715131	4.101248	0.000699	0.302321
-2.438670	-1.688312	4.111245	0.000664	0.302614
-2.320887	-1.641398	4.121242	0.000642	0.302940
-2.037252	-1.637915	4.131238	0.000589	0.303204
-2.079464	-1.570417	4.141235	0.000597	0.303489
-1.660414	-1.588363	4.151232	0.000519	0.303767
-1.619540	-1.532710	4.161229	0.000511	0.304068
-1.726631	-1.449934	4.171226	0.000531	0.304370
-1.783639	-1.372782	4.181222	0.000541	0.304687
-1.581776	-1.340997	4.191219	0.000503	0.305013
-1.288262	-1.322163	4.201216	0.000449	0.305356
-1.253719	-1.266176	4.211213	0.000442	0.305651
-1.118941	-1.223916	4.221210	0.000417	0.305967
-0.921838	-1.188577	4.231206	0.000380	0.306304
-0.837946	-1.129776	4.241203	0.000364	0.306654
-0.758851	-1.072851	4.251200	0.000349	0.306991
-0.794411	-0.985364	4.261197	0.000356	0.307373
-0.477213	-0.964767	4.271194	0.000297	0.307741
-0.453578	-0.891062	4.281190	0.000292	0.308108
-0.553135	-0.796638	4.291187	0.000310	0.308467
-0.425641	-0.739170	4.301184	0.000286	0.308845
-0.380196	-0.651911	4.311181	0.000278	0.309293
-0.427970	-0.563503	4.321178	0.000287	0.309666
-0.418805	-0.479575	4.331174	0.000285	0.310066
-0.351893	-0.388457	4.341171	0.000272	0.310548
-0.293479	-0.321966	4.351168	0.000261	0.310908
-0.266179	-0.234896	4.361165	0.000256	0.311336
-0.163220	-0.149857	4.371162	0.000236	0.311818
-0.248173	-0.044940	4.381158	0.000252	0.312234
-0.056755	0.032133	4.391155	0.000216	0.312752
-0.150049	0.142520	4.401152	0.000234	0.313184
0.000000	0.224507	4.411149	0.000205	0.313689

0.023314	0.493817	4.416154	0.000201	0.314948
0.156270	1.032045	4.421158	0.000176	0.317521
0.430577	1.834704	4.426163	0.000124	0.321382
0.514926	2.970602	4.431168	0.000108	0.326523
0.960348	4.330741	4.436173	0.000024	0.332847
1.592196	5.951503	4.441178	-0.000095	0.340306
2.251813	7.879297	4.446182	-0.000219	0.348902
2.548053	10.177622	4.451187	-0.000276	0.358522
3.403628	12.685512	4.456192	-0.000437	0.369111
4.287137	15.514944	4.461197	-0.000603	0.380647
4.840152	18.736306	4.466202	-0.000708	0.393068
5.771244	22.226298	4.471206	-0.000884	0.406309
6.783518	26.045806	4.476211	-0.001075	0.420318
7.863968	30.210965	4.481216	-0.001279	0.435066
8.660222	34.768223	4.486221	-0.001430	0.450425
10.180857	39.550841	4.491226	-0.001717	0.466382
11.790536	44.678808	4.496230	-0.002020	0.482894
12.584102	50.303404	4.501235	-0.002171	0.499871
14.138158	56.147495	4.506240	-0.002465	0.517286
15.522615	62.344536	4.511245	-0.002726	0.535005
17.117562	68.837613	4.516250	-0.003028	0.553029
18.865765	75.631007	4.521254	-0.003358	0.571312
20.174475	82.807023	4.526259	-0.003606	0.589772
22.008362	90.179867	4.531264	-0.003952	0.608362
23.934708	97.817015	4.536269	-0.004316	0.627048
26.447911	105.611112	4.541274	-0.004789	0.645777
29.781482	113.536139	4.546278	-0.005415	0.664580
32.017321	121.864191	4.551283	-0.005837	0.683301
34.211551	130.422058	4.556288	-0.006251	0.701979
36.475120	139.148948	4.561293	-0.006678	0.720534
38.344542	148.115237	4.566298	-0.007032	0.738953
40.399494	157.201194	4.571302	-0.007421	0.757213
42.403505	166.400817	4.576307	-0.007800	0.775236
44.178024	175.767412	4.581312	-0.008137	0.793078
46.176639	185.163393	4.586317	-0.008515	0.810650
48.707790	194.562441	4.591322	-0.008993	0.828016
51.200338	204.023101	4.596326	-0.009463	0.845117
53.257341	213.589667	4.601331	-0.009852	0.861926
56.071576	223.068015	4.606336	-0.010382	0.878485
61.607904	232.113632	4.611341	-0.011419	0.894810
65.395565	241.536252	4.616346	-0.012131	0.910949
67.411063	251.265739	4.621350	-0.012512	0.926798
68.709767	261.083614	4.626355	-0.012761	0.942323
70.122441	270.861980	4.631360	-0.013030	0.957565
71.254851	280.635063	4.636365	-0.013247	0.972487
72.601809	290.326508	4.641370	-0.013505	0.987117
73.923946	299.968864	4.646374	-0.013757	1.001457
75.027717	309.563253	4.651379	-0.013969	1.015470
75.838308	319.167378	4.656384	-0.014126	1.029234
77.099928	328.611022	4.661389	-0.014367	1.042702
78.039552	338.063692	4.666394	-0.014548	1.055934
79.032714	347.456020	4.671398	-0.014740	1.068932
79.946838	356.772943	4.676403	-0.014916	1.081655
81.161654	366.007085	4.681408	-0.015148	1.094188
82.085076	375.223540	4.686413	-0.015326	1.106490
82.791579	384.423940	4.691418	-0.015464	1.118587
83.715503	393.538075	4.696422	-0.015642	1.130492
84.566018	402.596417	4.701427	-0.015806	1.142186
85.469517	411.633064	4.706432	-0.015980	1.153745
86.037031	420.633465	4.711437	-0.016092	1.165073
86.876947	429.549952	4.716442	-0.016254	1.176246
88.342356	438.326068	4.721446	-0.016533	1.187272
89.160311	447.169693	4.726451	-0.016691	1.198144
89.736075	456.024711	4.731456	-0.016804	1.208882
90.478991	464.810839	4.736461	-0.016948	1.219478
91.149982	473.577220	4.741466	-0.017079	1.229944
91.896878	482.288608	4.746470	-0.017223	1.240273
92.576355	490.965971	4.751475	-0.017356	1.250464
93.131121	499.652707	4.756480	-0.017465	1.260558
94.179681	508.228575	4.761485	-0.017666	1.270541
94.574445	516.880307	4.766490	-0.017745	1.280407
95.387402	525.445490	4.771494	-0.017902	1.290179
96.012595	534.003362	4.776499	-0.018024	1.299834
97.270088	542.500286	4.781504	-0.018264	1.309467
97.930881	551.077675	4.786509	-0.018392	1.319008
98.642511	559.554496	4.791514	-0.018530	1.328380
99.383649	568.032415	4.796518	-0.018674	1.337693
100.071032	576.483001	4.801523	-0.018807	1.346902
101.068744	584.893401	4.806528	-0.018999	1.356060
101.835256	593.311308	4.811533	-0.019147	1.365124
102.393490	601.766942	4.816538	-0.019257	1.374131
102.842130	610.228161	4.821542	-0.019346	1.383066
103.458306	618.637529	4.826547	-0.019466	1.391918
103.992672	627.037322	4.831552	-0.019571	1.400690
104.494041	635.433636	4.836557	-0.019670	1.409398
105.020307	643.808640	4.841562	-0.019773	1.418035
105.763317	652.152009	4.846566	-0.019917	1.426624
106.158961	660.537470	4.851571	-0.019996	1.435146
106.603153	668.892170	4.856576	-0.020085	1.443594
107.235176	677.216547	4.861581	-0.020208	1.451994
107.822005	685.526122	4.866586	-0.020322	1.460323
108.215363	693.906161	4.871590	-0.020401	1.468643
108.569873	702.254759	4.876595	-0.020473	1.476879
109.208059	710.513679	4.881600	-0.020597	1.485027
109.672292	718.827358	4.886605	-0.020689	1.493155
110.118927	727.105287	4.891610	-0.020778	1.501202
111.063951	735.340946	4.896614	-0.020959	1.509244
111.682626	743.605005	4.901619	-0.021080	1.517219
113.142697	751.731652	4.906624	-0.021357	1.525152
113.965727	760.001297	4.911629	-0.021515	1.533080
114.679026	768.263008	4.916634	-0.021654	1.540943
115.449019	776.543416	4.921638	-0.021803	1.548792
116.123697	784.795232	4.926643	-0.021934	1.556560
116.906651	793.025402	4.931648	-0.022085	1.564285
117.407269	801.317794	4.936653	-0.022183	1.571987
118.158214	809.542512	4.941658	-0.022329	1.579627
119.084215	817.756557	4.946662	-0.022507	1.587246
119.762789	825.995547	4.951667	-0.022638	1.594814
120.265619	834.258616	4.956672	-0.022737	1.602343
121.328288	842.430206	4.961677	-0.022941	1.609834
122.527502	850.590336	4.966682	-0.023169	1.617301
123.476376	858.800057	4.971686	-0.023351	1.624740
124.212496	867.064976	4.976691	-0.023494	1.632164
125.283178	875.244960	4.981696	-0.023699	1.639527
126.186393	883.423252	4.986701	-0.023872	1.646831
126.948497	891.648371	4.991706	-0.024019	1.654124
127.961208	899.830274	4.996710	-0.024213	1.661382
129.229180	907.971814	5.001715	-0.024455	1.668609
130.024071	916.215526	5.006720	-0.024608	1.675826
131.116763	924.364773	5.011725	-0.024817	1.682972
132.047831	932.560521	5.016730	-0.024996	1.690106
132.992795	940.771738	5.021734	-0.025177	1.697224
133.949453	948.943015	5.026739	-0.025361	1.704279
134.802953	957.167186	5.031744	-0.025525	1.711337
135.835129	965.326802	5.036749	-0.025723	1.718334
136.635131	973.506402	5.041754	-0.025877	1.725289
138.284278	981.606103	5.046758	-0.026189	1.732260
139.302370	989.774051	5.051763	-0.026384	1.739177
140.773661	997.891032	5.056768	-0.026664	1.746083
141.951379	1006.081473	5.061773	-0.026888	1.752984
142.998278	1014.248742	5.066778	-0.027089	1.759822
143.668245	1022.484299	5.071782	-0.027219	1.766640
144.151659	1030.737165	5.076787	-0.027314	1.773422
145.077551	1038.903580	5.081792	-0.027492	1.780165
145.661492	1047.125389	5.086797	-0.027606	1.786883
146.153858	1055.376690	5.091802	-0.027703	1.793588
146.838968	1063.529811	5.096806	-0.027836	1.800213
147.535858	1071.674272	5.101811	-0.027971	1.806809
148.027722	1079.881964	5.106816	-0.028068	1.813405
148.808184	1088.000474	5.111821	-0.028219	1.819942
149.350546	1096.174290	5.116826	-0.028325	1.826470
150.008632	1104.357452	5.121830	-0.028453	1.832995
150.540759	1112.495022	5.126835	-0.028558	1.839447
151.126594	1120.639829	5.131840	-0.028672	1.845888
151.760755	1128.805832	5.136845	-0.028796	1.852328
152.185113	1136.966668	5.141850	-0.028880	1.858717
152.670909	1145.122745	5.146854	-0.028976	1.865088
153.192231	1153.278434	5.151859	-0.029078	1.871441
153.878972	1161.395948	5.156864	-0.029211	1.877762
154.429554	1169.526565	5.161869	-0.029319	1.884055
154.788954	1177.687250	5.166874	-0.029392	1.890329
155.841487	1185.767913	5.171878	-0.029593	1.896601
156.250931	1193.908225	5.176883	-0.029675	1.902823
156.698862	1202.074069	5.181888	-0.029763	1.909048
157.568459	1210.149247	5.186893	-0.029931	1.915233
158.080310	1218.278923	5.191898	-0.030031	1.921398
158.632355	1226.433072	5.196902	-0.030139	1.927566
158.995288	1234.598456	5.201907	-0.030212	1.933701
159.493364	1242.730201	5.206912	-0.030310	1.939806
160.090969	1250.831696	5.211917	-0.030427	1.945881
160.997691	1258.913765	5.216922	-0.030601	1.951957
161.969125	1266.976457	5.221926	-0.030787	1.958007
162.684427	1275.070015	5.226931	-0.030926	1.964033
163.357066	1283.201018	5.231936	-0.031056	1.970062
163.936773	1291.337627	5.236941	-0.031170	1.976067
164.312627	1299.478894	5.241946	-0.031245	1.982034
164.976821	1307.604754	5.246950	-0.031374	1.988004
165.698020	1315.701532	5.251955	-0.031514	1.993940
166.285866	1323.814341	5.256960	-0.031629	1.999856
166.882022	1331.918286	5.261965	-0.031745	2.005749
167.899804	1339.987625	5.266970	-0.031940	2.011645
169.028810	1348.056910	5.271974	-0.032155	2.017535
169.428014	1356.199934	5.276979	-0.032235	2.023383
170.020905	1364.357108	5.281984	-0.032351	2.029244
170.666345	1372.474594	5.286989	-0.032476	2.035065
171.474380	1380.525962	5.291994	-0.032632	2.040841
172.166959	1388.644675	5.296998	-0.032766	2.046635
172.697882	1396.767187	5.302003	-0.032870	2.052398
173.595357	1404.848824	5.307008	-0.033043	2.058154
174.137065	1412.981022	5.312013	-0.033149	2.063893
174.694170	1421.089192	5.317018	-0.033258	2.069600
175.423212	1429.187161	5.322022	-0.033399	2.075302
175.898233	1437.289218	5.327027	-0.033493	2.080966
176.792472	1445.356137	5.332032	-0.033665	2.086631
177.887571	1453.419819	5.337037	-0.033874	2.092300
178.660137	1461.533904	5.342042	-0.034023	2.097954
179.442405	1469.619393	5.347046	-0.034174	2.103575
179.993002	1477.771768	5.352051	-0.034282	2.109204
181.054396	1485.858297	5.357056	-0.034485	2.114823
181.590746	1493.953363	5.362061	-0.034590	2.120380
182.340435	1502.020346	5.367066	-0.034735	2.125925
183.112375	1510.141128	5.372070	-0.034884	2.131494
183.574426	1518.258736	5.377075	-0.034976	2.137016
184.512452	1526.307777	5.382080	-0.035156	2.142524
185.493583	1534.376956	5.387085	-0.035344	2.148034
186.202872	1542.485902	5.392090	-0.035481	2.153531
186.885273	1550.589789	5.397094	-0.035613	2.159008
187.605460	1558.646253	5.402099	-0.035753	2.164443
188.324955	1566.750915	5.407104	-0.035892	2.169896
188.915613	1574.887386	5.412109	-0.036007	2.175344
189.859857	1582.918847	5.417114	-0.036189	2.180742
190.740894	1591.000323	5.422118	-0.036358	2.186153
190.973201	1599.176973	5.427123	-0.036407	2.191553
191.704830	1607.250396	5.432128	-0.036548	2.196918
192.541038	1615.299191	5.437133	-0.036709	2.202264
193.012948	1623.406863	5.442138	-0.036802	2.207601
193.645791	1631.511753	5.447142	-0.036926	2.212938
194.259582	1639.592238	5.452147	-0.037045	2.218245
194.997859	1647.652553	5.457152	-0.037188	2.223537
195.451249	1655.793064	5.462157	-0.037278	2.228842
196.233069	1663.845577	5.467162	-0.037429	2.234108
196.944196	1671.919590	5.472166	-0.037566	2.239368
197.495968	1679.983382	5.477171	-0.037674	2.244595
198.140660	1688.078742	5.482176	-0.037800	2.249839
198.861703	1696.160288	5.487181	-0.037939	2.255068
199.545223	1704.247493	5.492186	-0.038072	2.260284
200.117447	1712.347546	5.497190	-0.038184	2.265487
200.840947	1720.434492	5.502195	-0.038324	2.270683
202.048620	1728.449696	5.507200	-0.038554	2.275864
202.762140	1736.521012	5.512205	-0.038692	2.281026
203.044771	1744.631468	5.517210	-0.038750	2.286162
203.940249	1752.684940	5.522214	-0.038922	2.291304
205.035243	1760.677748	5.527219	-0.039131	2.296414
205.762251	1768.772668	5.532224	-0.039272	2.301544
206.479498	1776.868256	5.537229	-0.039411	2.306662
207.188520	1784.945109	5.542234	-0.039548	2.311757
207.636379	1793.064137	5.547238	-0.039637	2.316844
208.232633	1801.110182	5.552243	-0.039753	2.321887
209.027432	1809.182010	5.557248	-0.039907	2.326951
209.508251	1817.292970	5.562253	-0.040001	2.332002
210.072031	1825.376547	5.567258	-0.040112	2.337032
211.018256	1833.418362	5.572262	-0.040293	2.342058
211.806402	1841.478787	5.577267	-0.040445	2.347071
212.407643	1849.581676	5.582272	-0.040563	2.352083
213.213826	1857.634526	5.587277	-0.040718	2.357071
214.286185	1865.623512	5.592282	-0.040923	2.362032
214.890597	1873.737626	5.597286	-0.041041	2.367019
215.244150	1881.865654	5.602291	-0.041112	2.371983
215.898673	1889.962813	5.607296	-0.041239	2.376943
216.780447	1897.975867	5.612301	-0.041409	2.381861
217.130312	1906.075941	5.617306	-0.041479	2.386777
217.701054	1914.172847	5.622310	-0.041591	2.391698
218.391167	1922.214103	5.627315	-0.041724	2.396586
219.246711	1930.250839	5.632320	-0.041889	2.401475
219.877613	1938.315302	5.637325	-0.042012	2.406351
220.203393	1946.421929	5.642330	-0.042078	2.411219
221.302005	1954.451393	5.647334	-0.042288	2.416092
222.095013	1962.488387	5.652339	-0.042441	2.420935
223.094328	1970.541919	5.657344	-0.042632	2.425795
224.056682	1978.623785	5.662349	-0.042817	2.430658
224.804310	1986.699719	5.667354	-0.042961	2.435491
226.018719	1994.714171	5.672358	-0.043192	2.440315
226.683785	2002.755641	5.677363	-0.043322	2.445102
227.293467	2010.864773	5.682368	-0.043440	2.449915
227.804943	2018.955534	5.687373	-0.043541	2.454700
228.526557	2027.008846	5.692378	-0.043681	2.459470
229.072699	2035.105371	5.697382	-0.043788	2.464242
229.871999	2043.148791	5.702387	-0.043942	2.468993
230.607370	2051.223602	5.707392	-0.044084	2.473748
231.462514	2059.247637	5.712397	-0.044249	2.478474
231.800338	2067.326091	5.717402	-0.044317	2.483183
232.542069	2075.402472	5.722406	-0.044460	2.487912
233.358680	2083.447608	5.727411	-0.044618	2.492619
234.019326	2091.532045	5.732416	-0.044746	2.497329
234.263705	2099.646630	5.737421	-0.044797	2.502015
235.063845	2107.667190	5.742426	-0.044951	2.506680
236.162874	2115.719822	5.747430	-0.045161	2.511377
236.851605	2123.766491	5.752435	-0.045294	2.516031
237.469801	2131.815727	5.757440	-0.045415	2.520673
238.407205	2139.848074	5.762445	-0.045595	2.525320
238.895734	2147.938250	5.767450	-0.045691	2.529958
239.652700	2156.010723	5.772454	-0.045837	2.534597
240.396811	2164.035891	5.777459	-0.045981	2.539199
240.937006	2172.102792	5.782464	-0.046087	2.543802
241.602355	2180.183297	5.787469	-0.046216	2.548414
242.085923	2188.253590	5.792474	-0.046312	2.552997
243.059205	2196.289817	5.797478	-0.046498	2.557589
243.445164	2204.358346	5.802483	-0.046575	2.562148
244.227606	2212.405273	5.807488	-0.046726	2.566715
245.183091	2220.443935	5.812493	-0.046909	2.571282
245.584320	2228.543445	5.817498	-0.046989	2.575835
246.497628	2236.573935	5.822502	-0.047165	2.580377
247.098200	2244.621074	5.827507	-0.047282	2.584899
247.769136	2252.706980	5.832512	-0.047412	2.589439
248.704231	2260.852522	5.837517	-0.047592	2.594022
249.682319	2268.803070	5.842522	-0.047779	2.598493
250.459972	2276.840865	5.847526	-0.047929	2.602989
250.989382	2284.890200	5.852531	-0.048033	2.607467
251.808965	2292.932118	5.857536	-0.048191	2.611953
252.625543	2301.001533	5.862541	-0.048348	2.616446
252.996956	2309.072015	5.867546	-0.048423	2.620902
253.620832	2317.122718	5.872550	-0.048544	2.625356
253.919215	2325.212273	5.877555	-0.048605	2.629801
254.807429	2333.219253	5.882560	-0.048776	2.634234
255.349600	2341.275165	5.887565	-0.048882	2.638662
255.697780	2349.344283	5.892570	-0.048952	2.643077
256.627907	2357.367232	5.897574	-0.049131	2.647499
257.207030	2365.419842	5.902579	-0.049244	2.651905
257.804043	2373.495826	5.907584	-0.049360	2.656318
258.522667	2381.534807	5.912589	-0.049499	2.660712
259.118962	2389.576490	5.917594	-0.049616	2.665091
259.676449	2397.680600	5.922598	-0.049725	2.669495
260.324022	2405.704915	5.927603	-0.049851	2.673854
261.166225	2413.706121	5.932608	-0.050013	2.678206
261.915214	2421.729897	5.937613	-0.050157	2.682556
262.369263	2429.806014	5.942618	-0.050247	2.686909
263.244073	2437.862436	5.947622	-0.050416	2.691271
263.859489	2445.927655	5.952627	-0.050535	2.695614
264.610933	2453.961012	5.957632	-0.050681	2.699941
265.379231	2461.984516	5.962637	-0.050829	2.704257
266.076533	2470.045182	5.967642	-0.050964	2.708581
266.953482	2478.096880	5.972646	-0.051133	2.712905
267.873438	2486.106582	5.977651	-0.051309	2.717203
268.880913	2494.118985	5.982656	-0.051502	2.721500
269.498666	2502.190266	5.987661	-0.051622	2.725797
270.150295	2510.253387	5.992666	-0.051749	2.730085
271.204618	2518.309304	5.997670	-0.051951	2.734387
271.527574	2526.399268	6.002675	-0.052016	2.738655
272.131667	2534.458377	6.007680	-0.052134	2.742917
272.721024	2542.521389	6.012685	-0.052249	2.747173
273.385696	2550.608034	6.017690	-0.052378	2.751440
274.262280	2558.659118	6.022694	-0.052547	2.755695
275.081213	2566.647217	6.027699	-0.052704	2.759907
275.973655	2574.628488	6.032704	-0.052876	2.764112
276.602945	2582.711876	6.037709	-0.052998	2.768349
277.407423	2590.720474	6.042714	-0.053153	2.772550
278.202425	2598.794104	6.047718	-0.053307	2.776778
278.792065	2606.843588	6.052723	-0.053422	2.780975
279.715178	2614.871906	6.057728	-0.053599	2.785174
280.666276	2622.906569	6.062733	-0.053781	2.789372
281.196038	2630.982502	6.067738	-0.053885	2.793560
282.304964	2638.984413	6.072742	-0.054097	2.797737
282.712920	2647.055628	6.077747	-0.054178	2.801902
283.636329	2655.096824	6.082752	-0.054356	2.806076
284.141357	2663.188723	6.087757	-0.054455	2.810244
284.809339	2671.205519	6.092762	-0.054585	2.814378
285.589860	2679.269868	6.097766	-0.054735	2.818536
286.148768	2687.312043	6.102771	-0.054845	2.822663
286.737409	2695.369643	6.107776	-0.054959	2.826794
287.356184	2703.448209	6.112781	-0.055080	2.830932
288.024036	2711.464895	6.117786	-0.055210	2.835034
288.748354	2719.493887	6.122790	-0.055350	2.839140
289.441587	2727.511895	6.127795	-0.055484	2.843233
290.097034	2735.569697	6.132800	-0.055612	2.847338
290.933563	2743.612632	6.137805	-0.055773	2.851439
291.325492	2751.674822	6.142810	-0.055851	2.855518
292.275842	2759.675923	6.147814	-0.056033	2.859593
292.651023	2767.732491	6.152819	-0.056108	2.863657
293.185451	2775.815092	6.157824	-0.056213	2.867737
294.273921	2783.815597	6.162829	-0.056421	2.871802
294.818596	2791.852579	6.167834	-0.056528	2.875848
295.489723	2799.906342	6.172838	-0.056658	2.879904
296.089871	2807.910218	6.177843	-0.056775	2.883925
296.759167	2815.978122	6.182848	-0.056905	2.887976
296.895250	2824.113137	6.187853	-0.056936	2.892025
297.611451	2832.103365	6.192858	-0.057074	2.896029
298.546236	2840.135485	6.197862	-0.057254	2.900059
298.951249	2848.164521	6.202867	-0.057334	2.904054
299.628362	2856.229555	6.207872	-0.057466	2.908075
300.129145	2864.336503	6.212877	-0.057564	2.912102
300.845593	2872.353651	6.217882	-0.057703	2.916091
301.428280	2880.383655	6.222886	-0.057817	2.920073
302.021152	2888.355139	6.227891	-0.057932	2.924021
302.665931	2896.399497	6.232896	-0.058058	2.928003
303.333227	2904.455233	6.237901	-0.058187	2.931985
303.743812	2912.509024	6.242906	-0.058269	2.935948
304.414097	2920.556282	6.247910	-0.058399	2.939916
304.966647	2928.566218	6.252915	-0.058507	2.943853
305.666083	2936.593555	6.257920	-0.058643	2.947802
306.302281	2944.671692	6.262925	-0.058767	2.951767
306.937726	2952.680761	6.267930	-0.058890	2.955692
307.451185	2960.728907	6.272934	-0.058991	2.959625
308.051391	2968.738654	6.277939	-0.059108	2.963539
308.598542	2976.808963	6.282944	-0.059215	2.967473
308.990156	2984.931032	6.287949	-0.059294	2.971419
309.769896	2992.896633	6.292954	-0.059444	2.975305
310.599741	3000.903311	6.297958	-0.059604	2.979208
311.248861	3008.927412	6.302963	-0.059730	2.983104
311.819600	3017.002620	6.307968	-0.059842	2.987016
312.123502	3025.094567	6.312973	-0.059903	2.990917
312.856453	3033.082266	6.317978	-0.060045	2.994785
313.711078	3041.074866	6.322982	-0.060210	2.998656
314.099264	3049.113625	6.327987	-0.060287	3.002521
314.628625	3057.184555	6.332992	-0.060391	3.006403
315.310151	3065.223842	6.337997	-0.060523	3.010272
315.575952	3073.288420	6.343002	-0.060578	3.014127
316.116129	3081.330488	6.348006	-0.060684	3.017981
316.587101	3089.354280	6.353011	-0.060777	3.021817
317.148887	3097.390139	6.358016	-0.060887	3.025659
317.424569	3105.468606	6.363021	-0.060943	3.029501
318.082613	3113.473093	6.368026	-0.061071	3.033323
318.710255	3121.518309	6.373030	-0.061193	3.037158
319.021673	3129.558827	6.378035	-0.061257	3.040969
319.664490	3137.572332	6.383040	-0.061382	3.044780
320.323599	3145.601817	6.388045	-0.061510	3.048593
320.557083	3153.678039	6.393050	-0.061558	3.052404
320.859472	3161.753332	6.398054	-0.061620	3.056212
321.609095	3169.723244	6.403059	-0.061765	3.059988
322.028210	3177.757601	6.408064	-0.061848	3.063773
322.406577	3185.839704	6.413069	-0.061924	3.067573
322.846945	3193.902252	6.418074	-0.062011	3.071363
323.552090	3201.952435	6.423078	-0.062148	3.075155
324.067214	3209.929262	6.428083	-0.062249	3.078899
324.541739	3217.941029	6.433088	-0.062343	3.082653
325.356277	3225.949522	6.438093	-0.062500	3.086416
325.708568	3233.996589	6.443098	-0.062570	3.090171
326.088436	3242.076408	6.448102	-0.062647	3.093938
326.697858	3250.072819	6.453107	-0.062765	3.097672
327.197676	3258.133524	6.458112	-0.062864	3.101426
327.924429	3266.133288	6.463117	-0.063004	3.105158
328.122791	3274.191754	6.468122	-0.063046	3.108888
328.728633	3282.237849	6.473126	-0.063165	3.112627
328.884946	3290.311410	6.478131	-0.063199	3.116352
329.605843	3298.277524	6.483136	-0.063338	3.120050
330.007285	3306.308633	6.488141	-0.063419	3.123759
330.375874	3314.339856	6.493146	-0.063492	3.127462
330.720021	3322.445935	6.498150	-0.063562	3.131193
330.990719	3330.488679	6.503155	-0.063618	3.134888
331.449613	3338.490213	6.508160	-0.063708	3.138568
332.339364	3346.469514	6.513165	-0.063879	3.142253
332.876386	3354.514846	6.518170	-0.063984	3.145947
333.692504	3362.536128	6.523174	-0.064142	3.149639
333.815190	3370.628865	6.528179	-0.064170	3.153328
334.436509	3378.616717	6.533184	-0.064291	3.156987
335.067775	3386.681979	6.538189	-0.064414	3.160677
335.419227	3394.654281	6.543194	-0.064484	3.164308
335.941384	3402.702641	6.548198	-0.064587	3.167977
336.229962	3410.779300	6.553203	-0.064646	3.171644
336.959124	3418.794127	6.558208	-0.064787	3.175298
337.497325	3426.801867	6.563213	-0.064892	3.178937
337.991443	3434.829578	6.568218	-0.064990	3.182578
338.337805	3442.908816	6.573222	-0.065060	3.186232
338.689856	3450.949738	6.578227	-0.065130	3.189864
339.502233	3458.931905	6.583232	-0.065287	3.193486
340.034269	3466.964495	6.588237	-0.065391	3.197114
340.121937	3475.054809	6.593242	-0.065413	3.200745
340.614800	3483.044300	6.598246	-0.065510	3.204343
340.900795	3491.110339	6.603251	-0.065569	3.207963
341.285898	3499.183854	6.608256	-0.065646	3.211587
341.727764	3507.192672	6.613261	-0.065733	3.215179
341.971271	3515.197327	6.618266	-0.065784	3.218758
342.524039	3523.234948	6.623270	-0.065892	3.222360
342.626297	3531.295773	6.628275	-0.065916	3.225949
342.520750	3539.401471	6.633280	-0.065902	3.229546
343.154228	3547.366118	6.638285	-0.066025	3.233107
343.979170	3555.314071	6.643290	-0.066184	3.236664
344.388664	3563.357523	6.648294	-0.066266	3.240243
344.703152	3571.389331	6.653299	-0.066329	3.243808
345.277899	3579.397278	6.658304	-0.066442	3.247370
345.697704	3587.488958	6.663309	-0.066525	3.250958
346.061509	3595.472420	6.668314	-0.066598	3.254492
346.348081	3603.553516	6.673318	-0.066657	3.258062
346.258077	3611.649480	6.678323	-0.066645	3.261619
346.832058	3619.614503	6.683328	-0.066758	3.265142
347.472059	3627.601529	6.688333	-0.066882	3.268673
347.968522	3635.647812	6.693338	-0.066980	3.272221
348.551457	3643.689411	6.698342	-0.067094	3.275766
348.872578	3651.674809	6.703347	-0.067159	3.279272
349.481268	3659.700455	6.708352	-0.067277	3.282803
350.075901	3667.715581	6.713357	-0.067393	3.286326
350.210889	3675.766523	6.718362	-0.067424	3.289841
350.766807	3683.847332	6.723366	-0.067532	3.293383
351.025694	3691.888734	6.728371	-0.067586	3.296892
351.414300	3699.904788	6.733376	-0.067664	3.300391
351.510914	3707.968926	6.738381	-0.067687	3.303896
351.805945	3716.005754	6.743386	-0.067747	3.307392
352.319604	3724.041632	6.748390	-0.067848	3.310894
352.815777	3732.028656	6.753395	-0.067946	3.314370
353.064675	3740.072513	6.758400	-0.067997	3.317857
353.401863	3748.115609	6.763405	-0.068065	3.321343
353.588006	3756.109858	6.768410	-0.068105	3.324799
353.894270	3764.170675	6.773414	-0.068168	3.328284
354.368276	3772.173659	6.778419	-0.068261	3.331747
354.752760	3780.199689	6.783424	-0.068338	3.335213
354.964643	3788.242273	6.788429	-0.068383	3.338676
355.359539	3796.250215	6.793434	-0.068462	3.342128
355.771676	3804.309560	6.798438	-0.068544	3.345598
355.999931	3812.322901	6.803443	-0.068591	3.349038
356.411562	3820.354790	6.808448	-0.068673	3.352490
356.869243	3828.396246	6.813453	-0.068764	3.355943
357.042768	3836.394944	6.818458	-0.068801	3.359364
357.612402	3844.396651	6.823462	-0.068913	3.362798
357.733840	3852.486863	6.828467	-0.068941	3.366249
357.616392	3860.556999	6.833472	-0.068924	3.369679
358.387437	3868.544413	6.838477	-0.069073	3.373103
359.007088	3876.537221	6.843482	-0.069194	3.376521
359.336884	3884.596545	6.848486	-0.069260	3.379952
359.615049	3892.586860	6.853491	-0.069317	3.383349
359.692497	3900.677815	6.858496	-0.069337	3.386777
360.222089	3908.697690	6.863501	-0.069441	3.390189
360.535142	3916.750312	6.868506	-0.069505	3.393603
361.021395	3924.779421	6.873510	-0.069600	3.397009
361.194774	3932.782690	6.878515	-0.069638	3.400390
361.531171	3940.700108	6.883520	-0.069706	3.403738
361.895043	3948.791640	6.888525	-0.069779	3.407156
362.222996	3956.861079	6.893530	-0.069845	3.410560
362.353918	3964.898820	6.898534	-0.069875	3.413941
362.444577	3972.950215	6.903539	-0.069897	3.417322
362.791521	3980.975477	6.908544	-0.069967	3.420698
363.328784	3988.951894	6.913549	-0.070072	3.424057
363.528289	3997.020591	6.918554	-0.070115	3.427440
364.078142	4005.030074	6.923558	-0.070222	3.430806
364.596485	4012.970256	6.928563	-0.070324	3.434139
365.082494	4021.016939	6.933568	-0.070420	3.437512
365.260392	4029.121224	6.938573	-0.070458	3.440895
365.503272	4037.065387	6.943578	-0.070509	3.444211
365.829569	4045.129134	6.948582	-0.070575	3.447575
366.301927	4053.183668	6.953587	-0.070668	3.450938
366.899165	4061.150269	6.958592	-0.070785	3.454264
367.306000	4069.197643	6.963597	-0.070866	3.457615
367.440826	4077.235224	6.968602	-0.070896	3.460949
367.975093	4085.229283	6.973606	-0.071001	3.464275
368.357887	4093.296453	6.978611	-0.071077	3.467623
368.793783	4101.349162	6.983616	-0.071164	3.470964
369.191199	4109.355415	6.988621	-0.071243	3.474280
369.454770	4117.353768	6.993626	-0.071298	3.477586
370.058467	4125.413699	6.998630	-0.071415	3.480926
370.093955	4133.382182	7.003635	-0.071427	3.484205
370.612402	4141.382666	7.008640	-0.071529	3.487511
371.114628	4149.496491	7.013645	-0.071628	3.490859
371.429741	4157.461923	7.018650	-0.071692	3.494137
371.772622	4165.547861	7.023654	-0.071761	3.497463
371.915454	4173.595705	7.028659	-0.071793	3.500762
372.437939	4181.550236	7.033664	-0.071895	3.504033
372.812160	4189.641822	7.038669	-0.071970	3.507352
373.301485	4197.654184	7.043674	-0.072067	3.510640
373.705434	4205.672557	7.048678	-0.072147	3.513923
374.071517	4213.693920	7.053683	-0.072221	3.517204
374.243156	4221.745013	7.058688	-0.072258	3.520487
374.869659	4229.711513	7.063693	-0.072380	3.523748
375.143416	4237.786068	7.068698	-0.072436	3.527038
375.366546	4245.841441	7.073702	-0.072483	3.530315
375.606932	4253.832234	7.078707	-0.072533	3.533564
376.022725	4261.894843	7.083712	-0.072616	3.536844
376.442847	4269.843682	7.088717	-0.072699	3.540075
376.708542	4277.871269	7.093722	-0.072754	3.543331
377.339207	4285.920999	7.098726	-0.072877	3.546603
377.670948	4293.971068	7.103731	-0.072944	3.549863
378.138990	4302.046217	7.108736	-0.073036	3.553135
378.546278	4310.061555	7.113741	-0.073117	3.556378
378.926934	4318.035990	7.118746	-0.073193	3.559600
379.314313	4326.050715	7.123750	-0.073271	3.562835
379.399487	4334.082428	7.128755	-0.073292	3.566066
380.024615	4342.074741	7.133760	-0.073414	3.569294
380.167089	4350.127825	7.138765	-0.073445	3.572528
380.638880	4358.134870	7.143770	-0.073539	3.575751
381.107218	4366.140259	7.148774	-0.073631	3.578971
381.468107	4374.163396	7.153779	-0.073703	3.582191
381.472057	4382.235201	7.158784	-0.073710	3.585417
381.877053	4390.269027	7.163789	-0.073790	3.588638
382.200230	4398.295933	7.168794	-0.073856	3.591849
382.524460	4406.313646	7.173798	-0.073921	3.595055
382.653554	4414.327081	7.178803	-0.073951	3.598250
383.047081	4422.381767	7.183808	-0.074029	3.601466
383.379185	4430.395673	7.188813	-0.074096	3.604661
383.810759	4438.388387	7.193818	-0.074182	3.607848
384.094449	4446.499053	7.198822	-0.074240	3.611075
384.139785	4454.483074	7.203827	-0.074254	3.614242
384.507790	4462.524200	7.208832	-0.074328	3.617437
384.767815	4470.555118	7.213837	-0.074381	3.620623
385.091068	4478.500231	7.218842	-0.074447	3.623774
385.566313	4486.583065	7.223846	-0.074541	3.626980
385.823921	4494.600956	7.228851	-0.074594	3.630152
385.750291	4502.659831	7.233856	-0.074585	3.633328
386.314388	4510.641671	7.238861	-0.074696	3.636489
386.426230	4518.621438	7.243866	-0.074722	3.639634
386.887240	4526.624835	7.248870	-0.074813	3.642794
387.100164	4534.721992	7.253875	-0.074858	3.645982
387.267080	4542.707854	7.258880	-0.074894	3.649122
387.482709	4550.765743	7.263885	-0.074940	3.652289
387.741069	4558.785516	7.268890	-0.074993	3.655440
388.155266	4566.803091	7.273894	-0.075075	3.658591
388.208263	4574.828869	7.278899	-0.075091	3.661732
388.588031	4582.817404	7.283904	-0.075167	3.664866
388.847762	4590.872408	7.288909	-0.075220	3.668019
388.931183	4598.903370	7.293914	-0.075241	3.671155
389.350893	4606.894960	7.298918	-0.075324	3.674282
389.590807	4614.930699	7.303923	-0.075374	3.677419
389.641141	4622.991151	7.308928	-0.075389	3.680558
390.148800	4630.982457	7.313933	-0.075489	3.683680
390.400415	4639.013401	7.318938	-0.075541	3.686807
390.799523	4647.045339	7.323942	-0.075621	3.689936
390.853257	4655.077762	7.328947	-0.075636	3.693053
391.274144	4663.144715	7.333952	-0.075720	3.696191
391.517393	4671.155611	7.338957	-0.075770	3.699299
391.455506	4679.175177	7.343962	-0.075764	3.702401
391.985668	4687.166864	7.348966	-0.075868	3.705504
392.412597	4695.161838	7.353971	-0.075953	3.708603
392.749431	4703.253827	7.358976	-0.076021	3.711735
393.322758	4711.300750	7.363981	-0.076133	3.714853
393.324031	4719.276423	7.368986	-0.076138	3.717926
393.774874	4727.310334	7.373990	-0.076227	3.721030
394.216984	4735.242113	7.378995	-0.076315	3.724092
394.282472	4743.306773	7.384000	-0.076333	3.727193
394.733838	4751.333572	7.389005	-0.076422	3.730287
394.943496	4759.368261	7.394010	-0.076466	3.733374
395.542290	4767.391882	7.399014	-0.076583	3.736465
395.348491	4775.442512	7.404019	-0.076552	3.739544
395.488476	4783.443163	7.409024	-0.076584	3.742610
395.679315	4791.502723	7.414029	-0.076624	3.745696
395.963542	4799.505023	7.419034	-0.076683	3.748761
396.378547	4807.531040	7.424038	-0.076765	3.751835
396.830468	4815.511543	7.429043	-0.076855	3.754890
397.386973	4823.469190	7.434048	-0.076963	3.757937
397.574540	4831.588039	7.439053	-0.077004	3.761033
397.614006	4839.527630	7.444058	-0.077016	3.764055
397.986182	4847.626922	7.449062	-0.077091	3.767144
398.147476	4855.662351	7.454067	-0.077126	3.770200
398.439572	4863.646862	7.459072	-0.077186	3.773238
398.950838	4871.663038	7.464077	-0.077286	3.776290
398.706563	4879.726106	7.469082	-0.077246	3.779340
399.291633	4887.726268	7.474086	-0.077360	3.782383
399.559826	4895.706399	7.479091	-0.077416	3.785409
400.087172	4903.731678	7.484096	-0.077519	3.788455
400.318912	4911.842082	7.489101	-0.077567	3.791524
400.388931	4919.802688	7.494106	-0.077586	3.794530
400.878190	4927.811269	7.499110	-0.077682	3.797561
400.953869	4935.868910	7.504115	-0.077702	3.800599
401.411346	4943.818758	7.509120	-0.077792	3.803603
401.540752	4951.922673	7.514125	-0.077821	3.806655
401.815394	4959.901485	7.519130	-0.077878	3.809660
402.118934	4967.962329	7.524134	-0.077940	3.812695
402.298650	4975.988844	7.529139	-0.077978	3.815711
402.270684	4984.009971	7.534144	-0.077978	3.818719
402.813857	4992.049470	7.539149	-0.078085	3.821743
402.868738	5000.045963	7.544154	-0.078100	3.824739
402.872979	5008.154415	7.549158	-0.078106	3.827772
403.429337	5016.131699	7.554163	-0.078215	3.830767
403.792139	5024.079949	7.559168	-0.078288	3.833743
403.911443	5032.188455	7.564173	-0.078316	3.836772
404.225648	5040.128821	7.569178	-0.078379	3.839741
404.866209	5048.165570	7.574182	-0.078504	3.842749
405.175818	5056.169251	7.579187	-0.078567	3.845736
405.316297	5064.193200	7.584192	-0.078598	3.848724
405.470210	5072.294095	7.589197	-0.078632	3.851739
405.770029	5080.250164	7.594202	-0.078693	3.854701
406.168785	5088.315412	7.599206	-0.078773	3.857703
406.206271	5096.334316	7.604211	-0.078785	3.860678
406.497110	5104.296256	7.609216	-0.078845	3.863635
406.704573	5112.411648	7.614221	-0.078889	3.866645
406.685690	5120.412783	7.619226	-0.078890	3.869605
406.805503	5128.577861	7.624230	-0.078918	3.872626
407.380412	5136.516944	7.629235	-0.079030	3.875571
407.728906	5144.413961	7.634240	-0.079100	3.878494
408.347725	5152.427461	7.639245	-0.079221	3.881463
408.403665	5160.428367	7.644250	-0.079236	3.884413
408.711787	5168.482606	7.649254	-0.079299	3.887386
408.937108	5176.488274	7.654259	-0.079346	3.890337
409.312737	5184.484296	7.659264	-0.079422	3.893285
409.322594	5192.604988	7.664269	-0.079429	3.896269
409.759253	5200.469831	7.669274	-0.079515	3.899166
410.243546	5208.587554	7.674278	-0.079611	3.902154
410.526961	5216.567459	7.679283	-0.079669	3.905085
410.545819	5224.623905	7.684288	-0.079678	3.908037
410.768989	5232.697752	7.689293	-0.079724	3.910997
411.200308	5240.606252	7.694298	-0.079810	3.913898
411.274817	5248.750736	7.699302	-0.079829	3.916876
411.614810	5256.673692	7.704307	-0.079898	3.919777
411.690389	5264.737211	7.709312	-0.079917	3.922721
411.704476	5272.824604	7.714317	-0.079925	3.925671
411.851812	5280.783450	7.719322	-0.079958	3.928574
412.280764	5288.866572	7.724326	-0.080043	3.931526
412.248851	5296.885383	7.729331	-0.080042	3.934443
412.543171	5304.840931	7.734336	-0.080102	3.937341
412.908244	5312.851278	7.739341	-0.080176	3.940258
413.291235	5320.854764	7.744346	-0.080252	3.943171
413.560771	5328.922635	7.749350	-0.080308	3.946103
413.744157	5336.948446	7.754355	-0.080347	3.949016
414.048541	5345.007779	7.759360	-0.080409	3.951941
414.483570	5353.008832	7.764365	-0.080495	3.954845
414.762475	5361.004795	7.769370	-0.080553	3.957742
414.931945	5369.069242	7.774374	-0.080589	3.960660
415.121325	5376.999501	7.779379	-0.080630	3.963527
415.234271	5385.023320	7.784384	-0.080656	3.966425
415.660392	5393.084364	7.789389	-0.080741	3.969340
415.898650	5401.113963	7.794394	-0.080791	3.972238
416.155106	5409.139103	7.799398	-0.080844	3.975132
416.517677	5417.100805	7.804403	-0.080916	3.978003
416.764874	5425.173912	7.809408	-0.080968	3.980911
416.981643	5433.160632	7.814413	-0.081013	3.983784
416.837237	5441.201071	7.819418	-0.080992	3.986669
417.303705	5449.194451	7.824422	-0.081084	3.989545
417.526233	5457.264702	7.829427	-0.081131	3.992442
417.684801	5465.277711	7.834432	-0.081165	3.995315
418.137976	5473.206697	7.839437	-0.081255	3.998162
418.553160	5481.248959	7.844442	-0.081338	4.001046
418.956586	5489.199913	7.849446	-0.081418	4.003895
418.947287	5497.336904	7.854451	-0.081422	4.006801
419.171904	5505.356909	7.859456	-0.081469	4.009668
419.522302	5513.405808	7.864461	-0.081539	4.012545
419.718963	5521.403789	7.869466	-0.081581	4.015399
420.042277	5529.399088	7.874470	-0.081646	4.018252
420.150871	5537.446034	7.879475	-0.081672	4.021118
420.254198	5545.396283	7.884480	-0.081696	4.023948
420.390331	5553.516757	7.889485	-0.081727	4.026836
420.791112	5561.482543	7.894490	-0.081807	4.029672
421.099353	5569.584999	7.899494	-0.081870	4.032553
421.474567	5577.587355	7.904499	-0.081945	4.035397
421.842516	5585.554429	7.909504	-0.082019	4.038226
422.237639	5593.609820	7.914509	-0.082098	4.041085
422.343783	5601.510925	7.919514	-0.082123	4.043883
422.614904	5609.612504	7.924518	-0.082178	4.046753
422.991651	5617.580995	7.929523	-0.082254	4.049575
423.185502	5625.656058	7.934528	-0.082295	4.052429
423.416154	5633.710525	7.939533	-0.082343	4.055275
423.557299	5641.709097	7.944538	-0.082375	4.058098
423.979819	5649.758779	7.949542	-0.082459	4.060942
423.928055	5657.775223	7.954547	-0.082455	4.063764
424.103281	5665.819478	7.959552	-0.082492	4.066597
424.193940	5673.841050	7.964557	-0.082515	4.069420
424.592333	5681.815217	7.969562	-0.082594	4.072228
424.912931	5689.830357	7.974566	-0.082659	4.075047
425.245545	5697.825768	7.979571	-0.082726	4.077858
425.400516	5705.826242	7.984576	-0.082760	4.080666
425.604267	5713.857008	7.989581	-0.082804	4.083483
425.701550	5721.939730	7.994586	-0.082827	4.086315
426.196374	5729.900193	7.999590	-0.082924	4.089108
426.492367	5737.969121	8.004595	-0.082985	4.091934
426.848573	5745.908147	8.009600	-0.083056	4.094714
427.245474	5753.971800	8.014605	-0.083136	4.097536
427.083433	5761.998424	8.019610	-0.083111	4.100334
427.507529	5769.994385	8.024614	-0.083195	4.103129
427.791977	5778.060710	8.029619	-0.083253	4.105944
428.312375	5786.020183	8.034624	-0.083355	4.108723
428.534969	5794.093977	8.039629	-0.083402	4.111536
428.939939	5802.053068	8.044634	-0.083483	4.114310
429.335176	5810.098065	8.049638	-0.083562	4.117111
429.630990	5818.105831	8.054643	-0.083622	4.119896
429.698469	5826.110910	8.059648	-0.083640	4.122675
430.366063	5834.126170	8.064653	-0.083769	4.125464
430.300756	5842.134745	8.069658	-0.083763	4.128239
430.732895	5850.175663	8.074662	-0.083848	4.131030
430.666583	5858.232135	8.079667	-0.083841	4.133818
430.965205	5866.245910	8.084672	-0.083902	4.136593
431.324318	5874.267442	8.089677	-0.083974	4.139371
431.868904	5882.202585	8.094682	-0.084081	4.142119
432.079596	5890.248854	8.099686	-0.084125	4.144899
432.124530	5898.287748	8.104691	-0.084139	4.147672
432.182620	5906.340624	8.109696	-0.084155	4.150449
432.371731	5914.385057	8.114701	-0.084196	4.153223
432.726936	5922.355415	8.119706	-0.084267	4.155971
433.080971	5930.345771	8.124710	-0.084338	4.158724
433.249775	5938.383685	8.129715	-0.084375	4.161490
433.464223	5946.329938	8.134720	-0.084420	4.164222
433.740975	5954.439378	8.139725	-0.084477	4.167010
433.596259	5962.471019	8.144730	-0.084455	4.169764
434.182667	5970.493051	8.149734	-0.084570	4.172522
434.324342	5978.512547	8.154739	-0.084601	4.175271
434.464164	5986.507363	8.159744	-0.084633	4.178010
435.043655	5994.574375	8.164749	-0.084746	4.180778
435.312052	6002.526201	8.169754	-0.084801	4.183500
435.739104	6010.568357	8.174758	-0.084886	4.186253
435.986547	6018.563590	8.179763	-0.084937	4.188987
436.154852	6026.669329	8.184768	-0.084974	4.191755
436.483723	6034.693593	8.189773	-0.085041	4.194496
436.484904	6042.703077	8.194778	-0.085046	4.197225
436.839384	6050.716097	8.199782	-0.085117	4.199959
437.539992	6058.640448	8.204787	-0.085253	4.202664
437.671091	6066.672503	8.209792	-0.085283	4.205398
438.125494	6074.729581	8.214797	-0.085373	4.208142
438.344979	6082.733565	8.219802	-0.085419	4.210863
438.562554	6090.759445	8.224806	-0.085465	4.213590
438.815936	6098.824451	8.229811	-0.085517	4.216329
438.919549	6106.789984	8.234816	-0.085542	4.219031
439.375998	6114.831502	8.239821	-0.085632	4.221760
439.155428	6122.783574	8.244826	-0.085596	4.224451
439.663752	6130.854361	8.249830	-0.085696	4.227187
440.125132	6138.894194	8.254835	-0.085787	4.229911
440.251882	6146.881385	8.259840	-0.085816	4.232611
441.012293	6154.905095	8.264845	-0.085963	4.235329
441.217803	6162.904981	8.269850	-0.086006	4.238031
441.342053	6170.962533	8.274854	-0.086035	4.240750
441.464467	6178.901216	8.279859	-0.086063	4.243427
441.957113	6186.945119	8.284864	-0.086160	4.246142
442.032682	6195.004024	8.289869	-0.086179	4.248855
442.346945	6202.995144	8.294874	-0.086243	4.251547
442.717669	6211.052970	8.299878	-0.086317	4.254259
442.848459	6219.053394	8.304883	-0.086347	4.256949
442.851924	6227.084024	8.309888	-0.086353	4.259645
443.076652	6235.102206	8.314893	-0.086400	4.262338
443.518857	6243.036449	8.319898	-0.086488	4.265003
443.865122	6251.091327	8.324902	-0.086557	4.267706
444.174404	6259.128261	8.329907	-0.086620	4.270400
444.276056	6267.145434	8.334912	-0.086644	4.273084
444.588927	6275.204766	8.339917	-0.086708	4.275783
444.705912	6283.122455	8.344922	-0.086735	4.278431
444.979883	6291.218416	8.349926	-0.086791	4.281138
445.485034	6299.147747	8.354931	-0.086891	4.283790
445.615544	6307.213089	8.359936	-0.086920	4.286482
446.034200	6315.184033	8.364941	-0.087003	4.289143
446.200786	6323.256800	8.369946	-0.087040	4.291835
446.388502	6331.265691	8.374950	-0.087080	4.294504
446.555773	6339.292384	8.379955	-0.087116	4.297176
446.778582	6347.304860	8.384960	-0.087163	4.299843
447.148673	6355.318598	8.389965	-0.087237	4.302510
447.242006	6363.317310	8.394970	-0.087260	4.305168
447.689861	6371.374062	8.399974	-0.087349	4.307846
448.203644	6379.441884	8.404979	-0.087450	4.310527
448.509131	6387.380765	8.409984	-0.087512	4.313162
448.840057	6395.446527	8.414989	-0.087579	4.315837
448.976594	6403.361907	8.419994	-0.087609	4.318459
449.179542	6411.494752	8.424998	-0.087653	4.321152
449.224131	6419.392986	8.430003	-0.087666	4.323765
449.748943	6427.453569	8.435008	-0.087769	4.326433
450.185166	6435.420305	8.440013	-0.087856	4.329068
450.530821	6443.544649	8.445018	-0.087925	4.331753
450.571585	6451.517588	8.450022	-0.087938	4.334383
450.838638	6459.568732	8.455027	-0.087993	4.337040
451.180438	6467.536950	8.460032	-0.088062	4.339668
451.396077	6475.606928	8.465037	-0.088107	4.342327
451.611980	6483.541493	8.470042	-0.088153	4.344940
451.929023	6491.606838	8.475046	-0.088217	4.347595
451.953644	6499.641029	8.480051	-0.088227	4.350235
452.262125	6507.682387	8.485056	-0.088290	4.352879
452.714266	6515.757005	8.490061	-0.088379	4.355533
452.810947	6523.667424	8.495066	-0.088403	4.358129
453.071199	6531.685752	8.500070	-0.088456	4.360760
453.246605	6539.678446	8.505075	-0.088494	4.363380
453.606571	6547.695954	8.510080	-0.088567	4.366008
453.800827	6555.752457	8.515085	-0.088608	4.368647
454.203021	6563.756126	8.520090	-0.088688	4.371267
454.387763	6571.746317	8.525094	-0.088728	4.373880
454.560762	6579.842937	8.530099	-0.088765	4.376526
454.552113	6587.801857	8.535104	-0.088769	4.379125
454.942754	6595.887685	8.540109	-0.088847	4.381766
454.823275	6603.834476	8.545114	-0.088830	4.384356
454.996121	6611.915305	8.550118	-0.088868	4.386991
455.483671	6619.918252	8.555123	-0.088964	4.389601
455.798755	6627.884389	8.560128	-0.089027	4.392196
456.013990	6635.935029	8.565133	-0.089073	4.394816
456.017746	6643.972458	8.570138	-0.089079	4.397429
456.660414	6651.983547	8.575143	-0.089204	4.400036
456.624381	6659.996782	8.580147	-0.089202	4.402638
457.110551	6667.989825	8.585152	-0.089298	4.405235
457.270412	6676.037970	8.590157	-0.089333	4.407846
457.371116	6684.116101	8.595162	-0.089357	4.410465
457.677135	6692.112551	8.600167	-0.089420	4.413057
457.935017	6700.179302	8.605171	-0.089473	4.415670
458.134346	6708.148681	8.610176	-0.089515	4.418250
458.589541	6716.218874	8.615181	-0.089605	4.420862
458.709235	6724.141216	8.620186	-0.089633	4.423423
458.950551	6732.240214	8.625191	-0.089683	4.426040
459.132813	6740.280265	8.630195	-0.089722	4.428637
459.154863	6748.300618	8.635200	-0.089732	4.431224
459.526471	6756.285182	8.640205	-0.089806	4.433801
459.880357	6764.288396	8.645210	-0.089877	4.436381
460.181326	6772.260399	8.650215	-0.089939	4.438950
460.452959	6780.335605	8.655219	-0.089994	4.441550
460.732616	6788.243689	8.660224	-0.090052	4.444095
460.952177	6796.375911	8.665229	-0.090098	4.446711
461.318285	6804.330033	8.670234	-0.090171	4.449268
461.749650	6812.412418	8.675239	-0.090257	4.451865
461.775633	6820.386861	8.680243	-0.090267	4.454424
461.811169	6828.416405	8.685248	-0.090279	4.457000
462.292596	6836.447239	8.690253	-0.090374	4.459576
462.371072	6844.469033	8.695258	-0.090394	4.462146
462.745326	6852.416318	8.700263	-0.090469	4.464692
463.128546	6860.481392	8.705267	-0.090545	4.467274
463.186110	6868.459935	8.710272	-0.090561	4.469826
463.379829	6876.580031	8.715277	-0.090603	4.472422
463.504953	6884.492677	8.720282	-0.090631	4.474949
463.813946	6892.537618	8.725287	-0.090694	4.477519
464.204920	6900.543212	8.730291	-0.090772	4.480075
464.523339	6908.544643	8.735296	-0.090837	4.482627
464.542884	6916.576947	8.740301	-0.090846	4.485187
464.600708	6924.585942	8.745306	-0.090862	4.487738
464.802344	6932.599792	8.750311	-0.090905	4.490289
465.323012	6940.601830	8.755315	-0.091007	4.492837
465.510246	6948.598672	8.760320	-0.091047	4.495380
465.798784	6956.709063	8.765325	-0.091106	4.497958
465.817308	6964.673796	8.770330	-0.091115	4.500488
466.256169	6972.695550	8.775335	-0.091202	4.503035
466.468033	6980.676197	8.780339	-0.091246	4.505568
466.520439	6988.721203	8.785344	-0.091261	4.508118
467.001120	6996.755578	8.790349	-0.091356	4.510665
467.238385	7004.754726	8.795354	-0.091406	4.513199
467.471735	7012.749629	8.800359	-0.091454	4.515730
467.539692	7020.752684	8.805363	-0.091472	4.518262
467.685709	7028.803980	8.810368	-0.091505	4.520808
467.966733	7036.755837	8.815373	-0.091562	4.523321
468.079008	7044.806724	8.820378	-0.091589	4.525863
468.465183	7052.836019	8.825383	-0.091666	4.528398
468.639373	7060.876759	8.830387	-0.091703	4.530935
468.771530	7068.846156	8.835392	-0.091733	4.533448
469.040271	7076.909107	8.840397	-0.091789	4.535989
469.207917	7084.858495	8.845402	-0.091825	4.538492
469.440473	7092.960685	8.850407	-0.091874	4.541043
469.662343	7100.867048	8.855411	-0.091920	4.543530
469.866633	7108.960762	8.860416	-0.091964	4.546075
469.863557	7116.989042	8.865421	-0.091968	4.548597
470.079821	7125.015258	8.870426	-0.092014	4.551118
470.727554	7132.956470	8.875431	-0.092140	4.553611
471.062059	7141.047770	8.880435	-0.092207	4.556150
471.338668	7148.958801	8.885440	-0.092264	4.558630
471.422521	7157.075823	8.890445	-0.092285	4.561173
471.742145	7164.972574	8.895450	-0.092350	4.563646
471.837963	7173.114557	8.900455	-0.092373	4.566195
471.904841	7181.051625	8.905459	-0.092391	4.568677
472.289489	7189.143138	8.910464	-0.092468	4.571207
472.489755	7197.114331	8.915469	-0.092510	4.573698
472.507385	7205.139896	8.920474	-0.092519	4.576204
472.737668	7213.127800	8.925479	-0.092567	4.578697
472.951107	7221.197330	8.930483	-0.092612	4.581215
473.087097	7229.119473	8.935488	-0.092642	4.583684
473.463915	7237.217300	8.940493	-0.092718	4.586208
473.647600	7245.210230	8.945498	-0.092757	4.588697
473.449069	7253.332512	8.950503	-0.092726	4.591225
473.673393	7261.226697	8.955507	-0.092773	4.593680
474.195433	7269.270799	8.960512	-0.092875	4.596182
474.142252	7277.273190	8.965517	-0.092871	4.598668
474.418606	7285.286899	8.970522	-0.092927	4.601157
474.467112	7293.248389	8.975527	-0.092942	4.603628
474.754843	7301.305129	8.980531	-0.093000	4.606128
475.003912	7309.284878	8.985536	-0.093052	4.608602
475.170036	7317.369999	8.990541	-0.093088	4.611107
475.305158	7325.300338	8.995546	-0.093119	4.613563
475.995774	7333.370055	9.000551	-0.093253	4.616061
475.899015	7341.412530	9.005555	-0.093240	4.618549
475.944622	7349.438883	9.010560	-0.093254	4.621031
476.025937	7357.428093	9.015565	-0.093274	4.623500
476.043797	7365.432812	9.020570	-0.093283	4.625972
476.321602	7373.421329	9.025575	-0.093340	4.628438
476.793962	7381.467708	9.030579	-0.093433	4.630921
477.155711	7389.439674	9.035584	-0.093506	4.633379
477.371217	7397.532615	9.040589	-0.093551	4.635873
477.542904	7405.510384	9.045594	-0.093588	4.638331
477.719574	7413.561437	9.050599	-0.093626	4.640809
477.827677	7421.471724	9.055603	-0.093652	4.643243
478.082774	7429.555847	9.060608	-0.093705	4.645729
478.545957	7437.574415	9.065613	-0.093796	4.648194
478.881055	7445.586151	9.070618	-0.093864	4.650655
479.156281	7453.577803	9.075623	-0.093920	4.653108
479.258816	7461.641775	9.080627	-0.093945	4.655583
479.544066	7469.584071	9.085632	-0.094003	4.658019
479.797952	7477.684426	9.090637	-0.094056	4.660502
479.754377	7485.636822	9.095642	-0.094053	4.662938
480.133046	7493.684941	9.100647	-0.094129	4.665402
480.371726	7501.684115	9.105651	-0.094178	4.667850
480.274493	7509.757258	9.110656	-0.094165	4.670320
480.778918	7517.789163	9.115661	-0.094265	4.672775
480.523010	7525.792785	9.120666	-0.094222	4.675221
480.601152	7533.790224	9.125671	-0.094242	4.677663
480.672937	7541.822555	9.130675	-0.094261	4.680115
480.606433	7549.783956	9.135680	-0.094254	4.682544
480.391636	7557.838058	9.140685	-0.094219	4.685000
480.721887	7565.812238	9.145690	-0.094286	4.687430
481.679102	7573.775685	9.150695	-0.094469	4.689854
481.998582	7581.833363	9.155699	-0.094534	4.692307
482.286279	7589.839833	9.160704	-0.094593	4.694743
482.541421	7597.911021	9.165709	-0.094646	4.697197
482.590944	7605.866402	9.170714	-0.094660	4.699615
482.581941	7613.926360	9.175719	-0.094664	4.702063
482.845737	7621.860256	9.180723	-0.094718	4.704472
482.925249	7630.005221	9.185728	-0.094738	4.706944
483.171430	7638.031867	9.190733	-0.094789	4.709378
483.196473	7646.020321	9.195738	-0.094799	4.711800
483.547274	7654.006554	9.200743	-0.094870	4.714219
483.922992	7662.044617	9.205747	-0.094945	4.716652
484.043719	7669.970881	9.210752	-0.094973	4.719051
484.158678	7678.123125	9.215757	-0.095000	4.721517
484.284792	7685.962698	9.220762	-0.095028	4.723888
484.557312	7694.068682	9.225767	-0.095084	4.726337
485.147479	7702.049911	9.230771	-0.095199	4.728746
485.121084	7710.138586	9.235776	-0.095200	4.731188
485.353353	7718.187814	9.240781	-0.095248	4.733617
485.484178	7726.148349	9.245786	-0.095278	4.736017
485.930619	7734.159983	9.250791	-0.095366	4.738431
485.987546	7742.200763	9.255795	-0.095382	4.740854
486.119166	7750.143626	9.260800	-0.095412	4.743245
486.199019	7758.250949	9.265805	-0.095432	4.745685
486.531403	7766.229691	9.270810	-0.095499	4.748084
486.541481	7774.302221	9.275815	-0.095506	4.750511
486.493057	7782.382524	9.280819	-0.095503	4.752939
486.912737	7790.315275	9.285824	-0.095586	4.755321
487.069013	7798.324607	9.290829	-0.095621	4.757725
487.417251	7806.309708	9.295834	-0.095691	4.760120
487.574265	7814.362712	9.300839	-0.095725	4.762534
487.790766	7822.336073	9.305843	-0.095771	4.764924
487.993143	7830.347783	9.310848	-0.095814	4.767323
488.600969	7838.448107	9.315853	-0.095932	4.769747
489.153848	7846.379004	9.320858	-0.096040	4.772119
489.665263	7854.420109	9.325863	-0.096141	4.774522
489.883974	7862.465410	9.330867	-0.096187	4.776927
489.894978	7870.452979	9.335872	-0.096194	4.779314
490.599145	7878.498400	9.340877	-0.096331	4.781714
490.746086	7886.420381	9.345882	-0.096363	4.784078
490.839196	7894.542484	9.350887	-0.096386	4.786501
491.242874	7902.451487	9.355891	-0.096466	4.788858
491.013308	7910.608340	9.360896	-0.096429	4.791290
491.414368	7918.531720	9.365901	-0.096509	4.793649
491.549953	7926.554433	9.370906	-0.096539	4.796038
491.704418	7934.557311	9.375911	-0.096573	4.798419
491.950887	7942.606359	9.380915	-0.096625	4.800812
492.037572	7950.588115	9.385920	-0.096646	4.803185
492.465255	7958.644588	9.390925	-0.096731	4.805577
492.457877	7966.584788	9.395930	-0.096735	4.807936
492.608936	7974.677273	9.400935	-0.096768	4.810337
493.170034	7982.655360	9.405939	-0.096878	4.812702
493.377697	7989.965051	9.410944	-0.096921	4.814869
493.688616	7994.645184	9.415949	-0.096982	4.816256

493.645533	7997.112533	9.420954	-0.096976	4.816987
493.844713	7998.552292	9.425959	-0.097014	4.817413
493.464608	7999.015695	9.430963	-0.096944	4.817552
493.647333	7999.752635	9.435968	-0.096978	4.817769
493.873162	7999.761131	9.440973	-0.097020	4.817771
493.927172	7999.742942	9.445978	-0.097030	4.817765
494.026400	7999.769648	9.450983	-0.097049	4.817773
494.080632	7999.777802	9.455987	-0.097059	4.817775
494.044757	7999.781508	9.460992	-0.097053	4.817776
494.607984	7999.770591	9.465997	-0.097157	4.817771
494.456107	7999.743139	9.471002	-0.097129	4.817763
494.795523	7999.754312	9.476007	-0.097192	4.817765
494.682538	7999.737952	9.481011	-0.097171	4.817761
494.716292	7999.758457	9.486016	-0.097178	4.817767
494.847569	7999.760336	9.491021	-0.097202	4.817767
494.560808	7999.752030	9.496026	-0.097149	4.817765
494.985883	7999.796035	9.501031	-0.097228	4.817777
495.207691	7999.756010	9.506035	-0.097270	4.817764
495.471987	7999.732395	9.511040	-0.097319	4.817756
495.521688	7999.762611	9.516045	-0.097328	4.817764
495.597000	7999.751048	9.521050	-0.097342	4.817761
495.717710	7999.792815	9.526055	-0.097365	4.817773
495.577086	7999.753932	9.531059	-0.097339	4.817762
495.622954	7999.771450	9.536064	-0.097347	4.817767
496.021364	7999.753967	9.541069	-0.097421	4.817760
495.843702	7999.728252	9.546074	-0.097388	4.817753
495.590694	7999.777323	9.551079	-0.097341	4.817768
495.920912	7999.721988	9.556083	-0.097403	4.817751
495.748346	7999.752189	9.561088	-0.097371	4.817760
496.105381	7999.759403	9.566093	-0.097437	4.817761
495.822476	7999.772222	9.571098	-0.097385	4.817766
496.088882	7999.789731	9.576103	-0.097434	4.817770
496.051150	7999.859790	9.581107	-0.097427	4.817791
496.023864	7999.789863	9.586112	-0.097422	4.817770
496.263506	7999.774327	9.591117	-0.097467	4.817765
496.158231	7999.845528	9.596122	-0.097448	4.817786
496.386609	7999.769773	9.601127	-0.097490	4.817763
496.305213	7999.814974	9.606131	-0.097475	4.817777
496.014339	7999.799230	9.611136	-0.097421	4.817773
496.593135	7999.786435	9.616141	-0.097529	4.817767
496.488126	7999.856587	9.621146	-0.097509	4.817788
496.635791	7999.787053	9.626151	-0.097537	4.817767
496.709662	7999.857655	9.631155	-0.097551	4.817788
496.473547	7999.765776	9.636160	-0.097507	4.817761
496.877995	7999.759972	9.641165	-0.097582	4.817758
496.811593	7999.832783	9.646170	-0.097570	4.817780
496.514404	7999.869631	9.651175	-0.097514	4.817792
496.675658	7999.795023	9.656179	-0.097544	4.817769
496.564893	7999.802926	9.661184	-0.097524	4.817772
496.658181	7999.805318	9.666189	-0.097541	4.817772
496.902141	7999.783522	9.671194	-0.097587	4.817765
496.886270	7999.805426	9.676199	-0.097584	4.817771
496.932850	7999.769218	9.681203	-0.097593	4.817760
496.849025	7999.879712	9.686208	-0.097577	4.817793
496.955894	7999.804326	9.691213	-0.097597	4.817771
496.861362	7999.785067	9.696218	-0.097579	4.817765
497.052613	7999.807825	9.701223	-0.097615	4.817771
497.275032	7999.787829	9.706227	-0.097657	4.817764
497.193978	7999.795103	9.711232	-0.097642	4.817767
497.157103	7999.785097	9.716237	-0.097635	4.817764
497.293766	7999.790216	9.721242	-0.097660	4.817765
497.081429	7999.895712	9.726247	-0.097621	4.817797
497.007438	7999.771379	9.731251	-0.097607	4.817761
496.841284	7999.811154	9.736256	-0.097576	4.817773
497.447066	7999.797693	9.741261	-0.097689	4.817767
497.255907	7999.885580	9.746266	-0.097654	4.817793
497.426972	7999.777394	9.751271	-0.097685	4.817761
497.385703	7999.765218	9.756275	-0.097678	4.817757
497.180765	7999.852907	9.761280	-0.097640	4.817784
497.031685	7999.789666	9.766285	-0.097612	4.817766
497.058211	7999.779513	9.771290	-0.097617	4.817763
497.224365	7999.816664	9.776295	-0.097648	4.817773
497.011394	7999.804140	9.781299	-0.097608	4.817770
497.124287	7999.788899	9.786304	-0.097629	4.817765
497.434190	7999.803872	9.791309	-0.097687	4.817768
497.451491	7999.869452	9.796314	-0.097690	4.817788
497.277716	7999.825877	9.801319	-0.097658	4.817776
497.514169	7999.793438	9.806323	-0.097702	4.817765
497.603923	7999.787350	9.811328	-0.097719	4.817763
497.369588	7999.815613	9.816333	-0.097675	4.817772
497.372835	7999.779838	9.821338	-0.097676	4.817762
497.525662	7999.896879	9.826343	-0.097705	4.817796
497.618766	7999.817081	9.831347	-0.097722	4.817772
497.331399	7999.802439	9.836352	-0.097668	4.817768
497.564594	7999.817368	9.841357	-0.097712	4.817772
497.406126	7999.786657	9.846362	-0.097682	4.817763
497.503814	7999.834420	9.851367	-0.097701	4.817777
497.513556	7999.783986	9.856371	-0.097703	4.817762
497.808184	7999.896735	9.861376	-0.097758	4.817794
498.086559	7999.787976	9.866381	-0.097809	4.817761
497.507938	7999.782865	9.871386	-0.097702	4.817762
497.691258	7999.810779	9.876391	-0.097736	4.817769
497.872870	7999.802844	9.881395	-0.097770	4.817766
497.742756	7999.785182	9.886400	-0.097746	4.817762
498.075107	7999.808907	9.891405	-0.097808	4.817767
497.891019	7999.777828	9.896410	-0.097773	4.817759
497.506600	7999.841876	9.901415	-0.097702	4.817779
497.374923	7999.926399	9.906419	-0.097677	4.817805
497.591769	7999.836780	9.911424	-0.097718	4.817778
497.635296	7999.804743	9.916429	-0.097726	4.817768
497.198120	7999.806924	9.921434	-0.097645	4.817770
497.281245	7999.838673	9.926439	-0.097660	4.817779
497.432177	7999.853480	9.931443	-0.097688	4.817783
497.379965	7999.899100	9.936448	-0.097679	4.817797
497.651808	7999.845040	9.941453	-0.097729	4.817780
497.711037	7999.787938	9.946458	-0.097740	4.817763
497.855852	7999.829000	9.951463	-0.097767	4.817774
497.711697	7999.825888	9.956467	-0.097741	4.817774
497.754823	7999.803328	9.961472	-0.097749	4.817767
498.003502	7999.840608	9.966477	-0.097795	4.817777
498.141572	7999.787795	9.971482	-0.097821	4.817761
498.143805	7999.832086	9.976487	-0.097821	4.817774
498.038101	7999.786323	9.981491	-0.097802	4.817761
497.825693	7999.822275	9.986496	-0.097762	4.817772
497.838664	7999.822465	9.991501	-0.097765	4.817772
498.082561	7999.803830	9.996506	-0.097810	4.817766
497.996243	7999.818405	10.001511	-0.097794	4.817770
498.039849	7999.823248	10.006515	-0.097802	4.817772
498.024919	7999.800911	10.011520	-0.097799	4.817765
498.174489	7999.861008	10.016525	-0.097827	4.817782
498.130504	7999.801376	10.021530	-0.097819	4.817765
497.967472	7999.862269	10.026535	-0.097789	4.817783
498.177946	7999.871607	10.031539	-0.097828	4.817785
498.283242	7999.841506	10.036544	-0.097848	4.817776
498.383238	7999.828189	10.041549	-0.097867	4.817772
498.295141	7999.901746	10.046554	-0.097850	4.817794
498.240387	7999.850389	10.051559	-0.097840	4.817779
498.174042	7999.802027	10.056563	-0.097828	4.817765
497.805958	7999.854718	10.061568	-0.097759	4.817782
497.336917	7999.949167	10.066573	-0.097672	4.817812
497.901699	7999.838183	10.071578	-0.097777	4.817777
497.743547	7999.897039	10.076583	-0.097748	4.817795
498.103347	7999.803143	10.081587	-0.097815	4.817765
497.709485	7999.870218	10.086592	-0.097742	4.817787
497.652144	7999.884153	10.091597	-0.097731	4.817791
497.475935	7999.862670	10.096602	-0.097698	4.817786
497.330214	7999.902737	10.101607	-0.097671	4.817798
497.208229	7999.972647	10.106611	-0.097649	4.817819
497.220641	7999.877997	10.111616	-0.097651	4.817791
497.231493	7999.929787	10.116621	-0.097653	4.817807
497.555775	7999.878584	10.121626	-0.097713	4.817790
497.364024	7999.941174	10.126631	-0.097678	4.817809
497.844091	7999.857428	10.131635	-0.097767	4.817783
498.178691	7999.807427	10.136640	-0.097829	4.817766
498.368261	7999.831218	10.141645	-0.097865	4.817773
498.456428	7999.814570	10.146650	-0.097881	4.817767
498.401336	7999.829592	10.151655	-0.097871	4.817772
498.163605	7999.825141	10.156659	-0.097827	4.817772
498.162146	7999.846198	10.161664	-0.097827	4.817778
498.168894	7999.843137	10.166669	-0.097828	4.817777
498.468839	7999.798963	10.171674	-0.097884	4.817763
498.342301	7999.822445	10.176679	-0.097860	4.817770
498.324615	7999.839055	10.181683	-0.097857	4.817775
498.037889	7999.836011	10.186688	-0.097804	4.817775
498.222612	7999.852356	10.191693	-0.097838	4.817779
498.636301	7999.796111	10.196698	-0.097915	4.817761
498.626175	7999.823367	10.201703	-0.097913	4.817769
498.182826	7999.852852	10.206707	-0.097831	4.817780
498.457399	7999.842034	10.211712	-0.097882	4.817775
498.610906	7999.840020	10.216717	-0.097911	4.817774
497.888864	7999.912934	10.221722	-0.097776	4.817799
497.929134	7999.882957	10.226727	-0.097784	4.817790
498.278683	7999.918521	10.231731	-0.097849	4.817799
498.297514	7999.831336	10.236736	-0.097853	4.817773
498.264061	7999.861419	10.241741	-0.097846	4.817782
498.264597	7999.806638	10.246746	-0.097847	4.817766
498.495409	7999.843664	10.251751	-0.097890	4.817776
498.081740	7999.851447	10.256755	-0.097813	4.817780
498.509097	7999.812257	10.261760	-0.097892	4.817766
498.446265	7999.808201	10.266765	-0.097881	4.817765
498.344421	7999.782512	10.271770	-0.097862	4.817758
498.398131	7999.834916	10.276775	-0.097872	4.817773
498.543108	7999.814867	10.281779	-0.097899	4.817767
498.551677	7999.800242	10.286784	-0.097900	4.817763
498.278602	7999.863776	10.291789	-0.097850	4.817783
498.109653	7999.848718	10.296794	-0.097818	4.817779
498.157550	7999.870481	10.301799	-0.097827	4.817785
498.746411	7999.826227	10.306803	-0.097937	4.817769
498.268755	7999.926873	10.311808	-0.097848	4.817801
498.575731	7999.850135	10.316813	-0.097905	4.817777
498.434169	7999.839683	10.321818	-0.097879	4.817775
498.451286	7999.837825	10.326823	-0.097882	4.817774
498.536494	7999.843263	10.331827	-0.097898	4.817775
498.724879	7999.816459	10.336832	-0.097933	4.817767
498.830850	7999.832732	10.341837	-0.097953	4.817771
498.561280	7999.853114	10.346842	-0.097903	4.817778
498.592538	7999.883069	10.351847	-0.097909	4.817787
498.274928	7999.931213	10.356851	-0.097850	4.817803
498.695722	7999.850835	10.361856	-0.097928	4.817777
498.943276	7999.850168	10.366861	-0.097974	4.817776
498.655740	7999.823928	10.371866	-0.097921	4.817769
498.225582	7999.902073	10.376871	-0.097841	4.817794
498.454481	7999.856882	10.381875	-0.097883	4.817780
498.771130	7999.830860	10.386880	-0.097942	4.817771
498.674550	7999.857933	10.391885	-0.097924	4.817779
498.262431	7999.872059	10.396890	-0.097848	4.817785
498.129820	7999.923905	10.401895	-0.097823	4.817801
498.287080	7999.912461	10.406899	-0.097853	4.817797
498.123048	7999.884829	10.411904	-0.097822	4.817789
498.710498	7999.839501	10.416909	-0.097931	4.817773
498.661345	7999.849338	10.421914	-0.097922	4.817777
498.760354	7999.833900	10.426919	-0.097941	4.817772
498.503319	7999.805990	10.431923	-0.097893	4.817764
498.611748	7999.808600	10.436928	-0.097913	4.817765
498.634692	7999.863725	10.441933	-0.097918	4.817781
498.611546	7999.883419	10.446938	-0.097913	4.817787
498.715552	7999.832225	10.451943	-0.097933	4.817771
498.929739	7999.843725	10.456947	-0.097973	4.817774
498.794640	7999.813345	10.461952	-0.097948	4.817765
499.145695	7999.822589	10.466957	-0.098013	4.817767
498.943080	7999.830230	10.471962	-0.097975	4.817770
498.940676	7999.821770	10.476967	-0.097975	4.817767
498.907544	7999.805494	10.481971	-0.097969	4.817763
499.107187	7999.870525	10.486976	-0.098006	4.817781
499.085534	7999.822802	10.491981	-0.098002	4.817767
499.098005	7999.786104	10.496986	-0.098004	4.817756
499.102047	7999.792488	10.501991	-0.098005	4.817758
499.088250	7999.880807	10.506995	-0.098003	4.817784
499.124644	7999.790712	10.512000	-0.098010	4.817757
498.905135	7999.864496	10.517005	-0.097969	4.817780
499.121500	7999.792783	10.522010	-0.098009	4.817758
499.229615	7999.810140	10.527015	-0.098029	4.817763
499.207632	7999.811937	10.532019	-0.098025	4.817763
499.188553	7999.882268	10.537024	-0.098022	4.817784
499.386423	7999.810290	10.542029	-0.098059	4.817762
499.268859	7999.769623	10.547034	-0.098037	4.817750
499.449183	7999.815411	10.552039	-0.098070	4.817763
499.302997	7999.913427	10.557043	-0.098043	4.817793
499.043918	7999.810672	10.562048	-0.097995	4.817763
498.956145	7999.851568	10.567053	-0.097979	4.817776
499.247037	7999.789352	10.572058	-0.098033	4.817756
499.270164	7999.837105	10.577063	-0.098037	4.817770
499.540130	7999.810416	10.582067	-0.098088	4.817761
499.364519	7999.797368	10.587072	-0.098055	4.817758
499.342624	7999.833939	10.592077	-0.098051	4.817769
499.227703	7999.801740	10.597082	-0.098030	4.817760
499.438418	7999.817406	10.602087	-0.098069	4.817764
499.641197	7999.884591	10.607091	-0.098107	4.817783
499.528949	7999.792367	10.612096	-0.098086	4.817756
499.529470	7999.816614	10.617101	-0.098086	4.817763
499.656003	7999.781549	10.622106	-0.098110	4.817752
499.542416	7999.832613	10.627111	-0.098089	4.817768
499.572446	7999.779307	10.632115	-0.098094	4.817752
499.372924	7999.891311	10.637120	-0.098057	4.817786
499.560273	7999.816022	10.642125	-0.098092	4.817763
499.406199	7999.772724	10.647130	-0.098063	4.817751
499.459025	7999.823010	10.652135	-0.098073	4.817765
499.679131	7999.805091	10.657139	-0.098114	4.817759
499.534627	7999.856766	10.662144	-0.098087	4.817775
499.466378	7999.813644	10.667149	-0.098075	4.817763
499.445323	7999.819669	10.672154	-0.098071	4.817764
499.608956	7999.798834	10.677159	-0.098101	4.817758
499.455026	7999.804010	10.682163	-0.098073	4.817760
499.509605	7999.787936	10.687168	-0.098083	4.817755
499.492080	7999.818247	10.692173	-0.098080	4.817764
499.574330	7999.800462	10.697178	-0.098095	4.817758
499.615809	7999.829510	10.702183	-0.098103	4.817767
499.402872	7999.837003	10.707187	-0.098063	4.817770
499.374265	7999.905090	10.712192	-0.098058	4.817790
499.519765	7999.810234	10.717197	-0.098085	4.817761
499.521395	7999.772327	10.722202	-0.098086	4.817750
499.592068	7999.798633	10.727207	-0.098099	4.817758
499.665405	7999.812331	10.732211	-0.098113	4.817761
499.661300	7999.825975	10.737216	-0.098112	4.817765
500.010811	7999.872080	10.742221	-0.098177	4.817778
499.779547	7999.786581	10.747226	-0.098134	4.817753
499.789676	7999.835202	10.752231	-0.098136	4.817768
499.558649	7999.846650	10.757235	-0.098093	4.817772
500.001098	7999.777121	10.762240	-0.098175	4.817749
499.913418	7999.821180	10.767245	-0.098159	4.817763
499.849138	7999.886649	10.772250	-0.098147	4.817783
499.973340	7999.784111	10.777255	-0.098170	4.817752
499.902650	7999.809447	10.782259	-0.098157	4.817759
499.869780	7999.807927	10.787264	-0.098151	4.817759
499.902429	7999.814721	10.792269	-0.098157	4.817761
499.781249	7999.879375	10.797274	-0.098135	4.817781
499.761521	7999.790583	10.802279	-0.098131	4.817754
499.775660	7999.786574	10.807283	-0.098134	4.817753
499.745722	7999.830407	10.812288	-0.098128	4.817766
499.839749	7999.876014	10.817293	-0.098146	4.817779
499.580953	7999.812249	10.822298	-0.098098	4.817762
499.869203	7999.816381	10.827303	-0.098152	4.817762
499.858610	7999.797266	10.832307	-0.098150	4.817756
499.779685	7999.780334	10.837312	-0.098135	4.817751
499.732896	7999.908224	10.842317	-0.098126	4.817789
499.692640	7999.786472	10.847322	-0.098119	4.817753
499.647669	7999.829035	10.852327	-0.098111	4.817766
499.819587	7999.806211	10.857331	-0.098143	4.817759
499.898114	7999.789426	10.862336	-0.098157	4.817753
499.944170	7999.828024	10.867341	-0.098166	4.817765
499.529096	7999.892685	10.872346	-0.098089	4.817786
499.722879	7999.820649	10.877351	-0.098125	4.817763
499.680529	7999.817939	10.882355	-0.098117	4.817763
499.727821	7999.788062	10.887360	-0.098126	4.817754
500.043114	7999.819978	10.892365	-0.098185	4.817762
499.744713	7999.784097	10.897370	-0.098129	4.817753
499.808145	7999.888276	10.902375	-0.098141	4.817783
499.745425	7999.807297	10.907379	-0.098129	4.817759
499.757883	7999.804319	10.912384	-0.098132	4.817758
499.706068	7999.841515	10.917389	-0.098122	4.817770
499.723150	7999.804883	10.922394	-0.098125	4.817759
499.722556	7999.773267	10.927399	-0.098125	4.817749
500.007431	7999.873241	10.932403	-0.098178	4.817778
499.881807	7999.755534	10.937408	-0.098155	4.817743
500.161852	7999.888106	10.942413	-0.098207	4.817782
500.079740	7999.763645	10.947418	-0.098192	4.817745
500.110701	7999.833640	10.952423	-0.098198	4.817766
499.926601	7999.865781	10.957427	-0.098164	4.817776
500.026986	7999.771332	10.962432	-0.098182	4.817748
500.006121	7999.827939	10.967437	-0.098178	4.817764
499.854286	7999.878456	10.972442	-0.098150	4.817780
500.112499	7999.826310	10.977447	-0.098198	4.817763
500.181156	7999.785147	10.982451	-0.098211	4.817751
500.051118	7999.805418	10.987456	-0.098187	4.817758
500.024484	7999.818739	10.992461	-0.098182	4.817762
500.033969	7999.781998	10.997466	-0.098184	4.817751
499.769086	7999.825627	11.002471	-0.098135	4.817765
499.879450	7999.829319	11.007475	-0.098155	4.817765
500.032552	7999.897902	11.012480	-0.098184	4.817785
500.046297	7999.811695	11.017485	-0.098186	4.817759
499.840076	7999.786618	11.022490	-0.098148	4.817753
500.008800	7999.853317	11.027495	-0.098180	4.817772
500.098091	7999.799804	11.032499	-0.098196	4.817756
499.985801	7999.899360	11.037504	-0.098176	4.817786
500.047602	7999.810681	11.042509	-0.098187	4.817759
499.976898	7999.780168	11.047514	-0.098174	4.817750
499.909047	7999.832941	11.052519	-0.098161	4.817766
499.906842	7999.902461	11.057523	-0.098161	4.817787
500.052465	7999.787584	11.062528	-0.098188	4.817752
500.134769	7999.799305	11.067533	-0.098203	4.817755
500.175595	7999.805162	11.072538	-0.098211	4.817757
500.229791	7999.838609	11.077543	-0.098221	4.817767
500.312481	7999.785002	11.082547	-0.098237	4.817750
499.995865	7999.818407	11.087552	-0.098178	4.817762
500.100901	7999.832560	11.092557	-0.098197	4.817765
500.134674	7999.802489	11.097562	-0.098204	4.817756
500.070941	7999.891149	11.102567	-0.098192	4.817783
500.048845	7999.805483	11.107571	-0.098188	4.817758
500.171420	7999.793544	11.112576	-0.098211	4.817753
500.338622	7999.815964	11.117581	-0.098242	4.817759
500.109917	7999.792671	11.122586	-0.098199	4.817753
499.858034	7999.834379	11.127591	-0.098153	4.817767
500.142780	7999.821601	11.132595	-0.098206	4.817762
499.998475	7999.816377	11.137600	-0.098179	4.817761
500.107728	7999.823215	11.142605	-0.098199	4.817763
500.017059	7999.808222	11.147610	-0.098182	4.817758
500.051864	7999.887755	11.152615	-0.098189	4.817782
500.103984	7999.810528	11.157619	-0.098199	4.817759
499.975431	7999.796046	11.162624	-0.098175	4.817755
499.938720	7999.843997	11.167629	-0.098168	4.817769
499.931850	7999.794377	11.172634	-0.098167	4.817755
499.986786	7999.825726	11.177639	-0.098177	4.817764
500.192432	7999.822353	11.182643	-0.098215	4.817762
500.070207	7999.796370	11.187648	-0.098193	4.817755
500.069639	7999.817441	11.192653	-0.098193	4.817761
500.018227	7999.858859	11.197658	-0.098183	4.817773
500.235311	7999.806123	11.202663	-0.098224	4.817757
500.056269	7999.785650	11.207667	-0.098190	4.817752
500.085945	7999.773434	11.212672	-0.098196	4.817748
500.199520	7999.833020	11.217677	-0.098217	4.817765
500.076247	7999.896592	11.222682	-0.098194	4.817784
500.205491	7999.805717	11.227687	-0.098218	4.817757
500.268602	7999.791872	11.232691	-0.098230	4.817753
500.163952	7999.789324	11.237696	-0.098211	4.817752
500.186240	7999.822313	11.242701	-0.098215	4.817762
500.243725	7999.784152	11.247706	-0.098226	4.817750
500.256020	7999.887600	11.252711	-0.098228	4.817781
500.229074	7999.795541	11.257715	-0.098223	4.817754
500.048965	7999.795073	11.262720	-0.098190	4.817754
500.160942	7999.862014	11.267725	-0.098211	4.817774
500.061044	7999.909060	11.272730	-0.098192	4.817788
499.768909	7999.819526	11.277735	-0.098138	4.817763
500.054332	7999.822564	11.282739	-0.098191	4.817763
499.998089	7999.792258	11.287744	-0.098180	4.817754
500.122283	7999.811954	11.292749	-0.098204	4.817759
500.301369	7999.821899	11.297754	-0.098237	4.817761
500.346293	7999.824654	11.302759	-0.098245	4.817762
500.230835	7999.811413	11.307763	-0.098224	4.817758
500.087780	7999.808315	11.312768	-0.098197	4.817758
500.539933	7999.810580	11.317773	-0.098282	4.817757
500.343957	7999.882594	11.322778	-0.098245	4.817779
500.183455	7999.804429	11.327783	-0.098215	4.817757
500.258850	7999.813943	11.332787	-0.098229	4.817759
500.231162	7999.798798	11.337792	-0.098224	4.817755
500.221557	7999.841868	11.342797	-0.098223	4.817768
500.176789	7999.811726	11.347802	-0.098214	4.817759
500.337017	7999.820347	11.352807	-0.098244	4.817761
500.419231	7999.827851	11.357811	-0.098260	4.817763
500.240334	7999.870605	11.362816	-0.098226	4.817776
500.488765	7999.828856	11.367821	-0.098273	4.817763
500.338551	7999.820386	11.372826	-0.098245	4.817761
500.389663	7999.851681	11.377831	-0.098254	4.817770
500.417469	7999.849976	11.382835	-0.098260	4.817769
500.402164	7999.814986	11.387840	-0.098257	4.817759
500.378430	7999.837833	11.392845	-0.098252	4.817766
500.483765	7999.781389	11.397850	-0.098272	4.817748
500.451031	7999.800946	11.402855	-0.098266	4.817754
500.451577	7999.803065	11.407859	-0.098266	4.817755
500.337282	7999.921561	11.412864	-0.098245	4.817791
500.499564	7999.837481	11.417869	-0.098275	4.817765
500.319024	7999.810663	11.422874	-0.098242	4.817758
500.270549	7999.821564	11.427879	-0.098233	4.817761
500.306891	7999.821035	11.432883	-0.098239	4.817761
500.280520	7999.789049	11.437888	-0.098235	4.817752
500.293924	7999.845094	11.442893	-0.098237	4.817768
500.210684	7999.818615	11.447898	-0.098222	4.817761
500.219913	7999.839827	11.452903	-0.098223	4.817767
500.193416	7999.828914	11.457907	-0.098219	4.817764
500.155397	7999.831534	11.462912	-0.098212	4.817765
500.160962	7999.836887	11.467917	-0.098213	4.817766
500.127966	7999.871192	11.472922	-0.098207	4.817777
500.304533	7999.777834	11.477927	-0.098239	4.817748
500.322988	7999.812876	11.482931	-0.098243	4.817758
500.236377	7999.806371	11.487936	-0.098227	4.817757
500.187222	7999.846767	11.492941	-0.098218	4.817769
500.113321	7999.801455	11.497946	-0.098204	4.817756
500.324025	7999.895100	11.502951	-0.098243	4.817783
500.119069	7999.867932	11.507955	-0.098205	4.817776
500.156878	7999.792608	11.512960	-0.098212	4.817753
500.531375	7999.781115	11.517965	-0.098282	4.817748
500.454900	7999.887508	11.522970	-0.098268	4.817780
499.719275	7999.859062	11.527975	-0.098131	4.817775
500.152498	7999.850518	11.532979	-0.098212	4.817770
500.105545	7999.845634	11.537984	-0.098203	4.817769
500.493440	7999.838549	11.542989	-0.098275	4.817765
500.227832	7999.774685	11.547994	-0.098226	4.817748
500.231648	7999.815840	11.552999	-0.098227	4.817760
500.489970	7999.912275	11.558003	-0.098275	4.817787
500.428273	7999.793374	11.563008	-0.098263	4.817752
500.720404	7999.811262	11.568013	-0.098318	4.817756
500.569209	7999.783810	11.573018	-0.098290	4.817749
500.657640	7999.811424	11.578023	-0.098306	4.817757
500.483815	7999.812100	11.583027	-0.098274	4.817758
500.221741	7999.831533	11.588032	-0.098225	4.817764
500.528935	7999.842260	11.593037	-0.098282	4.817766
500.121993	7999.814306	11.598042	-0.098207	4.817760
499.982139	7999.839705	11.603047	-0.098181	4.817768
500.023926	7999.825555	11.608051	-0.098189	4.817763
500.194147	7999.838534	11.613056	-0.098220	4.817767
500.231767	7999.862260	11.618061	-0.098227	4.817773
500.225130	7999.910642	11.623066	-0.098226	4.817788
500.384591	7999.839167	11.628071	-0.098256	4.817766
500.359673	7999.826169	11.633075	-0.098251	4.817762
500.257665	7999.802583	11.638080	-0.098232	4.817756
500.163896	7999.834964	11.643085	-0.098215	4.817766
500.177296	7999.817246	11.648090	-0.098218	4.817760
500.192432	7999.842757	11.653095	-0.098220	4.817768
500.327354	7999.851016	11.658099	-0.098246	4.817770
500.102017	7999.823557	11.663104	-0.098204	4.817763
500.504040	7999.836695	11.668109	-0.098279	4.817765
500.419463	7999.802821	11.673114	-0.098263	4.817755
500.332924	7999.820554	11.678119	-0.098247	4.817761
500.414976	7999.814357	11.683123	-0.098262	4.817758
500.407551	7999.893286	11.688128	-0.098261	4.817782
500.465369	7999.835108	11.693133	-0.098272	4.817764
499.971466	7999.847006	11.698138	-0.098180	4.817770
500.240047	7999.826620	11.703143	-0.098230	4.817763
500.663641	7999.814778	11.708147	-0.098309	4.817758
500.471182	7999.809917	11.713152	-0.098273	4.817757
500.775993	7999.827987	11.718157	-0.098330	4.817761
500.594764	7999.803266	11.723162	-0.098296	4.817754
500.761471	7999.892067	11.728167	-0.098327	4.817780
500.600943	7999.821276	11.733171	-0.098297	4.817760
500.614860	7999.805673	11.738176	-0.098300	4.817755
500.686458	7999.837262	11.743181	-0.098313	4.817764
500.613309	7999.771939	11.748186	-0.098300	4.817745
500.566467	7999.810261	11.753191	-0.098291	4.817757
500.854672	7999.841792	11.758195	-0.098345	4.817765
500.627729	7999.794287	11.763200	-0.098303	4.817752
500.679099	7999.826640	11.768205	-0.098312	4.817761
500.556687	7999.809084	11.773210	-0.098290	4.817756
500.745549	7999.900310	11.778215	-0.098325	4.817783
500.299951	7999.793823	11.783219	-0.098242	4.817753
500.271872	7999.800801	11.788224	-0.098237	4.817755
500.666550	7999.831749	11.793229	-0.098310	4.817763
500.398682	7999.769959	11.798234	-0.098260	4.817745
500.403993	7999.848017	11.803239	-0.098261	4.817768
500.675257	7999.899327	11.808243	-0.098312	4.817783
500.516352	7999.799055	11.813248	-0.098282	4.817753
500.455404	7999.825583	11.818253	-0.098271	4.817762
500.406558	7999.822780	11.823258	-0.098262	4.817761
500.544320	7999.813166	11.828263	-0.098288	4.817758
500.651773	7999.825247	11.833267	-0.098308	4.817761
500.668515	7999.810739	11.838272	-0.098311	4.817756
500.704881	7999.833393	11.843277	-0.098318	4.817763
500.481673	7999.871296	11.848282	-0.098276	4.817775
500.663183	7999.832803	11.853287	-0.098310	4.817763
500.638243	7999.826128	11.858291	-0.098306	4.817761
500.802822	7999.804253	11.863296	-0.098336	4.817754
500.805726	7999.806406	11.868301	-0.098337	4.817754
500.882909	7999.799086	11.873306	-0.098351	4.817752
500.763726	7999.832157	11.878311	-0.098329	4.817762
500.770936	7999.876522	11.883315	-0.098331	4.817775
500.943629	7999.782054	11.888320	-0.098363	4.817747
501.048265	7999.820439	11.893325	-0.098382	4.817758
501.024234	7999.808507	11.898330	-0.098378	4.817754
500.839530	7999.803758	11.903335	-0.098344	4.817753
500.953064	7999.814872	11.908339	-0.098365	4.817756
500.874045	7999.794776	11.913344	-0.098350	4.817751
500.848805	7999.918764	11.918349	-0.098346	4.817788
500.763555	7999.822707	11.923354	-0.098330	4.817759
500.837813	7999.842743	11.928359	-0.098344	4.817765
500.936464	7999.794633	11.933363	-0.098362	4.817750
500.842273	7999.767997	11.938368	-0.098344	4.817743
501.013351	7999.835786	11.943373	-0.098376	4.817762
500.943014	7999.894848	11.948378	-0.098363	4.817780
500.939010	7999.819976	11.953383	-0.098363	4.817758
501.021108	7999.830641	11.958387	-0.098378	4.817761
500.993787	7999.815500	11.963392	-0.098373	4.817756
500.845742	7999.860803	11.968397	-0.098345	4.817770
500.942587	7999.820044	11.973402	-0.098364	4.817758
500.916303	7999.822833	11.978407	-0.098359	4.817759
500.939705	7999.822118	11.983411	-0.098363	4.817758
500.837852	7999.843846	11.988416	-0.098344	4.817765
500.991348	7999.859748	11.993421	-0.098373	4.817769
501.208752	7999.835470	11.998426	-0.098413	4.817761
501.010893	7999.831585	12.003431	-0.098377	4.817761
501.087563	7999.821096	12.008435	-0.098391	4.817758
500.915022	7999.814413	12.013440	-0.098359	4.817756
501.024576	7999.854976	12.018445	-0.098379	4.817768
500.694712	7999.826017	12.023450	-0.098318	4.817761
500.966188	7999.832018	12.028455	-0.098369	4.817761
500.818169	7999.855192	12.033459	-0.098341	4.817769
500.366613	7999.819222	12.038464	-0.098257	4.817760
500.774205	7999.842979	12.043469	-0.098333	4.817765
500.943638	7999.811690	12.048474	-0.098365	4.817755
500.993457	7999.883011	12.053479	-0.098374	4.817776
500.969392	7999.790992	12.058483	-0.098369	4.817749
500.797585	7999.799072	12.063488	-0.098337	4.817752
500.828940	7999.831138	12.068493	-0.098343	4.817762
500.841464	7999.794440	12.073498	-0.098346	4.817751
501.225731	7999.895844	12.078503	-0.098417	4.817779
501.182495	7999.832001	12.083507	-0.098409	4.817760
500.875983	7999.778087	12.088512	-0.098352	4.817746
501.044024	7999.830025	12.093517	-0.098384	4.817760
500.856303	7999.818910	12.098522	-0.098349	4.817758
500.938600	7999.847491	12.103527	-0.098364	4.817766
500.599432	7999.857388	12.108531	-0.098301	4.817770
500.689675	7999.816535	12.113536	-0.098318	4.817758
500.935282	7999.817950	12.118541	-0.098364	4.817757
500.965895	7999.882673	12.123546	-0.098369	4.817776
500.942663	7999.762214	12.128551	-0.098365	4.817741
500.828081	7999.902836	12.133555	-0.098344	4.817783
500.814153	7999.803586	12.138560	-0.098341	4.817753
500.995711	7999.826213	12.143565	-0.098375	4.817759
500.983060	7999.811283	12.148570	-0.098373	4.817755
500.806071	7999.847740	12.153575	-0.098340	4.817767
500.916636	7999.809285	12.158579	-0.098361	4.817755
500.895913	7999.795293	12.163584	-0.098357	4.817751
500.953479	7999.868833	12.168589	-0.098368	4.817772
500.813808	7999.812039	12.173594	-0.098342	4.817756
500.884803	7999.836244	12.178599	-0.098355	4.817763
500.943728	7999.850791	12.183603	-0.098366	4.817767
500.824597	7999.823798	12.188608	-0.098344	4.817759
500.854994	7999.830560	12.193613	-0.098350	4.817761
500.949705	7999.800308	12.198618	-0.098367	4.817752
501.105013	7999.882624	12.203623	-0.098396	4.817776
501.029884	7999.828863	12.208627	-0.098382	4.817760
500.848461	7999.799923	12.213632	-0.098349	4.817752
500.868638	7999.851851	12.218637	-0.098352	4.817768
500.905228	7999.780723	12.223642	-0.098359	4.817746
500.852758	7999.825288	12.228647	-0.098349	4.817760
501.020067	7999.846657	12.233651	-0.098381	4.817765
500.939498	7999.805463	12.238656	-0.098366	4.817753
500.923315	7999.856870	12.243661	-0.098363	4.817769
500.552215	7999.917945	12.248666	-0.098294	4.817788
500.747220	7999.825903	12.253671	-0.098330	4.817760
500.830646	7999.831318	12.258675	-0.098346	4.817762
500.971514	7999.817534	12.263680	-0.098372	4.817757
501.092174	7999.828750	12.268685	-0.098395	4.817760
500.597124	7999.809017	12.273690	-0.098302	4.817756
500.850750	7999.840052	12.278695	-0.098350	4.817764
500.920879	7999.827362	12.283699	-0.098363	4.817760
500.809110	7999.807851	12.288704	-0.098342	4.817755
500.773580	7999.817884	12.293709	-0.098335	4.817758
501.062587	7999.799899	12.298714	-0.098389	4.817751
500.988607	7999.807273	12.303719	-0.098376	4.817754
500.872302	7999.916257	12.308723	-0.098354	4.817787
500.710738	7999.796978	12.313728	-0.098324	4.817752
501.063687	7999.804146	12.318733	-0.098390	4.817753
500.674665	7999.805953	12.323738	-0.098317	4.817755
500.257236	7999.840021	12.328743	-0.098240	4.817767
500.376669	7999.857542	12.333747	-0.098262	4.817771
500.352488	7999.843501	12.338752	-0.098258	4.817767
500.205508	7999.914109	12.343757	-0.098230	4.817789
500.907223	7999.887285	12.348762	-0.098361	4.817778
500.902306	7999.833476	12.353767	-0.098360	4.817762
501.248955	7999.814210	12.358771	-0.098425	4.817755
500.959912	7999.814288	12.363776	-0.098371	4.817756
500.837574	7999.865227	12.368781	-0.098348	4.817772
500.548211	7999.822097	12.373786	-0.098294	4.817760
500.524257	7999.848102	12.378791	-0.098290	4.817768
501.091518	7999.822512	12.383795	-0.098396	4.817758
500.604729	7999.822918	12.388800	-0.098305	4.817760
500.865285	7999.849838	12.393805	-0.098354	4.817767
501.051230	7999.831431	12.398810	-0.098388	4.817761
501.168302	7999.849973	12.403815	-0.098410	4.817766
501.291337	7999.841203	12.408819	-0.098433	4.817763
500.984123	7999.808353	12.413824	-0.098376	4.817754
501.112438	7999.848131	12.418829	-0.098400	4.817765
500.684912	7999.817773	12.423834	-0.098320	4.817758
500.022002	7999.912603	12.428839	-0.098197	4.817789
500.516921	7999.881762	12.433843	-0.098289	4.817778
500.848470	7999.805376	12.438848	-0.098351	4.817754
500.490843	7999.879289	12.443853	-0.098284	4.817777
500.757253	7999.835690	12.448858	-0.098334	4.817763
501.002847	7999.856073	12.453863	-0.098380	4.817768
500.833141	7999.817818	12.458867	-0.098348	4.817758
500.639709	7999.821373	12.463872	-0.098312	4.817759
500.785502	7999.882477	12.468877	-0.098340	4.817777
500.579016	7999.858447	12.473882	-0.098301	4.817771
500.532310	7999.857782	12.478887	-0.098293	4.817771
500.495216	7999.865685	12.483891	-0.098286	4.817773
500.613292	7999.926392	12.488896	-0.098308	4.817791
500.293107	7999.887035	12.493901	-0.098248	4.817780
500.225586	7999.830222	12.498906	-0.098236	4.817764
500.716245	7999.834094	12.503911	-0.098327	4.817763
500.601110	7999.848255	12.508915	-0.098306	4.817768
500.673408	7999.829273	12.513920	-0.098319	4.817762
500.704935	7999.842374	12.518925	-0.098325	4.817765
500.815919	7999.818678	12.523930	-0.098346	4.817758
500.788255	7999.826716	12.528935	-0.098341	4.817760
500.958876	7999.890283	12.533939	-0.098373	4.817778
500.722638	7999.803655	12.538944	-0.098329	4.817754
500.374842	7999.868225	12.543949	-0.098264	4.817774
500.655447	7999.825883	12.548954	-0.098316	4.817761
500.691240	7999.847475	12.553959	-0.098323	4.817767
500.626943	7999.887655	12.558963	-0.098311	4.817779
500.615758	7999.828488	12.563968	-0.098309	4.817762
500.959658	7999.846064	12.568973	-0.098373	4.817765
500.745946	7999.835630	12.573978	-0.098333	4.817763
500.740268	7999.834499	12.578983	-0.098332	4.817763
500.725838	7999.849049	12.583987	-0.098330	4.817767
500.925163	7999.855070	12.588992	-0.098367	4.817768
501.134181	7999.846478	12.593997	-0.098406	4.817765
500.753100	7999.839968	12.599002	-0.098335	4.817764
501.070118	7999.843461	12.604007	-0.098394	4.817764
501.248306	7999.915568	12.609011	-0.098427	4.817785
500.736932	7999.843964	12.614016	-0.098332	4.817766
501.001433	7999.851973	12.619021	-0.098381	4.817767
500.749645	7999.851530	12.624026	-0.098335	4.817768
500.637070	7999.867836	12.629031	-0.098314	4.817773
500.903909	7999.881147	12.634035	-0.098363	4.817776
500.898627	7999.842086	12.639040	-0.098362	4.817764
500.884980	7999.887206	12.644045	-0.098360	4.817778
500.721097	7999.846927	12.649050	-0.098329	4.817767
501.103599	7999.838712	12.654055	-0.098401	4.817763
500.861491	7999.872129	12.659059	-0.098356	4.817773
500.860991	7999.828922	12.664064	-0.098356	4.817761
500.814126	7999.858814	12.669069	-0.098347	4.817770
500.613924	7999.850680	12.674074	-0.098310	4.817768
500.750467	7999.860017	12.679079	-0.098335	4.817770
500.679911	7999.876924	12.684083	-0.098322	4.817776
500.756177	7999.862215	12.689088	-0.098336	4.817771
500.857365	7999.853131	12.694093	-0.098355	4.817768
500.947204	7999.837562	12.699098	-0.098372	4.817763
500.958147	7999.848260	12.704103	-0.098374	4.817766
501.281978	7999.821291	12.709107	-0.098435	4.817757
501.010175	7999.791056	12.714112	-0.098384	4.817749
501.111243	7999.861004	12.719117	-0.098403	4.817769
501.186245	7999.877890	12.724122	-0.098417	4.817774
501.098079	7999.836587	12.729127	-0.098400	4.817762
501.150780	7999.847884	12.734131	-0.098410	4.817765
501.140169	7999.819284	12.739136	-0.098408	4.817757
501.198511	7999.850683	12.744141	-0.098419	4.817766
501.184816	7999.834685	12.749146	-0.098417	4.817761
501.201264	7999.844408	12.754151	-0.098420	4.817764
501.268280	7999.852749	12.759155	-0.098433	4.817766
501.241540	7999.836563	12.764160	-0.098428	4.817761
501.262063	7999.834754	12.769165	-0.098431	4.817761
501.249756	7999.811399	12.774170	-0.098429	4.817754
501.227072	7999.788948	12.779175	-0.098425	4.817747
501.321165	7999.800839	12.784179	-0.098443	4.817750
501.392019	7999.790266	12.789184	-0.098456	4.817747
501.130939	7999.855025	12.794189	-0.098407	4.817767
501.031839	7999.838856	12.799194	-0.098389	4.817763
501.252582	7999.833593	12.804199	-0.098430	4.817760
501.134485	7999.825582	12.809203	-0.098408	4.817758
501.195512	7999.883365	12.814208	-0.098420	4.817775
501.222368	7999.823688	12.819213	-0.098425	4.817758
501.143769	7999.818351	12.824218	-0.098410	4.817756
501.228776	7999.851187	12.829223	-0.098426	4.817766
500.959981	7999.874737	12.834227	-0.098376	4.817774
500.725534	7999.830285	12.839232	-0.098332	4.817762
501.009952	7999.851224	12.844237	-0.098385	4.817767
500.987594	7999.855123	12.849242	-0.098381	4.817768
500.667025	7999.850534	12.854247	-0.098322	4.817768
500.685714	7999.908763	12.859251	-0.098325	4.817785
500.851593	7999.844757	12.864256	-0.098356	4.817765
500.944630	7999.843986	12.869261	-0.098373	4.817765
500.948586	7999.845101	12.874266	-0.098374	4.817765
501.179171	7999.916905	12.879271	-0.098417	4.817785
501.150137	7999.837459	12.884275	-0.098412	4.817762
500.838134	7999.840369	12.889280	-0.098354	4.817764
501.284116	7999.854140	12.894285	-0.098437	4.817766
501.395455	7999.804104	12.899290	-0.098458	4.817751
501.278467	7999.823508	12.904295	-0.098436	4.817757
501.237753	7999.832412	12.909299	-0.098428	4.817760
501.137859	7999.818340	12.914304	-0.098410	4.817756
501.062845	7999.866796	12.919309	-0.098396	4.817771
501.123762	7999.836060	12.924314	-0.098407	4.817762
501.040643	7999.849626	12.929319	-0.098392	4.817766
500.947998	7999.830388	12.934323	-0.098375	4.817761
500.979112	7999.811870	12.939328	-0.098381	4.817755
501.124421	7999.846624	12.944333	-0.098408	4.817765
501.024032	7999.824114	12.949338	-0.098389	4.817758
500.865439	7999.889287	12.954343	-0.098360	4.817778
501.184860	7999.849609	12.959347	-0.098419	4.817765
500.840709	7999.830983	12.964352	-0.098355	4.817761
500.754135	7999.888758	12.969357	-0.098339	4.817779
500.864601	7999.833441	12.974362	-0.098360	4.817762
500.878603	7999.883173	12.979367	-0.098362	4.817777
500.847969	7999.901706	12.984371	-0.098357	4.817782
500.880836	7999.861084	12.989376	-0.098363	4.817770
501.167336	7999.840957	12.994381	-0.098416	4.817763
500.756998	7999.840350	12.999386	-0.098340	4.817764
500.697965	7999.858476	13.004391	-0.098329	4.817770
500.511400	7999.906388	13.009395	-0.098294	4.817785
500.800298	7999.859951	13.014400	-0.098348	4.817770
500.388023	7999.918328	13.019405	-0.098271	4.817789
501.128908	7999.838323	13.024410	-0.098409	4.817762
501.013362	7999.879876	13.029415	-0.098388	4.817775
500.852800	7999.878633	13.034419	-0.098358	4.817775
500.926389	7999.835433	13.039424	-0.098372	4.817762
500.835930	7999.895260	13.044429	-0.098355	4.817780
500.942036	7999.843042	13.049434	-0.098375	4.817764
500.629620	7999.874398	13.054439	-0.098317	4.817775
500.982883	7999.881571	13.059443	-0.098383	4.817776
500.919102	7999.849048	13.064448	-0.098371	4.817766
501.069918	7999.852267	13.069453	-0.098399	4.817767
501.245913	7999.847417	13.074458	-0.098432	4.817764
501.016451	7999.875746	13.079463	-0.098389	4.817774
501.100190	7999.851659	13.084467	-0.098405	4.817766
501.142822	7999.820661	13.089472	-0.098413	4.817757
501.232766	7999.865159	13.094477	-0.098429	4.817770
500.898010	7999.871958	13.099482	-0.098367	4.817773
500.736835	7999.881244	13.104487	-0.098337	4.817777
500.827484	7999.888869	13.109491	-0.098354	4.817778
500.764448	7999.853196	13.114496	-0.098342	4.817768
500.836341	7999.875305	13.119501	-0.098356	4.817774
500.771739	7999.868061	13.124506	-0.098344	4.817773
500.792361	7999.837801	13.129511	-0.098348	4.817763
501.138305	7999.855408	13.134515	-0.098412	4.817767
500.452040	7999.841364	13.139520	-0.098285	4.817766
501.014647	7999.857859	13.144525	-0.098389	4.817768
500.996136	7999.840737	13.149530	-0.098386	4.817763
500.966527	7999.865608	13.154535	-0.098381	4.817771
501.224057	7999.844012	13.159539	-0.098429	4.817763
500.948008	7999.844275	13.164544	-0.098377	4.817765
501.007782	7999.855674	13.169549	-0.098388	4.817768
500.872638	7999.912753	13.174554	-0.098363	4.817785
500.822311	7999.928896	13.179559	-0.098354	4.817790
500.931142	7999.876717	13.184563	-0.098374	4.817774
501.132833	7999.820600	13.189568	-0.098412	4.817757
501.164178	7999.870580	13.194573	-0.098418	4.817772
501.107102	7999.868713	13.199578	-0.098407	4.817771
500.693796	7999.877548	13.204583	-0.098330	4.817776
501.056572	7999.891180	13.209587	-0.098398	4.817778
501.216817	7999.850275	13.214592	-0.098428	4.817765
501.404989	7999.839277	13.219597	-0.098463	4.817761
500.960015	7999.914045	13.224602	-0.098380	4.817785
501.116006	7999.845682	13.229607	-0.098409	4.817764
500.952407	7999.873901	13.234611	-0.098379	4.817773
500.769585	7999.855479	13.239616	-0.098345	4.817769
501.179008	7999.895071	13.244621	-0.098421	4.817779
500.701554	7999.908255	13.249626	-0.098332	4.817785
500.792718	7999.888490	13.254631	-0.098349	4.817778
500.780025	7999.915710	13.259635	-0.098347	4.817787
500.807809	7999.845509	13.264640	-0.098352	4.817766
500.900086	7999.926922	13.269645	-0.098369	4.817789
500.765068	7999.888110	13.274650	-0.098344	4.817778
500.765914	7999.894449	13.279655	-0.098345	4.817780
500.986518	7999.883915	13.284659	-0.098386	4.817776
501.376789	7999.796779	13.289664	-0.098458	4.817749
501.341422	7999.850019	13.294669	-0.098452	4.817765
501.598105	7999.815765	13.299674	-0.098500	4.817753
501.351803	7999.850176	13.304679	-0.098454	4.817765
501.375912	7999.856848	13.309683	-0.098458	4.817767
500.979377	7999.834309	13.314688	-0.098385	4.817762
500.899843	7999.901669	13.319693	-0.098370	4.817782
500.980160	7999.852243	13.324698	-0.098385	4.817767
501.476110	7999.916259	13.329703	-0.098477	4.817784
501.440126	7999.846197	13.334707	-0.098471	4.817763
501.200746	7999.863846	13.339712	-0.098426	4.817769
501.362202	7999.866164	13.344717	-0.098456	4.817769
501.653952	7999.828198	13.349722	-0.098511	4.817757
501.608896	7999.805427	13.354727	-0.098502	4.817750
501.607170	7999.812783	13.359731	-0.098502	4.817753
501.254585	7999.823541	13.364736	-0.098436	4.817757
501.632257	7999.847926	13.369741	-0.098507	4.817763
501.088821	7999.880185	13.374746	-0.098406	4.817775
501.083000	7999.860084	13.379751	-0.098405	4.817769
501.336799	7999.841596	13.384755	-0.098452	4.817762
501.157121	7999.837971	13.389760	-0.098418	4.817762
501.422314	7999.932401	13.394765	-0.098468	4.817789
501.270381	7999.831172	13.399770	-0.098440	4.817759
500.958815	7999.874132	13.404775	-0.098382	4.817773
501.023552	7999.889816	13.409779	-0.098394	4.817778
501.339375	7999.815313	13.414784	-0.098453	4.817754
501.446062	7999.851620	13.419789	-0.098473	4.817765
501.314199	7999.809691	13.424794	-0.098448	4.817753
501.307096	7999.826454	13.429799	-0.098447	4.817758
501.266413	7999.841682	13.434803	-0.098439	4.817763
501.018592	7999.830758	13.439808	-0.098393	4.817760
500.899825	7999.879642	13.444813	-0.098371	4.817775
501.110118	7999.851046	13.449818	-0.098410	4.817766
500.953340	7999.846696	13.454823	-0.098381	4.817765
501.001495	7999.884272	13.459827	-0.098390	4.817776
500.634422	7999.872694	13.464832	-0.098322	4.817774
500.821882	7999.900674	13.469837	-0.098357	4.817782
500.931843	7999.854834	13.474842	-0.098377	4.817768
501.193136	7999.880712	13.479847	-0.098426	4.817774
501.396795	7999.876258	13.484851	-0.098464	4.817772
501.157706	7999.870728	13.489856	-0.098420	4.817772
501.121765	7999.893401	13.494861	-0.098413	4.817778
500.980313	7999.851334	13.499866	-0.098387	4.817767
500.674066	7999.916499	13.504871	-0.098330	4.817787
500.877140	7999.884638	13.509875	-0.098368	4.817777
500.750079	7999.862800	13.514880	-0.098344	4.817771
501.066965	7999.858915	13.519885	-0.098403	4.817768
501.034615	7999.843702	13.524890	-0.098397	4.817764
500.561857	7999.862223	13.529895	-0.098309	4.817772
501.194223	7999.873396	13.534899	-0.098427	4.817772
501.387397	7999.840340	13.539904	-0.098463	4.817762
501.348245	7999.852428	13.544909	-0.098456	4.817765
501.145585	7999.857958	13.549914	-0.098418	4.817768
501.051864	7999.951460	13.554919	-0.098401	4.817796
500.746764	7999.913370	13.559923	-0.098344	4.817786
500.912704	7999.862010	13.564928	-0.098375	4.817770
501.302179	7999.867595	13.569933	-0.098447	4.817770
500.845585	7999.893723	13.574938	-0.098362	4.817780
500.393820	7999.947319	13.579943	-0.098278	4.817798
500.813122	7999.949116	13.584947	-0.098357	4.817796
500.656669	7999.866792	13.589952	-0.098327	4.817773
500.941731	7999.898279	13.594957	-0.098381	4.817781
501.050761	7999.864017	13.599962	-0.098401	4.817770
501.018083	7999.882520	13.604967	-0.098395	4.817776
501.233524	7999.895096	13.609971	-0.098435	4.817778
501.087386	7999.844532	13.614976	-0.098408	4.817764
501.084619	7999.895078	13.619981	-0.098407	4.817779
501.169164	7999.820421	13.624986	-0.098423	4.817757
500.813875	7999.855378	13.629991	-0.098357	4.817768
501.097158	7999.856280	13.634995	-0.098410	4.817768
501.177290	7999.844787	13.640000	-0.098425	4.817764
501.431636	7999.849490	13.645005	-0.098472	4.817764
501.177693	7999.836371	13.650010	-0.098425	4.817761
501.463483	7999.824663	13.655015	-0.098478	4.817757
501.378160	7999.854005	13.660019	-0.098463	4.817766
501.273663	7999.837758	13.665024	-0.098443	4.817761
501.224013	7999.854965	13.670029	-0.098434	4.817767
501.485840	7999.833430	13.675034	-0.098483	4.817759
501.166162	7999.858359	13.680039	-0.098423	4.817768
501.497356	7999.853626	13.685043	-0.098485	4.817765
501.321491	7999.853217	13.690048	-0.098452	4.817766
501.089492	7999.887832	13.695053	-0.098409	4.817777
501.269343	7999.844047	13.700058	-0.098443	4.817763
501.336349	7999.870303	13.705063	-0.098455	4.817771
501.524005	7999.857189	13.710067	-0.098490	4.817766
501.248676	7999.831118	13.715072	-0.098439	4.817759
501.467643	7999.854282	13.720077	-0.098480	4.817765
501.781904	7999.821908	13.725082	-0.098538	4.817754
501.602799	7999.819345	13.730087	-0.098505	4.817754
501.538785	7999.838453	13.735091	-0.098493	4.817760
501.732536	7999.805406	13.740096	-0.098529	4.817750
501.524943	7999.947858	13.745101	-0.098491	4.817793
501.404672	7999.857619	13.750106	-0.098468	4.817767
501.307863	7999.860451	13.755111	-0.098450	4.817768
501.142363	7999.892858	13.760115	-0.098420	4.817778
501.309474	7999.836245	13.765120	-0.098451	4.817761
501.434248	7999.869651	13.770125	-0.098474	4.817770
501.258141	7999.878723	13.775130	-0.098441	4.817773
501.285515	7999.850667	13.780135	-0.098447	4.817765
501.368667	7999.844486	13.785139	-0.098462	4.817763
501.147580	7999.860290	13.790144	-0.098421	4.817768
501.422004	7999.847367	13.795149	-0.098472	4.817763
500.771727	7999.850698	13.800154	-0.098351	4.817767
500.847047	7999.851781	13.805159	-0.098365	4.817767
501.230570	7999.896271	13.810163	-0.098437	4.817779
501.058658	7999.844283	13.815168	-0.098405	4.817764
501.380686	7999.838364	13.820173	-0.098465	4.817761
501.277197	7999.848477	13.825178	-0.098445	4.817764
501.302215	7999.849893	13.830183	-0.098450	4.817765
501.184523	7999.846103	13.835187	-0.098428	4.817764
501.201711	7999.838977	13.840192	-0.098432	4.817762
501.417943	7999.865263	13.845197	-0.098472	4.817769
501.459885	7999.896429	13.850202	-0.098480	4.817778
501.363896	7999.829722	13.855207	-0.098462	4.817758
501.422679	7999.854806	13.860211	-0.098473	4.817766
501.226448	7999.835137	13.865216	-0.098436	4.817761
501.083284	7999.893155	13.870221	-0.098410	4.817778
501.148607	7999.876181	13.875226	-0.098422	4.817773
500.871656	7999.894346	13.880231	-0.098371	4.817780
501.295284	7999.887775	13.885235	-0.098449	4.817776
501.015371	7999.854262	13.890240	-0.098397	4.817767
501.274307	7999.880106	13.895245	-0.098446	4.817774
501.399777	7999.834488	13.900250	-0.098469	4.817760
501.226394	7999.843599	13.905255	-0.098437	4.817763
501.423655	7999.885420	13.910259	-0.098474	4.817775
501.341300	7999.830501	13.915264	-0.098458	4.817759
501.156085	7999.866841	13.920269	-0.098424	4.817770
501.379869	7999.831062	13.925274	-0.098466	4.817759
501.219114	7999.855107	13.930279	-0.098436	4.817767
500.986245	7999.913947	13.935283	-0.098392	4.817785
501.041581	7999.861001	13.940288	-0.098403	4.817769
501.218725	7999.871974	13.945293	-0.098436	4.817772
501.381781	7999.836379	13.950298	-0.098466	4.817760
501.400882	7999.836656	13.955303	-0.098470	4.817760
501.861339	7999.846422	13.960307	-0.098556	4.817761
501.618608	7999.893529	13.965312	-0.098511	4.817776
501.568453	7999.845393	13.970317	-0.098501	4.817762
501.474401	7999.824027	13.975322	-0.098484	4.817756
501.645523	7999.819107	13.980327	-0.098516	4.817754
501.658910	7999.835110	13.985331	-0.098518	4.817759
501.384655	7999.801678	13.990336	-0.098467	4.817750
501.631502	7999.883200	13.995341	-0.098513	4.817773
501.400682	7999.850390	14.000346	-0.098470	4.817764
501.251959	7999.865123	14.005351	-0.098443	4.817769
501.553189	7999.843099	14.010355	-0.098499	4.817762
501.429993	7999.855037	14.015360	-0.098476	4.817766
501.150926	7999.909000	14.020365	-0.098424	4.817783
501.347498	7999.848594	14.025370	-0.098461	4.817764
501.667392	7999.838430	14.030375	-0.098520	4.817760
501.532092	7999.835441	14.035379	-0.098495	4.817759
501.144817	7999.817250	14.040384	-0.098423	4.817756
501.467984	7999.845068	14.045389	-0.098483	4.817763
501.257520	7999.834679	14.050394	-0.098444	4.817760
500.976360	7999.918118	14.055399	-0.098392	4.817786
501.320865	7999.852456	14.060403	-0.098456	4.817765
501.307681	7999.855432	14.065408	-0.098454	4.817766
501.162236	7999.891288	14.070413	-0.098427	4.817778
501.187829	7999.848454	14.075418	-0.098431	4.817765
501.291338	7999.879447	14.080423	-0.098451	4.817773
501.789491	7999.852870	14.085427	-0.098544	4.817763
501.437886	7999.853104	14.090432	-0.098478	4.817765
501.330247	7999.881071	14.095437	-0.098458	4.817774
501.208161	7999.860357	14.100442	-0.098436	4.817768
501.311952	7999.840773	14.105447	-0.098455	4.817762
501.074658	7999.891120	14.110451	-0.098411	4.817778
501.165163	7999.850269	14.115456	-0.098428	4.817765
501.831633	7999.848234	14.120461	-0.098552	4.817762
501.388747	7999.865073	14.125466	-0.098469	4.817769
501.316587	7999.891442	14.130471	-0.098456	4.817777
500.901434	7999.933970	14.135475	-0.098379	4.817791
500.653802	7999.898813	14.140480	-0.098333	4.817782
500.812790	7999.932708	14.145485	-0.098362	4.817791
501.072912	7999.874267	14.150490	-0.098411	4.817773
500.950111	7999.877780	14.155495	-0.098388	4.817774
501.074548	7999.902750	14.160499	-0.098411	4.817781
500.910122	7999.867731	14.165504	-0.098381	4.817772
500.803102	7999.913622	14.170509	-0.098361	4.817786
500.723108	7999.917748	14.175514	-0.098346	4.817787
500.713417	7999.955549	14.180519	-0.098344	4.817798
500.718054	7999.956674	14.185523	-0.098345	4.817799
501.077444	7999.919677	14.190528	-0.098412	4.817786
500.851414	7999.940679	14.195533	-0.098370	4.817793
501.247677	7999.877866	14.200538	-0.098444	4.817773
500.837228	7999.908870	14.205543	-0.098368	4.817784
501.226875	7999.924996	14.210547	-0.098440	4.817787
500.820571	7999.924446	14.215552	-0.098365	4.817789
500.733487	7999.977999	14.220557	-0.098348	4.817805
500.851801	7999.925956	14.225562	-0.098371	4.817789
500.794598	7999.930409	14.230567	-0.098360	4.817791
500.892071	7999.964477	14.235571	-0.098378	4.817800
500.513992	7999.968547	14.240576	-0.098308	4.817803
500.552334	7999.995445	14.245581	-0.098315	4.817811
501.209068	7999.871031	14.250586	-0.098437	4.817771
500.678356	7999.980399	14.255591	-0.098339	4.817806
500.779488	7999.987121	14.260595	-0.098357	4.817807
501.175623	7999.901123	14.265600	-0.098431	4.817780
501.588367	7999.890183	14.270605	-0.098508	4.817775
501.314466	7999.890476	14.275610	-0.098457	4.817777
501.469743	7999.891652	14.280615	-0.098486	4.817776
501.578400	7999.888998	14.285619	-0.098506	4.817775
501.341795	7999.877181	14.290624	-0.098462	4.817773
501.458595	7999.913634	14.295629	-0.098484	4.817783
501.305701	7999.907231	14.300634	-0.098456	4.817782
501.195966	7999.920416	14.305639	-0.098435	4.817786
500.869698	7999.942088	14.310643	-0.098375	4.817794
501.094497	7999.855743	14.315648	-0.098417	4.817767
501.027540	7999.907476	14.320653	-0.098404	4.817783
500.541404	7999.945826	14.325658	-0.098314	4.817796
500.445273	7999.964475	14.330663	-0.098296	4.817802
500.910237	7999.974303	14.335667	-0.098383	4.817803
501.082328	7999.901955	14.340672	-0.098415	4.817781
501.224096	7999.915583	14.345677	-0.098441	4.817784
501.154951	7999.918811	14.350682	-0.098428	4.817786
501.517058	7999.883961	14.355687	-0.098496	4.817774
501.109918	7999.927658	14.360691	-0.098420	4.817788
501.347901	7999.892082	14.365696	-0.098464	4.817777
501.476666	7999.892878	14.370701	-0.098488	4.817777
501.665335	7999.859758	14.375706	-0.098524	4.817766
501.355799	7999.876401	14.380711	-0.098466	4.817772
501.357625	7999.872216	14.385715	-0.098466	4.817771
501.189031	7999.845567	14.390720	-0.098435	4.817764
501.059763	7999.900623	14.395725	-0.098411	4.817781
501.295464	7999.888198	14.400730	-0.098455	4.817776
501.345103	7999.891021	14.405735	-0.098464	4.817777
501.527109	7999.890473	14.410739	-0.098498	4.817776
501.613070	7999.845342	14.415744	-0.098514	4.817762
501.560067	7999.652798	14.420749	-0.098504	4.817705

501.513431	7996.458449	14.425754	-0.098494	4.816759
501.549635	7990.808602	14.430759	-0.098497	4.815084
501.836830	7984.137734	14.435763	-0.098546	4.813105
501.482094	7976.798767	14.440768	-0.098475	4.810930
501.626746	7969.116634	14.445773	-0.098497	4.808649
501.570654	7961.393358	14.450778	-0.098482	4.806357
501.208206	7953.473255	14.455783	-0.098409	4.804005
501.047646	7945.627018	14.460787	-0.098374	4.801674
500.787091	7937.472660	14.465792	-0.098320	4.799251
500.916188	7929.639059	14.470797	-0.098339	4.796920
500.499450	7921.586411	14.475802	-0.098257	4.794525
500.719552	7913.560420	14.480807	-0.098292	4.792134
501.443506	7905.487856	14.485811	-0.098422	4.789726
501.252701	7897.480495	14.490816	-0.098381	4.787340
501.188052	7889.492283	14.495821	-0.098364	4.784958
501.140217	7881.580454	14.500826	-0.098350	4.782597
500.549150	7873.544108	14.505831	-0.098235	4.780200
500.945661	7865.551178	14.510835	-0.098303	4.777812
501.154316	7857.517235	14.515840	-0.098337	4.775410
501.199207	7849.460457	14.520845	-0.098340	4.773001
500.846800	7841.530870	14.525850	-0.098270	4.770630
500.912335	7833.474092	14.530855	-0.098277	4.768219
500.986116	7825.516313	14.535859	-0.098285	4.765836
501.075802	7817.460550	14.540864	-0.098297	4.763422
501.011248	7809.550010	14.545869	-0.098280	4.761051
500.944946	7801.510201	14.550874	-0.098262	4.758641
500.887154	7793.539078	14.555879	-0.098246	4.756249
500.817831	7785.524060	14.560883	-0.098228	4.753843
500.561384	7777.483404	14.565888	-0.098175	4.751429
500.878309	7769.459225	14.570893	-0.098229	4.749017
500.612289	7761.519156	14.575898	-0.098174	4.746631
500.723150	7753.401640	14.580903	-0.098190	4.744188
500.448000	7745.554767	14.585907	-0.098133	4.741828
500.662349	7737.465997	14.590912	-0.098168	4.739392
500.215607	7729.497394	14.595917	-0.098080	4.736992
500.404950	7721.457056	14.600922	-0.098110	4.734568
500.664436	7713.421290	14.605927	-0.098153	4.732144
500.418546	7705.463501	14.610931	-0.098102	4.729744
500.009805	7697.491140	14.615936	-0.098021	4.727338
500.221431	7689.446616	14.620941	-0.098055	4.724908
500.434239	7681.513584	14.625946	-0.098090	4.722510
500.280878	7673.482023	14.630951	-0.098056	4.720082
500.034512	7665.525278	14.635955	-0.098005	4.717676
499.694520	7657.521600	14.640960	-0.097936	4.715254
499.844593	7649.443601	14.645965	-0.097959	4.712807
500.108297	7641.400263	14.650970	-0.098003	4.710370
500.220308	7633.403416	14.655975	-0.098019	4.707946
500.362343	7625.391258	14.660979	-0.098040	4.705516
500.242521	7617.417871	14.665984	-0.098012	4.703096
500.173980	7609.478704	14.670989	-0.097995	4.700686
500.074870	7601.456160	14.675994	-0.097971	4.698249
499.894944	7593.424113	14.680999	-0.097932	4.695809
500.010424	7585.454038	14.686003	-0.097949	4.693385
499.940531	7577.482158	14.691008	-0.097930	4.690960
499.450190	7569.485116	14.696013	-0.097834	4.688526
499.715884	7561.457294	14.701018	-0.097878	4.686081
499.288864	7553.422953	14.706023	-0.097794	4.683633
499.300857	7545.573597	14.711027	-0.097791	4.681240
499.160099	7537.428992	14.716032	-0.097759	4.678756
499.451183	7529.527303	14.721037	-0.097808	4.676345
499.732035	7521.420011	14.726042	-0.097855	4.673869
499.750219	7513.343834	14.731047	-0.097854	4.671401
499.840742	7505.333361	14.736051	-0.097865	4.668953
499.736712	7497.399109	14.741056	-0.097841	4.666526
499.733913	7489.389665	14.746061	-0.097835	4.664076
499.538892	7481.478918	14.751066	-0.097794	4.661654
499.432234	7473.397240	14.756071	-0.097769	4.659179
499.229624	7465.499019	14.761075	-0.097726	4.656758
499.084129	7457.405553	14.766080	-0.097694	4.654276
499.136150	7449.467226	14.771085	-0.097698	4.651841
499.434231	7441.377664	14.776090	-0.097748	4.649358
499.142018	7433.421039	14.781095	-0.097689	4.646914
498.764690	7425.470718	14.786099	-0.097613	4.644471
498.876260	7417.480162	14.791104	-0.097629	4.642014
498.732730	7409.379147	14.796109	-0.097597	4.639522
498.812389	7401.433605	14.801114	-0.097607	4.637077
498.877478	7393.369597	14.806119	-0.097614	4.634594
499.030814	7385.407092	14.811123	-0.097637	4.632140
498.741749	7377.314439	14.816128	-0.097578	4.629646
498.793526	7369.401002	14.821133	-0.097583	4.627205
498.939073	7361.373285	14.826138	-0.097605	4.624728
498.801446	7353.427032	14.831143	-0.097574	4.622274
499.103419	7345.393448	14.836147	-0.097625	4.619792
498.922113	7337.426513	14.841152	-0.097586	4.617330
498.598008	7329.419777	14.846157	-0.097520	4.614853
498.419554	7321.461545	14.851162	-0.097482	4.612391
498.277001	7313.380532	14.856167	-0.097450	4.609889
498.119537	7305.458169	14.861171	-0.097416	4.607434
498.367400	7297.285219	14.866176	-0.097457	4.604902
498.713922	7289.352916	14.871181	-0.097516	4.602442
498.235637	7281.414211	14.876186	-0.097422	4.599978
497.977358	7273.432978	14.881191	-0.097369	4.597501
498.393059	7265.406573	14.886195	-0.097441	4.595008
498.280296	7257.377280	14.891200	-0.097415	4.592513
498.431840	7249.313234	14.896205	-0.097438	4.590005
498.346404	7241.350819	14.901210	-0.097417	4.587528
498.171327	7233.265790	14.906215	-0.097379	4.585011
498.243245	7225.361550	14.911219	-0.097387	4.582549
497.871701	7217.360441	14.916224	-0.097313	4.580055
497.868609	7209.360053	14.921229	-0.097307	4.577561
497.778654	7201.341462	14.926234	-0.097285	4.575059
498.140257	7193.276936	14.931239	-0.097347	4.572543
497.659493	7185.343223	14.936243	-0.097253	4.570064
497.544753	7177.355014	14.941248	-0.097226	4.567568
497.723211	7169.310618	14.946253	-0.097254	4.565053
497.916889	7161.334357	14.951258	-0.097285	4.562558
497.923899	7153.291753	14.956263	-0.097281	4.560041
498.283934	7145.346015	14.961267	-0.097343	4.557553
497.888149	7137.324803	14.966272	-0.097264	4.555039
498.114727	7129.319883	14.971277	-0.097301	4.552530
498.316732	7121.269718	14.976282	-0.097334	4.550005
498.259803	7113.276527	14.981287	-0.097318	4.547496
497.906503	7105.347609	14.986291	-0.097247	4.545006
497.968080	7097.298856	14.991296	-0.097253	4.542477
498.091510	7089.287842	14.996301	-0.097271	4.539959
497.873112	7081.304792	15.001306	-0.097225	4.537447
497.671463	7073.266618	15.006311	-0.097183	4.534917
497.873322	7065.288126	15.011315	-0.097215	4.532405
497.921808	7057.237040	15.016320	-0.097219	4.529868
497.736117	7049.280612	15.021325	-0.097179	4.527359
497.380648	7041.297539	15.026330	-0.097108	4.524840
497.670780	7033.263721	15.031335	-0.097157	4.522305
497.709611	7025.261354	15.036339	-0.097159	4.519778
497.630645	7017.336685	15.041344	-0.097139	4.517274
497.928330	7009.270629	15.046349	-0.097189	4.514725
497.309895	7001.373988	15.051354	-0.097069	4.512225
497.380676	6993.225523	15.056359	-0.097077	4.509646
497.555385	6985.234378	15.061363	-0.097104	4.507116
496.958621	6977.239006	15.066368	-0.096988	4.504581
497.099331	6969.275940	15.071373	-0.097009	4.502057
497.010237	6961.236162	15.076378	-0.096987	4.499506
496.562342	6953.282642	15.081383	-0.096899	4.496980
496.858137	6945.202549	15.086387	-0.096949	4.494415
497.028830	6937.191257	15.091392	-0.096975	4.491870
496.864798	6929.199145	15.096397	-0.096940	4.489328
496.445522	6921.257824	15.101402	-0.096856	4.486801
496.781680	6913.127713	15.106407	-0.096914	4.484214
496.846043	6905.271070	15.111411	-0.096921	4.481712
496.655689	6897.194733	15.116416	-0.096880	4.479138
496.804059	6889.258825	15.121421	-0.096903	4.476608
496.781363	6881.185733	15.126426	-0.096893	4.474032
496.425266	6873.262441	15.131431	-0.096822	4.471502
496.577173	6865.199291	15.136435	-0.096845	4.468927
496.757587	6857.150119	15.141440	-0.096873	4.466355
496.812909	6849.121862	15.146445	-0.096878	4.463788
496.907283	6841.208878	15.151450	-0.096891	4.461257
496.493243	6833.178772	15.156455	-0.096808	4.458684
496.728680	6825.202727	15.161459	-0.096847	4.456131
496.478119	6817.171934	15.166464	-0.096795	4.453556
496.900158	6809.176001	15.171469	-0.096869	4.450993
496.920267	6801.148618	15.176474	-0.096867	4.448418
496.943181	6793.157924	15.181479	-0.096866	4.445852
497.054826	6785.160780	15.186483	-0.096882	4.443284
496.850328	6777.203176	15.191488	-0.096839	4.440725
496.876092	6769.206882	15.196493	-0.096838	4.438154
496.666568	6761.248017	15.201498	-0.096794	4.435591
496.699150	6753.130051	15.206503	-0.096795	4.432978
496.744565	6745.162941	15.211507	-0.096798	4.430411
496.758547	6737.119623	15.216512	-0.096796	4.427818
496.717751	6729.112886	15.221517	-0.096783	4.425235
496.567876	6721.162956	15.226522	-0.096750	4.422669
496.237111	6713.157944	15.231527	-0.096683	4.420082
496.170382	6705.210234	15.236531	-0.096666	4.417513
496.094138	6697.151505	15.241536	-0.096646	4.414907
496.447995	6689.099702	15.246541	-0.096707	4.412305
496.153895	6681.143033	15.251546	-0.096647	4.409727
496.055536	6673.085498	15.256551	-0.096624	4.407117
496.457491	6665.094052	15.261555	-0.096693	4.404530
496.116630	6657.159209	15.266560	-0.096625	4.401955
496.194595	6649.083871	15.271565	-0.096634	4.399335
496.134107	6641.149528	15.276570	-0.096618	4.396759
496.429113	6633.040231	15.281575	-0.096667	4.394126
496.294415	6625.170471	15.286579	-0.096637	4.391567
495.977950	6617.121720	15.291584	-0.096573	4.388948
496.187571	6609.126198	15.296589	-0.096607	4.386347
496.172184	6601.105249	15.301594	-0.096599	4.383735
496.044833	6593.157408	15.306599	-0.096570	4.381145
496.031471	6585.171838	15.311603	-0.096562	4.378541
496.146245	6577.178876	15.316608	-0.096579	4.375935
496.042149	6569.188406	15.321613	-0.096554	4.373326
495.993298	6561.132810	15.326618	-0.096540	4.370695
496.058727	6553.151349	15.331623	-0.096547	4.368087
496.516485	6545.099595	15.336627	-0.096627	4.365457
496.182721	6537.157982	15.341632	-0.096560	4.362857
495.967252	6529.206326	15.346637	-0.096514	4.360252
495.962804	6521.234006	15.351642	-0.096508	4.357641
495.966107	6513.202509	15.356647	-0.096504	4.355008
495.890064	6505.221391	15.361651	-0.096485	4.352390
495.568989	6497.157333	15.366656	-0.096420	4.349741
495.729773	6489.162653	15.371661	-0.096444	4.347117
495.736073	6481.113529	15.376666	-0.096440	4.344473
495.635238	6473.209397	15.381671	-0.096416	4.341873
495.831124	6465.215964	15.386675	-0.096448	4.339245
495.466143	6457.241208	15.391680	-0.096375	4.336617
495.428210	6449.224971	15.396685	-0.096362	4.333977
495.378013	6441.239499	15.401690	-0.096348	4.331345
495.359417	6433.162572	15.406695	-0.096339	4.328681
495.260622	6425.214561	15.411699	-0.096316	4.326057
495.294339	6417.161413	15.416704	-0.096317	4.323399
495.373805	6409.226410	15.421709	-0.096327	4.320778
495.453746	6401.230098	15.426714	-0.096336	4.318135
495.058714	6393.218288	15.431719	-0.096258	4.315482
495.220230	6385.224145	15.436723	-0.096282	4.312837
495.125152	6377.172481	15.441728	-0.096260	4.310170
495.191781	6369.162264	15.446733	-0.096267	4.307516
494.964229	6361.159740	15.451738	-0.096219	4.304860
494.840560	6353.177463	15.456743	-0.096191	4.302210
495.134875	6345.116046	15.461747	-0.096241	4.299536
494.981844	6337.169812	15.466752	-0.096207	4.296895
495.113260	6329.122498	15.471757	-0.096226	4.294221
494.757783	6321.186835	15.476762	-0.096155	4.291578
494.714249	6313.109135	15.481767	-0.096142	4.288889
494.964646	6305.200143	15.486771	-0.096183	4.286257
494.550365	6297.164006	15.491776	-0.096101	4.283576
494.366056	6289.216677	15.496781	-0.096061	4.280924
494.732665	6281.159190	15.501786	-0.096125	4.278239
494.567536	6273.196062	15.506791	-0.096089	4.275578
494.600393	6265.179220	15.511795	-0.096090	4.272900
494.584079	6257.153835	15.516800	-0.096081	4.270217
494.671130	6249.132465	15.521805	-0.096092	4.267535
494.505272	6241.123279	15.526810	-0.096056	4.264852
494.000288	6233.208092	15.531815	-0.095957	4.262197
494.062669	6225.169068	15.536819	-0.095964	4.259503
494.519240	6217.127430	15.541824	-0.096043	4.256810
494.601394	6209.083004	15.546829	-0.096054	4.254112
494.473419	6201.133471	15.551834	-0.096025	4.251441
494.473031	6193.109058	15.556839	-0.096019	4.248745
494.288059	6185.171350	15.561843	-0.095980	4.246074
493.559274	6177.260544	15.566848	-0.095839	4.243406
493.912192	6169.132408	15.571853	-0.095900	4.240673
494.032150	6161.155408	15.576858	-0.095917	4.237987
494.092398	6153.112096	15.581863	-0.095923	4.235277
494.065309	6145.141368	15.586867	-0.095913	4.232588
493.790639	6137.157474	15.591872	-0.095856	4.229891
493.618719	6129.188538	15.596877	-0.095819	4.227198
493.578572	6121.116278	15.601882	-0.095806	4.224469
493.888472	6113.123159	15.606887	-0.095859	4.221770
493.685357	6105.084858	15.611891	-0.095816	4.219048
493.711119	6097.133960	15.616896	-0.095816	4.216356
494.102828	6089.105482	15.621901	-0.095883	4.213640
494.071260	6081.126969	15.626906	-0.095872	4.210935
493.749960	6073.112398	15.631911	-0.095807	4.208212
493.959895	6065.117085	15.636915	-0.095841	4.205501
493.697136	6057.143279	15.641920	-0.095787	4.202789
493.836397	6049.130246	15.646925	-0.095808	4.200067
493.942724	6041.155568	15.651930	-0.095823	4.197356
494.108542	6033.084983	15.656935	-0.095848	4.194611
493.900728	6025.101815	15.661939	-0.095804	4.191890
493.751528	6017.048679	15.666944	-0.095771	4.189144
493.668836	6009.125848	15.671949	-0.095751	4.186441
493.743202	6001.075676	15.676954	-0.095760	4.183695
493.103250	5993.188759	15.681959	-0.095635	4.180994
493.117520	5985.153066	15.686963	-0.095633	4.178249
493.112251	5977.085911	15.691968	-0.095627	4.175491
493.246683	5969.090366	15.696973	-0.095647	4.172757
493.421817	5961.067589	15.701978	-0.095674	4.170012
493.728780	5953.045371	15.706983	-0.095726	4.167268
493.703540	5945.070165	15.711987	-0.095716	4.164533
493.174139	5937.170083	15.716992	-0.095612	4.161817
493.274180	5929.120032	15.721997	-0.095626	4.159055
492.962289	5921.216466	15.727002	-0.095563	4.156336
493.021221	5913.114971	15.732007	-0.095568	4.153552
492.854584	5905.208603	15.737011	-0.095532	4.150831
492.701764	5897.171876	15.742016	-0.095499	4.148063
493.006768	5889.095604	15.747021	-0.095550	4.145285
492.850184	5881.161281	15.752026	-0.095516	4.142549
492.543538	5873.136507	15.757031	-0.095454	4.139777
492.818505	5865.138859	15.762035	-0.095500	4.137021
492.753938	5857.082402	15.767040	-0.095483	4.134238
492.907487	5849.148686	15.772045	-0.095506	4.131499
492.523667	5841.152173	15.777050	-0.095429	4.128728
492.244058	5833.157207	15.782055	-0.095372	4.125958
492.373228	5825.168245	15.787059	-0.095391	4.123194
492.569627	5817.147769	15.792064	-0.095422	4.120417
492.318478	5809.210311	15.797069	-0.095371	4.117662
492.564416	5801.168029	15.802074	-0.095411	4.114875
492.172672	5793.219930	15.807079	-0.095333	4.112110
492.224673	5785.182605	15.812083	-0.095338	4.109318
491.998989	5777.140180	15.817088	-0.095290	4.106519
491.951566	5769.110600	15.822093	-0.095276	4.103725
492.151240	5761.127730	15.827098	-0.095308	4.100948
491.921116	5753.141484	15.832103	-0.095260	4.098163
492.120755	5745.108502	15.837107	-0.095292	4.095365
492.271127	5737.109772	15.842112	-0.095315	4.092577
492.093695	5729.173608	15.847117	-0.095277	4.089804
491.977011	5721.202002	15.852122	-0.095250	4.087018
491.940142	5713.136182	15.857127	-0.095238	4.084198
492.212221	5705.170242	15.862131	-0.095284	4.081415
492.263933	5697.095747	15.867136	-0.095288	4.078589
492.404073	5689.130948	15.872141	-0.095309	4.075801
492.298138	5681.156936	15.877146	-0.095284	4.073005
491.895267	5673.124444	15.882151	-0.095204	4.070181
491.978698	5665.149139	15.887155	-0.095214	4.067383
492.063790	5657.088598	15.892160	-0.095225	4.064553
492.150666	5649.147215	15.897165	-0.095236	4.061763
492.165718	5641.127388	15.902170	-0.095234	4.058942
492.301758	5633.136297	15.907175	-0.095254	4.056131
492.469658	5625.129823	15.912179	-0.095280	4.053314
492.075428	5617.113452	15.917184	-0.095201	4.050482
492.131656	5609.125655	15.922189	-0.095207	4.047665
492.149762	5601.131812	15.927194	-0.095205	4.044844
492.014704	5593.214794	15.932199	-0.095175	4.042045
491.798312	5585.182427	15.937203	-0.095129	4.039203
491.819154	5577.214971	15.942208	-0.095128	4.036385
491.845375	5569.147915	15.947213	-0.095128	4.033530
491.839804	5561.107376	15.952218	-0.095121	4.030682
491.728712	5553.079924	15.957223	-0.095096	4.027834
491.678525	5545.121433	15.962227	-0.095081	4.025010
491.326287	5537.158537	15.967232	-0.095010	4.022178
491.598586	5529.144801	15.972237	-0.095056	4.019336
491.521148	5521.232541	15.977242	-0.095036	4.016522
491.667363	5513.119055	15.982247	-0.095058	4.013638
491.680644	5505.141101	15.987251	-0.095056	4.010798
491.639783	5497.108232	15.992256	-0.095043	4.007936
491.443422	5489.146151	15.997261	-0.095001	4.005095
491.220732	5481.236532	16.002266	-0.094955	4.002269
490.967200	5473.186308	16.007271	-0.094902	3.999391
491.235989	5465.262369	16.012275	-0.094947	3.996565
491.221597	5457.181877	16.017280	-0.094939	3.993676
490.890928	5449.239178	16.022285	-0.094873	3.990828
491.551472	5441.154718	16.027290	-0.094990	3.987945
491.371891	5433.158793	16.032295	-0.094952	3.985077
490.941827	5425.260845	16.037299	-0.094867	3.982238
491.113979	5417.176958	16.042304	-0.094893	3.979341
490.461659	5409.320558	16.047309	-0.094767	3.976508
490.848770	5401.198785	16.052314	-0.094834	3.973597
490.760295	5393.206748	16.057319	-0.094812	3.970721
490.701367	5385.215625	16.062323	-0.094796	3.967845
490.833531	5377.164574	16.067328	-0.094815	3.964948
490.753720	5369.241567	16.072333	-0.094795	3.962091
490.918058	5361.204875	16.077338	-0.094821	3.959196
490.441861	5353.298480	16.082343	-0.094727	3.956334
490.570943	5345.229443	16.087347	-0.094746	3.953422
490.438664	5337.192395	16.092352	-0.094716	3.950515
490.556471	5329.201339	16.097357	-0.094733	3.947627
490.663624	5321.170068	16.102362	-0.094748	3.944722
490.632877	5313.196490	16.107367	-0.094737	3.941833
490.537612	5305.213129	16.112371	-0.094714	3.938937
490.476484	5297.221893	16.117376	-0.094697	3.936037
490.478430	5289.204106	16.122381	-0.094693	3.933126
490.384179	5281.215266	16.127386	-0.094670	3.930222
490.260080	5273.206457	16.132391	-0.094642	3.927308
490.248655	5265.236389	16.137395	-0.094634	3.924408
490.256640	5257.244640	16.142400	-0.094631	3.921499
490.408327	5249.214466	16.147405	-0.094654	3.918575
490.201288	5241.279275	16.152410	-0.094610	3.915678
490.107653	5233.219205	16.157415	-0.094587	3.912735
490.082114	5225.254785	16.162419	-0.094577	3.909826
489.865429	5217.291106	16.167424	-0.094532	3.906911
489.753118	5209.207586	16.172429	-0.094506	3.903952
489.888891	5201.307947	16.177434	-0.094526	3.901064
489.921015	5193.216054	16.182439	-0.094527	3.898100
489.424175	5185.309539	16.187443	-0.094429	3.895192
489.516877	5177.275136	16.192448	-0.094441	3.892246
489.734467	5169.203443	16.197453	-0.094477	3.889287
489.141217	5161.341720	16.202458	-0.094361	3.886387
489.394651	5153.253902	16.207463	-0.094403	3.883418
489.485528	5145.276932	16.212467	-0.094415	3.880485
489.830295	5137.247050	16.217472	-0.094474	3.877535
489.671041	5129.237470	16.222477	-0.094439	3.874580
489.799640	5121.141939	16.227482	-0.094458	3.871597
490.028271	5113.089302	16.232487	-0.094495	3.868629
490.089129	5105.156053	16.237491	-0.094501	3.865700
489.566566	5097.278407	16.242496	-0.094399	3.862777
489.652376	5089.252076	16.247501	-0.094410	3.859810
489.704550	5081.285207	16.252506	-0.094414	3.856862
489.229927	5073.273409	16.257511	-0.094321	3.853883
489.400328	5065.315500	16.262515	-0.094347	3.850936
489.647280	5057.253281	16.267520	-0.094388	3.847950
489.509233	5049.277248	16.272525	-0.094357	3.844985
489.832598	5041.299400	16.277530	-0.094412	3.842026
489.559072	5033.257926	16.282535	-0.094356	3.839030
489.660729	5025.315180	16.287539	-0.094370	3.836075
489.362588	5017.330506	16.292544	-0.094309	3.833094
489.580073	5009.303741	16.297549	-0.094345	3.830107
489.274105	5001.369772	16.302554	-0.094283	3.827140
489.188913	4993.262833	16.307559	-0.094262	3.824111
489.203030	4985.375323	16.312563	-0.094259	3.821164
489.362231	4977.249182	16.317568	-0.094283	3.818128
489.364800	4969.307975	16.322573	-0.094279	3.815156
489.320975	4961.358221	16.327578	-0.094266	3.812177
489.366732	4953.233709	16.332583	-0.094269	3.809133
489.412707	4945.331114	16.337587	-0.094272	3.806169
489.325289	4937.306343	16.342592	-0.094251	3.803154
489.498920	4929.338718	16.347597	-0.094278	3.800164
489.422350	4921.358370	16.352602	-0.094259	3.797161
489.228966	4913.324281	16.357607	-0.094217	3.794133
489.218035	4905.362669	16.362611	-0.094210	3.791134
489.065688	4897.340647	16.367616	-0.094177	3.788107
488.904182	4889.330635	16.372621	-0.094141	3.785081
488.731087	4881.398072	16.377626	-0.094104	3.782082
488.810773	4873.325013	16.382631	-0.094114	3.779034
488.579167	4865.432796	16.387635	-0.094066	3.776044
488.775765	4857.325827	16.392640	-0.094097	3.772980
488.977819	4849.336251	16.397645	-0.094129	3.769959
488.826103	4841.373391	16.402650	-0.094096	3.766937
488.520675	4833.359970	16.407655	-0.094034	3.763889
488.777878	4825.452705	16.412659	-0.094077	3.760893
488.691408	4817.396673	16.417664	-0.094055	3.757830
488.876335	4809.360499	16.422669	-0.094085	3.754778
488.722217	4801.425206	16.427674	-0.094051	3.751754
488.908014	4793.365033	16.432679	-0.094080	3.748688
488.799852	4785.413586	16.437683	-0.094055	3.745654
488.513150	4777.439138	16.442688	-0.093996	3.742605
488.610989	4769.434437	16.447693	-0.094010	3.739550
488.550925	4761.498642	16.452698	-0.093993	3.736516
488.530419	4753.413386	16.457703	-0.093984	3.733423
488.486118	4745.435026	16.462707	-0.093971	3.730368
488.295970	4737.434397	16.467712	-0.093930	3.727298
488.250825	4729.427767	16.472717	-0.093917	3.724227
488.346017	4721.505632	16.477722	-0.093929	3.721189
488.298078	4713.458718	16.482727	-0.093915	3.718098
488.378999	4705.452289	16.487731	-0.093925	3.715022
488.031428	4697.443335	16.492736	-0.093855	3.711932
488.199006	4689.408841	16.497741	-0.093881	3.708843
488.217196	4681.450787	16.502746	-0.093879	3.705777
488.067104	4673.427950	16.507751	-0.093846	3.702679
488.057458	4665.443785	16.512755	-0.093839	3.699597
487.988828	4657.470221	16.517760	-0.093821	3.696515
487.911016	4649.455530	16.522765	-0.093802	3.693414
487.717874	4641.486805	16.527770	-0.093761	3.690326
488.069635	4633.434969	16.532775	-0.093821	3.687216
488.161849	4625.390395	16.537779	-0.093833	3.684101
488.036897	4617.505660	16.542784	-0.093805	3.681038
488.016060	4609.470174	16.547789	-0.093796	3.677918
488.037890	4601.519726	16.552794	-0.093794	3.674829
487.672205	4593.536633	16.557799	-0.093721	3.671715
487.590607	4585.555452	16.562803	-0.093701	3.668606
487.809292	4577.485156	16.567808	-0.093736	3.665467
487.747299	4569.501840	16.572813	-0.093720	3.662353
487.556781	4561.547022	16.577818	-0.093679	3.659243
487.758473	4553.526344	16.582823	-0.093711	3.656116
487.721116	4545.540227	16.587827	-0.093699	3.652993
487.706089	4537.536276	16.592832	-0.093691	3.649861
487.761256	4529.552634	16.597837	-0.093697	3.646736
487.779481	4521.539387	16.602842	-0.093695	3.643596
487.798136	4513.583136	16.607847	-0.093693	3.640476
487.641915	4505.634893	16.612851	-0.093659	3.637351
487.549775	4497.611995	16.617856	-0.093637	3.634196
487.674875	4489.602943	16.622861	-0.093655	3.631050
487.295726	4481.619152	16.627866	-0.093579	3.627896
487.413386	4473.565118	16.632871	-0.093596	3.624727
487.443953	4465.618479	16.637875	-0.093596	3.621594
487.427927	4457.615622	16.642880	-0.093588	3.618435
487.196357	4449.638402	16.647885	-0.093540	3.615278
487.256858	4441.657496	16.652890	-0.093546	3.612124
487.121485	4433.606195	16.657895	-0.093516	3.608934
487.076298	4425.641438	16.662899	-0.093502	3.605779
487.150120	4417.627020	16.667904	-0.093511	3.602604
487.062192	4409.628262	16.672909	-0.093489	3.599428
486.998044	4401.691456	16.677914	-0.093472	3.596274
486.843516	4393.663831	16.682919	-0.093438	3.593079
487.089511	4385.635226	16.687923	-0.093479	3.589893
487.091534	4377.610423	16.692928	-0.093474	3.586697
486.843972	4369.636237	16.697933	-0.093423	3.583512
486.953214	4361.681999	16.702938	-0.093438	3.580343
486.729133	4353.720383	16.707943	-0.093391	3.577158
486.898200	4345.664898	16.712947	-0.093417	3.573944
486.813750	4337.690096	16.717952	-0.093396	3.570752
486.921140	4329.666041	16.722957	-0.093411	3.567543
487.062619	4321.648166	16.727962	-0.093432	3.564335
486.716903	4313.723059	16.732967	-0.093363	3.561147
486.912007	4305.743506	16.737971	-0.093394	3.557950
486.624713	4297.758515	16.742976	-0.093335	3.554733
486.483877	4289.741091	16.747981	-0.093304	3.551505
486.490956	4281.708950	16.752986	-0.093300	3.548273
486.613485	4273.655984	16.757991	-0.093318	3.545032
486.539684	4265.767704	16.762995	-0.093299	3.541849
486.617428	4257.695579	16.768000	-0.093308	3.538594
486.529409	4249.737802	16.773005	-0.093287	3.535377
486.312795	4241.798739	16.778010	-0.093241	3.532160
486.405026	4233.734496	16.783015	-0.093253	3.528900
486.449509	4225.779197	16.788019	-0.093256	3.525679
486.446398	4217.784037	16.793024	-0.093251	3.522437
486.162107	4209.779617	16.798029	-0.093193	3.519180
486.234785	4201.852540	16.803034	-0.093201	3.515962
486.269137	4193.812870	16.808039	-0.093202	3.512695
486.266109	4185.808899	16.813043	-0.093196	3.509438
486.074572	4177.830972	16.818048	-0.093156	3.506182
486.105271	4169.801753	16.823053	-0.093156	3.502909
486.073127	4161.853037	16.828058	-0.093145	3.499665
485.718825	4153.866101	16.833063	-0.093074	3.496391
485.849728	4145.875883	16.838067	-0.093093	3.493129
485.734381	4137.836360	16.843072	-0.093066	3.489835
486.122448	4129.801008	16.848077	-0.093134	3.486556
485.700426	4121.895482	16.853082	-0.093050	3.483301
485.759835	4113.897470	16.858087	-0.093056	3.480021
485.725565	4105.927397	16.863091	-0.093044	3.476746
485.785217	4097.889764	16.868096	-0.093050	3.473443
485.708774	4089.872985	16.873101	-0.093031	3.470141
485.656129	4081.898316	16.878106	-0.093016	3.466854
485.557754	4073.860018	16.883111	-0.092992	3.463537
485.624611	4065.919653	16.888115	-0.093000	3.460262
485.659822	4057.888890	16.893120	-0.093001	3.456945
485.541176	4049.938729	16.898125	-0.092974	3.453654
485.628412	4041.939435	16.903130	-0.092985	3.450346
485.354560	4033.946459	16.908135	-0.092929	3.447025
485.446784	4025.944067	16.913139	-0.092941	3.443709
485.338322	4018.003439	16.918144	-0.092915	3.440409
485.452013	4009.990585	16.923149	-0.092931	3.437084
485.602019	4001.991441	16.928154	-0.092954	3.433762
485.269104	3994.016740	16.933159	-0.092887	3.430430
485.357472	3986.008228	16.938163	-0.092898	3.427096
485.358133	3977.998314	16.943168	-0.092893	3.423755
485.265993	3970.035354	16.948173	-0.092871	3.420427
485.315584	3962.072820	16.953178	-0.092875	3.417101
485.142676	3954.056858	16.958183	-0.092838	3.413741
485.270607	3946.062350	16.963187	-0.092856	3.410398
485.118229	3938.094016	16.968192	-0.092823	3.407052
485.023074	3930.064055	16.973197	-0.092800	3.403679
485.027859	3922.103486	16.978202	-0.092796	3.400336
484.910075	3914.116607	16.983207	-0.092769	3.396974
484.965225	3906.092600	16.988211	-0.092774	3.393599
484.881591	3898.064670	16.993216	-0.092753	3.390214
484.900377	3890.070839	16.998221	-0.092751	3.386844
484.963484	3882.064166	17.003226	-0.092758	3.383467
484.867064	3874.096126	17.008231	-0.092735	3.380096
484.931573	3866.137747	17.013235	-0.092742	3.376733
484.741953	3858.136193	17.018240	-0.092701	3.373338
484.629758	3850.124323	17.023245	-0.092675	3.369939
484.591367	3842.164227	17.028250	-0.092663	3.366560
484.438542	3834.158874	17.033255	-0.092629	3.363155
484.503298	3826.189775	17.038259	-0.092636	3.359770
484.580496	3818.198998	17.043264	-0.092645	3.356373
484.473638	3810.204509	17.048269	-0.092620	3.352963
484.282271	3802.222672	17.053274	-0.092580	3.349553
484.211964	3794.219437	17.058279	-0.092561	3.346134
484.313043	3786.231998	17.063283	-0.092575	3.342725
484.006836	3778.261539	17.068288	-0.092513	3.339305
484.123827	3770.278805	17.073293	-0.092529	3.335892
484.290249	3762.275063	17.078298	-0.092555	3.332468
484.122468	3754.246549	17.083303	-0.092519	3.329017
484.252318	3746.302447	17.088307	-0.092538	3.325610
484.076627	3738.318147	17.093312	-0.092500	3.322171
484.021361	3730.314054	17.098317	-0.092485	3.318724
483.927921	3722.363008	17.103322	-0.092462	3.315296
484.023437	3714.333115	17.108327	-0.092475	3.311836
484.028629	3706.316069	17.113331	-0.092470	3.308376
483.882833	3698.293564	17.118336	-0.092438	3.304903
483.886965	3690.354762	17.123341	-0.092434	3.301469
483.962428	3682.365894	17.128346	-0.092443	3.298012
483.505068	3674.391891	17.133351	-0.092352	3.294537
483.445054	3666.396923	17.138355	-0.092336	3.291065
483.543460	3658.350044	17.143360	-0.092349	3.287573
483.490552	3650.360624	17.148365	-0.092334	3.284097
483.693049	3642.424448	17.153370	-0.092367	3.280650
483.629390	3634.422798	17.158375	-0.092350	3.277160
483.588693	3626.447626	17.163379	-0.092337	3.273679
483.367083	3618.469016	17.168384	-0.092291	3.270185
483.272790	3610.492307	17.173389	-0.092268	3.266694
483.302167	3602.496360	17.178394	-0.092268	3.263196
483.308056	3594.489787	17.183399	-0.092264	3.259688
483.324059	3586.512947	17.188403	-0.092262	3.256189
483.222643	3578.490210	17.193408	-0.092238	3.252663
483.392434	3570.482208	17.198413	-0.092264	3.249149
483.250122	3562.572179	17.203418	-0.092233	3.245663
483.319776	3554.551034	17.208423	-0.092241	3.242132
483.399172	3546.561031	17.213427	-0.092250	3.238612
483.115380	3538.638514	17.218432	-0.092192	3.235102
483.007717	3530.619211	17.223437	-0.092167	3.231553
483.230552	3522.591017	17.228442	-0.092203	3.228011
482.930315	3514.576561	17.233447	-0.092142	3.224448
483.011233	3506.630733	17.238451	-0.092152	3.220928
482.923929	3498.618135	17.243456	-0.092131	3.217367
483.011817	3490.597101	17.248461	-0.092142	3.213806
482.763871	3482.642849	17.253466	-0.092091	3.210257
482.704006	3474.620025	17.258471	-0.092074	3.206681
482.715037	3466.671479	17.263475	-0.092071	3.203137
482.681971	3458.671645	17.268480	-0.092060	3.199565
482.452173	3450.726884	17.273485	-0.092012	3.196004
482.605494	3442.708902	17.278490	-0.092035	3.192424
482.583065	3434.679167	17.283495	-0.092026	3.188826
482.671831	3426.691605	17.288499	-0.092037	3.185249
482.733351	3418.719089	17.293504	-0.092044	3.181672
482.602670	3410.764429	17.298509	-0.092014	3.178092
482.527754	3402.790497	17.303514	-0.091995	3.174501
482.293959	3394.805076	17.308519	-0.091947	3.170894
482.474550	3386.780130	17.313523	-0.091975	3.167283
482.420485	3378.792026	17.318528	-0.091960	3.163674
482.206106	3370.872949	17.323533	-0.091915	3.160085
482.224513	3362.882900	17.328538	-0.091913	3.156471
482.193788	3354.857926	17.333543	-0.091902	3.152834
481.947678	3346.888218	17.338547	-0.091851	3.149208
481.921896	3338.888196	17.343552	-0.091841	3.145574
482.109852	3330.855013	17.348557	-0.091871	3.141931
482.044055	3322.895285	17.353562	-0.091854	3.138305
481.690034	3314.933010	17.358567	-0.091783	3.134661
481.773893	3306.970122	17.363571	-0.091793	3.131033
481.744725	3298.934779	17.368576	-0.091782	3.127362
481.509677	3290.977903	17.373581	-0.091734	3.123713
481.485731	3283.022268	17.378586	-0.091724	3.120070
481.344905	3275.001882	17.383591	-0.091693	3.116387
481.165164	3267.052076	17.388595	-0.091654	3.112731
481.378181	3258.999498	17.393600	-0.091688	3.109041
481.472483	3251.002263	17.398605	-0.091701	3.105367
481.338524	3243.055807	17.403610	-0.091671	3.101702
481.223629	3235.051917	17.408615	-0.091644	3.098006
481.374066	3227.064520	17.413619	-0.091667	3.094326
481.633109	3219.050534	17.418624	-0.091710	3.090635
481.359775	3211.104246	17.423629	-0.091654	3.086945
481.328377	3203.122040	17.428634	-0.091643	3.083246
481.409345	3195.131892	17.433639	-0.091653	3.079544
481.522578	3187.160104	17.438643	-0.091669	3.075848
481.318590	3179.146500	17.443648	-0.091626	3.072112
481.294969	3171.142979	17.448653	-0.091616	3.068385
481.168374	3163.188586	17.453658	-0.091588	3.064672
480.895263	3155.238290	17.458663	-0.091532	3.060949
481.080951	3147.224337	17.463667	-0.091561	3.057214
481.153909	3139.202411	17.468672	-0.091569	3.053465
481.333535	3131.183897	17.473677	-0.091598	3.049718
481.202152	3123.250059	17.478682	-0.091568	3.045992
480.879121	3115.310737	17.483687	-0.091503	3.042248
481.152057	3107.294616	17.488691	-0.091548	3.038493
480.917626	3099.341300	17.493696	-0.091500	3.034739
480.877007	3091.343887	17.498701	-0.091487	3.030968
480.931659	3083.342485	17.503706	-0.091492	3.027195
480.581974	3075.383625	17.508711	-0.091422	3.023418
480.724813	3067.396221	17.513715	-0.091443	3.019647
480.712353	3059.422590	17.518720	-0.091436	3.015870
480.598810	3051.436741	17.523725	-0.091409	3.012077
480.628861	3043.443178	17.528730	-0.091410	3.008283
480.627835	3035.436074	17.533735	-0.091405	3.004477
480.629855	3027.516795	17.538739	-0.091400	3.000707
480.255178	3019.557887	17.543744	-0.091325	2.996895
480.270186	3011.520668	17.548749	-0.091322	2.993060
480.622302	3003.487105	17.553754	-0.091383	2.989239
480.504195	2995.502879	17.558759	-0.091356	2.985413
480.462506	2987.556577	17.563763	-0.091343	2.981605
480.313825	2979.564950	17.568768	-0.091310	2.977764
480.111618	2971.596620	17.573773	-0.091267	2.973926
480.202348	2963.616830	17.578778	-0.091279	2.970093
480.145824	2955.612662	17.583783	-0.091263	2.966236
480.189781	2947.643005	17.588787	-0.091266	2.962396
480.057821	2939.679465	17.593792	-0.091237	2.958544
480.034097	2931.720421	17.598797	-0.091227	2.954695
480.177436	2923.709758	17.603802	-0.091249	2.950825
479.947842	2915.721847	17.608807	-0.091201	2.946941
479.824753	2907.738748	17.613811	-0.091173	2.943060
479.866950	2899.762934	17.618816	-0.091175	2.939187
479.692276	2891.832274	17.623821	-0.091138	2.935318
479.917096	2883.805566	17.628826	-0.091174	2.931419
479.795114	2875.820514	17.633831	-0.091146	2.927517
479.915129	2867.827184	17.638835	-0.091164	2.923618
479.607493	2859.905668	17.643840	-0.091101	2.919726
479.531210	2851.933006	17.648845	-0.091082	2.915816
479.825347	2843.862646	17.653850	-0.091132	2.911873
479.491139	2835.898157	17.658855	-0.091064	2.907943
479.357435	2827.909019	17.663859	-0.091034	2.904006
479.239144	2819.977212	17.668864	-0.091007	2.900093
479.318124	2811.956372	17.673869	-0.091016	2.896142
479.314854	2803.991630	17.678874	-0.091011	2.892208
479.332130	2795.965403	17.683879	-0.091009	2.888240
479.403941	2787.971805	17.688883	-0.091017	2.884285
479.321431	2780.041687	17.693888	-0.090997	2.880348
479.361949	2772.051449	17.698893	-0.090999	2.876382
479.327749	2764.106349	17.703898	-0.090987	2.872429
478.936222	2756.141103	17.708903	-0.090909	2.868441
478.862547	2748.171864	17.713907	-0.090891	2.864463
478.813895	2740.194032	17.718912	-0.090876	2.860477
478.954449	2732.170949	17.723917	-0.090897	2.856473
479.028275	2724.185310	17.728922	-0.090906	2.852478
478.947739	2716.200389	17.733927	-0.090886	2.848469
478.877472	2708.230551	17.738931	-0.090868	2.844463
478.797099	2700.303533	17.743936	-0.090847	2.840472
478.413713	2692.377756	17.748941	-0.090771	2.836459
478.333679	2684.398951	17.753946	-0.090751	2.832431
478.404286	2676.359886	17.758951	-0.090759	2.828375
478.328073	2668.352279	17.763955	-0.090739	2.824321
478.592825	2660.339116	17.768960	-0.090784	2.820278
478.674238	2652.356603	17.773965	-0.090794	2.816234
478.474379	2644.435824	17.778970	-0.090751	2.812199
478.355319	2636.424558	17.783975	-0.090724	2.808117
478.429199	2628.453468	17.788979	-0.090733	2.804061
478.133060	2620.540510	17.793984	-0.090672	2.800006
477.915472	2612.580576	17.798989	-0.090627	2.795927
478.202606	2604.549787	17.803994	-0.090675	2.791835
478.157764	2596.546220	17.808999	-0.090661	2.787732
478.085588	2588.567993	17.814003	-0.090643	2.783633
477.620341	2580.691900	17.819008	-0.090551	2.779558
477.607250	2572.703657	17.824013	-0.090544	2.775446
477.739824	2564.670198	17.829018	-0.090563	2.771313
477.858899	2556.646003	17.834023	-0.090580	2.767179
478.264330	2548.634375	17.839027	-0.090650	2.763062
477.717038	2540.771049	17.844032	-0.090543	2.758957
477.684102	2532.793922	17.849037	-0.090532	2.754819
477.862221	2524.741919	17.854042	-0.090560	2.750649
477.676771	2516.761358	17.859047	-0.090520	2.746487
477.810180	2508.803617	17.864051	-0.090540	2.742350
477.908860	2500.812901	17.869056	-0.090553	2.738188
477.690712	2492.863095	17.874061	-0.090508	2.734021
477.753706	2484.888379	17.879066	-0.090514	2.729852
477.516351	2476.917086	17.884071	-0.090465	2.725660
477.614010	2468.948960	17.889075	-0.090478	2.721484
477.670327	2460.980758	17.894080	-0.090483	2.717299
477.478769	2453.023777	17.899085	-0.090442	2.713097
477.317685	2445.072602	17.904090	-0.090407	2.708895
477.189642	2437.067850	17.909095	-0.090378	2.704659
477.166540	2429.155627	17.914099	-0.090369	2.700472
477.037834	2421.175421	17.919104	-0.090340	2.696236
477.115100	2413.165234	17.924109	-0.090349	2.691991
477.508104	2405.126385	17.929114	-0.090417	2.687744
477.216416	2397.184405	17.934119	-0.090358	2.683498
477.081300	2389.254239	17.939123	-0.090327	2.679261
476.539747	2381.382745	17.944128	-0.090221	2.675023
476.388154	2373.384839	17.949133	-0.090188	2.670736
476.653576	2365.344775	17.954138	-0.090232	2.666446
476.660374	2357.332897	17.959143	-0.090228	2.662148
476.629340	2349.366456	17.964147	-0.090217	2.657864
476.362863	2341.422105	17.969152	-0.090163	2.653570
476.602628	2333.377246	17.974157	-0.090202	2.649249
476.751992	2325.426697	17.979162	-0.090225	2.644965
476.516362	2317.486592	17.984167	-0.090176	2.640654
476.293482	2309.586221	17.989171	-0.090129	2.636359
476.111097	2301.598133	17.994176	-0.090090	2.632011
476.337437	2293.571494	17.999181	-0.090127	2.627663
476.285224	2285.608080	18.004186	-0.090112	2.623324
475.610905	2277.749588	18.009191	-0.089982	2.618992
476.003424	2269.699577	18.014195	-0.090049	2.614621
475.872023	2261.725913	18.019200	-0.090020	2.610248
476.115952	2253.703961	18.024205	-0.090060	2.605868
476.054165	2245.781351	18.029210	-0.090044	2.601514
475.524623	2237.876535	18.034215	-0.089940	2.597130
476.019471	2229.781971	18.039219	-0.090027	2.592704
476.146779	2221.710986	18.044224	-0.090045	2.588259
475.826616	2213.775617	18.049229	-0.089980	2.583850
475.916111	2205.834396	18.054234	-0.089992	2.579459
476.022831	2197.881968	18.059239	-0.090007	2.575055
475.962444	2189.933631	18.064243	-0.089990	2.570634
475.639107	2182.007112	18.069248	-0.089925	2.566200
475.491073	2174.055166	18.074253	-0.089892	2.561755
475.818826	2166.066103	18.079258	-0.089948	2.557316
475.156986	2158.189964	18.084263	-0.089820	2.552862
475.345714	2150.160778	18.089267	-0.089850	2.548375
475.534632	2142.136978	18.094272	-0.089880	2.543883
475.413790	2134.185708	18.099277	-0.089852	2.539402
475.595815	2126.215275	18.104282	-0.089881	2.534924
475.515987	2118.252344	18.109287	-0.089861	2.530424
475.403435	2110.312793	18.114291	-0.089835	2.525926
475.427419	2102.360789	18.119296	-0.089834	2.521423
475.601278	2094.373150	18.124301	-0.089862	2.516902
475.691109	2086.425681	18.129306	-0.089873	2.512391
475.302609	2078.463898	18.134311	-0.089796	2.507827
475.177337	2070.520481	18.139315	-0.089767	2.503286
475.407060	2062.515239	18.144320	-0.089805	2.498726
475.118525	2054.585491	18.149325	-0.089746	2.494164
475.259102	2046.600759	18.154330	-0.089767	2.489593
475.072649	2038.637372	18.159335	-0.089727	2.485002
475.214567	2030.688502	18.164339	-0.089748	2.480435
475.014510	2022.764512	18.169344	-0.089706	2.475849
474.790340	2014.798848	18.174349	-0.089659	2.471228
474.924487	2006.809623	18.179354	-0.089679	2.466612
474.936545	1998.837034	18.184359	-0.089676	2.461987
475.022596	1990.876662	18.189363	-0.089687	2.457367
474.719608	1982.944632	18.194368	-0.089625	2.452724
474.635182	1974.978154	18.199373	-0.089605	2.448070
474.811915	1966.992674	18.204378	-0.089632	2.443415
474.863473	1959.022057	18.209383	-0.089637	2.438751
474.703456	1951.110331	18.214387	-0.089602	2.434096
474.740914	1943.096413	18.219392	-0.089604	2.429387
474.516581	1935.147046	18.224397	-0.089557	2.424687
474.874857	1927.134987	18.229402	-0.089618	2.419986
474.826387	1919.195042	18.234407	-0.089604	2.415287
474.465313	1911.301458	18.239411	-0.089532	2.410581
474.629541	1903.295850	18.244416	-0.089557	2.405841
474.482330	1895.348331	18.249421	-0.089525	2.401102
474.459736	1887.425806	18.254426	-0.089515	2.396378
474.177294	1879.476721	18.259431	-0.089458	2.391608
474.274425	1871.494523	18.264435	-0.089471	2.386839
474.110466	1863.556553	18.269440	-0.089435	2.382066
474.194152	1855.568276	18.274445	-0.089445	2.377274
474.012554	1847.654874	18.279450	-0.089407	2.372495
473.834207	1839.696081	18.284455	-0.089368	2.367679
474.039893	1831.701904	18.289459	-0.089401	2.362863
474.064185	1823.766725	18.294464	-0.089401	2.358059
473.625184	1815.877130	18.299469	-0.089314	2.353234
473.423222	1807.928469	18.304474	-0.089271	2.348383
473.638536	1799.878192	18.309479	-0.089306	2.343495
473.712461	1791.954456	18.314483	-0.089315	2.338661
473.174190	1784.058441	18.319488	-0.089209	2.333784
473.335153	1776.042576	18.324493	-0.089234	2.328881
473.544703	1768.052555	18.329498	-0.089268	2.323988
473.687405	1760.074186	18.334503	-0.089290	2.319087
473.346081	1752.211820	18.339507	-0.089221	2.314205
473.312769	1744.252600	18.344512	-0.089210	2.309280
472.964429	1736.328550	18.349517	-0.089140	2.304339
473.146783	1728.353886	18.354522	-0.089168	2.299401
472.994695	1720.392503	18.359527	-0.089135	2.294432
472.840375	1712.470012	18.364531	-0.089101	2.289476
473.035084	1704.468598	18.369536	-0.089132	2.284490
472.743553	1696.586453	18.374541	-0.089073	2.279526
472.960696	1688.582566	18.379546	-0.089108	2.274519
472.854342	1680.593506	18.384551	-0.089083	2.269482
472.845001	1672.641875	18.389555	-0.089076	2.264466
472.633231	1664.726186	18.394560	-0.089032	2.259444
472.797206	1656.732992	18.399565	-0.089057	2.254394
473.054822	1648.752603	18.404570	-0.089100	2.249350
472.852259	1640.825866	18.409575	-0.089057	2.244287
472.404899	1632.989077	18.414579	-0.088969	2.239249
472.712169	1624.983891	18.419584	-0.089021	2.234159
472.389539	1617.079833	18.424589	-0.088956	2.229066
472.337720	1609.123431	18.429594	-0.088941	2.223951
471.981620	1601.231113	18.434599	-0.088869	2.218839
472.097300	1593.263862	18.439603	-0.088886	2.213709
471.940115	1585.321447	18.444608	-0.088851	2.208558
472.048526	1577.335079	18.449613	-0.088866	2.203392
472.009661	1569.405484	18.454618	-0.088854	2.198236
471.927986	1561.461309	18.459623	-0.088834	2.193055
471.892315	1553.532284	18.464627	-0.088822	2.187876
472.020770	1545.522695	18.469632	-0.088841	2.182647
471.650367	1537.645053	18.474637	-0.088767	2.177445
471.642131	1529.707105	18.479642	-0.088760	2.172225
471.689077	1521.721681	18.484647	-0.088764	2.166967
471.779114	1513.775150	18.489651	-0.088775	2.161725
471.414361	1505.915029	18.494656	-0.088702	2.156485
471.279133	1497.971848	18.499661	-0.088672	2.151199
471.758982	1489.941016	18.504666	-0.088756	2.145900
471.408729	1482.054793	18.509671	-0.088686	2.140605
471.785910	1474.075476	18.514675	-0.088751	2.135304
471.770529	1466.112951	18.519680	-0.088743	2.129964
471.640928	1458.194058	18.524685	-0.088714	2.124628
471.699532	1450.291076	18.529690	-0.088720	2.119309
471.390884	1442.404239	18.534695	-0.088657	2.113950
471.243253	1434.456967	18.539699	-0.088624	2.108553
471.165478	1426.506224	18.544704	-0.088605	2.103147
471.223883	1418.555494	18.549709	-0.088611	2.097740
470.982805	1410.674697	18.554714	-0.088561	2.092337
470.673987	1402.746599	18.559719	-0.088498	2.086880
470.973663	1394.755251	18.564723	-0.088549	2.081427
471.010012	1386.833472	18.569728	-0.088550	2.075982
470.605949	1378.946876	18.574733	-0.088470	2.070501
470.792275	1370.975170	18.579738	-0.088499	2.065007
470.725883	1363.050996	18.584743	-0.088482	2.059506
470.645269	1355.147868	18.589747	-0.088462	2.054003
470.543428	1347.216977	18.594752	-0.088438	2.048463
470.519384	1339.289230	18.599757	-0.088428	2.042919
470.456322	1331.386746	18.604762	-0.088411	2.037373
470.616210	1323.408583	18.609767	-0.088436	2.031783
470.402241	1315.507248	18.614771	-0.088391	2.026192
470.458320	1307.562325	18.619776	-0.088396	2.020582
470.449508	1299.639108	18.624781	-0.088390	2.014966
470.595067	1291.682820	18.629786	-0.088412	2.009327
470.564514	1283.758696	18.634791	-0.088401	2.003676
470.479820	1275.868682	18.639795	-0.088380	1.998028
470.328059	1267.978600	18.644800	-0.088347	1.992357
470.534040	1260.005258	18.649805	-0.088380	1.986648
470.589542	1252.090295	18.654810	-0.088385	1.980949
470.002124	1244.253825	18.659815	-0.088271	1.975220
469.992609	1236.322008	18.664819	-0.088264	1.969468
469.972520	1228.402280	18.669824	-0.088255	1.963707
469.777721	1220.532851	18.674829	-0.088214	1.957946
469.282726	1212.683019	18.679834	-0.088116	1.952150
469.585673	1204.670125	18.684839	-0.088168	1.946304
469.567869	1196.741196	18.689843	-0.088159	1.940468
469.273222	1188.851254	18.694848	-0.088099	1.934612
468.917841	1180.977957	18.699853	-0.088028	1.928743
469.417840	1172.953579	18.704858	-0.088116	1.922840
469.261297	1165.067435	18.709863	-0.088082	1.916948
469.451001	1157.118726	18.714867	-0.088112	1.911031
469.714390	1149.150610	18.719872	-0.088156	1.905089
469.633897	1141.272830	18.724877	-0.088136	1.899157
469.276798	1133.441536	18.729882	-0.088064	1.893209
469.101010	1125.529837	18.734887	-0.088026	1.887203
469.166166	1117.625984	18.739891	-0.088033	1.881212
469.090730	1109.725913	18.744896	-0.088014	1.875188
469.027382	1101.815133	18.749901	-0.087997	1.869138
468.998058	1093.913996	18.754906	-0.087987	1.863079
468.801820	1086.021572	18.759911	-0.087945	1.856988
468.606751	1078.139646	18.764915	-0.087904	1.850884
468.681354	1070.201727	18.769920	-0.087912	1.844750
468.354387	1062.383813	18.774925	-0.087846	1.838640
468.077317	1054.517044	18.779930	-0.087790	1.832477
468.270278	1046.535660	18.784935	-0.087821	1.826261
468.372159	1038.618743	18.789939	-0.087834	1.820063
467.932843	1030.804044	18.794944	-0.087748	1.813858
468.117471	1022.838140	18.799949	-0.087777	1.807589
467.970243	1014.985320	18.804954	-0.087744	1.801347
467.736611	1007.117970	18.809959	-0.087696	1.795061
467.491445	999.222742	18.814963	-0.087645	1.788729
467.829627	991.247947	18.819968	-0.087703	1.782384
467.855126	983.357271	18.824973	-0.087703	1.776044
467.646929	975.498511	18.829978	-0.087659	1.769679
467.593672	967.608756	18.834983	-0.087644	1.763284
467.635112	959.729361	18.839987	-0.087646	1.756887
467.424715	951.870434	18.844992	-0.087602	1.750451
467.214470	943.997900	18.849997	-0.087558	1.743979
467.337353	936.098277	18.855002	-0.087576	1.737505
467.373866	928.189545	18.860007	-0.087577	1.730987
467.058172	920.369878	18.865011	-0.087514	1.724473
467.041013	912.511046	18.870016	-0.087505	1.717941
467.026452	904.613667	18.875021	-0.087497	1.711351
466.923128	896.747097	18.880026	-0.087473	1.704751
466.656833	888.900293	18.885031	-0.087419	1.698119
466.678212	881.019059	18.890035	-0.087417	1.691471
466.285961	873.200815	18.895040	-0.087339	1.684795
465.787790	865.419898	18.900045	-0.087242	1.678109
465.978563	857.479995	18.905050	-0.087272	1.671354
466.033903	849.566404	18.910055	-0.087277	1.664575
466.044021	841.699003	18.915059	-0.087274	1.657803
465.826374	833.860529	18.920064	-0.087228	1.650996
465.948075	825.954254	18.925069	-0.087246	1.644150
466.024218	818.100328	18.930074	-0.087255	1.637314
465.621354	810.275091	18.935079	-0.087175	1.630407
465.695261	802.386261	18.940083	-0.087184	1.623482
465.540361	794.554759	18.945088	-0.087150	1.616546
465.692994	786.643464	18.950093	-0.087173	1.609553
465.606023	778.820225	18.955098	-0.087152	1.602573
465.666124	770.953608	18.960103	-0.087158	1.595545
465.428084	763.163138	18.965107	-0.087109	1.588512
465.193888	755.337182	18.970112	-0.087060	1.581415
465.102108	747.510643	18.975117	-0.087038	1.574307
464.734508	739.730214	18.980122	-0.086964	1.567168
464.656304	731.872145	18.985127	-0.086945	1.559968
464.707245	724.032815	18.990131	-0.086949	1.552771
464.628898	716.185900	18.995136	-0.086930	1.545514
464.338185	708.399436	19.000141	-0.086870	1.538247
464.245912	700.564102	19.005146	-0.086848	1.530930
464.454718	692.666666	19.010151	-0.086882	1.523565
464.370978	684.863548	19.015155	-0.086861	1.516209
463.907440	677.112879	19.020160	-0.086770	1.508807
463.667057	669.318183	19.025165	-0.086720	1.501362
463.699844	661.485855	19.030170	-0.086721	1.493886
463.527620	653.663726	19.035175	-0.086684	1.486351
463.414563	645.883450	19.040179	-0.086658	1.478826
463.135700	638.094406	19.045184	-0.086601	1.471228
462.865026	630.286352	19.050189	-0.086546	1.463574
462.633880	622.502223	19.055194	-0.086498	1.455909
462.261269	614.731210	19.060199	-0.086423	1.448193
462.032267	606.948256	19.065203	-0.086376	1.440447
461.825614	599.172382	19.070208	-0.086332	1.432670
461.298219	591.417579	19.075213	-0.086229	1.424819
460.344079	583.775319	19.080218	-0.086046	1.416966
459.123121	576.122041	19.085223	-0.085814	1.409013
459.033332	568.265568	19.090227	-0.085792	1.400998
457.189283	560.744022	19.095232	-0.085444	1.392982
455.228629	553.154368	19.100237	-0.085074	1.384828
453.453996	545.545831	19.105242	-0.084739	1.376638
452.306894	537.794439	19.110247	-0.084520	1.368358
451.437887	530.020530	19.115251	-0.084353	1.360053
450.302855	522.308791	19.120256	-0.084137	1.351714
449.080210	514.598457	19.125261	-0.083904	1.343310
448.395577	506.812428	19.130266	-0.083772	1.334867
447.361310	499.069037	19.135271	-0.083574	1.326353
446.231644	491.395804	19.140275	-0.083359	1.317843
444.984917	483.642340	19.145280	-0.083122	1.309167
443.804733	475.911686	19.150285	-0.082897	1.300471
442.890644	468.196085	19.155290	-0.082722	1.291782
441.568604	460.523093	19.160295	-0.082471	1.283004
440.477504	452.849213	19.165299	-0.082263	1.274208
439.421765	445.147661	19.170304	-0.082061	1.265326
437.695344	437.589599	19.175309	-0.081735	1.256415
436.989900	429.828809	19.180314	-0.081598	1.247405
435.864966	422.158313	19.185319	-0.081384	1.238352
434.874723	414.479022	19.190323	-0.081195	1.229247
434.229043	406.739271	19.195328	-0.081070	1.220072
432.729822	399.163827	19.200333	-0.080785	1.210850
431.571396	391.541464	19.205338	-0.080565	1.201570
430.568514	383.887997	19.210343	-0.080373	1.192211
429.529643	376.247106	19.215347	-0.080175	1.182786
428.511512	368.608965	19.220352	-0.079980	1.173292
427.200057	361.032768	19.225357	-0.079731	1.163734
425.920530	353.481432	19.230362	-0.079488	1.154135
424.827962	345.830329	19.235367	-0.079280	1.144369
423.916938	338.212251	19.240371	-0.079105	1.134600
423.008285	330.598106	19.245376	-0.078931	1.124752
421.706575	323.067031	19.250381	-0.078684	1.114835
420.493659	315.526362	19.255386	-0.078453	1.104837
419.514949	307.935345	19.260391	-0.078266	1.094733
419.032206	300.289974	19.265395	-0.078171	1.084576
417.794807	292.812937	19.270400	-0.077936	1.074374
416.729991	285.286944	19.275405	-0.077733	1.064047
416.004459	277.726610	19.280410	-0.077593	1.053651
414.817560	270.245158	19.285415	-0.077367	1.043151
413.640672	262.792818	19.290419	-0.077143	1.032585
412.625246	255.309902	19.295424	-0.076949	1.021906
411.734957	247.822970	19.300429	-0.076779	1.011139
410.386571	240.439099	19.305434	-0.076523	1.000289
409.144767	233.015684	19.310439	-0.076287	0.989289
408.067128	225.590319	19.315443	-0.076081	0.978203
407.166663	218.144234	19.320448	-0.075909	0.967005
405.729932	210.821168	19.325453	-0.075637	0.955720
404.928914	203.397910	19.330458	-0.075483	0.944315
404.570882	195.907962	19.335463	-0.075411	0.932787
403.918955	188.515669	19.340467	-0.075285	0.921186
402.509836	181.283060	19.345472	-0.075018	0.909479
401.607916	173.953109	19.350477	-0.074845	0.897606
400.473173	166.705182	19.355482	-0.074629	0.885639
399.267123	159.478042	19.360487	-0.074400	0.873522
398.132117	152.275294	19.365491	-0.074184	0.861294
397.472684	144.999073	19.370496	-0.074057	0.848907
396.430129	137.819557	19.375501	-0.073858	0.836386
395.896424	130.565341	19.380506	-0.073754	0.823701
394.796884	123.446798	19.385511	-0.073545	0.810879
393.603330	116.377048	19.390515	-0.073318	0.797909
392.507045	109.324007	19.395520	-0.073109	0.784785
391.732523	102.235181	19.400525	-0.072960	0.771478
390.524404	95.269822	19.405530	-0.072731	0.758023
389.011128	88.379273	19.410535	-0.072445	0.744365
388.219296	81.392823	19.415539	-0.072293	0.730514
387.218748	74.674273	19.420544	-0.072102	0.716855