Fri Apr 16 19:38:31 2021

Number of Points = 3643
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.069148	-0.083910	0.000000	-0.000024	0.314272

0.792807	-0.034888	0.005005	0.000027	0.314267
0.669963	-0.010554	0.010010	0.000050	0.314277
0.760598	-0.026185	0.015014	0.000033	0.314281
0.826889	-0.041996	0.020019	0.000021	0.314264
1.067294	-0.089352	0.025024	-0.000024	0.314247
1.009553	-0.081898	0.030029	-0.000014	0.314234
1.052433	-0.085785	0.035034	-0.000022	0.314252
0.975725	-0.072732	0.040038	-0.000008	0.314249
0.763325	-0.034372	0.045043	0.000032	0.314248
1.045906	-0.082748	0.050048	-0.000021	0.314262
1.237497	-0.121105	0.055053	-0.000056	0.314246
0.979076	-0.070209	0.060058	-0.000008	0.314264
1.018086	-0.077920	0.065062	-0.000016	0.314262
1.242641	-0.162771	0.070067	-0.000058	0.314059
1.116890	-0.168756	0.075072	-0.000034	0.313927
1.357928	-0.215606	0.080077	-0.000079	0.313913
1.172497	-0.180248	0.085082	-0.000045	0.313921
0.985378	-0.147254	0.090086	-0.000010	0.313917
1.056432	-0.165519	0.095091	-0.000023	0.313893
1.162584	-0.192475	0.100096	-0.000043	0.313858
1.440323	-0.302008	0.105101	-0.000095	0.313586
1.560758	-0.322995	0.110106	-0.000117	0.313590
1.499600	-0.310371	0.115110	-0.000106	0.313598
1.590349	-0.328744	0.120115	-0.000123	0.313589
1.680854	-0.393191	0.125120	-0.000140	0.313368
1.443540	-0.369672	0.130125	-0.000096	0.313278
1.739641	-0.426063	0.135130	-0.000151	0.313266
1.592091	-0.397729	0.140134	-0.000124	0.313274
1.472579	-0.436569	0.145139	-0.000102	0.312994
1.514822	-0.445456	0.150144	-0.000109	0.312989
1.554074	-0.454948	0.155149	-0.000117	0.312979
1.221197	-0.426686	0.160154	-0.000055	0.312830
1.187106	-0.460239	0.165158	-0.000049	0.312647
1.170949	-0.458536	0.170163	-0.000046	0.312641
1.372336	-0.499829	0.175168	-0.000083	0.312620
1.357213	-0.561458	0.180173	-0.000081	0.312322
1.201779	-0.529947	0.185178	-0.000052	0.312338
1.498856	-0.588119	0.190182	-0.000107	0.312319
1.235210	-0.607310	0.195187	-0.000058	0.312008
1.677444	-0.687422	0.200192	-0.000140	0.312010
1.540178	-0.683928	0.205197	-0.000115	0.311911
1.361930	-0.694807	0.210202	-0.000082	0.311710
1.428556	-0.706976	0.215206	-0.000094	0.311710
1.465670	-0.764322	0.220211	-0.000101	0.311476
1.279330	-0.749965	0.225216	-0.000067	0.311386
0.994400	-0.707932	0.230221	-0.000014	0.311341
1.052371	-0.773602	0.235226	-0.000025	0.311085
1.197358	-0.801182	0.240230	-0.000052	0.311079
1.111774	-0.832810	0.245235	-0.000036	0.310860
1.132061	-0.856109	0.250240	-0.000040	0.310769
1.215574	-0.887956	0.255245	-0.000055	0.310692
1.066592	-0.897620	0.260250	-0.000028	0.310521
0.902268	-0.867188	0.265254	0.000003	0.310525
0.973531	-0.956235	0.270259	-0.000010	0.310170
0.818650	-0.925261	0.275264	0.000018	0.310184
0.589400	-0.937953	0.280269	0.000061	0.309931
0.369951	-0.912200	0.285274	0.000102	0.309865
0.138252	-0.898958	0.290278	0.000145	0.309731
-0.063947	-0.902655	0.295283	0.000182	0.309542
0.229697	-0.962487	0.300288	0.000128	0.309512
0.291034	-1.027848	0.305293	0.000116	0.309259
0.454535	-1.057064	0.310298	0.000086	0.309262
0.793179	-1.191102	0.315302	0.000023	0.308923
0.352570	-1.109300	0.320307	0.000105	0.308931
0.691605	-1.235378	0.325312	0.000041	0.308630
0.501082	-1.206578	0.330317	0.000077	0.308603
0.395531	-1.251972	0.335322	0.000096	0.308300
0.529360	-1.286061	0.340326	0.000071	0.308255
-0.224755	-1.199252	0.345331	0.000212	0.308020
0.412852	-1.331661	0.350336	0.000093	0.307942
0.335475	-1.378442	0.355341	0.000107	0.307657
0.492519	-1.432241	0.360346	0.000078	0.307538
0.333737	-1.445081	0.365350	0.000108	0.307342
0.670329	-1.550682	0.370355	0.000045	0.307133
0.519997	-1.549016	0.375360	0.000073	0.307013
0.396445	-1.582593	0.380365	0.000096	0.306749
0.331468	-1.588603	0.385370	0.000108	0.306666
0.537873	-1.682455	0.390374	0.000069	0.306400
0.341064	-1.685962	0.395379	0.000106	0.306215
0.816015	-1.800572	0.400384	0.000017	0.306082
0.491377	-1.809547	0.405389	0.000078	0.305761
0.553775	-1.845021	0.410394	0.000066	0.305647
0.435987	-1.854311	0.415398	0.000088	0.305502
0.540056	-1.939446	0.420403	0.000069	0.305188
0.831016	-2.023863	0.425408	0.000014	0.305039
1.081138	-2.113868	0.430413	-0.000032	0.304828
0.691223	-2.108656	0.435418	0.000040	0.304517
0.697285	-2.145074	0.440422	0.000039	0.304350
0.323975	-2.114181	0.445427	0.000108	0.304174
0.562813	-2.217436	0.450432	0.000064	0.303890
0.752112	-2.300715	0.455437	0.000029	0.303657
0.712010	-2.334703	0.460442	0.000036	0.303461
0.824009	-2.400480	0.465446	0.000015	0.303245
0.490598	-2.399287	0.470451	0.000077	0.302962
-0.044829	-2.347237	0.475456	0.000177	0.302746
0.027726	-2.404760	0.480461	0.000163	0.302535
0.315193	-2.503838	0.485466	0.000110	0.302311
0.120824	-2.532763	0.490470	0.000146	0.302004
0.033874	-2.559510	0.495475	0.000162	0.301800
-0.119825	-2.572597	0.500480	0.000190	0.301604
0.014266	-2.649766	0.505485	0.000165	0.301351
-0.859700	-2.553577	0.510490	0.000328	0.301050
-3.053166	-2.185582	0.515494	0.000736	0.300904
-3.706973	-2.102795	0.520499	0.000858	0.300731
-3.186971	-2.233314	0.525504	0.000761	0.300558
-3.765768	-2.142476	0.530509	0.000869	0.300489
-4.118578	-2.146944	0.535514	0.000934	0.300159
-4.207369	-2.145618	0.540518	0.000951	0.300088
-4.980729	-2.054256	0.545523	0.001095	0.299851
-4.610281	-2.143430	0.550528	0.001025	0.299746
-5.467001	-2.032511	0.555533	0.001185	0.299530
-5.626866	-2.020393	0.560538	0.001215	0.299449
-6.030924	-1.984502	0.565542	0.001290	0.299268
-6.242838	-1.961368	0.570547	0.001329	0.299194
-6.084586	-2.047894	0.575552	0.001300	0.298915
-6.318268	-2.012273	0.580557	0.001343	0.298882
-6.828396	-1.974935	0.585562	0.001438	0.298614
-6.706589	-1.996707	0.590566	0.001415	0.298616
-6.812006	-2.046650	0.595571	0.001435	0.298282
-6.217265	-2.156954	0.600576	0.001324	0.298271
-6.830760	-2.102137	0.605581	0.001438	0.297997
-6.808328	-2.109482	0.610586	0.001434	0.297981
-7.121787	-2.114523	0.615590	0.001492	0.297680
-7.352737	-2.081260	0.620595	0.001535	0.297638
-7.583559	-2.088178	0.625600	0.001578	0.297401
-8.200146	-1.986317	0.630605	0.001693	0.297352
-8.190278	-2.028742	0.635610	0.001691	0.297155
-8.244029	-2.047975	0.640614	0.001701	0.297014
-8.218250	-2.077845	0.645619	0.001696	0.296891
-8.344067	-2.089100	0.650624	0.001719	0.296725
-8.733846	-2.031058	0.655629	0.001791	0.296663
-9.019636	-2.035265	0.660634	0.001845	0.296390
-8.207462	-2.186538	0.665638	0.001693	0.296372
-9.010587	-2.101758	0.670643	0.001843	0.296074
-9.002566	-2.103017	0.675648	0.001841	0.296075
-9.558618	-2.054775	0.680653	0.001945	0.295817
-9.345122	-2.104937	0.685658	0.001905	0.295762
-9.574685	-2.089913	0.690662	0.001948	0.295632
-10.087053	-2.022368	0.695667	0.002043	0.295507
-9.764837	-2.094358	0.700672	0.001983	0.295442
-10.505464	-2.013774	0.705677	0.002121	0.295177
-10.473739	-2.020943	0.710682	0.002115	0.295171
-10.190936	-2.129225	0.715686	0.002062	0.294892
-10.073574	-2.160932	0.720691	0.002040	0.294842
-10.052165	-2.211126	0.725696	0.002036	0.294615
-10.755164	-2.104444	0.730701	0.002167	0.294512
-10.411445	-2.195326	0.735706	0.002103	0.294372
-11.040989	-2.109627	0.740710	0.002220	0.294232
-11.230722	-2.087710	0.745715	0.002255	0.294170
-10.709443	-2.240534	0.750720	0.002158	0.293885
-11.019822	-2.188067	0.755725	0.002216	0.293866
-11.345606	-2.189551	0.760730	0.002276	0.293567
-11.095027	-2.234126	0.765734	0.002229	0.293572
-11.381684	-2.237252	0.770739	0.002283	0.293300
-11.863983	-2.158485	0.775744	0.002372	0.293257
-12.213533	-2.128911	0.780749	0.002437	0.293089
-12.196439	-2.157043	0.785754	0.002434	0.292966
-12.164876	-2.177780	0.790758	0.002428	0.292893
-12.819989	-2.113016	0.795763	0.002550	0.292625
-12.672075	-2.136637	0.800768	0.002522	0.292641
-12.798522	-2.170236	0.805773	0.002546	0.292362
-13.364856	-2.075205	0.810778	0.002651	0.292323
-13.301183	-2.110331	0.815782	0.002639	0.292207
-13.592911	-2.100113	0.820787	0.002694	0.291995
-13.228929	-2.166069	0.825792	0.002626	0.291996
-13.637991	-2.150734	0.830797	0.002702	0.291704
-13.751574	-2.130165	0.835802	0.002723	0.291704
-13.363803	-2.239600	0.840806	0.002651	0.291511
-14.084373	-2.139152	0.845811	0.002785	0.291360
-13.775891	-2.205506	0.850816	0.002727	0.291309
-14.112302	-2.196605	0.855821	0.002790	0.291050
-14.520947	-2.120950	0.860826	0.002866	0.291057
-14.357615	-2.200839	0.865830	0.002835	0.290808
-14.591586	-2.174505	0.870835	0.002879	0.290728
-14.386327	-2.231056	0.875840	0.002840	0.290632
-14.752305	-2.197348	0.880845	0.002909	0.290469
-14.561047	-2.235980	0.885850	0.002873	0.290450
-14.871000	-2.243226	0.890854	0.002930	0.290134
-15.530081	-2.122616	0.895859	0.003053	0.290138
-15.463408	-2.172665	0.900864	0.003041	0.289949
-15.607570	-2.172886	0.905869	0.003067	0.289818
-15.686383	-2.170483	0.910874	0.003082	0.289759
-15.884486	-2.187905	0.915878	0.003119	0.289492
-15.900565	-2.185992	0.920883	0.003122	0.289487
-15.938503	-2.217067	0.925888	0.003129	0.289298
-16.640647	-2.107832	0.930893	0.003259	0.289206
-16.190935	-2.204695	0.935898	0.003175	0.289131
-16.572606	-2.187683	0.940902	0.003246	0.288869
-16.896337	-2.130202	0.945907	0.003307	0.288863
-16.801206	-2.185638	0.950912	0.003289	0.288672
-17.073906	-2.159014	0.955917	0.003340	0.288557
-17.339286	-2.116807	0.960922	0.003389	0.288527
-17.608840	-2.124534	0.965926	0.003439	0.288243
-17.774268	-2.094818	0.970931	0.003470	0.288242
-17.610895	-2.149208	0.975936	0.003439	0.288118
-18.293943	-2.056190	0.980941	0.003566	0.287962
-18.040146	-2.103148	0.985946	0.003519	0.287958
-18.095431	-2.138579	0.990950	0.003529	0.287730
-18.945942	-2.005217	0.995955	0.003687	0.287623
-18.879615	-2.012544	1.000960	0.003675	0.287648
-18.764378	-2.090425	1.005965	0.003653	0.287361
-19.610238	-1.942182	1.010970	0.003811	0.287334
-18.781537	-2.097993	1.015974	0.003656	0.287308
-19.008817	-2.121598	1.020979	0.003699	0.286982
-19.014676	-2.118753	1.025984	0.003700	0.286991
-19.431014	-2.062343	1.030989	0.003777	0.286894
-19.739534	-2.043029	1.035994	0.003834	0.286709
-19.333149	-2.117025	1.040998	0.003759	0.286709
-19.547311	-2.119689	1.046003	0.003799	0.286499
-20.102162	-2.043978	1.051008	0.003902	0.286372
-20.089154	-2.045787	1.056013	0.003899	0.286376
-19.912541	-2.127423	1.061018	0.003866	0.286126
-20.288095	-2.072838	1.066022	0.003936	0.286057
-20.175045	-2.100139	1.071027	0.003915	0.286023
-19.933116	-2.201425	1.076032	0.003870	0.285733
-20.687253	-2.063353	1.081037	0.004010	0.285739
-20.599394	-2.099916	1.086042	0.003994	0.285635
-20.582444	-2.131628	1.091046	0.003991	0.285490
-21.177941	-2.024106	1.096051	0.004101	0.285487
-21.497496	-2.011017	1.101056	0.004161	0.285259
-21.876738	-1.961696	1.106061	0.004231	0.285160
-21.597769	-2.013011	1.111066	0.004179	0.285157
-21.287613	-2.116138	1.116070	0.004121	0.284920
-21.743614	-2.052619	1.121075	0.004206	0.284822
-21.546673	-2.086705	1.126080	0.004169	0.284831
-22.018392	-2.066686	1.131085	0.004257	0.284497
-22.057446	-2.059521	1.136090	0.004264	0.284498
-21.788756	-2.121357	1.141094	0.004214	0.284432
-22.014828	-2.124927	1.146099	0.004256	0.284205
-22.404978	-2.050833	1.151104	0.004329	0.284222
-22.387965	-2.091053	1.156109	0.004326	0.284033
-22.430138	-2.115517	1.161114	0.004333	0.283870
-22.660576	-2.071321	1.166118	0.004376	0.283882
-23.053187	-2.053643	1.171123	0.004449	0.283608
-22.962641	-2.075416	1.176128	0.004432	0.283582
-23.412047	-1.997061	1.181133	0.004516	0.283565
-23.652870	-2.013357	1.186138	0.004561	0.283258
-23.122544	-2.110681	1.191142	0.004462	0.283254
-23.405933	-2.076402	1.196147	0.004515	0.283167
-23.422972	-2.114828	1.201152	0.004518	0.282955
-23.714995	-2.061318	1.206157	0.004572	0.282957
-23.469987	-2.145902	1.211162	0.004526	0.282753
-24.147144	-2.048113	1.216166	0.004652	0.282623
-23.899430	-2.097283	1.221171	0.004606	0.282603
-23.645402	-2.195470	1.226176	0.004559	0.282337
-24.227808	-2.096831	1.231181	0.004667	0.282300
-24.488161	-2.066726	1.236186	0.004715	0.282212
-24.248686	-2.155631	1.241190	0.004671	0.281980
-24.236734	-2.160778	1.246195	0.004668	0.281965
-24.618859	-2.128320	1.251200	0.004739	0.281775
-25.021384	-2.073786	1.256205	0.004814	0.281680
-24.867923	-2.101110	1.261210	0.004786	0.281683
-24.994507	-2.142307	1.266214	0.004809	0.281353
-25.688546	-2.015136	1.271219	0.004938	0.281359
-25.451066	-2.071142	1.276224	0.004894	0.281293
-25.811970	-2.051671	1.281229	0.004961	0.281056
-25.951787	-2.026439	1.286234	0.004987	0.281055
-25.486787	-2.140415	1.291238	0.004900	0.280904
-25.747849	-2.128462	1.296243	0.004949	0.280721
-25.634887	-2.147572	1.301248	0.004928	0.280729
-26.150020	-2.094856	1.306253	0.005024	0.280518
-25.713546	-2.179930	1.311258	0.004942	0.280489
-25.667952	-2.212332	1.316262	0.004934	0.280365
-26.635017	-2.079738	1.321267	0.005114	0.280142
-26.188641	-2.159002	1.326272	0.005031	0.280153
-26.539687	-2.143646	1.331277	0.005096	0.279902
-26.766908	-2.116579	1.336282	0.005138	0.279829
-26.819994	-2.114121	1.341286	0.005148	0.279792
-27.503913	-2.041595	1.346291	0.005275	0.279524
-27.347901	-2.070131	1.351296	0.005246	0.279524
-27.652939	-2.035159	1.356301	0.005303	0.279418
-27.658982	-2.069344	1.361306	0.005304	0.279236
-27.609399	-2.077617	1.366310	0.005294	0.279240
-27.829909	-2.081699	1.371315	0.005335	0.279011
-28.399939	-1.997624	1.376320	0.005441	0.278910
-27.843666	-2.103382	1.381325	0.005338	0.278887
-28.264311	-2.077765	1.386330	0.005416	0.278623
-28.462460	-2.048462	1.391334	0.005453	0.278588
-27.940053	-2.158742	1.396339	0.005355	0.278509
-28.106464	-2.177621	1.401344	0.005386	0.278254
-28.612909	-2.086270	1.406349	0.005481	0.278251
-28.434160	-2.151181	1.411354	0.005447	0.278083
-28.587643	-2.145444	1.416358	0.005476	0.277968
-29.091187	-2.056129	1.421363	0.005569	0.277956
-29.347660	-2.069799	1.426368	0.005617	0.277642
-29.350720	-2.071240	1.431373	0.005618	0.277632
-29.245984	-2.107154	1.436378	0.005598	0.277545
-29.722919	-2.063865	1.441382	0.005687	0.277319
-29.664183	-2.076761	1.446387	0.005676	0.277308
-29.703298	-2.101061	1.451392	0.005683	0.277144
-30.490683	-1.986725	1.456397	0.005829	0.276994
-29.827506	-2.108007	1.461402	0.005706	0.276990
-29.665790	-2.181009	1.466406	0.005676	0.276763
-30.341426	-2.072363	1.471411	0.005801	0.276689
-29.976935	-2.150781	1.476416	0.005733	0.276626
-30.371028	-2.128981	1.481421	0.005807	0.276365
-30.614602	-2.085674	1.486426	0.005852	0.276360
-30.693593	-2.101556	1.491430	0.005867	0.276202
-30.948458	-2.082626	1.496435	0.005914	0.276059
-30.888516	-2.091970	1.501440	0.005903	0.276068
-31.091384	-2.110422	1.506445	0.005940	0.275778
-31.182883	-2.100553	1.511450	0.005957	0.275743
-31.166612	-2.112382	1.516454	0.005954	0.275696
-31.767101	-2.040132	1.521459	0.006066	0.275503
-31.743613	-2.042331	1.526464	0.006061	0.275514
-31.304684	-2.159123	1.531469	0.005980	0.275320
-31.899454	-2.081595	1.536474	0.006090	0.275159
-31.802029	-2.098425	1.541478	0.006072	0.275165
-32.405279	-2.043919	1.546483	0.006184	0.274874
-32.317578	-2.063179	1.551488	0.006168	0.274857
-32.610368	-2.019167	1.556493	0.006222	0.274809
-32.704277	-2.056205	1.561498	0.006240	0.274524
-32.481221	-2.096521	1.566502	0.006198	0.274526
-33.325350	-1.964006	1.571507	0.006355	0.274416
-33.062543	-2.045820	1.576512	0.006306	0.274237
-33.158991	-2.029263	1.581517	0.006324	0.274232
-32.662828	-2.162040	1.586522	0.006232	0.274008
-33.455433	-2.038384	1.591526	0.006379	0.273900
-33.154062	-2.095893	1.596531	0.006323	0.273886
-33.191133	-2.144564	1.601536	0.006330	0.273593
-33.885213	-2.020553	1.606541	0.006459	0.273582
-33.713087	-2.073815	1.611546	0.006427	0.273466
-33.726719	-2.108638	1.616550	0.006429	0.273269
-33.734071	-2.111503	1.621555	0.006431	0.273247
-34.205372	-2.061190	1.626560	0.006518	0.273060
-34.122327	-2.093649	1.631565	0.006503	0.272968
-34.109720	-2.102868	1.636570	0.006500	0.272932
-34.619427	-2.065785	1.641574	0.006595	0.272637
-34.483950	-2.093437	1.646579	0.006570	0.272622
-34.482763	-2.116464	1.651584	0.006569	0.272501
-35.105251	-2.038890	1.656589	0.006685	0.272312
-35.309975	-1.998655	1.661594	0.006723	0.272328
-34.826651	-2.128961	1.666598	0.006633	0.272103
-35.138729	-2.094173	1.671603	0.006691	0.271987
-34.885801	-2.147397	1.676608	0.006644	0.271949
-35.311031	-2.118093	1.681613	0.006723	0.271693
-35.186909	-2.140543	1.686618	0.006700	0.271694
-35.507444	-2.116793	1.691622	0.006760	0.271511
-35.828156	-2.085414	1.696627	0.006819	0.271367
-35.613466	-2.123155	1.701632	0.006779	0.271375
-36.444159	-2.028788	1.706637	0.006934	0.271072
-36.835616	-1.955449	1.711642	0.007006	0.271084
-36.503830	-2.023862	1.716646	0.006945	0.271042
-36.870229	-2.012038	1.721651	0.007013	0.270749
-36.637955	-2.051134	1.726656	0.006970	0.270766
-36.783226	-2.045162	1.731661	0.006996	0.270657
-36.532379	-2.121225	1.736666	0.006950	0.270495
-36.785449	-2.072421	1.741670	0.006997	0.270510
-37.404689	-2.013519	1.746675	0.007112	0.270223
-36.950391	-2.108879	1.751680	0.007027	0.270155
-37.387079	-2.037480	1.756685	0.007108	0.270113
-37.736038	-2.024961	1.761690	0.007173	0.269840
-37.716549	-2.026340	1.766694	0.007170	0.269852
-38.033169	-1.992673	1.771699	0.007229	0.269724
-38.056932	-2.027889	1.776704	0.007233	0.269512
-37.819420	-2.071989	1.781709	0.007189	0.269508
-37.818009	-2.110298	1.786714	0.007188	0.269303
-38.205699	-2.053926	1.791718	0.007260	0.269228
-38.380845	-2.026885	1.796723	0.007293	0.269202
-38.618849	-2.038566	1.801728	0.007337	0.268907
-38.723453	-2.021379	1.806733	0.007356	0.268898
-38.612992	-2.065145	1.811738	0.007336	0.268770
-38.795811	-2.066811	1.816742	0.007370	0.268583
-38.789474	-2.069710	1.821747	0.007369	0.268574
-39.219694	-2.031219	1.826752	0.007449	0.268360
-39.643676	-1.970790	1.831757	0.007527	0.268270
-39.252755	-2.042712	1.836762	0.007455	0.268266
-39.049251	-2.135046	1.841766	0.007417	0.267968
-40.039505	-1.954406	1.846771	0.007601	0.267971
-39.612249	-2.053781	1.851776	0.007521	0.267854
-40.268490	-1.973750	1.856781	0.007643	0.267642
-40.216413	-1.983285	1.861786	0.007634	0.267642
-40.192361	-2.019496	1.866790	0.007629	0.267470
-40.700815	-1.954821	1.871795	0.007724	0.267320
-40.783422	-1.937150	1.876800	0.007739	0.267335
-40.704338	-1.996184	1.881805	0.007724	0.267093
-40.657780	-2.023380	1.886810	0.007715	0.266992
-40.704507	-2.015477	1.891814	0.007724	0.266990
-40.826526	-2.047147	1.896819	0.007747	0.266698
-40.460516	-2.112430	1.901824	0.007678	0.266705
-40.924573	-2.056557	1.906829	0.007765	0.266551
-41.377497	-2.007692	1.911834	0.007849	0.266369
-41.668882	-1.949549	1.916838	0.007903	0.266397
-41.370844	-2.050251	1.921843	0.007848	0.266145
-41.232257	-2.090994	1.926848	0.007822	0.266061
-41.482373	-2.057201	1.931853	0.007868	0.265998
-41.390392	-2.122050	1.936858	0.007851	0.265736
-41.306733	-2.137388	1.941862	0.007835	0.265736
-42.182119	-2.011771	1.946867	0.007998	0.265553
-41.685990	-2.115802	1.951872	0.007906	0.265478
-41.727325	-2.123183	1.956877	0.007913	0.265397
-42.206310	-2.085569	1.961882	0.008002	0.265127
-42.035045	-2.115481	1.966886	0.007971	0.265135
-42.318526	-2.109235	1.971891	0.008023	0.264887
-42.677102	-2.055140	1.976896	0.008090	0.264827
-43.084629	-1.992063	1.981901	0.008166	0.264767
-43.095324	-2.040816	1.986906	0.008168	0.264490
-42.778058	-2.098127	1.991910	0.008108	0.264493
-43.191498	-2.055639	1.996915	0.008185	0.264314
-43.282328	-2.057474	2.001920	0.008202	0.264214

-44.007879	-1.982742	2.011917	0.008337	0.263901
-44.456627	-1.912972	2.021914	0.008420	0.263836
-44.468758	-1.959413	2.031910	0.008422	0.263570
-44.296750	-1.997922	2.041907	0.008390	0.263531
-44.304032	-2.049068	2.051904	0.008392	0.263244
-44.953664	-1.928507	2.061901	0.008512	0.263258
-44.682439	-2.004710	2.071898	0.008462	0.263111
-45.252548	-1.927913	2.081894	0.008568	0.262964
-45.421952	-1.895684	2.091891	0.008599	0.262972
-45.039194	-1.966846	2.101888	0.008528	0.262965
-45.028898	-1.968025	2.111885	0.008525	0.262969
-44.561684	-2.071654	2.121882	0.008438	0.262868
-45.462604	-1.953346	2.131878	0.008606	0.262617
-45.006842	-2.037879	2.141875	0.008521	0.262609
-45.289367	-1.984333	2.151872	0.008573	0.262622
-45.313177	-1.980535	2.161869	0.008578	0.262620
-45.185348	-2.000801	2.171866	0.008554	0.262637
-44.775421	-2.019245	2.181862	0.008477	0.262948
-44.694807	-2.032805	2.191859	0.008462	0.262955
-44.799334	-2.013448	2.201856	0.008481	0.262957
-45.172265	-1.943738	2.211853	0.008550	0.262968
-44.712903	-2.030186	2.221850	0.008465	0.262953
-44.721177	-2.030127	2.231846	0.008466	0.262946
-44.795956	-2.007203	2.241843	0.008480	0.262999
-44.822470	-1.956111	2.251840	0.008485	0.263254
-44.993687	-1.923163	2.261837	0.008516	0.263265
-44.575558	-2.002987	2.271834	0.008438	0.263245
-44.733541	-1.919350	2.281830	0.008468	0.263548
-44.689431	-1.920951	2.291827	0.008459	0.263584
-44.283310	-1.979816	2.301824	0.008383	0.263667
-43.762560	-2.035928	2.311821	0.008286	0.263880
-44.165104	-1.961266	2.321818	0.008361	0.263889
-44.001890	-1.947529	2.331814	0.008331	0.264128
-43.473822	-2.027465	2.341811	0.008232	0.264217
-43.631690	-1.982553	2.351808	0.008261	0.264307
-43.654687	-1.939188	2.361805	0.008265	0.264523
-43.770523	-1.898494	2.371802	0.008287	0.264631
-43.346646	-1.935982	2.381798	0.008208	0.264848
-42.922958	-1.994626	2.391795	0.008129	0.264950
-42.386012	-2.057501	2.401792	0.008029	0.265141
-42.696818	-1.978886	2.411789	0.008086	0.265263
-42.273520	-2.013822	2.421786	0.008007	0.265493
-42.578765	-1.938875	2.431782	0.008064	0.265600
-42.188088	-1.981234	2.441779	0.007991	0.265757
-42.234746	-1.934189	2.451776	0.008000	0.265968
-41.808541	-1.992512	2.461773	0.007920	0.266073
-41.884521	-1.924366	2.471770	0.007934	0.266370
-41.635024	-1.947872	2.481766	0.007887	0.266490
-41.190512	-1.986483	2.491763	0.007804	0.266720
-40.867293	-2.016667	2.501760	0.007744	0.266876
-40.969130	-1.975321	2.511757	0.007763	0.267001
-40.547948	-1.994250	2.521754	0.007684	0.267314
-40.438108	-1.995579	2.531750	0.007664	0.267416
-40.036014	-2.030158	2.541747	0.007589	0.267626
-39.804140	-2.026829	2.551744	0.007545	0.267873
-39.912939	-1.980579	2.561741	0.007565	0.268017
-39.181117	-2.071359	2.571738	0.007429	0.268246
-38.872437	-2.101574	2.581734	0.007371	0.268387
-38.679163	-2.103932	2.591731	0.007335	0.268565
-38.535773	-2.086392	2.601728	0.007308	0.268801
-38.173679	-2.133437	2.611725	0.007241	0.268903
-37.927335	-2.121437	2.621722	0.007195	0.269209
-38.088272	-2.067297	2.631718	0.007225	0.269344
-37.830911	-2.085189	2.641715	0.007176	0.269500
-37.676786	-2.058356	2.651712	0.007148	0.269796
-37.340529	-2.092490	2.661709	0.007085	0.269942
-37.524050	-2.019796	2.671706	0.007119	0.270153
-37.203782	-2.019901	2.681702	0.007059	0.270466
-37.271495	-1.979391	2.691699	0.007071	0.270617
-37.187017	-1.957815	2.701696	0.007056	0.270816
-36.985325	-1.942381	2.711693	0.007018	0.271095
-36.707096	-1.947524	2.721690	0.006966	0.271339
-36.244929	-1.992246	2.731686	0.006880	0.271549
-36.066036	-1.987346	2.741683	0.006846	0.271750
-35.835600	-1.979637	2.751680	0.006803	0.272015
-35.399575	-2.012546	2.761677	0.006722	0.272263
-34.834838	-2.084258	2.771674	0.006616	0.272428
-34.735459	-2.064476	2.781670	0.006598	0.272630
-34.673591	-2.017052	2.791667	0.006586	0.272942
-34.525988	-2.007796	2.801664	0.006558	0.273135
-33.937575	-2.081985	2.811661	0.006449	0.273310
-34.024447	-2.012566	2.821658	0.006465	0.273594
-33.584195	-2.049933	2.831654	0.006383	0.273821
-33.478282	-2.032859	2.841651	0.006363	0.274014
-32.858786	-2.106512	2.851648	0.006247	0.274221
-32.689204	-2.087096	2.861645	0.006215	0.274487
-32.305837	-2.124110	2.871642	0.006144	0.274660
-32.127060	-2.123637	2.881638	0.006110	0.274835
-31.809975	-2.123089	2.891635	0.006051	0.275142
-31.810031	-2.085826	2.901632	0.006051	0.275339
-31.497252	-2.108627	2.911629	0.005993	0.275519
-31.199631	-2.121315	2.921626	0.005937	0.275737
-31.197737	-2.079059	2.931622	0.005937	0.275962
-31.101481	-2.061081	2.941619	0.005918	0.276149
-30.369456	-2.155402	2.951616	0.005782	0.276353
-30.179415	-2.133407	2.961613	0.005747	0.276650
-30.029382	-2.128939	2.971610	0.005718	0.276817
-29.920617	-2.113565	2.981606	0.005698	0.277001
-30.071919	-2.026086	2.991603	0.005726	0.277316
-29.570097	-2.070223	3.001600	0.005632	0.277562
-29.650297	-2.012559	3.011597	0.005647	0.277788
-29.055048	-2.079967	3.021594	0.005536	0.278001
-29.036182	-2.033820	3.031590	0.005532	0.278260
-28.460742	-2.090698	3.041587	0.005425	0.278509
-28.516572	-2.038901	3.051584	0.005435	0.278727
-28.622519	-1.971770	3.061581	0.005455	0.278976
-27.880313	-2.057599	3.071578	0.005317	0.279232
-27.767329	-2.030061	3.081574	0.005295	0.279482
-27.272350	-2.077092	3.091571	0.005203	0.279705
-27.277408	-2.032843	3.101568	0.005204	0.279930
-26.809839	-2.074857	3.111565	0.005117	0.280153
-26.421618	-2.084177	3.121562	0.005044	0.280470
-26.375613	-2.063230	3.131558	0.005035	0.280622
-26.271685	-2.046947	3.141555	0.005016	0.280805
-25.792783	-2.087417	3.151552	0.004927	0.281046
-25.364579	-2.111444	3.161549	0.004847	0.281324
-25.523001	-2.039380	3.171546	0.004876	0.281547
-25.106886	-2.075807	3.181542	0.004798	0.281749
-24.716538	-2.104529	3.191539	0.004725	0.281967
-24.224409	-2.139268	3.201536	0.004634	0.282249
-24.206174	-2.106042	3.211533	0.004630	0.282437
-23.947728	-2.113743	3.221530	0.004582	0.282639
-23.823399	-2.076461	3.231526	0.004559	0.282947
-23.398910	-2.110806	3.241523	0.004479	0.283166
-23.390810	-2.074753	3.251520	0.004478	0.283359
-23.179535	-2.069475	3.261517	0.004438	0.283583
-22.599281	-2.118965	3.271514	0.004330	0.283869
-22.893621	-2.019399	3.281510	0.004385	0.284105
-22.229791	-2.099174	3.291507	0.004261	0.284314
-22.272168	-2.052070	3.301504	0.004268	0.284516
-21.541997	-2.126214	3.311501	0.004132	0.284814
-21.324382	-2.124396	3.321498	0.004092	0.285025
-21.237151	-2.102319	3.331494	0.004075	0.285219
-20.725792	-2.146960	3.341491	0.003980	0.285465
-20.537374	-2.138920	3.351488	0.003945	0.285680
-20.325836	-2.141924	3.361485	0.003905	0.285860
-20.352006	-2.094252	3.371482	0.003910	0.286078
-19.984255	-2.106722	3.381478	0.003841	0.286354
-19.591451	-2.130801	3.391475	0.003768	0.286594
-19.774515	-2.056705	3.401472	0.003802	0.286801
-18.999460	-2.163160	3.411469	0.003657	0.286976
-18.868428	-2.124130	3.421466	0.003633	0.287293
-18.586055	-2.138605	3.431462	0.003580	0.287480
-18.385416	-2.135458	3.441459	0.003543	0.287680
-18.287965	-2.098187	3.451456	0.003524	0.287957
-17.736896	-2.148871	3.461453	0.003421	0.288207
-17.946379	-2.069936	3.471450	0.003460	0.288413
-17.400190	-2.131873	3.481446	0.003358	0.288601
-17.249156	-2.104207	3.491443	0.003330	0.288878
-16.948667	-2.108006	3.501440	0.003274	0.289133
-16.507495	-2.150724	3.511437	0.003192	0.289322
-16.472247	-2.121739	3.521434	0.003185	0.289499
-16.048892	-2.133720	3.531430	0.003106	0.289825
-15.867065	-2.127772	3.541427	0.003072	0.290020
-15.644141	-2.130490	3.551424	0.003030	0.290210
-15.315436	-2.134524	3.561421	0.002969	0.290488
-15.262427	-2.102278	3.571418	0.002959	0.290698
-15.045230	-2.101713	3.581414	0.002918	0.290898
-14.969545	-2.071969	3.591411	0.002904	0.291115
-14.531932	-2.102244	3.601408	0.002822	0.291361
-14.017821	-2.140527	3.611405	0.002726	0.291635
-13.957181	-2.113236	3.621402	0.002715	0.291826
-13.726052	-2.119086	3.631398	0.002672	0.292006
-14.110894	-1.984387	3.641395	0.002743	0.292328
-13.104501	-2.118729	3.651392	0.002556	0.292569
-13.112048	-2.072642	3.661389	0.002557	0.292791
-12.644903	-2.117173	3.671386	0.002470	0.292991
-12.403590	-2.107094	3.681382	0.002425	0.293258
-12.079489	-2.122194	3.691379	0.002364	0.293475
-11.971946	-2.102362	3.701376	0.002344	0.293670
-11.589436	-2.129095	3.711373	0.002273	0.293882
-11.100283	-2.154596	3.721370	0.002181	0.294194
-11.070698	-2.125543	3.731366	0.002176	0.294365
-10.986810	-2.103017	3.741363	0.002160	0.294551
-10.510761	-2.132032	3.751360	0.002071	0.294834
-10.234471	-2.135153	3.761357	0.002020	0.295066
-10.557968	-2.029786	3.771354	0.002080	0.295295
-9.919564	-2.100924	3.781350	0.001961	0.295516
-10.076722	-2.023579	3.791347	0.001990	0.295755
-9.631620	-2.053820	3.801344	0.001907	0.296004
-9.261245	-2.081314	3.811341	0.001837	0.296199
-9.094534	-2.068940	3.821338	0.001806	0.296409
-8.557648	-2.105044	3.831334	0.001706	0.296709
-8.677125	-2.040712	3.841331	0.001728	0.296918
-8.086010	-2.110896	3.851328	0.001618	0.297100
-7.784544	-2.122323	3.861325	0.001562	0.297312
-7.570641	-2.098859	3.871322	0.001522	0.297616
-7.027903	-2.157135	3.881318	0.001420	0.297813
-6.961081	-2.134107	3.891315	0.001408	0.297985
-6.828877	-2.103086	3.901312	0.001383	0.298253
-6.459123	-2.123669	3.911309	0.001314	0.298479
-6.850843	-2.007881	3.921306	0.001387	0.298696
-6.162596	-2.091886	3.931302	0.001258	0.298896
-5.977072	-2.056503	3.941299	0.001224	0.299231
-5.709305	-2.066429	3.951296	0.001174	0.299419
-5.767156	-2.009753	3.961293	0.001184	0.299643
-4.805143	-2.142697	3.971290	0.001005	0.299846
-5.177541	-2.012587	3.981286	0.001074	0.300148
-4.444471	-2.102776	3.991283	0.000938	0.300356
-4.185900	-2.113588	4.001280	0.000889	0.300531
-4.266248	-2.054839	4.011277	0.000904	0.300744
-4.159053	-2.020834	4.021274	0.000884	0.301002
-3.612133	-2.077986	4.031270	0.000782	0.301206
-3.510135	-2.056182	4.041267	0.000763	0.301400
-3.192707	-2.051839	4.051264	0.000703	0.301699
-3.198514	-2.005060	4.061261	0.000704	0.301919
-2.650480	-2.060891	4.071258	0.000602	0.302129
-2.776214	-1.990742	4.081254	0.000625	0.302356
-2.552925	-1.973224	4.091251	0.000584	0.302635
-2.598923	-1.903194	4.101248	0.000592	0.302930
-2.380538	-1.894442	4.111245	0.000551	0.303162
-1.868397	-1.939656	4.121242	0.000456	0.303391
-2.157727	-1.832385	4.131238	0.000509	0.303653
-1.733859	-1.858106	4.141235	0.000430	0.303898
-1.323782	-1.861255	4.151232	0.000354	0.304238
-1.262308	-1.824991	4.161229	0.000342	0.304464
-1.302661	-1.762995	4.171226	0.000349	0.304725
-1.340230	-1.695168	4.181222	0.000356	0.305015
-1.749074	-1.555783	4.191219	0.000432	0.305324
-1.331881	-1.567643	4.201216	0.000354	0.305628
-0.648507	-1.638314	4.211213	0.000227	0.305882
-0.446725	-1.614325	4.221210	0.000189	0.306169
-0.564369	-1.528197	4.231206	0.000211	0.306476
-0.790125	-1.418636	4.241203	0.000253	0.306800
-0.683885	-1.368555	4.251200	0.000233	0.307128
-0.662094	-1.299194	4.261197	0.000228	0.307474
-0.967872	-1.166545	4.271194	0.000285	0.307837
-0.664353	-1.147045	4.281190	0.000228	0.308188
-0.743330	-1.055901	4.291187	0.000243	0.308549
-0.322140	-1.047122	4.301184	0.000164	0.308950
-1.121803	-0.811963	4.311181	0.000313	0.309371
-0.565828	-0.835689	4.321178	0.000209	0.309733
-0.239869	-0.812214	4.331174	0.000148	0.310120
-0.380078	-0.687856	4.341171	0.000174	0.310582
-0.360670	-0.616832	4.351168	0.000170	0.310929
-0.770934	-0.446669	4.361165	0.000246	0.311375
-0.383998	-0.414822	4.371162	0.000174	0.311850
-0.587449	-0.291380	4.381158	0.000212	0.312251
-0.541891	-0.185888	4.391155	0.000203	0.312779
-0.008930	-0.193929	4.401152	0.000104	0.313190
-0.076609	-0.071394	4.411149	0.000116	0.313699
0.238713	-0.034648	4.421146	0.000057	0.314134
0.000000	0.111755	4.431142	0.000101	0.314608

-0.059263	0.402361	4.436147	0.000112	0.315893
0.416600	0.876820	4.441152	0.000023	0.318452
0.532047	1.716005	4.446157	0.000001	0.322336
0.813753	2.823327	4.451162	-0.000052	0.327494
1.736651	4.100645	4.456166	-0.000225	0.333816
2.085863	5.790081	4.461171	-0.000291	0.341327
3.237682	7.639843	4.466176	-0.000507	0.349944
5.823511	9.542720	4.471181	-0.000990	0.359616
8.612920	11.741464	4.476186	-0.001511	0.370335
10.601164	14.419196	4.481190	-0.001883	0.382016
14.079442	17.183795	4.486195	-0.002532	0.394660
16.264836	20.534864	4.491200	-0.002942	0.408159
18.103558	24.313553	4.496205	-0.003286	0.422475
19.437326	28.539471	4.501210	-0.003538	0.437498
20.834514	33.106161	4.506214	-0.003801	0.453146
21.812134	38.107136	4.511219	-0.003986	0.469377
22.323071	43.542145	4.516224	-0.004085	0.486105
23.784607	49.153380	4.521229	-0.004361	0.503276
25.973472	54.987829	4.526234	-0.004772	0.520863
27.069964	61.350272	4.531238	-0.004981	0.538764
28.738897	67.940829	4.536243	-0.005296	0.556948
29.629445	74.984126	4.541248	-0.005466	0.575341
31.770002	82.115005	4.546253	-0.005870	0.593924
34.082676	89.501982	4.551258	-0.006305	0.612618
35.442131	97.341470	4.556262	-0.006563	0.631402
36.211172	105.535576	4.561267	-0.006712	0.650195
37.577376	113.845836	4.566272	-0.006972	0.668942
39.348324	122.285651	4.571277	-0.007307	0.687600
41.229623	130.905651	4.576282	-0.007663	0.706172
42.806298	139.745652	4.581286	-0.007963	0.724598
44.019199	148.829868	4.586291	-0.008195	0.742914
44.963580	158.067567	4.591296	-0.008377	0.760990
46.032355	167.407075	4.596301	-0.008582	0.778874
47.761360	176.707571	4.601306	-0.008910	0.796498
48.933605	186.194815	4.606310	-0.009134	0.813896
50.053004	195.773031	4.611315	-0.009349	0.831070
50.592638	205.466394	4.616320	-0.009456	0.847917
51.763261	215.070853	4.621325	-0.009680	0.864473
52.448295	224.781138	4.626330	-0.009814	0.880750
53.265365	234.462492	4.631334	-0.009973	0.896722
54.348490	244.105168	4.636339	-0.010181	0.912427
55.771388	253.650214	4.641344	-0.010452	0.927806
57.081684	263.209095	4.646349	-0.010702	0.942923
57.658876	272.884670	4.651354	-0.010816	0.957784
58.474492	282.470645	4.656358	-0.010974	0.972347
58.628779	292.156838	4.661363	-0.011010	0.986671
59.371288	301.647557	4.666368	-0.011154	1.000656
60.834540	310.979800	4.671373	-0.011433	1.014401
62.256789	320.285773	4.676378	-0.011704	1.027914
62.506717	329.751793	4.681382	-0.011756	1.041191
63.936660	338.955313	4.686387	-0.012029	1.054221
65.061279	348.165109	4.691392	-0.012244	1.067027
65.322715	357.513309	4.696397	-0.012299	1.079667
66.400056	366.622839	4.701402	-0.012506	1.092031
67.768648	375.652394	4.706406	-0.012767	1.104217
68.371066	384.803229	4.711411	-0.012885	1.116255
68.983539	393.857919	4.716416	-0.013005	1.128044
69.628641	402.890427	4.721421	-0.013131	1.139689
70.207190	411.906784	4.726426	-0.013245	1.151182
70.992986	420.806027	4.731430	-0.013397	1.162459
72.029525	429.641580	4.736435	-0.013596	1.173602
73.055446	438.423438	4.741440	-0.013792	1.184572
73.199563	447.360794	4.746445	-0.013825	1.195447
74.031243	456.103453	4.751450	-0.013986	1.206131
74.622911	464.874815	4.756454	-0.014102	1.216706
75.831237	473.503218	4.761459	-0.014332	1.227145
75.959005	482.295145	4.766464	-0.014362	1.237472
76.041715	491.059643	4.771469	-0.014383	1.247672
76.512876	499.720959	4.776474	-0.014477	1.257748
77.194750	508.300042	4.781478	-0.014609	1.267689
77.255012	516.984964	4.786483	-0.014626	1.277554
78.470376	525.399281	4.791488	-0.014858	1.287259
79.523243	533.881408	4.796493	-0.015060	1.296935
80.463878	542.366562	4.801498	-0.015241	1.306521
81.042159	550.980653	4.806502	-0.015354	1.316112
81.480002	559.483054	4.811507	-0.015441	1.325486
81.658220	568.022558	4.816512	-0.015480	1.334787
82.328087	576.450455	4.821517	-0.015610	1.343992
82.905581	584.896227	4.826522	-0.015723	1.353137
83.256200	593.341290	4.831526	-0.015794	1.362179
83.802175	601.773047	4.836531	-0.015901	1.371181
84.559291	610.130941	4.841536	-0.016048	1.380084
85.189121	618.530703	4.846541	-0.016171	1.388952
85.215998	627.001066	4.851546	-0.016181	1.397732
85.756381	635.349735	4.856550	-0.016288	1.406420
86.693751	643.667821	4.861555	-0.016468	1.415090
87.321493	651.993882	4.866560	-0.016590	1.423663
87.988950	660.347060	4.871565	-0.016720	1.432219
88.125192	668.757329	4.876570	-0.016751	1.440692
88.514219	677.108479	4.881574	-0.016829	1.449099
89.341901	685.391407	4.886579	-0.016988	1.457461
90.218658	693.639119	4.891584	-0.017157	1.465749
90.509144	702.041824	4.896589	-0.017217	1.474047
91.025152	710.329977	4.901594	-0.017318	1.482222
91.492774	718.625045	4.906598	-0.017411	1.490352
91.970587	726.935103	4.911603	-0.017505	1.498453
92.585746	735.196195	4.916608	-0.017625	1.506486
92.737417	743.550933	4.921613	-0.017659	1.514492
93.409245	751.778024	4.926618	-0.017790	1.522416
93.960791	760.025135	4.931622	-0.017898	1.530299
94.506638	768.309809	4.936627	-0.018005	1.538176
94.901172	776.580863	4.941632	-0.018084	1.545976
95.520068	784.829761	4.946637	-0.018204	1.553751
95.924340	793.080779	4.951642	-0.018285	1.561456
96.128955	801.368954	4.956646	-0.018329	1.569128
97.283774	809.498782	4.961651	-0.018549	1.576758
97.237124	817.831123	4.966656	-0.018546	1.584359
97.275072	826.154538	4.971661	-0.018559	1.591928
97.632573	834.377600	4.976666	-0.018631	1.599416
98.357042	842.534556	4.981670	-0.018771	1.606864
98.200926	850.891877	4.986675	-0.018747	1.614329
99.162097	858.985421	4.991680	-0.018932	1.621685
100.370710	867.094102	4.996685	-0.019162	1.629056
101.160719	875.294690	5.001690	-0.019315	1.636415
101.585532	883.500144	5.006694	-0.019399	1.643694
102.387826	891.667557	5.011699	-0.019554	1.650960
102.537581	899.941015	5.016704	-0.019587	1.658196
102.883126	908.144320	5.021709	-0.019657	1.665366
103.401620	916.366021	5.026714	-0.019759	1.672546
103.755163	924.555927	5.031718	-0.019830	1.679644
104.300960	932.742727	5.036723	-0.019937	1.686736
104.443330	941.019045	5.041728	-0.019969	1.693820
104.905606	949.187179	5.046733	-0.020061	1.700825
105.616532	957.340225	5.051738	-0.020199	1.707822
106.049815	965.517175	5.056742	-0.020285	1.714774
106.290718	973.740825	5.061747	-0.020335	1.721711
106.952598	981.864469	5.066752	-0.020464	1.728592
107.440472	990.051026	5.071757	-0.020560	1.735475
108.165583	998.170568	5.076762	-0.020700	1.742305
108.347648	1006.408173	5.081766	-0.020740	1.749137
109.556989	1014.462277	5.086771	-0.020970	1.755923
109.810192	1022.663378	5.091776	-0.021023	1.762680
110.540440	1030.816108	5.096781	-0.021164	1.769433
110.980952	1039.027348	5.101786	-0.021252	1.776170
111.502780	1047.164958	5.106790	-0.021354	1.782833
112.818815	1055.237363	5.111795	-0.021604	1.789518
113.166126	1063.452509	5.116800	-0.021675	1.796171
113.548873	1071.621777	5.121805	-0.021751	1.802767
113.921264	1079.804768	5.126810	-0.021826	1.809349
114.541298	1087.934182	5.131814	-0.021947	1.815894
114.893999	1096.140254	5.136819	-0.022018	1.822444
115.332802	1104.278393	5.141824	-0.022105	1.828927
115.882379	1112.414258	5.146829	-0.022213	1.835399
116.200404	1120.579805	5.151834	-0.022277	1.841843
116.388325	1128.779708	5.156838	-0.022318	1.848276
116.968130	1136.905979	5.161843	-0.022431	1.854676
117.607871	1144.988841	5.166848	-0.022556	1.861027
118.265905	1153.111076	5.171853	-0.022684	1.867389
118.602557	1161.295055	5.176858	-0.022752	1.873739
118.680012	1169.476580	5.181862	-0.022771	1.880035
118.995621	1177.621279	5.186867	-0.022836	1.886309
119.441225	1185.739984	5.191872	-0.022924	1.892558
120.116779	1193.852971	5.196877	-0.023055	1.898809
121.016016	1201.898048	5.201882	-0.023228	1.905013
121.125395	1210.097670	5.206886	-0.023254	1.911223
121.123729	1218.313545	5.211891	-0.023259	1.917412
121.478840	1226.414671	5.216896	-0.023330	1.923536
122.249250	1234.470101	5.221901	-0.023479	1.929653
122.580343	1242.629319	5.226906	-0.023546	1.935778
123.294474	1250.693592	5.231910	-0.023684	1.941857
123.967241	1258.813002	5.236915	-0.023815	1.947952
124.271787	1266.948545	5.241920	-0.023877	1.953999
124.731079	1275.044930	5.246925	-0.023968	1.960016
124.986742	1283.175702	5.251930	-0.024021	1.966017
125.433399	1291.296934	5.256934	-0.024110	1.972014
126.026157	1299.419907	5.261939	-0.024225	1.978009
125.930177	1307.601932	5.266944	-0.024213	1.983954
126.033036	1315.770982	5.271949	-0.024237	1.989894
126.287732	1323.901058	5.276954	-0.024290	1.995804
126.745990	1331.959910	5.281958	-0.024381	2.001667
127.474278	1340.009999	5.286963	-0.024522	2.007536
128.028847	1348.085893	5.291968	-0.024630	2.013387
128.457152	1356.210623	5.296973	-0.024716	2.019242
128.733350	1364.350068	5.301978	-0.024772	2.025075
129.012125	1372.479428	5.306982	-0.024830	2.030884
129.349083	1380.610042	5.311987	-0.024898	2.036684
129.864779	1388.665429	5.316992	-0.024999	2.042432
130.183895	1396.781138	5.321997	-0.025064	2.048186
130.572543	1404.896368	5.327002	-0.025142	2.053931
131.429445	1412.896002	5.332006	-0.025307	2.059627
132.211076	1420.967780	5.337011	-0.025457	2.065350
132.277642	1429.154224	5.342016	-0.025475	2.071063
132.880868	1437.228090	5.347021	-0.025593	2.076737
133.307108	1445.329001	5.352026	-0.025678	2.082396
133.538433	1453.459748	5.357030	-0.025726	2.088041
133.764114	1461.608763	5.362035	-0.025773	2.093683
133.928576	1469.718404	5.367040	-0.025809	2.099276
134.313036	1477.821238	5.372045	-0.025886	2.104871
134.558425	1485.960899	5.377050	-0.025937	2.110463
135.177476	1494.008349	5.382054	-0.026058	2.116014
135.642400	1502.078622	5.387059	-0.026150	2.121551
136.075341	1510.143887	5.392064	-0.026236	2.127066
135.915513	1518.345407	5.397069	-0.026212	2.132602
136.609436	1526.367390	5.402074	-0.026346	2.138085
136.881047	1534.440257	5.407078	-0.026402	2.143547
137.310322	1542.542437	5.412083	-0.026487	2.149030
137.497485	1550.651916	5.417088	-0.026528	2.154481
137.966673	1558.705600	5.422093	-0.026620	2.159908
138.133058	1566.823535	5.427098	-0.026657	2.165334
138.439295	1574.906232	5.432102	-0.026719	2.170738
139.083830	1582.981709	5.437107	-0.026844	2.176154
139.010836	1591.115943	5.442112	-0.026836	2.181529
139.452685	1599.184748	5.447117	-0.026924	2.186895
140.140056	1607.248511	5.452122	-0.027057	2.192268
140.152244	1615.368325	5.457126	-0.027065	2.197601
140.555280	1623.422358	5.462131	-0.027145	2.202915
140.835226	1631.509050	5.467136	-0.027203	2.208226
141.053675	1639.632046	5.472141	-0.027249	2.213542
141.608109	1647.664058	5.477146	-0.027357	2.218816
141.711597	1655.765759	5.482150	-0.027382	2.224082
142.592164	1663.793167	5.487155	-0.027551	2.229359
142.471468	1671.944622	5.492160	-0.027534	2.234611
143.096922	1679.977567	5.497165	-0.027656	2.239843
143.766782	1688.014531	5.502170	-0.027786	2.245069
143.933831	1696.140945	5.507174	-0.027822	2.250295
144.712879	1704.183631	5.512179	-0.027973	2.255510
144.833350	1712.294450	5.517184	-0.028001	2.260697
145.288880	1720.369138	5.522189	-0.028091	2.265879
145.544612	1728.502796	5.527194	-0.028144	2.271069
145.512287	1736.634446	5.532198	-0.028143	2.276221
146.173042	1744.626660	5.537203	-0.028271	2.281333
146.750525	1752.645369	5.542208	-0.028384	2.286444
146.716671	1760.817051	5.547213	-0.028383	2.291585
147.378638	1768.829684	5.552218	-0.028512	2.296676
147.714495	1776.885441	5.557222	-0.028580	2.301755
148.549628	1784.899587	5.562227	-0.028741	2.306839
148.739872	1793.019868	5.567232	-0.028781	2.311922
149.077261	1801.094501	5.572237	-0.028850	2.316978
149.152276	1809.220805	5.577242	-0.028869	2.322033
149.562543	1817.255864	5.582246	-0.028951	2.327049
149.898758	1825.370237	5.587251	-0.029019	2.332097
149.772237	1833.494349	5.592256	-0.029000	2.337101
150.553591	1841.480559	5.597261	-0.029151	2.342086
150.715361	1849.599619	5.602266	-0.029187	2.347089
151.219214	1857.629394	5.607270	-0.029286	2.352056
151.560788	1865.713381	5.612275	-0.029355	2.357031
151.753092	1873.768952	5.617280	-0.029396	2.361967
151.986601	1881.855670	5.622285	-0.029445	2.366914
152.239794	1889.951417	5.627290	-0.029497	2.371858
152.469736	1898.013052	5.632294	-0.029545	2.376770
152.870150	1906.059992	5.637299	-0.029625	2.381676
153.019779	1914.137457	5.642304	-0.029658	2.386570
153.503314	1922.193905	5.647309	-0.029754	2.391468
153.794258	1930.274669	5.652314	-0.029813	2.396355
153.953197	1938.349275	5.657318	-0.029848	2.401218
154.218393	1946.432117	5.662323	-0.029903	2.406084
154.504144	1954.484615	5.667328	-0.029962	2.410924
155.027180	1962.520205	5.672333	-0.030064	2.415763
155.665723	1970.552388	5.677338	-0.030188	2.420600
155.928170	1978.601529	5.682342	-0.030243	2.425407
156.105237	1986.777454	5.687347	-0.030281	2.430273
156.236255	1994.865200	5.692352	-0.030311	2.435073
156.565291	2002.897522	5.697357	-0.030377	2.439846
156.886748	2010.924289	5.702362	-0.030443	2.444607
157.488124	2018.939176	5.707366	-0.030560	2.449372
157.789814	2027.029875	5.712371	-0.030621	2.454150
158.000703	2035.093639	5.717376	-0.030666	2.458895
158.515888	2043.122905	5.722381	-0.030767	2.463635
158.771647	2051.226435	5.727386	-0.030820	2.468389
159.314001	2059.236844	5.732390	-0.030926	2.473101
159.787806	2067.281007	5.737395	-0.031020	2.477818
159.830562	2075.383802	5.742400	-0.031033	2.482528
160.096852	2083.461210	5.747405	-0.031088	2.487231
160.556231	2091.525102	5.752410	-0.031179	2.491932
160.689938	2099.589349	5.757414	-0.031209	2.496599
160.933722	2107.667467	5.762419	-0.031260	2.501274
160.770788	2115.783304	5.767424	-0.031235	2.505932
161.305831	2123.805352	5.772429	-0.031340	2.510579
161.807931	2131.830527	5.777434	-0.031439	2.515217
161.887176	2139.900968	5.782438	-0.031459	2.519841
162.109889	2147.962562	5.787443	-0.031506	2.524461
162.316919	2156.043292	5.792448	-0.031550	2.529083
162.859876	2164.057245	5.797453	-0.031656	2.533683
163.216585	2172.113637	5.802458	-0.031728	2.538286
163.592671	2180.127831	5.807462	-0.031803	2.542857
164.169544	2188.167117	5.812467	-0.031916	2.547448
164.431464	2196.246931	5.817472	-0.031970	2.552032
164.752273	2204.309259	5.822477	-0.032035	2.556601
165.316279	2212.338534	5.827482	-0.032145	2.561162
165.463546	2220.405821	5.832486	-0.032178	2.565705
165.829789	2228.485280	5.837491	-0.032252	2.570263
166.127269	2236.547308	5.842496	-0.032312	2.574798
166.317697	2244.626138	5.847501	-0.032353	2.579327
166.646610	2252.682156	5.852506	-0.032420	2.583844
166.938635	2260.742280	5.857510	-0.032480	2.588354
167.364483	2268.887999	5.862515	-0.032564	2.592913
167.582766	2276.920214	5.867520	-0.032610	2.597386
167.860298	2284.944297	5.872525	-0.032667	2.601851
168.204326	2292.974552	5.877530	-0.032737	2.606316
168.590166	2300.997704	5.882534	-0.032814	2.610772
168.641468	2309.106189	5.887539	-0.032829	2.615245
168.985504	2317.111916	5.892544	-0.032898	2.619674
169.531478	2325.094532	5.897549	-0.033005	2.624096
169.561534	2333.210540	5.902554	-0.033016	2.628549
169.846192	2341.264697	5.907558	-0.033074	2.632977
169.935192	2349.370059	5.912563	-0.033096	2.637413
170.050427	2357.393670	5.917568	-0.033123	2.641798
170.620144	2365.378117	5.922573	-0.033234	2.646186
170.874867	2373.466841	5.927578	-0.033287	2.650602
171.332448	2381.490635	5.932582	-0.033378	2.654988
171.321537	2389.596986	5.937587	-0.033381	2.659381
171.994292	2397.551736	5.942592	-0.033512	2.663730
172.245487	2405.649214	5.947597	-0.033564	2.668121
172.533222	2413.703561	5.952602	-0.033623	2.672483
172.864894	2421.746135	5.957606	-0.033690	2.676835
172.865377	2429.841931	5.962611	-0.033695	2.681187
173.163144	2437.837148	5.967616	-0.033756	2.685497
173.658810	2445.881914	5.972621	-0.033853	2.689840
174.030962	2453.942166	5.977626	-0.033928	2.694176
174.730593	2461.934877	5.982630	-0.034064	2.698490
175.141783	2470.005683	5.987635	-0.034146	2.702820
175.713841	2477.995064	5.992640	-0.034257	2.707110
176.133615	2486.083486	5.997645	-0.034341	2.711436
176.579154	2494.141928	6.002650	-0.034429	2.715740
176.417053	2502.240675	6.007654	-0.034404	2.720020
177.265780	2510.192039	6.012659	-0.034568	2.724280
177.400221	2518.304891	6.017664	-0.034598	2.728573
177.614197	2526.396178	6.022669	-0.034643	2.732853
178.376120	2534.368779	6.027674	-0.034790	2.737099
178.570463	2542.436933	6.032678	-0.034832	2.741352
178.548932	2550.542317	6.037683	-0.034833	2.745604
178.462700	2558.663801	6.042688	-0.034823	2.749855
178.660583	2566.768184	6.047693	-0.034865	2.754107
179.098690	2574.731078	6.052698	-0.034952	2.758294
179.887645	2582.641357	6.057702	-0.035104	2.762469
180.575438	2590.674427	6.062707	-0.035237	2.766695
180.455289	2598.800661	6.067712	-0.035220	2.770913
180.986843	2606.801533	6.072717	-0.035324	2.775099
181.494261	2614.800766	6.077722	-0.035424	2.779277
181.463963	2622.903342	6.082726	-0.035424	2.783470
181.880515	2630.954169	6.087731	-0.035507	2.787656
182.251556	2638.991197	6.092736	-0.035581	2.791826
182.494057	2647.046407	6.097741	-0.035632	2.795991
182.754871	2655.116494	6.102746	-0.035686	2.800159
183.128054	2663.092000	6.107750	-0.035760	2.804279
183.557191	2671.173428	6.112755	-0.035846	2.808450
183.589486	2679.248599	6.117760	-0.035857	2.812588
183.732897	2687.320961	6.122765	-0.035889	2.816726
184.168680	2695.334091	6.127770	-0.035976	2.820844
184.740877	2703.309709	6.132774	-0.036087	2.824945
184.700262	2711.459422	6.137779	-0.036085	2.829093
184.939702	2719.491102	6.142784	-0.036135	2.833191
185.425415	2727.490213	6.147789	-0.036231	2.837280
185.362613	2735.594352	6.152794	-0.036224	2.841385
185.463830	2743.611148	6.157798	-0.036249	2.845450
186.001759	2751.598125	6.162803	-0.036354	2.849519
186.176480	2759.673613	6.167808	-0.036392	2.853606
186.529722	2767.717482	6.172813	-0.036463	2.857681
186.981368	2775.719002	6.177818	-0.036552	2.861734
187.283611	2783.749113	6.182822	-0.036614	2.865788
187.462726	2791.863876	6.187827	-0.036653	2.869871
187.775535	2799.861709	6.192832	-0.036716	2.873898
187.953106	2807.923688	6.197837	-0.036755	2.877943
188.545464	2815.921523	6.202842	-0.036870	2.881974
189.050172	2823.923867	6.207846	-0.036970	2.885996
189.449470	2832.001551	6.212851	-0.037049	2.890044
189.639089	2840.053453	6.217856	-0.037090	2.894062
190.011040	2848.096210	6.222861	-0.037164	2.898080
190.195999	2856.165607	6.227866	-0.037204	2.902096
190.538243	2864.200347	6.232870	-0.037273	2.906097
190.530704	2872.327665	6.237875	-0.037277	2.910119
190.520200	2880.429900	6.242880	-0.037281	2.914123
191.142753	2888.345050	6.247885	-0.037402	2.918064
191.264924	2896.415504	6.252890	-0.037430	2.922048
191.237816	2904.441230	6.257894	-0.037430	2.925997
191.683215	2912.450329	6.262899	-0.037518	2.929959
191.978213	2920.503026	6.267904	-0.037579	2.933928
192.207203	2928.518625	6.272909	-0.037627	2.937869
192.616619	2936.542505	6.277914	-0.037708	2.941820
193.153211	2944.533402	6.282918	-0.037813	2.945755
193.413744	2952.627604	6.287923	-0.037867	2.949721
194.052404	2960.592807	6.292928	-0.037991	2.953639
194.386621	2968.656719	6.297933	-0.038059	2.957583
194.512957	2976.734971	6.302938	-0.038088	2.961518
194.859904	2984.762081	6.307942	-0.038158	2.965435
195.071946	2992.837196	6.312947	-0.038203	2.969362
195.497278	3000.864522	6.317952	-0.038287	2.973273
195.461926	3008.906652	6.322957	-0.038286	2.977161
195.995267	3016.946997	6.327962	-0.038391	2.981073
196.301118	3024.941781	6.332966	-0.038453	2.984945
196.408932	3033.057268	6.337971	-0.038478	2.988861
196.409812	3041.095615	6.342976	-0.038484	2.992729
196.645456	3049.130242	6.347981	-0.038533	2.996602
197.037614	3057.159291	6.352986	-0.038611	3.000476
197.117821	3065.153399	6.357990	-0.038631	3.004311
197.426998	3073.204486	6.362995	-0.038694	3.008181
197.868469	3081.231767	6.368000	-0.038782	3.012041
197.786938	3089.308812	6.373005	-0.038772	3.015893
197.881202	3097.358500	6.378010	-0.038795	3.019736
198.180507	3105.337095	6.383014	-0.038856	3.023551
198.482271	3113.410399	6.388019	-0.038917	3.027406
198.622884	3121.462495	6.393024	-0.038949	3.031238
199.139458	3129.491856	6.398029	-0.039050	3.035073
199.347111	3137.525881	6.403034	-0.039094	3.038890
199.445007	3145.507038	6.408038	-0.039118	3.042672
199.654689	3153.608760	6.413043	-0.039162	3.046511
199.755711	3161.669965	6.418048	-0.039187	3.050321
200.274734	3169.643364	6.423053	-0.039288	3.054106
200.434379	3177.710796	6.428058	-0.039324	3.057912
200.528255	3185.744054	6.433062	-0.039346	3.061695
201.054922	3193.749055	6.438067	-0.039450	3.065480
200.885191	3201.838339	6.443072	-0.039423	3.069266
201.555444	3209.841383	6.448077	-0.039554	3.073048
202.114970	3217.852044	6.453082	-0.039663	3.076824
202.088701	3225.915106	6.458086	-0.039663	3.080591
202.438199	3233.898553	6.463091	-0.039734	3.084334
202.735061	3241.920067	6.468096	-0.039794	3.088088
203.112836	3249.979447	6.473101	-0.039870	3.091859
203.326385	3258.061618	6.478106	-0.039915	3.095628
203.609634	3266.024246	6.483110	-0.039973	3.099340
204.054849	3274.074356	6.488115	-0.040061	3.103095
204.042366	3282.162076	6.493120	-0.040064	3.106843
204.317941	3290.202679	6.498125	-0.040121	3.110577
204.437864	3298.260735	6.503130	-0.040149	3.114307
205.088018	3306.190390	6.508134	-0.040275	3.117999
205.349591	3314.257018	6.513139	-0.040329	3.121731
205.721934	3322.262610	6.518144	-0.040404	3.125435
205.924286	3330.306512	6.523149	-0.040447	3.129145
206.421465	3338.357037	6.528154	-0.040545	3.132867
206.307168	3346.416620	6.533158	-0.040529	3.136561
206.692959	3354.442543	6.538163	-0.040606	3.140258
206.979695	3362.423180	6.543168	-0.040665	3.143925
207.245013	3370.486458	6.548173	-0.040719	3.147624
207.711374	3378.557876	6.553178	-0.040811	3.151332
207.536619	3386.608061	6.558182	-0.040784	3.154997
207.811905	3394.626463	6.563187	-0.040841	3.158664
207.954694	3402.629655	6.568192	-0.040873	3.162313
208.396872	3410.664222	6.573197	-0.040960	3.165986
208.580634	3418.719986	6.578202	-0.041000	3.169652
208.617888	3426.755472	6.583206	-0.041012	3.173299
209.197311	3434.777495	6.588211	-0.041125	3.176959
209.468562	3442.799828	6.593216	-0.041181	3.180601
209.534281	3450.823894	6.598221	-0.041199	3.184231
209.596702	3458.929431	6.603226	-0.041216	3.187894
209.465431	3466.977246	6.608230	-0.041197	3.191517
209.906793	3474.971724	6.613235	-0.041284	3.195138
210.265945	3482.943876	6.618240	-0.041356	3.198741
210.878476	3490.915342	6.623245	-0.041476	3.202350
211.187508	3499.000497	6.628250	-0.041538	3.205993
211.262658	3507.058280	6.633254	-0.041558	3.209610
211.637437	3515.109006	6.638259	-0.041633	3.213232
211.754479	3523.144113	6.643264	-0.041660	3.216832
211.701342	3531.203846	6.648269	-0.041655	3.220432
212.338502	3539.152181	6.653274	-0.041779	3.224007
212.545914	3547.198889	6.658278	-0.041823	3.227604
212.803115	3555.287128	6.663283	-0.041877	3.231217
213.255314	3563.257951	6.668288	-0.041966	3.234783
213.927358	3571.198734	6.673293	-0.042096	3.238340
214.084649	3579.306234	6.678298	-0.042131	3.241945
214.086468	3587.357177	6.683302	-0.042137	3.245515
214.574493	3595.380469	6.688307	-0.042233	3.249089
214.412514	3603.478038	6.693312	-0.042208	3.252665
214.784900	3611.486374	6.698317	-0.042283	3.256220
215.198251	3619.489920	6.703322	-0.042365	3.259770
215.057674	3627.535607	6.708326	-0.042344	3.263313
215.480682	3635.549617	6.713331	-0.042428	3.266860
215.187833	3643.687261	6.718336	-0.042379	3.270429
215.493432	3651.645339	6.723341	-0.042441	3.273939
215.960375	3659.629218	6.728346	-0.042534	3.277464
216.337877	3667.628038	6.733350	-0.042609	3.280987
216.349290	3675.677181	6.738355	-0.042617	3.284514
216.354526	3683.754827	6.743360	-0.042623	3.288050
216.321603	3691.843959	6.748365	-0.042622	3.291585
216.625224	3699.850920	6.753370	-0.042684	3.295093
216.625169	3707.853466	6.758374	-0.042689	3.298584
217.038336	3715.856977	6.763379	-0.042771	3.302089
217.201905	3723.892594	6.768384	-0.042807	3.305593
217.174397	3731.954148	6.773389	-0.042807	3.309097
217.705844	3739.959293	6.778394	-0.042912	3.312596
217.804700	3747.995659	6.783398	-0.042935	3.316087
217.991964	3756.020334	6.788403	-0.042976	3.319572
218.930807	3763.902307	6.793408	-0.043156	3.323022
218.928175	3772.012410	6.798413	-0.043161	3.326530
219.204468	3780.102505	6.803418	-0.043217	3.330036
219.352726	3788.118622	6.808422	-0.043250	3.333502
219.859494	3796.131501	6.813427	-0.043350	3.336976
219.841093	3804.180818	6.818432	-0.043352	3.340443
220.152084	3812.185318	6.823437	-0.043415	3.343899
220.601359	3820.224531	6.828442	-0.043504	3.347371
220.494444	3828.308344	6.833446	-0.043489	3.350838
220.930391	3836.315507	6.838451	-0.043576	3.354289
221.229223	3844.313301	6.843456	-0.043637	3.357728
221.692267	3852.310874	6.848461	-0.043728	3.361168
221.952026	3860.341972	6.853466	-0.043782	3.364612
221.974673	3868.392633	6.858470	-0.043792	3.368052
222.243773	3876.471789	6.863475	-0.043847	3.371510
222.221985	3884.515791	6.868480	-0.043848	3.374938
222.745108	3892.489153	6.873485	-0.043951	3.378353
223.225947	3900.514883	6.878490	-0.044046	3.381785
223.192768	3908.550033	6.883494	-0.044045	3.385198
223.314404	3916.612316	6.888499	-0.044073	3.388626
223.999655	3924.627006	6.893504	-0.044206	3.392050
224.234249	3932.669618	6.898509	-0.044255	3.395466
224.117295	3940.702566	6.903514	-0.044238	3.398862
224.423248	3948.686704	6.908518	-0.044301	3.402249
224.880123	3956.725249	6.913523	-0.044391	3.405661
224.954165	3964.740223	6.918528	-0.044410	3.409046
225.178502	3972.801585	6.923533	-0.044457	3.412452
225.273572	3980.864252	6.928538	-0.044480	3.415851
225.419453	3988.818607	6.933542	-0.044513	3.419203
225.520581	3996.916894	6.938547	-0.044537	3.422610
225.586692	4004.945164	6.943552	-0.044555	3.425984
225.924583	4012.936261	6.948557	-0.044623	3.429348
226.222130	4020.964089	6.953562	-0.044683	3.432722
226.433251	4028.984046	6.958566	-0.044728	3.436087
226.815634	4036.980537	6.963571	-0.044805	3.439445
226.779051	4045.022815	6.968576	-0.044803	3.442804
227.294234	4053.048921	6.973581	-0.044904	3.446172
227.601089	4061.074882	6.978586	-0.044967	3.449529
227.628870	4069.110834	6.983590	-0.044977	3.452878
227.932831	4077.192678	6.988595	-0.045039	3.456252
228.327244	4085.127900	6.993600	-0.045118	3.459565
228.941084	4093.118375	6.998605	-0.045237	3.462904
229.194911	4101.197451	7.003610	-0.045290	3.466266
229.499406	4109.216324	7.008614	-0.045352	3.469600
229.877997	4117.263435	7.013619	-0.045428	3.472946
229.835769	4125.323930	7.018624	-0.045425	3.476279
229.925365	4133.333880	7.023629	-0.045447	3.479593
230.028953	4141.365513	7.028634	-0.045472	3.482914
230.103673	4149.389019	7.033638	-0.045491	3.486226
230.543453	4157.393910	7.038643	-0.045578	3.489540
230.461096	4165.482592	7.043648	-0.045568	3.492869
230.522789	4173.522648	7.048653	-0.045585	3.496178
230.736070	4181.494433	7.053658	-0.045630	3.499462
230.866188	4189.506290	7.058662	-0.045660	3.502756
231.352243	4197.501321	7.063667	-0.045756	3.506051
231.183921	4205.614586	7.068672	-0.045730	3.509371
231.458015	4213.614329	7.073677	-0.045786	3.512655
231.630962	4221.680055	7.078682	-0.045823	3.515960
232.102311	4229.617662	7.083686	-0.045916	3.519219
232.331377	4237.645336	7.088691	-0.045964	3.522504
232.604873	4245.651108	7.093696	-0.046021	3.525778
232.600874	4253.725184	7.098701	-0.046025	3.529069
232.746569	4261.777512	7.103706	-0.046058	3.532352
232.819382	4269.806971	7.108710	-0.046077	3.535620
233.106886	4277.814987	7.113715	-0.046135	3.538884
233.455580	4285.833504	7.118720	-0.046206	3.542150
233.425338	4293.852580	7.123725	-0.046205	3.545402
233.888971	4301.898882	7.128730	-0.046297	3.548677
234.086651	4309.949300	7.133734	-0.046339	3.551943
234.567464	4317.974778	7.138739	-0.046434	3.555204
234.502625	4326.020849	7.143744	-0.046427	3.558454
235.013808	4333.939949	7.148749	-0.046528	3.561667
235.113664	4341.975063	7.153754	-0.046552	3.564912
235.076333	4350.006226	7.158758	-0.046550	3.568147
235.886951	4357.996210	7.163763	-0.046706	3.571389
235.794075	4366.073467	7.168768	-0.046694	3.574636
235.865102	4374.096771	7.173773	-0.046713	3.577863
236.337077	4382.095010	7.178778	-0.046806	3.581089
236.458087	4390.104311	7.183782	-0.046834	3.584305
236.836465	4398.167160	7.188787	-0.046910	3.587549
236.697171	4406.235378	7.193792	-0.046889	3.590775
236.561720	4414.276165	7.198797	-0.046869	3.593989
237.259752	4422.246884	7.203802	-0.047004	3.597196
237.470624	4430.278145	7.208806	-0.047049	3.600409
238.092248	4438.237966	7.213811	-0.047170	3.603604
238.246961	4446.303608	7.218816	-0.047204	3.606824
238.235057	4454.345587	7.223821	-0.047207	3.610027
238.306870	4462.398809	7.228826	-0.047226	3.613234
238.465339	4470.431715	7.233830	-0.047261	3.616432
238.963725	4478.399199	7.238835	-0.047359	3.619612
239.093303	4486.430500	7.243840	-0.047388	3.622803
239.426681	4494.468426	7.248845	-0.047456	3.626000
239.710213	4502.503789	7.253850	-0.047514	3.629191
239.542640	4510.582667	7.258854	-0.047488	3.632385
239.987209	4518.604258	7.263859	-0.047576	3.635570
239.920651	4526.587354	7.268864	-0.047569	3.638722
240.261330	4534.590303	7.273869	-0.047638	3.641891
240.498814	4542.600580	7.278874	-0.047687	3.645058
240.705720	4550.627234	7.283878	-0.047731	3.648227
240.895783	4558.690712	7.288883	-0.047772	3.651407
241.150309	4566.667065	7.293888	-0.047824	3.654552
241.689859	4574.647889	7.298893	-0.047930	3.657704
241.959158	4582.752582	7.303898	-0.047986	3.660895
241.868968	4590.728773	7.308902	-0.047974	3.664022
242.188807	4598.787573	7.313907	-0.048039	3.667190
242.489006	4606.783891	7.318912	-0.048100	3.670331
242.466589	4614.843043	7.323917	-0.048101	3.673484
242.598911	4622.891251	7.328922	-0.048131	3.676635
243.005568	4630.838816	7.333926	-0.048212	3.679751
243.386726	4638.878268	7.338931	-0.048289	3.682900
243.364249	4646.917160	7.343936	-0.048290	3.686034
243.453883	4654.953641	7.348941	-0.048312	3.689168
243.684599	4662.996229	7.353946	-0.048360	3.692306
243.798784	4671.009517	7.358950	-0.048387	3.695427
243.905265	4679.067924	7.363955	-0.048412	3.698562
244.130909	4687.077737	7.368960	-0.048459	3.701678
244.205448	4695.078009	7.373965	-0.048478	3.704785
244.659130	4703.130502	7.378970	-0.048568	3.707919
244.698027	4711.164539	7.383974	-0.048581	3.711032
244.944071	4719.184274	7.388979	-0.048632	3.714142
245.009460	4727.216397	7.393984	-0.048649	3.717250
245.274416	4735.207294	7.398989	-0.048704	3.720345
245.376477	4743.233532	7.403994	-0.048728	3.723446
245.191448	4751.277334	7.408998	-0.048699	3.726544
244.896170	4759.382808	7.414003	-0.048649	3.729661
245.667653	4767.288815	7.419008	-0.048798	3.732725
245.810315	4775.332017	7.424013	-0.048830	3.735824
246.156664	4783.309404	7.429018	-0.048900	3.738900
246.151208	4791.350505	7.434022	-0.048904	3.741989
246.639320	4799.363870	7.439027	-0.049000	3.745077
246.664838	4807.425323	7.444032	-0.049011	3.748169
246.566809	4815.507922	7.449037	-0.048998	3.751264
246.607040	4823.512429	7.454042	-0.049010	3.754330
246.811295	4831.473012	7.459046	-0.049054	3.757380
247.161817	4839.485579	7.464051	-0.049124	3.760452
247.622425	4847.438169	7.469056	-0.049215	3.763500
247.675661	4855.506705	7.474061	-0.049231	3.766581
247.930761	4863.521620	7.479066	-0.049283	3.769643
248.282276	4871.527265	7.484070	-0.049354	3.772702
248.490414	4879.605998	7.489075	-0.049398	3.775782
248.398348	4887.601831	7.494080	-0.049386	3.778821
248.641047	4895.634132	7.499085	-0.049437	3.781880
249.171490	4903.649398	7.504090	-0.049541	3.784937
248.988096	4911.704938	7.509094	-0.049512	3.787989
249.269942	4919.750507	7.514099	-0.049570	3.791046
249.456431	4927.726957	7.519104	-0.049610	3.794072
249.541960	4935.791147	7.524109	-0.049631	3.797127
249.521863	4943.831183	7.529114	-0.049633	3.800167
249.741471	4951.724192	7.534118	-0.049679	3.803155
250.053957	4959.832900	7.539123	-0.049743	3.806225
249.822215	4967.854650	7.544128	-0.049705	3.809246
250.176111	4975.883731	7.549133	-0.049776	3.812281
250.519831	4983.923302	7.554138	-0.049845	3.815318
250.484574	4991.908389	7.559142	-0.049844	3.818323
250.450114	4999.987732	7.564147	-0.049843	3.821361
250.769504	5007.905291	7.569152	-0.049908	3.824343
250.994614	5016.000292	7.574157	-0.049955	3.827388
251.295882	5024.028245	7.579162	-0.050016	3.830407
251.341422	5032.027795	7.584166	-0.050030	3.833408
251.426364	5040.124693	7.589171	-0.050051	3.836443
251.673103	5048.065866	7.594176	-0.050102	3.839421
251.418182	5056.167912	7.599181	-0.050060	3.842446
251.977527	5064.099243	7.604186	-0.050170	3.845422
251.851340	5072.142868	7.609190	-0.050152	3.848423
252.167859	5080.222329	7.614195	-0.050216	3.851445
252.050782	5088.245353	7.619200	-0.050199	3.854434
252.369666	5096.225176	7.624205	-0.050264	3.857414
252.991786	5104.177993	7.629210	-0.050385	3.860388
253.158997	5112.190914	7.634214	-0.050422	3.863373
253.407434	5120.305475	7.639219	-0.050473	3.866394
253.158930	5128.370604	7.644224	-0.050432	3.869384
253.471760	5136.403400	7.649229	-0.050496	3.872372
253.722159	5144.481434	7.654234	-0.050548	3.875373
254.179382	5152.323288	7.659238	-0.050638	3.878288
254.305943	5160.400624	7.664243	-0.050667	3.881282
254.557979	5168.317715	7.669248	-0.050719	3.884216
254.508532	5176.427466	7.674253	-0.050715	3.887213
254.617695	5184.423079	7.679258	-0.050741	3.890169
254.776874	5192.477911	7.684262	-0.050776	3.893145
255.561272	5200.466503	7.689267	-0.050927	3.896108
255.875013	5208.418668	7.694272	-0.050991	3.899045
255.796097	5216.504414	7.699277	-0.050982	3.902021
255.697824	5224.574444	7.704282	-0.050969	3.904989
256.206156	5232.499640	7.709286	-0.051069	3.907913
256.329490	5240.578439	7.714291	-0.051097	3.910884
256.696961	5248.546526	7.719296	-0.051171	3.913817
256.549043	5256.646287	7.724301	-0.051148	3.916786
257.051961	5264.621099	7.729306	-0.051247	3.919719
257.162873	5272.626384	7.734310	-0.051273	3.922654
257.377100	5280.686846	7.739315	-0.051318	3.925609
257.347730	5288.704019	7.744320	-0.051318	3.928541
257.445977	5296.727294	7.749325	-0.051342	3.931475
257.939565	5304.733312	7.754330	-0.051439	3.934408
258.269189	5312.728418	7.759334	-0.051506	3.937332
258.464810	5320.798256	7.764339	-0.051548	3.940279
258.147951	5328.819382	7.769344	-0.051494	3.943196
258.408199	5336.815642	7.774349	-0.051548	3.946112
258.300973	5344.920971	7.779354	-0.051533	3.949060
258.671699	5352.924486	7.784358	-0.051607	3.951977
259.123986	5360.904124	7.789363	-0.051697	3.954884
259.283991	5368.887503	7.794368	-0.051732	3.957785
259.547058	5376.916357	7.799373	-0.051786	3.960703
259.608232	5384.925262	7.804378	-0.051803	3.963607
259.070081	5393.065064	7.809382	-0.051708	3.966546
259.899000	5400.960984	7.814387	-0.051868	3.969419
259.872191	5409.024855	7.819392	-0.051868	3.972335
259.970958	5417.064210	7.824397	-0.051892	3.975243
260.301507	5425.072078	7.829402	-0.051959	3.978141
260.509247	5433.077282	7.834406	-0.052003	3.981034
261.032241	5441.042604	7.839411	-0.052105	3.983916
260.703063	5449.155292	7.844416	-0.052049	3.986834
260.868250	5457.140417	7.849421	-0.052085	3.989712
261.028573	5465.175017	7.854426	-0.052121	3.992606
261.263006	5473.173723	7.859430	-0.052169	3.995487
261.452074	5481.214390	7.864435	-0.052210	3.998379
261.375980	5489.250202	7.869440	-0.052201	4.001263
261.705516	5497.158384	7.874445	-0.052268	4.004106
261.976350	5505.251077	7.879450	-0.052324	4.007013
261.885246	5513.278878	7.884454	-0.052312	4.009887
262.424559	5521.289639	7.889459	-0.052418	4.012765
262.488511	5529.335708	7.894464	-0.052435	4.015644
262.668465	5537.315767	7.899469	-0.052474	4.018500
262.742634	5545.384320	7.904474	-0.052493	4.021384
262.614309	5553.372746	7.909478	-0.052474	4.024234
262.765288	5561.442299	7.914483	-0.052508	4.027115
263.030791	5569.456364	7.919488	-0.052562	4.029977
263.429359	5577.439461	7.924493	-0.052642	4.032827
263.444371	5585.545899	7.929498	-0.052650	4.035713
263.377271	5593.481905	7.934502	-0.052643	4.038535
263.339203	5601.574119	7.939507	-0.052641	4.041411
263.925673	5609.412726	7.944512	-0.052755	4.044205
264.036843	5617.508836	7.949517	-0.052782	4.047081
264.160921	5625.509812	7.954522	-0.052810	4.049921
264.228459	5633.556863	7.959526	-0.052828	4.052774
264.711973	5641.611486	7.964531	-0.052923	4.055635
264.935936	5649.577569	7.969536	-0.052970	4.058458
265.488408	5657.609053	7.974541	-0.053078	4.061307
265.567971	5665.603458	7.979546	-0.053098	4.064134
265.734531	5673.652738	7.984550	-0.053135	4.066980
266.028689	5681.683628	7.989555	-0.053195	4.069819
265.854198	5689.755507	7.994560	-0.053168	4.072664
266.212330	5697.756950	7.999565	-0.053240	4.075490
266.370969	5705.763757	8.004570	-0.053275	4.078312
266.272478	5713.813734	8.009574	-0.053262	4.081144
266.631446	5721.770887	8.014579	-0.053334	4.083948
267.052319	5729.773707	8.019584	-0.053417	4.086767
267.101328	5737.792494	8.024589	-0.053432	4.089585
267.340707	5745.897870	8.029594	-0.053482	4.092433
267.380602	5753.878388	8.034598	-0.053494	4.095233
267.707446	5761.897077	8.039603	-0.053561	4.098048
267.843548	5769.950672	8.044608	-0.053591	4.100871
267.942534	5777.912364	8.049613	-0.053615	4.103660
267.896065	5786.031873	8.054618	-0.053612	4.106499
267.753873	5794.015240	8.059622	-0.053590	4.109288
268.380990	5802.022095	8.064627	-0.053713	4.112093
268.631805	5810.033700	8.069632	-0.053765	4.114894
268.685457	5818.043538	8.074637	-0.053780	4.117688
268.675925	5826.073903	8.079642	-0.053783	4.120488
268.315523	5834.080591	8.084646	-0.053722	4.123272
268.542780	5842.131298	8.089651	-0.053769	4.126077
269.131555	5850.029777	8.094656	-0.053884	4.128833
269.189965	5858.109886	8.099661	-0.053900	4.131643
269.180540	5866.184676	8.104666	-0.053904	4.134448
269.449583	5874.167841	8.109670	-0.053959	4.137223
269.712261	5882.210741	8.114675	-0.054014	4.140017
269.942851	5890.139711	8.119680	-0.054062	4.142769
270.138655	5898.187152	8.124685	-0.054104	4.145560
270.126412	5906.243467	8.129690	-0.054107	4.148349
269.694201	5914.339971	8.134694	-0.054031	4.151145
270.132515	5922.224904	8.139699	-0.054118	4.153877
270.728057	5930.248546	8.144704	-0.054234	4.156657
271.041194	5938.208690	8.149709	-0.054298	4.159410
271.030484	5946.313794	8.154714	-0.054301	4.162207
271.087712	5954.305032	8.159718	-0.054317	4.164963
270.993927	5962.417667	8.164723	-0.054305	4.167757
270.852954	5970.456717	8.169728	-0.054284	4.170524
271.211510	5978.396819	8.174733	-0.054356	4.173261
271.427023	5986.471828	8.179738	-0.054402	4.176041
271.422123	5994.413885	8.184742	-0.054406	4.178771
271.553094	6002.496345	8.189747	-0.054436	4.181548
271.849750	6010.427351	8.194752	-0.054496	4.184274
272.086222	6018.509626	8.199757	-0.054546	4.187049
272.416989	6026.500235	8.204762	-0.054613	4.189792
272.095322	6034.585432	8.209766	-0.054558	4.192558
272.585386	6042.625008	8.214771	-0.054655	4.195316
272.587826	6050.618359	8.219776	-0.054660	4.198051
272.559000	6058.637181	8.224781	-0.054660	4.200792
272.637209	6066.584475	8.229786	-0.054680	4.203508
272.799361	6074.635646	8.234790	-0.054716	4.206259
273.073104	6082.630754	8.239795	-0.054772	4.208990
273.309447	6090.690124	8.244800	-0.054821	4.211741
273.659695	6098.661274	8.249805	-0.054892	4.214461
273.512472	6106.756842	8.254810	-0.054870	4.217216
273.271987	6114.761598	8.259814	-0.054830	4.219937
273.867448	6122.756129	8.264819	-0.054946	4.222663
274.184537	6130.709961	8.269824	-0.055011	4.225370
274.451060	6138.739619	8.274829	-0.055066	4.228100
274.485115	6146.831707	8.279834	-0.055077	4.230847
274.441658	6154.846839	8.284838	-0.055075	4.233565
274.783288	6162.862310	8.289843	-0.055144	4.236286
274.837272	6170.807306	8.294848	-0.055159	4.238978
275.139646	6178.826191	8.299853	-0.055220	4.241696
275.412920	6186.842946	8.304858	-0.055277	4.244411
275.648094	6194.891992	8.309862	-0.055326	4.247135
275.959305	6202.945829	8.314867	-0.055389	4.249860
276.068619	6210.965796	8.319872	-0.055415	4.252569
276.224185	6218.959918	8.324877	-0.055449	4.255268
276.273362	6226.998498	8.329882	-0.055463	4.257980
276.294050	6234.987483	8.334886	-0.055473	4.260673
276.397019	6242.993933	8.339891	-0.055497	4.263370
276.272154	6251.064175	8.344896	-0.055479	4.266086
276.527910	6259.026249	8.349901	-0.055532	4.268766
276.532847	6267.189318	8.354906	-0.055538	4.271511
276.575868	6275.077672	8.359910	-0.055552	4.274161
276.989822	6283.110991	8.364915	-0.055634	4.276862
276.984372	6291.120562	8.369920	-0.055638	4.279550
276.973906	6299.118552	8.374925	-0.055642	4.282232
277.413626	6307.133136	8.379930	-0.055729	4.284922
277.015983	6315.173516	8.384934	-0.055660	4.287611
277.529609	6323.187934	8.389939	-0.055761	4.290298
277.249184	6331.256524	8.394944	-0.055714	4.292994
277.637852	6339.238922	8.399949	-0.055792	4.295666
277.640910	6347.250006	8.404954	-0.055798	4.298342
277.709594	6355.239066	8.409958	-0.055816	4.301010
278.028799	6363.209574	8.414963	-0.055881	4.303672
277.931495	6371.294556	8.419968	-0.055868	4.306367
278.138198	6379.281901	8.424973	-0.055912	4.309030
278.119032	6387.385221	8.429978	-0.055913	4.311728
278.153286	6395.345843	8.434982	-0.055925	4.314378
278.633530	6403.339323	8.439987	-0.056020	4.317041
278.623588	6411.359872	8.444992	-0.056023	4.319707
278.730708	6419.392750	8.449997	-0.056048	4.322376
279.242184	6427.355551	8.455002	-0.056149	4.325024
279.059585	6435.416096	8.460006	-0.056120	4.327696
279.304174	6443.424813	8.465011	-0.056171	4.330354
279.627105	6451.438513	8.470016	-0.056237	4.333012
279.937824	6459.408532	8.475021	-0.056300	4.335654
280.489640	6467.447537	8.480026	-0.056408	4.338319
280.514362	6475.496821	8.485030	-0.056418	4.340981
280.770448	6483.491700	8.490035	-0.056471	4.343626
280.571727	6491.562812	8.495040	-0.056439	4.346290
280.731234	6499.531084	8.500045	-0.056474	4.348922
281.122133	6507.602052	8.505050	-0.056552	4.351588
281.255858	6515.563775	8.510054	-0.056582	4.354214
281.411243	6523.639806	8.515059	-0.056617	4.356877
281.502297	6531.577215	8.520064	-0.056639	4.359492
281.628711	6539.614475	8.525069	-0.056668	4.362138
281.802613	6547.556875	8.530074	-0.056705	4.364751
281.966393	6555.606938	8.535078	-0.056741	4.367399
282.159076	6563.640414	8.540083	-0.056782	4.370040
282.611703	6571.687468	8.545088	-0.056872	4.372685
282.355682	6579.714834	8.550093	-0.056830	4.375317
282.344719	6587.772197	8.555098	-0.056833	4.377959
282.617898	6595.726476	8.560103	-0.056889	4.380568
282.912533	6603.703281	8.565107	-0.056949	4.383183
283.014336	6611.795822	8.570112	-0.056973	4.385832
283.008091	6619.778102	8.575117	-0.056978	4.388443
283.126171	6627.861002	8.580122	-0.057005	4.391087
283.338059	6635.818865	8.585127	-0.057050	4.393688
283.456626	6643.859905	8.590131	-0.057077	4.396315
283.682051	6651.842457	8.595136	-0.057124	4.398922
283.627051	6659.891813	8.600141	-0.057119	4.401546
283.508906	6667.935685	8.605146	-0.057103	4.404168
283.595227	6675.975600	8.610151	-0.057124	4.406787
283.750991	6683.980658	8.615155	-0.057158	4.409395
283.754885	6692.074954	8.620160	-0.057164	4.412028
284.009286	6699.997541	8.625165	-0.057217	4.414606
284.480478	6707.994877	8.630170	-0.057310	4.417208
284.524863	6716.025073	8.635175	-0.057324	4.419816
284.718396	6724.107385	8.640179	-0.057365	4.422441
284.597735	6732.136637	8.645184	-0.057348	4.425045
284.406228	6740.182419	8.650189	-0.057318	4.427653
284.843719	6748.190129	8.655194	-0.057404	4.430250
284.913006	6756.179159	8.660199	-0.057423	4.432837
284.917095	6764.195230	8.665203	-0.057429	4.435432
285.465588	6772.180782	8.670208	-0.057536	4.438018
285.686156	6780.203718	8.675213	-0.057582	4.440612
285.580736	6788.227128	8.680218	-0.057568	4.443204
285.423975	6796.286005	8.685223	-0.057544	4.445805
285.921969	6804.290662	8.690227	-0.057642	4.448391
285.871122	6812.335988	8.695232	-0.057638	4.450985
286.216898	6820.267399	8.700237	-0.057708	4.453543
286.330344	6828.401967	8.705242	-0.057734	4.456164
286.390501	6836.334602	8.710247	-0.057751	4.458718
286.526361	6844.390060	8.715251	-0.057781	4.461311
286.618825	6852.366419	8.720256	-0.057804	4.463876
286.935649	6860.403396	8.725261	-0.057868	4.466461
287.039563	6868.461855	8.730266	-0.057893	4.469049
286.810092	6876.508394	8.735271	-0.057855	4.471631
286.700743	6884.464360	8.740275	-0.057840	4.474183
286.743586	6892.463625	8.745280	-0.057854	4.476748
286.684613	6900.450381	8.750285	-0.057848	4.479307
286.878600	6908.537733	8.755290	-0.057889	4.481898
287.140168	6916.426013	8.760295	-0.057943	4.484424
286.813950	6924.576472	8.765299	-0.057888	4.487030
287.095013	6932.576206	8.770304	-0.057946	4.489589
287.785096	6940.527528	8.775309	-0.058079	4.492133
287.869672	6948.542077	8.780314	-0.058100	4.494692
287.948588	6956.564241	8.785319	-0.058120	4.497253
288.403289	6964.572747	8.790323	-0.058210	4.499809
288.689577	6972.606620	8.795328	-0.058269	4.502372
288.260644	6980.627130	8.800333	-0.058194	4.504925
288.742215	6988.675833	8.805338	-0.058289	4.507490
288.838693	6996.672855	8.810343	-0.058313	4.510035
289.055399	7004.683898	8.815347	-0.058358	4.512584
289.244119	7012.696923	8.820352	-0.058399	4.515132
289.315809	7020.717785	8.825357	-0.058417	4.517681
289.526697	7028.722068	8.830362	-0.058462	4.520223
289.831039	7036.665028	8.835367	-0.058524	4.522745
289.700732	7044.733166	8.840371	-0.058505	4.525303
289.694574	7052.802615	8.845376	-0.058509	4.527861
289.766543	7060.758562	8.850381	-0.058528	4.530382
290.132737	7068.792094	8.855386	-0.058601	4.532926
290.092617	7076.834119	8.860391	-0.058599	4.535471
290.200439	7084.823992	8.865395	-0.058625	4.537998
290.353439	7092.847601	8.870400	-0.058658	4.540535
290.510593	7100.822349	8.875405	-0.058693	4.543055
290.474044	7108.884370	8.880410	-0.058691	4.545600
290.691724	7116.856722	8.885415	-0.058737	4.548116
290.828752	7124.945149	8.890419	-0.058768	4.550668
291.422041	7132.849234	8.895424	-0.058884	4.553161
291.210136	7140.906964	8.900429	-0.058850	4.555698
291.182111	7148.981589	8.905434	-0.058850	4.558241
291.251673	7156.981590	8.910439	-0.058868	4.560758
291.625296	7164.965961	8.915443	-0.058943	4.563270
291.184072	7173.040136	8.920448	-0.058866	4.565807
291.473828	7181.011216	8.925453	-0.058925	4.568312
291.732847	7189.081485	8.930458	-0.058979	4.570846
291.789593	7197.038237	8.935463	-0.058995	4.573343
291.864630	7205.135665	8.940467	-0.059014	4.575883
292.199941	7213.070660	8.945472	-0.059082	4.578371
292.144261	7221.112103	8.950477	-0.059077	4.580890
292.446600	7229.066148	8.955482	-0.059138	4.583381
292.590309	7237.094379	8.960487	-0.059170	4.585894
292.969295	7245.125824	8.965491	-0.059246	4.588406
292.910197	7253.171069	8.970496	-0.059241	4.590921
293.177668	7261.184113	8.975501	-0.059296	4.593425
293.526567	7269.211258	8.980506	-0.059366	4.595932
293.371549	7277.176174	8.985511	-0.059342	4.598417
293.796434	7285.192884	8.990515	-0.059427	4.600919
293.849840	7293.190630	8.995520	-0.059442	4.603412
293.652720	7301.230820	9.000525	-0.059411	4.605917
293.800205	7309.220866	9.005530	-0.059443	4.608405
294.016788	7317.252176	9.010535	-0.059489	4.610905
294.285962	7325.287759	9.015539	-0.059545	4.613404
294.327282	7333.325525	9.020544	-0.059558	4.615903
294.347885	7341.264214	9.025549	-0.059567	4.618370
294.800468	7349.353777	9.030554	-0.059656	4.620882
294.868283	7357.314104	9.035559	-0.059674	4.623353
294.409683	7365.435021	9.040563	-0.059594	4.625872
294.765720	7373.421407	9.045568	-0.059666	4.628348
295.097871	7381.398157	9.050573	-0.059733	4.630820
294.995728	7389.443622	9.055578	-0.059719	4.633312
295.074944	7397.432559	9.060583	-0.059739	4.635785
295.348463	7405.409371	9.065587	-0.059795	4.638253
295.404897	7413.440303	9.070592	-0.059811	4.640736
295.746787	7421.411606	9.075597	-0.059880	4.643200
295.670571	7429.474589	9.080602	-0.059871	4.645690
295.667056	7437.470007	9.085607	-0.059876	4.648158
295.951584	7445.557603	9.090611	-0.059934	4.650654
296.301306	7453.506859	9.095616	-0.060005	4.653105
296.061044	7461.574984	9.100621	-0.059965	4.655592
295.859975	7469.605779	9.105626	-0.059933	4.658066
295.786248	7477.638785	9.110631	-0.059925	4.660539
296.177080	7485.556526	9.115635	-0.060003	4.662976
295.942800	7493.622307	9.120640	-0.059964	4.665456
296.122107	7501.622573	9.125645	-0.060003	4.667915
296.257013	7509.718567	9.130650	-0.060034	4.670403
296.176370	7517.691537	9.135655	-0.060024	4.672851
296.771676	7525.715455	9.140659	-0.060140	4.675313
296.973084	7533.681080	9.145664	-0.060183	4.677757
297.407667	7541.628982	9.150669	-0.060269	4.680193
297.261029	7549.714528	9.155674	-0.060247	4.682671
297.364946	7557.667216	9.160679	-0.060272	4.685106
297.671465	7565.736812	9.165683	-0.060334	4.687576
297.952453	7573.728043	9.170688	-0.060392	4.690020
297.566085	7581.832980	9.175693	-0.060325	4.692499
297.672007	7589.834222	9.180698	-0.060350	4.694944
297.791582	7597.796789	9.185703	-0.060378	4.697376
298.158031	7605.779726	9.190707	-0.060451	4.699813
298.179040	7613.901823	9.195712	-0.060461	4.702291
298.376649	7621.785186	9.200717	-0.060503	4.704695
298.574239	7629.906255	9.205722	-0.060545	4.707170
298.725250	7637.846977	9.210727	-0.060578	4.709589
298.902106	7645.910929	9.215731	-0.060616	4.712044
298.742173	7653.918099	9.220736	-0.060592	4.714481
298.820136	7661.965405	9.225741	-0.060612	4.716929
298.925361	7669.963651	9.230746	-0.060637	4.719360
298.767512	7678.026371	9.235751	-0.060613	4.721811
299.106927	7685.948858	9.240755	-0.060681	4.724216
299.181033	7694.035564	9.245760	-0.060700	4.726671
299.044418	7702.041919	9.250765	-0.060680	4.729100
299.101971	7710.157520	9.255770	-0.060696	4.731561
299.035364	7718.020044	9.260775	-0.060689	4.733944
299.330526	7726.115610	9.265779	-0.060749	4.736395
299.604361	7734.077137	9.270784	-0.060805	4.738805
299.670758	7742.098193	9.275789	-0.060823	4.741232
299.892209	7750.093491	9.280794	-0.060870	4.743650
299.763512	7758.135920	9.285799	-0.060851	4.746081
300.203130	7766.142149	9.290803	-0.060938	4.748499
300.282130	7774.237825	9.295808	-0.060958	4.750944
300.805959	7782.129038	9.300813	-0.061061	4.753324
300.890772	7790.240402	9.305818	-0.061082	4.755771
301.044578	7798.213613	9.310823	-0.061116	4.758175
301.167266	7806.267348	9.315827	-0.061144	4.760601
301.197501	7814.201085	9.320832	-0.061155	4.762991
301.453681	7822.259041	9.325837	-0.061208	4.765416
301.627178	7830.317362	9.330842	-0.061246	4.767840
301.914732	7838.281210	9.335847	-0.061305	4.770235
301.660554	7846.321033	9.340851	-0.061263	4.772652
301.828321	7854.384429	9.345856	-0.061299	4.775074
301.929607	7862.370232	9.350861	-0.061323	4.777472
302.100288	7870.402397	9.355866	-0.061360	4.779882
301.755436	7878.457452	9.360871	-0.061302	4.782299
301.978894	7886.418127	9.365875	-0.061348	4.784686
302.312894	7894.413201	9.370880	-0.061416	4.787080
302.326873	7902.432991	9.375885	-0.061424	4.789483
302.576553	7910.529263	9.380890	-0.061476	4.791905
302.584013	7918.457995	9.385895	-0.061482	4.794278
302.471598	7926.556387	9.390899	-0.061467	4.796700
302.662724	7934.480526	9.395904	-0.061508	4.799068
302.945428	7942.535148	9.400909	-0.061566	4.801474
303.014772	7950.448141	9.405914	-0.061584	4.803837
302.871476	7958.544562	9.410919	-0.061562	4.806254
302.919415	7966.569881	9.415923	-0.061577	4.808648
303.292832	7974.643056	9.420928	-0.061652	4.811053
303.571287	7982.556812	9.425933	-0.061709	4.813411
304.006789	7990.114886	9.430938	-0.061795	4.815660
303.779008	7994.953931	9.435943	-0.061756	4.817102

303.852720	7997.471851	9.440947	-0.061771	4.817852
303.637875	7998.809513	9.445952	-0.061732	4.818251
303.577031	7999.306964	9.450957	-0.061721	4.818399
303.944978	8000.424711	9.455962	-0.061790	4.818730
304.065169	8000.404252	9.460967	-0.061813	4.818723
303.887280	8000.479569	9.465971	-0.061780	4.818747
304.277329	8000.477309	9.470976	-0.061852	4.818744
304.187855	8000.486640	9.475981	-0.061836	4.818748
304.331830	8000.467540	9.480986	-0.061863	4.818741
304.331844	8000.403556	9.485991	-0.061863	4.818722
304.431263	8000.471993	9.490995	-0.061881	4.818742
304.285530	8000.439680	9.496000	-0.061854	4.818733
304.470234	8000.483003	9.501005	-0.061889	4.818745
304.345854	8000.375438	9.506010	-0.061866	4.818714
304.374789	8000.461840	9.511015	-0.061871	4.818739
304.621674	8000.464011	9.516019	-0.061917	4.818739
304.627873	8000.429480	9.521024	-0.061919	4.818729
304.571334	8000.460221	9.526029	-0.061908	4.818738
304.812305	8000.438187	9.531034	-0.061953	4.818731
304.978562	8000.415181	9.536039	-0.061984	4.818723
304.981001	8000.466622	9.541043	-0.061985	4.818738
304.887425	8000.458066	9.546048	-0.061967	4.818736
305.003569	8000.478467	9.551053	-0.061989	4.818742
305.206120	8000.460130	9.556058	-0.062027	4.818736
304.934289	8000.421977	9.561063	-0.061976	4.818725
305.212467	8000.458126	9.566067	-0.062028	4.818735
305.264173	8000.468247	9.571072	-0.062038	4.818738
305.457279	8000.453983	9.576077	-0.062074	4.818733
305.070006	8000.494053	9.581082	-0.062002	4.818746
305.178730	8000.359100	9.586087	-0.062022	4.818706
305.451427	8000.479102	9.591091	-0.062073	4.818740
305.552975	8000.425880	9.596096	-0.062092	4.818724
305.533270	8000.471787	9.601101	-0.062089	4.818738
305.387260	8000.496117	9.606106	-0.062061	4.818746
305.299559	8000.485539	9.611111	-0.062045	4.818743
305.363660	8000.382524	9.616115	-0.062057	4.818712
305.553921	8000.477325	9.621120	-0.062093	4.818739
305.718237	8000.470030	9.626125	-0.062123	4.818737
305.642070	8000.464847	9.631130	-0.062109	4.818735
305.612752	8000.472863	9.636135	-0.062104	4.818738
305.491349	8000.450306	9.641139	-0.062081	4.818732
305.730088	8000.452373	9.646144	-0.062126	4.818731
305.508632	8000.445298	9.651149	-0.062085	4.818730
305.619451	8000.467728	9.656154	-0.062105	4.818736
305.272198	8000.488388	9.661159	-0.062041	4.818744
305.558954	8000.409254	9.666163	-0.062094	4.818719
305.908450	8000.466266	9.671168	-0.062160	4.818735
305.842373	8000.467509	9.676173	-0.062147	4.818735
306.124859	8000.448116	9.681178	-0.062200	4.818728
305.839234	8000.428664	9.686183	-0.062147	4.818724
306.122757	8000.472229	9.691187	-0.062200	4.818736
306.133396	8000.456637	9.696192	-0.062202	4.818731
305.911769	8000.468442	9.701197	-0.062161	4.818735
305.890303	8000.478659	9.706202	-0.062157	4.818738
305.773417	8000.445670	9.711207	-0.062135	4.818729
306.019354	8000.486646	9.716211	-0.062181	4.818740
306.164386	8000.449727	9.721216	-0.062208	4.818729
305.960403	8000.487988	9.726221	-0.062170	4.818741
306.116888	8000.405059	9.731226	-0.062199	4.818716
306.301251	8000.448381	9.736231	-0.062234	4.818728
306.427168	8000.431144	9.741235	-0.062257	4.818722
306.583504	8000.413255	9.746240	-0.062286	4.818716
306.149462	8000.402359	9.751245	-0.062206	4.818715
306.294081	8000.453556	9.756250	-0.062233	4.818729
306.375980	8000.437844	9.761255	-0.062248	4.818724
306.379487	8000.506085	9.766259	-0.062249	4.818745
306.498040	8000.452035	9.771264	-0.062271	4.818728
306.420532	8000.411166	9.776269	-0.062257	4.818716
306.435786	8000.469070	9.781274	-0.062260	4.818733
306.207343	8000.414694	9.786279	-0.062217	4.818718
306.390497	8000.451706	9.791283	-0.062251	4.818728
306.432569	8000.437573	9.796288	-0.062259	4.818724
306.425846	8000.472110	9.801293	-0.062258	4.818734
306.785861	8000.457926	9.806298	-0.062325	4.818729
306.659677	8000.409078	9.811303	-0.062302	4.818715
306.602696	8000.483875	9.816307	-0.062291	4.818737
306.721367	8000.456053	9.821312	-0.062313	4.818728
306.830498	8000.421813	9.826317	-0.062334	4.818718
306.889047	8000.453005	9.831322	-0.062345	4.818727
306.620056	8000.419081	9.836327	-0.062295	4.818718
306.894595	8000.424764	9.841331	-0.062346	4.818719
306.773885	8000.413754	9.846336	-0.062324	4.818716
306.766061	8000.373793	9.851341	-0.062322	4.818704
306.819417	8000.429047	9.856346	-0.062332	4.818720
306.857962	8000.397033	9.861351	-0.062339	4.818710
306.910434	8000.442834	9.866355	-0.062349	4.818724
306.796763	8000.419327	9.871360	-0.062328	4.818717
306.970791	8000.421601	9.876365	-0.062361	4.818717
306.979863	8000.426971	9.881370	-0.062362	4.818719
306.869108	8000.416091	9.886375	-0.062342	4.818716
307.185896	8000.491565	9.891379	-0.062401	4.818737
306.948653	8000.466447	9.896384	-0.062357	4.818731
306.759227	8000.432511	9.901389	-0.062322	4.818721
306.996801	8000.475479	9.906394	-0.062366	4.818733
307.005700	8000.417901	9.911399	-0.062368	4.818716
306.797239	8000.433024	9.916403	-0.062329	4.818721
306.891912	8000.427969	9.921408	-0.062347	4.818719
306.950835	8000.404614	9.926413	-0.062358	4.818712
307.069601	8000.454426	9.931418	-0.062380	4.818727
306.869645	8000.449727	9.936423	-0.062343	4.818726
307.048251	8000.461503	9.941427	-0.062376	4.818729
307.155870	8000.425145	9.946432	-0.062396	4.818718
306.954795	8000.418333	9.951437	-0.062359	4.818716
307.231314	8000.434533	9.956442	-0.062411	4.818720
307.071063	8000.440842	9.961447	-0.062381	4.818723
307.051919	8000.468924	9.966451	-0.062377	4.818731
307.213979	8000.439570	9.971456	-0.062408	4.818722
307.106398	8000.427682	9.976461	-0.062388	4.818719
307.117586	8000.457208	9.981466	-0.062390	4.818727
307.050175	8000.420666	9.986471	-0.062377	4.818717
307.132268	8000.461608	9.991475	-0.062393	4.818728
307.171624	8000.407574	9.996480	-0.062400	4.818712
307.179030	8000.349976	10.001485	-0.062401	4.818695
307.395534	8000.409456	10.006490	-0.062442	4.818712
307.416527	8000.422324	10.011495	-0.062446	4.818716
307.391966	8000.388439	10.016499	-0.062441	4.818706
307.262855	8000.427676	10.021504	-0.062417	4.818718
307.145153	8000.455522	10.026509	-0.062396	4.818727
307.421767	8000.444447	10.031514	-0.062447	4.818722
307.320627	8000.433692	10.036519	-0.062428	4.818719
307.571957	8000.468448	10.041523	-0.062475	4.818729
307.674102	8000.446706	10.046528	-0.062494	4.818722
307.400812	8000.428460	10.051533	-0.062444	4.818718
307.514858	8000.457230	10.056538	-0.062465	4.818726
307.415650	8000.410831	10.061543	-0.062447	4.818712
307.294638	8000.471155	10.066547	-0.062424	4.818731
307.200092	8000.455241	10.071552	-0.062407	4.818726
307.286704	8000.462671	10.076557	-0.062423	4.818728
307.330389	8000.466394	10.081562	-0.062431	4.818729
306.675695	8000.488287	10.086567	-0.062309	4.818738
307.025450	8000.501246	10.091571	-0.062374	4.818741
307.277524	8000.473065	10.096576	-0.062421	4.818731
306.615499	8000.403593	10.101581	-0.062298	4.818713
307.008661	8000.499995	10.106586	-0.062372	4.818740
307.008114	8000.439146	10.111591	-0.062372	4.818722
307.200226	8000.514045	10.116595	-0.062407	4.818744
307.337752	8000.488567	10.121600	-0.062433	4.818736
307.114177	8000.473068	10.126605	-0.062392	4.818732
307.194424	8000.487759	10.131610	-0.062407	4.818736
307.253773	8000.462311	10.136615	-0.062418	4.818728
307.405973	8000.488431	10.141619	-0.062446	4.818735
307.605971	8000.458523	10.146624	-0.062483	4.818726
307.368843	8000.468025	10.151629	-0.062439	4.818729
307.204611	8000.488970	10.156634	-0.062409	4.818736
307.277813	8000.442721	10.161639	-0.062423	4.818722
307.276563	8000.440612	10.166643	-0.062422	4.818722
307.435501	8000.435347	10.171648	-0.062452	4.818719
307.298024	8000.349632	10.176653	-0.062427	4.818694
307.484910	8000.458034	10.181658	-0.062462	4.818726
307.537634	8000.402076	10.186663	-0.062471	4.818709
307.523191	8000.456446	10.191667	-0.062469	4.818725
307.677025	8000.457409	10.196672	-0.062498	4.818725
307.511002	8000.398599	10.201677	-0.062467	4.818708
307.679216	8000.482628	10.206682	-0.062498	4.818733
307.682797	8000.432324	10.211687	-0.062499	4.818718
307.739585	8000.427824	10.216691	-0.062509	4.818716
307.810219	8000.419310	10.221696	-0.062523	4.818713
307.673965	8000.373476	10.226701	-0.062497	4.818700
307.707984	8000.436872	10.231706	-0.062504	4.818719
307.527993	8000.454463	10.236711	-0.062470	4.818725
307.174608	8000.505463	10.241715	-0.062405	4.818741
307.236236	8000.472701	10.246720	-0.062416	4.818731
307.320775	8000.421355	10.251725	-0.062432	4.818716
307.261903	8000.489833	10.256730	-0.062421	4.818736
307.563123	8000.454950	10.261735	-0.062477	4.818725
307.659844	8000.478249	10.266739	-0.062496	4.818731
307.651197	8000.448767	10.271744	-0.062494	4.818723
307.431503	8000.372471	10.276749	-0.062453	4.818701
307.866274	8000.436896	10.281754	-0.062534	4.818718
307.590950	8000.438557	10.286759	-0.062483	4.818720
307.564440	8000.452904	10.291763	-0.062478	4.818724
307.713115	8000.445407	10.296768	-0.062506	4.818721
307.687883	8000.431445	10.301773	-0.062501	4.818717
307.780858	8000.462039	10.306778	-0.062519	4.818726
307.806791	8000.418320	10.311783	-0.062524	4.818713
307.808260	8000.447720	10.316787	-0.062524	4.818722
307.787869	8000.472639	10.321792	-0.062520	4.818729
307.652582	8000.464585	10.326797	-0.062495	4.818727
307.906868	8000.425943	10.331802	-0.062543	4.818715
307.838391	8000.401976	10.336807	-0.062530	4.818708
307.677494	8000.435553	10.341811	-0.062500	4.818719
307.831099	8000.441758	10.346816	-0.062529	4.818720
307.758324	8000.395703	10.351821	-0.062515	4.818706
307.537004	8000.462064	10.356826	-0.062474	4.818727
307.635245	8000.425583	10.361831	-0.062492	4.818716
307.937131	8000.454705	10.366835	-0.062549	4.818723
307.974495	8000.445756	10.371840	-0.062556	4.818720
307.910432	8000.395618	10.376845	-0.062544	4.818706
308.144556	8000.458477	10.381850	-0.062588	4.818723
308.124155	8000.441431	10.386855	-0.062584	4.818719
307.745767	8000.428108	10.391859	-0.062514	4.818716
307.828482	8000.433389	10.396864	-0.062529	4.818717
307.869914	8000.474851	10.401869	-0.062537	4.818729
307.818584	8000.492022	10.406874	-0.062527	4.818735
307.861750	8000.456921	10.411879	-0.062535	4.818724
307.944962	8000.492633	10.416883	-0.062551	4.818734
308.063510	8000.470056	10.421888	-0.062573	4.818727
307.801786	8000.470844	10.426893	-0.062525	4.818728
307.912612	8000.483836	10.431898	-0.062545	4.818732
307.877188	8000.462397	10.436903	-0.062539	4.818726
307.802255	8000.493948	10.441907	-0.062525	4.818735
307.505262	8000.481687	10.446912	-0.062470	4.818733
307.987749	8000.491134	10.451917	-0.062560	4.818734
307.871610	8000.491723	10.456922	-0.062538	4.818734
307.759181	8000.450396	10.461927	-0.062517	4.818723
307.900623	8000.518341	10.466931	-0.062544	4.818742
307.590843	8000.521650	10.471936	-0.062486	4.818744
307.529049	8000.496720	10.476941	-0.062475	4.818737
307.812775	8000.489935	10.481946	-0.062528	4.818734
307.877744	8000.438333	10.486951	-0.062540	4.818719
307.835236	8000.479749	10.491955	-0.062532	4.818731
307.857746	8000.403463	10.496960	-0.062536	4.818708
307.960740	8000.431040	10.501965	-0.062555	4.818716
307.862995	8000.490619	10.506970	-0.062537	4.818734
307.790511	8000.428831	10.511975	-0.062524	4.818716
307.833936	8000.461926	10.516979	-0.062532	4.818726
307.718325	8000.468817	10.521984	-0.062511	4.818728
307.370660	8000.525136	10.526989	-0.062446	4.818746
307.682174	8000.483044	10.531994	-0.062504	4.818733
307.966852	8000.451094	10.536999	-0.062557	4.818722
308.062548	8000.468084	10.542003	-0.062575	4.818727
307.830805	8000.473460	10.547008	-0.062532	4.818729
308.008533	8000.361431	10.552013	-0.062565	4.818695
308.199612	8000.432122	10.557018	-0.062601	4.818715
308.209057	8000.420710	10.562023	-0.062603	4.818712
308.190637	8000.414181	10.567027	-0.062599	4.818710
308.324776	8000.405446	10.572032	-0.062624	4.818707
308.288281	8000.413368	10.577037	-0.062618	4.818709
308.193842	8000.501317	10.582042	-0.062600	4.818736
308.037334	8000.463611	10.587047	-0.062571	4.818725
308.048259	8000.411304	10.592051	-0.062573	4.818710
308.129184	8000.449084	10.597056	-0.062588	4.818721
308.246946	8000.426497	10.602061	-0.062610	4.818714
308.348501	8000.476087	10.607066	-0.062629	4.818728
308.029532	8000.424721	10.612071	-0.062570	4.818714
308.161509	8000.367698	10.617075	-0.062595	4.818696
308.346144	8000.445649	10.622080	-0.062629	4.818719
308.144696	8000.388473	10.627085	-0.062592	4.818703
308.171895	8000.484303	10.632090	-0.062597	4.818731
308.367196	8000.396633	10.637095	-0.062633	4.818704
308.267430	8000.390091	10.642099	-0.062615	4.818703
308.352947	8000.433178	10.647104	-0.062631	4.818715
308.149837	8000.379127	10.652109	-0.062593	4.818700
308.176898	8000.469710	10.657114	-0.062598	4.818727
307.841528	8000.448555	10.662119	-0.062536	4.818722
308.058544	8000.489160	10.667123	-0.062576	4.818733
308.106517	8000.473006	10.672128	-0.062585	4.818728
307.797260	8000.461633	10.677133	-0.062528	4.818726
307.706795	8000.484589	10.682138	-0.062511	4.818733
308.082392	8000.449628	10.687143	-0.062581	4.818721
307.944979	8000.480364	10.692147	-0.062556	4.818731
308.102258	8000.469832	10.697152	-0.062585	4.818727
307.999752	8000.460107	10.702157	-0.062566	4.818724
308.078472	8000.424421	10.707162	-0.062581	4.818714
307.986174	8000.454696	10.712167	-0.062564	4.818723
308.080969	8000.437055	10.717171	-0.062581	4.818717
308.229751	8000.458935	10.722176	-0.062609	4.818723
307.949652	8000.462630	10.727181	-0.062557	4.818725
307.903215	8000.503995	10.732186	-0.062549	4.818738
308.024926	8000.445789	10.737191	-0.062571	4.818720
308.118204	8000.457503	10.742195	-0.062589	4.818723
308.227709	8000.480969	10.747200	-0.062609	4.818730
308.399462	8000.489510	10.752205	-0.062641	4.818732
308.447238	8000.492238	10.757210	-0.062650	4.818732
308.468323	8000.433767	10.762215	-0.062654	4.818715
308.388037	8000.445315	10.767219	-0.062639	4.818719
308.600912	8000.471179	10.772224	-0.062679	4.818725
308.422633	8000.403813	10.777229	-0.062646	4.818706
308.329975	8000.477098	10.782234	-0.062629	4.818728
308.370440	8000.457698	10.787239	-0.062636	4.818722
308.546097	8000.480979	10.792243	-0.062669	4.818728
308.540756	8000.472522	10.797248	-0.062668	4.818726
308.456884	8000.468286	10.802253	-0.062653	4.818725
308.534913	8000.502882	10.807258	-0.062667	4.818735
308.317712	8000.447597	10.812263	-0.062627	4.818719
308.216507	8000.477756	10.817267	-0.062608	4.818729
308.290832	8000.477683	10.822272	-0.062622	4.818728
308.060867	8000.484130	10.827277	-0.062579	4.818731
308.094236	8000.508701	10.832282	-0.062586	4.818738
308.339567	8000.378670	10.837287	-0.062631	4.818699
308.482830	8000.413067	10.842291	-0.062658	4.818709
308.641201	8000.442417	10.847296	-0.062688	4.818717
308.536265	8000.423218	10.852301	-0.062668	4.818711
308.502514	8000.447963	10.857306	-0.062662	4.818719
308.337337	8000.446862	10.862311	-0.062632	4.818719
308.492295	8000.418465	10.867315	-0.062660	4.818710
308.491254	8000.461472	10.872320	-0.062660	4.818723
308.529473	8000.432601	10.877325	-0.062668	4.818714
308.598548	8000.488063	10.882330	-0.062680	4.818730
308.611803	8000.428441	10.887335	-0.062683	4.818713
308.610845	8000.477743	10.892339	-0.062683	4.818727
308.353605	8000.439771	10.897344	-0.062635	4.818717
308.494572	8000.448960	10.902349	-0.062661	4.818719
308.753942	8000.394648	10.907354	-0.062710	4.818702
308.723812	8000.447767	10.912359	-0.062704	4.818718
308.537098	8000.447434	10.917363	-0.062670	4.818719
308.619932	8000.433833	10.922368	-0.062685	4.818714
308.567902	8000.403785	10.927373	-0.062675	4.818705
308.554200	8000.501181	10.932378	-0.062673	4.818734
308.460324	8000.428621	10.937383	-0.062656	4.818713
308.557109	8000.463462	10.942387	-0.062674	4.818723
308.630386	8000.456030	10.947392	-0.062687	4.818721
308.683738	8000.459880	10.952397	-0.062698	4.818722
308.569460	8000.475181	10.957402	-0.062676	4.818727
308.636549	8000.446686	10.962407	-0.062689	4.818718
308.595119	8000.427267	10.967411	-0.062681	4.818712
308.556677	8000.437263	10.972416	-0.062674	4.818715
308.678551	8000.400041	10.977421	-0.062697	4.818704
308.443284	8000.431598	10.982426	-0.062653	4.818714
308.148501	8000.453986	10.987431	-0.062598	4.818722
308.409619	8000.461595	10.992435	-0.062647	4.818723
308.537797	8000.449635	10.997440	-0.062671	4.818719
308.559195	8000.428937	11.002445	-0.062675	4.818713
308.542420	8000.416135	11.007450	-0.062672	4.818709
308.380157	8000.436055	11.012455	-0.062642	4.818716
308.307981	8000.391056	11.017459	-0.062629	4.818703
308.306611	8000.445598	11.022464	-0.062628	4.818719
308.476584	8000.431036	11.027469	-0.062660	4.818714
308.732125	8000.467948	11.032474	-0.062708	4.818724
308.246442	8000.480501	11.037479	-0.062618	4.818729
308.293862	8000.465389	11.042483	-0.062626	4.818725
308.272342	8000.453573	11.047488	-0.062622	4.818721
308.414149	8000.425005	11.052493	-0.062649	4.818712
308.299763	8000.515841	11.057498	-0.062628	4.818740
308.345057	8000.449294	11.062503	-0.062636	4.818720
308.227079	8000.428876	11.067507	-0.062614	4.818714
308.095755	8000.463888	11.072512	-0.062590	4.818725
308.356243	8000.397001	11.077517	-0.062639	4.818704
308.550341	8000.450946	11.082522	-0.062675	4.818719
308.314826	8000.396472	11.087527	-0.062631	4.818704
308.404867	8000.427028	11.092531	-0.062648	4.818713
308.412051	8000.455454	11.097536	-0.062649	4.818721
308.421361	8000.445090	11.102541	-0.062651	4.818718
308.549446	8000.489782	11.107546	-0.062675	4.818731
308.330929	8000.443922	11.112551	-0.062634	4.818718
308.580048	8000.444031	11.117555	-0.062681	4.818717
308.713694	8000.434240	11.122560	-0.062706	4.818714
308.856848	8000.350085	11.127565	-0.062733	4.818688
308.810579	8000.380961	11.132570	-0.062724	4.818698
308.667029	8000.368603	11.137575	-0.062697	4.818694
308.808032	8000.405070	11.142579	-0.062724	4.818705
308.798502	8000.447966	11.147584	-0.062722	4.818718
308.501683	8000.408428	11.152589	-0.062667	4.818707
308.335244	8000.453473	11.157594	-0.062636	4.818721
308.818350	8000.466077	11.162599	-0.062726	4.818723
308.714439	8000.498299	11.167603	-0.062707	4.818733
308.632756	8000.489895	11.172608	-0.062692	4.818731
308.601539	8000.479002	11.177613	-0.062686	4.818728
308.715918	8000.502533	11.182618	-0.062707	4.818734
308.446817	8000.447619	11.187623	-0.062657	4.818719
308.347897	8000.446335	11.192627	-0.062639	4.818719
308.589343	8000.483063	11.197632	-0.062684	4.818729
308.634730	8000.457433	11.202637	-0.062693	4.818721
308.451155	8000.503303	11.207642	-0.062658	4.818735
308.329027	8000.493322	11.212647	-0.062636	4.818733
308.270126	8000.412826	11.217651	-0.062625	4.818709
308.085465	8000.506942	11.222656	-0.062591	4.818738
308.040023	8000.428720	11.227661	-0.062582	4.818715
308.398405	8000.514184	11.232666	-0.062649	4.818739
308.246487	8000.445064	11.237671	-0.062621	4.818719
308.058804	8000.452063	11.242675	-0.062586	4.818722
308.148930	8000.398691	11.247680	-0.062603	4.818705
307.983096	8000.525575	11.252685	-0.062572	4.818744
307.829578	8000.427059	11.257690	-0.062543	4.818715
308.103458	8000.486241	11.262695	-0.062595	4.818732
307.993677	8000.496355	11.267699	-0.062574	4.818735
307.976124	8000.421644	11.272704	-0.062571	4.818713
307.691735	8000.408499	11.277709	-0.062518	4.818710
307.738925	8000.436397	11.282714	-0.062527	4.818718
307.942045	8000.525080	11.287719	-0.062565	4.818744
307.906002	8000.478454	11.292723	-0.062558	4.818730
308.507533	8000.435950	11.297728	-0.062670	4.818715
308.666748	8000.441181	11.302733	-0.062700	4.818716
308.217201	8000.541282	11.307738	-0.062617	4.818748
308.543411	8000.365095	11.312743	-0.062677	4.818694
308.688254	8000.517016	11.317747	-0.062704	4.818738
308.588972	8000.484253	11.322752	-0.062686	4.818729
308.588447	8000.417107	11.327757	-0.062686	4.818709
308.572259	8000.491390	11.332762	-0.062683	4.818731
308.435757	8000.501155	11.337767	-0.062658	4.818735
308.853255	8000.470939	11.342771	-0.062736	4.818724
308.725609	8000.495507	11.347776	-0.062712	4.818732
308.262728	8000.490522	11.352781	-0.062626	4.818732
308.263711	8000.419200	11.357786	-0.062626	4.818711
308.495776	8000.471542	11.362791	-0.062669	4.818726
308.580814	8000.502034	11.367795	-0.062685	4.818734
308.584229	8000.476905	11.372800	-0.062686	4.818727
308.495900	8000.473660	11.377805	-0.062670	4.818726
308.517328	8000.504370	11.382810	-0.062674	4.818735
308.485878	8000.485081	11.387815	-0.062668	4.818730
308.594771	8000.466574	11.392819	-0.062688	4.818724
308.703782	8000.429185	11.397824	-0.062709	4.818712
308.591079	8000.443457	11.402829	-0.062688	4.818717
308.749739	8000.480155	11.407834	-0.062717	4.818727
308.962517	8000.444119	11.412839	-0.062757	4.818716
308.941362	8000.455390	11.417843	-0.062753	4.818719
308.789973	8000.467058	11.422848	-0.062725	4.818723
308.790099	8000.446083	11.427853	-0.062725	4.818717
309.070882	8000.479129	11.432858	-0.062778	4.818726
308.808319	8000.472561	11.437863	-0.062729	4.818725
308.751566	8000.429861	11.442867	-0.062718	4.818712
309.129530	8000.429554	11.447872	-0.062789	4.818711
309.095008	8000.352522	11.452877	-0.062782	4.818688
308.951884	8000.435640	11.457882	-0.062756	4.818713
308.900697	8000.419240	11.462887	-0.062746	4.818709
309.137873	8000.396113	11.467891	-0.062791	4.818701
308.642939	8000.454706	11.472896	-0.062699	4.818720
308.558891	8000.508170	11.477901	-0.062683	4.818736
308.856818	8000.493180	11.482906	-0.062739	4.818731
308.563454	8000.469423	11.487911	-0.062684	4.818725
308.855882	8000.483737	11.492915	-0.062739	4.818728
308.972250	8000.492606	11.497920	-0.062760	4.818730
308.756269	8000.478252	11.502925	-0.062720	4.818727
308.759510	8000.427942	11.507930	-0.062721	4.818712
308.926031	8000.441661	11.512935	-0.062752	4.818715
308.931765	8000.442791	11.517939	-0.062753	4.818715
308.754158	8000.475100	11.522944	-0.062720	4.818726
308.481737	8000.463158	11.527949	-0.062669	4.818723
308.602965	8000.505662	11.532954	-0.062692	4.818735
308.425120	8000.501249	11.537959	-0.062659	4.818735
308.509203	8000.520187	11.542963	-0.062675	4.818740
308.694393	8000.499529	11.547968	-0.062709	4.818733
308.830743	8000.465643	11.552973	-0.062735	4.818723
308.888374	8000.489482	11.557978	-0.062746	4.818729
308.493173	8000.392007	11.562983	-0.062672	4.818702
308.463379	8000.446179	11.567987	-0.062667	4.818718
308.247557	8000.513660	11.572992	-0.062627	4.818739
308.539979	8000.492303	11.577997	-0.062681	4.818732
308.534215	8000.425089	11.583002	-0.062680	4.818712
308.040988	8000.452232	11.588007	-0.062588	4.818722
308.184814	8000.393265	11.593011	-0.062615	4.818704
308.093045	8000.437186	11.598016	-0.062598	4.818717
308.679853	8000.439602	11.603021	-0.062708	4.818715
308.866294	8000.495547	11.608026	-0.062742	4.818731
308.676530	8000.445865	11.613031	-0.062707	4.818717
308.745591	8000.467755	11.618035	-0.062720	4.818723
308.802436	8000.484240	11.623040	-0.062731	4.818728
308.869424	8000.469383	11.628045	-0.062743	4.818723
308.911208	8000.462590	11.633050	-0.062751	4.818721
308.879868	8000.502054	11.638055	-0.062745	4.818733
309.008857	8000.475417	11.643059	-0.062769	4.818725
308.938546	8000.451424	11.648064	-0.062756	4.818718
309.187665	8000.444190	11.653069	-0.062803	4.818715
309.310757	8000.433212	11.658074	-0.062826	4.818711
309.270962	8000.463124	11.663079	-0.062819	4.818720
309.211280	8000.396255	11.668083	-0.062808	4.818700
309.263531	8000.437859	11.673088	-0.062817	4.818713
308.984342	8000.443663	11.678093	-0.062765	4.818715
309.141093	8000.493976	11.683098	-0.062795	4.818730
309.106690	8000.457861	11.688103	-0.062788	4.818719
309.084927	8000.440797	11.693107	-0.062784	4.818714
308.899890	8000.500287	11.698112	-0.062750	4.818733
309.042932	8000.478029	11.703117	-0.062777	4.818725
309.074699	8000.503629	11.708122	-0.062783	4.818733
308.825260	8000.475200	11.713127	-0.062736	4.818725
308.935097	8000.478738	11.718131	-0.062757	4.818726
309.220486	8000.453093	11.723136	-0.062810	4.818717
308.762158	8000.472296	11.728141	-0.062725	4.818725
308.809234	8000.420459	11.733146	-0.062734	4.818709
308.875758	8000.448610	11.738151	-0.062746	4.818717
308.955744	8000.477987	11.743155	-0.062761	4.818726
308.983053	8000.489890	11.748160	-0.062766	4.818729
308.655672	8000.544375	11.753165	-0.062706	4.818747
308.803707	8000.427760	11.758170	-0.062733	4.818711
308.464249	8000.489431	11.763175	-0.062670	4.818731
308.577408	8000.524486	11.768179	-0.062691	4.818741
309.053626	8000.521265	11.773184	-0.062780	4.818738
308.861260	8000.444271	11.778189	-0.062744	4.818716
309.067558	8000.500476	11.783194	-0.062783	4.818732
308.752694	8000.489028	11.788199	-0.062724	4.818730
308.506395	8000.409233	11.793203	-0.062678	4.818707
308.822044	8000.525616	11.798208	-0.062737	4.818740
308.837833	8000.460781	11.803213	-0.062740	4.818721
309.031160	8000.517865	11.808218	-0.062776	4.818737
308.561177	8000.408922	11.813223	-0.062689	4.818707
308.713235	8000.505334	11.818227	-0.062717	4.818735
308.643892	8000.526467	11.823232	-0.062705	4.818741
308.436495	8000.387379	11.828237	-0.062666	4.818701
308.859950	8000.511463	11.833242	-0.062745	4.818736
308.874847	8000.484386	11.838247	-0.062748	4.818728
308.806867	8000.505536	11.843251	-0.062735	4.818734
308.483259	8000.417388	11.848256	-0.062675	4.818709
308.304608	8000.448635	11.853261	-0.062642	4.818719
308.256642	8000.455359	11.858266	-0.062633	4.818722
308.264429	8000.505824	11.863271	-0.062635	4.818737
308.736259	8000.468973	11.868275	-0.062722	4.818724
308.668007	8000.507955	11.873280	-0.062710	4.818736
308.491398	8000.404940	11.878285	-0.062677	4.818706
308.878558	8000.517010	11.883290	-0.062749	4.818738
308.754670	8000.493367	11.888295	-0.062726	4.818731
308.220551	8000.422406	11.893299	-0.062627	4.818712
308.739656	8000.501575	11.898304	-0.062724	4.818733
308.818657	8000.467991	11.903309	-0.062738	4.818723
309.070248	8000.383152	11.908314	-0.062785	4.818697
308.847132	8000.506143	11.913319	-0.062744	4.818734
308.627970	8000.509583	11.918323	-0.062703	4.818736
308.791124	8000.534800	11.923328	-0.062734	4.818743
308.927746	8000.490426	11.928333	-0.062759	4.818729
308.767907	8000.439037	11.933338	-0.062729	4.818715
308.752394	8000.492346	11.938343	-0.062727	4.818731
308.262842	8000.397837	11.943347	-0.062636	4.818704
308.773421	8000.517811	11.948352	-0.062731	4.818738
308.946129	8000.485450	11.953357	-0.062763	4.818728
308.718895	8000.542291	11.958362	-0.062721	4.818746
309.039305	8000.488776	11.963367	-0.062780	4.818728
308.671196	8000.524893	11.968371	-0.062712	4.818741
309.004641	8000.422239	11.973376	-0.062774	4.818709
309.023332	8000.441373	11.978381	-0.062778	4.818714
309.092161	8000.514669	11.983386	-0.062791	4.818736
308.594480	8000.519719	11.988391	-0.062698	4.818739
309.178985	8000.506371	11.993395	-0.062807	4.818733
309.024081	8000.504355	11.998400	-0.062778	4.818733
308.918102	8000.491437	12.003405	-0.062759	4.818730
308.819752	8000.409375	12.008410	-0.062740	4.818706
308.901680	8000.490185	12.013415	-0.062756	4.818729
308.933567	8000.518934	12.018419	-0.062762	4.818738
308.872947	8000.510804	12.023424	-0.062751	4.818736
308.604262	8000.411832	12.028429	-0.062701	4.818707
308.612448	8000.430829	12.033434	-0.062702	4.818713
308.943780	8000.512796	12.038439	-0.062764	4.818736
309.122746	8000.496253	12.043443	-0.062797	4.818730
309.093915	8000.387821	12.048448	-0.062792	4.818698
308.918887	8000.484161	12.053453	-0.062760	4.818728
309.094693	8000.494855	12.058458	-0.062792	4.818730
308.967586	8000.462777	12.063463	-0.062769	4.818721
308.964247	8000.503655	12.068467	-0.062768	4.818733
309.165660	8000.481111	12.073472	-0.062806	4.818726
309.157169	8000.436942	12.078477	-0.062804	4.818713
309.131929	8000.477535	12.083482	-0.062800	4.818725
309.034235	8000.462626	12.088487	-0.062782	4.818721
309.124166	8000.517313	12.093491	-0.062798	4.818737
309.212392	8000.490143	12.098496	-0.062815	4.818728
309.160669	8000.447508	12.103501	-0.062805	4.818716
309.408560	8000.499011	12.108506	-0.062852	4.818730
309.362460	8000.481628	12.113511	-0.062843	4.818725
308.985749	8000.423210	12.118515	-0.062773	4.818709
308.827168	8000.498783	12.123520	-0.062744	4.818732
308.911156	8000.499885	12.128525	-0.062759	4.818732
309.000136	8000.549313	12.133530	-0.062776	4.818747
309.171346	8000.450835	12.138535	-0.062808	4.818717
309.290977	8000.448206	12.143539	-0.062830	4.818715
309.216433	8000.480812	12.148544	-0.062817	4.818725
308.981783	8000.493492	12.153549	-0.062773	4.818730
309.260454	8000.411105	12.158554	-0.062825	4.818704
309.121630	8000.485886	12.163559	-0.062799	4.818727
308.762207	8000.510577	12.168563	-0.062732	4.818736
308.770347	8000.520131	12.173568	-0.062734	4.818739
308.737929	8000.508173	12.178573	-0.062728	4.818735
309.076173	8000.411876	12.183578	-0.062791	4.818705
308.906515	8000.500943	12.188583	-0.062759	4.818733
308.891218	8000.537469	12.193587	-0.062757	4.818743
309.026470	8000.428031	12.198592	-0.062782	4.818710
308.874547	8000.397727	12.203597	-0.062754	4.818702
308.790727	8000.491062	12.208602	-0.062738	4.818730
308.631279	8000.417646	12.213607	-0.062709	4.818709
308.888474	8000.528020	12.218611	-0.062757	4.818741
308.873065	8000.387240	12.223616	-0.062754	4.818699
308.922796	8000.527431	12.228621	-0.062763	4.818740
309.147429	8000.412864	12.233626	-0.062805	4.818705
309.161120	8000.498030	12.238631	-0.062808	4.818731
309.230878	8000.530421	12.243635	-0.062821	4.818740
309.167087	8000.522250	12.248640	-0.062809	4.818738
309.087132	8000.386921	12.253645	-0.062794	4.818698
309.101663	8000.531899	12.258650	-0.062797	4.818741
309.120965	8000.511174	12.263655	-0.062801	4.818735
309.155638	8000.500091	12.268659	-0.062807	4.818731
309.137768	8000.500913	12.273664	-0.062804	4.818732
309.105019	8000.463771	12.278669	-0.062798	4.818721
309.120127	8000.518530	12.283674	-0.062801	4.818737
308.927264	8000.411104	12.288679	-0.062765	4.818706
308.978622	8000.528235	12.293683	-0.062775	4.818740
309.075374	8000.512717	12.298688	-0.062793	4.818735
308.734753	8000.532407	12.303693	-0.062729	4.818743
309.095739	8000.435358	12.308698	-0.062797	4.818712
308.876568	8000.509091	12.313703	-0.062756	4.818735
308.992624	8000.494874	12.318707	-0.062778	4.818730
309.019329	8000.372479	12.323712	-0.062783	4.818694
308.754681	8000.527451	12.328717	-0.062734	4.818741
309.056044	8000.511457	12.333722	-0.062790	4.818735
308.536558	8000.496289	12.338727	-0.062693	4.818733
308.921217	8000.491873	12.343731	-0.062765	4.818730
308.481427	8000.311984	12.348736	-0.062683	4.818678
308.724405	8000.420073	12.353741	-0.062728	4.818709
309.072942	8000.519050	12.358746	-0.062793	4.818737
308.668199	8000.505380	12.363751	-0.062718	4.818735
308.978455	8000.508386	12.368755	-0.062776	4.818734
308.660952	8000.427661	12.373760	-0.062717	4.818712
308.573463	8000.513603	12.378765	-0.062701	4.818738
309.034054	8000.514375	12.383770	-0.062786	4.818736
309.112550	8000.497570	12.388775	-0.062801	4.818731
309.097271	8000.521507	12.393779	-0.062798	4.818738
309.299567	8000.493728	12.398784	-0.062836	4.818729
309.203574	8000.389665	12.403789	-0.062818	4.818698
309.463523	8000.476996	12.408794	-0.062867	4.818723
309.512887	8000.452466	12.413799	-0.062876	4.818716
309.095643	8000.515220	12.418803	-0.062799	4.818736
309.294749	8000.530415	12.423808	-0.062836	4.818740
308.922367	8000.507724	12.428813	-0.062766	4.818734
308.650348	8000.343662	12.433818	-0.062716	4.818687
308.322811	8000.434865	12.438823	-0.062655	4.818715
308.266065	8000.337611	12.443827	-0.062644	4.818686
308.503734	8000.458220	12.448832	-0.062689	4.818721
308.357425	8000.433235	12.453837	-0.062662	4.818714
308.577535	8000.458145	12.458842	-0.062703	4.818721
308.784140	8000.516452	12.463847	-0.062741	4.818738
309.055221	8000.522094	12.468851	-0.062792	4.818738
309.033259	8000.501880	12.473856	-0.062788	4.818732
308.896857	8000.430862	12.478861	-0.062762	4.818712
309.266901	8000.522777	12.483866	-0.062832	4.818738
308.848752	8000.492145	12.488871	-0.062754	4.818730
309.224392	8000.497054	12.493875	-0.062824	4.818730
309.364966	8000.498895	12.498880	-0.062850	4.818730
309.341957	8000.486011	12.503885	-0.062846	4.818726
309.200016	8000.410723	12.508890	-0.062819	4.818704
309.317729	8000.499345	12.513895	-0.062841	4.818730
308.911863	8000.529723	12.518899	-0.062766	4.818741
308.389698	8000.306794	12.523904	-0.062669	4.818677
308.736231	8000.551573	12.528909	-0.062733	4.818748
308.791999	8000.456835	12.533914	-0.062744	4.818720
309.257680	8000.477607	12.538919	-0.062831	4.818724
308.991178	8000.391252	12.543923	-0.062781	4.818699
309.226193	8000.513928	12.548928	-0.062825	4.818735
308.958194	8000.518828	12.553933	-0.062775	4.818738
309.193470	8000.409647	12.558938	-0.062819	4.818704
309.190720	8000.484106	12.563943	-0.062819	4.818726
309.254936	8000.520621	12.568947	-0.062831	4.818737
309.377713	8000.509640	12.573952	-0.062854	4.818733
309.433651	8000.493590	12.578957	-0.062864	4.818728
309.407593	8000.513190	12.583962	-0.062859	4.818734
309.132474	8000.501210	12.588967	-0.062808	4.818732
308.899404	8000.421586	12.593971	-0.062765	4.818709
309.025226	8000.551230	12.598976	-0.062788	4.818747
309.069954	8000.519296	12.603981	-0.062797	4.818737
308.751698	8000.429118	12.608986	-0.062738	4.818712
308.946135	8000.520839	12.613991	-0.062774	4.818738
309.051250	8000.414155	12.618995	-0.062794	4.818706
309.381194	8000.518137	12.624000	-0.062855	4.818736
309.162501	8000.470174	12.629005	-0.062814	4.818722
309.125858	8000.512717	12.634010	-0.062808	4.818735
309.204370	8000.499060	12.639015	-0.062822	4.818731
309.263616	8000.495642	12.644019	-0.062834	4.818729
309.011647	8000.411575	12.649024	-0.062787	4.818705
309.149235	8000.480522	12.654029	-0.062812	4.818725
309.116077	8000.537798	12.659034	-0.062806	4.818743
309.304704	8000.380795	12.664039	-0.062841	4.818695
309.362304	8000.495911	12.669043	-0.062852	4.818729
308.613325	8000.434732	12.674048	-0.062713	4.818714
308.580725	8000.444804	12.679053	-0.062707	4.818717
309.018857	8000.454724	12.684058	-0.062789	4.818718
308.953742	8000.390932	12.689063	-0.062777	4.818699
309.068837	8000.501551	12.694067	-0.062798	4.818732
308.926576	8000.510191	12.699072	-0.062772	4.818735
308.649874	8000.396426	12.704077	-0.062720	4.818702
308.368590	8000.424235	12.709082	-0.062668	4.818712
308.489592	8000.381757	12.714087	-0.062690	4.818699
309.135807	8000.544420	12.719091	-0.062811	4.818744
309.162690	8000.505958	12.724096	-0.062816	4.818733
308.688982	8000.435783	12.729101	-0.062728	4.818714
309.050768	8000.446806	12.734106	-0.062795	4.818716
308.729618	8000.449964	12.739111	-0.062736	4.818718
308.660377	8000.419690	12.744115	-0.062723	4.818709
308.931003	8000.450506	12.749120	-0.062773	4.818717
308.952363	8000.478068	12.754125	-0.062777	4.818725
309.348159	8000.517863	12.759130	-0.062851	4.818736
309.086361	8000.472485	12.764135	-0.062802	4.818723
308.946594	8000.397226	12.769139	-0.062777	4.818701
309.132156	8000.517159	12.774144	-0.062811	4.818736
309.391870	8000.454458	12.779149	-0.062860	4.818717
309.341979	8000.509418	12.784154	-0.062850	4.818733
309.306515	8000.499518	12.789159	-0.062844	4.818730
309.628928	8000.510029	12.794163	-0.062904	4.818732
309.469885	8000.395698	12.799168	-0.062874	4.818699
309.117000	8000.528536	12.804173	-0.062809	4.818740
309.448575	8000.443693	12.809178	-0.062871	4.818713
309.011291	8000.528217	12.814183	-0.062789	4.818740
308.703513	8000.430832	12.819187	-0.062732	4.818712
309.384057	8000.418737	12.824192	-0.062859	4.818706
309.205054	8000.498240	12.829197	-0.062826	4.818730
308.999398	8000.437858	12.834202	-0.062787	4.818713
309.116523	8000.507588	12.839207	-0.062809	4.818733
308.912147	8000.440928	12.844211	-0.062771	4.818714
308.933793	8000.439118	12.849216	-0.062775	4.818714
309.037843	8000.419499	12.854221	-0.062795	4.818708
309.414486	8000.527238	12.859226	-0.062865	4.818738
309.331792	8000.455871	12.864231	-0.062850	4.818717
309.492522	8000.499942	12.869235	-0.062880	4.818730
309.488888	8000.505146	12.874240	-0.062879	4.818731
309.252538	8000.502066	12.879245	-0.062835	4.818731
309.456007	8000.445975	12.884250	-0.062873	4.818714
309.307646	8000.513288	12.889255	-0.062846	4.818734
309.123288	8000.431152	12.894259	-0.062812	4.818711
309.131697	8000.491069	12.899264	-0.062813	4.818728
309.436135	8000.449936	12.904269	-0.062870	4.818715
309.161609	8000.522946	12.909274	-0.062819	4.818738
308.979716	8000.537363	12.914279	-0.062785	4.818743
309.620039	8000.399896	12.919283	-0.062904	4.818699
308.951199	8000.496086	12.924288	-0.062780	4.818731
308.511545	8000.396981	12.929293	-0.062698	4.818703
308.744125	8000.429397	12.934298	-0.062742	4.818712
309.051562	8000.519446	12.939303	-0.062799	4.818737
309.041574	8000.423849	12.944307	-0.062797	4.818709
309.028115	8000.511807	12.949312	-0.062795	4.818735
309.238863	8000.456861	12.954317	-0.062834	4.818718
309.298615	8000.511154	12.959322	-0.062845	4.818734
309.545963	8000.486062	12.964327	-0.062891	4.818725
309.286345	8000.483727	12.969331	-0.062843	4.818726
308.962025	8000.427042	12.974336	-0.062783	4.818710
309.161112	8000.492595	12.979341	-0.062820	4.818729
309.606373	8000.479530	12.984346	-0.062903	4.818723
309.210396	8000.424006	12.989351	-0.062829	4.818708
309.206019	8000.506838	12.994355	-0.062829	4.818733
308.889250	8000.440809	12.999360	-0.062770	4.818714
308.644457	8000.387262	13.004365	-0.062724	4.818699
309.210001	8000.454450	13.009370	-0.062830	4.818717
309.200689	8000.502595	13.014375	-0.062828	4.818732
308.918280	8000.432818	13.019379	-0.062775	4.818712
309.246684	8000.505305	13.024384	-0.062837	4.818732
309.298818	8000.482911	13.029389	-0.062846	4.818725
309.472522	8000.510364	13.034394	-0.062879	4.818733
309.132981	8000.401022	13.039399	-0.062816	4.818702
309.341650	8000.535945	13.044403	-0.062855	4.818741
309.162166	8000.528362	13.049408	-0.062821	4.818739
308.945760	8000.425874	13.054413	-0.062781	4.818710
309.121846	8000.438669	13.059418	-0.062814	4.818713
308.858419	8000.537004	13.064423	-0.062765	4.818743
308.969789	8000.416762	13.069427	-0.062786	4.818707
308.978755	8000.459900	13.074432	-0.062788	4.818720
309.192200	8000.435414	13.079437	-0.062827	4.818712
308.835321	8000.444401	13.084442	-0.062761	4.818716
308.963489	8000.510077	13.089447	-0.062785	4.818735
308.496395	8000.339273	13.094451	-0.062698	4.818686
308.719884	8000.416683	13.099456	-0.062740	4.818708
309.029138	8000.436462	13.104461	-0.062797	4.818713
309.197232	8000.524693	13.109466	-0.062829	4.818738
308.922390	8000.396262	13.114471	-0.062778	4.818701
308.853079	8000.438378	13.119475	-0.062765	4.818714
309.073381	8000.543027	13.124480	-0.062806	4.818744
309.107574	8000.407090	13.129485	-0.062812	4.818704
308.809002	8000.418936	13.134490	-0.062757	4.818708
309.382752	8000.514560	13.139495	-0.062864	4.818734
309.171933	8000.522305	13.144499	-0.062825	4.818738
309.208545	8000.413677	13.149504	-0.062832	4.818705
309.172155	8000.488746	13.154509	-0.062825	4.818728
309.080505	8000.521129	13.159514	-0.062808	4.818738
308.912482	8000.442353	13.164519	-0.062777	4.818715
309.176019	8000.410128	13.169523	-0.062826	4.818704
309.307587	8000.499980	13.174528	-0.062851	4.818730
309.006902	8000.471930	13.179533	-0.062795	4.818723
309.087624	8000.545381	13.184538	-0.062810	4.818745
309.104494	8000.418660	13.189543	-0.062813	4.818707
309.079413	8000.428830	13.194547	-0.062808	4.818710
308.707722	8000.440771	13.199552	-0.062739	4.818715
308.435056	8000.349092	13.204557	-0.062688	4.818689
308.585053	8000.450722	13.209562	-0.062717	4.818719
308.849505	8000.448933	13.214567	-0.062766	4.818717
308.357318	8000.343898	13.219571	-0.062674	4.818688
308.647502	8000.445260	13.224576	-0.062728	4.818717
308.880054	8000.395843	13.229581	-0.062772	4.818701
308.901055	8000.533561	13.234586	-0.062776	4.818742
308.894272	8000.398139	13.239591	-0.062775	4.818702
308.875205	8000.516449	13.244595	-0.062771	4.818737
309.277219	8000.411542	13.249600	-0.062846	4.818704
308.801407	8000.508153	13.254605	-0.062758	4.818735
308.671701	8000.395258	13.259610	-0.062733	4.818702
308.728512	8000.406496	13.264615	-0.062744	4.818705
308.777302	8000.516249	13.269619	-0.062753	4.818737
308.598384	8000.466709	13.274624	-0.062720	4.818723
308.380691	8000.432400	13.279629	-0.062680	4.818714
308.714727	8000.437814	13.284634	-0.062742	4.818714
308.878252	8000.536475	13.289639	-0.062772	4.818743
308.882199	8000.404340	13.294643	-0.062773	4.818704
308.935374	8000.496315	13.299648	-0.062783	4.818731
308.586645	8000.489671	13.304653	-0.062718	4.818730
308.879831	8000.422162	13.309658	-0.062773	4.818709
308.921538	8000.497201	13.314663	-0.062781	4.818731
308.761486	8000.514003	13.319667	-0.062751	4.818737
308.757846	8000.423735	13.324672	-0.062751	4.818710
308.634962	8000.405351	13.329677	-0.062728	4.818705
309.020580	8000.516353	13.334682	-0.062800	4.818736
308.515102	8000.398553	13.339687	-0.062706	4.818703
309.029709	8000.490255	13.344691	-0.062802	4.818728
308.831217	8000.434164	13.349696	-0.062765	4.818713
308.439942	8000.442702	13.354701	-0.062692	4.818717
308.681766	8000.318919	13.359706	-0.062737	4.818679
308.855579	8000.517382	13.364711	-0.062770	4.818737
308.908381	8000.408966	13.369715	-0.062779	4.818705
309.037379	8000.507177	13.374720	-0.062804	4.818733
308.953464	8000.492448	13.379725	-0.062788	4.818729
309.062918	8000.523259	13.384730	-0.062808	4.818738
309.072418	8000.496111	13.389735	-0.062810	4.818730
309.208291	8000.486350	13.394739	-0.062836	4.818727
309.124680	8000.414971	13.399744	-0.062820	4.818706
309.079956	8000.498325	13.404749	-0.062812	4.818731
309.282572	8000.498878	13.409754	-0.062850	4.818730
309.071168	8000.494025	13.414759	-0.062810	4.818729
308.957890	8000.418063	13.419763	-0.062789	4.818707
308.984683	8000.427861	13.424768	-0.062794	4.818710
308.823053	8000.408971	13.429773	-0.062764	4.818705
309.170670	8000.523675	13.434778	-0.062829	4.818738
309.448413	8000.489537	13.439783	-0.062881	4.818727
309.427640	8000.496616	13.444787	-0.062877	4.818729
309.569713	8000.534148	13.449792	-0.062904	4.818739
309.276120	8000.403373	13.454797	-0.062849	4.818702
309.764405	8000.470605	13.459802	-0.062940	4.818720
309.726434	8000.458574	13.464807	-0.062933	4.818716
309.452852	8000.493827	13.469811	-0.062882	4.818728
309.445769	8000.511576	13.474816	-0.062881	4.818733
309.108231	8000.473602	13.479821	-0.062818	4.818723
309.005374	8000.414562	13.484826	-0.062799	4.818706
309.055903	8000.506503	13.489831	-0.062809	4.818733
309.407741	8000.448153	13.494835	-0.062874	4.818714
309.627478	8000.497191	13.499840	-0.062915	4.818728
309.547783	8000.392289	13.504845	-0.062901	4.818697
309.622987	8000.485603	13.509850	-0.062915	4.818725
309.510965	8000.499884	13.514855	-0.062894	4.818729
309.177345	8000.510222	13.519859	-0.062832	4.818734
309.545221	8000.518178	13.524864	-0.062901	4.818735
309.510022	8000.507233	13.529869	-0.062894	4.818732
309.824372	8000.500852	13.534874	-0.062953	4.818728
309.503264	8000.402240	13.539879	-0.062893	4.818700
309.118201	8000.529412	13.544883	-0.062821	4.818740
309.467201	8000.510894	13.549888	-0.062886	4.818733
309.726141	8000.459724	13.554893	-0.062935	4.818717
309.574014	8000.502858	13.559898	-0.062907	4.818730
309.594186	8000.510471	13.564903	-0.062910	4.818732
309.560361	8000.436594	13.569907	-0.062904	4.818710
309.547939	8000.489945	13.574912	-0.062902	4.818726
309.520676	8000.502184	13.579917	-0.062897	4.818730
309.260011	8000.440034	13.584922	-0.062848	4.818713
309.346519	8000.521954	13.589927	-0.062865	4.818737
309.409860	8000.411577	13.594931	-0.062876	4.818704
309.373647	8000.555893	13.599936	-0.062870	4.818747
309.351206	8000.425511	13.604941	-0.062866	4.818708
309.327298	8000.519628	13.609946	-0.062861	4.818736
309.371479	8000.486638	13.614951	-0.062870	4.818726
309.138514	8000.519273	13.619955	-0.062826	4.818737
309.136036	8000.344039	13.624960	-0.062826	4.818684
308.768732	8000.434723	13.629965	-0.062758	4.818713
308.750938	8000.451283	13.634970	-0.062754	4.818718
308.956968	8000.404668	13.639975	-0.062793	4.818703
308.911500	8000.513191	13.644979	-0.062785	4.818736
309.087975	8000.452552	13.649984	-0.062817	4.818717
309.239159	8000.461875	13.654989	-0.062846	4.818719
309.161957	8000.528019	13.659994	-0.062831	4.818739
309.293210	8000.498264	13.664999	-0.062856	4.818730
309.490671	8000.474619	13.670003	-0.062893	4.818722
309.060713	8000.419702	13.675008	-0.062813	4.818707
308.897890	8000.419680	13.680013	-0.062783	4.818708
309.045538	8000.548561	13.685018	-0.062810	4.818746
309.045303	8000.443648	13.690023	-0.062810	4.818714
308.408710	8000.346170	13.695027	-0.062692	4.818688
308.864372	8000.527328	13.700032	-0.062777	4.818740
308.821209	8000.389333	13.705037	-0.062769	4.818699
308.937010	8000.537730	13.710042	-0.062790	4.818743
308.885271	8000.424802	13.715047	-0.062781	4.818709
309.173621	8000.511455	13.720051	-0.062835	4.818734
308.688390	8000.454768	13.725056	-0.062744	4.818719
308.186409	8000.348556	13.730061	-0.062651	4.818689
308.854666	8000.336298	13.735066	-0.062775	4.818683
308.918237	8000.527029	13.740071	-0.062787	4.818740
308.907195	8000.448204	13.745075	-0.062785	4.818716
309.212961	8000.446956	13.750080	-0.062842	4.818715
309.085721	8000.385499	13.755085	-0.062819	4.818697
309.360527	8000.531777	13.760090	-0.062870	4.818739
309.340925	8000.428710	13.765095	-0.062866	4.818709
309.517859	8000.521253	13.770099	-0.062900	4.818736
309.566534	8000.476781	13.775104	-0.062909	4.818722
309.322752	8000.500882	13.780109	-0.062863	4.818730
309.444889	8000.425894	13.785114	-0.062886	4.818708
309.316011	8000.488215	13.790119	-0.062862	4.818727
309.013866	8000.503161	13.795123	-0.062806	4.818732
309.143759	8000.502765	13.800128	-0.062830	4.818732
309.168831	8000.472672	13.805133	-0.062835	4.818723
309.119971	8000.495122	13.810138	-0.062826	4.818729
309.436771	8000.469887	13.815143	-0.062885	4.818721
309.397783	8000.478826	13.820147	-0.062878	4.818723
309.614258	8000.434447	13.825152	-0.062918	4.818709
309.331519	8000.526234	13.830157	-0.062866	4.818738
309.269846	8000.339735	13.835162	-0.062854	4.818683
309.443905	8000.535057	13.840167	-0.062887	4.818740
309.290370	8000.404012	13.845171	-0.062858	4.818702
309.257819	8000.527393	13.850176	-0.062852	4.818738
309.338477	8000.431930	13.855181	-0.062867	4.818710
309.804533	8000.412841	13.860186	-0.062954	4.818702
309.681576	8000.535043	13.865191	-0.062932	4.818739
309.708123	8000.502871	13.870195	-0.062937	4.818729
309.831981	8000.527576	13.875200	-0.062960	4.818736
309.491035	8000.505294	13.880205	-0.062896	4.818731
309.685094	8000.533014	13.885210	-0.062933	4.818738
309.670928	8000.418476	13.890215	-0.062930	4.818704
309.581138	8000.503340	13.895219	-0.062913	4.818730
309.619773	8000.535326	13.900224	-0.062921	4.818739
309.533562	8000.525812	13.905229	-0.062905	4.818737
309.610615	8000.419810	13.910234	-0.062919	4.818705
309.546942	8000.482983	13.915239	-0.062907	4.818724
309.671953	8000.522391	13.920243	-0.062931	4.818735
309.204420	8000.506850	13.925248	-0.062844	4.818733
309.039138	8000.505747	13.930253	-0.062813	4.818733
308.868277	8000.444770	13.935258	-0.062781	4.818715
308.890960	8000.453465	13.940263	-0.062786	4.818718
309.204750	8000.405109	13.945267	-0.062844	4.818702
308.819244	8000.411624	13.950272	-0.062772	4.818706
309.100451	8000.518117	13.955277	-0.062825	4.818736
309.090487	8000.430913	13.960282	-0.062823	4.818710
309.214655	8000.509128	13.965287	-0.062846	4.818733
309.397056	8000.476893	13.970291	-0.062880	4.818723
309.731533	8000.528479	13.975296	-0.062943	4.818737
309.744298	8000.466751	13.980301	-0.062945	4.818719
309.347917	8000.407025	13.985306	-0.062871	4.818702
309.462690	8000.512396	13.990311	-0.062893	4.818733
309.603185	8000.514236	13.995315	-0.062919	4.818733
309.448781	8000.548946	14.000320	-0.062891	4.818744
308.985082	8000.455818	14.005325	-0.062804	4.818718
308.933678	8000.434170	14.010330	-0.062795	4.818712
308.869612	8000.444880	14.015335	-0.062783	4.818715
308.932468	8000.405839	14.020339	-0.062795	4.818704
309.240843	8000.489606	14.025344	-0.062852	4.818727
309.088124	8000.477126	14.030349	-0.062824	4.818724
309.341804	8000.499329	14.035354	-0.062871	4.818730
309.569820	8000.503361	14.040359	-0.062914	4.818730
309.335484	8000.411129	14.045363	-0.062870	4.818704
309.155642	8000.543078	14.050368	-0.062837	4.818743
309.064280	8000.410748	14.055373	-0.062820	4.818704
308.802771	8000.432520	14.060378	-0.062771	4.818712
308.747716	8000.376203	14.065383	-0.062761	4.818695
309.025903	8000.484754	14.070387	-0.062813	4.818727
308.869653	8000.500555	14.075392	-0.062784	4.818732
308.793382	8000.442912	14.080397	-0.062770	4.818715
308.755775	8000.349054	14.085402	-0.062763	4.818687
308.703284	8000.406077	14.090407	-0.062753	4.818704
308.819559	8000.419141	14.095411	-0.062775	4.818708
308.736536	8000.411768	14.100416	-0.062759	4.818706
308.235457	8000.309765	14.105421	-0.062666	4.818678
308.643235	8000.339221	14.110426	-0.062742	4.818685
309.029658	8000.452331	14.115431	-0.062814	4.818717
308.588019	8000.336414	14.120435	-0.062732	4.818684
308.741837	8000.334230	14.125440	-0.062761	4.818683
308.851264	8000.529755	14.130445	-0.062781	4.818741
309.210228	8000.419041	14.135450	-0.062848	4.818706
309.061719	8000.498942	14.140455	-0.062821	4.818731
308.402550	8000.324581	14.145459	-0.062698	4.818681
308.298969	8000.307499	14.150464	-0.062679	4.818677
308.179726	8000.453875	14.155469	-0.062657	4.818721
308.857937	8000.427061	14.160474	-0.062783	4.818710
309.032671	8000.414660	14.165479	-0.062816	4.818706
309.316300	8000.532726	14.170483	-0.062869	4.818740
309.550344	8000.513755	14.175488	-0.062912	4.818733
309.415841	8000.401843	14.180493	-0.062887	4.818700
309.182511	8000.516308	14.185498	-0.062844	4.818735
309.238555	8000.529636	14.190503	-0.062855	4.818739
309.238749	8000.421581	14.195507	-0.062855	4.818707
309.327045	8000.539196	14.200512	-0.062871	4.818742
308.462275	8000.431392	14.205517	-0.062710	4.818713
308.559949	8000.212355	14.210522	-0.062728	4.818647
308.632640	8000.282552	14.215527	-0.062742	4.818668
308.668974	8000.433058	14.220531	-0.062749	4.818713
308.783443	8000.303415	14.225536	-0.062770	4.818674
308.806242	8000.466335	14.230541	-0.062775	4.818722
308.656060	8000.335337	14.235546	-0.062747	4.818684
308.895841	8000.428698	14.240551	-0.062791	4.818710
308.696299	8000.350562	14.245555	-0.062754	4.818688
308.617066	8000.315961	14.250560	-0.062740	4.818678
308.648998	8000.451722	14.255565	-0.062746	4.818718
309.158440	8000.424805	14.260570	-0.062841	4.818708
309.225218	8000.507516	14.265575	-0.062853	4.818733
308.967608	8000.403441	14.270579	-0.062805	4.818703
309.113078	8000.428427	14.275584	-0.062832	4.818709
308.839533	8000.453189	14.280589	-0.062782	4.818718
308.902750	8000.445627	14.285594	-0.062794	4.818715
309.161500	8000.403897	14.290599	-0.062842	4.818702
308.620527	8000.419923	14.295603	-0.062741	4.818709
308.189466	8000.163565	14.300608	-0.062661	4.818634
308.385839	8000.263700	14.305613	-0.062697	4.818663
308.392180	8000.226020	14.310618	-0.062699	4.818652
309.027489	8000.323491	14.315623	-0.062817	4.818679
308.940725	8000.337052	14.320627	-0.062801	4.818683
309.303295	8000.543228	14.325632	-0.062869	4.818743
309.008099	8000.429219	14.330637	-0.062814	4.818710
309.092149	8000.517401	14.335642	-0.062830	4.818736
308.997223	8000.422793	14.340647	-0.062812	4.818708
309.124555	8000.420265	14.345651	-0.062836	4.818707
309.136861	8000.542133	14.350656	-0.062838	4.818743
308.761077	8000.346289	14.355661	-0.062768	4.818686
308.858384	8000.404218	14.360666	-0.062786	4.818703
308.693322	8000.325483	14.365671	-0.062756	4.818680
308.878914	8000.496823	14.370675	-0.062791	4.818731
308.870943	8000.446365	14.375680	-0.062789	4.818716
309.239873	8000.512038	14.380685	-0.062858	4.818734
309.333754	8000.313931	14.385690	-0.062875	4.818674
309.594628	8000.526125	14.390695	-0.062924	4.818737
309.160754	8000.444926	14.395699	-0.062843	4.818714
309.373135	8000.522195	14.400704	-0.062883	4.818736
309.546285	8000.498233	14.405709	-0.062915	4.818728
309.624957	8000.521298	14.410714	-0.062930	4.818735
309.158444	8000.386167	14.415719	-0.062843	4.818697
309.101406	8000.447328	14.420723	-0.062833	4.818715
309.601312	8000.525204	14.425728	-0.062926	4.818736
309.557862	8000.469036	14.430733	-0.062918	4.818720
309.598568	8000.515737	14.435738	-0.062926	4.818733
309.722371	7999.336037	14.440743	-0.062948	4.818382

309.373463	7996.244337	14.445747	-0.062881	4.817463
309.381952	7990.719877	14.450752	-0.062879	4.815818
309.324113	7984.003699	14.455757	-0.062864	4.813819
309.210464	7976.825538	14.460762	-0.062838	4.811680
309.194142	7969.153376	14.465767	-0.062830	4.809393
308.953739	7961.445531	14.470771	-0.062781	4.807096
309.191880	7953.511801	14.475776	-0.062820	4.804728
309.471769	7945.536384	14.480781	-0.062867	4.802346
309.425189	7937.594502	14.485786	-0.062853	4.799974
309.435436	7929.621702	14.490791	-0.062850	4.797592
308.911564	7921.622900	14.495795	-0.062747	4.795202
308.897573	7913.658923	14.500800	-0.062740	4.792820
308.956800	7905.569335	14.505805	-0.062745	4.790399
309.198040	7897.528486	14.510810	-0.062785	4.787990
309.198573	7889.576624	14.515815	-0.062780	4.785608
309.381473	7881.527487	14.520819	-0.062809	4.783195
309.143437	7873.637401	14.525824	-0.062760	4.780830
308.612408	7865.617365	14.530829	-0.062656	4.778426
308.856631	7857.622535	14.535834	-0.062696	4.776025
308.719773	7849.605193	14.540839	-0.062665	4.773618
308.507762	7841.577759	14.545843	-0.062621	4.771206
308.505234	7833.564668	14.550848	-0.062615	4.768797
308.309136	7825.541476	14.555853	-0.062573	4.766385
308.126144	7817.516320	14.560858	-0.062534	4.763970
308.750828	7809.578834	14.565863	-0.062645	4.761579
309.073741	7801.444717	14.570867	-0.062700	4.759128
308.801308	7793.561538	14.575872	-0.062645	4.756752
308.824100	7785.440446	14.580877	-0.062644	4.754303
308.927730	7777.583831	14.585882	-0.062658	4.751933
308.765008	7769.553329	14.590887	-0.062622	4.749509
308.506503	7761.515966	14.595891	-0.062569	4.747083
308.403893	7753.578957	14.600896	-0.062545	4.744685
308.370579	7745.537046	14.605901	-0.062534	4.742253
308.413867	7737.502889	14.610906	-0.062537	4.739823
308.420805	7729.532428	14.615911	-0.062533	4.737411
308.451579	7721.503300	14.620915	-0.062533	4.734980
308.605565	7713.503773	14.625920	-0.062557	4.732557
308.421652	7705.494966	14.630925	-0.062517	4.730129
308.651783	7697.514333	14.635930	-0.062555	4.727709
308.569346	7689.517461	14.640935	-0.062535	4.725283
308.807012	7681.517191	14.645939	-0.062574	4.722854
308.548291	7673.579034	14.650944	-0.062521	4.720443
308.620348	7665.521364	14.655949	-0.062529	4.717995
308.387010	7657.569067	14.660954	-0.062480	4.715578
308.619240	7649.550217	14.665959	-0.062518	4.713138
308.379878	7641.514919	14.670963	-0.062469	4.710693
308.217506	7633.564166	14.675968	-0.062433	4.708272
308.472577	7625.449169	14.680973	-0.062476	4.705799
308.359308	7617.533552	14.685978	-0.062449	4.703387
308.412089	7609.564309	14.690983	-0.062454	4.700956
308.422040	7601.503901	14.695987	-0.062451	4.698497
308.353191	7593.561970	14.700992	-0.062433	4.696072
308.154232	7585.510360	14.705997	-0.062391	4.693613
308.022494	7577.534735	14.711002	-0.062361	4.691176
308.127181	7569.481254	14.716007	-0.062375	4.688713
308.256327	7561.490183	14.721011	-0.062394	4.686268
308.189254	7553.482409	14.726016	-0.062377	4.683817
307.887754	7545.588449	14.731021	-0.062315	4.681400
308.421213	7537.494475	14.736026	-0.062410	4.678919
308.115825	7529.595623	14.741031	-0.062348	4.676498
307.942388	7521.452901	14.746035	-0.062310	4.674000
308.061320	7513.468543	14.751040	-0.062327	4.671550
307.929934	7505.414883	14.756045	-0.062298	4.669077
307.963222	7497.468303	14.761050	-0.062299	4.666635
307.914855	7489.423265	14.766055	-0.062284	4.664162
307.958845	7481.532765	14.771059	-0.062288	4.661736
308.249572	7473.447633	14.776064	-0.062337	4.659248
307.814714	7465.541006	14.781069	-0.062251	4.656814
308.027403	7457.423827	14.786074	-0.062285	4.654313
308.027099	7449.501383	14.791079	-0.062280	4.651871
308.090989	7441.374570	14.796083	-0.062286	4.649365
307.919111	7433.542615	14.801088	-0.062249	4.646949
307.932113	7425.486142	14.806093	-0.062247	4.644462
307.931682	7417.502719	14.811098	-0.062241	4.641996
307.695363	7409.444050	14.816103	-0.062192	4.639506
307.871346	7401.454828	14.821107	-0.062220	4.637036
308.068928	7393.432438	14.826112	-0.062252	4.634554
307.800789	7385.445381	14.831117	-0.062197	4.632082
308.060036	7377.387052	14.836122	-0.062240	4.629586
307.685951	7369.482454	14.841127	-0.062165	4.627137
307.459840	7361.418742	14.846131	-0.062118	4.624637
307.132552	7353.504646	14.851136	-0.062052	4.622182
307.324399	7345.421466	14.856141	-0.062082	4.619673
307.539638	7337.444058	14.861146	-0.062117	4.617196
307.307381	7329.415020	14.866151	-0.062069	4.614701
307.126405	7321.472581	14.871155	-0.062030	4.612232
306.958389	7313.450134	14.876160	-0.061994	4.609737
306.686192	7305.499694	14.881165	-0.061938	4.607262
306.743417	7297.405984	14.886170	-0.061943	4.604742
306.829955	7289.477866	14.891175	-0.061954	4.602272
306.357974	7281.436254	14.896179	-0.061861	4.599765
306.836630	7273.430922	14.901184	-0.061945	4.597269
306.903546	7265.352695	14.906189	-0.061952	4.594748
306.920980	7257.370097	14.911194	-0.061951	4.592256
306.595262	7249.381604	14.916199	-0.061885	4.589760
306.450998	7241.339708	14.921203	-0.061853	4.587246
306.671921	7233.355161	14.926208	-0.061889	4.584749
306.847483	7225.381129	14.931213	-0.061916	4.582255
306.807002	7217.350845	14.936218	-0.061904	4.579740
306.954415	7209.410536	14.941223	-0.061926	4.577253
306.936504	7201.354039	14.946227	-0.061918	4.574728
306.535571	7193.477669	14.951232	-0.061838	4.572258
306.764227	7185.326968	14.956237	-0.061875	4.569701
306.975155	7177.353858	14.961242	-0.061909	4.567198
307.232181	7169.301251	14.966247	-0.061952	4.564669
307.335935	7161.349466	14.971251	-0.061966	4.562170
307.423075	7153.346545	14.976256	-0.061977	4.559654
306.907318	7145.431983	14.981261	-0.061876	4.557163
307.289979	7137.330508	14.986266	-0.061942	4.554613
307.186107	7129.394888	14.991271	-0.061918	4.552114
306.744834	7121.300070	14.996275	-0.061831	4.549561
306.963918	7113.361796	15.001280	-0.061866	4.547059
306.746184	7105.337596	15.006285	-0.061821	4.544526
306.421245	7097.433595	15.011290	-0.061755	4.542030
306.876029	7089.280021	15.016295	-0.061834	4.539456
306.863548	7081.318888	15.021299	-0.061827	4.536940
306.579850	7073.360781	15.026304	-0.061769	4.534423
306.365035	7065.348351	15.031309	-0.061724	4.531887
306.417977	7057.265907	15.036314	-0.061729	4.529329
306.859688	7049.299431	15.041319	-0.061806	4.526807
306.617217	7041.269334	15.046323	-0.061755	4.524261
306.306516	7033.459139	15.051328	-0.061693	4.521784
306.728142	7025.295422	15.056333	-0.061766	4.519195
306.532246	7017.349323	15.061338	-0.061724	4.516672
305.804675	7009.367381	15.066343	-0.061584	4.514134
305.775085	7001.339243	15.071347	-0.061573	4.511582
305.507376	6993.334068	15.076352	-0.061518	4.509035
305.443548	6985.289981	15.081357	-0.061501	4.506476
306.001227	6977.214786	15.086362	-0.061600	4.503907
306.000490	6969.296628	15.091367	-0.061594	4.501385
305.953645	6961.213083	15.096371	-0.061581	4.498808
305.735565	6953.302680	15.101376	-0.061535	4.496285
305.846813	6945.238152	15.106381	-0.061550	4.493712
306.269538	6937.262239	15.111386	-0.061624	4.491167
306.088238	6929.247659	15.116391	-0.061585	4.488606
305.558839	6921.278412	15.121395	-0.061481	4.486057
305.641929	6913.272607	15.126400	-0.061492	4.483497
305.841455	6905.323428	15.131405	-0.061524	4.480954
305.516885	6897.291289	15.136410	-0.061458	4.478381
305.571418	6889.300546	15.141415	-0.061463	4.475821
305.662926	6881.209660	15.146419	-0.061475	4.473228
305.632256	6873.273088	15.151424	-0.061464	4.470682
304.899197	6865.294782	15.156429	-0.061323	4.468118
305.462806	6857.216860	15.161434	-0.061422	4.465527
304.867642	6849.272292	15.166439	-0.061307	4.462972
305.378008	6841.181946	15.171443	-0.061396	4.460373
305.629458	6833.210671	15.176448	-0.061438	4.457810
305.407585	6825.216265	15.181453	-0.061392	4.455236
305.496501	6817.237236	15.186458	-0.061403	4.452667
305.477086	6809.228657	15.191463	-0.061394	4.450086
305.770845	6801.205215	15.196467	-0.061444	4.447501
305.235951	6793.279062	15.201472	-0.061339	4.444941
305.026094	6785.249882	15.206477	-0.061295	4.442349
305.834239	6777.141948	15.211482	-0.061440	4.439734
305.678437	6769.252611	15.216487	-0.061406	4.437184
305.734546	6761.125875	15.221491	-0.061411	4.434556
305.691223	6753.218836	15.226496	-0.061398	4.431998
305.614400	6745.167532	15.231501	-0.061379	4.429391
305.884125	6737.184308	15.236506	-0.061424	4.426807
305.791808	6729.143690	15.241511	-0.061402	4.424200
305.874475	6721.183639	15.246515	-0.061412	4.421619
305.968531	6713.210691	15.251520	-0.061424	4.419033
305.607233	6705.222835	15.256525	-0.061352	4.416437
305.699436	6697.150743	15.261530	-0.061364	4.413815
305.774365	6689.163432	15.266535	-0.061373	4.411219
305.805064	6681.125981	15.271539	-0.061373	4.408605
305.869241	6673.178965	15.276544	-0.061380	4.406019
305.737843	6665.151229	15.281549	-0.061350	4.403404
305.928158	6657.251375	15.286554	-0.061381	4.400831
305.765325	6649.245263	15.291559	-0.061345	4.398220
305.654308	6641.247734	15.296563	-0.061320	4.395610
305.703068	6633.259454	15.301568	-0.061324	4.393003
305.610944	6625.230976	15.306573	-0.061301	4.390380
305.383854	6617.267398	15.311578	-0.061254	4.387776
305.217069	6609.274951	15.316583	-0.061218	4.385162
305.370463	6601.234895	15.321587	-0.061241	4.382532
305.723912	6593.253562	15.326592	-0.061302	4.379921
305.466251	6585.266943	15.331597	-0.061249	4.377303
305.384921	6577.275727	15.336602	-0.061228	4.374683
305.418960	6569.286849	15.341607	-0.061230	4.372063
305.399103	6561.224994	15.346611	-0.061221	4.369417
305.607660	6553.270418	15.351616	-0.061254	4.366807
305.331343	6545.277128	15.356621	-0.061198	4.364178
305.191204	6537.351229	15.361626	-0.061167	4.361571
305.014546	6529.298135	15.366631	-0.061129	4.358921
304.887184	6521.344659	15.371635	-0.061100	4.356302
305.173321	6513.283253	15.376640	-0.061148	4.353649
305.276614	6505.186376	15.381645	-0.061162	4.350981
305.275502	6497.218008	15.386650	-0.061157	4.348353
305.086101	6489.212547	15.391655	-0.061116	4.345710
305.331096	6481.214027	15.396659	-0.061157	4.343071
305.386388	6473.275827	15.401664	-0.061162	4.340449
305.042724	6465.265166	15.406669	-0.061093	4.337798
305.047086	6457.252036	15.411674	-0.061089	4.335147
304.958799	6449.257397	15.416679	-0.061067	4.332501
304.875507	6441.227985	15.421683	-0.061046	4.329841
304.900804	6433.251702	15.426688	-0.061046	4.327198
304.788653	6425.248912	15.431693	-0.061020	4.324543
304.555471	6417.349150	15.436698	-0.060971	4.321920
304.302248	6409.284646	15.441703	-0.060919	4.319240
304.580330	6401.264237	15.446707	-0.060966	4.316578
304.519784	6393.270568	15.451712	-0.060949	4.313920
304.121608	6385.302848	15.456717	-0.060870	4.311267
304.497695	6377.215802	15.461722	-0.060935	4.308578
304.787866	6369.192158	15.466727	-0.060984	4.305909
304.493065	6361.180525	15.471731	-0.060924	4.303236
304.230115	6353.260187	15.476736	-0.060870	4.300593
304.076832	6345.242718	15.481741	-0.060836	4.297916
304.309747	6337.237569	15.486746	-0.060874	4.295246
304.565528	6329.203988	15.491751	-0.060917	4.292564
304.162589	6321.189770	15.496755	-0.060837	4.289881
304.260891	6313.171475	15.501760	-0.060850	4.287200
303.959775	6305.174935	15.506765	-0.060789	4.284521
304.342152	6297.236957	15.511770	-0.060855	4.281866
304.071325	6289.224496	15.516775	-0.060799	4.279178
303.891497	6281.290907	15.521779	-0.060761	4.276516
303.852099	6273.228082	15.526784	-0.060748	4.273810
303.927875	6265.246064	15.531789	-0.060757	4.271131
303.839478	6257.207860	15.536794	-0.060735	4.268430
304.067467	6249.143226	15.541799	-0.060773	4.265721
303.661539	6241.211826	15.546803	-0.060692	4.263049
303.893492	6233.174821	15.551808	-0.060730	4.260345
303.771766	6225.183061	15.556813	-0.060702	4.257652
303.947213	6217.152278	15.561818	-0.060730	4.254948
303.969725	6209.178370	15.566823	-0.060729	4.252259
304.129573	6201.150750	15.571827	-0.060753	4.249551
303.794181	6193.209009	15.576832	-0.060686	4.246866
303.807226	6185.155453	15.581837	-0.060683	4.244145
303.902717	6177.221731	15.586842	-0.060696	4.241463
303.968482	6169.180460	15.591847	-0.060703	4.238743
304.075866	6161.194647	15.596851	-0.060718	4.236041
304.143549	6153.196725	15.601856	-0.060725	4.233332
303.896629	6145.157758	15.606861	-0.060674	4.230605
303.990036	6137.175747	15.611866	-0.060686	4.227898
303.657844	6129.218053	15.616871	-0.060619	4.225194
303.590568	6121.200952	15.621875	-0.060602	4.222470
303.336957	6113.209831	15.626880	-0.060549	4.219751
303.533929	6105.211936	15.631885	-0.060581	4.217034
303.435107	6097.150932	15.636890	-0.060557	4.214289
303.511901	6089.184716	15.641895	-0.060567	4.211578
303.343343	6081.130131	15.646899	-0.060530	4.208831
303.338986	6073.205343	15.651904	-0.060524	4.206129
302.914247	6065.184601	15.656909	-0.060440	4.203388
303.325613	6057.175599	15.661914	-0.060511	4.200658
303.628797	6049.168945	15.666919	-0.060563	4.197926
303.242339	6041.169175	15.671923	-0.060486	4.195187
303.301535	6033.193151	15.676928	-0.060492	4.192459
303.023984	6025.110917	15.681933	-0.060435	4.189690
303.157686	6017.098135	15.686938	-0.060454	4.186947
303.270219	6009.085838	15.691943	-0.060470	4.184202
302.800189	6001.250400	15.696947	-0.060378	4.181509
302.928514	5993.179790	15.701952	-0.060396	4.178740
302.493636	5985.226388	15.706957	-0.060310	4.176004
302.998834	5977.122926	15.711962	-0.060399	4.173225
303.176332	5969.119990	15.716967	-0.060427	4.170475
302.635061	5961.181919	15.721971	-0.060321	4.167737
302.917878	5953.148521	15.726976	-0.060369	4.164974
302.698312	5945.221201	15.731981	-0.060323	4.162240
302.494767	5937.199935	15.736986	-0.060280	4.159472
302.601731	5929.244046	15.741991	-0.060295	4.156728
302.613849	5921.155890	15.746995	-0.060292	4.153936
302.114446	5913.321792	15.752000	-0.060194	4.151223
302.279570	5905.156552	15.757005	-0.060219	4.148402
302.218759	5897.178566	15.762010	-0.060203	4.145641
302.389494	5889.191708	15.767015	-0.060229	4.142879
302.234818	5881.182918	15.772019	-0.060195	4.140102
302.132760	5873.260379	15.777024	-0.060171	4.137354
302.294619	5865.144916	15.782029	-0.060196	4.134542
302.216477	5857.223156	15.787034	-0.060177	4.131791
302.291610	5849.155172	15.792039	-0.060185	4.128989
302.321241	5841.183315	15.797043	-0.060186	4.126219
302.381477	5833.202143	15.802048	-0.060192	4.123444
302.289249	5825.210842	15.807053	-0.060170	4.120661
301.772177	5817.267875	15.812058	-0.060068	4.117888
302.197296	5809.214008	15.817063	-0.060142	4.115086
302.356290	5801.160934	15.822067	-0.060167	4.112280
302.245418	5793.189474	15.827072	-0.060141	4.109497
302.500525	5785.123727	15.832077	-0.060183	4.106683
301.880832	5777.241055	15.837082	-0.060063	4.103920
301.973942	5769.224105	15.842087	-0.060075	4.101117
301.980810	5761.168885	15.847091	-0.060071	4.098299
301.686254	5753.236834	15.852096	-0.060011	4.095517
302.180551	5745.134155	15.857101	-0.060098	4.092684
302.229861	5737.115971	15.862106	-0.060102	4.089873
302.194821	5729.177972	15.867111	-0.060091	4.087087
302.359397	5721.101910	15.872115	-0.060116	4.084254
302.406471	5713.236194	15.877120	-0.060120	4.081490
302.336446	5705.196160	15.882125	-0.060101	4.078662
302.199129	5697.242661	15.887130	-0.060071	4.075861
302.325786	5689.214241	15.892135	-0.060089	4.073036
302.349681	5681.174516	15.897139	-0.060089	4.070204
302.124949	5673.248501	15.902144	-0.060042	4.067405
301.943433	5665.190840	15.907149	-0.060003	4.064559
301.825259	5657.239549	15.912154	-0.059976	4.061750
302.035910	5649.173410	15.917159	-0.060010	4.058903
301.815497	5641.233335	15.922163	-0.059963	4.056092
302.065340	5633.174867	15.927168	-0.060005	4.053244
301.839086	5625.151932	15.932173	-0.059958	4.050400
301.878105	5617.192476	15.937178	-0.059960	4.047580
302.148878	5609.156880	15.942183	-0.060005	4.044735
302.073853	5601.190770	15.947187	-0.059986	4.041907
302.141877	5593.170194	15.952192	-0.059993	4.039060
301.936677	5585.277440	15.957197	-0.059950	4.036252
302.065339	5577.200395	15.962202	-0.059969	4.033382
301.687354	5569.189962	15.967207	-0.059893	4.030525
301.995931	5561.116996	15.972211	-0.059946	4.027656
302.157265	5553.158927	15.977216	-0.059971	4.024823
301.806200	5545.211781	15.982221	-0.059900	4.021983
301.863523	5537.247014	15.987226	-0.059906	4.019141
301.978744	5529.267678	15.992231	-0.059922	4.016294
301.751199	5521.224466	15.997235	-0.059875	4.013416
301.528337	5513.273301	16.002240	-0.059828	4.010568
301.446678	5505.226147	16.007245	-0.059808	4.007687
301.233452	5497.253816	16.012250	-0.059763	4.004828
301.254588	5489.298730	16.017255	-0.059762	4.001978
300.816265	5481.296492	16.022259	-0.059675	3.999100
300.690624	5473.352986	16.027264	-0.059646	3.996247
301.419229	5465.155853	16.032269	-0.059777	3.993315
301.665133	5457.159766	16.037274	-0.059817	3.990446
301.456947	5449.244372	16.042279	-0.059774	3.987595
301.275607	5441.211168	16.047283	-0.059735	3.984700
301.211406	5433.281238	16.052288	-0.059718	3.981843
301.081357	5425.234741	16.057293	-0.059688	3.978940
301.226126	5417.286131	16.062298	-0.059710	3.976075
301.439183	5409.236063	16.067303	-0.059745	3.973173
301.101787	5401.246015	16.072307	-0.059677	3.970280
301.416313	5393.224997	16.077312	-0.059730	3.967386
301.207279	5385.185114	16.082317	-0.059686	3.964474
301.058569	5377.312832	16.087322	-0.059653	3.961621
301.233043	5369.275745	16.092327	-0.059681	3.958712
300.981241	5361.284236	16.097331	-0.059629	3.955810
301.255191	5353.269305	16.102336	-0.059674	3.952907
301.104571	5345.254390	16.107341	-0.059641	3.949993
301.097589	5337.211453	16.112346	-0.059635	3.947071
300.907522	5329.224263	16.117351	-0.059594	3.944162
300.853787	5321.275439	16.122355	-0.059579	3.941269
300.725055	5313.324384	16.127360	-0.059550	3.938371
301.051896	5305.227888	16.132365	-0.059606	3.935426
300.894118	5297.259385	16.137370	-0.059571	3.932516
300.890408	5289.262249	16.142375	-0.059565	3.929597
300.662163	5281.284618	16.147379	-0.059518	3.926679
300.894314	5273.273278	16.152384	-0.059556	3.923755
300.922826	5265.261577	16.157389	-0.059556	3.920825
301.079340	5257.258411	16.162394	-0.059580	3.917898
301.072506	5249.330388	16.167399	-0.059574	3.914993
301.104556	5241.281044	16.172403	-0.059575	3.912042
300.907499	5233.284990	16.177408	-0.059533	3.909105
300.608791	5225.311588	16.182413	-0.059472	3.906171
300.616012	5217.290330	16.187418	-0.059468	3.903223
300.673252	5209.297019	16.192423	-0.059474	3.900285
300.641709	5201.302697	16.197427	-0.059463	3.897342
300.529262	5193.354461	16.202432	-0.059437	3.894412
300.675790	5185.315023	16.207437	-0.059459	3.891452
300.471606	5177.304413	16.212442	-0.059416	3.888493
300.431942	5169.339904	16.217447	-0.059403	3.885552
300.281141	5161.369048	16.222451	-0.059370	3.882604
300.433515	5153.358686	16.227456	-0.059393	3.879646
300.422375	5145.358478	16.232461	-0.059386	3.876686
300.399115	5137.348217	16.237466	-0.059377	3.873719
300.499427	5129.182177	16.242471	-0.059390	3.870695
300.443717	5121.221497	16.247475	-0.059375	3.867742
300.296301	5113.286434	16.252480	-0.059342	3.864794
300.350476	5105.308192	16.257485	-0.059347	3.861831
300.317364	5097.283116	16.262490	-0.059336	3.858848
300.204642	5089.361120	16.267495	-0.059310	3.855898
300.151215	5081.309377	16.272499	-0.059294	3.852900
300.291138	5073.353274	16.277504	-0.059315	3.849939
299.815686	5065.360240	16.282509	-0.059222	3.846948
300.245358	5057.278328	16.287514	-0.059297	3.843941
300.105573	5049.371176	16.292519	-0.059266	3.840986
299.925456	5041.348120	16.297523	-0.059227	3.837983
299.821946	5033.406190	16.302528	-0.059202	3.835010
299.917072	5025.404569	16.307533	-0.059215	3.832017
299.841078	5017.355972	16.312538	-0.059196	3.829001
299.672523	5009.390004	16.317543	-0.059159	3.826010
299.446692	5001.351409	16.322547	-0.059112	3.822989
299.472386	4993.396503	16.327552	-0.059112	3.820003
299.490156	4985.385174	16.332557	-0.059110	3.816992
299.653672	4977.312489	16.337562	-0.059135	3.813960
299.891094	4969.329590	16.342567	-0.059174	3.810961
299.701187	4961.363817	16.347571	-0.059134	3.807956
299.397205	4953.408031	16.352576	-0.059072	3.804950
299.522349	4945.385399	16.357581	-0.059090	3.801926
299.643129	4937.359450	16.362586	-0.059108	3.798898
299.663246	4929.418694	16.367591	-0.059106	3.795898
299.539544	4921.355247	16.372595	-0.059078	3.792845
299.554511	4913.418427	16.377600	-0.059076	3.789842
299.523225	4905.418259	16.382605	-0.059065	3.786810
299.725052	4897.350784	16.387610	-0.059097	3.783757
299.747787	4889.410283	16.392615	-0.059096	3.780745
299.428180	4881.442410	16.397619	-0.059032	3.777712
299.508787	4873.434670	16.402624	-0.059042	3.774670
299.394605	4865.443128	16.407629	-0.059015	3.771628
299.726659	4857.421775	16.412634	-0.059072	3.768583
299.608066	4849.418043	16.417639	-0.059045	3.765531
299.475762	4841.439735	16.422643	-0.059015	3.762487
299.677435	4833.453257	16.427648	-0.059047	3.759444
299.402320	4825.513377	16.432653	-0.058991	3.756406
299.762833	4817.437315	16.437658	-0.059053	3.753328
299.793838	4809.469642	16.442663	-0.059054	3.750281
299.403733	4801.501298	16.447667	-0.058976	3.747221
299.271565	4793.453752	16.452672	-0.058946	3.744135
299.339426	4785.509830	16.457677	-0.058954	3.741091
299.567947	4777.457825	16.462682	-0.058991	3.738006
299.742266	4769.457341	16.467687	-0.059018	3.734938
299.377036	4761.500231	16.472691	-0.058945	3.731870
299.583583	4753.453961	16.477696	-0.058979	3.728780
299.666359	4745.477526	16.482701	-0.058989	3.725711
299.479480	4737.477621	16.487706	-0.058949	3.722624
299.282345	4729.533672	16.492711	-0.058907	3.719555
299.192359	4721.545607	16.497715	-0.058885	3.716470
299.159107	4713.530560	16.502720	-0.058874	3.713373
299.077191	4705.467348	16.507725	-0.058853	3.710253
299.002424	4697.487098	16.512730	-0.058834	3.707163
299.006741	4689.471975	16.517735	-0.058830	3.704060
298.698683	4681.535309	16.522739	-0.058768	3.700975
298.566413	4673.569409	16.527744	-0.058738	3.697882
298.449200	4665.545722	16.532749	-0.058711	3.694763
298.763361	4657.479524	16.537754	-0.058764	3.691637
299.008013	4649.459258	16.542759	-0.058805	3.688525
299.050159	4641.474709	16.547763	-0.058807	3.685418
299.055295	4633.525046	16.552768	-0.058803	3.682321
298.999185	4625.506237	16.557773	-0.058788	3.679193
298.867669	4617.594632	16.562778	-0.058758	3.676103
298.908320	4609.580383	16.567783	-0.058761	3.672974
298.475609	4601.606502	16.572787	-0.058675	3.669845
298.767776	4593.596501	16.577792	-0.058724	3.666719
298.504745	4585.609521	16.582797	-0.058670	3.663585
298.568364	4577.605116	16.587802	-0.058677	3.660450
298.696997	4569.603792	16.592807	-0.058696	3.657315
298.385252	4561.590093	16.597811	-0.058632	3.654161
298.441022	4553.695008	16.602816	-0.058638	3.651060
298.421536	4545.609558	16.607821	-0.058629	3.647880
298.302236	4537.590564	16.612826	-0.058602	3.644721
298.120526	4529.723227	16.617831	-0.058563	3.641616
298.093450	4521.672804	16.622835	-0.058552	3.638442
298.407277	4513.649398	16.627840	-0.058606	3.635284
298.434745	4505.666738	16.632845	-0.058606	3.632132
298.186221	4497.629479	16.637850	-0.058554	3.628948
298.038311	4489.656046	16.642855	-0.058522	3.625789
298.006564	4481.622943	16.647859	-0.058511	3.622607
298.209363	4473.651612	16.652864	-0.058543	3.619454
297.940404	4465.682003	16.657869	-0.058488	3.616285
298.129263	4457.651651	16.662874	-0.058518	3.613102
298.321677	4449.646099	16.667879	-0.058549	3.609926
298.054990	4441.641038	16.672883	-0.058494	3.606735
297.974392	4433.672671	16.677888	-0.058474	3.603560
298.078023	4425.673557	16.682893	-0.058488	3.600376
297.954576	4417.746716	16.687898	-0.058460	3.597211
297.942194	4409.712384	16.692903	-0.058452	3.594004
297.844195	4401.707976	16.697907	-0.058429	3.590803
297.913836	4393.704556	16.702912	-0.058437	3.587605
298.075767	4385.673308	16.707917	-0.058462	3.584396
297.974400	4377.740501	16.712922	-0.058438	3.581215
297.965123	4369.747193	16.717927	-0.058431	3.578010
298.034402	4361.689845	16.722931	-0.058439	3.574779
297.848594	4353.773144	16.727936	-0.058399	3.571593
297.935161	4345.724299	16.732941	-0.058410	3.568360
298.249730	4337.713566	16.737946	-0.058464	3.565146
297.856656	4329.822423	16.742951	-0.058385	3.561956
297.746620	4321.791623	16.747955	-0.058360	3.558716
297.603452	4313.878223	16.752960	-0.058328	3.555518
297.677666	4305.758370	16.757965	-0.058337	3.552242
297.566410	4297.724254	16.762970	-0.058311	3.548991
297.594644	4289.777094	16.767975	-0.058311	3.545776
297.575981	4281.778321	16.772979	-0.058302	3.542536
297.673734	4273.797149	16.777984	-0.058315	3.539305
297.692264	4265.793200	16.782989	-0.058314	3.536058
297.664858	4257.807075	16.787994	-0.058303	3.532814
297.437996	4249.830748	16.792999	-0.058256	3.529565
297.156208	4241.866154	16.798003	-0.058198	3.526316
297.683119	4233.816763	16.803008	-0.058291	3.523055
297.435378	4225.855136	16.808013	-0.058240	3.519802
297.645181	4217.821480	16.813018	-0.058274	3.516532
297.574445	4209.842496	16.818023	-0.058256	3.513271
297.458336	4201.869952	16.823027	-0.058229	3.510009
297.296805	4193.881009	16.828032	-0.058194	3.506736
297.458439	4185.829794	16.833037	-0.058219	3.503444
297.643267	4177.865700	16.838042	-0.058248	3.500186
297.428066	4169.911131	16.843047	-0.058203	3.496916
297.043162	4161.931297	16.848051	-0.058126	3.493627
297.202562	4153.926995	16.853056	-0.058151	3.490342
297.376382	4145.881974	16.858061	-0.058178	3.487038
296.875878	4137.943433	16.863066	-0.058080	3.483752
296.821574	4130.000122	16.868071	-0.058064	3.480476
296.833660	4121.965925	16.873075	-0.058062	3.477162
296.961155	4113.945153	16.878080	-0.058080	3.473854
296.850489	4105.974703	16.883085	-0.058054	3.470556
296.831864	4097.927470	16.888090	-0.058046	3.467225
296.853993	4089.913289	16.893095	-0.058045	3.463907
296.661640	4082.010130	16.898099	-0.058004	3.460624
296.892325	4073.991157	16.903104	-0.058042	3.457305
296.684110	4065.994049	16.908109	-0.057998	3.453976
296.659108	4058.017437	16.913114	-0.057988	3.450659
296.744411	4050.022912	16.918119	-0.057999	3.447335
296.614049	4041.998468	16.923123	-0.057969	3.443988
296.633499	4034.060772	16.928128	-0.057968	3.440679
296.673416	4026.054240	16.933133	-0.057970	3.437338
296.868576	4018.027604	16.938138	-0.058001	3.433992
296.649050	4010.088852	16.943143	-0.057955	3.430664
296.470468	4002.076206	16.948147	-0.057917	3.427304
296.389167	3994.091646	16.953152	-0.057897	3.423956
296.306297	3986.128464	16.958157	-0.057876	3.420613
296.475284	3978.087218	16.963162	-0.057903	3.417243
296.466933	3970.091085	16.968167	-0.057896	3.413883
296.383249	3962.106244	16.973171	-0.057875	3.410521
296.244047	3954.167379	16.978176	-0.057844	3.407173
296.089280	3946.109630	16.983181	-0.057810	3.403772
296.048127	3938.166448	16.988186	-0.057797	3.400419
295.705779	3930.228778	16.993191	-0.057729	3.397054
295.553901	3922.183918	16.998195	-0.057695	3.393648
295.985630	3914.090488	17.003200	-0.057770	3.390239
295.795475	3906.135840	17.008205	-0.057730	3.386862
295.695079	3898.135118	17.013210	-0.057706	3.383466
295.952045	3890.129983	17.018215	-0.057749	3.380078
295.959168	3882.158799	17.023219	-0.057745	3.376691
295.788630	3874.213233	17.028224	-0.057708	3.373306
296.042406	3866.153797	17.033229	-0.057750	3.369884
296.092254	3858.169266	17.038234	-0.057754	3.366483
295.898564	3850.221376	17.043239	-0.057713	3.363086
295.930870	3842.211405	17.048243	-0.057714	3.359666
295.979169	3834.265113	17.053248	-0.057718	3.356272
296.016983	3826.238067	17.058253	-0.057720	3.352838
295.829762	3818.260917	17.063258	-0.057680	3.349414
295.802457	3810.290992	17.068263	-0.057670	3.345996
296.150788	3802.245084	17.073267	-0.057729	3.342556
296.069574	3794.302780	17.078272	-0.057709	3.339140
295.846413	3786.347166	17.083277	-0.057662	3.335710
295.745810	3778.353412	17.088282	-0.057639	3.332265
295.703080	3770.336745	17.093287	-0.057625	3.328808
295.488480	3762.345257	17.098291	-0.057580	3.325352
295.351005	3754.421737	17.103296	-0.057550	3.321925
295.507887	3746.365971	17.108301	-0.057574	3.318448
295.206737	3738.424000	17.113306	-0.057513	3.314999
295.424001	3730.384587	17.118311	-0.057548	3.311525
295.360416	3722.360929	17.123315	-0.057531	3.308042
295.458180	3714.354127	17.128320	-0.057544	3.304570
295.385572	3706.415689	17.133325	-0.057525	3.301117
295.439532	3698.401634	17.138330	-0.057530	3.297633
295.568416	3690.395640	17.143335	-0.057549	3.294151
295.401798	3682.437950	17.148339	-0.057513	3.290675
295.053354	3674.505411	17.153344	-0.057443	3.287199
294.887551	3666.486820	17.158349	-0.057407	3.283689
294.858374	3658.497847	17.163354	-0.057396	3.280194
295.179296	3650.520763	17.168359	-0.057451	3.276714
294.881340	3642.542260	17.173363	-0.057391	3.273205
294.791681	3634.580200	17.178368	-0.057369	3.269707
294.935117	3626.503498	17.183373	-0.057390	3.266166
295.024769	3618.516417	17.188378	-0.057402	3.262657
294.836055	3610.584377	17.193383	-0.057362	3.259158
294.615298	3602.622874	17.198387	-0.057315	3.255640
295.126071	3594.513242	17.203392	-0.057405	3.252083
295.249575	3586.510005	17.208397	-0.057423	3.248554
295.130356	3578.557971	17.213402	-0.057396	3.245033
295.229965	3570.600376	17.218407	-0.057409	3.241515
295.218411	3562.606224	17.223411	-0.057402	3.237973
295.204093	3554.653450	17.228416	-0.057394	3.234445
294.777540	3546.694299	17.233421	-0.057310	3.230893
294.743533	3538.655622	17.238426	-0.057298	3.227317
294.910760	3530.630574	17.243431	-0.057324	3.223753
294.731047	3522.664190	17.248435	-0.057286	3.220196
294.865851	3514.703254	17.253440	-0.057306	3.216651
294.898983	3506.651745	17.258445	-0.057307	3.213057
294.961206	3498.642040	17.263450	-0.057313	3.209480
294.803956	3490.709734	17.268455	-0.057279	3.205923
294.504333	3482.743601	17.273459	-0.057218	3.202341
294.816655	3474.753253	17.278464	-0.057271	3.198771
294.382517	3466.813236	17.283469	-0.057185	3.195187
294.409859	3458.806424	17.288474	-0.057185	3.191589
294.528458	3450.782444	17.293479	-0.057202	3.187983
294.638772	3442.745438	17.298483	-0.057217	3.184367
294.593237	3434.826770	17.303488	-0.057204	3.180793
294.304037	3426.861346	17.308493	-0.057145	3.177183
294.324219	3418.819651	17.313498	-0.057143	3.173548
294.067105	3410.863969	17.318503	-0.057090	3.169936
294.253654	3402.849825	17.323507	-0.057120	3.166313
294.663625	3394.820032	17.328512	-0.057191	3.162689
294.318139	3386.895692	17.333517	-0.057122	3.159075
294.305381	3378.923717	17.338522	-0.057114	3.155449
294.167387	3370.961652	17.343527	-0.057083	3.151819
294.189177	3362.916994	17.348531	-0.057082	3.148153
294.316793	3354.891699	17.353536	-0.057101	3.144498
294.192772	3346.949220	17.358541	-0.057073	3.140864
294.242360	3338.971392	17.363546	-0.057077	3.137218
294.037980	3330.994119	17.368551	-0.057034	3.133556
293.953536	3322.972068	17.373555	-0.057013	3.129875
294.111332	3314.991630	17.378560	-0.057037	3.126220
294.074405	3306.993842	17.383565	-0.057025	3.122543
293.964860	3299.025014	17.388570	-0.057000	3.118872
294.078136	3291.062116	17.393575	-0.057016	3.115210
294.025101	3283.063083	17.398579	-0.057001	3.111519
294.145752	3275.066794	17.403584	-0.057018	3.107833
293.809779	3267.096562	17.408589	-0.056950	3.104134
293.916461	3259.116626	17.413594	-0.056965	3.100446
294.048458	3251.149615	17.418599	-0.056984	3.096761
294.111023	3243.117044	17.423603	-0.056991	3.093038
293.939687	3235.152291	17.428608	-0.056954	3.089331
293.939450	3227.188385	17.433613	-0.056949	3.085628
293.672389	3219.222551	17.438618	-0.056894	3.081907
293.645015	3211.249865	17.443623	-0.056884	3.078190
293.635158	3203.227522	17.448627	-0.056877	3.074446
293.451093	3195.246962	17.453632	-0.056837	3.070708
293.235107	3187.247501	17.458637	-0.056792	3.066955
293.462245	3179.216036	17.463642	-0.056829	3.063204
293.357512	3171.271983	17.468647	-0.056805	3.059474
293.246622	3163.283159	17.473651	-0.056779	3.055718
293.375630	3155.279228	17.478656	-0.056798	3.051961
293.451434	3147.274068	17.483661	-0.056807	3.048197
293.130967	3139.334755	17.488666	-0.056742	3.044440
293.168797	3131.385733	17.493671	-0.056744	3.040691
293.420706	3123.357989	17.498675	-0.056786	3.036911
293.320425	3115.406820	17.503680	-0.056762	3.033145
293.136223	3107.398001	17.508685	-0.056722	3.029342
293.124806	3099.417289	17.513690	-0.056715	3.025557
293.062847	3091.460457	17.518695	-0.056699	3.021776
293.191082	3083.452784	17.523699	-0.056717	3.017976
293.256093	3075.462497	17.528704	-0.056724	3.014176
293.310304	3067.481437	17.533709	-0.056729	3.010375
293.050205	3059.524940	17.538714	-0.056676	3.006564
293.138602	3051.529735	17.543719	-0.056687	3.002749
293.121686	3043.548076	17.548723	-0.056679	2.998929
293.039726	3035.609613	17.553728	-0.056658	2.995122
292.848686	3027.623384	17.558733	-0.056618	2.991282
293.114804	3019.555515	17.563738	-0.056662	2.987421
292.954563	3011.602224	17.568743	-0.056627	2.983588
292.814488	3003.635680	17.573747	-0.056596	2.979745
292.895471	2995.670492	17.578752	-0.056606	2.975909
292.809804	2987.668292	17.583757	-0.056585	2.972041
292.582842	2979.713173	17.588762	-0.056537	2.968184
292.655029	2971.693482	17.593767	-0.056546	2.964306
292.461811	2963.775568	17.598771	-0.056505	2.960459
292.262910	2955.812092	17.603776	-0.056463	2.956584
292.087294	2947.812960	17.608781	-0.056425	2.952687
292.402662	2939.753463	17.613786	-0.056478	2.948783
292.615856	2931.754092	17.618791	-0.056513	2.944897
292.358866	2923.822533	17.623795	-0.056460	2.941014
292.424727	2915.843732	17.628800	-0.056467	2.937120
292.232676	2907.899423	17.633805	-0.056426	2.933223
292.047450	2899.868836	17.638810	-0.056387	2.929280
292.048388	2891.928454	17.643815	-0.056382	2.925385
292.062992	2883.931064	17.648819	-0.056379	2.921459
292.237664	2875.941890	17.653824	-0.056407	2.917539
292.224885	2867.938571	17.658829	-0.056399	2.913597
292.286771	2859.897919	17.663834	-0.056405	2.909636
292.161749	2851.949681	17.668839	-0.056377	2.905704
291.952015	2843.967466	17.673843	-0.056333	2.901746
291.992934	2836.004127	17.678848	-0.056335	2.897805
292.323279	2827.961896	17.683853	-0.056392	2.893836
292.088217	2820.037989	17.688858	-0.056343	2.889889
292.228755	2812.063338	17.693863	-0.056364	2.885932
291.977362	2804.112370	17.698867	-0.056312	2.881960
292.032818	2796.134742	17.703872	-0.056317	2.877986
291.916206	2788.163806	17.708877	-0.056290	2.874000
291.857053	2780.183755	17.713882	-0.056274	2.870007
291.764397	2772.224874	17.718887	-0.056252	2.866018
291.679411	2764.230201	17.723891	-0.056231	2.862005
291.800444	2756.259381	17.728896	-0.056248	2.858010
291.705710	2748.265284	17.733901	-0.056226	2.853986
291.620250	2740.286412	17.738906	-0.056205	2.849964
291.541525	2732.306940	17.743911	-0.056185	2.845937
291.597906	2724.327031	17.748915	-0.056190	2.841912
291.548069	2716.387249	17.753920	-0.056176	2.837894
291.456045	2708.405049	17.758925	-0.056154	2.833848
291.341318	2700.419686	17.763930	-0.056127	2.829792
291.437414	2692.425199	17.768935	-0.056140	2.825739
291.432688	2684.418809	17.773939	-0.056134	2.821667
291.227335	2676.487632	17.778944	-0.056091	2.817616
291.097600	2668.508430	17.783949	-0.056061	2.813540
291.123031	2660.501463	17.788954	-0.056061	2.809452
291.030644	2652.547898	17.793959	-0.056039	2.805379
291.257739	2644.529118	17.798963	-0.056076	2.801285
291.389579	2636.569542	17.803968	-0.056095	2.797210
290.889390	2628.645575	17.808973	-0.055997	2.793110
290.967832	2620.627562	17.813978	-0.056006	2.788990
291.150289	2612.637611	17.818983	-0.056035	2.784884
290.870853	2604.689418	17.823987	-0.055978	2.780766
290.668679	2596.770626	17.828992	-0.055935	2.776662
290.615306	2588.770760	17.833997	-0.055920	2.772519
290.812130	2580.732877	17.839002	-0.055952	2.768365
290.661505	2572.786498	17.844007	-0.055919	2.764231
290.454844	2564.847323	17.849011	-0.055875	2.760092
290.729025	2556.840956	17.854016	-0.055921	2.755940
290.656018	2548.829717	17.859021	-0.055902	2.751759
290.409096	2540.843629	17.864026	-0.055851	2.747573
290.774408	2532.833840	17.869031	-0.055914	2.743407
290.576502	2524.885398	17.874035	-0.055872	2.739231
290.691697	2516.928388	17.879040	-0.055889	2.735064
290.586991	2508.961685	17.884045	-0.055864	2.730872
290.628290	2500.971968	17.889050	-0.055867	2.726670
290.760727	2492.991282	17.894055	-0.055886	2.722473
290.576894	2485.041985	17.899059	-0.055847	2.718265
290.615090	2477.085409	17.904064	-0.055849	2.714061
290.376909	2469.132090	17.909069	-0.055799	2.709835
290.364567	2461.131055	17.914074	-0.055792	2.705591
290.407317	2453.198160	17.919079	-0.055795	2.701381
290.500628	2445.168849	17.924083	-0.055807	2.697116
290.505958	2437.216153	17.929088	-0.055803	2.692879
290.424594	2429.242093	17.934093	-0.055783	2.688618
290.470077	2421.239573	17.939098	-0.055786	2.684344
290.535690	2413.309078	17.944103	-0.055793	2.680103
290.435601	2405.347946	17.949107	-0.055769	2.675827
290.506561	2397.357148	17.954112	-0.055777	2.671540
290.348795	2389.385156	17.959117	-0.055743	2.667242
290.184097	2381.417693	17.964122	-0.055707	2.662938
290.183670	2373.455702	17.969127	-0.055702	2.658641
290.249375	2365.453991	17.974131	-0.055709	2.654320
290.167784	2357.507363	17.979136	-0.055689	2.650012
290.068553	2349.525837	17.984141	-0.055665	2.645677
289.988471	2341.574601	17.989146	-0.055645	2.641353
290.046879	2333.614379	17.994151	-0.055651	2.637026
289.700993	2325.677055	17.999155	-0.055581	2.632677
289.891810	2317.671128	18.004160	-0.055612	2.628319
290.013534	2309.660157	18.009165	-0.055629	2.623947
289.877869	2301.713664	18.014170	-0.055599	2.619586
289.834218	2293.765569	18.019175	-0.055586	2.615222
289.749659	2285.783659	18.024179	-0.055565	2.610830
289.704062	2277.822808	18.029184	-0.055551	2.606445
289.656231	2269.864061	18.034189	-0.055537	2.602053
289.601051	2261.901626	18.039194	-0.055522	2.597651
289.396004	2253.942558	18.044199	-0.055479	2.593234
289.376478	2245.838406	18.049203	-0.055470	2.588741
289.610622	2237.864045	18.054208	-0.055508	2.584330
289.535641	2229.929930	18.059213	-0.055489	2.579912
289.552097	2221.964820	18.064218	-0.055487	2.575476
289.443514	2214.020345	18.069223	-0.055462	2.571035
289.253383	2206.058732	18.074227	-0.055421	2.566571
289.103284	2198.126872	18.079232	-0.055388	2.562119
289.028516	2190.177038	18.084237	-0.055369	2.557654
289.061236	2182.183272	18.089242	-0.055370	2.553164
289.308575	2174.203799	18.094247	-0.055411	2.548690
289.000070	2166.245211	18.099251	-0.055349	2.544179
288.949538	2158.316969	18.104256	-0.055334	2.539697
289.141672	2150.324175	18.109261	-0.055365	2.535187
288.934851	2142.362970	18.114266	-0.055321	2.530659
289.020833	2134.383901	18.119271	-0.055332	2.526133
288.912971	2126.428188	18.124275	-0.055307	2.521599
289.067135	2118.467757	18.129280	-0.055331	2.517073
288.829772	2110.527698	18.134285	-0.055281	2.512521
289.008748	2102.521486	18.139290	-0.055309	2.507954
289.055755	2094.547686	18.144295	-0.055313	2.503388
288.999042	2086.581512	18.149299	-0.055297	2.498810
288.892430	2078.627785	18.154304	-0.055272	2.494227
288.847887	2070.680103	18.159309	-0.055259	2.489643
288.549730	2062.766418	18.164314	-0.055198	2.485052
288.789245	2054.777001	18.169319	-0.055238	2.480449
288.835788	2046.793622	18.174323	-0.055241	2.475826
288.638127	2038.872456	18.179328	-0.055200	2.471212
288.531210	2030.886180	18.184333	-0.055175	2.466559
288.415597	2022.936785	18.189338	-0.055148	2.461917
288.540307	2014.978265	18.194343	-0.055166	2.457280
288.320017	2007.025812	18.199347	-0.055120	2.452611
288.429741	1999.044765	18.204352	-0.055135	2.447942
288.327172	1991.088897	18.209357	-0.055111	2.443262
288.351597	1983.129645	18.214362	-0.055110	2.438581
288.132614	1975.207634	18.219367	-0.055065	2.433894
288.281858	1967.163360	18.224371	-0.055087	2.429155
288.008733	1959.246232	18.229376	-0.055031	2.424449
287.687979	1951.343891	18.234381	-0.054967	2.419738
287.708068	1943.351006	18.239386	-0.054965	2.414991
287.839736	1935.365712	18.244391	-0.054985	2.410248
287.894329	1927.350403	18.249395	-0.054990	2.405472
287.973117	1919.413223	18.254400	-0.054999	2.400735
288.115252	1911.438871	18.259405	-0.055021	2.395971
287.990940	1903.504658	18.264410	-0.054992	2.391201
287.820041	1895.587434	18.269415	-0.054955	2.386427
287.792831	1887.605169	18.274419	-0.054945	2.381617
287.966087	1879.639102	18.279424	-0.054972	2.376822
287.850913	1871.699103	18.284429	-0.054946	2.372011
287.650691	1863.761322	18.289434	-0.054903	2.367183
287.584124	1855.833545	18.294439	-0.054886	2.362363
287.738059	1847.833874	18.299443	-0.054909	2.357508
287.612634	1839.925634	18.304448	-0.054881	2.352675
287.586481	1831.941090	18.309453	-0.054871	2.347794
287.735376	1823.943940	18.314458	-0.054894	2.342909
287.570277	1816.038759	18.319463	-0.054858	2.338045
287.509544	1808.060794	18.324467	-0.054841	2.333134
287.657020	1800.087594	18.329472	-0.054864	2.328233
287.543020	1792.156317	18.334477	-0.054837	2.323326
287.399432	1784.235593	18.339482	-0.054806	2.318413
287.584736	1776.277720	18.344487	-0.054835	2.313494
287.306678	1768.332941	18.349491	-0.054778	2.308532
287.274954	1760.390227	18.354496	-0.054767	2.303583
287.259674	1752.442834	18.359501	-0.054759	2.298622
287.384173	1744.454877	18.364506	-0.054777	2.293636
287.419511	1736.513949	18.369511	-0.054779	2.288662
287.285054	1728.559185	18.374515	-0.054749	2.283653
287.335800	1720.639826	18.379520	-0.054753	2.278671
287.227734	1712.689882	18.384525	-0.054728	2.273646
287.144353	1704.708277	18.389530	-0.054707	2.268591
287.284086	1696.738982	18.394535	-0.054728	2.263552
287.151508	1688.801283	18.399539	-0.054698	2.258499
287.012174	1680.885067	18.404544	-0.054667	2.253447
287.121232	1672.907435	18.409549	-0.054682	2.248366
287.117245	1664.944573	18.414554	-0.054677	2.243274
286.672144	1657.097711	18.419559	-0.054589	2.238204
286.655820	1649.126611	18.424563	-0.054581	2.233082
286.519899	1641.208309	18.429568	-0.054550	2.227971
286.642967	1633.202411	18.434573	-0.054568	2.222815
286.818625	1625.231181	18.439578	-0.054596	2.217675
286.644190	1617.328740	18.444583	-0.054558	2.212535
286.561872	1609.372712	18.449587	-0.054538	2.207357
286.415467	1601.463387	18.454592	-0.054505	2.202191
286.380019	1593.529501	18.459597	-0.054494	2.197007
285.922102	1585.646278	18.464602	-0.054403	2.191805
285.924394	1577.678332	18.469607	-0.054399	2.186578
286.022951	1569.677058	18.474611	-0.054412	2.181325
286.405775	1561.678765	18.479616	-0.054478	2.176088
286.021735	1553.803812	18.484621	-0.054401	2.170848
286.080008	1545.829774	18.489626	-0.054407	2.165572
286.376095	1537.867570	18.494631	-0.054457	2.160313
286.075205	1529.978542	18.499635	-0.054396	2.155033
286.163086	1522.025867	18.504640	-0.054407	2.149734
286.116035	1514.083689	18.509645	-0.054393	2.144417
286.173304	1506.149455	18.514650	-0.054399	2.139102
286.156309	1498.227965	18.519655	-0.054391	2.133774
285.986716	1490.289300	18.524659	-0.054354	2.128408
285.918928	1482.381193	18.529664	-0.054336	2.123058
285.974558	1474.451242	18.534669	-0.054342	2.117692
285.710535	1466.530743	18.539674	-0.054287	2.112287
285.669113	1458.552122	18.544679	-0.054275	2.106850
285.781470	1450.575173	18.549683	-0.054290	2.101416
285.667831	1442.682856	18.554688	-0.054264	2.096004
285.623580	1434.741576	18.559693	-0.054251	2.090551
285.642442	1426.800033	18.564698	-0.054249	2.085089
285.647473	1418.902978	18.569703	-0.054245	2.079643
285.607218	1410.957696	18.574707	-0.054233	2.074144
285.626153	1403.025043	18.579712	-0.054231	2.068645
285.622084	1395.085652	18.584717	-0.054225	2.063125
285.336386	1387.205062	18.589722	-0.054167	2.057602
285.296837	1379.290217	18.594727	-0.054154	2.052065
284.937505	1371.384680	18.599731	-0.054083	2.046487
285.012876	1363.443273	18.604736	-0.054091	2.040914
285.038193	1355.506093	18.609741	-0.054091	2.035323
284.869839	1347.580271	18.614746	-0.054055	2.029704
285.179419	1339.595181	18.619751	-0.054107	2.024078
284.942181	1331.709359	18.624755	-0.054058	2.018449
285.224897	1323.749481	18.629760	-0.054105	2.012807
285.027543	1315.853141	18.634765	-0.054064	2.007143
284.852106	1307.945071	18.639770	-0.054026	2.001457
284.794045	1300.057279	18.644775	-0.054010	1.995782
284.776271	1292.103529	18.649779	-0.054002	1.990047
284.652616	1284.198860	18.654784	-0.053974	1.984320
284.467232	1276.318361	18.659789	-0.053934	1.978588
284.728793	1268.332561	18.664794	-0.053978	1.972810
284.634676	1260.431588	18.669799	-0.053955	1.967039
284.375784	1252.549608	18.674803	-0.053902	1.961246
284.482041	1244.623868	18.679808	-0.053916	1.955445
284.547967	1236.693703	18.684813	-0.053924	1.949618
284.370745	1228.779027	18.689818	-0.053886	1.943758
284.467131	1220.851461	18.694823	-0.053898	1.937902
284.441201	1212.922978	18.699827	-0.053888	1.932013
284.372689	1205.019446	18.704832	-0.053871	1.926121
284.165856	1197.136668	18.709837	-0.053827	1.920210
284.153225	1189.225752	18.714842	-0.053820	1.914281
284.136066	1181.306203	18.719847	-0.053811	1.908327
283.993646	1173.395874	18.724851	-0.053780	1.902347
284.044895	1165.497501	18.729856	-0.053784	1.896380
284.002281	1157.575151	18.734861	-0.053771	1.890365
283.912393	1149.663734	18.739866	-0.053749	1.884333
283.928135	1141.782568	18.744871	-0.053747	1.878317
283.792058	1133.886353	18.749875	-0.053717	1.872253
283.959417	1125.943350	18.754880	-0.053743	1.866169
283.811354	1118.051209	18.759885	-0.053710	1.860066
283.812795	1110.154237	18.764890	-0.053706	1.853958
283.946921	1102.229910	18.769895	-0.053725	1.847824
283.551238	1094.395709	18.774899	-0.053647	1.841676
283.560693	1086.506965	18.779904	-0.053643	1.835514
283.580893	1078.587342	18.784909	-0.053642	1.829308
283.603820	1070.674499	18.789914	-0.053641	1.823087
283.569119	1062.804232	18.794919	-0.053630	1.816871
282.941795	1054.983452	18.799923	-0.053508	1.810600
283.159985	1047.038542	18.804928	-0.053544	1.804312
282.986296	1039.192303	18.809933	-0.053506	1.798033
282.906760	1031.287490	18.814938	-0.053486	1.791697
282.611817	1023.406183	18.819943	-0.053426	1.785330
282.823800	1015.445773	18.824947	-0.053461	1.778940
283.019269	1007.525348	18.829952	-0.053492	1.772557
283.034579	999.610705	18.834957	-0.053490	1.766134
283.032276	991.743038	18.839962	-0.053484	1.759722
283.014251	983.891026	18.844967	-0.053476	1.753298
282.844702	976.014646	18.849971	-0.053439	1.746811
282.913325	968.137418	18.854976	-0.053447	1.740330
282.858142	960.273273	18.859981	-0.053432	1.733820
282.793945	952.386968	18.864986	-0.053415	1.727265
282.956589	944.496162	18.869991	-0.053440	1.720711
282.694776	936.677783	18.874995	-0.053386	1.714137
282.662310	928.805122	18.880000	-0.053375	1.707522
282.619357	920.919504	18.885005	-0.053362	1.700869
282.656906	913.035774	18.890010	-0.053364	1.694203
282.712786	905.146696	18.895015	-0.053369	1.687508
282.580998	897.297415	18.900019	-0.053340	1.680795
282.714617	889.435925	18.905024	-0.053360	1.674080
282.625710	881.580856	18.910029	-0.053338	1.667314
282.376713	873.753615	18.915034	-0.053287	1.660522
282.360946	865.900542	18.920039	-0.053279	1.653712
282.243884	858.035818	18.925043	-0.053252	1.646850
282.139201	850.204623	18.930048	-0.053227	1.639990
282.287366	842.318737	18.935053	-0.053250	1.633088
282.015210	834.461585	18.940058	-0.053194	1.626123
282.188382	826.579348	18.945063	-0.053221	1.619169
282.105942	818.733065	18.950067	-0.053201	1.612181
282.106761	810.871496	18.955072	-0.053196	1.605161
282.027407	803.056634	18.960077	-0.053176	1.598140
281.970555	795.212505	18.965082	-0.053161	1.591065
281.837370	787.388379	18.970087	-0.053131	1.583965
281.949640	779.526153	18.975091	-0.053147	1.576835
281.710795	771.717544	18.980096	-0.053097	1.569669
281.816403	763.864705	18.985101	-0.053112	1.562481
281.598898	756.074343	18.990106	-0.053066	1.555269
281.376250	748.279059	18.995111	-0.053020	1.548018
281.484768	740.395822	19.000115	-0.053035	1.540701
281.488549	732.571196	19.005120	-0.053031	1.533389
281.502915	724.724042	19.010125	-0.053028	1.526021
281.380509	716.926424	19.015130	-0.053001	1.518644
281.575347	709.081771	19.020135	-0.053032	1.511235
281.351012	701.289220	19.025139	-0.052985	1.503774
281.220858	693.512292	19.030144	-0.052956	1.496305
281.102444	685.704547	19.035149	-0.052929	1.488771
280.975529	677.907664	19.040154	-0.052900	1.481208
281.001582	670.104716	19.045159	-0.052900	1.473624
280.883058	662.268406	19.050163	-0.052873	1.465946
281.139415	654.429701	19.055168	-0.052916	1.458285
280.841995	646.672117	19.060173	-0.052855	1.450574
280.790699	638.879848	19.065178	-0.052841	1.442827
280.840330	631.077155	19.070183	-0.052845	1.435045
280.730701	623.304178	19.075187	-0.052820	1.427224
280.641419	615.534066	19.080192	-0.052798	1.419365
280.404750	607.784938	19.085197	-0.052749	1.411460
280.628289	599.958666	19.090202	-0.052786	1.403509
280.342284	592.248081	19.095207	-0.052727	1.395545
280.399606	584.441140	19.100211	-0.052733	1.387495
280.368934	576.677164	19.105216	-0.052722	1.379427
280.348248	568.911854	19.110221	-0.052713	1.371311
280.320719	561.140519	19.115226	-0.052703	1.363140
280.273396	553.410886	19.120231	-0.052690	1.354961
280.091431	545.676182	19.125235	-0.052651	1.346702
280.065837	537.935728	19.130240	-0.052641	1.338414
280.170416	530.167595	19.135245	-0.052656	1.330068
279.973997	522.460514	19.140250	-0.052614	1.321681
279.936185	514.730528	19.145255	-0.052602	1.313244
279.749726	506.939942	19.150259	-0.052562	1.304659
279.744327	499.223414	19.155264	-0.052556	1.296132
279.634777	491.510355	19.160269	-0.052531	1.287534
279.185065	483.872932	19.165274	-0.052442	1.278897
279.665314	476.078674	19.170279	-0.052527	1.270203
279.600221	468.373654	19.175283	-0.052510	1.261445
279.356522	460.724255	19.180288	-0.052459	1.252655
279.134229	453.059428	19.185293	-0.052413	1.243789
279.123715	445.374360	19.190298	-0.052406	1.234877
279.369420	437.644715	19.195303	-0.052447	1.225900
279.021053	430.019484	19.200307	-0.052377	1.216860
278.798190	422.382923	19.205312	-0.052331	1.207765
278.551492	414.759650	19.210317	-0.052280	1.198611
278.757967	407.048023	19.215322	-0.052314	1.189374
278.963944	399.366636	19.220327	-0.052347	1.180101
279.110954	391.691129	19.225331	-0.052369	1.170749
278.639485	384.147096	19.230336	-0.052277	1.161354
278.660900	376.509019	19.235341	-0.052276	1.151870
278.694474	368.855007	19.240346	-0.052277	1.142290
278.519345	361.278061	19.245351	-0.052240	1.132681
278.280816	353.701065	19.250355	-0.052191	1.122976
278.314279	346.108689	19.255360	-0.052192	1.113227
278.140338	338.544163	19.260365	-0.052155	1.103382
277.977626	330.989760	19.265370	-0.052120	1.093463
278.002339	323.412565	19.270375	-0.052119	1.083466
277.865565	315.880057	19.275379	-0.052089	1.073399
278.036116	308.290071	19.280384	-0.052116	1.063230
278.089789	300.739783	19.285389	-0.052121	1.052990
278.036880	293.213595	19.290394	-0.052106	1.042657
278.047061	285.716310	19.295399	-0.052103	1.032276
277.856814	278.237097	19.300403	-0.052063	1.021766
277.935262	270.741478	19.305408	-0.052073	1.011190
277.582162	263.330873	19.310413	-0.052003	1.000516
277.560120	255.855713	19.315418	-0.051994	0.989717
277.531303	248.392516	19.320423	-0.051984	0.978815
277.368817	240.968214	19.325427	-0.051949	0.967812
277.192126	233.590531	19.330432	-0.051911	0.956750
276.988934	226.209398	19.335437	-0.051868	0.945546
277.153914	218.781445	19.340442	-0.051894	0.934234
277.002494	211.436809	19.345447	-0.051861	0.922827
276.968546	204.084698	19.350451	-0.051850	0.911298
277.051521	196.725302	19.355456	-0.051861	0.899643
276.947783	189.417738	19.360461	-0.051837	0.887865
276.719944	182.169599	19.365466	-0.051790	0.875990
276.204957	174.993121	19.370471	-0.051690	0.863987
276.649230	167.634617	19.375475	-0.051768	0.851793
276.533825	160.434305	19.380480	-0.051741	0.839524
276.242045	153.265918	19.385485	-0.051683	0.827074
276.144060	146.088490	19.390490	-0.051660	0.814478
276.331717	138.888231	19.395495	-0.051690	0.801734
276.151126	131.794011	19.400499	-0.051652	0.788858
276.074839	124.712059	19.405504	-0.051633	0.775826
276.043415	117.649729	19.410509	-0.051623	0.762622
275.920500	110.641397	19.415514	-0.051595	0.749259
275.774670	103.667991	19.420519	-0.051564	0.735713
275.741115	96.697588	19.425523	-0.051553	0.721958
275.707157	89.782625	19.430528	-0.051542	0.708049
275.453358	82.945835	19.435533	-0.051491	0.693941
275.458302	76.271183	19.440538	-0.051487	0.679981