Fri Apr 16 19:44:36 2021

Number of Points = 3635
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.645583	-0.043833	0.000000	-0.000048	0.313263

3.661260	-0.047518	0.005005	-0.000051	0.313259
3.809465	-0.074625	0.010010	-0.000078	0.313259
3.662906	-0.049209	0.015014	-0.000051	0.313254
3.701917	-0.053834	0.020019	-0.000059	0.313266
3.580481	-0.033903	0.025024	-0.000036	0.313256
3.321563	0.014117	0.030029	0.000012	0.313261
3.423139	-0.002794	0.035034	-0.000007	0.313269
3.368742	0.004953	0.040038	0.000003	0.313259
3.593372	-0.034715	0.045043	-0.000039	0.313265
3.627660	-0.042884	0.050048	-0.000045	0.313256
3.409245	-0.002627	0.055053	-0.000005	0.313259
3.615222	-0.040314	0.060058	-0.000043	0.313259
3.542702	-0.066085	0.065062	-0.000030	0.313079
3.646851	-0.109059	0.070067	-0.000049	0.312968
3.609445	-0.103565	0.075072	-0.000042	0.312963
3.682420	-0.117304	0.080077	-0.000056	0.312961
3.798186	-0.136943	0.085082	-0.000078	0.312968
3.572931	-0.097821	0.090086	-0.000036	0.312960
3.750496	-0.131738	0.095091	-0.000069	0.312953
3.613054	-0.177702	0.100096	-0.000043	0.312625
3.644188	-0.183018	0.105101	-0.000049	0.312627
3.681398	-0.189787	0.110106	-0.000056	0.312627
3.658163	-0.187359	0.115110	-0.000052	0.312619
3.633653	-0.183932	0.120115	-0.000048	0.312615
3.369287	-0.201554	0.125120	0.000002	0.312312
3.493708	-0.224108	0.130125	-0.000022	0.312312
3.608030	-0.245161	0.135130	-0.000043	0.312311
3.535967	-0.233043	0.140134	-0.000030	0.312307
3.867460	-0.340038	0.145139	-0.000092	0.312091
3.618893	-0.317213	0.150144	-0.000045	0.311988
3.469373	-0.289781	0.155149	-0.000018	0.311989
3.741467	-0.338398	0.160154	-0.000068	0.311994
3.533516	-0.364544	0.165158	-0.000030	0.311698
3.699536	-0.393635	0.170163	-0.000061	0.311703
3.639723	-0.384364	0.175168	-0.000050	0.311696
3.470509	-0.398260	0.180173	-0.000018	0.311489
3.650340	-0.456370	0.185178	-0.000052	0.311371
3.409266	-0.413082	0.190182	-0.000007	0.311369
3.598282	-0.477722	0.195187	-0.000042	0.311229
3.576218	-0.510398	0.200192	-0.000038	0.311059
3.565739	-0.509301	0.205197	-0.000036	0.311055
3.590185	-0.551937	0.210202	-0.000041	0.310878
3.470077	-0.561319	0.215206	-0.000019	0.310733
3.552022	-0.573907	0.220211	-0.000034	0.310745
3.446400	-0.601750	0.225216	-0.000014	0.310526
3.424936	-0.605575	0.230221	-0.000011	0.310490
3.559842	-0.646588	0.235226	-0.000036	0.310414
3.571323	-0.707048	0.240230	-0.000038	0.310142
3.701821	-0.729483	0.245235	-0.000062	0.310148
3.452740	-0.741212	0.250240	-0.000016	0.309883
3.591485	-0.778654	0.255245	-0.000042	0.309826
3.518890	-0.798233	0.260250	-0.000028	0.309674
3.301535	-0.796739	0.265254	0.000012	0.309496
3.467003	-0.838203	0.270259	-0.000019	0.309444
3.363838	-0.868013	0.275264	0.000000	0.309217
3.451985	-0.886045	0.280269	-0.000016	0.309208
3.462966	-0.957158	0.285274	-0.000018	0.308885
3.212642	-0.913082	0.290278	0.000028	0.308879
3.301674	-0.987456	0.295283	0.000011	0.308606
3.361951	-1.007334	0.300288	0.000000	0.308565
3.357649	-1.064154	0.305293	0.000001	0.308295
3.423007	-1.085220	0.310298	-0.000011	0.308252
3.397724	-1.135873	0.315302	-0.000007	0.307994
3.478847	-1.157178	0.320307	-0.000022	0.307963
3.424714	-1.217161	0.325312	-0.000012	0.307635
3.225327	-1.190267	0.330317	0.000025	0.307592
3.479775	-1.296614	0.335322	-0.000022	0.307309
3.285313	-1.282780	0.340326	0.000014	0.307209
3.331365	-1.339860	0.345331	0.000005	0.306980
3.428237	-1.388361	0.350336	-0.000013	0.306834
3.395935	-1.411652	0.355341	-0.000007	0.306697
3.239968	-1.437909	0.360346	0.000022	0.306440
3.069196	-1.429478	0.365350	0.000054	0.306334
2.862190	-1.450557	0.370355	0.000092	0.306057
2.933928	-1.486967	0.375360	0.000079	0.305947
2.684078	-1.486608	0.380365	0.000125	0.305734
2.720157	-1.525868	0.385370	0.000118	0.305580
2.818902	-1.566445	0.390374	0.000100	0.305473
2.968921	-1.660954	0.395379	0.000072	0.305155
2.911833	-1.677804	0.400384	0.000083	0.305026
2.838946	-1.709226	0.405389	0.000096	0.304815
2.803285	-1.753178	0.410394	0.000103	0.304576
2.895710	-1.801629	0.415398	0.000085	0.304426
3.027022	-1.871345	0.420403	0.000061	0.304208
2.961540	-1.907650	0.425408	0.000073	0.303979
3.014122	-1.955552	0.430413	0.000063	0.303797
2.737047	-1.955873	0.435418	0.000115	0.303556
2.630285	-1.987028	0.440422	0.000134	0.303315
2.570238	-2.007976	0.445427	0.000146	0.303164
2.131094	-1.974673	0.450432	0.000227	0.302942
2.185563	-2.037870	0.455437	0.000217	0.302688
2.275784	-2.087079	0.460442	0.000200	0.302532
2.313162	-2.145439	0.465446	0.000193	0.302285
2.440535	-2.221793	0.470451	0.000169	0.302031
2.399547	-2.252161	0.475456	0.000177	0.301850
2.327841	-2.274869	0.480461	0.000190	0.301679
2.381378	-2.352484	0.485466	0.000180	0.301354
2.172481	-2.357371	0.490470	0.000219	0.301149
1.969250	-2.358542	0.495475	0.000257	0.300966
1.728511	-2.365824	0.500480	0.000302	0.300721
1.353830	-2.340471	0.505485	0.000371	0.300516
0.987732	-2.306757	0.510490	0.000439	0.300358
0.952758	-2.345027	0.515494	0.000446	0.300144
0.762262	-2.371220	0.520499	0.000481	0.299851
0.867966	-2.427965	0.525504	0.000461	0.299670
1.056044	-2.503612	0.530509	0.000426	0.299470
0.733260	-2.498246	0.535514	0.000486	0.299213
0.103146	-2.430184	0.540518	0.000604	0.298989
0.365653	-2.512776	0.545523	0.000555	0.298820
-0.099715	-2.481451	0.550528	0.000641	0.298563
-0.483737	-2.459557	0.555533	0.000713	0.298331
-0.595925	-2.467676	0.560538	0.000733	0.298193
-0.852913	-2.471168	0.565542	0.000781	0.297950
-1.359542	-2.421614	0.570547	0.000875	0.297744
-1.514195	-2.422926	0.575552	0.000904	0.297601
-1.602428	-2.469044	0.580557	0.000920	0.297299
-1.677781	-2.482885	0.585562	0.000934	0.297166
-2.588938	-2.356546	0.590566	0.001104	0.296975
-2.330644	-2.446222	0.595571	0.001056	0.296767
-2.501139	-2.436836	0.600576	0.001087	0.296662
-2.868241	-2.434278	0.605581	0.001156	0.296350
-2.595410	-2.508206	0.610586	0.001105	0.296231
-3.274810	-2.423090	0.615590	0.001231	0.296044
-3.378982	-2.449414	0.620595	0.001250	0.295823
-3.800575	-2.391389	0.625600	0.001329	0.295733
-4.041904	-2.394576	0.630605	0.001374	0.295503
-3.950009	-2.422816	0.635610	0.001356	0.295447
-4.299629	-2.422233	0.640614	0.001421	0.295139
-4.262553	-2.448907	0.645619	0.001414	0.295042
-4.944017	-2.367265	0.650624	0.001541	0.294835
-5.070139	-2.376273	0.655629	0.001565	0.294679
-5.070073	-2.412485	0.660634	0.001565	0.294501
-5.057828	-2.449528	0.665638	0.001562	0.294330
-5.552113	-2.384512	0.670643	0.001654	0.294209
-5.757463	-2.390418	0.675648	0.001692	0.293997
-5.873885	-2.395581	0.680653	0.001714	0.293867
-5.893064	-2.433038	0.685658	0.001717	0.293666
-6.330384	-2.376122	0.690662	0.001799	0.293555
-6.213544	-2.440965	0.695667	0.001777	0.293341
-6.393107	-2.428634	0.700672	0.001810	0.293241
-6.771799	-2.404393	0.705677	0.001881	0.293021
-6.930743	-2.388435	0.710682	0.001910	0.292958
-7.347555	-2.361985	0.715686	0.001988	0.292715
-7.646976	-2.326733	0.720691	0.002043	0.292620
-7.570888	-2.378241	0.725696	0.002029	0.292434
-7.495214	-2.420238	0.730701	0.002015	0.292295
-7.786665	-2.397879	0.735706	0.002069	0.292144
-8.628656	-2.279922	0.740710	0.002226	0.291970
-7.975998	-2.414843	0.745715	0.002104	0.291890
-8.478561	-2.364714	0.750720	0.002198	0.291686
-8.626250	-2.345862	0.755725	0.002225	0.291647
-8.542910	-2.418355	0.760730	0.002209	0.291363
-8.588118	-2.412367	0.765734	0.002218	0.291352
-8.911473	-2.412553	0.770739	0.002278	0.291060
-9.249719	-2.353303	0.775744	0.002341	0.291049
-9.207075	-2.409877	0.780749	0.002333	0.290806
-9.573177	-2.358135	0.785754	0.002401	0.290733
-9.848042	-2.336689	0.790758	0.002452	0.290592
-9.884657	-2.351242	0.795763	0.002458	0.290486
-9.718826	-2.401069	0.800768	0.002428	0.290389
-10.182260	-2.368524	0.805773	0.002514	0.290132
-10.117560	-2.379350	0.810778	0.002502	0.290137
-10.786772	-2.321307	0.815782	0.002626	0.289820
-10.719658	-2.333245	0.820787	0.002614	0.289821
-10.964952	-2.328425	0.825792	0.002659	0.289623
-11.235502	-2.304834	0.830797	0.002709	0.289496
-11.217341	-2.316269	0.835802	0.002706	0.289455
-11.976226	-2.225895	0.840806	0.002847	0.289218
-11.582126	-2.297093	0.845811	0.002774	0.289221
-11.791939	-2.302123	0.850816	0.002813	0.289005
-12.479301	-2.202751	0.855821	0.002940	0.288877
-11.907056	-2.312185	0.860826	0.002834	0.288851
-12.029774	-2.348661	0.865830	0.002857	0.288556
-12.153554	-2.325031	0.870835	0.002880	0.288563
-12.545279	-2.295550	0.875840	0.002952	0.288354
-12.893538	-2.255557	0.880845	0.003017	0.288237
-12.230588	-2.385562	0.885850	0.002894	0.288190
-12.959005	-2.302338	0.890854	0.003029	0.287943
-12.872889	-2.316472	0.895859	0.003013	0.287951
-12.885236	-2.359788	0.900864	0.003015	0.287723
-13.302106	-2.307498	0.905869	0.003093	0.287605
-13.287867	-2.321103	0.910874	0.003090	0.287550
-13.619740	-2.312525	0.915878	0.003152	0.287290
-13.629737	-2.308768	0.920883	0.003154	0.287300
-13.963073	-2.290192	0.925888	0.003215	0.287089
-14.168936	-2.274875	0.930893	0.003254	0.286978
-13.744518	-2.359254	0.935898	0.003175	0.286942
-14.616510	-2.253148	0.940902	0.003337	0.286678
-14.536566	-2.266701	0.945907	0.003322	0.286683
-14.275713	-2.344624	0.950912	0.003273	0.286529
-14.678174	-2.309271	0.955917	0.003348	0.286339
-14.890176	-2.267116	0.960922	0.003387	0.286357
-14.917094	-2.320249	0.965926	0.003392	0.286064
-14.933509	-2.322229	0.970931	0.003395	0.286040
-15.356266	-2.262591	0.975936	0.003474	0.285953
-15.814200	-2.223897	0.980941	0.003559	0.285728
-15.517753	-2.276696	0.985946	0.003504	0.285734
-15.601646	-2.294371	0.990950	0.003519	0.285568
-16.132287	-2.216071	0.995955	0.003618	0.285476
-15.715814	-2.292809	1.000960	0.003540	0.285471
-16.336851	-2.243302	1.005965	0.003656	0.285150
-16.553604	-2.207797	1.010970	0.003696	0.285131
-16.335701	-2.260402	1.015974	0.003656	0.285065
-16.197722	-2.335569	1.020979	0.003630	0.284811
-16.485147	-2.282811	1.025984	0.003683	0.284814
-16.694385	-2.283930	1.030989	0.003722	0.284616
-16.701149	-2.307406	1.035994	0.003723	0.284490
-17.140658	-2.229552	1.040998	0.003805	0.284480
-17.240657	-2.263751	1.046003	0.003824	0.284214
-17.065291	-2.300134	1.051008	0.003791	0.284192
-16.928423	-2.346149	1.056013	0.003765	0.284085
-17.587599	-2.269969	1.061018	0.003888	0.283862
-17.856528	-2.221034	1.066022	0.003938	0.283863
-17.394831	-2.344143	1.071027	0.003852	0.283664
-18.189932	-2.222672	1.076032	0.004000	0.283546
-17.995693	-2.258471	1.081037	0.003963	0.283544
-17.802799	-2.351183	1.086042	0.003928	0.283250
-18.305489	-2.264999	1.091046	0.004021	0.283224
-18.357119	-2.273174	1.096051	0.004031	0.283135
-18.445174	-2.295383	1.101056	0.004047	0.282940
-18.499082	-2.286968	1.106061	0.004057	0.282933
-18.770832	-2.281531	1.111066	0.004107	0.282709
-19.210993	-2.223359	1.116070	0.004189	0.282597
-18.605557	-2.334223	1.121075	0.004076	0.282594
-19.069560	-2.311022	1.126080	0.004163	0.282281
-19.462652	-2.240735	1.131085	0.004236	0.282275
-19.197613	-2.307866	1.136090	0.004186	0.282178
-19.632562	-2.273527	1.141094	0.004267	0.281949
-19.693098	-2.261454	1.146099	0.004278	0.281955
-19.633878	-2.306463	1.151104	0.004267	0.281780
-19.853223	-2.288461	1.156109	0.004308	0.281668
-20.012238	-2.257846	1.161114	0.004337	0.281677
-20.506076	-2.234396	1.166118	0.004429	0.281336
-20.254827	-2.280040	1.171123	0.004382	0.281337
-20.180582	-2.310124	1.176128	0.004369	0.281252
-20.842448	-2.234512	1.181133	0.004492	0.281022
-20.699916	-2.257700	1.186138	0.004465	0.281037
-20.938393	-2.246884	1.191142	0.004509	0.280870
-21.258362	-2.218814	1.196147	0.004569	0.280715
-21.189243	-2.230828	1.201152	0.004556	0.280718
-21.204620	-2.261944	1.206157	0.004559	0.280544
-21.486189	-2.222346	1.211162	0.004611	0.280484
-21.616459	-2.198881	1.216166	0.004635	0.280484
-21.654259	-2.253290	1.221171	0.004642	0.280168
-21.958134	-2.203088	1.226176	0.004699	0.280142
-22.438625	-2.122942	1.231181	0.004788	0.280105
-22.056866	-2.244440	1.236186	0.004717	0.279836
-22.166081	-2.227767	1.241190	0.004737	0.279820
-22.328477	-2.217399	1.246195	0.004767	0.279722
-22.558381	-2.217988	1.251200	0.004810	0.279503
-22.411434	-2.244831	1.256205	0.004782	0.279502
-22.513766	-2.258012	1.261210	0.004801	0.279338
-23.257481	-2.147321	1.266214	0.004940	0.279212
-22.814753	-2.227173	1.271219	0.004857	0.279215
-23.109691	-2.222823	1.276224	0.004912	0.278960
-23.549223	-2.159163	1.281229	0.004994	0.278876
-23.264753	-2.208819	1.286234	0.004941	0.278887
-23.751264	-2.179222	1.291238	0.005031	0.278582
-23.960493	-2.143500	1.296243	0.005070	0.278571
-24.423003	-2.056588	1.301248	0.005156	0.278586
-24.044809	-2.186575	1.306253	0.005086	0.278268
-23.796314	-2.235148	1.311258	0.005039	0.278251
-24.311747	-2.149323	1.316262	0.005135	0.278210
-24.123466	-2.232467	1.321267	0.005100	0.277956
-24.232633	-2.212713	1.326272	0.005120	0.277956
-24.667508	-2.158404	1.331277	0.005201	0.277827
-24.543398	-2.221198	1.336282	0.005178	0.277618
-24.446919	-2.239771	1.341286	0.005160	0.277613
-24.681178	-2.234496	1.346291	0.005203	0.277419
-25.144015	-2.172314	1.351296	0.005289	0.277305
-24.991699	-2.200625	1.356301	0.005261	0.277302
-24.959447	-2.259795	1.361306	0.005255	0.277024
-25.635464	-2.145526	1.366310	0.005381	0.276979
-25.757113	-2.122752	1.371315	0.005403	0.276983
-25.339233	-2.253403	1.376320	0.005325	0.276698
-26.329224	-2.071992	1.381325	0.005510	0.276705
-26.329907	-2.079330	1.386330	0.005510	0.276667
-26.278584	-2.145645	1.391334	0.005500	0.276369
-26.306725	-2.139421	1.396339	0.005505	0.276375
-26.566346	-2.103834	1.401344	0.005553	0.276315
-26.386777	-2.186355	1.406349	0.005520	0.276054
-26.330378	-2.194643	1.411354	0.005509	0.276065
-26.672402	-2.160055	1.416358	0.005573	0.275920
-26.716145	-2.187452	1.421363	0.005581	0.275735
-26.452191	-2.236296	1.426368	0.005532	0.275731
-26.673141	-2.231413	1.431373	0.005573	0.275546
-26.632232	-2.248999	1.436378	0.005565	0.275494
-26.631425	-2.261212	1.441382	0.005565	0.275431
-26.925795	-2.262067	1.446387	0.005620	0.275145
-27.150327	-2.221535	1.451392	0.005661	0.275144
-27.292049	-2.231029	1.456397	0.005688	0.274959
-27.609013	-2.195081	1.461402	0.005746	0.274845
-27.727197	-2.175875	1.466406	0.005768	0.274833
-27.703964	-2.233154	1.471411	0.005764	0.274554
-27.779722	-2.226475	1.476416	0.005778	0.274517
-28.286614	-2.148214	1.481421	0.005872	0.274444
-28.648902	-2.121523	1.486426	0.005940	0.274238
-28.642377	-2.126173	1.491430	0.005938	0.274220
-28.400605	-2.192464	1.496435	0.005893	0.274103
-28.591772	-2.199265	1.501440	0.005929	0.273884
-28.491388	-2.218301	1.506445	0.005910	0.273880
-28.573335	-2.243433	1.511450	0.005925	0.273669
-29.262202	-2.136819	1.516454	0.006053	0.273570
-28.882399	-2.208277	1.521459	0.005982	0.273558
-28.737197	-2.292544	1.526464	0.005955	0.273252
-29.008763	-2.244152	1.531469	0.006006	0.273248
-29.223609	-2.229748	1.536474	0.006046	0.273117
-29.560079	-2.197242	1.541478	0.006108	0.272966
-29.265975	-2.250649	1.546483	0.006053	0.272967
-30.013548	-2.171422	1.551488	0.006193	0.272666
-30.299267	-2.127181	1.556493	0.006246	0.272625
-30.165400	-2.153979	1.561498	0.006221	0.272613
-30.385183	-2.169838	1.566502	0.006261	0.272317
-30.500488	-2.148014	1.571507	0.006283	0.272322
-30.275550	-2.210240	1.576512	0.006241	0.272209
-30.723851	-2.170942	1.581517	0.006324	0.271985
-30.545073	-2.201780	1.586522	0.006291	0.271994
-30.791659	-2.194402	1.591526	0.006337	0.271795
-30.935086	-2.186318	1.596531	0.006363	0.271700
-31.267519	-2.124535	1.601536	0.006425	0.271707
-31.619542	-2.120504	1.606541	0.006491	0.271388
-31.200653	-2.199013	1.611546	0.006412	0.271376
-31.635103	-2.131271	1.616550	0.006493	0.271316
-31.753420	-2.158331	1.621555	0.006515	0.271057
-31.328703	-2.234562	1.626560	0.006436	0.271063
-31.561009	-2.226130	1.631565	0.006479	0.270883
-31.943223	-2.181967	1.636570	0.006550	0.270748
-32.035935	-2.166574	1.641574	0.006567	0.270740
-31.789257	-2.253663	1.646579	0.006521	0.270515
-32.282512	-2.168252	1.651584	0.006613	0.270492
-32.326639	-2.179322	1.656589	0.006621	0.270391
-32.261051	-2.236180	1.661594	0.006609	0.270150
-32.273864	-2.236120	1.666598	0.006611	0.270139
-32.888472	-2.165354	1.671603	0.006726	0.269919
-32.807232	-2.197323	1.676608	0.006710	0.269828
-32.713698	-2.221940	1.681613	0.006693	0.269787
-32.994479	-2.224406	1.686618	0.006745	0.269500
-33.352008	-2.159185	1.691622	0.006812	0.269502
-32.854613	-2.275989	1.696627	0.006719	0.269361
-33.518634	-2.181724	1.701632	0.006842	0.269219
-33.744039	-2.142482	1.706637	0.006884	0.269210
-33.280564	-2.278058	1.711642	0.006798	0.268934
-33.539510	-2.242399	1.716646	0.006846	0.268873
-34.033224	-2.172028	1.721651	0.006938	0.268769
-34.067453	-2.202281	1.726656	0.006944	0.268573
-34.070440	-2.202649	1.731661	0.006945	0.268568
-34.223817	-2.216767	1.736666	0.006973	0.268342
-34.776830	-2.135125	1.741670	0.007076	0.268241
-34.427103	-2.200961	1.746675	0.007011	0.268229
-34.589762	-2.221924	1.751680	0.007041	0.267956
-34.891752	-2.167963	1.756685	0.007097	0.267952
-34.611567	-2.245186	1.761690	0.007045	0.267810
-35.241124	-2.165922	1.766694	0.007162	0.267620
-35.265992	-2.161013	1.771699	0.007166	0.267623
-35.188211	-2.224808	1.776704	0.007152	0.267354
-35.521601	-2.173995	1.781709	0.007214	0.267302
-35.723512	-2.146330	1.786714	0.007251	0.267253
-36.149635	-2.118653	1.791718	0.007331	0.266983
-35.724808	-2.196375	1.796723	0.007251	0.266981
-35.579680	-2.249811	1.801728	0.007224	0.266835
-36.375146	-2.132617	1.806733	0.007372	0.266686
-36.089951	-2.181872	1.811738	0.007319	0.266701
-35.929627	-2.269416	1.816742	0.007289	0.266385
-36.252801	-2.216555	1.821747	0.007349	0.266353
-36.398251	-2.210394	1.826752	0.007376	0.266243
-36.517818	-2.224641	1.831757	0.007398	0.266048
-36.359978	-2.251979	1.836762	0.007369	0.266056
-37.029752	-2.182982	1.841766	0.007494	0.265768
-36.900764	-2.213657	1.846771	0.007470	0.265729
-36.714812	-2.261999	1.851776	0.007435	0.265651
-37.315463	-2.187008	1.856781	0.007547	0.265464
-37.215207	-2.201052	1.861786	0.007528	0.265488
-37.366056	-2.224453	1.866790	0.007556	0.265211
-37.937770	-2.134976	1.871795	0.007662	0.265132
-37.973233	-2.132555	1.876800	0.007669	0.265111
-37.904575	-2.200240	1.881805	0.007656	0.264809
-38.296418	-2.125606	1.886810	0.007729	0.264828
-38.492372	-2.115833	1.891814	0.007765	0.264687
-38.354178	-2.177428	1.896819	0.007739	0.264488
-37.795536	-2.279674	1.901824	0.007635	0.264485
-38.668518	-2.167522	1.906829	0.007798	0.264230
-38.807968	-2.146745	1.911834	0.007823	0.264206
-38.463364	-2.225259	1.916838	0.007759	0.264119
-38.556369	-2.255526	1.921843	0.007776	0.263861
-38.777596	-2.214527	1.926848	0.007818	0.263866
-39.221303	-2.177849	1.931853	0.007900	0.263624
-39.214422	-2.190869	1.936858	0.007899	0.263560
-39.292579	-2.187401	1.941862	0.007913	0.263502
-39.524084	-2.194398	1.946867	0.007956	0.263232
-39.616000	-2.176629	1.951872	0.007973	0.263238
-39.775121	-2.181041	1.956877	0.008003	0.263055
-39.909715	-2.176169	1.961882	0.008028	0.262948
-40.152051	-2.131435	1.966886	0.008073	0.262952
-40.323825	-2.158707	1.971891	0.008105	0.262630
-40.787962	-2.076740	1.976896	0.008191	0.262617
-40.540767	-2.133532	1.981901	0.008145	0.262552
-40.638964	-2.158791	1.986906	0.008163	0.262314
-41.229929	-2.053744	1.991910	0.008273	0.262301
-41.163084	-2.093495	1.996915	0.008260	0.262150
-40.954206	-2.164369	2.001920	0.008221	0.261968

-40.959318	-2.207065	2.011917	0.008222	0.261728
-41.314526	-2.166655	2.021914	0.008288	0.261595
-41.563957	-2.166394	2.031910	0.008334	0.261346
-41.528406	-2.201537	2.041907	0.008328	0.261188
-41.944883	-2.152413	2.051904	0.008405	0.261041
-41.895878	-2.171662	2.061901	0.008396	0.260985
-42.129155	-2.177494	2.071898	0.008439	0.260718
-41.978781	-2.205079	2.081894	0.008411	0.260718
-42.190443	-2.167034	2.091891	0.008450	0.260716
-42.097442	-2.228234	2.101888	0.008432	0.260471
-42.242334	-2.202110	2.111885	0.008459	0.260471
-42.370570	-2.178687	2.121882	0.008483	0.260472
-42.231225	-2.204009	2.131878	0.008457	0.260474
-42.438431	-2.166732	2.141875	0.008495	0.260472
-42.242390	-2.202719	2.151872	0.008459	0.260471
-42.278967	-2.196669	2.161869	0.008465	0.260469
-42.259645	-2.199654	2.171866	0.008461	0.260473
-42.388581	-2.175871	2.181862	0.008485	0.260476
-42.771719	-2.105411	2.191859	0.008556	0.260481
-42.446251	-2.165464	2.201856	0.008496	0.260477
-42.648857	-2.128156	2.211853	0.008533	0.260481
-42.476629	-2.161181	2.221850	0.008501	0.260472
-42.346824	-2.178375	2.231846	0.008476	0.260509
-42.021739	-2.202175	2.241843	0.008416	0.260706
-41.920954	-2.220295	2.251840	0.008397	0.260709
-42.293162	-2.151074	2.261837	0.008466	0.260718
-42.007625	-2.192691	2.271834	0.008413	0.260776
-41.915166	-2.162536	2.281830	0.008395	0.261038
-42.145509	-2.119551	2.291827	0.008438	0.261045
-41.932225	-2.138672	2.301824	0.008398	0.261155
-41.571242	-2.170668	2.311821	0.008331	0.261343
-41.427245	-2.197332	2.321818	0.008304	0.261341
-41.178637	-2.196603	2.331814	0.008257	0.261597
-41.159961	-2.187148	2.341811	0.008253	0.261669
-41.193815	-2.162791	2.351808	0.008260	0.261771
-40.873245	-2.187595	2.361805	0.008200	0.261957
-40.725855	-2.205779	2.371802	0.008172	0.262006
-40.721091	-2.156291	2.381798	0.008171	0.262285
-40.523905	-2.188038	2.391795	0.008134	0.262309
-40.398261	-2.158426	2.401792	0.008111	0.262599
-40.619268	-2.102461	2.411789	0.008151	0.262687
-39.826714	-2.200419	2.421786	0.008004	0.262943
-39.985929	-2.152987	2.431782	0.008033	0.263045
-39.791844	-2.154058	2.441779	0.007997	0.263235
-39.626454	-2.148974	2.451776	0.007966	0.263429
-39.520641	-2.144040	2.461773	0.007946	0.263563
-39.295848	-2.134673	2.471770	0.007904	0.263840
-39.186804	-2.133647	2.481766	0.007883	0.263955
-38.720875	-2.173704	2.491763	0.007797	0.264202
-38.679002	-2.151888	2.501760	0.007789	0.264364
-38.516100	-2.159481	2.511757	0.007758	0.264486
-38.132292	-2.169937	2.521754	0.007686	0.264811
-38.396275	-2.097797	2.531750	0.007735	0.264944
-38.006231	-2.133561	2.541747	0.007663	0.265137
-37.970770	-2.083889	2.551744	0.007656	0.265445
-37.757848	-2.094978	2.561741	0.007616	0.265596
-37.628438	-2.089172	2.571738	0.007592	0.265757
-37.948888	-1.971233	2.581734	0.007651	0.266083
-37.072758	-2.091005	2.591731	0.007488	0.266300
-37.093647	-2.055491	2.601728	0.007491	0.266473
-36.802649	-2.062812	2.611725	0.007437	0.266722
-36.322061	-2.103436	2.621722	0.007347	0.266977
-36.030494	-2.123505	2.631718	0.007293	0.267156
-35.915254	-2.110689	2.641715	0.007271	0.267340
-35.941127	-2.051619	2.651712	0.007276	0.267635
-35.267171	-2.128928	2.661709	0.007150	0.267881
-35.243396	-2.098956	2.671706	0.007146	0.268068
-34.883284	-2.129723	2.681702	0.007078	0.268256
-34.572210	-2.131938	2.691699	0.007020	0.268550
-34.686409	-2.077499	2.701696	0.007041	0.268733
-34.059155	-2.154970	2.711693	0.006925	0.268931
-34.072930	-2.096484	2.721690	0.006927	0.269233
-33.735218	-2.119157	2.731686	0.006864	0.269442
-33.260557	-2.171681	2.741683	0.006775	0.269625
-32.870278	-2.205929	2.751680	0.006702	0.269823
-32.655548	-2.192004	2.761677	0.006662	0.270108
-32.577687	-2.172452	2.771674	0.006648	0.270290
-32.079189	-2.226220	2.781670	0.006555	0.270489
-32.199128	-2.157429	2.791667	0.006577	0.270741
-32.132359	-2.134870	2.801664	0.006564	0.270927
-31.689626	-2.176943	2.811661	0.006481	0.271134
-31.552414	-2.157507	2.821658	0.006456	0.271372
-31.538626	-2.105493	2.831654	0.006453	0.271663
-31.279044	-2.113721	2.841651	0.006404	0.271872
-31.453240	-2.040266	2.851648	0.006437	0.272095
-31.399241	-1.997632	2.861645	0.006426	0.272375
-30.575598	-2.096873	2.871642	0.006273	0.272645
-30.418762	-2.073505	2.881638	0.006243	0.272921
-30.395279	-2.035139	2.891635	0.006239	0.273148
-29.867351	-2.094287	2.901632	0.006140	0.273344
-29.161068	-2.177732	2.911629	0.006009	0.273584
-29.584770	-2.046617	2.921626	0.006087	0.273870
-28.879262	-2.130081	2.931622	0.005956	0.274108
-28.687202	-2.126585	2.941619	0.005920	0.274312
-28.673970	-2.089054	2.951616	0.005917	0.274524
-28.771673	-2.006390	2.961613	0.005935	0.274867
-28.313041	-2.044353	2.971610	0.005850	0.275107
-28.165921	-2.021975	2.981606	0.005822	0.275366
-27.863735	-2.033928	2.991603	0.005766	0.275593
-27.501391	-2.066157	3.001600	0.005698	0.275771
-27.303831	-2.044360	3.011597	0.005661	0.276075
-26.918265	-2.069096	3.021594	0.005589	0.276314
-26.509519	-2.098976	3.031590	0.005513	0.276547
-26.433977	-2.072380	3.041587	0.005499	0.276759
-26.369399	-2.037647	3.051584	0.005486	0.277003
-25.934947	-2.057487	3.061581	0.005405	0.277313
-25.485540	-2.096077	3.071578	0.005321	0.277539
-25.073246	-2.130473	3.081574	0.005245	0.277752
-24.954358	-2.109971	3.091571	0.005222	0.277972
-24.627045	-2.114516	3.101568	0.005161	0.278259
-24.571368	-2.081088	3.111565	0.005150	0.278487
-24.122817	-2.123405	3.121562	0.005067	0.278692
-23.871978	-2.128703	3.131558	0.005020	0.278902
-24.093946	-2.024070	3.141555	0.005061	0.279236
-23.364724	-2.115972	3.151552	0.004925	0.279448
-22.996033	-2.145904	3.161549	0.004856	0.279641
-23.000611	-2.100176	3.171546	0.004857	0.279874
-22.997850	-2.043426	3.181542	0.004856	0.280171
-22.248135	-2.130451	3.191539	0.004716	0.280427
-22.131118	-2.118643	3.201536	0.004694	0.280598
-22.140924	-2.083058	3.211533	0.004696	0.280774
-21.693186	-2.109273	3.221530	0.004613	0.281059
-21.310187	-2.132484	3.231526	0.004541	0.281299
-21.495845	-2.057233	3.241523	0.004575	0.281513
-21.080372	-2.086683	3.251520	0.004498	0.281751
-20.618293	-2.125918	3.261517	0.004412	0.281982
-20.148694	-2.158684	3.271514	0.004324	0.282253
-20.327877	-2.085227	3.281510	0.004357	0.282463
-20.004388	-2.101033	3.291507	0.004297	0.282685
-19.640018	-2.115251	3.301504	0.004229	0.282952
-19.682290	-2.056750	3.311501	0.004236	0.283213
-18.939014	-2.148699	3.321498	0.004098	0.283434
-19.062243	-2.085128	3.331494	0.004121	0.283645
-18.610797	-2.122493	3.341491	0.004036	0.283874
-18.243794	-2.131052	3.351488	0.003968	0.284172
-17.812551	-2.175918	3.361485	0.003887	0.284343
-17.717887	-2.156641	3.371482	0.003870	0.284530
-17.392437	-2.159108	3.381478	0.003809	0.284819
-17.071576	-2.173204	3.391475	0.003749	0.285045
-17.017800	-2.144046	3.401472	0.003739	0.285243
-16.540339	-2.185085	3.411469	0.003650	0.285476
-16.104700	-2.219068	3.421466	0.003568	0.285706
-16.290045	-2.150108	3.431462	0.003603	0.285886
-15.900354	-2.183298	3.441459	0.003530	0.286077
-15.657386	-2.172125	3.451456	0.003485	0.286358
-15.527969	-2.148692	3.461453	0.003460	0.286596
-15.267419	-2.156056	3.471450	0.003412	0.286799
-15.137990	-2.141997	3.481446	0.003387	0.286990
-14.475305	-2.201958	3.491443	0.003264	0.287296
-14.418178	-2.175356	3.501440	0.003253	0.287483
-14.174277	-2.179617	3.511437	0.003207	0.287685
-13.726552	-2.207793	3.521434	0.003124	0.287954
-13.802068	-2.148091	3.531430	0.003138	0.288186
-13.284477	-2.204611	3.541427	0.003041	0.288375
-13.086460	-2.202909	3.551424	0.003004	0.288565
-12.922691	-2.170617	3.561421	0.002973	0.288877
-12.350715	-2.233641	3.571418	0.002867	0.289083
-11.949591	-2.276045	3.581414	0.002792	0.289237
-11.731439	-2.264621	3.591411	0.002751	0.289493
-11.685901	-2.232192	3.601408	0.002742	0.289698
-11.542111	-2.223077	3.611405	0.002715	0.289875
-11.055539	-2.258245	3.621402	0.002625	0.290141
-11.052073	-2.210960	3.631398	0.002624	0.290381
-10.912685	-2.196870	3.641395	0.002598	0.290578
-11.080672	-2.131249	3.651392	0.002629	0.290754
-10.300898	-2.210144	3.661389	0.002483	0.291068
-10.282044	-2.175577	3.671386	0.002480	0.291257
-9.743542	-2.237189	3.681382	0.002379	0.291438
-9.691945	-2.192463	3.691379	0.002369	0.291708
-9.334175	-2.211525	3.701376	0.002303	0.291937
-9.090637	-2.219862	3.711373	0.002257	0.292116
-8.908895	-2.211182	3.721370	0.002223	0.292323
-8.538965	-2.216608	3.731366	0.002154	0.292630
-8.386129	-2.199891	3.741363	0.002125	0.292851
-8.080962	-2.220447	3.751360	0.002068	0.293024
-7.899176	-2.203942	3.761357	0.002034	0.293269
-7.626657	-2.202338	3.771354	0.001983	0.293523
-7.192928	-2.245081	3.781350	0.001902	0.293701
-7.159418	-2.213342	3.791347	0.001896	0.293889
-7.274268	-2.120933	3.801344	0.001917	0.294241
-6.465208	-2.229951	3.811341	0.001766	0.294429
-6.689748	-2.150282	3.821338	0.001808	0.294621
-5.671446	-2.290477	3.831334	0.001618	0.294842
-6.062003	-2.165140	3.841331	0.001691	0.295110
-5.572543	-2.212151	3.851328	0.001599	0.295316
-5.085402	-2.261965	3.861325	0.001509	0.295507
-5.181011	-2.195777	3.871322	0.001526	0.295747
-4.898064	-2.204688	3.881318	0.001473	0.295956
-4.679949	-2.207023	3.891315	0.001432	0.296139
-4.864783	-2.123705	3.901312	0.001467	0.296383
-4.661475	-2.094556	3.911309	0.001429	0.296706
-4.845946	-2.018529	3.921306	0.001463	0.296914
-3.959840	-2.126542	3.931302	0.001298	0.297173
-3.333064	-2.204134	3.941299	0.001181	0.297351
-3.568547	-2.104357	3.951296	0.001224	0.297629
-3.504729	-2.056957	3.961293	0.001212	0.297916
-2.789537	-2.144265	3.971290	0.001079	0.298124
-3.141997	-2.032657	3.981286	0.001144	0.298356
-2.608053	-2.083017	3.991283	0.001045	0.298583
-3.254967	-1.899782	4.001280	0.001165	0.298902
-2.745275	-1.933799	4.011277	0.001070	0.299187
-2.569482	-1.912766	4.021274	0.001037	0.299444
-2.257694	-1.913860	4.031270	0.000979	0.299713
-1.974473	-1.911956	4.041267	0.000926	0.299971
-1.957607	-1.852173	4.051264	0.000922	0.300275
-1.451089	-1.892043	4.061261	0.000828	0.300527
-1.511657	-1.836481	4.071258	0.000839	0.300743
-2.035925	-1.674801	4.081254	0.000936	0.301063
-1.986061	-1.615266	4.091251	0.000927	0.301393
-1.044728	-1.721078	4.101248	0.000751	0.301707
-1.430849	-1.591020	4.111245	0.000823	0.301995
-1.476608	-1.508853	4.121242	0.000831	0.302349
-1.183602	-1.492186	4.131238	0.000777	0.302685
-1.843970	-1.290256	4.141235	0.000899	0.303077
-1.470087	-1.288793	4.151232	0.000829	0.303409
-1.681495	-1.176298	4.161229	0.000869	0.303763
-1.376522	-1.146888	4.171226	0.000812	0.304167
-1.092871	-1.125490	4.181222	0.000759	0.304515
-1.130677	-1.029596	4.191219	0.000765	0.304938
-0.226573	-1.118057	4.201216	0.000597	0.305299
-0.018887	-1.085246	4.211213	0.000558	0.305634
0.067317	-1.030143	4.221210	0.000542	0.305970
-0.245662	-0.891032	4.231206	0.000600	0.306359
-0.335366	-0.780522	4.241203	0.000616	0.306804
-0.612377	-0.647230	4.251200	0.000667	0.307196
-0.113802	-0.651220	4.261197	0.000574	0.307605
0.054803	-0.581203	4.271194	0.000543	0.308079
0.121594	-0.511617	4.281190	0.000530	0.308463
0.055746	-0.403563	4.291187	0.000542	0.308914
-0.128979	-0.267336	4.301184	0.000576	0.309395
0.432257	-0.281339	4.311181	0.000472	0.309807
0.549278	-0.195732	4.321178	0.000450	0.310307
0.590709	-0.120348	4.331174	0.000442	0.310694
0.024337	0.095397	4.341171	0.000547	0.311220
0.000000	0.192382	4.351168	0.000551	0.311651

0.617349	0.360616	4.356173	0.000436	0.312950
0.954431	0.868919	4.361178	0.000373	0.315572
1.146539	1.687299	4.366182	0.000336	0.319461
1.915239	2.693003	4.371187	0.000192	0.324606
2.567324	4.020398	4.376192	0.000070	0.330988
3.092613	5.663242	4.381197	-0.000029	0.338500
3.568906	7.621677	4.386202	-0.000119	0.347130
4.365500	9.832695	4.391206	-0.000269	0.356812
4.892905	12.401549	4.396211	-0.000369	0.367456
5.663214	15.249025	4.401216	-0.000514	0.379034
6.594953	18.403162	4.406221	-0.000690	0.391511
8.607542	21.699566	4.411226	-0.001067	0.404812
10.090585	25.448815	4.416230	-0.001345	0.418923
11.617267	29.551939	4.421235	-0.001632	0.433780
13.087491	34.008792	4.426240	-0.001909	0.449252
14.577017	38.828695	4.431245	-0.002190	0.465347
16.228348	43.974863	4.436250	-0.002501	0.481971
18.455467	49.377210	4.441254	-0.002919	0.499084
20.431591	55.199157	4.446259	-0.003291	0.516675
22.980085	61.243432	4.451264	-0.003769	0.534567
26.033186	67.552904	4.456269	-0.004342	0.552809
29.066803	74.202842	4.461274	-0.004911	0.571318
30.852226	81.395472	4.466278	-0.005249	0.590025
32.691192	88.880090	4.471283	-0.005596	0.608872
35.380322	96.485851	4.476288	-0.006102	0.627781
37.682184	104.433119	4.481293	-0.006536	0.646743
41.888936	112.301264	4.486298	-0.007324	0.665730
46.530899	120.327224	4.491302	-0.008194	0.684684
48.923681	128.993652	4.496307	-0.008645	0.703616
51.242171	137.850987	4.501312	-0.009083	0.722404
53.416684	146.905954	4.506317	-0.009494	0.741049
55.542335	156.115123	4.511322	-0.009895	0.759512
57.798161	165.402183	4.516326	-0.010322	0.777722
60.377680	174.751087	4.521331	-0.010808	0.795729
63.244363	184.130617	4.526336	-0.011348	0.813481
65.699402	193.675706	4.531341	-0.011812	0.831012
67.965550	203.290242	4.536346	-0.012240	0.848241
69.723682	213.029367	4.541350	-0.012574	0.865183
72.236814	222.649812	4.546355	-0.013048	0.881822
73.767950	232.456735	4.551360	-0.013340	0.898172
76.433251	242.055869	4.556365	-0.013842	0.914216
78.641746	251.742338	4.561370	-0.014260	0.929992
79.613362	261.611534	4.566374	-0.014447	0.945451
81.272756	271.301132	4.571379	-0.014763	0.960572
82.254416	281.083253	4.576384	-0.014952	0.975419
84.068645	290.674887	4.581389	-0.015296	0.989976
86.078688	300.172251	4.586394	-0.015677	1.004235
87.628499	309.697843	4.591398	-0.015971	1.018219
89.873919	319.076120	4.596403	-0.016396	1.031976
91.803478	328.452842	4.601408	-0.016761	1.045472
94.416522	337.675340	4.606413	-0.017254	1.058747
100.291438	346.327857	4.611418	-0.018354	1.071847
106.209787	354.996629	4.616422	-0.019461	1.084817
108.715858	364.276599	4.621427	-0.019934	1.097659
110.407072	373.625104	4.626432	-0.020255	1.110259
112.232299	382.875603	4.631437	-0.020601	1.122620
114.466479	392.016569	4.636442	-0.021023	1.134795
116.908097	401.062379	4.641446	-0.021484	1.146765
120.334923	409.924545	4.646451	-0.022128	1.158591
122.849396	418.890397	4.651456	-0.022602	1.170231
124.798069	427.899628	4.656461	-0.022971	1.181689
127.150587	436.812326	4.661466	-0.023415	1.193004
129.340715	445.683900	4.666470	-0.023828	1.204128
131.379658	454.576125	4.671475	-0.024214	1.215144
134.055313	463.303274	4.676480	-0.024718	1.225992
137.829326	471.830645	4.681485	-0.025426	1.236728
141.254575	480.413541	4.686490	-0.026070	1.247366
144.048961	489.088375	4.691494	-0.026596	1.257895
146.918001	497.740223	4.696499	-0.027136	1.268323
149.307281	506.426828	4.701504	-0.027586	1.278613
151.341975	515.163359	4.706509	-0.027971	1.288809
153.371316	523.857053	4.711514	-0.028355	1.298875
155.473762	532.506664	4.716518	-0.028752	1.308827
157.954896	541.117340	4.721523	-0.029219	1.318730
160.328271	549.632479	4.726528	-0.029667	1.328435
162.947930	558.108330	4.731533	-0.030160	1.338071
166.054605	566.501125	4.736538	-0.030744	1.347635
168.328024	575.026295	4.741542	-0.031173	1.357123
170.325644	583.565161	4.746547	-0.031551	1.366509
171.678777	592.207569	4.751552	-0.031809	1.375827
174.406386	600.552553	4.756557	-0.032322	1.385010
177.462867	608.884609	4.761562	-0.032897	1.394175
179.681184	617.322059	4.766566	-0.033315	1.403243
181.900842	625.765456	4.771571	-0.033734	1.412259
183.545674	634.256374	4.776576	-0.034046	1.421168
184.693574	642.826084	4.781581	-0.034266	1.430018
186.013529	651.314492	4.786586	-0.034517	1.438760
187.371436	659.745623	4.791590	-0.034775	1.447397
188.994367	668.149972	4.796595	-0.035083	1.456000
190.129700	676.590421	4.801600	-0.035300	1.464508
191.332504	685.042592	4.806605	-0.035530	1.472989
192.466933	693.430540	4.811610	-0.035746	1.481347
193.894547	701.751280	4.816614	-0.036018	1.489639
195.280402	710.090516	4.821619	-0.036281	1.497896
196.376450	718.437385	4.826624	-0.036491	1.506069
197.495413	726.783047	4.831629	-0.036705	1.514201
198.394141	735.158204	4.836634	-0.036878	1.522282
199.477676	743.453760	4.841638	-0.037085	1.530273
200.693170	751.761160	4.846643	-0.037317	1.538254
202.248084	759.965121	4.851648	-0.037612	1.546148
203.179231	768.325859	4.856653	-0.037791	1.554053
204.764809	776.511546	4.861658	-0.038091	1.561854
205.801812	784.800529	4.866662	-0.038290	1.569629
207.071087	793.067713	4.871667	-0.038532	1.577379
208.167189	801.324324	4.876672	-0.038741	1.585057
209.556329	809.548322	4.881677	-0.039006	1.592710
211.245320	817.705598	4.886682	-0.039325	1.600309
212.532570	825.956977	4.891686	-0.039571	1.607898
213.970862	834.179971	4.896691	-0.039844	1.615447
215.458987	842.379016	4.901696	-0.040126	1.622947
216.871019	850.615983	4.906701	-0.040395	1.630434
218.511642	858.804573	4.911706	-0.040706	1.637876
219.870137	866.978003	4.916710	-0.040964	1.645231
221.541259	875.173048	4.921715	-0.041281	1.652615
223.004478	883.373548	4.926720	-0.041558	1.659942
224.192597	891.616508	4.931725	-0.041785	1.667235
225.465126	899.867342	4.936730	-0.042028	1.674514
226.486023	908.094947	4.941734	-0.042223	1.681707
227.742716	916.296627	4.946739	-0.042463	1.688878
228.865552	924.523760	4.951744	-0.042677	1.696023
229.576729	932.797251	4.956749	-0.042815	1.703121
230.564240	941.027344	4.961754	-0.043004	1.710190
231.154604	949.296727	4.966758	-0.043120	1.717210
232.406629	957.424892	4.971763	-0.043358	1.724170
232.873285	965.716659	4.976768	-0.043451	1.731135
234.488024	973.793268	4.981773	-0.043757	1.738043
235.419576	981.993146	4.986778	-0.043936	1.744937
236.346399	990.196963	4.991782	-0.044114	1.751806
237.161475	998.403936	4.996787	-0.044271	1.758636
237.964352	1006.571053	5.001792	-0.044426	1.765405
239.005435	1014.742209	5.006797	-0.044625	1.772181
239.753068	1022.959049	5.011802	-0.044770	1.778931
240.696441	1031.112665	5.016806	-0.044951	1.785629
241.753265	1039.292478	5.021811	-0.045153	1.792337
242.893340	1047.422349	5.026816	-0.045371	1.798990
244.038009	1055.511805	5.031821	-0.045589	1.805587
244.697582	1063.753182	5.036826	-0.045717	1.812220
245.729809	1071.865102	5.041830	-0.045915	1.818772
246.997919	1079.963515	5.046835	-0.046156	1.825318
248.028455	1088.124342	5.051840	-0.046354	1.831860
248.875637	1096.297721	5.056845	-0.046517	1.838367
250.028608	1104.402953	5.061850	-0.046737	1.844834
250.705151	1112.616414	5.066854	-0.046868	1.851305
251.379577	1120.820883	5.071859	-0.046999	1.857746
252.677721	1128.879113	5.076864	-0.047246	1.864126
253.096699	1137.102636	5.081869	-0.047330	1.870507
253.458052	1145.322715	5.086874	-0.047403	1.876857
254.048772	1153.475441	5.091878	-0.047518	1.883160
254.846902	1161.598774	5.096883	-0.047672	1.889444
255.316827	1169.765114	5.101888	-0.047765	1.895702
256.068387	1177.877840	5.106893	-0.047910	1.901931
257.069789	1186.001457	5.111898	-0.048102	1.908176
257.721097	1194.134434	5.116902	-0.048229	1.914368
258.648817	1202.231609	5.121907	-0.048407	1.920544
259.777747	1210.289473	5.126912	-0.048622	1.926693
260.526636	1218.424403	5.131917	-0.048767	1.932837
261.525066	1226.543821	5.136922	-0.048959	1.938977
262.006968	1234.716196	5.141926	-0.049054	1.945080
263.039584	1242.821616	5.146931	-0.049251	1.951175
263.598638	1250.972204	5.151936	-0.049361	1.957232
264.607892	1259.008252	5.156941	-0.049554	1.963235
265.601607	1267.127300	5.161946	-0.049744	1.969279
265.660614	1275.375009	5.166950	-0.049761	1.975296
266.957860	1283.390482	5.171955	-0.050008	1.981260
267.891166	1291.493569	5.176960	-0.050187	1.987230
268.941042	1299.577610	5.181965	-0.050388	1.993181
269.259617	1307.796939	5.186970	-0.050453	1.999132
270.509904	1315.792929	5.191974	-0.050691	2.005005
271.867322	1323.839896	5.196979	-0.050949	2.010909
272.468505	1332.019680	5.201984	-0.051066	2.016809
273.346527	1340.139209	5.206989	-0.051235	2.022679
274.044009	1348.313308	5.211994	-0.051370	2.028550
274.570868	1356.455789	5.216998	-0.051474	2.034365
275.010148	1364.597263	5.222003	-0.051561	2.040153
276.201752	1372.615611	5.227008	-0.051788	2.045916
277.465521	1380.667002	5.232013	-0.052029	2.051693
278.458063	1388.784672	5.237018	-0.052219	2.057472
279.391818	1396.849212	5.242022	-0.052398	2.063191
279.802589	1405.067262	5.247027	-0.052480	2.068948
280.237289	1413.222550	5.252032	-0.052567	2.074647
281.022621	1421.289947	5.257037	-0.052718	2.080306
282.155131	1429.320448	5.262042	-0.052934	2.085958
282.774663	1437.460001	5.267046	-0.053055	2.091619
282.802684	1445.713213	5.272051	-0.053066	2.097282
283.337267	1453.804332	5.277056	-0.053171	2.102870
284.126586	1461.877690	5.282061	-0.053323	2.108457
285.163490	1469.933075	5.287066	-0.053521	2.114040
285.967839	1477.978831	5.292070	-0.053676	2.119579
286.302999	1486.130028	5.297075	-0.053744	2.125129
286.822529	1494.255591	5.302080	-0.053846	2.130665
287.045160	1502.393969	5.307085	-0.053893	2.136166
288.202748	1510.377734	5.312090	-0.054114	2.141640
288.516181	1518.501607	5.317094	-0.054178	2.147112
288.961117	1526.636707	5.322099	-0.054266	2.152590
288.946988	1534.806630	5.327104	-0.054269	2.158033
289.415698	1542.863408	5.332109	-0.054361	2.163434
289.923584	1550.977277	5.337114	-0.054461	2.168862
290.275826	1559.061078	5.342118	-0.054532	2.174242
291.126588	1567.087242	5.347123	-0.054696	2.179618
291.716633	1575.156028	5.352128	-0.054811	2.184983
292.511562	1583.220739	5.357133	-0.054965	2.190352
293.481421	1591.254760	5.362138	-0.055151	2.195704
293.586920	1599.400560	5.367142	-0.055176	2.201036
294.119882	1607.505688	5.372147	-0.055280	2.206367
294.987010	1615.549210	5.377152	-0.055447	2.211676
295.503814	1623.622410	5.382157	-0.055549	2.216959
296.021388	1631.722885	5.387162	-0.055650	2.222248
296.379705	1639.837383	5.392166	-0.055722	2.227518
296.607760	1648.005706	5.397171	-0.055770	2.232799
296.830167	1656.095815	5.402176	-0.055817	2.238016
297.281958	1664.128441	5.407181	-0.055907	2.243205
297.713789	1672.265166	5.412186	-0.055992	2.248446
298.666251	1680.224707	5.417190	-0.056175	2.253609
299.203482	1688.322548	5.422195	-0.056280	2.258811
299.734857	1696.394740	5.427200	-0.056385	2.263984
299.836819	1704.555431	5.432205	-0.056409	2.269163
300.383223	1712.667387	5.437210	-0.056516	2.274338
300.611291	1720.742051	5.442214	-0.056564	2.279451
301.856744	1728.659723	5.447219	-0.056801	2.284541
302.561908	1736.734950	5.452224	-0.056938	2.289672
303.077213	1744.824857	5.457229	-0.057039	2.294784
303.749444	1752.900520	5.462234	-0.057170	2.299890
304.084207	1760.993007	5.467238	-0.057237	2.304965
304.875168	1769.046573	5.472243	-0.057390	2.310044
305.420147	1777.131592	5.477248	-0.057497	2.315110
305.933367	1785.188367	5.482253	-0.057598	2.320145
306.550828	1793.268447	5.487258	-0.057718	2.325192
307.128692	1801.321775	5.492262	-0.057831	2.330207
307.581522	1809.439405	5.497267	-0.057921	2.335242
307.688258	1817.591052	5.502272	-0.057946	2.340257
307.975562	1825.657640	5.507277	-0.058005	2.345224
308.862654	1833.693421	5.512282	-0.058175	2.350212
309.408310	1841.742055	5.517286	-0.058282	2.355168
309.976566	1849.785971	5.522291	-0.058393	2.360113
310.169938	1857.885589	5.527296	-0.058435	2.365050
310.907222	1865.923300	5.532301	-0.058577	2.369985
311.494998	1874.003887	5.537306	-0.058692	2.374922
311.654954	1882.107377	5.542310	-0.058727	2.379828
312.119725	1890.166694	5.547315	-0.058819	2.384722
312.732771	1898.228152	5.552320	-0.058939	2.389619
313.101968	1906.288273	5.557325	-0.059013	2.394486
313.659053	1914.372475	5.562330	-0.059122	2.399372
313.900042	1922.437941	5.567334	-0.059172	2.404212
313.958295	1930.594297	5.572339	-0.059188	2.409081
314.348204	1938.649958	5.577344	-0.059266	2.413907
314.292441	1946.776410	5.582349	-0.059261	2.418730
314.422238	1954.851401	5.587354	-0.059291	2.423528
314.691203	1962.910528	5.592358	-0.059346	2.428317
315.028989	1971.007581	5.597363	-0.059415	2.433125
315.748663	1978.956808	5.602368	-0.059554	2.437866
316.136509	1986.973061	5.607373	-0.059631	2.442611
316.950331	1994.984293	5.612378	-0.059788	2.447377
317.231163	2003.081187	5.617382	-0.059846	2.452143
317.625728	2011.153929	5.622387	-0.059925	2.456894
317.625601	2019.260469	5.627392	-0.059930	2.461625
317.313086	2027.426855	5.632397	-0.059877	2.466358
318.099915	2035.440673	5.637402	-0.060029	2.471077
318.795194	2043.383489	5.642406	-0.060164	2.475739
319.497049	2051.408587	5.647411	-0.060300	2.480440
319.851027	2059.490454	5.652416	-0.060371	2.485138
319.883994	2067.632941	5.657421	-0.060383	2.489839
321.059892	2075.594901	5.662426	-0.060607	2.494512
321.370952	2083.670791	5.667430	-0.060670	2.499177
321.891811	2091.723321	5.672435	-0.060772	2.503835
322.319422	2099.815822	5.677440	-0.060857	2.508501
323.110576	2107.814046	5.682445	-0.061010	2.513131
323.599376	2115.894242	5.687450	-0.061106	2.517777
323.859980	2123.954626	5.692454	-0.061160	2.522386
324.246722	2132.024407	5.697459	-0.061238	2.527001
324.624312	2140.118908	5.702464	-0.061313	2.531621
324.923004	2148.180632	5.707469	-0.061374	2.536208
325.681169	2156.187757	5.712474	-0.061521	2.540789
326.076806	2164.223813	5.717478	-0.061600	2.545352
326.579115	2172.321665	5.722483	-0.061699	2.549949
326.291912	2180.501550	5.727488	-0.061651	2.554527
326.905246	2188.473493	5.732493	-0.061770	2.559045
327.645517	2196.458271	5.737498	-0.061913	2.563571
327.391093	2204.606847	5.742502	-0.061871	2.568110
327.507928	2212.710025	5.747507	-0.061898	2.572642
327.857500	2220.763344	5.752512	-0.061969	2.577154
328.034027	2228.810464	5.757517	-0.062007	2.581643
328.778602	2236.815775	5.762522	-0.062151	2.586141
329.036732	2244.916793	5.767526	-0.062204	2.590649
329.390740	2253.049677	5.772531	-0.062276	2.595174
329.478196	2261.088480	5.777536	-0.062297	2.599621
329.580749	2269.110317	5.782541	-0.062322	2.604052
330.096622	2277.105485	5.787546	-0.062423	2.608489
330.288776	2285.156480	5.792550	-0.062464	2.612926
330.517497	2293.216724	5.797555	-0.062512	2.617364
331.141865	2301.209536	5.802560	-0.062634	2.621784
331.050947	2309.320089	5.807565	-0.062622	2.626213
331.550670	2317.363463	5.812570	-0.062721	2.630637
331.687251	2325.423874	5.817574	-0.062751	2.635039
332.254730	2333.412611	5.822579	-0.062862	2.639423
332.271599	2341.506364	5.827584	-0.062871	2.643820
332.239860	2349.602898	5.832589	-0.062870	2.648208
333.578665	2357.533528	5.837594	-0.063125	2.652590
334.118456	2365.558774	5.842598	-0.063231	2.656963
334.842713	2373.590546	5.847603	-0.063371	2.661344
335.026925	2381.687736	5.852608	-0.063411	2.665717
335.113331	2389.809158	5.857613	-0.063432	2.670090
336.113038	2397.765928	5.862618	-0.063623	2.674427
336.586177	2405.784756	5.867622	-0.063717	2.678755
336.963967	2413.852405	5.872627	-0.063793	2.683097
337.929410	2421.845469	5.877632	-0.063978	2.687430
338.126219	2429.951248	5.882637	-0.064020	2.691765
339.001034	2437.976838	5.887642	-0.064188	2.696095
338.976243	2446.094226	5.892646	-0.064189	2.700409
339.586799	2454.103625	5.897651	-0.064308	2.704699
339.679596	2462.225748	5.902656	-0.064330	2.709009
340.253380	2470.232040	5.907661	-0.064442	2.713282
340.597730	2478.287769	5.912666	-0.064512	2.717559
340.859731	2486.308231	5.917670	-0.064566	2.721805
341.293468	2494.386649	5.922675	-0.064652	2.726086
341.541450	2502.475305	5.927680	-0.064704	2.730355
341.608306	2510.538895	5.932685	-0.064721	2.734591
342.297952	2518.549070	5.937690	-0.064855	2.738833
342.613969	2526.578364	5.942694	-0.064919	2.743054
342.919241	2534.638837	5.947699	-0.064981	2.747284
343.365073	2542.719787	5.952704	-0.065070	2.751527
343.545983	2550.787291	5.957709	-0.065109	2.755741
343.941511	2558.809414	5.962714	-0.065188	2.759937
344.434902	2566.768035	5.967718	-0.065285	2.764100
344.558993	2574.878921	5.972723	-0.065313	2.768313
344.534736	2583.001002	5.977728	-0.065314	2.772516
345.243703	2590.947657	5.982733	-0.065452	2.776666
345.687083	2598.980765	5.987738	-0.065540	2.780839
346.082963	2606.999631	5.992742	-0.065619	2.784996
345.831415	2615.142263	5.997747	-0.065577	2.789170
345.968901	2623.221127	6.002752	-0.065608	2.793329
346.125960	2631.239193	6.007757	-0.065643	2.797452
346.254887	2639.300513	6.012762	-0.065672	2.801590
346.358258	2647.320606	6.017766	-0.065697	2.805698
346.990645	2655.320520	6.022771	-0.065820	2.809822
347.389813	2663.373033	6.027776	-0.065899	2.813952
347.417177	2671.432124	6.032781	-0.065910	2.818058
348.051547	2679.434169	6.037786	-0.066033	2.822164
348.257701	2687.482184	6.042790	-0.066077	2.826263
348.653331	2695.535002	6.047795	-0.066156	2.830369
348.883143	2703.575585	6.052800	-0.066204	2.834453
349.214515	2711.596484	6.057805	-0.066271	2.838527
349.691322	2719.630406	6.062810	-0.066365	2.842611
349.616242	2727.714404	6.067814	-0.066356	2.846681
349.644453	2735.816161	6.072819	-0.066367	2.850761
349.688642	2743.858737	6.077824	-0.066381	2.854806
349.795390	2751.894439	6.082829	-0.066406	2.858846
350.483669	2759.868744	6.087834	-0.066539	2.862882
350.608510	2767.944716	6.092838	-0.066568	2.866931
350.625839	2776.034337	6.097843	-0.066577	2.870976
350.897651	2784.065974	6.102848	-0.066632	2.874999
351.079551	2792.045183	6.107853	-0.066672	2.878987
351.348593	2800.089785	6.112858	-0.066727	2.883006
351.341767	2808.179257	6.117862	-0.066731	2.887026
351.953124	2816.191838	6.122867	-0.066850	2.891037
352.324675	2824.223180	6.127872	-0.066925	2.895038
352.648271	2832.197976	6.132877	-0.066990	2.899003
353.138928	2840.226561	6.137882	-0.067087	2.902998
353.460060	2848.291679	6.142886	-0.067152	2.906996
352.743844	2856.535942	6.147891	-0.067024	2.911021
352.707406	2864.597784	6.152896	-0.067023	2.914987
353.261635	2872.509865	6.157901	-0.067131	2.918906
354.031592	2880.449140	6.162906	-0.067280	2.922845
353.910041	2888.531675	6.167910	-0.067263	2.926801
353.935872	2896.624811	6.172915	-0.067273	2.930764
354.746451	2904.559585	6.177920	-0.067429	2.934687
354.681039	2912.613701	6.182925	-0.067422	2.938616
355.278920	2920.628981	6.187930	-0.067539	2.942556
355.585342	2928.682710	6.192934	-0.067601	2.946493
355.794310	2936.765090	6.197939	-0.067645	2.950435
356.219153	2944.772474	6.202944	-0.067730	2.954345
356.456383	2952.811752	6.207949	-0.067779	2.958257
356.717060	2960.843777	6.212954	-0.067833	2.962160
356.698879	2968.929035	6.217958	-0.067835	2.966070
357.247339	2976.909986	6.222963	-0.067943	2.969954
357.524967	2984.994392	6.227968	-0.068000	2.973868
357.417953	2993.062971	6.232973	-0.067985	2.977750
357.718514	3001.099482	6.237978	-0.068046	2.981632
358.284903	3009.062824	6.242982	-0.068157	2.985488
358.312695	3017.171970	6.247987	-0.068168	2.989381
358.643321	3025.226715	6.252992	-0.068235	2.993258
358.798570	3033.222702	6.257997	-0.068269	2.997093
359.197896	3041.267701	6.263002	-0.068349	3.000959
359.747269	3049.227492	6.268006	-0.068456	3.004787
359.921514	3057.297853	6.273011	-0.068494	3.008643
360.140432	3065.344409	6.278016	-0.068540	3.012486
360.359263	3073.393489	6.283021	-0.068586	3.016325
360.690324	3081.435830	6.288026	-0.068653	3.020161
361.057582	3089.413633	6.293030	-0.068727	3.023964
361.135728	3097.500023	6.298035	-0.068747	3.027798
361.324083	3105.581175	6.303040	-0.068787	3.031631
362.014392	3113.544011	6.308045	-0.068921	3.035428
362.141880	3121.589980	6.313050	-0.068950	3.039232
362.591830	3129.557412	6.318054	-0.069039	3.043009
362.820827	3137.643626	6.323059	-0.069087	3.046827
363.253545	3145.698979	6.328064	-0.069173	3.050636
363.481338	3153.747329	6.333069	-0.069221	3.054426
363.583926	3161.804128	6.338074	-0.069245	3.058210
363.550321	3169.872385	6.343078	-0.069244	3.061987
363.872982	3177.889764	6.348083	-0.069310	3.065754
364.086801	3185.941100	6.353088	-0.069355	3.069526
364.634021	3193.962134	6.358093	-0.069462	3.073296
364.922310	3202.009171	6.363098	-0.069521	3.077060
365.188228	3210.010801	6.368102	-0.069576	3.080798
365.376108	3218.032962	6.373107	-0.069616	3.084537
365.679668	3226.058533	6.378112	-0.069678	3.088278
365.815949	3234.092187	6.383117	-0.069709	3.092011
366.013834	3242.190051	6.388122	-0.069751	3.095772
365.993506	3250.192420	6.393126	-0.069752	3.099473
366.227834	3258.222488	6.398131	-0.069801	3.103195
366.197811	3266.322895	6.403136	-0.069801	3.106933
366.148950	3274.386163	6.408141	-0.069797	3.110648
366.897210	3282.326524	6.413146	-0.069942	3.114339
366.999341	3290.326709	6.418150	-0.069966	3.118024
367.313203	3298.343051	6.423155	-0.070030	3.121721
367.492515	3306.402963	6.428160	-0.070069	3.125427
368.006227	3314.379134	6.433165	-0.070170	3.129106
367.903519	3322.519946	6.438170	-0.070156	3.132828
368.337426	3330.504917	6.443174	-0.070242	3.136498
368.885607	3338.505899	6.448179	-0.070349	3.140177
368.857525	3346.575750	6.453184	-0.070350	3.143857
369.004568	3354.610975	6.458189	-0.070382	3.147524
369.289334	3362.706578	6.463194	-0.070441	3.151221
369.212556	3370.744389	6.468198	-0.070432	3.154871
369.151168	3378.771385	6.473203	-0.070426	3.158512
369.312458	3386.785756	6.478208	-0.070461	3.162154
369.255820	3394.825292	6.483213	-0.070456	3.165793
369.308128	3402.891021	6.488218	-0.070471	3.169444
369.466635	3410.892125	6.493222	-0.070506	3.173067
369.856995	3418.901327	6.498227	-0.070584	3.176700
370.171407	3426.925205	6.503232	-0.070648	3.180331
370.321245	3434.895312	6.508237	-0.070681	3.183927
370.816295	3442.963999	6.513242	-0.070778	3.187578
371.480726	3450.940314	6.518246	-0.070907	3.191191
371.899228	3458.962948	6.523251	-0.070990	3.194810
371.199017	3467.177813	6.528256	-0.070866	3.198462
371.402832	3475.130732	6.533261	-0.070909	3.202032
371.739670	3483.154612	6.538266	-0.070977	3.205635
372.133122	3491.118655	6.543270	-0.071055	3.209211
372.124427	3499.210665	6.548275	-0.071059	3.212821
372.618321	3507.257598	6.553280	-0.071156	3.216430
372.825838	3515.230903	6.558285	-0.071200	3.219989
373.036030	3523.292949	6.563290	-0.071245	3.223583
372.868947	3531.405450	6.568294	-0.071219	3.227180
373.085453	3539.444933	6.573299	-0.071265	3.230757
373.822151	3547.342921	6.578304	-0.071407	3.234289
374.048620	3555.380457	6.583309	-0.071455	3.237858
374.440959	3563.393043	6.588314	-0.071533	3.241418
374.650364	3571.425416	6.593318	-0.071577	3.244976
375.309946	3579.409760	6.598323	-0.071705	3.248527
375.336606	3587.520331	6.603328	-0.071716	3.252103
375.293057	3595.585384	6.608333	-0.071713	3.255653
375.689796	3603.583518	6.613338	-0.071792	3.259187
375.888247	3611.616743	6.618342	-0.071834	3.262725
375.883653	3619.674730	6.623347	-0.071839	3.266262
376.188608	3627.698628	6.628352	-0.071901	3.269792
376.399117	3635.700114	6.633357	-0.071946	3.273305
376.267998	3643.806689	6.638362	-0.071927	3.276846
376.281538	3651.833654	6.643366	-0.071934	3.280355
376.495671	3659.795051	6.648371	-0.071980	3.283839
376.887456	3667.831160	6.653376	-0.072058	3.287359
376.815071	3675.894013	6.658381	-0.072050	3.290868
377.335422	3683.882097	6.663386	-0.072152	3.294365
377.776277	3691.873209	6.668390	-0.072239	3.297856
378.267441	3699.869173	6.673395	-0.072336	3.301347
378.273141	3707.980375	6.678400	-0.072342	3.304866
378.793880	3715.977369	6.683405	-0.072445	3.308351
378.687405	3724.101559	6.688410	-0.072430	3.311864
378.467515	3732.181660	6.693414	-0.072395	3.315349
378.663821	3740.154047	6.698419	-0.072437	3.318800
378.907457	3748.159561	6.703424	-0.072487	3.322263
379.273992	3756.111860	6.708429	-0.072561	3.325705
379.772078	3764.113831	6.713434	-0.072659	3.329169
380.097523	3772.159326	6.718438	-0.072725	3.332642
380.141177	3780.249983	6.723443	-0.072738	3.336120
380.488832	3788.266921	6.728448	-0.072808	3.339574
380.456170	3796.305490	6.733453	-0.072808	3.343020
380.548108	3804.373463	6.738458	-0.072830	3.346479
380.381180	3812.449212	6.743462	-0.072804	3.349928
380.542250	3820.436503	6.748467	-0.072840	3.353348
381.220433	3828.413148	6.753472	-0.072971	3.356780
381.327518	3836.420290	6.758477	-0.072996	3.360199
381.543160	3844.429862	6.763482	-0.073042	3.363620
381.965325	3852.431226	6.768486	-0.073126	3.367042
382.107465	3860.534989	6.773491	-0.073158	3.370493
382.246445	3868.568732	6.778496	-0.073189	3.373911
382.340781	3876.595410	6.783501	-0.073212	3.377321
382.585377	3884.648263	6.788506	-0.073263	3.380744
382.791126	3892.617596	6.793510	-0.073306	3.384127
383.046941	3900.683740	6.798515	-0.073359	3.387549
383.289986	3908.745960	6.803520	-0.073410	3.390965
383.289151	3916.792849	6.808525	-0.073415	3.394363
383.468093	3924.816218	6.813530	-0.073454	3.397754
383.711566	3932.845921	6.818534	-0.073504	3.401146
384.019154	3940.790777	6.823539	-0.073567	3.404502
383.865598	3948.878410	6.828544	-0.073544	3.407898
383.931887	3956.939151	6.833549	-0.073561	3.411287
384.591292	3964.906698	6.838554	-0.073689	3.414654
384.680336	3972.918382	6.843558	-0.073711	3.418016
384.937535	3980.948531	6.848563	-0.073764	3.421389
385.345993	3988.959168	6.853568	-0.073846	3.424755
385.509572	3997.000538	6.858573	-0.073882	3.428123
385.716662	4005.073207	6.863578	-0.073925	3.431501
386.010568	4013.065132	6.868582	-0.073985	3.434846
386.076215	4021.077139	6.873587	-0.074003	3.438188
386.141013	4029.137555	6.878592	-0.074020	3.441547
386.177879	4037.124088	6.883597	-0.074033	3.444870
386.651291	4045.162153	6.888602	-0.074126	3.448227
386.823953	4053.220899	6.893606	-0.074164	3.451579
387.286930	4061.193792	6.898611	-0.074255	3.454902
387.501236	4069.248390	6.903616	-0.074300	3.458246
387.380652	4077.286845	6.908621	-0.074283	3.461570
387.473023	4085.328524	6.913626	-0.074306	3.464899
387.607838	4093.376818	6.918630	-0.074336	3.468229
387.811085	4101.394850	6.923635	-0.074379	3.471546
387.993023	4109.400403	6.928640	-0.074418	3.474853
388.476053	4117.347766	6.933645	-0.074514	3.478143
388.885626	4125.399084	6.938650	-0.074595	3.481471
388.619061	4133.438731	6.943654	-0.074551	3.484768
388.493708	4141.514900	6.948659	-0.074533	3.488082
388.985968	4149.527442	6.953664	-0.074630	3.491386
389.210636	4157.547741	6.958669	-0.074677	3.494682
389.339156	4165.590968	6.963674	-0.074706	3.497981
389.477207	4173.612862	6.968678	-0.074737	3.501269
389.855455	4181.594397	6.973683	-0.074813	3.504544
390.093322	4189.668796	6.978688	-0.074863	3.507850
390.078574	4197.716409	6.983693	-0.074865	3.511134
390.414831	4205.726464	6.988698	-0.074933	3.514410
390.569454	4213.706961	6.993702	-0.074967	3.517666
390.320204	4221.806973	6.998707	-0.074926	3.520954
390.742397	4229.763186	7.003712	-0.075010	3.524202
390.685342	4237.839435	7.008717	-0.075005	3.527481
391.048946	4245.858338	7.013722	-0.075078	3.530747
391.533454	4253.810036	7.018726	-0.075173	3.533986
391.797456	4261.850219	7.023731	-0.075228	3.537251
391.906143	4269.938431	7.028736	-0.075254	3.540527
391.627278	4277.966506	7.033741	-0.075207	3.543765
392.326560	4285.955761	7.038746	-0.075342	3.547013
392.516656	4293.996074	7.043750	-0.075383	3.550264
392.764647	4302.059597	7.048755	-0.075435	3.553523
392.900173	4310.091861	7.053760	-0.075465	3.556762
393.062354	4318.038701	7.058765	-0.075501	3.559966
392.840240	4326.095529	7.063770	-0.075465	3.563198
393.175596	4334.071037	7.068774	-0.075532	3.566413
393.169814	4342.139392	7.073779	-0.075537	3.569651
393.530817	4350.152606	7.078784	-0.075609	3.572875
393.368825	4358.217684	7.083789	-0.075584	3.576101
394.178047	4366.143621	7.088794	-0.075740	3.579298
394.417421	4374.169273	7.093798	-0.075790	3.582514
394.534387	4382.219908	7.098803	-0.075817	3.585734
394.743309	4390.292966	7.103808	-0.075862	3.588963
395.166764	4398.277728	7.108813	-0.075946	3.592160
395.416397	4406.299021	7.113818	-0.075998	3.595364
395.217455	4414.374544	7.118822	-0.075966	3.598573
395.569479	4422.378495	7.123827	-0.076037	3.601766
395.290815	4430.476503	7.128832	-0.075990	3.604977
395.556303	4438.443767	7.133837	-0.076045	3.608148
395.914775	4446.491745	7.138842	-0.076117	3.611350
396.416461	4454.453161	7.143846	-0.076216	3.614520
396.516517	4462.447571	7.148851	-0.076240	3.617689
396.685543	4470.571982	7.153856	-0.076277	3.620908
396.730989	4478.502375	7.158861	-0.076290	3.624044
396.626768	4486.648860	7.163866	-0.076276	3.627258
397.024334	4494.627470	7.168870	-0.076356	3.630418
397.037488	4502.652412	7.173875	-0.076363	3.633582
397.386063	4510.653460	7.178880	-0.076434	3.636743
397.537951	4518.629502	7.183885	-0.076467	3.639886
397.471440	4526.690654	7.188890	-0.076460	3.643054
397.819262	4534.712196	7.193894	-0.076530	3.646215
398.104023	4542.704701	7.198899	-0.076589	3.649360
398.144720	4550.801726	7.203904	-0.076601	3.652537
398.094942	4558.827639	7.208909	-0.076598	3.655681
398.452131	4566.793075	7.213914	-0.076669	3.658809
398.024973	4574.891707	7.218918	-0.076595	3.661965
398.585543	4582.818608	7.223923	-0.076705	3.665078
398.781035	4590.904038	7.228928	-0.076747	3.668241
399.436411	4598.862476	7.233933	-0.076874	3.671364
399.702604	4606.897920	7.238938	-0.076929	3.674503
399.796796	4614.928055	7.243942	-0.076952	3.677633
399.838565	4622.973468	7.248947	-0.076965	3.680765
400.252162	4630.953110	7.253952	-0.077047	3.683879
400.546482	4638.991188	7.258957	-0.077107	3.687009
400.640166	4647.054614	7.263962	-0.077130	3.690142
400.873995	4655.055102	7.268966	-0.077179	3.693251
400.891972	4663.116432	7.273971	-0.077187	3.696375
401.239219	4671.152874	7.278976	-0.077257	3.699495
401.271314	4679.125256	7.283981	-0.077269	3.702580
401.397151	4687.208776	7.288986	-0.077298	3.705708
401.638673	4695.219532	7.293990	-0.077348	3.708807
401.613951	4703.287099	7.298995	-0.077349	3.711920
402.241739	4711.283552	7.304000	-0.077471	3.715019
402.260363	4719.287307	7.309005	-0.077480	3.718102
402.263171	4727.349070	7.314010	-0.077485	3.721205
402.390672	4735.264042	7.319014	-0.077514	3.724252
402.703592	4743.317342	7.324019	-0.077578	3.727355
402.977433	4751.390614	7.329024	-0.077634	3.730461
403.082769	4759.380704	7.334029	-0.077659	3.733529
403.585747	4767.392473	7.339034	-0.077758	3.736612
403.879689	4775.411506	7.344038	-0.077818	3.739690
403.861360	4783.411626	7.349043	-0.077820	3.742751
404.143173	4791.460347	7.354048	-0.077878	3.745835
404.136917	4799.491706	7.359053	-0.077882	3.748903
404.158297	4807.561437	7.364058	-0.077891	3.751984
404.392515	4815.555529	7.369062	-0.077940	3.755039
404.828890	4823.501657	7.374067	-0.078027	3.758077
405.024394	4831.591000	7.379072	-0.078069	3.761162
405.327136	4839.521077	7.384077	-0.078130	3.764186
405.216423	4847.665971	7.389082	-0.078115	3.767280
405.139668	4855.682188	7.394086	-0.078106	3.770323
405.237812	4863.713716	7.399091	-0.078130	3.773374
405.789725	4871.703864	7.404096	-0.078238	3.776417
405.662420	4879.708935	7.409101	-0.078219	3.779447
405.870598	4887.740113	7.414106	-0.078263	3.782492
405.995247	4895.773916	7.419110	-0.078292	3.785534
406.448682	4903.741212	7.424115	-0.078382	3.788557
406.396453	4911.853470	7.429120	-0.078377	3.791619
406.828176	4919.803762	7.434125	-0.078463	3.794629
406.930344	4927.853456	7.439130	-0.078487	3.797667
407.037764	4935.869540	7.444134	-0.078513	3.800690
407.375932	4943.812605	7.449139	-0.078581	3.803688
407.410155	4951.933133	7.454144	-0.078593	3.806743
407.364217	4959.939539	7.459149	-0.078589	3.809752
408.147987	4967.914349	7.464154	-0.078741	3.812765
408.026692	4976.013779	7.469158	-0.078723	3.815801
408.169195	4983.961533	7.474163	-0.078755	3.818785
408.703327	4992.031620	7.479168	-0.078860	3.821820
408.804186	4999.976229	7.484173	-0.078884	3.824797
408.722281	5008.101456	7.489178	-0.078874	3.827834
408.833741	5016.183351	7.494182	-0.078900	3.830858
408.966774	5024.089803	7.499187	-0.078930	3.833814
408.982615	5032.207577	7.504192	-0.078939	3.836844
409.276608	5040.114649	7.509197	-0.078999	3.839799
409.641028	5048.154635	7.514202	-0.079072	3.842802
409.613333	5056.226171	7.519206	-0.079072	3.845807
409.796673	5064.197881	7.524211	-0.079111	3.848777
410.252704	5072.269461	7.529216	-0.079202	3.851787
410.189768	5080.259422	7.534221	-0.079195	3.854753
410.286267	5088.296952	7.539226	-0.079219	3.857739
410.642650	5096.335310	7.544230	-0.079290	3.860727
410.878875	5104.294973	7.549235	-0.079340	3.863682
410.897790	5112.395353	7.554240	-0.079348	3.866682
411.171151	5120.381430	7.559245	-0.079405	3.869642
411.383327	5128.497963	7.564250	-0.079450	3.872648
411.586709	5136.552067	7.569254	-0.079493	3.875627
411.713391	5144.439044	7.574259	-0.079522	3.878541
412.005981	5152.507430	7.579264	-0.079581	3.881524
411.918740	5160.465790	7.584269	-0.079570	3.884455
412.257284	5168.503450	7.589274	-0.079639	3.887422
412.427864	5176.513303	7.594278	-0.079676	3.890373
412.652965	5184.500022	7.599283	-0.079723	3.893315
412.856977	5192.598573	7.604288	-0.079766	3.896295
412.559500	5200.562966	7.609293	-0.079716	3.899213
412.802438	5208.610496	7.614298	-0.079767	3.902171
413.020767	5216.600822	7.619302	-0.079813	3.905105
413.359422	5224.607020	7.624307	-0.079881	3.908044
413.600122	5232.657894	7.629312	-0.079931	3.910996
413.489186	5240.656785	7.634317	-0.079916	3.913920
413.777759	5248.735331	7.639322	-0.079975	3.916878
413.767014	5256.709333	7.644326	-0.079978	3.919791
413.981298	5264.687722	7.649331	-0.080024	3.922706
414.256456	5272.766591	7.654336	-0.080080	3.925658
414.065647	5280.801387	7.659341	-0.080050	3.928582
414.597189	5288.810596	7.664346	-0.080154	3.931509
415.091611	5296.811621	7.669350	-0.080252	3.934430
414.861282	5304.850141	7.674355	-0.080214	3.937348
415.162461	5312.897337	7.679360	-0.080276	3.940277
415.456804	5320.861542	7.684365	-0.080336	3.943174
415.478601	5328.917075	7.689370	-0.080345	3.946097
415.526412	5336.987615	7.694374	-0.080359	3.949024
415.515626	5345.078340	7.699379	-0.080363	3.951954
415.782290	5353.046349	7.704384	-0.080418	3.954843
416.116017	5360.985857	7.709389	-0.080485	3.957721
416.394349	5369.018741	7.714394	-0.080542	3.960630
416.484322	5376.996989	7.719398	-0.080564	3.963513
416.657996	5384.998576	7.724403	-0.080602	3.966404
416.694528	5393.080401	7.729408	-0.080614	3.969319
416.706320	5401.105277	7.734413	-0.080621	3.972211
416.951586	5409.154064	7.739418	-0.080672	3.975114
417.050457	5417.127464	7.744422	-0.080696	3.977985
417.277801	5425.176860	7.749427	-0.080744	3.980884
417.039224	5433.199154	7.754432	-0.080705	3.983762
417.169382	5441.185894	7.759437	-0.080734	3.986632
417.470785	5449.198954	7.764442	-0.080796	3.989513
417.742563	5457.225454	7.769446	-0.080852	3.992395
417.920447	5465.244045	7.774451	-0.080890	3.995271
418.071558	5473.254936	7.779456	-0.080924	3.998142
418.260262	5481.281230	7.784461	-0.080964	4.001017
418.406545	5489.234136	7.789466	-0.080997	4.003862
418.558967	5497.327109	7.794470	-0.081030	4.006756
418.379563	5505.359251	7.799475	-0.081002	4.009621
418.498278	5513.404229	7.804480	-0.081030	4.012492
418.268706	5521.436099	7.809485	-0.080992	4.015352
418.297268	5529.445055	7.814490	-0.081003	4.018205
418.631615	5537.499213	7.819494	-0.081070	4.021078
418.802800	5545.373579	7.824499	-0.081108	4.023882
419.066718	5553.490032	7.829504	-0.081162	4.026771
419.207173	5561.491417	7.834509	-0.081194	4.029616
419.451927	5569.566848	7.839514	-0.081244	4.032486
419.248695	5577.633037	7.844518	-0.081212	4.035344
419.466525	5585.563570	7.849523	-0.081258	4.038158
420.059579	5593.580906	7.854528	-0.081374	4.041008
420.209389	5601.514386	7.859533	-0.081407	4.043818
420.346251	5609.621793	7.864538	-0.081438	4.046688
420.508620	5617.611962	7.869542	-0.081473	4.049514
420.786964	5625.611560	7.874547	-0.081530	4.052344
420.902862	5633.690310	7.879552	-0.081557	4.055197
420.944014	5641.724917	7.884557	-0.081570	4.058032
421.045430	5649.742186	7.889562	-0.081594	4.060859
420.909832	5657.751331	7.894566	-0.081574	4.063678
420.574651	5665.836634	7.899571	-0.081517	4.066519
421.087103	5673.791045	7.904576	-0.081618	4.069324
421.391097	5681.812423	7.909581	-0.081680	4.072148
421.534319	5689.824054	7.914586	-0.081712	4.074964
421.922640	5697.847024	7.919590	-0.081790	4.077786
421.905208	5705.830343	7.924595	-0.081792	4.080586
421.964297	5713.852496	7.929600	-0.081808	4.083398
422.289694	5721.903964	7.934605	-0.081874	4.086223
422.615676	5729.893311	7.939610	-0.081940	4.089024
422.177797	5738.016029	7.944614	-0.081864	4.091859
422.019269	5745.974655	7.949619	-0.081839	4.094638
422.547187	5753.993906	7.954624	-0.081943	4.097447
422.627037	5761.975259	7.959629	-0.081963	4.100234
422.597277	5770.022899	7.964634	-0.081963	4.103041
422.795534	5778.051687	7.969638	-0.082005	4.105842
423.367814	5786.001217	7.974643	-0.082117	4.108619
423.666460	5794.091032	7.979648	-0.082178	4.111439
423.303349	5802.079754	7.984653	-0.082116	4.114213
423.587398	5810.103130	7.989658	-0.082174	4.117006
423.735164	5818.104139	7.994662	-0.082207	4.119787
423.963754	5826.066999	7.999667	-0.082255	4.122555
424.215335	5834.137952	8.004672	-0.082307	4.125358
424.241900	5842.125869	8.009677	-0.082317	4.128127
424.220827	5850.206632	8.014682	-0.082319	4.130927
424.414690	5858.203503	8.019686	-0.082360	4.133698
424.711297	5866.201936	8.024691	-0.082420	4.136469
424.754931	5874.275919	8.029696	-0.082434	4.139261
424.984291	5882.250792	8.034701	-0.082482	4.142019
425.300420	5890.233275	8.039706	-0.082546	4.144779
425.310271	5898.295940	8.044710	-0.082553	4.147561
425.229304	5906.332963	8.049715	-0.082544	4.150331
425.685872	5914.325687	8.054720	-0.082634	4.153091
425.509800	5922.371513	8.059725	-0.082606	4.155860
425.851998	5930.338471	8.064730	-0.082675	4.158605
425.854705	5938.443894	8.069734	-0.082681	4.161393
425.970199	5946.346231	8.074739	-0.082708	4.164110
426.221651	5954.438988	8.079744	-0.082760	4.166892
426.168608	5962.447077	8.084749	-0.082756	4.169640
426.410610	5970.492804	8.089754	-0.082806	4.172402
426.390184	5978.485765	8.094758	-0.082808	4.175141
426.684282	5986.497600	8.099763	-0.082868	4.177889
426.505691	5994.627071	8.104768	-0.082840	4.180669
426.413430	6002.597301	8.109773	-0.082828	4.183395
426.408756	6010.640949	8.114778	-0.082832	4.186144
426.772226	6018.600516	8.119782	-0.082905	4.188868
426.890530	6026.650594	8.124787	-0.082933	4.191617
426.955762	6034.714216	8.129792	-0.082950	4.194369
427.143369	6042.664555	8.134797	-0.082990	4.197082
427.328235	6050.649545	8.139802	-0.083030	4.199804
427.409466	6058.692771	8.144806	-0.083050	4.202544
427.575903	6066.651281	8.149811	-0.083087	4.205254
427.628521	6074.748232	8.154816	-0.083102	4.208008
428.052015	6082.707000	8.159821	-0.083186	4.210717
427.998850	6090.757339	8.164826	-0.083182	4.213450
428.352876	6098.832898	8.169830	-0.083253	4.216195
428.306871	6106.783959	8.174835	-0.083249	4.218891
428.700247	6114.821933	8.179840	-0.083328	4.221620
428.468204	6122.818680	8.184845	-0.083290	4.224326
428.912822	6130.842552	8.189850	-0.083378	4.227047
429.062018	6138.869014	8.194854	-0.083411	4.229763
429.170308	6146.876110	8.199859	-0.083437	4.232471
429.055200	6154.951668	8.204864	-0.083421	4.235198
429.566754	6162.863326	8.209869	-0.083521	4.237875
429.624481	6170.915282	8.214874	-0.083537	4.240592
429.808930	6178.929697	8.219878	-0.083577	4.243297
430.010817	6186.946931	8.224883	-0.083620	4.246000
430.116938	6195.004685	8.229888	-0.083645	4.248715
430.157272	6203.025981	8.234893	-0.083658	4.251415
430.213837	6210.975781	8.239898	-0.083674	4.254089
430.548948	6219.059037	8.244902	-0.083741	4.256809
430.232038	6227.051297	8.249907	-0.083688	4.259491
430.473675	6235.103959	8.254912	-0.083738	4.262196
430.349259	6243.129533	8.259917	-0.083720	4.264887
430.574827	6251.132453	8.264922	-0.083768	4.267573
430.656756	6259.170680	8.269926	-0.083788	4.270267
430.730218	6267.143379	8.274931	-0.083807	4.272937
431.138962	6275.177064	8.279936	-0.083888	4.275629
431.128302	6283.141707	8.284941	-0.083892	4.278292
430.866648	6291.215413	8.289946	-0.083848	4.280988
431.041001	6299.255067	8.294950	-0.083886	4.283675
430.692983	6307.242928	8.299955	-0.083827	4.286338
430.994751	6315.271464	8.304960	-0.083888	4.289019
430.848231	6323.324649	8.309965	-0.083866	4.291702
431.468965	6331.255570	8.314970	-0.083987	4.294350
431.496809	6339.327347	8.319974	-0.083998	4.297038
431.901495	6347.217879	8.324979	-0.084078	4.299667
431.885656	6355.375093	8.329984	-0.084081	4.302379
432.420504	6363.293015	8.334989	-0.084186	4.305015
432.384325	6371.363217	8.339994	-0.084184	4.307695
432.306080	6379.415984	8.344998	-0.084175	4.310367
432.489695	6387.384271	8.350003	-0.084214	4.313012
432.887370	6395.391743	8.355008	-0.084294	4.315670
433.090301	6403.395014	8.360013	-0.084337	4.318323
433.178136	6411.408017	8.365018	-0.084359	4.320976
433.291421	6419.380063	8.370022	-0.084385	4.323615
433.281599	6427.449736	8.375027	-0.084388	4.326283
433.514176	6435.456198	8.380032	-0.084437	4.328931
433.503659	6443.499936	8.385037	-0.084440	4.331588
433.909727	6451.504702	8.390042	-0.084521	4.334233
434.149728	6459.530733	8.395046	-0.084571	4.336882
434.051952	6467.549738	8.400051	-0.084558	4.339525
434.220315	6475.609171	8.405056	-0.084595	4.342182
434.311774	6483.559657	8.410061	-0.084617	4.344800
434.084841	6491.668359	8.415066	-0.084581	4.347467
433.940022	6499.714585	8.420070	-0.084559	4.350111
434.336487	6507.678526	8.425075	-0.084638	4.352732
434.756572	6515.690649	8.430080	-0.084722	4.355366
434.635660	6523.673027	8.435085	-0.084704	4.357986
434.820346	6531.694470	8.440090	-0.084744	4.360619
434.919338	6539.648387	8.445094	-0.084768	4.363227
435.147426	6547.694907	8.450099	-0.084816	4.365865
435.768786	6555.671330	8.455104	-0.084937	4.368481
435.716347	6563.761362	8.460109	-0.084932	4.371128
435.522232	6571.775193	8.465114	-0.084901	4.373748
435.692685	6579.851244	8.470118	-0.084938	4.376389
435.406006	6587.799100	8.475123	-0.084890	4.378983
435.859436	6595.835183	8.480128	-0.084980	4.381610
435.819596	6603.783701	8.485133	-0.084978	4.384203
436.248734	6611.858862	8.490138	-0.085063	4.386839
436.523087	6619.860632	8.495142	-0.085120	4.389448
436.527221	6627.954977	8.500147	-0.085126	4.392085
435.921655	6636.038054	8.505152	-0.085018	4.394712
436.852855	6643.934335	8.510157	-0.085197	4.397286
437.157298	6651.947295	8.515162	-0.085259	4.399893
437.142750	6659.945110	8.520166	-0.085262	4.402492
437.367383	6667.960567	8.525171	-0.085309	4.405096
437.569128	6676.003415	8.530176	-0.085352	4.407707
437.873018	6683.994398	8.535181	-0.085413	4.410300
437.467332	6692.096300	8.540186	-0.085343	4.412924
437.866151	6700.151110	8.545190	-0.085423	4.415536
437.629000	6708.185271	8.550195	-0.085384	4.418135
437.955816	6716.197962	8.555200	-0.085450	4.420730
438.248863	6724.158127	8.560205	-0.085510	4.423305
438.121185	6732.232565	8.565210	-0.085492	4.425914
438.535088	6740.229235	8.570215	-0.085574	4.428499
438.719682	6748.277087	8.575219	-0.085614	4.431098
439.182228	6756.253598	8.580224	-0.085705	4.433673
439.156578	6764.279577	8.585229	-0.085706	4.436261
439.179058	6772.222250	8.590234	-0.085715	4.438820
439.250983	6780.334577	8.595239	-0.085734	4.441433
439.026674	6788.262233	8.600243	-0.085697	4.443984
439.246828	6796.374957	8.605248	-0.085744	4.446594
439.595158	6804.304095	8.610253	-0.085814	4.449145
439.968281	6812.395028	8.615258	-0.085889	4.451746
440.071383	6820.372266	8.620263	-0.085913	4.454308
439.958436	6828.429287	8.625267	-0.085898	4.456893
440.129047	6836.400237	8.630272	-0.085935	4.459450
439.993793	6844.483421	8.635277	-0.085915	4.462041
439.799505	6852.426827	8.640282	-0.085884	4.464584
439.949777	6860.520182	8.645287	-0.085917	4.467176
440.125988	6868.448138	8.650291	-0.085955	4.469714
440.173739	6876.521053	8.655296	-0.085970	4.472296
440.012057	6884.534965	8.660301	-0.085945	4.474856
440.187776	6892.528520	8.665306	-0.085983	4.477411
440.465440	6900.527375	8.670311	-0.086040	4.479965
440.532693	6908.537467	8.675315	-0.086058	4.482521
441.344247	6916.455819	8.680320	-0.086214	4.485049
441.518409	6924.579752	8.685325	-0.086252	4.487639
441.176673	6932.629316	8.690330	-0.086194	4.490202
441.305039	6940.678807	8.695335	-0.086223	4.492765
441.916728	6948.648840	8.700339	-0.086342	4.495302
441.527645	6956.707677	8.705344	-0.086275	4.497863
441.856552	6964.632241	8.710349	-0.086341	4.500383
442.000993	6972.654853	8.715354	-0.086374	4.502931
442.211138	6980.707930	8.720359	-0.086418	4.505488
442.068793	6988.721167	8.725363	-0.086397	4.508030
442.302939	6996.713299	8.730368	-0.086446	4.510565
442.328043	7004.744679	8.735373	-0.086456	4.513110
442.378498	7012.763594	8.740378	-0.086470	4.515649
442.813269	7020.711259	8.745383	-0.086557	4.518166
442.838821	7028.749404	8.750387	-0.086567	4.520709
443.001667	7036.768083	8.755392	-0.086602	4.523245
442.388191	7044.880520	8.760397	-0.086494	4.525807
442.894989	7052.773614	8.765402	-0.086593	4.528301
443.289973	7060.846391	8.770407	-0.086672	4.530850
442.961081	7068.848952	8.775411	-0.086616	4.533373
442.985567	7076.937061	8.780416	-0.086626	4.535923
443.570538	7084.816000	8.785421	-0.086740	4.538408
443.318117	7092.901587	8.790426	-0.086699	4.540953
443.139140	7100.931511	8.795431	-0.086671	4.543480
443.400358	7108.928717	8.800435	-0.086724	4.545997
443.643162	7116.947488	8.805440	-0.086775	4.548518
443.878795	7124.993723	8.810445	-0.086824	4.551047
444.287279	7132.921994	8.815450	-0.086906	4.553538
444.157532	7141.063440	8.820455	-0.086887	4.556093
444.216913	7148.987142	8.825459	-0.086903	4.558579
444.601486	7157.070469	8.830464	-0.086980	4.561114
444.788484	7164.985286	8.835469	-0.087020	4.563594
445.113081	7173.063199	8.840474	-0.087086	4.566124
445.100542	7181.025996	8.845479	-0.087089	4.568617
445.438050	7189.053038	8.850483	-0.087157	4.571128
445.376816	7197.125790	8.855488	-0.087151	4.573652
445.505145	7205.141013	8.860493	-0.087180	4.576157
445.716925	7213.071264	8.865498	-0.087225	4.578634
445.892188	7221.180166	8.870503	-0.087263	4.581165
445.610286	7229.155647	8.875507	-0.087216	4.583653
445.671766	7237.273020	8.880512	-0.087233	4.586184
445.592269	7245.234177	8.885517	-0.087223	4.588665
445.967088	7253.244860	8.890522	-0.087298	4.591160
445.998905	7261.259406	8.895527	-0.087309	4.593655
446.359274	7269.206829	8.900531	-0.087382	4.596128
446.648025	7277.197100	8.905536	-0.087441	4.598613
446.709689	7285.276990	8.910541	-0.087458	4.601124
447.014150	7293.194659	8.915546	-0.087520	4.603583
447.126136	7301.313428	8.920551	-0.087546	4.606104
446.891223	7309.306812	8.925555	-0.087507	4.608583
447.424940	7317.323576	8.930560	-0.087612	4.611070
447.862584	7325.303801	8.935565	-0.087699	4.613543
447.737850	7333.360297	8.940570	-0.087681	4.616039
447.437753	7341.414402	8.945575	-0.087630	4.618532
447.619291	7349.377007	8.950579	-0.087669	4.620996
447.835697	7357.347924	8.955584	-0.087715	4.623461
447.534271	7365.467393	8.960589	-0.087664	4.625970
447.835601	7373.411493	8.965594	-0.087726	4.628425
448.235118	7381.491321	8.970599	-0.087805	4.630919
448.054792	7389.457751	8.975603	-0.087777	4.633378
448.513582	7397.534257	8.980608	-0.087868	4.635869
448.305623	7405.461603	8.985613	-0.087834	4.638312
448.407518	7413.544006	8.990618	-0.087859	4.640802
448.693354	7421.483735	8.995623	-0.087917	4.643247
448.613401	7429.545422	9.000627	-0.087908	4.645728
449.226078	7437.547667	9.005632	-0.088027	4.648190
449.145332	7445.641391	9.010637	-0.088017	4.650678
449.161053	7453.583997	9.015642	-0.088026	4.653118
449.400868	7461.663186	9.020647	-0.088076	4.655599
449.589581	7469.581907	9.025651	-0.088116	4.658030
449.571238	7477.690861	9.030656	-0.088118	4.660518
449.420707	7485.632840	9.035661	-0.088095	4.662953
449.837227	7493.615550	9.040666	-0.088178	4.665399
449.745755	7501.704634	9.045671	-0.088166	4.667876
449.712668	7509.774648	9.050675	-0.088166	4.670347
449.968623	7517.793454	9.055680	-0.088219	4.672800
450.236499	7525.804357	9.060685	-0.088274	4.675250
450.352667	7533.731298	9.065690	-0.088301	4.677672
450.116173	7541.832109	9.070695	-0.088262	4.680147
450.691232	7549.728911	9.075699	-0.088374	4.682558
450.965257	7557.734436	9.080704	-0.088431	4.685000
451.054532	7565.799929	9.085709	-0.088453	4.687460
451.224990	7573.769603	9.090714	-0.088490	4.689889
451.184675	7581.839021	9.095719	-0.088488	4.692348
451.241755	7589.836143	9.100723	-0.088503	4.694783
451.910243	7597.910836	9.105728	-0.088633	4.697240
451.629296	7605.867756	9.110733	-0.088586	4.699661
451.696566	7613.887809	9.115738	-0.088604	4.702099
451.788719	7621.924511	9.120743	-0.088627	4.704541
451.718575	7630.012943	9.125747	-0.088619	4.706998
452.052484	7637.960579	9.130752	-0.088686	4.709410
452.246524	7646.064003	9.135757	-0.088728	4.711868
452.071006	7653.974007	9.140762	-0.088700	4.714267
452.666755	7662.022274	9.145767	-0.088817	4.716705
452.754930	7669.967783	9.150771	-0.088838	4.719112
452.755564	7678.089095	9.155776	-0.088844	4.721571
452.778558	7685.989827	9.160781	-0.088853	4.723962
453.030496	7694.063344	9.165786	-0.088906	4.726403
453.326745	7702.067065	9.170791	-0.088966	4.728822
453.497234	7710.117539	9.175795	-0.089003	4.731254
453.495315	7718.115153	9.180800	-0.089008	4.733669
453.799634	7726.178087	9.185805	-0.089070	4.736102
453.832673	7734.142833	9.190810	-0.089082	4.738505
453.925012	7742.231205	9.195815	-0.089104	4.740943
454.083150	7750.142971	9.200819	-0.089139	4.743327
454.485341	7758.252569	9.205824	-0.089219	4.745769
454.626656	7766.300022	9.210829	-0.089251	4.748192
454.609521	7774.303594	9.215834	-0.089253	4.750600
454.789720	7782.304643	9.220839	-0.089292	4.753006
454.830956	7790.307545	9.225843	-0.089305	4.755411
455.010621	7798.281485	9.230848	-0.089343	4.757806
455.231003	7806.269258	9.235853	-0.089390	4.760204
455.427352	7814.281733	9.240858	-0.089432	4.762609
455.447324	7822.387196	9.245863	-0.089441	4.765040
455.566125	7830.355104	9.250867	-0.089468	4.767429
455.883941	7838.364499	9.255872	-0.089533	4.769828
455.877948	7846.433112	9.260877	-0.089537	4.772245
455.906838	7854.415435	9.265882	-0.089548	4.774634
456.087320	7862.455576	9.270887	-0.089586	4.777039
456.356966	7870.409974	9.275891	-0.089642	4.779417
456.416801	7878.488352	9.280896	-0.089658	4.781832
456.503134	7886.391364	9.285901	-0.089680	4.784193
456.644569	7894.494507	9.290906	-0.089711	4.786612
456.926077	7902.503001	9.295911	-0.089769	4.789001
456.797398	7910.519125	9.300915	-0.089751	4.791393
457.177852	7918.506594	9.305920	-0.089827	4.793773
457.262421	7926.599352	9.310925	-0.089848	4.796185
457.326799	7934.532423	9.315930	-0.089865	4.798548
457.354166	7942.635746	9.320935	-0.089876	4.800960
457.172877	7950.577825	9.325939	-0.089847	4.803324
457.415085	7958.646863	9.330944	-0.089898	4.805723
457.630313	7966.625133	9.335949	-0.089943	4.808094
457.755161	7974.616731	9.340954	-0.089971	4.810468
458.047672	7982.670344	9.345959	-0.090031	4.812858
457.921640	7990.124743	9.350963	-0.090013	4.815071
458.230775	7994.820720	9.355968	-0.090073	4.816463

458.488555	7997.497493	9.360973	-0.090123	4.817256
458.434466	7998.768238	9.365978	-0.090114	4.817634
458.434373	7999.162975	9.370983	-0.090114	4.817751
458.366221	8000.110471	9.375987	-0.090102	4.818032
458.547465	8000.133022	9.380992	-0.090136	4.818038
458.563861	8000.127995	9.385997	-0.090139	4.818036
458.744356	8000.140009	9.391002	-0.090173	4.818039
458.858281	8000.219515	9.396007	-0.090195	4.818062
458.706267	8000.141594	9.401011	-0.090166	4.818040
458.699533	8000.158350	9.406016	-0.090165	4.818045
458.810999	8000.236768	9.411021	-0.090186	4.818068
459.013339	8000.190138	9.416026	-0.090224	4.818053
459.149852	8000.238381	9.421031	-0.090249	4.818067
459.109951	8000.179928	9.426035	-0.090242	4.818049
459.159438	8000.256425	9.431040	-0.090251	4.818072
459.154632	8000.216362	9.436045	-0.090250	4.818060
459.002118	8000.161592	9.441050	-0.090222	4.818044
459.219166	8000.179384	9.446055	-0.090263	4.818049
459.205296	8000.228673	9.451059	-0.090260	4.818064
459.424823	8000.211761	9.456064	-0.090301	4.818058
459.468924	8000.255548	9.461069	-0.090309	4.818070
459.506923	8000.216085	9.466074	-0.090317	4.818059
459.391613	8000.235528	9.471079	-0.090295	4.818065
459.372583	8000.217371	9.476083	-0.090292	4.818059
459.425678	8000.236020	9.481088	-0.090302	4.818065
459.600809	8000.223748	9.486093	-0.090334	4.818060
459.536397	8000.192321	9.491098	-0.090323	4.818051
459.595647	8000.174211	9.496103	-0.090334	4.818046
459.692459	8000.142943	9.501107	-0.090352	4.818036
459.733683	8000.140370	9.506112	-0.090359	4.818035
459.766115	8000.194521	9.511117	-0.090366	4.818051
459.712289	8000.147453	9.516122	-0.090356	4.818037
459.997371	8000.173570	9.521127	-0.090409	4.818044
459.863029	8000.151688	9.526131	-0.090384	4.818038
459.905041	8000.193342	9.531136	-0.090392	4.818050
459.892946	8000.184757	9.536141	-0.090390	4.818048
459.888696	8000.135226	9.541146	-0.090389	4.818033
459.992462	8000.243016	9.546151	-0.090408	4.818064
459.935775	8000.160114	9.551155	-0.090398	4.818040
460.111007	8000.148896	9.556160	-0.090431	4.818036
459.721769	8000.287661	9.561165	-0.090358	4.818079
459.741028	8000.213194	9.566170	-0.090362	4.818057
459.610735	8000.187159	9.571175	-0.090338	4.818049
459.824395	8000.199641	9.576179	-0.090378	4.818052
459.854603	8000.170595	9.581184	-0.090383	4.818044
459.951786	8000.213024	9.586189	-0.090402	4.818056
460.027258	8000.170928	9.591194	-0.090416	4.818043
460.373664	8000.206330	9.596199	-0.090480	4.818052
460.079822	8000.230634	9.601203	-0.090426	4.818060
460.099171	8000.235123	9.606208	-0.090429	4.818062
460.301991	8000.186394	9.611213	-0.090467	4.818046
460.225360	8000.157954	9.616218	-0.090453	4.818038
460.211028	8000.249348	9.621223	-0.090451	4.818065
460.164539	8000.157114	9.626227	-0.090442	4.818038
460.305915	8000.163317	9.631232	-0.090468	4.818039
460.264776	8000.189065	9.636237	-0.090461	4.818047
459.913017	8000.158866	9.641242	-0.090395	4.818040
460.204813	8000.182973	9.646247	-0.090450	4.818046
460.042502	8000.217546	9.651251	-0.090420	4.818057
459.948999	8000.234136	9.656256	-0.090402	4.818062
460.133230	8000.256733	9.661261	-0.090437	4.818068
459.780978	8000.262320	9.666266	-0.090371	4.818071
459.910170	8000.291512	9.671271	-0.090395	4.818079
460.113892	8000.194370	9.676275	-0.090433	4.818049
460.292929	8000.233738	9.681280	-0.090467	4.818060
460.242611	8000.202508	9.686285	-0.090458	4.818051
460.282088	8000.145169	9.691290	-0.090465	4.818034
460.653946	8000.184087	9.696295	-0.090534	4.818044
460.463467	8000.152994	9.701299	-0.090499	4.818036
460.613227	8000.203531	9.706304	-0.090527	4.818050
460.534218	8000.210850	9.711309	-0.090512	4.818053
460.434272	8000.182081	9.716314	-0.090494	4.818044
460.486002	8000.201764	9.721319	-0.090504	4.818050
460.469991	8000.174175	9.726323	-0.090501	4.818042
460.589500	8000.185335	9.731328	-0.090523	4.818045
460.504061	8000.188353	9.736333	-0.090507	4.818046
460.454094	8000.206608	9.741338	-0.090498	4.818052
460.645054	8000.237721	9.746343	-0.090534	4.818060
460.628058	8000.192221	9.751347	-0.090531	4.818047
460.508506	8000.241081	9.756352	-0.090508	4.818062
460.715812	8000.197679	9.761357	-0.090547	4.818048
460.575878	8000.156768	9.766362	-0.090521	4.818036
460.615116	8000.257338	9.771367	-0.090529	4.818066
460.286379	8000.221144	9.776371	-0.090467	4.818057
460.155397	8000.317217	9.781376	-0.090443	4.818086
460.412342	8000.328202	9.786381	-0.090491	4.818088
460.116379	8000.299838	9.791386	-0.090436	4.818081
460.435049	8000.325377	9.796391	-0.090496	4.818087
460.459129	8000.265715	9.801395	-0.090500	4.818069
460.568695	8000.228310	9.806400	-0.090521	4.818058
460.658892	8000.230636	9.811405	-0.090537	4.818058
460.548623	8000.246991	9.816410	-0.090517	4.818063
460.602939	8000.261447	9.821415	-0.090527	4.818067
460.446071	8000.312940	9.826419	-0.090498	4.818083
460.410084	8000.304020	9.831424	-0.090492	4.818081
460.552252	8000.293391	9.836429	-0.090518	4.818077
460.496002	8000.265236	9.841434	-0.090508	4.818069
460.679297	8000.210969	9.846439	-0.090542	4.818052
460.651832	8000.207432	9.851443	-0.090537	4.818051
460.440836	8000.244480	9.856448	-0.090498	4.818063
460.857791	8000.213498	9.861453	-0.090575	4.818052
460.791948	8000.216791	9.866458	-0.090563	4.818053
461.078689	8000.277676	9.871463	-0.090617	4.818070
460.804535	8000.215929	9.876467	-0.090566	4.818053
460.835544	8000.197422	9.881472	-0.090572	4.818047
460.747128	8000.287776	9.886477	-0.090555	4.818074
460.408749	8000.281976	9.891482	-0.090492	4.818074
460.746381	8000.294096	9.896487	-0.090555	4.818076
460.986826	8000.229052	9.901491	-0.090600	4.818056
461.016201	8000.228419	9.906496	-0.090606	4.818056
460.784901	8000.228334	9.911501	-0.090563	4.818057
460.763631	8000.191196	9.916506	-0.090559	4.818046
461.038601	8000.217174	9.921511	-0.090610	4.818052
461.055817	8000.142677	9.926515	-0.090613	4.818030
460.999175	8000.196632	9.931520	-0.090603	4.818046
460.750931	8000.232103	9.936525	-0.090557	4.818058
460.873324	8000.227513	9.941530	-0.090580	4.818056
461.103309	8000.231804	9.946535	-0.090623	4.818056
461.050509	8000.191064	9.951539	-0.090613	4.818044
461.071995	8000.184003	9.956544	-0.090617	4.818042
460.822084	8000.246823	9.961549	-0.090571	4.818062
460.913532	8000.266012	9.966554	-0.090588	4.818067
460.776236	8000.369366	9.971559	-0.090562	4.818098
460.688393	8000.280759	9.976563	-0.090546	4.818073
460.759074	8000.290181	9.981568	-0.090559	4.818075
460.891404	8000.290995	9.986573	-0.090584	4.818075
460.570026	8000.338071	9.991578	-0.090524	4.818090
460.989639	8000.266070	9.996583	-0.090602	4.818067
460.975519	8000.192185	10.001587	-0.090600	4.818045
460.955428	8000.282447	10.006592	-0.090596	4.818072
461.064445	8000.207134	10.011597	-0.090617	4.818049
461.024154	8000.185520	10.016602	-0.090609	4.818043
461.329034	8000.214025	10.021607	-0.090666	4.818050
461.084345	8000.251651	10.026611	-0.090621	4.818062
461.207252	8000.204958	10.031616	-0.090644	4.818048
461.063670	8000.262955	10.036621	-0.090617	4.818066
461.213093	8000.215581	10.041626	-0.090645	4.818051
461.221558	8000.260976	10.046631	-0.090647	4.818064
461.358330	8000.265011	10.051635	-0.090672	4.818065
461.307341	8000.290620	10.056640	-0.090663	4.818073
461.260518	8000.308919	10.061645	-0.090654	4.818078
461.163283	8000.313876	10.066650	-0.090636	4.818080
461.187493	8000.306854	10.071655	-0.090641	4.818078
461.152717	8000.266367	10.076659	-0.090634	4.818066
461.096633	8000.250847	10.081664	-0.090624	4.818062
461.201669	8000.324971	10.086669	-0.090644	4.818083
460.944489	8000.308731	10.091674	-0.090596	4.818080
461.028428	8000.362556	10.096679	-0.090612	4.818095
460.985594	8000.304058	10.101683	-0.090604	4.818078
461.032303	8000.291036	10.106688	-0.090612	4.818074
461.347347	8000.259676	10.111693	-0.090671	4.818064
461.093649	8000.266645	10.116698	-0.090624	4.818067
461.097579	8000.320398	10.121703	-0.090625	4.818083
461.458956	8000.254949	10.126707	-0.090692	4.818062
461.374276	8000.235868	10.131712	-0.090677	4.818056
461.264047	8000.225904	10.136717	-0.090656	4.818054
461.317096	8000.212970	10.141722	-0.090666	4.818050
461.367300	8000.264216	10.146727	-0.090676	4.818065
461.399508	8000.247831	10.151731	-0.090682	4.818060
461.456539	8000.234953	10.156736	-0.090692	4.818056
461.170484	8000.324637	10.161741	-0.090639	4.818083
461.104221	8000.253177	10.166746	-0.090627	4.818063
461.406213	8000.313225	10.171751	-0.090683	4.818079
461.510555	8000.271535	10.176755	-0.090703	4.818066
461.115394	8000.305993	10.181760	-0.090629	4.818078
461.286238	8000.261026	10.186765	-0.090661	4.818064
461.179147	8000.282689	10.191770	-0.090641	4.818071
461.326014	8000.261599	10.196775	-0.090669	4.818064
461.088538	8000.304591	10.201779	-0.090625	4.818078
461.158084	8000.293995	10.206784	-0.090638	4.818074
461.027887	8000.330071	10.211789	-0.090614	4.818086
461.004414	8000.308693	10.216794	-0.090609	4.818079
461.375498	8000.344446	10.221799	-0.090678	4.818088
461.361536	8000.360048	10.226803	-0.090676	4.818093
461.434852	8000.305289	10.231808	-0.090690	4.818077
461.504730	8000.349442	10.236813	-0.090703	4.818089
461.242346	8000.353130	10.241818	-0.090654	4.818092
461.509666	8000.304255	10.246823	-0.090704	4.818076
461.510579	8000.291642	10.251827	-0.090704	4.818072
461.632095	8000.253351	10.256832	-0.090727	4.818060
461.659588	8000.326387	10.261837	-0.090732	4.818082
461.587448	8000.302218	10.266842	-0.090719	4.818075
461.601828	8000.259263	10.271847	-0.090721	4.818062
461.541168	8000.263681	10.276851	-0.090710	4.818064
461.509172	8000.267450	10.281856	-0.090704	4.818065
461.542256	8000.344775	10.286861	-0.090711	4.818088
461.607270	8000.266737	10.291866	-0.090723	4.818064
461.622096	8000.291166	10.296871	-0.090726	4.818072
461.655461	8000.243214	10.301875	-0.090732	4.818057
461.705220	8000.212337	10.306880	-0.090741	4.818048
461.698510	8000.266994	10.311885	-0.090740	4.818064
461.527435	8000.230908	10.316890	-0.090708	4.818054
461.328458	8000.367085	10.321895	-0.090672	4.818095
461.672299	8000.237169	10.326899	-0.090736	4.818055
461.490727	8000.220938	10.331904	-0.090702	4.818051
461.383856	8000.314192	10.336909	-0.090682	4.818079
461.658382	8000.212780	10.341914	-0.090733	4.818048
461.823455	8000.244585	10.346919	-0.090764	4.818057
461.660794	8000.229672	10.351923	-0.090734	4.818053
461.693787	8000.213299	10.356928	-0.090740	4.818048
461.735528	8000.287587	10.361933	-0.090748	4.818070
461.391571	8000.258545	10.366938	-0.090684	4.818063
461.409131	8000.310385	10.371943	-0.090687	4.818078
461.488781	8000.302037	10.376947	-0.090702	4.818075
461.584586	8000.259173	10.381952	-0.090720	4.818062
461.711722	8000.276759	10.386957	-0.090744	4.818067
461.817390	8000.200346	10.391962	-0.090764	4.818044
461.841503	8000.205955	10.396967	-0.090768	4.818045
461.750951	8000.187845	10.401971	-0.090752	4.818040
461.937414	8000.231531	10.406976	-0.090786	4.818053
461.863508	8000.277875	10.411981	-0.090773	4.818067
461.829010	8000.187910	10.416986	-0.090766	4.818040
461.906185	8000.213216	10.421991	-0.090781	4.818047
461.940179	8000.225281	10.426995	-0.090787	4.818051
462.037910	8000.170865	10.432000	-0.090806	4.818034
462.021851	8000.216968	10.437005	-0.090803	4.818048
462.063308	8000.177552	10.442010	-0.090810	4.818036
462.119682	8000.262575	10.447015	-0.090821	4.818061
461.741534	8000.286743	10.452019	-0.090751	4.818070
461.724442	8000.268613	10.457024	-0.090748	4.818064
461.883842	8000.304550	10.462029	-0.090777	4.818074
461.478445	8000.314649	10.467034	-0.090702	4.818079
461.711442	8000.311615	10.472039	-0.090746	4.818077
461.729631	8000.318194	10.477043	-0.090749	4.818079
461.849573	8000.310412	10.482048	-0.090771	4.818076
461.484140	8000.384241	10.487053	-0.090704	4.818100
461.325900	8000.378865	10.492058	-0.090674	4.818099
461.540654	8000.408211	10.497063	-0.090714	4.818107
461.481391	8000.357903	10.502067	-0.090703	4.818092
461.797426	8000.312872	10.507072	-0.090762	4.818077
461.912202	8000.358710	10.512077	-0.090784	4.818090
461.357487	8000.335127	10.517082	-0.090681	4.818086
461.664495	8000.339450	10.522087	-0.090738	4.818086
461.841556	8000.239825	10.527091	-0.090771	4.818055
461.478456	8000.261048	10.532096	-0.090703	4.818063
461.489798	8000.352806	10.537101	-0.090706	4.818090
461.718505	8000.258119	10.542106	-0.090748	4.818061
461.998957	8000.274702	10.547111	-0.090800	4.818065
461.985993	8000.185040	10.552115	-0.090798	4.818039
461.884405	8000.250997	10.557120	-0.090779	4.818059
462.071812	8000.324176	10.562125	-0.090814	4.818079
461.929345	8000.243221	10.567130	-0.090788	4.818056
461.788616	8000.309680	10.572135	-0.090762	4.818076
461.493850	8000.358183	10.577139	-0.090707	4.818092
461.796138	8000.213996	10.582144	-0.090763	4.818048
461.716852	8000.285531	10.587149	-0.090749	4.818069
462.012355	8000.223366	10.592154	-0.090804	4.818050
462.132618	8000.273493	10.597159	-0.090826	4.818064
462.106767	8000.287875	10.602163	-0.090822	4.818068
462.230284	8000.246454	10.607168	-0.090845	4.818056
462.313552	8000.267635	10.612173	-0.090860	4.818062
462.059927	8000.313557	10.617178	-0.090813	4.818076
461.954820	8000.292083	10.622183	-0.090794	4.818070
461.961288	8000.354296	10.627187	-0.090795	4.818089
462.081590	8000.243345	10.632192	-0.090817	4.818055
462.046426	8000.283917	10.637197	-0.090811	4.818068
462.110525	8000.242713	10.642202	-0.090823	4.818055
462.218993	8000.264248	10.647207	-0.090843	4.818061
462.319314	8000.263560	10.652211	-0.090862	4.818060
462.128191	8000.296675	10.657216	-0.090827	4.818071
462.452525	8000.365464	10.662221	-0.090887	4.818090
462.203169	8000.314588	10.667226	-0.090841	4.818076
462.235965	8000.324531	10.672231	-0.090847	4.818079
461.844295	8000.334823	10.677235	-0.090774	4.818083
462.056148	8000.219896	10.682240	-0.090814	4.818049
462.092301	8000.288842	10.687245	-0.090820	4.818069
461.990900	8000.196884	10.692250	-0.090802	4.818042
462.150170	8000.254928	10.697255	-0.090831	4.818059
462.003376	8000.212865	10.702259	-0.090804	4.818047
461.896708	8000.322968	10.707264	-0.090784	4.818080
461.946341	8000.313145	10.712269	-0.090794	4.818077
462.119450	8000.159773	10.717274	-0.090826	4.818030
461.995108	8000.274891	10.722279	-0.090803	4.818065
462.091808	8000.260466	10.727283	-0.090821	4.818060
462.266246	8000.236605	10.732288	-0.090854	4.818053
462.309155	8000.261430	10.737293	-0.090862	4.818060
462.185551	8000.255488	10.742298	-0.090839	4.818059
462.503069	8000.221006	10.747303	-0.090898	4.818047
462.343617	8000.247196	10.752307	-0.090868	4.818055
462.332695	8000.202832	10.757312	-0.090866	4.818042
462.311171	8000.298341	10.762317	-0.090863	4.818071
462.327543	8000.255413	10.767322	-0.090866	4.818058
462.355988	8000.221078	10.772327	-0.090871	4.818048
462.217577	8000.253881	10.777331	-0.090845	4.818058
462.090699	8000.209992	10.782336	-0.090822	4.818045
462.078108	8000.298257	10.787341	-0.090820	4.818072
462.258117	8000.254472	10.792346	-0.090853	4.818058
462.435480	8000.263289	10.797351	-0.090886	4.818060
462.242762	8000.227950	10.802355	-0.090851	4.818050
462.136530	8000.228569	10.807360	-0.090831	4.818051
462.150143	8000.240348	10.812365	-0.090833	4.818054
462.260832	8000.211380	10.817370	-0.090854	4.818045
462.261073	8000.286139	10.822375	-0.090854	4.818067
462.229187	8000.258325	10.827379	-0.090848	4.818059
462.202373	8000.203209	10.832384	-0.090844	4.818043
462.303203	8000.266749	10.837389	-0.090862	4.818061
462.229531	8000.216239	10.842394	-0.090849	4.818047
462.488782	8000.227260	10.847399	-0.090897	4.818049
462.537582	8000.185841	10.852403	-0.090906	4.818036
462.211769	8000.227590	10.857408	-0.090846	4.818050
461.966468	8000.305213	10.862413	-0.090800	4.818074
462.091381	8000.254337	10.867418	-0.090824	4.818059
461.649143	8000.386042	10.872423	-0.090741	4.818099
461.689815	8000.361354	10.877427	-0.090749	4.818092
461.787134	8000.290086	10.882432	-0.090767	4.818070
462.215910	8000.309808	10.887437	-0.090847	4.818074
461.934269	8000.291116	10.892442	-0.090795	4.818070
462.364839	8000.277174	10.897447	-0.090875	4.818064
461.964470	8000.317874	10.902451	-0.090801	4.818078
462.009084	8000.319561	10.907456	-0.090809	4.818078
462.281014	8000.330762	10.912461	-0.090860	4.818080
462.142047	8000.327762	10.917466	-0.090834	4.818080
462.464341	8000.291242	10.922471	-0.090894	4.818068
462.240922	8000.224939	10.927475	-0.090852	4.818049
462.317255	8000.251286	10.932480	-0.090867	4.818057
462.441308	8000.281463	10.937485	-0.090890	4.818065
462.183683	8000.212574	10.942490	-0.090842	4.818046
462.375459	8000.235281	10.947495	-0.090878	4.818052
462.432488	8000.267674	10.952499	-0.090889	4.818061
462.234949	8000.277536	10.957504	-0.090852	4.818065
462.086646	8000.292303	10.962509	-0.090824	4.818070
462.209110	8000.222442	10.967514	-0.090847	4.818049
462.120509	8000.290687	10.972519	-0.090831	4.818069
462.073135	8000.301609	10.977523	-0.090822	4.818073
461.999742	8000.291109	10.982528	-0.090809	4.818070
462.087192	8000.359724	10.987533	-0.090825	4.818090
462.034000	8000.251598	10.992538	-0.090815	4.818058
462.371739	8000.293202	10.997543	-0.090878	4.818069
462.009236	8000.353385	11.002547	-0.090811	4.818088
461.607796	8000.325639	11.007552	-0.090736	4.818082
462.138136	8000.309941	11.012557	-0.090835	4.818075
462.262228	8000.239050	11.017562	-0.090858	4.818053
462.295788	8000.315330	11.022567	-0.090864	4.818076
461.861496	8000.347131	11.027571	-0.090784	4.818087
461.913718	8000.271018	11.032576	-0.090794	4.818064
462.026706	8000.333676	11.037581	-0.090815	4.818082
461.907315	8000.246728	11.042586	-0.090792	4.818057
462.178818	8000.245288	11.047591	-0.090843	4.818055
462.289649	8000.280543	11.052595	-0.090864	4.818065
462.197540	8000.258199	11.057600	-0.090847	4.818059
462.391744	8000.275676	11.062605	-0.090883	4.818064
462.267138	8000.226554	11.067610	-0.090860	4.818049
462.280568	8000.245701	11.072615	-0.090863	4.818055
462.204171	8000.255161	11.077619	-0.090848	4.818058
462.265000	8000.234968	11.082624	-0.090860	4.818052
462.300558	8000.309170	11.087629	-0.090867	4.818074
461.973348	8000.270887	11.092634	-0.090806	4.818064
462.062046	8000.282669	11.097639	-0.090822	4.818067
462.311206	8000.272493	11.102643	-0.090869	4.818063
462.331500	8000.246465	11.107648	-0.090873	4.818055
462.227891	8000.291338	11.112653	-0.090853	4.818069
462.208055	8000.263694	11.117658	-0.090850	4.818061
462.141665	8000.333305	11.122663	-0.090838	4.818082
461.924065	8000.311301	11.127667	-0.090797	4.818076
462.104914	8000.222258	11.132672	-0.090831	4.818049
462.478262	8000.269627	11.137677	-0.090901	4.818061
462.434586	8000.286917	11.142682	-0.090893	4.818067
462.450503	8000.283989	11.147687	-0.090896	4.818066
462.365878	8000.323866	11.152691	-0.090880	4.818078
462.354294	8000.274228	11.157696	-0.090878	4.818063
462.188886	8000.340341	11.162701	-0.090847	4.818083
462.225969	8000.233484	11.167706	-0.090854	4.818052
462.367552	8000.284963	11.172711	-0.090881	4.818066
462.279200	8000.326893	11.177715	-0.090864	4.818079
462.429259	8000.217413	11.182720	-0.090892	4.818046
462.723202	8000.226817	11.187725	-0.090947	4.818048
462.676301	8000.192475	11.192730	-0.090938	4.818038
462.561504	8000.275092	11.197735	-0.090917	4.818063
462.585971	8000.254387	11.202739	-0.090922	4.818056
462.686821	8000.222122	11.207744	-0.090941	4.818046
462.578628	8000.289040	11.212749	-0.090921	4.818067
462.291288	8000.267108	11.217754	-0.090867	4.818061
462.050558	8000.296367	11.222759	-0.090822	4.818071
462.416727	8000.314157	11.227763	-0.090891	4.818075
462.464663	8000.280095	11.232768	-0.090900	4.818064
462.533771	8000.334767	11.237773	-0.090913	4.818080
462.620253	8000.230710	11.242778	-0.090929	4.818049
462.384079	8000.275824	11.247783	-0.090885	4.818064
462.421672	8000.262674	11.252787	-0.090892	4.818059
462.721060	8000.258468	11.257792	-0.090948	4.818057
462.529680	8000.320005	11.262797	-0.090912	4.818076
462.477816	8000.281382	11.267802	-0.090903	4.818065
462.683955	8000.316925	11.272807	-0.090941	4.818074
462.584848	8000.302904	11.277811	-0.090923	4.818071
462.521713	8000.206218	11.282816	-0.090911	4.818042
462.560768	8000.254150	11.287821	-0.090919	4.818056
462.729940	8000.222846	11.292826	-0.090950	4.818046
462.609506	8000.284328	11.297831	-0.090928	4.818065
462.442150	8000.308301	11.302835	-0.090897	4.818073
462.589423	8000.246158	11.307840	-0.090924	4.818054
462.573001	8000.365955	11.312845	-0.090921	4.818089
462.222851	8000.265232	11.317850	-0.090856	4.818061
462.411204	8000.247884	11.322855	-0.090891	4.818055
462.434371	8000.269273	11.327859	-0.090896	4.818061
462.558992	8000.272085	11.332864	-0.090919	4.818062
462.388617	8000.394980	11.337869	-0.090888	4.818099
462.237384	8000.348642	11.342874	-0.090860	4.818086
461.999729	8000.352677	11.347879	-0.090815	4.818088
462.328192	8000.289923	11.352883	-0.090877	4.818068
462.504795	8000.231351	11.357888	-0.090910	4.818050
462.624326	8000.310947	11.362893	-0.090932	4.818073
462.418664	8000.276477	11.367898	-0.090894	4.818064
462.573718	8000.356573	11.372903	-0.090923	4.818087
462.654500	8000.309286	11.377907	-0.090938	4.818072
462.452183	8000.262230	11.382912	-0.090900	4.818059
462.641610	8000.252267	11.387917	-0.090936	4.818055
462.803375	8000.211384	11.392922	-0.090966	4.818043
462.823898	8000.254845	11.397927	-0.090970	4.818055
462.619722	8000.244611	11.402931	-0.090932	4.818053
462.800352	8000.188201	11.407936	-0.090965	4.818036
462.975142	8000.243307	11.412941	-0.090998	4.818051
462.711026	8000.188011	11.417946	-0.090949	4.818036
462.854872	8000.221625	11.422951	-0.090976	4.818045
462.958672	8000.259941	11.427955	-0.090995	4.818056
462.734716	8000.227319	11.432960	-0.090954	4.818048
462.906734	8000.296073	11.437965	-0.090986	4.818067
462.540971	8000.269879	11.442970	-0.090918	4.818061
462.678802	8000.285511	11.447975	-0.090944	4.818065
462.494570	8000.340831	11.452979	-0.090909	4.818082
462.598882	8000.247552	11.457984	-0.090929	4.818054
462.790685	8000.292369	11.462989	-0.090965	4.818067
462.800240	8000.220919	11.467994	-0.090967	4.818045
462.905325	8000.221352	11.472999	-0.090986	4.818045
462.759071	8000.294051	11.478003	-0.090959	4.818067
462.832015	8000.210859	11.483008	-0.090973	4.818042
462.614541	8000.302560	11.488013	-0.090932	4.818070
462.529344	8000.281366	11.493018	-0.090917	4.818064
462.711402	8000.266035	11.498023	-0.090951	4.818059
462.463563	8000.320461	11.503027	-0.090905	4.818076
462.497994	8000.312530	11.508032	-0.090911	4.818074
462.904167	8000.352993	11.513037	-0.090987	4.818084
462.425089	8000.306254	11.518042	-0.090898	4.818072
462.528233	8000.337190	11.523047	-0.090917	4.818081
462.513883	8000.373844	11.528051	-0.090914	4.818092
462.595534	8000.332887	11.533056	-0.090930	4.818079
462.715986	8000.418813	11.538061	-0.090952	4.818104
462.787811	8000.340869	11.543066	-0.090966	4.818081
462.456605	8000.381488	11.548071	-0.090904	4.818094
462.616867	8000.291102	11.553075	-0.090934	4.818067
462.830737	8000.303593	11.558080	-0.090974	4.818070
462.835548	8000.389998	11.563085	-0.090975	4.818095
462.738980	8000.339164	11.568090	-0.090957	4.818081
462.727810	8000.335856	11.573095	-0.090955	4.818080
462.543404	8000.365906	11.578099	-0.090921	4.818089
462.686469	8000.338447	11.583104	-0.090948	4.818081
462.433265	8000.353843	11.588109	-0.090900	4.818086
462.592474	8000.309765	11.593114	-0.090930	4.818073
462.891622	8000.239230	11.598119	-0.090986	4.818050
462.810482	8000.286525	11.603123	-0.090971	4.818065
462.605496	8000.298388	11.608128	-0.090933	4.818069
462.637322	8000.360959	11.613133	-0.090939	4.818088
462.751553	8000.233077	11.618138	-0.090960	4.818049
463.025388	8000.299051	11.623143	-0.091011	4.818068
462.886014	8000.322365	11.628147	-0.090986	4.818075
462.846232	8000.230218	11.633152	-0.090978	4.818048
462.901143	8000.254159	11.638157	-0.090988	4.818055
462.760507	8000.263769	11.643162	-0.090962	4.818058
462.769908	8000.311284	11.648167	-0.090964	4.818072
462.611034	8000.366961	11.653171	-0.090935	4.818089
462.656443	8000.321283	11.658176	-0.090943	4.818076
462.655555	8000.359179	11.663181	-0.090943	4.818087
462.556894	8000.277785	11.668186	-0.090925	4.818063
462.655549	8000.288654	11.673191	-0.090943	4.818066
462.123161	8000.383296	11.678195	-0.090844	4.818096
462.430778	8000.303405	11.683200	-0.090902	4.818071
462.357614	8000.377132	11.688205	-0.090888	4.818093
462.686914	8000.284912	11.693210	-0.090950	4.818065
462.770914	8000.351375	11.698215	-0.090965	4.818084
462.452686	8000.321638	11.703219	-0.090906	4.818077
462.836080	8000.238601	11.708224	-0.090978	4.818050
462.669865	8000.400510	11.713229	-0.090947	4.818099
462.693971	8000.318736	11.718234	-0.090951	4.818075
462.685506	8000.320729	11.723239	-0.090950	4.818075
462.651667	8000.371848	11.728243	-0.090944	4.818091
462.939709	8000.255886	11.733248	-0.090997	4.818055
462.597427	8000.392155	11.738253	-0.090934	4.818097
462.563162	8000.325353	11.743258	-0.090928	4.818077
463.119855	8000.295290	11.748263	-0.091031	4.818066
463.064356	8000.232399	11.753267	-0.091021	4.818048
462.822175	8000.272165	11.758272	-0.090976	4.818060
462.987114	8000.297654	11.763277	-0.091007	4.818067
463.050248	8000.202743	11.768282	-0.091019	4.818039
462.607083	8000.299692	11.773287	-0.090936	4.818069
463.023678	8000.266605	11.778291	-0.091014	4.818058
463.134197	8000.196575	11.783296	-0.091034	4.818037
462.851274	8000.274722	11.788301	-0.090982	4.818061
462.860656	8000.192741	11.793306	-0.090984	4.818037
462.987859	8000.266129	11.798311	-0.091008	4.818058
462.879896	8000.297254	11.803315	-0.090988	4.818068
462.794868	8000.227632	11.808320	-0.090972	4.818047
462.926143	8000.230539	11.813325	-0.090996	4.818048
462.904536	8000.259720	11.818330	-0.090992	4.818056
462.839033	8000.315658	11.823335	-0.090980	4.818073
462.645442	8000.335051	11.828339	-0.090944	4.818080
462.653738	8000.294115	11.833344	-0.090946	4.818068
462.786530	8000.342314	11.838349	-0.090971	4.818081
462.769655	8000.247330	11.843354	-0.090968	4.818053
462.855181	8000.236959	11.848359	-0.090984	4.818050
462.945597	8000.266663	11.853363	-0.091001	4.818058
462.681134	8000.310327	11.858368	-0.090952	4.818072
462.966735	8000.322774	11.863373	-0.091005	4.818075
462.934606	8000.229681	11.868378	-0.090999	4.818047
462.788077	8000.261317	11.873383	-0.090972	4.818057
463.051261	8000.271343	11.878387	-0.091021	4.818059
463.141260	8000.270510	11.883392	-0.091038	4.818059
463.228178	8000.266476	11.888397	-0.091054	4.818057
462.686742	8000.326247	11.893402	-0.090953	4.818077
462.347634	8000.394128	11.898407	-0.090890	4.818098
462.419121	8000.367767	11.903411	-0.090904	4.818090
462.522784	8000.310275	11.908416	-0.090923	4.818073
462.680023	8000.379874	11.913421	-0.090952	4.818093
462.582322	8000.338499	11.918426	-0.090934	4.818081
462.383295	8000.369397	11.923431	-0.090897	4.818091
462.833406	8000.251503	11.928435	-0.090981	4.818054
462.893079	8000.232346	11.933440	-0.090992	4.818048
462.872999	8000.319454	11.938445	-0.090989	4.818074
462.416575	8000.357259	11.943450	-0.090904	4.818087
462.537214	8000.300005	11.948455	-0.090926	4.818070
462.765168	8000.270581	11.953459	-0.090969	4.818060
462.753192	8000.257786	11.958464	-0.090967	4.818056
462.917854	8000.287482	11.963469	-0.090998	4.818064
462.868469	8000.274161	11.968474	-0.090988	4.818061
462.648731	8000.308978	11.973479	-0.090948	4.818072
462.823102	8000.289329	11.978483	-0.090980	4.818065
462.639661	8000.298336	11.983488	-0.090946	4.818069
462.656408	8000.357536	11.988493	-0.090949	4.818086
462.804788	8000.263824	11.993498	-0.090977	4.818058
463.057620	8000.267388	11.998503	-0.091024	4.818058
463.049700	8000.308343	12.003507	-0.091023	4.818070
463.032746	8000.280738	12.008512	-0.091020	4.818062
462.683416	8000.394800	12.013517	-0.090955	4.818097
462.316583	8000.389646	12.018522	-0.090887	4.818097
462.214972	8000.432442	12.023527	-0.090868	4.818110
462.257316	8000.394091	12.028531	-0.090876	4.818099
462.654172	8000.327036	12.033536	-0.090950	4.818077
462.823191	8000.369427	12.038541	-0.090981	4.818089
462.736533	8000.316627	12.043546	-0.090965	4.818074
462.745165	8000.344129	12.048551	-0.090967	4.818082
462.578158	8000.373371	12.053555	-0.090936	4.818091
462.780042	8000.337263	12.058560	-0.090974	4.818080
462.472801	8000.417174	12.063565	-0.090917	4.818105
462.688650	8000.343361	12.068570	-0.090957	4.818082
462.913078	8000.288620	12.073575	-0.090999	4.818065
462.639968	8000.302684	12.078579	-0.090948	4.818070
462.798519	8000.267019	12.083584	-0.090978	4.818059
462.768394	8000.349775	12.088589	-0.090972	4.818083
462.518285	8000.364162	12.093594	-0.090926	4.818089
462.869778	8000.278571	12.098599	-0.090991	4.818062
462.949223	8000.283906	12.103603	-0.091006	4.818063
462.614238	8000.341317	12.108608	-0.090944	4.818082
462.875439	8000.349210	12.113613	-0.090992	4.818083
462.823570	8000.282160	12.118618	-0.090983	4.818063
462.985336	8000.270755	12.123623	-0.091013	4.818059
462.942186	8000.317532	12.128627	-0.091005	4.818073
462.865364	8000.283821	12.133632	-0.090991	4.818064
462.856543	8000.342662	12.138637	-0.090989	4.818081
462.569926	8000.338637	12.143642	-0.090936	4.818081
462.940574	8000.289111	12.148647	-0.091005	4.818065
463.063344	8000.326641	12.153651	-0.091028	4.818075
462.898831	8000.256953	12.158656	-0.090998	4.818055
463.006217	8000.318482	12.163661	-0.091018	4.818073
462.734302	8000.290449	12.168666	-0.090967	4.818066
462.685208	8000.328719	12.173671	-0.090958	4.818078
462.740367	8000.371615	12.178675	-0.090969	4.818090
462.583897	8000.369421	12.183680	-0.090939	4.818090
462.810823	8000.349458	12.188685	-0.090982	4.818083
462.824150	8000.338071	12.193690	-0.090984	4.818080
462.852900	8000.336377	12.198695	-0.090990	4.818079
463.105336	8000.348358	12.203699	-0.091037	4.818082
463.113807	8000.227409	12.208704	-0.091039	4.818046
463.139144	8000.242512	12.213709	-0.091043	4.818050
462.995418	8000.326829	12.218714	-0.091017	4.818076
463.051185	8000.256028	12.223719	-0.091027	4.818054
463.243080	8000.289267	12.228723	-0.091063	4.818064
462.835522	8000.347762	12.233728	-0.090987	4.818083
462.733979	8000.401087	12.238733	-0.090968	4.818099
462.755155	8000.347698	12.243738	-0.090972	4.818083
463.016069	8000.317685	12.248743	-0.091021	4.818073
463.031190	8000.392656	12.253747	-0.091024	4.818095
462.845117	8000.330034	12.258752	-0.090989	4.818077
462.747452	8000.398153	12.263757	-0.090971	4.818098
462.920370	8000.359533	12.268762	-0.091004	4.818086
463.161283	8000.370299	12.273767	-0.091049	4.818088
462.903821	8000.404585	12.278771	-0.091001	4.818099
462.819845	8000.333924	12.283776	-0.090985	4.818078
463.161019	8000.367157	12.288781	-0.091049	4.818087
462.913593	8000.378423	12.293786	-0.091003	4.818091
462.758313	8000.380456	12.298791	-0.090974	4.818093
462.952274	8000.392668	12.303795	-0.091010	4.818095
462.838718	8000.390024	12.308800	-0.090989	4.818095
462.792816	8000.429392	12.313805	-0.090981	4.818107
462.529197	8000.381472	12.318810	-0.090932	4.818094
462.436668	8000.404392	12.323815	-0.090915	4.818101
462.652086	8000.453754	12.328819	-0.090955	4.818115
462.196727	8000.471570	12.333824	-0.090870	4.818122
462.507536	8000.452787	12.338829	-0.090928	4.818115
462.302660	8000.433067	12.343834	-0.090890	4.818110
462.520994	8000.352973	12.348839	-0.090931	4.818085
462.626636	8000.418687	12.353843	-0.090951	4.818104
462.174398	8000.428125	12.358848	-0.090866	4.818109
462.683570	8000.412133	12.363853	-0.090961	4.818102
462.516316	8000.377149	12.368858	-0.090930	4.818093
463.062095	8000.306925	12.373863	-0.091032	4.818069
462.886131	8000.395000	12.378867	-0.090999	4.818096
462.778522	8000.325059	12.383872	-0.090979	4.818076
462.945119	8000.370576	12.388877	-0.091011	4.818089
462.795284	8000.358999	12.393882	-0.090983	4.818086
462.778776	8000.338770	12.398887	-0.090980	4.818080
463.226903	8000.338765	12.403891	-0.091063	4.818078
462.959889	8000.347649	12.408896	-0.091014	4.818082
462.507101	8000.484469	12.413901	-0.090929	4.818124
462.311143	8000.476456	12.418906	-0.090893	4.818123
462.388960	8000.468082	12.423911	-0.090908	4.818120
462.281685	8000.422362	12.428915	-0.090888	4.818107
462.322176	8000.434519	12.433920	-0.090895	4.818110
462.350419	8000.398075	12.438925	-0.090901	4.818099
462.408268	8000.421004	12.443930	-0.090912	4.818106
462.520844	8000.406803	12.448935	-0.090933	4.818101
461.846914	8000.521562	12.453939	-0.090807	4.818138
462.280059	8000.430803	12.458944	-0.090888	4.818109
462.679836	8000.397479	12.463949	-0.090963	4.818098
462.497098	8000.340169	12.468954	-0.090929	4.818082
462.781855	8000.309439	12.473959	-0.090982	4.818071
463.109406	8000.342480	12.478963	-0.091043	4.818080
462.859207	8000.277903	12.483968	-0.090996	4.818062
463.163847	8000.374845	12.488973	-0.091053	4.818089
462.774069	8000.353575	12.493978	-0.090981	4.818084
462.823055	8000.363747	12.498983	-0.090990	4.818087
462.888363	8000.336246	12.503987	-0.091002	4.818079
463.111105	8000.254108	12.508992	-0.091044	4.818054
462.808153	8000.336185	12.513997	-0.090987	4.818079
462.646930	8000.329712	12.519002	-0.090957	4.818078
462.680219	8000.378617	12.524007	-0.090964	4.818092
462.498900	8000.409764	12.529011	-0.090930	4.818102
462.205995	8000.316162	12.534016	-0.090876	4.818076
462.638328	8000.442271	12.539021	-0.090956	4.818111
463.013200	8000.368590	12.544026	-0.091026	4.818088
462.908921	8000.350285	12.549031	-0.091007	4.818083
462.940556	8000.407589	12.554035	-0.091013	4.818100
462.996753	8000.333636	12.559040	-0.091023	4.818078
463.242231	8000.342361	12.564045	-0.091069	4.818079
463.202552	8000.355497	12.569050	-0.091062	4.818083
463.038561	8000.376358	12.574055	-0.091031	4.818090
462.865374	8000.404460	12.579059	-0.090999	4.818099
463.048958	8000.222806	12.584064	-0.091033	4.818044
463.127029	8000.351303	12.589069	-0.091048	4.818082
462.983518	8000.404038	12.594074	-0.091021	4.818098
463.204908	8000.303983	12.599079	-0.091063	4.818068
462.990350	8000.340978	12.604083	-0.091023	4.818080
463.078219	8000.274841	12.609088	-0.091039	4.818060
463.218888	8000.363159	12.614093	-0.091066	4.818085
463.078252	8000.298017	12.619098	-0.091039	4.818067
463.084212	8000.250731	12.624103	-0.091041	4.818053
463.072141	8000.340058	12.629107	-0.091039	4.818079
463.001137	8000.350647	12.634112	-0.091025	4.818083
463.275719	8000.322933	12.639117	-0.091077	4.818073
462.962368	8000.292210	12.644122	-0.091018	4.818065
463.335415	8000.245877	12.649127	-0.091088	4.818050
463.171457	8000.332015	12.654131	-0.091057	4.818076
463.162657	8000.280309	12.659136	-0.091056	4.818061
463.500064	8000.281905	12.664141	-0.091119	4.818060
463.265349	8000.314406	12.669146	-0.091075	4.818071
463.510658	8000.311547	12.674151	-0.091121	4.818069
463.769996	8000.267826	12.679155	-0.091169	4.818055
463.460263	8000.221361	12.684160	-0.091112	4.818042
463.295761	8000.283276	12.689165	-0.091081	4.818061
463.366058	8000.252688	12.694170	-0.091094	4.818052
463.257874	8000.332240	12.699175	-0.091074	4.818076
463.410647	8000.315446	12.704179	-0.091103	4.818070
463.203609	8000.254634	12.709184	-0.091064	4.818053
463.463777	8000.258302	12.714189	-0.091113	4.818053
463.471667	8000.198408	12.719194	-0.091114	4.818035
463.630798	8000.236450	12.724199	-0.091144	4.818046
463.686622	8000.254088	12.729203	-0.091155	4.818051
463.460598	8000.303556	12.734208	-0.091113	4.818067
463.378946	8000.362426	12.739213	-0.091098	4.818084
463.459475	8000.342509	12.744218	-0.091113	4.818078
463.344570	8000.306156	12.749223	-0.091091	4.818068
463.630736	8000.307031	12.754227	-0.091145	4.818067
463.259854	8000.231280	12.759232	-0.091076	4.818046
463.474288	8000.292210	12.764237	-0.091116	4.818063
463.444648	8000.281271	12.769242	-0.091110	4.818060
463.318535	8000.258447	12.774247	-0.091087	4.818054
463.438267	8000.310674	12.779251	-0.091109	4.818069
463.265812	8000.294568	12.784256	-0.091077	4.818065
463.361563	8000.296975	12.789261	-0.091095	4.818065
463.221070	8000.325537	12.794266	-0.091069	4.818074
463.125021	8000.306295	12.799271	-0.091051	4.818069
463.302566	8000.307747	12.804275	-0.091085	4.818068
463.198366	8000.236801	12.809280	-0.091065	4.818048
463.144303	8000.362387	12.814285	-0.091055	4.818085
463.425828	8000.356880	12.819290	-0.091108	4.818083
463.450746	8000.357237	12.824295	-0.091113	4.818083
463.178586	8000.414479	12.829299	-0.091062	4.818101
463.075502	8000.368816	12.834304	-0.091043	4.818088
463.030558	8000.389247	12.839309	-0.091035	4.818094
463.021283	8000.428079	12.844314	-0.091033	4.818105
462.723108	8000.462845	12.849319	-0.090978	4.818117
462.667835	8000.439965	12.854323	-0.090967	4.818110
463.336678	8000.344100	12.859328	-0.091092	4.818079
463.299671	8000.372012	12.864333	-0.091085	4.818088
463.270958	8000.335819	12.869338	-0.091080	4.818077
463.181125	8000.321928	12.874343	-0.091063	4.818073
462.956964	8000.363000	12.879347	-0.091022	4.818086
463.471630	8000.334452	12.884352	-0.091118	4.818076
463.223611	8000.380452	12.889357	-0.091072	4.818090
462.976573	8000.370666	12.894362	-0.091026	4.818088
463.034939	8000.335698	12.899367	-0.091037	4.818078
463.061695	8000.349768	12.904371	-0.091042	4.818082
463.234513	8000.264822	12.909376	-0.091074	4.818056
463.359839	8000.305547	12.914381	-0.091097	4.818068
463.113551	8000.321040	12.919386	-0.091052	4.818073
462.985859	8000.360310	12.924391	-0.091028	4.818085
462.952887	8000.403019	12.929395	-0.091022	4.818098
463.107597	8000.267282	12.934400	-0.091051	4.818057
463.144841	8000.323613	12.939405	-0.091058	4.818074
463.179680	8000.304107	12.944410	-0.091064	4.818068
463.149814	8000.267897	12.949415	-0.091059	4.818057
463.302601	8000.306903	12.954419	-0.091087	4.818068
462.853126	8000.320590	12.959424	-0.091004	4.818074
463.355095	8000.311867	12.964429	-0.091097	4.818069
463.336805	8000.291612	12.969434	-0.091094	4.818064
462.974750	8000.388650	12.974439	-0.091027	4.818094
463.102123	8000.428351	12.979443	-0.091051	4.818105
462.940315	8000.409235	12.984448	-0.091021	4.818100
463.003218	8000.410127	12.989453	-0.091032	4.818100
463.239370	8000.343971	12.994458	-0.091076	4.818079
463.109581	8000.428483	12.999463	-0.091052	4.818105
462.819300	8000.438092	13.004467	-0.090998	4.818109
463.080570	8000.336493	13.009472	-0.091047	4.818078
462.985049	8000.405695	13.014477	-0.091029	4.818099
462.801416	8000.409435	13.019482	-0.090995	4.818101
462.799262	8000.419940	13.024487	-0.090995	4.818104
462.904790	8000.398270	13.029491	-0.091015	4.818097
462.776231	8000.385940	13.034496	-0.090991	4.818094
463.224441	8000.332242	13.039501	-0.091074	4.818076
462.857777	8000.398682	13.044506	-0.091006	4.818097
463.041103	8000.365472	13.049511	-0.091040	4.818087
462.819537	8000.443429	13.054515	-0.090999	4.818111
462.203207	8000.433713	13.059520	-0.090885	4.818110
462.651178	8000.448444	13.064525	-0.090968	4.818113
462.708508	8000.425043	13.069530	-0.090979	4.818106
462.727184	8000.427418	13.074535	-0.090983	4.818106
462.220156	8000.491884	13.079539	-0.090888	4.818128
462.176480	8000.374414	13.084544	-0.090880	4.818093
462.352007	8000.488488	13.089549	-0.090913	4.818126
462.448881	8000.439323	13.094554	-0.090931	4.818111
462.541974	8000.422741	13.099559	-0.090949	4.818106
462.867935	8000.446285	13.104563	-0.091009	4.818111
462.403391	8000.438704	13.109568	-0.090923	4.818111
462.680414	8000.446819	13.114573	-0.090975	4.818112
463.149649	8000.314455	13.119578	-0.091062	4.818071
463.118451	8000.344555	13.124583	-0.091056	4.818080
463.414956	8000.325572	13.129587	-0.091112	4.818073
463.252164	8000.318024	13.134592	-0.091081	4.818072
463.035350	8000.430792	13.139597	-0.091041	4.818106
462.443025	8000.434046	13.144602	-0.090931	4.818109
462.655784	8000.449680	13.149607	-0.090971	4.818113
462.878625	8000.473879	13.154611	-0.091012	4.818119
462.887072	8000.389778	13.159616	-0.091014	4.818094
462.439750	8000.446661	13.164621	-0.090931	4.818113
463.157725	8000.295687	13.169626	-0.091064	4.818065
462.589447	8000.404563	13.174631	-0.090959	4.818100
462.567533	8000.431635	13.179635	-0.090955	4.818108
462.742543	8000.319346	13.184640	-0.090987	4.818074
463.469280	8000.269567	13.189645	-0.091123	4.818056
463.115616	8000.319345	13.194650	-0.091057	4.818073
462.930965	8000.314648	13.199655	-0.091023	4.818072
463.157209	8000.414699	13.204659	-0.091065	4.818101
462.681912	8000.455395	13.209664	-0.090977	4.818115
463.177190	8000.382356	13.214669	-0.091069	4.818091
463.122115	8000.407908	13.219674	-0.091059	4.818099
463.025882	8000.396033	13.224679	-0.091041	4.818096
463.432496	8000.370177	13.229683	-0.091117	4.818086
463.125638	8000.325858	13.234688	-0.091060	4.818074
463.542081	8000.321197	13.239693	-0.091137	4.818071
463.567648	8000.345779	13.244698	-0.091142	4.818078
463.021245	8000.327569	13.249703	-0.091040	4.818075
463.153045	8000.419973	13.254707	-0.091065	4.818102
463.213657	8000.341871	13.259712	-0.091076	4.818079
463.266567	8000.308932	13.264717	-0.091086	4.818069
463.373718	8000.317816	13.269722	-0.091106	4.818071
463.410414	8000.276226	13.274727	-0.091113	4.818059
463.096833	8000.341308	13.279731	-0.091055	4.818079
463.365165	8000.317717	13.284736	-0.091105	4.818071
463.642893	8000.349006	13.289741	-0.091157	4.818079
463.734568	8000.273445	13.294746	-0.091174	4.818056
463.564816	8000.278433	13.299751	-0.091143	4.818059
463.617190	8000.368669	13.304755	-0.091152	4.818085
463.638352	8000.259478	13.309760	-0.091156	4.818053
463.535541	8000.330684	13.314765	-0.091137	4.818074
463.711782	8000.225782	13.319770	-0.091170	4.818042
463.638738	8000.235289	13.324775	-0.091157	4.818045
463.792046	8000.260616	13.329779	-0.091185	4.818052
463.811969	8000.220895	13.334784	-0.091189	4.818040
463.493663	8000.258537	13.339789	-0.091130	4.818053
463.449270	8000.301085	13.344794	-0.091122	4.818066
463.675236	8000.255841	13.349799	-0.091164	4.818051
463.616728	8000.333988	13.354803	-0.091153	4.818075
463.639483	8000.263775	13.359808	-0.091158	4.818054
463.486524	8000.276369	13.364813	-0.091129	4.818058
463.412355	8000.247959	13.369818	-0.091115	4.818050
463.664667	8000.235724	13.374823	-0.091162	4.818045
463.741108	8000.321033	13.379827	-0.091177	4.818070
463.323983	8000.373076	13.384832	-0.091099	4.818088
463.747273	8000.328504	13.389837	-0.091178	4.818073
463.879320	8000.290361	13.394842	-0.091203	4.818061
463.623486	8000.248866	13.399847	-0.091155	4.818049
463.420860	8000.379731	13.404851	-0.091118	4.818089
463.324837	8000.307847	13.409856	-0.091100	4.818068
463.079564	8000.392841	13.414861	-0.091054	4.818094
463.110525	8000.373280	13.419866	-0.091060	4.818088
463.458906	8000.263430	13.424871	-0.091125	4.818054
463.426439	8000.296671	13.429875	-0.091119	4.818064
463.534635	8000.246611	13.434880	-0.091139	4.818049
463.450876	8000.383361	13.439885	-0.091124	4.818090
463.359208	8000.354704	13.444890	-0.091107	4.818082
463.427651	8000.285134	13.449895	-0.091120	4.818061
463.265327	8000.353397	13.454899	-0.091090	4.818082
463.417542	8000.241840	13.459904	-0.091118	4.818048
463.536199	8000.286682	13.464909	-0.091140	4.818061
463.738148	8000.351649	13.469914	-0.091178	4.818079
463.735845	8000.300034	13.474919	-0.091178	4.818064
463.534312	8000.298258	13.479923	-0.091140	4.818064
463.315566	8000.274130	13.484928	-0.091100	4.818058
463.789827	8000.277652	13.489933	-0.091188	4.818057
463.797686	8000.271453	13.494938	-0.091189	4.818055
463.530574	8000.248750	13.499943	-0.091140	4.818050
463.602076	8000.367681	13.504947	-0.091153	4.818085
463.368378	8000.319127	13.509952	-0.091110	4.818071
463.419019	8000.335639	13.514957	-0.091119	4.818076
463.450513	8000.343459	13.519962	-0.091125	4.818078
463.431133	8000.305291	13.524967	-0.091122	4.818067
463.347722	8000.297807	13.529971	-0.091106	4.818065
463.204155	8000.276843	13.534976	-0.091080	4.818059
463.326636	8000.307000	13.539981	-0.091103	4.818068
463.246535	8000.266925	13.544986	-0.091088	4.818056
463.271231	8000.315710	13.549991	-0.091092	4.818071
463.258299	8000.396603	13.554995	-0.091090	4.818095
463.101439	8000.400720	13.560000	-0.091061	4.818097
463.125136	8000.375792	13.565005	-0.091066	4.818089
463.062807	8000.378080	13.570010	-0.091054	4.818090
463.111560	8000.379826	13.575015	-0.091063	4.818090
463.037678	8000.449333	13.580019	-0.091050	4.818111
463.177923	8000.314446	13.585024	-0.091076	4.818071
463.239562	8000.392177	13.590029	-0.091087	4.818093
463.099982	8000.399695	13.595034	-0.091061	4.818096
463.142767	8000.355032	13.600039	-0.091070	4.818083
463.165982	8000.422747	13.605043	-0.091074	4.818103
463.308742	8000.347906	13.610048	-0.091101	4.818080
463.165664	8000.381696	13.615053	-0.091074	4.818091
463.439658	8000.357132	13.620058	-0.091125	4.818082
463.306172	8000.329992	13.625063	-0.091100	4.818075
463.578800	8000.366474	13.630067	-0.091151	4.818084
463.169840	8000.391258	13.635072	-0.091075	4.818093
463.120851	8000.429530	13.640077	-0.091066	4.818105
463.265963	8000.401047	13.645082	-0.091093	4.818096
463.379656	8000.352118	13.650087	-0.091115	4.818081
463.605371	8000.363724	13.655091	-0.091157	4.818083
463.314078	8000.333311	13.660096	-0.091103	4.818076
463.229099	8000.399503	13.665101	-0.091087	4.818096
462.990450	8000.418261	13.670106	-0.091042	4.818102
463.343612	8000.260049	13.675111	-0.091108	4.818054
463.599696	8000.322618	13.680115	-0.091156	4.818071
463.178288	8000.326171	13.685120	-0.091078	4.818074
463.320023	8000.349229	13.690125	-0.091104	4.818080
463.115469	8000.402157	13.695130	-0.091066	4.818097
463.312832	8000.430210	13.700135	-0.091103	4.818104
463.429524	8000.467656	13.705139	-0.091125	4.818115
463.371720	8000.419471	13.710144	-0.091114	4.818101
463.058045	8000.406641	13.715149	-0.091056	4.818098
462.863972	8000.429185	13.720154	-0.091020	4.818106
463.570418	8000.323321	13.725159	-0.091151	4.818072
463.606419	8000.420697	13.730163	-0.091158	4.818100
463.317750	8000.389267	13.735168	-0.091105	4.818092
463.221609	8000.425823	13.740173	-0.091087	4.818103
463.257768	8000.403176	13.745178	-0.091094	4.818097
463.204125	8000.333994	13.750183	-0.091084	4.818076
463.442270	8000.297344	13.755187	-0.091128	4.818064
463.097027	8000.366192	13.760192	-0.091064	4.818086
463.401619	8000.327319	13.765197	-0.091121	4.818073
463.389585	8000.346107	13.770202	-0.091119	4.818079
463.335805	8000.301138	13.775207	-0.091109	4.818066
463.320630	8000.364102	13.780211	-0.091106	4.818085
463.290248	8000.340519	13.785216	-0.091100	4.818078
463.255006	8000.403200	13.790221	-0.091094	4.818097
463.279264	8000.382492	13.795226	-0.091099	4.818090
463.113643	8000.374904	13.800231	-0.091068	4.818089
463.417983	8000.392880	13.805235	-0.091125	4.818093
463.568222	8000.291823	13.810240	-0.091153	4.818062
463.700622	8000.347389	13.815245	-0.091177	4.818078
463.397771	8000.355767	13.820250	-0.091121	4.818082
463.239109	8000.320904	13.825255	-0.091092	4.818072
463.584467	8000.356303	13.830259	-0.091156	4.818081
463.667730	8000.289047	13.835264	-0.091172	4.818061
463.335678	8000.331759	13.840269	-0.091110	4.818075
463.643952	8000.288726	13.845274	-0.091167	4.818061
463.517342	8000.348016	13.850279	-0.091144	4.818079
463.333700	8000.384394	13.855283	-0.091110	4.818091
463.244520	8000.333662	13.860288	-0.091093	4.818076
463.714529	8000.339231	13.865293	-0.091181	4.818076
463.368423	8000.355424	13.870298	-0.091116	4.818082
463.390855	8000.272572	13.875303	-0.091121	4.818057
463.547511	8000.344271	13.880307	-0.091150	4.818078
463.297613	8000.313388	13.885312	-0.091104	4.818070
463.538098	8000.371526	13.890317	-0.091148	4.818086
463.900549	8000.298724	13.895322	-0.091216	4.818063
463.266889	8000.375093	13.900327	-0.091098	4.818088
463.061562	8000.454332	13.905331	-0.091060	4.818113
463.100336	8000.403296	13.910336	-0.091067	4.818097
463.765739	8000.376871	13.915341	-0.091191	4.818087
463.280898	8000.404798	13.920346	-0.091101	4.818097
463.419018	8000.353054	13.925351	-0.091127	4.818081
463.477205	8000.399152	13.930355	-0.091138	4.818094
462.747648	8000.448903	13.935360	-0.091002	4.818112
463.080300	8000.416742	13.940365	-0.091064	4.818101
463.196105	8000.453122	13.945370	-0.091086	4.818112
463.793048	8000.345718	13.950375	-0.091197	4.818077
463.531607	8000.424167	13.955379	-0.091148	4.818102
463.462238	8000.431621	13.960384	-0.091136	4.818104
463.648413	8000.407927	13.965389	-0.091170	4.818096
463.545993	8000.382277	13.970394	-0.091151	4.818089
463.604285	8000.293613	13.975399	-0.091162	4.818063
463.619407	8000.398064	13.980403	-0.091165	4.818093
463.224740	8000.426207	13.985408	-0.091092	4.818103
462.988375	8000.466054	13.990413	-0.091048	4.818116
462.875880	8000.369723	13.995418	-0.091027	4.818088
463.441118	8000.413481	14.000423	-0.091132	4.818099
463.479127	8000.416128	14.005427	-0.091140	4.818099
463.264971	8000.427861	14.010432	-0.091100	4.818104
463.333427	8000.459364	14.015437	-0.091113	4.818113
463.480851	8000.414068	14.020442	-0.091140	4.818099
463.448418	8000.377822	14.025447	-0.091134	4.818088
463.341237	8000.349999	14.030451	-0.091114	4.818080
463.502905	8000.367021	14.035456	-0.091145	4.818085
463.286852	8000.456637	14.040461	-0.091104	4.818112
463.662189	8000.385069	14.045466	-0.091174	4.818089
463.526139	8000.416853	14.050471	-0.091149	4.818099
463.651733	8000.425997	14.055475	-0.091173	4.818102
463.365253	8000.472508	14.060480	-0.091119	4.818117
463.259102	8000.449964	14.065485	-0.091100	4.818110
463.191769	8000.444812	14.070490	-0.091087	4.818109
463.171952	8000.411902	14.075495	-0.091084	4.818099
463.258765	8000.467879	14.080499	-0.091100	4.818116
463.435280	8000.449313	14.085504	-0.091133	4.818109
463.257248	8000.409965	14.090509	-0.091100	4.818098
462.843092	8000.467314	14.095514	-0.091023	4.818117
463.779017	8000.306774	14.100519	-0.091197	4.818066
463.537974	8000.410778	14.105523	-0.091152	4.818098
462.899221	8000.430222	14.110528	-0.091034	4.818106
462.681947	8000.494553	14.115533	-0.090993	4.818126
462.788749	8000.423418	14.120538	-0.091013	4.818104
462.980273	8000.488237	14.125543	-0.091049	4.818123
462.939967	8000.485571	14.130547	-0.091042	4.818122
463.178433	8000.432081	14.135552	-0.091086	4.818105
463.035291	8000.454288	14.140557	-0.091059	4.818113
462.985418	8000.415691	14.145562	-0.091050	4.818101
463.135995	8000.412553	14.150567	-0.091078	4.818100
463.047156	8000.443948	14.155571	-0.091062	4.818109
463.150395	8000.372762	14.160576	-0.091081	4.818088
463.582249	8000.351473	14.165581	-0.091162	4.818080
463.571651	8000.409237	14.170586	-0.091160	4.818097
463.220511	8000.411672	14.175591	-0.091095	4.818099
463.289892	8000.343168	14.180595	-0.091108	4.818078
463.400235	8000.413162	14.185600	-0.091128	4.818099
463.232031	8000.455021	14.190605	-0.091097	4.818112
463.197719	8000.416643	14.195610	-0.091091	4.818101
463.364988	8000.420057	14.200615	-0.091122	4.818101
463.484744	8000.450176	14.205619	-0.091144	4.818109
463.127563	8000.367246	14.210624	-0.091078	4.818086
463.411717	8000.389150	14.215629	-0.091131	4.818092
463.155260	8000.465563	14.220634	-0.091083	4.818115
463.155726	8000.416094	14.225639	-0.091083	4.818101
463.009058	8000.487735	14.230643	-0.091056	4.818123
463.085229	8000.440383	14.235648	-0.091071	4.818108
463.466900	8000.340478	14.240653	-0.091142	4.818077
463.425471	8000.389385	14.245658	-0.091134	4.818092
463.113717	8000.471337	14.250663	-0.091076	4.818117
463.375601	8000.463449	14.255667	-0.091125	4.818114
462.932232	8000.454058	14.260672	-0.091043	4.818113
463.519228	8000.419159	14.265677	-0.091152	4.818100
463.511227	8000.423265	14.270682	-0.091150	4.818101
463.248333	8000.407991	14.275687	-0.091102	4.818098
463.530832	8000.423555	14.280691	-0.091154	4.818101
463.601473	8000.384548	14.285696	-0.091168	4.818089
463.433404	8000.372714	14.290701	-0.091136	4.818087
463.303037	8000.442479	14.295706	-0.091112	4.818108
462.646762	8000.378504	14.300711	-0.090990	4.818092
462.904294	8000.506369	14.305715	-0.091038	4.818128
462.632729	8000.438331	14.310720	-0.090988	4.818109
462.961220	8000.487180	14.315725	-0.091049	4.818123
463.402064	8000.472335	14.320730	-0.091131	4.818116
463.118304	8000.430445	14.325735	-0.091078	4.818105
463.322168	8000.457537	14.330739	-0.091116	4.818112
463.766892	8000.381682	14.335744	-0.091199	4.818088
463.862318	8000.327231	14.340749	-0.091217	4.818071
463.786904	8000.370396	14.345754	-0.091203	4.818084
463.796075	8000.318942	14.350759	-0.091205	4.818069
463.633862	8000.355621	14.355763	-0.091175	4.818081
463.367366	7999.303284	14.360768	-0.091125	4.817770

463.253510	7996.302634	14.365773	-0.091102	4.816880
463.878287	7990.637861	14.370778	-0.091214	4.815197
463.703324	7984.002587	14.375783	-0.091177	4.813229
463.734264	7976.788330	14.380787	-0.091179	4.811087
463.656997	7969.081951	14.385792	-0.091159	4.808798
463.658686	7961.362458	14.390797	-0.091155	4.806504
463.848176	7953.400286	14.395802	-0.091185	4.804136
463.682451	7945.578052	14.400807	-0.091149	4.801810
464.078357	7937.548587	14.405811	-0.091218	4.799419
463.683953	7929.597071	14.410816	-0.091139	4.797052
463.676433	7921.529666	14.415821	-0.091132	4.794649
463.706633	7913.613376	14.420826	-0.091133	4.792289
463.594926	7905.522423	14.425831	-0.091107	4.789877
463.514568	7897.606482	14.430835	-0.091087	4.787516
463.710569	7889.490599	14.435840	-0.091118	4.785092
463.619503	7881.535447	14.440845	-0.091096	4.782717
463.326386	7873.552820	14.445850	-0.091037	4.780333
463.357105	7865.518285	14.450855	-0.091037	4.777930
463.564498	7857.560621	14.455859	-0.091071	4.775550
463.554527	7849.534710	14.460864	-0.091064	4.773148
463.533895	7841.515868	14.465869	-0.091055	4.770747
463.500993	7833.469699	14.470874	-0.091043	4.768337
463.225508	7825.509587	14.475879	-0.090987	4.765952
462.851411	7817.504743	14.480883	-0.090912	4.763553
463.258480	7809.534350	14.485888	-0.090983	4.761160
462.804777	7801.564010	14.490893	-0.090893	4.758769
463.122096	7793.562232	14.495898	-0.090947	4.756365
463.098771	7785.459566	14.500903	-0.090938	4.753931
463.196877	7777.528241	14.505907	-0.090951	4.751546
462.977337	7769.467422	14.510912	-0.090905	4.749122
463.001135	7761.479207	14.515917	-0.090904	4.746718
463.153638	7753.455649	14.520922	-0.090928	4.744302
462.953448	7745.510018	14.525927	-0.090885	4.741909
463.091981	7737.450960	14.530931	-0.090906	4.739480
463.144946	7729.437786	14.535936	-0.090911	4.737063
463.167444	7721.431569	14.540941	-0.090910	4.734648
463.059601	7713.479178	14.545946	-0.090884	4.732248
463.211676	7705.368344	14.550951	-0.090908	4.729798
463.171905	7697.503118	14.555955	-0.090895	4.727421
463.128088	7689.416772	14.560960	-0.090882	4.724977
462.784695	7681.531893	14.565965	-0.090813	4.722593
462.680271	7673.560813	14.570970	-0.090788	4.720181
462.707644	7665.509080	14.575975	-0.090788	4.717743
462.721117	7657.536640	14.580979	-0.090786	4.715327
462.494720	7649.518553	14.585984	-0.090738	4.712898
462.530116	7641.480372	14.590989	-0.090740	4.710460
462.581096	7633.450542	14.595994	-0.090744	4.708024
462.565657	7625.370034	14.600999	-0.090736	4.705571
462.724401	7617.479562	14.606003	-0.090761	4.703174
462.636915	7609.459431	14.611008	-0.090739	4.700737
462.507466	7601.482326	14.616013	-0.090710	4.698312
462.721858	7593.486220	14.621018	-0.090745	4.695879
462.508898	7585.461702	14.626023	-0.090700	4.693437
462.657324	7577.495106	14.631027	-0.090722	4.691011
462.553127	7569.429221	14.636032	-0.090698	4.688553
462.543035	7561.482615	14.641037	-0.090691	4.686131
462.765647	7553.398634	14.646042	-0.090727	4.683665
462.294879	7545.528449	14.651047	-0.090635	4.681264
462.164625	7537.496826	14.656051	-0.090605	4.678812
462.289437	7529.525325	14.661056	-0.090623	4.676377
462.407324	7521.451711	14.666061	-0.090640	4.673909
462.412425	7513.431061	14.671066	-0.090636	4.671457
462.074511	7505.418000	14.676071	-0.090568	4.669005
462.146902	7497.483468	14.681075	-0.090576	4.666576
462.186019	7489.384844	14.686080	-0.090578	4.664096
462.281250	7481.466812	14.691085	-0.090591	4.661670
462.164290	7473.439600	14.696090	-0.090564	4.659209
462.011215	7465.446150	14.701095	-0.090530	4.656756
461.949429	7457.433671	14.706099	-0.090514	4.654297
461.941292	7449.437694	14.711104	-0.090507	4.651842
462.111711	7441.385093	14.716109	-0.090534	4.649368
462.322885	7433.440295	14.721114	-0.090568	4.646925
462.414225	7425.346353	14.726119	-0.090580	4.644436
462.132209	7417.515377	14.731123	-0.090522	4.642026
461.804510	7409.428075	14.736128	-0.090456	4.639536
461.997464	7401.449370	14.741133	-0.090487	4.637078
462.456543	7393.350106	14.746138	-0.090567	4.634582
462.048085	7385.431863	14.751143	-0.090486	4.632139
462.008487	7377.412383	14.756147	-0.090474	4.629665
461.698287	7369.460226	14.761152	-0.090411	4.627210
461.595258	7361.389862	14.766157	-0.090386	4.624717
461.551954	7353.486393	14.771162	-0.090373	4.622274
461.454414	7345.404533	14.776167	-0.090350	4.619775
461.759510	7337.422121	14.781171	-0.090402	4.617306
461.947760	7329.320109	14.786176	-0.090431	4.614798
461.919921	7321.369074	14.791181	-0.090421	4.612335
462.201350	7313.336900	14.796186	-0.090468	4.609846
462.120615	7305.349229	14.801191	-0.090448	4.607370
461.976183	7297.416386	14.806195	-0.090416	4.604908
461.679875	7289.447102	14.811200	-0.090356	4.602435
461.693792	7281.377667	14.816205	-0.090353	4.599929
461.803268	7273.401690	14.821210	-0.090369	4.597450
461.679611	7265.356564	14.826215	-0.090341	4.594949
461.736041	7257.416505	14.831219	-0.090346	4.592479
461.577153	7249.347215	14.836224	-0.090311	4.589967
461.614167	7241.325664	14.841229	-0.090313	4.587470
461.595124	7233.361822	14.846234	-0.090304	4.584988
461.882176	7225.339789	14.851239	-0.090353	4.582488
461.748276	7217.317095	14.856243	-0.090323	4.579985
461.541834	7209.346221	14.861248	-0.090279	4.577497
461.522891	7201.353786	14.866253	-0.090270	4.575002
461.768310	7193.370270	14.871258	-0.090311	4.572508
461.537476	7185.317849	14.876263	-0.090263	4.569990
461.504000	7177.360609	14.881267	-0.090252	4.567501
461.369462	7169.280681	14.886272	-0.090221	4.564972
461.330447	7161.349227	14.891277	-0.090209	4.562489
461.302654	7153.355294	14.896282	-0.090199	4.559984
461.416351	7145.325997	14.901287	-0.090215	4.557468
461.275526	7137.350611	14.906291	-0.090183	4.554966
461.237846	7129.352088	14.911296	-0.090171	4.552456
461.093580	7121.297140	14.916301	-0.090139	4.549927
461.274305	7113.308897	14.921306	-0.090168	4.547417
461.109883	7105.249191	14.926311	-0.090132	4.544884
461.060283	7097.362853	14.931315	-0.090118	4.542403
461.170600	7089.281199	14.936320	-0.090133	4.539860
461.283611	7081.298187	14.941325	-0.090149	4.537347
461.128620	7073.253455	14.946330	-0.090115	4.534812
461.247269	7065.261435	14.951335	-0.090132	4.532293
461.400054	7057.217111	14.956339	-0.090155	4.529757
461.382099	7049.271749	14.961344	-0.090147	4.527250
461.469079	7041.226044	14.966349	-0.090158	4.524709
461.469503	7033.328899	14.971354	-0.090153	4.522215
461.466449	7025.288039	14.976359	-0.090147	4.519673
461.128612	7017.357614	14.981363	-0.090079	4.517164
460.956658	7009.308768	14.986368	-0.090042	4.514616
460.589648	7001.360167	14.991373	-0.089969	4.512098
460.933859	6993.264960	14.996378	-0.090028	4.509535
460.579790	6985.241651	15.001383	-0.089956	4.506991
460.557641	6977.237170	15.006387	-0.089947	4.504452
460.297777	6969.304730	15.011392	-0.089894	4.501934
460.573062	6961.216560	15.016397	-0.089940	4.499366
460.490124	6953.274496	15.021402	-0.089919	4.496843
460.696140	6945.186328	15.026407	-0.089952	4.494272
460.943394	6937.247461	15.031411	-0.089993	4.491748
460.854756	6929.197314	15.036416	-0.089972	4.489186
460.943121	6921.234942	15.041421	-0.089983	4.486651
460.671070	6913.221714	15.046426	-0.089927	4.484097
460.557718	6905.301260	15.051431	-0.089901	4.481572
460.810681	6897.213356	15.056435	-0.089943	4.478993
460.286421	6889.281821	15.061440	-0.089840	4.476459
460.556352	6881.196055	15.066445	-0.089885	4.473878
460.671284	6873.233152	15.071450	-0.089902	4.471334
460.493422	6865.195700	15.076455	-0.089864	4.468764
460.331271	6857.250549	15.081459	-0.089828	4.466222
460.512360	6849.173600	15.086464	-0.089857	4.463638
460.258191	6841.200932	15.091469	-0.089804	4.461083
460.439481	6833.171225	15.096474	-0.089833	4.458511
460.134640	6825.230002	15.101479	-0.089771	4.455963
460.181718	6817.177396	15.106483	-0.089775	4.453380
460.433462	6809.168229	15.111488	-0.089816	4.450810
460.348181	6801.161851	15.116493	-0.089795	4.448239
460.445764	6793.185531	15.121498	-0.089809	4.445676
460.337537	6785.178122	15.126503	-0.089783	4.443100
460.140634	6777.281556	15.131507	-0.089742	4.440559
460.160825	6769.200996	15.136512	-0.089740	4.437957
460.060770	6761.193950	15.141517	-0.089716	4.435378
460.255316	6753.164575	15.146522	-0.089747	4.432791
460.351298	6745.106589	15.151527	-0.089760	4.430193
460.196513	6737.167717	15.156531	-0.089726	4.427630
460.299483	6729.104492	15.161536	-0.089740	4.425027
460.431736	6721.147890	15.166541	-0.089760	4.422458
460.023401	6713.194510	15.171546	-0.089679	4.419885
460.245997	6705.129815	15.176551	-0.089715	4.417277
460.370977	6697.125518	15.181555	-0.089733	4.414688
460.373340	6689.138651	15.186560	-0.089728	4.412101
460.087114	6681.088435	15.191565	-0.089670	4.409491
460.344345	6673.158418	15.196570	-0.089713	4.406922
460.310347	6665.095864	15.201575	-0.089701	4.404306
460.505288	6657.178123	15.206579	-0.089733	4.401738
460.206898	6649.070420	15.211584	-0.089672	4.399103
460.344845	6641.178440	15.216589	-0.089692	4.396539
460.460101	6633.137871	15.221594	-0.089709	4.393925
460.293986	6625.127615	15.226599	-0.089673	4.391318
460.306698	6617.133091	15.231603	-0.089670	4.388715
460.051996	6609.162940	15.236608	-0.089617	4.386118
460.036873	6601.097108	15.241613	-0.089609	4.383489
460.029761	6593.197701	15.246618	-0.089603	4.380912
460.032964	6585.180318	15.251623	-0.089599	4.378296
460.091513	6577.188588	15.256627	-0.089604	4.375687
459.724817	6569.239994	15.261632	-0.089531	4.373088
459.902349	6561.176112	15.266637	-0.089559	4.370453
460.126911	6553.163748	15.271642	-0.089596	4.367833
459.655071	6545.180415	15.276647	-0.089503	4.365217
460.026415	6537.237385	15.281651	-0.089567	4.362618
459.863733	6529.234286	15.286656	-0.089531	4.359995
459.703602	6521.280759	15.291661	-0.089496	4.357385
459.856383	6513.237671	15.296666	-0.089520	4.354748
459.942546	6505.185670	15.301671	-0.089530	4.352105
460.095391	6497.169344	15.306675	-0.089554	4.349473
459.359267	6489.259540	15.311680	-0.089412	4.346867
459.529551	6481.170927	15.316685	-0.089438	4.344208
459.830242	6473.249233	15.321690	-0.089489	4.341604
459.335844	6465.198933	15.326695	-0.089392	4.338949
459.504009	6457.206502	15.331699	-0.089418	4.336317
459.721638	6449.213913	15.336704	-0.089453	4.333684
459.447133	6441.213182	15.341709	-0.089397	4.331042
459.503205	6433.210488	15.346714	-0.089403	4.328401
459.430061	6425.149636	15.351719	-0.089384	4.325738
459.536402	6417.246181	15.356723	-0.089399	4.323126
459.516711	6409.212765	15.361728	-0.089390	4.320470
459.455343	6401.245700	15.366733	-0.089373	4.317833
459.455853	6393.279165	15.371738	-0.089368	4.315195
459.297330	6385.240484	15.376743	-0.089334	4.312530
459.170396	6377.248410	15.381747	-0.089305	4.309880
459.297147	6369.187107	15.386752	-0.089323	4.307207
459.445300	6361.118932	15.391757	-0.089346	4.304530
459.521015	6353.177877	15.396762	-0.089355	4.301893
459.234103	6345.129034	15.401767	-0.089296	4.299216
459.551070	6337.137987	15.406771	-0.089350	4.296561
459.246729	6329.128796	15.411776	-0.089288	4.293893
458.953510	6321.220027	15.416781	-0.089229	4.291257
458.987550	6313.165072	15.421786	-0.089230	4.288574
458.885052	6305.167524	15.426791	-0.089205	4.285907
459.193938	6297.134801	15.431795	-0.089258	4.283230
458.913679	6289.206351	15.436800	-0.089201	4.280581
459.359653	6281.153550	15.441805	-0.089278	4.277896
459.134151	6273.224223	15.446810	-0.089231	4.275243
459.246540	6265.134601	15.451815	-0.089247	4.272539
459.070901	6257.150517	15.456819	-0.089209	4.269866
459.184752	6249.122282	15.461824	-0.089225	4.267179
459.081657	6241.115513	15.466829	-0.089201	4.264495
459.307916	6233.202103	15.471834	-0.089238	4.261844
459.092176	6225.118409	15.476839	-0.089193	4.259130
459.073008	6217.205302	15.481843	-0.089184	4.256474
458.855600	6209.104131	15.486848	-0.089139	4.253750
458.914731	6201.200640	15.491853	-0.089144	4.251094
458.869331	6193.162273	15.496858	-0.089131	4.248390
458.747033	6185.148045	15.501863	-0.089103	4.245692
458.948815	6177.131984	15.506867	-0.089135	4.242995
458.836186	6169.154562	15.511872	-0.089109	4.240305
458.486142	6161.194128	15.516877	-0.089039	4.237618
458.644095	6153.214967	15.521882	-0.089063	4.234927
458.671332	6145.127458	15.526887	-0.089063	4.232197
458.757305	6137.159740	15.531891	-0.089074	4.229506
458.797301	6129.139416	15.536896	-0.089076	4.226795
458.610185	6121.096321	15.541901	-0.089036	4.224072
458.772731	6113.152530	15.546906	-0.089062	4.221385
458.632984	6105.138600	15.551911	-0.089031	4.218670
458.609382	6097.189710	15.556915	-0.089021	4.215975
458.664747	6089.134778	15.561920	-0.089026	4.213244
458.729340	6081.107746	15.566925	-0.089033	4.210521
458.638489	6073.136000	15.571930	-0.089011	4.207813
458.459387	6065.123648	15.576935	-0.088973	4.205088
458.020353	6057.243566	15.581939	-0.088886	4.202404
457.998577	6049.162207	15.586944	-0.088877	4.199654
458.196086	6041.184246	15.591949	-0.088908	4.196940
458.149789	6033.162771	15.596954	-0.088894	4.194207
458.282781	6025.069996	15.601959	-0.088914	4.191449
458.542071	6017.060543	15.606963	-0.088957	4.188720
458.274320	6009.061440	15.611968	-0.088902	4.185987
458.095870	6001.102069	15.616973	-0.088864	4.183266
458.168385	5993.162102	15.621978	-0.088872	4.180553
458.226425	5985.076295	15.626983	-0.088878	4.177788
458.344700	5977.101322	15.631987	-0.088895	4.175060
458.192371	5969.119166	15.636992	-0.088861	4.172324
458.077468	5961.088172	15.641997	-0.088835	4.169571
458.114288	5953.121758	15.647002	-0.088837	4.166839
457.791450	5945.067919	15.652007	-0.088771	4.164072
458.097321	5937.163299	15.657011	-0.088823	4.161361
458.303599	5929.120166	15.662016	-0.088856	4.158600
457.984455	5921.178544	15.667021	-0.088792	4.155865
457.906725	5913.155459	15.672026	-0.088772	4.153104
457.962125	5905.120168	15.677031	-0.088778	4.150338
457.937921	5897.163817	15.682035	-0.088768	4.147597
457.687197	5889.105274	15.687040	-0.088716	4.144815
457.850046	5881.179760	15.692045	-0.088741	4.142083
457.911701	5873.153817	15.697050	-0.088748	4.139314
457.837599	5865.216947	15.702055	-0.088729	4.136571
457.995537	5857.137546	15.707059	-0.088753	4.133780
457.808644	5849.180435	15.712064	-0.088713	4.131025
457.704816	5841.113731	15.717069	-0.088689	4.128232
457.918588	5833.160159	15.722074	-0.088723	4.125480
457.814596	5825.140357	15.727079	-0.088699	4.122699
457.887920	5817.193814	15.732083	-0.088707	4.119943
457.700641	5809.197096	15.737088	-0.088667	4.117165
457.856512	5801.109720	15.742093	-0.088691	4.114359
457.621705	5793.203957	15.747098	-0.088642	4.111608
457.333579	5785.157631	15.752103	-0.088584	4.108806
457.678838	5777.182270	15.757107	-0.088643	4.106035
457.830095	5769.155396	15.762112	-0.088666	4.103242
457.685389	5761.151207	15.767117	-0.088634	4.100450
457.475971	5753.177526	15.772122	-0.088590	4.097667
457.606482	5745.134739	15.777127	-0.088609	4.094862
457.764404	5737.134728	15.782131	-0.088633	4.092070
457.559030	5729.128215	15.787136	-0.088590	4.089270
457.612827	5721.146952	15.792141	-0.088595	4.086480
457.549174	5713.159038	15.797146	-0.088578	4.083684
457.216177	5705.193173	15.802151	-0.088511	4.080889
457.397540	5697.187379	15.807155	-0.088539	4.078087
457.361621	5689.164986	15.812160	-0.088527	4.075273
457.331801	5681.136336	15.817165	-0.088517	4.072456
457.287799	5673.147637	15.822170	-0.088503	4.069650
457.314501	5665.108173	15.827175	-0.088503	4.066825
457.306509	5657.115714	15.832179	-0.088497	4.064015
457.126255	5649.177876	15.837184	-0.088458	4.061219
457.179535	5641.149540	15.842189	-0.088463	4.058393
457.196963	5633.169963	15.847194	-0.088461	4.055582
457.001498	5625.161812	15.852199	-0.088419	4.052755
457.235143	5617.144120	15.857203	-0.088458	4.049930
457.186480	5609.139906	15.862208	-0.088444	4.047103
457.033290	5601.134439	15.867213	-0.088410	4.044272
457.140543	5593.209614	15.872218	-0.088425	4.041471
457.061639	5585.162691	15.877223	-0.088405	4.038623
457.285739	5577.192565	15.882227	-0.088442	4.035804
457.182396	5569.136916	15.887232	-0.088417	4.032948
457.238351	5561.078086	15.892237	-0.088423	4.030092
457.122521	5553.147068	15.897242	-0.088396	4.027275
456.960800	5545.093658	15.902247	-0.088361	4.024413
457.054382	5537.182830	15.907251	-0.088373	4.021604
456.934151	5529.161792	15.912256	-0.088345	4.018750
456.993583	5521.202263	15.917261	-0.088351	4.015918
456.964538	5513.206846	15.922266	-0.088341	4.013071
456.962441	5505.146683	15.927271	-0.088335	4.010198
456.968441	5497.198697	15.932275	-0.088331	4.007364
456.706583	5489.147312	15.937280	-0.088277	4.004487
456.760664	5481.234676	15.942285	-0.088282	4.001662
456.835529	5473.206987	15.947290	-0.088291	3.998794
456.897728	5465.235375	15.952295	-0.088298	3.995945
456.846897	5457.206788	15.957299	-0.088283	3.993070
456.851167	5449.183992	15.962304	-0.088279	3.990197
456.755679	5441.204855	15.967309	-0.088256	3.987336
456.868811	5433.202302	15.972314	-0.088272	3.984468
456.686862	5425.254520	15.977319	-0.088233	3.981612
456.892688	5417.220709	15.982323	-0.088266	3.978730
456.736991	5409.258016	15.987328	-0.088232	3.975865
456.482600	5401.213993	15.992333	-0.088179	3.972968
456.668556	5393.183798	15.997338	-0.088209	3.970080
456.754293	5385.208501	16.002343	-0.088220	3.967209
456.567477	5377.214352	16.007347	-0.088180	3.964324
456.642211	5369.269339	16.012352	-0.088189	3.961459
456.675455	5361.231838	16.017357	-0.088190	3.958558
456.766466	5353.262116	16.022362	-0.088202	3.955681
456.553313	5345.217641	16.027367	-0.088157	3.952769
456.535208	5337.195222	16.032371	-0.088148	3.949866
456.353241	5329.193054	16.037376	-0.088109	3.946965
456.244540	5321.141446	16.042381	-0.088084	3.944046
456.606859	5313.262008	16.047386	-0.088146	3.941195
456.497861	5305.190390	16.052391	-0.088121	3.938264
456.353063	5297.227227	16.057395	-0.088089	3.935370
456.379185	5289.233682	16.062400	-0.088088	3.932466
456.352264	5281.155251	16.067405	-0.088078	3.929527
456.384796	5273.231564	16.072410	-0.088079	3.926644
456.263153	5265.224917	16.077415	-0.088052	3.923726
456.288871	5257.256802	16.082419	-0.088051	3.920822
456.181757	5249.275907	16.087424	-0.088026	3.917909
456.003056	5241.283408	16.092429	-0.087988	3.914988
456.006349	5233.270223	16.097434	-0.087983	3.912060
456.023931	5225.201671	16.102439	-0.087981	3.909111
455.921340	5217.260782	16.107443	-0.087957	3.906204
456.034729	5209.214551	16.112448	-0.087973	3.903260
455.825215	5201.268373	16.117453	-0.087929	3.900345
455.821938	5193.335824	16.122458	-0.087923	3.897436
455.946465	5185.236442	16.127463	-0.087941	3.894466
455.860432	5177.310154	16.132467	-0.087920	3.891554
455.681780	5169.259028	16.137472	-0.087882	3.888591
455.721093	5161.269220	16.142477	-0.087884	3.885653
455.794423	5153.275944	16.147482	-0.087893	3.882713
455.722648	5145.272978	16.152487	-0.087874	3.879763
455.687093	5137.341011	16.157491	-0.087862	3.876839
455.678320	5129.272290	16.162496	-0.087856	3.873862
455.723742	5121.168724	16.167501	-0.087859	3.870871
455.567560	5113.179815	16.172506	-0.087825	3.867916
455.397890	5105.212190	16.177511	-0.087788	3.864966
455.471853	5097.277489	16.182515	-0.087797	3.862032
455.632523	5089.241085	16.187520	-0.087821	3.859059
455.476821	5081.309585	16.192525	-0.087787	3.856116
455.673602	5073.285068	16.197530	-0.087819	3.853144
455.530085	5065.300381	16.202535	-0.087787	3.850177
455.491373	5057.282311	16.207539	-0.087775	3.847198
455.325434	5049.326475	16.212544	-0.087739	3.844237
455.423281	5041.319696	16.217549	-0.087752	3.841260
455.498743	5033.316192	16.222554	-0.087761	3.838281
455.324186	5025.322501	16.227559	-0.087723	3.835299
455.458656	5017.316273	16.232563	-0.087743	3.832316
455.405277	5009.312153	16.237568	-0.087728	3.829328
455.230574	5001.300535	16.242573	-0.087690	3.826332
455.296004	4993.333747	16.247578	-0.087697	3.823355
455.430030	4985.289840	16.252583	-0.087717	3.820349
455.351969	4977.361466	16.257587	-0.087698	3.817379
455.080235	4969.332532	16.262592	-0.087642	3.814365
455.453944	4961.297401	16.267597	-0.087706	3.811360
455.482365	4953.305729	16.272602	-0.087706	3.808362
455.347584	4945.280276	16.277607	-0.087676	3.805344
455.319509	4937.366922	16.282611	-0.087666	3.802370
455.279130	4929.346031	16.287616	-0.087653	3.799351
455.193534	4921.384844	16.292621	-0.087632	3.796352
455.324743	4913.367119	16.297626	-0.087652	3.793335
455.229738	4905.324819	16.302631	-0.087629	3.790300
455.287078	4897.349158	16.307635	-0.087634	3.787292
455.039473	4889.327458	16.312640	-0.087583	3.784257
454.827406	4881.376999	16.317645	-0.087538	3.781247
455.006259	4873.370063	16.322650	-0.087567	3.778222
454.803328	4865.369203	16.327655	-0.087524	3.775188
454.887494	4857.408926	16.332659	-0.087534	3.772174
454.992571	4849.342570	16.337664	-0.087549	3.769118
454.926026	4841.372390	16.342669	-0.087531	3.766092
454.859586	4833.402071	16.347674	-0.087514	3.763063
454.840278	4825.394188	16.352679	-0.087505	3.760019
454.563916	4817.459884	16.357683	-0.087448	3.756994
454.592453	4809.434932	16.362688	-0.087449	3.753940
454.721042	4801.477315	16.367693	-0.087467	3.750911
454.841388	4793.404664	16.372698	-0.087485	3.747835
454.652774	4785.385307	16.377703	-0.087444	3.744770
454.755220	4777.456906	16.382707	-0.087458	3.741744
454.694695	4769.443305	16.387712	-0.087442	3.738679
454.672085	4761.465676	16.392717	-0.087433	3.735627
454.814130	4753.466012	16.397722	-0.087454	3.732567
454.782806	4745.387996	16.402727	-0.087443	3.729471
454.693256	4737.463701	16.407731	-0.087421	3.726429
454.437429	4729.500668	16.412736	-0.087369	3.723366
454.181713	4721.506119	16.417741	-0.087316	3.720289
454.622128	4713.484810	16.422746	-0.087393	3.717216
454.388512	4705.493210	16.427751	-0.087344	3.714135
454.287593	4697.463941	16.432755	-0.087320	3.711040
454.358189	4689.428449	16.437760	-0.087328	3.707944
454.368677	4681.395542	16.442765	-0.087325	3.704846
454.433322	4673.458703	16.447770	-0.087332	3.701783
454.377276	4665.408059	16.452775	-0.087316	3.698671
454.262375	4657.451277	16.457779	-0.087290	3.695590
454.239021	4649.476492	16.462784	-0.087280	3.692503
454.372854	4641.427723	16.467789	-0.087300	3.689389
454.372311	4633.507458	16.472794	-0.087295	3.686318
454.103953	4625.472005	16.477799	-0.087240	3.683193
454.014077	4617.506102	16.482803	-0.087218	3.680097
454.048506	4609.534465	16.487808	-0.087219	3.676999
453.889539	4601.517773	16.492813	-0.087185	3.673876
453.951203	4593.564191	16.497818	-0.087191	3.670781
453.781131	4585.501885	16.502823	-0.087154	3.667634
453.897138	4577.486076	16.507827	-0.087171	3.664511
453.773779	4569.565543	16.512832	-0.087143	3.661416
453.898963	4561.517929	16.517837	-0.087161	3.658275
454.007056	4553.547795	16.522842	-0.087176	3.655162
453.870968	4545.551188	16.527847	-0.087145	3.652029
453.579606	4537.576342	16.532851	-0.087086	3.648897
453.715481	4529.572973	16.537856	-0.087106	3.645763
453.639958	4521.607984	16.542861	-0.087087	3.642636
453.610827	4513.621973	16.547866	-0.087076	3.639499
453.515226	4505.630094	16.552871	-0.087054	3.636355
453.705382	4497.597169	16.557875	-0.087084	3.633200
453.529984	4489.619299	16.562880	-0.087046	3.630054
453.336447	4481.644178	16.567885	-0.087005	3.626906
453.560421	4473.590081	16.572890	-0.087041	3.623735
453.352712	4465.622072	16.577895	-0.086998	3.620584
453.423311	4457.630848	16.582899	-0.087006	3.617429
453.754578	4449.566250	16.587904	-0.087062	3.614249
453.765637	4441.579817	16.592909	-0.087059	3.611088
453.524422	4433.648572	16.597914	-0.087009	3.607939
453.201299	4425.646096	16.602919	-0.086944	3.604757
453.533503	4417.658191	16.607923	-0.087001	3.601597
453.546234	4409.628185	16.612928	-0.086998	3.598407
453.238186	4401.675077	16.617933	-0.086935	3.595237
453.586665	4393.677835	16.622938	-0.086995	3.592065
453.403657	4385.643535	16.627943	-0.086956	3.588860
453.251994	4377.665858	16.632947	-0.086923	3.585675
453.206307	4369.694547	16.637952	-0.086909	3.582494
453.158183	4361.685980	16.642957	-0.086895	3.579294
453.316962	4353.710605	16.647962	-0.086919	3.576111
453.196316	4345.658554	16.652967	-0.086892	3.572887
453.000313	4337.729355	16.657971	-0.086850	3.569706
452.654441	4329.774158	16.662976	-0.086781	3.566507
452.807364	4321.705559	16.667981	-0.086804	3.563276
452.871013	4313.738768	16.672986	-0.086811	3.560079
452.871072	4305.751294	16.677991	-0.086806	3.556869
452.856732	4297.716262	16.682995	-0.086798	3.553637
452.819182	4289.695740	16.688000	-0.086786	3.550407
452.575308	4281.730761	16.693005	-0.086735	3.547190
452.646246	4273.702691	16.698010	-0.086743	3.543954
452.194918	4265.802251	16.703015	-0.086654	3.540751
452.518243	4257.760977	16.708019	-0.086709	3.537512
452.648195	4249.713234	16.713024	-0.086728	3.534262
452.590161	4241.766727	16.718029	-0.086712	3.531043
452.729088	4233.774545	16.723034	-0.086733	3.527809
452.719493	4225.731108	16.728039	-0.086726	3.524547
452.609621	4217.834372	16.733043	-0.086701	3.521338
452.627119	4209.819767	16.738048	-0.086699	3.518083
452.617923	4201.797010	16.743053	-0.086692	3.514820
452.765250	4193.830039	16.748058	-0.086714	3.511582
452.536209	4185.833985	16.753063	-0.086667	3.508317
452.617440	4177.798912	16.758067	-0.086676	3.505043
452.518917	4169.863455	16.763072	-0.086653	3.501801
452.331848	4161.851498	16.768077	-0.086613	3.498521
452.595737	4153.845782	16.773082	-0.086657	3.495256
452.381731	4145.850288	16.778087	-0.086612	3.491976
452.417864	4137.840986	16.783091	-0.086614	3.488696
452.366691	4129.865191	16.788096	-0.086599	3.485423
452.567185	4121.857791	16.793101	-0.086631	3.482143
452.595632	4113.858725	16.798106	-0.086631	3.478858
452.089846	4105.963235	16.803111	-0.086532	3.475594
452.187059	4097.897975	16.808115	-0.086545	3.472277
452.362621	4089.918122	16.813120	-0.086573	3.468995
452.126165	4081.929900	16.818125	-0.086524	3.465692
452.189642	4073.937176	16.823130	-0.086530	3.462395
452.089810	4065.896597	16.828135	-0.086507	3.459069
451.895738	4057.969560	16.833139	-0.086465	3.455784
452.217000	4049.919122	16.838144	-0.086520	3.452462
452.002423	4041.922420	16.843149	-0.086475	3.449140
451.970838	4033.993734	16.848154	-0.086464	3.445851
451.893678	4025.957643	16.853159	-0.086445	3.442511
451.860020	4018.007643	16.858163	-0.086433	3.439206
451.663560	4010.089262	16.863168	-0.086392	3.435905
452.001601	4001.975441	16.868173	-0.086449	3.432538
451.636685	3994.057313	16.873178	-0.086376	3.429225
451.885972	3986.016613	16.878183	-0.086418	3.425879
451.534735	3978.082321	16.883187	-0.086347	3.422553
451.449904	3970.067201	16.888192	-0.086326	3.419199
451.660694	3962.052363	16.893197	-0.086360	3.415853
451.303577	3954.121302	16.898202	-0.086289	3.412518
451.467978	3946.021779	16.903207	-0.086314	3.409128
451.512964	3938.057790	16.908211	-0.086317	3.405787
451.321704	3930.135695	16.913216	-0.086277	3.402452
451.293127	3922.096363	16.918221	-0.086266	3.399070
451.340691	3914.159396	16.923226	-0.086270	3.395731
451.817302	3906.035936	16.928231	-0.086354	3.392325
451.392549	3898.072817	16.933235	-0.086269	3.388951
451.274962	3890.104858	16.938240	-0.086242	3.385583
451.399522	3882.070962	16.943245	-0.086260	3.382192
451.465546	3874.114271	16.948250	-0.086268	3.378829
451.284624	3866.142535	16.953255	-0.086229	3.375446
451.311105	3858.151405	16.958259	-0.086229	3.372060
451.419952	3850.115573	16.963264	-0.086244	3.368654
451.384963	3842.126741	16.968269	-0.086232	3.365259
451.378113	3834.197120	16.973274	-0.086226	3.361888
451.193786	3826.210272	16.978279	-0.086186	3.358482
451.426534	3818.194476	16.983283	-0.086225	3.355075
451.245425	3810.246336	16.988288	-0.086186	3.351679
451.420342	3802.196186	16.993293	-0.086213	3.348249
451.416834	3794.210044	16.998298	-0.086207	3.344836
451.399662	3786.235452	17.003303	-0.086199	3.341424
451.030502	3778.302271	17.008307	-0.086125	3.338012
450.945430	3770.326043	17.013312	-0.086104	3.334590
450.674452	3762.320719	17.018317	-0.086049	3.331145
451.125344	3754.240061	17.023322	-0.086127	3.327691
450.592701	3746.323369	17.028327	-0.086023	3.324266
450.033230	3738.451558	17.033331	-0.085914	3.320856
450.333180	3730.382345	17.038336	-0.085965	3.317391
450.887604	3722.258107	17.043341	-0.086063	3.313908
450.794862	3714.317341	17.048346	-0.086040	3.310476
450.844632	3706.289013	17.053351	-0.086045	3.307008
450.734778	3698.312331	17.058355	-0.086019	3.303552
450.594017	3690.378543	17.063360	-0.085988	3.300110
450.228737	3682.414433	17.068365	-0.085915	3.296642
450.688504	3674.358103	17.073370	-0.085995	3.293163
450.707024	3666.335848	17.078375	-0.085993	3.289678
450.620919	3658.385430	17.083379	-0.085972	3.286217
450.563784	3650.406390	17.088384	-0.085956	3.282740
450.359655	3642.433545	17.093389	-0.085913	3.279256
450.981952	3634.423483	17.098394	-0.086024	3.275786
450.779161	3626.442470	17.103399	-0.085981	3.272292
450.546886	3618.472088	17.108403	-0.085933	3.268797
450.391350	3610.478313	17.113408	-0.085899	3.265291
450.220029	3602.518159	17.118413	-0.085862	3.261796
450.149552	3594.548740	17.123418	-0.085844	3.258297
450.484691	3586.485579	17.128423	-0.085901	3.254769
450.258537	3578.547842	17.133427	-0.085854	3.251270
450.160758	3570.534476	17.138432	-0.085830	3.247739
450.424949	3562.471956	17.143437	-0.085874	3.244197
450.683816	3554.568582	17.148442	-0.085917	3.240722
450.240484	3546.629248	17.153447	-0.085830	3.237198
450.168451	3538.610205	17.158451	-0.085811	3.233650
450.260801	3530.616941	17.163456	-0.085823	3.230116
450.159304	3522.588008	17.168461	-0.085799	3.226555
450.305351	3514.582552	17.173466	-0.085821	3.223011
450.189935	3506.578306	17.178471	-0.085795	3.219452
450.188531	3498.634611	17.183475	-0.085789	3.215921
450.231428	3490.623902	17.188480	-0.085792	3.212358
450.231625	3482.612129	17.193485	-0.085787	3.208789
450.427632	3474.629030	17.198490	-0.085819	3.205237
450.299189	3466.664108	17.203495	-0.085790	3.201676
450.097863	3458.713716	17.208499	-0.085747	3.198113
450.200582	3450.722116	17.213504	-0.085761	3.194542
449.859425	3442.782192	17.218509	-0.085692	3.190970
449.404196	3434.813645	17.223514	-0.085603	3.187377
449.642711	3426.721848	17.228519	-0.085642	3.183754
450.087418	3418.671905	17.233523	-0.085719	3.180155
449.980794	3410.775262	17.238528	-0.085694	3.176597
450.017683	3402.729489	17.243533	-0.085696	3.172974
449.921677	3394.778494	17.248538	-0.085673	3.169383
449.933929	3386.795572	17.253543	-0.085670	3.165779
449.859892	3378.855037	17.258547	-0.085652	3.162187
449.880582	3370.871524	17.263552	-0.085650	3.158574
450.141433	3362.805346	17.268557	-0.085694	3.154931
449.951389	3354.880136	17.273562	-0.085653	3.151328
449.631835	3346.890990	17.278567	-0.085589	3.147686
449.965160	3338.837072	17.283571	-0.085646	3.144039
449.790799	3330.922161	17.288576	-0.085608	3.140428
449.445807	3322.940267	17.293581	-0.085539	3.136775
449.664902	3314.932929	17.298586	-0.085574	3.133132
449.374315	3306.945984	17.303591	-0.085515	3.129470
449.089909	3299.004761	17.308595	-0.085457	3.125826
448.873263	3291.015055	17.313600	-0.085412	3.122158
449.357879	3282.955008	17.318605	-0.085497	3.118485
449.377169	3275.012148	17.323610	-0.085495	3.114841
449.362628	3267.019506	17.328615	-0.085487	3.111168
449.401784	3258.999697	17.333619	-0.085490	3.107480
449.207360	3251.068542	17.338624	-0.085448	3.103819
448.751506	3243.128652	17.343629	-0.085358	3.100136
449.051204	3235.116391	17.348634	-0.085409	3.096451
449.123826	3227.085964	17.353639	-0.085417	3.092743
449.077301	3219.084682	17.358643	-0.085404	3.089038
449.132144	3211.119049	17.363648	-0.085409	3.085350
448.919335	3203.170761	17.368653	-0.085364	3.081653
448.849856	3195.200652	17.373658	-0.085346	3.077948
448.550253	3187.214801	17.378663	-0.085285	3.074220
448.804389	3179.151050	17.383667	-0.085327	3.070478
448.843249	3171.155984	17.388672	-0.085329	3.066754
448.927764	3163.125790	17.393677	-0.085340	3.063010
448.681329	3155.219038	17.398682	-0.085289	3.059303
448.754824	3147.208837	17.403687	-0.085297	3.055560
448.825657	3139.225346	17.408691	-0.085306	3.051823
448.740463	3131.239207	17.413696	-0.085285	3.048074
448.536262	3123.256728	17.418701	-0.085241	3.044316
448.733143	3115.308733	17.423706	-0.085273	3.040589
448.452634	3107.346707	17.428711	-0.085216	3.036827
448.403602	3099.373102	17.433715	-0.085201	3.033066
448.364784	3091.385200	17.438720	-0.085189	3.029295
448.175176	3083.395381	17.443725	-0.085149	3.025511
448.432755	3075.365935	17.448730	-0.085192	3.021725
448.393482	3067.403422	17.453735	-0.085179	3.017951
448.358578	3059.420166	17.458739	-0.085168	3.014163
448.129763	3051.479321	17.463744	-0.085120	3.010381
447.762827	3043.509418	17.468749	-0.085046	3.006573
448.003393	3035.490495	17.473754	-0.085086	3.002768
448.284717	3027.443237	17.478759	-0.085133	2.998946
448.340861	3019.494824	17.483763	-0.085139	2.995155
448.353267	3011.542837	17.488768	-0.085136	2.991356
448.353633	3003.497909	17.493773	-0.085131	2.987506
447.926126	2995.603003	17.498778	-0.085046	2.983702
448.025387	2987.566203	17.503783	-0.085059	2.979852
448.214868	2979.576795	17.508787	-0.085090	2.976024
448.586839	2971.529244	17.513792	-0.085154	2.972172
448.462902	2963.564273	17.518797	-0.085126	2.968330
448.293308	2955.649560	17.523802	-0.085089	2.964505
447.870399	2947.728668	17.528807	-0.085005	2.960658
447.995352	2939.716863	17.533811	-0.085023	2.956791
448.224808	2931.698305	17.538816	-0.085061	2.952922
448.234031	2923.667794	17.543821	-0.085057	2.949029
448.311958	2915.708516	17.548826	-0.085067	2.945170
448.286292	2907.735651	17.553831	-0.085057	2.941294
448.391902	2899.756366	17.558835	-0.085071	2.937416
448.130444	2891.830402	17.563840	-0.085018	2.933540
448.198107	2883.779768	17.568845	-0.085025	2.929615
448.393621	2875.817756	17.573850	-0.085056	2.925736
448.274087	2867.837188	17.578855	-0.085029	2.921825
448.256184	2859.907084	17.583859	-0.085021	2.917939
448.563235	2851.874628	17.588864	-0.085073	2.914015
448.081612	2843.902178	17.593869	-0.084978	2.910073
448.124972	2835.893888	17.598874	-0.084981	2.906136
447.946370	2827.933161	17.603879	-0.084943	2.902205
448.183020	2819.940189	17.608883	-0.084981	2.898276
447.966273	2811.979502	17.613888	-0.084936	2.894332
447.846577	2804.015140	17.618893	-0.084909	2.890386
448.081062	2796.011951	17.623898	-0.084947	2.886436
447.932451	2788.030510	17.628903	-0.084914	2.882469
447.965320	2780.070513	17.633907	-0.084915	2.878518
448.007516	2772.080226	17.638912	-0.084918	2.874547
447.773008	2764.134057	17.643917	-0.084869	2.870577
447.840663	2756.130448	17.648922	-0.084877	2.866589
447.845541	2748.128803	17.653927	-0.084873	2.862594
447.711125	2740.193427	17.658931	-0.084843	2.858618
447.819279	2732.206096	17.663936	-0.084858	2.854624
447.651788	2724.229522	17.668941	-0.084821	2.850614
447.493714	2716.271885	17.673946	-0.084787	2.846609
447.556507	2708.280464	17.678951	-0.084793	2.842594
447.414658	2700.313173	17.683955	-0.084762	2.838574
447.619193	2692.318800	17.688960	-0.084795	2.834554
447.520838	2684.335203	17.693965	-0.084771	2.830516
447.491156	2676.342204	17.698970	-0.084761	2.826472
447.548197	2668.346978	17.703975	-0.084766	2.822426
447.293435	2660.424367	17.708979	-0.084714	2.818392
447.194767	2652.455279	17.713984	-0.084690	2.814339
446.894318	2644.501452	17.718989	-0.084629	2.810275
447.206859	2636.457616	17.723994	-0.084682	2.806196
447.126301	2628.494184	17.728999	-0.084662	2.802128
447.105883	2620.518875	17.734003	-0.084653	2.798053
447.213923	2612.534135	17.739008	-0.084668	2.793974
446.878611	2604.585939	17.744013	-0.084601	2.789881
446.834665	2596.611280	17.749018	-0.084587	2.785786
447.045731	2588.592409	17.754023	-0.084622	2.781678
447.072079	2580.623900	17.759027	-0.084621	2.777579
446.706225	2572.719262	17.764032	-0.084548	2.773482
446.720673	2564.677809	17.769037	-0.084546	2.769332
446.762789	2556.725399	17.774042	-0.084549	2.765224
447.006820	2548.719371	17.779047	-0.084589	2.761094
447.089785	2540.727982	17.784051	-0.084599	2.756955
447.233763	2532.729905	17.789056	-0.084621	2.752811
447.059666	2524.739531	17.794061	-0.084583	2.748644
446.947719	2516.791716	17.799066	-0.084557	2.744498
447.047869	2508.800832	17.804071	-0.084571	2.740335
447.106800	2500.849634	17.809075	-0.084577	2.736185
446.794699	2492.916606	17.814080	-0.084514	2.732015
446.508451	2484.932651	17.819085	-0.084455	2.727813
446.342531	2477.016286	17.824090	-0.084419	2.723647
446.025791	2469.076214	17.829095	-0.084355	2.719453
446.219645	2461.064694	17.834099	-0.084386	2.715248
446.337969	2453.060958	17.839104	-0.084403	2.711035
446.350912	2445.045082	17.844109	-0.084400	2.706803
446.432770	2437.070568	17.849114	-0.084410	2.702590
446.399452	2429.098225	17.854119	-0.084399	2.698364
446.206048	2421.160131	17.859123	-0.084358	2.694140
446.392753	2413.170280	17.864128	-0.084388	2.689906
446.239673	2405.193165	17.869133	-0.084354	2.685650
446.191801	2397.262201	17.874138	-0.084340	2.681418
446.278181	2389.253218	17.879143	-0.084351	2.677148
446.354060	2381.265244	17.884147	-0.084360	2.672880
446.278837	2373.304381	17.889152	-0.084341	2.668611
446.096652	2365.334515	17.894157	-0.084302	2.664323
446.249760	2357.377662	17.899162	-0.084325	2.660057
445.961321	2349.435576	17.904167	-0.084267	2.655763
446.294220	2341.383746	17.909171	-0.084323	2.651444
446.300513	2333.411666	17.914176	-0.084320	2.647139
445.943321	2325.502321	17.919181	-0.084248	2.642838
446.048017	2317.529661	17.924186	-0.084262	2.638525
446.304735	2309.536774	17.929191	-0.084305	2.634205
445.983040	2301.605342	17.934195	-0.084240	2.629872
445.961710	2293.621207	17.939200	-0.084231	2.625523
445.812735	2285.668764	17.944205	-0.084198	2.621176
445.823992	2277.715627	17.949210	-0.084195	2.616833
445.598085	2269.752264	17.954215	-0.084148	2.612460
445.522614	2261.772464	17.959219	-0.084129	2.608081
445.660152	2253.773190	17.964224	-0.084149	2.603699
445.640487	2245.807290	17.969229	-0.084141	2.599316
445.671646	2237.856660	17.974234	-0.084141	2.594939
445.089132	2229.847086	17.979239	-0.084028	2.590478
445.546218	2221.763307	17.984243	-0.084108	2.586042
445.231620	2213.884833	17.989248	-0.084044	2.581657
445.302148	2205.913902	17.994253	-0.084052	2.577241
445.451500	2197.922191	17.999258	-0.084075	2.572811
445.213035	2189.968918	18.004263	-0.084025	2.568368
445.497290	2181.952850	18.009267	-0.084073	2.563919
445.681870	2174.001168	18.014272	-0.084102	2.559491
445.519252	2166.069418	18.019277	-0.084067	2.555042
445.344611	2158.159790	18.024282	-0.084029	2.550596
445.469282	2150.153603	18.029287	-0.084047	2.546110
445.469483	2142.185682	18.034291	-0.084042	2.541629
445.160461	2134.286362	18.039296	-0.083980	2.537156
444.959996	2126.314557	18.044301	-0.083937	2.532642
444.959043	2118.331726	18.049306	-0.083932	2.528128
444.875375	2110.373513	18.054311	-0.083911	2.523614
444.839067	2102.402319	18.059315	-0.083899	2.519088
444.641312	2094.479469	18.064320	-0.083858	2.514570
444.554010	2086.496728	18.069325	-0.083836	2.510017
445.064420	2078.417531	18.074330	-0.083926	2.505445
444.961209	2070.474045	18.079335	-0.083902	2.500897
445.008413	2062.520092	18.084339	-0.083905	2.496346
445.044653	2054.554847	18.089344	-0.083907	2.491780
444.813658	2046.622959	18.094349	-0.083859	2.487204
444.685763	2038.695883	18.099354	-0.083830	2.482630
444.700279	2030.710009	18.104359	-0.083828	2.478024
444.502771	2022.791520	18.109363	-0.083786	2.473433
444.815317	2014.776064	18.114368	-0.083839	2.468816
444.651503	2006.812073	18.119373	-0.083803	2.464183
444.483551	1998.907167	18.124378	-0.083767	2.459576
444.546263	1990.923885	18.129383	-0.083774	2.454933
444.493200	1982.963962	18.134387	-0.083759	2.450285
444.628686	1974.967076	18.139392	-0.083779	2.445621
444.586805	1967.015975	18.144397	-0.083766	2.440962
444.682069	1959.073621	18.149402	-0.083779	2.436309
444.279943	1951.142777	18.154407	-0.083699	2.431616
444.053832	1943.162831	18.159411	-0.083651	2.426898
444.296740	1935.163159	18.164416	-0.083691	2.422196
444.418526	1927.173085	18.169421	-0.083709	2.417481
444.324417	1919.248873	18.174426	-0.083686	2.412779
444.149858	1911.300719	18.179431	-0.083649	2.408047
444.242086	1903.312440	18.184435	-0.083661	2.403304
444.398508	1895.366859	18.189440	-0.083685	2.398581
444.756983	1887.343133	18.194445	-0.083747	2.393818
444.656988	1879.438905	18.199450	-0.083723	2.389081
444.226682	1871.535250	18.204455	-0.083638	2.384308
444.233748	1863.582056	18.209459	-0.083634	2.379531
443.776030	1855.710853	18.214464	-0.083544	2.374756
443.800346	1847.694247	18.219469	-0.083543	2.369923
443.761585	1839.735265	18.224474	-0.083531	2.365110
443.789941	1831.762040	18.229479	-0.083531	2.360284
443.824559	1823.796279	18.234483	-0.083532	2.355452
444.149209	1815.795646	18.239488	-0.083588	2.350614
444.055960	1807.835331	18.244493	-0.083565	2.345756
443.750320	1799.957510	18.249498	-0.083503	2.340920
444.027180	1791.943328	18.254503	-0.083550	2.336040
443.998691	1783.983581	18.259507	-0.083539	2.331157
443.889474	1776.049529	18.264512	-0.083514	2.326272
443.804022	1768.106915	18.269517	-0.083493	2.321375
443.872551	1760.168078	18.274522	-0.083500	2.316482
443.614934	1752.252415	18.279527	-0.083447	2.311565
443.584731	1744.288510	18.284531	-0.083437	2.306628
443.432498	1736.368765	18.289536	-0.083403	2.301696
443.603464	1728.354612	18.294541	-0.083430	2.296724
443.564751	1720.426896	18.299546	-0.083418	2.291776
443.486155	1712.471685	18.304551	-0.083398	2.286797
443.153185	1704.572802	18.309555	-0.083331	2.281820
442.948169	1696.673871	18.314560	-0.083288	2.276843
442.230027	1688.791229	18.319565	-0.083149	2.271821
442.481365	1680.725904	18.324570	-0.083191	2.266757
442.382301	1672.750153	18.329575	-0.083167	2.261708
442.519873	1664.778470	18.334579	-0.083188	2.256671
442.375130	1656.859723	18.339584	-0.083155	2.251631
442.660180	1648.796005	18.344589	-0.083203	2.246526
442.707937	1640.886082	18.349594	-0.083207	2.241487
442.469504	1632.991091	18.354599	-0.083158	2.236419
442.528043	1625.009647	18.359603	-0.083164	2.231312
442.848559	1617.022456	18.364608	-0.083218	2.226213
442.798185	1609.080345	18.369613	-0.083204	2.221097
442.530121	1601.215526	18.374618	-0.083149	2.216000
442.760625	1593.212004	18.379623	-0.083187	2.210847
442.610477	1585.280536	18.384627	-0.083153	2.205694
442.186324	1577.437691	18.389632	-0.083070	2.200561
442.572503	1569.403005	18.394637	-0.083136	2.195365
442.349060	1561.506550	18.399642	-0.083090	2.190192
442.278959	1553.549420	18.404647	-0.083071	2.184980
441.846767	1545.675925	18.409651	-0.082986	2.179777
442.249925	1537.662610	18.414656	-0.083056	2.174548
441.977801	1529.745233	18.419661	-0.083000	2.169306
442.280926	1521.749381	18.424666	-0.083051	2.164054
442.254568	1513.824563	18.429671	-0.083041	2.158804
442.148572	1505.905765	18.434675	-0.083017	2.153539
441.840610	1498.047559	18.439680	-0.082954	2.148281
441.681203	1490.089507	18.444685	-0.082920	2.142958
441.730002	1482.136292	18.449690	-0.082924	2.137646
441.177053	1474.295069	18.454695	-0.082816	2.132336
441.372967	1466.256455	18.459699	-0.082847	2.126954
441.532336	1458.299538	18.464704	-0.082871	2.121609
441.871280	1450.302162	18.469709	-0.082929	2.116241
441.284372	1442.469951	18.474714	-0.082815	2.110881
440.755664	1434.574285	18.479719	-0.082712	2.105469
441.253005	1426.538838	18.484723	-0.082799	2.100050
441.165866	1418.621521	18.489728	-0.082778	2.094639
440.990943	1410.695100	18.494733	-0.082740	2.089199
441.187171	1402.723956	18.499738	-0.082772	2.083751
441.188678	1394.801912	18.504743	-0.082767	2.078304
441.283151	1386.861023	18.509747	-0.082779	2.072838
441.458928	1378.909237	18.514752	-0.082807	2.067359
441.531194	1370.950811	18.519757	-0.082815	2.061850
441.427267	1363.077116	18.524762	-0.082791	2.056367
441.460942	1355.126183	18.529767	-0.082792	2.050830
441.229260	1347.240848	18.534771	-0.082744	2.045297
441.300468	1339.322594	18.539776	-0.082752	2.039756
440.933268	1331.458053	18.544781	-0.082679	2.034193
441.313725	1323.448645	18.549786	-0.082744	2.028590
441.365196	1315.495795	18.554791	-0.082749	2.022977
441.118425	1307.617701	18.559795	-0.082698	2.017371
440.974322	1299.725606	18.564800	-0.082666	2.011749
441.012074	1291.762573	18.569805	-0.082668	2.006081
440.860534	1283.876970	18.574810	-0.082635	2.000431
441.453283	1275.850718	18.579815	-0.082740	1.994744
441.206779	1267.993425	18.584819	-0.082689	1.989073
441.235845	1260.079507	18.589824	-0.082689	1.983374
441.091914	1252.175738	18.594829	-0.082658	1.977647
441.480887	1244.188324	18.599834	-0.082725	1.971901
441.484783	1236.287543	18.604839	-0.082720	1.966159
440.724074	1228.515528	18.609843	-0.082574	1.960411
440.916578	1220.568080	18.614848	-0.082605	1.954622
440.861558	1212.628497	18.619853	-0.082589	1.948794
441.188847	1204.629887	18.624858	-0.082645	1.942947
441.005561	1196.749990	18.629863	-0.082606	1.937114
440.738794	1188.858946	18.634867	-0.082551	1.931246
440.378116	1181.017404	18.639872	-0.082479	1.925386
440.605407	1173.033548	18.644877	-0.082516	1.919468
440.306995	1165.193830	18.649882	-0.082456	1.913580
440.550604	1157.211111	18.654887	-0.082496	1.907628
440.802605	1149.240794	18.659891	-0.082538	1.901668
440.629032	1141.385384	18.664896	-0.082500	1.895727
440.693493	1133.433533	18.669901	-0.082507	1.889722
440.795752	1125.543428	18.674906	-0.082521	1.883749
440.923025	1117.632416	18.679911	-0.082540	1.877744
440.972469	1109.712119	18.684915	-0.082544	1.871703
440.769003	1101.849309	18.689920	-0.082501	1.865658
440.711138	1093.943968	18.694925	-0.082485	1.859577
440.146821	1086.154752	18.699930	-0.082375	1.853506
440.548593	1078.155826	18.704935	-0.082445	1.847367
440.357517	1070.278512	18.709939	-0.082404	1.841231
440.508975	1062.366415	18.714944	-0.082427	1.835089
440.009893	1054.546650	18.719949	-0.082330	1.828920
440.388138	1046.570488	18.724954	-0.082395	1.822714
440.270436	1038.695406	18.729959	-0.082368	1.816506
439.874046	1030.847406	18.734963	-0.082289	1.810263
440.083587	1022.919895	18.739968	-0.082323	1.804011
440.035742	1015.041141	18.744973	-0.082309	1.797744
439.743355	1007.179397	18.749978	-0.082250	1.791438
439.789374	999.242100	18.754983	-0.082253	1.785091
440.073261	991.300935	18.759987	-0.082301	1.778748
440.007876	983.441089	18.764992	-0.082284	1.772405
439.960183	975.533822	18.769997	-0.082270	1.766002
440.017995	967.655622	18.775002	-0.082275	1.759613
439.860522	959.818209	18.780007	-0.082241	1.753207
439.187330	952.027489	18.785011	-0.082111	1.746749
439.769925	944.027954	18.790016	-0.082214	1.740257
440.027570	936.114372	18.795021	-0.082257	1.733770
439.867197	928.267216	18.800026	-0.082222	1.727259
439.589589	920.442124	18.805031	-0.082165	1.720727
439.632719	912.551711	18.810035	-0.082168	1.714157
439.043736	904.781174	18.815040	-0.082054	1.707579
438.917759	896.882594	18.820045	-0.082025	1.700929
439.462997	888.919847	18.825050	-0.082122	1.694288
439.268197	881.066117	18.830055	-0.082080	1.687615
439.070132	873.224675	18.835059	-0.082039	1.680925
439.245897	865.343719	18.840064	-0.082066	1.674225
439.516777	857.398927	18.845069	-0.082112	1.667456
439.596954	849.545208	18.850074	-0.082121	1.660712
439.613784	841.698887	18.855079	-0.082120	1.653938
439.457135	833.865960	18.860083	-0.082085	1.647124
439.615981	825.990989	18.865088	-0.082110	1.640289
439.277697	818.196055	18.870093	-0.082042	1.633426
439.432467	810.280707	18.875098	-0.082066	1.626498
439.270432	802.459359	18.880103	-0.082031	1.619578
439.035476	794.641386	18.885107	-0.081982	1.612620
439.244628	786.742706	18.890112	-0.082016	1.605625
439.025774	778.934984	18.895117	-0.081970	1.598618
439.080175	771.080317	18.900122	-0.081975	1.591578
439.160894	763.214203	18.905127	-0.081985	1.584500
438.984354	755.420307	18.910131	-0.081947	1.577418
439.012417	747.568340	18.915136	-0.081947	1.570282
438.421176	739.821672	18.920141	-0.081832	1.563117
438.415173	731.994382	18.925146	-0.081826	1.555932
438.542093	724.116746	18.930151	-0.081845	1.548688
438.082014	716.343676	18.935155	-0.081754	1.541418
438.172237	708.494310	18.940160	-0.081766	1.534125
437.792740	700.699928	18.945165	-0.081690	1.526778
438.049939	692.831526	18.950170	-0.081733	1.519423
437.782867	685.049767	18.955175	-0.081678	1.512034
437.905680	677.170708	18.960179	-0.081696	1.504576
437.506962	669.441238	18.965184	-0.081617	1.497142
437.520050	661.586120	18.970189	-0.081614	1.489615
437.643455	653.747329	18.975194	-0.081632	1.482083
437.824419	645.908296	18.980199	-0.081661	1.474522
437.581693	638.109492	18.985203	-0.081611	1.466893
437.528215	630.313319	18.990208	-0.081596	1.459257
437.317623	622.540250	18.995213	-0.081552	1.451578
437.594887	614.680002	19.000218	-0.081598	1.443852
437.660431	606.890204	19.005223	-0.081606	1.436120
437.767915	599.079310	19.010227	-0.081621	1.428331
437.568892	591.339165	19.015232	-0.081579	1.420520
437.831840	583.504668	19.020237	-0.081623	1.412648
437.994558	575.699051	19.025242	-0.081648	1.404744
437.982674	567.957786	19.030247	-0.081641	1.396832
437.536715	560.259859	19.035251	-0.081553	1.388845
437.297014	552.532303	19.040256	-0.081503	1.380816
437.615685	544.690853	19.045261	-0.081557	1.372719
437.705017	536.908639	19.050266	-0.081569	1.364596
437.435437	529.222360	19.055271	-0.081514	1.356462
437.537869	521.439958	19.060275	-0.081528	1.348243
437.785856	513.650995	19.065280	-0.081569	1.339992
437.658867	505.936660	19.070285	-0.081541	1.331703
437.656842	498.200357	19.075290	-0.081535	1.323361
437.821337	490.448300	19.080295	-0.081561	1.314980
437.504645	482.689216	19.085299	-0.081497	1.306448
437.517127	474.970029	19.090304	-0.081494	1.297966
437.410307	467.256669	19.095309	-0.081470	1.289411
437.343315	459.556477	19.100314	-0.081452	1.280822
437.370478	451.849234	19.105319	-0.081452	1.272184
437.354053	444.132927	19.110323	-0.081444	1.263469
437.442636	436.437632	19.115328	-0.081456	1.254738
437.074350	428.793671	19.120333	-0.081382	1.245916
437.070636	421.120765	19.125338	-0.081377	1.237068
437.262469	413.394761	19.130343	-0.081408	1.228134
436.934902	405.763730	19.135347	-0.081342	1.219142
436.793180	398.119694	19.140352	-0.081311	1.210105
436.919147	390.409584	19.145357	-0.081329	1.200975
436.815737	382.784745	19.150362	-0.081305	1.191831
436.486708	375.182328	19.155367	-0.081239	1.182597
436.440727	367.534503	19.160371	-0.081225	1.173294
436.372371	359.917232	19.165376	-0.081208	1.163949
436.377840	352.270363	19.170381	-0.081204	1.154507
436.267614	344.632063	19.175386	-0.081178	1.144974
436.152908	337.031144	19.180391	-0.081152	1.135406
436.222604	329.387474	19.185395	-0.081160	1.125744
436.244199	321.796780	19.190400	-0.081159	1.116054
435.977531	314.244024	19.195405	-0.081105	1.106265
436.119562	306.637430	19.200410	-0.081127	1.096410
435.902243	299.094818	19.205415	-0.081081	1.086468
435.683510	291.574218	19.210419	-0.081036	1.076463
435.381021	284.068745	19.215424	-0.080975	1.066366
435.209421	276.532672	19.220429	-0.080938	1.056160
434.928578	269.040392	19.225434	-0.080881	1.045889
434.615878	261.570528	19.230439	-0.080818	1.035540
434.414065	254.066208	19.235443	-0.080775	1.025064
434.502392	246.541185	19.240448	-0.080787	1.014522
433.804668	239.157560	19.245453	-0.080652	1.003876
433.379885	231.741990	19.250458	-0.080569	0.993138
432.595831	224.360078	19.255463	-0.080418	0.982240
431.485262	217.054379	19.260467	-0.080206	0.971248
430.184799	209.796255	19.265472	-0.079960	0.960151
428.886752	202.528703	19.270477	-0.079713	0.948910
427.794049	195.231089	19.275482	-0.079505	0.937542
426.836777	187.915083	19.280487	-0.079322	0.926042
424.711848	180.822651	19.285491	-0.078922	0.914427
421.422416	173.913984	19.290496	-0.078305	0.902628
417.891012	167.013889	19.295501	-0.077643	0.890616
415.336875	159.951604	19.300506	-0.077163	0.878454
411.739490	153.062747	19.305511	-0.076489	0.866102
407.370834	146.284233	19.310515	-0.075671	0.853526
401.015704	139.845420	19.315520	-0.074484	0.840741
389.435649	134.232510	19.320525	-0.072324	0.827586
371.306461	129.628978	19.325530	-0.068945	0.813947
350.866927	125.218082	19.330535	-0.065137	0.799676
336.625938	119.558801	19.335539	-0.062481	0.784858
333.032155	112.030367	19.340544	-0.061807	0.769782
331.084925	104.340366	19.345549	-0.061440	0.754652
325.809360	97.337428	19.350554	-0.060453	0.739395
316.047061	91.182599	19.355559	-0.058632	0.723910
305.615686	85.333473	19.360563	-0.056685	0.708456