Number of Data Points = 30
        
File	hc(nm)	Pmax(N)	S(N/nm)	A(nm^2)	hmax(nm)	heff(nm)	Er(GPa)	H(GPa)	A	hf(nm)	m	X(mm)	Y(mm)	Drift(nm/s)
HIP_00000 LC.hys	250.278009	7999.354873	444.043447	2605733.577653	265.930557	263.789110	243.722312	3.069905	3.568215	225.625989	2.118431	-136.776993	-56.991998	0.363860
HIP_00001 LC.hys	572.765384	7999.350842	360.390893	13390652.622984	590.811593	589.412623	87.258504	0.597383	0.030290	523.300375	2.978523	-136.766991	-56.991998	0.016124
HIP_00002 LC.hys	332.198293	7999.213364	381.064833	4608714.479950	349.165009	347.942097	157.269244	1.735671	22.325119	313.156641	1.657102	-136.756996	-56.991998	0.004711
HIP_00003 LC.hys	319.597773	7999.528845	298.997734	4265762.353725	339.774392	339.663633	128.263887	1.875287	105.972816	306.596835	1.235935	-136.746994	-56.991998	-0.131199
HIP_00004 LC.hys	284.314192	7999.225993	333.899172	3372137.930101	302.425196	302.281950	161.100729	2.372153	83.471358	270.640096	1.320776	-136.736992	-56.991998	-0.099309
HIP_00005 LC.hys	536.157712	7999.385958	318.314201	11792860.660128	554.727287	555.005565	82.126111	0.678324	121.133767	524.265461	1.223220	-136.726998	-56.991998	-0.113578
HIP_00006 LC.hys	461.518694	7999.362922	317.398308	8818563.882479	481.046276	480.420881	94.697934	0.907105	63.709537	446.000813	1.365718	-136.776993	-56.981996	-0.046434
HIP_00007 LC.hys	346.201378	7999.435608	317.282850	5004276.864520	365.519039	365.110615	125.663966	1.598520	86.723210	332.403137	1.297282	-136.766991	-56.981996	-0.017924
HIP_00008 LC.hys	349.822029	7999.123409	260.932312	5109005.297244	373.056017	372.813978	102.280894	1.565691	9.138746	320.366820	1.710832	-136.756996	-56.981996	-0.005208
HIP_00009 LC.hys	292.372875	7999.285609	305.244106	3567470.260921	312.200101	312.027518	143.186454	2.242285	106.881780	279.538792	1.239735	-136.746994	-56.981996	-0.035630
HIP_00010 LC.hys	531.745568	7999.459089	447.467081	11606391.591387	546.468959	545.153469	116.371682	0.689229	0.164624	495.700571	2.766255	-136.736992	-56.981996	-0.015613
HIP_00011 LC.hys	344.837437	7999.118918	310.249613	4965084.738853	364.533347	364.174574	123.362381	1.611074	62.308608	329.012601	1.363774	-136.726998	-56.981996	0.000139
HIP_00012 LC.hys	232.768325	7999.570576	348.886753	2249143.981721	250.300160	249.964959	206.115513	3.556718	88.771674	219.699719	1.319964	-136.776993	-56.971998	0.047521
HIP_00013 LC.hys	557.114653	7999.119980	329.789392	12696535.436042	575.792471	575.306081	82.002841	0.630024	29.775623	537.858771	1.543886	-136.766991	-56.971998	0.041475
HIP_00014 LC.hys	446.646494	7999.339123	326.212255	8272390.023227	465.420789	465.037907	100.489249	0.966993	38.304267	428.606865	1.485654	-136.756493	-56.971998	0.033951
HIP_00015 LC.hys	387.577671	7999.367909	337.062308	6260219.990337	405.636515	405.377128	119.357639	1.277809	67.436829	372.831413	1.371350	-136.746994	-56.971998	0.046522
HIP_00016 LC.hys	333.899950	7999.506497	350.461419	4655975.440628	351.501461	351.019181	143.902952	1.718116	18.441125	312.936912	1.668399	-136.736992	-56.971998	0.040838
HIP_00017 LC.hys	520.602411	7999.321570	324.447721	11141348.043484	539.897504	539.093806	86.121322	0.717985	5.615873	492.490610	1.890198	-136.726998	-56.971998	0.049623
HIP_00018 LC.hys	316.777663	7999.421543	331.472382	4190706.374844	335.622611	334.877410	143.462555	1.908848	90.011866	303.464053	1.301677	-136.776993	-56.961999	0.044297
HIP_00019 LC.hys	238.114525	7999.438859	374.869973	2355260.721345	255.022429	254.118952	216.419300	3.396413	41.218991	221.779789	1.515479	-136.766991	-56.961999	0.046017
HIP_00020 LC.hys	258.713899	7999.129314	279.222233	2786753.793325	280.331105	280.199821	148.195673	2.870411	83.158070	243.805510	1.270401	-136.756493	-56.961999	0.043331
HIP_00021 LC.hys	373.259048	7999.389028	344.662838	5811018.208057	391.143831	390.666036	126.678575	1.376590	52.242605	357.358009	1.435114	-136.746994	-56.961999	0.045688
HIP_00022 LC.hys	431.443418	7999.243895	303.845785	7730355.117725	451.476321	451.188411	96.825182	1.034783	51.301042	414.333861	1.399895	-136.736992	-56.961999	0.067225
HIP_00023 LC.hys	517.917068	7999.482501	301.119433	11030546.165609	537.508055	537.841427	80.329507	0.725212	103.163635	504.797354	1.243857	-136.726998	-56.961999	0.085463
HIP_00024 LC.hys	479.659157	7999.652798	280.201809	9505891.250024	501.861339	501.071366	80.521034	0.841547	21.922404	456.668712	1.555280	-136.776993	-56.951997	0.056874
HIP_00025 LC.hys	291.771605	7999.336037	341.463007	3552715.426962	309.831981	309.341596	160.508589	2.251612	50.025555	275.566185	1.441751	-136.766991	-56.951997	0.088990
HIP_00026 LC.hys	509.149690	7999.418487	279.887882	10672228.357138	531.020804	530.585288	75.908668	0.749555	57.477472	491.974202	1.350945	-136.756493	-56.951997	0.043280
HIP_00027 LC.hys	448.047747	7999.303284	382.710235	8323180.112509	464.078357	463.724039	117.533118	0.961087	33.451605	430.925623	1.569173	-136.746994	-56.951997	0.098545
HIP_00028 LC.hys	274.707805	7999.131273	356.652876	3146173.200707	291.843632	291.529058	178.151402	2.542496	137.514247	264.030376	1.226069	-136.736992	-56.951997	0.069713
HIP_00029 LC.hys	271.249009	7999.194288	345.885254	3066659.868131	288.707258	288.594055	174.998397	2.608439	39.995408	254.012601	1.495302	-136.726998	-56.951997	0.069665