3897_Position 118_00010.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: 316-F_400C_3DPA_(ID-643)
Additional Information
| Field | Value |
|---|---|
| Data last updated | February 10, 2026 |
| Metadata last updated | February 10, 2026 |
| Created | February 10, 2026 |
| Format | TXT |
| License | Creative Commons Attribution |
| Datastore active | False |
| Has views | True |
| Id | f2921b80-aca7-477b-8dac-251e34a22e8f |
| Mimetype | text/plain |
| Package id | 41dcb6f8-89d7-4a7e-ac22-94e353e56e5a |
| Position | 10 |
| Size | 318.4 KiB |
| State | active |
| Tracking summary | {'total': 0, 'recent': 0} |
| Url type | upload |