3483 bulk_00015.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: 625-F_400C_1DPA_(ID-448)
Additional Information