Tue Jun 08 16:11:20 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.119534	93.835769	0.000000
-0.906413	100.514921	0.005005
-1.588569	70.943927	0.010010
-2.581185	18.690013	0.015014
-6.117852	-21.493827	0.020019
-11.441718	-28.803589	0.025024
-17.808565	-22.980111	0.030029
-21.864385	-30.895673	0.035034
-26.019001	-27.140067	0.040038
-30.355376	-26.079952	0.045043
-33.929226	-33.510153	0.050048
-37.558442	-22.339597	0.055053
-40.846403	-21.063344	0.060058
-44.594515	-19.959618	0.065062
-48.466144	-16.900628	0.070067
-51.971216	-22.277090	0.075072
-55.974897	-22.898232	0.080077
-59.988159	-24.368723	0.085082
-63.601609	-21.376490	0.090086
-67.288470	-25.507242	0.095091
-70.969513	-38.171439	0.100096
-74.862963	-27.997588	0.105101
-78.849151	-31.606902	0.110106
-82.135466	-23.782658	0.115110
-85.754992	-18.705294	0.120115
-89.484841	-26.990088	0.125120
-93.415277	-19.919404	0.130125
-97.238173	-19.961682	0.135130
-101.345992	-24.543212	0.140134
-105.142875	-25.686055	0.145139
-108.830232	-29.935493	0.150144
-112.697066	-27.770898	0.155149
-116.288431	-24.098774	0.160154
-120.100255	-26.709732	0.165158
-123.712238	-16.812642	0.170163
-127.123340	-28.925886	0.175168
-131.029032	-29.900847	0.180173
-135.074198	-27.170031	0.185178
-138.887749	-25.565961	0.190182
-142.880175	-27.352955	0.195187
-146.498564	-31.624450	0.200192
-149.842194	-26.382395	0.205197
-153.773097	-29.592992	0.210202
-157.139833	-34.185509	0.215206
-161.412470	-34.191655	0.220211
-165.226974	-39.512584	0.225216
-169.178803	-30.288981	0.230221
-173.220294	-27.272203	0.235226
-176.926412	-25.456805	0.240230
-180.749593	-19.659229	0.245235
-183.913740	-26.837481	0.250240
-187.840187	-21.860554	0.255245
-191.543899	-27.039422	0.260250
-194.657635	-20.829856	0.265254
-199.463951	-22.009882	0.270259
-202.719204	-26.722925	0.275264
-206.033844	-18.038010	0.280269
-209.994127	-14.690544	0.285274
-213.791942	-19.678005	0.290278
-218.021565	-19.755024	0.295283
-221.411157	-26.433167	0.300288
-225.344101	-20.197944	0.305293
-229.057043	-10.144919	0.310298
-233.003675	-26.025305	0.315302
-236.882497	-20.887965	0.320307
-240.736497	-27.030947	0.325312
-244.408969	-26.041077	0.330317
-247.964932	-19.394866	0.335322
-251.642694	-26.120659	0.340326
-255.611044	-23.622371	0.345331
-258.791791	-23.963714	0.350336
-262.566122	-24.223773	0.355341
-266.684367	-17.145211	0.360346
-270.260541	-28.667160	0.365350
-274.507868	-19.575932	0.370355
-278.223905	-19.805321	0.375360
-281.869483	-23.837583	0.380365
-285.381177	-25.270354	0.385370
-289.210486	-26.907969	0.390374
-293.379437	-13.545989	0.395379
-296.918752	-27.048574	0.400384
-300.449545	-20.142188	0.405389
-304.183764	-24.844047	0.410394
-308.001058	-23.603118	0.415398
-312.058670	-18.270455	0.420403
-315.773635	-31.000048	0.425408
-319.524282	-23.704253	0.430413
-323.419846	-26.583282	0.435418
-326.884049	-23.631445	0.440422
-330.817897	-22.198806	0.445427
-334.109456	-27.437982	0.450432
-338.433967	-27.617024	0.455437
-341.895842	-23.893919	0.460442
-345.269830	-24.258892	0.465446
-349.452593	-21.068133	0.470451
-352.969860	-28.197916	0.475456
-357.008508	-22.504154	0.480461
-361.177282	-28.255947	0.485466
-364.723645	-34.656829	0.490470
-368.552742	-27.175843	0.495475
-371.968490	-19.630371	0.500480
-375.833962	-22.534250	0.505485
-379.771382	-21.612103	0.510490
-382.764762	-23.666171	0.515494
-387.240290	-20.046236	0.520499
-391.133707	-26.349673	0.525504
-394.862878	-23.836246	0.530509
-399.003009	-19.223514	0.535514
-402.325826	-26.133209	0.540518
-405.757634	-20.657970	0.545523
-409.601357	-28.209695	0.550528
-413.308511	-23.651491	0.555533
-417.379275	-25.491898	0.560538
-420.717622	-35.438957	0.565542
-424.950980	-22.935375	0.570547
-428.260389	-36.616996	0.575552
-432.112208	-30.799708	0.580557
-436.036675	-28.995587	0.585562
-439.518147	-24.754348	0.590566
-443.593089	-26.954383	0.595571
-447.413367	-32.022243	0.600576
-451.532264	-31.774639	0.605581
-455.135500	-41.939097	0.610586
-458.299448	-30.109185	0.615590
-462.502219	-24.869512	0.620595
-465.881926	-26.609366	0.625600
-469.856146	-34.347838	0.630605
-473.463562	-26.096044	0.635610
-477.138171	-36.490592	0.640614
-481.350642	-26.681672	0.645619
-484.735907	-36.325778	0.650624
-488.913588	-26.631365	0.655629
-492.668683	-26.511266	0.660634
-496.381098	-27.141328	0.665638
-500.105260	-30.259981	0.670643
-503.592160	-34.271118	0.675648
-507.301426	-26.867815	0.680653
-511.431680	-24.715319	0.685658
-514.577741	-31.360002	0.690662
-518.830769	-27.551947	0.695667
-522.486358	-29.215610	0.700672
-526.353909	-23.378572	0.705677
-530.166761	-26.306338	0.710682
-534.051102	-35.256134	0.715686
-537.539626	-28.396698	0.720691
-541.367060	-23.189381	0.725696
-545.132509	-26.635230	0.730701
-548.615226	-21.209572	0.735706
-552.689424	-33.254444	0.740710
-556.483364	-27.577634	0.745715
-560.076109	-27.880832	0.750720
-563.794346	-20.602646	0.755725
-567.686517	-28.295896	0.760730
-570.915084	-34.562062	0.765734
-574.892739	-24.692702	0.770739
-578.715793	-27.053846	0.775744
-582.579486	-20.622993	0.780749
-587.001919	-21.449679	0.785754
-590.781974	-28.611921	0.790758
-594.597226	-26.941263	0.795763
-598.017947	-38.020264	0.800768
-601.558949	-34.723492	0.805773
-605.396235	-32.438825	0.810778
-609.049619	-34.243308	0.815782
-612.749477	-18.734629	0.820787
-616.426038	-32.026265	0.825792
-620.342306	-30.020906	0.830797
-624.244502	-28.802243	0.835802
-627.717078	-27.947012	0.840806
-632.025492	-22.524070	0.845811
-635.404104	-25.808472	0.850816
-638.986062	-30.311568	0.855821
-642.929204	-29.482149	0.860826
-646.483956	-30.667256	0.865830
-650.434899	-22.526502	0.870835
-654.165121	-28.762962	0.875840
-658.178755	-20.947733	0.880845
-661.663144	-25.652278	0.885850
-665.103249	-41.267424	0.890854
-669.234241	-28.238095	0.895859
-673.153261	-29.413561	0.900864
-676.877066	-33.127733	0.905869
-680.924575	-25.720329	0.910874
-684.355801	-28.057046	0.915878
-688.317364	-18.388102	0.920883
-691.784915	-24.388968	0.925888
-695.445443	-35.737760	0.930893
-699.247789	-30.225171	0.935898
-702.972921	-31.355731	0.940902
-706.918209	-27.835165	0.945907
-710.756971	-38.097115	0.950912
-714.358968	-27.603349	0.955917
-718.195622	-28.057175	0.960922
-721.518832	-34.904169	0.965926
-725.474552	-24.779525	0.970931
-729.190439	-28.831696	0.975936
-733.299678	-25.004700	0.980941
-737.302531	-25.205792	0.985946
-740.911885	-28.805745	0.990950
-744.931142	-29.667912	0.995955
-748.449723	-25.654137	1.000960
-751.749753	-24.664223	1.005965
-755.670296	-29.167526	1.010970
-759.343981	-36.266156	1.015974
-763.247250	-31.643232	1.020979
-767.114308	-26.021592	1.025984
-770.811530	-27.319898	1.030989
-774.880283	-22.451865	1.035994
-777.963741	-34.227622	1.040998
-781.885181	-21.781227	1.046003
-785.754535	-22.843545	1.051008
-789.647548	-24.854623	1.056013
-793.503475	-20.197562	1.061018
-797.111618	-22.175822	1.066022
-801.256711	-19.722112	1.071027
-804.677814	-18.645857	1.076032
-808.410782	-28.811409	1.081037
-812.153353	-22.706267	1.086042
-815.948252	-32.048873	1.091046
-819.854123	-25.908198	1.096051
-823.504327	-20.260578	1.101056
-826.786509	-28.440745	1.106061
-830.991321	-24.766586	1.111066
-834.774197	-25.248880	1.116070
-838.709925	-13.933581	1.121075
-842.430368	-23.446434	1.126080
-846.118935	-19.065141	1.131085
-850.233240	-23.835864	1.136090
-853.403672	-31.216566	1.141094
-857.464574	-20.833383	1.146099
-861.276989	-32.281462	1.151104
-864.414594	-27.976177	1.156109
-868.655805	-21.474765	1.161114
-872.338421	-26.173522	1.166118
-876.474667	-24.389501	1.171123
-879.891220	-34.836643	1.176128
-883.478706	-31.830859	1.181133
-887.285396	-27.171910	1.186138
-890.960037	-24.549023	1.191142
-895.521909	-21.774624	1.196147
-898.666143	-22.343200	1.201152
-902.441007	-31.329977	1.206157
-906.254252	-22.436262	1.211162
-910.142544	-28.865991	1.216166
-913.764289	-27.988875	1.221171
-917.253849	-24.622929	1.226176
-921.406628	-24.067117	1.231181
-924.794459	-19.989208	1.236186
-928.430306	-33.836164	1.241190
-933.094652	-19.588170	1.246195
-936.233978	-18.547553	1.251200
-939.973621	-27.421535	1.256205
-943.685713	-25.427258	1.261210
-947.270977	-31.308621	1.266214
-951.326893	-24.328193	1.271219
-955.091150	-17.648862	1.276224
-958.686657	-20.034122	1.281229
-962.967104	-22.905694	1.286234
-966.291455	-26.566218	1.291238
-970.337869	-19.914615	1.296243
-974.170245	-19.394811	1.301248
-977.603204	-24.152911	1.306253
-981.797562	-22.832856	1.311258
-985.044054	-22.089571	1.316262
-989.072439	-25.833667	1.321267
-992.621751	-28.077628	1.326272
-996.511151	-16.362823	1.331277
-1000.615515	-15.845245	1.336282
-1003.795009	-26.383896	1.341286
-1007.493866	-26.031842	1.346291
-1011.241585	-22.740702	1.351296
-1015.489106	-22.543111	1.356301
-1019.672432	-23.428953	1.361306
-1022.758839	-22.160535	1.366310
-1026.676165	-21.092852	1.371315
-1029.918542	-24.915018	1.376320
-1033.977636	-28.772209	1.381325
-1038.219134	-20.908855	1.386330
-1042.133529	-28.486121	1.391334
-1045.687334	-16.452742	1.396339
-1049.218784	-24.821616	1.401344
-1052.374743	-19.993221	1.406349
-1056.530133	-15.366225	1.411354
-1060.308016	-25.055304	1.416358
-1064.481957	-19.031409	1.421363
-1068.134093	-25.406407	1.426368
-1071.869449	-29.518077	1.431373
-1075.508030	-24.081054	1.436378
-1079.165273	-30.288203	1.441382
-1083.196174	-22.246249	1.446387
-1086.818089	-28.965075	1.451392
-1090.491518	-27.423331	1.456397
-1094.377304	-31.316928	1.461402
-1097.615050	-41.701023	1.466406
-1102.024030	-24.472094	1.471411
-1105.743677	-25.150121	1.476416
-1109.237103	-31.958087	1.481421
-1113.211918	-22.929500	1.486426
-1116.686419	-37.833360	1.491430
-1120.614706	-27.537465	1.496435
-1124.290126	-24.681374	1.501440
-1128.340109	-21.618475	1.506445
-1132.200543	-18.708899	1.511450
-1135.262478	-28.731610	1.516454
-1139.071454	-32.375085	1.521459
-1143.196812	-37.175974	1.526464
-1146.922560	-34.805395	1.531469
-1150.781813	-25.074310	1.536474
-1154.916404	-32.587204	1.541478
-1158.550066	-17.810645	1.546483
-1162.000734	-33.681639	1.551488
-1165.449400	-33.413855	1.556493
-1169.742184	-28.099664	1.561498
-1173.265164	-22.343362	1.566502
-1177.160024	-17.108939	1.571507
-1180.875050	-22.814270	1.576512
-1184.573283	-26.837481	1.581517
-1188.390524	-20.650139	1.586522
-1191.868666	-26.003405	1.591526
-1195.824042	-19.863777	1.596531
-1199.835802	-27.867025	1.601536
-1203.320278	-26.107784	1.606541
-1207.400689	-23.492314	1.611546
-1210.567530	-26.740773	1.616550
-1214.830909	-26.698536	1.621555
-1218.259255	-22.809224	1.626560
-1221.832402	-28.988843	1.631565
-1226.080598	-23.876844	1.636570
-1229.679060	-28.270409	1.641574
-1233.314213	-26.480926	1.646579
-1237.116804	-16.619772	1.651584
-1240.920317	-29.674261	1.656589
-1245.020568	-25.721640	1.661594
-1248.359841	-30.417442	1.666598
-1252.423398	-24.631789	1.671603
-1256.424112	-23.114215	1.676608
-1259.952784	-29.368932	1.681613
-1263.808809	-23.944937	1.686618
-1267.244249	-29.636626	1.691622
-1270.890230	-25.080738	1.696627
-1274.453773	-31.031449	1.701632
-1278.369312	-31.406885	1.706637
-1282.367433	-28.398537	1.711642
-1286.015306	-38.550595	1.716646
-1290.013922	-31.332629	1.721651
-1293.735474	-31.469020	1.726656
-1297.469908	-29.095635	1.731661
-1301.372914	-29.205592	1.736666
-1304.947026	-27.958989	1.741670
-1308.572157	-25.142168	1.746675
-1312.465620	-31.369311	1.751680
-1316.159251	-32.086353	1.756685
-1320.318817	-28.983930	1.761690
-1323.516290	-36.090407	1.766694
-1327.629195	-25.969853	1.771699
-1330.972823	-20.839448	1.776704
-1334.573987	-37.265029	1.781709
-1338.846634	-28.689532	1.786714
-1342.465628	-28.301960	1.791718
-1346.319901	-30.159709	1.796723
-1350.215568	-27.221392	1.801728
-1353.765744	-32.045866	1.806733
-1358.173203	-17.678580	1.811738
-1361.531183	-24.423146	1.816742
-1364.906802	-15.754217	1.821747
-1368.928120	-25.106723	1.826752
-1372.426679	-31.058245	1.831757
-1376.721301	-26.365987	1.836762
-1380.103503	-27.861143	1.841766
-1383.557867	-23.957367	1.846771
-1387.683253	-32.254293	1.851776
-1391.136278	-27.911436	1.856781
-1395.341510	-22.145919	1.861786
-1398.802070	-34.684063	1.866790
-1402.932336	-32.138786	1.871795
-1406.681673	-24.596065	1.876800
-1410.310468	-34.637606	1.881805
-1414.162343	-22.755251	1.886810
-1417.595051	-32.794157	1.891814
-1421.630949	-23.443395	1.896819
-1425.121568	-24.459665	1.901824
-1428.722544	-35.426417	1.906829
-1432.825764	-26.711792	1.911834
-1436.820436	-31.676922	1.916838
-1440.513555	-20.277699	1.921843
-1444.053359	-24.154611	1.926848
-1447.312646	-31.212475	1.931853
-1451.539813	-22.006052	1.936858
-1455.169023	-31.463712	1.941862
-1459.023608	-19.868593	1.946867
-1462.841136	-23.064278	1.951872
-1466.539441	-28.898908	1.956877
-1470.875646	-19.843062	1.961882
-1474.370383	-24.725106	1.966886
-1477.835907	-19.224733	1.971891
-1481.659888	-19.570710	1.976896
-1485.774405	-32.580193	1.981901
-1489.551762	-21.494066	1.986906
-1492.719101	-32.689189	1.991910
-1496.899157	-21.092595	1.996915
-1500.723742	-23.593984	2.006912
-1501.589054	-24.982626	2.016909
-1499.185417	-28.087671	2.026906
-1496.420391	-26.428502	2.036902
-1493.960861	-27.134739	2.046899
-1492.385872	-26.697434	2.056896
-1490.428226	-27.705938	2.066893
-1488.450504	-21.322333	2.076890
-1486.680998	-30.171089	2.086886
-1484.816336	-22.867773	2.096883
-1482.899988	-30.044329	2.106880
-1480.803654	-25.158786	2.116877
-1478.989916	-23.444862	2.126874
-1477.139262	-26.208286	2.136870
-1475.066020	-27.170246	2.146867
-1473.127753	-28.015749	2.156864
-1471.670108	-21.846706	2.166861
-1469.586909	-26.359753	2.176858
-1467.744716	-27.567755	2.186854
-1465.809121	-33.755633	2.196851
-1463.886413	-25.777775	2.206848
-1462.023596	-27.339868	2.216845
-1460.232491	-25.614143	2.226842
-1458.596168	-26.808511	2.236838
-1455.986145	-26.388543	2.246835
-1454.264225	-24.502332	2.256832
-1452.489449	-24.572793	2.266829
-1450.810745	-29.538020	2.276826
-1448.703256	-24.408160	2.286822
-1446.794108	-29.862327	2.296819
-1445.220993	-30.645089	2.306816
-1443.354069	-33.656322	2.316813
-1441.205336	-34.035653	2.326810
-1439.389283	-33.242553	2.336806
-1437.381616	-34.442607	2.346803
-1435.560815	-27.760511	2.356800
-1433.839772	-28.976537	2.366797
-1431.805911	-26.894129	2.376794
-1430.037211	-30.399490	2.386790
-1427.940681	-32.064950	2.396787
-1426.223020	-27.079155	2.406784
-1424.327323	-31.754809	2.416781
-1422.703311	-32.792126	2.426778
-1420.518474	-27.754976	2.436774
-1418.518350	-29.235906	2.446771
-1416.750924	-28.366466	2.456768
-1415.160422	-18.845918	2.466765
-1413.143244	-20.023488	2.476762
-1411.091680	-24.040619	2.486758
-1409.001284	-20.802041	2.496755
-1407.411353	-24.589298	2.506752
-1405.637802	-22.969215	2.516749
-1403.690703	-25.128696	2.526746
-1401.851353	-24.374359	2.536742
-1399.965793	-23.417706	2.546739
-1398.161984	-23.374568	2.556736
-1396.173603	-31.095022	2.566733
-1394.117178	-27.539176	2.576730
-1392.267712	-23.843838	2.586726
-1390.554111	-26.736630	2.596723
-1388.332847	-25.727769	2.606720
-1386.564640	-26.492248	2.616717
-1385.118254	-27.795052	2.626714
-1382.992242	-26.868629	2.636710
-1381.160801	-28.064471	2.646707
-1379.089594	-30.734133	2.656704
-1377.550480	-21.556479	2.666701
-1375.637317	-24.509233	2.676698
-1373.649362	-31.479890	2.686694
-1371.784088	-29.142829	2.696691
-1369.730637	-26.643647	2.706688
-1367.772742	-28.618426	2.716685
-1366.000711	-22.444454	2.726682
-1364.238228	-20.833913	2.736678
-1362.347949	-22.228369	2.746675
-1360.064140	-25.176804	2.756672
-1358.674178	-28.621432	2.766669
-1357.128077	-29.734264	2.776666
-1354.625185	-30.955318	2.786662
-1352.849940	-29.431540	2.796659
-1350.900441	-28.221847	2.806656
-1349.019832	-28.069760	2.816653
-1347.211660	-35.677035	2.826650
-1345.414241	-31.409167	2.836646
-1343.625467	-31.486334	2.846643
-1341.555024	-29.723961	2.856640
-1339.981663	-28.999395	2.866637
-1338.016256	-19.249958	2.876634
-1336.044235	-22.028241	2.886630
-1334.093138	-24.836523	2.896627
-1332.168347	-25.561479	2.906624
-1330.396084	-34.076702	2.916621
-1328.576047	-29.797693	2.926618
-1326.909348	-26.052358	2.936614
-1324.725647	-25.579634	2.946611
-1323.083201	-34.275697	2.956608
-1320.912323	-33.678254	2.966605
-1319.120922	-30.966468	2.976602
-1317.452605	-33.021117	2.986598
-1315.093807	-27.561663	2.996595
-1313.548221	-30.754383	3.006592
-1311.483951	-36.846922	3.016589
-1309.908649	-35.442126	3.026586
-1307.820660	-38.635128	3.036582
-1305.803707	-39.021002	3.046579
-1304.088033	-38.260398	3.056576
-1302.487127	-36.451350	3.066573
-1300.578712	-30.540666	3.076570
-1298.204496	-37.580398	3.086566
-1296.690117	-35.828810	3.096563
-1294.712920	-32.971869	3.106560
-1292.984853	-29.197539	3.116557
-1291.002016	-29.096576	3.126554
-1289.228714	-33.417201	3.136550
-1287.190727	-29.727318	3.146547
-1285.104971	-40.851005	3.156544
-1283.528940	-41.747633	3.166541
-1281.501701	-26.112647	3.176538
-1279.451589	-33.335415	3.186534
-1278.156597	-38.034308	3.196531
-1276.230479	-34.672992	3.206528
-1273.970173	-31.946472	3.216525
-1272.035778	-35.010324	3.226522
-1270.570065	-30.347547	3.236518
-1268.307606	-28.220928	3.246515
-1266.631799	-33.515593	3.256512
-1264.590804	-30.772744	3.266509
-1262.822303	-28.015897	3.276506
-1261.173470	-27.955569	3.286502
-1259.111109	-30.143080	3.296499
-1256.857672	-36.989342	3.306496
-1255.293703	-32.861556	3.316493
-1253.715078	-30.255078	3.326490
-1251.796363	-34.943310	3.336486
-1249.560200	-34.852636	3.346483
-1247.708460	-36.534459	3.356480
-1245.694875	-34.812464	3.366477
-1244.090824	-26.718899	3.376474
-1242.091769	-32.159178	3.386470
-1240.317292	-32.680038	3.396467
-1238.032215	-35.250411	3.406464
-1236.487910	-32.206858	3.416461
-1234.990000	-29.105144	3.426458
-1232.746538	-39.086073	3.436454
-1230.821279	-34.873304	3.446451
-1229.246365	-32.639259	3.456448
-1227.738168	-31.668704	3.466445
-1225.257196	-32.244491	3.476442
-1223.223416	-32.400437	3.486438
-1221.250651	-31.319564	3.496435
-1219.726105	-30.843456	3.506432
-1217.778222	-30.151939	3.516429
-1215.960858	-27.206252	3.526426
-1214.059323	-34.120112	3.536422
-1212.016643	-30.379618	3.546419
-1210.438223	-31.590823	3.556416
-1208.287445	-32.582568	3.566413
-1206.470730	-31.354746	3.576410
-1204.777920	-36.005350	3.586406
-1202.801652	-42.117507	3.596403
-1201.195720	-31.139606	3.606400
-1198.944557	-28.232443	3.616397
-1197.064267	-32.227573	3.626394
-1195.124898	-32.213951	3.636390
-1193.402050	-32.907327	3.646387
-1191.448585	-30.017408	3.656384
-1189.644969	-32.188514	3.666381
-1187.683391	-29.437520	3.676378
-1185.978904	-29.224288	3.686374
-1183.981668	-32.094965	3.696371
-1182.019550	-38.327596	3.706368
-1180.161040	-33.830644	3.716365
-1178.669429	-35.976226	3.726362
-1176.657912	-36.497058	3.736358
-1174.591719	-42.542442	3.746355
-1172.503654	-34.934682	3.756352
-1171.129626	-34.693153	3.766349
-1168.960720	-29.920285	3.776346
-1167.017882	-38.788422	3.786342
-1165.189127	-32.519761	3.796339
-1163.533418	-34.054856	3.806336
-1161.394036	-27.334057	3.816333
-1159.485619	-30.347952	3.826330
-1157.700967	-30.918740	3.836326
-1155.720545	-35.777195	3.846323
-1154.272195	-31.195965	3.856320
-1152.310667	-33.128195	3.866317
-1150.073838	-34.191993	3.876314
-1148.293546	-36.270153	3.886310
-1146.445690	-37.628379	3.896307
-1144.355928	-30.770608	3.906304
-1142.809092	-36.250175	3.916301
-1141.061554	-35.977923	3.926298
-1138.825157	-32.016534	3.936294
-1137.007487	-33.918126	3.946291
-1135.186942	-33.147399	3.956288
-1133.487588	-25.592220	3.966285
-1131.359577	-29.352819	3.976282
-1129.208173	-29.068496	3.986278
-1127.706457	-26.409239	3.996275
-1126.232248	-31.998848	4.006272
-1123.926654	-26.953411	4.016269
-1122.138342	-35.659442	4.026266
-1119.844489	-33.414430	4.036262
-1118.017202	-28.887581	4.046259
-1116.400182	-29.931487	4.056256
-1114.568884	-32.694994	4.066253
-1112.966444	-26.868417	4.076250
-1110.876937	-27.240968	4.086246
-1108.919192	-30.283072	4.096243
-1106.983788	-29.029741	4.106240
-1105.074836	-29.340461	4.116237
-1103.355404	-35.502541	4.126234
-1101.713876	-33.369200	4.136230
-1099.386879	-34.453197	4.146227
-1097.675260	-30.276396	4.156224
-1095.902321	-32.434688	4.166221
-1093.932005	-30.705188	4.176218
-1092.012421	-28.121619	4.186214
-1090.115844	-31.054015	4.196211
-1088.408347	-30.347641	4.206208
-1086.374283	-31.198352	4.216205
-1084.334912	-29.551842	4.226202
-1082.775886	-31.317709	4.236198
-1080.863032	-35.839272	4.246195
-1078.548947	-35.680868	4.256192
-1076.463548	-32.342455	4.266189
-1075.437307	-29.944979	4.276186
-1073.694041	-35.148803	4.286182
-1071.291987	-38.284961	4.296179
-1069.846327	-36.760591	4.306176
-1067.599228	-36.072162	4.316173
-1065.790417	-27.801838	4.326170
-1063.939538	-23.409432	4.336166
-1062.013067	-30.723520	4.346163
-1059.972707	-23.746161	4.356160
-1058.501634	-29.066864	4.366157
-1056.188241	-30.244538	4.376154
-1054.414360	-34.101988	4.386150
-1052.736482	-36.964806	4.396147
-1050.666542	-27.842968	4.406144
-1049.122919	-25.517322	4.416141
-1046.985774	-29.670314	4.426138
-1045.276472	-27.512226	4.436134
-1043.232553	-27.520041	4.446131
-1041.124423	-32.154159	4.456128
-1039.571027	-32.721554	4.466125
-1037.624431	-23.940938	4.476122
-1035.644114	-28.337720	4.486118
-1033.877565	-28.068292	4.496115
-1031.847745	-23.048960	4.506112
-1030.007694	-24.266289	4.516109
-1028.375290	-27.877727	4.526106
-1026.577847	-28.461329	4.536102
-1024.666061	-33.230089	4.546099
-1022.326720	-25.564600	4.556096
-1020.789497	-28.096575	4.566093
-1018.873268	-27.080199	4.576090
-1017.267903	-29.348014	4.586086
-1015.043313	-35.795979	4.596083
-1012.994920	-28.001887	4.606080
-1011.177815	-27.556565	4.616077
-1009.257292	-29.055654	4.626074
-1007.780618	-31.665756	4.636070
-1006.132188	-28.341998	4.646067
-1003.770853	-32.585232	4.656064
-1001.721189	-32.549750	4.666061
-1000.359152	-23.097675	4.676058
-998.290277	-24.087902	4.686054
-996.322022	-29.226780	4.696051
-994.471892	-20.275049	4.706048
-992.594035	-22.098785	4.716045
-990.862820	-22.987171	4.726042
-988.880617	-23.653458	4.736038
-986.821341	-28.028602	4.746035
-984.904136	-26.930964	4.756032
-983.149808	-24.826424	4.766029
-981.228149	-25.317511	4.776026
-979.408688	-17.718453	4.786022
-977.748415	-28.401443	4.796019
-975.605610	-24.750732	4.806016
-973.577087	-24.628217	4.816013
-972.298060	-27.242318	4.826010
-970.343365	-25.054398	4.836006
-968.433003	-24.759834	4.846003
-966.046251	-28.159289	4.856000
-964.139770	-29.233466	4.865997
-962.768282	-24.388005	4.875994
-960.774595	-23.467104	4.885990
-958.786125	-18.745343	4.895987
-956.800453	-22.167629	4.905984
-955.136806	-24.242290	4.915981
-952.966092	-28.989868	4.925978
-951.567501	-23.347566	4.935974
-949.197547	-24.807590	4.945971
-947.403819	-25.130867	4.955968
-946.061410	-24.421834	4.965965
-943.856342	-25.940891	4.975962
-941.856042	-28.321927	4.985958
-939.821157	-24.147194	4.995955
-938.007141	-24.477507	5.005952
-936.457287	-25.519302	5.015949
-934.521017	-22.474937	5.025946
-932.508271	-20.926931	5.035942
-930.779489	-23.217484	5.045939
-928.700758	-21.881966	5.055936
-926.843668	-25.817679	5.065933
-925.017976	-22.918341	5.075930
-922.997277	-24.643261	5.085926
-921.133200	-20.272417	5.095923
-919.482674	-24.535078	5.105920
-917.866928	-20.987118	5.115917
-915.979678	-23.608786	5.125914
-913.749763	-25.847823	5.135910
-911.777318	-23.692957	5.145907
-909.890178	-28.271693	5.155904
-908.222677	-24.315666	5.165901
-906.413263	-34.026718	5.175898
-904.394711	-31.514589	5.185894
-902.404641	-35.504734	5.195891
-900.664642	-37.746217	5.205888
-898.632916	-35.654085	5.215885
-896.528451	-34.464456	5.225882
-894.888626	-31.694843	5.235878
-893.021160	-38.347427	5.245875
-891.542291	-37.597777	5.255872
-889.790206	-30.895312	5.265869
-887.798110	-38.006392	5.275866
-885.398012	-38.503287	5.285862
-883.607469	-35.173046	5.295859
-881.521062	-40.101353	5.305856
-879.929152	-35.556517	5.315853
-878.243465	-29.061990	5.325850
-876.226520	-40.474867	5.335846
-874.138149	-43.459459	5.345843
-872.809515	-32.759056	5.355840
-870.576315	-35.902880	5.365837
-868.732940	-35.904644	5.375834
-867.171677	-34.441543	5.385830
-865.036643	-42.314219	5.395827
-863.019533	-30.154695	5.405824
-861.251977	-38.146092	5.415821
-859.571455	-33.094382	5.425818
-857.317943	-33.283128	5.435814
-855.741423	-42.026226	5.445811
-853.056772	-39.261650	5.455808
-851.945471	-41.888029	5.465805
-850.288147	-32.453383	5.475802
-848.161889	-40.400032	5.485798
-846.295841	-35.497539	5.495795
-844.325846	-30.950002	5.505792
-842.211919	-29.657238	5.515789
-840.566962	-30.973397	5.525786
-838.979346	-32.066694	5.535782
-837.281308	-37.593858	5.545779
-834.787942	-36.787120	5.555776
-832.966870	-36.171672	5.565773
-831.110211	-38.451331	5.575770
-829.332763	-36.374408	5.585766
-827.489357	-37.953056	5.595763
-825.533415	-33.763927	5.605760
-823.593544	-42.796629	5.615757
-822.005454	-37.986322	5.625754
-819.775087	-39.616762	5.635750
-818.188924	-39.162150	5.645747
-816.192460	-41.379643	5.655744
-814.517407	-42.004989	5.665741
-812.583318	-39.532067	5.675738
-810.582520	-42.795638	5.685734
-808.490104	-39.490698	5.695731
-806.740822	-39.628442	5.705728
-804.660199	-37.505926	5.715725
-802.871192	-32.108820	5.725722
-801.488710	-34.862356	5.735718
-799.408946	-33.249514	5.745715
-797.390508	-41.641220	5.755712
-795.617248	-43.185289	5.765709
-793.776511	-36.325288	5.775706
-791.630186	-36.913342	5.785702
-790.148457	-39.115988	5.795699
-788.221107	-40.024915	5.805696
-786.287267	-37.982720	5.815693
-784.006940	-32.011506	5.825690
-782.306852	-25.121426	5.835686
-780.804441	-35.898595	5.845683
-778.701004	-33.415991	5.855680
-776.523828	-36.137947	5.865677
-774.837350	-29.233674	5.875674
-773.029057	-25.784702	5.885670
-771.501079	-32.771426	5.895667
-769.045855	-40.574130	5.905664
-767.469099	-33.413896	5.915661
-765.622369	-31.967342	5.925658
-763.671839	-29.305144	5.935654
-761.827814	-37.723421	5.945651
-760.086750	-39.646492	5.955648
-757.996147	-34.535488	5.965645
-755.739469	-39.964847	5.975642
-754.333122	-38.105593	5.985638
-752.397003	-40.825687	5.995635
-750.539606	-44.445210	6.005632
-748.622799	-40.477761	6.015629
-746.761320	-36.187411	6.025626
-744.953193	-29.469595	6.035622
-743.091753	-39.088348	6.045619
-740.847585	-34.821780	6.055616
-739.250204	-32.675183	6.065613
-737.112877	-37.369902	6.075610
-736.115883	-31.759772	6.085606
-734.053592	-35.907285	6.095603
-731.340351	-36.463369	6.105600
-729.941245	-38.304029	6.115597
-728.109405	-37.579725	6.125594
-726.116645	-29.026206	6.135590
-724.229448	-37.168512	6.145587
-722.179571	-34.401619	6.155584
-720.440067	-32.689241	6.165581
-718.455266	-35.855573	6.175578
-716.936683	-28.800338	6.185574
-715.239527	-36.831775	6.195571
-712.654301	-36.865539	6.205568
-711.163369	-35.674467	6.215565
-709.312977	-30.849053	6.225562
-707.343993	-30.260910	6.235558
-705.719737	-33.577197	6.245555
-703.507665	-35.089038	6.255552
-701.636308	-36.064594	6.265549
-699.782910	-39.140786	6.275546
-697.772940	-36.689131	6.285542
-696.117770	-37.582531	6.295539
-694.167587	-35.701181	6.305536
-692.506165	-35.168144	6.315533
-690.362936	-31.943395	6.325530
-688.677745	-30.046603	6.335526
-686.917727	-38.147706	6.345523
-684.587262	-31.738842	6.355520
-682.936134	-32.369123	6.365517
-681.323618	-35.399623	6.375514
-679.339368	-29.365286	6.385510
-677.164695	-37.157744	6.395507
-675.460420	-35.901306	6.405504
-673.353711	-37.618346	6.415501
-671.891665	-31.681329	6.425498
-669.963290	-35.563173	6.435494
-668.025641	-36.553649	6.445491
-666.035010	-29.100004	6.455488
-664.207725	-34.757976	6.465485
-662.165376	-37.642492	6.475482
-660.514557	-34.914191	6.485478
-658.357618	-33.011394	6.495475
-656.551796	-36.967053	6.505472
-655.018351	-33.381942	6.515469
-653.471288	-36.371165	6.525466
-651.034325	-36.188958	6.535462
-649.114534	-37.864822	6.545459
-647.628902	-31.923543	6.555456
-645.126502	-33.763801	6.565453
-643.306368	-38.128981	6.575450
-641.832052	-33.149682	6.585446
-639.941400	-34.864807	6.595443
-637.763852	-35.703967	6.605440
-635.678188	-37.355725	6.615437
-634.486272	-41.215516	6.625434
-632.479278	-35.925294	6.635430
-630.313227	-38.342540	6.645427
-628.540159	-34.009692	6.655424
-626.936751	-27.225862	6.665421
-625.256937	-33.115404	6.675418
-622.605900	-33.729514	6.685414
-620.930561	-27.987160	6.695411
-619.227083	-34.219063	6.705408
-617.312022	-34.233416	6.715405
-615.493591	-34.280590	6.725402
-613.477323	-36.312087	6.735398
-611.701215	-32.164712	6.745395
-609.743681	-34.808985	6.755392
-607.615242	-34.041462	6.765389
-605.784829	-35.805518	6.775386
-604.402980	-36.702967	6.785382
-602.768459	-35.536100	6.795379
-600.449446	-35.831199	6.805376
-598.337178	-36.232309	6.815373
-596.676856	-33.535649	6.825370
-594.814253	-40.804615	6.835366
-592.723325	-37.806783	6.845363
-591.105841	-36.504592	6.855360
-589.170651	-30.142854	6.865357
-587.395846	-29.690884	6.875354
-585.196875	-35.134374	6.885350
-583.734840	-33.426102	6.895347
-581.821360	-41.278433	6.905344
-579.449465	-36.034197	6.915341
-577.775525	-34.532224	6.925338
-576.002303	-33.413254	6.935334
-574.380385	-38.903163	6.945331
-572.278027	-41.022527	6.955328
-570.431595	-39.657647	6.965325
-568.571418	-35.465002	6.975322
-566.642318	-36.714412	6.985318
-564.502369	-33.715492	6.995315
-562.882883	-38.224061	7.005312
-561.231269	-38.714869	7.015309
-559.389904	-36.508495	7.025306
-557.180218	-35.281817	7.035302
-555.062120	-34.106214	7.045299
-553.475320	-37.155972	7.055296
-551.508839	-33.164936	7.065293
-549.476237	-34.187856	7.075290
-548.154519	-31.701429	7.085286
-546.298808	-38.880274	7.095283
-544.119537	-38.876299	7.105280
-541.848593	-45.235178	7.115277
-540.695235	-36.268795	7.125274
-538.429823	-38.325222	7.135270
-536.438714	-38.815778	7.145267
-534.675816	-35.435189	7.155264
-533.130918	-36.321466	7.165261
-530.806937	-42.994545	7.175258
-529.015889	-36.836085	7.185254
-527.349552	-34.541966	7.195251
-525.501365	-34.760593	7.205248
-523.289599	-39.515811	7.215245
-521.790911	-33.769191	7.225242
-519.967986	-26.589822	7.235238
-517.597504	-31.597147	7.245235
-515.935895	-30.907570	7.255232
-513.995495	-32.388912	7.265229
-511.924757	-30.151126	7.275226
-510.391134	-25.130967	7.285222
-508.327393	-26.913280	7.295219
-506.688663	-34.844523	7.305216
-504.815024	-35.601046	7.315213
-502.948458	-41.893297	7.325210
-501.116538	-34.298911	7.335206
-499.025943	-32.845469	7.345203
-497.211780	-32.770531	7.355200
-495.313499	-35.892285	7.365197
-493.584660	-31.982965	7.375194
-491.714262	-33.672422	7.385190
-489.621775	-34.587025	7.395187
-487.723852	-39.591512	7.405184
-485.864710	-33.707926	7.415181
-483.823871	-31.628616	7.425178
-482.253205	-31.243151	7.435174
-480.544176	-40.228624	7.445171
-478.564038	-41.892638	7.455168
-476.431776	-37.349440	7.465165
-474.677313	-39.070772	7.475162
-472.809506	-33.959728	7.485158
-470.888839	-39.278353	7.495155
-469.078065	-29.773415	7.505152
-467.313057	-32.344289	7.515149
-465.235334	-32.465920	7.525146
-463.395835	-29.978186	7.535142
-461.458801	-34.379559	7.545139
-459.633878	-31.145135	7.555136
-458.274254	-32.946139	7.565133
-455.540595	-37.171166	7.575130
-453.845747	-34.479581	7.585126
-452.131935	-29.191135	7.595123
-450.426948	-27.116635	7.605120
-448.449478	-25.155670	7.615117
-446.601963	-26.547540	7.625114
-444.557326	-27.260259	7.635110
-442.665503	-26.720017	7.645107
-441.033390	-25.251125	7.655104
-439.281267	-33.725857	7.665101
-436.890537	-24.873297	7.675098
-435.320726	-25.398637	7.685094
-433.605020	-20.776046	7.695091
-431.628639	-24.530870	7.705088
-429.186056	-26.987164	7.715085
-427.888515	-20.928159	7.725082
-425.992063	-16.891450	7.735078
-424.344163	-25.039245	7.745075
-422.115721	-23.643796	7.755072
-420.180627	-27.577679	7.765069
-418.118523	-20.080038	7.775066
-416.598204	-22.032300	7.785062
-414.773266	-18.717232	7.795059
-412.979612	-25.801607	7.805056
-411.212480	-20.470513	7.815053
-408.767257	-25.516299	7.825050
-407.067253	-25.766367	7.835046
-405.233694	-26.727808	7.845043
-403.198663	-26.180498	7.855040
-401.562277	-26.129959	7.865037
-399.742355	-25.831091	7.875034
-397.772284	-25.493165	7.885030
-395.645151	-26.316051	7.895027
-393.972242	-28.128096	7.905024
-392.253845	-27.579423	7.915021
-390.043851	-28.580535	7.925018
-388.315127	-25.083357	7.935014
-386.965320	-24.235115	7.945011
-384.540924	-24.993982	7.955008
-382.557194	-23.349836	7.965005
-380.809529	-25.105933	7.975002
-378.890483	-22.859054	7.984998
-377.130697	-19.592471	7.994995
-375.079015	-28.737083	8.004992
-373.632991	-25.866432	8.014989
-371.260552	-26.227092	8.024986
-369.739217	-29.713340	8.034982
-367.751878	-27.521250	8.044979
-365.883154	-24.865381	8.054976
-364.008092	-19.316046	8.064973
-362.194146	-24.365368	8.074970
-359.875084	-27.344252	8.084966
-358.512732	-20.547803	8.094963
-356.530513	-27.974352	8.104960
-354.678789	-23.982898	8.114957
-352.469029	-23.241055	8.124954
-350.863453	-26.259191	8.134950
-349.087631	-24.152140	8.144947
-347.139340	-29.866724	8.154944
-344.923589	-25.906882	8.164941
-343.354135	-24.588848	8.174938
-341.488571	-24.403703	8.184934
-339.694469	-25.870548	8.194931
-337.773268	-26.814984	8.204928
-335.848600	-23.069210	8.214925
-333.678884	-28.408375	8.224922
-332.218530	-25.291577	8.234918
-330.384804	-24.311327	8.244915
-328.227531	-21.238187	8.254912
-326.305805	-21.500962	8.264909
-324.837884	-19.523281	8.274906
-322.577235	-26.562445	8.284902
-320.775590	-21.570001	8.294899
-318.991347	-31.418837	8.304896
-317.352327	-31.878150	8.314893
-315.347309	-24.524007	8.324890
-313.284994	-32.973260	8.334886
-311.393257	-27.502644	8.344883
-309.332413	-27.576253	8.354880
-307.742639	-29.368080	8.364877
-305.894238	-27.198370	8.374874
-304.292531	-26.878633	8.384870
-301.996734	-22.811957	8.394867
-299.972193	-26.854801	8.404864
-298.498564	-27.423274	8.414861
-296.168395	-22.240079	8.424858
-294.561356	-29.220872	8.434854
-292.658246	-25.953543	8.444851
-290.958121	-26.524898	8.454848
-288.452190	-19.228594	8.464845
-286.965899	-18.364605	8.474842
-285.340422	-21.812571	8.484838
-283.330360	-24.079200	8.494835
-281.364665	-20.479158	8.504832
-279.299692	-25.933523	8.514829
-277.958649	-25.188872	8.524826
-275.997202	-22.092392	8.534822
-274.075213	-24.089394	8.544819
-272.095097	-21.711059	8.554816
-270.114168	-25.644446	8.564813
-268.154014	-26.526370	8.574810
-266.306411	-25.367070	8.584807
-264.654347	-17.632237	8.594803
-262.696165	-21.186266	8.604800
-260.761100	-26.136180	8.614797
-258.829470	-19.771287	8.624794
-257.007099	-20.203139	8.634791
-254.922752	-24.177575	8.644787
-253.238900	-25.741276	8.654784
-251.259979	-26.937447	8.664781
-249.583249	-30.125048	8.674778
-247.522169	-27.813548	8.684775
-245.804351	-27.956345	8.694771
-243.950645	-38.552169	8.704768
-241.968513	-33.574049	8.714765
-239.928456	-26.773645	8.724762
-238.225037	-25.453255	8.734759
-236.268476	-29.284830	8.744755
-234.567434	-36.141819	8.754752
-232.781267	-28.018162	8.764749
-230.759701	-25.337068	8.774746
-228.654849	-24.706406	8.784743
-226.843601	-22.504995	8.794739
-225.162009	-30.774704	8.804736
-223.451986	-33.476753	8.814733
-221.556913	-30.890551	8.824730
-219.252348	-33.922210	8.834727
-217.800754	-34.582520	8.844723
-216.100724	-32.587304	8.854720
-214.122861	-32.480648	8.864717
-211.545661	-34.190036	8.874714
-209.857537	-35.492426	8.884711
-208.382887	-30.017417	8.894707
-206.534229	-34.583753	8.904704
-204.183673	-32.132570	8.914701
-202.844509	-28.597751	8.924698
-200.640197	-27.461658	8.934695
-198.811160	-26.484502	8.944691
-196.675271	-27.168890	8.954688
-195.429450	-31.515644	8.964685
-193.248658	-28.828643	8.974682
-191.358230	-25.089972	8.984679
-189.596914	-26.608838	8.994675
-187.592213	-26.385442	9.004672
-185.364309	-29.019394	9.014669
-183.967685	-25.936272	9.024666
-182.044349	-32.866543	9.034663
-179.846949	-28.526036	9.044659
-178.259575	-27.074271	9.054656
-176.150268	-30.283865	9.064653
-174.418030	-29.740248	9.074650
-172.859682	-29.987276	9.084647
-170.736424	-30.555270	9.094643
-168.860480	-27.527073	9.104640
-166.896520	-28.557023	9.114637
-165.120885	-30.908683	9.124634
-163.302047	-27.335965	9.134631
-161.296943	-30.130886	9.144627
-159.551347	-27.198106	9.154624
-157.399395	-28.751148	9.164621
-155.587837	-22.022172	9.174618
-154.043732	-27.305353	9.184615
-152.091341	-22.705840	9.194611
-150.263880	-23.665343	9.204608
-148.237977	-27.340810	9.214605
-146.123466	-19.149315	9.224602
-144.547044	-19.505351	9.234599
-142.569843	-15.848327	9.244595
-140.676404	-18.694441	9.254592
-138.795112	-21.984273	9.264589
-136.934843	-23.471478	9.274586
-135.021354	-22.677139	9.284583
-133.543028	-24.343088	9.294579
-131.106869	-18.200605	9.304576
-129.292544	-27.399675	9.314573
-127.716575	-24.912051	9.324570
-125.738791	-18.000519	9.334567
-123.403491	-19.537561	9.344563
-122.145354	-17.727371	9.354560
-120.045330	-19.577784	9.364557
-118.106140	-19.987720	9.374554
-116.273790	-20.119282	9.384551
-114.398005	-21.058208	9.394547
-112.877092	-20.721386	9.404544
-110.704082	-19.836375	9.414541
-108.908991	-23.888013	9.424538
-106.993000	-16.003920	9.434535
-105.161877	-20.496473	9.444531
-103.215340	-20.417200	9.454528
-101.146146	-18.093581	9.464525
-99.355360	-15.790988	9.474522
-97.403683	-20.679271	9.484519
-95.812198	-16.443093	9.494515
-93.666247	-14.241712	9.504512
-91.958932	-20.114862	9.514509
-90.079687	-27.490461	9.524506
-87.757143	-21.441897	9.534503
-86.184707	-18.619299	9.544499
-84.467288	-13.758532	9.554496
-82.607825	-19.365705	9.564493
-80.670788	-18.109025	9.574490
-78.798205	-22.243499	9.584487
-77.091861	-16.495547	9.594483
-75.062469	-11.169747	9.604480
-73.014184	-19.705833	9.614477
-71.447743	-19.757792	9.624474
-69.405867	-13.875296	9.634471
-67.748307	-12.669096	9.644467
-65.541735	-16.937113	9.654464
-63.524585	-17.505833	9.664461
-61.893506	-21.072462	9.674458
-59.995599	-21.001826	9.684455
-58.497674	-22.239141	9.694451
-56.283172	-24.413867	9.704448
-54.567278	-18.704299	9.714445
-52.239153	-20.377611	9.724442
-50.803093	-16.307630	9.734439
-48.689388	-17.059286	9.744435
-46.782801	-12.146362	9.754432
-45.085780	-18.201509	9.764429
-42.871316	-20.215765	9.774426
-41.396132	-20.869789	9.784423
-39.366922	-21.987150	9.794419
-37.352840	-23.841761	9.804416
-35.563683	-19.974202	9.814413
-33.810434	-25.074261	9.824410
-31.865638	-24.484830	9.834407
-30.055431	-21.841305	9.844403
-27.975350	-20.894080	9.854400
-26.419713	-22.682332	9.864397
-24.366525	-20.469755	9.874394
-22.409033	-17.015202	9.884391
-20.767809	-15.822784	9.894387
-18.590914	-21.122738	9.904384
-16.836295	-22.910720	9.914381
-14.964887	-21.321844	9.924378
-13.065070	-21.431338	9.934375
-11.195576	-14.796010	9.944371
-9.605613	-20.482628	9.954368
-7.229752	-25.655442	9.964365
-5.770311	-10.796097	9.974362
-4.402506	3.603133	9.984359
-3.404903	42.464210	9.994355
-2.179452	97.707670	10.004352
-0.815831	172.459058	10.014349
0.000000	236.953739	10.019354
1.304522	278.147851	10.024359
1.702469	320.352078	10.029363
2.686632	358.501599	10.034368
2.996268	390.408695	10.039373
3.515096	413.566501	10.044378
4.165512	432.640088	10.049383
3.936245	448.574510	10.054387
4.513318	444.904543	10.059392
4.493618	447.682063	10.064397
4.532509	451.733571	10.069402
4.857585	449.056513	10.074407
4.866619	463.638824	10.079411
4.613161	456.885576	10.084416
4.825340	467.882133	10.089421
4.925400	467.222005	10.094426
4.805354	469.773190	10.099431
5.622542	487.600529	10.104435
5.317087	471.980040	10.109440
5.352584	475.256900	10.114445
5.200237	475.247132	10.119450
5.499513	482.873618	10.124455
5.185213	483.216081	10.129459
5.135332	486.457452	10.134464
4.837656	479.365998	10.139469
5.058991	487.046111	10.144474
5.301714	487.911997	10.149479
5.175467	509.135089	10.154483
5.782510	507.406750	10.159488
5.813014	512.809274	10.164493
6.024436	513.119624	10.169498
5.862467	508.494416	10.174503
5.518325	510.545231	10.179507
5.591801	501.061259	10.184512
5.831510	501.696748	10.189517
5.871827	509.185284	10.194522
5.733380	500.431178	10.199527
5.709964	506.759494	10.204531
5.873920	504.773188	10.209536
5.811323	517.205926	10.214541
5.736156	527.891409	10.219546
6.123699	531.495540	10.224551
6.079493	533.817423	10.229555
6.332553	541.095820	10.234560
6.287194	544.523527	10.239565
6.246692	538.993694	10.244570
6.406520	534.305805	10.249575
6.212218	534.845977	10.254579
6.554242	544.562338	10.259584
6.436925	547.775021	10.264589
6.302821	540.916408	10.269594
6.444742	544.007671	10.274599
6.307027	545.179176	10.279603
6.810668	547.538968	10.284608
6.282595	551.087333	10.289613
6.015535	550.706061	10.294618
6.403547	550.241683	10.299623
5.854333	552.875148	10.304627
6.430863	566.511990	10.309632
6.424298	578.498209	10.314637
6.897063	582.375495	10.319642
6.672189	579.174171	10.324647
6.597184	591.691988	10.329651
6.904571	590.551451	10.334656
7.025885	587.600235	10.339661
7.022642	598.230409	10.344666
7.267375	588.218086	10.349671
6.749994	594.757049	10.354675
7.350804	608.398843	10.359680
6.925174	612.994631	10.364685
7.281776	619.978609	10.369690
7.913887	621.865213	10.374695
7.648775	624.444847	10.379699
7.681622	615.103163	10.384704
7.135762	613.128416	10.389709
7.368208	624.451995	10.394714
7.810312	626.966031	10.399719
7.644167	637.943102	10.404723
7.689369	632.113154	10.409728
7.346136	634.380534	10.414733
7.517472	631.291263	10.419738
8.205503	622.026709	10.424743
7.723679	633.548153	10.429747
7.995054	635.311876	10.434752
8.222532	636.890499	10.439757
8.115809	638.445503	10.444762
8.370995	633.070987	10.449767
8.001982	634.250577	10.454771
8.061742	638.032114	10.459776
7.998721	649.186113	10.464781
7.794989	644.337504	10.469786
8.435509	641.163445	10.474791
7.948749	644.007264	10.479795
8.199023	633.439370	10.484800
7.971738	650.681390	10.489805
7.820686	650.145622	10.494810
8.065092	654.384573	10.499815
8.082069	672.127093	10.504819
8.782875	667.182204	10.509824
8.715104	682.174984	10.514829
8.735057	677.174331	10.519834
8.592313	676.525035	10.524839
8.362522	679.169279	10.529843
8.703748	675.066418	10.534848
8.833107	683.118837	10.539853
8.934192	682.508655	10.544858
8.981439	679.659330	10.549863
8.814694	688.984206	10.554867
8.921628	685.428344	10.559872
9.309192	694.291482	10.564877
9.090652	690.123146	10.569882
9.239218	686.510016	10.574887
9.232785	685.179336	10.579891
9.218573	687.959116	10.584896
9.138573	691.570027	10.589901
9.280355	693.916097	10.594906
9.254426	684.697735	10.599911
9.216955	683.689739	10.604915
9.329917	688.596617	10.609920
9.417754	688.226333	10.614925
9.269752	694.902527	10.619930
9.628849	688.837558	10.624935
9.465727	705.948640	10.629939
9.564393	691.409279	10.634944
9.672471	702.756607	10.639949
9.928068	712.436971	10.644954
10.282396	710.559707	10.649959
9.829411	707.645752	10.654963
9.958144	699.373872	10.659968
9.716634	695.300261	10.664973
9.642376	699.967669	10.669978
10.136758	704.056014	10.674983
9.820563	722.769908	10.679987
9.945966	717.943790	10.684992
10.024339	721.516107	10.689997
10.196574	724.747076	10.695002
10.445328	727.841770	10.700007
10.316824	724.488500	10.705011
10.404485	718.147564	10.710016
10.836123	719.736980	10.715021
10.472349	720.487791	10.720026
10.502542	713.887505	10.725031
10.243501	725.017930	10.730035
10.458494	725.363988	10.735040
10.195062	729.392405	10.740045
10.529341	737.421166	10.745050
10.555017	733.985012	10.750055
10.343960	738.152080	10.755059
10.537173	729.751894	10.760064
10.622577	738.025822	10.765069
10.753087	732.980933	10.770074
10.822152	738.500474	10.775079
10.786806	735.553196	10.780083
10.681996	728.768817	10.785088
11.018602	751.506405	10.790093
11.386887	754.717977	10.795098
11.024267	736.764298	10.800103
10.726807	751.082064	10.805107
11.289070	750.853064	10.810112
11.252591	767.376851	10.815117
11.147453	768.766993	10.820122
11.225016	766.049426	10.825127
11.282225	767.780017	10.830131
11.329424	763.245184	10.835136
11.454184	772.031058	10.840141
11.291581	773.157505	10.845146
11.768325	772.946325	10.850151
11.581347	777.575058	10.855155
11.936028	770.690564	10.860160
11.849538	773.895640	10.865165
11.736734	769.786127	10.870170
12.076098	768.515360	10.875175
11.725662	774.644068	10.880179
11.587033	775.594302	10.885184
11.878717	776.827988	10.890189
11.448552	771.482117	10.895194
11.757733	775.634602	10.900199
11.766772	773.574562	10.905203
11.849818	777.265695	10.910208
11.537066	779.722077	10.915213
11.723690	795.383049	10.920218
12.216645	801.961630	10.925223
12.106291	804.376999	10.930227
12.482288	798.147251	10.935232
12.224762	806.176858	10.940237
12.353295	801.249521	10.945242
12.643720	796.235219	10.950247
12.470983	808.076028	10.955251
12.742316	793.441047	10.960256
12.595063	798.178236	10.965261
12.648902	806.935238	10.970266
12.605525	793.442885	10.975271
12.611815	802.265668	10.980275
12.933330	802.450571	10.985280
12.838814	804.539149	10.990285
12.840117	805.403420	10.995290
13.158424	802.611018	11.000295
12.677991	810.082800	11.005299
12.942197	806.727312	11.010304
13.122579	804.496971	11.015309
12.953340	806.237971	11.020314
12.856444	807.295128	11.025319
13.190489	816.645138	11.030323
13.279191	801.850806	11.035328
13.433107	808.849489	11.040333
13.049587	812.478916	11.045338
13.186855	808.712960	11.050343
13.294892	811.489170	11.055347
13.241018	807.662434	11.060352
13.358635	806.638891	11.065357
13.296045	810.739866	11.070362
13.594377	811.662156	11.075367
13.085216	810.516343	11.080371
12.973133	809.952178	11.085376
13.119560	822.698659	11.090381
13.363924	838.530957	11.095386
13.713140	837.372178	11.100391
13.895627	844.749265	11.105395
14.069635	841.621600	11.110400
14.074278	835.826161	11.115405
14.116648	824.852867	11.120410
14.536192	838.702785	11.125415
14.041087	831.450811	11.130419
14.294458	814.123657	11.135424
14.141828	811.811071	11.140429
13.994772	814.169576	11.145434
14.589085	813.542323	11.150439
14.021373	809.613030	11.155443
14.336939	803.618638	11.160448
14.353811	813.683807	11.165453
14.093242	815.444809	11.170458
14.104260	822.383526	11.175463
14.028720	836.507007	11.180467
14.844838	844.827812	11.185472
14.519564	842.896134	11.190477
14.643385	853.428908	11.195482
15.319213	849.100477	11.200487
14.885264	836.198862	11.205491
14.577357	818.030448	11.210496
14.532784	815.945647	11.215501
14.070698	830.963545	11.220506
14.472083	835.537601	11.225511
14.734780	851.426374	11.230515
14.605493	841.418017	11.235520
14.433700	844.626680	11.240525
14.687579	848.444460	11.245530
15.013716	847.389505	11.250535
15.267616	862.692435	11.255539
14.896080	853.915725	11.260544
15.223167	865.336937	11.265549
15.052002	871.593235	11.270554
15.809481	867.198695	11.275559
15.379845	863.434397	11.280563
15.049073	854.635698	11.285568
15.236764	859.728369	11.290573
15.385956	876.128070	11.295578
15.476724	866.682752	11.300583
15.229853	871.199019	11.305587
15.658227	871.034816	11.310592
16.107189	872.627594	11.315597
15.556511	876.311747	11.320602
15.845223	874.860580	11.325607
15.470098	877.118857	11.330611
15.573519	876.174322	11.335616
15.765096	872.020489	11.340621
15.690811	883.443427	11.345626
15.923452	873.214707	11.350631
15.674494	882.013009	11.355635
15.665145	883.020425	11.360640
15.650552	885.897015	11.365645
15.760075	896.500164	11.370650
16.153348	896.097639	11.375655
15.837283	905.799954	11.380659
16.235427	906.174614	11.385664
16.640992	903.304866	11.390669
16.521818	902.602572	11.395674
16.572024	906.149762	11.400679
16.054751	909.602802	11.405683
16.224390	910.058482	11.410688
16.284874	912.907600	11.415693
16.461596	901.991743	11.420698
16.496738	905.489806	11.425703
16.095176	920.448860	11.430707
16.230270	909.104743	11.435712
16.511919	915.958023	11.440717
16.666925	928.827462	11.445722
17.268775	922.872756	11.450727
16.701247	919.291954	11.455731
17.154151	905.478759	11.460736
16.921685	910.720062	11.465741
16.730631	906.319194	11.470746
17.155229	912.841254	11.475751
16.825199	920.028356	11.480755
17.360654	925.098528	11.485760
17.710483	928.462116	11.490765
17.174885	916.648383	11.495770
17.393551	900.886285	11.500775
17.100514	909.285189	11.505779
16.939908	898.579538	11.510784
17.379887	910.590503	11.515789
17.696159	925.609250	11.520794
17.651915	923.825166	11.525799
17.379316	911.494242	11.530803
17.452105	917.934520	11.535808
17.785668	921.151290	11.540813
17.443611	921.605492	11.545818
17.409786	922.430003	11.550823
17.398825	931.638315	11.555827
17.839304	937.294378	11.560832
17.882273	934.372713	11.565837
17.975300	935.902183	11.570842
18.147677	929.331902	11.575847
18.282251	939.571576	11.580851
18.043471	933.742837	11.585856
18.002283	932.125595	11.590861
18.218047	936.277957	11.595866
18.490959	929.820701	11.600871
18.150103	926.373532	11.605875
18.268561	911.125181	11.610880
18.431239	902.936584	11.615885
18.088073	914.986298	11.620890
18.306388	914.633112	11.625895
18.334648	929.998479	11.630899
18.456572	935.091003	11.635904
18.956120	933.151316	11.640909
18.484266	925.041104	11.645914
17.915108	909.206441	11.650919
17.934943	914.942906	11.655923
18.031353	927.342788	11.660928
18.542386	931.191893	11.665933
18.202671	926.017169	11.670938
18.450970	941.975608	11.675943
18.444133	958.373332	11.680947
18.858379	961.551804	11.685952
18.938346	957.756558	11.690957
19.001329	963.540511	11.695962
19.019264	955.680254	11.700967
19.168228	962.352225	11.705971
19.178481	958.773404	11.710976
19.285691	961.528467	11.715981
18.941394	967.772250	11.720986
19.146706	966.168005	11.725991
18.859653	963.415812	11.730995
19.093661	961.520465	11.736000
19.131532	968.082802	11.741005
18.898784	965.587745	11.746010
19.424212	964.107037	11.751015
19.099287	975.549330	11.756019
19.516381	977.933898	11.761024
19.818042	983.906673	11.766029
19.736750	988.826426	11.771034
20.227200	982.921587	11.776039
19.793598	965.156260	11.781043
19.631066	967.602705	11.786048
19.547145	962.590954	11.791053
19.602936	968.873509	11.796058
20.187055	965.486821	11.801063
19.882154	979.537257	11.806067
20.202376	978.182125	11.811072
20.265055	971.149845	11.816077
19.824251	975.012156	11.821082
20.119024	965.508907	11.826087
19.928868	971.100212	11.831091
19.919991	982.270034	11.836096
20.122733	988.079376	11.841101
20.356957	995.776874	11.846106
20.478315	988.453868	11.851111
20.501023	993.356581	11.856115
20.323392	990.846938	11.861120
20.455655	996.913499	11.866125
19.914819	995.581259	11.871130
20.556469	998.441671	11.876135
20.276240	1003.742905	11.881139
20.325207	1003.729804	11.886144
20.653180	1001.829789	11.891149
20.506778	1000.469395	11.896154
20.907591	997.935971	11.901159
20.959651	994.037343	11.906163
20.452569	995.466419	11.911168
20.412925	993.269038	11.916173
20.372364	1008.776151	11.921178
21.160152	1004.723352	11.926183
21.188193	1012.103313	11.931187
21.457324	1013.300624	11.936192
21.583864	1007.725800	11.941197
21.230590	996.211536	11.946202
21.098889	985.372974	11.951207
20.891085	993.067310	11.956211
21.144895	1001.483031	11.961216
21.478278	1015.061695	11.966221
21.494103	1015.676777	11.971226
21.415320	1011.836499	11.976231
21.269317	1022.027622	11.981235
21.507478	1015.124710	11.986240
21.575100	1015.960254	11.991245
21.543517	1020.744388	11.996250
21.726453	1009.219101	12.001255
21.590728	1023.191623	12.006259
21.980070	1018.207660	12.011264
21.852718	1008.456627	12.016269
21.977812	1018.828242	12.021274
21.801401	1009.028778	12.026279
21.673207	1002.473683	12.031283
21.983473	1018.448024	12.036288
21.721732	997.492534	12.041293
21.424111	999.550434	12.046298
21.760591	1007.796459	12.051303
21.982984	1015.507443	12.056307
22.151642	1005.301450	12.061312
21.937691	993.195668	12.066317
21.512410	988.409409	12.071322
21.670790	980.658086	12.076327
21.607104	990.094551	12.081331
21.833464	1005.551949	12.086336
22.030620	1003.513310	12.091341
21.763433	995.127576	12.096346
21.929085	983.717771	12.101351
21.744545	989.594698	12.106355
21.701188	989.662953	12.111360
22.051791	984.990378	12.116365
21.505360	981.409891	12.121370
21.836621	984.928649	12.126375
21.686458	981.266800	12.131379
21.891649	985.130461	12.136384
22.072030	990.592323	12.141389
21.450151	991.117397	12.146394
21.692738	981.347165	12.151399
21.821853	990.425706	12.156403
21.575563	990.527570	12.161408
21.836069	994.078197	12.166413
21.843762	1004.775458	12.171418
22.005402	992.885545	12.176423
21.882630	996.671228	12.181427
21.788590	994.193043	12.186432
21.518808	995.018144	12.191437
21.427574	1009.723551	12.196442
22.074269	1011.347575	12.201447
21.846912	1013.955536	12.206451
21.713457	998.256870	12.211456
22.121663	995.722968	12.216461
22.138154	995.330172	12.221466
22.378923	989.756692	12.226471
21.891578	1003.342639	12.231475
21.898137	994.004446	12.236480
22.045890	995.957170	12.241485
21.469360	1002.472098	12.246490
21.715209	991.919327	12.251495
21.820159	1004.019779	12.256499
21.734976	998.518759	12.261504
21.753865	1000.569762	12.266509
21.634588	1004.818664	12.271514
21.810896	1000.137284	12.276519
21.533869	1005.860733	12.281523
21.830142	1003.846942	12.286528
21.976529	997.791087	12.291533
21.676604	1004.458724	12.296538
22.113212	988.324829	12.301543
21.877635	1003.867346	12.306547
22.040255	993.530949	12.311552
21.943167	991.351707	12.316557
21.781282	994.895412	12.321562
21.914884	987.096229	12.326567
21.851431	1000.498182	12.331571
21.823506	998.940239	12.336576
22.123580	999.803822	12.341581
21.513029	997.561035	12.346586
21.692981	990.557587	12.351591
21.936863	997.700799	12.356595
21.638866	996.007582	12.361600
21.714873	996.776161	12.366605
21.822407	1005.121042	12.371610
21.889577	1002.321531	12.376615
21.773695	998.705906	12.381619
22.150653	1002.089333	12.386624
22.007199	986.023314	12.391629
21.772456	988.465564	12.396634
21.801504	974.005374	12.401639
21.740101	980.461580	12.406643
21.557065	979.901284	12.411648
21.796344	978.502398	12.416653
21.559935	977.389938	12.421658
21.645118	979.131546	12.426663
21.742012	987.601005	12.431667
21.757810	1000.574503	12.436672
21.938010	999.273376	12.441677
21.947172	1005.346441	12.446682
21.960524	986.675511	12.451687
21.818504	990.991072	12.456691
21.358333	981.801985	12.461696
21.576558	987.670647	12.466701
21.612814	1006.277083	12.471706
21.995640	1009.726216	12.476711
21.769346	1010.724257	12.481715
21.821917	1007.170537	12.486720
22.017745	1008.265152	12.491725
21.747676	996.568464	12.496730
22.309267	999.971945	12.501735
21.915455	996.450551	12.506739
21.836800	988.576838	12.511744
22.094060	985.368950	12.516749
22.122494	988.635681	12.521754
21.816786	984.868263	12.526759
21.961702	988.720549	12.531763
21.703066	989.454529	12.536768
22.111303	987.034307	12.541773
21.903204	984.937257	12.546778
22.050915	984.394464	12.551783
22.063541	981.698651	12.556787
21.778575	986.815955	12.561792
21.914699	984.153440	12.566797
21.699696	984.199019	12.571802
22.065034	983.113651	12.576807
21.762958	970.965759	12.581811
21.451232	968.640558	12.586816
21.627717	976.487683	12.591821
21.862192	991.645650	12.596826
22.159878	983.971494	12.601831
21.749478	970.392704	12.606835
21.756978	956.109909	12.611840
21.814354	954.553925	12.616845
21.417462	959.219489	12.621850
21.732948	972.561975	12.626855
22.114505	985.132882	12.631859
22.259868	975.191034	12.636864
22.097879	965.293993	12.641869
21.980891	956.156609	12.646874
21.969455	959.206750	12.651879
21.420198	959.589504	12.656883
21.400432	958.626217	12.661888
21.684966	953.442744	12.666893
21.322608	964.808948	12.671898
21.619712	969.213029	12.676903
21.920561	986.337239	12.681907
21.900143	979.323939	12.686912
21.890910	964.798874	12.691917
21.698613	962.753592	12.696922
21.563735	958.808076	12.701927
21.460810	977.790840	12.706931
21.519628	985.086565	12.711936
22.112974	991.083544	12.716941
21.869201	1003.208259	12.721946
22.236263	985.114187	12.726951
22.147242	976.470547	12.731955
21.541964	968.476740	12.736960
21.893350	967.896265	12.741965
21.698341	963.400532	12.746970
21.798333	959.179484	12.751975
21.621236	965.136442	12.756979
21.648946	967.099876	12.761984
22.114461	952.754346	12.766989
21.238875	959.062374	12.771994
21.641582	974.455953	12.776999
21.778847	984.781644	12.782003
21.933950	991.913627	12.787008
22.245628	982.714574	12.792013
21.784380	966.998719	12.797018
22.178134	964.608220	12.802023
22.014436	966.418945	12.807027
21.890560	961.798517	12.812032
22.336804	963.216509	12.817037
21.821546	973.668279	12.822042
22.099971	960.946000	12.827047
22.012265	963.588036	12.832051
21.935898	961.204720	12.837056
21.958071	962.759366	12.842061
22.132501	967.162375	12.847066
21.973874	947.371902	12.852071
21.308347	944.609208	12.857075
21.414793	956.680946	12.862080
21.707102	961.792030	12.867085
21.449615	967.983034	12.872090
21.817090	965.578094	12.877095
21.670939	970.235014	12.882099
21.696854	976.517563	12.887104
21.767928	966.043327	12.892109
21.726995	964.359723	12.897114
21.955192	966.475493	12.902119
21.557636	971.827226	12.907123
21.533785	966.495702	12.912128
22.063514	962.989262	12.917133
21.850070	966.911668	12.922138
21.873994	966.292994	12.927143
22.167504	967.025464	12.932147
21.828342	966.919435	12.937152
21.776254	967.419844	12.942157
21.896675	979.113810	12.947162
21.999097	967.370648	12.952167
21.605012	976.260990	12.957171
21.528374	967.891942	12.962176
21.782204	973.718178	12.967181
21.590204	969.943110	12.972186
21.911238	972.641384	12.977191
21.843484	966.806203	12.982195
21.724114	972.954187	12.987200
21.858113	965.354288	12.992205
21.695053	971.957393	12.997210
21.826619	963.884623	13.002215
21.567070	974.959656	13.007219
21.595516	974.528495	13.012224
21.759923	972.041528	13.017229
21.886571	968.701696	13.022234
22.277316	969.430126	13.027239
22.271981	966.755553	13.032243
21.909463	958.368420	13.037248
21.660971	944.052553	13.042253
21.594711	943.951840	13.047258
21.744625	942.630253	13.052263
21.821039	955.257795	13.057267
21.902939	962.772973	13.062272
21.730340	947.677120	13.067277
21.573268	954.325769	13.072282
21.598546	965.571039	13.077287
21.655507	964.165124	13.082291
21.530630	971.778521	13.087296
21.485103	970.336493	13.092301
21.693027	980.455461	13.097306
22.029691	964.910699	13.102311
21.606930	968.621889	13.107315
21.317653	974.992425	13.112320
21.692347	972.365588	13.117325
21.398131	978.381710	13.122330
21.677001	972.343019	13.127335
21.856337	975.389271	13.132339
21.671222	977.818668	13.137344
21.675002	975.729503	13.142349
21.503185	978.164909	13.147354
21.663911	974.698443	13.152359
21.653750	976.936002	13.157363
21.804904	992.450887	13.162368
22.146875	987.260713	13.167373
21.669391	983.028142	13.172378
21.787821	981.263135	13.177383
21.912539	978.128104	13.182387
21.918839	975.099430	13.187392
21.959807	980.009665	13.192397
21.588947	986.981561	13.197402
21.840714	977.380283	13.202407
21.933161	975.312232	13.207411
21.951762	977.960517	13.212416
22.099569	976.952314	13.217421
21.701866	979.006844	13.222426
22.131659	986.954623	13.227431
21.803945	987.418604	13.232435
21.835518	987.208749	13.237440
22.078103	976.003259	13.242445
21.596609	986.485564	13.247450
21.979156	981.718303	13.252455
22.365485	987.699854	13.257459
21.906338	987.034528	13.262464
22.005974	975.514469	13.267469
21.746352	965.906140	13.272474
21.825690	960.986003	13.277479
21.762161	953.547871	13.282483
21.943059	964.465671	13.287488
21.916259	958.324657	13.292493
21.195500	964.065748	13.297498
21.548040	965.893752	13.302503
21.876597	987.103859	13.307507
21.897408	986.403613	13.312512
22.134947	979.005824	13.317517
21.838398	974.159209	13.322522
21.712789	967.525528	13.327527
21.940807	960.796089	13.332531
22.012116	955.725357	13.337536
22.252119	957.869101	13.342541
22.012561	967.446232	13.347546
21.818041	960.610422	13.352551
21.964283	967.572993	13.357555
21.294120	967.515426	13.362560
21.589706	957.262044	13.367565
21.796907	959.997989	13.372570
21.580342	958.893181	13.377575
21.716257	958.626753	13.382579
21.160046	957.871098	13.387584
21.820268	966.990013	13.392589
21.515811	980.844189	13.397594
21.631213	991.184685	13.402599
21.777634	993.235927	13.407603
21.626260	991.089282	13.412608
21.858056	993.671806	13.417613
21.883613	993.297983	13.422618
21.880313	998.257656	13.427623
21.912797	994.267252	13.432627
22.013080	994.563511	13.437632
21.629298	978.725415	13.442637
21.491014	982.340071	13.447642
21.959442	983.735708	13.452647
21.829097	990.837290	13.457651
21.563096	996.650818	13.462656
22.076531	993.837954	13.467661
21.771707	996.571694	13.472666
21.952536	994.157303	13.477671
21.824580	982.601654	13.482675
21.407340	978.749544	13.487680
21.654161	984.798038	13.492685
21.655602	996.810047	13.497690
22.045936	988.723689	13.502695
22.025560	996.202339	13.507699
21.869000	985.917512	13.512704
22.050298	978.953707	13.517709
21.561240	971.305499	13.522714
21.948519	965.606644	13.527719
21.993128	970.598358	13.532723
21.662155	969.283033	13.537728
21.967405	961.184434	13.542733
21.839647	969.645032	13.547738
21.766384	960.319755	13.552743
22.232978	968.014504	13.557747
21.651558	969.940270	13.562752
21.863124	962.544178	13.567757
21.746294	971.242508	13.572762
21.839648	970.199431	13.577767
22.007466	973.263052	13.582771
21.815871	969.833703	13.587776
22.189136	965.056197	13.592781
21.970562	977.070782	13.597786
22.071974	969.897652	13.602791
22.392496	964.734058	13.607795
21.884405	948.969805	13.612800
22.224919	947.266592	13.617805
21.513505	943.325981	13.622810
21.283914	931.725427	13.627815
21.386272	947.112055	13.632819
21.292238	957.421726	13.637824
22.099472	963.899916	13.642829
21.575797	977.508254	13.647834
21.573191	979.657282	13.652839
21.316003	982.516273	13.657843
21.434704	981.140034	13.662848
21.973436	981.745987	13.667853
21.571683	980.180692	13.672858
21.771813	970.596167	13.677863
22.036893	978.094551	13.682867
21.921052	977.936023	13.687872
22.249348	977.628321	13.692877
21.714266	986.765869	13.697882
21.900886	983.894960	13.702887
22.174315	979.862855	13.707891
21.856822	985.634287	13.712896
22.193642	985.049597	13.717901
21.731649	972.701754	13.722906
21.659605	966.808099	13.727911
21.372063	981.107401	13.732915
21.385800	986.326254	13.737920
22.032129	979.067193	13.742925
21.850381	985.193113	13.747930
21.954846	978.512086	13.752935
22.329615	982.493909	13.757939
22.009863	976.011932	13.762944
21.957353	959.236797	13.767949
21.466480	959.455594	13.772954
21.903340	953.175482	13.777959
21.889091	948.171527	13.782963
22.093086	947.927768	13.787968
21.965595	945.745851	13.792973
21.528662	951.096828	13.797978
21.783824	949.945879	13.802983
21.572992	951.990867	13.807987
21.946133	951.558240	13.812992
21.831353	955.710832	13.817997
21.817087	959.370140	13.823002
22.043439	958.844260	13.828007
21.859401	959.640053	13.833011
21.621733	962.515825	13.838016
21.586024	954.356083	13.843021
21.546533	955.605118	13.848026
21.930275	962.144468	13.853031
21.661460	955.906792	13.858035
21.513063	957.568840	13.863040
22.018683	956.998631	13.868045
21.467009	966.482432	13.873050
21.735207	961.737546	13.878055
21.612284	963.511674	13.883059
21.667204	980.712384	13.888064
22.047302	978.056989	13.893069
21.923060	977.510691	13.898074
21.875655	964.198091	13.903079
22.161633	959.867393	13.908083
22.274788	970.254049	13.913088
21.826674	970.308016	13.918093
21.590078	968.040197	13.923098
21.747044	959.872680	13.928103
21.520854	955.595453	13.933107
21.532463	958.599406	13.938112
21.868148	957.333993	13.943117
21.450940	964.629614	13.948122
21.626147	961.775271	13.953127
21.664774	957.754218	13.958131
21.790051	969.447740	13.963136
22.192163	976.947892	13.968141
22.053326	974.360548	13.973146
22.030964	961.973654	13.978151
22.299827	952.702617	13.983155
21.522626	960.782323	13.988160
22.085051	962.281053	13.993165
21.709400	965.954955	13.998170
21.711910	960.512334	14.003175
21.587042	965.394551	14.008179
21.526619	964.447708	14.013184
21.787539	956.012502	14.018189
21.811454	963.587958	14.023207
21.469974	959.373399	14.028224
21.726711	956.450075	14.033242
21.622508	963.199946	14.038259
21.984038	957.541533	14.043277
21.689256	960.591137	14.048295
21.763538	958.413319	14.053312
21.627784	970.208330	14.058330
21.732845	980.109172	14.063347
21.970160	987.468264	14.068365
22.047637	990.659182	14.073383
22.039471	995.016050	14.078400
22.048337	989.361787	14.083418
21.622377	995.078963	14.088435
21.960427	987.181881	14.093453
22.041325	993.167692	14.098471
22.096920	1000.476051	14.103488
22.109430	1000.151080	14.108506
22.085443	1001.194277	14.113523
22.542312	991.329828	14.118541
22.043636	995.853478	14.123559
22.197595	1002.667379	14.128576
22.259269	992.788397	14.133594
21.933260	991.776135	14.138611
22.313769	996.770353	14.143629
21.958928	991.417835	14.148647
22.071179	994.893364	14.153664
22.300332	998.025599	14.158682
22.086599	1003.681193	14.163699
22.076107	995.924579	14.168717
22.210526	1001.870113	14.173735
21.806375	1005.495998	14.178752
22.029264	991.952887	14.183770
21.993407	1006.515254	14.188787
22.214743	1006.174165	14.193805
22.156858	1014.225268	14.198823
22.404734	1026.325048	14.203840
22.613449	1027.877603	14.208858
22.384429	1021.751084	14.213875
22.862173	1024.773375	14.218893
22.697119	1021.128990	14.223911
22.539538	1023.394002	14.228928
22.721690	1025.625571	14.233946
22.401413	1026.775873	14.238963
22.341240	1022.496529	14.243981
22.745861	1026.858623	14.248999
22.756036	1024.327193	14.254016
22.941845	1019.739908	14.259034
22.755485	1009.927064	14.264051
22.894456	1001.476269	14.269069
22.759698	1001.550984	14.274087
22.566777	1001.358879	14.279104
22.555004	995.384112	14.284122
22.651190	1009.957704	14.289139
22.666651	1020.796049	14.294157
22.724740	1030.867981	14.299175
22.525171	1024.634435	14.304192
22.660293	1024.410497	14.309210
22.353857	1031.074589	14.314227
22.740415	1022.119881	14.319245
22.784832	1030.091244	14.324263
22.941679	1023.275291	14.329280
23.144955	1019.507120	14.334298
22.666618	1024.804121	14.339315
22.764026	1019.177977	14.344333
22.770209	1027.800429	14.349351
22.744544	1023.569110	14.354368
22.941879	1024.494042	14.359386
22.592032	1028.006283	14.364403
23.237412	1023.542581	14.369421
22.877891	1024.481090	14.374439
22.996753	1024.800138	14.379456
22.933941	1029.784148	14.384474
23.051226	1043.025312	14.389491
23.520858	1044.139798	14.394509
23.539831	1035.138649	14.399527
23.252926	1034.865405	14.404544
23.433212	1026.681550	14.409562
23.269614	1033.754650	14.414579
23.076752	1019.113023	14.419597
23.232420	1017.753982	14.424615
23.185597	1018.615649	14.429632
23.103265	1018.553413	14.434650
23.135622	1019.747987	14.439667
23.122394	1029.380536	14.444685
23.435277	1046.695959	14.449703
23.669944	1055.837170	14.454720
23.871521	1029.275817	14.459738
23.757612	1025.680933	14.464755
23.804373	1024.515774	14.469773
23.949462	1020.837900	14.474791
23.548452	1030.707422	14.479808
23.349052	1020.546781	14.484826
23.493422	1034.232934	14.489843
23.175141	1027.092111	14.494861
23.516215	1023.552695	14.499879
23.079947	1028.767675	14.504896
23.121925	1021.128047	14.509914
23.354951	1027.649248	14.514931
23.362916	1034.209433	14.519949
23.441560	1040.420863	14.524967
23.732933	1054.747629	14.529984
23.768408	1051.217685	14.535002
23.800846	1058.193402	14.540019
23.862880	1059.734886	14.545037
23.824274	1047.189390	14.550055
23.497586	1052.306451	14.555072
23.859031	1047.101599	14.560090
23.951121	1054.799032	14.565107
23.975629	1055.918964	14.570125
23.744019	1032.495104	14.575143
23.750748	1039.652005	14.580160
24.211603	1032.369327	14.585178
24.005445	1034.521400	14.590195
23.462569	1020.328788	14.595213
23.939181	1030.016735	14.600231
23.820159	1053.793313	14.605248
24.030267	1052.440292	14.610266
23.953496	1054.959978	14.615283
24.063554	1058.089808	14.620301
24.312831	1054.668100	14.625319
23.927192	1042.363224	14.630336
24.349185	1041.631012	14.635354
24.111479	1026.803350	14.640371
23.609355	1021.866654	14.645389
24.340777	1034.149303	14.650407
24.531880	1040.372163	14.655424
24.416587	1025.311688	14.660442
24.300991	1025.547303	14.665459
24.123047	1025.316800	14.670477
24.341169	1023.308814	14.675495
23.979468	1024.514646	14.680512
24.107575	1020.242789	14.685530
24.057137	1026.899211	14.690547
24.137627	1029.996307	14.695565
24.190116	1042.330795	14.700583
23.954906	1053.718085	14.705600
24.529852	1045.409070	14.710618
24.334717	1054.472777	14.715635
24.375564	1059.874884	14.720653
24.745519	1049.437460	14.725671
24.267400	1051.524738	14.730688
24.197336	1050.105570	14.735706
24.150128	1058.569858	14.740723
24.241787	1053.039970	14.745741
24.154488	1058.268757	14.750759
24.268222	1060.296297	14.755776
24.138882	1051.840292	14.760794
24.193109	1062.338136	14.765811
24.344516	1083.552451	14.770829
24.854267	1079.252943	14.775847
24.514968	1090.710473	14.780864
24.891103	1083.673417	14.785882
24.581982	1083.072066	14.790899
24.654401	1080.687054	14.795917
24.750109	1073.809508	14.800935
24.830003	1076.531883	14.805952
24.874390	1076.571552	14.810970
24.670641	1079.220895	14.815987
24.718874	1077.421178	14.821005
24.750861	1077.740948	14.826023
24.648737	1082.295854	14.831040
25.104154	1071.609098	14.836058
24.964175	1082.941496	14.841075
25.305946	1077.553772	14.846093
25.130500	1074.174956	14.851111
25.116989	1077.534653	14.856128
25.414733	1073.118334	14.861146
25.017061	1064.203958	14.866163
24.790862	1065.764543	14.871181
25.144112	1064.045220	14.876199
24.977481	1081.136177	14.881216
25.136344	1079.407263	14.886234
24.999204	1082.448761	14.891251
24.681544	1085.212918	14.896269
24.932766	1080.601014	14.901287
24.897003	1088.319203	14.906304
25.287389	1081.549018	14.911322
25.198466	1085.089770	14.916339
25.151075	1084.577414	14.921357
25.230769	1078.987358	14.926375
25.334677	1089.840905	14.931392
25.298962	1083.285124	14.936410
25.135985	1091.328693	14.941427
25.110785	1079.053730	14.946445
25.360410	1083.563683	14.951463
24.971980	1083.462582	14.956480
25.037616	1081.621688	14.961498
25.323966	1073.247957	14.966515
25.217874	1078.708730	14.971533
25.578793	1098.079522	14.976551
25.359827	1107.189476	14.981568
25.615442	1104.061182	14.986586
25.427876	1108.992978	14.991603
25.542429	1102.601599	14.996621
25.981879	1100.953326	15.001639
25.743327	1090.276869	15.006656
25.541256	1077.776699	15.011674
25.558237	1081.206373	15.016691
25.576130	1094.744172	15.021709
26.025039	1084.985762	15.026727
25.536602	1085.788884	15.031744
25.782127	1081.514597	15.036762
25.709783	1080.995495	15.041779
25.725185	1086.020841	15.046797
25.952897	1089.271068	15.051815
25.522057	1087.687750	15.056832
25.614223	1084.740252	15.061850
25.659595	1088.712740	15.066867
25.889739	1105.351021	15.071885
26.118832	1107.624558	15.076903
25.680298	1106.371324	15.081920
25.900955	1115.364173	15.086938
26.255659	1106.499137	15.091955
25.678434	1111.151650	15.096973
25.785846	1101.539189	15.101991
25.895117	1109.693977	15.107008
26.015718	1100.360773	15.112026
26.094726	1108.097880	15.117043
25.924938	1107.632100	15.122061
26.339481	1096.973597	15.127079
26.282085	1104.122229	15.132096
26.232428	1101.935716	15.137114
26.204534	1105.389626	15.142131
26.342911	1106.779432	15.147149
26.273563	1101.879936	15.152167
26.004594	1115.268888	15.157184
26.147234	1111.635511	15.162202
26.139395	1101.774284	15.167219
25.856202	1109.432535	15.172237
26.503484	1103.064395	15.177255
26.545282	1111.175629	15.182272
26.381803	1108.170374	15.187290
26.472146	1105.753149	15.192307
26.121071	1109.839680	15.197325
26.206968	1103.308714	15.202343
26.265823	1108.711294	15.207360
26.418774	1107.166082	15.212378
26.543192	1105.612376	15.217395
26.194704	1110.405607	15.222413
26.515165	1106.196425	15.227431
26.472663	1118.061393	15.232448
26.571929	1129.088218	15.237466
26.857276	1137.715629	15.242483
26.840401	1132.609866	15.247501
27.114288	1117.277049	15.252519
26.540725	1109.357448	15.257536
26.273129	1109.019470	15.262554
26.842280	1107.908453	15.267571
26.925573	1109.312035	15.272589
26.759242	1099.937861	15.277607
26.821827	1102.561232	15.282624
26.731755	1100.341488	15.287642
26.893448	1106.134736	15.292659
26.848427	1113.677739	15.297677
27.167343	1113.248259	15.302695
27.116923	1117.483262	15.307712
26.871752	1110.928338	15.312730
27.107023	1104.801716	15.317747
26.780258	1100.932655	15.322765
26.876156	1109.404327	15.327783
26.928473	1109.874955	15.332800
26.638745	1129.347497	15.337818
27.184373	1125.426503	15.342835
27.100359	1135.567358	15.347853
27.233965	1135.252333	15.352871
26.841750	1137.686340	15.357888
26.787391	1138.318184	15.362906
27.079734	1130.123330	15.367923
26.719626	1139.117332	15.372941
27.126725	1137.827387	15.377959
27.019427	1131.711059	15.382976
27.095136	1132.637951	15.387994
27.335275	1137.006228	15.393011
26.906273	1133.750405	15.398029
27.182933	1151.393441	15.403047
27.441364	1162.032340	15.408064
27.568136	1168.241082	15.413082
27.909677	1156.988310	15.418099
27.389933	1144.904393	15.423117
27.315420	1137.459498	15.428135
27.700963	1133.888416	15.433152
27.398870	1137.310597	15.438170
27.465909	1135.898232	15.443187
27.183812	1147.955495	15.448205
27.687263	1149.064978	15.453223
27.811388	1150.669454	15.458240
27.804792	1147.062443	15.463258
27.967812	1140.794639	15.468275
27.609964	1139.660650	15.473293
27.442433	1143.112916	15.478311
27.410508	1138.472762	15.483328
27.474988	1158.328741	15.488346
27.871012	1155.950839	15.493363
27.524907	1168.458105	15.498381
28.034987	1164.630999	15.503399
28.120604	1174.799494	15.508416
27.939659	1171.770841	15.513434
28.151064	1161.758197	15.518451
27.785451	1154.199804	15.523469
27.738314	1148.035750	15.528487
28.496777	1152.562823	15.533504
27.681166	1145.194982	15.538522
27.763389	1149.496628	15.543539
27.795974	1156.409366	15.548557
27.931710	1162.601213	15.553575
28.024286	1159.353999	15.558592
27.865942	1167.555094	15.563610
27.880705	1156.476075	15.568627
27.947343	1164.926808	15.573645
28.083414	1169.014880	15.578663
27.856685	1163.235972	15.583680
28.076554	1164.651579	15.588698
28.337353	1167.396501	15.593715
27.916941	1162.768217	15.598733
27.974187	1169.173934	15.603751
28.758993	1180.699454	15.608768
28.176219	1178.111378	15.613786
28.661887	1171.225598	15.618803
28.474965	1170.071750	15.623821
28.423071	1168.402979	15.628839
28.451627	1163.231932	15.633856
28.646773	1164.132836	15.638874
28.727914	1160.980504	15.643891
28.460452	1162.667475	15.648909
28.725489	1165.853440	15.653927
29.069462	1156.183456	15.658944
28.541567	1168.091915	15.663962
28.642066	1158.904655	15.668979
28.589931	1171.641861	15.673997
29.093110	1165.192488	15.679015
28.966222	1157.322274	15.684032
28.843047	1168.080546	15.689050
28.660483	1163.035861	15.694067
28.430627	1156.887775	15.699085
28.759098	1162.885934	15.704103
28.826933	1159.790219	15.709120
28.589898	1164.997859	15.714138
28.803616	1158.183122	15.719155
28.682585	1164.894623	15.724173
28.819385	1159.742423	15.729191
28.594258	1159.832239	15.734208
28.715739	1161.614743	15.739226
28.750309	1168.870875	15.744243
28.629742	1169.933398	15.749261
28.906086	1180.081009	15.754279
28.850466	1175.122439	15.759296
29.019627	1181.249502	15.764314
28.948636	1174.849350	15.769331
29.060291	1176.522508	15.774349
28.903125	1181.660156	15.779367
28.976117	1178.568671	15.784384
28.683967	1180.804017	15.789402
28.976850	1181.687772	15.794419
28.808292	1190.045760	15.799437
29.240552	1196.910466	15.804455
29.531807	1204.092682	15.809472
29.521824	1214.711490	15.814490
29.320356	1196.503537	15.819507
29.409677	1193.084026	15.824525
29.088397	1192.864314	15.829543
29.508590	1200.781968	15.834560
29.540164	1199.813511	15.839578
29.820510	1194.006320	15.844595
29.558301	1183.743339	15.849613
29.093225	1185.353159	15.854631
29.566812	1195.022042	15.859648
29.615194	1205.285925	15.864666
29.935110	1196.965827	15.869683
29.973208	1204.141836	15.874701
29.453957	1193.057883	15.879719
29.887916	1189.372967	15.884736
29.509729	1182.510869	15.889754
29.895958	1198.013339	15.894771
29.811635	1187.399356	15.899789
29.498643	1180.203613	15.904807
29.509325	1186.158227	15.909824
29.661503	1199.830588	15.914842
29.798532	1203.267267	15.919859
29.875237	1207.315523	15.924877
29.414361	1207.506393	15.929895
29.975762	1205.868306	15.934912
29.621371	1208.426165	15.939930
29.944318	1209.234682	15.944947
29.917836	1206.239782	15.949965
29.440292	1204.880225	15.954983
29.645719	1198.823256	15.960000
29.794721	1223.209707	15.965018
30.158181	1222.789912	15.970035
30.237307	1234.977059	15.975053
30.306788	1238.323744	15.980071
30.473447	1229.735783	15.985088
30.500517	1232.879483	15.990106
30.755198	1212.191519	15.995123
30.353478	1198.220233	16.000141
30.004803	1201.210613	16.005159
30.645135	1198.854209	16.010176
30.484966	1203.434064	16.015194
30.409923	1194.874568	16.020211
30.606367	1201.790338	16.025229
30.428480	1192.527942	16.030247
30.624377	1194.369745	16.035264
30.681820	1196.648708	16.040282
30.669689	1197.279220	16.045299
30.696373	1196.379324	16.050317
30.510194	1200.000168	16.055335
30.489212	1189.468639	16.060352
30.425997	1201.282493	16.065370
30.451319	1198.457861	16.070387
30.464910	1196.973939	16.075405
30.452148	1201.912017	16.080423
30.556134	1196.536278	16.085440
30.330935	1197.050945	16.090458
30.807769	1217.122547	16.095475
31.008022	1226.245348	16.100493
31.324002	1223.574440	16.105511
31.110250	1208.657844	16.110528
31.020540	1207.801134	16.115546
31.071597	1198.055743	16.120563
30.671658	1199.256331	16.125581
30.494675	1196.761686	16.130599
30.545786	1200.656047	16.135616
30.607799	1215.317980	16.140634
30.811254	1225.173760	16.145651
31.259330	1227.710191	16.150669
30.868560	1237.355626	16.155687
30.775037	1228.872515	16.160704
30.996010	1228.781901	16.165722
31.188854	1234.770268	16.170739
30.951950	1232.914292	16.175757
30.573055	1233.821879	16.180775
31.230471	1238.453318	16.185792
31.062907	1251.045797	16.190810
31.626489	1254.567244	16.195827
31.827390	1259.040717	16.200845
31.364512	1249.811399	16.205863
31.643785	1229.999589	16.210880
31.499299	1221.505927	16.215898
30.961839	1223.642380	16.220915
31.279872	1229.987267	16.225933
31.465532	1241.276943	16.230951
31.697276	1242.418056	16.235968
31.288268	1255.283057	16.240986
31.322271	1250.794573	16.246003
31.593088	1248.740120	16.251021
31.575036	1251.799425	16.256039
31.861989	1255.293490	16.261056
31.680310	1249.381618	16.266074
31.781964	1247.701475	16.271091
31.863365	1248.943962	16.276109
31.829445	1253.388396	16.281127
31.897642	1251.660046	16.286144
31.943895	1251.747431	16.291162
31.967368	1252.682893	16.296179
31.949700	1249.096656	16.301197
31.754536	1262.499066	16.306215
31.949750	1250.857498	16.311232
31.508848	1253.807002	16.316250
31.847709	1253.167782	16.321267
32.091226	1254.820309	16.326285
31.724804	1258.846512	16.331303
31.758249	1248.183161	16.336320
31.925537	1250.292104	16.341338
31.881131	1258.497335	16.346355
31.999428	1250.908295	16.351373
31.710247	1246.562238	16.356391
31.834589	1264.437047	16.361408
32.349370	1270.739163	16.366426
32.618729	1278.235433	16.371443
32.500384	1259.971025	16.376461
32.303152	1276.187441	16.381479
32.983052	1262.877581	16.386496
32.814351	1249.425403	16.391514
32.161855	1245.390872	16.396531
32.694838	1239.913217	16.401549
32.621259	1248.441190	16.406567
32.542622	1237.187559	16.411584
32.531110	1240.229992	16.416602
32.577320	1248.041696	16.421619
32.576126	1244.386487	16.426637
32.462548	1246.184891	16.431655
32.346430	1237.949766	16.436672
32.539593	1239.947569	16.441690
32.401265	1246.375036	16.446707
32.486749	1250.208788	16.451725
32.554720	1266.694321	16.456743
32.824078	1269.405508	16.461760
32.825717	1270.713251	16.466778
32.562292	1269.305165	16.471795
32.881605	1268.448410	16.476813
33.012408	1272.865395	16.481831
32.953758	1266.592235	16.486848
32.732721	1267.657028	16.491866
32.721893	1277.003073	16.496883
33.054475	1270.084435	16.501901
32.951970	1274.092562	16.506919
32.750123	1271.291509	16.511936
32.784403	1270.690727	16.516954
32.785423	1269.904686	16.521971
33.268262	1291.100259	16.526989
32.997912	1295.396641	16.532007
33.171528	1298.930622	16.537024
33.305610	1298.220594	16.542042
33.163766	1302.156331	16.547059
33.421931	1292.628152	16.552077
33.463106	1297.219580	16.557095
33.380388	1295.021385	16.562112
33.362260	1298.194896	16.567130
33.106210	1298.376636	16.572147
33.496346	1288.186404	16.577165
33.473777	1296.333969	16.582183
33.533635	1295.433499	16.587200
33.697716	1299.214019	16.592218
33.508178	1302.014126	16.597235
34.077832	1289.168857	16.602253
33.982874	1294.186417	16.607271
33.784222	1274.575399	16.612288
33.883287	1272.351552	16.617306
33.857744	1261.549866	16.622323
34.045782	1261.902339	16.627341
33.663353	1267.357402	16.632359
34.109164	1259.453914	16.637376
34.152416	1262.653119	16.642394
33.943456	1267.913465	16.647411
33.662925	1265.137322	16.652429
33.648833	1261.717413	16.657447
34.004055	1258.634223	16.662464
33.678142	1267.015293	16.667482
33.564943	1266.163788	16.672499
33.676462	1274.907701	16.677517
33.699607	1280.648383	16.682535
33.756605	1285.358760	16.687552
33.800426	1297.427982	16.692570
33.622907	1301.006809	16.697587
34.110634	1295.492797	16.702605
33.931631	1299.404980	16.707623
33.816379	1312.194464	16.712640
33.929706	1315.964791	16.717658
33.897043	1327.600257	16.722675
34.303351	1319.396003	16.727693
34.461702	1323.400761	16.732711
34.261841	1320.780478	16.737728
34.863832	1310.958672	16.742746
34.439409	1315.894917	16.747763
34.361783	1318.904602	16.752781
34.454571	1325.554313	16.757799
34.442582	1318.628583	16.762816
34.565401	1317.912217	16.767834
34.418521	1321.499183	16.772851
34.657608	1320.775088	16.777869
34.661688	1321.096892	16.782887
34.850810	1320.445937	16.787904
34.824349	1311.513841	16.792922
34.713153	1323.102920	16.797939
34.845286	1314.816923	16.802957
35.070074	1319.962760	16.807975
35.333943	1312.488115	16.812992
35.430685	1316.817243	16.818010
35.236995	1323.831454	16.823027
35.150479	1317.492965	16.828045
35.144011	1315.765597	16.833063
35.060470	1310.505049	16.838080
34.933962	1299.660011	16.843098
34.665535	1316.198153	16.848115
34.875986	1314.184752	16.853133
34.970599	1317.112540	16.858151
34.681497	1318.223654	16.863168
34.897353	1314.084325	16.868186
34.450825	1324.908380	16.873203
34.803080	1322.971463	16.878221
34.913040	1347.961710	16.883239
34.984894	1348.353004	16.888256
35.450649	1347.894801	16.893274
35.806621	1351.977506	16.898291
35.923508	1346.207340	16.903309
35.698387	1343.721318	16.908327
36.049193	1343.025710	16.913344
35.637024	1318.540539	16.918362
35.414170	1316.927443	16.923379
35.427502	1312.803149	16.928397
35.589002	1316.827840	16.933415
35.219207	1333.132962	16.938432
35.762044	1336.832805	16.943450
35.736242	1342.697267	16.948467
35.804533	1343.861293	16.953485
36.095231	1339.140174	16.958503
35.800124	1334.348608	16.963520
35.828957	1332.268303	16.968538
35.415868	1343.961524	16.973555
35.742475	1346.742051	16.978573
35.597983	1345.273406	16.983591
35.488293	1343.411749	16.988608
35.586409	1339.754454	16.993626
35.411828	1353.398319	16.998643
35.756038	1351.209210	17.003661
36.445458	1367.693825	17.008679
36.161474	1364.238663	17.013696
36.350502	1353.840325	17.018714
36.062318	1357.864558	17.023731
36.146069	1352.040223	17.028749
36.375880	1363.778367	17.033767
35.940282	1371.119928	17.038784
36.494005	1357.211876	17.043802
36.422282	1369.945909	17.048819
36.350310	1359.762017	17.053837
36.465701	1368.067480	17.058855
36.403277	1361.446076	17.063872
36.345516	1363.557001	17.068890
35.996400	1369.590302	17.073907
36.224365	1359.554218	17.078925
36.582401	1366.894369	17.083943
36.565349	1365.566093	17.088960
36.762982	1355.691920	17.093978
36.607284	1355.244585	17.098995
36.570063	1351.284868	17.104013
36.848873	1362.184610	17.109031
36.524143	1363.819603	17.114048
36.531683	1364.961760	17.119066
36.588897	1368.228678	17.124083
36.618469	1363.115270	17.129101
36.551558	1362.655075	17.134119
36.856051	1382.508776	17.139136
37.311397	1389.531044	17.144154
36.961980	1379.263985	17.149171
36.887044	1369.898391	17.154189
37.249739	1377.522815	17.159207
36.976858	1370.167729	17.164224
37.050987	1376.846254	17.169242
37.076212	1393.637311	17.174259
37.570502	1396.066625	17.179277
37.409347	1373.568848	17.184295
37.046904	1381.281767	17.189312
37.550197	1369.590441	17.194330
37.450922	1374.923759	17.199347
36.686812	1369.398340	17.204365
36.765311	1385.732572	17.209383
36.752589	1389.810383	17.214400
37.007766	1397.424114	17.219418
36.829736	1402.889459	17.224435
36.828982	1411.651516	17.229453
37.567563	1417.164853	17.234471
37.442148	1434.818085	17.239488
37.552644	1430.117203	17.244506
37.733694	1432.925064	17.249523
37.834082	1433.966259	17.254541
38.204632	1424.106496	17.259559
37.912753	1427.343111	17.264576
37.999031	1426.944847	17.269594
38.125601	1427.889418	17.274611
37.933210	1427.664929	17.279629
38.029888	1422.519522	17.284647
37.911771	1429.273554	17.289664
37.839964	1422.668301	17.294682
38.047289	1424.918450	17.299699
37.831402	1425.509882	17.304717
38.038696	1429.722440	17.309735
37.927878	1435.470791	17.314752
38.136418	1431.891403	17.319770
37.849327	1442.234614	17.324787
38.056558	1438.245958	17.329805
37.958845	1438.339128	17.334823
38.122381	1434.175663	17.339840
38.106842	1429.916117	17.344858
38.105664	1431.342085	17.349875
38.074809	1430.024832	17.354893
38.358980	1429.613902	17.359911
38.099236	1435.540164	17.364928
38.574108	1454.788704	17.369946
38.764669	1458.984452	17.374963
38.295974	1456.945725	17.379981
38.478751	1450.755127	17.384999
38.431698	1469.830543	17.390016
38.801172	1468.145801	17.395034
38.647869	1465.502549	17.400051
38.596404	1465.253898	17.405069
39.056791	1460.176844	17.410087
38.499949	1465.953639	17.415104
38.825069	1459.828013	17.420122
38.489714	1460.959273	17.425139
38.646429	1463.939833	17.430157
39.158435	1458.681865	17.435175
38.658434	1465.458861	17.440192
39.080414	1463.046540	17.445210
39.146939	1460.026589	17.450227
39.460284	1462.326684	17.455245
39.241188	1461.713818	17.460263
39.140375	1459.323012	17.465280
39.054415	1455.650001	17.470298
39.141327	1453.654614	17.475315
38.687323	1460.947398	17.480333
39.040436	1456.927033	17.485351
39.261115	1454.424410	17.490368
39.382505	1459.389575	17.495386
39.392050	1459.089514	17.500403
39.297879	1467.059267	17.505421
39.374276	1457.379457	17.510439
39.035160	1462.133782	17.515456
39.108386	1460.927829	17.520474
39.440900	1472.481895	17.525491
39.552745	1486.642968	17.530509
39.493956	1480.894997	17.535527
39.499789	1492.123944	17.540544
39.426005	1481.490630	17.545562
39.408844	1481.283740	17.550579
39.489774	1484.681669	17.555597
39.857659	1481.418688	17.560615
39.641002	1488.757809	17.565632
39.681844	1477.259875	17.570650
39.616315	1479.011874	17.575667
39.337792	1494.879424	17.580685
40.139006	1499.974924	17.585703
39.995771	1512.392164	17.590720
40.095934	1513.297168	17.595738
40.134185	1505.885132	17.600755
40.375350	1508.727980	17.605773
40.406842	1501.663204	17.610791
40.140161	1509.160927	17.615808
40.365841	1509.295907	17.620826
40.290889	1504.421264	17.625843
40.347039	1501.643659	17.630861
40.158454	1483.202036	17.635879
40.176569	1495.609318	17.640896
40.446197	1502.397308	17.645914
40.554447	1493.922771	17.650931
40.391280	1505.742966	17.655949
40.311529	1501.596782	17.660967
40.239764	1509.287096	17.665984
41.023328	1506.345010	17.671002
40.908510	1499.640788	17.676019
40.812212	1510.513203	17.681037
41.022029	1499.899371	17.686055
40.764367	1491.335586	17.691072
40.474444	1473.092076	17.696090
40.635207	1487.494790	17.701107
40.645478	1499.498259	17.706125
40.811784	1495.449670	17.711143
40.523807	1505.053232	17.716160
40.508320	1501.193306	17.721178
40.766199	1498.977636	17.726195
40.333950	1506.812438	17.731213
40.891564	1500.115777	17.736231
41.003368	1524.073991	17.741248
41.348650	1520.117165	17.746266
41.498413	1523.900982	17.751283
40.981713	1518.950480	17.756301
41.384165	1521.719610	17.761319
41.200168	1532.387762	17.766336
40.933301	1524.368508	17.771354
41.350764	1524.978142	17.776371
41.301637	1533.790692	17.781389
41.246342	1525.940304	17.786407
41.401139	1523.373761	17.791424
41.431817	1526.638174	17.796442
41.689528	1522.285293	17.801459
41.281523	1520.510197	17.806477
41.588555	1518.977903	17.811495
41.388492	1526.702034	17.816512
41.199511	1526.571456	17.821530
41.584260	1522.336180	17.826547
41.449191	1545.198836	17.831565
41.894918	1556.442578	17.836583
41.864401	1555.089032	17.841600
41.770383	1564.102229	17.846618
41.922509	1554.253058	17.851635
41.996520	1559.678790	17.856653
42.099133	1557.991755	17.861671
42.044960	1559.450052	17.866688
41.866857	1554.804518	17.871706
42.228051	1556.739692	17.876723
42.075904	1554.734091	17.881741
42.255586	1557.867048	17.886759
42.304176	1556.331811	17.891776
42.116528	1555.776155	17.896794
42.172255	1549.012354	17.901811
42.246182	1552.810362	17.906829
42.425976	1545.880787	17.911847
42.403429	1558.302177	17.916864
42.374073	1552.957446	17.921882
42.775085	1546.743963	17.926899
42.686701	1559.984998	17.931917
42.825748	1560.539207	17.936935
42.524221	1558.754119	17.941952
42.593790	1554.316150	17.946970
42.590603	1557.030804	17.951987
42.270186	1558.497341	17.957005
42.661916	1552.463813	17.962023
42.544065	1553.067578	17.967040
42.453029	1559.635508	17.972058
42.932467	1545.496693	17.977075
42.596149	1558.766059	17.982093
42.743049	1560.507634	17.987111
42.928787	1571.858567	17.992128
42.917603	1569.936288	17.997146
43.234159	1570.732929	18.002163
43.117074	1578.790928	18.007181
43.237653	1567.276895	18.012199
43.230978	1576.075103	18.017216
43.501827	1573.042542	18.022234
43.496536	1568.893418	18.027251
43.122723	1568.122801	18.032269
43.176930	1559.993358	18.037287
43.630333	1564.878009	18.042304
43.279096	1570.752678	18.047322
43.347785	1566.051441	18.052339
43.477020	1575.409482	18.057357
43.482055	1569.976950	18.062375
43.552247	1567.146921	18.067392
43.796133	1576.087231	18.072410
44.172498	1571.798255	18.077427
43.625302	1574.902275	18.082445
43.431724	1572.478532	18.087463
43.725388	1563.601655	18.092480
43.025351	1575.045392	18.097498
43.550390	1576.070885	18.102515
43.308155	1571.572970	18.107533
43.835064	1577.105726	18.112551
43.908951	1593.093291	18.117568
43.858368	1609.378227	18.122586
44.110716	1600.550150	18.127603
43.876405	1608.299880	18.132621
44.099558	1612.431413	18.137639
44.238262	1608.879708	18.142656
43.656593	1612.035321	18.147674
43.955122	1602.809518	18.152691
43.821579	1608.517335	18.157709
44.132416	1601.545976	18.162727
44.395134	1609.718817	18.167744
44.031204	1610.727413	18.172762
44.357349	1618.540920	18.177779
44.479120	1632.028695	18.182797
44.604797	1628.907614	18.187815
44.788546	1627.159412	18.192832
44.673891	1631.693788	18.197850
44.802868	1625.327678	18.202867
44.957682	1628.325133	18.207885
44.763474	1617.917514	18.212903
44.822334	1602.259630	18.217920
44.597958	1603.572682	18.222938
44.990598	1599.040724	18.227955
44.668529	1603.162570	18.232973
44.919238	1622.191847	18.237991
45.553617	1622.557581	18.243008
45.411404	1611.877241	18.248026
45.700403	1604.808825	18.253043
45.316248	1590.977496	18.258061
45.237617	1590.875642	18.263079
45.155795	1588.906016	18.268096
44.869533	1591.113241	18.273114
45.190566	1585.931678	18.278131
44.986281	1587.760240	18.283149
44.949102	1590.277162	18.288167
45.045709	1600.244422	18.293184
45.057678	1613.824636	18.298202
45.251687	1614.085140	18.303219
44.984569	1616.806467	18.308237
44.963682	1614.904746	18.313255
45.201721	1617.387480	18.318272
45.301239	1638.264558	18.323290
45.727166	1644.417476	18.328307
45.493762	1646.641633	18.333325
45.631997	1652.099304	18.338343
45.725996	1652.455310	18.343360
45.640025	1647.676616	18.348378
45.819172	1649.711525	18.353395
45.937918	1644.647312	18.358413
45.850178	1642.388503	18.363431
46.034564	1639.516834	18.368448
46.008457	1646.161866	18.373466
46.145525	1640.784241	18.378483
46.286234	1637.547183	18.383501
46.326038	1642.784691	18.388519
46.309440	1645.553240	18.393536
46.343513	1648.144185	18.398554
46.205815	1639.717643	18.403571
46.362067	1647.719759	18.408589
45.937748	1649.901049	18.413607
46.305424	1641.709946	18.418624
46.181054	1658.567884	18.423642
46.503566	1668.702386	18.428659
46.914980	1668.125919	18.433677
46.598709	1671.754212	18.438695
46.860297	1669.837130	18.443712
46.707002	1662.702375	18.448730
47.056007	1647.855825	18.453747
46.672190	1649.146605	18.458765
46.659696	1644.740004	18.463783
46.734885	1640.884578	18.468800
46.810140	1661.183496	18.473818
46.918845	1660.163594	18.478835
47.114059	1660.834569	18.483853
46.976387	1665.613480	18.488871
47.407092	1664.054064	18.493888
46.690534	1665.721614	18.498906
46.996002	1655.563380	18.503923
46.895180	1663.072115	18.508941
46.731648	1668.894557	18.513959
46.838407	1660.131176	18.518976
46.725404	1671.895253	18.523994
47.005725	1673.669090	18.529011
47.221128	1688.910359	18.534029
47.369596	1692.749959	18.539047
47.567895	1694.013390	18.544064
47.380418	1694.306618	18.549082
47.597159	1696.192552	18.554099
47.675644	1701.864052	18.559117
47.406149	1702.118974	18.564135
47.603095	1697.134260	18.569152
47.332448	1694.825297	18.574170
47.597196	1692.908458	18.579187
47.566021	1689.838276	18.584205
47.771335	1709.197921	18.589223
48.183405	1714.014501	18.594240
48.482180	1717.672413	18.599258
48.437839	1701.359602	18.604275
48.379880	1692.912666	18.609293
47.902711	1691.065539	18.614311
48.596029	1686.082747	18.619328
48.235882	1692.196023	18.624346
47.986904	1690.564528	18.629363
48.387210	1687.197510	18.634381
47.966602	1691.248074	18.639399
48.057032	1689.513108	18.644416
47.515169	1705.581943	18.649434
47.954456	1711.768035	18.654451
48.236819	1716.514322	18.659469
48.126332	1721.592563	18.664487
48.576042	1717.252779	18.669504
48.385858	1727.230702	18.674522
48.654745	1736.919271	18.679539
48.884257	1741.957339	18.684557
49.037648	1745.361409	18.689575
49.275544	1732.430121	18.694592
48.858843	1717.153297	18.699610
49.083812	1711.362498	18.704627
49.008382	1704.971945	18.709645
48.980049	1710.520013	18.714663
49.215513	1703.189439	18.719680
48.652961	1710.069007	18.724698
48.853235	1709.618118	18.729715
49.569510	1717.093103	18.734733
49.339354	1730.664924	18.739751
49.587494	1714.342118	18.744768
49.571443	1713.409750	18.749786
49.259607	1704.725986	18.754803
49.303196	1701.835525	18.759821
49.118183	1714.669192	18.764839
49.323648	1714.333568	18.769856
49.472630	1730.162711	18.774874
49.379026	1735.510535	18.779891
49.532014	1732.663526	18.784909
49.541066	1743.803902	18.789927
49.783790	1738.718796	18.794944
49.640832	1734.269176	18.799962
49.746610	1735.292930	18.804979
50.011390	1737.641950	18.809997
49.539783	1740.925192	18.815015
49.845236	1743.563338	18.820032
49.550275	1742.822111	18.825050
49.554574	1733.078891	18.830067
50.003097	1749.853277	18.835085
49.847891	1771.939306	18.840103
50.076184	1768.294244	18.845120
50.046712	1772.695537	18.850138
49.722054	1770.034755	18.855155
50.432905	1765.625774	18.860173
50.133077	1765.236605	18.865191
50.273844	1761.278557	18.870208
50.300517	1755.773344	18.875226
50.722222	1766.587840	18.880243
50.628660	1759.423113	18.885261
50.797993	1766.920231	18.890279
50.658437	1761.783321	18.895296
50.498742	1767.051531	18.900314
50.266682	1774.888762	18.905331
50.901384	1781.816672	18.910349
50.744966	1793.610333	18.915367
51.025897	1786.810576	18.920384
50.924952	1793.544889	18.925402
50.862835	1799.695311	18.930419
51.114143	1787.192835	18.935437
51.176516	1789.513564	18.940455
51.345705	1785.420700	18.945472
51.062224	1792.973807	18.950490
51.303117	1788.113437	18.955507
51.544935	1781.692874	18.960525
51.169214	1787.296196	18.965543
51.430168	1789.701004	18.970560
51.689295	1792.322295	18.975578
51.194393	1797.700747	18.980595
51.463633	1792.498466	18.985613
51.406578	1794.170297	18.990631
51.538508	1788.283990	18.995648
51.292069	1781.682143	19.000666
51.584945	1785.189883	19.005683
51.827927	1775.888058	19.010701
51.491569	1785.044912	19.015719
51.475329	1789.664441	19.020736
51.693751	1782.947065	19.025754
51.435269	1780.387547	19.030771
51.825063	1796.948008	19.035789
51.748700	1809.203212	19.040807
51.993411	1804.943833	19.045824
52.034274	1819.429228	19.050842
51.747521	1807.841528	19.055859
51.761872	1815.899559	19.060877
51.724222	1817.053040	19.065895
52.056637	1808.528877	19.070912
52.305712	1819.039500	19.075930
52.317844	1830.460154	19.080947
52.507550	1827.039831	19.085965
52.524976	1828.684328	19.090983
52.759024	1823.665651	19.096000
52.853851	1829.155633	19.101018
52.808280	1828.587027	19.106035
53.430808	1805.143142	19.111053
53.163313	1797.565642	19.116071
53.438938	1790.832548	19.121088
53.181628	1789.526133	19.126106
53.135646	1793.249470	19.131123
53.295705	1788.471077	19.136141
52.972283	1792.544379	19.141159
52.787262	1798.523329	19.146176
53.274204	1794.600816	19.151194
53.273802	1798.044259	19.156211
53.389539	1798.183917	19.161229
53.092878	1800.647315	19.166247
53.319750	1787.033928	19.171264
53.301741	1788.428952	19.176282
53.486481	1793.332176	19.181299
53.372044	1793.537283	19.186317
52.942533	1797.494506	19.191335
52.950695	1793.227647	19.196352
53.092874	1794.316434	19.201370
53.024774	1805.540169	19.206387
53.446286	1817.775384	19.211405
53.053703	1823.707241	19.216423
53.210290	1824.987678	19.221440
53.743653	1822.544002	19.226458
53.653032	1819.059917	19.231475
53.745261	1833.753870	19.236493
53.760178	1848.934773	19.241511
53.682672	1851.430694	19.246528
54.143414	1841.249657	19.251546
53.838641	1847.545256	19.256563
53.906184	1843.628879	19.261581
53.902305	1852.180275	19.266599
54.088184	1846.740267	19.271616
54.182074	1839.449652	19.276634
54.093006	1848.134170	19.281651
54.467593	1855.669379	19.286669
54.998272	1860.330613	19.291687
54.982463	1851.051850	19.296704
55.079896	1839.190753	19.301722
54.642039	1837.115973	19.306739
54.698363	1825.144596	19.311757
54.603684	1824.456834	19.316775
54.610637	1833.990345	19.321792
54.802800	1830.521169	19.326810
54.860883	1836.949068	19.331827
54.663052	1827.066011	19.336845
54.439946	1830.584655	19.341863
54.701033	1851.466211	19.346880
55.331295	1853.497045	19.351898
55.105004	1864.551461	19.356915
55.077949	1859.386963	19.361933
55.145049	1867.791928	19.366951
55.203210	1867.719776	19.371968
55.474492	1868.209588	19.376986
55.225437	1869.072897	19.382003
55.359071	1860.289834	19.387021
55.508964	1854.481141	19.392039
55.599123	1853.323837	19.397056
55.811592	1860.100915	19.402074
55.241388	1861.943811	19.407091
55.362992	1856.388425	19.412109
55.525482	1857.983642	19.417127
55.380269	1861.731096	19.422144
55.725487	1871.319643	19.427162
55.729770	1876.599938	19.432179
55.797391	1886.611333	19.437197
55.815969	1883.957441	19.442215
56.023055	1888.199297	19.447232
56.057009	1885.547100	19.452250
55.880937	1893.121215	19.457267
56.039662	1892.442375	19.462285
55.821299	1882.867567	19.467303
55.718045	1896.128761	19.472320
56.433410	1899.918865	19.477338
56.477748	1912.014855	19.482355
56.887643	1914.733957	19.487373
56.953566	1918.701165	19.492391
56.383045	1903.942720	19.497408
56.990075	1901.127695	19.502426
56.677074	1906.474997	19.507443
56.772921	1895.423684	19.512461
56.895611	1899.394937	19.517479
56.446875	1904.540677	19.522496
56.857171	1913.355394	19.527514
56.755167	1916.581999	19.532531
57.405962	1917.994673	19.537549
56.943979	1920.866798	19.542567
56.907805	1923.294219	19.547584
57.565643	1916.430181	19.552602
57.061837	1924.741692	19.557619
57.075565	1926.723098	19.562637
57.028517	1921.209203	19.567655
57.184472	1929.835614	19.572672
57.309664	1918.048055	19.577690
56.955910	1917.160185	19.582707
56.936259	1923.436070	19.587725
57.053195	1931.179290	19.592743
57.230080	1935.382237	19.597760
58.081491	1928.863797	19.602778
57.945441	1942.980372	19.607795
57.985694	1944.669400	19.612813
57.750291	1938.725131	19.617831
57.621985	1939.832738	19.622848
57.797073	1942.131016	19.627866
57.923702	1937.422885	19.632883
57.790603	1933.823599	19.637901
57.689819	1935.999071	19.642919
57.450338	1944.693285	19.647936
58.070831	1950.209739	19.652954
58.182961	1966.194279	19.657971
58.011283	1973.650341	19.662989
58.215430	1967.029441	19.668007
58.383713	1968.309460	19.673024
58.627180	1967.385348	19.678042
58.373915	1966.321564	19.683059
58.553601	1958.941371	19.688077
58.528779	1964.116042	19.693095
58.453743	1969.090633	19.698112
58.742068	1971.373439	19.703130
58.513042	1987.683456	19.708147
58.942597	1995.093545	19.713165
59.092077	1990.073564	19.718183
59.278835	1996.556644	19.723200
59.434182	1992.383804	19.728218
59.454077	1983.584734	19.733235
59.345345	1967.481531	19.738253
58.729376	1959.970389	19.743271
58.941460	1971.488379	19.748288
59.261842	1979.779894	19.753306
59.302870	1989.391134	19.758323
59.501440	1986.595327	19.763341
59.289417	1979.215343	19.768359
59.299280	1986.893077	19.773376
59.178333	1977.168028	19.778394
59.341598	1988.127000	19.783411
59.291139	1988.579051	19.788429
59.685404	1992.328546	19.793447
59.725873	2003.425527	19.798464
60.028682	2011.056594	19.803482
59.836018	2018.709215	19.808499
60.055337	2011.925043	19.813517
60.753249	2017.451479	19.818535
60.369985	2013.867107	19.823552
60.225291	1994.479035	19.828570
60.077520	1984.860956	19.833587
60.081797	1980.256083	19.838605
59.928234	1998.723154	19.843623
59.772936	2006.253599	19.848640
60.189057	2008.489301	19.853658
59.726955	2002.435428	19.858675
59.943119	2012.399780	19.863693
60.508426	2028.135799	19.868711
60.277920	2040.141588	19.873728
60.805904	2041.254812	19.878746
60.476913	2037.305962	19.883763
61.070034	2034.362965	19.888781
61.058874	2027.932517	19.893799
61.201378	2031.251497	19.898816
61.729717	2036.458145	19.903834
61.724539	2025.911924	19.908851
61.407218	2015.929532	19.913869
61.781538	1996.445388	19.918887
61.359124	2003.979889	19.923904
60.761409	1995.930487	19.928922
60.934175	2000.477118	19.933939
61.000185	1997.930445	19.938957
61.318857	2010.414972	19.943975
60.879471	2022.281730	19.948992
61.330711	2020.942020	19.954010
61.140526	2028.986008	19.959027
61.193099	2027.489418	19.964045
61.364693	2044.024551	19.969063
61.733323	2053.109520	19.974080
61.678671	2056.243378	19.979098
62.038090	2057.900930	19.984115
62.191517	2057.278511	19.989133
62.454056	2053.796827	19.994151
62.168264	2057.481801	19.999168
62.332393	2048.305949	20.004186
62.694285	2056.432492	20.009203
62.272148	2063.064090	20.014221
62.070664	2053.596142	20.019239
62.032155	2053.972907	20.024256
62.153639	2056.267004	20.029274
62.154531	2058.705810	20.034291
62.279130	2057.716233	20.039309
62.276616	2045.209423	20.044327
62.349629	2069.396416	20.049344
62.559368	2077.131673	20.054362
62.738733	2071.522208	20.059379
62.475716	2086.501744	20.064397
62.413877	2070.041527	20.069415
62.588340	2086.063541	20.074432
62.972513	2083.730456	20.079450
63.094965	2083.602393	20.084467
63.138248	2099.053124	20.089485
63.574713	2100.640772	20.094503
63.049111	2089.284389	20.099520
62.984254	2090.961132	20.104538
63.275081	2102.553134	20.109555
63.114089	2109.769205	20.114573
63.425014	2113.730685	20.119591
63.469215	2112.949011	20.124608
63.345782	2110.656484	20.129626
63.754224	2106.187431	20.134643
63.497264	2114.220860	20.139661
63.702918	2107.083820	20.144679
63.538108	2111.146548	20.149696
63.739379	2107.298137	20.154714
63.858210	2112.656526	20.159731
63.883416	2127.090552	20.164749
64.263369	2124.295913	20.169767
64.019538	2137.969657	20.174784
64.170733	2135.785972	20.179802
64.414738	2142.675106	20.184819
64.124808	2142.891010	20.189837
64.369187	2127.350818	20.194855
64.434226	2136.171696	20.199872
64.237704	2136.735419	20.204890
64.403513	2129.643788	20.209907
64.120731	2134.987561	20.214925
64.183204	2130.461263	20.219943
64.776965	2146.197249	20.224960
64.822278	2158.255856	20.229978
64.876604	2154.104230	20.234995
64.510574	2165.089100	20.240013
64.951473	2158.685836	20.245031
64.826425	2162.509443	20.250048
65.058699	2162.598806	20.255066
65.427910	2157.250507	20.260083
65.113070	2165.681344	20.265101
65.110378	2167.645908	20.270119
64.944832	2165.003059	20.275136
65.172974	2170.235625	20.280154
65.590519	2181.504341	20.285171
65.250856	2191.478260	20.290189
65.263933	2185.987827	20.295207
65.032854	2193.585299	20.300224
65.895178	2187.190101	20.305242
65.797882	2191.095584	20.310259
65.471269	2190.391654	20.315277
65.714135	2200.127105	20.320295
65.747606	2214.329051	20.325312
66.008114	2214.730945	20.330330
66.142484	2212.825766	20.335347
66.110410	2219.091299	20.340365
66.287352	2215.563616	20.345383
66.456430	2210.384276	20.350400
66.376516	2211.094176	20.355418
66.658709	2205.453646	20.360435
66.397561	2207.857073	20.365453
66.430658	2210.974736	20.370471
66.535337	2213.041388	20.375488
66.291240	2211.153843	20.380506
66.304286	2206.988806	20.385523
66.299231	2213.971073	20.390541
66.620568	2214.453103	20.395559
66.871717	2232.069449	20.400576
67.106855	2228.622351	20.405594
67.516385	2223.156865	20.410611
67.382277	2227.617570	20.415629
67.267502	2212.839761	20.420647
67.165477	2207.791165	20.425664
67.512215	2213.996476	20.430682
67.363241	2202.200581	20.435699
67.102018	2200.885350	20.440717
67.384335	2217.082738	20.445735
67.541665	2226.673004	20.450752
67.624295	2233.262236	20.455770
67.860100	2224.496104	20.460787
67.649950	2227.348340	20.465805
67.596252	2225.202132	20.470823
67.701336	2223.943803	20.475840
67.644035	2228.055069	20.480858
68.069044	2225.630698	20.485875
67.652735	2236.339942	20.490893
67.717463	2227.760643	20.495911
67.696593	2241.945942	20.500928
68.023732	2245.770797	20.505946
68.261115	2257.117707	20.510963
68.326576	2253.812309	20.515981
68.275276	2252.341380	20.520999
68.257151	2256.623918	20.526016
68.330835	2258.093434	20.531034
68.453030	2251.975516	20.536051
68.369211	2272.805727	20.541069
68.777861	2280.806243	20.546087
68.945071	2281.654122	20.551104
68.801043	2293.642915	20.556122
69.167440	2281.718440	20.561139
69.160009	2284.479230	20.566157
69.557045	2283.109416	20.571175
69.692351	2272.768902	20.576192
69.302926	2274.976973	20.581210
69.489005	2256.650939	20.586227
68.827654	2259.433268	20.591245
69.503758	2267.576143	20.596263
69.824301	2274.697134	20.601280
68.912783	2280.671663	20.606298
69.212827	2274.802029	20.611315
69.070523	2280.986469	20.616333
69.181869	2290.189320	20.621351
68.938235	2297.649602	20.626368
69.311941	2309.444118	20.631386
69.430652	2306.372137	20.636403
69.419707	2314.138259	20.641421
69.497383	2325.680341	20.646439
69.780283	2329.509652	20.651456
69.896354	2331.873627	20.656474
70.168430	2333.271337	20.661491
69.956171	2338.517248	20.666509
70.076575	2356.022270	20.671527
70.164003	2358.375409	20.676544
70.359608	2363.441937	20.681562
70.848964	2363.121815	20.686579
70.819926	2368.138654	20.691597
70.816574	2369.187461	20.696615
70.644512	2368.589331	20.701632
70.581882	2373.431587	20.706650
70.924201	2363.841476	20.711667
70.977501	2355.022295	20.716685
70.858067	2356.398138	20.721703
71.054300	2366.260604	20.726720
70.558822	2359.498024	20.731738
71.013520	2367.800976	20.736755
71.192820	2377.784482	20.741773
71.080131	2375.483773	20.746791
71.618307	2383.548764	20.751808
71.774919	2393.276285	20.756826
71.954083	2387.985691	20.761843
71.624431	2385.483556	20.766861
71.797482	2392.168395	20.771879
71.797868	2390.427920	20.776896
71.673536	2388.689927	20.781914
72.086063	2380.933737	20.786931
71.789130	2387.430602	20.791949
71.731496	2385.021224	20.796967
72.126327	2386.841273	20.801984
71.797742	2390.384030	20.807002
72.446234	2406.067583	20.812019
72.158350	2417.525137	20.817037
72.249990	2417.328326	20.822055
72.642155	2417.285538	20.827072
72.255787	2415.329430	20.832090
72.500581	2422.479226	20.837107
72.337943	2421.803875	20.842125
72.329366	2413.692235	20.847143
72.556088	2421.571232	20.852160
72.701524	2439.933615	20.857178
73.088457	2435.211422	20.862195
72.906362	2441.510639	20.867213
73.130990	2437.400620	20.872231
73.339190	2438.552556	20.877248
73.216437	2440.005365	20.882266
73.626015	2436.245592	20.887283
73.832443	2438.965020	20.892301
73.692374	2435.692457	20.897319
73.731493	2427.293846	20.902336
73.493213	2441.476435	20.907354
73.787125	2437.089928	20.912371
73.509807	2434.609526	20.917389
73.293162	2431.332766	20.922407
73.768748	2443.749394	20.927424
73.696591	2445.468378	20.932442
73.745989	2438.413892	20.937459
73.902904	2436.194533	20.942477
73.723005	2446.347556	20.947495
74.212732	2462.397023	20.952512
73.915566	2466.846373	20.957530
73.728720	2475.556270	20.962547
73.898860	2466.704395	20.967565
73.717350	2471.637940	20.972583
74.061665	2482.333504	20.977600
74.359328	2496.045455	20.982618
74.622591	2491.975264	20.987635
74.488978	2491.208305	20.992653
74.550351	2494.259749	20.997671
74.851860	2492.728313	21.002688
75.167136	2508.006024	21.007706
75.371801	2515.474607	21.012723
75.236023	2508.730623	21.017741
75.086942	2499.479837	21.022759
75.600956	2505.869222	21.027776
75.526401	2493.665006	21.032794
75.474491	2480.347282	21.037811
75.524514	2490.540456	21.042829
75.212995	2505.720864	21.047847
76.001559	2501.674805	21.052864
75.541562	2524.603257	21.057882
75.422420	2506.378874	21.062899
75.505925	2518.191799	21.067917
75.221821	2518.168871	21.072935
75.403930	2512.092558	21.077952
75.384474	2531.636270	21.082970
75.679068	2533.562513	21.087987
75.972908	2538.867419	21.093005
76.254583	2545.206873	21.098023
76.761733	2544.765568	21.103040
76.455433	2537.033308	21.108058
76.301724	2540.058632	21.113075
76.392284	2543.735899	21.118093
76.598139	2552.756532	21.123111
76.811000	2555.789892	21.128128
76.880082	2555.460703	21.133146
76.863985	2559.381495	21.138163
77.067589	2557.767608	21.143181
76.863665	2555.320281	21.148199
77.520465	2546.634578	21.153216
77.127179	2553.389015	21.158234
77.238536	2550.933314	21.163251
77.895581	2550.178072	21.168269
77.500255	2549.169314	21.173287
77.828080	2546.877326	21.178304
77.711965	2544.333043	21.183322
77.452123	2548.401937	21.188339
78.112581	2547.264942	21.193357
77.520648	2546.644282	21.198375
77.741688	2547.820014	21.203392
77.513172	2557.414416	21.208410
77.746132	2546.116660	21.213427
77.680514	2552.289634	21.218445
77.834430	2545.841698	21.223463
77.736889	2543.245404	21.228480
77.546887	2554.495692	21.233498
78.177292	2568.570420	21.238515
78.110339	2568.785115	21.243533
78.247910	2580.399809	21.248551
78.455302	2571.611579	21.253568
78.704189	2574.329265	21.258586
78.618604	2574.845632	21.263603
78.906541	2569.948212	21.268621
78.564501	2583.962071	21.273639
79.007217	2581.244797	21.278656
79.002624	2586.568594	21.283674
79.167471	2590.532401	21.288691
79.197392	2586.177724	21.293709
78.844134	2594.841399	21.298727
79.472411	2592.356137	21.303744
79.435227	2596.786154	21.308762
79.394593	2598.302079	21.313779
79.397134	2596.168229	21.318797
79.405994	2602.815942	21.323815
79.579453	2599.795946	21.328832
79.771134	2596.142008	21.333850
79.605248	2601.334378	21.338867
79.818457	2599.696001	21.343885
79.678143	2602.533181	21.348903
79.857898	2616.470214	21.353920
80.093227	2618.505071	21.358938
80.136208	2620.536677	21.363955
80.175166	2624.036951	21.368973
80.237864	2625.880893	21.373991
80.358929	2627.552596	21.379008
80.322338	2625.177376	21.384026
80.044769	2629.925040	21.389043
80.663271	2644.969767	21.394061
80.620220	2650.627008	21.399079
80.892959	2649.610030	21.404096
80.971378	2646.468499	21.409114
80.880116	2648.401842	21.414131
81.018033	2653.429527	21.419149
81.050166	2653.703628	21.424167
81.258613	2647.313243	21.429184
81.263161	2656.024291	21.434202
81.131886	2648.994384	21.439219
81.392287	2646.242203	21.444237
81.294267	2651.231581	21.449255
81.788345	2650.029386	21.454272
81.431399	2664.912957	21.459290
81.583999	2676.104597	21.464307
81.851040	2674.785389	21.469325
81.536528	2688.737918	21.474343
81.833584	2674.819947	21.479360
81.755629	2687.074927	21.484378
81.710291	2689.493405	21.489395
82.136718	2671.885663	21.494413
81.866340	2682.172481	21.499431
82.079339	2697.456099	21.504448
82.103990	2706.034571	21.509466
82.099576	2709.810064	21.514483
82.280550	2705.145153	21.519501
82.112365	2702.485339	21.524519
82.170216	2712.632425	21.529536
82.726759	2723.887156	21.534554
82.552024	2735.779169	21.539571
83.005806	2729.399457	21.544589
83.071823	2721.908056	21.549607
83.039459	2726.213638	21.554624
82.994675	2734.176355	21.559642
82.926700	2741.045211	21.564659
83.177257	2746.031564	21.569677
83.217213	2749.615174	21.574695
83.594173	2745.514400	21.579712
83.544210	2750.630242	21.584730
83.423930	2756.625231	21.589747
83.459595	2752.664871	21.594765
83.590606	2749.007123	21.599783
83.854695	2761.422461	21.604800
84.003133	2773.656810	21.609818
83.872994	2781.342790	21.614835
84.228249	2775.016966	21.619853
84.107112	2783.586609	21.624871
84.847729	2778.350053	21.629888
84.346336	2773.465035	21.634906
84.352956	2773.450543	21.639923
84.481560	2769.929449	21.644941
84.656514	2777.422152	21.649959
84.701201	2774.318668	21.654976
84.661783	2781.171620	21.659994
84.432066	2790.975858	21.665011
85.244199	2797.730869	21.670029
85.003542	2800.326971	21.675047
84.948001	2799.368625	21.680064
85.430343	2802.556661	21.685082
85.027931	2803.956641	21.690099
85.440753	2801.229493	21.695117
85.309146	2804.433789	21.700135
85.550283	2801.511623	21.705152
85.484898	2803.976082	21.710170
85.514966	2820.788315	21.715187
86.021200	2827.681626	21.720205
85.894304	2837.951822	21.725223
85.705950	2838.072350	21.730240
85.977504	2829.128069	21.735258
85.874364	2840.913380	21.740275
85.932818	2837.539757	21.745293
85.941266	2838.107740	21.750311
86.544478	2838.365845	21.755328
86.614115	2832.893054	21.760346
86.201051	2837.659284	21.765363
86.907353	2842.770725	21.770381
86.782679	2863.719767	21.775399
86.727821	2863.800083	21.780416
86.818696	2854.719014	21.785434
86.600154	2864.504842	21.790451
86.725720	2865.589860	21.795469
86.527417	2859.076171	21.800487
86.810210	2860.397276	21.805504
86.945153	2866.427307	21.810522
86.867475	2885.920799	21.815539
87.281106	2874.313828	21.820557
87.280753	2892.207151	21.825575
87.140862	2886.572586	21.830592
87.364249	2897.939687	21.835610
87.134168	2906.053966	21.840627
87.669150	2915.685442	21.845645
87.819470	2926.509863	21.850663
87.812713	2918.991467	21.855680
87.711469	2922.636339	21.860698
87.968093	2934.879832	21.865715
88.289334	2931.420971	21.870733
88.739111	2943.423441	21.875751
88.501200	2934.987784	21.880768
88.943557	2941.632990	21.885786
88.723296	2946.678072	21.890803
88.901726	2934.067866	21.895821
88.960165	2938.539865	21.900839
88.878138	2939.241496	21.905856
88.936508	2939.190568	21.910874
89.156483	2949.505328	21.915891
89.178053	2938.490824	21.920909
88.995149	2930.668697	21.925927
88.850949	2940.976578	21.930944
89.270459	2932.919652	21.935962
88.858291	2951.482185	21.940979
89.158583	2956.143481	21.945997
89.344805	2964.927512	21.951015
89.265909	2972.537858	21.956032
89.422563	2971.373799	21.961050
89.406472	2993.321136	21.966067
89.279248	2992.272685	21.971085
89.846573	2998.560204	21.976103
89.824095	2999.379214	21.981120
90.370443	3012.073985	21.986138
90.409789	3025.043913	21.991155
90.392707	3028.221533	21.996173
90.476407	3029.216082	22.001191
90.730845	3029.296140	22.006208
90.957321	3019.390779	22.011226
90.719177	3025.988084	22.016243
90.627133	3030.214198	22.021261
90.795531	3027.060317	22.026279
90.647508	3028.156021	22.031296
90.991099	3019.730886	22.036314
91.044102	3023.183950	22.041331
91.140080	3036.700196	22.046349
91.293264	3040.955941	22.051367
91.409747	3047.348335	22.056384
91.287331	3046.515636	22.061402
91.356218	3048.565696	22.066419
91.648765	3045.336973	22.071437
91.688193	3043.978001	22.076455
91.902118	3041.438485	22.081472
91.971787	3035.919153	22.086490
91.760473	3046.396909	22.091507
92.175694	3056.819241	22.096525
92.533720	3072.977759	22.101543
92.301154	3070.960545	22.106560
93.078072	3069.038041	22.111578
92.426479	3076.527675	22.116595
92.706072	3066.271375	22.121613
93.025733	3063.464860	22.126631
92.926473	3069.046043	22.131648
92.924558	3067.598861	22.136666
92.699190	3067.924202	22.141683
92.624354	3073.689428	22.146701
92.881443	3070.237597	22.151719
92.786907	3071.534414	22.156736
93.223592	3071.148495	22.161754
93.114910	3087.653235	22.166771
93.544226	3096.837489	22.171789
93.494175	3088.355367	22.176807
93.238192	3104.578228	22.181824
93.605660	3089.034100	22.186842
93.759168	3094.717658	22.191859
93.391429	3090.322330	22.196877
94.267705	3106.102212	22.201895
94.412586	3117.516009	22.206912
94.276151	3118.127743	22.211930
94.224946	3123.524292	22.216947
94.211225	3123.045473	22.221965
94.587548	3117.712173	22.226983
94.491094	3123.988315	22.232000
94.517900	3115.418184	22.237018
94.552264	3113.114207	22.242035
94.461943	3118.557627	22.247053
94.869583	3121.482888	22.252071
95.129179	3144.724399	22.257088
95.380077	3139.803227	22.262106
95.360586	3143.119108	22.267123
95.203122	3138.720008	22.272141
95.583032	3136.574945	22.277159
95.339603	3135.687380	22.282176
95.542445	3126.960265	22.287194
95.763728	3137.700998	22.292211
95.478281	3137.426276	22.297229
95.671629	3140.851367	22.302247
95.411828	3142.262367	22.307264
95.976935	3159.284088	22.312282
95.793922	3159.755745	22.317299
96.135169	3164.476238	22.322317
96.229918	3157.034047	22.327335
96.123388	3171.553836	22.332352
96.310020	3162.648339	22.337370
96.030656	3175.024073	22.342387
96.149445	3185.906846	22.347405
96.646910	3182.352352	22.352423
96.378989	3194.948234	22.357440
96.681868	3186.133843	22.362458
96.586469	3201.025846	22.367475
96.759396	3212.726304	22.372493
96.957660	3207.747191	22.377511
97.209744	3221.464443	22.382528
97.064217	3217.013657	22.387546
97.304791	3226.622555	22.392563
97.323964	3242.707028	22.397581
98.000387	3246.550222	22.402599
98.087315	3243.139340	22.407616
98.194524	3240.444823	22.412634
98.072023	3248.032849	22.417651
97.959147	3239.442492	22.422669
98.595107	3232.447758	22.427687
98.588274	3235.100715	22.432704
98.781612	3226.892609	22.437722
98.607953	3235.373842	22.442739
98.765207	3230.760098	22.447757
98.598451	3228.781985	22.452775
98.486808	3234.924526	22.457792
98.474635	3221.563920	22.462810
98.934498	3222.476667	22.467827
98.821508	3230.977425	22.472845
98.843507	3221.710271	22.477863
99.002656	3242.000004	22.482880
99.186144	3251.430474	22.487898
99.076000	3251.629743	22.492915
99.051032	3257.655048	22.497933
99.400639	3251.793097	22.502951
99.522971	3271.041707	22.507968
99.636171	3275.392579	22.512986
99.604504	3291.888268	22.518003
99.698673	3290.117440	22.523021
99.823867	3284.915345	22.528039
99.922112	3291.335380	22.533056
99.868302	3303.389019	22.538074
99.951283	3326.232636	22.543091
99.947522	3325.028320	22.548109
100.470440	3335.281948	22.553127
100.168868	3333.248964	22.558144
100.601020	3340.877412	22.563162
100.660836	3347.259953	22.568179
100.564872	3355.503472	22.573197
101.250641	3346.003528	22.578215
101.008384	3353.543616	22.583232
101.365012	3346.468344	22.588250
101.226740	3346.184926	22.593267
101.266914	3352.797659	22.598285
101.460766	3347.965748	22.603303
101.675961	3374.328505	22.608320
101.780860	3381.841383	22.613338
101.481011	3380.227089	22.618355
101.503077	3382.830225	22.623373
102.206927	3366.533513	22.628391
102.009793	3376.736555	22.633408
102.097515	3376.434869	22.638426
102.115759	3366.950114	22.643443
102.266989	3375.459209	22.648461
102.136786	3386.094190	22.653479
102.317742	3395.216449	22.658496
102.411399	3392.945584	22.663514
102.421769	3396.669878	22.668531
102.566012	3406.347380	22.673549
102.713290	3421.163334	22.678567
102.658541	3436.714884	22.683584
102.613706	3441.395326	22.688602
103.158412	3435.729834	22.693619
103.174127	3441.571030	22.698637
103.396486	3444.152440	22.703655
103.476352	3457.351264	22.708672
103.732327	3456.729328	22.713690
103.723117	3445.423616	22.718707
103.803568	3452.787928	22.723725
104.454831	3450.575041	22.728743
103.966932	3450.535852	22.733760
104.231416	3453.944092	22.738778
104.067676	3453.293298	22.743795
103.891012	3465.203517	22.748813
104.097365	3477.830942	22.753831
104.047674	3483.962170	22.758848
104.493994	3486.740681	22.763866
104.859794	3485.413930	22.768883
104.850767	3510.863952	22.773901
105.047691	3508.249307	22.778919
105.319321	3507.855447	22.783936
105.311302	3511.026097	22.788954
105.592529	3505.350620	22.793971
105.439131	3511.697322	22.798989
105.934636	3507.321642	22.804007
105.589128	3511.343248	22.809024
105.521698	3517.374357	22.814042
105.257654	3513.219460	22.819059
105.394482	3520.886023	22.824077
105.543385	3526.539811	22.829095
105.723976	3539.094518	22.834112
105.818724	3544.752872	22.839130
106.369293	3545.065701	22.844147
106.353507	3548.192798	22.849165
106.537060	3564.880276	22.854183
106.686491	3560.796249	22.859200
106.944208	3555.466597	22.864218
107.241508	3558.486467	22.869235
107.300598	3566.611366	22.874253
107.085761	3547.597266	22.879271
107.330318	3548.480000	22.884288
107.021172	3550.720160	22.889306
107.412740	3546.755294	22.894323
107.142576	3558.573713	22.899341
106.972088	3548.349368	22.904359
107.274943	3550.614562	22.909376
107.475013	3553.612508	22.914394
107.551725	3558.503698	22.919411
107.314827	3574.192146	22.924429
107.857265	3581.245768	22.929447
107.822208	3577.175249	22.934464
106.976454	3590.787258	22.939482
107.926796	3609.549370	22.944499
107.826855	3615.671150	22.949517
108.110060	3631.588679	22.954535
108.564605	3639.162241	22.959552
108.511783	3639.020111	22.964570
108.594250	3642.854967	22.969587
108.889348	3657.355181	22.974605
108.773482	3666.054351	22.979623
109.023298	3666.954305	22.984640
108.984791	3672.101561	22.989658
108.745812	3665.079424	22.994675
109.090500	3687.773162	22.999693
109.319411	3694.966432	23.004711
109.917833	3699.736724	23.009728
109.569288	3699.886293	23.014746
109.797424	3691.492410	23.019763
109.774560	3703.269329	23.024781
110.047377	3719.446271	23.029799
110.130776	3718.835796	23.034816
110.274417	3718.740319	23.039834
110.523374	3717.432793	23.044851
110.823879	3730.292372	23.049869
110.979562	3715.784185	23.054887
110.872901	3717.078407	23.059904
110.719957	3721.452187	23.064922
111.185381	3708.562186	23.069939
111.440558	3731.197299	23.074957
111.499968	3732.773365	23.079975
111.741866	3733.065081	23.084992
111.605413	3740.866811	23.090010
111.977011	3737.004559	23.095027
111.550918	3746.092473	23.100045
111.895218	3740.170608	23.105063
111.984442	3738.717979	23.110080
111.765523	3749.825219	23.115098
112.194018	3749.312314	23.120115
112.285122	3757.304232	23.125133
112.114179	3743.291493	23.130151
112.103760	3745.310348	23.135168
111.888874	3750.625695	23.140186
112.407929	3759.925697	23.145203
112.439605	3780.216711	23.150221
112.345547	3777.101374	23.155239
112.604062	3780.473692	23.160256
112.326422	3794.985582	23.165274
112.686076	3801.241297	23.170291
113.079479	3816.227293	23.175309
112.765025	3815.956740	23.180327
113.479768	3829.362079	23.185344
113.661044	3837.699302	23.190362
114.017483	3827.917650	23.195379
113.571083	3840.150053	23.200397
113.935218	3835.308492	23.205415
114.309764	3832.575920	23.210432
113.948779	3835.277089	23.215450
114.237833	3824.628028	23.220467
114.249231	3827.434692	23.225485
114.221198	3834.749259	23.230503
114.681432	3841.869861	23.235520
114.571321	3850.144416	23.240538
114.828689	3853.342886	23.245555
115.035310	3854.411716	23.250573
115.287390	3852.213652	23.255591
115.698530	3849.114083	23.260608
115.358378	3856.963392	23.265626
115.492619	3855.473107	23.270643
114.971645	3848.349585	23.275661
115.039787	3853.618810	23.280679
115.306507	3872.341700	23.285696
115.599318	3875.160775	23.290714
115.766174	3868.633685	23.295731
115.734611	3884.170674	23.300749
116.074125	3888.385256	23.305767
116.774349	3894.276246	23.310784
116.919886	3892.593420	23.315802
116.918659	3895.691311	23.320819
116.797112	3897.982845	23.325837
116.493643	3893.032823	23.330855
116.803548	3893.581457	23.335872
116.926737	3900.696070	23.340890
117.243814	3891.177098	23.345907
117.263689	3889.600089	23.350925
117.310653	3891.519338	23.355943
117.653104	3885.701700	23.360960
117.241425	3890.490056	23.365978
117.553877	3916.714970	23.370995
117.719918	3916.213973	23.376013
117.625778	3918.008557	23.381031
117.975881	3913.368643	23.386048
118.011635	3924.290578	23.391066
118.080980	3919.597979	23.396083
117.948233	3936.145536	23.401101
117.765440	3943.110996	23.406119
118.101511	3950.154482	23.411136
118.227261	3956.104597	23.416154
118.198787	3958.977978	23.421171
118.209735	3975.875057	23.426189
118.233925	3980.212241	23.431207
118.448381	3986.017993	23.436224
118.564849	4008.587496	23.441242
118.894785	3999.385237	23.446259
119.007184	4006.407235	23.451277
119.079128	4025.236157	23.456295
119.697961	4024.357455	23.461312
119.687011	4027.977650	23.466330
119.864976	4026.494818	23.471347
119.796860	4026.372633	23.476365
120.201976	4040.718871	23.481383
120.678228	4043.870406	23.486400
120.689630	4056.248176	23.491418
121.003801	4050.825194	23.496435
120.701812	4041.224808	23.501453
121.018077	4039.493009	23.506471
121.329168	4041.451271	23.511488
121.116569	4034.822189	23.516506
121.249751	4031.430775	23.521523
121.176531	4029.781498	23.526541
121.318957	4040.960103	23.531559
121.723959	4036.966823	23.536576
121.306191	4047.612952	23.541594
121.459902	4044.885123	23.546611
121.605214	4044.189198	23.551629
121.506993	4053.439248	23.556647
122.273965	4055.774601	23.561664
121.561577	4072.192473	23.566682
121.912345	4068.633794	23.571699
121.937832	4081.384072	23.576717
122.095731	4092.108758	23.581735
122.344285	4099.580024	23.586752
122.237092	4109.971324	23.591770
122.148368	4107.387435	23.596787
122.525121	4118.099036	23.601805
122.385967	4133.174268	23.606823
123.025503	4149.157255	23.611840
123.110546	4159.636925	23.616858
123.625339	4162.196677	23.621875
123.464671	4161.494918	23.626893
123.518481	4165.975148	23.631911
123.817040	4155.157261	23.636928
123.907300	4163.639429	23.641946
124.660130	4180.872666	23.646963
124.579737	4179.074169	23.651981
124.236898	4174.523828	23.656999
124.599365	4169.372132	23.662016
124.417415	4188.779566	23.667034
124.211652	4181.048159	23.672051
124.616010	4185.065040	23.677069
124.572054	4186.489534	23.682087
125.065118	4198.510753	23.687104
124.873492	4215.176599	23.692122
125.109213	4218.150446	23.697139
124.874608	4215.961729	23.702157
124.880919	4216.738060	23.707175
125.194192	4226.894319	23.712192
125.827262	4241.834910	23.717210
125.681132	4249.754330	23.722227
125.486444	4249.187569	23.727245
125.361759	4250.636934	23.732263
126.039645	4262.175210	23.737280
126.235130	4272.313097	23.742298
126.114198	4272.386630	23.747315
126.263739	4275.665107	23.752333
126.329866	4291.339336	23.757351
126.636617	4294.140345	23.762368
126.872188	4304.849497	23.767386
126.959847	4302.427520	23.772403
127.080050	4301.145958	23.777421
127.159126	4307.260157	23.782439
127.912542	4320.434815	23.787456
127.948837	4329.264214	23.792474
127.698050	4326.522192	23.797491
128.110168	4325.499335	23.802509
128.128207	4320.798872	23.807527
128.368500	4313.979404	23.812544
128.734834	4323.097202	23.817562
128.542711	4323.587780	23.822579
128.575134	4323.914631	23.827597
128.195689	4321.012723	23.832615
128.639116	4316.778075	23.837632
128.590280	4317.612698	23.842650
128.675389	4331.987281	23.847667
128.810389	4337.185347	23.852685
128.719115	4354.263392	23.857703
128.816803	4347.983464	23.862720
128.924804	4367.109062	23.867738
129.185711	4376.155174	23.872755
129.386536	4374.855847	23.877773
129.427739	4396.204592	23.882791
129.514345	4397.136508	23.887808
129.979136	4402.367062	23.892826
129.761305	4402.212254	23.897843
129.887081	4419.471335	23.902861
129.937625	4441.037500	23.907879
130.161017	4434.923445	23.912896
130.212739	4445.284571	23.917914
130.542088	4458.081517	23.922931
131.174058	4467.854067	23.927949
130.649435	4464.429614	23.932967
130.755831	4466.190670	23.937984
130.951465	4495.430365	23.943002
131.356085	4501.150149	23.948019
131.609268	4498.595798	23.953037
131.489026	4503.046101	23.958055
131.916657	4506.792068	23.963072
132.158197	4513.737018	23.968090
132.204846	4519.333080	23.973107
132.644717	4515.711770	23.978125
132.413179	4517.800922	23.983143
132.735527	4509.598393	23.988160
132.865658	4506.214489	23.993178
132.748819	4507.423092	23.998195
133.150904	4505.015707	24.003213
132.832465	4507.853042	24.008231
132.906536	4510.697129	24.013248
132.875757	4507.320332	24.018266
133.093414	4521.556582	24.023283
133.498124	4531.777702	24.028301
133.225729	4533.343780	24.033319
133.396758	4540.477261	24.038336
133.755607	4548.978966	24.043354
133.827068	4560.248868	24.048371
134.073198	4566.310901	24.053389
133.870639	4575.897347	24.058407
134.416386	4563.699397	24.063424
134.553771	4567.365962	24.068442
134.648210	4584.533716	24.073459
135.082287	4596.247933	24.078477
134.817607	4603.043411	24.083495
135.188470	4602.767204	24.088512
134.985015	4606.045614	24.093530
135.044924	4612.147464	24.098547
135.490424	4609.588483	24.103565
135.400916	4625.583513	24.108583
135.688243	4626.547983	24.113600
135.815388	4623.858479	24.118618
135.661623	4635.349776	24.123635
136.221203	4636.048611	24.128653
136.268557	4649.998328	24.133671
136.696476	4650.451936	24.138688
136.419153	4649.576391	24.143706
136.709687	4658.935795	24.148723
136.508930	4644.872231	24.153741
136.621853	4657.984478	24.158759
136.606042	4674.397764	24.163776
136.944172	4678.220551	24.168794
136.377420	4689.902406	24.173811
136.843245	4699.821730	24.178829
136.616958	4714.860467	24.183847
137.276111	4724.195313	24.188864
137.538073	4738.529709	24.193882
137.109706	4748.251061	24.198899
137.756006	4761.418461	24.203917
138.046689	4769.277436	24.208935
138.157495	4778.733883	24.213952
138.541555	4780.346556	24.218970
138.700275	4795.120881	24.223987
139.126671	4803.640288	24.229005
139.000547	4797.675803	24.234023
139.030782	4801.001622	24.239040
139.630325	4798.645410	24.244058
139.370107	4801.385388	24.249075
139.750958	4788.545245	24.254093
139.677283	4797.312629	24.259111
139.495387	4796.019016	24.264128
139.829369	4789.050959	24.269146
139.691992	4804.925201	24.274163
140.144818	4813.796888	24.279181
139.970705	4827.853252	24.284199
140.040230	4824.178000	24.289216
140.048585	4827.924243	24.294234
140.238011	4846.311034	24.299251
141.022166	4834.238992	24.304269
140.574952	4849.352748	24.309287
140.658545	4847.833247	24.314304
140.774179	4856.843102	24.319322
140.995386	4879.766877	24.324339
141.153811	4881.420604	24.329357
141.191336	4903.718998	24.334375
141.512192	4901.794134	24.339392
141.751522	4902.529766	24.344410
141.737934	4909.825812	24.349427
141.990423	4925.909809	24.354445
142.458783	4937.600287	24.359463
142.396341	4937.808725	24.364480
142.712945	4940.573505	24.369498
142.787115	4938.644454	24.374515
142.925463	4942.299914	24.379533
142.759334	4961.658321	24.384551
143.035467	4965.231880	24.389568
143.122321	4960.688778	24.394586
142.939404	4968.920472	24.399603
143.491373	4989.969003	24.404621
143.638002	4990.818201	24.409639
143.905985	4991.095234	24.414656
143.954816	4988.760937	24.419674
144.027850	4991.106700	24.424691
144.059473	5004.307211	24.429709
144.313583	5009.477203	24.434727
144.930437	5014.132897	24.439744
145.241393	5007.261637	24.444762
145.074170	5019.013871	24.449779
145.411527	5011.259842	24.454797
145.177753	5004.415011	24.459815
144.783282	5018.154871	24.464832
145.620194	5022.139565	24.469850
145.767892	5044.203451	24.474867
145.778170	5043.920526	24.479885
145.761437	5045.763404	24.484903
145.521450	5052.163371	24.489920
146.087326	5063.810446	24.494938
145.991165	5078.221507	24.499955
146.242101	5078.147803	24.504973
146.415977	5079.390892	24.509991
146.323881	5084.609230	24.515008
146.536462	5093.790853	24.520026
146.765676	5107.628668	24.525043
146.716093	5102.721383	24.530061
147.141185	5118.197053	24.535079
146.985474	5132.780630	24.540096
147.528985	5131.539074	24.545114
147.485752	5132.019116	24.550131
147.804237	5130.512883	24.555149
148.181262	5133.238198	24.560167
148.368417	5141.188358	24.565184
149.002742	5132.487786	24.570202
148.969153	5139.271445	24.575219
150.110596	5123.689536	24.580237
149.964376	5100.419434	24.585255
149.590619	5098.405677	24.590272
149.937274	5091.745656	24.595290
149.518687	5077.980552	24.600307
150.007916	5070.538367	24.605325
149.883456	5059.164615	24.610343
149.894091	5061.533688	24.615360
149.518068	5057.206172	24.620378
149.626679	5067.925005	24.625395
149.807721	5079.551419	24.630413
149.939695	5091.437518	24.635431
149.529911	5093.873152	24.640448
150.325538	5099.292192	24.645466
150.388798	5114.376979	24.650483
150.338107	5123.120911	24.655501
150.180021	5129.484815	24.660519
150.821319	5143.440273	24.665536
151.113090	5139.307812	24.670554
150.716459	5167.158435	24.675571
150.948463	5173.744560	24.680589
151.592995	5180.888531	24.685607
151.196599	5199.280060	24.690624
151.645796	5201.243941	24.695642
151.920276	5214.050119	24.700659
152.150664	5216.859661	24.705677
152.448743	5237.022593	24.710695
152.572508	5242.986925	24.715712
152.750639	5235.397925	24.720730
152.439795	5240.563231	24.725747
152.708356	5238.867053	24.730765
152.898531	5261.091734	24.735783
152.800902	5274.049967	24.740800
153.190447	5266.605876	24.745818
153.270922	5287.065320	24.750835
152.994444	5291.415809	24.755853
153.477526	5302.402217	24.760871
153.615488	5321.666400	24.765888
153.858844	5327.504715	24.770906
153.887185	5338.654170	24.775923
154.320638	5348.836237	24.780941
154.431549	5355.275420	24.785959
154.153983	5359.195255	24.790976
153.933028	5361.651333	24.795994
154.288630	5379.770803	24.801011
154.378893	5399.452850	24.806029
155.005340	5406.874136	24.811047
155.537770	5417.191302	24.816064
155.416117	5423.753087	24.821082
155.809716	5440.514453	24.826099
156.206812	5440.480284	24.831117
156.406774	5443.093436	24.836135
156.275351	5457.591228	24.841152
156.681011	5454.004719	24.846170
156.855664	5449.775678	24.851187
156.409705	5453.344739	24.856205
156.819661	5459.538145	24.861223
156.919866	5470.704519	24.866240
157.194225	5480.035676	24.871258
157.110665	5483.649745	24.876275
156.962309	5489.950685	24.881293
157.507142	5497.931870	24.886311
157.556387	5514.775975	24.891328
157.943998	5514.908847	24.896346
157.876034	5514.692100	24.901363
157.951733	5530.893662	24.906381
158.279448	5536.830233	24.911399
158.506821	5548.212742	24.916416
158.521624	5535.006248	24.921434
158.331857	5555.826649	24.926451
159.242771	5565.315763	24.931469
159.205613	5569.359852	24.936487
158.881130	5571.539901	24.941504
159.468034	5581.895886	24.946522
159.393225	5590.292900	24.951539
159.330539	5596.608340	24.956557
159.639641	5594.183654	24.961575
160.178446	5623.287045	24.966592
160.227130	5620.702984	24.971610
160.248787	5624.416415	24.976627
160.503722	5641.310465	24.981645
160.978298	5648.770503	24.986663
160.913814	5651.104492	24.991680
161.454817	5636.325276	24.996698
161.671346	5633.325684	25.001715
161.779052	5637.923910	25.006733
161.784776	5635.918287	25.011751
161.712345	5640.550544	25.016768
162.510918	5648.939658	25.021786
162.425648	5652.425664	25.026803
162.645111	5658.397379	25.031821
162.887228	5651.762924	25.036839
162.746489	5663.920692	25.041856
162.879766	5660.115379	25.046874
163.068028	5657.312037	25.051891
163.016493	5663.978479	25.056909
163.221099	5650.942576	25.061927
163.105770	5650.470858	25.066944
163.640295	5659.729167	25.071962
163.314150	5678.945734	25.076979
163.066002	5688.730497	25.081997
163.660634	5689.154776	25.087015
163.384999	5704.977209	25.092032
163.795992	5712.018884	25.097050
163.788828	5721.717459	25.102067
163.816132	5738.433230	25.107085
164.215614	5745.672242	25.112103
164.258496	5759.704833	25.117120
164.468458	5768.737634	25.122138
164.806501	5777.088394	25.127155
164.887706	5791.501991	25.132173
165.643396	5800.213617	25.137191
165.347240	5799.217563	25.142208
165.558130	5817.385184	25.147226
165.349696	5830.868568	25.152243
165.806540	5841.104445	25.157261
166.401726	5852.361106	25.162279
166.356047	5861.809578	25.167296
166.706311	5860.433317	25.172314
166.862103	5867.870124	25.177331
167.027300	5870.797298	25.182349
167.363688	5873.680948	25.187367
167.298192	5892.074841	25.192384
167.353326	5892.176488	25.197402
167.656055	5885.375581	25.202419
167.634414	5894.971978	25.207437
167.487453	5908.088060	25.212455
167.611386	5929.624761	25.217472
168.059985	5925.214726	25.222490
168.182969	5945.794550	25.227507
168.458833	5966.766467	25.232525
168.983164	5946.942194	25.237543
168.973742	5953.833124	25.242560
168.863602	5972.480526	25.247578
169.717891	5973.952068	25.252595
169.599641	5980.932558	25.257613
169.516177	5980.560133	25.262631
169.795658	5993.979709	25.267648
169.993039	5993.020348	25.272666
170.267206	6014.173791	25.277683
169.806774	6014.386660	25.282701
170.318566	6012.609323	25.287719
170.352641	6046.854747	25.292736
170.477794	6047.383936	25.297754
170.838193	6052.540778	25.302771
171.199718	6058.389827	25.307789
171.570803	6062.850079	25.312807
171.735109	6067.293789	25.317824
171.577999	6071.350690	25.322842
171.943364	6069.466899	25.327859
172.062102	6074.446977	25.332877
172.482371	6093.177684	25.337895
172.118033	6102.368199	25.342912
172.286475	6091.283792	25.347930
172.630273	6095.570707	25.352947
172.431274	6101.452840	25.357965
172.110805	6113.959996	25.362983
172.428163	6123.015551	25.368000
172.583229	6144.176192	25.373018
173.097432	6158.240984	25.378035
173.086384	6172.545493	25.383053
173.332548	6179.923630	25.388071
173.410531	6194.913178	25.393088
173.395994	6203.485297	25.398106
173.884179	6212.899178	25.403123
173.763844	6223.832909	25.408141
174.475516	6242.290127	25.413159
174.842790	6253.174165	25.418176
174.932081	6254.065558	25.423194
175.206439	6258.493607	25.428211
175.020149	6281.684613	25.433229
175.346002	6276.440057	25.438247
175.553337	6276.060313	25.443264
175.916007	6288.174800	25.448282
176.032693	6304.411873	25.453299
175.911430	6308.285451	25.458317
176.425173	6308.849654	25.463335
176.502742	6324.150546	25.468352
176.534367	6336.559710	25.473370
176.734319	6343.376318	25.478387
176.663646	6352.682847	25.483405
177.055836	6354.248608	25.488423
177.550622	6365.177035	25.493440
177.566334	6370.237097	25.498458
177.832696	6371.774014	25.503475
177.656078	6394.999761	25.508493
178.055349	6395.102288	25.513511
178.173268	6409.952855	25.518528
178.214513	6420.403715	25.523546
178.543338	6429.829288	25.528563
178.309574	6437.749059	25.533581
178.540985	6441.938750	25.538599
178.928763	6458.821138	25.543616
179.099298	6466.295872	25.548634
179.430175	6476.287500	25.553651
179.674266	6493.526979	25.558669
179.958054	6496.134602	25.563687
180.132597	6498.656971	25.568704
180.277893	6509.400421	25.573722
180.589579	6521.962593	25.578739
180.682843	6535.523255	25.583757
180.620557	6525.732173	25.588775
180.903030	6528.099768	25.593792
181.031144	6542.357908	25.598810
181.427816	6541.620368	25.603827
181.182002	6554.538085	25.608845
180.828818	6561.332231	25.613863
181.122871	6580.011099	25.618880
181.279077	6586.042846	25.623898
181.578091	6603.115481	25.628915
181.574218	6615.333224	25.633933
182.072184	6636.794160	25.638951
182.520066	6640.397742	25.643968
182.689684	6644.316068	25.648986
183.421692	6644.635695	25.654003
183.757879	6656.337500	25.659021
184.091958	6654.945044	25.664039
184.233605	6653.494195	25.669056
184.153406	6653.113316	25.674074
184.601482	6643.494632	25.679092
184.124819	6646.520947	25.684109
184.618024	6653.808118	25.689127
184.784061	6647.344630	25.694144
184.229904	6651.520152	25.699162
184.309293	6656.563087	25.704180
184.517944	6674.966817	25.709197
184.616956	6672.158906	25.714215
184.956848	6692.463826	25.719232
184.756651	6714.511676	25.724250
185.369789	6728.059010	25.729268
185.369448	6748.818559	25.734285
185.746076	6752.753418	25.739303
186.158861	6759.400593	25.744320
186.129322	6775.370168	25.749338
186.455409	6785.134366	25.754356
186.457750	6811.893025	25.759373
186.775216	6809.487207	25.764391
187.007865	6826.991328	25.769408
187.059702	6839.443895	25.774426
187.614404	6841.407235	25.779444
187.453427	6859.605126	25.784461
187.482163	6873.680509	25.789479
187.996392	6876.437755	25.794496
188.115435	6897.262897	25.799514
188.602804	6900.632898	25.804532
188.424608	6907.068700	25.809549
188.439996	6921.404796	25.814567
188.831296	6926.438465	25.819584
189.198895	6940.711840	25.824602
189.348939	6948.265150	25.829620
189.385928	6962.295081	25.834637
189.732234	6979.126048	25.839655
190.142207	6984.778863	25.844672
190.061034	7005.514000	25.849690
189.879819	6994.800858	25.854708
190.452663	7006.021997	25.859725
190.577483	7034.228415	25.864743
190.474717	7031.461331	25.869760
190.487952	7057.046345	25.874778
191.576454	7062.531674	25.879796
191.461874	7069.200055	25.884813
191.620349	7072.448436	25.889831
192.269220	7084.597974	25.894848
192.228184	7098.820221	25.899866
192.731603	7083.640423	25.904884
192.753244	7082.434619	25.909901
192.857062	7076.184080	25.914919
193.393782	7074.756066	25.919936
193.490153	7077.553464	25.924954
193.574460	7079.303632	25.929972
193.527072	7070.250159	25.934989
193.526017	7077.079481	25.940007
193.855436	7083.095906	25.945024
193.876086	7104.792907	25.950042
193.666355	7104.857249	25.955060
193.913338	7114.394152	25.960077
194.452216	7121.201052	25.965095
194.226045	7119.179848	25.970112
194.192656	7145.772670	25.975130
194.472191	7150.391510	25.980148
194.738255	7162.642176	25.985165
194.894417	7183.295109	25.990183
195.480537	7192.955113	25.995200
195.378936	7213.972891	26.000218
195.347132	7218.200029	26.005236
195.614240	7235.420608	26.010253
195.951615	7244.081850	26.015271
196.540028	7257.620483	26.020288
196.468076	7275.081987	26.025306
196.698364	7282.289260	26.030324
197.019922	7309.170493	26.035341
197.438420	7315.508904	26.040359
197.507277	7310.166267	26.045376
197.430887	7336.906212	26.050394
197.812166	7347.731093	26.055412
197.898350	7362.773112	26.060429
198.040670	7369.266022	26.065447
198.404039	7374.167549	26.070464
198.309714	7395.499428	26.075482
198.723706	7414.580174	26.080500
198.782174	7412.360465	26.085517
199.281136	7432.872242	26.090535
199.456386	7439.944069	26.095552
199.489623	7447.683071	26.100570
199.924695	7455.433551	26.105588
200.073787	7470.515306	26.110605
200.119691	7472.798338	26.115623
200.566066	7478.757839	26.120640
200.393348	7500.991914	26.125658
201.291572	7492.043172	26.130676
201.373697	7493.592087	26.135693
201.216293	7520.254054	26.140711
201.265198	7524.060153	26.145728
202.022226	7529.240087	26.150746
202.360542	7528.509359	26.155764
202.447086	7538.856288	26.160781
202.223173	7545.857145	26.165799
202.524452	7553.807071	26.170816
202.525419	7553.580842	26.175834
202.680457	7555.983042	26.180852
203.225966	7574.666450	26.185869
203.042921	7591.461179	26.190887
203.385330	7589.803309	26.195904
202.866173	7595.640028	26.200922
203.257546	7607.801019	26.205940
203.513853	7627.350998	26.210957
203.689811	7651.564312	26.215975
204.025869	7656.018416	26.220992
203.888466	7679.684402	26.226010
204.043954	7691.629070	26.231028
204.691948	7705.660483	26.236045
204.597878	7723.726564	26.241063
205.149039	7740.884817	26.246080
205.221203	7753.217228	26.251098
205.333895	7763.241549	26.256116
205.212772	7792.267438	26.261133
205.445257	7815.172231	26.266151
206.239297	7811.900718	26.271168
206.184184	7835.149475	26.276186
206.405072	7853.745474	26.281204
206.659539	7864.590866	26.286221
206.934809	7886.244490	26.291239
207.110707	7897.617020	26.296256
207.325120	7912.609213	26.301274
207.766110	7911.263716	26.306292
208.431840	7924.001072	26.311309
208.580039	7942.044777	26.316327
208.997850	7930.302658	26.321344
209.193603	7933.638574	26.326362
210.025943	7908.622611	26.331380
210.570576	7907.427150	26.336397
210.557660	7913.540385	26.341415
210.814944	7903.834699	26.346432
210.857804	7904.984667	26.351450
210.764232	7893.858846	26.356468
211.028822	7902.314701	26.361485
211.007952	7907.540655	26.366503
211.507655	7895.838882	26.371520
211.467250	7902.550827	26.376538
211.541311	7900.192875	26.381556
211.623783	7905.216769	26.386573
211.685957	7909.688742	26.391591
212.113766	7906.927460	26.396608
211.615706	7904.877918	26.401626
211.483591	7908.383472	26.406644
211.962589	7921.505770	26.411661
211.858744	7941.917488	26.416679
212.091817	7954.681763	26.421696
212.014192	7973.383428	26.426714
212.378126	7998.879107	26.431732
212.863804	8017.697764	26.436749
212.528040	8036.173531	26.441767
213.181982	8053.383830	26.446784
213.265369	8069.162805	26.451802
213.502320	8075.575181	26.456820
213.710223	8095.011129	26.461837
213.418985	8120.616940	26.466855
213.970770	8127.930990	26.471872
213.976039	8147.062186	26.476890
214.101208	8171.894759	26.481908
214.728485	8186.547795	26.486925
215.094064	8210.838169	26.491943
215.282637	8212.605253	26.496960
215.884940	8235.871104	26.501978
215.930670	8255.037248	26.506996
216.178060	8259.855724	26.512013
216.010749	8276.430243	26.517031
216.594971	8280.614305	26.522048
216.820217	8302.054112	26.527066
217.305303	8317.636849	26.532084
217.590319	8320.877188	26.537101
217.269018	8342.824338	26.542119
217.711829	8338.918855	26.547136
217.920445	8357.284345	26.552154
218.552942	8370.439788	26.557172
219.121107	8369.253657	26.562189
218.576023	8380.754838	26.567207
218.798497	8379.881641	26.572224
219.443430	8394.007149	26.577242
219.281912	8408.188968	26.582260
219.803390	8416.245752	26.587277
219.679239	8426.844444	26.592295
220.241168	8433.035816	26.597312
220.473762	8438.557263	26.602330
220.263308	8457.078209	26.607348
220.803357	8449.141252	26.612365
221.180534	8466.424647	26.617383
221.117780	8477.602145	26.622400
221.150550	8492.446390	26.627418
220.989576	8506.761346	26.632436
221.595664	8519.852110	26.637453
221.476987	8549.310675	26.642471
221.872731	8557.473381	26.647488
222.486326	8575.328516	26.652506
222.426714	8594.365795	26.657524
222.781075	8592.550574	26.662541
222.855379	8615.709732	26.667559
222.988358	8630.157977	26.672576
223.304512	8649.652461	26.677594
223.660562	8666.526865	26.682612
223.779036	8670.367006	26.687629
223.878291	8693.741018	26.692647
224.290249	8694.757659	26.697664
224.993108	8706.451690	26.702682
225.604587	8705.965594	26.707700
226.093973	8703.730934	26.712717
226.254325	8710.894902	26.717735
225.921962	8701.653792	26.722752
226.338635	8704.001077	26.727770
226.402884	8701.821956	26.732788
226.256188	8694.015986	26.737805
226.639272	8709.555925	26.742823
226.731066	8728.103371	26.747840
226.764550	8733.083135	26.752858
226.719055	8740.632203	26.757876
227.075457	8751.712834	26.762893
226.915240	8764.552256	26.767911
227.066617	8772.217284	26.772928
227.456398	8793.746933	26.777946
227.520196	8816.374020	26.782964
227.683273	8826.600724	26.787981
228.161955	8850.976675	26.792999
228.407887	8860.428137	26.798016
228.897860	8875.686773	26.803034
229.112158	8888.499916	26.808052
229.674334	8905.069794	26.813069
230.202636	8908.108619	26.818087
230.331506	8909.142283	26.823104
230.784059	8907.303108	26.828122
231.179423	8920.387775	26.833140
231.065207	8927.583146	26.838157
231.280563	8935.922718	26.843175
231.384003	8920.374864	26.848192
231.652744	8930.099782	26.853210
231.471074	8946.362307	26.858228
232.237153	8944.905859	26.863245
232.300814	8960.715088	26.868263
232.507647	8960.884510	26.873280
232.733503	8972.966186	26.878298
232.870519	8983.388118	26.883316
233.594977	8987.652330	26.888333
233.202004	8995.938632	26.893351
233.436681	9011.910836	26.898368
233.826971	9023.906064	26.903386
233.917086	9034.301402	26.908404
234.058700	9032.964589	26.913421
234.283555	9055.353260	26.918439
234.285006	9071.647552	26.923456
234.858418	9085.117826	26.928474
234.894616	9100.364640	26.933492
235.243994	9105.659092	26.938509
235.315693	9128.622468	26.943527
235.233780	9136.551410	26.948544
235.781586	9147.768110	26.953562
235.624351	9178.922036	26.958580
236.117007	9180.882922	26.963597
236.360193	9199.784711	26.968615
236.375611	9221.914850	26.973632
237.183496	9240.702562	26.978650
236.940749	9250.290014	26.983668
237.204776	9266.692343	26.988685
237.417726	9280.925770	26.993703
237.563966	9301.659548	26.998720
238.112764	9302.438475	27.003738
238.097764	9331.675848	27.008756
238.533453	9346.313939	27.013773
238.541801	9359.506270	27.018791
239.076823	9379.404544	27.023808
239.481611	9380.636763	27.028826
239.744221	9393.442027	27.033844
239.729646	9404.621363	27.038861
239.897478	9406.543409	27.043879
240.378471	9422.521072	27.048896
240.823967	9425.662434	27.053914
240.858267	9439.635107	27.058932
241.628473	9443.971966	27.063949
241.837582	9447.100275	27.068967
241.742755	9459.095463	27.073984
242.331728	9464.364725	27.079002
241.993539	9475.725640	27.084020
242.237613	9481.153297	27.089037
242.948776	9496.357278	27.094055
242.572136	9516.768106	27.099072
242.500816	9524.460633	27.104090
242.747170	9541.931487	27.109108
242.802260	9551.723340	27.114125
243.126400	9572.915462	27.119143
243.286810	9597.911222	27.124160
243.733087	9610.426750	27.129178
243.971852	9641.636600	27.134196
244.457077	9653.455297	27.139213
244.838374	9678.318774	27.144231
245.159448	9685.151503	27.149248
245.467938	9694.277576	27.154266
245.428344	9708.215874	27.159284
245.736253	9719.341728	27.164301
246.427450	9741.175531	27.169319
246.270577	9759.624962	27.174336
246.842131	9760.477228	27.179354
247.282623	9780.814512	27.184372
247.797040	9779.732049	27.189389
247.960663	9785.487181	27.194407
247.995291	9785.703463	27.199424
248.733091	9793.657684	27.204442
249.021742	9799.301570	27.209460
249.159622	9793.097720	27.214477
249.343060	9780.333932	27.219495
249.472950	9793.586150	27.224512
249.683079	9784.798230	27.229530
249.929604	9802.028241	27.234548
250.136958	9806.551495	27.239565
250.320129	9805.220104	27.244583
250.090491	9816.964476	27.249600
250.345755	9824.947843	27.254618
250.475842	9845.891517	27.259636
250.639079	9862.459852	27.264653
251.189433	9872.449078	27.269671
250.764866	9887.961554	27.274688
251.607710	9900.540128	27.279706
251.474426	9903.374233	27.284724
251.380625	9922.753792	27.289741
251.937961	9941.180289	27.294759
251.782506	9962.587493	27.299776
252.372099	9986.463955	27.304794
252.260121	10003.029180	27.309812
252.824636	10027.357531	27.314829
253.060473	10033.467538	27.319847
252.942223	10056.819346	27.324864
253.446966	10070.899452	27.329882
253.659948	10087.993693	27.334900
254.167548	10094.394368	27.339917
254.691020	10115.094472	27.344935
254.908871	10135.678373	27.349952
255.024562	10140.092942	27.354970
255.277720	10158.628553	27.359988
255.796246	10176.122778	27.365005
255.800112	10183.807458	27.370023
256.065667	10201.296220	27.375040
256.265105	10215.750251	27.380058
256.443979	10228.606774	27.385076
256.853062	10245.924431	27.390093
257.189586	10264.373385	27.395111
257.365328	10283.097326	27.400128
257.625668	10292.035012	27.405146
258.085067	10312.208989	27.410164
258.038752	10329.617397	27.415181
258.407885	10341.324128	27.420199
258.376544	10362.248862	27.425216
258.949312	10371.070007	27.430234
259.399941	10397.028950	27.435252
259.940362	10416.839333	27.440269
260.150307	10424.326492	27.445287
260.413788	10434.425120	27.450304
260.780922	10441.338524	27.455322
261.012910	10463.683798	27.460340
260.949158	10455.263935	27.465357
261.416701	10463.431853	27.470375
261.319952	10484.875381	27.475392
261.894684	10489.777100	27.480410
262.066629	10513.941819	27.485428
262.080545	10515.187546	27.490445
262.680074	10524.703872	27.495463
262.420202	10543.567387	27.500480
263.003788	10563.181447	27.505498
263.064027	10567.898748	27.510516
263.267157	10592.430143	27.515533
263.626459	10604.189177	27.520551
264.177514	10614.619989	27.525568
264.464892	10631.500340	27.530586
264.763400	10637.590379	27.535604
265.025413	10649.284176	27.540621
265.606217	10664.339837	27.545639
265.625261	10666.123646	27.550656
265.619433	10663.890086	27.555674
265.594764	10678.698117	27.560692
265.747842	10704.771588	27.565709
266.084178	10709.313961	27.570727
266.250256	10733.905500	27.575744
266.452769	10744.358314	27.580762
266.681567	10767.394789	27.585780
267.396074	10779.769124	27.590797
268.292339	10782.001429	27.595815
268.094372	10796.855029	27.600832
268.085072	10796.364978	27.605850
268.777687	10819.229052	27.610868
268.445860	10832.534466	27.615885
269.167847	10838.381802	27.620903
268.926705	10859.369925	27.625920
269.256474	10875.469502	27.630938
269.407458	10893.536514	27.635956
269.694168	10914.478360	27.640973
269.765234	10926.923695	27.645991
269.853577	10950.900102	27.651008
270.229777	10981.340420	27.656026
270.483924	10997.774563	27.661044
270.360419	11026.674279	27.666061
271.307929	11033.578290	27.671079
271.795261	11049.997734	27.676096
272.596594	11068.588565	27.681114
272.474151	11070.311570	27.686132
272.765034	11087.976601	27.691149
273.000854	11101.985505	27.696167
273.541692	11116.917637	27.701184
274.181883	11121.135414	27.706202
274.612167	11125.571976	27.711220
274.700386	11134.400948	27.716237
275.253138	11127.455718	27.721255
275.385410	11133.136331	27.726272
275.582889	11140.846588	27.731290
275.786194	11136.054070	27.736308
276.150627	11145.195016	27.741325
276.436941	11141.349581	27.746343
276.503403	11150.866240	27.751360
276.926561	11166.269301	27.756378
277.416853	11174.394284	27.761396
277.604226	11183.518321	27.766413
277.761254	11175.022422	27.771431
277.646953	11186.614057	27.776448
277.666308	11207.264857	27.781466
277.831561	11214.909755	27.786484
277.830181	11247.801244	27.791501
278.493521	11251.484000	27.796519
278.449451	11281.624994	27.801536
278.237409	11292.699215	27.806554
278.727880	11310.145895	27.811572
279.101246	11337.241653	27.816589
278.977583	11354.068707	27.821607
279.346833	11386.123163	27.826624
279.581828	11407.307748	27.831642
280.068350	11437.455797	27.836660
280.069742	11460.555869	27.841677
280.898202	11480.292970	27.846695
281.016256	11502.569370	27.851712
281.178617	11520.353032	27.856730
281.642296	11518.004214	27.861748
281.892216	11544.226330	27.866765
282.126490	11562.035535	27.871783
281.935851	11572.155972	27.876800
282.273041	11598.943172	27.881818
282.879482	11627.342186	27.886836
282.668719	11650.532471	27.891853
283.542767	11668.972845	27.896871
283.827835	11699.953350	27.901888
283.850550	11714.235703	27.906906
284.421453	11725.697673	27.911924
284.526017	11757.391621	27.916941
285.436070	11779.461737	27.921959
285.831605	11799.837629	27.926976
286.446055	11809.569644	27.931994
286.448103	11817.453979	27.937012
286.473337	11837.349671	27.942029
286.958831	11836.327203	27.947047
287.107323	11859.634298	27.952064
286.779349	11870.084198	27.957082
287.580996	11890.707374	27.962100
287.899099	11907.282770	27.967117
288.415633	11928.591562	27.972135
288.661921	11939.237793	27.977152
288.530046	11958.270120	27.982170
289.017232	11972.591292	27.987188
288.986825	11992.734685	27.992205
289.720943	12000.312397	27.997223
290.065436	12019.576774	28.002240
290.431623	12026.746334	28.007258
290.524593	12041.176108	28.012276
290.834469	12056.960335	28.017293
291.215433	12072.426647	28.022311
291.559592	12087.886674	28.027328
291.769906	12103.027660	28.032346
292.242719	12112.773101	28.037364
291.991564	12143.611526	28.042381
293.080372	12143.565210	28.047399
293.533458	12153.320361	28.052416
293.626868	12171.879343	28.057434
293.643235	12165.898727	28.062452
293.978126	12182.145290	28.067469
294.419088	12200.206603	28.072487
294.378845	12199.614643	28.077504
294.745614	12219.022009	28.082522
295.158666	12230.311235	28.087540
294.787995	12251.253996	28.092557
295.707936	12260.666000	28.097575
296.141239	12267.165383	28.102592
296.135860	12288.540458	28.107610
296.306133	12305.548212	28.112628
296.338818	12313.358190	28.117645
296.431986	12332.766878	28.122663
296.625133	12345.641541	28.127680
297.394401	12366.653848	28.132698
297.456379	12383.777959	28.137716
297.320783	12410.835072	28.142733
297.871109	12430.052048	28.147751
298.241322	12449.526866	28.152768
298.425953	12473.391290	28.157786
299.070864	12497.930214	28.162804
298.925645	12516.872489	28.167821
299.595887	12536.116318	28.172839
299.796062	12552.731495	28.177856
299.851454	12571.845914	28.182874
300.454829	12580.697699	28.187892
300.576521	12615.544069	28.192909
301.295947	12632.834722	28.197927
301.809583	12650.288326	28.202944
302.027566	12664.697224	28.207962
302.708093	12677.167098	28.212980
302.745281	12694.138175	28.217997
302.994485	12701.679546	28.223015
302.797655	12712.993256	28.228032
302.559593	12733.081736	28.233050
303.914540	12754.378726	28.238068
304.004400	12778.166848	28.243085
304.415721	12794.832766	28.248103
304.518454	12809.345076	28.253120
304.217336	12840.423479	28.258138
304.840935	12856.055416	28.263156
304.930956	12890.308885	28.268173
305.079302	12904.433624	28.273191
305.648535	12933.080855	28.278208
305.822237	12967.124706	28.283226
305.816842	12990.281685	28.288244
306.280113	13023.175906	28.293261
306.723060	13050.106545	28.298279
306.879652	13069.960729	28.303296
307.376902	13101.560029	28.308314
307.974237	13123.282082	28.313332
308.330228	13145.802062	28.318349
308.396790	13158.705364	28.323367
308.932906	13191.518089	28.328384
309.043079	13215.060640	28.333402
309.583954	13227.720364	28.338420
309.836828	13257.845620	28.343437
310.042912	13281.669715	28.348455
310.761078	13303.968651	28.353472
310.764609	13327.348384	28.358490
311.249989	13348.502027	28.363508
311.284962	13364.837418	28.368525
311.900939	13382.628894	28.373543
312.282597	13407.507462	28.378560
312.171538	13430.136249	28.383578
312.419191	13444.365795	28.388596
312.368149	13461.726330	28.393613
312.904334	13481.189692	28.398631
313.477884	13503.977072	28.403648
313.391056	13527.451384	28.408666
313.826877	13551.143502	28.413684
314.140469	13570.156512	28.418701
314.658450	13595.153854	28.423719
314.993357	13616.396678	28.428736
315.586757	13644.123684	28.433754
315.898549	13641.573640	28.438772
316.361639	13665.196627	28.443789
316.566507	13678.090818	28.448807
317.040953	13692.502373	28.453824
317.039497	13717.365111	28.458842
317.619091	13730.217186	28.463860
317.638824	13742.955593	28.468877
318.071018	13762.730279	28.473895
318.494123	13787.488835	28.478912
318.945439	13814.896876	28.483930
319.450956	13829.071528	28.488948
319.375551	13838.431225	28.493965
319.133356	13855.317406	28.498983
319.755813	13883.954023	28.504000
320.103830	13911.721961	28.509018
320.061684	13935.581665	28.514036
320.408608	13965.326421	28.519053
320.816027	13991.643674	28.524071
321.392672	14008.506311	28.529088
321.853545	14026.400727	28.534106
322.285286	14041.765627	28.539124
322.583922	14064.763251	28.544141
322.756075	14086.477488	28.549159
323.911136	14096.482327	28.554176
324.020526	14111.319342	28.559194
324.465154	14117.715073	28.564212
324.906951	14137.992952	28.569229
324.983905	14139.797163	28.574247
325.378593	14146.579754	28.579264
325.658116	14168.015623	28.584282
325.956934	14169.168667	28.589300
325.748042	14184.173785	28.594317
325.998715	14204.087295	28.599335
326.550242	14219.233228	28.604352
326.895065	14249.465909	28.609370
326.976000	14265.061373	28.614388
327.463876	14282.346171	28.619405
327.542561	14301.031449	28.624423
328.003187	14322.044001	28.629440
327.927666	14349.636221	28.634458
328.583265	14363.913288	28.639476
329.269689	14392.710062	28.644493
329.275370	14413.635196	28.649511
329.747165	14419.331270	28.654528
329.493843	14444.742663	28.659546
330.136504	14459.929945	28.664564
330.523845	14474.666059	28.669581
330.839008	14497.421866	28.674599
331.632228	14513.718289	28.679616
331.500536	14537.701393	28.684634
331.865174	14544.960598	28.689652
332.552276	14569.235312	28.694669
332.471010	14573.079558	28.699687
332.960276	14596.756142	28.704704
332.878902	14622.824009	28.709722
333.551484	14637.613840	28.714740
333.671832	14661.432557	28.719757
333.810205	14688.632450	28.724775
334.073435	14708.241774	28.729792
334.151991	14745.030962	28.734810
334.698665	14767.252516	28.739828
335.159165	14797.598782	28.744845
335.432030	14812.684258	28.749863
336.673452	14819.374030	28.754880
336.988558	14841.435185	28.759898
337.283171	14860.180242	28.764916
337.725802	14870.774237	28.769933
337.981236	14884.303828	28.774951
338.186551	14899.917980	28.779968
338.123930	14919.947522	28.784986
338.605999	14935.213208	28.790004
339.195546	14960.755212	28.795021
338.942991	14976.671741	28.800039
339.385659	15008.477940	28.805056
339.818550	15032.719667	28.810074
339.915929	15048.987705	28.815092
340.004097	15077.131583	28.820109
340.125393	15114.388731	28.825127
340.840484	15139.308925	28.830144
340.914899	15172.147977	28.835162
341.426776	15198.211230	28.840180
341.644245	15227.228547	28.845197
341.916370	15256.559691	28.850215
342.364946	15284.383638	28.855232
342.865686	15319.334694	28.860250
343.015654	15348.162021	28.865268
343.492868	15372.722948	28.870285
343.903534	15404.120819	28.875303
344.485906	15415.945974	28.880320
345.136371	15448.333751	28.885338
345.290347	15468.213337	28.890356
345.752375	15490.217074	28.895373
346.011834	15521.485023	28.900391
346.379555	15544.743998	28.905408
346.447751	15560.314491	28.910426
346.709441	15595.557736	28.915444
346.974436	15616.042706	28.920461
347.460469	15644.844480	28.925479
348.202587	15666.431583	28.930496
347.985231	15690.222954	28.935514
348.202626	15710.095113	28.940532
349.232753	15722.944050	28.945549
349.311812	15750.991321	28.950567
350.055285	15765.902432	28.955584
350.650253	15785.851847	28.960602
351.539683	15788.250008	28.965620
351.640122	15791.418661	28.970637
351.838659	15800.224927	28.975655
352.316884	15809.544451	28.980672
352.137805	15819.296632	28.985690
352.404610	15836.092863	28.990708
352.791283	15849.044293	28.995725
352.629348	15862.874786	29.000743
353.498513	15886.719839	29.005760
353.454134	15907.080058	29.010778
353.688559	15937.290604	29.015796
353.844768	15958.277012	29.020813
354.300003	15994.126368	29.025831
354.282286	16014.694962	29.030848
354.641367	16054.112525	29.035866
355.069835	16086.077713	29.040884
355.593914	16105.711773	29.045901
355.850846	16144.510192	29.050919
356.377655	16169.924516	29.055936
356.652991	16210.736153	29.060954
357.131672	16235.214558	29.065972
357.649631	16260.773990	29.070989
357.653607	16291.959484	29.076007
358.530275	16314.869055	29.081024
358.762990	16334.413018	29.086042
358.963465	16367.154005	29.091060
359.518924	16376.351841	29.096077
359.846345	16396.770325	29.101095
360.316606	16416.114455	29.106112
360.798063	16444.235810	29.111130
361.378156	16464.560629	29.116148
361.723798	16483.117486	29.121165
361.770513	16505.184287	29.126183
362.483297	16526.071298	29.131200
363.067745	16553.714869	29.136218
363.267182	16573.969484	29.141236
363.249143	16588.151109	29.146253
363.799270	16611.684571	29.151271
363.993567	16639.888575	29.156288
364.258808	16654.128906	29.161306
364.735078	16681.334058	29.166324
365.029175	16707.332960	29.171341
364.823147	16740.629893	29.176359
365.539263	16757.767815	29.181376
365.814224	16779.028127	29.186394
365.949672	16819.658713	29.191412
366.656948	16839.804549	29.196429
366.818480	16870.812782	29.201447
367.054792	16894.837107	29.206464
367.556214	16926.156087	29.211482
367.831508	16954.431870	29.216500
368.235590	16969.200444	29.221517
368.502137	17000.498333	29.226535
368.832206	17026.844700	29.231552
369.390425	17055.893515	29.236570
369.281972	17092.749893	29.241588
370.217633	17118.943751	29.246605
370.507423	17143.170518	29.251623
370.598646	17179.346505	29.256640
371.081330	17210.932506	29.261658
371.470181	17236.640107	29.266676
372.131042	17250.403258	29.271693
372.688108	17279.777421	29.276711
372.904521	17299.430935	29.281728
373.862832	17329.549900	29.286746
373.876943	17352.419545	29.291764
374.570697	17360.648322	29.296781
374.888549	17386.658399	29.301799
374.839183	17405.295014	29.306816
375.431567	17424.501149	29.311834
375.617100	17445.698810	29.316852
376.324103	17466.162333	29.321869
375.941368	17491.209564	29.326887
376.646586	17512.461713	29.331904
377.322309	17536.835744	29.336922
377.638076	17569.050110	29.341940
378.343214	17576.364231	29.346957
378.713654	17609.046994	29.351975
379.158454	17624.200152	29.356992
379.813260	17638.871173	29.362010
379.722994	17658.396364	29.367028
380.375833	17670.773883	29.372045
380.221996	17691.802992	29.377063
380.354072	17718.376719	29.382080
380.387685	17743.037664	29.387098
380.886936	17785.862715	29.392116
381.550511	17808.842398	29.397133
381.425869	17833.123845	29.402151
381.731972	17871.839022	29.407168
382.354766	17904.327765	29.412186
382.959877	17922.520139	29.417204
383.663902	17956.976807	29.422221
383.620188	17987.035349	29.427239
383.738493	18007.455379	29.432256
384.773274	18035.174005	29.437274
384.708894	18075.116655	29.442292
385.089843	18107.090704	29.447309
385.352470	18137.016609	29.452327
385.778899	18173.637074	29.457344
386.166673	18190.476434	29.462362
386.109889	18233.940264	29.467380
386.733072	18266.825369	29.472397
386.963744	18310.635862	29.477415
387.171093	18345.490612	29.482432
388.241566	18379.287817	29.487450
388.076312	18413.126584	29.492468
388.967615	18438.415683	29.497485
389.590434	18465.951788	29.502503
389.969233	18494.005895	29.507520
390.199615	18514.117236	29.512538
390.396756	18542.539952	29.517556
390.880765	18559.736851	29.522573
391.297210	18588.161478	29.527591
391.866745	18619.531868	29.532608
392.447785	18639.389341	29.537626
392.459204	18670.499152	29.542644
393.080075	18697.490455	29.547661
393.293642	18726.935483	29.552679
393.616566	18748.514865	29.557696
394.314780	18778.255324	29.562714
395.135513	18797.784959	29.567732
395.992832	18809.538618	29.572749
396.020965	18823.001572	29.577767
396.421572	18851.296920	29.582784
396.892808	18854.133006	29.587802
397.012239	18882.137610	29.592820
397.674626	18901.260921	29.597837
397.816957	18919.675586	29.602855
397.895697	18946.170524	29.607872
398.324546	18973.259821	29.612890
398.038355	19009.625829	29.617908
398.576763	19035.744144	29.622925
399.244365	19077.998112	29.627943
399.260108	19105.596731	29.632960
400.062687	19127.242609	29.637978
400.136403	19168.866999	29.642996
400.647419	19195.561015	29.648013
401.098495	19233.280091	29.653031
401.679271	19260.143575	29.658048
402.452247	19281.725351	29.663066
402.372172	19317.936872	29.668084
403.043064	19344.996325	29.673101
403.594386	19372.041625	29.678119
403.737689	19409.142162	29.683136
404.239940	19428.984115	29.688154
404.366208	19467.747972	29.693172
404.903085	19497.816928	29.698189
405.397661	19522.576499	29.703207
405.846929	19547.222464	29.708224
406.704038	19563.057238	29.713242
407.126538	19595.643494	29.718260
407.606793	19612.526770	29.723277
407.997759	19627.807644	29.728295
408.228152	19656.578151	29.733312
409.026399	19681.495622	29.738330
408.944045	19691.093139	29.743348
409.018983	19717.921052	29.748365
409.757173	19739.805805	29.753383
409.557393	19770.118163	29.758400
410.265535	19790.518113	29.763418
410.262336	19823.631860	29.768436
411.630835	19829.258136	29.773453
412.239990	19841.647907	29.778471
412.179410	19869.905741	29.783488
412.795156	19880.148457	29.788506
413.232931	19905.446537	29.793524
413.548891	19917.328437	29.798541
414.500399	19937.965948	29.803559
414.607457	19955.954181	29.808576
414.790718	19967.551389	29.813594
415.213620	19990.285184	29.818612
415.190867	20011.126004	29.823629
415.698788	20033.785371	29.828647
415.540413	20064.363940	29.833664
416.020689	20087.969447	29.838682
416.194827	20130.504558	29.843700
416.779373	20162.133841	29.848717
416.985173	20191.721512	29.853735
417.032267	20237.235121	29.858752
417.760100	20269.751431	29.863770
418.044438	20323.480666	29.868788
418.394349	20359.742142	29.873805
419.314400	20403.936623	29.878823
419.463745	20438.461892	29.883840
419.900774	20473.876132	29.888858
420.429388	20504.388225	29.893876
420.626195	20553.847427	29.898893
421.099420	20598.235669	29.903911
421.529320	20631.502259	29.908928
422.022593	20666.470484	29.913946
422.438309	20712.275405	29.918964
422.895446	20756.737775	29.923981
423.644828	20791.030060	29.928999
423.601118	20820.912301	29.934016
424.105266	20859.724965	29.939034
424.661516	20905.321833	29.944052
425.189173	20930.431012	29.949069
425.904034	20961.386643	29.954087
426.032249	21002.187810	29.959104
426.819621	21035.400243	29.964122
427.367283	21065.396026	29.969140
428.322636	21096.643410	29.974157
428.861372	21124.337032	29.979175
429.002666	21139.089656	29.984192
429.634492	21167.126922	29.989210
430.021172	21187.703491	29.994228
429.881842	21211.639079	29.999245
430.546432	21233.703955	30.004263
430.954379	21256.768426	30.009280
431.857103	21271.184114	30.014298
432.196355	21307.968234	30.019316
432.562332	21328.252067	30.024333
433.086306	21342.026276	30.029351
433.382531	21370.272767	30.034368
433.868842	21392.492974	30.039386
433.956304	21400.846573	30.044404
434.083673	21421.828969	30.049421
434.853171	21445.393114	30.054439
435.203567	21477.777734	30.059456
435.951853	21500.861484	30.064474
436.073986	21524.501980	30.069492
435.787737	21547.909724	30.074509
436.573258	21571.040803	30.079527
436.593036	21607.572819	30.084544
436.931664	21645.958339	30.089562
437.637022	21681.472615	30.094580
437.681656	21721.290062	30.099597
438.213915	21751.806927	30.104615
438.682121	21790.285683	30.109632
439.261297	21823.776605	30.114650
439.372139	21865.648820	30.119668
439.895770	21909.246534	30.124685
440.439705	21940.477666	30.129703
440.708801	21988.257090	30.134720
441.326650	22029.224391	30.139738
441.734506	22065.424381	30.144756
442.175001	22111.834370	30.149773
442.814342	22152.397738	30.154791
442.933688	22198.024051	30.159808
443.682857	22232.939031	30.164826
443.987126	22273.342482	30.169844
444.155276	22322.442715	30.174861
444.738362	22352.280154	30.179879
445.389608	22405.372754	30.184896
446.127793	22453.429493	30.189914
446.601796	22479.800705	30.194932
446.776302	22526.153317	30.199949
447.739609	22564.079033	30.204967
447.796732	22600.655656	30.209984
448.033431	22630.839951	30.215002
449.063622	22663.411539	30.220020
449.157531	22708.396997	30.225037
449.957852	22726.319824	30.230055
450.052379	22772.768813	30.235072
450.838157	22803.934850	30.240090
451.317518	22843.962701	30.245108
451.631971	22874.077328	30.250125
452.042975	22898.668481	30.255143
452.375167	22948.297511	30.260160
452.583485	22986.460775	30.265178
453.157374	23025.321615	30.270196
453.453929	23068.002353	30.275213
454.329009	23099.696131	30.280231
454.867788	23137.374147	30.285248
455.206350	23177.840091	30.290266
455.931123	23207.415031	30.295284
455.874301	23244.359503	30.300301
456.765231	23278.772902	30.305319
456.566943	23312.026200	30.310336
457.296080	23344.436194	30.315354
457.785540	23382.470155	30.320372
457.865299	23417.871298	30.325389
458.620227	23453.286139	30.330407
458.997550	23490.544708	30.335424
459.359115	23518.886061	30.340442
460.040589	23551.386623	30.345460
460.306609	23600.041618	30.350477
461.140287	23628.292791	30.355495
461.429943	23670.733336	30.360512
461.950011	23696.966053	30.365530
462.242439	23723.209430	30.370548
462.367120	23763.019475	30.375565
463.189117	23794.748869	30.380583
463.959522	23828.026426	30.385600
464.466283	23866.433847	30.390618
465.095427	23891.067899	30.395636
465.109796	23933.247148	30.400653
465.492751	23961.516173	30.405671
465.959610	24002.958818	30.410688
466.497962	24039.903946	30.415706
467.482942	24076.204853	30.420724
467.637767	24106.503553	30.425741
468.416218	24138.181114	30.430759
468.839772	24162.699378	30.435776
469.560156	24200.137271	30.440794
469.739830	24225.265188	30.445812
470.317416	24253.337318	30.450829
470.785923	24282.544811	30.455847
470.929577	24316.817072	30.460864
471.454652	24346.387189	30.465882
472.345508	24371.923383	30.470900
472.333951	24402.512922	30.475917
472.996313	24430.775847	30.480935
473.527473	24470.975255	30.485952
473.989543	24504.351116	30.490970
474.500732	24537.377955	30.495988
474.576650	24573.015549	30.501005
475.190176	24606.974449	30.506023
475.690389	24637.599731	30.511040
476.114229	24682.032265	30.516058
476.782297	24713.673021	30.521076
476.682818	24764.368576	30.526093
477.498694	24788.363119	30.531111
477.775207	24834.284931	30.536128
477.865517	24877.396640	30.541146
478.266342	24926.313019	30.546164
478.716273	24971.543050	30.551181
479.463607	25010.930681	30.556199
479.672205	25063.927537	30.561216
480.837336	25103.215399	30.566234
481.406662	25146.583225	30.571252
481.513051	25184.696268	30.576269
482.246102	25219.986007	30.581287
482.861564	25256.336949	30.586304
483.070418	25283.672699	30.591322
483.822746	25318.565026	30.596340
484.060065	25359.413050	30.601357
484.301174	25381.879181	30.606375
484.878367	25418.946787	30.611392
485.284937	25458.226638	30.616410
485.813386	25491.075688	30.621428
485.916285	25537.521219	30.626445
486.135183	25579.085842	30.631463
486.647485	25625.205937	30.636480
486.972186	25673.500249	30.641498
487.794777	25712.037468	30.646516
488.090364	25770.368573	30.651533
488.683051	25812.781380	30.656551
489.591118	25863.581951	30.661568
489.706990	25906.855875	30.666586
490.835851	25944.407369	30.671604
490.875445	25994.776687	30.676621
491.662321	26034.819189	30.681639
492.342336	26067.816866	30.686656
492.641218	26113.009509	30.691674
493.320147	26152.458778	30.696692
493.623903	26188.988117	30.701709
493.965526	26233.426095	30.706727
494.580771	26277.533382	30.711744
494.829538	26321.381798	30.716762
496.073591	26355.658817	30.721780
496.681677	26403.105307	30.726797
497.040619	26433.953564	30.731815
497.334758	26471.305366	30.736832
497.788919	26505.408865	30.741850
498.595047	26536.653887	30.746868
499.736950	26591.019210	30.751885
499.812302	26612.016838	30.756903
500.524900	26635.861289	30.761920
500.589408	26670.088663	30.766938
500.928120	26698.158371	30.771956
501.570424	26741.631248	30.776973
501.961868	26778.452810	30.781991
502.827428	26806.886706	30.787008
503.264656	26838.028277	30.792026
503.916205	26875.187203	30.797044
504.469528	26908.845452	30.802061
504.799452	26937.283007	30.807079
505.515581	26974.210243	30.812096
505.549067	27003.600971	30.817114
506.152843	27041.951490	30.822132
506.412110	27076.960231	30.827149
506.770379	27116.381450	30.832167
507.434619	27146.654957	30.837184
507.491745	27205.034877	30.842202
508.086503	27236.257432	30.847220
508.414517	27294.323073	30.852237
509.052411	27333.321441	30.857255
509.342360	27368.735641	30.862272
509.848976	27418.625221	30.867290
510.565665	27457.619830	30.872308
510.649188	27508.809413	30.877325
511.022984	27546.323384	30.882343
511.636839	27588.635933	30.887360
511.850465	27638.405976	30.892378
512.254004	27682.865429	30.897396
512.971046	27742.143642	30.902413
513.510884	27793.082345	30.907431
514.179083	27837.241292	30.912448
514.183942	27897.689503	30.917466
514.939363	27948.118473	30.922484
515.549458	28002.872731	30.927501
516.156749	28051.958120	30.932519
516.842311	28102.632974	30.937536
517.584318	28163.804491	30.942554
518.265727	28191.975629	30.947572
518.820133	28231.110195	30.952589
519.517416	28274.284047	30.957607
520.549229	28314.207786	30.962624
520.694200	28351.040183	30.967642
521.648273	28381.698410	30.972660
522.079054	28412.446353	30.977677
522.277895	28454.235796	30.982695
522.973906	28488.957980	30.987712
523.059901	28533.694852	30.992730
523.801050	28570.125826	30.997748
524.373172	28611.892701	31.002765
524.655449	28654.494958	31.007783
525.363889	28693.925983	31.012800
525.736692	28743.558300	31.017818
526.259436	28784.775591	31.022836
526.588206	28820.952764	31.027853
526.992865	28879.455388	31.032871
528.007071	28913.161574	31.037888
528.385455	28964.910662	31.042906
529.357509	29009.203494	31.047924
529.508504	29049.245121	31.052941
530.076629	29091.177888	31.057959
530.447649	29130.566740	31.062976
530.624918	29175.131842	31.067994
531.658611	29219.354694	31.073012
532.238534	29274.471466	31.078029
532.089801	29318.300828	31.083047
533.215815	29367.654397	31.088064
533.883067	29414.335343	31.093082
534.749634	29441.820474	31.098100
535.577433	29470.757395	31.103117
535.733648	29516.503872	31.108135
536.276834	29542.482718	31.113152
536.796339	29596.181515	31.118170
537.308571	29626.494818	31.123188
537.892145	29665.867378	31.128205
538.019490	29699.663921	31.133223
538.737232	29739.335497	31.138240
539.333128	29771.250224	31.143258
539.491917	29796.137311	31.148276
539.856330	29842.369584	31.153293
539.997839	29893.120725	31.158311
540.609970	29928.292401	31.163328
541.228533	29988.453306	31.168346
541.655960	30028.203670	31.173364
542.268587	30081.039196	31.178381
542.548607	30127.270896	31.183399
543.148713	30180.837754	31.188416
543.630376	30237.971717	31.193434
544.040887	30286.396552	31.198452
544.634598	30336.538222	31.203469
544.821818	30405.423400	31.208487
545.661426	30452.879033	31.213504
546.066058	30507.019945	31.218522
546.640624	30562.491901	31.223540
547.689371	30618.154155	31.228557
548.305892	30679.049817	31.233575
549.002818	30718.638803	31.238592
549.547665	30777.862065	31.243610
550.138252	30827.166300	31.248628
550.933633	30861.484851	31.253645
551.119504	30918.984080	31.258663
552.057917	30960.517042	31.263680
552.093980	31009.074270	31.268698
553.048073	31055.347514	31.273716
553.585654	31105.914349	31.278733
553.887167	31158.828479	31.283751
554.308077	31209.305153	31.288768
555.035850	31263.500293	31.293786
555.908162	31308.702695	31.298804
556.909092	31348.392467	31.303821
557.658109	31396.506728	31.308839
558.067174	31426.692475	31.313856
558.738710	31463.838733	31.318874
558.956528	31504.322548	31.323892
559.589157	31547.922553	31.328909
559.982324	31590.197309	31.333927
560.228800	31632.721348	31.338944
560.937801	31687.548967	31.343962
561.260184	31732.073535	31.348980
562.002536	31780.552875	31.353997
562.080768	31845.258963	31.359015
562.543801	31898.535760	31.364032
562.915826	31949.805514	31.369050
563.548542	32010.586196	31.374068
564.376622	32060.130856	31.379085
564.652131	32121.904051	31.384103
565.386946	32173.664540	31.389120
565.915973	32233.094159	31.394138
566.575107	32286.360604	31.399156
567.358180	32338.971667	31.404173
567.875760	32395.746643	31.409191
568.300080	32431.510868	31.414208
569.163953	32484.007529	31.419226
569.108212	32533.206315	31.424244
570.115282	32577.003456	31.429261
570.543522	32635.972000	31.434279
571.427451	32688.033478	31.439296
571.972650	32728.113676	31.444314
572.216999	32776.450668	31.449332
572.876992	32826.054653	31.454349
573.033959	32885.452351	31.459367
574.121035	32933.247743	31.464384
574.872686	32992.222010	31.469402
575.283572	33039.565481	31.474420
575.888514	33088.557917	31.479437
576.057650	33135.605381	31.484455
577.004295	33186.818096	31.489472
577.010183	33243.970614	31.494490
577.633402	33315.225516	31.499508
578.467217	33351.549447	31.504525
579.011277	33413.561956	31.509543
579.611437	33466.299190	31.514560
580.369317	33526.441847	31.519578
580.957145	33584.584549	31.524596
581.654799	33628.730780	31.529613
582.238332	33682.020636	31.534631
583.004599	33734.117934	31.539648
584.202665	33781.622001	31.544666
584.285101	33830.216798	31.549684
585.093439	33870.933008	31.554701
585.382883	33927.341630	31.559719
586.086313	33973.971517	31.564736
586.857279	34008.890485	31.569754
586.917685	34066.213007	31.574772
587.560915	34111.531176	31.579789
588.134844	34168.519869	31.584807
589.120536	34216.711624	31.589824
589.599944	34269.636015	31.594842
589.633392	34323.618514	31.599860
590.692887	34379.432672	31.604877
590.887590	34439.321380	31.609895
591.506631	34492.497084	31.614912
592.574078	34551.169866	31.619930
592.770316	34608.256216	31.624948
593.385114	34656.825150	31.629965
594.095012	34710.519321	31.634983
594.917887	34755.861985	31.640000
595.767829	34806.789732	31.645018
596.339688	34858.797340	31.650036
597.005249	34906.521857	31.655053
597.402761	34948.440807	31.660071
598.058310	35000.295611	31.665088
598.361144	35053.265172	31.670106
599.052372	35107.263561	31.675124
599.574949	35160.950131	31.680141
599.703486	35212.397144	31.685159
600.772356	35248.823510	31.690176
601.255078	35295.021182	31.695194
601.745265	35347.041028	31.700212
602.373838	35380.715066	31.705229
602.850478	35435.814867	31.710247
603.110811	35481.946957	31.715264
604.340875	35534.351904	31.720282
605.103558	35586.436222	31.725300
605.636302	35617.864037	31.730317
606.138411	35670.094241	31.735335
606.825782	35715.737128	31.740352
607.380770	35775.114007	31.745370
607.829271	35824.197485	31.750388
608.820266	35864.375566	31.755405
608.936462	35913.080636	31.760423
609.916132	35960.021833	31.765440
610.644115	36001.637245	31.770458
610.940690	36056.763465	31.775476
611.623817	36107.587722	31.780493
611.845242	36170.744450	31.785511
612.488602	36220.341673	31.790528
612.885772	36275.489198	31.795546
613.286266	36334.247299	31.800564
614.106361	36395.480968	31.805581
614.533936	36452.602920	31.810599
615.209111	36521.743552	31.815616
615.857495	36576.078765	31.820634
616.333726	36646.431324	31.825652
617.425025	36701.881033	31.830669
617.763798	36769.631396	31.835687
618.711704	36816.103610	31.840704
619.990718	36876.183892	31.845722
620.203027	36932.517211	31.850740
621.207327	36974.109604	31.855757
621.501797	37036.300372	31.860775
622.243816	37090.996708	31.865792
622.903277	37136.919405	31.870810
623.507533	37188.347312	31.875828
624.565953	37220.988355	31.880845
625.298530	37264.872309	31.885863
625.726194	37307.814270	31.890880
626.656023	37355.645145	31.895898
626.677430	37405.797227	31.900916
627.643814	37467.587095	31.905933
628.230868	37515.483425	31.910951
628.610070	37567.010929	31.915968
629.456185	37612.479851	31.920986
629.436923	37671.408861	31.926004
629.921820	37718.287831	31.931021
630.358716	37783.291440	31.936039
631.045652	37846.566759	31.941056
631.604485	37901.369505	31.946074
631.886548	37970.380927	31.951092
632.858522	38030.476570	31.956109
633.214301	38093.970468	31.961127
633.663210	38166.410688	31.966144
634.558575	38221.210399	31.971162
635.064867	38294.307372	31.976180
635.781887	38351.906529	31.981197
636.241355	38405.957544	31.986215
637.005674	38468.126333	31.991232
637.390435	38527.920130	31.996250
637.803540	38604.983492	32.001268
638.501195	38659.433245	32.006285
638.993415	38735.615466	32.011303
639.788915	38794.601054	32.016320
640.769188	38854.846343	32.021338
641.180343	38928.792390	32.026356
642.131489	38987.862425	32.031373
643.171286	39057.392115	32.036391
643.623199	39109.631258	32.041408
644.521085	39168.543678	32.046426
644.816457	39238.248935	32.051444
645.919397	39293.969678	32.056461
646.424898	39352.309043	32.061479
647.148647	39424.934423	32.066496
647.830768	39478.641052	32.071514
648.307221	39547.369353	32.076532
648.548183	39600.870940	32.081549
648.898976	39672.298378	32.086567
649.400579	39744.565283	32.091584
650.272503	39806.991654	32.096602
650.781850	39888.833119	32.101620
651.917476	39956.913314	32.106637
652.795405	40026.275483	32.111655
653.260208	40093.940713	32.116672
654.573532	40163.475061	32.121690
655.153929	40225.772830	32.126708
655.694044	40284.244956	32.131725
656.086932	40340.125221	32.136743
656.191987	40407.856380	32.141760
657.243035	40464.644028	32.146778
657.843851	40548.073407	32.151796
658.688847	40615.492288	32.156813
659.477061	40682.785382	32.161831
660.189182	40741.248422	32.166848
660.862516	40796.343228	32.171866
661.368151	40866.564775	32.176884
662.070734	40928.922899	32.181901
662.799515	40997.559666	32.186919
663.325498	41056.661776	32.191936
664.346069	41127.503318	32.196954
664.712287	41195.318889	32.201972
665.586341	41259.129509	32.206989
666.214082	41320.071509	32.212007
666.367267	41392.413976	32.217024
667.130335	41459.584733	32.222042
667.739560	41524.404612	32.227060
668.294303	41595.536117	32.232077
668.898823	41665.892127	32.237095
669.194521	41739.022961	32.242112
670.447859	41806.262531	32.247130
670.801177	41874.584800	32.252148
671.156925	41941.789179	32.257165
671.944967	41997.265714	32.262183
672.833400	42082.758678	32.267200
673.230414	42154.399256	32.272218
673.967186	42219.177590	32.277236
674.607084	42286.097716	32.282253
675.309999	42359.416966	32.287271
675.982137	42427.314049	32.292288
676.738287	42501.673022	32.297306
677.582014	42577.577098	32.302324
678.074884	42645.120463	32.307341
679.118728	42723.134806	32.312359
679.590621	42797.319459	32.317376
680.378673	42872.706955	32.322394
680.862283	42937.155385	32.327412
681.398369	43009.236404	32.332429
682.508469	43082.684494	32.337447
683.062965	43158.438377	32.342464
683.562276	43224.258661	32.347482
684.372622	43304.822571	32.352500
685.266687	43375.962689	32.357517
686.219785	43443.048002	32.362535
686.694791	43518.798005	32.367552
687.651600	43581.715049	32.372570
688.262546	43652.061609	32.377588
689.381245	43713.514610	32.382605
690.169738	43772.930813	32.387623
690.790115	43838.612509	32.392640
691.722658	43888.032304	32.397658
691.893291	43954.811395	32.402676
692.465206	44019.602065	32.407693
693.410772	44089.352956	32.412711
693.864326	44160.315715	32.417728
694.402790	44231.106304	32.422746
695.022098	44297.632908	32.427764
695.599743	44364.012150	32.432781
696.871654	44426.653828	32.437799
697.145578	44509.155776	32.442816
697.930308	44579.457069	32.447834
698.657017	44658.215840	32.452852
699.346171	44726.917226	32.457869
699.679736	44795.477671	32.462887
701.048364	44876.476852	32.467904
701.399939	44945.628438	32.472922
702.084442	45020.754874	32.477940
702.811591	45084.458371	32.482957
703.437336	45161.951249	32.487975
703.669485	45233.751750	32.492992
704.381874	45312.300945	32.498010
705.375445	45390.331758	32.503028
706.030158	45461.277551	32.508045
707.064654	45536.592394	32.513063
707.740070	45594.284142	32.518080
709.155825	45643.556268	32.523098
709.632276	45695.759021	32.528116
710.538661	45754.378048	32.533133
711.373339	45803.254315	32.538151
712.105934	45866.621588	32.543168
712.952586	45904.897611	32.548186
713.966433	45965.425302	32.553204
714.318265	46003.874713	32.558221
714.894345	46047.739812	32.563239
715.351929	46108.688529	32.568256
715.900335	46161.805556	32.573274
716.874710	46225.290510	32.578292
717.125975	46291.233402	32.583309
718.207239	46357.160670	32.588327
719.106972	46419.042085	32.593344
719.449955	46473.720556	32.598362
720.293311	46533.871852	32.603380
720.354747	46608.337523	32.608397
721.082724	46672.996802	32.613415
721.824064	46756.189529	32.618432
722.353564	46832.859277	32.623450
722.897150	46906.134976	32.628468
723.252134	46986.385087	32.633485
724.214632	47057.517796	32.638503
724.796001	47144.377922	32.643520
725.640811	47216.630460	32.648538
726.767325	47302.851539	32.653556
727.407559	47386.418046	32.658573
728.089235	47467.283766	32.663591
728.703194	47546.926514	32.668608
729.402176	47620.806829	32.673626
730.239226	47703.412444	32.678644
731.114328	47783.330433	32.683661
731.965883	47858.234106	32.688679
732.639490	47950.555562	32.693696
733.146706	48028.358285	32.698714
734.843948	48100.130174	32.703732
735.267980	48176.273776	32.708749
736.063311	48236.410207	32.713767
737.169179	48310.921489	32.718784
738.100084	48374.929516	32.723802
740.057808	48419.539339	32.728820
740.107276	48477.868137	32.733837
741.416873	48521.439527	32.738855
741.876542	48582.073565	32.743872
742.642996	48620.634069	32.748890
743.397374	48674.452379	32.753908
743.689855	48730.737809	32.758925
744.210664	48785.758777	32.763943
744.784445	48857.309003	32.768960
745.387753	48908.803880	32.773978
745.719382	48979.492687	32.778996
746.603567	49054.913421	32.784013
747.238645	49125.904546	32.789031
747.758133	49192.721099	32.794048
748.407442	49259.945217	32.799066
748.910466	49326.714514	32.804084
749.477547	49391.135674	32.809101
750.331724	49454.844555	32.814119
751.325344	49535.801322	32.819136
751.891338	49605.890023	32.824154
752.767532	49673.278865	32.829172
753.069672	49755.662688	32.834189
753.374734	49829.934788	32.839207
754.243871	49921.167660	32.844224
754.946118	50004.539015	32.849242
755.963205	50083.958897	32.854260
756.589007	50168.102147	32.859277
757.360895	50245.012405	32.864295
758.124688	50335.153371	32.869312
758.927862	50425.730241	32.874330
760.064760	50498.819996	32.879348
760.532143	50588.077892	32.884365
761.451823	50664.332721	32.889383
762.215289	50758.525338	32.894400
762.512035	50842.702588	32.899418
763.639660	50924.273947	32.904436
764.255453	51016.098662	32.909453
764.990343	51101.364451	32.914471
765.840391	51184.759753	32.919488
766.311510	51282.005948	32.924506
767.050005	51367.594490	32.929524
767.912533	51470.081625	32.934541
769.056770	51554.748562	32.939559
769.781984	51648.459208	32.944576
770.546993	51726.115674	32.949594
771.770662	51804.091922	32.954612
772.247566	51901.738232	32.959629
773.256910	51986.329048	32.964647
774.077527	52077.201199	32.969664
774.634046	52159.690562	32.974682
776.046841	52233.244991	32.979700
776.562879	52321.144023	32.984717
777.120266	52393.676700	32.989735
778.233362	52484.917639	32.994752
778.752577	52564.167492	32.999770
779.938088	52645.078986	33.004788
780.658457	52732.104513	33.009805
781.694721	52802.275742	33.014823
782.304876	52876.949406	33.019840
783.274205	52960.237031	33.024858
784.081938	53022.625975	33.029876
784.595336	53116.329335	33.034893
785.653851	53198.105208	33.039911
786.232047	53264.325334	33.044928
786.892222	53342.018760	33.049946
787.781362	53415.332412	33.054964
788.650503	53494.911492	33.059981
789.355585	53584.483465	33.064999
790.245977	53648.869550	33.070016
791.309917	53713.106064	33.075034
791.913399	53772.941705	33.080052
792.104474	53840.361108	33.085069
792.987407	53908.938620	33.090087
793.865875	53986.932076	33.095104
794.339025	54065.690329	33.100122
795.379331	54138.367842	33.105140
795.898037	54218.477439	33.110157
796.564180	54293.443835	33.115175
797.257880	54378.996232	33.120192
798.065670	54455.594523	33.125210
799.152716	54537.478454	33.130228
799.730643	54636.081422	33.135245
800.418784	54711.323657	33.140263
800.953026	54806.794416	33.145280
801.386824	54896.639929	33.150298
802.487545	54979.079407	33.155316
803.282771	55080.686825	33.160333
803.743741	55180.348845	33.165351
804.686913	55275.897143	33.170368
805.259307	55377.146126	33.175386
806.349002	55476.973660	33.180404
807.065246	55577.731396	33.185421
807.952891	55679.774693	33.190439
808.724106	55773.320007	33.195456
809.347737	55876.793457	33.200474
810.113062	55974.625240	33.205492
811.270168	56071.758454	33.210509
811.963668	56176.472725	33.215527
813.505426	56267.221558	33.220544
814.264691	56357.352805	33.225562
815.381510	56447.360020	33.230580
816.372689	56540.176083	33.235597
816.976468	56614.700528	33.240615
818.349731	56703.988773	33.245632
819.089201	56791.685986	33.250650
820.542725	56853.180032	33.255668
821.653924	56935.897512	33.260685
822.537967	56997.672811	33.265703
823.509401	57061.234452	33.270720
824.068170	57137.784533	33.275738
825.288556	57199.313251	33.280756
826.128635	57268.250886	33.285773
826.403728	57337.904867	33.290791
827.493846	57407.413174	33.295808
827.586071	57477.503425	33.300826
828.422730	57554.367721	33.305844
829.462817	57623.866382	33.310861
830.160826	57699.187641	33.315879
830.722021	57780.997918	33.320896
831.517368	57868.614398	33.325914
832.471260	57935.588264	33.330932
832.880278	58020.073649	33.335949
833.311933	58110.824998	33.340967
834.324108	58193.002100	33.345984
835.278517	58281.585373	33.351002
836.109704	58353.814684	33.356020
836.815264	58438.503824	33.361037
837.559246	58513.245098	33.366055
838.408429	58585.642796	33.371072
838.774047	58674.101097	33.376090
839.700029	58761.945547	33.381108
840.712180	58853.921721	33.386125
841.285425	58945.271930	33.391143
842.328262	59029.570787	33.396160
843.011102	59129.328059	33.401178
843.760677	59216.964511	33.406196
844.636591	59313.529418	33.411213
845.573337	59399.788347	33.416231
846.522523	59500.076974	33.421248
847.200232	59603.067205	33.426266
848.006694	59686.638159	33.431284
848.825098	59786.356458	33.436301
849.252941	59885.920914	33.441319
850.693183	59980.780567	33.446336
851.537008	60082.651290	33.451354
852.677732	60173.157634	33.456372
853.457812	60270.287050	33.461389
854.009551	60355.731048	33.466407
855.266212	60454.366218	33.471424
855.893776	60552.414319	33.476442
856.995297	60646.804121	33.481460
858.756980	60716.398336	33.486477
859.703750	60796.656619	33.491495
860.847226	60873.379746	33.496512
861.625300	60961.985879	33.501530
862.364547	61038.386955	33.506548
862.862309	61121.555194	33.511565
863.365506	61203.306933	33.516583
864.485968	61297.860825	33.521600
864.881380	61380.485065	33.526618
865.813092	61480.969672	33.531636
866.790927	61572.034723	33.536653
867.243454	61670.762877	33.541671
868.193815	61763.780391	33.546688
868.806448	61866.812065	33.551706
869.729098	61959.734068	33.556724
870.798045	62059.603788	33.561741
871.398707	62153.447819	33.566759
872.592995	62253.221151	33.571776
873.081641	62357.951652	33.576794
874.371648	62455.844766	33.581812
874.916098	62561.350588	33.586829
875.296127	62669.571722	33.591847
876.679013	62770.061170	33.596864
877.274302	62879.618292	33.601882
878.230071	62992.679606	33.606900
879.388418	63085.243883	33.611917
880.093331	63186.692228	33.616935
880.833234	63282.521458	33.621952
881.475778	63381.610818	33.626970
882.614764	63478.927734	33.631988
883.110099	63570.046255	33.637005
883.792266	63680.484067	33.642023
884.507183	63792.788105	33.647040
885.593213	63906.141829	33.652058
886.313048	64006.516889	33.657076
887.257446	64106.499945	33.662093
887.952780	64224.682687	33.667111
889.041647	64330.970318	33.672128
890.073105	64455.045753	33.677146
890.839232	64547.702649	33.682164
892.293538	64651.014866	33.687181
893.016439	64759.864557	33.692199
894.175787	64859.978768	33.697216
894.899965	64960.490413	33.702234
896.161702	65079.036155	33.707252
897.147193	65174.990037	33.712269
897.689234	65282.349753	33.717287
898.678218	65378.480986	33.722304
899.595369	65493.395870	33.727322
900.490694	65592.389156	33.732340
901.176627	65698.525102	33.737357
902.089778	65812.386572	33.742375
903.075077	65919.597747	33.747392
903.821366	66038.882048	33.752410
904.841629	66147.428752	33.757428
905.624199	66253.860738	33.762445
906.584105	66368.943766	33.767463
907.559966	66473.895887	33.772480
908.446348	66593.968612	33.777498
909.286535	66711.217373	33.782516
910.364767	66819.087387	33.787533
911.212090	66951.125045	33.792551
911.800983	67055.507715	33.797568
912.801832	67175.425021	33.802586
913.872417	67298.688487	33.807604
914.942041	67399.196810	33.812621
915.569771	67521.032560	33.817639
916.746305	67630.894216	33.822656
917.772171	67745.037600	33.827674
918.632607	67854.303273	33.832692
919.744472	67959.517641	33.837709
920.948168	68067.492627	33.842727
921.915041	68174.490698	33.847744
923.017443	68278.917871	33.852762
924.471088	68385.365723	33.857780
925.684526	68471.096209	33.862797
926.591296	68553.218417	33.867815
927.560108	68650.512408	33.872832
928.425164	68742.032496	33.877850
929.221551	68848.007142	33.882868
930.087372	68932.528021	33.887885
931.211660	69036.126782	33.892903
931.995408	69106.087076	33.897920
932.804117	69186.521190	33.902938
933.746183	69271.858713	33.907956
934.447617	69351.287420	33.912973
935.078026	69443.280672	33.917991
936.292334	69540.087682	33.923008
936.758724	69629.612035	33.928026
937.716871	69735.139670	33.933044
938.404039	69824.500551	33.938061
938.931545	69934.219560	33.943079
939.907630	70031.037952	33.948096
940.846653	70146.239724	33.953114
941.626481	70255.101396	33.958132
942.506838	70356.927047	33.963149
943.162881	70481.127154	33.968167
944.302054	70594.241807	33.973184
945.254394	70706.313993	33.978202
945.642405	70836.424235	33.983220
946.924721	70957.300964	33.988237
947.729170	71087.948492	33.993255
948.623112	71195.638055	33.998272
949.786670	71326.099037	34.003290
950.581123	71453.544192	34.008308
951.967560	71565.698246	34.013325
952.359251	71710.478648	34.018343
953.295843	71825.708713	34.023360
954.872509	71949.633061	34.028378
955.431819	72073.428769	34.033396
956.737086	72194.953507	34.038413
957.555099	72311.629401	34.043431
958.535534	72446.802101	34.048448
959.485383	72568.237990	34.053466
960.198640	72701.895894	34.058484
961.827251	72817.499655	34.063501
962.798000	72934.095786	34.068519
964.313832	73042.427916	34.073536
965.459331	73157.186494	34.078554
966.609274	73266.828324	34.083572
968.063693	73366.292860	34.088589
968.865873	73473.591922	34.093607
970.207068	73565.000182	34.098624
971.175227	73661.690573	34.103642
971.871225	73764.778016	34.108660
972.975283	73863.299164	34.113677
973.796816	73969.477843	34.118695
974.736411	74069.362603	34.123712
975.647275	74176.924765	34.128730
976.526036	74285.795871	34.133748
977.501005	74388.515883	34.138765
977.932791	74490.311073	34.143783
979.035746	74603.806825	34.148800
980.254542	74712.862150	34.153818
980.980100	74822.818403	34.158836
981.972313	74932.830739	34.163853
982.837111	75031.461308	34.168871
983.924036	75134.956240	34.173888
985.045682	75223.967461	34.178906
985.768416	75320.985431	34.183924
987.003141	75415.854136	34.188941
987.915518	75524.763513	34.193959
988.433198	75631.748554	34.198976
989.754882	75729.216035	34.203994
990.599907	75837.891788	34.209012
991.671764	75934.447824	34.214029
992.526432	76048.347682	34.219047
993.176693	76149.385626	34.224064
994.737421	76264.196719	34.229082
995.541089	76366.885616	34.234100
996.586897	76465.086700	34.239117
997.417849	76576.924874	34.244135
998.082054	76689.848526	34.249152
999.566641	76800.772544	34.254170
1000.447119	76917.120401	34.259188
1001.577430	77019.421094	34.264205
1002.267714	77135.872234	34.269223
1003.160441	77245.881365	34.274240
1004.190669	77363.110463	34.279258
1005.259057	77485.286720	34.284276
1006.589694	77603.186765	34.289293
1007.735495	77730.234620	34.294311
1008.085222	77849.284424	34.299328
1009.270304	77964.421570	34.304346
1010.167486	78078.337086	34.309364
1011.305906	78202.725640	34.314381
1011.932132	78332.358284	34.319399
1013.116347	78453.267392	34.324416
1014.440393	78572.748811	34.329434
1015.018972	78716.410408	34.334452
1015.864564	78831.901098	34.339469
1016.935382	78967.692503	34.344487
1018.080619	79100.688435	34.349504
1019.037305	79232.306675	34.354522
1019.972282	79371.305860	34.359540
1020.629827	79487.331855	34.364557
1021.896051	79633.443655	34.369575
1023.133228	79772.216399	34.374592
1024.288431	79897.807047	34.379610
1025.145150	80039.695910	34.384628
1026.654385	80163.822919	34.389645
1027.738260	80290.218752	34.394663
1028.877481	80408.292666	34.399680
1029.813682	80534.613909	34.404698
1030.900056	80666.888826	34.409716
1032.038649	80783.300868	34.414733
1033.484124	80903.083710	34.419751
1034.665047	81011.170017	34.424768
1036.126806	81120.360219	34.429786
1036.970730	81244.334948	34.434804
1037.981451	81344.828151	34.439821
1039.008738	81457.555134	34.444839
1039.858236	81562.031190	34.449856
1041.010659	81656.142948	34.454874
1041.321496	81758.073794	34.459892
1042.396652	81865.568505	34.464909
1043.347692	81981.170901	34.469927
1044.075049	82100.899450	34.474944
1045.483088	82214.077422	34.479962
1045.971583	82339.744949	34.484980
1047.152012	82457.632498	34.489997
1048.489190	82572.260617	34.495015
1048.927090	82696.420215	34.500032
1050.090561	82825.264948	34.505050
1050.948360	82951.131965	34.510068
1051.771319	83073.202910	34.515085
1052.854725	83203.385856	34.520103
1053.873531	83343.881582	34.525120
1055.203475	83469.879362	34.530138
1055.762111	83610.215042	34.535156
1057.258110	83753.314370	34.540173
1058.516186	83896.252832	34.545191
1059.533840	84020.168345	34.550208
1060.931754	84145.525375	34.555226
1061.413826	84289.674803	34.560244
1062.213034	84436.339856	34.565261
1063.179198	84578.180821	34.570279
1064.231281	84720.463530	34.575296
1065.812419	84850.690645	34.580314
1067.018378	84990.493456	34.585332
1068.235583	85128.605630	34.590349
1069.760550	85261.552968	34.595367
1070.914703	85383.319795	34.600384
1072.173690	85506.822149	34.605402
1072.990552	85648.581221	34.610420
1074.297110	85771.001050	34.615437
1075.465822	85893.078087	34.620455
1076.740619	86035.552080	34.625472
1077.904964	86140.589535	34.630490
1078.543766	86264.366566	34.635508
1079.688136	86396.157787	34.640525
1081.106451	86510.303989	34.645543
1082.079073	86642.784124	34.650560
1083.212012	86765.599530	34.655578
1084.162604	86896.793876	34.660596
1085.628612	87017.420902	34.665613
1086.448547	87132.476251	34.670631
1087.003871	87260.993750	34.675648
1088.010804	87404.249581	34.680666
1089.415445	87538.344099	34.685684
1089.989714	87676.473603	34.690701
1091.047809	87813.457860	34.695719
1092.188448	87947.188514	34.700736
1093.667611	88065.983286	34.705754
1094.660705	88206.588253	34.710772
1096.104842	88335.851687	34.715789
1097.246017	88470.110449	34.720807
1097.704717	88598.474458	34.725824
1099.285336	88714.337495	34.730842
1099.901907	88831.309151	34.735860
1100.813651	88963.148022	34.740877
1101.959384	89091.276776	34.745895
1102.970563	89227.688537	34.750912
1103.719822	89351.285401	34.755930
1104.602004	89482.904328	34.760948
1105.551950	89626.202143	34.765965
1106.574323	89774.836495	34.770983
1107.684975	89918.924980	34.776000
1109.192010	90056.737534	34.781018
1110.735752	90193.076210	34.786036
1111.494965	90334.012093	34.791053
1112.838047	90458.753464	34.796071
1113.872504	90598.789302	34.801088
1115.305879	90734.909400	34.806106
1116.440490	90880.695751	34.811124
1117.614192	91016.570729	34.816141
1119.011023	91142.103906	34.821159
1119.687413	91287.173624	34.826176
1121.416847	91418.885830	34.831194
1122.546469	91553.264912	34.836212
1123.123384	91682.125010	34.841229
1124.629354	91818.561527	34.846247
1125.743637	91961.762652	34.851264
1126.863229	92092.114406	34.856282
1128.053409	92237.836027	34.861300
1128.848211	92376.460898	34.866317
1130.545082	92506.424844	34.871335
1131.570111	92655.304136	34.876352
1132.186480	92791.657827	34.881370
1133.573679	92924.753320	34.886388
1134.501934	93077.740853	34.891405
1135.641019	93211.500705	34.896423
1136.836396	93354.189635	34.901440
1138.255049	93496.068894	34.906458
1139.094358	93636.250406	34.911476
1140.236578	93788.762589	34.916493
1141.612159	93929.208428	34.921511
1142.576430	94078.942263	34.926528
1143.876329	94223.333781	34.931546
1144.839792	94367.245663	34.936564
1145.901509	94511.685961	34.941581
1147.605496	94659.175982	34.946599
1148.382288	94806.211568	34.951616
1149.514264	94940.937829	34.956634
1150.692042	95091.900942	34.961652
1151.453212	95239.498828	34.966669
1153.166276	95380.958585	34.971687
1154.385099	95533.227752	34.976704
1155.630879	95672.217931	34.981722
1157.068507	95820.064263	34.986740
1157.892125	95965.383020	34.991757
1159.294155	96095.068003	34.996775
1160.130211	96228.066572	35.001792
1161.249226	96357.180944	35.006810
1162.724365	96476.143689	35.011828
1163.043583	96613.911246	35.016845
1164.296401	96753.507614	35.021863
1165.323959	96892.877419	35.026880
1166.760941	97018.142180	35.031898
1168.017151	97149.592223	35.036916
1169.042921	97294.358538	35.041933
1170.132915	97429.143277	35.046951
1170.856368	97579.015149	35.051968
1172.516013	97724.454119	35.056986
1173.561646	97865.598882	35.062004
1174.060722	98011.890292	35.067021
1175.589121	98156.132275	35.072039
1176.885783	98316.451850	35.077056
1177.985615	98467.423128	35.082074
1179.087612	98618.420252	35.087092
1179.927078	98779.276856	35.092109
1181.430840	98932.657295	35.097127
1182.192692	99096.251685	35.102144
1183.346076	99252.904073	35.107162
1184.821930	99410.863491	35.112180
1185.550879	99585.857070	35.117197
1187.087436	99740.566348	35.122215
1188.279284	99915.235980	35.127232
1189.342332	100080.209675	35.132250
1190.790867	100249.360698	35.137268
1191.741390	100419.034978	35.142285
1193.144057	100581.395683	35.147303
1193.964052	100751.708672	35.152320
1195.050988	100931.164680	35.157338
1196.688415	101101.859239	35.162356
1197.545204	101279.121867	35.167373
1199.078563	101438.654147	35.172391
1200.610618	101607.217165	35.177408
1201.916514	101774.996815	35.182426
1203.289199	101935.762742	35.187444
1204.565013	102098.458564	35.192461
1206.101612	102253.347434	35.197479
1207.296751	102419.199846	35.202496
1208.781489	102574.327452	35.207514
1209.661720	102722.365917	35.212532
1210.925235	102894.174690	35.217549
1212.488121	103037.652728	35.222567
1213.504670	103197.208198	35.227584
1215.091792	103349.802530	35.232602
1216.314909	103505.309698	35.237620
1217.547427	103663.260543	35.242637
1218.875601	103812.811584	35.247655
1220.040526	103959.187099	35.252672
1221.503517	104106.348310	35.257690
1222.954504	104238.491206	35.262708
1223.785390	104380.341348	35.267725
1225.119242	104523.740001	35.272743
1226.027259	104674.900356	35.277760
1226.978192	104804.117248	35.282778
1228.074460	104931.625342	35.287796
1229.026893	105086.352166	35.292813
1230.113987	105226.858372	35.297831
1231.213887	105381.283008	35.302848
1232.268044	105533.829127	35.307866
1233.684683	105684.414146	35.312884
1234.585183	105846.601919	35.317901
1235.808484	106002.908936	35.322919
1237.016499	106163.386700	35.327936
1237.532832	106329.962368	35.332954
1239.250033	106495.459506	35.337972
1240.450691	106671.103334	35.342989
1241.572211	106828.243222	35.348007
1243.076130	107011.259998	35.353024
1244.044909	107184.198175	35.358042
1245.405257	107345.176222	35.363060
1246.562514	107534.576648	35.368077
1248.033904	107701.415272	35.373095
1249.542197	107874.164150	35.378112
1250.876039	108050.300797	35.383130
1252.145570	108212.186228	35.388148
1253.209519	108388.611939	35.393165
1254.954540	108551.038685	35.398183
1256.238833	108713.190574	35.403200
1257.555931	108888.866796	35.408218
1258.879522	109051.064629	35.413236
1259.854151	109219.593690	35.418253
1261.130742	109380.458732	35.423271
1262.857264	109549.545168	35.428288
1264.229577	109720.213434	35.433306
1265.762813	109884.381834	35.438324
1267.043755	110059.222960	35.443341
1268.406128	110219.609494	35.448359
1269.443348	110379.279853	35.453376
1270.385439	110548.544692	35.458394
1271.862828	110698.437582	35.463412
1273.383000	110857.837999	35.468429
1274.897025	111024.524811	35.473447
1275.891854	111179.164936	35.478464
1277.163781	111350.671221	35.483482
1278.597083	111504.883372	35.488500
1279.589476	111672.132095	35.493517
1281.279308	111833.536072	35.498535
1282.750350	112002.123756	35.503552
1283.828787	112158.693350	35.508570
1285.084632	112311.179319	35.513588
1286.107955	112481.227461	35.518605
1287.389424	112645.037152	35.523623
1288.772208	112811.262974	35.528640
1289.729440	112985.506371	35.533658
1291.039973	113148.211769	35.538676
1292.240038	113315.485403	35.543693
1293.483145	113479.939989	35.548711
1294.617416	113632.618623	35.553728
1295.597301	113803.746424	35.558746
1297.266904	113955.384925	35.563764
1298.154683	114118.979138	35.568781
1299.213445	114282.012882	35.573799
1301.055148	114445.356995	35.578816
1302.159505	114611.007531	35.583834
1303.495874	114773.477090	35.588852
1304.707401	114945.560382	35.593869
1305.878799	115117.360158	35.598887
1307.435600	115269.759845	35.603904
1308.416363	115453.833950	35.608922
1310.042703	115620.376611	35.613940
1311.233171	115799.804929	35.618957
1312.552948	115971.774480	35.623975
1313.492916	116159.141813	35.628992
1314.485642	116348.224579	35.634010
1315.763599	116527.160949	35.639028
1317.087917	116707.788418	35.644045
1318.079643	116896.735556	35.649063
1319.590841	117087.863163	35.654080
1321.038993	117290.318341	35.659098
1322.508958	117471.039670	35.664116
1323.475246	117667.307588	35.669133
1325.234287	117859.322859	35.674151
1326.721708	118048.471398	35.679168
1327.718762	118238.972271	35.684186
1329.358901	118427.488873	35.689204
1330.643179	118630.969796	35.694221
1332.175738	118823.891850	35.699239
1333.235587	119004.996976	35.704256
1334.551632	119206.550282	35.709274
1336.309595	119394.077154	35.714292
1337.598094	119595.473091	35.719309
1339.068755	119789.653945	35.724327
1340.783861	119967.852208	35.729344
1342.164393	120163.546296	35.734362
1343.489753	120343.866487	35.739380
1344.782048	120529.832805	35.744397
1345.781007	120718.676533	35.749415
1347.527902	120908.369251	35.754432
1348.713819	121109.856366	35.759450
1350.499780	121285.883306	35.764468
1352.037194	121477.377045	35.769485
1353.603687	121657.524488	35.774503
1355.228666	121828.170699	35.779520
1356.091631	122008.415316	35.784538
1357.710766	122191.535191	35.789556
1359.152939	122367.487904	35.794573
1360.586089	122547.562107	35.799591
1362.055258	122715.020911	35.804608
1363.144011	122906.917369	35.809626
1364.465496	123076.051034	35.814644
1366.016002	123255.881231	35.819661
1367.081398	123428.039054	35.824679
1368.372539	123592.250610	35.829696
1369.255934	123762.971287	35.834714
1370.684179	123932.965953	35.839732
1371.941465	124104.929987	35.844749
1372.742841	124277.986964	35.849767
1374.663618	124446.683450	35.854784
1375.859074	124638.103579	35.859802
1377.361045	124809.003049	35.864820
1378.786805	124980.182680	35.869837
1380.130890	125162.087348	35.874855
1381.305827	125340.143563	35.879872
1382.446799	125539.031371	35.884890
1384.383665	125692.737601	35.889908
1386.649970	125863.144518	35.894925
1388.026794	126025.668637	35.899943
1389.390472	126191.884313	35.904960
1390.632664	126370.619394	35.909978
1392.143186	126539.917215	35.914996
1393.280287	126715.313319	35.920013
1394.473081	126889.712195	35.925031
1395.867348	127064.483176	35.930048
1397.145669	127250.695633	35.935066
1398.664443	127430.390804	35.940084
1399.991032	127612.401520	35.945101
1401.199689	127803.547342	35.950119
1402.969342	127984.711159	35.955136
1404.022723	128174.060484	35.960154
1405.205050	128364.022673	35.965172
1406.925410	128550.661523	35.970189
1408.293364	128745.119581	35.975207
1410.292585	128919.556468	35.980224
1411.796649	129104.739807	35.985242
1413.614745	129278.651909	35.990260
1415.174190	129455.752981	35.995277
1416.002352	129633.550637	36.000295
1417.619362	129801.985738	36.005312
1419.041615	129993.577224	36.010330
1420.446774	130165.232330	36.015348
1421.680707	130351.812862	36.020365
1422.974109	130543.518421	36.025383
1424.522146	130725.154099	36.030400
1425.459563	130918.228536	36.035418
1426.926116	131105.318731	36.040436
1428.292956	131296.242894	36.045453
1430.029839	131501.937198	36.050471
1431.261922	131689.730114	36.055488
1432.758952	131882.701847	36.060506
1434.151643	132074.361451	36.065524
1435.587154	132260.880458	36.070541
1437.044232	132457.665690	36.075559
1438.676359	132638.422933	36.080576
1440.345902	132831.890541	36.085594
1441.687180	133020.851459	36.090612
1443.102268	133224.862162	36.095629
1443.940255	133411.870322	36.100647
1445.618600	133585.106838	36.105664
1447.061742	133768.996086	36.110682
1448.423699	133940.171371	36.115700
1450.062333	134114.368324	36.120717
1451.104655	134304.376661	36.125735
1452.319679	134484.822392	36.130752
1453.681445	134667.120398	36.135770
1454.959998	134861.719123	36.140788
1456.180306	135056.392345	36.145805
1457.444021	135251.135345	36.150823
1459.011729	135456.414201	36.155840
1460.419428	135658.526636	36.160858
1461.748394	135864.216532	36.165876
1463.223994	136073.508778	36.170893
1464.299121	136289.616117	36.175911
1465.944120	136494.254129	36.180928
1467.597973	136720.750828	36.185946
1468.992844	136935.095878	36.190964
1470.394312	137142.645009	36.195981
1471.656184	137372.509779	36.200999
1473.960101	137586.386380	36.206016
1475.285509	137804.527299	36.211034
1476.335784	138019.673567	36.216052
1477.854975	138242.260048	36.221069
1479.216956	138458.699784	36.226087
1480.688819	138689.120736	36.231104
1482.241873	138922.978304	36.236122
1483.883832	139143.901204	36.241140
1485.870412	139353.164165	36.246157
1487.582388	139577.628308	36.251175
1489.364109	139780.233725	36.256192
1490.999022	139997.359170	36.261210
1492.827905	140205.728590	36.266228
1494.575144	140405.959618	36.271245
1496.137708	140606.324843	36.276263
1497.838973	140806.971817	36.281280
1499.506547	141005.571417	36.286298
1501.169228	141211.591283	36.291316
1502.761040	141396.777028	36.296333
1503.945764	141593.611163	36.301351
1505.457839	141781.716524	36.306368
1507.327511	141982.468191	36.311386
1508.694926	142182.076870	36.316404
1510.222856	142368.001464	36.321421
1511.480009	142572.399367	36.326439
1513.354557	142758.989526	36.331456
1514.175236	142961.904540	36.336474
1515.586103	143154.752003	36.341492
1517.415481	143352.462038	36.346509
1518.358364	143579.784462	36.351527
1520.144532	143779.241637	36.356544
1521.014384	143984.183102	36.361562
1522.324461	144198.244789	36.366580
1523.954460	144413.280239	36.371597
1525.451708	144626.652968	36.376615
1527.185649	144831.273813	36.381632
1528.379778	145037.091539	36.386650
1529.891647	145243.731133	36.391668
1531.509101	145424.634012	36.396685
1532.799570	145627.001663	36.401703
1534.443941	145825.048556	36.406720
1536.460013	146023.971421	36.411738
1537.995355	146235.749038	36.416756
1539.353805	146442.814813	36.421773
1540.804638	146642.903099	36.426791
1542.641677	146841.417122	36.431808
1544.022135	147040.720585	36.436826
1545.668145	147248.287029	36.441844
1547.280087	147442.264236	36.446861
1548.885548	147649.497417	36.451879
1550.671814	147845.869371	36.456896
1552.137508	148042.398682	36.461914
1553.682465	148254.033976	36.466932
1555.145599	148451.174669	36.471949
1556.570801	148662.185905	36.476967
1558.166168	148865.635191	36.481984
1559.892040	149070.762844	36.487002
1561.155583	149290.315951	36.492020
1562.814782	149502.217751	36.497037
1564.618350	149721.338486	36.502055
1566.060238	149935.829338	36.507072
1567.459678	150149.390049	36.512090
1569.071771	150366.987138	36.517108
1570.951685	150579.022055	36.522125
1572.655222	150809.518427	36.527143
1573.897544	151012.151712	36.532160
1575.525249	151221.227168	36.537178
1576.879305	151449.808425	36.542196
1578.954302	151666.813605	36.547213
1580.091310	151898.314023	36.552231
1581.162528	152117.383482	36.557248
1582.750967	152347.616977	36.562266
1584.185786	152588.228877	36.567284
1586.091269	152813.146696	36.572301
1587.572426	153054.983966	36.577319
1589.181235	153288.822030	36.582336
1590.708968	153522.497767	36.587354
1592.213596	153762.737055	36.592372
1594.234541	153993.464346	36.597389
1595.491527	154235.258417	36.602407
1596.924195	154474.791276	36.607424
1598.754945	154710.959247	36.612442
1599.547096	154960.169441	36.617460
1601.514079	155190.989024	36.622477
1603.423651	155446.607550	36.627495
1604.793432	155691.689409	36.632512
1606.830704	155934.552699	36.637530
1607.921181	156186.624503	36.642548
1609.608170	156424.400197	36.647565
1611.668894	156669.801082	36.652583
1613.066312	156895.513905	36.657600
1615.142107	157115.821760	36.662618
1616.651539	157339.805238	36.667636
1617.873429	157547.803624	36.672653
1619.537763	157766.206318	36.677671
1621.121988	157995.496176	36.682688
1622.490695	158223.441354	36.687706
1623.746324	158459.628056	36.692724
1625.562764	158700.591830	36.697741
1627.121458	158942.501865	36.702759
1628.560630	159174.055934	36.707776
1630.156928	159416.951860	36.712794
1631.679611	159665.114198	36.717812
1633.590133	159905.421798	36.722829
1634.967159	160150.465540	36.727847
1636.583752	160394.632361	36.732864
1638.594766	160638.479362	36.737882
1639.902642	160901.961202	36.742900
1642.051414	161146.320421	36.747917
1643.428866	161397.956072	36.752935
1644.827973	161651.721011	36.757952
1646.933723	161903.488776	36.762970
1648.766126	162155.913798	36.767988
1650.603700	162394.636608	36.773005
1652.858115	162641.561898	36.778023
1654.215003	162892.905310	36.783040
1656.047195	163128.600676	36.788058
1657.928524	163374.046037	36.793076
1659.994450	163593.488580	36.798093
1661.925872	163833.903456	36.803111
1663.280228	164073.898168	36.808128
1665.143089	164307.577211	36.813146
1666.647897	164542.727168	36.818164
1668.670812	164773.006177	36.823181
1670.447874	165013.288953	36.828199
1671.587983	165245.003002	36.833216
1673.326997	165469.687770	36.838234
1674.745619	165725.122550	36.843252
1676.375461	165960.131725	36.848269
1677.949606	166207.726339	36.853287
1679.361647	166456.580880	36.858304
1681.015335	166700.637066	36.863322
1682.171527	166963.077354	36.868340
1684.447347	167214.617944	36.873357
1686.445188	167472.640929	36.878375
1687.722949	167733.237609	36.883392
1689.499655	167985.311970	36.888410
1690.838002	168246.091540	36.893428
1692.330186	168497.430644	36.898445
1694.676648	168756.987394	36.903463
1695.834065	169018.804760	36.908480
1698.083555	169264.003560	36.913498
1699.213437	169524.610269	36.918516
1700.883880	169783.070189	36.923533
1702.643147	170045.259870	36.928551
1704.254420	170285.141923	36.933568
1706.165231	170526.090676	36.938586
1707.422991	170780.159774	36.943604
1709.095841	171025.580641	36.948621
1710.774150	171258.083151	36.953639
1712.411789	171522.154602	36.958656
1714.021934	171768.757534	36.963674
1715.293720	172024.099899	36.968692
1717.151801	172289.038882	36.973709
1718.668021	172552.768746	36.978727
1720.207525	172809.934985	36.983744
1722.613153	173079.086754	36.988762
1724.143387	173356.765715	36.993780
1725.764265	173621.244916	36.998797
1727.787173	173887.331969	37.003815
1729.319391	174149.087936	37.008832
1731.094512	174423.697879	37.013850
1732.794954	174705.238805	37.018868
1734.246585	174978.168473	37.023885
1736.582877	175243.650789	37.028903
1738.263115	175523.194566	37.033920
1740.337697	175793.509218	37.038938
1742.139452	176065.801105	37.043956
1743.699661	176334.353696	37.048973
1745.766790	176601.259914	37.053991
1747.676985	176877.751237	37.059008
1749.404312	177145.479942	37.064026
1751.084966	177417.977473	37.069044
1753.121682	177686.252588	37.074061
1755.444706	177933.449524	37.079079
1757.324028	178202.566536	37.084096
1759.260743	178470.126689	37.089114
1760.782202	178743.204196	37.094132
1761.885550	179007.647789	37.099149
1763.858430	179267.577809	37.104167
1765.613806	179544.274850	37.109184
1767.409174	179812.081803	37.114202
1769.160365	180083.895800	37.119220
1770.900931	180356.398401	37.124237
1772.562285	180630.362904	37.129255
1774.025267	180914.529584	37.134272
1775.412536	181184.647150	37.139290
1777.447270	181473.059884	37.144308
1779.523182	181751.122410	37.149325
1781.516525	182026.344572	37.154343
1782.977298	182312.702150	37.159360
1785.112143	182581.200989	37.164378
1787.033794	182859.054374	37.169396
1788.836501	183137.488007	37.174413
1790.590804	183409.432369	37.179431
1792.236096	183680.444711	37.184448
1794.098415	183969.191984	37.189466
1795.779484	184235.923225	37.194484
1796.888722	184563.847452	37.199501
1799.072087	184866.761159	37.204519
1800.683329	185140.642415	37.209536
1802.116124	185402.268000	37.214554
1803.991484	185670.153266	37.219572
1805.855362	185930.793570	37.224589
1807.807681	186199.061644	37.229607
1809.419830	186480.336982	37.234624
1811.153345	186745.230344	37.239642
1813.034265	187019.734490	37.244660
1814.783666	187290.860397	37.249677
1816.477760	187562.796751	37.254695
1818.368950	187854.376720	37.259712
1820.337741	188126.230594	37.264730
1821.889406	188412.095477	37.269748
1823.713086	188689.536877	37.274765
1825.534442	188983.393926	37.279783
1827.048769	189268.494916	37.284800
1829.132612	189563.896709	37.289818
1831.153021	189862.065534	37.294836
1832.639198	190153.332408	37.299853
1834.766991	190442.218542	37.304871
1836.704276	190733.334831	37.309888
1838.786060	191020.923979	37.314906
1840.832184	191312.621034	37.319924
1842.501603	191607.583040	37.324941
1844.914129	191891.628497	37.329959
1846.684672	192180.913893	37.334976
1848.336978	192468.875146	37.339994
1850.700099	192756.652639	37.345012
1852.435486	193049.743890	37.350029
1854.642843	193326.569149	37.355047
1856.207258	193618.816263	37.360064
1857.810090	193911.197778	37.365082
1859.920620	194197.603031	37.370100
1861.855359	194491.199930	37.375117
1863.909282	194770.253931	37.380135
1865.799863	195068.279050	37.385152
1867.827968	195342.083862	37.390170
1870.167347	195627.237400	37.395188
1871.699459	195914.828195	37.400205
1873.942038	196190.605750	37.405223
1875.488913	196483.071684	37.410240
1877.018405	196756.281977	37.415258
1878.921933	197039.332330	37.420276
1880.835007	197339.293473	37.425293
1882.473331	197623.026407	37.430311
1884.480932	197924.395902	37.435328
1886.228721	198225.214422	37.440346
1888.253992	198514.648934	37.445364
1889.460729	198809.493659	37.450381
1891.592148	199112.218308	37.455399
1893.502276	199407.364196	37.460416
1894.926108	199709.399846	37.465434
1897.771939	200018.938476	37.470452
1899.299126	200319.905198	37.475469
1900.968571	200614.513173	37.480487
1903.103135	200895.850836	37.485504
1904.637178	201163.960639	37.490522
1906.891724	201447.578024	37.495540
1908.380612	201730.387890	37.500557
1910.308079	202010.914545	37.505575
1911.906269	202307.407933	37.510592
1913.754321	202598.958689	37.515610
1915.361649	202889.891497	37.520628
1917.208351	203192.186529	37.525645
1919.251433	203483.288321	37.530663
1920.909460	203788.551038	37.535680
1922.832907	204095.458308	37.540698
1924.855306	204402.679998	37.545716
1926.892658	204714.560291	37.550733
1929.148228	205008.005880	37.555751
1931.127573	205312.965655	37.560768
1933.151222	205623.823387	37.565786
1935.030116	205925.640999	37.570804
1936.868861	206239.745242	37.575821
1939.062555	206548.520448	37.580839
1940.952985	206855.926549	37.585856
1943.219228	207158.203104	37.590874
1945.431233	207468.946810	37.595892
1947.054913	207781.328754	37.600909
1949.019159	208082.035003	37.605927
1951.274132	208401.079286	37.610944
1953.172203	208697.862678	37.615962
1955.017751	209012.281019	37.620980
1956.882670	209334.265284	37.625997
1959.394765	209627.569180	37.631015
1961.446565	209931.847861	37.636032
1963.174257	210245.732127	37.641050
1965.210051	210554.968033	37.646068
1967.787050	210865.306100	37.651085
1969.669223	211159.687929	37.656103
1971.360105	211464.998695	37.661120
1973.523772	211771.778846	37.666138
1975.783478	212071.356247	37.671156
1977.495995	212401.377775	37.676173
1979.615527	212700.981207	37.681191
1981.357673	213013.780550	37.686208
1983.294228	213321.265037	37.691226
1985.557501	213642.612456	37.696244
1987.549096	213956.946914	37.701261
1989.354176	214265.422057	37.706279
1991.204535	214583.947937	37.711296
1992.936456	214891.777252	37.716314
1994.741759	215214.300355	37.721332
1996.297045	215538.848315	37.726349
1998.713189	215850.373302	37.731367
2000.410848	216187.318665	37.736384
2002.665545	216503.876723	37.741402
2004.451626	216835.678688	37.746420
2006.361739	217170.025749	37.751437
2008.085185	217487.973024	37.756455
2010.086986	217816.998216	37.761472
2011.809186	218119.378331	37.766490
2013.737209	218437.064905	37.771508
2015.860232	218750.782271	37.776525
2018.330946	219065.177653	37.781543
2019.945280	219384.596996	37.786560
2021.935161	219701.641739	37.791578
2023.995762	220009.023663	37.796596
2025.797391	220327.905724	37.801613
2028.137571	220642.505722	37.806631
2030.419515	220956.176783	37.811648
2032.598407	221284.496338	37.816666
2034.452713	221592.832219	37.821684
2036.341975	221919.374351	37.826701
2038.740290	222231.073207	37.831719
2041.002208	222566.519434	37.836736
2042.906744	222883.282766	37.841754
2045.092258	223205.307420	37.846772
2046.997656	223539.979132	37.851789
2049.117632	223861.584923	37.856807
2051.200377	224190.792495	37.861824
2053.035256	224518.163718	37.866842
2055.384790	224851.670787	37.871860
2057.355935	225186.005439	37.876877
2059.497069	225511.218612	37.881895
2061.485207	225843.951834	37.886912
2063.532518	226185.591288	37.891930
2065.919600	226513.889104	37.896948
2067.779070	226853.936753	37.901965
2069.737973	227196.482893	37.906983
2071.992128	227531.130611	37.912000
2073.653596	227873.932487	37.917018
2075.698935	228216.948953	37.922036
2077.854619	228565.408533	37.927053
2079.812945	228911.286414	37.932071
2082.220847	229269.153645	37.937088
2084.014237	229630.555951	37.942106
2086.462995	229969.748177	37.947124
2088.462690	230325.401632	37.952141
2090.398805	230670.652320	37.957159
2092.855721	231015.001867	37.962176
2094.835494	231369.467240	37.967194
2097.010077	231715.949477	37.972212
2099.312901	232083.595229	37.977229
2101.152955	232430.339386	37.982247
2103.356229	232777.911194	37.987264
2105.425498	233137.292918	37.992282
2107.426501	233487.948928	37.997300
2109.479181	233839.511258	38.002317
2111.586414	234195.942065	38.007335
2113.816013	234557.331379	38.012352
2115.709066	234920.252252	38.017370
2118.458806	235272.866614	38.022388
2120.392471	235631.616013	38.027405
2122.252766	235966.983489	38.032423
2124.516403	236298.040442	38.037440
2126.429738	236629.462668	38.042458
2128.966843	236951.253016	38.047476
2131.091418	237280.277785	38.052493
2133.137953	237594.125968	38.057511
2135.443013	237918.726304	38.062528
2137.274950	238236.905076	38.067546
2139.687696	238567.940106	38.072564
2141.736505	238904.448531	38.077581
2144.053191	239232.630502	38.082599
2146.031614	239563.080777	38.087616
2147.979943	239892.063320	38.092634
2150.328755	240218.412187	38.097652
2153.037085	240562.608702	38.102669
2155.094291	240894.901672	38.107687
2157.155196	241226.965814	38.112704
2158.979698	241557.851477	38.117722
2161.711400	241884.314793	38.122740
2163.323924	242230.377427	38.127757
2165.392011	242572.653807	38.132775
2167.730819	242905.180498	38.137792
2169.417118	243258.750921	38.142810
2171.626496	243610.911372	38.147828
2173.692674	243964.976507	38.152845
2175.740793	244323.820834	38.157863
2177.988741	244692.589266	38.162880
2179.839184	245058.250717	38.167898
2182.318213	245417.047916	38.172916
2184.398171	245787.141764	38.177933
2186.376857	246160.327040	38.182951
2188.807922	246532.393803	38.187968
2190.719837	246909.935098	38.192986
2192.999331	247281.266370	38.198004
2195.424721	247656.027815	38.203021
2197.316351	248036.952148	38.208039
2199.944849	248419.198763	38.213056
2201.590540	248799.124226	38.218074
2204.074409	249180.049785	38.223092
2206.481282	249559.286771	38.228109
2208.404913	249944.957403	38.233127
2211.357681	250326.057578	38.238144
2212.836440	250713.227322	38.243162
2214.978713	251092.916931	38.248180
2217.525059	251493.393612	38.253197
2219.643846	251891.631917	38.258215
2221.912784	252272.494382	38.263232
2224.158448	252665.148049	38.268250
2226.653706	253046.099136	38.273268
2229.334278	253419.067473	38.278285
2231.342633	253807.037122	38.283303
2234.409421	254181.667053	38.288320
2236.397017	254562.146502	38.293338
2238.702431	254938.557980	38.298356
2240.882286	255315.854695	38.303373
2242.869196	255690.872754	38.308391
2245.050360	256037.253622	38.313408
2247.065754	256400.886226	38.318426
2249.588694	256739.562319	38.323444
2251.153919	257087.826747	38.328461
2252.860183	257449.276716	38.333479
2255.574408	257805.245051	38.338496
2257.729504	258178.862561	38.343514
2260.343877	258543.789810	38.348532
2262.509470	258905.161072	38.353549
2264.638413	259288.232849	38.358567
2266.690711	259646.955987	38.363584
2268.727194	260023.133714	38.368602
2271.158516	260408.490569	38.373620
2273.552899	260772.819791	38.378637
2275.445004	261154.508894	38.383655
2277.955194	261531.951450	38.388672
2279.995029	261927.535873	38.393690
2282.580062	262310.071295	38.398708
2284.937112	262691.527758	38.403725
2287.306425	263082.355645	38.408743
2289.661681	263466.072837	38.413760
2291.787662	263859.863186	38.418778
2294.525169	264250.144704	38.423796
2296.633613	264639.314144	38.428813
2298.871597	265045.100098	38.433831
2301.382323	265429.094144	38.438848
2303.340259	265829.719700	38.443866
2305.671693	266238.740212	38.448884
2307.960250	266635.548868	38.453901
2310.038661	267041.309475	38.458919
2312.456877	267445.080952	38.463936
2315.058961	267864.062253	38.468954
2317.867241	268249.552349	38.473972
2320.395303	268649.315476	38.478989
2322.496874	269047.499870	38.484007
2324.898227	269452.770689	38.489024
2327.444119	269862.817386	38.494042
2329.994537	270253.531363	38.499060
2332.381698	270653.062041	38.504077
2334.389408	271053.698548	38.509095
2336.946440	271463.360083	38.514112
2338.689407	271864.421726	38.519130
2341.257619	272268.415382	38.524148
2343.569128	272678.650487	38.529165
2345.626406	273083.924128	38.534183
2348.302542	273503.824657	38.539200
2350.303774	273914.517202	38.544218
2352.885333	274330.774521	38.549236
2355.306085	274738.193216	38.554253
2357.609982	275150.736984	38.559271
2360.229340	275563.784896	38.564288
2362.547907	275980.261912	38.569306
2364.975619	276381.732270	38.574324
2367.908433	276784.563411	38.579341
2369.931184	277194.433244	38.584359
2372.236700	277566.024118	38.589376
2374.342916	277947.250234	38.594394
2376.632874	278324.227491	38.599412
2378.838821	278702.818662	38.604429
2381.169138	279093.504380	38.609447
2383.142188	279485.418806	38.614464
2385.386799	279886.963932	38.619482
2387.393661	280292.943236	38.624500
2389.740940	280681.590434	38.629517
2391.787561	281117.229830	38.634535
2394.121275	281522.972507	38.639552
2396.353885	281940.517629	38.644570
2398.789806	282364.986830	38.649588
2401.529953	282780.563313	38.654605
2404.122972	283215.544814	38.659623
2406.700230	283631.908888	38.664640
2409.021470	284065.308763	38.669658
2410.889679	284488.929312	38.674676
2414.030376	284914.236165	38.679693
2415.885056	285339.837805	38.684711
2418.545055	285772.590470	38.689728
2421.044592	286222.590758	38.694746
2423.240954	286667.815329	38.699764
2426.009650	287104.558499	38.704781
2428.112931	287559.981566	38.709799
2431.033282	287995.298874	38.714816
2433.506251	288444.102436	38.719834
2435.872392	288887.944295	38.724852
2438.464197	289321.916267	38.729869
2440.728139	289772.935239	38.734887
2443.855889	290219.893347	38.739904
2446.442810	290654.344055	38.744922
2448.945956	291094.547801	38.749940
2451.715644	291528.049700	38.754957
2453.444698	291964.369407	38.759975
2456.539942	292418.385788	38.764992
2458.937251	292859.413716	38.770010
2461.689431	293302.715968	38.775028
2464.122576	293733.117536	38.780045
2466.460633	294176.029898	38.785063
2469.390281	294610.000576	38.790080
2471.673784	295050.048626	38.795098
2473.735176	295499.479472	38.800116
2476.289640	295948.570128	38.805133
2478.600532	296396.659146	38.810151
2481.365731	296835.982374	38.815168
2483.464702	297287.126091	38.820186
2485.644649	297743.536713	38.825204
2488.215584	298193.554345	38.830221
2490.076242	298670.435117	38.835239
2492.260121	299124.273479	38.840256
2494.969273	299590.921829	38.845274
2497.708451	300063.962884	38.850292
2500.311597	300524.910338	38.855309
2502.480163	300987.275834	38.860327
2505.285525	301422.583980	38.865344
2507.511349	301868.097050	38.870362
2509.527006	302308.386722	38.875380
2512.761581	302739.856435	38.880397
2514.947998	303186.944253	38.885415
2516.673858	303635.708482	38.890432
2519.343132	304075.979183	38.895450
2521.792051	304537.795768	38.900468
2524.755564	304998.633036	38.905485
2527.677155	305459.424160	38.910503
2530.069280	305898.335998	38.915520
2532.474906	306345.192002	38.920538
2535.112880	306816.613981	38.925556
2537.661384	307275.147743	38.930573
2540.096000	307741.748602	38.935591
2543.077529	308200.431616	38.940608
2545.797545	308660.553381	38.945626
2548.487116	309120.550677	38.950644
2550.994773	309576.843352	38.955661
2553.611980	310042.307352	38.960679
2556.103720	310507.129710	38.965696
2558.647443	310967.115467	38.970714
2561.286365	311441.505850	38.975732
2564.045406	311902.591772	38.980749
2566.059752	312376.143356	38.985767
2568.545490	312852.150646	38.990784
2571.397707	313324.207016	38.995802
2573.950167	313806.976599	39.000820
2576.594773	314284.978700	39.005837
2579.196830	314772.761031	39.010855
2581.554578	315244.076588	39.015872
2584.580074	315732.922509	39.020890
2586.872884	316219.808033	39.025908
2589.423955	316705.884196	39.030925
2592.196391	317199.765111	39.035943
2594.139036	317697.313657	39.040960
2596.936353	318188.136048	39.045978
2599.604288	318698.629727	39.050996
2602.453100	319184.002186	39.056013
2605.323648	319688.207324	39.061031
2607.782923	320169.144815	39.066048
2610.740226	320657.255258	39.071066
2613.661861	321151.207816	39.076084
2616.060337	321642.478406	39.081101
2618.710565	322143.197932	39.086119
2621.316549	322635.999419	39.091136
2624.244189	323128.284993	39.096154
2626.788316	323621.774674	39.101172
2629.355375	324110.077070	39.106189
2631.796353	324610.736042	39.111207
2634.467937	325100.738980	39.116224
2637.217140	325596.208518	39.121242
2639.838661	326101.597122	39.126260
2642.709226	326584.140404	39.131277
2645.666397	327058.870843	39.136295
2648.255364	327518.021567	39.141312
2650.977448	327982.020252	39.146330
2653.307322	328442.959574	39.151348
2655.598187	328887.044877	39.156365
2658.109908	329346.955668	39.161383
2660.594294	329818.037439	39.166400
2663.289996	330274.685061	39.171418
2665.168980	330754.544474	39.176436
2667.985400	331233.604851	39.181453
2670.711205	331714.047339	39.186471
2673.279822	332203.371957	39.191488
2675.685509	332687.896789	39.196506
2678.636628	333189.763511	39.201524
2680.908155	333680.420045	39.206541
2683.628127	334183.662260	39.211559
2686.110537	334686.407183	39.216576
2689.631133	335187.472193	39.221594
2691.941241	335698.867343	39.226612
2694.863899	336201.040062	39.231629
2697.961198	336705.360973	39.236647
2700.683029	337217.102120	39.241664
2703.566694	337725.104552	39.246682
2706.209989	338232.939864	39.251700
2709.030844	338730.561392	39.256717
2711.693067	339234.017512	39.261735
2714.211445	339751.859127	39.266752
2717.272076	340256.708833	39.271770
2719.847170	340779.225438	39.276788
2722.530093	341295.702704	39.281805
2725.918857	341806.901541	39.286823
2728.530675	342328.151402	39.291840
2731.523498	342840.498171	39.296858
2734.120603	343352.729347	39.301876
2736.691967	343863.817258	39.306893
2739.752340	344379.612692	39.311911
2742.208403	344888.957885	39.316928
2745.456382	345403.466281	39.321946
2748.279455	345920.858517	39.326964
2751.136911	346427.910116	39.331981
2753.901707	346936.621439	39.336999
2756.422189	347446.815292	39.342016
2759.487196	347953.255969	39.347034
2762.128910	348479.861782	39.352052
2765.264535	348991.861492	39.357069
2767.913685	349504.268276	39.362087
2770.779643	350019.905539	39.367104
2773.640728	350529.218969	39.372122
2776.210390	351048.751779	39.377140
2779.078718	351555.514337	39.382157
2781.546940	352063.125898	39.387175
2784.620483	352581.868918	39.392192
2787.173866	353099.907876	39.397210
2790.003628	353621.293358	39.402228
2792.637523	354137.022140	39.407245
2795.098837	354648.942672	39.412263
2797.367765	355150.233108	39.417280
2800.448867	355630.420835	39.422298
2802.768436	356136.206970	39.427316
2805.339326	356627.532565	39.432333
2807.983784	357136.092470	39.437351
2810.673380	357634.565808	39.442368
2813.860824	358141.548731	39.447386
2816.479766	358647.785145	39.452404
2819.441668	359159.411192	39.457421
2822.346762	359677.864925	39.462439
2824.743027	360198.707448	39.467456
2827.531174	360718.156896	39.472474
2830.405165	361246.489347	39.477492
2832.924799	361784.210889	39.482509
2835.699376	362313.738128	39.487527
2838.550177	362871.758795	39.492544
2841.301275	363407.160364	39.497562
2844.019090	363958.668373	39.502580
2847.365648	364501.258586	39.507597
2850.299581	365058.421203	39.512615
2852.943858	365604.768285	39.517632
2855.889496	366158.310522	39.522650
2859.155616	366704.383029	39.527668
2862.065675	367264.306926	39.532685
2864.976997	367817.043863	39.537703
2867.628115	368374.991234	39.542720
2870.635956	368933.046653	39.547738
2873.276172	369502.468433	39.552756
2876.323488	370073.257361	39.557773
2879.575327	370638.853620	39.562791
2881.941568	371208.827731	39.567808
2885.054373	371774.936935	39.572826
2887.852654	372349.003599	39.577844
2890.893160	372922.106502	39.582861
2893.423178	373500.790501	39.587879
2896.431846	374090.490897	39.592896
2899.229631	374668.222077	39.597914
2902.350689	375251.568845	39.602932
2905.345975	375844.766454	39.607949
2908.484248	376422.993142	39.612967
2911.124858	377006.772353	39.617984
2914.620678	377593.844006	39.623002
2917.961056	378183.949468	39.628020
2920.894382	378757.048952	39.633037
2923.666107	379330.952225	39.638055
2926.703574	379920.115115	39.643072
2929.573038	380488.124386	39.648090
2932.295353	381079.500922	39.653108
2935.153143	381665.519154	39.658125
2938.360637	382243.024167	39.663143
2941.110103	382831.651304	39.668160
2944.509409	383411.257702	39.673178
2947.674177	383996.319165	39.678196
2950.153040	384577.811005	39.683213
2953.497642	385141.727622	39.688231
2955.893920	385691.498033	39.693248
2958.175969	386238.895376	39.698266
2961.104838	386789.873827	39.703284
2963.776634	387336.069968	39.708301
2966.784404	387895.279490	39.713319
2969.296645	388463.207604	39.718336
2972.386302	389014.600693	39.723354
2975.218087	389596.825955	39.728372
2977.844213	390173.295985	39.733389
2981.324056	390746.238067	39.738407
2983.991228	391328.711772	39.743424
2987.211555	391902.588742	39.748442
2990.036657	392496.165205	39.753460
2992.660050	393085.607722	39.758477
2996.227937	393672.444122	39.763495
2998.997484	394279.807373	39.768512
3002.180914	394870.918140	39.773530
3005.091852	395479.068834	39.778548
3008.384522	396076.675155	39.783565
3011.456865	396666.678863	39.788583
3014.542788	397273.064269	39.793600
3017.641722	397885.491229	39.798618
3021.005929	398482.300733	39.803636
3024.047716	399090.555869	39.808653
3027.303771	399688.372236	39.813671
3030.715723	400291.115804	39.818688
3033.888473	400891.429548	39.823706
3037.014990	401489.609999	39.828724
3039.890868	402084.957376	39.833741
3043.501887	402685.537864	39.838759
3046.290755	403292.047802	39.843776
3049.670326	403882.912777	39.848794
3052.769145	404482.604325	39.853812
3055.171289	405095.550410	39.858829
3058.990261	405683.084069	39.863847
3061.910121	406295.585404	39.868864
3064.567028	406900.289961	39.873882
3067.535404	407503.939809	39.878900
3070.663960	408108.992650	39.883917
3074.272090	408710.631515	39.888935
3077.258809	409326.573409	39.893952
3080.739927	409924.457599	39.898970
3083.921814	410522.379386	39.903988
3086.686116	411140.090106	39.909005
3090.368047	411732.985154	39.914023
3093.000811	412345.446965	39.919040
3095.997497	412948.461191	39.924058
3099.349017	413549.324013	39.929076
3102.310200	414163.257045	39.934093
3105.114949	414769.098057	39.939111
3108.277764	415377.497358	39.944128
3111.567971	415986.670771	39.949146
3114.729605	416597.219022	39.954164
3117.368168	417221.035115	39.959181
3120.368122	417815.425582	39.964199
3123.424230	418404.449532	39.969216
3126.003704	418985.742153	39.974234
3128.935301	419569.872947	39.979252
3131.628571	420156.030998	39.984269
3134.446648	420761.345877	39.989287
3137.357698	421365.313463	39.994304
3140.274690	421978.075871	39.999322
3143.058148	422595.453526	40.004340
3146.171672	423223.797282	40.009357
3149.664128	423845.984218	40.014375
3152.407233	424488.029184	40.019392
3155.283506	425123.098084	40.024410
3158.936855	425750.828283	40.029428
3161.486628	426404.853938	40.034445
3165.002615	427056.924744	40.039463
3168.233636	427708.823826	40.044480
3171.737401	428365.011909	40.049498
3174.940834	429019.258794	40.054516
3178.045410	429682.615891	40.059533
3181.305924	430331.855649	40.064551
3184.813384	430993.942452	40.069568
3187.796680	431660.908360	40.074586
3191.136479	432325.263443	40.079604
3194.697946	432994.622754	40.084621
3198.255947	433652.120142	40.089639
3201.754586	434316.441048	40.094656
3204.974173	434976.741581	40.099674
3208.842354	435635.798773	40.104692
3211.761715	436304.411349	40.109709
3215.154876	436954.705832	40.114727
3218.234650	437607.109675	40.119744
3221.444907	438271.009153	40.124762
3225.028493	438924.806431	40.129780
3228.262308	439596.150979	40.134797
3231.574913	440239.279608	40.139815
3234.947530	440906.715256	40.144832
3237.995828	441567.406508	40.149850
3241.633429	442227.420641	40.154868
3244.400990	442898.339047	40.159885
3247.349380	443555.546935	40.164903
3250.550150	444222.050338	40.169920
3253.843559	444907.992672	40.174938
3257.402937	445579.097208	40.179956
3260.308685	446248.926593	40.184973
3263.636278	446935.759117	40.189991
3267.117658	447610.555953	40.195008
3270.089324	448289.110457	40.200026
3273.457854	448965.956921	40.205044
3276.998856	449655.496777	40.210061
3280.637442	450344.339805	40.215079
3283.744683	451021.518411	40.220096
3286.700658	451699.611023	40.225114
3290.561952	452371.155325	40.230132
3293.562410	453048.740968	40.235149
3296.958055	453709.348376	40.240167
3300.419628	454350.861150	40.245184
3303.053135	454989.663764	40.250202
3306.666431	455602.240912	40.255220
3309.490327	456249.465393	40.260237
3312.559635	456873.725274	40.265255
3315.823052	457523.159451	40.270272
3318.618778	458174.927386	40.275290
3322.133705	458821.900565	40.280308
3325.421227	459491.082914	40.285325
3328.223843	460153.501581	40.290343
3331.439018	460823.813975	40.295360
3334.770605	461507.882405	40.300378
3338.443318	462182.518401	40.305396
3341.827133	462866.429543	40.310413
3344.932498	463545.714705	40.315431
3348.125513	464230.924651	40.320448
3351.072354	464924.086569	40.325466
3354.772233	465625.180494	40.330484
3358.266816	466336.744118	40.335501
3362.063683	467026.855537	40.340519
3364.937012	467732.864638	40.345536
3368.678052	468442.387896	40.350554
3372.081287	469152.548673	40.355572
3375.012454	469875.040465	40.360589
3378.221821	470591.748299	40.365607
3382.068881	471305.490915	40.370624
3385.551083	472030.230841	40.375642
3389.217919	472753.648284	40.380660
3392.755745	473473.776338	40.385677
3396.837702	474186.964581	40.390695
3400.593767	474891.796490	40.395712
3404.203456	475603.040869	40.400730
3407.814620	476307.944342	40.405748
3411.611064	477016.122279	40.410765
3414.845464	477721.439658	40.415783
3418.427485	478426.266367	40.420800
3421.224120	479137.764462	40.425818
3424.752319	479848.503720	40.430836
3428.150805	480567.063574	40.435853
3431.255645	481280.696692	40.440871
3435.100065	482001.041640	40.445888
3438.562742	482726.875322	40.450906
3441.951879	483446.381310	40.455924
3445.005218	484174.649026	40.460941
3448.452887	484896.206400	40.465959
3452.223790	485622.424057	40.470976
3455.707506	486353.102682	40.475994
3459.029324	487079.437623	40.481012
3462.732504	487804.768706	40.486029
3466.402954	488533.254769	40.491047
3469.698524	489258.998464	40.496064
3473.471079	489995.530955	40.501082
3477.328352	490715.868958	40.506100
3480.277094	491436.937404	40.511117
3483.575563	492148.029360	40.516122
3487.217448	492809.604681	40.521127
3490.441644	493429.239930	40.526132
3493.337739	493995.239556	40.531136
3495.979986	494508.709015	40.536141
3498.691659	494969.951923	40.541146
3501.395443	495368.111173	40.546151
3503.411437	495724.954838	40.551156
3506.171210	496020.111315	40.556160
3508.170399	496273.515030	40.561165
3509.961620	496474.351404	40.566170
3511.829112	496623.332430	40.571175
3513.113225	496742.521790	40.576180
3514.564270	496824.003466	40.581184
3515.659634	496868.018967	40.586189
3517.053591	496869.803992	40.591194
3518.008302	496850.017962	40.596199
3518.508571	496808.815122	40.601204
3519.353591	496722.389636	40.606208
3519.958012	496628.216147	40.611213
3520.341591	496516.277120	40.616218
3520.994968	496379.610050	40.621223
3521.489127	496235.331961	40.626228
3521.908455	496067.597572	40.631232
3522.021222	495880.036772	40.636237
3522.185334	495694.690563	40.641242
3522.509771	495492.421561	40.646247
3522.284752	495289.232351	40.651252
3522.453472	495075.351614	40.656256
3522.386973	494855.033971	40.661261
3522.297489	494628.394680	40.666266
3522.270076	494397.189346	40.671271
3522.326223	494177.196003	40.676276
3521.985476	493932.835671	40.681280
3522.063040	493696.392728	40.686285
3521.926172	493455.986881	40.691290
3521.429722	493217.308356	40.696295
3520.859790	492996.243124	40.701300
3520.891995	492752.763277	40.706304
3520.742128	492533.036750	40.711309
3520.099848	492296.191370	40.716314
3519.789347	492061.208447	40.721319
3519.504015	491845.239797	40.726324
3519.406488	491633.081233	40.731328
3519.191155	491416.538726	40.736333
3519.099340	491203.564409	40.741338
3518.971316	490975.567681	40.746343
3518.274335	490772.961607	40.751348
3518.183699	490568.327057	40.756352
3518.215765	490356.737711	40.761357
3517.809887	490152.303821	40.766362
3517.570104	489952.240952	40.771367
3517.436336	489757.116070	40.776372
3517.025672	489556.673021	40.781376
3516.880961	489369.641086	40.786381
3516.690514	489183.981074	40.791386
3516.501985	488996.396010	40.796391
3516.110517	488813.245659	40.801396
3515.976241	488629.998859	40.806400
3515.822923	488466.133107	40.811405
3515.247096	488290.295079	40.816410
3515.216116	488122.964380	40.821415
3514.850505	487961.710756	40.826420
3514.964762	487786.913640	40.831424
3514.524852	487626.226214	40.836429
3513.727189	487477.591224	40.841434
3514.194392	487330.358302	40.846439
3513.618291	487180.417872	40.851444
3513.337461	487031.134193	40.856448
3513.522101	486893.054542	40.861453
3512.849226	486770.554658	40.866458
3513.068428	486627.457141	40.871463
3512.514975	486504.277135	40.876468
3512.647279	486374.957079	40.881472
3512.223517	486245.984043	40.886477
3512.028743	486122.082227	40.891482
3512.147348	485993.925652	40.896487
3511.800619	485879.511566	40.901492
3511.722943	485768.896976	40.906496
3511.868503	485648.881104	40.911501
3511.469222	485536.700509	40.916506
3511.660260	485420.926412	40.921511
3511.414334	485315.752819	40.926516
3511.382814	485206.392033	40.931520
3511.327815	485100.931512	40.936525
3510.893433	484996.547332	40.941530
3510.975381	484886.051768	40.946535
3510.632936	484782.460386	40.951540
3510.873247	484685.095236	40.956544
3510.408628	484590.279238	40.961549
3510.356741	484496.758764	40.966554
3510.093277	484402.160466	40.971559
3509.713385	484314.819028	40.976564
3509.664947	484224.889963	40.981568
3510.028898	484134.485132	40.986573
3509.490845	484061.138433	40.991578
3509.370802	483970.309276	40.996583
3509.131124	483901.719184	41.001588
3508.890943	483827.359011	41.006592
3508.964945	483759.271555	41.011597
3508.871523	483687.213952	41.016602
3509.073705	483612.676122	41.021607
3508.431714	483539.749921	41.026612
3508.858428	483468.209988	41.031616
3508.822341	483406.264291	41.036621
3508.361355	483343.834166	41.041626
3508.819196	483271.174606	41.046631
3508.410502	483219.313596	41.051636
3508.440135	483148.245093	41.056640
3508.546353	483093.714430	41.061645
3508.313989	483025.474009	41.066650
3508.462605	482963.849544	41.071655
3508.396056	482906.260250	41.076660
3508.030352	482835.308613	41.081664
3508.045479	482787.524492	41.086669
3507.594265	482724.989292	41.091674
3507.878898	482667.896046	41.096679
3507.882723	482629.072544	41.101684
3507.599976	482570.557363	41.106688
3507.430177	482517.894267	41.111693
3507.467936	482473.699241	41.116698
3507.313950	482421.893651	41.121703
3507.214468	482382.530461	41.126708
3507.372728	482325.558932	41.131712
3507.194300	482287.930007	41.136717
3507.241944	482249.654990	41.141722
3507.062178	482194.461758	41.146727
3506.927484	482164.367158	41.151732
3507.115771	482123.941907	41.156736
3507.189109	482080.043539	41.161741
3506.891860	482037.625648	41.166746
3507.011577	481999.540264	41.171751
3507.197336	481963.923827	41.176756
3506.936392	481922.663690	41.181760
3507.068706	481878.552283	41.186765
3506.941293	481848.202814	41.191770
3506.981841	481800.107997	41.196775
3507.021264	481771.349718	41.201780
3506.917170	481722.975675	41.206784
3507.170810	481683.449415	41.211789
3507.244338	481644.814350	41.216794
3507.288678	481597.831968	41.221799
3507.108616	481559.088157	41.226804
3507.150272	481511.599811	41.231808
3507.524398	481469.116561	41.236813
3507.021039	481427.795433	41.241818
3506.983714	481385.685956	41.246823
3506.775132	481347.705860	41.251828
3506.590307	481309.974728	41.256832
3506.962104	481275.590667	41.261837
3506.865260	481243.007654	41.266842
3506.837194	481196.340306	41.271847
3506.740618	481159.758064	41.276852
3506.646553	481125.250775	41.281856
3506.934764	481088.855794	41.286861
3506.723355	481059.076160	41.291866
3506.616653	481008.777036	41.296871
3506.544424	480974.164485	41.301876
3506.476509	480938.893053	41.306880
3506.410064	480911.518248	41.311885
3506.247933	480881.527419	41.316890
3506.224664	480850.449777	41.321895
3506.149905	480834.364891	41.326900
3506.260741	480801.897483	41.331904
3506.343991	480775.306859	41.336909
3506.117541	480746.440467	41.341914
3506.178272	480714.133321	41.346919
3506.100519	480693.442218	41.351924
3505.739293	480661.105777	41.356928
3505.908589	480648.471983	41.361933
3505.968032	480624.973155	41.366938
3506.408991	480598.776796	41.371943
3505.834975	480587.130452	41.376948
3505.976766	480560.985117	41.381952
3506.113554	480524.462982	41.386957
3505.799616	480498.192878	41.391962
3506.148752	480472.670107	41.396967
3505.809049	480449.846673	41.401972
3506.114979	480433.949544	41.406976
3506.131373	480402.206259	41.411981
3506.194019	480378.099087	41.416986
3506.351425	480349.520878	41.421991
3506.509445	480327.523522	41.426996
3506.766874	480296.295750	41.432000
3506.468919	480250.380752	41.437005
3506.309843	480226.209988	41.442010
3506.170331	480192.316148	41.447015
3505.673783	480173.012161	41.452020
3505.890310	480134.855669	41.457024
3506.155293	480121.243319	41.462029
3505.619521	480101.287845	41.467034
3505.876347	480064.440540	41.472039
3505.625202	480047.524463	41.477044
3505.545231	480032.806594	41.482048
3506.047946	480016.875499	41.487053
3505.987696	479994.155645	41.492058
3506.015766	479968.231364	41.497063
3505.929441	479941.263470	41.502068
3506.127502	479912.475131	41.507072
3506.367158	479890.868298	41.512077
3506.113646	479876.230558	41.517082
3506.253919	479838.997699	41.522087
3506.427620	479807.935252	41.527092
3506.365809	479779.089822	41.532096
3505.952824	479749.747434	41.537101
3505.870476	479723.284783	41.542106
3506.375319	479690.089977	41.547111
3505.917957	479662.678770	41.552116
3506.174169	479635.905060	41.557120
3506.421468	479611.208461	41.562125
3506.088020	479594.255385	41.567130
3506.250762	479556.613107	41.572135
3506.332050	479534.627887	41.577140
3506.084563	479508.901872	41.582144
3505.993492	479479.655957	41.587149
3505.864072	479460.187270	41.592154
3505.658659	479432.428942	41.597159
3505.582503	479414.216751	41.602164
3505.663162	479388.940794	41.607168
3505.483873	479378.745039	41.612173
3505.211201	479356.566909	41.617178
3505.426824	479333.495366	41.622183
3505.816541	479331.707577	41.627188
3505.616340	479312.706449	41.632192
3506.014037	479290.666909	41.637197
3505.953655	479264.554218	41.642202
3506.105164	479235.114611	41.647207
3505.674970	479215.848894	41.652212
3505.940791	479200.311913	41.657216
3505.972178	479177.524760	41.662221
3505.291603	479153.947864	41.667226
3505.470738	479120.200110	41.672231
3505.265816	479116.843157	41.677236
3505.404764	479095.657582	41.682240
3505.442293	479084.462737	41.687245
3505.285377	479076.288054	41.692250
3505.616465	479055.575892	41.697255
3505.383658	479041.895845	41.702260
3505.517923	479018.989674	41.707264
3505.488225	479010.388225	41.712269
3505.514047	479002.891083	41.717274
3505.409685	478982.354441	41.722279
3505.745076	478966.552248	41.727284
3505.547587	478952.258580	41.732288
3505.643574	478918.777784	41.737293
3505.568860	478907.196977	41.742298
3505.947892	478881.109961	41.747303
3505.808002	478872.932279	41.752308
3505.949496	478843.645628	41.757312
3505.850071	478820.525970	41.762317
3506.133642	478799.973512	41.767322
3506.013327	478767.035641	41.772327
3505.921603	478745.635906	41.777332
3505.914539	478720.373995	41.782336
3505.984586	478698.440308	41.787341
3505.643921	478676.424836	41.792346
3506.010936	478646.339945	41.797351
3505.584036	478634.819097	41.802356
3505.579793	478602.671155	41.807360
3505.856795	478585.866043	41.812365
3505.710495	478570.095122	41.817370
3505.935929	478541.299931	41.822375
3505.931877	478526.821016	41.827380
3505.486573	478496.165780	41.832384
3505.865437	478476.862392	41.837389
3505.305552	478458.833090	41.842394
3505.683737	478442.516853	41.847399
3505.546259	478416.973016	41.852404
3505.362973	478400.752607	41.857408
3505.660520	478389.715452	41.862413
3505.364829	478382.171692	41.867418
3505.392727	478357.814620	41.872423
3505.508804	478360.832548	41.877428
3505.396042	478336.043806	41.882432
3505.803233	478308.432302	41.887437
3505.124781	478295.030296	41.892442
3505.465156	478273.961258	41.897447
3505.180406	478266.820612	41.902452
3505.263517	478248.276284	41.907456
3505.666478	478240.461289	41.912461
3505.115707	478230.176427	41.917466
3505.488432	478198.621582	41.922471
3505.225260	478202.868758	41.927476
3505.482758	478177.409033	41.932480
3505.573516	478161.647911	41.937485
3504.960634	478145.551253	41.942490
3504.785422	478132.772011	41.947495
3504.990447	478132.939553	41.952500
3505.130000	478116.714398	41.957504
3505.323355	478106.808705	41.962509
3504.893413	478107.084663	41.967514
3505.158385	478091.850657	41.972519
3505.169423	478073.774121	41.977524
3505.127276	478058.238119	41.982528
3505.099774	478061.331242	41.987533
3505.190882	478041.772749	41.992538
3505.606367	478022.817035	41.997543
3505.348379	478018.557605	42.002548
3505.187469	477997.168801	42.007552
3505.250987	477981.209656	42.012557
3505.282220	477982.166318	42.017562
3505.375677	477963.619933	42.022567
3505.189668	477961.322758	42.027572
3505.352921	477943.473251	42.032576
3505.347174	477926.665179	42.037581
3505.206788	477912.057162	42.042586
3505.553540	477885.569194	42.047591
3505.305761	477882.168697	42.052596
3505.094762	477861.243955	42.057600
3505.514131	477864.159551	42.062605
3505.129632	477848.479304	42.067610
3505.137771	477829.896721	42.072615
3505.293286	477837.160928	42.077620
3505.185759	477816.522248	42.082624
3505.663324	477799.834057	42.087629
3505.229073	477789.984721	42.092634
3505.362004	477758.976360	42.097639
3505.605413	477752.251636	42.102644
3504.981041	477733.321277	42.107648
3505.437541	477721.446493	42.112653
3504.947842	477703.201934	42.117658
3505.032192	477685.720060	42.122663
3505.382441	477682.014896	42.127668
3505.446113	477671.371652	42.132672
3505.620477	477650.077087	42.137677
3505.479448	477634.810761	42.142682
3505.179805	477612.685733	42.147687
3505.214637	477610.148284	42.152692
3505.630125	477587.597340	42.157696
3505.481466	477569.851355	42.162701
3505.159971	477554.058835	42.167706
3505.145106	477533.758429	42.172711
3505.567103	477538.243188	42.177716
3505.392781	477513.666361	42.182720
3505.432211	477490.774458	42.187725
3505.330226	477479.045505	42.192730
3505.435881	477455.078999	42.197735
3505.455493	477455.683255	42.202740
3505.238479	477434.404632	42.207744
3505.418422	477417.716278	42.212749
3505.068449	477397.726094	42.217754
3504.715716	477385.837369	42.222759
3505.052333	477389.070960	42.227764
3505.164413	477373.001729	42.232768
3505.136427	477353.969146	42.237773
3504.697161	477349.436722	42.242778
3505.069990	477342.537856	42.247783
3505.328971	477325.278978	42.252788
3505.219394	477319.829519	42.257792
3505.571543	477304.428079	42.262797
3505.512336	477288.944966	42.267802
3505.399362	477276.559548	42.272807
3505.301834	477259.057689	42.277812
3505.209179	477244.947304	42.282816
3505.537011	477238.309241	42.287821
3504.809680	477222.889516	42.292826
3505.085946	477200.665657	42.297831
3504.945033	477214.613492	42.302836
3505.165252	477184.247465	42.307840
3504.964895	477173.649012	42.312845
3505.222367	477169.453267	42.317850
3505.117764	477160.711838	42.322855
3505.082267	477148.161209	42.327860
3505.122530	477140.660835	42.332864
3505.354862	477121.330403	42.337869
3505.091564	477114.995753	42.342874
3505.141959	477097.367218	42.347879
3505.010541	477080.276031	42.352884
3504.933433	477070.365325	42.357888
3505.006861	477061.593451	42.362893
3505.017703	477068.629505	42.367898
3505.351476	477038.294480	42.372903
3505.020130	477036.123266	42.377908
3505.011016	477026.049030	42.382912
3505.409668	477001.576212	42.387917
3505.314222	477010.959525	42.392922
3505.249294	476982.920305	42.397927
3505.233529	476966.923178	42.402932
3505.135501	476959.648872	42.407936
3505.403404	476948.464012	42.412941
3505.193861	476931.537922	42.417946
3505.197109	476919.385581	42.422951
3504.820548	476905.070245	42.427956
3504.788457	476894.544166	42.432960
3505.082119	476890.696607	42.437965
3504.738185	476892.578138	42.442970
3505.253102	476866.313145	42.447975
3505.026114	476859.820309	42.452980
3504.914054	476853.561011	42.457984
3505.085472	476843.911545	42.462989
3505.174993	476839.491237	42.467994
3505.629668	476811.768100	42.472999
3505.375131	476803.912859	42.478004
3505.332658	476787.565705	42.483008
3505.301554	476765.748230	42.488013
3504.968356	476759.526658	42.493018
3505.187767	476741.160059	42.498023
3505.313656	476731.923372	42.503028
3505.163291	476710.885692	42.508032
3505.271958	476697.702541	42.513037
3504.746798	476692.374485	42.518042
3505.249941	476672.845443	42.523047
3505.244310	476675.124933	42.528052
3505.292685	476666.762214	42.533056
3505.145238	476639.344157	42.538061
3505.229983	476648.038656	42.543066
3505.108213	476624.818760	42.548071
3504.997012	476603.217301	42.553076
3505.339525	476604.374055	42.558080
3505.644155	476579.663561	42.563085
3505.241482	476568.339797	42.568090
3505.462372	476549.365152	42.573095
3505.143068	476533.520740	42.578100
3504.640222	476525.403974	42.583104
3505.369075	476516.216129	42.588109
3505.224371	476506.519193	42.593114
3505.038241	476489.386161	42.598119
3505.184020	476484.297924	42.603124
3505.333547	476466.348053	42.608128
3505.524723	476454.517754	42.613133
3505.095310	476429.831122	42.618138
3505.601187	476413.997616	42.623143
3505.275334	476404.483457	42.628148
3505.172013	476385.310829	42.633152
3505.182157	476379.688746	42.638157
3505.130768	476359.545176	42.643162
3504.932779	476340.135493	42.648167
3505.189353	476333.053563	42.653172
3504.988029	476326.859959	42.658176
3505.198654	476305.152566	42.663181
3505.120602	476301.570889	42.668186
3505.478517	476302.573130	42.673191
3505.365985	476278.743607	42.678196
3505.529913	476262.158206	42.683200
3505.933118	476238.949455	42.688205
3505.197745	476227.226575	42.693210
3504.838432	476205.717645	42.698215
3504.917196	476194.412718	42.703220
3504.927140	476189.094418	42.708224
3505.217315	476167.018837	42.713229
3504.969697	476161.744506	42.718234
3504.976241	476147.211260	42.723239
3505.007314	476140.572836	42.728244
3504.952027	476130.252817	42.733248
3505.249483	476107.922748	42.738253
3505.096924	476107.189305	42.743258
3504.947622	476111.316250	42.748263
3505.154687	476088.799052	42.753268
3505.071415	476087.901873	42.758272
3505.203430	476083.423494	42.763277
3504.743070	476064.159586	42.768282
3505.158455	476041.758666	42.773287
3505.179066	476048.033919	42.778292
3504.889969	476035.728368	42.783296
3504.973840	476017.991810	42.788301
3504.898159	476014.409673	42.793306
3505.089442	476020.048173	42.798311
3504.848032	475994.265517	42.803316
3504.618520	475982.456108	42.808321
3505.205839	475981.343156	42.813325
3504.667186	475982.093416	42.818330
3505.029078	475967.600626	42.823335
3504.975290	475949.786235	42.828340
3504.989064	475950.745985	42.833345
3505.193812	475940.229555	42.838349
3505.106883	475922.015714	42.843354
3504.934735	475900.677010	42.848359
3505.280948	475901.124283	42.853364
3505.227601	475890.803798	42.858369
3505.526252	475865.030021	42.863373
3505.392034	475860.343867	42.868378
3505.581692	475827.955394	42.873383
3505.663215	475818.675189	42.878388
3505.458031	475789.594744	42.883393
3505.282307	475783.143407	42.888397
3504.683829	475766.130741	42.893402
3504.486931	475747.682324	42.898407
3504.824252	475752.131349	42.903412
3504.990766	475754.482832	42.908417
3505.096233	475741.248906	42.913421
3504.922806	475736.214964	42.918426
3505.023834	475709.461995	42.923431
3505.155246	475702.958189	42.928436
3504.803106	475689.194726	42.933441
3504.783553	475668.487967	42.938445
3504.924814	475667.957519	42.943450
3505.098805	475670.409009	42.948455
3504.909321	475663.909343	42.953460
3504.823980	475646.555771	42.958465
3505.214611	475637.172061	42.963469
3504.909559	475638.591352	42.968474
3505.032046	475617.202013	42.973479
3505.104267	475607.973926	42.978484
3504.881880	475600.062042	42.983489
3505.207555	475586.891679	42.988493
3504.974457	475575.943437	42.993498
3505.068759	475567.217922	42.998503
3504.920049	475562.939257	43.003508
3505.001879	475551.886593	43.008513
3505.333860	475528.182745	43.013517
3505.186998	475525.676030	43.018522
3505.095237	475512.171796	43.023527
3505.179703	475488.307612	43.028532
3505.155545	475482.741749	43.033537
3505.061844	475459.768770	43.038541
3504.815972	475444.012151	43.043546
3504.958892	475437.050556	43.048551
3505.116996	475437.124866	43.053556
3504.742211	475425.998180	43.058561
3505.445387	475406.079187	43.063565
3505.343885	475400.475867	43.068570
3505.017149	475379.568048	43.073575
3504.899522	475369.663341	43.078580
3504.535816	475370.485025	43.083585
3504.880454	475357.969540	43.088589
3504.950413	475369.148377	43.093594
3505.169383	475333.817093	43.098599
3505.176763	475336.955356	43.103604
3504.878105	475333.259246	43.108609
3505.209546	475308.086736	43.113613
3505.055873	475298.593241	43.118618
3505.155515	475289.613498	43.123623
3505.047521	475273.276183	43.128628
3505.152995	475258.725345	43.133633
3505.067969	475257.220779	43.138637
3504.515980	475237.364001	43.143642
3504.906303	475213.751063	43.148647
3504.776706	475203.696398	43.153652
3504.813059	475211.589643	43.158657
3505.042011	475207.499598	43.163661
3505.110722	475203.588825	43.168666
3505.258161	475185.536788	43.173671
3505.424326	475178.621765	43.178676
3505.377443	475152.956628	43.183681
3505.248222	475134.496042	43.188685
3505.557332	475124.872803	43.193690
3505.172975	475105.392362	43.198695
3505.348882	475096.450141	43.203700
3505.165114	475071.821015	43.208705
3505.296638	475056.657918	43.213709
3505.440324	475049.189669	43.218714
3505.187743	475029.230908	43.223719
3505.350395	475021.759410	43.228724
3505.161823	474999.510985	43.233729
3505.122655	474982.402093	43.238733
3504.794005	474988.230962	43.243738
3505.226308	474970.889646	43.248743
3505.097229	474953.846717	43.253748
3504.820596	474945.842537	43.258753
3505.156463	474930.289979	43.263757
3505.246716	474915.944022	43.268762
3505.184545	474909.523628	43.273767
3505.095887	474895.562669	43.278772
3504.899184	474881.063127	43.283777
3504.642388	474865.206602	43.288781
3504.665912	474872.291970	43.293786
3504.747701	474869.138466	43.298791
3504.958499	474871.330588	43.303796
3504.459259	474846.653749	43.308801
3504.888579	474835.136219	43.313805
3504.430762	474840.430166	43.318810
3504.602652	474832.349355	43.323815
3504.834670	474837.981264	43.328820
3504.782253	474837.028117	43.333825
3505.510716	474819.281624	43.338829
3504.686000	474808.079470	43.343834
3504.599022	474802.676043	43.348839
3505.054084	474782.849382	43.353844
3504.647668	474777.854958	43.358849
3504.835239	474757.770112	43.363853
3504.888615	474747.380126	43.368858
3504.848520	474755.185341	43.373863
3505.455547	474751.638306	43.378868
3504.807666	474734.379925	43.383873
3505.066854	474724.967558	43.388877
3505.138914	474724.145067	43.393882
3505.199695	474699.271135	43.398887
3505.212414	474689.748917	43.403892
3504.915883	474678.912249	43.408897
3504.948475	474657.891619	43.413901
3504.745965	474644.355020	43.418906
3504.831328	474642.314923	43.423911
3505.068979	474636.147074	43.428916
3504.552191	474628.588872	43.433921
3504.703993	474603.597992	43.438925
3504.530215	474608.894146	43.443930
3504.489122	474611.028030	43.448935
3504.574262	474607.367520	43.453940
3504.481630	474608.244230	43.458945
3504.848645	474612.435268	43.463949
3504.795684	474607.734920	43.468954
3504.536272	474591.270938	43.473959
3504.920640	474583.862686	43.478964
3504.463206	474576.496883	43.483969
3504.749245	474565.256845	43.488973
3504.587760	474572.171361	43.493978
3504.653262	474570.185286	43.498983
3505.012222	474570.579779	43.503988
3504.931458	474546.945147	43.508993
3505.009871	474532.904749	43.513997
3504.642837	474533.220644	43.519002
3504.849153	474536.325077	43.524007
3505.198569	474510.692661	43.529012
3505.125415	474505.894457	43.534017
3505.075952	474494.914217	43.539021
3504.575609	474481.377712	43.544026
3504.484345	474461.897186	43.549031
3504.977006	474452.039702	43.554036
3504.803245	474463.513898	43.559041
3505.010448	474452.540449	43.564045
3504.676077	474439.937723	43.569050
3505.233745	474423.992395	43.574055
3505.121728	474419.302083	43.579060
3504.681976	474425.960328	43.584065
3504.926006	474407.840401	43.589069
3504.771430	474393.839678	43.594074
3504.772146	474384.218073	43.599079
3505.009190	474386.152574	43.604084
3504.797745	474391.050105	43.609089
3504.704950	474360.175832	43.614093
3504.999924	474352.377634	43.619098
3504.978549	474347.165431	43.624103
3505.002024	474351.060708	43.629108
3504.584694	474334.522181	43.634113
3504.916142	474310.968785	43.639117
3505.139590	474313.260094	43.644122
3504.817220	474316.758670	43.649127
3504.993923	474310.854319	43.654132
3504.828440	474296.399628	43.659137
3504.904420	474284.739528	43.664141
3505.119502	474285.664993	43.669146
3505.209538	474265.444347	43.674151
3505.170516	474252.031466	43.679156
3504.971539	474247.507877	43.684161
3505.341601	474230.429697	43.689165
3505.259757	474210.390258	43.694170
3505.185646	474201.490295	43.699175
3505.587356	474178.583055	43.704180
3505.242140	474172.615854	43.709185
3505.658584	474150.566946	43.714189
3505.528171	474131.953641	43.719194
3505.493026	474109.728589	43.724199
3505.573419	474091.383092	43.729204
3505.192390	474082.535475	43.734209
3505.254448	474054.419474	43.739213
3505.226313	474045.410304	43.744218
3504.968827	474031.578800	43.749223
3505.082060	474004.618718	43.754228
3504.865452	474004.605093	43.759233
3505.078147	474002.289982	43.764237
3504.690398	473988.278124	43.769242
3505.066680	473970.590956	43.774247
3505.220510	473972.894194	43.779252
3504.877849	473972.851450	43.784257
3505.211506	473939.422270	43.789261
3504.967698	473931.969093	43.794266
3504.915392	473928.888966	43.799271
3505.326247	473919.551577	43.804276
3505.119038	473901.052434	43.809281
3505.013163	473891.955182	43.814285
3504.791783	473878.927653	43.819290
3504.653741	473857.833969	43.824295
3504.629107	473851.356157	43.829300
3504.628561	473854.749230	43.834305
3504.708384	473843.797171	43.839309
3504.849669	473848.128208	43.844314
3504.769525	473832.696404	43.849319
3505.131192	473826.051343	43.854324
3504.936499	473817.323707	43.859329
3505.171903	473815.865594	43.864333
3504.910070	473802.743637	43.869338
3505.213282	473782.789914	43.874343
3505.199083	473778.133378	43.879348
3505.063669	473771.016118	43.884353
3505.050648	473741.393225	43.889357
3505.081327	473734.045025	43.894362
3505.054738	473724.326457	43.899367
3505.082325	473703.052393	43.904372
3505.152221	473697.672499	43.909377
3505.221849	473692.697780	43.914381
3505.121361	473680.662300	43.919386
3505.336360	473668.978077	43.924391
3505.085940	473657.829088	43.929396
3504.017957	473631.880413	43.934401
3504.498112	473616.150195	43.939405
3504.673834	473620.222197	43.944410
3504.377576	473617.791372	43.949415
3504.657056	473608.324334	43.954420
3504.378130	473614.246424	43.959425
3504.882426	473610.919284	43.964429
3504.675317	473620.677876	43.969434
3504.476935	473613.621948	43.974439
3504.534077	473596.545973	43.979444
3504.448812	473599.649708	43.984449
3504.385943	473578.289662	43.989453
3504.584514	473594.106654	43.994458
3504.828649	473590.520081	43.999463
3505.063315	473584.301753	44.004468
3504.788406	473592.299475	44.009473
3504.942533	473572.928042	44.014477
3504.870268	473559.925471	44.019482
3504.748411	473553.818648	44.024487
3505.298068	473541.520145	44.029492
3504.854500	473536.329158	44.034497
3504.718782	473517.918710	44.039501
3504.800351	473515.423359	44.044506
3505.155508	473523.212249	44.049511
3504.893864	473496.416721	44.054516
3504.363452	473479.137106	44.059521
3504.900588	473467.195187	44.064525
3504.982596	473475.790365	44.069530
3504.924245	473474.686235	44.074535
3504.680086	473461.561018	44.079540
3504.173389	473437.086139	44.084545
3505.056723	473433.491682	44.089549
3504.942055	473434.777345	44.094554
3504.820593	473429.379404	44.099559
3504.845684	473425.273136	44.104564
3504.748154	473421.491656	44.109569
3504.993090	473401.344906	44.114573
3505.023740	473405.796221	44.119578
3504.583786	473403.946967	44.124583
3505.362474	473390.748342	44.129588
3505.076756	473379.858423	44.134593
3505.392414	473373.372985	44.139597
3505.059479	473352.717142	44.144602
3504.506699	473329.819903	44.149607
3504.765769	473317.317656	44.154612
3504.664099	473325.032701	44.159617
3504.669525	473308.927499	44.164621
3504.608818	473320.535024	44.169626
3504.455124	473306.178832	44.174631
3504.939889	473281.179965	44.179636
3504.704112	473285.069089	44.184641
3504.612301	473284.375800	44.189645
3504.342644	473283.763520	44.194650
3504.611468	473279.666246	44.199655
3504.585727	473282.050874	44.204660
3504.506455	473283.583718	44.209665
3504.743134	473263.539514	44.214669
3504.956360	473242.131941	44.219674
3504.522031	473245.801761	44.224679
3505.046152	473240.192251	44.229684
3504.704909	473254.329207	44.234689
3504.762792	473241.354834	44.239693
3504.616961	473226.186955	44.244698
3504.851369	473205.991150	44.249703
3505.062814	473201.650442	44.254708
3504.844795	473214.550962	44.259713
3504.972659	473189.258411	44.264717
3504.934546	473179.693454	44.269722
3504.426496	473175.880732	44.274727
3504.785500	473167.716607	44.279732
3504.849476	473174.897003	44.284737
3504.615861	473162.124274	44.289741
3504.554945	473147.600190	44.294746
3504.246615	473136.359488	44.299751
3504.436987	473122.805339	44.304756
3504.519918	473138.490534	44.309761
3504.304802	473129.360917	44.314765
3504.636064	473137.761765	44.319770
3504.507877	473137.327897	44.324775
3504.894375	473137.464509	44.329780
3504.737303	473134.756639	44.334785
3505.242986	473123.123728	44.339789
3504.846386	473115.341809	44.344794
3504.871972	473111.792460	44.349799
3505.052823	473096.011623	44.354804
3504.755558	473083.350994	44.359809
3505.121329	473071.792584	44.364813
3504.918163	473072.637594	44.369818
3504.603809	473071.830366	44.374823
3505.105857	473054.931147	44.379828
3504.851773	473040.845106	44.384833
3504.635561	473022.599841	44.389837
3504.831007	473024.541590	44.394842
3504.847081	473026.260747	44.399847
3504.334603	473013.484887	44.404852
3504.375465	472996.259212	44.409857
3504.744828	472985.459785	44.414861
3504.941199	472987.958456	44.419866
3504.718061	472993.921860	44.424871
3504.829680	472983.774160	44.429876
3504.572558	472998.454024	44.434881
3504.675798	472980.103530	44.439885
3505.002138	472960.043692	44.444890
3504.900917	472954.996661	44.449895
3505.173332	472942.846390	44.454900
3504.848594	472936.875291	44.459905
3505.253872	472922.271432	44.464909
3504.930123	472907.943969	44.469914
3504.889953	472914.230662	44.474919
3505.007081	472887.572159	44.479924
3504.551843	472882.433623	44.484929
3504.732066	472869.235528	44.489933
3504.967335	472867.979940	44.494938
3504.510668	472881.984955	44.499943
3504.784558	472857.477320	44.504948
3504.580532	472848.852108	44.509953
3504.726396	472833.836680	44.514957
3504.870707	472833.254990	44.519962
3504.864987	472833.711792	44.524967
3504.998701	472824.370534	44.529972
3504.438944	472804.208603	44.534977
3504.486603	472796.603916	44.539981
3505.024151	472797.423755	44.544986
3504.595901	472799.066867	44.549991
3504.834366	472786.111988	44.554996
3505.025525	472795.853654	44.560001
3505.066208	472762.573674	44.565005
3505.233851	472757.987123	44.570010
3505.225238	472763.154312	44.575015
3505.387816	472735.221731	44.580020
3504.736130	472723.735541	44.585025
3504.525002	472713.136360	44.590029
3504.731543	472714.265941	44.595034
3504.541270	472694.597890	44.600039
3504.565637	472680.160168	44.605044
3504.533490	472683.761427	44.610049
3504.711322	472680.388578	44.615053
3504.975019	472677.203644	44.620058
3504.974066	472675.988378	44.625063
3504.854527	472654.940814	44.630068
3504.859877	472643.848833	44.635073
3504.595962	472645.311966	44.640077
3504.784523	472641.684057	44.645082
3504.281433	472643.745115	44.650087
3504.902026	472641.512124	44.655092
3504.616851	472628.494611	44.660097
3504.929810	472611.728566	44.665101
3504.763009	472608.414547	44.670106
3504.596398	472606.771761	44.675111
3504.752492	472604.010343	44.680116
3504.924282	472599.017890	44.685121
3505.037885	472577.373343	44.690125
3504.763573	472579.243412	44.695130
3504.779834	472570.884327	44.700135
3504.811928	472556.495835	44.705140
3504.753783	472547.896220	44.710145
3504.764180	472538.626519	44.715149
3504.738219	472529.261733	44.720154
3504.614056	472526.649444	44.725159
3505.001976	472524.304233	44.730164
3504.788509	472510.717303	44.735169
3504.541707	472499.313776	44.740173
3504.923605	472491.398672	44.745178
3504.869348	472496.826952	44.750183
3505.283018	472487.792238	44.755188
3504.864894	472474.746673	44.760193
3504.750610	472466.308540	44.765197
3504.914442	472464.558676	44.770202
3504.797312	472470.554790	44.775207
3505.009085	472457.553597	44.780212
3504.783810	472438.347056	44.785217
3505.088840	472422.493803	44.790221
3504.842454	472423.194287	44.795226
3504.912570	472410.622407	44.800231
3505.029551	472386.799331	44.805236
3504.811934	472389.621993	44.810241
3504.333471	472381.144713	44.815245
3504.604679	472371.475883	44.820250
3504.755507	472379.958526	44.825255
3504.959402	472357.994439	44.830260
3505.016627	472341.119881	44.835265
3505.057609	472338.732595	44.840269
3504.715808	472333.473247	44.845274
3504.590703	472324.125285	44.850279
3504.786841	472308.037302	44.855284
3504.707944	472295.288206	44.860289
3504.823625	472303.473014	44.865293
3504.737880	472303.386396	44.870298
3504.601789	472302.194178	44.875303
3504.867618	472287.613635	44.880308
3504.498296	472266.912155	44.885313
3504.705040	472267.079467	44.890317
3504.678438	472262.931124	44.895322
3504.630632	472270.991924	44.900327
3505.166482	472260.670108	44.905332
3504.822308	472249.536281	44.910337
3504.991872	472232.895672	44.915341
3504.568983	472227.396911	44.920346
3504.448302	472221.795905	44.925351
3504.703697	472223.676856	44.930356
3504.828060	472220.667573	44.935361
3504.859838	472206.430802	44.940365
3505.069261	472189.479475	44.945370
3505.047479	472189.128707	44.950375
3505.110814	472173.772322	44.955380
3504.992124	472155.357620	44.960385
3505.196313	472146.662384	44.965389
3505.206578	472143.469986	44.970394
3504.756756	472127.188267	44.975399
3504.965096	472107.957995	44.980404
3504.844469	472110.764139	44.985409
3504.664054	472098.690638	44.990413
3504.896719	472088.319202	44.995418
3504.943946	472080.714297	45.000423
3505.181703	472060.668621	45.005428
3504.606466	472064.615956	45.010433
3504.595694	472045.625615	45.015437
3504.543401	472034.036656	45.020442
3504.484789	472029.083391	45.025447
3504.476271	472016.474026	45.030452
3504.621790	472019.285388	45.035457
3504.834751	472016.564820	45.040461
3504.510263	472022.951004	45.045466
3504.357128	472025.053667	45.050471
3504.705187	472017.144142	45.055476
3504.445618	472024.430870	45.060481
3504.671459	471997.296722	45.065485
3505.135262	471988.709024	45.070490
3504.895340	471995.941761	45.075495
3504.925277	471988.086541	45.080500
3504.946177	471971.065914	45.085505
3504.685757	471951.560996	45.090509
3505.143383	471938.618758	45.095514
3504.566716	471943.427348	45.100519
3504.948890	471939.664954	45.105524
3504.780911	471921.157145	45.110529
3504.690447	471910.587551	45.115533
3504.485423	471902.823059	45.120538
3504.638190	471911.305584	45.125543
3504.882808	471897.842579	45.130548
3504.601373	471898.751651	45.135553
3504.731828	471891.081812	45.140557
3504.759325	471877.453278	45.145562
3504.721621	471878.371382	45.150567
3504.658363	471868.050351	45.155572
3504.638615	471871.801588	45.160577
3504.596302	471869.580403	45.165581
3505.110992	471857.033537	45.170586
3504.908440	471845.520762	45.175591
3504.781366	471835.565135	45.180596
3504.619366	471842.936566	45.185601
3504.457855	471842.710942	45.190605
3504.906507	471833.568649	45.195610
3504.545303	471820.158381	45.200615
3504.930776	471800.948197	45.205620
3504.778168	471803.557261	45.210625
3504.870082	471801.059916	45.215629
3505.115744	471797.118215	45.220634
3504.658483	471782.964622	45.225639
3505.235682	471763.215198	45.230644
3504.523495	471768.300204	45.235649
3504.305678	471765.551859	45.240653
3504.607961	471763.980878	45.245658
3504.689230	471752.470233	45.250663
3504.361022	471729.228800	45.255668
3504.647730	471725.786544	45.260673
3504.591760	471719.769163	45.265677
3504.772373	471720.346118	45.270682
3504.530874	471721.805494	45.275687
3504.699013	471723.650748	45.280692
3504.549652	471720.688121	45.285697
3504.262894	471715.621787	45.290701
3504.389172	471704.812483	45.295706
3504.812647	471706.715436	45.300711
3504.634377	471684.208049	45.305716
3504.781190	471689.956759	45.310721
3504.774138	471685.247834	45.315725
3504.767649	471683.932154	45.320730
3504.581222	471686.192480	45.325735
3504.781523	471648.122456	45.330740
3504.959392	471641.102831	45.335745
3504.947176	471643.890534	45.340749
3504.984687	471639.579164	45.345754
3505.150396	471640.209314	45.350759
3504.953248	471616.590834	45.355764
3504.562708	471610.731838	45.360769
3504.789225	471609.021839	45.365773
3505.443053	471592.348625	45.370778
3504.830841	471578.525216	45.375783
3505.268150	471560.774705	45.380788
3504.771588	471557.516803	45.385793
3504.963445	471542.036662	45.390797
3505.050795	471534.374038	45.395802
3505.031654	471527.084124	45.400807
3504.959004	471512.054299	45.405812
3504.770144	471491.878268	45.410817
3504.732612	471497.759808	45.415821
3505.103056	471483.363369	45.420826
3504.703425	471487.686018	45.425831
3504.526278	471466.089832	45.430836
3504.662810	471444.642652	45.435841
3504.569832	471439.188623	45.440845
3504.770273	471436.824643	45.445850
3504.687382	471439.269910	45.450855
3504.599203	471438.626579	45.455860
3504.302401	471448.452264	45.460865
3504.549602	471438.584464	45.465869
3504.766128	471414.135385	45.470874
3504.417010	471406.901765	45.475879
3504.578705	471395.326522	45.480884
3504.861509	471396.493811	45.485889
3504.582105	471389.754759	45.490893
3504.539114	471393.459412	45.495898
3504.613294	471402.158177	45.500903
3504.507359	471398.377721	45.505908
3504.180154	471386.024937	45.510913
3504.418244	471374.943114	45.515917
3504.559464	471366.308917	45.520922
3504.500821	471370.218838	45.525927
3505.525953	471360.420762	45.530932
3504.871876	471359.418221	45.535937
3504.842112	471354.510500	45.540941
3504.910870	471332.568286	45.545946
3504.817363	471323.670260	45.550951
3504.757147	471321.148179	45.555956
3504.754940	471328.036698	45.560961
3504.636252	471312.558743	45.565965
3504.560160	471293.274906	45.570970
3504.412541	471287.019795	45.575975
3504.734412	471290.054395	45.580980
3504.972402	471282.062060	45.585985
3504.887624	471287.040069	45.590989
3504.776451	471273.890605	45.595994
3504.673809	471258.916346	45.600999
3504.445852	471245.736155	45.606004
3504.470074	471242.946406	45.611009
3504.557292	471241.361455	45.616013
3505.024545	471229.176809	45.621018
3504.921474	471238.361747	45.626023
3504.930183	471237.853811	45.631028
3504.714941	471221.733841	45.636033
3504.563124	471216.289794	45.641037
3504.758914	471209.216300	45.646042
3504.682418	471221.891433	45.651047
3505.028627	471215.805222	45.656052
3504.543978	471192.539186	45.661057
3504.611269	471172.167131	45.666061
3504.762492	471171.888101	45.671066
3504.688458	471179.852552	45.676071
3504.672172	471178.032026	45.681076
3504.374313	471178.032267	45.686081
3504.553776	471176.431560	45.691085
3504.572405	471165.792271	45.696090
3504.501616	471149.900818	45.701095
3504.899127	471136.613756	45.706100
3504.420753	471136.492873	45.711105
3504.351044	471141.822885	45.716109
3504.589618	471136.210861	45.721114
3504.219033	471156.280265	45.726119
3504.731313	471144.442414	45.731124
3504.462540	471149.350578	45.736129
3504.806507	471140.782957	45.741133
3504.458193	471119.924674	45.746138
3504.370469	471108.797028	45.751143
3504.517066	471099.199470	45.756148
3504.702317	471103.523640	45.761153
3504.508639	471100.771074	45.766157
3504.672421	471098.767851	45.771162
3504.785656	471102.496535	45.776167
3504.667723	471106.771174	45.781172
3504.998507	471101.852474	45.786177
3504.585875	471076.244168	45.791181
3504.696443	471073.237057	45.796186
3504.552505	471073.160367	45.801191
3504.623753	471066.057436	45.806196
3504.813227	471074.432776	45.811201
3504.517456	471062.125060	45.816205
3504.683994	471037.987919	45.821210
3504.365740	471035.256614	45.826215
3504.619883	471026.299089	45.831220
3504.598107	471031.165110	45.836225
3504.330901	471031.413359	45.841229
3504.662663	471032.521664	45.846234
3504.308985	471031.873002	45.851239
3504.884587	471022.050210	45.856244
3504.618608	471028.274793	45.861249
3504.696189	471008.964426	45.866253
3505.205708	470992.821811	45.871258
3504.821089	470989.747290	45.876263
3505.073812	470976.738081	45.881268
3505.070714	470973.547766	45.886273
3505.139795	470950.136236	45.891277
3505.005752	470944.537128	45.896282
3504.383439	470947.327806	45.901287
3504.820051	470929.323575	45.906292
3504.713490	470918.654873	45.911297
3504.502438	470906.636484	45.916301
3504.919597	470905.045818	45.921306
3504.452719	470907.100877	45.926311
3504.578817	470907.991060	45.931316
3504.677700	470910.607955	45.936321
3504.496233	470890.987155	45.941325
3504.767289	470875.340996	45.946330
3504.444023	470873.674154	45.951335
3504.821245	470865.657870	45.956340
3504.819162	470864.847871	45.961345
3504.873615	470863.926921	45.966349
3504.584777	470857.442534	45.971354
3505.112219	470831.774682	45.976359
3505.296498	470825.817293	45.981364
3505.156597	470833.337293	45.986369
3505.188172	470807.652776	45.991373
3505.298972	470792.540404	45.996378
3505.018733	470792.942829	46.001383
3504.939918	470759.173204	46.006388
3504.614979	470757.101442	46.011393
3504.622591	470751.072894	46.016397
3505.031894	470748.977064	46.021402
3504.992453	470740.120180	46.026407
3505.152918	470710.817413	46.031412
3504.903929	470702.401485	46.036417
3504.909796	470706.199230	46.041421
3504.997775	470686.481562	46.046426
3504.819631	470674.558704	46.051431
3504.862300	470667.004655	46.056436
3505.042349	470658.312855	46.061441
3504.936872	470643.389239	46.066445
3505.030046	470625.595308	46.071450
3504.862742	470629.574586	46.076455
3504.670473	470624.035974	46.081460
3504.392735	470621.956137	46.086465
3504.493511	470617.785681	46.091469
3504.900436	470595.784870	46.096474
3504.762874	470593.883695	46.101479
3504.861491	470587.434359	46.106484
3504.610558	470589.148680	46.111489
3504.598313	470594.266436	46.116493
3504.460080	470581.627607	46.121498
3504.857820	470581.053229	46.126503
3504.710722	470561.274267	46.131508
3504.779464	470563.845707	46.136513
3504.225946	470559.381754	46.141517
3504.756389	470545.818331	46.146522
3504.351651	470553.636912	46.151527
3504.604201	470551.010675	46.156532
3504.743472	470547.289480	46.161537
3504.209865	470533.553177	46.166541
3504.645075	470511.142238	46.171546
3504.387409	470513.262916	46.176551
3504.586742	470510.291210	46.181556
3504.424656	470515.181321	46.186561
3504.323615	470510.842700	46.191565
3504.693636	470509.817202	46.196570
3504.453060	470512.492113	46.201575
3504.588996	470500.110318	46.206580
3504.754476	470496.840489	46.211585
3504.590584	470501.528312	46.216589
3504.498382	470493.592021	46.221594
3504.443871	470478.507623	46.226599
3504.740889	470466.300902	46.231604
3505.127421	470465.728435	46.236609
3504.830167	470467.096125	46.241613
3504.940033	470462.214980	46.246618
3504.024248	470444.694451	46.251623
3504.331652	470434.056093	46.256628
3504.433318	470439.964846	46.261633
3504.261075	470437.715025	46.266637
3504.368318	470436.481140	46.271642
3504.320901	470442.972499	46.276647
3504.162815	470434.946133	46.281652
3504.392574	470428.322399	46.286657
3504.275456	470435.281515	46.291661
3504.561899	470428.648103	46.296666
3504.727134	470430.645933	46.301671
3504.756712	470430.843516	46.306676
3504.595756	470435.328252	46.311681
3504.404214	470439.463659	46.316685
3504.743965	470440.874538	46.321690
3504.475209	470436.615186	46.326695
3504.512348	470418.172174	46.331700
3504.507706	470400.344081	46.336705
3504.520375	470397.100327	46.341709
3504.704576	470393.219479	46.346714
3504.629891	470398.905104	46.351719
3504.376511	470387.349462	46.356724
3504.258900	470399.626965	46.361729
3504.460652	470396.908080	46.366733
3504.858227	470392.990801	46.371738
3504.833190	470393.653562	46.376743
3505.030466	470363.432264	46.381748
3504.800917	470356.583026	46.386753
3504.417935	470354.622430	46.391757
3504.879008	470347.553970	46.396762
3504.961549	470355.340083	46.401767
3505.051689	470331.367034	46.406772
3505.127031	470315.449925	46.411777
3504.952320	470315.631739	46.416781
3504.854673	470299.946756	46.421786
3504.647259	470286.661083	46.426791
3504.886036	470274.210930	46.431796
3505.046720	470277.881026	46.436801
3504.779535	470274.178526	46.441805
3504.718807	470240.759440	46.446810
3504.293620	470243.972417	46.451815
3504.264566	470239.621442	46.456820
3504.662620	470238.895049	46.461825
3504.392123	470240.865995	46.466829
3504.829765	470228.483159	46.471834
3504.436686	470241.820814	46.476839
3504.624704	470240.319870	46.481844
3504.725191	470240.505348	46.486849
3504.385438	470222.025194	46.491853
3504.590727	470199.906398	46.496858
3504.551794	470204.319704	46.501863
3504.744631	470203.678999	46.506868
3504.736332	470202.819383	46.511873
3504.957740	470195.133325	46.516877
3504.943476	470190.577210	46.521882
3504.990670	470180.084441	46.526887
3504.672681	470162.258975	46.531892
3504.744279	470157.890796	46.536897
3504.380960	470162.055592	46.541901
3504.824294	470160.966908	46.546906
3504.717829	470147.866505	46.551911
3504.861735	470117.856531	46.556916
3504.651390	470122.400426	46.561921
3504.652075	470118.702809	46.566925
3504.482969	470118.883668	46.571930
3504.153080	470124.967506	46.576935
3504.453696	470124.612303	46.581940
3505.011680	470116.666142	46.586945
3504.765965	470106.881809	46.591949
3504.922047	470081.934813	46.596954
3504.720168	470081.158894	46.601959
3504.705213	470078.628918	46.606964
3504.911655	470076.314397	46.611969
3504.465190	470065.399340	46.616973
3504.899679	470038.530654	46.621978
3504.551880	470039.096583	46.626983
3504.658425	470038.268002	46.631988
3504.784280	470034.954208	46.636993
3504.896958	470043.444423	46.641997
3504.833523	470020.003714	46.647002
3504.745624	470007.507860	46.652007
3505.005245	470003.310147	46.657012
3504.832232	469996.349822	46.662017
3504.519286	469996.352635	46.667021
3504.870706	469985.959768	46.672026
3504.550907	469978.062121	46.677031
3504.497330	469971.030743	46.682036
3504.545282	469964.285935	46.687041
3504.375661	469970.798322	46.692045
3504.442139	469968.963549	46.697050
3504.300160	469971.469746	46.702055
3504.606005	469970.049966	46.707060
3504.666818	469976.472355	46.712065
3504.439820	469979.145022	46.717069
3504.527876	469954.412078	46.722074
3504.605875	469940.672217	46.727079
3504.374204	469930.834743	46.732084
3504.446969	469928.289769	46.737089
3504.339691	469930.790047	46.742093
3504.520895	469922.958789	46.747098
3504.670484	469933.316861	46.752103
3504.799022	469927.571314	46.757108
3504.926437	469933.323874	46.762113
3504.789501	469917.088114	46.767117
3504.671738	469896.290413	46.772122
3504.750468	469894.504192	46.777127
3504.719494	469898.612300	46.782132
3504.903724	469892.401368	46.787137
3504.319124	469893.564901	46.792141
3504.409408	469885.698500	46.797146
3504.563600	469869.818205	46.802151
3504.609154	469855.931867	46.807156
3504.710107	469843.656919	46.812161
3504.578333	469847.680945	46.817165
3504.673222	469840.674820	46.822170
3504.554599	469844.038128	46.827175
3504.462213	469839.647223	46.832180
3504.319551	469842.862679	46.837185
3504.296005	469843.879768	46.842189
3504.660860	469841.538170	46.847194
3504.408885	469833.730186	46.852199
3504.030558	469817.535556	46.857204
3504.373317	469820.262919	46.862209
3504.371890	469842.296761	46.867213
3504.681182	469819.653245	46.872218
3504.568585	469815.519045	46.877223
3504.769880	469817.409479	46.882228
3504.611733	469817.639121	46.887233
3504.460578	469812.498465	46.892237
3504.650108	469813.276566	46.897242
3504.533614	469815.373217	46.902247
3504.795701	469805.805936	46.907252
3504.851848	469783.053643	46.912257
3504.200753	469783.418103	46.917261
3504.663352	469773.056789	46.922266
3504.743041	469774.714732	46.927271
3504.520621	469774.043611	46.932276
3504.752823	469778.410722	46.937281
3504.460787	469774.813671	46.942285
3504.316353	469759.490792	46.947290
3504.743132	469744.627544	46.952295
3504.398120	469739.013446	46.957300
3504.554469	469731.946135	46.962305
3504.284084	469734.727548	46.967309
3504.502908	469723.445439	46.972314
3504.653715	469729.346025	46.977319
3504.470428	469724.565396	46.982324
3504.702513	469722.904931	46.987329
3504.471642	469730.795467	46.992333
3504.913949	469726.363893	46.997338
3504.733179	469709.932830	47.002343
3504.662471	469700.776883	47.007348
3504.954673	469692.926579	47.012353
3504.623631	469694.553353	47.017357
3504.610210	469690.351539	47.022362
3504.719832	469693.675902	47.027367
3504.623971	469669.733773	47.032372
3504.796617	469656.585373	47.037377
3504.739962	469657.810734	47.042381
3504.569465	469654.547474	47.047386
3504.562236	469655.004611	47.052391
3504.256120	469649.231888	47.057396
3505.055732	469655.578894	47.062401
3504.712216	469643.126444	47.067405
3504.802595	469621.077245	47.072410
3504.714110	469615.672572	47.077415
3504.791745	469620.116764	47.082420
3505.088325	469615.102216	47.087425
3505.053615	469608.219439	47.092429
3504.833762	469586.679042	47.097434
3505.145089	469586.423306	47.102439
3505.018976	469564.562963	47.107444
3504.709869	469541.771440	47.112449
3504.473745	469545.863999	47.117453
3504.814370	469535.827298	47.122458
3504.626577	469539.506386	47.127463
3504.708061	469540.404253	47.132468
3504.930535	469531.755345	47.137473
3504.375103	469516.806360	47.142477
3504.462651	469500.025385	47.147482
3504.196714	469501.944976	47.152487
3504.334131	469500.705878	47.157492
3504.670809	469493.708995	47.162497
3504.297009	469504.612542	47.167501
3504.399677	469500.188254	47.172506
3504.297132	469501.066891	47.177511
3504.298538	469495.950752	47.182516
3504.515634	469497.737216	47.187521
3504.441059	469513.705597	47.192525
3504.415134	469510.164364	47.197530
3504.304255	469513.222491	47.202535
3504.344488	469499.235495	47.207540
3504.428569	469501.095322	47.212545
3504.070100	469503.790503	47.217549
3504.380961	469503.585499	47.222554
3504.454689	469503.826206	47.227559
3504.332710	469505.417300	47.232564
3504.781998	469497.590746	47.237569
3504.608985	469484.754510	47.242573
3505.002243	469472.682677	47.247578
3504.475856	469464.009642	47.252583
3504.462390	469455.958166	47.257588
3504.783042	469453.978639	47.262593
3504.535489	469459.390144	47.267597
3504.412692	469456.017399	47.272602
3504.309216	469463.531723	47.277607
3504.650761	469448.834756	47.282612
3504.659757	469435.156963	47.287617
3504.484893	469424.144507	47.292621
3504.470795	469410.521293	47.297626
3504.621222	469418.954689	47.302631
3504.598052	469421.035449	47.307636
3504.575223	469418.354771	47.312641
3504.264463	469418.965045	47.317645
3504.878754	469415.821012	47.322650
3504.760651	469415.132067	47.327655
3504.712290	469400.197717	47.332660
3505.381807	469379.011761	47.337665
3504.793030	469385.849181	47.342669
3504.900701	469372.863638	47.347674
3504.520399	469366.191739	47.352679
3504.586919	469353.517128	47.357684
3505.024402	469348.883678	47.362689
3504.872332	469356.558301	47.367693
3504.869954	469343.135650	47.372698
3504.869437	469328.851566	47.377703
3504.640039	469309.693185	47.382708
3504.670690	469304.673308	47.387713
3504.399897	469309.379677	47.392717
3504.120002	469302.082772	47.397722
3504.230080	469306.673458	47.402727
3504.207868	469306.322709	47.407732
3504.326753	469307.366161	47.412737
3504.279027	469306.817155	47.417741
3504.706051	469310.847191	47.422746
3505.072670	469307.137589	47.427751
3504.618712	469299.414524	47.432756
3504.730080	469283.439743	47.437761
3504.872772	469275.513488	47.442765
3504.849589	469267.818165	47.447770
3504.663427	469267.394102	47.452775
3504.603513	469273.229502	47.457780
3504.669061	469247.334451	47.462785
3504.459052	469238.961867	47.467789
3504.810111	469227.808847	47.472794
3504.433932	469234.154140	47.477799
3504.299096	469234.329154	47.482804
3504.371105	469221.501557	47.487809
3503.913764	469238.497941	47.492813
3504.523243	469223.704398	47.497818
3504.180225	469223.560383	47.502823
3504.306086	469231.339563	47.507828
3504.430480	469225.341243	47.512833
3504.168914	469231.413700	47.517837
3504.353487	469232.192673	47.522842
3504.323262	469226.676635	47.527847
3504.263001	469220.304614	47.532852
3504.707475	469225.648680	47.537857
3504.619412	469228.095115	47.542861
3504.784803	469225.939461	47.547866
3504.481856	469234.956885	47.552871
3504.474215	469219.711520	47.557876
3504.825246	469195.540528	47.562881
3504.350302	469199.370017	47.567885
3504.652556	469193.594587	47.572890
3504.511581	469197.519014	47.577895
3504.451916	469197.427926	47.582900
3504.470203	469191.549019	47.587905
3504.852460	469193.206005	47.592909
3504.957059	469184.222491	47.597914
3504.921798	469169.032454	47.602919
3504.837032	469153.749551	47.607924
3505.067912	469145.099032	47.612929
3504.675894	469146.381687	47.617933
3504.701073	469129.408419	47.622938
3504.975608	469117.305979	47.627943
3504.531111	469107.656375	47.632948
3504.927931	469105.207923	47.637953
3504.659389	469110.420495	47.642957
3504.971537	469090.308312	47.647962
3504.993970	469078.147584	47.652967
3504.775226	469078.438233	47.657972
3504.747839	469066.336657	47.662977
3504.742280	469070.795183	47.667981
3504.978766	469052.671381	47.672986
3504.693691	469031.344105	47.677991
3504.609712	469032.827441	47.682996
3504.599226	469022.546496	47.688001
3504.469750	469036.802414	47.693005
3504.466631	469016.338751	47.698010
3504.341135	469024.566165	47.703015
3504.238915	469032.789601	47.708020
3504.560789	469025.693766	47.713025
3504.508640	469024.335043	47.718029
3504.311270	468993.875021	47.723034
3504.383753	468997.307156	47.728039
3504.376028	468988.393381	47.733044
3504.890062	468988.913495	47.738049
3504.491524	468997.136887	47.743053
3504.856173	468989.881773	47.748058
3504.642665	468990.728725	47.753063
3504.605690	468991.849461	47.758068
3504.679275	468984.796004	47.763073
3504.387684	468972.688825	47.768077
3504.769031	468955.806552	47.773082
3504.570885	468957.866583	47.778087
3503.908562	468950.432222	47.783092
3504.413129	468947.661429	47.788097
3504.262450	468958.780462	47.793101
3504.497633	468951.446131	47.798106
3504.439269	468958.851643	47.803111
3504.409796	468958.400819	47.808116
3504.573528	468950.268219	47.813121
3504.578666	468953.863824	47.818125
3504.468886	468950.032878	47.823130
3504.485865	468962.136368	47.828135
3504.409171	468947.358462	47.833140
3504.193538	468951.751576	47.838145
3504.166976	468958.645116	47.843149
3504.681188	468941.588182	47.848154
3504.851121	468927.325348	47.853159
3504.721529	468917.267299	47.858164
3504.686889	468906.686489	47.863169
3504.877145	468914.201532	47.868173
3504.804859	468908.743238	47.873178
3504.798018	468895.878230	47.878183
3504.597781	468883.147543	47.883188
3504.518121	468867.964847	47.888193
3504.614039	468876.053212	47.893197
3505.049825	468860.275956	47.898202
3504.759062	468863.567519	47.903207
3504.538823	468855.348476	47.908212
3504.540301	468837.061977	47.913217
3504.606724	468839.228812	47.918221
3504.844661	468834.578655	47.923226
3504.550318	468828.601052	47.928231
3504.741454	468835.761394	47.933236
3505.063915	468830.387641	47.938241
3504.632752	468820.127759	47.943245
3504.557391	468803.981840	47.948250
3504.791451	468792.797888	47.953255
3504.537562	468792.790614	47.958260
3504.881560	468781.233301	47.963265
3504.434062	468796.050246	47.968269
3504.613600	468780.620606	47.973274
3504.576042	468764.012306	47.978279
3504.533450	468752.419674	47.983284
3504.859322	468744.816505	47.988289
3504.369374	468751.789239	47.993293
3504.480298	468741.386103	47.998298
3504.619235	468749.923069	48.003303
3504.736045	468742.355595	48.008308
3504.336518	468743.588902	48.013313
3504.764798	468751.265988	48.018317
3504.729314	468740.330647	48.023322
3504.770129	468738.196208	48.028327
3504.512425	468726.336360	48.033332
3504.601599	468718.520320	48.038337
3504.459354	468724.369946	48.043341
3504.523606	468726.233235	48.048346
3504.645961	468723.325050	48.053351
3504.178537	468704.662592	48.058356
3504.377980	468702.501065	48.063361
3504.379393	468720.230059	48.068365
3504.759900	468705.272592	48.073370
3504.818491	468693.510683	48.078375
3504.761021	468689.113548	48.083380
3504.750832	468679.034986	48.088385
3504.844277	468678.461858	48.093389
3505.098434	468669.807150	48.098394
3504.805816	468645.542739	48.103399
3504.644788	468639.035763	48.108404
3504.569095	468632.210284	48.113409
3504.379385	468634.876771	48.118413
3504.315839	468631.848348	48.123418
3504.363244	468640.299682	48.128423
3504.470613	468643.118064	48.133428
3504.276085	468629.575751	48.138433
3504.358983	468647.594830	48.143437
3504.208252	468640.832822	48.148442
3504.135911	468639.376208	48.153447
3504.319179	468642.130976	48.158452
3504.568197	468639.302462	48.163457
3503.940752	468644.981680	48.168461
3504.080471	468637.967459	48.173466
3504.188229	468639.215468	48.178471
3504.159121	468644.741870	48.183476
3504.579053	468644.822166	48.188481
3504.355646	468645.974754	48.193485
3503.927860	468645.946516	48.198490
3504.453408	468647.629741	48.203495
3504.113761	468643.686016	48.208500
3504.543465	468639.408309	48.213505
3504.368290	468652.051356	48.218509
3504.291136	468642.541414	48.223514
3504.611476	468648.869285	48.228519
3504.406296	468648.853695	48.233524
3504.698226	468639.128767	48.238529
3504.446477	468620.530712	48.243533
3504.524194	468609.829242	48.248538
3504.789466	468602.945536	48.253543
3504.763961	468598.441613	48.258548
3504.742868	468602.598969	48.263553
3504.809179	468606.893366	48.268557
3504.743767	468590.694913	48.273562
3504.866020	468579.124684	48.278567
3504.727871	468572.563123	48.283572
3504.559805	468561.700972	48.288577
3504.870789	468569.144883	48.293581
3504.577401	468561.394099	48.298586
3504.591025	468550.500918	48.303591
3504.514004	468540.788281	48.308596
3505.079958	468526.964083	48.313601
3504.858962	468523.810560	48.318605
3505.031918	468517.702416	48.323610
3505.085606	468501.939450	48.328615
3504.520886	468488.004345	48.333620
3504.680414	468475.465235	48.338625
3504.536973	468484.759711	48.343629
3504.625884	468482.566377	48.348634
3504.513738	468483.953254	48.353639
3504.510055	468490.792402	48.358644
3505.108494	468472.808871	48.363649
3505.005360	468457.275266	48.368653
3504.952868	468443.050047	48.373658
3505.094520	468440.290491	48.378663
3505.164612	468429.387600	48.383668
3505.170705	468407.047450	48.388673
3505.284522	468410.219356	48.393677
3505.000817	468375.062105	48.398682
3504.741438	468366.393631	48.403687
3505.025930	468367.611482	48.408692
3505.222101	468348.531435	48.413697
3504.801200	468326.314753	48.418701
3504.717978	468322.732425	48.423706
3505.149002	468316.782777	48.428711
3505.141191	468302.448512	48.433716
3504.675316	468282.417663	48.438721
3504.791813	468271.405447	48.443725
3504.636178	468267.176944	48.448730
3504.741432	468268.628030	48.453735
3504.782061	468264.163392	48.458740
3504.926446	468243.876337	48.463745
3504.572451	468244.038122	48.468749
3504.783072	468241.266762	48.473754
3504.535128	468236.496796	48.478759
3504.118420	468244.824925	48.483764
3504.107029	468239.508009	48.488769
3504.609031	468241.600541	48.493773
3504.496501	468231.488560	48.498778
3504.484554	468239.747581	48.503783
3504.073043	468231.712893	48.508788
3504.167903	468227.036362	48.513793
3504.531616	468232.951718	48.518797
3504.458526	468216.956882	48.523802
3504.293997	468199.103365	48.528807
3504.227331	468199.823966	48.533812
3504.207662	468207.375133	48.538817
3504.282726	468226.814322	48.543821
3504.388235	468215.145419	48.548826
3504.528852	468204.483638	48.553831
3504.643421	468194.434175	48.558836
3504.674083	468187.438408	48.563841
3504.335965	468197.830045	48.568845
3504.513866	468193.696546	48.573850
3504.515850	468198.153988	48.578855
3504.547541	468193.842828	48.583860
3504.592396	468198.647543	48.588865
3504.564625	468199.209535	48.593869
3504.540067	468188.373323	48.598874
3504.513479	468169.837695	48.603879
3504.523350	468162.997438	48.608884
3504.667506	468157.096722	48.613889
3504.645584	468158.265592	48.618893
3504.249169	468160.663500	48.623898
3504.608946	468161.767198	48.628903
3504.292398	468157.110238	48.633908
3504.604758	468152.345896	48.638913
3504.519223	468159.452420	48.643917
3504.504238	468159.252385	48.648922
3504.581142	468151.742147	48.653927
3504.409776	468138.043560	48.658932
3504.760280	468125.117018	48.663937
3504.454110	468120.407621	48.668941
3504.186761	468114.019931	48.673946
3504.576727	468115.422416	48.678951
3504.388790	468118.341954	48.683956
3504.293476	468106.960556	48.688961
3504.697452	468120.112947	48.693965
3504.866320	468115.626379	48.698970
3504.803674	468111.888529	48.703975
3504.480600	468106.016916	48.708980
3504.533285	468088.835398	48.713985
3504.552045	468081.588342	48.718989
3504.454655	468082.820759	48.723994
3504.541570	468081.691507	48.728999
3504.475225	468090.415790	48.734004
3504.417494	468082.168664	48.739009
3504.366823	468092.612591	48.744013
3504.500976	468090.766083	48.749018
3504.501847	468080.584003	48.754023
3504.145610	468093.612930	48.759028
3504.361091	468087.396075	48.764033
3504.388566	468090.126867	48.769037
3504.325296	468088.314067	48.774042
3504.609341	468089.228074	48.779047
3504.610847	468078.083410	48.784052
3504.246732	468061.580912	48.789057
3504.166788	468055.971710	48.794061
3504.586412	468042.476088	48.799066
3505.054946	468041.079048	48.804071
3504.346164	468040.693532	48.809076
3504.651092	468039.679023	48.814081
3504.752635	468049.691731	48.819085
3504.228390	468050.186527	48.824090
3504.645206	468043.884624	48.829095
3504.589038	468046.984301	48.834100
3504.643982	468023.115662	48.839105
3504.484753	468015.189777	48.844109
3504.467004	468011.342928	48.849114
3504.785447	468003.892704	48.854119
3504.563743	468011.934354	48.859124
3504.698015	468009.581250	48.864129
3504.423929	468007.196557	48.869133
3504.233841	468009.457941	48.874138
3504.766231	467999.792945	48.879143
3504.516028	467995.833813	48.884148
3504.558118	467969.890374	48.889153
3504.403843	467965.560258	48.894157
3504.329344	467964.762500	48.899162
3504.645179	467964.202037	48.904167
3504.204998	467972.179694	48.909172
3504.815602	467960.576365	48.914177
3504.624235	467963.141913	48.919181
3504.684972	467968.045289	48.924186
3504.913905	467960.711645	48.929191
3504.467180	467946.604025	48.934196
3504.656755	467930.006874	48.939201
3504.406278	467930.708213	48.944205
3504.874899	467925.258594	48.949210
3504.739441	467917.885837	48.954215
3504.668959	467922.102431	48.959220
3504.662666	467918.202951	48.964225
3504.902912	467900.583983	48.969229
3504.623630	467881.584651	48.974234
3505.042023	467881.057331	48.979239
3504.288412	467886.555685	48.984244
3504.652904	467880.515948	48.989249
3504.543415	467884.080669	48.994253
3504.660028	467876.158286	48.999258
3504.855803	467847.554272	49.004263
3504.560220	467841.171311	49.009268
3504.567365	467841.727352	49.014273
3504.817508	467836.213697	49.019277
3504.602571	467843.798348	49.024282
3504.756374	467838.301143	49.029287
3504.610626	467823.990071	49.034292
3504.746857	467802.994739	49.039297
3504.501883	467800.908992	49.044301
3504.255850	467801.406947	49.049306
3504.738610	467790.534546	49.054311
3504.535482	467794.267244	49.059316
3504.763230	467797.217170	49.064321
3505.097423	467798.882489	49.069325
3505.048193	467779.387858	49.074330
3505.005467	467765.059152	49.079335
3505.094037	467764.689459	49.084340
3504.923161	467752.206289	49.089345
3504.725552	467732.230371	49.094349
3504.563997	467722.278463	49.099354
3504.049834	467719.580121	49.104359
3503.944752	467723.650694	49.109364
3504.111642	467719.873576	49.114369
3504.124907	467717.034522	49.119373
3504.076538	467712.888896	49.124378
3504.255030	467718.633408	49.129383
3503.888838	467715.403226	49.134388
3504.667587	467715.472922	49.139393
3504.735723	467725.491505	49.144397
3504.878928	467723.643415	49.149402
3505.047465	467716.066703	49.154407
3504.518909	467722.438511	49.159412
3504.603813	467713.255038	49.164417
3504.645834	467699.823647	49.169421
3504.458887	467679.693881	49.174426
3504.543937	467680.084652	49.179431
3504.223269	467682.976261	49.184436
3504.602999	467673.438483	49.189441
3504.320539	467674.601210	49.194445
3504.610058	467680.934668	49.199450
3504.822862	467667.018176	49.204455
3505.048065	467674.477085	49.209460
3505.123637	467652.985370	49.214465
3505.137978	467641.331683	49.219469
3504.602196	467629.265341	49.224474
3504.706198	467632.287080	49.229479
3504.314312	467625.211281	49.234484
3504.944951	467597.292510	49.239489
3504.987308	467598.045176	49.244493
3504.647015	467597.039496	49.249498
3504.708112	467596.826464	49.254503
3504.673085	467605.444305	49.259508
3504.662230	467583.967269	49.264513
3504.317450	467561.027486	49.269517
3504.483883	467553.045805	49.274522
3504.712741	467547.130439	49.279527
3504.511096	467555.472803	49.284532
3504.438246	467547.278686	49.289537
3504.463238	467549.199452	49.294541
3504.416970	467551.993571	49.299546
3504.687563	467554.024376	49.304551
3504.468460	467559.431559	49.309556
3504.660831	467552.965187	49.314561
3504.655606	467535.691744	49.319565
3504.527903	467520.161571	49.324570
3504.600457	467519.895924	49.329575
3503.968357	467522.182177	49.334580
3504.391957	467512.130249	49.339585
3504.414936	467524.284285	49.344589
3504.063615	467518.113365	49.349594
3504.348676	467511.935101	49.354599
3503.957004	467514.332278	49.359604
3504.577289	467517.772463	49.364609
3504.431650	467516.682884	49.369613
3504.193596	467513.582763	49.374618
3504.489401	467510.391489	49.379623
3504.407516	467528.946341	49.384628
3504.068728	467516.846293	49.389633
3504.161043	467519.616754	49.394637
3504.324470	467518.474405	49.399642
3504.672588	467514.058406	49.404647
3504.604188	467522.631324	49.409652
3504.508053	467512.820111	49.414657
3504.579584	467514.428987	49.419661
3504.600809	467514.222762	49.424666
3504.704690	467505.998451	49.429671
3504.183038	467493.423030	49.434676
3504.481034	467474.831307	49.439681
3504.458916	467481.521990	49.444685
3504.465079	467473.770273	49.449690
3504.644835	467478.906744	49.454695
3504.475919	467477.821137	49.459700
3504.193819	467473.867341	49.464705
3504.367484	467474.192328	49.469709
3504.343789	467466.293732	49.474714
3504.819147	467468.593534	49.479719
3504.438099	467480.360659	49.484724
3504.572995	467476.082374	49.489729
3504.872309	467477.044463	49.494733
3504.200549	467464.646627	49.499738
3504.758360	467451.076337	49.504743
3504.805941	467451.422851	49.509748
3504.768149	467453.455664	49.514753
3504.740099	467450.522309	49.519757
3504.434510	467451.790314	49.524762
3504.790418	467447.980869	49.529767
3504.756743	467424.835829	49.534772
3504.867993	467406.427901	49.539777
3504.961716	467403.473746	49.544781
3504.530976	467404.003248	49.549786
3504.770142	467398.795293	49.554791
3504.633481	467390.308053	49.559796
3504.742370	467366.986627	49.564801
3504.820065	467354.359438	49.569805
3504.808817	467368.089830	49.574810
3505.174184	467353.539161	49.579815
3504.800259	467327.412590	49.584820
3504.485941	467321.336605	49.589825
3504.665860	467321.001965	49.594829
3504.411038	467318.816529	49.599834
3504.660936	467309.756666	49.604839
3504.506164	467317.280593	49.609844
3504.633631	467307.279120	49.614849
3504.595809	467311.642248	49.619853
3504.329077	467295.831679	49.624858
3504.694496	467280.875677	49.629863
3504.499439	467282.175480	49.634868
3504.807477	467276.449145	49.639873
3505.034958	467282.742670	49.644877
3504.754094	467276.914251	49.649882
3504.698887	467262.232688	49.654887
3504.456655	467253.054191	49.659892
3504.733177	467241.203519	49.664897
3504.293482	467239.302933	49.669901
3504.063309	467237.974478	49.674906
3504.241722	467231.105111	49.679911
3504.167418	467243.073301	49.684916
3504.534112	467240.224490	49.689921
3504.503997	467242.053379	49.694925
3504.422983	467238.065200	49.699930
3504.481211	467237.953972	49.704935
3504.223127	467238.099387	49.709940
3504.524922	467233.995187	49.714945
3504.557179	467232.419288	49.719949
3504.274931	467237.178779	49.724954
3504.626345	467230.381190	49.729959
3504.487821	467238.105009	49.734964
3504.300047	467232.615294	49.739969
3504.389631	467210.462126	49.744973
3504.375981	467208.894063	49.749978
3504.443955	467197.281608	49.754983
3504.323204	467204.850429	49.759988
3504.453516	467189.883840	49.764993
3504.802219	467196.663284	49.769997
3504.547782	467200.100904	49.775002
3504.502594	467199.298108	49.780007
3504.519951	467214.746128	49.785012
3504.866412	467201.414384	49.790017
3504.494188	467200.464792	49.795021
3504.551459	467184.497493	49.800026
3504.679386	467166.289122	49.805031
3504.194795	467164.497512	49.810036
3504.182107	467156.900863	49.815041
3504.235259	467154.358869	49.820045
3504.091688	467163.198078	49.825050
3504.169071	467155.940662	49.830055
3504.075516	467159.198842	49.835060
3504.345109	467162.091064	49.840065
3504.415065	467163.801556	49.845069
3504.172722	467162.627150	49.850074
3504.774511	467152.949882	49.855079
3504.334164	467167.057638	49.860084
3504.440621	467160.808439	49.865089
3504.810861	467152.589157	49.870093
3504.440493	467166.786283	49.875098
3504.775070	467158.725069	49.880103
3504.721693	467163.800113	49.885108
3504.772046	467157.661810	49.890113
3504.534665	467131.663635	49.895117
3504.549583	467132.522323	49.900122
3504.707146	467121.654411	49.905127
3504.386843	467127.585585	49.910132
3504.449716	467126.966972	49.915137
3504.692527	467122.112933	49.920141
3504.879648	467126.539014	49.925146
3504.900970	467105.613197	49.930151
3504.734017	467097.637591	49.935156
3504.642236	467079.922584	49.940161
3504.440662	467081.628786	49.945165
3504.369016	467074.548763	49.950170
3504.658244	467079.362694	49.955175
3504.499645	467074.729159	49.960180
3504.779831	467068.754222	49.965185
3504.873456	467056.478732	49.970189
3504.296882	467037.326683	49.975194
3504.328860	467029.317082	49.980199
3504.515654	467038.809171	49.985204
3504.537714	467034.398076	49.990209
3504.391678	467036.196118	49.995213
3504.339204	467036.964999	50.000218
3504.584167	467035.707381	50.005223
3504.317102	467038.032681	50.010228
3504.752747	467035.526683	50.015233
3505.124845	467035.919115	50.020237
3504.524399	467016.365846	50.025242
3504.667930	467000.636962	50.030247
3504.643481	467000.083915	50.035252
3505.236356	466992.485124	50.040257
3505.032191	466988.973855	50.045261
3504.978696	466970.390999	50.050266
3504.874590	466951.107533	50.055271
3504.549311	466963.270728	50.060276
3504.704355	466964.054839	50.065281
3504.659605	466956.058309	50.070285
3504.751446	466936.690712	50.075290
3504.794370	466918.952557	50.080295
3504.859937	466919.802607	50.085300
3504.716298	466916.990225	50.090305
3504.821040	466921.177121	50.095309
3504.407786	466898.805490	50.100314
3504.747215	466879.800840	50.105319
3504.323794	466882.304834	50.110324
3504.315100	466868.982841	50.115329
3504.205834	466865.354026	50.120333
3504.388473	466870.692807	50.125338
3504.280221	466863.568296	50.130343
3504.520286	466869.403870	50.135348
3504.485819	466866.724820	50.140353
3504.505487	466869.203821	50.145357
3504.538989	466873.250912	50.150362
3504.324750	466868.677486	50.155367
3504.550933	466872.691678	50.160372
3504.289476	466871.419198	50.165377
3504.916085	466876.378215	50.170381
3504.500721	466863.733570	50.175386
3504.513657	466839.516010	50.180391
3504.464579	466843.627867	50.185396
3504.845735	466828.010249	50.190401
3504.721557	466828.690061	50.195405
3504.623123	466826.933804	50.200410
3504.984210	466824.744468	50.205415
3504.538343	466814.891292	50.210420
3504.258488	466809.822456	50.215425
3504.349411	466794.457006	50.220429
3504.636257	466798.308876	50.225434
3504.747604	466795.098319	50.230439
3504.542032	466797.311828	50.235444
3504.693218	466797.083406	50.240449
3504.607947	466798.567135	50.245453
3504.352632	466798.762740	50.250458
3504.662400	466785.842252	50.255463
3504.476456	466794.232926	50.260468
3504.502973	466766.416098	50.265473
3504.583232	466754.801278	50.270477
3504.515474	466761.094724	50.275482
3504.849279	466757.795518	50.280487
3504.654337	466759.247315	50.285492
3504.648929	466757.272529	50.290497
3504.992960	466751.539894	50.295501
3504.816385	466741.488719	50.300506
3504.896383	466717.208895	50.305511
3504.779073	466723.156193	50.310516
3504.565392	466722.635447	50.315521
3504.935248	466714.669346	50.320525
3504.734478	466696.871273	50.325530
3504.522564	466670.817465	50.330535
3504.693651	466681.578920	50.335540
3504.648414	466668.769629	50.340545
3504.774892	466660.591758	50.345549
3504.470617	466676.196448	50.350554
3504.764210	466665.254392	50.355559
3504.615628	466648.055288	50.360564
3504.527286	466638.191635	50.365569
3504.533947	466630.338172	50.370573
3504.515942	466636.673824	50.375578
3504.475180	466633.083930	50.380583
3504.140195	466631.874648	50.385588
3504.246151	466635.200173	50.390593
3504.065480	466637.561429	50.395597
3504.325004	466632.197810	50.400602
3504.094238	466630.464130	50.405607
3504.279147	466630.077967	50.410612
3504.361695	466621.198336	50.415617
3504.135388	466631.318425	50.420621
3503.837341	466633.243780	50.425626
3504.210221	466626.898257	50.430631
3503.857048	466637.901232	50.435636
3503.961771	466651.257713	50.440641
3504.145287	466668.653554	50.445645
3503.928290	466683.280791	50.450650
3504.182924	466669.001813	50.455655
3504.355808	466675.406180	50.460660
3503.808884	466676.310159	50.465665
3504.529315	466677.555009	50.470669
3504.242716	466680.744911	50.475674
3504.514133	466677.608324	50.480679
3504.538832	466681.606298	50.485684
3504.561240	466668.177534	50.490689
3504.703599	466678.386633	50.495693
3504.412320	466667.443120	50.500698
3504.773208	466647.269390	50.505703
3504.562570	466642.138032	50.510708
3504.287193	466633.876783	50.515713
3504.729232	466635.067849	50.520717
3504.556914	466634.894661	50.525722
3504.761810	466626.754047	50.530727
3504.182856	466606.639425	50.535732
3504.380966	466584.618986	50.540737
3504.588834	466560.874397	50.545741
3504.316927	466512.742599	50.550746
3504.220269	466454.093966	50.555751
3504.096924	466394.740456	50.560756
3503.975402	466323.481077	50.565761
3503.995670	466250.930690	50.570765
3503.627123	466173.886875	50.575770
3503.752001	466075.075247	50.580775
3503.667463	465969.003524	50.585780
3502.966013	465854.018643	50.590785
3503.349646	465723.952958	50.595789
3502.581230	465601.378587	50.600794
3502.507820	465462.776454	50.605799
3501.929693	465323.550211	50.610804
3501.520278	465180.443679	50.615809
3501.453161	465016.961144	50.620813
3501.001028	464879.483452	50.625818
3501.275217	464701.044468	50.630823
3501.194318	464533.304309	50.635828
3500.934039	464348.062777	50.640833
3500.457069	464153.533775	50.645837
3499.511833	463960.957473	50.650842
3499.218693	463757.272992	50.655847
3499.102647	463561.815096	50.660852
3498.373957	463356.883420	50.665857
3498.094406	463140.776286	50.670861
3497.568315	462926.330300	50.675866
3497.285324	462715.438069	50.680871
3496.742429	462495.112437	50.685876
3496.185624	462264.196308	50.690881
3495.745326	462037.311358	50.695885
3495.418845	461812.329926	50.700890
3495.010932	461565.114141	50.705895
3494.252444	461319.171294	50.710900
3493.696582	461077.700841	50.715905
3493.703337	460836.587449	50.720909
3492.724055	460589.558352	50.725914
3492.289634	460334.527571	50.730919
3491.694577	460079.977032	50.735924
3491.457070	459825.007431	50.740929
3490.808495	459550.340056	50.745933
3490.493608	459290.511657	50.750938
3489.947607	459024.333646	50.755943
3489.317010	458748.233101	50.760948
3488.514677	458469.522626	50.765953
3488.219565	458198.678762	50.770957
3487.417463	457922.241325	50.775962
3487.087490	457633.048572	50.780967
3486.371175	457352.990114	50.785972
3486.059035	457074.328611	50.790977
3485.650918	456790.256272	50.795981
3484.759276	456495.415600	50.800986
3484.226251	456202.435505	50.805991
3483.444827	455910.051149	50.810996
3482.958062	455622.731814	50.816001
3482.457895	455318.176317	50.821005
3481.489817	455037.976719	50.826010
3481.066295	454736.136687	50.831015
3480.336513	454439.971246	50.836020
3479.727285	454140.384542	50.841025
3479.061298	453836.697002	50.846029
3478.261112	453542.102067	50.851034
3477.771859	453243.242164	50.856039
3476.936450	452942.611990	50.861044
3476.355635	452642.440914	50.866049
3475.928956	452338.234105	50.871053
3475.096182	452049.301400	50.876058
3474.751529	451729.203307	50.881063
3474.540627	451425.503911	50.886068
3473.455831	451116.575115	50.891073
3473.079248	450807.977102	50.896077
3472.379247	450499.733946	50.901082
3471.899120	450178.925291	50.906087
3471.108878	449863.133535	50.911092
3470.132573	449544.275863	50.916097
3469.181445	449229.718907	50.921101
3468.665184	448923.854959	50.926106
3468.113710	448617.485516	50.931111
3467.604489	448306.185866	50.936116
3466.948101	447990.343094	50.941121
3466.575876	447685.298601	50.946125
3465.338228	447361.280269	50.951130
3464.622723	447045.585616	50.956135
3464.209161	446743.120812	50.961140
3463.169557	446432.441997	50.966145
3462.850949	446116.361513	50.971149
3462.173441	445806.118860	50.976154
3461.706830	445493.300030	50.981159
3460.840747	445178.921993	50.986164
3459.623295	444875.959444	50.991169
3459.214944	444555.509778	50.996173
3458.517527	444248.696646	51.001178
3457.816154	443937.112431	51.006183
3457.038269	443630.152091	51.011188
3456.476808	443323.657623	51.016193
3456.035662	443012.117085	51.021197
3454.893783	442714.183197	51.026202
3454.474717	442398.572504	51.031207
3453.804031	442079.043944	51.036212
3453.077136	441777.120834	51.041217
3452.514285	441463.296430	51.046221
3451.744576	441161.625745	51.051226
3451.141319	440847.342907	51.056231
3450.094035	440539.319821	51.061236
3449.453561	440238.679611	51.066241
3449.046647	439934.393855	51.071245
3448.065307	439637.455940	51.076250
3447.567932	439320.749083	51.081255
3446.864919	439013.051730	51.086260
3446.438841	438715.296440	51.091265
3445.609746	438404.111875	51.096269
3444.822874	438097.177106	51.101274
3444.516029	437790.460531	51.106279
3443.567732	437482.022933	51.111284
3442.858798	437173.540209	51.116289
3442.333100	436856.701701	51.121293
3441.459125	436557.421402	51.126298
3440.582069	436246.823830	51.131303
3440.077976	435948.182556	51.136308
3439.216459	435643.104160	51.141313
3438.867170	435337.731234	51.146317
3438.501712	435037.278476	51.151322
3437.461766	434723.186911	51.156327
3436.909135	434421.083606	51.161332
3435.810097	434116.583367	51.166337
3435.470239	433805.099518	51.171341
3434.587450	433513.695984	51.176346
3434.028824	433202.748695	51.181351
3433.608425	432891.570617	51.186356
3432.750855	432591.677127	51.191361
3432.341591	432277.342785	51.196365
3431.448564	431983.536643	51.201370
3430.569434	431665.417646	51.206375
3429.875277	431371.214547	51.211380
3429.195354	431065.891887	51.216385
3428.845767	430754.825165	51.221389
3428.103597	430457.015657	51.226394
3427.193784	430148.218632	51.231399
3426.458957	429845.173000	51.236404
3425.687650	429539.642948	51.241409
3425.429976	429237.167707	51.246413
3424.450921	428931.817458	51.251418
3424.233936	428624.810569	51.256423
3423.493762	428332.505608	51.261428
3422.443465	428021.877511	51.266433
3421.899604	427704.966941	51.271437
3420.981048	427411.767491	51.276442
3420.348931	427106.537406	51.281447
3419.763544	426810.786663	51.286452
3418.842646	426507.780684	51.291457
3418.236320	426210.807926	51.296461
3417.459107	425917.565933	51.301466
3417.347682	425624.257413	51.306471
3416.268121	425326.390092	51.311476
3415.584140	425031.903143	51.316481
3414.924883	424719.540952	51.321485
3413.786650	424427.712928	51.326490
3413.194440	424136.803353	51.331495
3412.766670	423833.983995	51.336500
3412.244914	423548.588335	51.341505
3411.874443	423241.843113	51.346509
3410.627135	422946.614766	51.351514
3410.228918	422649.613398	51.356519
3409.527684	422351.949455	51.361524
3408.783010	422052.563288	51.366529
3408.167773	421760.360116	51.371533
3407.507683	421464.658237	51.376538
3406.760384	421162.088749	51.381543
3406.099225	420871.608940	51.386548
3405.173248	420576.119485	51.391553
3404.647640	420277.359685	51.396557
3404.204190	419988.888471	51.401562
3403.508562	419691.267572	51.406567
3402.867489	419399.421659	51.411572
3401.792404	419101.477722	51.416577
3401.186356	418806.826466	51.421581
3400.633955	418528.460556	51.426586
3399.944717	418233.588279	51.431591
3399.103056	417937.342287	51.436596
3398.342862	417641.662795	51.441601
3397.975842	417349.670034	51.446605
3396.874963	417061.175779	51.451610
3396.167066	416779.922873	51.456615
3395.567811	416482.526714	51.461620
3394.776305	416197.778036	51.466625
3394.174195	415907.002048	51.471629
3393.601662	415625.256234	51.476634
3393.128072	415343.363464	51.481639
3392.083743	415056.690219	51.486644
3391.388351	414774.803669	51.491649
3390.795639	414489.392624	51.496653
3390.266089	414205.516449	51.501658
3389.551187	413914.051537	51.506663
3388.945576	413640.693942	51.511668
3388.230640	413340.157919	51.516673
3387.772280	413056.104596	51.521677
3386.832119	412781.652431	51.526682
3385.972462	412491.922875	51.531687
3385.448765	412209.979015	51.536692
3384.827138	411923.071840	51.541697
3384.306614	411634.696842	51.546701
3383.084233	411354.285071	51.551706
3382.763373	411065.844321	51.556711
3382.178050	410784.962166	51.561716
3381.435200	410501.005823	51.566721
3381.062696	410210.888508	51.571725
3380.248880	409928.106265	51.576730
3379.432834	409630.439902	51.581735
3378.864065	409354.517134	51.586740
3377.887872	409083.206878	51.591745
3377.344650	408797.623660	51.596749
3377.000571	408515.355660	51.601754
3376.138017	408227.179677	51.606759
3375.312220	407948.568843	51.611764
3374.829681	407671.217133	51.616769
3374.361733	407379.917032	51.621773
3373.406926	407095.503431	51.626778
3373.040699	406820.713634	51.631783
3372.403921	406531.414219	51.636788
3371.412255	406243.493025	51.641793
3370.860953	405961.716203	51.646797
3369.937483	405682.057315	51.651802
3369.371847	405389.711133	51.656807
3368.922993	405106.053834	51.661812
3368.063476	404822.819314	51.666817
3367.485730	404530.567611	51.671821
3366.963366	404258.801205	51.676826
3366.424970	403964.352352	51.681831
3365.540584	403682.939150	51.686836
3364.686654	403394.862850	51.691841
3364.381787	403107.401016	51.696845
3363.546902	402827.342314	51.701850
3362.551668	402539.382856	51.706855
3362.174365	402251.746723	51.711860
3361.216436	401971.217778	51.716865
3361.018422	401682.046429	51.721869
3360.322699	401406.471318	51.726874
3359.152785	401120.940319	51.731879
3358.680918	400840.571073	51.736884
3357.734144	400563.404761	51.741889
3357.576398	400271.951120	51.746893
3356.523934	399996.397723	51.751898
3355.976027	399709.907885	51.756903
3355.574258	399440.131735	51.761908
3354.560184	399159.279526	51.766913
3354.000782	398870.649200	51.771917
3353.272109	398604.934952	51.776922
3352.592900	398312.559479	51.781927
3351.479887	398032.576875	51.786932
3350.918749	397764.539710	51.791937
3350.552039	397484.729190	51.796941
3349.718809	397212.084019	51.801946
3349.262339	396932.258066	51.806951
3348.460079	396659.348327	51.811956
3347.580619	396377.505886	51.816961
3347.246637	396099.988444	51.821965
3346.361818	395822.689466	51.826970
3345.605187	395544.603724	51.831975
3345.224711	395267.086302	51.836980
3344.119807	394991.544777	51.841985
3343.997255	394718.246720	51.846989
3343.429550	394445.860637	51.851994
3342.562322	394164.782468	51.856999
3341.740619	393888.775712	51.862004
3341.014180	393609.345233	51.867009
3340.476001	393323.883258	51.872013
3339.995286	393055.408041	51.877018
3339.040142	392775.144833	51.882023
3338.823474	392494.422541	51.887028
3337.517049	392221.938924	51.892033
3337.567007	391942.995501	51.897037
3336.417649	391664.127248	51.902042
3335.981542	391389.734072	51.907047
3335.438005	391107.860303	51.912052
3334.386327	390823.224549	51.917057
3334.093464	390541.201042	51.922061
3333.180140	390271.351756	51.927066
3332.203793	389989.693976	51.932071
3332.034965	389705.659354	51.937076
3330.841888	389437.654770	51.942081
3330.357000	389160.886373	51.947085
3329.569960	388893.468430	51.952090
3329.186678	388608.875752	51.957095
3328.219966	388332.233004	51.962100
3327.699884	388063.796531	51.967105
3327.192696	387788.874847	51.972109
3326.799841	387519.776569	51.977114
3326.076310	387240.312332	51.982119
3325.828606	386960.027286	51.987124
3324.796371	386681.271547	51.992129
3324.122440	386395.488265	51.997133
3323.584275	386115.016506	52.002138
3322.607273	385830.220214	52.007143
3322.095848	385555.228752	52.012148
3321.368687	385280.652983	52.017153
3321.020947	384985.956257	52.022157
3320.170540	384711.904932	52.027162
3319.437104	384423.699329	52.032167
3318.251247	384133.509572	52.037172
3317.201555	383869.550304	52.042177
3316.915859	383589.140143	52.047181
3316.302899	383319.967353	52.052186
3315.475464	383053.879124	52.057191
3315.188284	382781.595996	52.062196
3314.542475	382509.702259	52.067201
3313.961255	382223.763975	52.072205
3313.276999	381954.693634	52.077210
3312.238474	381670.938356	52.082215
3311.891725	381395.984719	52.087220
3310.995200	381127.655531	52.092225
3310.543997	380848.241240	52.097229
3309.354797	380580.516784	52.102234
3308.923928	380300.306322	52.107239
3308.373496	380023.850721	52.112244
3307.440274	379759.634746	52.117249
3306.748805	379487.850747	52.122253
3305.902679	379223.107188	52.127258
3305.279902	378960.738406	52.132263
3304.820199	378684.129011	52.137268
3304.000970	378420.391330	52.142273
3303.880766	378136.804675	52.147277
3303.024296	377870.806455	52.152282
3302.418696	377593.196060	52.157287
3302.090748	377327.306651	52.162292
3301.050960	377055.053884	52.167297
3300.574469	376773.906333	52.172301
3299.872752	376506.294678	52.177306
3299.092439	376218.533507	52.182311
3298.725428	375940.106088	52.187316
3297.497403	375675.603201	52.192321
3297.106448	375396.616111	52.197325
3296.495927	375120.638892	52.202330
3295.711836	374843.850089	52.207335
3295.056510	374576.749310	52.212340
3294.027139	374296.947035	52.217345
3293.343893	374026.185575	52.222349
3292.844689	373757.653421	52.227354
3291.898626	373484.364660	52.232359
3291.468946	373212.561955	52.237364
3290.485288	372955.166533	52.242369
3290.206157	372683.842521	52.247373
3288.960850	372416.291953	52.252378
3288.619100	372151.814195	52.257383
3288.306668	371889.872111	52.262388
3287.431686	371625.990011	52.267393
3286.480348	371346.405060	52.272397
3285.605777	371090.070733	52.277402
3285.373818	370819.029458	52.282407
3284.626830	370557.533161	52.287412
3283.708872	370302.395673	52.292417
3283.401382	370027.445407	52.297421
3282.407523	369769.291154	52.302426
3281.836681	369514.165060	52.307431
3281.766336	369250.305975	52.312436
3280.835556	368980.717877	52.317441
3280.344326	368714.205888	52.322445
3279.092698	368443.651435	52.327450
3278.725309	368176.987211	52.332455
3278.387362	367920.818387	52.337460
3277.651496	367652.967224	52.342465
3277.096877	367381.446678	52.347469
3276.277998	367111.901942	52.352474
3275.304827	366836.176608	52.357479
3274.828222	366565.145325	52.362484
3274.269036	366304.476417	52.367489
3273.779977	366036.673082	52.372493
3272.922110	365774.067863	52.377498
3272.047307	365499.638204	52.382503
3271.669101	365221.688484	52.387508
3270.801202	364953.764064	52.392513
3270.361188	364694.157114	52.397517
3269.266325	364435.626628	52.402522
3268.586170	364163.646285	52.407527
3268.166423	363886.711090	52.412532
3267.294355	363630.680275	52.417537
3266.910219	363357.829761	52.422541
3265.931473	363100.109615	52.427546
3265.253056	362837.911106	52.432551
3264.612586	362568.430451	52.437556
3264.111456	362303.654700	52.442561
3263.734893	362038.906721	52.447565
3262.899377	361774.159012	52.452570
3262.384505	361503.810157	52.457575
3261.246148	361234.990208	52.462580
3260.812389	360972.482905	52.467585
3260.658800	360703.745441	52.472589
3259.885602	360440.453204	52.477594
3259.289704	360166.726131	52.482599
3258.603372	359888.866716	52.487604
3257.736173	359618.056304	52.492609
3256.892824	359344.696441	52.497613
3256.294974	359076.557888	52.502618
3255.485000	358802.196607	52.507623
3255.136044	358523.049085	52.512628
3254.624205	358266.412778	52.517633
3253.977624	357987.693892	52.522637
3253.166063	357718.692463	52.527642
3252.276953	357448.863079	52.532647
3251.865693	357171.878904	52.537652
3250.786381	356905.334262	52.542657
3250.156896	356627.798596	52.547661
3249.458649	356365.458734	52.552666
3248.712015	356095.596020	52.557671
3248.012316	355833.838050	52.562676
3247.300012	355577.168082	52.567681
3246.697721	355305.723827	52.572685
3246.254519	355047.503770	52.577690
3245.279184	354782.886279	52.582695
3244.461579	354512.694622	52.587700
3244.257607	354245.372697	52.592705
3243.477734	353983.540398	52.597709
3242.982200	353728.678983	52.602714
3241.886976	353461.249882	52.607719
3241.568427	353189.234593	52.612724
3240.399531	352927.182321	52.617729
3239.859670	352662.248095	52.622733
3239.239919	352409.816663	52.627738
3238.462887	352152.526179	52.632743
3238.188700	351893.825387	52.637748
3236.967197	351625.795716	52.642753
3236.406208	351357.040990	52.647757
3235.821513	351110.192726	52.652762
3235.380523	350848.359526	52.657767
3234.868005	350589.945997	52.662772
3234.075011	350326.567005	52.667777
3233.449986	350056.746621	52.672781
3233.300580	349788.929497	52.677786
3232.076619	349525.670156	52.682791
3231.906100	349252.688792	52.687796
3230.883236	348989.188355	52.692801
3230.248314	348721.676621	52.697805
3229.468211	348458.691271	52.702810
3228.671682	348195.503630	52.707815
3228.298012	347924.278819	52.712820
3226.850909	347670.307476	52.717825
3226.685070	347413.393509	52.722829
3225.976323	347155.425885	52.727834
3225.329930	346888.057768	52.732839
3224.966679	346638.220728	52.737844
3223.996029	346374.237969	52.742849
3223.473994	346103.918031	52.747853
3222.454278	345839.329909	52.752858
3221.980839	345581.109585	52.757863
3221.709330	345318.095363	52.762868
3220.766183	345063.972442	52.767873
3220.575703	344797.481055	52.772877
3219.767093	344538.014484	52.777882
3218.832444	344255.719116	52.782887
3217.990387	343980.785075	52.787892
3217.842327	343740.309920	52.792897
3217.037238	343461.193613	52.797901
3216.267972	343205.376929	52.802906
3215.498392	342936.353005	52.807911
3214.958517	342668.026220	52.812916
3213.997400	342397.530687	52.817921
3213.612397	342137.037007	52.822925
3212.808768	341869.437784	52.827930
3211.862103	341615.525786	52.832935
3211.586932	341348.978442	52.837940
3210.564649	341087.112044	52.842945
3210.293395	340811.375090	52.847949
3209.255368	340553.172714	52.852954
3208.637709	340298.128845	52.857959
3208.164386	340035.908538	52.862964
3207.110816	339790.198969	52.867969
3206.434397	339526.432933	52.872973
3205.962242	339266.040468	52.877978
3204.988258	339003.569350	52.882983
3204.258933	338752.684376	52.887988
3203.709779	338503.217851	52.892993
3203.892365	338241.842964	52.897997
3202.927189	337976.642047	52.903002
3202.252997	337724.037496	52.908007
3201.737709	337450.486475	52.913012
3200.401027	337177.735914	52.918017
3199.922615	336926.697144	52.923021
3199.523617	336661.087221	52.928026
3198.722386	336413.612902	52.933031
3197.780069	336156.033015	52.938036
3197.254859	335902.757736	52.943041
3196.723548	335632.660682	52.948045
3196.232593	335379.631466	52.953050
3195.499190	335118.218830	52.958055
3195.103196	334855.576590	52.963060
3193.723791	334592.744710	52.968065
3193.103753	334339.630683	52.973069
3192.588490	334083.698102	52.978074
3191.692543	333822.892085	52.983079
3191.232489	333561.526782	52.988084
3190.513147	333312.089535	52.993089
3189.763810	333056.293760	52.998093
3189.394972	332795.876208	53.003098
3188.824682	332549.209437	53.008103
3188.151390	332281.180887	53.013108
3187.151381	332029.825928	53.018113
3186.808787	331772.834742	53.023117
3186.134747	331516.382516	53.028122
3185.479817	331256.235454	53.033127
3185.017225	330995.494381	53.038132
3184.035788	330745.199251	53.043137
3183.883546	330476.131121	53.048141
3182.728486	330208.683692	53.053146
3181.795887	329953.006411	53.058151
3181.640336	329687.167338	53.063156
3180.705616	329436.018410	53.068161
3179.962131	329170.302754	53.073165
3179.371775	328919.728985	53.078170
3179.128918	328660.568340	53.083175
3178.563156	328396.523961	53.088180
3177.286986	328134.737683	53.093185
3176.859107	327866.416775	53.098189
3176.562082	327614.234550	53.103194
3175.217134	327355.027145	53.108199
3174.763053	327085.688961	53.113204
3174.414341	326834.606617	53.118209
3173.611444	326563.823876	53.123213
3172.804890	326313.250185	53.128218
3172.077207	326045.328379	53.133223
3172.039772	325787.417833	53.138228
3170.899032	325531.985417	53.143233
3169.719226	325262.610079	53.148237
3169.315859	324989.613755	53.153242
3168.658308	324748.069437	53.158247
3168.061688	324490.452403	53.163252
3167.355682	324235.831052	53.168257
3166.899146	323973.682539	53.173261
3166.215175	323723.153357	53.178266
3165.348122	323460.869114	53.183271
3164.717317	323196.099774	53.188276
3164.271916	322953.748425	53.193281
3163.328429	322682.997581	53.198285
3162.457587	322426.156830	53.203290
3162.150061	322174.309742	53.208295
3161.734348	321907.843573	53.213300
3160.608199	321657.636064	53.218305
3160.254999	321402.509974	53.223309
3159.233258	321147.089763	53.228314
3158.772717	320889.918066	53.233319
3158.478363	320617.316438	53.238324
3157.584403	320368.998771	53.243329
3156.876253	320112.502616	53.248333
3156.545025	319843.976882	53.253338
3155.725541	319589.534114	53.258343
3154.832814	319326.346032	53.263348
3154.061794	319070.161947	53.268353
3153.445767	318801.171425	53.273357
3152.957302	318551.810189	53.278362
3152.057912	318291.088328	53.283367
3151.571182	318035.360771	53.288372
3150.699724	317781.199878	53.293377
3149.908409	317519.641918	53.298381
3149.821175	317253.991424	53.303386
3148.898299	317005.920517	53.308391
3148.295920	316740.559648	53.313396
3147.484573	316488.852917	53.318401
3147.198055	316221.857736	53.323405
3146.781046	315959.720664	53.328410
3145.999534	315702.405365	53.333415
3145.369426	315425.002841	53.338420
3144.650548	315168.413119	53.343425
3143.802208	314899.166702	53.348429
3143.153433	314637.522456	53.353434
3142.366412	314380.279582	53.358439
3141.670976	314115.560979	53.363444
3140.843330	313848.216346	53.368449
3140.028452	313587.105746	53.373453
3139.635038	313343.335552	53.378458
3138.383742	313085.123523	53.383463
3138.143877	312827.781588	53.388468
3137.012133	312583.574866	53.393473
3136.538198	312317.513424	53.398477
3136.308064	312070.681502	53.403482
3135.498945	311819.619684	53.408487
3134.557632	311553.864442	53.413492
3133.767710	311308.423991	53.418497
3133.439752	311048.901419	53.423501
3132.957522	310802.923028	53.428506
3131.854858	310551.856163	53.433511
3131.105980	310284.968804	53.438516
3130.405706	310046.077386	53.443521
3130.382787	309797.038538	53.448525
3129.443173	309538.862783	53.453530
3128.423411	309292.360305	53.458535
3127.831047	309032.825105	53.463540
3127.305601	308784.607161	53.468545
3126.894778	308531.124140	53.473549
3126.076855	308282.903647	53.478554
3125.218999	308025.650927	53.483559
3125.104493	307769.950751	53.488564
3124.163006	307523.302047	53.493569
3123.891097	307256.424682	53.498573
3123.598286	306995.813223	53.503578
3122.037673	306745.423398	53.508583
3122.083378	306480.857030	53.513588
3120.697668	306228.017000	53.518593
3120.042358	305963.263184	53.523597
3119.468670	305703.994075	53.528602
3118.440988	305450.224842	53.533607
3117.836987	305198.623012	53.538612
3117.543071	304949.157094	53.543617
3116.992065	304698.206697	53.548621
3116.365169	304441.896246	53.553626
3115.387661	304184.448245	53.558631
3114.873235	303933.132892	53.563636
3114.056336	303675.655930	53.568641
3113.865291	303416.747303	53.573645
3112.953689	303171.837457	53.578650
3112.006847	302917.308511	53.583655
3111.020352	302648.934520	53.588660
3110.967742	302406.320117	53.593665
3109.682862	302143.851742	53.598669
3109.799580	301898.890020	53.603674
3108.797529	301644.341402	53.608679
3108.258042	301396.842383	53.613684
3107.011690	301141.824849	53.618689
3106.670736	300894.468787	53.623693
3106.327584	300643.929672	53.628698
3105.360135	300388.124004	53.633703
3105.333013	300129.865400	53.638708
3104.317446	299885.422738	53.643713
3103.804733	299625.234174	53.648717
3102.877665	299370.641031	53.653722
3101.972037	299112.071392	53.658727
3101.549066	298850.592256	53.663732
3100.547382	298604.208780	53.668737
3100.001638	298358.918076	53.673741
3099.317001	298103.592681	53.678746
3099.006988	297868.827538	53.683751
3098.350187	297611.229918	53.688756
3097.461075	297352.270851	53.693761
3096.898511	297101.709063	53.698765
3096.259888	296842.476722	53.703770
3095.549423	296595.376463	53.708775
3095.239823	296337.207007	53.713780
3094.325328	296085.149573	53.718785
3093.134871	295832.909496	53.723789
3092.956897	295578.204137	53.728794
3092.303589	295331.320258	53.733799
3091.480564	295071.452921	53.738804
3090.984161	294828.156886	53.743809
3089.919336	294572.047319	53.748813
3089.501209	294315.673885	53.753818
3088.696311	294071.843170	53.758823
3088.241049	293820.287563	53.763828
3087.446299	293571.514010	53.768833
3086.956474	293317.136663	53.773837
3086.065269	293062.114308	53.778842
3085.001441	292814.811010	53.783847
3084.890516	292561.283922	53.788852
3084.355692	292317.301359	53.793857
3083.416987	292072.241378	53.798861
3082.779882	291817.325599	53.803866
3081.991373	291571.194859	53.808871
3081.773165	291315.289701	53.813876
3081.042848	291070.548509	53.818881
3080.253554	290808.526481	53.823885
3080.166390	290553.692263	53.828890
3079.202699	290309.575060	53.833895
3078.736371	290047.165157	53.838900
3077.645464	289791.482216	53.843905
3077.086899	289536.140703	53.848909
3076.469660	289283.737142	53.853914
3075.632969	289026.328512	53.858919
3075.469040	288769.288260	53.863924
3074.621158	288520.869633	53.868929
3073.866040	288256.620887	53.873933
3073.342186	287997.068598	53.878938
3072.344826	287743.148081	53.883943
3071.707802	287480.380023	53.888948
3070.953827	287235.915463	53.893953
3070.239717	286975.502374	53.898957
3069.283040	286721.190968	53.903962
3068.864601	286473.382670	53.908967
3068.303074	286219.333869	53.913972
3067.459296	285973.558167	53.918977
3066.628300	285723.399775	53.923981
3066.220418	285469.705336	53.928986
3065.289830	285216.609050	53.933991
3064.637598	284970.264092	53.938996
3064.122800	284730.261657	53.944001
3063.212784	284483.297796	53.949005
3062.748896	284238.778417	53.954010
3062.185109	283999.267000	53.959015
3061.683902	283738.200382	53.964020
3061.186746	283494.118381	53.969025
3059.976124	283241.932369	53.974029
3059.548607	282994.094175	53.979034
3059.132816	282743.630577	53.984039
3058.438643	282485.345116	53.989044
3057.641573	282231.406050	53.994049
3057.063734	281988.965295	53.999053
3056.113398	281744.397717	54.004058
3055.379050	281494.750557	54.009063
3055.099986	281248.615981	54.014068
3054.428624	281000.892746	54.019073
3053.346868	280739.614757	54.024077
3052.835912	280497.771570	54.029082
3051.892291	280250.399341	54.034087
3051.358513	280007.005908	54.039092
3050.689385	279759.509685	54.044097
3050.139563	279519.760023	54.049101
3049.783583	279269.561097	54.054106
3048.726643	279032.596871	54.059111
3048.321295	278769.952519	54.064116
3047.630151	278526.049153	54.069121
3047.237922	278278.045194	54.074125
3046.584889	278021.172105	54.079130
3045.465708	277777.137156	54.084135
3045.065661	277522.919655	54.089140
3044.421834	277277.835129	54.094145
3043.863235	277021.963252	54.099149
3042.994358	276771.313835	54.104154
3042.251253	276533.095950	54.109159
3041.866928	276273.144108	54.114164
3040.990555	276028.989136	54.119169
3040.414462	275777.346209	54.124173
3039.907148	275532.185332	54.129178
3038.744267	275280.056322	54.134183
3038.692733	275029.774529	54.139188
3038.008937	274773.513819	54.144193
3037.755765	274518.987418	54.149197
3036.863203	274254.153880	54.154202
3035.888138	274007.390397	54.159207
3035.486589	273748.992008	54.164212
3034.709815	273493.000430	54.169217
3034.292854	273237.125381	54.174221
3033.675423	272978.661176	54.179226
3032.705464	272727.616996	54.184231
3031.958053	272458.248961	54.189236
3031.286229	272212.552425	54.194241
3030.373952	271952.915113	54.199245
3029.708734	271706.987767	54.204250
3028.844311	271464.379535	54.209255
3028.755132	271211.910056	54.214260
3027.909164	270956.488067	54.219265
3027.140057	270704.898317	54.224269
3026.712847	270444.412689	54.229274
3026.048896	270200.826824	54.234279
3025.361830	269942.626297	54.239284
3024.639694	269689.066652	54.244289
3023.860023	269432.842525	54.249293
3023.461015	269184.982959	54.254298
3022.459757	268934.271840	54.259303
3022.061941	268673.219412	54.264308
3021.047498	268417.110999	54.269313
3020.711323	268177.415091	54.274317
3020.012955	267917.992437	54.279322
3019.078389	267661.971697	54.284327
3018.444520	267413.718023	54.289332
3017.857998	267172.179602	54.294337
3017.510948	266910.404118	54.299341
3016.856777	266658.256844	54.304346
3015.925473	266416.369376	54.309351
3015.409878	266158.849865	54.314356
3015.003325	265907.169186	54.319361
3014.308143	265653.220091	54.324365
3013.721242	265388.199270	54.329370
3012.712241	265122.639178	54.334375
3011.740558	264857.021627	54.339380
3010.608872	264608.112791	54.344385
3010.207792	264365.904433	54.349389
3009.774037	264113.641685	54.354394
3008.780937	263872.043605	54.359399
3008.182579	263622.304617	54.364404
3007.576797	263378.449904	54.369409
3006.708245	263129.622780	54.374413
3006.300238	262889.630692	54.379418
3005.562388	262648.650676	54.384423
3005.099361	262400.568964	54.389428
3004.380599	262149.067196	54.394433
3003.568100	261904.686952	54.399437
3002.982708	261658.612403	54.404442
3002.484845	261420.367000	54.409447
3001.750218	261170.141030	54.414452
3001.396232	260923.186281	54.419457
3000.351626	260678.514247	54.424461
2999.829013	260434.822632	54.429466
2999.006621	260182.854096	54.434471
2998.532040	259932.303233	54.439476
2998.108117	259690.759386	54.444481
2997.305851	259440.697366	54.449485
2996.626191	259184.858550	54.454490
2995.869116	258946.402204	54.459495
2995.189701	258690.690608	54.464500
2994.290080	258442.682518	54.469505
2993.674843	258189.659519	54.474509
2993.255920	257935.686099	54.479514
2992.162203	257699.451922	54.484519
2991.667355	257458.658482	54.489524
2991.162077	257217.561192	54.494529
2990.459488	256966.081117	54.499533
2989.767962	256706.958691	54.504538
2988.947334	256477.961708	54.509543
2988.400607	256224.341135	54.514548
2987.781189	255981.276812	54.519553
2987.272683	255736.308903	54.524557
2986.770754	255478.936879	54.529562
2985.965115	255243.366582	54.534567
2985.195774	254990.395339	54.539572
2984.714679	254755.329933	54.544577
2983.812887	254507.627811	54.549581
2983.367368	254259.185592	54.554586
2982.435194	254016.200335	54.559591
2982.093574	253761.831823	54.564596
2981.626238	253504.963487	54.569601
2980.622291	253258.144925	54.574605
2980.159474	253008.432463	54.579610
2979.178780	252762.195797	54.584615
2978.709570	252506.881549	54.589620
2978.179840	252270.373180	54.594625
2977.081057	252017.102199	54.599629
2976.828626	251755.027529	54.604634
2975.859910	251521.268509	54.609639
2975.530645	251278.639278	54.614644
2974.946781	251029.151770	54.619649
2973.996930	250772.850494	54.624653
2973.289085	250518.901962	54.629658
2972.360540	250274.592689	54.634663
2972.079767	250027.982582	54.639668
2971.234859	249786.638967	54.644673
2970.881966	249539.481080	54.649677
2970.028081	249289.785686	54.654682
2969.371185	249043.443992	54.659687
2968.860876	248795.956771	54.664692
2967.871895	248545.317015	54.669697
2967.454699	248306.931656	54.674701
2966.652603	248048.925441	54.679706
2965.888259	247803.850629	54.684711
2965.531311	247557.331072	54.689716
2964.704423	247315.756311	54.694721
2963.910950	247061.467489	54.699725
2963.510403	246813.173041	54.704730
2962.622415	246568.527522	54.709735
2961.906956	246315.473746	54.714740
2961.435219	246077.761066	54.719745
2960.601038	245826.612507	54.724749
2960.133409	245573.898885	54.729754
2959.380127	245339.290904	54.734759
2959.020638	245079.733775	54.739764
2957.977379	244846.041562	54.744769
2957.192491	244604.512233	54.749773
2956.515085	244352.904960	54.754778
2955.631811	244107.368894	54.759783
2955.147698	243861.764812	54.764788
2954.667078	243623.724216	54.769793
2953.898561	243381.174280	54.774797
2953.089695	243127.043657	54.779802
2952.275888	242891.632778	54.784807
2952.103815	242643.098505	54.789812
2951.425359	242406.951792	54.794817
2950.645959	242168.555907	54.799821
2950.280133	241916.693645	54.804826
2949.470535	241667.123103	54.809831
2949.018236	241412.398246	54.814836
2948.234595	241169.063255	54.819841
2947.463842	240918.569938	54.824845
2946.764864	240676.952720	54.829850
2946.080470	240426.419654	54.834855
2945.414439	240170.357284	54.839860
2944.814049	239929.207812	54.844865
2944.217349	239687.675936	54.849869
2943.508562	239433.455281	54.854874
2942.773488	239194.341465	54.859879
2941.969286	238950.655603	54.864884
2941.405373	238709.246455	54.869889
2940.572939	238452.552206	54.874893
2940.180296	238214.857992	54.879898
2939.115230	237976.031032	54.884903
2938.373393	237725.077707	54.889908
2938.144513	237485.879207	54.894913
2937.428282	237246.891578	54.899917
2936.976007	236997.570452	54.904922
2936.231752	236755.506661	54.909927
2935.682166	236496.983720	54.914932
2934.963047	236249.542707	54.919937
2934.174987	236014.006807	54.924941
2933.795471	235759.708720	54.929946
2932.925023	235511.887010	54.934951
2932.021509	235264.071266	54.939956
2931.413067	235019.439701	54.944961
2930.669050	234770.069341	54.949965
2929.881137	234530.282282	54.954970
2929.285044	234284.197964	54.959975
2928.729036	234048.140969	54.964980
2928.140173	233806.563648	54.969985
2927.395538	233560.760354	54.974989
2927.171360	233302.440818	54.979994
2925.916430	233071.343168	54.984999
2925.278923	232824.274740	54.990004
2924.647893	232580.898187	54.995009
2923.939616	232335.828934	55.000013
2923.219118	232103.749949	55.005018
2922.548191	231869.116188	55.010023
2922.241021	231617.332750	55.015028
2921.650535	231374.358484	55.020033
2920.532345	231133.613905	55.025037
2920.104850	230887.836707	55.030042
2919.070030	230655.304164	55.035047
2918.900260	230413.634638	55.040052
2918.292663	230168.958905	55.045057
2917.252276	229924.714031	55.050061
2916.893331	229679.512734	55.055066
2916.201894	229442.823322	55.060071
2915.439763	229192.242001	55.065076
2914.702763	228955.637538	55.070081
2914.151263	228708.458927	55.075085
2913.789206	228466.035920	55.080090
2912.932121	228227.441356	55.085095
2912.228196	227978.965810	55.090100
2911.689670	227734.104016	55.095105
2911.005546	227492.883631	55.100109
2910.157984	227242.651327	55.105114
2909.422168	227002.510170	55.110119
2908.649960	226758.148387	55.115124
2907.985554	226514.074203	55.120129
2907.546964	226272.330149	55.125133
2906.843629	226027.397671	55.130138
2906.260805	225796.832911	55.135143
2905.518597	225542.664082	55.140148
2904.937537	225304.231133	55.145153
2904.144374	225052.465682	55.150157
2903.656839	224812.693467	55.155162
2902.749763	224575.616279	55.160167
2902.062090	224331.550108	55.165172
2901.626224	224080.183882	55.170177
2900.576771	223846.290032	55.175181
2900.386909	223598.855253	55.180186
2899.498741	223368.779928	55.185191
2898.783074	223124.058812	55.190196
2898.676222	222880.634715	55.195201
2897.447003	222637.963104	55.200205
2896.904653	222389.725202	55.205210
2896.007396	222157.030875	55.210215
2895.657448	221900.255971	55.215220
2894.966570	221672.161863	55.220225
2894.156283	221431.636536	55.225229
2893.753325	221181.518458	55.230234
2892.922207	220939.877279	55.235239
2892.266528	220698.155704	55.240244
2891.583417	220464.664243	55.245249
2890.984895	220221.889885	55.250253
2890.464535	219969.324508	55.255258
2889.825755	219730.963366	55.260263
2889.446663	219486.828983	55.265268
2888.874512	219229.970736	55.270273
2887.934718	218997.086414	55.275277
2887.530117	218741.524804	55.280282
2886.677895	218496.633173	55.285287
2885.916674	218241.846665	55.290292
2885.287101	217995.263001	55.295297
2884.664978	217743.738718	55.300301
2884.170785	217490.920004	55.305306
2883.237997	217247.470977	55.310311
2882.365784	216991.280509	55.315316
2881.807681	216757.419207	55.320321
2880.931078	216513.911381	55.325325
2880.773201	216264.424803	55.330330
2879.832839	216019.477655	55.335335
2879.226563	215771.138361	55.340340
2878.427332	215523.927560	55.345345
2877.504366	215288.094962	55.350349
2876.978253	215037.019271	55.355354
2876.099341	214809.252005	55.360359
2875.416198	214556.752995	55.365364
2874.600469	214324.978419	55.370369
2873.841590	214084.639258	55.375373
2873.414711	213849.412857	55.380378
2872.482618	213617.379781	55.385383
2872.196285	213375.230208	55.390388
2871.675769	213128.716288	55.395393
2870.534537	212893.741630	55.400397
2869.806911	212660.555628	55.405402
2869.094359	212431.365188	55.410407
2868.630734	212185.175045	55.415412
2868.131521	211956.000254	55.420417
2867.184082	211729.550667	55.425421
2867.100309	211492.540159	55.430426
2865.973264	211258.891264	55.435431
2865.419113	211020.129119	55.440436
2864.914434	210791.289206	55.445441
2864.054180	210559.760785	55.450445
2863.581703	210319.535244	55.455450
2862.824139	210081.039527	55.460455
2862.163784	209837.206414	55.465460
2862.005193	209598.940655	55.470465
2861.170881	209367.971088	55.475469
2860.488364	209115.945256	55.480474
2859.542295	208885.225226	55.485479
2858.820014	208644.359542	55.490484
2858.471337	208406.817007	55.495489
2857.278505	208169.546687	55.500493
2856.944964	207929.889648	55.505498
2856.209963	207707.831626	55.510503
2855.643468	207459.711842	55.515508
2855.145926	207218.493571	55.520513
2854.029693	206983.568634	55.525517
2853.389184	206753.145961	55.530522
2852.729945	206520.703034	55.535527
2852.410669	206276.363625	55.540532
2851.756668	206041.846152	55.545537
2850.727244	205820.454580	55.550541
2850.264946	205571.877157	55.555546
2849.420391	205344.344884	55.560551
2849.015181	205106.337795	55.565556
2848.456555	204864.067644	55.570561
2847.676931	204631.167016	55.575565
2847.761364	204392.963833	55.580570
2846.841358	204141.261184	55.585575
2846.145854	203900.901408	55.590580
2845.305163	203656.824641	55.595585
2844.626734	203408.163686	55.600589
2844.209329	203165.250927	55.605594
2843.334568	202930.869557	55.610599
2842.513428	202687.759984	55.615604
2842.099294	202444.454345	55.620609
2841.375018	202206.434311	55.625613
2840.822168	201954.816136	55.630618
2840.223385	201718.010963	55.635623
2839.547362	201469.648742	55.640628
2838.407890	201217.127679	55.645633
2837.607354	200986.902192	55.650637
2836.775251	200743.062525	55.655642
2836.042743	200514.634448	55.660647
2835.524400	200274.981553	55.665652
2835.456614	200039.669463	55.670657
2834.231125	199810.398617	55.675661
2833.797104	199564.432772	55.680666
2832.626972	199330.151487	55.685671
2832.084321	199089.475642	55.690676
2831.552727	198856.270595	55.695681
2830.725243	198626.948268	55.700685
2830.328878	198385.231508	55.705690
2829.395175	198163.566140	55.710695
2828.656043	197929.304952	55.715700
2828.231692	197697.167369	55.720705
2827.095056	197468.449002	55.725709
2826.721436	197236.342480	55.730714
2826.330329	197013.340660	55.735719
2825.474793	196786.256696	55.740724
2824.820571	196546.919734	55.745729
2824.094604	196314.532876	55.750733
2823.441234	196083.343608	55.755738
2822.901284	195858.792681	55.760743
2822.101249	195620.145787	55.765748
2821.598131	195390.677001	55.770753
2820.885624	195165.394187	55.775757
2820.583778	194939.494649	55.780762
2819.841373	194697.264590	55.785767
2819.391782	194460.993042	55.790772
2818.476489	194222.599972	55.795777
2817.324728	193992.050444	55.800781
2817.144633	193756.919085	55.805786
2816.497602	193528.206868	55.810791
2815.811717	193298.229312	55.815796
2815.563896	193060.388288	55.820801
2814.272472	192828.555801	55.825805
2813.916146	192579.738303	55.830810
2813.190558	192361.174930	55.835815
2812.880927	192120.446051	55.840820
2812.248220	191875.916836	55.845825
2811.180760	191641.084879	55.850829
2810.735970	191400.840029	55.855834
2810.034772	191174.767376	55.860839
2809.214797	190934.270246	55.865844
2808.579941	190692.698769	55.870849
2807.667063	190450.921197	55.875853
2807.056429	190214.107456	55.880858
2806.355364	189986.562752	55.885863
2806.064597	189746.539806	55.890868
2805.304233	189516.207010	55.895873
2803.954209	189287.973998	55.900877
2803.709101	189056.307642	55.905882
2802.998795	188823.614424	55.910887
2802.594958	188587.191656	55.915892
2801.872240	188354.133294	55.920897
2800.752841	188122.543576	55.925901
2800.504404	187894.471225	55.930906
2800.047540	187661.204689	55.935911
2799.113051	187424.304508	55.940916
2798.801617	187189.945938	55.945921
2797.871831	186965.111622	55.950925
2797.306467	186717.639070	55.955930
2796.510253	186489.691212	55.960935
2795.917556	186252.762806	55.965940
2795.076185	186023.526400	55.970945
2794.537537	185793.615579	55.975949
2793.727050	185548.964228	55.980954
2793.256632	185327.010242	55.985959
2792.600587	185090.199244	55.990964
2792.101700	184864.255907	55.995969
2790.996332	184628.427164	56.000973
2790.420793	184390.243632	56.005978
2789.944605	184155.925535	56.010983
2789.012634	183928.316486	56.015988
2788.739445	183699.437728	56.020993
2787.979754	183463.198461	56.025997
2787.262750	183230.057977	56.031002
2786.667499	183007.141829	56.036007
2785.702762	182761.930801	56.041012
2785.485820	182524.062975	56.046017
2784.727392	182294.063995	56.051021
2783.904764	182066.113023	56.056026
2783.121424	181837.634544	56.061031
2782.572537	181596.989694	56.066036
2782.028969	181360.315291	56.071041
2781.205940	181133.971669	56.076045
2781.215515	180895.804988	56.081050
2780.488007	180667.423693	56.086055
2779.806604	180426.883041	56.091060
2778.857559	180188.361584	56.096065
2778.412252	179946.650216	56.101069
2777.764345	179704.287423	56.106074
2777.470628	179460.732695	56.111079
2776.370311	179225.231747	56.116084
2775.897176	178981.010026	56.121089
2774.903813	178741.751891	56.126093
2774.035098	178495.322316	56.131098
2773.543846	178266.376552	56.136103
2772.812550	178028.362075	56.141108
2772.027145	177779.224054	56.146113
2771.190063	177553.305325	56.151117
2770.765497	177323.436168	56.156122
2769.986818	177087.851737	56.161127
2769.227859	176858.792534	56.166132
2768.518552	176623.083865	56.171137
2767.550416	176391.021434	56.176141
2767.147456	176158.659890	56.181146
2766.704158	175930.708798	56.186151
2765.663021	175691.791094	56.191156
2765.196997	175465.296511	56.196161
2764.281592	175251.030976	56.201165
2763.935706	175023.856213	56.206170
2763.213129	174788.311051	56.211175
2762.402854	174552.731093	56.216180
2762.175780	174326.073592	56.221185
2761.492028	174106.951149	56.226189
2760.771394	173869.132502	56.231194
2760.039919	173633.772468	56.236199
2759.218322	173401.240817	56.241204
2758.747585	173167.301640	56.246209
2757.893696	172955.274816	56.251213
2757.329942	172713.605270	56.256218
2756.723502	172482.669783	56.261223
2755.839972	172249.441712	56.266228
2755.249529	172026.126762	56.271233
2754.447971	171798.535857	56.276237
2753.979755	171559.667508	56.281242
2753.475155	171338.071386	56.286247
2752.459873	171117.161533	56.291252
2752.130693	170887.967494	56.296257
2751.103887	170653.499395	56.301261
2750.579234	170425.422412	56.306266
2749.739645	170203.341750	56.311271
2749.277835	169964.543917	56.316276
2748.997024	169738.604110	56.321281
2747.958191	169507.935017	56.326285
2747.469317	169276.358848	56.331290
2746.763493	169050.176938	56.336295
2746.109814	168822.167952	56.341300
2745.375197	168588.118221	56.346305
2744.791143	168364.132474	56.351309
2743.997866	168135.463733	56.356314
2743.018775	167908.240009	56.361319
2742.418949	167680.710876	56.366324
2741.873727	167445.349673	56.371329
2741.218359	167235.858937	56.376333
2740.749871	167002.356986	56.381338
2740.111656	166780.207413	56.386343
2739.330005	166547.613660	56.391348
2739.282877	166313.699755	56.396353
2738.191600	166089.493799	56.401357
2738.050805	165854.046278	56.406362
2737.298781	165620.447256	56.411367
2736.258248	165367.956964	56.416372
2735.640989	165149.831725	56.421377
2734.636739	164926.214604	56.426381
2734.631519	164685.025602	56.431386
2733.837524	164451.363547	56.436391
2732.479115	164231.181489	56.441396
2731.954332	163990.263155	56.446401
2731.371535	163768.691497	56.451405
2730.793976	163540.161879	56.456410
2729.966406	163309.806258	56.461415
2729.441571	163093.189124	56.466420
2728.533130	162861.424994	56.471425
2727.677380	162636.585688	56.476429
2727.252756	162404.283376	56.481434
2726.652813	162185.330348	56.486439
2725.888265	161953.584638	56.491444
2725.248645	161724.579083	56.496449
2724.683060	161510.927887	56.501453
2724.303817	161289.321369	56.506458
2723.690708	161055.086952	56.511463
2722.643031	160837.781859	56.516468
2722.358670	160601.573054	56.521473
2721.314479	160373.152672	56.526477
2720.563830	160144.276326	56.531482
2720.055896	159925.179232	56.536487
2719.639099	159705.915065	56.541492
2719.218747	159464.749808	56.546497
2717.690833	159242.180118	56.551501
2717.448803	159021.452369	56.556506
2716.896108	158800.181076	56.561511
2716.266853	158570.809227	56.566516
2715.488575	158332.993209	56.571521
2714.537831	158111.373880	56.576525
2714.105100	157893.215787	56.581530
2713.244836	157665.770828	56.586535
2712.461838	157435.782878	56.591540
2712.157750	157212.124603	56.596545
2711.305653	156998.151073	56.601549
2710.740149	156771.640024	56.606554
2710.050318	156548.165767	56.611559
2709.568592	156323.537946	56.616564
2709.035694	156101.400195	56.621569
2707.860108	155879.246317	56.626573
2707.163307	155642.640221	56.631578
2706.616299	155424.680175	56.636583
2705.860211	155207.418382	56.641588
2705.120253	154976.444973	56.646593
2704.637657	154768.918972	56.651597
2704.200759	154545.272668	56.656602
2703.708564	154326.469837	56.661607
2702.729457	154093.698314	56.666612
2702.518622	153867.015789	56.671617
2701.931230	153657.160715	56.676621
2701.296984	153418.407808	56.681626
2700.734910	153192.615811	56.686631
2699.541025	152959.798639	56.691636
2698.905707	152718.951782	56.696641
2698.352615	152502.954532	56.701645
2697.676002	152263.452841	56.706650
2696.916172	152049.502738	56.711655
2696.328029	151832.052721	56.716660
2695.557525	151587.509857	56.721665
2694.984762	151375.515330	56.726669
2694.341609	151141.864581	56.731674
2693.592370	150921.967426	56.736679
2692.896936	150693.478595	56.741684
2692.334229	150469.838880	56.746689
2691.240712	150251.695698	56.751693
2691.173894	150015.549864	56.756698
2690.221744	149799.890230	56.761703
2689.735226	149572.898333	56.766708
2689.491285	149339.902435	56.771713
2688.662944	149121.173598	56.776717
2688.359136	148891.509589	56.781722
2687.282716	148666.188007	56.786727
2686.657212	148427.782350	56.791732
2685.800424	148195.012685	56.796737
2684.959950	147973.100905	56.801741
2684.526346	147734.666844	56.806746
2683.882737	147508.121106	56.811751
2682.901871	147284.889550	56.816756
2682.561832	147054.441885	56.821761
2681.878844	146835.281908	56.826765
2680.886433	146603.740579	56.831770
2680.013610	146373.884093	56.836775
2679.183164	146154.371892	56.841780
2678.921588	145937.904381	56.846785
2678.084867	145715.242538	56.851789
2677.757833	145486.874955	56.856794
2676.863153	145263.857024	56.861799
2676.013774	145047.889383	56.866804
2675.601918	144818.129133	56.871809
2674.822752	144607.682968	56.876813
2674.146425	144380.602597	56.881818
2673.551562	144156.929899	56.886823
2672.756824	143940.539917	56.891828
2672.130970	143718.362803	56.896833
2671.330349	143505.701709	56.901837
2670.734145	143286.840589	56.906842
2670.486893	143063.318680	56.911847
2669.390545	142845.664565	56.916852
2669.082470	142623.363619	56.921857
2668.150457	142407.629305	56.926861
2667.514472	142176.640093	56.931866
2667.052141	141959.582269	56.936871
2666.178775	141745.787128	56.941876
2665.621242	141519.200386	56.946881
2664.729219	141306.568010	56.951885
2664.845595	141074.008057	56.956890
2663.732833	140855.796838	56.961895
2662.788177	140641.575601	56.966900
2662.313335	140420.766271	56.971905
2661.995947	140194.744514	56.976909
2661.275260	139976.357335	56.981914
2660.273447	139753.442948	56.986919
2659.337404	139531.078108	56.991924
2659.048728	139299.400063	56.996929
2658.090721	139087.593336	57.001933
2657.174319	138868.941457	57.006938
2656.840531	138647.331083	57.011943
2655.802040	138434.245445	57.016948
2655.486738	138219.867988	57.021953
2654.571466	138010.247077	57.026957
2654.074926	137789.725150	57.031962
2653.436802	137577.021320	57.036967
2652.900297	137361.364981	57.041972
2652.401853	137142.601799	57.046977
2651.563244	136932.631167	57.051981
2650.993017	136714.010124	57.056986
2650.474277	136489.801280	57.061991
2649.591534	136277.871935	57.066996
2649.085640	136051.744349	57.072001
2648.357215	135841.939600	57.077005
2647.961197	135623.079733	57.082010
2647.164366	135393.853880	57.087015
2646.426225	135178.652657	57.092020
2645.719577	134950.164377	57.097025
2644.918365	134739.285804	57.102029
2644.233329	134525.312669	57.107034
2643.713186	134301.487267	57.112039
2642.869940	134086.120383	57.117044
2642.607800	133859.444785	57.122049
2641.727309	133648.726488	57.127053
2640.940471	133427.634487	57.132058
2640.497906	133220.237764	57.137063
2639.483669	132991.370660	57.142068
2639.291213	132779.599745	57.147073
2638.392138	132567.035840	57.152077
2637.581596	132346.005992	57.157082
2636.917800	132126.210839	57.162087
2636.460561	131913.143518	57.167092
2635.944696	131696.198407	57.172097
2635.558712	131475.025623	57.177101
2634.764211	131246.603421	57.182106
2634.270373	131025.032715	57.187111
2633.207735	130803.980157	57.192116
2632.777537	130579.999531	57.197121
2631.797300	130367.082582	57.202125
2630.969786	130144.227761	57.207130
2630.850574	129917.783831	57.212135
2629.860342	129694.705756	57.217140
2629.437511	129483.770951	57.222145
2628.710661	129262.976597	57.227149
2627.934467	129029.445322	57.232154
2627.444687	128804.203682	57.237159
2626.385722	128592.925980	57.242164
2625.844791	128371.000379	57.247169
2625.124149	128152.195190	57.252173
2624.575066	127927.694279	57.257178
2624.011613	127716.528345	57.262183
2623.368242	127497.549269	57.267188
2622.623068	127271.777600	57.272193
2622.192418	127053.896264	57.277197
2621.622198	126823.777201	57.282202
2620.815351	126604.285850	57.287207
2619.781299	126389.752749	57.292212
2619.598293	126156.420899	57.297217
2618.634810	125943.912015	57.302221
2617.695102	125723.636285	57.307226
2617.271070	125500.300457	57.312231
2616.506409	125289.820648	57.317236
2615.776957	125061.063367	57.322241
2614.702838	124857.132749	57.327245
2614.131278	124632.341672	57.332250
2613.466113	124428.115263	57.337255
2612.678372	124220.493031	57.342260
2612.377114	124008.240043	57.347265
2611.384258	123797.453640	57.352269
2610.969758	123588.768061	57.357274
2610.508691	123370.447668	57.362279
2609.372269	123166.335629	57.367284
2608.921010	122946.313942	57.372289
2608.353741	122739.248568	57.377293
2607.496914	122521.256032	57.382298
2606.890976	122320.032225	57.387303
2606.394962	122110.532114	57.392308
2605.754561	121893.193223	57.397313
2605.127340	121682.511452	57.402317
2604.048806	121468.185540	57.407322
2603.752490	121262.278294	57.412327
2602.943724	121053.321799	57.417332
2602.545747	120842.695663	57.422337
2601.545396	120629.899724	57.427341
2601.231690	120413.989501	57.432346
2600.625400	120198.410362	57.437351
2600.005784	120003.188512	57.442356
2599.221230	119774.950585	57.447361
2598.507752	119568.884913	57.452365
2597.630059	119353.383699	57.457370
2597.228803	119137.040334	57.462375
2596.402674	118929.778716	57.467380
2596.099141	118713.574200	57.472385
2595.370312	118501.738048	57.477389
2594.719934	118292.456277	57.482394
2593.828216	118072.596535	57.487399
2593.167666	117862.506497	57.492404
2592.815346	117636.968011	57.497409
2591.720048	117428.708552	57.502413
2591.135978	117215.726294	57.507418
2590.525294	116998.761167	57.512423
2589.962756	116793.578408	57.517428
2589.520504	116575.927052	57.522433
2588.729843	116362.554429	57.527437
2587.968656	116153.548297	57.532442
2587.612954	115936.242641	57.537447
2586.537649	115727.293283	57.542452
2586.352288	115496.013734	57.547457
2585.566092	115284.668095	57.552461
2584.600841	115069.353205	57.557466
2584.002422	114857.711848	57.562471
2583.142780	114640.159137	57.567476
2582.874301	114430.789127	57.572481
2581.763558	114217.321983	57.577485
2581.238011	114006.627151	57.582490
2580.800966	113793.632330	57.587495
2580.031599	113583.617420	57.592500
2579.661782	113361.443335	57.597505
2578.642709	113146.101343	57.602509
2578.018940	112931.849295	57.607514
2577.486003	112729.129317	57.612519
2576.565681	112499.384182	57.617524
2576.163431	112292.123183	57.622529
2575.307127	112073.484522	57.627533
2574.693648	111865.411768	57.632538
2574.129501	111648.491976	57.637543
2573.517311	111438.313743	57.642548
2572.895788	111225.725461	57.647553
2572.073641	111012.817460	57.652557
2571.055668	110801.087644	57.657562
2570.649480	110587.324327	57.662567
2570.193916	110385.243110	57.667572
2569.619344	110160.779693	57.672577
2568.741351	109960.945589	57.677581
2568.370531	109741.645277	57.682586
2567.906234	109524.572548	57.687591
2566.589484	109313.121068	57.692596
2566.084319	109090.953217	57.697601
2565.473934	108888.160085	57.702605
2564.673295	108669.995870	57.707610
2563.742743	108460.262928	57.712615
2563.277307	108247.213634	57.717620
2563.044714	108023.471146	57.722625
2562.258686	107828.792880	57.727629
2561.549999	107610.900774	57.732634
2560.860542	107400.715662	57.737639
2559.884221	107182.961624	57.742644
2559.452601	106961.865224	57.747649
2558.540138	106758.695059	57.752653
2558.072748	106547.500756	57.757658
2557.212861	106331.867080	57.762663
2556.305712	106126.834011	57.767668
2555.695296	105911.173748	57.772673
2555.140449	105713.232974	57.777677
2554.131039	105515.003102	57.782682
2553.804637	105311.235709	57.787687
2553.330018	105108.587255	57.792692
2552.677770	104895.964489	57.797697
2552.134514	104688.594504	57.802701
2551.357844	104488.757868	57.807706
2550.665543	104275.499282	57.812711
2549.965841	104065.507011	57.817716
2549.424393	103848.924615	57.822721
2548.533090	103650.142381	57.827725
2548.147651	103447.250042	57.832730
2547.466290	103224.741509	57.837735
2546.668013	103032.207842	57.842740
2546.256511	102809.910612	57.847745
2545.214529	102607.581344	57.852749
2544.735456	102404.916161	57.857754
2544.111065	102182.279702	57.862759
2543.549666	101991.097110	57.867764
2542.818987	101762.705312	57.872769
2541.921652	101564.688930	57.877773
2541.253453	101356.363378	57.882778
2540.929124	101139.937516	57.887783
2540.075756	100937.144513	57.892788
2539.709979	100732.574790	57.897793
2538.753627	100528.437727	57.902797
2537.795147	100312.120793	57.907802
2537.208490	100109.110905	57.912807
2536.631562	99896.718729	57.917812
2536.058185	99699.556204	57.922817
2535.481115	99497.285822	57.927821
2534.788456	99287.939985	57.932826
2534.173017	99079.071420	57.937831
2533.398231	98867.775243	57.942836
2532.788430	98662.057534	57.947841
2532.175655	98456.792656	57.952845
2531.322673	98253.011366	57.957850
2530.729542	98037.139808	57.962855
2529.999234	97845.610417	57.967860
2529.593825	97637.047745	57.972865
2528.692923	97433.858782	57.977869
2528.074176	97223.393685	57.982874
2527.765696	97016.761774	57.987879
2526.652119	96810.193003	57.992884
2526.088807	96596.226342	57.997889
2525.362153	96396.278289	58.002893
2524.422822	96199.598790	58.007898
2524.385189	95989.679281	58.012903
2523.434968	95796.044969	58.017908
2522.908220	95575.372023	58.022913
2522.053781	95383.133507	58.027917
2521.167954	95171.779102	58.032922
2520.751895	94965.607569	58.037927
2519.842608	94765.798865	58.042932
2519.479204	94560.649812	58.047937
2518.764193	94355.283299	58.052941
2517.753438	94160.948437	58.057946
2517.445563	93957.984370	58.062951
2516.588694	93760.230983	58.067956
2515.827109	93546.444751	58.072961
2515.432226	93348.774314	58.077965
2514.787127	93154.809993	58.082970
2514.170492	92946.112857	58.087975
2513.427713	92745.060729	58.092980
2512.610078	92549.061808	58.097985
2512.084746	92337.669805	58.102989
2511.380021	92141.274056	58.107994
2511.018295	91935.245253	58.112999
2509.974828	91738.644093	58.118004
2509.545031	91530.796357	58.123009
2508.906711	91326.279472	58.128013
2508.064267	91131.895198	58.133018
2507.492720	90930.530359	58.138023
2506.814419	90721.228044	58.143028
2506.208552	90516.388746	58.148033
2505.386222	90320.592425	58.153037
2504.748562	90125.813104	58.158042
2504.254705	89914.151056	58.163047
2503.316900	89721.539293	58.168052
2502.851967	89516.512985	58.173057
2502.316394	89314.209897	58.178061
2501.432956	89112.729387	58.183066
2500.621734	88908.744574	58.188071
2500.080804	88709.867473	58.193076
2499.567627	88509.337560	58.198081
2498.937236	88310.561527	58.203085
2498.009169	88107.142786	58.208090
2497.753139	87904.384951	58.213095
2496.828462	87708.982558	58.218100
2496.450745	87507.784315	58.223105
2495.591548	87303.212208	58.228109
2494.882153	87095.856318	58.233114
2494.673239	86882.065731	58.238119
2493.566025	86689.285113	58.243124
2493.151010	86487.518128	58.248129
2492.330678	86275.836008	58.253133
2491.452073	86074.754492	58.258138
2491.287213	85866.573907	58.263143
2490.412240	85668.921138	58.268148
2489.814892	85465.728467	58.273153
2488.834633	85262.647409	58.278157
2488.036941	85056.929457	58.283162
2487.582146	84857.390876	58.288167
2486.735106	84654.596784	58.293172
2486.167741	84456.933281	58.298177
2485.572505	84265.816751	58.303181
2484.631951	84060.690178	58.308186
2484.222627	83857.320620	58.313191
2483.214820	83676.086906	58.318196
2482.671236	83468.366499	58.323201
2482.139085	83273.009696	58.328205
2481.495633	83072.414734	58.333210
2480.958836	82875.184355	58.338215
2480.305384	82684.071651	58.343220
2479.427257	82476.867639	58.348225
2478.774527	82277.860607	58.353229
2477.960145	82089.571372	58.358234
2478.047641	81886.076958	58.363239
2476.985455	81692.092677	58.368244
2476.299940	81489.983498	58.373249
2475.553846	81289.078941	58.378253
2474.719312	81090.804576	58.383258
2474.448729	80905.641574	58.388263
2473.421554	80668.381820	58.393268
2473.044502	80445.855629	58.398273
2472.451496	80245.530220	58.403277
2471.936349	80053.020187	58.408282
2471.658905	79843.149258	58.413287
2470.708797	79644.938828	58.418292
2470.036284	79436.236441	58.423297
2469.718633	79224.443571	58.428301
2468.844177	79024.513107	58.433306
2468.377488	78810.180865	58.438311
2467.191711	78609.184663	58.443316
2466.107030	78405.211109	58.448321
2465.555774	78209.875097	58.453325
2465.123801	78007.429822	58.458330
2464.488972	77801.031843	58.463335
2463.794303	77605.592368	58.468340
2463.310429	77406.218210	58.473345
2462.759951	77201.206521	58.478349
2462.103316	77003.133844	58.483354
2461.296968	76797.389515	58.488359
2460.318821	76599.844645	58.493364
2459.591903	76395.320717	58.498369
2458.991966	76201.697286	58.503373
2457.933301	75998.945933	58.508378
2457.948921	75800.730867	58.513383
2457.269439	75608.686177	58.518388
2456.444812	75406.921153	58.523393
2455.876719	75211.373040	58.528397
2455.034031	75010.876618	58.533402
2454.513784	74806.496745	58.538407
2453.619892	74612.074920	58.543412
2452.911134	74409.119650	58.548417
2452.199369	74225.646612	58.553421
2451.275487	74040.036374	58.558426
2450.890402	73838.952319	58.563431
2450.287853	73650.563779	58.568436
2449.515663	73448.389059	58.573441
2448.992128	73261.106323	58.578445
2447.805111	73066.285293	58.583450
2447.693120	72862.696865	58.588455
2447.235557	72676.415987	58.593460
2446.529889	72467.695322	58.598465
2446.006108	72271.480793	58.603469
2445.109184	72073.708647	58.608474
2444.717733	71882.059147	58.613479
2443.834665	71681.225744	58.618484
2443.057534	71472.970586	58.623489
2442.082768	71288.495459	58.628493
2441.578080	71092.567198	58.633498
2441.015715	70902.464470	58.638503
2439.693213	70712.271455	58.643508
2439.693144	70511.253473	58.648513
2438.945461	70320.198467	58.653517
2437.966774	70132.950549	58.658522
2437.648706	69945.198232	58.663527
2437.148989	69751.981978	58.668532
2436.213339	69560.109928	58.673537
2435.895651	69367.411204	58.678541
2435.220167	69176.531449	58.683546
2434.447662	68985.016991	58.688551
2433.803731	68793.526629	58.693556
2433.118465	68586.430916	58.698561
2432.431525	68393.227131	58.703565
2431.248905	68198.924368	58.708570
2431.067425	68007.666226	58.713575
2430.022818	67822.522583	58.718580
2429.458459	67636.246127	58.723585
2428.940254	67444.822364	58.728589
2427.957577	67265.587362	58.733594
2427.762716	67062.023123	58.738599
2426.714013	66885.553734	58.743604
2425.985945	66700.638267	58.748609
2425.709381	66506.316418	58.753613
2424.835374	66325.986792	58.758618
2424.290144	66123.651418	58.763623
2423.467852	65948.076553	58.768628
2422.980046	65755.705626	58.773633
2422.299354	65556.194159	58.778637
2421.649054	65382.711655	58.783642
2421.485409	65189.510810	58.788647
2420.582091	64996.558621	58.793652
2420.071540	64796.023770	58.798657
2419.563326	64601.435735	58.803661
2418.560801	64410.217211	58.808666
2418.148054	64210.755045	58.813671
2416.916652	64022.849669	58.818676
2416.167545	63827.492363	58.823681
2415.773017	63641.538878	58.828685
2414.636195	63445.985220	58.833690
2414.664241	63260.767784	58.838695
2413.804784	63079.899362	58.843700
2412.909635	62885.507475	58.848705
2412.888621	62693.965683	58.853709
2411.962510	62506.205529	58.858714
2411.532384	62316.327901	58.863719
2410.701358	62119.485884	58.868724
2410.045701	61916.347989	58.873729
2409.238497	61721.362550	58.878733
2408.474729	61535.801500	58.883738
2407.941019	61340.760206	58.888743
2407.357651	61154.652068	58.893748
2406.615780	60965.841380	58.898753
2406.164236	60768.966320	58.903757
2405.260659	60583.932007	58.908762
2404.751660	60383.490007	58.913767
2404.055064	60193.626702	58.918772
2403.512766	59999.385327	58.923777
2403.123370	59797.287332	58.928781
2402.102346	59608.739586	58.933786
2401.158279	59412.627065	58.938791
2400.261808	59226.602557	58.943796
2399.586432	59034.046937	58.948801
2399.021203	58841.505979	58.953805
2398.381832	58669.465317	58.958810
2397.843300	58474.255600	58.963815
2396.713417	58291.099220	58.968820
2396.322213	58101.095380	58.973825
2395.763616	57920.898748	58.978829
2394.818996	57736.549814	58.983834
2394.642877	57547.407772	58.988839
2393.673283	57364.435089	58.993844
2392.922264	57179.544892	58.998849
2392.530865	57003.148431	59.003853
2391.491045	56806.880958	59.008858
2390.744955	56623.293857	59.013863
2390.038184	56453.817818	59.018868
2389.404360	56265.817740	59.023873
2389.061328	56089.344956	59.028877
2388.025057	55913.676490	59.033882
2387.792426	55726.126037	59.038887
2387.234605	55538.404852	59.043892
2386.466017	55362.923508	59.048897
2386.017837	55185.215880	59.053901
2385.023135	54997.010605	59.058906
2384.598647	54810.078022	59.063911
2384.012475	54633.399851	59.068916
2383.132775	54442.392638	59.073921
2382.706794	54248.737629	59.078925
2381.737212	54067.245668	59.083930
2381.268990	53878.593477	59.088935
2380.685082	53699.237159	59.093940
2379.615234	53505.560088	59.098945
2379.046490	53318.070667	59.103949
2378.362790	53141.447732	59.108954
2377.644722	52952.226241	59.113959
2376.591944	52777.132964	59.118964
2376.239614	52597.056530	59.123969
2375.586917	52420.973151	59.128973
2374.615764	52242.177636	59.133978
2374.159196	52058.114226	59.138983
2373.341318	51888.372887	59.143988
2372.748996	51714.198455	59.148993
2372.235723	51535.502080	59.153997
2371.263376	51358.874747	59.159002
2370.735358	51183.401845	59.164007
2370.145000	51009.024290	59.169012
2369.638786	50837.154827	59.174017
2368.951881	50665.539451	59.179021
2368.190091	50485.501649	59.184026
2367.755900	50303.876704	59.189031
2367.068850	50131.765657	59.194036
2366.685722	49948.634175	59.199041
2365.672650	49767.961901	59.204045
2364.661842	49598.051687	59.209050
2364.281762	49414.608013	59.214055
2363.260077	49242.473355	59.219060
2363.053825	49065.444396	59.224065
2362.570789	48880.136001	59.229069
2362.127425	48715.760491	59.234074
2361.140104	48529.509335	59.239079
2360.169193	48362.003400	59.244084
2359.584501	48178.137723	59.249089
2358.974584	47998.784084	59.254093
2358.444003	47829.944016	59.259098
2358.076605	47654.057433	59.264103
2356.981651	47471.121672	59.269108
2356.518099	47299.925270	59.274113
2355.998583	47114.820492	59.279117
2354.628304	46937.968845	59.284122
2354.632814	46760.589290	59.289127
2353.880520	46593.754748	59.294132
2353.434751	46410.946035	59.299137
2352.708073	46225.081007	59.304141
2351.477652	46049.410471	59.309146
2351.029802	45868.389864	59.314151
2350.194416	45700.257002	59.319156
2349.848534	45526.653166	59.324161
2349.433250	45343.459990	59.329165
2348.818258	45170.893222	59.334170
2348.017272	44981.209373	59.339175
2347.564905	44811.264860	59.344180
2346.609568	44630.672019	59.349185
2345.731165	44453.692751	59.354189
2344.935149	44280.408339	59.359194
2344.931652	44100.667710	59.364199
2343.857905	43922.295810	59.369204
2343.273102	43751.348178	59.374209
2342.990152	43565.721291	59.379213
2341.829250	43396.825499	59.384218
2341.617072	43215.634692	59.389223
2340.513462	43029.390443	59.394228
2339.993669	42850.718657	59.399233
2339.502206	42676.364837	59.404237
2338.605052	42498.124965	59.409242
2338.434650	42316.524112	59.414247
2337.360044	42144.307237	59.419252
2336.506604	41959.167229	59.424257
2336.331429	41779.861053	59.429261
2335.188361	41602.497915	59.434266
2334.650574	41419.844799	59.439271
2333.846445	41250.521078	59.444276
2333.163151	41077.512712	59.449281
2332.466219	40902.324181	59.454285
2331.824291	40731.144686	59.459290
2331.078973	40550.035909	59.464295
2330.421172	40378.691434	59.469300
2329.553600	40212.838107	59.474305
2328.897500	40038.359718	59.479309
2327.840905	39876.878042	59.484314
2327.623236	39705.749366	59.489319
2327.171657	39537.555183	59.494324
2326.540947	39362.300173	59.499329
2325.751277	39195.445597	59.504333
2324.839677	39036.468996	59.509338
2324.369262	38860.855823	59.514343
2323.618014	38691.384919	59.519348
2322.794105	38527.251441	59.524353
2322.548327	38354.734797	59.529357
2321.627300	38186.819878	59.534362
2321.186312	38026.024474	59.539367
2320.172882	37858.207469	59.544372
2319.688726	37680.348172	59.549377
2318.823886	37508.996007	59.554381
2318.109389	37345.053725	59.559386
2317.476264	37172.386517	59.564391
2316.852421	37016.204221	59.569396
2315.831686	36852.369336	59.574401
2315.278292	36690.889609	59.579405
2314.201926	36532.127355	59.584410
2313.767134	36368.301040	59.589415
2313.062139	36220.867314	59.594420
2312.379417	36057.839337	59.599425
2311.995365	35903.587534	59.604429
2311.365614	35753.233374	59.609434
2310.476452	35591.586598	59.614439
2309.817181	35438.819277	59.619444
2309.043788	35283.572882	59.624449
2309.075504	35126.592138	59.629453
2308.089546	34972.365697	59.634458
2307.689070	34803.968763	59.639463
2306.878770	34646.088759	59.644468
2305.590362	34478.732671	59.649473
2305.421759	34324.792816	59.654477
2304.144530	34180.536434	59.659482
2303.852221	34018.716160	59.664487
2302.801246	33860.412693	59.669492
2301.990101	33726.778211	59.674497
2301.306543	33576.520886	59.679501
2300.560432	33438.982411	59.684506
2300.145335	33289.127706	59.689511
2298.986940	33141.404170	59.694516
2298.668583	33000.195246	59.699521
2297.751093	32852.502493	59.704525
2297.099279	32723.277759	59.709530
2296.286318	32583.694354	59.714535
2295.648053	32452.419029	59.719540
2294.665676	32313.800041	59.724545
2294.339032	32169.609193	59.729549
2293.359085	32048.462616	59.734554
2292.839567	31912.017066	59.739559
2291.936173	31783.038275	59.744564
2291.255003	31653.047978	59.749569
2290.354273	31522.071119	59.754573
2289.103643	31412.548075	59.759578
2288.745740	31291.844412	59.764583
2288.430220	31173.510235	59.769588
2287.275210	31056.997127	59.774593
2287.033705	30934.906111	59.779597
2286.470060	30814.161767	59.784602
2285.938333	30692.444726	59.789607
2284.965126	30575.017877	59.794612
2284.510941	30460.726704	59.799617
2283.850308	30329.398029	59.804621
2282.927698	30216.248306	59.809626
2282.313448	30094.116068	59.814631
2281.828731	29985.517945	59.819636
2280.777919	29862.591999	59.824641
2280.038694	29746.364357	59.829645
2279.794561	29636.132869	59.834650
2278.985987	29508.590517	59.839655
2278.225793	29407.299826	59.844660
2277.183343	29287.859295	59.849665
2276.668860	29176.028800	59.854669
2276.032707	29076.430147	59.859674
2275.395404	28956.789713	59.864679
2274.683153	28858.211225	59.869684
2274.078063	28744.605384	59.874689
2273.489287	28631.152482	59.879693
2272.715382	28527.996550	59.884698
2272.351253	28410.634893	59.889703
2271.381940	28302.661377	59.894708
2270.843481	28194.387101	59.899713
2270.184491	28077.830909	59.904718
2270.038141	27976.683857	59.909722
2269.681996	27867.159459	59.914727
2268.640497	27746.849865	59.919732
2267.970216	27635.267705	59.924737
2267.545736	27511.849321	59.929742
2266.659928	27399.941764	59.934746
2266.081862	27281.238828	59.939751
2265.213565	27159.173497	59.944756
2264.773447	27050.146159	59.949761
2264.035082	26930.951122	59.954766
2262.714369	26824.903415	59.959770
2262.091140	26708.483041	59.964775
2261.626078	26611.266549	59.969780
2261.384064	26507.028910	59.974785
2260.740046	26388.422374	59.979790
2260.092065	26274.934724	59.984794
2259.749700	26160.687088	59.989799
2258.964740	26054.947789	59.994804
2258.014773	25931.718960	59.999809
2257.980390	25806.484249	60.004814
2256.954242	25701.259583	60.009818
2256.154899	25578.946812	60.014823
2255.221471	25471.177547	60.019828
2254.464253	25357.129463	60.024833
2254.040488	25252.854494	60.029838
2252.965201	25132.710997	60.034842
2252.407345	25026.553276	60.039847
2252.164248	24922.847117	60.044852
2251.333271	24811.329456	60.049857
2250.973661	24705.750163	60.054862
2249.865710	24594.395112	60.059866
2249.202833	24485.406095	60.064871
2248.795744	24371.760007	60.069876
2248.155341	24262.174011	60.074881
2246.810745	24153.395373	60.079886
2245.862030	24049.192111	60.084890
2245.834774	23940.300225	60.089895
2245.399327	23841.696385	60.094900
2244.592347	23738.656641	60.099905
2244.110048	23621.397987	60.104910
2243.422928	23521.808098	60.109914
2242.667754	23407.747204	60.114919
2242.009317	23299.447958	60.119924
2241.367756	23200.323312	60.124929
2240.724327	23091.077301	60.129934
2239.754550	22984.667362	60.134938
2239.539262	22870.040214	60.139943
2238.672806	22772.781063	60.144948
2237.865663	22671.578621	60.149953
2237.631053	22559.508691	60.154958
2236.564975	22463.237229	60.159962
2235.970868	22347.151053	60.164967
2235.406121	22245.697811	60.169972
2234.657130	22140.709894	60.174977
2234.579479	22030.608660	60.179982
2233.511025	21920.557412	60.184986
2233.164048	21820.441754	60.189991
2232.292250	21705.416084	60.194996
2231.405583	21597.460666	60.200001
2231.142311	21481.140389	60.205006
2230.356602	21382.664307	60.210010
2229.448316	21273.228541	60.215015
2229.201271	21160.183381	60.220020
2228.205704	21053.117957	60.225025
2227.477047	20939.884698	60.230030
2226.474886	20842.259757	60.235034
2225.998104	20735.031731	60.240039
2225.515247	20629.157071	60.245044
2224.503873	20533.687054	60.250049
2223.893930	20427.900194	60.255054
2222.641119	20329.105380	60.260058
2222.571102	20224.213906	60.265063
2221.801554	20129.171155	60.270068
2221.134139	20023.840852	60.275073
2220.517111	19923.466344	60.280078
2219.953596	19836.750929	60.285082
2219.095380	19732.917308	60.290087
2218.429315	19627.744150	60.295092
2217.723066	19536.661672	60.300097
2217.380035	19436.777491	60.305102
2216.226291	19341.152001	60.310106
2215.796123	19251.927077	60.315111
2215.146051	19151.045889	60.320116
2214.327221	19060.688655	60.325121
2213.983510	18957.557427	60.330126
2213.023711	18871.822059	60.335130
2212.147387	18756.696983	60.340135
2211.314135	18669.997319	60.345140
2210.596449	18584.144555	60.350145
2210.123749	18493.075180	60.355150
2209.321487	18411.903929	60.360154
2208.790959	18321.986614	60.365159
2208.241844	18245.660291	60.370164
2207.339337	18153.891729	60.375169
2206.925825	18067.967447	60.380174
2205.872245	17991.848674	60.385178
2205.163976	17898.809069	60.390183
2204.576087	17819.149868	60.395188
2203.772599	17740.929918	60.400193
2203.281065	17656.729720	60.405198
2202.343787	17581.982267	60.410202
2201.835046	17486.859206	60.415207
2200.728994	17409.572930	60.420212
2199.402862	17339.151142	60.425217
2199.516596	17259.725494	60.430222
2198.424557	17194.586047	60.435226
2197.773033	17132.606911	60.440231
2197.132473	17063.734942	60.445236
2196.436217	16992.222215	60.450241
2195.593059	16931.016292	60.455246
2194.889762	16863.380791	60.460250
2194.306992	16796.181723	60.465255
2193.534521	16733.459777	60.470260
2192.817461	16671.876042	60.475265
2192.637029	16604.295997	60.480270
2191.893657	16547.044641	60.485274
2191.328754	16483.311389	60.490279
2190.500162	16417.804335	60.495284
2189.714931	16351.207495	60.500289
2189.218688	16280.199391	60.505294
2188.654126	16218.878893	60.510298
2187.777966	16146.694082	60.515303
2187.143875	16084.918151	60.520308
2186.488853	16022.882092	60.525313
2186.132596	15950.029196	60.530318
2185.280743	15906.934071	60.535322
2184.318234	15840.127783	60.540327
2184.015941	15774.893589	60.545332
2182.997865	15715.869838	60.550337
2182.765549	15648.963147	60.555342
2181.792193	15592.298066	60.560346
2181.010778	15520.226202	60.565351
2180.497310	15466.450895	60.570356
2179.839932	15406.890856	60.575361
2179.243244	15341.675518	60.580366
2178.541918	15291.801685	60.585370
2177.894036	15223.613389	60.590375
2177.327056	15163.989770	60.595380
2176.653430	15107.049094	60.600385
2176.024985	15044.473237	60.605390
2175.133876	14982.652114	60.610394
2174.754912	14922.791762	60.615399
2174.381823	14860.670735	60.620404
2173.394029	14799.969906	60.625409
2172.886199	14735.664666	60.630414
2172.336277	14678.799124	60.635418
2171.603783	14613.295390	60.640423
2171.053637	14549.407411	60.645428
2169.906129	14485.941062	60.650433
2169.393242	14425.996366	60.655438
2168.748265	14373.696224	60.660442
2167.894045	14304.853248	60.665447
2167.598517	14242.288276	60.670452
2166.596927	14192.026628	60.675457
2166.058999	14120.499169	60.680462
2165.051239	14069.238641	60.685466
2164.448169	14019.440332	60.690471
2163.929904	13955.528652	60.695476
2163.117928	13906.978463	60.700481
2162.855756	13845.855214	60.705486
2161.979661	13789.073798	60.710490
2161.429196	13731.302972	60.715495
2160.765914	13679.912051	60.720500
2159.763431	13627.744944	60.725505
2159.382751	13572.320710	60.730510
2158.604641	13516.525333	60.735514
2158.156186	13460.025883	60.740519
2157.642343	13407.251278	60.745524
2156.601047	13345.362417	60.750529
2155.979226	13292.857896	60.755534
2155.130416	13238.982840	60.760538
2154.770720	13174.849543	60.765543
2154.471941	13119.028842	60.770548
2153.499880	13070.440552	60.775553
2153.240985	13007.289333	60.780558
2152.402371	12948.995352	60.785562
2151.639934	12885.527779	60.790567
2151.016390	12824.572827	60.795572
2150.001196	12775.239060	60.800577
2149.668052	12707.073688	60.805582
2148.863882	12651.413695	60.810586
2148.308225	12599.713838	60.815591
2147.733048	12545.217515	60.820596
2147.059770	12490.033420	60.825601
2146.905794	12424.625895	60.830606
2145.887052	12369.698801	60.835610
2145.200998	12303.693834	60.840615
2144.501699	12245.457530	60.845620
2143.674119	12188.802915	60.850625
2143.293371	12125.364648	60.855630
2142.345292	12072.262517	60.860634
2141.748191	12009.092392	60.865639
2141.297217	11955.913521	60.870644
2140.403135	11904.215275	60.875649
2140.011868	11841.996546	60.880654
2138.869773	11779.464053	60.885658
2138.303047	11723.219910	60.890663
2137.494088	11667.208572	60.895668
2136.972090	11615.556625	60.900673
2136.374063	11559.321559	60.905678
2135.214855	11505.516349	60.910682
2135.142611	11453.149668	60.915687
2134.800488	11395.803309	60.920692
2133.933172	11349.166165	60.925697
2133.382853	11284.518275	60.930702
2132.579547	11226.289169	60.935706
2131.982305	11164.923519	60.940711
2131.550673	11107.568200	60.945716
2130.307170	11045.812674	60.950721
2129.917519	10989.436494	60.955726
2129.215685	10940.237951	60.960730
2128.626035	10878.958975	60.965735
2127.681067	10820.295781	60.970740
2127.118949	10769.429129	60.975745
2126.409377	10700.976260	60.980750
2125.845637	10650.225594	60.985754
2124.898312	10589.816226	60.990759
2124.789394	10538.559959	60.995764
2123.694051	10485.706212	61.000769
2123.534806	10429.131412	61.005774
2122.541301	10375.506987	61.010778
2121.578112	10313.587808	61.015783
2121.452749	10264.998929	61.020788
2120.636339	10211.335279	61.025793
2119.980389	10145.112705	61.030798
2119.066713	10099.479242	61.035802
2118.231899	10043.937655	61.040807
2117.925155	9986.290028	61.045812
2116.985086	9938.419697	61.050817
2116.395092	9868.584877	61.055822
2115.995943	9835.229718	61.060826
2115.347659	9774.574756	61.065831
2114.739862	9712.947812	61.070836
2113.907966	9665.560597	61.075841
2113.510468	9602.441494	61.080846
2112.760103	9557.769022	61.085850
2112.119810	9501.290783	61.090855
2111.836762	9435.029446	61.095860
2110.856763	9380.951016	61.100865
2110.467458	9321.533103	61.105870
2109.258888	9266.475174	61.110874
2108.862583	9210.468075	61.115879
2108.001843	9152.610101	61.120884
2107.042825	9103.026673	61.125889
2106.635907	9057.037755	61.130894
2106.259463	8996.195455	61.135898
2105.361417	8942.204002	61.140903
2105.196699	8883.027326	61.145908
2104.195503	8827.218216	61.150913
2103.805845	8763.018908	61.155918
2102.936511	8719.435434	61.160922
2102.153393	8659.644977	61.165927
2101.711433	8598.069742	61.170932
2100.738509	8550.757310	61.175937
2100.190138	8487.693633	61.180942
2099.531139	8438.836578	61.185946
2099.035024	8379.138669	61.190951
2098.182697	8323.982747	61.195956
2097.351184	8266.508400	61.200961
2096.719098	8203.429349	61.205966
2096.386609	8152.891808	61.210970
2095.823542	8096.015090	61.215975
2095.038575	8036.325202	61.220980
2094.127271	7986.814453	61.225985
2093.550126	7927.976410	61.230990
2092.765372	7871.702343	61.235994
2092.097091	7818.018147	61.240999
2091.560226	7759.574274	61.246004
2091.010752	7718.132943	61.251009
2090.576694	7656.930378	61.256014
2089.898606	7600.237788	61.261018
2089.006409	7537.433302	61.266023
2088.501785	7489.543155	61.271028
2087.311617	7436.288326	61.276033
2086.881984	7380.694503	61.281038
2086.243589	7326.993410	61.286042
2085.588281	7263.238835	61.291047
2085.130369	7219.106492	61.296052
2084.155643	7160.020972	61.301057
2083.959818	7108.367888	61.306062
2082.931035	7048.104966	61.311066
2082.276125	6994.771114	61.316071
2081.610761	6937.781727	61.321076
2080.736935	6888.310607	61.326081
2080.459843	6823.225489	61.331086
2079.641812	6769.159729	61.336090
2078.848773	6726.263621	61.341095
2078.137710	6673.406411	61.346100
2077.448714	6626.925369	61.351105
2076.982773	6568.736695	61.356110
2076.317510	6518.423114	61.361114
2075.925530	6467.190261	61.366119
2075.238164	6402.637456	61.371124
2074.352944	6352.356491	61.376129
2073.508760	6301.109903	61.381134
2072.878481	6252.622617	61.386138
2072.598228	6194.815003	61.391143
2071.991252	6140.231945	61.396148
2070.815691	6094.183954	61.401153
2070.399879	6033.046066	61.406158
2069.762164	5983.909331	61.411162
2068.707826	5933.733636	61.416167
2068.848058	5875.011820	61.421172
2068.018636	5820.047766	61.426177
2067.534456	5763.120815	61.431182
2066.623010	5711.255844	61.436186
2066.065473	5658.126972	61.441191
2065.677453	5598.990309	61.446196
2064.595107	5542.870097	61.451201
2064.180661	5480.131755	61.456206
2063.386074	5428.000539	61.461210
2061.881641	5379.891281	61.466215
2061.506309	5315.702520	61.471220
2060.641209	5269.505891	61.476225
2060.569234	5217.810877	61.481230
2059.642148	5173.762062	61.486234
2058.916824	5124.432113	61.491239
2058.460720	5064.930023	61.496244
2057.620843	5013.303841	61.501249
2057.418135	4967.844500	61.506254
2056.632962	4908.736477	61.511258
2055.567750	4858.940347	61.516263
2054.976225	4801.505317	61.521268
2054.053366	4757.892837	61.526273
2053.735830	4700.283381	61.531278
2053.178623	4647.770613	61.536282
2052.226716	4600.456810	61.541287
2051.628698	4546.933472	61.546292
2051.054024	4501.887329	61.551297
2050.835909	4448.115352	61.556302
2050.264386	4393.810179	61.561306
2049.543625	4346.121204	61.566311
2049.401681	4285.743893	61.571316
2048.221608	4230.222277	61.576321
2047.346516	4163.431724	61.581326
2046.668769	4117.204828	61.586330
2045.781174	4062.008858	61.591335
2045.213943	4003.572083	61.596340
2044.047190	3956.750207	61.601345
2043.373403	3908.102213	61.606350
2043.331365	3867.645365	61.611354
2042.440434	3817.288910	61.616359
2042.218827	3766.763647	61.621364
2041.503862	3714.996358	61.626369
2040.727461	3661.434667	61.631374
2039.964114	3614.673514	61.636378
2039.384345	3559.853831	61.641383
2038.830355	3505.452374	61.646388
2037.741448	3453.544604	61.651393
2037.332096	3403.212116	61.656398
2036.542948	3351.522666	61.661402
2035.767779	3307.008515	61.666407
2035.444199	3244.941738	61.671412
2034.630527	3206.804975	61.676417
2034.083920	3146.943398	61.681422
2033.287051	3104.790480	61.686426
2032.517783	3051.115939	61.691431
2032.225221	2997.953814	61.696436
2031.551613	2951.693301	61.701441
2031.113038	2897.332627	61.706446
2029.865913	2845.281006	61.711450
2029.534197	2801.787582	61.716455
2028.404213	2747.946006	61.721460
2027.567486	2705.075355	61.726465
2027.165724	2644.858496	61.731470
2026.319526	2598.393251	61.736474
2025.559062	2555.326783	61.741479
2025.133926	2508.248926	61.746484
2024.286074	2466.811523	61.751489
2024.113790	2417.218563	61.756494
2023.449609	2367.561460	61.761498
2022.261767	2319.146840	61.766503
2021.753019	2277.648774	61.771508
2021.079302	2235.943748	61.776513
2020.247702	2184.308820	61.781518
2019.506371	2146.424388	61.786522
2019.193233	2095.965134	61.791527
2019.012074	2045.673746	61.796532
2017.932613	2005.159888	61.801537
2017.548273	1963.955608	61.806542
2016.964324	1918.377594	61.811546
2016.158763	1869.296558	61.816551
2015.657060	1816.746607	61.821556
2014.252840	1772.183339	61.826561
2013.708620	1721.182143	61.831566
2013.322381	1677.489956	61.836570
2012.367757	1638.711598	61.841575
2012.058039	1586.973577	61.846580
2011.340240	1542.198809	61.851585
2010.617781	1494.745746	61.856590
2009.993769	1452.766261	61.861594
2009.306646	1410.375692	61.866599
2008.708873	1360.796869	61.871604
2007.856332	1326.059112	61.876609
2007.063948	1272.928311	61.881614
2006.417599	1234.890096	61.886618
2005.442333	1192.142813	61.891623
2005.238355	1148.064862	61.896628
2004.176023	1101.016140	61.901633
2003.860076	1064.967407	61.906638
2003.238760	1033.093325	61.911642
2002.354801	992.989584	61.916647
2002.281364	946.998251	61.921652
2001.632926	911.667941	61.926657
2001.208614	855.389104	61.931662
1999.978250	816.761008	61.936666
1999.017794	773.868652	61.941671
1998.387119	722.437865	61.946676
1997.710013	689.483761	61.951681
1996.980864	644.651534	61.956686
1996.662664	602.130579	61.961690
1995.879393	576.269716	61.966695
1995.194586	518.123375	61.971700
1994.366578	493.381082	61.976705
1993.545083	449.152971	61.981710
1993.271137	408.650340	61.986714
1992.343446	380.096001	61.991719
1991.588602	338.971219	61.996724
1990.681443	302.933798	62.001729
1990.564404	267.786017	62.006734
1989.307732	230.638975	62.011738
1988.755489	213.586983	62.016743
1988.154762	170.412922	62.021748
1987.063634	146.167757	62.026753
1986.541877	124.418567	62.031758
1985.819708	96.535360	62.036762
1985.075853	63.425849	62.041767
1984.884852	37.407734	62.046772
1983.507043	21.651731	62.051777
1982.818648	-9.192336	62.056782
1980.277325	20.341576	62.061786
1978.740807	39.071059	62.066791
1978.620455	36.529543	62.071796
1978.604852	43.630907	62.076801
1978.232035	31.355734	62.081806
1977.696858	38.510449	62.086810
1977.111358	48.128150	62.091815
1976.462244	39.999810	62.096820
1975.834821	39.803232	62.101825
1974.784029	45.480686	62.106830
1974.242313	40.725419	62.111834
1973.571484	49.138819	62.116839
1973.387763	45.828963	62.121844
1972.445671	45.515298	62.126849
1971.750560	51.756361	62.131854
1970.662232	50.261839	62.136858
1970.416133	56.527539	62.141863
1970.200458	51.909120	62.146868
1969.707684	52.825913	62.151873
1968.701790	57.074301	62.156878
1968.159557	50.419325	62.161882
1966.979528	53.434786	62.166887
1966.200125	40.304722	62.171892
1965.724722	54.375390	62.176897
1965.695099	55.552811	62.181902
1965.527977	47.923443	62.186906
1963.882299	62.718496	62.191911
1963.597016	46.540333	62.196916
1963.385677	55.781417	62.201921
1962.252111	49.569425	62.206926
1961.409339	48.961284	62.211930
1960.916810	62.154265	62.216935
1960.437041	49.548443	62.221940
1959.820203	62.584274	62.226945
1959.009613	59.438884	62.231950
1957.737953	56.692485	62.236954
1956.971588	57.905939	62.241959
1956.766770	49.393712	62.246964
1955.828209	55.015265	62.251969
1955.201479	46.193123	62.256974
1955.093791	48.742528	62.261978
1954.375003	60.191650	62.266983
1953.816506	45.863710	62.271988
1953.048271	51.390997	62.276993
1952.437464	49.585064	62.281998
1951.802260	52.366018	62.287002
1951.068892	59.852266	62.292007
1950.783292	53.201547	62.297012
1949.603968	60.771187	62.302017
1949.258384	51.063351	62.307022
1948.396571	49.480350	62.312026
1947.510115	55.894669	62.317031
1947.070410	49.944104	62.322036
1946.334008	60.033662	62.327041
1945.811063	50.408666	62.332046
1945.316685	54.014576	62.337050
1944.312860	60.663308	62.342055
1943.736656	49.968255	62.347060
1942.842209	55.789886	62.352065
1942.163944	50.821541	62.357070
1942.153338	52.335169	62.362074
1940.748597	46.378776	62.367079
1940.769440	46.162093	62.372084
1939.791175	49.004891	62.377089
1939.111154	46.915549	62.382094
1938.727433	47.000564	62.387098
1937.717168	51.010106	62.392103
1936.888334	53.221051	62.397108
1936.479675	52.533520	62.402113
1936.012715	58.411493	62.407118
1935.408984	52.841475	62.412122
1934.763618	51.138952	62.417127
1934.000940	49.254006	62.422132
1933.518418	52.486851	62.427137
1932.681489	51.792455	62.432142
1932.138235	48.906853	62.437146
1931.322090	53.756313	62.442151
1930.873691	48.022756	62.447156
1929.970744	48.182778	62.452161
1929.198412	48.263222	62.457166
1929.147228	46.871145	62.462170
1927.924951	54.290639	62.467175
1927.333973	43.219583	62.472180
1926.894530	49.152448	62.477185
1926.713972	60.036227	62.482190
1925.603442	48.443413	62.487194
1924.181226	55.816983	62.492199
1923.759510	60.000968	62.497204
1923.551303	58.621541	62.502209
1922.968967	62.285525	62.507214
1922.378494	55.446184	62.512218
1921.022289	58.467715	62.517223
1920.921877	54.388507	62.522228
1920.138100	57.598286	62.527233
1919.205647	51.981483	62.532238
1918.816020	56.914290	62.537242
1918.033912	54.738997	62.542247
1917.617700	51.818244	62.547252
1916.867349	51.974268	62.552257
1916.295274	50.229607	62.557262
1916.076855	56.816216	62.562266
1914.814710	57.558721	62.567271
1914.977086	55.688021	62.572276
1914.005736	54.321520	62.577281
1912.529633	54.357762	62.582286
1911.786101	46.840823	62.587290
1911.477075	52.254820	62.592295
1911.492591	51.173425	62.597300
1910.161506	52.589671	62.602305
1909.516191	54.297928	62.607310
1909.229411	52.605116	62.612314
1908.576172	51.775488	62.617319
1907.455716	51.266962	62.622324
1906.755989	54.319870	62.627329
1906.035324	53.818343	62.632334
1905.608819	45.072876	62.637338
1904.989791	52.849024	62.642343
1904.803674	43.693765	62.647348
1903.918836	43.403080	62.652353
1903.276076	51.256705	62.657358
1902.788587	45.768252	62.662362
1901.099514	50.523899	62.667367
1901.039636	47.242202	62.672372
1900.239983	48.850157	62.677377
1899.337481	45.653797	62.682382
1899.350388	43.390659	62.687386
1898.471013	50.745179	62.692391
1898.159142	49.994122	62.697396
1897.537851	48.748521	62.702401
1896.686227	50.034986	62.707406
1896.049273	41.531175	62.712410
1895.345715	43.866740	62.717415
1894.330482	39.071707	62.722420
1893.484799	44.069109	62.727425
1892.811898	41.270034	62.732430
1892.935250	41.395799	62.737434
1891.528715	47.048075	62.742439
1890.961558	40.111208	62.747444
1890.134418	42.091352	62.752449
1889.666778	51.517584	62.757454
1889.465821	50.122710	62.762458
1888.822468	52.159831	62.767463
1888.529795	43.967765	62.772468
1888.017248	47.812828	62.777473
1886.701258	46.777650	62.782478
1886.192636	45.329625	62.787482
1884.940232	47.986839	62.792487
1884.519049	40.627518	62.797492
1883.962618	43.454998	62.802497
1883.527690	47.752552	62.807502
1883.070952	47.070883	62.812506
1882.078612	54.444732	62.817511
1881.533861	51.305588	62.822516
1880.122631	48.280337	62.827521
1879.488131	44.873929	62.832526
1879.731061	41.203339	62.837530
1878.730074	53.987524	62.842535
1878.091116	43.442168	62.847540
1877.684309	39.985360	62.852545
1877.216959	48.251852	62.857550
1876.399638	32.092511	62.862554
1874.980563	44.650990	62.867559
1874.241421	46.028343	62.872564
1874.181442	50.307146	62.877569
1873.611491	46.715228	62.882574
1873.181902	41.787642	62.887578
1871.973854	41.740538	62.892583
1871.688261	46.862774	62.897588
1871.058930	45.123572	62.902593
1870.573756	40.621136	62.907598
1869.288577	37.456700	62.912602
1868.296480	47.401320	62.917607
1867.760783	42.647407	62.922612
1867.124866	48.360870	62.927617
1866.546143	47.223644	62.932622
1865.953719	43.170592	62.937626
1865.202240	61.152410	62.942631
1865.621089	52.456527	62.947636
1864.758579	47.550111	62.952641
1864.326316	52.443635	62.957646
1863.393878	47.554314	62.962650
1862.221069	53.848689	62.967655
1861.449552	49.688123	62.972660
1860.965446	46.594658	62.977665
1860.299143	53.816812	62.982670
1860.018852	44.266372	62.987674
1858.486395	52.458911	62.992679
1857.647046	40.389881	62.997684
1857.145310	48.266746	63.002689
1857.084259	59.390983	63.007694
1856.568431	47.367648	63.012698
1855.505786	58.429564	63.017703
1855.262888	49.364151	63.022708
1854.542174	52.777086	63.027713
1853.732598	52.935357	63.032718
1853.609578	51.390578	63.037722
1852.068654	53.078386	63.042727
1851.118501	53.912392	63.047732
1850.563838	50.334045	63.052737
1850.095068	56.794937	63.057742
1849.785583	53.663702	63.062746
1849.114690	54.589268	63.067751
1848.750574	48.764728	63.072756
1848.424300	53.662224	63.077761
1847.034465	52.844155	63.082766
1846.424278	49.639635	63.087770
1845.457216	54.300589	63.092775
1844.959079	46.531691	63.097780
1844.728842	49.151401	63.102785
1844.239058	52.485751	63.107790
1843.767855	46.354678	63.112794
1842.614070	45.568460	63.117799
1842.008485	42.138559	63.122804
1841.210165	52.355151	63.127809
1840.372714	48.780977	63.132814
1840.013984	43.528259	63.137818
1838.589486	54.441299	63.142823
1837.840145	49.149621	63.147828
1838.089302	46.203461	63.152833
1837.137370	49.942127	63.157838
1836.933441	47.359655	63.162842
1835.737775	50.060066	63.167847
1835.254238	47.721607	63.172852
1834.841971	52.297118	63.177857
1833.639825	64.006959	63.182862
1832.913958	53.841197	63.187866
1832.255057	57.898402	63.192871
1831.703904	48.341806	63.197876
1830.794962	52.681384	63.202881
1830.365433	44.805624	63.207886
1830.555556	43.443314	63.212890
1829.429112	51.832832	63.217895
1829.410141	38.498503	63.222900
1828.315571	47.223999	63.227905
1827.139075	43.504554	63.232910
1826.841049	36.300613	63.237914
1826.217290	44.872930	63.242919
1825.622834	41.468758	63.247924
1824.287002	44.669184	63.252929
1823.415655	47.911322	63.257934
1822.972776	47.078478	63.262938
1822.278765	46.982518	63.267943
1822.029362	47.154687	63.272948
1821.510318	42.257017	63.277953
1820.958717	60.392128	63.282958
1820.573739	48.247734	63.287962
1819.793071	57.589767	63.292967
1818.936803	48.903236	63.297972
1818.218193	47.483646	63.302977
1817.405560	49.323165	63.307982
1817.153694	40.594415	63.312986
1815.765143	42.368264	63.317991
1815.073342	45.246540	63.322996
1814.190058	45.029023	63.328001
1813.654712	48.281568	63.333006
1813.245358	39.689891	63.338010
1812.736170	51.201828	63.343015
1812.526331	43.758597	63.348020
1812.477229	45.988516	63.353025
1811.322402	47.924080	63.358030
1810.761387	47.122896	63.363034
1810.066571	42.620811	63.368039
1808.469949	43.837391	63.373044
1807.470635	42.507274	63.378049
1806.721548	46.232159	63.383054
1807.147132	37.859592	63.388058
1806.115230	43.503838	63.393063
1805.495084	47.696907	63.398068
1805.275079	44.137492	63.403073
1804.646564	44.998972	63.408078
1803.850702	41.493478	63.413082
1802.587345	54.663201	63.418087
1801.981198	45.336276	63.423092
1801.344609	45.705344	63.428097
1800.944916	50.305940	63.433102
1800.750899	39.491460	63.438106
1799.937677	51.146200	63.443111
1798.997542	41.185266	63.448116
1798.127243	43.484240	63.453121
1797.117989	47.140749	63.458126
1797.038156	38.482434	63.463130
1796.621225	51.888638	63.468135
1795.856137	49.003511	63.473140
1794.628347	35.608389	63.478145
1793.791141	51.613892	63.483150
1793.764669	57.610706	63.488154
1793.009718	52.209474	63.493159
1792.477289	43.845294	63.498164
1792.331417	42.493104	63.503169
1790.920344	46.342699	63.508174
1790.554082	45.034927	63.513178
1789.603289	53.417292	63.518183
1788.963223	45.709001	63.523188
1788.652837	45.958314	63.528193
1787.714862	48.583461	63.533198
1786.761247	37.878423	63.538202
1785.850713	44.782378	63.543207
1785.203496	34.864095	63.548212
1785.065363	44.351966	63.553217
1784.045673	44.987494	63.558222
1783.841503	40.051351	63.563226
1783.048759	47.103701	63.568231
1782.906605	36.050231	63.573236
1782.391033	42.921741	63.578241
1780.775347	40.469902	63.583246
1780.076179	38.915550	63.588250
1779.470814	47.076976	63.593255
1779.482609	43.843020	63.598260
1779.044198	45.204455	63.603265
1778.317194	52.699488	63.608270
1777.546334	37.635073	63.613274
1776.562559	45.505995	63.618279
1775.714281	36.004203	63.623284
1775.069412	38.009620	63.628289
1774.112867	44.080301	63.633294
1773.969783	44.220467	63.638298
1773.113999	45.866462	63.643303
1772.451522	36.904435	63.648308
1772.181568	33.928678	63.653313
1771.600956	44.081573	63.658318
1770.206047	40.135446	63.663322
1769.484769	46.336788	63.668327
1769.186691	46.725700	63.673332
1768.874123	40.578946	63.678337
1768.057957	48.001211	63.683342
1767.781368	40.872157	63.688346
1766.546040	49.279127	63.693351
1765.697685	43.275753	63.698356
1765.237138	39.317781	63.703361
1764.658014	46.257400	63.708366
1764.306649	41.419861	63.713370
1763.217343	38.005635	63.718375
1762.663603	36.499032	63.723380
1761.912982	36.362242	63.728385
1761.262189	36.775189	63.733390
1760.883843	37.451377	63.738394
1760.193475	41.638699	63.743399
1759.075067	35.571803	63.748404
1758.531911	41.188086	63.753409
1757.988679	43.328478	63.758414
1757.346539	36.365785	63.763418
1757.165433	38.064101	63.768423
1756.337877	49.837736	63.773428
1755.230677	40.656158	63.778433
1754.253596	48.174242	63.783438
1754.084047	42.664570	63.788442
1753.258186	51.244630	63.793447
1753.082708	43.776186	63.798452
1752.675073	48.110521	63.803457
1751.168922	44.198827	63.808462
1750.376911	37.692023	63.813466
1749.872460	47.919516	63.818471
1749.513990	39.392561	63.823476
1749.507346	38.594027	63.828481
1748.038717	40.964595	63.833486
1747.565515	34.077600	63.838490
1746.809909	41.648179	63.843495
1746.125843	37.224001	63.848500
1745.639602	36.907378	63.853505
1745.149139	41.375090	63.858510
1744.186840	41.144263	63.863514
1743.411830	45.447513	63.868519
1743.369868	37.137973	63.873524
1742.294513	40.474629	63.878529
1741.181023	40.385326	63.883534
1740.816188	39.237570	63.888538
1739.620050	46.198293	63.893543
1739.261839	40.561042	63.898548
1739.059809	44.694415	63.903553
1738.509057	41.628158	63.908558
1738.107845	42.436149	63.913562
1736.912176	49.127989	63.918567
1736.163808	43.353819	63.923572
1736.065170	45.433535	63.928577
1734.844535	47.556420	63.933582
1733.991346	43.516429	63.938586
1733.236824	47.760915	63.943591
1732.605969	46.362242	63.948596
1732.241262	39.625229	63.953601
1731.977488	45.728162	63.958606
1731.717602	42.890810	63.963610
1729.974637	42.293451	63.968615
1729.382816	46.713379	63.973620
1729.164984	41.869574	63.978625
1728.530785	42.822821	63.983630
1727.992115	39.697660	63.988634
1726.710334	46.305160	63.993639
1725.849376	43.192908	63.998644
1725.454495	37.379179	64.003649
1725.113256	45.140953	64.008654
1724.733868	43.278482	64.013658
1723.825880	41.922099	64.018663
1723.019822	41.626649	64.023668
1722.296613	31.078386	64.028673
1721.727558	48.058352	64.033678
1721.586658	42.841005	64.038682
1720.958448	40.028784	64.043687
1719.490964	38.537224	64.048692
1719.028863	41.498569	64.053697
1718.322527	47.922744	64.058702
1718.074310	38.547228	64.063706
1717.414241	37.211186	64.068711
1715.982516	37.609348	64.073716
1715.435061	39.686520	64.078721
1714.765916	45.646061	64.083726
1714.803421	40.707254	64.088730
1714.349500	46.543920	64.093735
1713.192854	41.689447	64.098740
1712.184872	45.848230	64.103745
1711.273929	44.259074	64.108750
1711.024020	37.574262	64.113754
1710.477538	40.428472	64.118759
1709.900915	37.438880	64.123764
1709.650669	32.458528	64.128769
1708.495471	41.876089	64.133774
1708.230023	40.099514	64.138778
1707.401630	44.126125	64.143783
1706.469515	37.550150	64.148788
1705.737387	34.296655	64.153793
1704.773109	38.556901	64.158798
1704.576707	37.591108	64.163802
1703.909121	45.740289	64.168807
1703.461363	42.562470	64.173812
1703.463215	45.839545	64.178817
1701.754111	43.916063	64.183822
1701.083266	36.198458	64.188826
1700.719408	39.170229	64.193831
1700.114362	39.690220	64.198836
1699.103887	39.953940	64.203841
1698.295301	44.924885	64.208846
1697.749527	41.536480	64.213850
1697.153229	38.827745	64.218855
1696.756769	37.276080	64.223860
1696.635514	37.696711	64.228865
1695.322845	47.282137	64.233870
1694.683083	33.094099	64.238874
1694.031271	50.387818	64.243879
1693.422030	42.936368	64.248884
1693.175076	34.465341	64.253889
1691.851678	45.073741	64.258894
1691.309516	33.718486	64.263898
1690.811264	40.522299	64.268903
1690.413206	38.132128	64.273908
1689.611738	33.167549	64.278913
1688.344068	48.838171	64.283918
1688.111688	42.783885	64.288922
1687.179517	42.062408	64.293927
1687.125964	40.079452	64.298932
1686.034907	38.191137	64.303937
1684.812625	39.673683	64.308942
1684.486093	37.278379	64.313946
1683.896760	38.119748	64.318951
1683.319095	45.661857	64.323956
1683.123748	34.705923	64.328961
1682.680747	47.567126	64.333966
1681.886556	35.993693	64.338970
1680.871197	39.706129	64.343975
1680.606688	42.960493	64.348980
1679.404291	39.258152	64.353985
1678.060535	42.535751	64.358990
1677.534846	34.902650	64.363994
1677.099433	36.989863	64.368999
1676.461868	41.255390	64.374004
1676.708229	27.515707	64.379009
1675.827560	37.556132	64.384014
1675.465201	41.582339	64.389018
1674.463217	39.721019	64.394023
1673.400460	42.554237	64.399028
1672.929194	41.565219	64.404033
1672.160969	48.368261	64.409038
1671.255432	40.822261	64.414042
1670.926602	45.638881	64.419047
1670.069187	43.392839	64.424052
1669.902215	34.441570	64.429057
1669.382361	38.604063	64.434062
1668.282268	43.244383	64.439066
1667.770100	44.259646	64.444071
1667.006425	41.416142	64.449076
1666.348680	36.539469	64.454081
1665.184604	46.701420	64.459086
1664.809755	42.225922	64.464090
1663.798395	39.125605	64.469095
1663.469824	40.290233	64.474100
1663.074091	40.638233	64.479105
1662.570940	47.734586	64.484110
1662.218941	37.520296	64.489114
1661.096061	32.652168	64.494119
1660.419585	43.181844	64.499124
1659.744229	35.278712	64.504129
1658.833602	39.331635	64.509134
1658.072284	37.215988	64.514138
1657.492411	43.790623	64.519143
1657.245308	45.423264	64.524148
1657.248051	34.957625	64.529153
1655.831761	41.855378	64.534158
1655.291602	35.129849	64.539162
1654.472690	43.974764	64.544167
1653.737877	47.414209	64.549172
1652.844222	42.727898	64.554177
1651.761542	40.690137	64.559182
1651.760554	38.955545	64.564186
1650.898215	38.478298	64.569191
1650.184717	33.799845	64.574196
1650.286230	30.263977	64.579201
1649.066603	43.880150	64.584206
1648.227513	39.870132	64.589210
1647.583730	39.552847	64.594215
1647.117390	43.944596	64.599220
1646.924457	32.801159	64.604225
1646.472631	38.239192	64.609230
1645.128263	44.170209	64.614234
1644.359321	37.185818	64.619239
1643.777144	45.743919	64.624244
1643.455797	41.905031	64.629249
1642.286152	37.981973	64.634254
1641.162682	36.770632	64.639258
1640.776222	36.474443	64.644263
1640.371501	39.926478	64.649268
1640.298467	35.312105	64.654273
1639.706725	36.466903	64.659278
1639.017205	38.604312	64.664282
1637.677116	33.817568	64.669287
1636.890669	38.623288	64.674292
1636.932953	39.283555	64.679297
1635.868597	45.964781	64.684302
1635.138541	41.017199	64.689306
1634.915609	44.102221	64.694311
1633.975113	42.856412	64.699316
1633.849872	32.753715	64.704321
1632.493413	48.084286	64.709326
1631.499656	33.710931	64.714330
1631.297341	39.432702	64.719335
1630.559365	33.035490	64.724340
1630.547823	35.174113	64.729345
1629.229417	40.988983	64.734350
1628.360266	41.470891	64.739354
1627.764257	39.737863	64.744359
1627.695421	43.893046	64.749364
1627.133133	37.496952	64.754369
1625.723399	42.534855	64.759374
1625.268510	35.017538	64.764378
1624.749467	35.038499	64.769383
1624.398760	50.646944	64.774388
1623.369587	47.236669	64.779393
1622.358316	54.037100	64.784398
1622.232290	48.403547	64.789402
1621.522121	48.484846	64.794407
1620.854169	52.617428	64.799412
1619.824260	46.104389	64.804417
1619.086873	52.423364	64.809422
1618.565224	45.485469	64.814426
1618.077028	39.129194	64.819431
1617.648699	45.026216	64.824436
1617.228657	38.629465	64.829441
1615.884330	45.226372	64.834446
1615.471068	43.210636	64.839450
1615.010260	44.800511	64.844455
1614.180859	45.866514	64.849460
1613.324126	38.031533	64.854465
1612.433772	40.228575	64.859470
1612.393118	40.913692	64.864474
1611.814491	41.450091	64.869479
1610.598015	41.415938	64.874484
1610.032918	35.460836	64.879489
1609.251523	46.439897	64.884494
1608.973759	33.895912	64.889498
1608.678109	42.297221	64.894503
1607.485157	42.685340	64.899508
1607.018766	33.336128	64.904513
1606.141534	37.285058	64.909518
1605.806084	32.661913	64.914522
1604.720649	33.484770	64.919527
1603.634240	37.002938	64.924532
1602.890244	32.352607	64.929537
1602.693574	44.304846	64.934542
1602.196773	31.402049	64.939546
1601.853257	43.490728	64.944551
1601.136096	36.845233	64.949556
1600.773656	36.837424	64.954561
1599.594539	35.122875	64.959566
1599.084221	28.691450	64.964570
1598.772893	42.272578	64.969575
1597.790551	52.137399	64.974580
1597.111712	37.603981	64.979585
1596.340409	42.089366	64.984590
1595.902689	40.684502	64.989594
1594.686138	40.178281	64.994599
1594.211435	43.230996	64.999604
1593.889052	39.804772	65.004609
1592.600683	39.118219	65.009614
1592.452581	35.496389	65.014618
1591.659323	43.137760	65.019623
1590.453301	33.277259	65.024628
1590.205264	29.597931	65.029633
1589.949969	35.805191	65.034638
1589.661978	34.101164	65.039642
1588.232751	41.323235	65.044647
1587.109518	42.605703	65.049652
1586.729699	28.951083	65.054657
1586.090178	34.084148	65.059662
1586.024188	20.474903	65.064666
1585.844265	33.687367	65.069671
1584.803031	35.637482	65.074676
1584.207708	32.978727	65.079681
1583.281572	37.723099	65.084686
1582.346137	34.313374	65.089690
1581.501553	33.311677	65.094695
1580.690679	33.202593	65.099700
1580.635014	26.283252	65.104705
1579.891158	36.105673	65.109710
1578.977955	26.093231	65.114714
1578.400074	24.247378	65.119719
1577.460271	27.636648	65.124724
1577.043010	24.853480	65.129729
1576.790367	31.729728	65.134734
1575.866237	30.525734	65.139738
1574.781853	35.349686	65.144743
1574.040548	35.756436	65.149748
1573.681967	24.275855	65.154753
1573.360591	31.722392	65.159758
1573.045739	36.022300	65.164762
1572.001502	34.262571	65.169767
1571.108472	36.964923	65.174772
1570.937512	34.479456	65.179777
1569.992121	35.843987	65.184782
1568.926677	37.942715	65.189786
1568.616127	35.251411	65.194791
1567.987641	35.559911	65.199796
1567.353549	26.998850	65.204801
1566.634428	41.338941	65.209806
1565.680107	37.408264	65.214810
1565.130784	38.928031	65.219815
1564.722686	40.557833	65.224820
1564.303099	36.543538	65.229825
1562.873840	45.403706	65.234830
1562.296613	39.335823	65.239834
1561.705985	44.337768	65.244839
1561.276411	41.628544	65.249844
1560.812040	38.698313	65.254849
1560.584766	43.293484	65.259854
1559.534909	41.725763	65.264858
1558.887230	35.441397	65.269863
1558.134940	37.624292	65.274868
1557.684455	32.907950	65.279873
1556.102535	40.278916	65.284878
1555.414750	37.299293	65.289882
1555.146933	40.789872	65.294887
1554.693264	37.904387	65.299892
1554.654977	29.414644	65.304897
1553.126923	35.683413	65.309902
1552.925896	36.889769	65.314906
1552.359875	36.540636	65.319911
1551.457628	32.843409	65.324916
1550.565240	29.502506	65.329921
1549.737283	38.745270	65.334926
1549.146819	36.501722	65.339930
1548.740511	38.477782	65.344935
1548.402824	32.908885	65.349940
1547.872358	38.084077	65.354945
1546.740677	43.305717	65.359950
1545.974577	42.125602	65.364954
1545.630397	31.900920	65.369959
1545.000056	39.415732	65.374964
1543.936802	37.972670	65.379969
1542.943724	30.888512	65.384974
1542.592903	33.458207	65.389978
1542.233604	30.461841	65.394983
1541.676282	38.763462	65.399988
1541.502839	30.382504	65.404993
1540.158192	35.602303	65.409998
1539.676091	31.746730	65.415002
1538.937153	31.221544	65.420007
1537.679772	36.403909	65.425012
1537.525491	35.094221	65.430017
1536.507085	39.314020	65.435022
1536.277323	35.685250	65.440026
1535.915578	25.826327	65.445031
1535.226801	33.579284	65.450036
1534.601642	23.213232	65.455041
1534.182053	40.280485	65.460046
1532.966902	31.639275	65.465050
1531.899877	31.298918	65.470055
1531.295672	39.960257	65.475060
1531.077041	32.543043	65.480065
1530.234901	39.511103	65.485070
1529.565386	31.805545	65.490074
1529.047414	35.980355	65.495079
1527.738422	35.816009	65.500084
1527.940347	25.234989	65.505089
1527.439393	36.643661	65.510094
1526.302558	32.119785	65.515098
1525.394186	36.023925	65.520103
1524.998173	40.490086	65.525108
1524.546634	31.264264	65.530113
1523.480226	43.089437	65.535118
1522.383428	37.368235	65.540122
1522.126714	36.934592	65.545127
1521.806111	34.533552	65.550132
1521.722890	32.493315	65.555137
1520.446666	37.688777	65.560142
1519.505460	33.087213	65.565146
1519.121727	34.836000	65.570151
1518.542077	42.290035	65.575156
1518.260927	28.355661	65.580161
1516.841605	31.718461	65.585166
1516.476293	30.105038	65.590170
1515.873804	34.709557	65.595175
1514.448170	45.465737	65.600180
1513.960335	33.423097	65.605185
1513.243533	35.732550	65.610190
1512.958350	35.602976	65.615194
1512.540183	32.602084	65.620199
1511.896271	41.392189	65.625204
1511.740357	31.136872	65.630209
1510.614727	37.469403	65.635214
1509.845495	36.948616	65.640218
1509.540174	35.804510	65.645223
1508.523984	44.142827	65.650228
1507.497021	23.463257	65.655233
1507.001029	34.515041	65.660238
1506.299521	45.189130	65.665242
1506.226934	35.556231	65.670247
1505.295211	35.712568	65.675252
1504.708044	29.639295	65.680257
1503.602449	36.752705	65.685262
1503.505825	39.083905	65.690266
1502.795259	35.838202	65.695271
1501.401463	40.144753	65.700276
1501.167283	28.640128	65.705281
1500.287104	36.309010	65.710286
1500.116026	28.700119	65.715290
1499.502660	33.676746	65.720295
1498.246987	37.145747	65.725300
1497.977785	31.247387	65.730305
1497.037376	32.267672	65.735310
1496.627259	36.743746	65.740314
1495.990386	28.098312	65.745319
1495.076258	36.393502	65.750324
1494.218803	27.480308	65.755329
1494.018961	37.856174	65.760334
1493.428454	27.342100	65.765338
1493.189996	29.835330	65.770343
1491.683211	33.528486	65.775348
1491.174295	27.188415	65.780353
1490.770054	26.612662	65.785358
1490.173681	30.586954	65.790362
1489.300340	30.395421	65.795367
1488.480573	43.151366	65.800372
1488.356518	29.475492	65.805377
1487.522252	37.713201	65.810382
1486.749236	37.610678	65.815386
1486.050437	32.643570	65.820391
1485.398895	40.593045	65.825396
1485.171036	31.237373	65.830401
1484.253763	33.270891	65.835406
1483.231331	34.161934	65.840410
1482.707074	33.381733	65.845415
1481.954497	27.542424	65.850420
1481.182121	26.545755	65.855425
1480.572244	42.359185	65.860430
1479.702516	40.856569	65.865434
1479.646069	38.519263	65.870439
1479.225956	44.026083	65.875444
1478.176704	32.655041	65.880449
1477.580189	33.843434	65.885454
1476.776443	40.972683	65.890458
1476.455924	42.678287	65.895463
1475.267472	39.268865	65.900468
1474.846165	32.568815	65.905473
1474.398954	39.757431	65.910478
1473.845762	37.093060	65.915482
1472.750215	27.532232	65.920487
1471.739931	45.919475	65.925492
1471.246455	31.935005	65.930497
1471.024885	43.115081	65.935502
1470.461592	29.563728	65.940506
1469.163011	28.736462	65.945511
1467.897118	35.527591	65.950516
1467.959360	28.871487	65.955521
1467.473274	35.275343	65.960526
1467.143914	42.337216	65.965530
1466.874862	35.315068	65.970535
1465.618126	39.545671	65.975540
1465.087353	30.248558	65.980545
1464.268308	36.330079	65.985550
1463.516987	31.162369	65.990554
1462.625382	38.256132	65.995559
1461.700709	41.755722	66.000564
1461.882921	35.757998	66.005569
1460.892372	41.347847	66.010574
1460.657335	29.649962	66.015578
1459.699516	29.926821	66.020583
1458.834510	33.756839	66.025588
1458.386112	39.457174	66.030593
1457.889208	45.840783	66.035598
1456.535948	35.069649	66.040602
1455.778428	28.054930	66.045607
1455.483720	36.750135	66.050612
1455.375648	32.133483	66.055617
1454.904758	31.812288	66.060622
1454.351457	35.974596	66.065626
1453.282714	31.011606	66.070631
1452.064984	37.724630	66.075636
1451.242871	32.495226	66.080641
1450.769592	40.042367	66.085646
1450.147723	25.114796	66.090650
1449.838554	26.949899	66.095655
1449.169343	31.792409	66.100660
1448.421003	26.597353	66.105665
1447.069678	34.689495	66.110670
1446.370651	35.984644	66.115674
1446.320536	31.688847	66.120679
1445.322339	36.577406	66.125684
1445.578703	27.010974	66.130689
1444.950503	39.482297	66.135694
1444.186126	26.845199	66.140698
1443.458344	34.274458	66.145703
1442.446130	33.777508	66.150708
1441.510819	25.936290	66.155713
1440.483576	32.949853	66.160718
1440.111717	32.601051	66.165722
1440.038581	32.430057	66.170727
1439.093514	36.325884	66.175732
1439.130383	35.850285	66.180737
1438.337284	40.204817	66.185742
1437.548121	27.877079	66.190746
1436.396964	28.289661	66.195751
1435.477220	38.149298	66.200756
1435.318234	33.577676	66.205761
1434.882950	35.297398	66.210766
1433.911432	36.057373	66.215770
1433.306799	26.345432	66.220775
1432.460001	28.938051	66.225780
1432.321014	24.949166	66.230785
1430.923922	29.684169	66.235790
1430.091777	33.109900	66.240794
1429.603281	38.440143	66.245799
1428.799657	36.150996	66.250804
1428.218687	33.620853	66.255809
1427.744675	34.871174	66.260814
1427.672795	34.013549	66.265818
1427.130287	30.251223	66.270823
1425.786962	38.958552	66.275828
1425.638601	29.467315	66.280833
1424.722458	32.299953	66.285838
1423.617194	36.582397	66.290842
1423.366395	26.712398	66.295847
1422.714038	34.824242	66.300852
1422.116095	29.946457	66.305857
1421.169781	28.133294	66.310862
1420.243781	27.393445	66.315866
1419.779357	30.149159	66.320871
1419.100673	34.517659	66.325876
1419.037133	23.770124	66.330881
1418.480936	33.774760	66.335886
1417.100252	33.642844	66.340890
1416.622954	27.782877	66.345895
1415.979761	35.710004	66.350900
1415.721293	27.924248	66.355905
1414.374702	29.049201	66.360910
1413.788901	29.033455	66.365914
1413.434640	30.963115	66.370919
1412.782308	31.070462	66.375924
1412.491299	29.950754	66.380929
1411.391109	37.641908	66.385934
1410.715820	36.953485	66.390938
1410.469738	30.121222	66.395943
1409.005039	31.382046	66.400948
1408.180756	22.925809	66.405953
1407.954974	26.212228	66.410958
1407.350508	27.623426	66.415962
1407.306765	19.978150	66.420967
1406.415041	28.917241	66.425972
1405.439053	27.128107	66.430977
1405.151956	33.441065	66.435982
1404.183780	34.376517	66.440986
1403.502383	26.337118	66.445991
1402.391642	35.848940	66.450996
1401.940946	28.916709	66.456001
1401.897407	35.152058	66.461006
1401.197632	26.275450	66.466010
1399.850010	29.691133	66.471015
1399.094728	35.486627	66.476020
1398.630660	32.302561	66.481025
1398.451936	26.655558	66.486030
1397.832938	35.219960	66.491034
1396.816820	26.112120	66.496039
1395.736381	30.157433	66.501044
1395.458284	31.642631	66.506049
1395.300770	26.023574	66.511054
1394.446359	26.234984	66.516058
1393.368476	23.323347	66.521063
1392.718350	29.386616	66.526068
1392.517951	27.491567	66.531073
1391.906901	34.604020	66.536078
1391.073257	34.566361	66.541082
1390.584309	35.863450	66.546087
1389.720922	35.843512	66.551092
1388.616299	30.771818	66.556097
1387.750603	38.133903	66.561102
1387.181584	35.388573	66.566106
1386.850210	32.340472	66.571111
1386.442069	35.505351	66.576116
1386.357366	29.801203	66.581121
1385.295172	36.118158	66.586126
1384.649528	40.672445	66.591130
1384.005208	36.817425	66.596135
1382.428186	37.313967	66.601140
1381.876029	37.780337	66.606145
1381.443484	32.762542	66.611150
1380.796227	36.840285	66.616154
1380.691275	38.164799	66.621159
1379.893901	39.870720	66.626164
1378.943549	30.848725	66.631169
1378.844852	40.269025	66.636174
1378.409240	42.487732	66.641178
1377.335767	32.719085	66.646183
1376.306104	35.322884	66.651188
1376.039467	34.278740	66.656193
1374.698989	40.047703	66.661198
1373.751831	39.525816	66.666202
1373.417891	32.464264	66.671207
1372.401502	33.567442	66.676212
1372.322265	33.695900	66.681217
1372.059141	28.627792	66.686222
1371.519310	27.348978	66.691226
1370.793815	31.266437	66.696231
1369.694339	26.793050	66.701236
1369.160087	26.099043	66.706241
1368.701625	29.608835	66.711246
1367.888801	26.435528	66.716250
1367.381793	20.013053	66.721255
1366.415549	32.268300	66.726260
1365.630547	17.822216	66.731265
1364.781602	23.180210	66.736270
1363.991671	38.940771	66.741274
1363.812271	34.288574	66.746279
1363.148436	30.698597	66.751284
1363.170404	23.239829	66.756289
1361.948115	21.655489	66.761294
1361.337986	25.472677	66.766298
1360.874071	27.845826	66.771303
1359.743059	28.330762	66.776308
1358.805905	20.226213	66.781313
1358.515374	28.506635	66.786318
1357.562986	27.335547	66.791322
1357.533563	30.853606	66.796327
1356.984105	26.578163	66.801332
1355.939091	28.238454	66.806337
1355.070933	30.621198	66.811342
1354.517386	30.658356	66.816346
1354.717564	32.538504	66.821351
1352.867747	31.366701	66.826356
1352.251023	20.724527	66.831361
1351.841828	20.044640	66.836366
1351.377409	31.356658	66.841370
1351.033876	21.287032	66.846375
1349.538435	32.541867	66.851380
1349.068225	20.243639	66.856385
1348.669099	29.944688	66.861390
1348.144404	36.863160	66.866394
1347.784962	25.159754	66.871399
1346.974516	34.562549	66.876404
1346.302922	27.994967	66.881409
1345.692285	34.836574	66.886414
1344.488057	37.492366	66.891418
1343.944572	30.754044	66.896423
1343.289808	41.090543	66.901428
1343.383017	20.693353	66.906433
1342.108019	21.856198	66.911438
1341.118442	29.297119	66.916442
1340.486535	20.366281	66.921447
1340.324459	30.679615	66.926452
1338.984252	28.057227	66.931457
1338.645811	27.672714	66.936462
1337.791105	23.335454	66.941466
1337.467488	27.729227	66.946471
1336.857632	29.524626	66.951476
1336.168005	27.572807	66.956481
1335.237497	31.218668	66.961486
1334.667521	33.598924	66.966490
1333.969631	28.790761	66.971495
1333.695534	32.134003	66.976500
1332.882795	31.890679	66.981505
1331.963839	29.018559	66.986510
1331.406688	26.284232	66.991514
1331.141935	24.661112	66.996519
1330.270538	31.809844	67.001524
1329.561573	34.621241	67.006529
1328.713626	36.062286	67.011534
1328.064160	27.777843	67.016538
1328.058362	24.110754	67.021543
1326.789079	32.812132	67.026548
1326.079781	24.182687	67.031553
1325.953236	24.189776	67.036558
1324.812362	29.715376	67.041562
1323.775155	25.227001	67.046567
1322.883670	30.473079	67.051572
1322.724395	26.494384	67.056577
1322.468930	33.780432	67.061582
1321.784301	39.287142	67.066586
1321.365709	26.441288	67.071591
1319.855373	38.477855	67.076596
1319.371196	29.211085	67.081601
1319.137446	33.737100	67.086606
1318.548128	24.006776	67.091610
1317.652844	32.389933	67.096615
1316.534684	33.349498	67.101620
1316.301961	27.302029	67.106625
1316.210810	26.626118	67.111630
1315.216900	25.375703	67.116634
1314.124157	24.467060	67.121639
1313.591116	36.730256	67.126644
1313.305013	30.434173	67.131649
1312.262572	28.778796	67.136654
1311.288688	29.970625	67.141658
1310.955913	23.173349	67.146663
1310.030712	31.140464	67.151668
1309.703650	25.077569	67.156673
1309.496052	26.454389	67.161678
1308.354904	29.208725	67.166682
1307.864451	29.298242	67.171687
1307.067273	37.396201	67.176692
1306.287638	34.629307	67.181697
1305.254343	29.773178	67.186702
1304.626955	35.697568	67.191706
1304.434760	30.584958	67.196711
1303.836247	34.012946	67.201716
1303.678812	30.453127	67.206721
1302.776219	25.933423	67.211726
1302.134253	37.323599	67.216730
1301.328278	20.883850	67.221735
1299.795037	35.612366	67.226740
1299.555247	26.327843	67.231745
1298.943675	21.531754	67.236750
1298.456627	34.665716	67.241754
1298.337841	32.854986	67.246759
1296.889558	38.570186	67.251764
1296.119359	36.437175	67.256769
1295.885062	34.627273	67.261774
1295.602072	35.218486	67.266778
1294.568797	37.836339	67.271783
1293.424319	38.850149	67.276788
1292.990284	35.889101	67.281793
1292.573417	35.516833	67.286798
1291.893717	37.027761	67.291802
1291.283460	32.252760	67.296807
1290.269097	26.594090	67.301812
1289.785926	29.740240	67.306817
1289.313149	37.199273	67.311822
1288.414736	40.189548	67.316826
1287.966869	28.922847	67.321831
1287.137213	38.310385	67.326836
1286.896885	30.833366	67.331841
1286.586292	29.244937	67.336846
1285.147199	38.579313	67.341850
1284.701864	31.382115	67.346855
1284.330124	31.700773	67.351860
1283.105805	31.099253	67.356865
1282.251014	30.393422	67.361870
1281.347677	31.996316	67.366874
1281.255526	34.272673	67.371879
1280.760315	37.451279	67.376884
1280.287079	35.089021	67.381889
1279.237707	34.518338	67.386894
1278.514577	35.049908	67.391898
1278.265049	26.224138	67.396903
1277.787698	38.645556	67.401908
1276.760737	34.467658	67.406913
1276.062051	40.630431	67.411918
1275.221857	40.330240	67.416922
1274.505967	40.187181	67.421927
1273.575761	40.513029	67.426932
1272.944106	35.992734	67.431937
1272.674573	37.795402	67.436942
1272.197661	37.570777	67.441946
1272.002312	31.610855	67.446951
1270.916180	37.876270	67.451956
1269.924387	39.273663	67.456961
1269.560753	32.270103	67.461966
1269.021846	38.151324	67.466970
1268.156296	32.259560	67.471975
1267.162726	35.850705	67.476980
1266.832585	29.858994	67.481985
1266.509513	33.981111	67.486990
1264.679473	34.538767	67.491994
1264.449503	28.772660	67.496999
1263.754892	36.886613	67.502004
1263.301715	37.908392	67.507009
1263.448243	32.038357	67.512014
1262.094308	48.786754	67.517018
1261.543759	39.196630	67.522023
1260.750697	40.560398	67.527028
1260.191178	34.821498	67.532033
1259.834371	31.640402	67.537038
1258.664769	43.750486	67.542042
1257.831051	38.755599	67.547047
1257.416644	40.135065	67.552052
1256.807056	33.355183	67.557057
1256.749891	34.873217	67.562062
1255.547476	29.959215	67.567066
1255.141174	26.316091	67.572071
1254.527184	37.815551	67.577076
1253.198347	37.538232	67.582081
1252.693503	34.931532	67.587086
1251.931831	34.783684	67.592090
1251.633258	27.558211	67.597095
1251.068204	33.792838	67.602100
1250.307179	43.949383	67.607105
1249.904308	41.970983	67.612110
1249.185910	31.363995	67.617114
1248.233032	30.277087	67.622119
1247.539234	30.166170	67.627124
1246.745350	36.736012	67.632129
1246.228379	30.141583	67.637134
1245.613798	39.925703	67.642138
1245.073191	41.121128	67.647143
1244.180169	37.324103	67.652148
1243.568953	32.918335	67.657153
1243.413522	28.215075	67.662158
1242.039003	37.115265	67.667162
1241.380217	29.736339	67.672167
1240.921602	33.083148	67.677172
1240.495539	35.108395	67.682177
1239.943753	38.123409	67.687182
1238.739714	35.922583	67.692186
1238.322564	32.987466	67.697191
1237.838186	36.401051	67.702196
1237.049860	33.325016	67.707201
1236.592522	33.785826	67.712206
1235.915576	39.376486	67.717210
1234.927396	36.398215	67.722215
1234.380673	39.177901	67.727220
1234.129700	30.261598	67.732225
1232.691685	28.527522	67.737230
1232.373094	34.850606	67.742234
1232.244741	37.454460	67.747239
1231.002127	42.399106	67.752244
1230.211256	33.077889	67.757249
1229.838972	31.048075	67.762254
1229.243297	38.200928	67.767258
1228.747764	30.206321	67.772263
1227.444308	33.715531	67.777268
1226.666806	27.113213	67.782273
1226.651410	26.078168	67.787278
1226.042936	30.332432	67.792282
1225.643990	22.568781	67.797287
1224.273500	29.354175	67.802292
1223.771683	32.190116	67.807297
1223.380931	32.394012	67.812302
1222.468482	38.143407	67.817306
1221.639745	26.742201	67.822311
1220.871265	27.203388	67.827316
1220.545888	33.210281	67.832321
1219.776232	23.220737	67.837326
1219.465755	31.617065	67.842330
1218.648712	33.037836	67.847335
1217.818769	37.664344	67.852340
1217.431378	33.840757	67.857345
1216.679687	29.425888	67.862350
1215.724760	30.175563	67.867354
1215.125018	20.852423	67.872359
1214.594676	33.448688	67.877364
1214.101628	33.344852	67.882369
1213.663275	26.306728	67.887374
1212.531843	36.516818	67.892378
1212.223673	30.806339	67.897383
1211.151532	29.141071	67.902388
1210.059751	32.521286	67.907393
1209.573460	27.513113	67.912398
1208.905585	35.375398	67.917402
1208.718871	24.088085	67.922407
1208.390469	36.160329	67.927412
1207.344610	32.068969	67.932417
1206.840523	25.531157	67.937422
1205.788027	25.711777	67.942426
1205.280040	26.056925	67.947431
1205.190480	31.913317	67.952436
1203.715919	30.103011	67.957441
1203.557268	28.641331	67.962446
1203.012522	36.943171	67.967450
1202.442862	28.646671	67.972455
1201.210354	31.312860	67.977460
1200.424318	24.446760	67.982465
1200.169746	25.325203	67.987470
1199.449873	32.312618	67.992474
1198.440710	27.290551	67.997479
1198.064518	28.866757	68.002484
1197.271730	29.756825	68.007489
1197.079749	21.717757	68.012494
1195.966069	35.138202	68.017498
1195.375998	32.036521	68.022503
1194.689911	26.267202	68.027508
1194.353971	25.482818	68.032513
1193.531362	27.861340	68.037518
1192.755913	32.784031	68.042522
1192.190113	27.383704	68.047527
1191.686950	32.232541	68.052532
1191.019710	34.160932	68.057537
1190.168446	31.026607	68.062542
1189.509367	34.928372	68.067546
1189.056462	20.080501	68.072551
1187.854087	29.963673	68.077556
1186.905915	37.860135	68.082561
1186.798182	29.236273	68.087566
1186.065974	36.477632	68.092570
1186.032838	28.752007	68.097575
1184.818898	25.113359	68.102580
1183.872519	22.586213	68.107585
1183.589975	27.317544	68.112590
1182.769547	27.431596	68.117594
1182.732699	25.977483	68.122599
1181.436196	36.766074	68.127604
1180.687444	32.474255	68.132609
1180.641960	22.850578	68.137614
1179.941334	24.221819	68.142618
1178.767398	21.057879	68.147623
1177.932832	34.656709	68.152628
1177.538442	27.399495	68.157633
1177.480991	22.465531	68.162638
1175.993681	28.481501	68.167642
1175.208536	21.803141	68.172647
1174.833864	28.716848	68.177652
1174.270983	38.060296	68.182657
1174.004532	26.159432	68.187662
1173.026353	31.084863	68.192666
1172.251756	26.798656	68.197671
1171.949435	30.125023	68.202676
1171.451960	31.191496	68.207681
1170.406867	27.233036	68.212686
1169.669403	28.368229	68.217690
1169.299895	28.442183	68.222695
1168.292500	24.540029	68.227700
1166.841640	28.657881	68.232705
1166.713818	28.514017	68.237710
1166.379814	27.693778	68.242714
1165.837241	26.834648	68.247719
1165.142713	33.061843	68.252724
1164.536317	25.222804	68.257729
1163.892232	14.600363	68.262734
1163.263351	28.198707	68.267738
1162.519312	16.799207	68.272743
1161.839179	27.317271	68.277748
1160.787291	26.091815	68.282753
1160.348092	30.516038	68.287758
1159.955049	29.086597	68.292762
1159.053276	22.608200	68.297767
1158.559116	29.653676	68.302772
1157.864989	29.681374	68.307777
1157.879303	36.367044	68.312782
1156.427424	30.563066	68.317786
1155.524733	25.501467	68.322791
1155.145714	32.463680	68.327796
1154.527983	31.145338	68.332801
1153.527459	29.195466	68.337806
1152.349199	30.670989	68.342810
1152.521280	34.813324	68.347815
1151.995981	34.409504	68.352820
1151.379267	28.025188	68.357825
1151.164795	20.894669	68.362830
1149.985909	31.794169	68.367834
1149.611876	26.792442	68.372839
1148.171789	30.349140	68.377844
1147.304840	31.487560	68.382849
1146.882419	19.797349	68.387854
1146.570016	30.254427	68.392858
1146.110755	28.261617	68.397863
1145.610661	23.907102	68.402868
1144.295229	28.362938	68.407873
1143.907530	29.998351	68.412878
1143.311613	31.667047	68.417882
1142.994755	25.782023	68.422887
1141.572331	30.105002	68.427892
1141.021110	32.643107	68.432897
1140.968669	22.953130	68.437902
1140.029998	26.404241	68.442906
1139.342069	18.758767	68.447911
1138.442953	23.384493	68.452916
1137.561783	26.500118	68.457921
1137.836434	21.219967	68.462926
1136.962472	29.358316	68.467930
1135.971875	27.486481	68.472935
1135.193540	28.946029	68.477940
1134.923382	27.743433	68.482945
1133.684126	19.924345	68.487950
1132.734767	22.080642	68.492954
1132.385984	26.605825	68.497959
1131.589671	25.950795	68.502964
1131.188344	26.463599	68.507969
1131.056208	21.547952	68.512974
1130.400830	24.515975	68.517978
1129.495715	17.613839	68.522983
1128.847503	25.025937	68.527988
1128.467803	26.504463	68.532993
1127.706619	22.308729	68.537998
1126.703648	29.042266	68.543002
1126.505501	31.429528	68.548007
1125.329648	30.250567	68.553012
1124.538594	32.460283	68.558017
1124.132059	31.714437	68.563022
1123.586868	31.877288	68.568026
1123.209196	24.423811	68.573031
1122.078584	21.291546	68.578036
1121.167447	25.668687	68.583041
1121.108050	25.401798	68.588046
1120.057314	36.554085	68.593050
1119.279970	25.591325	68.598055
1118.635140	25.279026	68.603060
1117.752544	28.450158	68.608065
1117.331630	24.242345	68.613070
1116.875938	27.741414	68.618074
1116.302562	24.688991	68.623079
1115.350312	25.088112	68.628084
1114.954230	24.308900	68.633089
1114.574648	15.432012	68.638094
1113.532983	27.464537	68.643098
1112.574728	24.268816	68.648103
1112.086535	21.581527	68.653108
1111.892408	29.570317	68.658113
1111.263867	15.643419	68.663118
1110.026602	32.661162	68.668122
1109.637045	26.680831	68.673127
1109.027379	23.602257	68.678132
1108.125919	25.892060	68.683137
1107.213849	22.615804	68.688142
1106.759946	22.558563	68.693146
1106.289621	22.194281	68.698151
1105.545932	27.929394	68.703156
1105.174709	23.640446	68.708161
1104.261131	25.488663	68.713166
1103.241127	28.934366	68.718170
1103.034051	25.012818	68.723175
1102.622363	26.594317	68.728180
1101.750418	31.773133	68.733185
1100.833618	28.872668	68.738190
1100.311044	34.387959	68.743194
1099.789879	29.803385	68.748199
1099.235227	28.801470	68.753204
1097.945186	33.042585	68.758209
1097.728386	27.366606	68.763214
1097.082880	24.414163	68.768218
1096.693514	25.590414	68.773223
1095.692650	27.704224	68.778228
1094.810019	36.328777	68.783233
1094.605908	32.998401	68.788238
1093.782811	29.967819	68.793242
1092.766128	27.025252	68.798247
1092.212525	23.903925	68.803252
1091.474814	30.648097	68.808257
1091.363205	21.229560	68.813262
1090.393897	24.419491	68.818266
1089.976488	23.851159	68.823271
1089.246239	22.280923	68.828276
1088.637624	28.094351	68.833281
1087.687085	24.434706	68.838286
1086.784118	26.515966	68.843290
1086.486220	27.541562	68.848295
1085.849233	23.651790	68.853300
1085.013322	33.821553	68.858305
1084.325415	22.441274	68.863310
1083.418141	26.246210	68.868314
1083.099287	18.879770	68.873319
1082.645207	25.458933	68.878324
1082.180835	27.758367	68.883329
1081.415778	19.432200	68.888334
1080.738578	30.312510	68.893338
1080.022609	28.325377	68.898343
1079.265370	31.341241	68.903348
1077.919185	35.092263	68.908353
1077.796008	20.283877	68.913358
1077.095408	30.271003	68.918362
1076.732242	25.932522	68.923367
1076.164978	30.469068	68.928372
1075.053807	27.136521	68.933377
1074.707977	23.091505	68.938382
1074.032759	39.455282	68.943386
1073.471791	24.488184	68.948391
1072.585712	30.861073	68.953396
1071.600118	33.696973	68.958401
1071.681372	20.771906	68.963406
1070.535988	33.595844	68.968410
1069.530148	30.113821	68.973415
1069.238859	32.835964	68.978420
1068.464550	33.140680	68.983425
1068.303829	22.849152	68.988430
1067.619108	33.130783	68.993434
1066.873344	24.712107	68.998439
1066.351064	29.286342	69.003444
1065.503616	17.811028	69.008449
1064.657564	17.741997	69.013454
1063.390680	27.824905	69.018458
1063.401804	20.743789	69.023463
1062.832585	18.651404	69.028468
1061.721748	26.927814	69.033473
1061.056460	29.042191	69.038478
1060.492926	29.452125	69.043482
1060.035376	22.709012	69.048487
1059.795903	24.101559	69.053492
1058.695499	26.251761	69.058497
1058.077629	19.052180	69.063502
1057.390743	27.282442	69.068506
1056.719284	22.038779	69.073511
1056.237535	22.610752	69.078516
1055.247224	23.397698	69.083521
1054.704633	14.709778	69.088526
1054.251515	30.478173	69.093530
1053.062606	16.415548	69.098535
1052.484913	20.616396	69.103540
1051.756351	26.859292	69.108545
1052.033933	23.215528	69.113550
1051.266261	21.703019	69.118554
1050.200975	22.695426	69.123559
1049.639785	26.844899	69.128564
1048.821120	24.896277	69.133569
1048.086325	15.746296	69.138574
1047.038135	22.240097	69.143578
1046.713209	28.838591	69.148583
1046.296619	22.437396	69.153588
1045.593763	21.144304	69.158593
1045.015591	23.936492	69.163598
1044.254595	25.145990	69.168602
1043.925650	14.511455	69.173607
1042.844077	21.824878	69.178612
1041.578863	25.265609	69.183617
1041.178458	25.412754	69.188622
1040.286673	27.237119	69.193626
1040.592573	29.009544	69.198631
1040.032606	16.227838	69.203636
1039.135918	23.719197	69.208641
1038.362931	23.184919	69.213646
1037.500777	27.033843	69.218650
1037.023863	24.782766	69.223655
1036.004351	27.419622	69.228660
1034.982335	28.389623	69.233665
1034.966355	23.679870	69.238670
1034.552733	30.200005	69.243674
1033.874665	31.801074	69.248679
1033.124987	25.506652	69.253684
1031.869804	26.644470	69.258689
1031.774754	25.660567	69.263694
1031.386673	30.736797	69.268698
1030.210556	27.125661	69.273703
1029.431595	23.876363	69.278708
1028.556245	29.846387	69.283713
1028.820850	20.392644	69.288718
1027.813410	28.217560	69.293722
1026.919390	26.610645	69.298727
1026.287244	21.984302	69.303732
1025.634139	32.063950	69.308737
1025.431172	20.444733	69.313742
1024.143729	21.716360	69.318746
1023.243089	21.319990	69.323751
1022.862592	26.998837	69.328756
1022.550909	27.032901	69.333761
1021.910422	24.691028	69.338766
1021.101275	29.104795	69.343770
1020.563261	33.589365	69.348775
1020.457696	19.670034	69.353780
1018.721235	30.326758	69.358785
1018.086826	13.487095	69.363790
1017.673540	30.013626	69.368794
1017.585094	26.917253	69.373799
1016.539580	13.699650	69.378804
1015.125819	27.412266	69.383809
1014.984447	25.522526	69.388814
1014.330930	24.142441	69.393818
1014.227090	30.699918	69.398823
1013.181103	31.018010	69.403828
1012.448749	27.966380	69.408833
1011.722550	18.245753	69.413838
1011.421011	26.426606	69.418842
1010.551243	29.622004	69.423847
1009.781360	27.145982	69.428852
1008.928190	37.939991	69.433857
1008.740109	22.858139	69.438862
1007.980223	31.227215	69.443866
1007.040042	25.876033	69.448871
1006.498445	22.181113	69.453876
1006.022029	30.158637	69.458881
1005.744585	14.151093	69.463886
1004.450463	19.162620	69.468890
1003.643546	22.730918	69.473895
1003.270873	18.709455	69.478900
1002.855048	22.402612	69.483905
1001.853335	11.880533	69.488910
1000.956344	24.060781	69.493914
1000.483203	24.203412	69.498919
1000.223115	14.165352	69.503924
999.124076	25.821283	69.508929
998.706939	27.979614	69.513934
997.674477	28.773395	69.518938
997.290316	16.440385	69.523943
996.936954	22.669554	69.528948
995.962693	20.466550	69.533953
995.213447	17.621097	69.538958
994.713535	26.983361	69.543962
994.088442	19.001912	69.548967
993.022619	27.115894	69.553972
991.985223	24.014670	69.558977
991.973568	30.854370	69.563982
991.356564	25.028660	69.568986
991.272274	25.306402	69.573991
990.308997	23.075861	69.578996
989.104669	26.510913	69.584001
988.904307	20.178088	69.589006
988.379273	34.980297	69.594010
987.104952	27.308963	69.599015
986.592848	25.985187	69.604020
985.792276	21.992400	69.609025
985.613658	16.417261	69.614030
984.831058	23.079130	69.619034
983.749902	28.451673	69.624039
983.362198	17.351576	69.629044
982.728719	19.563534	69.634049
982.704238	22.113283	69.639054
981.622337	23.807986	69.644058
980.985106	20.457062	69.649063
980.412928	18.664390	69.654068
979.431752	22.009915	69.659073
978.724191	22.053754	69.664078
978.000456	15.083099	69.669082
977.470295	20.652186	69.674087
976.877704	23.589342	69.679092
975.826866	21.699046	69.684097
975.273961	15.900652	69.689102
974.744452	24.755247	69.694106
974.457652	14.395334	69.699111
973.667790	11.467636	69.704116
972.755530	27.534902	69.709121
972.368887	20.493887	69.714126
971.694366	17.562619	69.719130
970.533855	20.255998	69.724135
970.228427	27.275472	69.729140
969.278003	29.062920	69.734145
969.044411	19.396883	69.739150
968.452699	33.831186	69.744154
967.659344	17.981863	69.749159
967.143529	18.988340	69.754164
966.466904	24.983544	69.759169
965.550327	20.227906	69.764174
964.732298	26.585993	69.769178
964.173322	21.112701	69.774183
963.625408	19.949395	69.779188
962.989119	22.423533	69.784193
961.907137	14.694409	69.789198
961.367778	22.934143	69.794202
960.700592	22.862128	69.799207
960.661985	16.184254	69.804212
959.951251	27.902763	69.809217
959.074893	18.143922	69.814222
958.128361	32.217037	69.819226
957.464528	23.144127	69.824231
957.416204	16.876449	69.829236
955.910234	23.617599	69.834241
955.460939	22.629237	69.839246
955.118634	22.279754	69.844250
954.959212	10.905322	69.849255
954.180933	17.172919	69.854260
953.129106	20.281482	69.859265
952.573120	14.433492	69.864270
951.128266	24.240199	69.869274
950.607511	20.582373	69.874279
950.055124	15.806605	69.879284
949.452487	20.435262	69.884289
949.410992	22.879377	69.889294
948.760950	31.474764	69.894298
947.833556	23.065909	69.899303
947.057869	19.182153	69.904308
946.434760	29.515203	69.909313
946.234028	18.913196	69.914318
944.788728	30.598438	69.919322
943.913303	30.314601	69.924327
943.949400	23.259214	69.929332
943.149370	24.605273	69.934337
942.675192	22.934368	69.939342
941.922462	31.577340	69.944346
941.096258	24.596607	69.949351
941.105895	21.852896	69.954356
939.762401	34.522101	69.959361
939.285360	21.764896	69.964366
938.633979	26.094025	69.969370
937.973040	19.099202	69.974375
937.308222	23.692723	69.979380
936.298405	24.644471	69.984385
935.706428	16.647892	69.989390
935.158895	23.803953	69.994394
934.417040	28.238967	69.999399
933.627367	23.204248	70.004404
932.697955	30.675963	70.009409
932.506959	21.023950	70.014414
932.140962	26.731497	70.019418
931.697105	27.080293	70.024423
930.582891	27.393904	70.029428
929.943241	30.316625	70.034433
929.619770	24.178170	70.039438
928.167998	32.527200	70.044442
927.358542	36.445270	70.049447
927.030875	25.254374	70.054452
926.363396	32.656760	70.059457
926.285420	23.978101	70.064462
925.783394	29.838413	70.069466
924.405272	27.296454	70.074471
923.822197	24.123359	70.079476
923.393139	22.501567	70.084481
923.103554	13.755740	70.089486
922.145608	25.393435	70.094490
921.462550	31.425271	70.099495
920.863346	16.125316	70.104500
919.630533	21.143729	70.109505
919.096397	22.465963	70.114510
918.126775	30.282048	70.119514
917.997679	32.097780	70.124519
917.850891	22.935934	70.129524
916.678624	26.046580	70.134529
915.999050	29.807017	70.139534
915.335792	30.312200	70.144538
914.798144	27.327895	70.149543
914.385758	23.792033	70.154548
913.064534	30.756543	70.159553
912.671360	25.852068	70.164558
912.184166	26.823255	70.169562
911.512311	26.308780	70.174567
910.833962	20.524776	70.179572
909.788202	29.457527	70.184577
909.940101	19.205242	70.189582
909.050011	20.338584	70.194586
907.989926	24.546275	70.199591
907.182257	16.812026	70.204596
906.576796	29.153525	70.209601
906.399253	21.106891	70.214606
905.830909	25.606922	70.219610
904.549093	26.656575	70.224615
904.059096	22.583773	70.229620
903.514954	30.776571	70.234625
903.144748	16.343669	70.239630
902.087321	19.069536	70.244634
900.922210	27.731428	70.249639
900.692940	20.901880	70.254644
900.270853	19.975965	70.259649
900.235988	22.360131	70.264654
898.751237	24.209105	70.269658
898.096060	31.056782	70.274663
897.790256	14.957414	70.279668
896.621082	22.022980	70.284673
896.278002	20.688423	70.289678
895.494068	25.142094	70.294682
895.211489	28.518768	70.299687
894.780780	9.088082	70.304692
893.200942	30.410068	70.309697
892.563963	25.469593	70.314702
892.427236	21.433784	70.319706
892.081540	21.422763	70.324711
890.917078	18.431350	70.329716
889.796070	28.944407	70.334721
889.807520	23.048184	70.339726
889.233202	24.783072	70.344730
887.960622	20.057243	70.349735
887.217485	19.739312	70.354740
886.746058	22.244430	70.359745
886.442510	12.806301	70.364750
886.208088	18.552491	70.369754
885.148504	22.286836	70.374759
884.647867	17.377879	70.379764
884.062891	21.864181	70.384769
882.731478	16.075199	70.389774
882.026392	22.436843	70.394778
881.818759	25.779760	70.399783
881.619372	26.676790	70.404788
880.742772	23.822776	70.409793
879.744128	14.843547	70.414798
879.052990	20.182066	70.419802
878.243191	22.869869	70.424807
877.362321	14.775948	70.429812
876.677603	27.038262	70.434817
876.362290	15.118596	70.439822
875.776302	29.055358	70.444826
875.089790	25.640658	70.449831
874.756652	18.147229	70.454836
873.583489	21.760509	70.459841
873.043301	19.441348	70.464846
872.573208	26.815847	70.469850
871.680557	31.953634	70.474855
870.678522	21.036535	70.479860
869.822675	31.344321	70.484865
869.797122	26.219396	70.489870
869.279520	20.317084	70.494874
868.834183	20.093406	70.499879
868.509514	16.502267	70.504884
867.375228	33.604225	70.509889
866.752308	16.104649	70.514894
865.768253	19.375689	70.519898
864.531057	25.266397	70.524903
864.747202	20.966478	70.529908
864.004859	26.825717	70.534913
863.815887	17.195869	70.539918
862.594685	28.125936	70.544922
861.481174	22.327268	70.549927
861.453406	20.477286	70.554932
860.504445	22.376206	70.559937
859.471595	17.260399	70.564942
859.002012	15.476222	70.569946
858.485589	19.086752	70.574951
858.573097	22.834620	70.579956
857.184875	18.226892	70.584961
856.107889	13.712693	70.589966
855.903231	19.585226	70.594970
855.832585	15.602836	70.599975
855.027358	13.611294	70.604980
853.707786	20.831699	70.609985
853.575489	13.745168	70.614990
852.966334	18.457443	70.619994
851.644177	21.500227	70.624999
850.545702	19.541150	70.630004
850.136383	29.587334	70.635009
849.879115	15.776910	70.640014
849.453063	16.381597	70.645018
848.583623	19.877732	70.650023
848.708174	18.278358	70.655028
847.322421	24.511075	70.660033
846.981316	19.686504	70.665038
846.292614	28.840327	70.670042
844.876810	30.330159	70.675047
844.775403	29.407741	70.680052
843.930136	22.186364	70.685057
843.859953	16.785682	70.690062
843.029261	16.014623	70.695066
841.719966	21.538361	70.700071
841.956014	10.424614	70.705076
840.855252	23.673925	70.710081
840.070661	18.724800	70.715086
839.609659	28.285256	70.720090
839.102922	21.002346	70.725095
838.011230	15.072062	70.730100
836.927482	21.785524	70.735105
836.547632	17.841491	70.740110
836.238861	15.244289	70.745114
835.785679	13.452176	70.750119
834.977083	19.838261	70.755124
834.069568	28.821548	70.760129
833.713349	7.001146	70.765134
832.563762	12.025054	70.770138
831.595546	28.788317	70.775143
831.124339	22.427298	70.780148
830.514258	20.461543	70.785153
830.186166	20.237523	70.790158
830.171997	18.603096	70.795162
828.828837	15.720856	70.800167
828.168281	13.510734	70.805172
827.510032	17.370941	70.810177
827.641446	9.207065	70.815182
826.305334	18.816755	70.820186
825.253968	19.238433	70.825191
825.155591	9.563869	70.830196
824.196202	21.129582	70.835201
823.273679	12.117203	70.840206
822.445352	12.007680	70.845210
821.598107	14.776109	70.850215
821.628284	4.444038	70.855220
820.964638	13.305025	70.860225
820.683969	15.332233	70.865230
819.793110	14.374126	70.870234
819.035733	25.058971	70.875239
818.936352	21.249257	70.880244
817.450915	21.876728	70.885249
816.679639	17.880933	70.890254
816.057611	18.024612	70.895258
815.811645	23.805937	70.900263
815.553362	20.289480	70.905268
814.574322	19.527652	70.910273
814.012610	10.887268	70.915278
812.683174	11.579987	70.920282
811.370781	15.870775	70.925287
811.414576	14.068930	70.930292
810.844240	20.117381	70.935297
810.323032	19.058066	70.940302
810.085390	23.006091	70.945306
809.236371	24.855140	70.950311
808.553189	18.716346	70.955316
807.413253	17.236856	70.960321
807.094382	20.539619	70.965326
806.800527	15.988393	70.970330
805.301144	24.885175	70.975335
804.847789	10.059594	70.980340
804.525282	12.130677	70.985345
803.898090	16.306469	70.990350
803.433232	16.505724	70.995354
802.248814	17.881331	71.000359
801.638009	7.203156	71.005364
800.865248	18.255744	71.010369
800.848486	15.975218	71.015374
799.979454	23.309898	71.020378
799.105504	25.571355	71.025383
798.454001	15.678131	71.030388
797.679407	18.602268	71.035393
797.401925	17.062679	71.040398
796.578296	19.578792	71.045402
795.797146	17.828649	71.050407
795.227405	17.749044	71.055412
794.390051	15.690784	71.060417
793.687020	17.540485	71.065422
793.281390	25.405626	71.070426
792.823022	19.669619	71.075431
792.223523	17.778631	71.080436
791.155344	24.701002	71.085441
790.604330	21.494806	71.090446
790.409438	19.512804	71.095450
788.788781	25.033444	71.100455
788.374848	9.346161	71.105460
787.713136	17.070435	71.110465
787.437873	17.013807	71.115470
786.922126	17.103760	71.120474
785.537753	19.728161	71.125479
785.054557	13.885100	71.130484
784.598658	24.523831	71.135489
784.269086	15.504626	71.140494
783.180568	21.988794	71.145498
782.549989	23.057576	71.150503
782.117029	13.889512	71.155508
781.625359	19.135059	71.160513
780.553828	25.450539	71.165518
780.128988	17.643640	71.170522
779.261775	23.822285	71.175527
779.264508	19.478795	71.180532
777.958920	21.867084	71.185537
777.677841	19.398557	71.190542
776.701318	13.373963	71.195546
775.552574	24.910147	71.200551
774.931683	6.681224	71.205556
773.874273	18.491874	71.210561
773.708653	19.899410	71.215566
773.473458	15.874952	71.220570
772.768815	21.096589	71.225575
772.698482	8.739480	71.230580
771.645171	10.985087	71.235585
770.657691	10.849548	71.240590
770.247181	14.139194	71.245594
769.443535	14.521609	71.250599
768.544127	5.943424	71.255604
767.737785	19.259141	71.260609
767.365755	15.179574	71.265614
767.187394	13.893388	71.270618
765.924679	23.426180	71.275623
765.480124	19.359430	71.280628
764.722278	14.156281	71.285633
764.564881	17.093509	71.290638
763.628278	15.754059	71.295642
762.356445	17.132413	71.300647
762.417412	6.000116	71.305652
761.659310	21.765461	71.310657
760.516635	11.402994	71.315662
759.755188	16.346614	71.320666
759.134749	29.967582	71.325671
758.701806	19.577872	71.330676
758.487368	30.719162	71.335681
758.276838	21.642858	71.340686
756.990265	18.908043	71.345690
756.019042	22.536490	71.350695
755.989116	14.828124	71.355700
754.683748	21.802575	71.360705
754.156189	23.229088	71.365710
753.700544	22.357880	71.370714
752.937579	34.624131	71.375719
751.963076	21.570496	71.380724
751.198230	20.796857	71.385729
751.037851	17.186666	71.390734
750.369786	9.850101	71.395738
749.929099	17.492309	71.400743
749.208314	15.026084	71.405748
748.209475	21.208333	71.410753
747.762424	20.350258	71.415758
746.852850	23.328313	71.420762
745.599662	16.557346	71.425767
745.383414	23.076433	71.430772
744.998043	27.718018	71.435777
744.681855	21.021397	71.440782
744.411167	15.739933	71.445786
743.169639	24.657686	71.450791
742.828715	12.239174	71.455796
741.285180	27.012947	71.460801
740.524932	22.234925	71.465806
740.486890	16.869006	71.470810
739.902717	25.114843	71.475815
739.354679	16.196618	71.480820
737.943554	21.531780	71.485825
737.163112	15.729777	71.490830
737.462452	24.078464	71.495834
736.821671	23.022668	71.500839
736.019601	15.144616	71.505844
734.853119	20.066444	71.510849
734.525949	10.762644	71.515854
733.972378	11.218667	71.520858
732.623794	21.119048	71.525863
732.162705	12.196984	71.530868
731.581979	9.158512	71.535873
731.390756	19.703744	71.540878
730.600752	11.409967	71.545882
729.302831	15.897231	71.550887
728.754214	10.959021	71.555892
728.387840	17.870513	71.560897
727.801979	20.060131	71.565902
727.639883	17.479259	71.570906
726.461226	20.373944	71.575911
725.866931	24.911589	71.580916
725.419112	13.740139	71.585921
724.698126	19.922159	71.590926
723.393301	18.714475	71.595930
722.708684	22.644732	71.600935
722.257580	18.870410	71.605940
721.914181	15.241445	71.610945
721.436763	23.716087	71.615950
721.421833	10.481909	71.620954
720.228190	17.354336	71.625959
719.814057	5.754383	71.630964
718.078854	17.342086	71.635969
717.693717	18.025823	71.640974
717.478527	11.427955	71.645978
716.727747	23.615930	71.650983
715.517273	16.049805	71.655988
714.700095	22.539210	71.660993
714.295592	20.456944	71.665998
714.105605	22.733476	71.671002
713.600686	26.014433	71.676007
712.911421	18.415466	71.681012
711.867815	14.848034	71.686017
711.306664	21.275422	71.691022
710.895024	18.134964	71.696026
709.740209	19.442367	71.701031
709.053845	21.280541	71.706036
708.261702	12.364670	71.711041
707.962489	16.825318	71.716046
707.747619	13.616418	71.721050
706.629491	10.917497	71.726055
706.349528	8.536414	71.731060
705.351884	26.282821	71.736065
704.880537	16.794522	71.741070
704.182676	14.081629	71.746074
703.132153	24.606708	71.751079
702.881986	18.520066	71.756084
702.345002	15.674224	71.761089
701.422246	12.965123	71.766094
700.651896	13.958390	71.771098
700.236714	15.579986	71.776103
699.485578	13.323038	71.781108
698.434769	20.308756	71.786113
698.052157	20.283548	71.791118
697.331092	13.907730	71.796122
696.769111	21.823731	71.801127
696.286370	12.131742	71.806132
695.122000	15.214238	71.811137
694.516619	17.439965	71.816142
694.319770	9.914536	71.821146
693.524632	18.323215	71.826151
692.847622	11.866040	71.831156
691.911515	26.571286	71.836161
691.355448	24.909701	71.841166
691.245010	24.397365	71.846170
689.930227	26.128866	71.851175
689.487631	18.102800	71.856180
688.711784	17.870632	71.861185
688.283360	13.585616	71.866190
687.580805	14.230185	71.871194
686.564579	21.914152	71.876199
686.284782	13.550743	71.881204
685.793873	16.437743	71.886209
685.452554	24.540141	71.891214
684.494563	13.692928	71.896218
683.968912	25.233293	71.901223
682.755891	13.037216	71.906228
682.176309	16.861460	71.911233
681.222251	14.856371	71.916238
681.263142	17.567009	71.921242
679.982466	19.275301	71.926247
678.906900	10.159323	71.931252
678.228156	19.420778	71.936257
677.911586	20.712868	71.941262
677.793370	13.372511	71.946266
676.849722	12.328743	71.951271
676.821876	7.754856	71.956276
675.773656	16.963165	71.961281
675.200242	19.986662	71.966286
674.723785	9.374312	71.971290
673.938466	18.614158	71.976295
673.309186	7.868920	71.981300
672.451321	16.412681	71.986305
671.292865	19.444041	71.991310
670.457325	13.121391	71.996314
669.733804	19.470024	72.001319
669.633702	20.177166	72.006324
669.060732	15.975728	72.011329
668.586720	20.949455	72.016334
668.412463	16.807993	72.021338
667.027795	18.237673	72.026343
666.426174	7.689003	72.031348
665.947226	11.322728	72.036353
664.407876	7.929050	72.041358
663.934024	8.183934	72.046362
663.315528	14.388265	72.051367
663.198015	12.902987	72.056372
662.877877	13.541251	72.061377
662.112417	10.432602	72.066382
661.371748	6.370812	72.071386
660.767548	13.726838	72.076391
659.702766	6.430629	72.081396
658.928279	4.818311	72.086401
658.104279	14.975784	72.091406
657.874406	10.509925	72.096410
657.594696	16.052303	72.101415
656.621908	15.657706	72.106420
655.591867	13.236190	72.111425
655.194237	15.396331	72.116430
654.687493	4.039220	72.121434
653.495919	12.635414	72.126439
653.288545	11.174215	72.131444
652.198723	8.013775	72.136449
651.938084	10.039530	72.141454
651.505587	3.072347	72.146458
650.583606	9.708384	72.151463
650.094417	9.981686	72.156468
649.069752	12.798297	72.161473
648.556800	12.960019	72.166478
647.722435	13.530864	72.171482
647.004772	16.924846	72.176487
647.075710	6.685276	72.181492
645.909041	12.781031	72.186497
644.948089	18.470119	72.191502
644.627564	14.608310	72.196506
643.753552	14.597034	72.201511
643.591313	12.993111	72.206516
643.035588	18.109908	72.211521
641.630423	18.793149	72.216526
641.360875	12.830225	72.221530
640.524942	16.952982	72.226535
640.153507	12.062586	72.231540
639.379302	11.277150	72.236545
638.536199	18.571482	72.241550
638.480410	13.966858	72.246554
637.206711	16.973366	72.251559
636.401239	13.017413	72.256564
636.240039	13.380569	72.261569
635.541333	17.981104	72.266574
634.536332	6.221491	72.271578
633.368832	22.048684	72.276583
633.404389	14.524495	72.281588
632.941401	11.608359	72.286593
632.359272	12.798718	72.291598
631.376809	10.580625	72.296602
630.411760	17.941242	72.301607
629.752736	7.237425	72.306612
629.594984	17.474957	72.311617
628.750133	15.610634	72.316622
627.581334	15.005691	72.321626
626.760719	11.908076	72.326631
626.960179	11.264497	72.331636
626.400115	19.021889	72.336641
625.979891	16.510114	72.341646
625.049175	12.345108	72.346650
624.175833	18.530739	72.351655
623.469476	13.124994	72.356660
622.533670	12.039634	72.361665
621.892702	17.038807	72.366670
622.042722	12.967313	72.371674
620.893626	19.012304	72.376679
620.086881	10.678795	72.381684
619.150534	11.723012	72.386689
618.220808	12.053241	72.391694
618.442238	11.011182	72.396698
617.713141	13.130619	72.401703
616.732855	16.726694	72.406708
616.175231	12.810778	72.411713
615.524855	18.457317	72.416718
615.465753	13.586041	72.421722
614.292442	12.248100	72.426727
613.899834	13.681108	72.431732
613.170891	15.275549	72.436737
611.866647	9.307938	72.441742
611.208558	12.380681	72.446746
610.435810	11.187260	72.451751
610.195409	13.940561	72.456756
609.829456	14.804955	72.461761
609.257960	18.780575	72.466766
608.370278	21.771873	72.471770
607.603641	24.500078	72.476775
607.247554	17.325210	72.481780
605.882722	14.790549	72.486785
605.400661	22.908769	72.491790
604.826075	12.809400	72.496794
604.195229	21.669123	72.501799
604.149176	15.490290	72.506804
603.275766	17.121325	72.511809
602.183585	16.080128	72.516814
601.965140	13.831005	72.521818
600.388293	18.030579	72.526823
599.824212	13.223717	72.531828
599.232791	13.412308	72.536833
598.770300	15.819209	72.541838
598.650266	15.169581	72.546842
598.103877	17.588488	72.551847
597.608090	27.437912	72.556852
597.029162	22.510440	72.561857
596.077516	23.009815	72.566862
594.855934	9.788194	72.571866
593.916614	24.527936	72.576871
593.297235	13.826805	72.581876
592.897885	12.548098	72.586881
592.578561	14.714166	72.591886
591.644557	17.728796	72.596890
590.937455	16.059552	72.601895
590.477241	11.037540	72.606900
590.135282	7.385452	72.611905
589.239457	12.753536	72.616910
588.219387	14.762576	72.621914
587.705711	16.451578	72.626919
587.690965	19.977357	72.631924
586.317684	22.130593	72.636929
585.355901	20.263420	72.641934
584.877239	18.822653	72.646938
584.565844	21.194195	72.651943
584.099128	10.483885	72.656948
583.383514	14.055932	72.661953
582.450261	12.635820	72.666958
582.288551	2.453093	72.671962
581.203872	21.055937	72.676967
580.143652	9.669333	72.681972
579.488843	19.506526	72.686977
579.028739	23.512009	72.691982
578.695151	15.074547	72.696986
578.529813	18.738620	72.701991
577.587962	7.598565	72.706996
576.655543	20.045017	72.712001
575.555280	13.851426	72.717006
574.908335	11.477575	72.722010
573.713236	20.295824	72.727015
573.605008	8.362846	72.732020
573.467073	13.359910	72.737025
572.951051	13.374542	72.742030
572.504258	11.357166	72.747034
571.071970	18.851527	72.752039
570.640978	16.490016	72.757044
570.205765	16.512907	72.762049
569.354752	25.222077	72.767054
568.459846	11.545437	72.772058
567.944203	13.735670	72.777063
567.669288	21.214091	72.782068
566.515538	19.927676	72.787073
565.545929	19.493082	72.792078
565.311027	13.045837	72.797082
564.505525	18.301746	72.802087
564.452635	10.464710	72.807092
563.064602	18.077009	72.812097
562.168957	22.097515	72.817102
561.915826	10.382380	72.822106
561.768931	21.266168	72.827111
560.929148	21.687966	72.832116
559.971329	14.989605	72.837121
559.178399	19.044219	72.842126
559.099639	15.108234	72.847130
557.816916	18.220116	72.852135
556.873424	20.808113	72.857140
556.654373	23.896030	72.862145
555.859863	28.121433	72.867150
555.985311	25.734842	72.872154
555.048346	22.619677	72.877159
554.097730	19.658027	72.882164
553.346129	18.093513	72.887169
552.662308	25.989346	72.892174
552.561334	19.934787	72.897178
550.909587	19.240121	72.902183
550.494141	23.403734	72.907188
550.344848	16.756305	72.912193
549.802259	25.198301	72.917198
549.051928	14.677898	72.922202
548.313661	24.389666	72.927207
547.953834	19.538341	72.932212
546.855596	27.396240	72.937217
545.515209	20.788297	72.942222
545.253510	21.772194	72.947226
544.578397	22.298403	72.952231
544.282929	23.428604	72.957236
543.821434	23.904397	72.962241
542.759208	30.183191	72.967246
542.081667	17.877653	72.972250
541.485474	27.036557	72.977255
541.258633	28.960612	72.982260
540.132917	23.647655	72.987265
539.428871	28.573177	72.992270
539.073652	26.554323	72.997274
538.329468	21.550973	73.002279
537.523160	22.280836	73.007284
536.852829	16.087796	73.012289
535.951470	25.439111	73.017294
536.346681	23.243916	73.022298
534.932213	15.094288	73.027303
534.137372	19.328827	73.032308
533.440261	18.597300	73.037313
533.147539	24.099281	73.042318
532.481405	18.631796	73.047322
531.459823	18.299267	73.052327
530.551273	10.833439	73.057332
530.425801	20.580330	73.062337
529.755930	12.448773	73.067342
529.174798	15.215856	73.072346
528.308132	18.583279	73.077351
527.935269	18.466815	73.082356
527.517482	13.746208	73.087361
525.892383	20.519713	73.092366
525.737399	15.148584	73.097370
524.848578	22.914947	73.102375
524.660942	18.249241	73.107380
523.561371	15.995188	73.112385
522.618473	11.385083	73.117390
522.253596	12.021549	73.122394
522.015085	18.350638	73.127399
521.494818	17.005819	73.132404
520.262495	20.692462	73.137409
519.623543	28.176423	73.142414
519.073838	18.988939	73.147418
518.847800	16.692178	73.152423
517.927159	14.331682	73.157428
517.147186	18.613805	73.162433
516.570103	16.271806	73.167438
515.549833	12.488071	73.172442
514.343594	25.322877	73.177447
513.873409	21.119245	73.182452
513.776749	14.980273	73.187457
513.331471	23.730840	73.192462
512.744618	13.912656	73.197466
512.617778	20.617325	73.202471
511.337682	18.662613	73.207476
511.114394	21.999926	73.212481
509.658028	25.190124	73.217486
509.012609	21.839104	73.222490
508.249659	23.326893	73.227495
507.757903	13.333347	73.232500
507.575806	13.136041	73.237505
506.349355	17.539270	73.242510
506.062034	13.161422	73.247514
505.370258	19.273721	73.252519
504.643455	22.480613	73.257524
503.791431	19.247885	73.262529
502.925423	16.196361	73.267534
502.764240	15.918107	73.272538
502.239188	26.723016	73.277543
501.437935	12.666424	73.282548
500.995077	13.788332	73.287553
500.359514	19.932444	73.292558
499.094162	10.852202	73.297562
498.518693	22.034409	73.302567
497.688446	14.722135	73.307572
497.057931	7.461688	73.312577
496.585512	18.102844	73.317582
495.676621	15.920724	73.322586
494.855041	15.547617	73.327591
494.364187	19.162474	73.332596
494.180278	20.930366	73.337601
493.841182	21.890819	73.342606
492.672202	16.029929	73.347610
491.611528	15.616086	73.352615
491.275192	15.288114	73.357620
491.056459	20.584005	73.362625
490.281023	25.230465	73.367630
489.230307	14.401571	73.372634
488.671301	18.812797	73.377639
487.794801	11.403459	73.382644
487.602061	11.965829	73.387649
486.238965	17.521358	73.392654
485.855727	8.882435	73.397658
485.371657	9.793917	73.402663
484.873099	24.000270	73.407668
484.346568	10.983653	73.412673
483.333328	19.609316	73.417678
482.897984	5.245314	73.422682
482.288839	18.774731	73.427687
481.769310	13.766056	73.432692
481.132982	12.514546	73.437697
480.041496	19.598050	73.442702
479.644043	11.666916	73.447706
478.413400	17.266062	73.452711
478.203464	12.465639	73.457716
477.509615	9.696050	73.462721
476.923467	16.636122	73.467726
475.951920	-1.276437	73.472730
475.187959	9.981479	73.477735
474.661506	6.193265	73.482740
474.634314	5.013421	73.487745
473.591982	14.822682	73.492750
472.932885	12.992477	73.497754
472.102408	16.961172	73.502759
471.662378	14.392023	73.507764
470.928046	15.266659	73.512769
469.584711	20.586716	73.517774
469.435598	5.275301	73.522778
469.198141	9.472357	73.527783
468.657369	11.691771	73.532788
467.489307	15.923565	73.537793
466.281528	15.555066	73.542798
466.047770	6.137024	73.547802
465.754507	6.373218	73.552807
465.295881	6.344872	73.557812
464.218599	9.536037	73.562817
463.472356	24.496500	73.567822
463.398414	10.760924	73.572826
462.148505	14.774258	73.577831
461.183424	18.942457	73.582836
460.988975	13.318771	73.587841
460.171761	13.153331	73.592846
460.095543	9.765175	73.597850
459.108711	20.446721	73.602855
457.967966	22.033596	73.607860
457.522049	14.967693	73.612865
457.112330	21.531371	73.617870
456.733324	10.266090	73.622874
455.515935	21.846437	73.627879
454.862630	19.201342	73.632884
454.379537	13.151883	73.637889
453.951101	23.231327	73.642894
452.858730	14.593930	73.647898
452.149631	21.133914	73.652903
451.692673	20.716490	73.657908
451.394274	17.065634	73.662913
450.187414	31.349948	73.667918
449.933708	20.278703	73.672922
449.189283	30.491243	73.677927
448.764484	25.777371	73.682932
447.613445	13.238415	73.687937
446.384665	27.581347	73.692942
446.459711	15.175292	73.697946
445.936095	17.643596	73.702951
445.126273	13.601198	73.707956
444.589845	15.123595	73.712961
443.395560	27.421920	73.717966
443.311878	13.386848	73.722970
442.616921	14.912333	73.727975
441.884370	16.480970	73.732980
441.078643	20.372801	73.737985
440.021219	23.688459	73.742990
440.218145	19.988642	73.747994
439.530379	25.550031	73.752999
438.563259	24.178380	73.758004
438.016923	15.731217	73.763009
437.507705	19.352382	73.768014
436.381662	12.666306	73.773018
435.572564	17.695490	73.778023
435.079881	16.637253	73.783028
434.684700	15.684275	73.788033
433.991771	14.510758	73.793038
433.250036	14.656448	73.798042
432.329932	15.697522	73.803047
432.280789	12.671416	73.808052
431.601587	17.171134	73.813057
430.449638	26.224763	73.818062
429.838914	18.049540	73.823066
428.979773	21.185571	73.828071
428.992596	17.589536	73.833076
428.402552	21.698604	73.838081
427.240951	22.482265	73.843086
426.595125	8.186711	73.848090
425.389671	10.978690	73.853095
424.919273	7.142985	73.858100
424.621241	10.381795	73.863105
424.069368	27.224891	73.868110
423.983098	13.438935	73.873114
422.832744	19.991778	73.878119
421.772988	32.460070	73.883124
421.965367	21.990109	73.888129
420.640893	31.049230	73.893134
419.775288	16.792517	73.898138
419.268032	23.132925	73.903143
418.881820	19.225952	73.908148
418.154239	14.858431	73.913153
416.689048	21.373655	73.918158
416.547861	20.259922	73.923162
415.929912	21.502626	73.928167
415.511709	18.783698	73.933172
415.006499	12.744747	73.938177
413.760788	24.229697	73.943182
413.353077	15.401172	73.948186
412.632226	16.261665	73.953191
412.576513	13.420228	73.958196
411.713389	23.842569	73.963201
410.898747	25.261472	73.968206
410.250888	13.338891	73.973210
409.380052	16.865721	73.978215
408.475815	15.859069	73.983220
408.004451	13.557388	73.988225
406.853194	21.639509	73.993230
407.089916	10.488576	73.998234
406.589697	20.650183	74.003239
405.566434	14.526732	74.008244
404.707894	14.529427	74.013249
404.135563	23.828314	74.018254
404.099558	15.337910	74.023258
402.665179	19.112491	74.028263
401.923512	22.563506	74.033268
401.489469	18.246731	74.038273
400.762592	22.702127	74.043278
400.083878	20.234675	74.048282
399.004973	28.741744	74.053287
398.484195	24.081826	74.058292
398.215134	12.828501	74.063297
397.976492	18.647246	74.068302
397.658419	14.168107	74.073306
396.964135	19.279061	74.078311
395.401620	11.778903	74.083316
394.594846	20.789958	74.088321
393.459323	20.876041	74.093326
393.240041	17.088088	74.098330
392.961901	20.725310	74.103335
392.586673	17.417608	74.108340
392.180899	15.990030	74.113345
390.918282	20.635915	74.118350
390.350690	14.647919	74.123354
389.973491	21.067085	74.128359
388.606962	22.241512	74.133364
388.286557	19.236633	74.138369
387.285158	25.513314	74.143374
387.261915	17.248473	74.148378
386.668948	21.032407	74.153383
385.472045	21.387153	74.158388
384.898510	14.972701	74.163393
384.108625	30.685473	74.168398
383.863509	24.223418	74.173402
382.851049	20.848089	74.178407
382.084679	23.067493	74.183412
381.734555	17.985199	74.188417
381.029037	24.825743	74.193422
380.883007	21.956365	74.198426
379.592103	22.942186	74.203431
378.836554	22.891317	74.208436
378.695589	17.961062	74.213441
378.175129	25.414459	74.218446
376.932285	26.220739	74.223450
376.338848	25.160040	74.228455
375.853873	20.531883	74.233460
375.307414	14.175158	74.238465
373.918677	23.366867	74.243470
373.597583	23.211545	74.248474
373.093033	20.045210	74.253479
372.525619	29.422201	74.258484
372.435542	23.692218	74.263489
371.343439	26.969624	74.268494
370.174754	19.029764	74.273498
369.932816	19.803057	74.278503
369.148330	23.750465	74.283508
368.351436	20.539896	74.288513
367.678901	27.974754	74.293518
367.060996	19.157786	74.298522
366.875585	17.314309	74.303527
365.654555	23.016432	74.308532
365.146787	20.754544	74.313537
364.226609	28.062511	74.318542
364.364280	20.573336	74.323546
363.362275	20.925475	74.328551
362.390720	21.627637	74.333556
361.350565	21.940922	74.338561
361.316490	24.164294	74.343566
361.111577	24.471796	74.348570
359.910888	18.809790	74.353575
359.225539	30.324631	74.358580
358.842142	15.624531	74.363585
357.576353	19.514302	74.368590
356.653649	16.285826	74.373594
356.152867	26.716727	74.378599
355.933250	20.144524	74.383604
355.540629	14.143520	74.388609
355.138352	27.261327	74.393614
354.482879	18.859328	74.398618
353.648249	14.269392	74.403623
352.248709	27.109321	74.408628
351.570485	11.206934	74.413633
350.679579	19.947033	74.418638
350.657584	17.814646	74.423642
350.214167	15.075181	74.428647
349.914393	19.863938	74.433652
349.011442	6.962789	74.438657
348.011487	18.284844	74.443662
347.684860	11.360744	74.448666
346.740766	9.852545	74.453671
345.963868	19.289115	74.458676
345.393617	21.080593	74.463681
344.671876	14.583397	74.468686
344.441427	19.155417	74.473690
343.358749	14.030529	74.478695
342.851931	21.004773	74.483700
342.373040	22.526004	74.488705
341.083467	15.036322	74.493710
340.324845	11.884724	74.498714
340.120067	14.749550	74.503719
339.661780	23.685098	74.508724
338.995004	12.627438	74.513729
337.678673	13.509476	74.518734
337.257456	13.882075	74.523738
336.975375	12.728944	74.528743
336.387895	12.945706	74.533748
335.688770	6.212943	74.538753
334.680980	14.137860	74.543758
334.317346	9.640882	74.548762
333.975464	3.436201	74.553767
332.678750	12.631482	74.558772
331.892788	8.333983	74.563777
331.174786	15.488095	74.568782
330.544821	17.129555	74.573786
330.488847	20.173735	74.578791
328.981674	16.103650	74.583796
328.712361	15.336334	74.588801
328.023449	13.686516	74.593806
327.991783	13.070696	74.598810
327.487725	9.361555	74.603815
325.770223	8.661662	74.608820
325.361169	14.684468	74.613825
324.954501	17.413775	74.618830
324.524710	2.782827	74.623834
324.050509	10.894566	74.628839
323.139487	16.838415	74.633844
322.338334	11.908427	74.638849
320.912561	21.453446	74.643854
320.362883	20.398675	74.648858
320.073302	14.468432	74.653863
320.027058	16.714413	74.658868
319.429059	5.877857	74.663873
318.171612	19.514435	74.668878
317.180421	12.697923	74.673882
316.856891	16.073336	74.678887
316.425430	15.700105	74.683892
316.256705	1.475574	74.688897
314.972916	13.558731	74.693902
314.687283	14.479638	74.698906
313.772847	19.099416	74.703911
313.184650	8.985478	74.708916
312.722657	9.702942	74.713921
311.749311	15.792859	74.718926
310.924640	12.610353	74.723930
309.686142	11.568647	74.728935
308.834750	18.924429	74.733940
308.972849	11.364140	74.738945
308.550549	21.013475	74.743950
308.129271	11.652855	74.748954
307.263246	23.727574	74.753959
306.008303	10.631385	74.758964
305.608214	10.030160	74.763969
305.011857	17.450383	74.768974
304.932252	14.653306	74.773978
303.783663	13.957750	74.778983
303.064425	12.905597	74.783988
302.802320	13.614854	74.788993
301.655692	16.216789	74.793998
300.681740	9.381540	74.799002
300.504287	13.691859	74.804007
299.959840	13.943090	74.809012
299.598529	6.518527	74.814017
298.621881	19.966463	74.819022
297.857811	12.694212	74.824026
297.347089	15.370306	74.829031
296.265037	11.186321	74.834036
295.448889	12.024087	74.839041
295.038068	16.506238	74.844046
294.553038	6.862490	74.849050
294.029705	9.915327	74.854055
293.114045	14.632416	74.859060
292.645287	12.064266	74.864065
292.076679	16.277426	74.869070
291.522109	15.405066	74.874074
290.205514	13.710081	74.879079
289.383130	18.592358	74.884084
289.208881	9.574644	74.889089
288.879291	18.525233	74.894094
288.335613	15.743358	74.899098
287.083545	9.395886	74.904103
286.400890	15.178236	74.909108
286.096675	10.360835	74.914113
285.520024	21.986901	74.919118
284.579567	15.483393	74.924122
283.732293	17.426561	74.929127
282.767174	13.061100	74.934132
282.824200	15.846715	74.939137
282.228316	21.387631	74.944142
281.178714	14.156428	74.949146
280.992465	12.600451	74.954151
279.925973	14.311999	74.959156
279.526757	7.675073	74.964161
278.379192	10.169417	74.969166
277.518917	10.392288	74.974170
277.235358	10.505654	74.979175
276.616592	19.825920	74.984180
276.560891	6.142907	74.989185
275.461031	17.443409	74.994190
274.665692	6.605163	74.999194
274.071893	22.803365	75.004199
273.475186	18.583168	75.009204
272.738833	8.091237	75.014209
271.643505	23.615973	75.019214
271.458759	23.002709	75.024218
270.998727	12.427495	75.029223
269.925852	18.777228	75.034228
269.408822	12.233516	75.039233
268.689789	12.209167	75.044238
268.740001	10.735812	75.049242
267.437993	9.149249	75.054247
266.589002	12.380268	75.059252
265.982978	3.572742	75.064257
265.487790	9.445716	75.069262
264.937578	10.589200	75.074266
263.799679	10.598753	75.079271
263.222779	18.388251	75.084276
263.441302	11.778068	75.089281
262.619147	10.258856	75.094286
261.607353	10.797813	75.099290
261.046676	5.711367	75.104295
259.537950	14.846297	75.109300
258.870200	11.985042	75.114305
258.815681	21.027423	75.119310
257.954324	6.057985	75.124314
257.645872	10.139718	75.129319
257.014168	17.065505	75.134324
256.719149	13.770122	75.139329
255.304813	13.531419	75.144334
254.836113	10.710253	75.149338
254.151958	11.749994	75.154343
253.752325	15.446329	75.159348
252.857601	10.548184	75.164353
252.420645	9.613831	75.169358
251.995944	6.129506	75.174362
250.865856	3.082648	75.179367
249.825045	14.376187	75.184372
249.512501	6.581322	75.189377
248.918631	16.610171	75.194382
248.494141	11.216978	75.199386
248.443959	0.880193	75.204391
246.977337	17.660598	75.209396
246.454670	10.312249	75.214401
245.199695	9.791249	75.219406
244.471475	4.299735	75.224410
244.200661	5.205474	75.229415
243.505978	17.295820	75.234420
243.571713	10.870896	75.239425
242.296291	22.463981	75.244430
241.386549	17.028049	75.249434
241.268097	10.192618	75.254439
240.426908	14.290276	75.259444
240.398004	4.549806	75.264449
239.055676	12.006319	75.269454
238.434609	6.760896	75.274458
238.093605	12.489425	75.279463
236.864890	19.198617	75.284468
236.034238	7.043357	75.289473
235.204036	12.950075	75.294478
235.062860	10.121716	75.299482
234.861983	14.950360	75.304487
233.677918	12.019723	75.309492
233.339212	8.034375	75.314497
232.270744	12.545179	75.319502
232.002410	17.729576	75.324506
231.001688	9.933072	75.329511
230.141605	14.385659	75.334516
230.016337	6.520410	75.339521
229.638611	14.262742	75.344526
228.350106	17.646861	75.349530
227.682819	15.388652	75.354535
227.006932	13.032451	75.359540
226.777466	7.542680	75.364545
225.618992	17.008743	75.369550
224.690206	17.020353	75.374554
224.520202	13.684599	75.379559
224.103707	17.249229	75.384564
223.553635	11.494695	75.389569
222.358797	16.675675	75.394574
221.535621	14.758380	75.399578
221.414240	7.739518	75.404583
220.511270	14.630887	75.409588
220.059929	9.192963	75.414593
219.346621	10.574001	75.419598
218.688985	9.279213	75.424602
218.090698	11.427987	75.429607
216.914940	20.266264	75.434612
216.328056	11.871492	75.439617
215.761215	16.188954	75.444622
215.267903	7.746173	75.449626
214.981452	9.193772	75.454631
213.618811	26.267400	75.459636
213.148328	14.310126	75.464641
212.674133	13.263745	75.469646
212.278593	10.902910	75.474650
211.339072	12.395747	75.479655
210.529455	16.116179	75.484660
209.966406	13.596173	75.489665
209.578002	21.410598	75.494670
208.427166	13.552204	75.499674
207.935837	15.587126	75.504679
207.000162	14.332104	75.509684
207.113366	8.662815	75.514689
206.531076	6.970664	75.519694
205.123975	18.011227	75.524698
204.579422	11.352647	75.529703
204.167214	12.976925	75.534708
203.728117	7.308367	75.539713
202.726481	14.116394	75.544718
202.230127	18.505454	75.549722
201.423331	17.856330	75.554727
199.980042	13.815997	75.559732
199.271089	10.166075	75.564737
198.933690	21.597981	75.569742
198.878077	13.750000	75.574746
198.523653	20.074085	75.579751
197.813554	23.614051	75.584756
197.078406	19.155903	75.589761
196.262276	21.638057	75.594766
195.508074	20.122207	75.599770
195.181499	14.362522	75.604775
193.510127	17.176397	75.609780
193.312293	9.781849	75.614785
192.749546	13.294581	75.619790
192.598950	6.539662	75.624794
191.632810	17.145451	75.629799
190.453601	16.113351	75.634804
190.411371	5.764945	75.639809
189.985603	19.342260	75.644814
188.662322	16.624961	75.649818
188.230113	16.430281	75.654823
187.686283	26.369643	75.659828
186.930904	16.606474	75.664833
185.762496	16.390763	75.669838
185.239543	16.324921	75.674842
184.786609	13.441459	75.679847
184.021520	16.969932	75.684852
184.178731	8.483536	75.689857
183.295044	18.475230	75.694862
182.501500	17.255056	75.699866
181.495787	8.011618	75.704871
180.039679	18.044597	75.709876
180.079937	22.488902	75.714881
179.068756	15.949391	75.719886
178.828346	10.969890	75.724890
178.566823	7.559834	75.729895
177.934538	13.720376	75.734900
177.205008	8.086214	75.739905
176.192772	9.734013	75.744910
175.700217	16.808046	75.749914
175.356273	2.521609	75.754919
174.144291	21.217729	75.759924
173.898963	14.574567	75.764929
173.259679	15.676097	75.769934
172.358115	18.896407	75.774938
171.688390	13.458032	75.779943
170.399158	23.883568	75.784948
170.462096	14.452995	75.789953
169.779058	23.433779	75.794958
168.915496	19.852598	75.799962
168.220799	18.970723	75.804967
167.370394	13.558190	75.809972
167.283613	9.886484	75.814977
166.582252	5.184543	75.819982
165.704062	10.023113	75.824986
165.079516	0.687899	75.829991
164.413148	11.017313	75.834996
163.781516	8.742742	75.840001
163.053971	7.555861	75.845006
162.407004	8.033090	75.850010
162.300777	7.094549	75.855015
160.919607	17.491240	75.860020
160.267698	6.097947	75.865025
159.739092	21.438703	75.870030
159.233097	14.048040	75.875034
158.945148	7.981364	75.880039
157.337469	6.711690	75.885044
157.142277	10.425874	75.890049
156.508934	17.828366	75.895054
156.065392	4.831953	75.900058
155.055752	8.339195	75.905063
154.283039	15.133248	75.910068
153.879866	15.258837	75.915073
153.506375	19.074635	75.920078
152.425346	18.395561	75.925082
151.658842	15.479809	75.930087
150.887389	26.472208	75.935092
150.731881	14.091898	75.940097
150.267457	11.307511	75.945102
149.380111	23.742318	75.950106
148.603706	14.080259	75.955111
147.941111	18.468217	75.960116
147.459972	17.811431	75.965121
146.208350	15.546044	75.970126
145.773147	21.010479	75.975130
145.219797	13.721089	75.980135
144.674778	10.939466	75.985140
144.037259	7.291124	75.990145
142.901857	18.013560	75.995150
142.488854	14.665392	76.000154
142.352715	15.208203	76.005159
141.283609	19.778737	76.010164
140.752559	13.138379	76.015169
139.905708	14.231287	76.020174
139.326433	11.197396	76.025178
138.844499	14.181969	76.030183
137.605969	24.028460	76.035188
137.082807	20.820747	76.040193
136.682538	18.527436	76.045198
136.204945	25.669958	76.050202
135.685590	14.298939	76.055207
134.638095	21.562839	76.060212
133.990310	15.758759	76.065217
133.363600	20.280689	76.070222
132.494590	10.347162	76.075226
132.070476	13.307613	76.080231
131.170189	21.643184	76.085236
130.805977	13.557209	76.090241
130.585381	14.512763	76.095246
129.378918	11.554025	76.100250
128.688448	12.674597	76.105255
128.059957	22.485980	76.110260
127.426092	18.356647	76.115265
126.456900	23.094386	76.120270
125.690628	22.565031	76.125274
125.620589	17.246478	76.130279
124.942796	14.707473	76.135284
124.095429	6.777747	76.140289
123.215000	9.255539	76.145294
122.869474	17.697308	76.150298
122.807737	4.764521	76.155303
121.165526	16.155646	76.160308
120.733081	7.614429	76.165313
120.214185	16.586414	76.170318
119.752961	13.881213	76.175322
119.622425	5.481650	76.180327
118.200526	17.609039	76.185332
117.607183	12.154818	76.190337
116.158453	15.187508	76.195342
115.546327	16.917508	76.200346
115.207073	14.117192	76.205351
114.464544	20.742666	76.210356
114.295654	10.125472	76.215361
113.991104	13.483033	76.220366
112.978484	20.758718	76.225370
112.362916	9.636294	76.230375
111.682992	11.366075	76.235380
111.109981	19.790400	76.240385
110.340996	18.834828	76.245390
109.419518	27.921622	76.250394
109.277712	23.807008	76.255399
108.535894	23.631073	76.260404
107.574555	25.754474	76.265409
106.745035	24.522324	76.270414
106.259357	24.355370	76.275418
106.123286	16.996818	76.280423
104.713284	23.910790	76.285428
103.624172	22.340668	76.290433
103.187292	23.306067	76.295438
103.023934	21.447773	76.300442
102.813823	12.173352	76.305447
101.668314	22.137708	76.310452
100.855440	18.770865	76.315457
100.342813	17.375450	76.320462
99.607815	26.448432	76.325466
99.616318	16.405129	76.330471
98.241591	14.278879	76.335476
97.579261	13.600271	76.340481
97.145662	16.179085	76.345486
96.337067	16.124725	76.350490
95.642078	13.251195	76.355495
94.734170	23.500062	76.360500
94.756252	13.366018	76.365505
94.187391	16.547459	76.370510
92.978416	12.504493	76.375514
92.595132	18.877734	76.380519
91.242255	21.016949	76.385524
90.851131	14.791531	76.390529
90.182699	17.318638	76.395534
89.310758	20.641639	76.400538
88.980564	14.436564	76.405543
88.546184	17.911510	76.410548
88.436520	8.168323	76.415553
87.785652	16.101947	76.420558
86.747605	17.652748	76.425562
86.133006	12.727934	76.430567
84.799281	17.288583	76.435572
84.496317	10.801753	76.440577
83.962569	15.559971	76.445582
82.996075	16.900361	76.450586
82.397724	6.898345	76.455591
80.940993	8.743543	76.460596
81.079167	4.162937	76.465601
80.477910	10.896024	76.470606
80.229938	16.305862	76.475610
79.760721	6.353941	76.480615
78.644624	8.949112	76.485620
78.030025	5.508813	76.490625
77.458698	13.951793	76.495630
76.053297	15.050082	76.500634
75.987317	2.814303	76.505639
75.369770	21.615347	76.510644
75.071127	7.008551	76.515649
73.777331	7.042509	76.520654
72.826187	15.133001	76.525658
73.226450	11.367538	76.530663
72.042973	11.957284	76.535668
71.350676	14.114692	76.540673
70.554376	19.776423	76.545678
70.152375	10.103486	76.550682
69.147156	7.676281	76.555687
67.796383	14.108817	76.560692
67.679882	9.145583	76.565697
67.349329	16.347757	76.570702
66.767820	12.751795	76.575706
66.587051	9.966943	76.580711
65.307459	13.216949	76.585716
64.777798	18.752051	76.590721
64.133118	13.765691	76.595726
63.149218	16.209921	76.600730
62.372102	7.900295	76.605735
61.496478	9.658897	76.610740
61.284190	9.360609	76.615745
60.565115	6.399248	76.620750
60.501607	10.908304	76.625754
59.454427	11.507842	76.630759
58.863247	13.327014	76.635764
58.157985	12.011207	76.640769
57.875592	17.945994	76.645774
56.514118	10.968054	76.650778
55.953777	14.871940	76.655783
55.501114	17.377057	76.660788
54.476658	5.351392	76.665793
54.233126	5.691183	76.670798
53.246819	9.947553	76.675802
52.999689	3.422345	76.680807
52.458103	15.083443	76.685812
51.471733	6.333674	76.690817
50.835085	10.691140	76.695822
50.143803	12.081451	76.700826
49.746539	-0.055685	76.705831
48.464279	10.307487	76.710836
47.971862	6.205234	76.715841
47.343348	7.537812	76.720846
46.817264	10.775077	76.725850
46.891807	15.056399	76.730855
45.362323	10.326734	76.735860
44.786487	8.007882	76.740865
44.232999	14.705547	76.745870
43.480183	10.983443	76.750874
42.409369	8.355531	76.755879
41.832572	13.747934	76.760884
41.699912	5.780558	76.765889
41.233485	9.361256	76.770894
40.674341	19.045889	76.775898
39.474937	10.513818	76.780903
38.886698	14.538927	76.785908
38.397628	11.166712	76.790913
37.441729	7.882035	76.795918
36.358915	7.976930	76.800922
36.185057	3.888742	76.805927
35.609862	10.563288	76.810932
35.304234	4.567946	76.815937
34.455448	1.384109	76.820942
33.420066	8.505818	76.825946
33.265618	3.328057	76.830951
32.774036	4.424410	76.835956
31.644896	7.249970	76.840961
30.928972	5.622990	76.845966
30.183682	16.021597	76.850970
30.054125	5.767915	76.855975
29.022036	13.057999	76.860980
28.356537	11.347378	76.865985
28.266391	6.965776	76.870990
26.981671	9.941557	76.875994
26.209376	4.176612	76.880999
24.956466	7.448104	76.886004
25.117965	2.489709	76.891009
25.095551	8.096515	76.896014
23.951638	1.391534	76.901018
23.220212	3.785772	76.906023
22.458092	11.423097	76.911028
20.972021	8.910595	76.916033
20.544049	7.415814	76.921038
19.412237	16.171985	76.926042
19.507795	9.865900	76.931047
18.821169	9.991550	76.936052
18.761017	5.599281	76.941057
18.385599	7.020698	76.946062
17.186946	9.426365	76.951066
16.517335	1.700652	76.956071
16.418857	17.469722	76.961076
15.374635	9.677980	76.966081
14.289546	7.194224	76.971086
13.418530	14.339860	76.976090
13.327752	11.886533	76.981095
12.525061	12.764669	76.986100
11.997498	12.966857	76.991105
11.219586	11.818241	76.996110
10.683123	20.074866	77.001114
10.201733	3.907547	77.006119
9.231909	6.287402	77.011124
8.541186	12.682961	77.016129
8.144445	19.896878	77.021134
7.099320	15.470999	77.026139
6.488713	11.970030	77.031143
5.749910	13.660582	77.036148
5.513641	15.255498	77.041153
4.486373	9.068119	77.046158