3473_Position 111_00017.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: 690-F_400C_1DPA_(ID-415)
Additional Information
| Field | Value |
|---|---|
| Data last updated | February 10, 2026 |
| Metadata last updated | February 10, 2026 |
| Created | February 10, 2026 |
| Format | TXT |
| License | Creative Commons Attribution |
| Datastore active | False |
| Has views | True |
| Id | d1ad9bfc-654a-479c-98b4-fa1dbcd5e779 |
| Mimetype | text/plain |
| Package id | 433e91be-4bc5-48c8-915b-c7525c6bf780 |
| Position | 16 |
| Size | 318.1 KiB |
| State | active |
| Url type | upload |